Mon Mar 08 19:36:31 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.063467	87.864466	0.000000
-0.029598	97.689233	0.005005
-0.633293	60.740798	0.010010
-2.218571	15.828308	0.015014
-6.835078	5.774491	0.020019
-11.637358	2.480264	0.025024
-16.789735	15.600005	0.030029
-21.493792	3.962848	0.035034
-25.616833	-0.355844	0.040038
-29.083700	-0.852878	0.045043
-32.576784	9.055091	0.050048
-36.216088	2.560480	0.055053
-40.091911	17.089732	0.060058
-43.664076	-1.227665	0.065062
-47.645540	14.168362	0.070067
-51.484246	11.015364	0.075072
-54.894181	1.377823	0.080077
-58.960049	5.292192	0.085082
-62.356066	4.312428	0.090086
-66.290159	13.827211	0.095091
-69.926886	3.628251	0.100096
-73.966302	2.527240	0.105101
-77.700526	5.418975	0.110106
-81.309865	6.961519	0.115110
-85.599660	7.899901	0.120115
-89.276649	5.544273	0.125120
-92.602993	5.698219	0.130125
-96.358440	3.526995	0.135130
-100.150406	6.558855	0.140134
-104.263211	5.225194	0.145139
-107.651524	6.630017	0.150144
-111.701397	-1.383685	0.155149
-115.163301	3.881945	0.160154
-118.631762	-1.627465	0.165158
-122.734387	-0.329404	0.170163
-126.580404	-4.993294	0.175168
-130.472446	-4.745879	0.180173
-134.317501	4.196595	0.185178
-138.162786	-5.959508	0.190182
-142.399197	2.774209	0.195187
-145.972353	6.168586	0.200192
-149.256813	-2.213172	0.205197
-152.933015	9.230054	0.210202
-156.669241	1.423404	0.215206
-160.313153	9.625825	0.220211
-164.052072	3.770161	0.225216
-167.818818	-1.445590	0.230221
-171.996076	8.625356	0.235226
-175.102279	0.869574	0.240230
-179.690234	9.567999	0.245235
-183.251952	-0.360491	0.250240
-186.901327	1.311591	0.255245
-190.461878	15.658291	0.260250
-194.018796	9.936042	0.265254
-198.292239	3.995439	0.270259
-201.862312	8.726560	0.275264
-205.607356	7.840545	0.280269
-209.520360	6.670705	0.285274
-213.004394	4.068448	0.290278
-216.971819	9.708191	0.295283
-220.667778	2.516491	0.300288
-224.307710	2.509371	0.305293
-228.276814	-1.037232	0.310298
-232.153180	-1.536420	0.315302
-235.883868	11.464069	0.320307
-239.381054	5.358649	0.325312
-243.133441	2.540667	0.330317
-247.031085	12.899820	0.335322
-250.655753	0.690344	0.340326
-254.525732	17.259394	0.345331
-258.204046	11.916138	0.350336
-262.293196	1.937927	0.355341
-265.880088	6.649749	0.360346
-269.536161	6.074460	0.365350
-273.404821	8.024506	0.370355
-277.133518	-3.465050	0.375360
-280.719083	3.534563	0.380365
-284.748755	13.539562	0.385370
-288.389139	7.151168	0.390374
-292.224279	6.938786	0.395379
-295.781133	10.264551	0.400384
-299.328883	12.194949	0.405389
-303.440353	4.943564	0.410394
-307.151488	-1.220630	0.415398
-311.419981	2.032694	0.420403
-314.895748	11.889395	0.425408
-318.216436	2.449302	0.430413
-322.261999	6.464934	0.435418
-325.761279	-2.714839	0.440422
-329.874911	10.507753	0.445427
-333.423835	-0.280337	0.450432
-337.470447	-4.971775	0.455437
-341.389418	6.504163	0.460442
-344.957105	3.811386	0.465446
-348.756995	11.507585	0.470451
-352.406436	1.997037	0.475456
-355.638469	-4.407558	0.480461
-360.118089	6.546109	0.485466
-363.753013	-2.436920	0.490470
-367.523720	13.296485	0.495475
-371.312558	12.600634	0.500480
-374.851668	3.365797	0.505485
-378.707077	12.059579	0.510490
-382.393601	0.049417	0.515494
-386.253516	0.000402	0.520499
-390.078043	11.377765	0.525504
-393.668010	6.550436	0.530509
-397.578955	14.575078	0.535514
-401.187556	0.359132	0.540518
-405.143253	9.228225	0.545523
-408.575909	1.649462	0.550528
-412.657569	1.027241	0.555533
-416.449045	8.791578	0.560538
-419.965297	2.296848	0.565542
-424.077287	2.904686	0.570547
-427.834938	0.308597	0.575552
-431.172604	0.220410	0.580557
-435.056000	11.055350	0.585562
-438.911037	6.014973	0.590566
-442.679482	6.974805	0.595571
-446.518061	14.048175	0.600576
-450.199685	12.250469	0.605581
-454.348259	18.378378	0.610586
-457.506149	6.283916	0.615590
-461.428760	12.908717	0.620595
-465.254306	4.755744	0.625600
-469.142833	11.471300	0.630605
-472.735234	8.795278	0.635610
-476.141332	5.307401	0.640614
-480.477728	9.866442	0.645619
-484.012936	1.736513	0.650624
-487.622062	9.135970	0.655629
-491.803140	-3.361102	0.660634
-495.453983	7.655964	0.665638
-498.908284	5.970250	0.670643
-502.723918	2.841112	0.675648
-506.563988	13.673972	0.680653
-510.587076	9.739106	0.685658
-513.877962	-4.158414	0.690662
-518.112841	9.922712	0.695667
-521.917465	12.987206	0.700672
-525.232484	1.864041	0.705677
-529.194775	2.066557	0.710682
-532.632584	4.895871	0.715686
-536.597196	-2.041106	0.720691
-540.516003	2.493913	0.725696
-544.290686	8.880765	0.730701
-548.199117	12.720336	0.735706
-551.567868	-5.188753	0.740710
-555.722071	-1.443944	0.745715
-559.428628	1.409416	0.750720
-562.929131	-4.652401	0.755725
-567.265254	16.174880	0.760730
-570.338035	2.807104	0.765734
-574.293565	4.664283	0.770739
-577.892996	0.012207	0.775744
-582.002556	3.407758	0.780749
-585.744618	8.665185	0.785754
-589.220692	-1.542820	0.790758
-593.155202	12.124621	0.795763
-597.372189	7.962283	0.800768
-600.669835	4.040981	0.805773
-604.418612	4.419229	0.810778
-607.890915	6.377445	0.815782
-611.736745	3.846197	0.820787
-615.741505	15.046127	0.825792
-619.800203	-5.460035	0.830797
-623.468011	8.699382	0.835802
-626.728885	2.621451	0.840806
-630.524360	12.614806	0.845811
-634.511309	6.272876	0.850816
-638.132707	10.612313	0.855821
-642.119221	14.967518	0.860826
-645.699380	7.231346	0.865830
-649.591953	13.741268	0.870835
-653.408501	-1.931128	0.875840
-656.909066	11.897289	0.880845
-660.851401	13.716236	0.885850
-664.349427	6.909913	0.890854
-668.816822	7.142911	0.895859
-672.504048	10.119502	0.900864
-675.819458	3.097954	0.905869
-679.533998	9.910606	0.910874
-682.818841	6.920856	0.915878
-686.955179	12.063259	0.920883
-691.062697	-3.054835	0.925888
-694.969372	0.064079	0.930893
-698.863240	5.940398	0.935898
-702.311403	6.975604	0.940902
-706.083193	11.359674	0.945907
-709.693312	15.129758	0.950912
-713.367154	3.289999	0.955917
-717.221395	9.798629	0.960922
-720.716390	11.744867	0.965926
-724.947958	8.018720	0.970931
-729.031796	-0.827324	0.975936
-732.266739	-0.578295	0.980941
-736.210419	6.827679	0.985946
-739.467421	6.600888	0.990950
-743.455844	4.023266	0.995955
-747.412050	6.525761	1.000960
-751.086582	-0.165489	1.005965
-755.073579	13.958404	1.010970
-758.818403	-7.931642	1.015974
-762.535538	6.497603	1.020979
-766.109060	7.288031	1.025984
-769.847608	-4.088736	1.030989
-773.841243	10.006283	1.035994
-777.366056	-2.730743	1.040998
-781.221199	3.215203	1.046003
-785.104164	7.568282	1.051008
-788.551204	3.142893	1.056013
-792.591786	9.958947	1.061018
-796.038196	-9.752250	1.066022
-800.073855	7.047466	1.071027
-804.026297	4.090490	1.076032
-807.498792	4.858524	1.081037
-811.573461	16.664399	1.086042
-815.220877	-0.225246	1.091046
-818.595431	17.288781	1.096051
-822.195675	3.641438	1.101056
-826.006844	4.799500	1.106061
-830.316977	8.363144	1.111066
-834.056107	-0.465276	1.116070
-837.718017	9.254744	1.121075
-841.558217	5.106732	1.126080
-844.734653	-3.313344	1.131085
-849.039786	11.938518	1.136090
-852.335373	2.632400	1.141094
-856.355841	12.551683	1.146099
-860.476541	11.132297	1.151104
-864.329820	3.465371	1.156109
-868.096367	9.666929	1.161114
-871.373345	-1.471247	1.166118
-875.198389	11.989901	1.171123
-878.769509	0.564474	1.176128
-882.636263	5.630994	1.181133
-886.896671	3.842940	1.186138
-890.269530	8.278622	1.191142
-893.893410	-0.579161	1.196147
-897.731733	-0.094675	1.201152
-901.328251	4.772563	1.206157
-905.428939	3.299600	1.211162
-909.074365	-2.721164	1.216166
-912.909668	6.079017	1.221171
-916.729294	12.022655	1.226176
-920.171318	-7.949212	1.231181
-924.274635	5.244286	1.236186
-928.007405	-0.450272	1.241190
-931.636309	3.613280	1.246195
-935.465775	7.048220	1.251200
-939.080322	-4.220361	1.256205
-943.044796	14.014143	1.261210
-946.824006	-2.116244	1.266214
-950.529246	-2.201686	1.271219
-954.505930	2.180841	1.276224
-957.975537	3.645589	1.281229
-961.937539	14.162770	1.286234
-965.140472	-4.319319	1.291238
-969.119408	1.739751	1.296243
-973.476252	3.098843	1.301248
-977.121644	-3.628231	1.306253
-980.739311	16.017313	1.311258
-984.067872	-9.956622	1.316262
-987.860943	6.541257	1.321267
-992.037852	7.901568	1.326272
-995.656041	4.628137	1.331277
-999.516845	6.130279	1.336282
-1003.501671	2.060860	1.341286
-1006.848703	8.649663	1.346291
-1010.375637	-4.354698	1.351296
-1014.128610	4.963859	1.356301
-1018.199645	16.521923	1.361306
-1022.094221	2.048435	1.366310
-1025.789080	6.657220	1.371315
-1029.607817	10.372846	1.376320
-1033.060931	3.395929	1.381325
-1037.291756	20.544180	1.386330
-1040.761790	12.737415	1.391334
-1044.585745	16.528011	1.396339
-1048.227686	6.497059	1.401344
-1051.901039	5.260330	1.406349
-1055.718836	19.717143	1.411354
-1059.623040	11.869477	1.416358
-1063.371057	9.827916	1.421363
-1067.067643	16.467986	1.426368
-1070.670479	2.963392	1.431373
-1074.606114	5.712276	1.436378
-1078.182489	12.093456	1.441382
-1082.269015	11.328108	1.446387
-1085.695520	-0.889595	1.451392
-1089.051236	-2.154999	1.456397
-1093.922033	11.371264	1.461402
-1097.392137	-1.241535	1.466406
-1101.035858	10.803342	1.471411
-1104.782315	3.417763	1.476416
-1108.471774	-0.099530	1.481421
-1112.485765	11.217765	1.486426
-1116.307434	0.272746	1.491430
-1119.885594	5.085337	1.496435
-1123.462405	9.225993	1.501440
-1126.643072	-6.274482	1.506445
-1131.104236	9.371785	1.511450
-1134.883284	1.636688	1.516454
-1138.595744	11.204399	1.521459
-1142.647492	0.898580	1.526464
-1145.647132	-2.232318	1.531469
-1149.796128	0.115624	1.536474
-1153.496050	2.308154	1.541478
-1157.342419	2.720242	1.546483
-1161.360538	6.862182	1.551488
-1164.987313	8.227813	1.556493
-1168.945554	12.033785	1.561498
-1172.271025	-0.029648	1.566502
-1176.048570	0.371459	1.571507
-1179.702076	5.183579	1.576512
-1183.565774	7.537968	1.581517
-1187.715474	3.140469	1.586522
-1191.298813	10.398061	1.591526
-1195.078493	5.182920	1.596531
-1198.789381	-1.936975	1.601536
-1202.125164	11.351762	1.606541
-1206.571487	15.904467	1.611546
-1210.088314	7.113643	1.616550
-1213.723288	8.468047	1.621555
-1217.576432	8.595915	1.626560
-1221.196588	6.068992	1.631565
-1225.151357	6.112219	1.636570
-1228.924616	7.321632	1.641574
-1232.335165	2.597794	1.646579
-1236.732612	17.406229	1.651584
-1240.154709	-2.319152	1.656589
-1244.002937	7.410778	1.661594
-1247.379306	12.309528	1.666598
-1251.099882	5.225957	1.671603
-1255.455027	15.295631	1.676608
-1258.977683	13.797016	1.681613
-1262.725340	6.948012	1.686618
-1266.459740	11.787404	1.691622
-1270.258203	5.690803	1.696627
-1273.766176	0.815478	1.701632
-1277.606695	2.876177	1.706637
-1281.653926	13.278205	1.711642
-1285.217959	11.193369	1.716646
-1288.905708	5.924253	1.721651
-1292.811032	15.746973	1.726656
-1296.318706	2.883489	1.731661
-1300.060451	14.312041	1.736666
-1303.679572	11.444490	1.741670
-1308.158633	11.585966	1.746675
-1312.099158	13.698996	1.751680
-1314.989927	3.699636	1.756685
-1319.091629	6.152262	1.761690
-1322.679423	2.830337	1.766694
-1326.622895	10.112659	1.771699
-1330.495036	15.196531	1.776704
-1334.357310	4.299392	1.781709
-1338.436650	9.071119	1.786714
-1341.495347	12.719196	1.791718
-1345.305852	1.645073	1.796723
-1348.964358	13.093486	1.801728
-1352.503875	4.746458	1.806733
-1356.800592	9.426868	1.811738
-1360.868223	13.372087	1.816742
-1364.311224	5.044317	1.821747
-1368.254725	21.672492	1.826752
-1371.246239	4.798656	1.831757
-1375.399279	12.579768	1.836762
-1379.405293	1.812947	1.841766
-1382.796892	12.319896	1.846771
-1386.881981	6.373450	1.851776
-1390.770769	10.406772	1.856781
-1394.445128	7.847805	1.861786
-1398.033983	10.674163	1.866790
-1401.830325	5.080451	1.871795
-1405.254860	11.792586	1.876800
-1408.973741	5.718171	1.881805
-1413.296378	11.382035	1.886810
-1416.977465	1.827866	1.891814
-1421.045223	13.833873	1.896819
-1424.723833	3.306426	1.901824
-1428.054348	4.479965	1.906829
-1431.884258	20.807799	1.911834
-1435.618641	4.245374	1.916838
-1439.280142	4.871159	1.921843
-1443.438784	8.838975	1.926848
-1447.085953	1.453851	1.931853
-1451.227783	13.116985	1.936858
-1454.631122	0.719566	1.941862
-1457.986072	7.378056	1.946867
-1461.805390	16.349986	1.951872
-1465.386738	-0.139122	1.956877
-1469.617685	12.793454	1.961882
-1473.331778	8.489139	1.966886
-1477.223823	7.038975	1.971891
-1481.027063	18.037717	1.976896
-1484.391363	3.557430	1.981901
-1488.468956	18.070679	1.986906
-1492.116878	15.070859	1.991910
-1495.847982	10.884413	1.996915
-1499.908937	13.614220	2.006912
-1500.839558	10.506333	2.016909
-1497.984238	16.639325	2.026906
-1495.577251	13.407446	2.036902
-1493.185129	12.119911	2.046899
-1491.601583	7.875249	2.056896
-1489.538087	11.414727	2.066893
-1487.512438	5.534651	2.076890
-1485.602530	15.928749	2.086886
-1483.920934	6.624027	2.096883
-1482.153523	11.900274	2.106880
-1479.962620	10.948110	2.116877
-1477.935671	9.412775	2.126874
-1476.208477	2.858975	2.136870
-1474.215478	3.043689	2.146867
-1472.565204	8.627626	2.156864
-1470.619410	8.742540	2.166861
-1468.518036	13.745864	2.176858
-1466.713656	8.300679	2.186854
-1464.633026	8.386113	2.196851
-1462.850079	11.200070	2.206848
-1461.107568	18.212302	2.216845
-1459.385776	10.479988	2.226842
-1457.552974	15.640005	2.236838
-1454.867062	6.572351	2.246835
-1453.348831	7.254653	2.256832
-1451.861268	13.117274	2.266829
-1449.955391	9.803060	2.276826
-1448.100989	5.537161	2.286822
-1445.904903	11.019515	2.296819
-1443.985685	13.151717	2.306816
-1442.318595	18.178819	2.316813
-1440.360201	10.866495	2.326810
-1438.519369	11.580831	2.336806
-1436.234756	5.938785	2.346803
-1434.739152	12.085899	2.356800
-1432.974867	6.157721	2.366797
-1431.136502	9.562786	2.376794
-1429.098599	13.313246	2.386790
-1427.114905	3.230771	2.396787
-1425.229158	5.472550	2.406784
-1423.239234	9.139124	2.416781
-1421.629936	10.997305	2.426778
-1419.534228	7.624303	2.436774
-1417.687453	5.885778	2.446771
-1416.041152	6.486025	2.456768
-1414.079281	4.260163	2.466765
-1412.209629	9.311692	2.476762
-1410.103054	1.873047	2.486758
-1408.404861	5.448982	2.496755
-1406.619975	8.993673	2.506752
-1404.636432	8.196349	2.516749
-1402.603484	9.178355	2.526746
-1400.712713	1.946360	2.536742
-1398.876885	7.495911	2.546739
-1397.083686	3.517724	2.556736
-1395.404343	6.747766	2.566733
-1393.351116	6.412945	2.576730
-1391.166915	2.207967	2.586726
-1389.537522	-1.429802	2.596723
-1388.127232	4.751526	2.606720
-1385.594222	8.365923	2.616717
-1384.091772	11.152223	2.626714
-1382.158998	8.796844	2.636710
-1380.194473	8.231517	2.646707
-1378.262215	12.830981	2.656704
-1376.613279	10.236856	2.666701
-1374.513985	7.455382	2.676698
-1372.686812	4.823254	2.686694
-1370.601078	9.311318	2.696691
-1368.787001	5.937660	2.706688
-1367.272125	6.015863	2.716685
-1365.090356	11.060097	2.726682
-1363.181674	3.095841	2.736678
-1361.366327	6.476230	2.746675
-1359.766856	11.072145	2.756672
-1357.710049	6.211849	2.766669
-1355.865192	6.349333	2.776666
-1353.871693	5.083124	2.786662
-1351.908246	-4.111902	2.796659
-1349.778919	1.749100	2.806656
-1348.307115	10.280965	2.816653
-1346.632947	1.684837	2.826650
-1344.405264	0.959002	2.836646
-1342.470958	4.520875	2.846643
-1340.703851	12.126066	2.856640
-1338.948273	4.397899	2.866637
-1336.908391	5.029932	2.876634
-1335.202894	2.717288	2.886630
-1333.503074	-0.688576	2.896627
-1331.383348	8.037986	2.906624
-1329.460535	-3.518769	2.916621
-1327.526792	-1.180389	2.926618
-1325.698878	4.632576	2.936614
-1323.820283	3.032705	2.946611
-1322.160559	3.442990	2.956608
-1320.205378	0.234664	2.966605
-1318.261488	4.448661	2.976602
-1316.171834	0.743585	2.986598
-1314.521514	5.823989	2.996595
-1312.582036	5.910049	3.006592
-1310.730743	10.699361	3.016589
-1308.896079	4.229518	3.026586
-1307.139346	7.600387	3.036582
-1305.103232	2.569776	3.046579
-1303.105078	11.307933	3.056576
-1301.098184	11.717925	3.066573
-1299.756851	5.898586	3.076570
-1297.460067	5.172788	3.086566
-1295.427608	13.223407	3.096563
-1293.821401	13.774900	3.106560
-1291.792622	4.373681	3.116557
-1290.028251	12.358273	3.126554
-1288.236130	2.671275	3.136550
-1286.292300	1.654635	3.146547
-1284.571004	6.881586	3.156544
-1282.720984	4.501641	3.166541
-1280.543617	11.179179	3.176538
-1278.550148	8.147902	3.186534
-1276.809039	2.989278	3.196531
-1275.162379	7.110367	3.206528
-1273.371362	4.289905	3.216525
-1271.530826	4.363416	3.226522
-1269.493346	5.452176	3.236518
-1267.375953	4.775642	3.246515
-1265.685834	8.959253	3.256512
-1263.511699	7.602637	3.266509
-1262.116575	9.739928	3.276506
-1260.169332	12.691954	3.286502
-1258.080854	6.168895	3.296499
-1256.421187	6.782906	3.306496
-1254.506600	7.013515	3.316493
-1252.392498	19.015566	3.326490
-1250.469561	5.472665	3.336486
-1248.901734	7.852306	3.346483
-1246.806511	8.437670	3.356480
-1245.074118	7.421745	3.366477
-1243.004653	4.526747	3.376474
-1241.317616	4.148038	3.386470
-1239.528489	6.146506	3.396467
-1237.772743	7.637197	3.406464
-1235.825058	10.500758	3.416461
-1233.509934	6.912817	3.426458
-1231.679685	8.860504	3.436454
-1229.993244	9.617081	3.446451
-1227.978310	5.728262	3.456448
-1226.328796	6.511276	3.466445
-1224.841783	6.406149	3.476442
-1222.294593	-1.518081	3.486438
-1220.651162	6.160680	3.496435
-1218.562100	3.409399	3.506432
-1216.882287	5.955866	3.516429
-1214.729451	8.946079	3.526426
-1213.178404	2.126980	3.536422
-1211.473679	-0.087564	3.546419
-1209.288941	4.626372	3.556416
-1207.599354	3.513121	3.566413
-1205.684620	3.445347	3.576410
-1203.607680	2.396424	3.586406
-1201.685889	1.470216	3.596403
-1200.128870	10.203275	3.606400
-1198.239174	8.063344	3.616397
-1196.005467	8.343984	3.626394
-1194.280645	0.390328	3.636390
-1192.502808	5.911441	3.646387
-1190.792752	5.789594	3.656384
-1188.937630	3.887292	3.666381
-1186.811765	5.852446	3.676378
-1184.846532	5.260329	3.686374
-1183.204668	5.106770	3.696371
-1181.276916	10.240775	3.706368
-1179.193667	7.558348	3.716365
-1177.246796	6.958124	3.726362
-1175.753879	4.888012	3.736358
-1173.656418	5.169948	3.746355
-1171.665235	11.856861	3.756352
-1169.923268	5.229855	3.766349
-1167.928162	3.627255	3.776346
-1166.182200	9.295587	3.786342
-1164.173140	6.129288	3.796339
-1162.668141	3.042060	3.806336
-1160.700256	3.881544	3.816333
-1158.781331	5.867203	3.826330
-1156.980951	10.890566	3.836326
-1154.893224	0.821648	3.846323
-1152.900570	4.516447	3.856320
-1151.183377	5.369207	3.866317
-1149.311097	2.726875	3.876314
-1147.477433	13.562932	3.886310
-1145.316120	4.312715	3.896307
-1143.768837	4.505871	3.906304
-1142.067968	3.482435	3.916301
-1139.781541	4.599371	3.926298
-1138.206208	3.817059	3.936294
-1136.390375	6.588123	3.946291
-1133.971687	3.613666	3.956288
-1132.284283	6.138457	3.966285
-1130.681473	4.071318	3.976282
-1128.883536	9.758205	3.986278
-1126.739451	5.168329	3.996275
-1124.681783	9.730586	4.006272
-1123.061854	9.897925	4.016269
-1121.205375	12.340418	4.026266
-1119.283810	5.155803	4.036262
-1117.363263	4.433534	4.046259
-1115.634717	8.323765	4.056256
-1113.597571	2.828968	4.066253
-1111.903555	1.846120	4.076250
-1109.994763	8.138930	4.086246
-1108.026320	-0.354135	4.096243
-1106.034143	-2.110940	4.106240
-1104.283778	11.608805	4.116237
-1102.266387	2.204819	4.126234
-1100.443448	-1.340571	4.136230
-1098.727819	6.634611	4.146227
-1096.968434	1.968942	4.156224
-1094.849769	12.350537	4.166221
-1092.865677	7.318947	4.176218
-1091.152571	8.306607	4.186214
-1089.262729	7.232455	4.196211
-1087.813299	3.178441	4.206208
-1085.475493	15.706945	4.216205
-1083.482727	7.509984	4.226202
-1081.725173	5.943876	4.236198
-1079.993764	7.463842	4.246195
-1078.149431	8.561565	4.256192
-1075.914502	10.255184	4.266189
-1074.338457	10.833759	4.276186
-1072.374760	15.257951	4.286182
-1070.299621	8.116697	4.296179
-1068.652331	9.342254	4.306176
-1066.708912	8.055879	4.316173
-1065.145601	6.164037	4.326170
-1062.776857	6.595298	4.336166
-1060.928534	11.784744	4.346163
-1059.408650	7.534752	4.356160
-1057.241678	9.082955	4.366157
-1055.560768	9.611613	4.376154
-1053.610148	1.380369	4.386150
-1051.881159	13.253185	4.396147
-1049.603032	12.383781	4.406144
-1048.002834	4.909593	4.416141
-1046.004705	8.996744	4.426138
-1044.553185	6.192859	4.436134
-1042.242406	6.038191	4.446131
-1040.520632	8.355463	4.456128
-1038.445742	6.048679	4.466125
-1036.760994	4.802122	4.476122
-1035.101396	7.557208	4.486118
-1033.112286	9.770153	4.496115
-1031.033521	6.655969	4.506112
-1029.198881	-0.850965	4.516109
-1027.274953	7.594610	4.526106
-1025.509487	11.089035	4.536102
-1023.635935	8.152931	4.546099
-1021.610372	5.405661	4.556096
-1019.704484	3.561682	4.566093
-1017.852142	3.627190	4.576090
-1016.226012	-5.939924	4.586086
-1014.201453	8.868073	4.596083
-1012.479707	2.056527	4.606080
-1010.358217	10.334742	4.616077
-1008.655980	7.552356	4.626074
-1006.777518	7.316874	4.636070
-1004.733877	3.201031	4.646067
-1002.989468	3.714835	4.656064
-1001.006983	8.202395	4.666061
-999.126756	5.464177	4.676058
-997.560799	2.061007	4.686054
-995.365623	10.066945	4.696051
-993.434254	8.027872	4.706048
-991.581651	4.627807	4.716045
-990.023525	5.913466	4.726042
-987.782261	2.836486	4.736038
-985.595757	-0.154371	4.746035
-984.581472	5.567964	4.756032
-982.445721	6.374439	4.766029
-980.374317	4.707692	4.776026
-978.677219	5.448539	4.786022
-976.665967	9.626805	4.796019
-974.643629	4.377630	4.806016
-972.807875	2.529115	4.816013
-971.353109	7.067936	4.826010
-969.111297	3.665645	4.836006
-967.235860	5.249500	4.846003
-965.382355	2.288229	4.856000
-963.624520	6.467560	4.865997
-961.473819	3.463503	4.875994
-959.668395	1.501436	4.885990
-958.111541	6.535485	4.895987
-956.220643	4.463442	4.905984
-954.344286	-2.374366	4.915981
-952.120267	-5.200677	4.925978
-950.303589	-3.269541	4.935974
-948.410276	-6.382416	4.945971
-946.384672	-4.910972	4.955968
-944.888311	0.517994	4.965965
-943.056358	2.647206	4.975962
-941.171318	-2.407893	4.985958
-939.333926	-1.116332	4.995955
-937.345953	7.565383	5.005952
-935.198986	8.458524	5.015949
-933.548002	4.339214	5.025946
-931.794592	8.577695	5.035942
-929.747006	2.775082	5.045939
-927.784455	9.934135	5.055936
-926.039324	7.312305	5.065933
-924.248748	6.652023	5.075930
-922.260802	3.533508	5.085926
-920.098913	-1.927396	5.095923
-918.662064	0.176595	5.105920
-916.644382	-0.267379	5.115917
-914.726777	4.516401	5.125914
-912.628930	4.751145	5.135910
-911.081813	-0.205694	5.145907
-909.039801	1.725760	5.155904
-907.398770	3.441874	5.165901
-905.677678	4.718902	5.175898
-903.676552	-2.059878	5.185894
-901.278160	3.235950	5.195891
-899.689292	-0.079249	5.205888
-897.659665	6.249687	5.215885
-896.057489	4.811183	5.225882
-894.178519	0.254424	5.235878
-892.276642	3.755562	5.245875
-890.312307	1.774455	5.255872
-888.567068	9.542985	5.265869
-886.465418	8.338821	5.275866
-884.617271	-6.674399	5.285862
-882.622759	3.179398	5.295859
-881.645804	4.466474	5.305856
-879.291401	8.686275	5.315853
-877.276965	10.453232	5.325850
-875.297074	9.674306	5.335846
-873.325589	3.366045	5.345843
-871.858504	9.301817	5.355840
-869.477209	7.236699	5.365837
-867.881658	9.053264	5.375834
-865.910106	11.365472	5.385830
-864.016633	9.932520	5.395827
-862.124742	1.174001	5.405824
-860.394465	2.901142	5.415821
-858.644591	10.381608	5.425818
-856.391116	4.558769	5.435814
-854.829812	7.233393	5.445811
-853.069726	11.568758	5.455808
-850.959518	-4.147872	5.465805
-848.721050	0.764657	5.475802
-847.142251	5.160583	5.485798
-845.354474	4.335030	5.495795
-843.349602	0.656542	5.505792
-841.527674	10.446400	5.515789
-839.987590	5.253900	5.525786
-837.931341	8.122554	5.535782
-835.731824	2.793064	5.545779
-834.190557	6.906072	5.555776
-832.426873	6.226476	5.565773
-830.035414	4.543431	5.575770
-828.371641	7.558511	5.585766
-826.823123	4.483477	5.595763
-824.670242	6.600955	5.605760
-822.624914	3.189156	5.615757
-821.142879	5.688591	5.625754
-819.135095	4.287926	5.635750
-817.359057	5.971472	5.645747
-814.977316	8.453402	5.655744
-813.476811	9.975745	5.665741
-811.877467	12.004888	5.675738
-809.419524	7.895606	5.685734
-807.729883	8.771972	5.695731
-805.762074	10.851161	5.705728
-804.085084	2.875404	5.715725
-802.440667	12.526314	5.725722
-800.429842	10.632579	5.735718
-798.022261	1.321180	5.745715
-796.635941	5.135318	5.755712
-794.844823	5.217103	5.765709
-792.929026	8.223503	5.775706
-790.635771	7.427715	5.785702
-788.951985	6.561988	5.795699
-787.122163	11.693048	5.805696
-785.370799	8.685084	5.815693
-783.499012	8.952918	5.825690
-781.439461	8.213439	5.835686
-779.584340	4.498942	5.845683
-777.666743	14.903526	5.855680
-776.230530	9.437157	5.865677
-774.035117	10.730045	5.875674
-772.093625	10.715186	5.885670
-770.469518	7.785989	5.895667
-768.150780	6.874052	5.905664
-766.659646	6.331218	5.915661
-764.574839	9.283789	5.925658
-762.776634	10.311772	5.935654
-761.040771	6.862648	5.945651
-758.751388	5.477022	5.955648
-757.250657	14.999367	5.965645
-755.598821	15.558150	5.975642
-753.277012	9.184515	5.985638
-751.400331	14.977547	5.995635
-749.575714	11.710021	6.005632
-748.045605	11.104131	6.015629
-745.542463	10.047489	6.025626
-743.918490	11.502780	6.035622
-742.276762	8.086081	6.045619
-740.071843	5.645094	6.055616
-738.116113	9.289327	6.065613
-736.718815	4.798610	6.075610
-734.746784	5.822517	6.085606
-732.663831	14.823966	6.095603
-730.833002	8.664598	6.105600
-729.155515	11.213380	6.115597
-726.964579	9.527749	6.125594
-725.170270	6.268244	6.135590
-723.543309	8.480916	6.145587
-721.763720	11.708078	6.155584
-719.715340	12.301404	6.165581
-717.597514	10.401690	6.175578
-715.815456	8.792462	6.185574
-713.989502	9.163986	6.195571
-711.876613	11.221649	6.205568
-710.447557	7.946318	6.215565
-708.537899	6.299338	6.225562
-706.228648	10.476013	6.235558
-704.495404	7.276804	6.245555
-702.731374	6.365158	6.255552
-700.812852	8.578621	6.265549
-698.835778	10.143296	6.275546
-697.269458	11.835187	6.285542
-695.190447	9.408045	6.295539
-693.386584	7.023295	6.305536
-691.455830	15.370202	6.315533
-689.753735	8.320441	6.325530
-687.501196	10.913144	6.335526
-685.517024	10.596292	6.345523
-684.063588	11.177356	6.355520
-682.113398	15.967186	6.365517
-680.523605	11.752035	6.375514
-678.267969	11.123408	6.385510
-676.327153	13.132816	6.395507
-674.783436	11.586965	6.405504
-672.661565	12.029650	6.415501
-671.030858	7.141695	6.425498
-669.104755	15.715141	6.435494
-666.939176	12.440560	6.445491
-665.165162	14.312430	6.455488
-663.452454	11.280730	6.465485
-661.437664	15.280307	6.475482
-659.307407	5.800200	6.485478
-657.732188	16.760097	6.495475
-655.924552	11.910192	6.505472
-653.916572	5.616791	6.515469
-651.944951	9.211194	6.525466
-650.169581	20.352264	6.535462
-648.333427	7.924084	6.545459
-646.094344	6.335037	6.555456
-644.634016	9.387495	6.565453
-642.971564	10.759346	6.575450
-640.814765	4.337974	6.585446
-638.813198	9.345406	6.595443
-637.128720	9.261204	6.605440
-635.268520	9.608371	6.615437
-633.278012	9.486327	6.625434
-631.245622	9.559687	6.635430
-629.701940	7.672839	6.645427
-627.834348	10.439201	6.655424
-625.934682	8.686520	6.665421
-623.794866	12.531953	6.675418
-621.838891	5.065909	6.685414
-620.014551	6.260342	6.695411
-618.496267	3.914958	6.705408
-616.750102	9.859999	6.715405
-614.699434	13.222346	6.725402
-612.553260	8.945189	6.735398
-610.620369	6.130964	6.745395
-608.818900	3.072492	6.755392
-606.996637	7.696519	6.765389
-605.151208	5.398345	6.775386
-603.190010	16.143473	6.785382
-601.542481	10.359247	6.795379
-599.726845	4.382388	6.805376
-597.716903	9.914275	6.815373
-595.588904	1.795547	6.825370
-593.760648	2.520458	6.835366
-592.039459	2.774610	6.845363
-590.348732	8.840627	6.855360
-588.550344	7.214674	6.865357
-586.427615	7.311532	6.875354
-584.478228	3.351608	6.885350
-582.385576	0.177169	6.895347
-580.773369	4.264811	6.905344
-578.900902	6.850445	6.915341
-577.133081	8.952304	6.925338
-575.291578	5.914300	6.935334
-573.138337	1.722886	6.945331
-571.155357	5.910769	6.955328
-569.443636	7.511628	6.965325
-567.685352	3.457516	6.975322
-565.824899	7.404467	6.985318
-564.030478	3.744033	6.995315
-562.056178	7.837001	7.005312
-560.228221	9.742963	7.015309
-558.025912	7.469916	7.025306
-556.428656	11.424184	7.035302
-554.330271	12.497529	7.045299
-552.580761	11.037295	7.055296
-551.005838	7.318780	7.065293
-549.319601	18.565748	7.075290
-546.763208	6.399930	7.085286
-544.729367	2.691793	7.095283
-543.462939	5.082175	7.105280
-541.334224	7.037999	7.115277
-539.287912	9.046458	7.125274
-537.913915	10.112376	7.135270
-535.824920	8.736866	7.145267
-533.844892	10.932749	7.155264
-531.849593	5.950333	7.165261
-530.135307	6.911379	7.175258
-528.449041	11.189323	7.185254
-526.240578	2.869915	7.195251
-524.489641	4.725052	7.205248
-522.552851	4.142764	7.215245
-520.727865	4.061463	7.225242
-518.730055	9.050657	7.235238
-516.905871	5.369714	7.245235
-515.265763	7.615169	7.255232
-513.279022	6.243380	7.265229
-511.341204	4.361545	7.275226
-509.604385	8.328290	7.285222
-507.534292	10.580858	7.295219
-505.599503	8.522680	7.305216
-504.159666	7.105627	7.315213
-502.077683	14.740174	7.325210
-499.964435	6.890701	7.335206
-498.163981	8.957410	7.345203
-496.278814	6.381409	7.355200
-494.287397	11.840565	7.365197
-492.264769	9.242612	7.375194
-490.930003	9.286993	7.385190
-488.814120	7.520412	7.395187
-486.980179	0.721287	7.405184
-485.290402	7.889572	7.415181
-483.375177	0.468033	7.425178
-481.340771	4.777247	7.435174
-479.113218	3.051257	7.445171
-477.758775	2.882516	7.455168
-475.615998	6.007659	7.465165
-473.926842	5.771255	7.475162
-472.003348	6.897866	7.485158
-469.819010	4.760391	7.495155
-468.102200	1.931843	7.505152
-466.516858	1.145217	7.515149
-464.303695	5.691145	7.525146
-462.451207	10.514136	7.535142
-460.587803	6.187537	7.545139
-458.840445	7.478068	7.555136
-457.245330	9.206572	7.565133
-455.017801	6.926432	7.575130
-453.074806	8.332558	7.585126
-451.196299	-0.297228	7.595123
-449.492429	5.831530	7.605120
-447.454236	6.444086	7.615117
-445.658907	3.918783	7.625114
-443.720912	2.092234	7.635110
-442.220070	6.069873	7.645107
-440.072496	8.952720	7.655104
-438.121807	6.394719	7.665101
-436.209437	8.039419	7.675098
-434.297283	1.478878	7.685094
-432.570201	13.207280	7.695091
-430.754419	4.510158	7.705088
-428.787158	7.685476	7.715085
-427.018015	8.478373	7.725082
-425.003239	-2.669315	7.735078
-422.987968	2.631365	7.745075
-421.252005	3.585870	7.755072
-419.354967	4.336246	7.765069
-417.429085	6.760334	7.775066
-415.671679	8.420323	7.785062
-414.006169	3.547499	7.795059
-411.704383	3.843274	7.805056
-409.809677	5.891844	7.815053
-408.211727	4.247507	7.825050
-406.246137	5.575858	7.835046
-404.504247	2.793871	7.845043
-402.615161	-1.186280	7.855040
-400.644946	-1.833804	7.865037
-398.979502	3.491180	7.875034
-396.792147	2.340069	7.885030
-394.711196	5.607783	7.895027
-393.057040	-0.033692	7.905024
-391.620204	3.783685	7.915021
-389.590461	1.432560	7.925018
-387.146811	6.811707	7.935014
-385.668345	4.026008	7.945011
-383.795139	7.367952	7.955008
-382.099454	10.098809	7.965005
-379.751375	2.396664	7.975002
-378.030401	6.111845	7.984998
-376.533937	3.179602	7.994995
-374.348915	4.915022	8.004992
-372.313390	6.472220	8.014989
-370.772097	3.128638	8.024986
-368.496232	5.875811	8.034982
-366.999487	1.459411	8.044979
-364.997679	1.572614	8.054976
-363.197026	7.433372	8.064973
-361.318957	16.160020	8.074970
-359.430186	13.616702	8.084966
-357.460237	8.245334	8.094963
-355.353558	10.269579	8.104960
-353.793881	14.927845	8.114957
-351.717321	9.965750	8.124954
-350.176468	11.339855	8.134950
-348.465200	15.650258	8.144947
-345.853210	7.429195	8.154944
-344.241298	11.577052	8.164941
-342.665886	7.309147	8.174938
-340.862451	13.106328	8.184934
-338.603615	8.127775	8.194931
-336.664347	14.171678	8.204928
-334.886326	13.240700	8.214925
-333.047564	13.492059	8.224922
-330.955555	16.279675	8.234918
-329.446227	15.527378	8.244915
-327.663077	14.331917	8.254912
-325.613501	10.430403	8.264909
-323.610488	12.145983	8.274906
-321.750246	15.652671	8.284902
-320.080937	21.575489	8.294899
-318.062551	13.616572	8.304896
-316.242638	9.683838	8.314893
-314.163689	15.504949	8.324890
-312.501352	18.651684	8.334886
-310.695154	15.998434	8.344883
-308.907318	13.000769	8.354880
-306.789173	11.118727	8.364877
-304.597478	11.893205	8.374874
-303.065773	14.492413	8.384870
-301.189597	16.381409	8.394867
-299.201938	16.179577	8.404864
-297.490942	10.890641	8.414861
-295.971206	15.807940	8.424858
-294.020243	10.010203	8.434854
-291.646507	5.104924	8.444851
-289.687770	1.116895	8.454848
-287.994950	3.933535	8.464845
-286.201969	7.106797	8.474842
-284.526892	8.667928	8.484838
-282.411658	3.215010	8.494835
-280.509474	1.721127	8.504832
-278.674248	12.183526	8.514829
-276.861430	5.122669	8.524826
-274.763124	0.976592	8.534822
-273.070152	5.086298	8.544819
-271.069996	5.004066	8.554816
-269.523303	14.936250	8.564813
-267.504107	15.528310	8.574810
-265.337069	6.833645	8.584807
-263.633079	5.475615	8.594803
-261.982496	2.883554	8.604800
-259.974806	8.821871	8.614797
-258.150806	12.201771	8.624794
-256.282573	3.804268	8.634791
-254.112743	12.018677	8.644787
-252.267176	3.702159	8.654784
-250.527654	7.656040	8.664781
-248.635815	10.278322	8.674778
-246.950246	6.493390	8.684775
-244.952817	9.929298	8.694771
-243.031106	9.128601	8.704768
-241.143807	13.887803	8.714765
-239.257700	18.042497	8.724762
-237.482335	10.896068	8.734759
-235.535528	7.820981	8.744755
-233.466247	8.176142	8.754752
-231.733492	15.404082	8.764749
-230.030905	9.481834	8.774746
-228.305663	10.984475	8.784743
-226.139907	11.358979	8.794739
-223.989420	9.152918	8.804736
-222.231727	8.239476	8.814733
-220.472879	8.066333	8.824730
-218.729123	9.933900	8.834727
-216.565969	0.993596	8.844723
-214.660240	1.730117	8.854720
-212.840378	6.212751	8.864717
-211.315017	2.890754	8.874714
-209.145157	3.611966	8.884711
-207.262009	3.137959	8.894707
-205.716055	-1.832485	8.904704
-203.569869	0.537674	8.914701
-201.639120	-0.755456	8.924698
-199.924539	3.972923	8.934695
-198.155454	-5.116038	8.944691
-195.973155	0.410805	8.954688
-194.216350	-1.037706	8.964685
-192.636028	5.976181	8.974682
-190.311759	-2.170387	8.984679
-188.447715	-0.287261	8.994675
-187.093134	1.506653	9.004672
-185.063032	4.706885	9.014669
-183.284811	1.720319	9.024666
-180.977984	0.613491	9.034663
-179.094649	-1.979345	9.044659
-177.352680	-0.242509	9.054656
-175.300449	-4.562718	9.064653
-173.558418	4.522092	9.074650
-171.659609	6.879656	9.084647
-170.067517	1.387163	9.094643
-168.134826	-4.548078	9.104640
-166.024565	0.409272	9.114637
-164.204498	6.844955	9.124634
-162.101255	-0.792662	9.134631
-160.659931	-2.334482	9.144627
-158.917425	1.418477	9.154624
-156.609142	8.583054	9.164621
-154.809170	0.239144	9.174618
-153.009627	2.405732	9.184615
-151.103793	0.714010	9.194611
-149.090787	2.431300	9.204608
-147.607405	-4.908456	9.214605
-145.362394	6.341247	9.224602
-143.462678	3.038497	9.234599
-141.884361	-1.932337	9.244595
-139.843674	2.262501	9.254592
-137.956146	-0.869361	9.264589
-136.121552	8.709103	9.274586
-134.085047	0.960585	9.284583
-132.553519	1.973183	9.294579
-130.373916	2.206624	9.304576
-128.689986	-4.138868	9.314573
-126.812927	0.239976	9.324570
-124.833916	1.231702	9.334567
-122.879813	3.166822	9.344563
-121.254621	3.687669	9.354560
-119.140071	9.441702	9.364557
-117.358603	5.357360	9.374554
-115.438286	8.302029	9.384551
-113.417367	3.778454	9.394547
-111.491406	9.314705	9.404544
-109.889166	16.579356	9.414541
-107.879320	15.453668	9.424538
-106.282298	12.270289	9.434535
-104.439495	12.546440	9.444531
-102.269587	19.584744	9.454528
-100.408935	3.957396	9.464525
-98.671375	15.199704	9.474522
-96.712266	15.059432	9.484519
-94.718148	1.224902	9.494515
-92.944484	-0.357272	9.504512
-91.059800	6.761278	9.514509
-89.114488	9.274112	9.524506
-87.346346	7.575987	9.534503
-85.184647	5.374574	9.544499
-83.793455	6.149082	9.554496
-81.865199	13.784872	9.564493
-79.684233	5.869668	9.574490
-78.110814	2.116950	9.584487
-75.956307	6.131065	9.594483
-74.138380	5.435475	9.604480
-72.368403	6.177978	9.614477
-70.542131	12.571700	9.624474
-68.429197	9.737065	9.634471
-66.629030	10.312135	9.644467
-64.820596	9.453864	9.654464
-62.910920	7.581607	9.664461
-61.130234	14.443636	9.674458
-59.214972	15.248231	9.684455
-57.135455	6.806102	9.694451
-55.341694	12.407701	9.704448
-53.541396	6.913637	9.714445
-51.696003	10.538168	9.724442
-49.988304	9.034438	9.734439
-47.755410	6.798016	9.744435
-46.208045	9.928548	9.754432
-44.252657	14.162345	9.764429
-42.290731	12.220192	9.774426
-40.446211	12.492960	9.784423
-38.251397	5.532367	9.794419
-36.457059	4.509008	9.804416
-34.894040	12.386250	9.814413
-32.919263	10.847821	9.824410
-31.134997	6.763091	9.834407
-29.088694	7.538910	9.844403
-26.966918	11.987744	9.854400
-25.396930	14.394723	9.864397
-23.574603	11.786472	9.874394
-21.983270	16.326243	9.884391
-19.869450	12.110006	9.894387
-17.887269	8.301591	9.904384
-15.812129	12.401052	9.914381
-14.019486	11.955841	9.924378
-12.221189	16.498918	9.934375
-10.393033	11.481990	9.944371
-8.587148	14.437107	9.954368
-6.476234	12.494900	9.964365
-4.873961	15.523550	9.974362
-3.718850	26.217837	9.984359
-2.413772	72.744166	9.994355
-1.233244	124.857606	10.004352
0.000000	186.412195	10.009357
0.470942	209.187436	10.014362
0.828614	253.817185	10.019367
1.512894	293.407337	10.024371
2.112064	314.643767	10.029376
1.989525	345.388785	10.034381
2.671179	361.960348	10.039386
2.930527	388.618780	10.044391
3.304557	408.475222	10.049395
3.346059	415.329719	10.054400
3.144906	416.640760	10.059405
3.360500	412.612232	10.064410
3.300624	426.979404	10.069415
3.558126	431.885118	10.074419
3.790658	447.615403	10.079424
3.959052	463.542009	10.084429
4.074542	454.049755	10.089434
4.247977	452.517845	10.094439
3.866519	466.756585	10.099443
4.223115	463.927641	10.104448
3.846593	469.459604	10.109453
4.077752	468.858310	10.114458
3.991431	466.822229	10.119463
3.906856	473.189106	10.124467
3.996086	467.882940	10.129472
3.913688	474.635808	10.134477
4.418163	468.724111	10.139482
4.057198	485.058439	10.144487
4.391317	501.554716	10.149491
4.459072	510.371454	10.154496
4.128694	514.735481	10.159501
4.264074	522.984797	10.164506
4.613684	525.832197	10.169511
4.761650	518.695332	10.174515
4.814482	521.886526	10.179520
4.824580	529.673300	10.184525
5.237781	514.742117	10.189530
5.182528	522.104088	10.194535
5.051401	530.255575	10.199539
5.094590	524.732813	10.204544
4.879970	529.258146	10.209549
5.081995	526.149504	10.214554
4.984564	529.897658	10.219559
5.256284	527.996839	10.224563
5.357508	536.437685	10.229568
5.240315	535.753187	10.234573
5.149589	551.440533	10.239578
5.260026	532.418271	10.244583
5.200591	530.157127	10.249587
5.358266	546.367797	10.254592
5.018127	544.648148	10.259597
5.594157	535.905521	10.264602
5.255807	548.661491	10.269607
5.206440	543.421558	10.274611
5.492723	546.465138	10.279616
5.345885	551.413312	10.284621
5.642670	545.910014	10.289626
5.396123	549.702458	10.294631
5.597422	564.882785	10.299635
5.748707	576.043703	10.304640
5.747470	583.816545	10.309645
6.160009	588.308090	10.314650
5.951689	590.651582	10.319655
5.809216	593.894445	10.324659
6.186608	585.345893	10.329664
5.903240	597.046074	10.334669
5.840386	592.599879	10.339674
6.009826	599.579131	10.344679
5.826434	598.528310	10.349683
5.947981	600.730882	10.354688
5.836894	601.843075	10.359693
5.851512	597.868630	10.364698
6.122867	629.671023	10.369703
6.368680	624.059136	10.374707
6.524773	627.937182	10.379712
6.337346	636.681163	10.384717
6.494460	627.962725	10.389722
6.421859	638.284220	10.394727
6.206950	642.016449	10.399731
6.506957	643.911450	10.404736
6.579762	643.851057	10.409741
6.987298	635.056401	10.414746
6.610611	645.738633	10.419751
6.544707	644.684837	10.424755
6.996382	662.315266	10.429760
6.820358	674.651227	10.434765
7.257071	676.895001	10.439770
7.093816	673.565479	10.444775
7.270672	675.450166	10.449779
6.982761	665.795044	10.454784
7.113222	658.176790	10.459789
7.223730	670.968502	10.464794
7.165195	685.756751	10.469799
7.167895	686.336728	10.474803
7.478549	680.698707	10.479808
7.442866	702.604660	10.484813
7.576776	688.533112	10.489818
7.531537	688.087859	10.494823
7.466082	696.173771	10.499827
7.241422	690.124405	10.504832
7.593747	692.551947	10.509837
7.713781	686.001336	10.514842
7.671935	684.096898	10.519847
7.441660	693.920048	10.524851
7.792074	689.423673	10.529856
7.432823	701.919768	10.534861
7.702334	700.918120	10.539866
7.774134	699.927508	10.544871
7.889245	705.745408	10.549875
8.076734	695.203903	10.554880
7.833250	701.714495	10.559885
7.930553	706.278436	10.564890
7.953412	726.648635	10.569895
8.001930	732.696359	10.574899
8.072471	736.067698	10.579904
8.211245	745.319519	10.584909
7.986271	740.971676	10.589914
8.247009	729.937502	10.594919
8.236838	735.288130	10.599923
8.482931	731.711956	10.604928
8.304346	752.836552	10.609933
8.392683	736.610271	10.614938
8.256460	747.568028	10.619943
8.213817	746.871629	10.624947
8.774597	762.483669	10.629952
8.774089	756.874750	10.634957
8.626879	764.834972	10.639962
8.583593	777.389540	10.644967
8.454177	758.389471	10.649971
8.704099	773.568570	10.654976
8.683877	770.820172	10.659981
8.755155	768.164411	10.664986
8.811797	766.813521	10.669991
8.819901	775.166859	10.674995
9.188165	769.410807	10.680000
8.768973	776.961842	10.685005
8.785200	791.421313	10.690010
8.942348	804.754472	10.695015
9.122946	813.250627	10.700019
9.372062	811.236685	10.705024
9.196751	821.259308	10.710029
9.409790	813.750802	10.715034
9.400215	825.563610	10.720039
9.111158	815.181607	10.725043
9.625195	821.822155	10.730048
9.507660	825.332322	10.735053
9.425855	822.587430	10.740058
9.738797	819.628189	10.745063
9.826629	823.812061	10.750067
9.653935	812.681382	10.755072
9.315208	829.674858	10.760077
9.862365	822.966171	10.765082
10.191741	847.900161	10.770087
9.601076	834.109624	10.775091
9.881644	826.183493	10.780096
9.928791	853.953671	10.785101
10.074862	843.557434	10.790106
9.966670	857.465968	10.795111
10.250962	851.265968	10.800115
10.158311	851.448005	10.805120
10.120455	848.409096	10.810125
10.170369	852.341986	10.815130
10.182880	854.017947	10.820135
10.216288	858.406050	10.825139
10.298748	855.997644	10.830144
10.287117	853.736709	10.835149
10.431229	845.083292	10.840154
10.190780	869.086358	10.845159
10.229833	855.100741	10.850163
10.613013	877.088378	10.855168
10.408020	890.339033	10.860173
10.487209	886.748444	10.865178
11.065867	886.336132	10.870183
10.655569	902.500603	10.875187
10.908105	887.943168	10.880192
10.874731	906.349845	10.885197
10.857143	898.382924	10.890202
10.866487	902.401145	10.895207
10.904980	903.995699	10.900211
11.062704	902.956675	10.905216
10.778421	904.978024	10.910221
10.999378	907.574790	10.915226
11.236628	901.445350	10.920231
11.264207	899.933505	10.925235
11.423647	886.472698	10.930240
11.232999	900.086923	10.935245
11.520042	888.494929	10.940250
11.390556	900.289078	10.945255
11.486013	910.109303	10.950259
11.504223	892.099481	10.955264
11.407889	908.910885	10.960269
11.181356	902.005452	10.965274
11.282126	913.597307	10.970279
11.752955	931.698092	10.975283
11.877419	933.171705	10.980288
11.963494	930.198166	10.985293
11.957082	938.446682	10.990298
12.061753	928.168951	10.995303
11.959219	940.867151	11.000307
12.058598	923.875661	11.005312
11.967186	946.732304	11.010317
11.959083	935.444391	11.015322
12.185698	935.610197	11.020327
12.089057	946.746293	11.025331
11.971848	941.165379	11.030336
11.742518	947.090355	11.035341
12.324361	940.634701	11.040346
12.232776	936.743335	11.045351
12.101783	949.592737	11.050355
12.565126	939.752947	11.055360
12.562389	936.293684	11.060365
12.227711	945.914462	11.065370
12.487130	940.576247	11.070375
12.505987	942.457786	11.075379
12.654736	945.198539	11.080384
12.593753	942.822460	11.085389
12.802007	925.383098	11.090394
12.897473	936.419159	11.095399
12.452967	943.018692	11.100403
12.777774	944.192270	11.105408
12.784710	935.899721	11.110413
12.758277	945.015596	11.115418
12.573214	940.342785	11.120423
12.784032	971.811814	11.125427
13.054277	963.576597	11.130432
12.863489	982.309675	11.135437
12.895905	972.242133	11.140442
13.120203	968.554262	11.145447
13.284373	973.711591	11.150451
13.416508	973.387846	11.155456
13.299021	965.771133	11.160461
13.456430	973.807460	11.165466
13.796630	955.345658	11.170471
13.571183	967.659789	11.175475
14.011556	957.025719	11.180480
13.901670	972.268725	11.185485
13.890945	952.675462	11.190490
13.597418	949.049690	11.195495
13.519607	942.703983	11.200499
13.565706	943.825823	11.205504
13.638336	953.859452	11.210509
13.685655	970.320011	11.215514
14.020104	963.028604	11.220519
13.725896	971.483891	11.225523
13.815098	972.368625	11.230528
13.636309	974.147653	11.235533
13.919117	964.068563	11.240538
13.801852	969.619285	11.245543
13.482753	972.819441	11.250547
14.020389	975.651134	11.255552
14.220459	979.210027	11.260557
14.176697	970.384653	11.265562
14.128244	971.121032	11.270567
14.086214	980.543768	11.275571
14.504123	984.306034	11.280576
14.645915	1000.045087	11.285581
15.016469	996.983582	11.290586
14.365869	989.256349	11.295591
14.214831	982.136987	11.300595
14.557348	976.127920	11.305600
14.680899	987.583737	11.310605
14.605111	1001.499856	11.315610
14.786577	1006.236547	11.320615
15.006025	1001.308384	11.325619
14.930182	985.841292	11.330624
14.875305	981.578208	11.335629
14.769908	969.146733	11.340634
14.528878	984.196206	11.345639
14.745847	1001.440289	11.350643
15.004696	996.972620	11.355648
14.613159	995.742080	11.360653
15.009167	1001.996264	11.365658
14.978524	996.619139	11.370663
14.849810	1013.377483	11.375667
14.715167	999.832591	11.380672
14.841390	1014.605899	11.385677
15.344339	1030.714732	11.390682
15.696765	1036.707801	11.395687
15.255332	1034.953784	11.400691
15.578894	1030.657131	11.405696
15.766129	1045.072233	11.410701
15.597086	1029.624690	11.415706
15.807202	1038.838512	11.420711
15.908609	1044.559387	11.425715
15.936509	1016.780235	11.430720
15.618743	1010.584735	11.435725
15.362263	1002.387780	11.440730
15.904625	1017.714455	11.445735
15.792046	1034.580635	11.450739
16.016978	1037.306101	11.455744
15.788036	1037.721190	11.460749
15.796427	1044.410956	11.465754
15.899191	1040.710912	11.470759
15.775180	1029.469799	11.475763
15.970763	1039.830805	11.480768
15.999102	1038.397672	11.485773
16.070116	1044.741559	11.490778
16.086716	1036.538874	11.495783
15.819438	1034.878504	11.500787
16.219745	1037.080834	11.505792
15.970827	1048.118294	11.510797
16.549766	1055.912390	11.515802
16.557226	1060.329924	11.520807
16.515280	1075.762476	11.525811
16.800595	1065.577260	11.530816
16.642450	1069.220119	11.535821
16.934358	1065.007353	11.540826
17.092498	1044.932868	11.545831
16.869299	1041.554474	11.550835
16.914934	1031.103161	11.555840
16.860374	1026.359043	11.560845
16.781585	1031.313872	11.565850
16.856561	1025.517769	11.570855
16.754884	1039.368667	11.575859
16.761836	1021.229593	11.580864
17.028269	1047.020789	11.585869
17.072822	1056.625306	11.590874
17.188152	1059.669455	11.595879
17.166279	1072.925762	11.600883
17.270518	1053.485913	11.605888
17.035895	1069.871707	11.610893
17.224114	1054.561119	11.615898
17.687006	1065.076625	11.620903
17.286892	1069.462977	11.625907
17.507551	1054.110945	11.630912
17.515240	1065.549035	11.635917
17.602831	1073.788943	11.640922
17.660467	1064.799104	11.645927
17.543465	1052.758916	11.650931
17.669698	1058.928422	11.655936
17.651289	1068.164521	11.660941
17.554817	1060.623254	11.665946
18.010769	1058.327130	11.670951
17.689268	1063.923079	11.675955
17.725655	1062.573816	11.680960
17.472504	1059.148156	11.685965
17.271419	1064.005809	11.690970
17.520825	1067.714549	11.695975
17.511837	1086.004025	11.700979
18.143616	1091.099427	11.705984
18.368947	1085.859637	11.710989
18.208099	1091.139813	11.715994
18.324073	1095.664629	11.720999
18.189913	1093.659743	11.726003
18.473378	1088.738687	11.731008
18.302472	1088.386004	11.736013
18.456502	1096.638982	11.741018
18.762403	1092.103854	11.746023
18.340295	1086.836444	11.751027
18.541077	1089.326075	11.756032
18.551553	1079.353421	11.761037
18.657983	1087.289133	11.766042
18.829732	1082.202971	11.771047
18.660360	1093.030657	11.776051
18.922783	1084.388189	11.781056
18.962735	1082.547922	11.786061
18.891088	1088.958738	11.791066
18.627669	1080.214064	11.796071
18.775141	1083.672563	11.801075
18.790497	1077.354514	11.806080
18.811149	1092.479054	11.811085
18.917195	1086.264808	11.816090
19.077646	1087.246995	11.821095
18.511437	1092.817331	11.826099
19.151597	1086.448507	11.831104
19.170433	1076.086591	11.836109
18.805864	1099.048544	11.841114
19.360862	1109.986210	11.846119
19.545043	1108.163936	11.851123
19.912420	1113.621642	11.856128
19.324276	1105.766111	11.861133
19.222088	1109.338554	11.866138
19.603779	1107.839592	11.871143
19.488246	1115.670374	11.876147
19.488503	1116.269681	11.881152
19.769844	1114.570682	11.886157
19.698926	1123.559724	11.891162
19.902745	1106.716942	11.896167
19.739601	1114.246233	11.901171
19.944031	1108.755879	11.906176
19.536142	1124.912327	11.911181
19.415227	1126.163322	11.916186
19.796158	1107.399939	11.921191
19.617396	1125.087337	11.926195
19.780521	1118.335692	11.931200
19.895267	1125.951553	11.936205
20.051963	1151.041344	11.941210
20.492004	1142.171814	11.946215
20.146835	1154.151959	11.951219
21.001321	1144.743235	11.956224
20.500703	1133.183638	11.961229
20.307680	1114.770413	11.966234
20.523410	1111.804542	11.971239
20.253400	1120.409021	11.976243
20.228070	1120.487282	11.981248
20.371287	1127.937754	11.986253
20.573184	1141.021235	11.991258
20.947104	1135.341410	11.996263
21.021839	1137.280294	12.001267
21.104784	1123.096606	12.006272
21.012074	1117.218401	12.011277
20.730146	1108.271657	12.016282
21.022601	1109.382602	12.021287
21.119947	1116.353104	12.026291
20.715463	1108.927172	12.031296
20.486676	1111.549979	12.036301
20.876091	1106.947909	12.041306
20.862333	1115.276546	12.046311
20.589684	1111.917062	12.051315
20.834005	1098.783142	12.056320
20.804032	1118.173568	12.061325
20.384035	1106.014506	12.066330
20.794132	1104.454244	12.071335
20.512780	1108.141995	12.076339
20.686804	1113.118030	12.081344
20.539551	1117.440409	12.086349
20.571036	1112.468072	12.091354
20.659832	1110.292004	12.096359
20.566825	1113.457705	12.101363
20.820260	1122.122198	12.106368
20.831132	1116.459285	12.111373
20.533518	1121.458510	12.116378
20.789253	1129.092886	12.121383
20.784142	1134.141655	12.126387
20.790919	1131.000950	12.131392
20.796543	1129.606124	12.136397
20.469514	1125.151439	12.141402
20.760736	1133.040355	12.146407
20.840851	1151.383511	12.151411
20.978286	1135.674081	12.156416
20.942567	1122.024986	12.161421
20.790148	1125.578636	12.166426
20.882297	1106.044450	12.171431
20.717069	1120.411766	12.176435
20.749951	1109.640730	12.181440
20.858730	1109.109396	12.186445
20.560701	1118.420088	12.191450
20.649595	1111.183544	12.196455
20.955926	1120.738466	12.201459
20.642424	1119.113843	12.206464
20.774489	1110.312378	12.211469
20.715534	1115.909049	12.216474
20.818729	1112.787662	12.221479
20.762841	1119.875647	12.226483
20.918393	1107.410317	12.231488
20.979620	1101.576952	12.236493
20.888814	1112.458354	12.241498
21.195658	1110.184428	12.246503
20.919810	1106.759223	12.251507
21.192719	1105.563042	12.256512
21.156313	1112.600608	12.261517
20.914884	1111.048069	12.266522
21.236610	1086.227600	12.271527
20.672140	1087.921501	12.276531
20.870637	1085.284814	12.281536
20.810558	1081.533463	12.286541
20.683306	1083.789986	12.291546
20.762533	1077.695139	12.296551
20.828518	1090.435977	12.301555
21.003198	1082.140243	12.306560
21.337729	1077.206314	12.311565
21.107178	1084.957654	12.316570
21.322329	1082.871823	12.321575
20.871051	1088.638291	12.326579
20.923351	1088.962791	12.331584
20.972685	1077.820147	12.336589
20.638072	1060.300053	12.341594
20.855067	1051.735813	12.346599
20.470391	1058.499319	12.351603
20.641517	1076.460434	12.356608
21.079422	1075.740986	12.361613
20.748111	1066.721720	12.366618
20.759596	1052.763964	12.371623
20.496976	1047.715557	12.376627
20.666409	1062.101976	12.381632
20.866138	1079.698988	12.386637
20.536869	1082.320470	12.391642
20.997103	1079.690922	12.396647
20.629222	1083.108617	12.401651
20.786365	1082.966962	12.406656
21.070222	1084.826753	12.411661
21.119656	1075.988026	12.416666
21.059215	1064.191119	12.421671
20.796632	1059.084355	12.426675
20.952593	1053.366786	12.431680
20.643794	1059.351791	12.436685
20.615634	1056.350716	12.441690
20.839526	1059.435897	12.446695
20.498542	1073.668774	12.451699
20.802522	1064.683798	12.456704
20.727397	1061.628712	12.461709
20.683166	1073.153937	12.466714
20.897537	1057.515899	12.471719
21.089579	1064.658929	12.476723
20.910624	1066.674537	12.481728
20.783219	1065.480709	12.486733
20.664479	1069.574599	12.491738
21.007011	1061.111755	12.496743
20.911758	1068.907738	12.501747
21.034264	1077.045885	12.506752
21.039091	1069.493187	12.511757
20.868277	1066.540094	12.516762
20.930452	1065.409067	12.521767
20.964027	1074.460260	12.526771
20.892200	1059.041334	12.531776
20.676718	1053.783556	12.536781
20.828005	1047.779730	12.541786
20.776323	1041.128614	12.546791
20.617309	1053.447992	12.551795
20.481317	1041.935966	12.556800
20.603506	1056.692614	12.561805
20.697442	1061.462209	12.566810
21.154818	1065.618749	12.571815
20.954097	1063.779025	12.576819
20.966771	1049.247071	12.581824
20.779478	1044.251305	12.586829
20.558311	1047.607744	12.591834
20.976744	1044.467630	12.596839
20.568351	1040.510072	12.601843
20.436044	1050.428223	12.606848
20.668842	1053.524599	12.611853
20.578207	1055.552926	12.616858
20.708192	1064.636044	12.621863
20.937193	1080.854863	12.626867
20.875664	1070.704465	12.631872
20.484564	1063.875664	12.636877
20.468801	1078.923997	12.641882
20.931749	1073.409769	12.646887
20.805448	1084.049229	12.651891
20.872794	1061.576461	12.656896
21.042321	1054.949980	12.661901
20.977328	1053.732005	12.666906
20.888783	1048.909722	12.671911
20.979646	1039.917752	12.676915
20.938731	1041.507641	12.681920
20.610422	1063.547547	12.686925
20.407128	1059.468961	12.691930
20.662358	1048.222536	12.696935
20.620523	1058.574116	12.701939
20.825735	1048.217186	12.706944
21.210208	1051.104865	12.711949
20.863510	1053.120418	12.716954
21.022618	1047.545853	12.721959
21.054672	1052.763707	12.726963
21.089243	1049.255888	12.731968
21.360590	1051.653833	12.736973
20.984827	1052.278420	12.741978
20.907166	1028.510500	12.746983
20.954028	1030.934785	12.751987
20.553359	1018.958793	12.756992
20.462043	1025.702301	12.761997
20.602221	1037.757901	12.767002
20.943436	1049.707330	12.772007
20.749002	1043.254024	12.777011
20.856772	1043.024050	12.782016
20.769755	1030.974366	12.787021
20.477826	1034.728442	12.792026
20.662458	1039.592372	12.797031
20.417920	1058.714168	12.802035
20.910342	1052.742660	12.807040
20.980272	1050.911808	12.812045
20.706943	1063.315659	12.817050
20.930282	1054.961717	12.822055
20.616453	1050.151712	12.827059
20.578548	1053.319650	12.832064
20.630245	1049.646673	12.837069
20.625792	1059.837750	12.842074
20.534481	1059.207445	12.847079
20.801017	1063.981049	12.852083
20.863608	1059.763860	12.857088
20.993653	1062.618007	12.862093
20.923865	1052.703905	12.867098
21.037776	1060.359289	12.872103
20.757477	1045.262211	12.877107
20.755326	1043.370317	12.882112
20.950808	1029.339080	12.887117
20.507374	1036.730112	12.892122
20.689970	1038.539816	12.897127
20.829889	1043.622191	12.902131
20.721707	1048.908143	12.907136
20.837930	1044.464785	12.912141
20.792422	1041.964796	12.917146
20.866192	1023.264705	12.922151
20.769235	1026.276476	12.927155
20.411278	1030.619822	12.932160
20.765185	1033.160713	12.937165
20.359134	1053.896252	12.942170
20.498583	1065.828990	12.947175
20.693712	1060.926764	12.952179
20.655190	1067.486828	12.957184
20.950445	1072.949715	12.962189
20.845222	1077.435690	12.967194
21.027018	1064.496278	12.972199
20.548112	1075.291321	12.977203
20.563856	1073.298798	12.982208
21.065586	1060.592211	12.987213
20.800395	1070.487416	12.992218
20.844186	1068.971391	12.997223
20.743113	1070.853152	13.002227
20.886799	1068.999495	13.007232
20.822474	1060.631508	13.012237
20.931661	1049.659111	13.017242
20.737362	1049.139850	13.022247
20.844398	1045.111118	13.027251
20.383887	1040.315051	13.032256
20.862331	1054.294207	13.037261
20.481353	1056.684236	13.042266
20.699002	1069.228977	13.047271
20.664533	1077.013692	13.052275
20.980886	1077.521579	13.057280
21.042543	1071.035299	13.062285
21.177494	1055.406776	13.067290
20.950023	1046.213265	13.072295
20.741366	1046.574656	13.077299
20.864165	1040.763034	13.082304
21.066614	1043.187736	13.087309
20.404996	1053.338547	13.092314
20.486837	1045.737308	13.097319
20.678567	1042.302194	13.102323
20.663603	1043.862712	13.107328
20.930360	1047.075095	13.112333
20.328906	1045.874878	13.117338
20.916288	1032.310985	13.122343
20.778524	1040.671974	13.127347
20.559106	1048.744793	13.132352
21.146228	1050.310204	13.137357
20.726328	1042.915150	13.142362
20.868591	1038.306791	13.147367
20.606876	1049.075058	13.152371
20.748845	1049.823647	13.157376
20.823844	1035.400037	13.162381
20.587525	1045.752666	13.167386
21.138015	1045.113034	13.172391
21.114397	1047.507563	13.177395
20.981461	1047.327020	13.182400
21.085448	1038.094839	13.187405
20.538992	1039.509895	13.192410
20.845906	1045.723117	13.197415
20.878702	1042.448971	13.202419
20.782641	1045.331293	13.207424
20.924516	1041.311198	13.212429
20.841469	1055.170180	13.217434
20.929828	1037.694612	13.222439
21.023256	1043.233834	13.227443
20.934448	1032.669921	13.232448
21.098727	1011.894336	13.237453
20.658630	1013.000691	13.242458
20.738743	1017.840284	13.247463
20.838132	1005.753005	13.252467
20.690645	1010.430203	13.257472
20.773639	1009.677481	13.262477
20.778212	1017.241473	13.267482
20.693621	1003.974021	13.272487
20.814327	1014.837383	13.277491
20.740407	1003.818533	13.282496
20.588000	1006.127942	13.287501
20.294033	1015.425305	13.292506
20.749215	1024.131677	13.297511
20.688072	1031.814967	13.302515
20.926769	1040.708843	13.307520
21.201046	1032.528138	13.312525
21.033413	1029.666009	13.317530
21.078952	1015.679202	13.322535
20.810982	1010.141230	13.327539
20.333716	1022.137606	13.332544
20.751658	1008.689071	13.337549
20.108919	1013.566688	13.342554
20.651541	1019.933114	13.347559
20.703034	1034.986444	13.352563
20.740799	1048.739417	13.357568
20.877002	1044.718649	13.362573
20.585211	1049.489839	13.367578
20.735524	1042.506884	13.372583
20.645012	1051.715049	13.377587
20.805445	1051.498752	13.382592
21.080818	1046.569539	13.387597
20.931398	1023.478547	13.392602
20.960280	1022.452181	13.397607
20.506906	1027.714337	13.402611
20.689186	1014.041611	13.407616
20.888222	1014.270165	13.412621
20.419974	1017.513043	13.417626
20.621816	1020.857199	13.422631
20.774803	1033.150449	13.427635
20.242734	1045.918829	13.432640
20.646131	1049.598273	13.437645
20.533077	1051.215438	13.442650
20.421457	1051.889357	13.447655
20.430422	1054.027954	13.452659
20.641384	1057.058427	13.457664
20.732056	1065.545421	13.462669
20.794538	1066.404460	13.467674
21.050554	1052.740437	13.472679
20.838118	1051.462401	13.477683
20.429154	1080.294514	13.482688
20.921845	1050.586662	13.487693
20.996372	1054.067827	13.492698
21.162906	1066.709028	13.497703
20.881048	1058.885094	13.502707
20.871611	1050.844249	13.507712
21.098027	1066.066830	13.512717
20.969864	1066.021144	13.517722
20.905790	1040.082728	13.522727
20.450313	1046.076930	13.527731
20.669260	1019.820596	13.532736
21.185901	1059.417517	13.537741
20.942218	1040.408493	13.542746
20.678194	1016.615124	13.547751
20.839731	1040.510203	13.552755
20.607729	1020.993141	13.557760
20.946686	1035.136452	13.562765
20.675265	1021.321620	13.567770
20.577801	1017.735521	13.572775
20.455932	1026.570204	13.577779
20.499888	1032.170928	13.582784
20.941524	1033.163455	13.587789
20.768551	1048.216331	13.592794
21.119004	1053.536365	13.597799
20.609871	1037.690472	13.602803
20.600746	1038.997746	13.607808
21.069251	1028.747068	13.612813
20.465084	1030.429948	13.617818
20.742610	1025.919866	13.622823
20.934195	1037.438990	13.627827
20.855081	1034.288351	13.632832
21.015023	1029.905833	13.637837
20.919993	1032.453675	13.642842
20.656732	1022.236140	13.647847
20.788096	1028.002693	13.652851
20.808587	1033.550390	13.657856
20.682596	1025.302645	13.662861
20.458139	1042.238719	13.667866
20.565750	1025.059717	13.672871
20.930847	1026.606921	13.677875
20.776034	1030.105737	13.682880
20.488630	1038.053777	13.687885
20.757470	1033.198150	13.692890
20.696870	1041.286634	13.697895
20.649537	1032.956953	13.702899
20.429035	1037.760924	13.707904
20.794707	1039.664429	13.712909
20.820464	1058.106023	13.717914
20.782505	1062.584419	13.722919
20.902612	1070.672482	13.727923
20.799170	1052.815904	13.732928
20.858126	1034.461937	13.737933
20.683991	1062.324581	13.742938
20.742802	1028.229512	13.747943
20.437122	1039.310712	13.752947
20.660643	1061.376138	13.757952
21.010305	1062.982579	13.762957
20.774687	1063.677853	13.767962
20.473052	1053.896924	13.772967
20.655639	1049.581751	13.777971
20.787803	1067.640533	13.782976
20.655707	1069.871018	13.787981
20.477004	1087.466898	13.792986
21.047279	1067.900657	13.797991
21.251222	1066.833750	13.802995
20.951248	1070.497654	13.808000
21.106654	1042.291261	13.813005
20.645705	1033.246962	13.818010
20.631654	1046.929350	13.823015
20.757889	1039.595423	13.828019
20.786561	1053.619510	13.833024
20.525892	1046.842453	13.838029
20.529851	1047.971022	13.843034
20.956793	1047.899875	13.848039
20.811406	1044.483838	13.853043
20.540923	1059.943363	13.858048
20.918728	1028.730545	13.863053
20.422420	1037.654921	13.868058
20.647874	1056.790058	13.873063
20.909016	1068.509423	13.878067
20.923788	1056.938646	13.883072
20.986949	1046.946572	13.888077
20.591678	1074.675778	13.893082
20.826311	1050.436964	13.898087
21.132829	1036.378549	13.903091
20.405629	1048.898935	13.908096
20.581175	1041.746375	13.913101
20.484579	1057.717480	13.918106
20.928423	1061.504016	13.923111
20.683078	1043.786777	13.928115
20.712765	1050.134105	13.933120
20.702771	1050.302960	13.938125
20.754057	1059.531091	13.943130
20.408330	1052.710828	13.948135
20.636809	1062.352245	13.953139
20.348911	1080.870704	13.958144
21.039360	1075.668695	13.963149
20.985466	1076.051133	13.968154
20.947579	1076.736948	13.973159
20.999107	1081.915436	13.978163
20.661623	1061.377508	13.983168
20.934988	1050.894588	13.988173
20.842216	1058.616053	13.993178
20.984437	1038.110453	13.998183
20.765976	1045.960769	14.003187
20.324960	1052.145055	14.008192
20.567034	1048.349828	14.013210
20.811693	1063.189246	14.018227
20.830003	1065.828952	14.023245
20.910840	1076.603322	14.028263
20.606198	1071.351239	14.033280
20.892805	1064.271485	14.038298
21.168119	1085.326975	14.043315
20.961046	1070.628031	14.048333
21.098890	1057.486339	14.053351
20.602626	1060.895490	14.058368
21.054558	1049.482692	14.063386
20.855761	1043.065499	14.068403
20.552881	1055.961593	14.073421
20.921521	1072.775720	14.078439
20.753951	1088.849602	14.083456
20.924220	1087.812726	14.088474
20.620628	1084.641460	14.093491
20.942901	1092.105634	14.098509
21.047441	1093.908948	14.103527
21.047421	1085.132090	14.108544
21.100269	1084.428529	14.113562
21.041378	1087.697143	14.118579
21.096131	1090.230373	14.123597
21.258862	1085.918280	14.128615
21.155056	1097.230174	14.133632
21.434321	1078.010114	14.138650
21.214532	1093.598430	14.143667
21.076802	1104.874844	14.148685
21.391569	1090.646319	14.153703
20.736909	1095.238420	14.158720
21.140597	1090.790371	14.163738
21.144844	1086.571192	14.168755
21.223792	1100.208619	14.173773
21.444431	1081.638089	14.178791
21.218046	1099.873136	14.183808
21.082783	1093.939688	14.188826
21.385872	1112.101309	14.193843
21.495477	1128.275736	14.198861
21.607090	1121.812144	14.203879
21.541133	1122.313524	14.208896
21.641173	1111.342175	14.213914
21.403947	1108.037630	14.218931
21.538070	1096.861092	14.223949
21.472031	1099.935804	14.228967
21.242732	1101.767200	14.233984
21.704674	1118.055294	14.239002
21.763230	1124.624078	14.244019
21.832002	1118.164174	14.249037
21.506796	1107.325145	14.254055
21.456274	1113.832675	14.259072
21.580573	1127.338632	14.264090
21.803715	1128.245334	14.269107
21.888815	1133.785907	14.274125
21.591777	1114.558624	14.279143
21.572196	1128.071801	14.284160
21.935732	1112.209059	14.289178
21.488005	1143.720440	14.294195
21.681732	1138.983413	14.299213
22.036899	1107.633297	14.304231
21.655760	1125.205686	14.309248
21.648900	1135.366486	14.314266
21.721538	1129.171788	14.319283
21.637276	1131.689448	14.324301
21.596723	1132.891453	14.329319
21.567031	1144.578504	14.334336
21.420655	1122.415671	14.339354
21.701542	1124.006828	14.344371
21.419665	1140.592902	14.349389
21.890127	1145.197459	14.354407
21.705504	1162.614287	14.359424
22.056987	1162.564622	14.364442
22.120309	1161.912866	14.369459
21.961772	1170.422702	14.374477
22.123137	1166.957045	14.379495
21.853845	1165.699280	14.384512
22.106058	1154.401621	14.389530
22.132055	1161.315370	14.394547
21.766059	1168.189404	14.399565
22.018302	1161.745832	14.404583
22.064968	1161.836016	14.409600
22.047207	1166.468118	14.414618
22.253156	1166.484134	14.419635
22.044736	1167.294515	14.424653
22.400173	1173.502953	14.429671
22.208537	1169.701937	14.434688
22.100480	1167.860060	14.439706
22.454139	1168.189126	14.444723
22.342882	1178.541204	14.449741
22.216762	1167.325901	14.454759
22.227263	1190.371083	14.459776
22.101736	1194.177285	14.464794
22.888502	1197.164757	14.469811
22.475104	1196.252427	14.474829
22.746201	1199.208896	14.479847
22.373978	1187.347027	14.484864
22.362443	1189.893994	14.489882
22.335825	1198.148436	14.494899
22.222076	1201.255947	14.499917
22.750188	1194.445906	14.504935
22.843276	1195.233364	14.509952
22.650543	1199.217019	14.514970
22.753194	1198.986830	14.519987
22.820683	1200.594730	14.525005
23.087596	1186.622269	14.530023
22.617482	1168.768959	14.535040
22.640769	1174.890384	14.540058
22.837290	1161.025125	14.545075
22.620946	1162.818284	14.550093
22.904127	1158.486957	14.555111
23.055221	1163.238410	14.560128
22.755082	1169.524671	14.565146
22.594628	1158.893693	14.570163
22.560060	1165.721154	14.575181
22.657595	1175.690735	14.580199
22.935527	1186.661827	14.585216
23.093108	1191.382368	14.590234
23.270176	1193.518601	14.595251
22.549680	1175.379620	14.600269
22.876062	1177.849093	14.605287
22.876820	1197.285938	14.610304
22.923180	1181.920426	14.615322
23.015242	1207.530680	14.620339
23.267035	1193.198847	14.625357
23.280482	1182.387539	14.630375
22.932499	1192.582340	14.635392
22.593534	1211.159509	14.640410
23.006523	1176.707610	14.645427
22.814877	1207.212497	14.650445
23.392532	1187.799988	14.655463
23.054240	1180.860745	14.660480
22.754042	1206.832423	14.665498
23.305831	1198.442513	14.670515
22.997875	1190.855092	14.675533
23.011016	1181.731602	14.680551
23.138451	1202.735349	14.685568
23.083631	1193.709203	14.690586
23.569930	1180.450478	14.695603
23.131107	1197.237818	14.700621
23.221211	1189.075701	14.705639
23.303401	1186.780355	14.710656
23.141029	1202.321879	14.715674
23.736021	1208.081585	14.720691
23.524343	1195.454818	14.725709
23.745113	1207.309600	14.730727
23.301959	1196.366626	14.735744
23.242370	1190.892952	14.740762
23.968539	1186.503545	14.745779
23.731482	1197.632287	14.750797
23.631343	1186.239801	14.755815
23.964390	1196.985044	14.760832
23.956410	1185.573141	14.765850
23.991292	1176.576741	14.770867
23.707615	1198.333430	14.775885
23.674188	1181.387252	14.780903
23.675996	1183.312349	14.785920
23.364010	1197.749932	14.790938
23.938143	1175.104028	14.795955
23.613748	1191.196746	14.800973
23.246898	1204.257322	14.805991
23.645045	1189.847095	14.811008
23.459807	1189.821692	14.816026
23.580520	1189.168646	14.821043
23.366312	1219.565479	14.826061
23.831225	1214.217340	14.831079
24.067549	1208.628824	14.836096
23.830096	1224.032917	14.841114
24.377251	1227.569821	14.846131
24.240321	1226.607100	14.851149
24.180708	1213.820789	14.856167
24.366403	1190.642243	14.861184
24.121600	1181.665283	14.866202
24.191770	1189.009277	14.871219
24.261588	1180.966798	14.876237
23.976928	1182.166845	14.881255
24.085777	1187.242778	14.886272
23.848643	1193.589782	14.891290
24.317225	1175.336644	14.896307
24.172235	1182.911572	14.901325
23.975859	1180.166754	14.906343
23.986563	1189.432932	14.911360
23.914259	1186.076896	14.916378
24.243289	1178.416196	14.921395
24.016431	1183.890147	14.926413
24.126494	1187.127116	14.931431
24.194416	1197.876896	14.936448
24.480022	1211.921891	14.941466
24.510581	1215.599388	14.946483
24.540500	1215.347768	14.951501
24.342204	1202.037775	14.956519
24.486350	1189.151349	14.961536
24.263504	1186.096163	14.966554
24.549582	1192.076585	14.971571
24.430826	1206.440887	14.976589
24.411012	1206.835815	14.981607
24.445222	1217.227636	14.986624
24.176468	1226.170342	14.991642
24.546435	1210.370958	14.996659
24.621714	1223.445971	15.001677
24.242345	1219.954870	15.006695
24.590810	1215.915120	15.011712
24.587974	1217.529520	15.016730
24.724683	1212.235303	15.021747
24.650106	1214.773454	15.026765
24.757898	1212.879841	15.031783
25.182689	1207.094533	15.036800
24.665149	1223.120569	15.041818
24.705587	1214.278981	15.046835
24.945241	1213.444950	15.051853
24.945014	1217.229600	15.056871
25.115981	1217.592526	15.061888
24.935592	1217.564776	15.066906
24.804812	1208.508267	15.071923
24.734245	1223.339929	15.076941
24.665331	1214.849247	15.081959
24.979570	1214.904618	15.086976
24.627800	1216.134247	15.091994
25.085120	1205.151456	15.097011
24.899471	1215.543739	15.102029
24.583341	1217.884476	15.107047
24.993216	1208.979248	15.112064
24.920643	1213.379447	15.117082
24.817144	1211.975689	15.122099
25.108867	1219.202568	15.127117
24.811443	1222.594196	15.132135
25.122175	1230.414196	15.137152
25.160232	1239.875808	15.142170
25.054743	1246.385873	15.147187
25.223607	1242.587111	15.152205
25.074426	1257.734926	15.157223
25.088961	1248.949356	15.162240
24.963984	1235.997280	15.167258
25.554342	1247.565069	15.172275
25.337050	1249.564446	15.177293
25.170603	1240.659890	15.182311
25.614188	1246.816550	15.187328
25.579459	1250.213474	15.192346
25.340730	1245.501346	15.197363
25.138725	1242.708653	15.202381
24.949771	1242.186790	15.207399
25.450462	1234.075557	15.212416
25.278120	1236.552231	15.217434
25.298171	1230.431940	15.222451
25.335992	1247.601043	15.227469
25.192967	1266.892609	15.232487
25.405441	1258.254779	15.237504
25.826520	1261.770905	15.242522
25.452852	1268.006017	15.247539
25.967281	1266.027091	15.252557
26.066112	1261.789629	15.257575
26.127912	1267.121620	15.262592
25.982951	1250.155400	15.267610
26.029049	1237.636911	15.272627
26.101560	1227.964401	15.277645
26.226254	1234.753910	15.282663
26.325041	1224.460615	15.287680
25.859315	1228.110312	15.292698
25.810495	1219.789447	15.297715
26.008770	1226.542048	15.302733
25.903345	1225.604188	15.307751
26.004938	1231.879880	15.312768
25.783283	1233.139092	15.317786
26.076093	1228.925754	15.322803
26.069955	1233.093577	15.327821
25.863067	1235.248587	15.332839
26.003749	1227.611610	15.337856
26.182132	1232.660739	15.342874
25.874260	1231.058353	15.347891
26.295473	1227.025873	15.352909
26.231036	1227.670152	15.357927
26.227429	1215.755757	15.362944
26.227173	1220.808207	15.367962
26.293446	1221.810719	15.372979
26.270899	1228.795161	15.377997
26.096047	1228.950563	15.383015
26.308204	1230.590445	15.388032
26.260922	1230.963015	15.393050
26.242273	1224.691604	15.398067
26.350647	1230.491184	15.403085
25.884965	1219.377188	15.408103
26.159552	1234.200998	15.413120
25.995944	1236.915367	15.418138
26.179179	1246.860317	15.423155
26.598305	1260.687445	15.428173
26.137543	1270.285264	15.433191
26.688597	1253.233194	15.438208
26.780263	1262.302470	15.443226
26.887581	1258.678679	15.448243
27.306409	1249.691778	15.453261
26.497392	1245.617997	15.458279
26.518005	1233.748485	15.463296
26.411766	1234.043946	15.468314
26.941103	1249.898318	15.473331
26.601528	1237.540439	15.478349
26.691238	1254.471623	15.483367
26.859686	1258.655650	15.488384
26.542070	1257.117733	15.493402
26.625854	1264.656213	15.498419
26.840559	1259.988157	15.503437
26.457922	1270.012368	15.508455
26.588453	1259.386812	15.513472
26.575429	1262.964312	15.518490
26.737738	1254.402122	15.523507
26.660275	1258.862887	15.528525
26.727018	1250.581771	15.533543
27.240217	1257.820533	15.538560
27.216319	1258.279032	15.543578
26.873205	1265.979980	15.548595
26.937066	1257.166089	15.553613
26.579516	1265.920071	15.558631
26.809334	1273.870972	15.563648
27.222752	1285.327021	15.568666
27.432681	1282.998702	15.573683
27.622457	1284.261505	15.578701
27.246369	1272.110758	15.583719
27.150924	1262.175591	15.588736
27.413742	1270.341440	15.593754
27.339199	1264.251952	15.598771
27.510626	1255.350123	15.603789
27.138714	1249.120891	15.608807
27.364369	1254.807397	15.613824
27.599737	1261.698810	15.618842
27.101568	1258.160584	15.623859
27.495212	1264.060961	15.628877
27.207764	1279.273322	15.633895
27.706819	1278.552063	15.638912
27.671025	1287.235862	15.643930
27.733684	1286.368713	15.648947
27.675467	1266.565185	15.653965
27.543392	1257.016518	15.658983
27.301571	1245.961173	15.664000
27.564246	1260.467601	15.669018
27.832965	1276.840175	15.674035
28.043477	1262.607662	15.679053
27.652268	1258.668575	15.684071
27.668321	1259.831675	15.689088
27.573216	1245.706123	15.694106
27.586039	1251.761613	15.699123
28.038478	1257.987649	15.704141
27.856570	1274.952742	15.709159
27.819191	1263.993757	15.714176
27.528148	1267.505496	15.719194
27.721281	1279.602262	15.724211
28.179582	1279.397140	15.729229
27.729573	1280.043148	15.734247
27.845708	1282.656280	15.739264
27.629301	1271.062058	15.744282
27.665350	1284.793014	15.749299
27.591165	1286.734965	15.754317
27.720941	1280.927473	15.759335
27.844815	1282.839406	15.764352
27.942429	1292.695803	15.769370
28.026324	1302.518216	15.774387
28.605296	1294.616252	15.779405
28.118856	1291.670723	15.784423
28.079377	1286.343235	15.789440
28.616867	1288.628053	15.794458
28.386728	1292.938582	15.799475
28.446995	1280.998215	15.804493
28.191305	1278.707985	15.809511
28.240323	1276.463531	15.814528
28.413080	1281.467959	15.819546
28.311038	1287.650318	15.824563
28.553048	1272.233056	15.829581
28.509069	1273.723470	15.834599
28.336694	1275.018867	15.839616
28.737837	1272.013569	15.844634
28.366064	1280.264909	15.849651
28.510447	1279.271473	15.854669
28.329133	1291.662342	15.859687
28.393466	1299.281018	15.864704
29.106263	1305.396339	15.869722
28.579411	1309.790375	15.874739
28.891337	1303.566874	15.879757
28.978226	1307.628650	15.884775
28.656181	1289.523494	15.889792
28.713660	1287.932038	15.894810
28.730022	1291.075442	15.899827
28.925456	1278.869710	15.904845
28.935579	1281.668057	15.909863
28.931965	1285.684489	15.914880
28.895801	1276.557793	15.919898
28.835355	1273.604095	15.924915
29.343392	1272.755567	15.929933
28.936375	1267.043136	15.934951
28.787473	1275.639581	15.939968
28.958365	1265.100387	15.944986
28.906113	1279.123833	15.950003
29.043054	1274.710411	15.955021
28.533149	1288.945281	15.960039
28.978523	1299.757625	15.965056
28.993596	1303.629516	15.970074
28.826667	1311.370024	15.975091
28.797978	1300.714779	15.980109
28.992783	1304.158472	15.985127
28.760234	1309.669555	15.990144
28.978945	1308.735044	15.995162
29.152845	1316.908810	16.000179
29.274179	1336.142574	16.005197
29.335342	1333.869435	16.010215
29.478407	1342.222731	16.015232
29.889754	1324.986803	16.020250
29.356801	1316.574793	16.025267
29.233029	1304.240636	16.030285
29.375031	1311.754126	16.035303
29.076309	1335.468605	16.040320
29.429449	1339.061651	16.045338
29.388225	1340.051431	16.050355
29.471148	1337.875489	16.055373
29.467645	1339.274513	16.060391
29.545769	1337.022262	16.065408
30.093444	1332.458371	16.070426
29.594724	1348.111897	16.075443
29.918069	1338.062693	16.080461
30.059892	1342.175489	16.085479
29.711242	1346.004734	16.090496
29.891711	1330.756095	16.095514
29.826451	1336.319154	16.100531
29.800924	1338.018980	16.105549
30.083550	1333.327484	16.110567
29.957326	1344.303386	16.115584
30.105644	1327.552982	16.120602
29.912973	1344.900529	16.125619
29.966830	1340.223497	16.130637
30.095652	1332.191972	16.135655
29.784982	1339.713185	16.140672
30.091488	1344.156777	16.145690
30.324689	1332.294174	16.150707
30.215497	1339.507984	16.155725
30.344009	1339.295690	16.160743
30.133567	1339.475645	16.165760
30.470427	1337.120780	16.170778
30.055428	1342.274028	16.175795
30.083780	1330.925426	16.180813
30.465934	1334.652263	16.185831
30.134055	1342.464712	16.190848
30.328352	1327.084888	16.195866
30.191538	1338.183593	16.200883
30.297112	1331.083822	16.205901
30.519041	1330.175537	16.210919
30.295895	1334.908089	16.215936
30.290589	1329.241668	16.220954
30.211874	1335.594925	16.225971
30.325470	1329.812016	16.230989
30.577016	1326.896630	16.236007
30.259558	1337.354066	16.241024
30.362611	1341.421138	16.246042
30.392708	1345.800282	16.251059
30.834582	1344.778268	16.256077
30.684207	1337.231700	16.261095
30.644798	1333.019412	16.266112
30.647831	1333.089816	16.271130
30.191871	1345.189496	16.276147
30.836421	1344.495363	16.281165
30.980722	1349.754454	16.286183
30.925437	1370.822195	16.291200
30.865806	1354.383341	16.296218
31.155870	1362.920835	16.301235
31.074510	1358.584675	16.306253
30.870230	1355.551659	16.311271
30.433180	1353.694593	16.316288
31.185267	1350.512186	16.321306
30.988762	1357.744651	16.326323
30.932606	1354.411168	16.331341
30.965331	1351.135866	16.336359
30.734789	1358.499596	16.341376
30.996499	1349.982841	16.346394
30.993203	1353.517915	16.351411
31.001610	1358.918230	16.356429
31.047687	1356.232231	16.361447
30.983981	1363.114767	16.366464
31.241080	1371.383829	16.371482
31.386747	1390.495812	16.376499
31.304048	1393.087197	16.381517
31.664834	1383.878245	16.386535
31.453705	1393.670701	16.391552
31.631441	1378.891191	16.396570
31.856299	1374.775162	16.401587
31.476308	1363.620646	16.406605
31.640997	1353.911329	16.411623
31.499881	1358.055100	16.416640
31.707655	1339.404499	16.421658
31.715774	1344.015228	16.426675
31.529983	1342.361897	16.431693
31.923853	1339.367183	16.436711
31.632732	1355.231414	16.441728
31.432172	1341.660541	16.446746
31.876799	1351.169060	16.451763
31.446546	1361.056215	16.456781
32.042019	1361.244477	16.461799
31.704040	1378.292783	16.466816
31.954022	1369.177015	16.471834
31.951066	1380.770334	16.476851
31.859332	1395.825764	16.481869
32.275049	1376.877690	16.486887
32.084258	1368.101202	16.491904
32.310386	1381.657220	16.496922
32.235918	1359.528169	16.501939
31.650297	1342.718636	16.506957
32.090814	1349.882526	16.511975
31.791036	1343.344457	16.516992
32.016931	1369.499919	16.522010
32.082705	1366.365628	16.527027
32.145493	1368.979420	16.532045
32.628752	1360.375416	16.537063
32.238395	1385.745192	16.542080
32.102705	1381.666219	16.547098
31.977732	1371.147398	16.552115
32.138578	1381.959570	16.557133
32.175151	1386.325110	16.562151
32.176468	1376.747223	16.567168
32.490904	1363.059584	16.572186
32.401128	1383.720729	16.577203
32.068630	1383.890265	16.582221
32.563474	1368.755032	16.587239
32.424221	1398.243695	16.592256
32.276196	1373.661517	16.597274
32.537243	1399.223138	16.602291
32.646519	1406.112710	16.607309
32.686302	1398.266803	16.612327
32.503401	1419.177222	16.617344
32.497428	1396.148464	16.622362
32.904544	1415.956503	16.627379
32.395973	1415.899301	16.632397
32.659872	1393.049292	16.637415
32.664975	1419.376908	16.642432
32.671589	1398.098426	16.647450
33.089595	1411.205459	16.652467
33.048397	1408.478317	16.657485
32.943313	1393.544133	16.662503
33.161062	1406.324466	16.667520
32.938813	1392.544653	16.672538
32.944031	1418.697650	16.677555
32.701357	1397.897787	16.682573
32.813002	1413.444595	16.687591
33.101071	1418.888413	16.692608
33.447581	1427.643450	16.697626
33.467026	1434.690504	16.702643
33.370469	1426.432187	16.707661
33.432108	1405.067843	16.712679
33.186585	1392.255972	16.717696
33.435719	1397.904185	16.722714
33.288312	1395.653291	16.727731
33.414690	1402.351378	16.732749
33.435066	1411.663345	16.737767
33.573585	1399.966794	16.742784
33.287549	1428.940976	16.747802
33.495568	1407.474633	16.752819
33.583015	1436.416002	16.757837
33.728349	1416.844062	16.762855
33.734325	1423.477995	16.767872
33.573445	1425.718500	16.772890
33.971997	1410.740149	16.777907
33.532745	1409.754851	16.782925
33.699220	1398.568202	16.787943
33.668667	1426.254269	16.792960
33.918206	1437.414119	16.797978
33.943049	1420.359270	16.802995
33.825534	1415.685952	16.808013
33.952417	1424.068618	16.813031
34.078733	1414.941087	16.818048
34.082221	1391.050414	16.823066
33.900785	1388.916629	16.828083
33.894867	1409.896331	16.833101
33.789850	1392.409212	16.838119
33.873672	1415.820571	16.843136
33.548029	1421.521144	16.848154
33.806759	1412.628889	16.853171
34.182644	1428.320751	16.858189
34.003407	1421.631291	16.863207
33.835280	1427.501791	16.868224
34.002111	1423.126027	16.873242
34.172518	1412.107048	16.878259
34.448254	1421.543454	16.883277
34.030441	1426.041252	16.888295
34.453094	1435.787704	16.893312
34.398441	1438.748991	16.898330
34.430633	1446.080298	16.903347
34.274561	1466.755280	16.908365
34.763206	1454.902171	16.913383
34.725494	1451.792232	16.918400
34.632333	1455.533567	16.923418
34.768694	1447.109105	16.928435
34.554417	1443.291178	16.933453
34.597959	1450.571915	16.938471
34.503991	1453.086460	16.943488
34.347157	1455.320032	16.948506
34.631439	1453.033309	16.953523
34.525450	1439.467708	16.958541
34.084450	1454.600926	16.963559
34.549175	1445.919606	16.968576
34.654943	1453.228171	16.973594
34.863591	1483.477892	16.978611
35.061564	1461.313098	16.983629
35.164336	1490.308757	16.988647
35.386399	1468.388640	16.993664
35.304962	1437.219131	16.998682
35.285926	1447.454448	17.003699
35.041540	1441.489499	17.008717
34.959178	1433.766870	17.013735
35.273163	1441.594332	17.018752
35.165660	1454.818254	17.023770
35.581029	1431.513032	17.028787
35.298739	1441.334172	17.033805
35.467015	1438.444630	17.038823
35.462007	1429.875991	17.043840
35.326189	1435.783811	17.048858
35.052421	1443.716029	17.053875
35.403628	1442.912956	17.058893
35.333953	1429.440670	17.063911
35.644444	1433.989044	17.068928
35.352477	1437.650402	17.073946
35.757272	1434.042041	17.078963
35.609839	1440.401586	17.083981
35.578556	1441.023284	17.088999
35.880447	1435.331420	17.094016
35.892207	1429.526962	17.099034
35.615496	1448.039450	17.104051
35.853700	1445.758504	17.109069
35.454903	1431.236057	17.114087
35.691992	1455.138969	17.119104
35.725590	1467.689187	17.124122
36.068337	1450.311473	17.129139
35.914357	1477.613070	17.134157
35.720327	1473.735279	17.139175
35.853629	1466.272381	17.144192
36.094826	1465.581232	17.149210
36.151918	1467.030377	17.154227
36.075448	1484.674152	17.159245
36.297743	1466.079273	17.164263
36.099093	1465.527487	17.169280
35.855034	1474.985487	17.174298
36.298725	1465.113623	17.179315
36.306322	1471.741028	17.184333
36.111279	1468.173276	17.189351
36.120987	1455.679278	17.194368
35.721542	1486.230478	17.199386
36.420206	1463.602017	17.204403
36.232268	1467.641606	17.209421
36.214383	1467.559623	17.214439
36.503287	1463.175387	17.219456
36.172539	1468.025813	17.224474
36.717309	1467.904424	17.229491
36.822730	1485.539639	17.234509
36.451303	1462.613106	17.239527
36.744666	1472.295264	17.244544
36.878557	1468.840210	17.249562
36.656187	1463.807660	17.254579
36.779677	1461.414451	17.259597
36.899339	1467.270527	17.264615
36.863590	1469.758485	17.269632
36.616481	1465.464459	17.274650
36.784492	1464.204555	17.279667
36.967772	1481.454552	17.284685
37.127593	1490.154463	17.289703
37.163939	1492.417002	17.294720
37.225574	1499.230850	17.299738
36.972683	1479.200112	17.304755
36.821525	1480.177548	17.309773
37.116222	1493.963401	17.314791
37.447851	1482.413730	17.319808
37.170836	1494.033548	17.324826
37.271428	1492.040377	17.329843
37.499596	1486.597770	17.334861
37.057273	1475.549059	17.339879
37.451586	1473.133103	17.344896
37.184786	1477.850641	17.349914
37.271805	1476.825444	17.354931
37.324941	1484.268257	17.359949
37.449702	1490.972935	17.364967
37.462916	1481.740709	17.369984
37.369515	1488.292998	17.375002
37.160725	1481.056109	17.380019
37.354327	1480.216826	17.385037
37.101988	1489.968729	17.390055
37.315850	1491.502981	17.395072
37.554241	1492.618055	17.400090
37.663684	1500.486038	17.405107
37.581165	1524.844296	17.410125
37.764509	1521.176856	17.415143
37.814721	1520.802447	17.420160
38.013865	1527.490560	17.425178
38.010203	1519.332201	17.430195
37.855160	1515.169763	17.435213
38.082914	1521.379843	17.440231
38.071771	1513.532558	17.445248
38.185619	1523.300009	17.450266
38.366263	1509.026402	17.455283
38.291998	1517.203684	17.460301
38.514924	1501.333060	17.465319
38.672200	1477.147164	17.470336
38.233852	1488.242168	17.475354
38.141908	1487.687519	17.480371
37.988847	1480.521964	17.485389
38.311081	1474.636509	17.490407
38.028925	1479.345486	17.495424
38.439389	1499.006819	17.500442
38.604052	1504.047222	17.505459
38.661857	1520.340458	17.510477
38.583427	1509.107845	17.515495
38.428854	1491.984002	17.520512
38.214467	1511.597152	17.525530
38.358110	1519.090040	17.530547
38.408250	1512.700571	17.535565
38.569846	1517.489791	17.540583
38.625192	1514.236011	17.545600
38.312509	1519.879501	17.550618
38.603845	1506.917409	17.555635
38.482735	1518.707431	17.560653
38.370708	1528.982018	17.565671
38.820544	1526.960668	17.570688
38.743075	1535.093641	17.575706
38.755112	1547.241537	17.580723
38.911698	1541.248773	17.585741
38.890524	1558.399340	17.590759
39.021351	1532.643014	17.595776
38.960387	1543.940557	17.600794
38.834493	1540.929604	17.605811
39.144122	1536.998206	17.610829
38.721941	1556.666580	17.615847
39.151865	1544.394913	17.620864
39.022108	1553.362839	17.625882
39.268989	1567.338854	17.630899
39.790814	1564.034258	17.635917
39.680348	1563.369306	17.640935
39.787812	1541.166917	17.645952
39.621933	1524.023604	17.650970
39.694020	1538.276787	17.655987
40.025892	1527.592968	17.661005
39.740863	1532.974870	17.666023
39.872638	1518.033453	17.671040
39.912606	1518.483347	17.676058
39.760597	1542.792159	17.681075
39.989280	1539.024677	17.686093
39.603540	1523.071000	17.691111
39.818822	1523.684836	17.696128
39.826726	1529.847403	17.701146
39.797219	1535.126419	17.706163
39.996542	1518.275640	17.711181
39.709743	1526.340538	17.716199
40.034914	1514.785579	17.721216
40.328941	1517.349934	17.726234
40.035760	1514.260278	17.731251
40.119236	1523.505626	17.736269
39.915833	1525.246428	17.741287
40.246999	1515.633143	17.746304
40.231823	1520.019561	17.751322
40.068637	1518.392491	17.756339
39.996293	1515.085147	17.761357
39.817238	1530.153857	17.766375
40.201335	1533.430566	17.771392
40.144475	1542.182370	17.776410
40.262931	1543.746002	17.781427
40.395273	1553.667822	17.786445
40.430847	1547.302683	17.791463
41.064648	1551.947390	17.796480
40.867005	1533.933766	17.801498
40.965829	1557.896652	17.806515
41.066080	1542.950014	17.811533
40.884841	1514.780988	17.816551
40.812278	1524.052796	17.821568
41.009404	1525.231082	17.826586
40.622823	1504.424129	17.831603
40.698098	1522.421264	17.836621
40.693750	1514.075832	17.841639
40.669958	1511.920031	17.846656
40.410439	1546.015770	17.851674
40.866372	1543.339871	17.856691
40.966176	1533.969535	17.861709
40.927533	1542.067220	17.866727
41.228500	1545.141692	17.871744
41.232572	1544.862729	17.876762
41.090257	1555.706081	17.881779
41.392012	1549.013777	17.886797
41.205557	1548.345215	17.891815
41.370340	1544.636685	17.896832
41.365528	1549.243250	17.901850
40.947847	1560.857242	17.906867
41.447934	1534.154856	17.911885
41.091828	1559.034994	17.916903
41.335133	1544.139468	17.921920
41.228209	1540.556069	17.926938
41.023750	1553.693301	17.931955
41.513991	1571.304996	17.936973
41.343899	1580.139376	17.941991
41.494670	1571.939053	17.947008
41.621330	1576.998127	17.952026
41.245844	1583.472756	17.957043
41.954190	1571.940007	17.962061
41.580625	1579.175652	17.967079
41.527496	1573.700802	17.972096
41.621188	1574.816940	17.977114
41.969023	1602.422544	17.982131
42.321135	1605.175847	17.987149
42.261752	1596.925660	17.992167
41.971758	1573.078349	17.997184
42.163980	1585.364276	18.002202
42.069757	1599.281471	18.007219
42.239406	1593.100989	18.012237
42.363539	1592.190984	18.017255
42.325086	1588.974171	18.022272
42.427277	1580.890128	18.027290
42.003869	1592.601011	18.032307
42.302605	1590.486564	18.037325
42.548759	1594.551333	18.042343
42.497586	1606.934298	18.047360
42.547032	1596.698945	18.052378
42.380766	1592.385694	18.057395
42.760185	1591.738560	18.062413
42.581552	1596.363425	18.067431
42.253627	1604.261896	18.072448
42.516272	1594.363767	18.077466
42.592863	1600.569677	18.082483
42.621590	1596.005107	18.087501
42.267758	1602.737407	18.092519
42.587723	1595.405116	18.097536
42.498400	1605.573107	18.102554
42.347973	1625.029921	18.107571
43.040595	1607.934411	18.112589
43.128275	1631.634934	18.117607
43.219774	1618.927981	18.122624
43.377041	1616.810925	18.127642
42.970208	1613.204558	18.132659
43.091453	1617.896429	18.137677
43.258050	1626.140748	18.142695
43.302197	1614.136613	18.147712
43.480337	1614.690311	18.152730
43.364680	1609.637543	18.157747
43.676073	1615.297935	18.162765
43.523374	1629.620880	18.167783
43.993557	1623.744802	18.172800
44.059111	1611.152102	18.177818
43.390614	1612.042175	18.182835
43.374285	1604.702170	18.187853
43.318803	1594.216146	18.192871
43.177525	1604.710166	18.197888
43.542818	1608.320219	18.202906
43.492832	1614.003642	18.207923
43.670595	1610.230106	18.212941
43.674703	1612.345226	18.217959
43.480623	1614.650828	18.222976
43.849202	1608.383557	18.227994
43.538327	1606.369481	18.233011
43.961289	1615.694447	18.238029
43.960802	1635.795882	18.243047
44.147151	1649.635344	18.248064
44.335779	1642.874525	18.253082
44.238215	1645.929213	18.258099
44.417590	1627.465239	18.263117
44.250906	1618.881376	18.268135
43.898459	1624.734163	18.273152
44.167690	1636.708984	18.278170
44.107732	1646.477498	18.283187
44.426765	1644.238686	18.288205
44.328197	1647.589257	18.293223
44.510410	1645.649112	18.298240
44.860419	1632.001165	18.303258
44.464491	1651.059877	18.308275
44.504692	1645.035297	18.313293
44.500481	1641.382010	18.318311
44.524133	1646.957749	18.323328
44.604081	1637.054123	18.328346
44.339563	1649.315425	18.333363
44.557947	1645.241252	18.338381
44.824945	1650.801775	18.343399
44.589061	1660.099718	18.348416
44.850407	1660.750258	18.353434
44.805288	1670.083848	18.358451
45.055757	1677.416638	18.363469
44.857916	1678.066484	18.368487
45.037133	1678.217326	18.373504
45.374993	1667.055046	18.378522
44.941941	1679.892229	18.383539
45.155568	1676.902601	18.388557
45.333634	1675.121987	18.393575
45.551211	1677.173183	18.398592
45.464553	1666.150968	18.403610
45.390500	1667.877448	18.408627
45.517028	1663.342875	18.413645
45.526834	1661.724377	18.418663
45.269582	1676.447853	18.423680
45.258198	1678.763651	18.428698
45.125913	1673.178694	18.433715
45.450918	1671.695537	18.438733
45.506309	1670.827951	18.443751
45.493771	1698.164031	18.448768
45.763315	1690.072113	18.453786
45.476495	1704.273378	18.458803
45.999467	1694.366694	18.463821
46.043810	1686.966635	18.468839
46.063697	1687.223112	18.473856
46.176895	1679.613877	18.478874
46.302611	1691.009174	18.483891
46.174782	1689.695764	18.488909
46.408223	1687.310151	18.493927
46.238779	1687.804460	18.498944
46.619504	1670.495931	18.503962
46.427830	1663.023417	18.508979
46.150100	1656.101022	18.513997
46.524698	1660.324646	18.519015
46.225318	1654.357368	18.524032
46.252570	1642.230064	18.529050
46.461977	1661.560325	18.534067
46.420972	1679.357554	18.539085
46.528833	1677.385220	18.544103
46.749056	1691.353025	18.549120
46.713694	1685.902039	18.554138
46.765140	1677.539750	18.559155
46.525750	1686.018738	18.564173
46.956668	1679.629812	18.569191
46.724875	1687.623105	18.574208
46.941747	1687.069531	18.579226
46.923760	1681.016464	18.584243
46.820070	1678.650016	18.589261
46.973960	1692.680310	18.594279
46.697570	1688.625262	18.599296
46.979744	1677.322421	18.604314
47.000632	1682.187619	18.609331
46.843510	1690.958650	18.614349
47.317150	1685.986471	18.619367
47.029720	1681.508477	18.624384
47.063842	1679.794864	18.629402
47.304190	1686.545692	18.634419
47.131712	1686.735323	18.639437
47.477465	1704.044616	18.644455
47.157816	1711.635090	18.649472
47.674525	1705.103484	18.654490
47.305672	1710.076469	18.659507
47.151847	1708.951243	18.664525
47.586720	1695.347903	18.669543
47.277959	1708.490898	18.674560
47.119792	1701.695702	18.679578
47.125360	1721.198550	18.684595
47.567497	1727.210936	18.689613
47.913939	1732.453658	18.694631
47.765358	1729.507631	18.699648
48.067259	1725.067763	18.704666
48.056958	1728.191919	18.709683
47.798174	1734.204414	18.714701
48.015337	1729.538964	18.719719
48.015685	1727.552311	18.724736
47.993616	1719.108916	18.729754
48.097275	1718.604857	18.734771
48.019047	1732.779174	18.739789
48.230685	1740.160661	18.744807
47.847122	1751.494087	18.749824
48.672738	1749.747039	18.754842
48.685708	1756.809439	18.759859
48.625169	1750.306958	18.764877
48.652790	1748.644711	18.769895
48.633819	1751.430486	18.774912
48.557621	1752.729461	18.779930
48.568043	1752.628803	18.784947
48.863609	1754.115448	18.789965
49.125110	1752.093432	18.794983
48.705377	1755.756369	18.800000
49.143279	1746.144786	18.805018
49.453525	1738.865884	18.810035
48.856154	1738.514530	18.815053
49.088820	1718.936119	18.820071
48.876209	1719.909214	18.825088
48.905509	1738.977299	18.830106
49.107763	1745.878946	18.835123
49.203797	1742.230095	18.840141
49.336188	1742.292454	18.845159
49.152676	1743.271920	18.850176
49.279577	1744.302552	18.855194
49.611354	1738.698611	18.860211
49.430490	1744.239366	18.865229
49.754494	1733.264860	18.870247
49.484625	1740.144277	18.875264
49.456592	1741.960953	18.880282
49.423131	1739.753178	18.885299
49.263378	1732.907883	18.890317
49.732944	1731.670648	18.895335
49.664981	1733.965591	18.900352
49.730450	1742.329924	18.905370
49.837826	1730.071792	18.910387
49.727226	1733.271720	18.915405
49.793277	1730.955268	18.920423
49.584529	1737.096636	18.925440
50.118566	1754.547417	18.930458
49.848136	1765.950899	18.935475
49.770304	1769.724476	18.940493
50.269567	1762.693838	18.945511
50.014020	1772.370937	18.950528
50.106560	1766.666717	18.955546
50.322772	1770.797659	18.960563
50.077337	1766.377434	18.965581
50.430859	1767.027435	18.970599
50.390960	1762.324322	18.975616
50.196006	1758.589744	18.980634
50.471578	1760.976191	18.985651
50.308638	1778.557038	18.990669
50.716568	1784.968156	18.995687
50.488012	1795.396009	19.000704
50.402832	1788.252507	19.005722
50.808050	1793.874412	19.010739
50.176247	1799.136326	19.015757
50.776880	1785.509611	19.020775
50.780541	1799.328017	19.025792
51.004153	1791.023147	19.030810
50.942974	1790.388075	19.035827
50.537531	1801.787950	19.040845
51.198214	1801.300441	19.045863
51.198057	1807.427446	19.050880
51.086743	1815.382719	19.055898
51.434364	1811.503390	19.060915
51.374902	1815.616965	19.065933
51.461947	1814.564999	19.070951
51.646864	1817.118497	19.075968
51.680963	1801.966639	19.080986
51.536988	1792.035700	19.086003
51.346959	1783.285577	19.091021
51.441672	1797.564509	19.096039
51.617279	1804.423244	19.101056
51.554692	1826.746501	19.106074
52.101258	1817.875733	19.111091
51.644693	1819.757618	19.116109
51.700319	1807.512394	19.121127
52.085846	1814.800120	19.126144
51.909312	1807.650729	19.131162
52.029015	1817.142169	19.136179
51.545259	1823.473723	19.141197
51.815285	1820.792819	19.146215
52.158687	1806.159485	19.151232
51.870229	1813.023025	19.156250
52.244440	1810.507976	19.161267
51.989763	1809.060630	19.166285
52.234261	1824.235910	19.171303
52.189937	1832.361404	19.176320
52.333539	1835.041043	19.181338
52.300459	1842.054201	19.186355
52.592633	1833.993200	19.191373
53.025829	1837.656977	19.196391
52.622499	1832.371587	19.201408
52.568351	1825.982883	19.206426
53.179299	1828.592704	19.211443
52.763227	1837.711860	19.216461
53.121524	1825.014084	19.221479
53.030897	1827.347263	19.226496
53.164097	1818.839721	19.231514
53.273396	1828.170808	19.236531
53.032828	1833.518200	19.241549
53.198101	1818.063835	19.246567
52.923376	1822.490167	19.251584
52.964126	1834.010812	19.256602
53.021405	1822.938779	19.261619
53.273071	1828.481369	19.266637
53.153779	1827.696689	19.271655
53.450820	1834.314276	19.276672
53.324457	1820.968642	19.281690
53.677711	1829.387800	19.286707
53.148576	1829.742853	19.291725
53.099605	1820.408644	19.296743
53.259017	1824.860118	19.301760
52.899714	1842.288317	19.306778
53.492405	1844.388249	19.311795
53.678210	1856.625095	19.316813
53.556581	1852.030942	19.321831
53.634236	1866.433784	19.326848
53.733355	1861.791837	19.331866
53.869301	1849.123211	19.336883
53.683769	1861.729168	19.341901
54.179798	1870.644674	19.346919
54.472780	1877.291244	19.351936
54.105155	1868.124229	19.356954
54.011465	1859.171506	19.361971
54.014967	1880.581395	19.366989
54.164016	1879.911217	19.372007
54.384873	1883.138538	19.377024
54.411472	1884.251244	19.382042
54.660525	1874.158466	19.387059
54.602645	1879.547524	19.392077
54.220953	1873.318003	19.397095
54.622104	1880.219454	19.402112
53.946829	1885.172154	19.407130
54.304179	1877.588371	19.412147
54.422761	1904.705729	19.417165
54.892627	1900.592950	19.422183
55.114359	1904.946420	19.427200
55.061211	1906.839480	19.432218
55.266734	1908.802971	19.437235
55.210809	1910.004345	19.442253
54.990132	1915.833086	19.447271
55.267978	1902.540887	19.452288
55.184690	1915.800692	19.457306
55.166045	1902.167243	19.462323
55.348936	1909.021721	19.467341
55.463776	1902.610750	19.472359
55.441426	1901.941166	19.477376
55.138473	1909.930200	19.482394
55.476070	1902.879662	19.487411
55.317253	1905.629568	19.492429
55.821630	1905.582265	19.497447
55.477601	1907.207112	19.502464
55.327353	1910.448009	19.507482
55.932451	1914.592476	19.512499
56.143685	1923.830289	19.517517
56.136475	1914.918795	19.522535
56.008855	1899.798919	19.527552
55.890537	1906.109978	19.532570
56.343032	1918.524566	19.537587
55.982372	1914.721993	19.542605
55.987655	1927.308586	19.547623
56.393448	1914.933492	19.552640
56.153087	1906.483904	19.557658
56.390592	1916.342011	19.562675
56.335451	1910.230280	19.567693
56.315019	1907.877256	19.572711
56.743771	1904.818667	19.577728
56.361082	1914.791416	19.582746
56.384772	1917.863001	19.587763
56.465616	1913.961700	19.592781
56.446469	1918.238760	19.597799
56.943710	1911.859606	19.602816
56.454067	1919.732129	19.607834
56.595011	1912.970925	19.612851
57.016452	1907.516215	19.617869
56.776086	1914.996622	19.622887
57.100824	1904.161870	19.627904
56.787462	1908.315964	19.632922
57.000581	1918.374590	19.637939
56.978732	1932.870446	19.642957
56.945512	1943.769047	19.647975
57.410007	1933.107039	19.652992
57.355344	1944.644562	19.658010
57.373040	1942.098262	19.663027
57.025766	1947.409230	19.668045
57.288845	1946.697268	19.673063
57.639205	1943.592971	19.678080
57.276396	1935.689858	19.683098
57.456867	1948.666954	19.688115
57.678771	1955.216357	19.693133
57.801269	1964.155315	19.698151
58.079593	1967.297985	19.703168
57.915085	1976.215084	19.708186
57.751303	1973.007161	19.713203
58.352468	1973.326668	19.718221
58.076855	1971.733206	19.723239
57.897830	1958.545281	19.728256
57.814272	1972.212595	19.733274
58.052292	1962.920613	19.738291
58.306978	1967.578733	19.743309
57.994500	1964.263966	19.748327
58.206177	1953.236424	19.753344
58.181114	1968.925182	19.758362
58.669356	1978.641097	19.763379
58.794987	1966.909966	19.768397
58.481817	1967.092150	19.773415
59.031595	1970.550179	19.778432
58.529798	1963.751460	19.783450
58.726495	1972.971174	19.788467
58.659616	1976.066654	19.793485
58.886959	1978.053416	19.798503
59.232216	1981.462268	19.803520
59.016975	1990.069714	19.808538
59.090599	1987.309992	19.813555
59.471008	1987.685156	19.818573
59.522387	1988.005830	19.823591
59.425608	1962.903241	19.828608
59.111768	1961.647785	19.833626
59.262839	1945.673305	19.838643
59.480864	1953.204894	19.843661
59.235687	1974.093010	19.848679
59.559122	1978.716574	19.853696
59.776674	1990.640157	19.858714
59.791853	1980.881907	19.863731
59.585652	1977.016930	19.868749
59.499381	1981.317299	19.873767
60.045750	1970.346477	19.878784
59.625555	1984.456028	19.883802
59.618598	1978.836807	19.888819
59.794277	1981.928211	19.893837
59.662496	1989.032687	19.898855
60.038990	1980.641979	19.903872
59.910993	1983.235973	19.908890
60.185445	1976.326032	19.913907
60.373757	1967.628716	19.918925
59.878343	1975.651626	19.923943
60.333261	1985.640275	19.928960
60.431942	2004.944611	19.933978
60.597043	2006.914562	19.938995
60.528112	2005.767908	19.944013
60.345936	2010.824478	19.949031
60.598806	2001.089655	19.954048
60.886096	2006.581014	19.959066
60.884448	2002.719588	19.964083
60.573578	2000.634666	19.969101
60.497605	1997.906666	19.974119
60.344545	1994.374557	19.979136
60.565698	2004.520052	19.984154
60.606570	2019.536103	19.989171
61.019132	2020.201871	19.994189
60.857498	2028.435847	19.999207
61.471885	2027.118864	20.004224
61.484456	2016.412466	20.009242
61.611670	2026.786891	20.014259
61.528256	2025.532432	20.019277
61.605168	2025.144315	20.024295
61.801119	2019.576088	20.029312
61.837380	2015.853331	20.034330
61.770439	2015.365460	20.039347
62.046077	2017.689019	20.044365
61.814571	2020.307394	20.049383
61.964852	2014.107801	20.054400
62.000517	2014.962666	20.059418
61.761711	2010.266027	20.064435
61.926149	2021.819005	20.069453
61.707590	2028.095767	20.074471
61.930496	2018.438070	20.079488
62.078984	2016.180785	20.084506
61.600443	2019.455187	20.089523
61.810965	2011.410257	20.094541
61.835279	2025.787158	20.099559
62.149562	2028.360961	20.104576
62.220175	2036.292059	20.109594
62.113269	2037.555057	20.114611
62.287592	2034.131176	20.119629
62.606198	2035.057322	20.124647
62.526542	2034.233276	20.129664
62.698044	2043.658401	20.134682
62.567923	2050.693429	20.139699
62.901065	2045.521740	20.144717
62.610233	2076.772589	20.149735
63.032138	2070.642911	20.154752
62.978660	2064.456917	20.159770
63.311196	2055.305534	20.164787
62.884033	2065.255590	20.169805
62.854791	2072.574990	20.174823
63.010121	2062.402647	20.179840
62.972605	2057.757260	20.184858
62.941811	2062.528582	20.189875
63.372759	2078.226530	20.194893
63.603756	2088.166019	20.199911
63.280093	2089.528085	20.204928
64.063840	2091.338036	20.209946
63.826735	2087.732791	20.214963
63.913145	2080.306946	20.219981
64.118351	2083.996137	20.224999
64.141800	2075.185049	20.230016
64.347191	2077.370383	20.235034
64.067331	2087.092466	20.240051
64.576358	2082.499908	20.245069
64.277745	2066.730720	20.250087
64.131026	2056.033967	20.255104
64.374845	2057.574516	20.260122
64.423333	2067.178153	20.265139
64.366908	2063.004546	20.270157
64.647584	2072.405987	20.275175
64.759042	2079.706097	20.280192
64.916923	2071.796946	20.285210
64.362028	2060.885285	20.290227
64.792345	2061.620584	20.295245
64.687513	2074.438800	20.300263
64.621866	2070.762169	20.305280
64.682555	2076.580706	20.310298
64.677331	2078.135807	20.315315
64.718507	2070.641675	20.320333
64.512252	2074.196709	20.325351
64.631372	2077.237379	20.330368
64.966072	2088.089995	20.335386
64.943269	2104.028653	20.340403
65.556266	2098.722650	20.345421
65.474836	2101.807894	20.350439
65.373475	2102.016074	20.355456
65.358189	2106.566284	20.360474
65.668451	2109.118721	20.365491
65.541502	2097.868218	20.370509
65.144007	2103.283207	20.375527
65.280495	2099.612085	20.380544
65.602314	2110.381828	20.385562
65.394872	2129.208181	20.390579
65.771980	2119.911221	20.395597
65.735655	2128.161449	20.400615
65.741821	2127.160113	20.405632
65.909259	2124.374392	20.410650
65.921221	2125.616867	20.415667
66.031435	2128.679417	20.420685
66.281255	2148.084110	20.425703
66.355565	2157.767060	20.430720
66.509509	2144.801146	20.435738
66.441247	2159.787556	20.440755
66.606829	2146.338432	20.445773
66.947979	2146.200757	20.450791
67.003286	2151.600180	20.455808
67.171019	2137.343747	20.460826
66.896042	2143.332249	20.465843
67.131343	2146.760251	20.470861
66.941058	2123.662201	20.475879
66.994214	2139.670582	20.480896
67.238800	2149.856488	20.485914
67.064804	2152.306836	20.490931
67.012956	2137.522270	20.495949
67.063070	2163.040233	20.500967
67.421234	2148.150941	20.505984
67.513719	2140.098023	20.511002
67.424527	2143.917553	20.516019
67.582528	2143.183015	20.521037
67.282292	2154.363461	20.526055
67.300813	2157.920421	20.531072
67.477594	2136.080453	20.536090
67.552711	2146.993389	20.541107
67.711769	2159.357455	20.546125
67.472706	2170.960747	20.551143
67.610029	2174.604158	20.556160
68.057940	2183.000563	20.561178
67.558702	2173.495686	20.566195
67.668352	2181.090297	20.571213
68.357266	2191.862905	20.576231
68.388993	2204.813616	20.581248
68.698908	2195.653169	20.586266
68.578512	2197.744185	20.591283
68.618505	2198.170501	20.596301
68.942131	2201.313864	20.601319
68.633525	2200.671042	20.606336
68.695355	2196.187522	20.611354
68.676497	2192.673288	20.616371
68.902500	2195.492440	20.621389
69.090974	2197.592400	20.626407
69.046567	2192.359747	20.631424
69.374507	2181.618663	20.636442
69.035386	2192.904442	20.641459
69.195821	2188.485424	20.646477
69.201331	2188.478358	20.651495
69.485806	2190.912224	20.656512
69.497078	2188.300837	20.661530
69.092451	2183.677777	20.666547
69.432175	2186.934975	20.671565
69.520563	2198.567865	20.676583
69.376938	2195.425892	20.681600
69.698456	2189.515099	20.686618
69.551151	2188.272389	20.691635
69.350268	2186.125853	20.696653
69.445519	2184.910528	20.701671
69.714574	2202.135123	20.706688
69.826937	2206.845908	20.711706
69.936889	2220.109779	20.716723
70.074113	2217.781899	20.721741
70.222427	2206.001339	20.726759
70.089079	2208.113299	20.731776
70.370881	2199.899593	20.736794
70.036208	2209.344203	20.741811
70.232913	2206.327279	20.746829
70.454667	2205.787068	20.751847
70.668203	2229.949855	20.756864
70.739255	2238.448867	20.761882
70.679733	2232.837930	20.766899
70.820597	2232.346798	20.771917
70.819950	2240.443532	20.776935
70.801110	2240.575631	20.781952
71.073193	2227.488554	20.786970
71.266022	2225.445967	20.791987
71.031841	2233.317241	20.797005
71.482526	2222.827116	20.802023
71.378323	2229.784163	20.807040
71.427494	2215.079365	20.812058
71.275070	2228.940377	20.817075
71.258029	2225.122245	20.822093
71.378342	2227.591737	20.827111
71.404330	2236.986711	20.832128
71.819619	2247.049506	20.837146
71.834821	2250.734435	20.842163
71.523963	2263.294658	20.847181
72.001881	2245.848823	20.852199
71.946584	2260.789224	20.857216
72.001828	2255.260651	20.862234
71.707073	2253.221886	20.867251
71.801679	2264.013823	20.872269
72.139400	2255.614985	20.877287
71.979393	2285.863830	20.882304
72.383261	2276.480705	20.887322
72.509641	2286.910507	20.892339
72.459131	2290.922112	20.897357
72.929076	2279.436273	20.902375
72.662156	2284.226447	20.907392
72.742037	2281.800735	20.912410
72.853923	2281.112871	20.917427
72.775090	2277.806386	20.922445
72.849462	2272.699483	20.927463
73.202318	2273.226920	20.932480
73.156216	2269.334758	20.937498
73.229959	2274.982976	20.942515
73.252817	2278.095670	20.947533
73.337513	2273.274991	20.952551
73.209811	2264.376206	20.957568
73.404686	2272.715488	20.962586
73.361623	2274.020236	20.967603
73.351151	2289.651957	20.972621
73.832955	2284.706594	20.977639
73.348910	2291.353004	20.982656
73.510670	2295.959984	20.987674
73.780656	2282.382396	20.992691
73.665235	2286.729976	20.997709
73.936815	2292.791827	21.002727
73.769818	2290.748412	21.007744
73.970394	2294.126930	21.012762
74.287429	2308.503048	21.017779
74.320775	2319.002767	21.022797
74.796820	2308.085383	21.027815
74.377141	2316.440900	21.032832
74.829268	2300.108125	21.037850
74.853630	2308.292146	21.042867
74.562044	2325.946081	21.047885
74.555765	2324.197936	21.052903
74.772285	2318.122934	21.057920
74.641972	2315.630061	21.062938
75.037860	2309.771856	21.067955
74.692641	2303.322391	21.072973
74.739370	2298.446409	21.077991
74.597056	2311.686100	21.083008
74.924664	2322.296200	21.088026
75.460235	2324.106438	21.093043
75.107740	2334.804559	21.098061
75.282558	2339.233286	21.103079
75.061055	2332.784528	21.108096
75.372205	2337.704332	21.113114
75.698246	2334.764287	21.118131
75.909052	2359.402792	21.123149
76.123888	2355.881137	21.128167
75.471042	2353.636763	21.133184
76.152347	2353.948223	21.138202
76.329887	2360.380614	21.143219
76.021815	2367.477208	21.148237
76.241434	2364.061757	21.153255
76.291526	2365.115696	21.158272
76.576190	2356.261206	21.163290
76.655659	2358.137894	21.168307
76.640998	2358.063256	21.173325
77.196826	2343.894170	21.178343
76.772479	2354.411850	21.183360
76.731576	2346.315595	21.188378
76.990086	2342.783832	21.193395
76.614581	2338.107312	21.198413
76.781459	2331.289868	21.203431
76.615493	2341.157555	21.208448
76.627325	2338.922015	21.213466
77.051498	2346.576668	21.218483
77.025615	2345.127384	21.223501
77.031784	2337.997357	21.228519
76.923714	2344.679788	21.233536
77.231138	2363.827040	21.238554
77.126756	2357.571958	21.243571
77.389436	2359.974722	21.248589
77.496754	2364.989966	21.253607
77.154573	2352.702328	21.258624
77.373990	2359.395462	21.263642
77.731713	2375.845544	21.268659
77.481465	2389.666465	21.273677
77.885356	2393.750355	21.278695
77.787056	2397.881299	21.283712
77.743439	2398.797596	21.288730
78.222737	2392.771895	21.293747
78.088536	2412.091103	21.298765
78.221141	2399.621525	21.303783
78.178148	2414.294272	21.308800
78.474157	2418.886173	21.313818
78.752979	2415.215083	21.318835
78.573359	2413.910650	21.323853
78.649291	2417.473462	21.328871
78.894931	2427.321971	21.333888
78.714878	2422.996510	21.338906
78.991558	2411.545322	21.343923
79.019137	2427.108987	21.348941
79.697367	2444.359855	21.353959
79.489786	2440.086758	21.358976
79.418735	2418.856918	21.363994
79.338658	2410.078653	21.369011
79.588487	2440.536962	21.374029
79.951726	2432.711274	21.379047
79.891534	2431.785782	21.384064
79.410178	2413.496185	21.389082
79.559919	2416.721599	21.394099
79.700746	2426.102315	21.399117
79.818737	2437.001553	21.404135
79.924018	2432.853176	21.409152
80.025472	2432.052921	21.414170
80.358223	2432.440421	21.419187
80.028790	2446.159976	21.424205
80.165081	2436.684137	21.429223
80.445772	2433.861420	21.434240
80.407777	2439.735168	21.439258
80.679852	2443.841667	21.444275
80.509765	2447.693841	21.449293
80.717262	2458.979171	21.454311
80.731577	2466.460929	21.459328
80.600204	2461.889371	21.464346
81.029832	2451.496041	21.469363
81.018206	2466.425756	21.474381
80.704108	2453.231392	21.479399
81.010910	2454.957790	21.484416
80.938952	2455.929736	21.489434
81.413689	2443.354433	21.494451
81.167104	2456.515713	21.499469
81.222809	2471.123225	21.504487
81.538708	2476.220079	21.509504
81.391090	2481.557601	21.514522
81.872217	2471.556394	21.519539
81.981024	2475.544216	21.524557
81.814053	2475.898149	21.529575
81.964906	2471.316975	21.534592
81.890410	2481.034884	21.539610
81.700035	2471.514372	21.544627
81.454177	2483.572829	21.549645
81.661031	2494.610529	21.554663
81.978471	2499.824340	21.559680
82.121727	2501.853690	21.564698
82.625637	2519.822247	21.569715
82.182438	2528.246131	21.574733
82.450422	2522.628472	21.579751
83.121816	2525.759708	21.584768
82.902012	2535.096542	21.589786
83.035694	2525.901857	21.594803
83.035916	2521.656161	21.599821
83.222262	2517.209316	21.604839
83.497588	2521.301161	21.609856
83.248003	2526.749346	21.614874
83.622598	2512.760017	21.619891
83.461501	2532.391213	21.624909
83.239038	2520.023776	21.629927
83.589603	2526.515954	21.634944
83.215411	2527.171934	21.639962
83.460054	2520.166601	21.644979
83.447278	2529.486933	21.649997
83.618520	2522.196778	21.655015
83.841221	2537.410107	21.660032
83.975319	2542.290575	21.665050
84.321421	2538.393998	21.670067
84.320727	2542.886172	21.675085
84.331878	2540.459579	21.680103
84.652941	2542.643844	21.685120
84.611329	2550.321762	21.690138
84.631257	2534.596435	21.695155
84.790337	2544.510741	21.700173
84.717073	2537.655989	21.705191
84.679815	2541.185757	21.710208
84.562426	2537.475572	21.715226
84.831035	2539.495161	21.720243
85.050391	2540.175253	21.725261
84.950681	2536.632928	21.730279
85.477383	2538.465061	21.735296
85.164668	2545.212468	21.740314
85.113433	2557.667829	21.745331
85.325718	2564.160840	21.750349
85.484120	2564.075906	21.755367
85.535527	2565.595285	21.760384
85.344072	2582.207905	21.765402
85.734256	2570.339713	21.770419
85.258849	2577.310503	21.775437
85.550876	2568.355606	21.780455
85.664590	2571.040937	21.785472
85.651960	2594.843981	21.790490
85.735890	2594.871601	21.795507
85.995865	2600.174841	21.800525
86.117618	2594.355523	21.805543
86.055039	2601.943999	21.810560
86.453840	2610.104658	21.815578
86.471674	2613.480146	21.820595
86.969896	2618.038291	21.825613
86.829708	2625.588031	21.830631
87.271933	2618.194836	21.835648
87.059101	2620.632576	21.840666
86.995509	2619.951445	21.845683
87.405847	2609.412422	21.850701
87.191636	2622.515203	21.855719
87.444725	2611.300440	21.860736
87.172673	2622.596304	21.865754
87.347133	2609.212194	21.870771
87.384439	2618.619769	21.875789
87.481337	2616.152746	21.880807
87.669636	2605.082034	21.885824
87.551270	2606.522308	21.890842
87.688883	2614.659339	21.895859
87.706099	2625.098928	21.900877
87.677726	2626.193715	21.905895
88.381313	2627.149751	21.910912
88.085769	2639.729877	21.915930
87.947201	2637.470296	21.920947
88.197540	2626.747554	21.925965
88.031916	2632.398690	21.930983
88.492592	2641.167728	21.936000
88.406644	2670.681935	21.941018
88.611822	2660.995181	21.946035
88.501224	2664.143398	21.951053
88.668548	2656.672894	21.956071
88.644567	2663.365658	21.961088
88.732994	2673.735721	21.966106
89.293579	2678.167531	21.971123
89.581642	2680.134485	21.976141
89.375199	2690.040324	21.981159
89.710293	2672.210898	21.986176
89.993931	2682.109367	21.991194
89.894650	2668.107366	21.996211
89.343673	2654.772831	22.001229
89.666949	2658.524358	22.006247
90.096471	2658.139772	22.011264
90.039249	2675.988001	22.016282
90.199801	2671.429600	22.021299
90.157314	2669.401669	22.026317
89.731321	2686.025066	22.031335
90.083350	2670.720136	22.036352
89.871415	2675.468633	22.041370
89.909906	2670.826659	22.046387
90.050245	2665.035024	22.051405
90.076460	2692.472983	22.056423
90.601774	2702.567318	22.061440
90.770754	2709.746097	22.066458
90.594741	2700.500011	22.071475
90.903420	2703.093711	22.076493
90.542937	2725.832389	22.081511
90.844927	2728.758300	22.086528
91.374338	2728.972869	22.091546
91.093739	2727.475286	22.096563
91.419334	2727.720785	22.101581
91.357947	2722.470198	22.106599
91.942952	2708.299256	22.111616
91.667270	2716.503040	22.116634
91.654366	2721.115986	22.121651
92.319559	2728.814211	22.126669
91.695756	2733.905275	22.131687
91.913369	2731.116945	22.136704
91.861178	2736.439342	22.141722
91.937434	2739.523169	22.146739
92.290920	2747.750912	22.151757
92.277875	2770.958100	22.156775
92.467500	2754.211266	22.161792
92.509251	2753.209718	22.166810
92.661500	2755.108674	22.171827
92.724955	2746.955439	22.176845
92.658083	2740.211263	22.181863
92.825245	2750.149591	22.186880
92.859294	2753.465107	22.191898
92.857170	2758.899084	22.196915
93.031890	2763.512013	22.201933
92.973328	2778.486501	22.206951
93.406688	2768.627999	22.211968
93.070725	2768.910568	22.216986
93.233567	2768.238940	22.222003
93.630568	2763.231435	22.227021
93.712422	2779.889575	22.232039
94.034883	2789.796085	22.237056
94.217320	2796.197214	22.242074
94.236219	2796.737030	22.247091
94.286624	2789.976489	22.252109
94.177651	2786.977519	22.257127
94.263157	2780.949963	22.262144
94.575301	2794.235602	22.267162
94.439472	2793.942743	22.272179
94.593491	2780.910182	22.277197
94.823334	2787.781975	22.282215
94.600948	2785.070881	22.287232
94.792312	2786.526277	22.292250
94.664186	2786.814243	22.297267
94.860946	2782.544207	22.302285
94.657612	2791.404283	22.307303
94.939375	2798.032620	22.312320
95.141369	2811.565517	22.317338
94.954407	2820.125679	22.322355
95.438296	2817.041598	22.327373
95.352567	2816.811540	22.332391
95.092956	2817.809501	22.337408
95.372929	2821.026037	22.342426
95.396700	2836.239154	22.347443
95.939771	2831.715664	22.352461
95.969207	2842.022105	22.357479
96.317673	2837.042765	22.362496
96.130271	2831.562108	22.367514
95.928205	2840.947434	22.372531
96.007932	2831.423727	22.377549
96.265178	2845.794971	22.382567
96.365451	2855.380646	22.387584
96.872610	2851.356838	22.392602
96.875878	2849.847795	22.397619
97.082597	2859.901807	22.402637
97.005032	2857.102320	22.407655
97.102127	2846.996923	22.412672
97.450735	2844.257687	22.417690
97.240650	2863.339467	22.422707
97.225392	2860.489929	22.427725
97.431180	2851.124656	22.432743
97.414607	2852.718618	22.437760
97.386972	2850.240740	22.442778
97.432175	2863.616992	22.447795
97.742990	2881.379253	22.452813
97.920491	2881.789167	22.457831
97.876150	2885.017320	22.462848
98.105009	2886.037284	22.467866
97.933170	2882.704591	22.472883
98.277743	2879.955766	22.477901
98.249987	2883.787715	22.482919
97.928631	2891.328727	22.487936
98.553939	2894.561000	22.492954
98.528785	2903.028550	22.497971
98.896322	2904.700486	22.502989
98.470908	2903.248787	22.508007
98.888086	2898.329261	22.513024
99.140285	2904.425138	22.518042
98.613161	2919.834740	22.523059
98.936758	2912.107935	22.528077
99.255232	2925.623149	22.533095
99.160596	2930.305041	22.538112
99.358122	2934.688643	22.543130
99.347923	2927.849607	22.548147
99.891478	2948.349840	22.553165
100.060511	2955.467381	22.558183
100.011159	2955.258262	22.563200
100.345379	2947.372431	22.568218
100.600891	2957.031739	22.573235
100.782346	2936.750376	22.578253
100.372151	2926.935834	22.583271
100.636342	2920.994564	22.588288
100.718040	2917.064543	22.593306
100.376950	2915.283197	22.598323
100.574272	2918.752838	22.603341
100.562613	2923.928044	22.608359
100.667934	2931.998039	22.613376
101.142236	2933.668685	22.618394
100.608646	2939.255913	22.623411
101.080085	2939.137576	22.628429
101.069035	2937.263481	22.633447
101.212276	2935.670756	22.638464
101.474679	2934.891216	22.643482
101.251478	2960.357417	22.648499
101.845477	2955.909145	22.653517
101.748107	2961.053985	22.658535
101.665055	2971.466551	22.663552
102.069941	2961.902705	22.668570
101.730979	2970.370783	22.673587
101.955536	2960.762543	22.678605
102.027789	2965.019043	22.683623
102.077355	2977.914899	22.688640
102.336180	2989.911383	22.693658
102.301445	2996.965477	22.698675
102.381031	2993.786946	22.703693
102.360959	2997.004962	22.708711
102.301902	3001.694575	22.713728
102.859868	3011.409515	22.718746
102.970105	3024.287084	22.723763
102.928010	3019.208718	22.728781
103.240981	3014.116995	22.733799
103.191595	3013.958221	22.738816
103.587331	3023.166531	22.743834
103.557093	3040.562558	22.748851
103.755016	3032.099048	22.753869
103.952469	3047.632355	22.758887
103.963440	3044.255527	22.763904
104.362788	3035.740231	22.768922
103.754089	3043.593790	22.773939
103.965886	3041.069046	22.778957
104.089489	3038.599267	22.783975
103.989987	3032.268390	22.788992
104.522398	3048.851844	22.794010
104.117850	3067.224735	22.799027
104.871801	3059.407989	22.804045
105.083719	3060.379540	22.809063
104.721777	3073.018607	22.814080
105.270615	3047.560270	22.819098
105.069293	3058.248180	22.824115
104.872801	3064.070371	22.829133
105.385884	3054.799121	22.834151
105.482805	3065.797368	22.839168
105.384649	3057.425894	22.844186
105.237442	3070.677278	22.849203
105.843022	3070.768018	22.854221
105.777588	3074.088459	22.859239
105.732420	3066.311832	22.864256
105.836370	3078.915938	22.869274
106.072110	3071.982555	22.874291
106.018107	3071.463480	22.879309
106.243906	3066.112699	22.884327
106.094559	3076.478492	22.889344
106.407640	3087.163838	22.894362
106.449219	3096.232813	22.899379
106.677168	3099.879313	22.904397
106.608380	3097.252999	22.909415
106.816676	3104.942485	22.914432
106.997037	3101.036797	22.919450
106.588411	3099.843543	22.924467
106.665298	3109.337153	22.929485
107.049927	3118.233451	22.934503
107.070622	3135.661584	22.939520
107.441399	3128.785299	22.944538
107.458273	3140.973086	22.949555
107.417086	3155.348965	22.954573
107.626690	3154.931008	22.959591
107.843032	3160.235908	22.964608
107.787436	3148.649927	22.969626
108.120767	3158.071998	22.974643
108.271475	3163.558053	22.979661
108.567370	3167.202387	22.984679
108.616523	3175.826574	22.989696
108.829564	3167.753866	22.994714
108.617677	3174.833935	22.999731
109.032377	3177.394299	23.004749
109.006169	3175.201665	23.009767
108.897245	3181.913718	23.014784
108.860193	3172.866987	23.019802
109.064832	3176.299341	23.024819
109.238983	3187.935866	23.029837
109.174444	3198.477787	23.034855
109.509295	3200.699286	23.039872
109.767990	3198.211085	23.044890
109.550508	3196.608996	23.049907
110.080101	3197.888580	23.054925
109.918843	3198.108684	23.059943
109.591884	3207.968804	23.064960
109.961977	3207.040720	23.069978
110.306766	3222.393402	23.074995
110.022968	3224.455559	23.080013
110.693074	3211.371779	23.085031
110.589482	3225.935446	23.090048
111.052157	3223.218855	23.095066
110.665494	3226.719555	23.100083
111.066660	3242.441615	23.105101
111.575150	3232.812305	23.110119
111.144829	3249.762674	23.115136
111.555766	3245.780063	23.120154
111.561163	3248.397843	23.125171
111.733023	3241.450969	23.130189
111.866558	3241.100988	23.135207
111.735119	3245.158796	23.140224
111.578437	3244.570351	23.145242
111.483362	3249.904493	23.150259
111.793438	3249.231390	23.155277
112.146341	3241.268485	23.160295
112.290506	3235.843349	23.165312
112.085567	3240.966111	23.170330
112.218871	3243.417189	23.175347
112.306489	3256.265534	23.180365
112.556706	3269.082456	23.185383
112.619994	3264.870534	23.190400
112.877369	3269.294250	23.195418
112.523294	3272.431081	23.200435
112.983299	3283.575320	23.205453
113.136806	3303.213231	23.210471
112.800945	3309.391256	23.215488
113.151344	3299.098062	23.220506
113.471165	3299.598564	23.225523
113.495546	3320.021650	23.230541
113.781292	3317.002889	23.235559
113.574659	3322.236858	23.240576
113.935376	3317.150003	23.245594
113.958863	3321.771495	23.250611
113.713338	3324.655838	23.255629
114.295676	3339.187323	23.260647
114.067303	3352.849919	23.265664
114.577953	3347.317533	23.270682
115.038245	3345.781970	23.275699
114.741866	3344.830368	23.280717
115.141848	3340.306733	23.285735
115.163215	3335.885164	23.290752
115.284559	3335.628369	23.295770
115.552342	3329.192386	23.300787
115.239960	3332.876339	23.305805
115.586552	3341.843341	23.310823
115.444025	3361.468757	23.315840
115.830817	3357.323997	23.320858
115.803858	3353.816279	23.325875
115.829331	3364.008879	23.330893
116.051848	3352.624590	23.335911
116.012686	3365.155801	23.340928
116.272041	3367.814124	23.345946
116.385088	3372.776103	23.350963
116.414294	3380.989846	23.355981
116.923219	3386.665067	23.360999
116.829576	3382.469483	23.366016
116.773556	3373.971545	23.371034
116.834053	3376.442908	23.376051
116.893367	3380.707100	23.381069
117.281954	3373.848312	23.386087
117.097814	3381.762562	23.391104
117.209563	3388.693589	23.396122
117.545019	3392.480339	23.401139
117.462051	3405.201846	23.406157
117.671851	3400.835161	23.411175
117.661552	3406.399684	23.416192
117.760042	3406.458023	23.421210
117.927624	3401.103032	23.426227
118.036957	3419.048319	23.431245
118.332732	3430.262123	23.436263
118.364846	3438.971775	23.441280
118.448107	3436.367563	23.446298
118.457368	3438.032982	23.451315
118.447919	3449.663598	23.456333
118.626191	3439.142898	23.461351
118.997949	3444.309850	23.466368
118.938926	3456.292118	23.471386
119.594612	3461.449198	23.476403
119.678100	3454.824661	23.481421
119.363325	3447.412539	23.486439
119.846482	3455.380099	23.491456
119.635818	3445.873981	23.496474
119.845401	3449.193915	23.501491
119.506735	3460.821975	23.506509
119.867772	3449.144934	23.511527
119.929608	3465.523091	23.516544
120.036197	3479.049799	23.521562
120.283447	3489.030925	23.526579
120.395211	3483.687951	23.531597
120.533508	3481.037985	23.536615
120.822067	3495.840654	23.541632
120.869667	3497.020143	23.546650
121.108559	3501.284052	23.551667
121.249985	3512.278686	23.556685
121.537646	3497.803581	23.561703
121.307045	3501.342386	23.566720
121.320996	3494.676217	23.571738
121.303655	3503.557406	23.576755
121.290570	3513.343295	23.581773
121.562073	3525.800721	23.586791
121.627706	3530.299142	23.591808
121.551060	3529.760849	23.596826
122.075784	3545.846610	23.601843
121.886699	3560.016784	23.606861
122.221499	3550.109764	23.611879
122.303574	3559.111215	23.616896
122.517630	3565.465167	23.621914
122.717670	3570.997000	23.626931
123.073650	3587.831028	23.631949
123.555807	3572.822196	23.636967
123.121198	3587.630150	23.641984
123.365959	3578.105599	23.647002
123.419000	3574.719580	23.652019
123.264380	3578.339894	23.657037
123.603895	3567.421328	23.662055
123.758567	3577.961605	23.667072
123.572746	3588.408302	23.672090
123.796239	3601.304506	23.677107
123.928783	3611.053867	23.682125
124.160880	3598.657075	23.687143
124.035332	3604.800899	23.692160
124.304511	3591.374830	23.697178
124.874802	3602.168997	23.702195
124.447777	3623.864845	23.707213
124.907253	3622.393101	23.712231
125.191566	3621.580930	23.717248
124.973714	3627.854326	23.722266
125.274653	3621.463272	23.727283
125.059896	3616.919589	23.732301
125.489494	3623.951073	23.737319
125.539186	3626.866273	23.742336
125.328094	3625.346495	23.747354
125.520719	3643.344852	23.752371
125.310790	3658.449784	23.757389
125.701754	3651.705334	23.762407
125.815813	3655.145953	23.767424
126.244938	3683.734476	23.772442
126.443589	3672.994043	23.777459
126.639166	3686.522486	23.782477
126.430023	3679.596042	23.787495
126.672225	3672.732142	23.792512
126.822295	3690.250433	23.797530
127.057641	3692.550019	23.802547
127.046050	3717.231010	23.807565
127.271335	3699.230634	23.812583
127.564220	3700.147630	23.817600
127.565471	3700.466898	23.822618
127.648489	3692.111792	23.827635
127.777555	3701.009085	23.832653
128.050083	3719.288986	23.837671
128.095273	3732.704582	23.842688
127.843969	3740.628947	23.847706
128.347719	3729.699805	23.852723
128.211089	3736.694990	23.857741
128.398657	3731.719770	23.862759
128.567883	3737.376145	23.867776
128.659624	3755.026525	23.872794
129.054763	3762.808493	23.877811
129.191660	3759.841696	23.882829
129.222425	3750.989884	23.887847
129.558643	3745.090289	23.892864
129.307166	3750.821618	23.897882
129.615912	3753.453259	23.902899
129.249018	3766.138546	23.907917
129.572154	3778.834952	23.912935
130.027906	3775.678078	23.917952
130.066198	3783.612138	23.922970
130.149457	3772.442450	23.927987
130.378652	3779.167722	23.933005
130.636617	3792.555738	23.938023
130.791774	3802.373990	23.943040
130.714142	3800.870670	23.948058
131.239232	3788.267316	23.953075
131.234272	3799.224940	23.958093
131.185346	3797.125510	23.963111
131.476697	3796.703155	23.968128
131.122320	3803.898281	23.973146
131.487995	3797.500761	23.978163
131.013507	3802.827168	23.983181
131.113444	3797.031303	23.988199
131.151134	3808.328243	23.993216
130.965849	3826.528676	23.998234
131.812870	3815.209638	24.003251
131.797462	3837.094241	24.008269
131.826750	3848.865308	24.013287
132.160597	3858.826587	24.018304
131.725741	3870.288598	24.023322
131.938312	3872.788500	24.028339
132.339728	3884.558468	24.033357
132.756166	3909.114108	24.038375
133.164805	3909.943438	24.043392
132.690820	3910.822260	24.048410
133.387188	3907.152661	24.053427
133.678991	3929.340821	24.058445
133.699206	3938.925817	24.063463
134.295728	3929.651730	24.068480
134.027747	3924.829321	24.073498
134.085756	3923.728347	24.078515
134.328791	3932.783026	24.083533
134.045217	3936.877082	24.088551
134.462694	3930.450006	24.093568
134.410497	3946.788676	24.098586
134.958099	3956.483098	24.103603
135.124786	3953.742779	24.108621
134.669422	3959.490967	24.113639
134.735781	3956.771366	24.118656
135.153264	3958.918454	24.123674
135.546859	3975.197871	24.128691
135.988347	3970.396045	24.133709
135.986824	3974.919471	24.138727
136.010050	3978.717618	24.143744
136.006937	3978.295803	24.148762
135.909875	3980.486396	24.153779
136.164246	3968.693800	24.158797
135.961398	3985.301960	24.163815
136.405061	3969.852848	24.168832
136.718913	3995.417710	24.173850
136.444685	4002.503397	24.178867
136.580131	4006.649438	24.183885
136.821719	4011.776782	24.188903
136.995749	4000.365112	24.193920
137.044301	4022.176077	24.198938
137.207463	4019.877605	24.203955
137.400522	4034.793593	24.208973
137.309766	4037.234122	24.213991
137.690434	4037.564481	24.219008
137.687731	4067.164990	24.224026
138.062075	4061.143556	24.229043
137.973501	4048.018757	24.234061
138.018278	4054.710633	24.239079
138.356467	4054.440490	24.244096
138.403221	4083.878182	24.249114
138.397310	4090.148658	24.254131
138.642954	4075.651366	24.259149
138.670864	4076.029321	24.264167
138.638398	4093.114664	24.269184
139.056038	4097.494988	24.274202
139.270954	4103.815214	24.279219
139.417236	4109.937144	24.284237
139.190484	4116.175981	24.289255
139.618289	4123.543100	24.294272
139.616905	4126.630950	24.299290
139.939674	4136.246495	24.304307
140.086804	4141.082947	24.309325
140.101186	4141.121663	24.314343
140.373801	4149.504697	24.319360
140.196180	4170.782425	24.324378
140.320289	4149.209798	24.329395
140.780212	4174.112935	24.334413
141.083558	4183.742622	24.339431
141.634301	4177.689081	24.344448
141.547195	4173.369512	24.349466
141.756387	4179.787440	24.354483
142.006459	4169.622914	24.359501
142.006780	4172.579134	24.364519
142.421749	4166.312830	24.369536
142.484938	4175.756614	24.374554
142.608131	4160.478757	24.379571
142.547082	4159.580035	24.384589
142.465960	4169.482621	24.389607
142.943547	4163.955208	24.394624
142.780774	4160.280160	24.399642
142.668472	4165.941474	24.404659
142.747125	4178.922642	24.409677
142.583083	4190.653227	24.414695
143.009420	4186.778829	24.419712
143.152939	4194.640483	24.424730
143.351918	4216.537881	24.429747
143.489758	4231.779889	24.434765
143.124381	4233.527948	24.439783
143.988864	4231.419686	24.444800
144.395533	4238.964868	24.449818
144.179567	4255.816923	24.454835
144.687558	4255.718722	24.459853
144.176483	4248.986464	24.464871
144.485213	4254.148027	24.469888
144.536493	4275.508191	24.474906
144.808968	4266.954995	24.479923
145.226186	4274.456821	24.484941
144.923072	4283.603522	24.489959
145.605016	4303.114468	24.494976
145.487426	4308.202432	24.499994
145.292526	4315.198529	24.505011
145.599701	4316.589993	24.510029
145.869846	4315.249852	24.515047
146.013831	4313.829924	24.520064
146.119149	4332.994695	24.525082
146.012651	4339.663624	24.530099
146.165246	4343.585194	24.535117
146.698257	4344.817936	24.540135
147.003296	4328.612564	24.545152
147.001972	4343.866652	24.550170
146.826009	4354.038569	24.555187
147.246946	4342.432296	24.560205
147.492490	4351.401092	24.565223
147.546846	4348.489818	24.570240
147.316630	4357.503797	24.575258
147.635055	4367.601614	24.580275
148.045806	4367.752552	24.585293
148.098862	4382.747070	24.590311
148.112677	4379.967331	24.595328
148.215781	4377.973372	24.600346
148.311311	4385.002644	24.605363
148.848533	4398.256226	24.610381
148.697553	4398.766550	24.615399
148.872496	4394.575834	24.620416
148.941300	4406.549510	24.625434
149.027533	4420.311609	24.630451
149.524106	4428.961167	24.635469
149.288580	4434.982849	24.640487
149.716205	4432.867127	24.645504
149.662756	4447.417719	24.650522
149.791380	4464.375545	24.655539
150.018644	4460.595751	24.660557
149.884098	4472.980282	24.665575
150.143729	4482.678496	24.670592
150.415233	4491.552774	24.675610
150.941434	4503.128711	24.680627
150.915956	4497.364368	24.685645
150.748829	4512.529431	24.690663
151.277446	4519.221465	24.695680
151.285765	4527.222066	24.700698
151.540447	4533.391395	24.705715
151.940304	4519.420521	24.710733
151.970709	4528.282918	24.715751
152.170284	4527.232486	24.720768
152.247185	4530.618666	24.725786
152.171989	4545.018638	24.730803
152.688085	4543.721860	24.735821
152.515042	4554.361509	24.740839
152.776110	4549.633105	24.745856
153.022137	4544.402070	24.750874
153.047601	4553.395068	24.755891
153.266217	4562.727001	24.760909
153.314115	4570.829087	24.765927
153.459535	4577.054402	24.770944
153.569824	4577.663885	24.775962
153.399969	4582.246591	24.780979
154.022876	4571.135782	24.785997
153.666902	4584.335287	24.791015
154.235568	4583.081257	24.796032
154.249550	4602.115411	24.801050
154.232030	4601.455945	24.806067
154.507761	4595.356407	24.811085
154.392042	4615.985358	24.816103
154.358273	4633.816503	24.821120
154.777465	4629.792093	24.826138
154.438452	4639.357732	24.831155
155.056768	4658.503279	24.836173
154.958721	4678.101336	24.841191
155.275643	4677.019597	24.846208
155.642517	4681.166691	24.851226
155.739950	4691.451007	24.856243
155.732848	4703.201816	24.861261
156.566067	4713.039219	24.866279
156.573846	4710.825203	24.871296
157.026503	4713.727503	24.876314
156.996854	4709.376587	24.881331
157.164471	4704.043145	24.886349
157.286183	4704.514720	24.891367
157.043922	4710.912826	24.896384
157.418731	4722.659396	24.901402
157.640862	4727.902590	24.906419
157.284907	4733.702876	24.911437
157.568015	4739.730094	24.916455
157.703662	4758.317894	24.921472
158.122378	4761.161109	24.926490
158.448188	4761.336611	24.931507
158.611144	4761.842518	24.936525
158.695947	4761.844047	24.941543
158.786966	4787.979970	24.946560
159.151819	4786.622328	24.951578
159.092075	4792.317195	24.956595
159.375981	4777.524406	24.961613
159.564707	4785.573476	24.966631
159.770923	4773.252197	24.971648
159.987495	4789.376671	24.976666
159.895164	4807.665763	24.981683
160.192230	4804.811674	24.986701
160.213839	4813.519099	24.991719
159.860338	4815.591009	24.996736
160.478303	4814.465195	25.001754
160.536072	4839.491804	25.006771
160.923033	4838.972368	25.011789
161.009629	4842.389329	25.016807
161.232251	4834.638290	25.021824
161.467583	4851.765204	25.026842
161.282075	4871.467144	25.031859
161.696139	4867.891105	25.036877
161.899757	4870.545223	25.041895
161.635592	4873.338434	25.046912
162.176444	4878.725172	25.051930
162.064439	4893.718997	25.056947
162.091938	4897.180006	25.061965
161.993618	4893.890979	25.066983
162.088912	4911.100864	25.072000
162.640851	4924.212552	25.077018
162.361049	4931.078515	25.082035
163.083405	4929.959650	25.087053
163.267175	4954.107316	25.092071
163.148680	4958.091156	25.097088
163.565423	4946.787949	25.102106
163.701495	4968.420379	25.107123
163.857708	4974.249231	25.112141
164.186222	4981.383244	25.117159
164.127662	4981.601155	25.122176
164.381990	4980.990368	25.127194
164.456771	5003.537299	25.132211
164.654406	4999.327062	25.137229
164.960588	5017.006134	25.142247
165.288620	5017.518771	25.147264
165.531813	5023.973345	25.152282
165.369387	5035.666583	25.157299
165.835529	5031.669196	25.162317
166.061566	5023.661843	25.167335
166.244504	5028.234851	25.172352
166.477687	5030.243141	25.177370
166.622385	5033.907340	25.182387
166.501383	5029.423786	25.187405
166.787377	5031.108198	25.192423
166.492056	5059.023522	25.197440
166.826011	5050.567061	25.202458
167.091381	5061.432179	25.207475
167.147060	5067.561090	25.212493
167.267865	5071.872612	25.217511
167.324258	5090.407388	25.222528
167.567300	5083.610356	25.227546
167.859500	5108.998893	25.232563
168.031803	5106.395138	25.237581
168.249522	5115.899852	25.242599
168.202049	5114.029712	25.247616
168.409832	5125.101516	25.252634
168.701428	5144.052776	25.257651
168.837421	5133.936457	25.262669
168.856117	5147.059418	25.267687
169.064010	5161.644570	25.272704
169.371132	5158.298706	25.277722
169.465830	5173.970237	25.282739
169.626001	5182.395395	25.287757
169.684728	5191.264690	25.292775
169.535419	5205.146110	25.297792
169.946216	5207.785351	25.302810
170.093365	5221.229322	25.307827
170.497429	5227.943119	25.312845
170.638684	5228.248751	25.317863
170.641360	5250.931068	25.322880
171.159821	5262.102126	25.327898
170.868047	5250.297249	25.332915
171.102627	5257.558084	25.337933
171.625315	5272.134850	25.342951
171.377804	5285.220136	25.347968
171.610914	5278.769956	25.352986
172.232171	5287.455217	25.358003
172.122182	5306.739764	25.363021
172.757967	5310.582196	25.368039
172.828976	5309.427912	25.373056
173.224738	5314.020573	25.378074
173.169186	5302.318809	25.383091
173.238415	5309.992300	25.388109
173.217051	5297.986145	25.393127
172.826821	5320.097138	25.398144
173.535413	5327.660047	25.403162
173.616378	5331.038684	25.408179
173.690686	5354.313922	25.413197
174.036625	5354.701780	25.418215
173.926280	5361.035865	25.423232
173.980046	5361.485254	25.428250
174.392192	5370.685364	25.433267
174.525581	5398.854737	25.438285
175.145856	5395.563523	25.443303
175.035020	5421.031020	25.448320
175.167810	5423.134829	25.453338
175.280977	5415.734499	25.458355
175.397762	5446.992834	25.463373
175.704491	5449.169613	25.468391
175.811589	5455.868713	25.473408
176.397171	5462.237424	25.478426
176.337109	5485.567334	25.483443
176.270175	5480.072761	25.488461
176.817750	5483.949759	25.493479
176.757716	5486.393495	25.498496
177.018724	5512.482362	25.503514
177.384082	5499.401109	25.508531
177.311145	5506.680417	25.513549
177.853864	5513.017436	25.518567
178.275811	5525.778281	25.523584
178.457653	5533.265580	25.528602
178.457428	5535.824088	25.533619
178.615494	5536.420489	25.538637
179.216443	5530.558225	25.543655
178.521078	5533.091463	25.548672
178.671536	5525.596235	25.553690
179.010282	5531.998824	25.558707
178.637673	5538.422001	25.563725
178.938516	5550.754541	25.568743
179.357887	5561.294168	25.573760
179.361155	5570.820781	25.578778
179.463995	5566.811160	25.583795
179.661146	5590.342533	25.588813
180.065138	5593.533629	25.593831
180.136032	5606.046058	25.598848
180.493064	5631.344131	25.603866
181.037467	5630.244942	25.608883
181.047042	5632.667376	25.613901
181.168761	5629.483135	25.618919
181.326716	5637.609958	25.623936
181.302641	5630.935509	25.628954
181.719111	5654.465846	25.633971
181.356948	5657.311014	25.638989
181.881298	5654.718692	25.644007
181.920983	5686.319461	25.649024
182.296897	5687.919598	25.654042
182.225809	5685.036715	25.659059
182.774556	5700.663952	25.664077
182.826647	5704.883557	25.669095
182.978495	5717.361933	25.674112
183.247707	5705.289450	25.679130
183.336373	5722.760171	25.684148
183.049552	5750.004377	25.689165
183.845606	5737.944637	25.694183
184.018890	5749.827225	25.699200
184.117332	5767.201248	25.704218
184.302655	5775.558226	25.709236
184.306326	5778.343516	25.714253
184.658512	5779.120606	25.719271
184.733547	5803.756675	25.724288
184.808759	5809.732518	25.729306
185.290002	5802.581706	25.734324
185.341230	5820.373200	25.739341
185.719495	5827.010355	25.744359
185.627471	5828.868420	25.749376
185.786978	5838.330960	25.754394
186.139065	5857.656631	25.759412
186.258090	5848.751723	25.764429
186.558941	5861.099470	25.769447
186.440867	5870.544135	25.774464
186.502777	5874.604879	25.779482
187.075383	5889.669940	25.784500
187.042606	5910.893256	25.789517
187.538797	5921.571948	25.794535
187.621612	5911.126070	25.799552
187.853556	5933.463702	25.804570
188.071752	5948.427981	25.809588
188.212541	5950.695018	25.814605
188.615573	5941.891892	25.819623
188.550834	5956.360807	25.824640
188.600401	5970.540090	25.829658
189.103205	5966.302955	25.834676
189.223890	5984.317232	25.839693
189.518903	5980.995932	25.844711
189.772836	5993.322162	25.849728
189.583242	6006.892918	25.854746
189.873230	6002.604735	25.859764
190.018308	6009.412109	25.864781
190.263434	6016.688949	25.869799
190.365739	6034.348254	25.874816
190.494160	6018.571211	25.879834
190.587225	6045.325051	25.884852
190.364442	6055.227099	25.889869
190.834301	6066.581965	25.894887
191.148113	6066.667357	25.899904
191.331622	6087.597609	25.904922
191.388192	6088.715299	25.909940
191.613893	6097.223370	25.914957
191.999472	6113.654357	25.919975
192.005995	6118.251112	25.924992
192.134525	6134.192842	25.930010
192.774969	6148.295401	25.935028
192.577730	6150.145104	25.940045
192.899407	6161.618865	25.945063
193.580179	6171.033130	25.950080
193.385945	6176.912040	25.955098
193.812329	6179.349934	25.960116
193.496372	6184.486688	25.965133
194.064578	6194.004670	25.970151
194.114538	6208.818233	25.975168
194.344126	6206.539520	25.980186
194.514601	6207.984439	25.985204
194.692815	6227.135337	25.990221
195.070899	6223.053335	25.995239
195.512913	6233.703129	26.000256
195.410102	6255.573007	26.005274
196.099220	6263.399140	26.010292
195.682856	6258.784493	26.015309
196.000802	6252.623264	26.020327
196.384568	6260.785238	26.025344
196.219379	6282.739056	26.030362
196.764847	6277.674457	26.035380
196.474106	6292.419688	26.040397
196.770057	6303.645903	26.045415
197.243905	6305.313894	26.050432
196.998797	6330.628132	26.055450
197.331666	6321.483506	26.060468
197.614028	6347.169207	26.065485
198.085644	6328.923372	26.070503
198.187638	6347.064591	26.075520
198.664992	6360.597001	26.080538
198.884023	6364.515605	26.085556
199.037783	6363.089994	26.090573
198.962671	6373.646102	26.095591
199.207440	6360.642324	26.100608
199.417264	6387.096513	26.105626
199.821675	6393.425286	26.110644
199.639065	6398.846114	26.115661
199.720085	6402.167557	26.120679
199.801537	6406.060114	26.125696
199.699852	6432.352411	26.130714
200.431779	6432.989536	26.135732
200.548490	6443.552877	26.140749
200.509833	6457.738825	26.145767
200.942477	6466.672010	26.150784
201.002300	6483.715515	26.155802
201.078833	6487.704076	26.160820
201.037774	6499.397215	26.165837
201.545067	6504.376081	26.170855
202.061055	6515.804192	26.175872
202.167477	6517.431655	26.180890
203.098088	6528.556073	26.185908
202.938683	6542.961978	26.190925
202.743438	6546.671311	26.195943
203.125659	6528.997296	26.200960
203.162940	6531.142456	26.205978
203.314754	6549.842448	26.210996
203.470492	6549.105706	26.216013
203.673974	6553.293551	26.221031
203.988961	6570.042353	26.226048
204.246290	6580.944497	26.231066
204.736244	6586.458794	26.236084
204.709149	6589.257797	26.241101
204.785137	6601.433524	26.246119
204.968520	6609.096574	26.251136
205.300432	6611.244341	26.256154
205.662730	6609.049837	26.261172
205.762897	6631.197108	26.266189
206.052711	6638.262574	26.271207
206.094112	6626.807868	26.276224
205.889268	6643.829238	26.281242
206.429471	6654.160780	26.286260
206.784445	6660.615567	26.291277
206.485873	6665.117940	26.296295
207.085146	6682.841984	26.301312
206.926941	6694.195974	26.306330
207.316904	6705.280839	26.311348
207.350473	6722.863021	26.316365
207.840461	6723.437241	26.321383
208.380868	6743.284005	26.326400
208.391153	6759.353049	26.331418
208.841931	6754.340367	26.336436
209.337475	6753.863364	26.341453
209.076356	6750.669108	26.346471
209.718444	6753.824080	26.351488
209.631954	6774.253118	26.356506
209.679636	6771.678384	26.361524
209.817568	6778.309443	26.366541
209.922714	6788.011785	26.371559
210.343248	6789.586841	26.376576
210.066481	6811.323197	26.381594
210.708600	6811.984891	26.386612
210.905273	6830.187140	26.391629
210.970701	6830.161078	26.396647
210.926330	6830.924346	26.401664
211.216465	6849.788346	26.406682
211.534331	6864.655843	26.411700
211.573354	6866.617455	26.416717
211.960393	6878.474744	26.421735
212.426961	6885.125056	26.426752
212.304887	6894.464009	26.431770
212.581202	6915.873951	26.436788
212.884081	6919.112148	26.441805
213.051393	6919.254736	26.446823
213.279817	6924.923366	26.451840
213.733808	6938.371128	26.456858
213.649841	6942.709552	26.461876
213.697339	6953.908209	26.466893
213.917822	6967.930596	26.471911
214.120995	6973.838518	26.476928
213.952616	6990.782874	26.481946
214.409402	6988.961924	26.486964
215.084878	7006.573503	26.491981
214.921648	7005.903325	26.496999
215.166706	7034.205932	26.502016
215.723563	7034.082644	26.507034
215.999306	7039.200105	26.512052
215.962219	7053.454824	26.517069
216.084959	7063.490499	26.522087
216.540929	7062.916729	26.527104
216.545864	7089.546461	26.532122
216.658886	7099.590005	26.537140
217.394627	7108.085802	26.542157
217.189322	7124.553108	26.547175
217.566635	7114.378872	26.552192
217.803238	7132.195894	26.557210
217.723542	7148.456733	26.562228
218.249040	7152.934882	26.567245
218.259695	7159.858633	26.572263
218.711416	7173.095325	26.577280
218.868525	7180.122412	26.582298
219.092958	7195.533076	26.587316
219.298516	7201.518601	26.592333
219.216349	7210.483957	26.597351
219.457154	7221.939967	26.602368
219.955460	7229.605851	26.607386
219.976879	7242.299075	26.612404
220.049795	7250.558366	26.617421
220.264399	7277.185694	26.622439
220.711088	7277.205070	26.627456
220.869709	7297.890016	26.632474
221.280894	7307.550991	26.637492
221.930183	7313.379276	26.642509
222.160231	7327.650682	26.647527
222.249310	7334.727241	26.652544
222.126269	7332.026200	26.657562
222.370493	7318.685709	26.662580
222.901736	7336.565372	26.667597
222.986005	7350.932426	26.672615
223.540603	7345.696069	26.677632
223.498283	7349.478785	26.682650
223.695988	7353.882578	26.687668
224.182938	7367.740124	26.692685
224.103353	7381.374850	26.697703
224.254368	7375.566297	26.702720
224.260910	7378.910849	26.707738
224.629670	7395.218487	26.712756
224.607789	7401.150656	26.717773
224.678177	7404.658919	26.722791
225.240744	7420.477768	26.727808
225.340256	7432.603221	26.732826
225.358033	7432.417165	26.737844
225.843474	7443.665185	26.742861
226.000376	7453.473013	26.747879
226.097979	7459.906238	26.752896
226.017382	7473.844918	26.757914
226.537614	7488.806674	26.762932
226.637498	7493.010517	26.767949
226.532705	7528.890961	26.772967
227.296593	7527.945498	26.777984
227.486144	7550.844676	26.783002
227.343242	7556.148652	26.788020
228.015008	7565.994073	26.793037
227.927485	7587.972845	26.798055
228.185904	7600.977940	26.803072
228.624526	7614.489356	26.808090
228.984676	7616.875899	26.813108
229.451559	7632.955717	26.818125
229.119489	7646.427936	26.823143
229.409767	7649.193068	26.828160
229.921757	7659.489691	26.833178
229.957760	7679.529855	26.838196
230.263409	7694.579531	26.843213
230.282090	7696.705007	26.848231
230.901166	7693.182178	26.853248
231.363439	7719.938413	26.858266
231.436372	7733.089643	26.863284
232.027676	7728.719104	26.868301
231.602773	7742.998540	26.873319
232.446103	7752.986692	26.878336
232.566729	7763.795840	26.883354
232.471542	7763.036883	26.888372
232.869171	7767.532461	26.893389
233.453618	7791.962381	26.898407
233.501027	7783.682242	26.903424
233.544471	7803.489273	26.908442
233.863579	7790.799718	26.913460
234.189012	7802.876870	26.918477
234.078519	7814.265809	26.923495
234.629756	7816.646316	26.928512
234.788592	7810.047160	26.933530
234.753775	7828.217511	26.938548
234.858823	7833.194080	26.943565
235.092835	7852.534895	26.948583
235.171830	7856.505336	26.953600
235.399321	7863.646634	26.958618
235.321164	7897.187623	26.963636
235.968152	7899.250737	26.968653
235.978169	7923.092622	26.973671
236.059623	7934.377091	26.978688
236.505074	7959.662702	26.983706
236.627859	7964.756086	26.988724
237.107914	7975.641854	26.993741
237.278293	7988.359180	26.998759
237.768344	7996.370631	27.003776
237.944304	8020.260180	27.008794
238.231733	8017.558100	27.013812
238.720063	8017.142806	27.018829
238.469426	8042.135874	27.023847
238.624090	8047.998454	27.028864
239.068104	8048.487221	27.033882
239.232852	8064.833627	27.038900
239.706894	8067.671048	27.043917
240.054208	8094.459661	27.048935
240.626980	8093.693349	27.053952
240.790039	8101.560667	27.058970
240.662340	8097.302280	27.063988
241.140119	8095.713124	27.069005
241.198242	8106.777981	27.074023
241.456949	8119.388492	27.079040
241.874070	8116.476091	27.084058
241.994058	8122.133355	27.089076
242.190628	8133.207636	27.094093
242.546326	8147.304008	27.099111
242.628571	8141.450255	27.104128
242.737747	8167.169871	27.109146
243.031209	8177.425370	27.114164
243.462513	8183.698703	27.119181
243.826806	8198.273730	27.124199
243.829540	8201.255550	27.129216
244.246902	8211.483454	27.134234
244.240320	8223.672889	27.139252
244.535240	8234.177626	27.144269
244.704021	8241.969749	27.149287
245.045012	8257.505358	27.154304
245.557880	8243.258830	27.159322
245.449538	8257.509537	27.164340
245.750013	8258.374490	27.169357
245.840224	8277.256443	27.174375
245.789212	8284.384114	27.179392
246.224588	8291.863875	27.184410
246.431708	8316.405956	27.189428
246.713998	8331.332532	27.194445
246.804537	8347.266178	27.199463
246.964133	8362.847337	27.204480
247.619542	8358.374340	27.209498
247.857258	8391.767733	27.214516
248.722874	8377.965289	27.219533
248.688806	8391.315136	27.224551
248.604873	8395.568209	27.229568
249.294824	8409.927079	27.234586
249.535085	8433.336502	27.239604
249.813723	8413.322487	27.244621
249.841739	8434.432709	27.249639
250.190868	8449.926306	27.254656
250.602427	8444.441696	27.259674
250.395020	8465.244057	27.264692
250.511239	8468.037092	27.269709
250.853118	8471.209619	27.274727
250.943943	8491.621405	27.279744
251.351171	8489.022896	27.284762
251.188667	8503.130607	27.289780
251.292769	8518.148725	27.294797
251.657077	8533.961031	27.299815
251.840494	8550.264866	27.304832
252.357054	8551.320436	27.309850
252.394749	8581.076982	27.314868
252.892008	8584.390008	27.319885
253.289332	8596.806505	27.324903
253.220850	8618.130659	27.329920
253.690462	8628.984740	27.334938
253.887115	8646.095473	27.339956
253.990810	8658.053656	27.344973
254.406950	8684.905542	27.349991
254.980924	8681.187455	27.355008
255.150179	8689.510877	27.360026
255.129100	8699.128363	27.365044
255.602914	8710.988246	27.370061
255.837145	8726.376121	27.375079
256.077719	8729.700982	27.380096
256.629574	8738.651173	27.385114
256.630089	8758.491497	27.390132
257.004024	8764.648324	27.395149
257.140749	8774.414604	27.400167
257.449158	8774.341153	27.405184
257.718030	8797.368100	27.410202
257.861663	8816.298875	27.415220
258.108869	8820.622824	27.420237
258.471416	8824.409835	27.425255
258.536334	8844.823087	27.430272
259.044875	8849.482303	27.435290
259.162451	8867.407728	27.440308
259.684386	8865.271657	27.445325
259.680885	8880.156211	27.450343
259.811646	8894.054658	27.455360
260.598985	8900.818431	27.460378
260.187680	8925.028094	27.465396
260.929229	8922.650058	27.470413
261.305969	8936.846123	27.475431
260.889357	8960.505474	27.480448
261.412320	8958.050538	27.485466
261.849483	8967.810760	27.490484
261.825083	8986.139419	27.495501
261.797613	9012.800575	27.500519
262.110841	9028.755715	27.505536
262.801863	9040.376648	27.510554
262.796607	9068.961069	27.515572
263.242998	9072.110379	27.520589
263.500887	9077.441105	27.525607
263.459929	9103.680044	27.530624
263.879552	9117.941447	27.535642
264.525612	9115.493620	27.540660
264.560279	9133.896849	27.545677
264.636952	9136.504311	27.550695
265.190867	9158.340657	27.555712
265.669632	9165.210003	27.560730
265.732713	9172.463126	27.565748
265.713166	9172.394345	27.570765
266.103241	9188.493213	27.575783
266.054420	9199.652651	27.580800
266.611981	9204.928967	27.585818
266.681951	9217.696400	27.590836
266.998691	9230.801828	27.595853
266.900522	9254.153566	27.600871
267.105146	9271.488407	27.605888
267.589246	9280.101522	27.610906
268.018059	9307.454557	27.615924
268.459658	9322.798191	27.620941
269.163865	9342.714800	27.625959
269.065514	9341.799276	27.630976
269.530315	9342.854111	27.635994
269.945066	9371.889948	27.641012
270.235904	9367.810784	27.646029
270.798845	9361.282668	27.651047
270.897251	9373.914682	27.656064
271.329871	9386.928201	27.661082
271.224373	9401.745726	27.666100
271.438499	9398.560122	27.671117
272.107807	9412.480229	27.676135
272.198880	9427.635508	27.681152
272.312432	9427.136709	27.686170
272.350654	9446.292044	27.691188
272.805748	9453.482425	27.696205
272.852810	9460.471477	27.701223
272.988230	9466.106334	27.706240
273.776836	9488.250819	27.711258
273.581365	9482.326706	27.716276
273.642168	9518.805233	27.721293
274.294617	9521.476009	27.726311
274.188298	9549.804791	27.731328
274.529888	9555.965138	27.736346
274.841283	9578.426619	27.741364
275.085542	9588.493421	27.746381
275.405065	9604.777108	27.751399
275.793208	9616.485333	27.756416
276.277237	9639.981736	27.761434
276.439342	9650.591667	27.766452
276.442357	9660.512437	27.771469
276.998030	9651.539596	27.776487
276.794038	9687.967491	27.781504
277.293950	9704.582946	27.786522
277.686960	9721.197754	27.791540
277.945869	9721.347026	27.796557
278.578024	9741.300051	27.801575
278.919165	9766.564049	27.806592
279.089075	9770.262791	27.811610
279.140724	9776.440722	27.816628
279.167586	9794.405326	27.821645
279.647751	9798.007013	27.826663
279.966030	9818.647192	27.831680
280.235949	9824.208415	27.836698
280.577575	9822.976422	27.841716
280.621986	9846.257171	27.846733
281.058909	9854.027466	27.851751
281.067038	9872.153323	27.856768
281.430377	9874.839558	27.861786
281.767155	9888.319708	27.866804
281.969346	9905.696594	27.871821
282.552581	9918.811302	27.876839
282.693503	9938.212553	27.881856
283.148779	9955.001053	27.886874
283.290327	9961.185192	27.891892
283.515935	9971.311098	27.896909
283.914636	9986.694519	27.901927
283.896502	10020.069380	27.906944
284.101020	10019.200365	27.911962
284.872417	10033.165772	27.916980
284.464231	10052.536653	27.921997
285.032393	10060.280629	27.927015
285.172674	10086.795375	27.932032
285.526000	10103.442510	27.937050
285.927029	10125.126401	27.942068
286.161564	10138.913851	27.947085
286.471704	10147.368693	27.952103
286.448120	10162.003537	27.957120
287.175764	10183.377333	27.962138
287.779037	10196.846762	27.967156
287.751352	10221.376281	27.972173
288.211293	10233.577986	27.977191
288.446475	10247.619226	27.982208
288.872562	10253.440203	27.987226
289.293775	10272.785013	27.992244
289.561006	10288.585934	27.997261
290.031645	10282.135096	28.002279
289.839555	10312.773360	28.007296
290.167451	10311.519516	28.012314
290.712929	10326.674104	28.017332
290.701131	10356.585688	28.022349
291.073268	10359.481909	28.027367
291.120382	10378.675185	28.032384
291.378781	10384.545370	28.037402
291.860318	10404.545719	28.042420
292.285410	10424.163971	28.047437
292.614844	10436.543643	28.052455
292.804598	10447.020277	28.057472
293.085365	10473.003753	28.062490
293.490405	10470.239215	28.067508
293.618348	10501.963629	28.072525
293.978248	10511.141447	28.077543
294.537960	10526.843274	28.082560
294.404880	10538.019104	28.087578
294.671992	10542.970355	28.092596
294.624555	10565.517663	28.097613
295.230411	10568.992087	28.102631
295.443576	10589.412812	28.107648
295.638799	10602.653713	28.112666
296.057653	10620.698089	28.117684
295.959017	10637.365128	28.122701
296.163662	10660.878548	28.127719
296.690029	10671.891133	28.132736
297.179420	10689.840537	28.137754
297.804439	10702.343304	28.142772
297.853373	10726.146070	28.147789
298.428798	10736.477622	28.152807
298.587517	10747.352903	28.157824
298.717504	10752.669991	28.162842
299.251855	10754.056977	28.167860
299.311697	10783.426778	28.172877
299.483584	10805.034457	28.177895
300.176513	10810.391300	28.182912
300.115070	10825.928411	28.187930
300.473690	10844.437929	28.192948
300.585573	10863.688001	28.197965
300.858752	10876.651111	28.202983
301.376993	10900.005138	28.208000
301.538629	10917.512038	28.213018
302.212517	10943.144058	28.218036
302.141372	10962.335285	28.223053
302.753275	10980.019969	28.228071
303.138148	10990.674437	28.233088
303.311742	11003.567747	28.238106
303.909894	11023.685308	28.243124
303.801429	11042.963252	28.248141
304.356613	11057.001468	28.253159
304.906959	11069.781270	28.258176
304.762879	11082.879925	28.263194
305.158612	11093.043616	28.268212
305.181577	11115.697002	28.273229
305.855231	11134.349481	28.278247
306.202359	11138.384700	28.283264
306.390226	11161.570250	28.288282
306.793263	11156.995017	28.293300
306.788916	11194.027485	28.298317
307.232432	11196.854652	28.303335
307.597820	11217.414880	28.308352
307.764347	11237.344170	28.313370
308.262588	11241.947949	28.318388
308.731147	11269.436356	28.323405
308.634645	11281.629230	28.328423
309.123723	11303.804479	28.333440
309.477887	11314.375534	28.338458
309.851505	11324.930511	28.343476
310.112147	11358.146248	28.348493
310.374683	11363.944541	28.353511
310.517681	11381.479349	28.358528
310.655467	11411.821916	28.363546
311.321940	11408.257650	28.368564
311.773210	11427.590898	28.373581
311.815210	11445.955654	28.378599
312.214009	11449.052467	28.383616
312.537678	11473.929012	28.388634
312.970787	11464.322991	28.393652
312.813590	11488.689478	28.398669
313.231927	11497.785004	28.403687
313.609168	11523.734459	28.408704
314.012337	11539.857780	28.413722
314.475643	11540.968512	28.418740
314.657087	11564.087628	28.423757
315.019906	11576.297254	28.428775
315.334171	11590.884755	28.433792
315.732317	11612.172628	28.438810
316.081043	11618.736440	28.443828
316.127601	11637.562293	28.448845
316.305835	11638.542567	28.453863
316.641421	11666.246896	28.458880
316.629771	11677.523842	28.463898
317.311157	11701.736951	28.468916
317.472912	11719.096802	28.473933
317.951615	11747.225898	28.478951
318.667358	11766.039702	28.483968
318.978958	11778.540201	28.488986
319.453564	11796.926157	28.494004
319.176190	11815.561846	28.499021
319.675804	11832.884509	28.504039
320.072019	11837.479944	28.509056
320.260348	11871.046762	28.514074
320.528580	11882.976179	28.519092
320.846755	11907.617416	28.524109
320.979243	11923.910216	28.529127
321.544889	11946.761694	28.534144
321.812040	11971.381260	28.539162
322.233236	11977.417772	28.544180
322.702904	12005.760112	28.549197
322.812962	12005.713161	28.554215
323.771269	12027.763538	28.559232
323.657538	12041.492546	28.564250
323.852528	12049.018424	28.569268
324.304966	12075.243724	28.574285
324.427514	12091.872000	28.579303
324.853867	12113.430768	28.584320
324.980963	12140.354596	28.589338
325.397859	12145.557191	28.594356
325.760117	12162.347252	28.599373
325.576059	12191.792115	28.604391
326.476100	12210.087948	28.609408
326.370600	12232.213329	28.614426
326.896640	12246.365723	28.619444
327.496863	12268.426497	28.624461
327.921861	12284.689203	28.629479
328.479721	12296.061001	28.634496
328.413893	12316.998410	28.639514
328.917057	12321.631848	28.644532
329.102508	12337.483768	28.649549
328.984345	12345.647247	28.654567
329.721313	12363.086171	28.659584
330.031819	12392.018142	28.664602
330.160917	12399.959250	28.669620
330.474872	12421.210919	28.674637
330.531052	12440.198177	28.679655
330.938990	12457.773472	28.684672
331.316621	12483.213511	28.689690
331.602750	12493.842482	28.694708
331.891426	12523.938919	28.699725
332.084590	12547.753446	28.704743
332.536876	12569.344545	28.709760
332.826576	12590.525545	28.714778
333.145894	12625.760656	28.719796
333.761087	12642.370644	28.724813
333.780279	12659.705694	28.729831
334.403601	12682.418638	28.734848
334.736558	12706.814434	28.739866
335.274874	12718.380929	28.744884
335.679687	12735.801991	28.749901
335.917217	12755.016347	28.754919
336.663284	12777.145728	28.759936
336.721570	12778.215049	28.764954
336.875409	12796.560275	28.769972
337.485590	12818.336719	28.774989
337.963091	12823.850828	28.780007
338.151985	12848.012631	28.785024
338.430432	12865.393179	28.790042
338.850247	12878.515873	28.795060
339.350200	12902.809024	28.800077
339.195038	12922.821715	28.805095
339.379173	12928.415478	28.810112
339.639057	12969.015466	28.815130
340.170317	12980.255855	28.820148
340.728779	13000.618323	28.825165
340.911225	13041.921526	28.830183
341.173166	13048.718415	28.835200
341.400540	13061.237730	28.840218
341.889939	13097.854958	28.845236
342.223163	13112.055819	28.850253
342.563367	13141.464033	28.855271
343.217802	13152.707157	28.860288
343.562966	13183.199098	28.865306
343.530680	13191.364101	28.870324
343.874583	13210.263375	28.875341
344.078870	13229.532431	28.880359
344.746481	13257.654700	28.885376
344.932428	13275.249009	28.890394
345.329954	13295.165451	28.895412
345.960489	13316.858297	28.900429
345.980860	13342.233335	28.905447
346.424059	13366.617939	28.910464
346.672110	13378.517122	28.915482
346.997407	13410.886223	28.920500
347.603741	13417.694709	28.925517
347.690110	13442.521793	28.930535
348.179587	13453.276260	28.935552
348.347921	13468.097027	28.940570
348.275645	13487.742061	28.945588
348.896268	13507.287323	28.950605
348.819358	13545.003400	28.955623
349.898302	13563.826512	28.960640
349.770059	13576.184104	28.965658
350.262887	13589.238911	28.970676
350.467231	13634.222030	28.975693
350.960919	13650.890473	28.980711
351.619036	13656.619528	28.985728
351.606884	13694.439789	28.990746
351.951744	13711.922891	28.995764
352.833299	13721.678573	29.000781
352.793330	13756.215160	29.005799
353.179350	13775.186156	29.010816
354.089811	13785.359967	29.015834
354.080636	13807.618695	29.020852
354.314042	13823.313003	29.025869
354.628959	13848.111805	29.030887
355.358551	13865.903139	29.035904
355.564490	13883.927404	29.040922
355.944841	13904.132132	29.045940
356.826356	13915.219010	29.050957
356.716957	13945.673245	29.055975
357.255020	13945.486159	29.060992
357.599327	13955.234925	29.066010
358.155720	13980.077816	29.071028
358.454641	13989.836001	29.076045
358.704365	14000.464355	29.081063
358.969946	14017.764837	29.086080
359.329192	14045.405597	29.091098
359.443730	14065.630073	29.096116
360.042571	14077.743208	29.101133
360.168644	14102.593674	29.106151
360.492075	14113.287306	29.111168
360.991606	14142.036439	29.116186
361.384956	14164.674023	29.121204
361.463927	14183.535750	29.126221
361.979548	14213.697275	29.131239
362.284527	14220.430075	29.136256
362.598192	14252.069778	29.141274
362.615010	14271.782725	29.146292
363.098192	14289.705335	29.151309
363.148393	14321.463029	29.156327
363.573274	14344.225640	29.161344
364.158864	14367.849814	29.166362
364.224329	14405.950525	29.171380
365.021200	14438.541361	29.176397
365.440377	14453.992999	29.181415
365.460647	14484.439746	29.186432
366.066257	14501.075152	29.191450
366.932523	14531.687485	29.196468
367.514936	14538.045601	29.201485
367.441665	14555.500074	29.206503
367.917206	14573.976738	29.211520
368.213980	14582.112678	29.216538
368.338119	14607.451835	29.221556
369.018181	14607.081927	29.226573
369.347440	14632.312474	29.231591
369.834089	14646.249348	29.236608
369.933891	14671.625746	29.241626
369.954096	14689.894184	29.246644
370.529034	14706.370283	29.251661
370.994522	14736.412915	29.256679
371.249837	14759.483112	29.261696
371.617648	14777.885975	29.266714
371.776433	14805.997344	29.271732
372.451258	14811.133888	29.276749
372.773315	14843.605838	29.281767
373.299128	14870.677601	29.286784
373.430134	14881.935173	29.291802
373.622589	14913.067452	29.296820
374.228512	14934.199558	29.301837
374.295610	14963.696045	29.306855
375.108420	14986.971274	29.311872
375.327606	15007.079461	29.316890
375.641255	15032.653623	29.321908
376.144102	15063.838689	29.326925
376.553677	15092.667297	29.331943
376.735287	15116.906283	29.336960
377.500981	15137.908908	29.341978
377.287349	15159.256058	29.346996
378.045583	15171.919236	29.352013
378.403253	15213.085662	29.357031
378.786343	15241.527650	29.362048
379.466151	15250.223925	29.367066
379.695149	15272.670106	29.372084
380.140093	15292.138703	29.377101
380.340624	15307.366956	29.382119
381.179090	15324.986296	29.387136
381.309728	15349.095420	29.392154
381.307526	15373.072832	29.397172
382.208828	15387.602624	29.402189
382.339560	15409.115669	29.407207
382.352212	15438.832722	29.412224
382.893876	15459.142619	29.417242
383.258688	15489.509695	29.422260
383.525339	15515.094613	29.427277
384.057323	15552.533318	29.432295
384.228292	15570.807024	29.437312
385.208855	15596.685610	29.442330
385.358552	15616.489205	29.447348
385.928853	15643.781088	29.452365
386.234841	15661.354102	29.457383
386.332308	15696.432498	29.462400
387.078853	15709.694321	29.467418
387.319790	15722.669576	29.472436
387.817209	15741.271604	29.477453
388.189176	15758.364726	29.482471
388.454385	15773.869005	29.487488
388.992533	15779.894417	29.492506
389.144378	15812.415817	29.497524
390.002359	15805.468271	29.502541
390.452462	15807.349605	29.507559
390.860277	15816.809189	29.512576
391.411046	15846.714064	29.517594
391.740188	15846.420627	29.522612
392.069462	15854.525108	29.527629
392.206260	15885.287599	29.532647
392.417540	15894.083999	29.537664
393.178954	15913.119669	29.542682
392.829370	15932.851193	29.547700
393.558208	15957.031865	29.552717
393.981682	15994.365344	29.557735
394.068146	16008.050563	29.562752
394.396888	16028.024842	29.567770
394.437156	16055.206483	29.572788
394.979636	16096.466580	29.577805
395.040499	16124.377999	29.582823
395.555649	16154.236305	29.587840
396.212658	16190.243023	29.592858
396.232082	16224.443387	29.597876
396.782739	16245.955936	29.602893
397.405018	16281.778475	29.607911
397.894336	16300.434730	29.612928
398.625360	16338.543916	29.617946
399.170493	16352.474708	29.622964
399.746219	16372.872602	29.627981
400.082008	16392.018022	29.632999
400.529378	16401.779687	29.638016
400.851199	16431.036765	29.643034
401.018130	16456.692777	29.648052
401.237218	16481.933104	29.653069
401.890598	16500.145712	29.658087
401.931883	16533.161672	29.663104
402.623292	16556.403535	29.668122
402.674890	16586.076546	29.673140
403.367362	16602.799806	29.678157
403.572182	16630.012828	29.683175
403.918923	16660.830707	29.688192
404.479726	16676.849348	29.693210
404.953775	16700.256557	29.698228
405.075717	16736.355129	29.703245
406.009409	16752.426621	29.708263
406.233589	16787.161572	29.713280
406.674045	16803.746690	29.718298
406.942702	16838.653190	29.723316
407.216671	16866.739941	29.728333
407.660127	16881.241280	29.733351
407.490702	16914.149326	29.738368
408.456479	16938.139090	29.743386
408.748347	16963.679201	29.748404
409.092678	17004.312861	29.753421
409.898742	17012.354386	29.758439
410.001609	17040.511232	29.763456
410.144138	17063.852543	29.768474
410.732550	17077.387776	29.773492
411.380097	17103.286160	29.778509
411.624653	17140.329806	29.783527
411.811633	17160.199618	29.788544
412.381092	17182.809575	29.793562
413.019653	17221.107220	29.798580
413.251187	17250.862275	29.803597
413.612199	17269.927613	29.808615
414.112363	17296.814074	29.813632
414.514461	17328.564135	29.818650
414.860289	17357.128666	29.823668
415.131898	17380.219399	29.828685
415.795862	17418.130848	29.833703
416.009724	17435.360175	29.838720
416.361317	17456.424691	29.843738
416.866078	17488.646472	29.848756
417.185610	17515.297750	29.853773
417.763397	17532.697722	29.858791
418.695534	17578.292524	29.863808
418.675138	17597.902462	29.868826
419.122781	17638.059755	29.873844
419.802485	17653.383559	29.878861
419.944918	17680.572354	29.883879
420.046461	17715.664734	29.888896
420.809175	17729.297171	29.893914
421.198320	17774.565521	29.898932
421.344068	17806.561332	29.903949
422.151270	17827.738197	29.908967
422.208303	17871.306129	29.913984
422.715528	17887.546565	29.919002
422.990943	17922.096193	29.924020
424.006160	17959.808528	29.929037
424.308135	17971.320830	29.934055
424.934069	18007.957583	29.939072
425.164394	18024.838902	29.944090
425.748808	18049.452752	29.949108
425.764433	18082.052903	29.954125
426.494647	18097.066954	29.959143
426.694944	18131.192820	29.964160
427.590151	18162.819179	29.969178
427.802654	18187.052371	29.974196
428.422915	18221.256003	29.979213
428.867967	18243.281855	29.984231
428.847626	18272.635130	29.989248
429.862825	18303.075385	29.994266
430.171189	18322.126791	29.999284
430.461732	18343.610891	30.004301
431.047094	18361.911939	30.009319
431.874164	18386.249878	30.014336
431.920881	18408.599660	30.019354
432.442024	18425.926403	30.024372
432.752897	18444.872840	30.029389
433.212856	18454.163943	30.034407
433.234990	18485.503706	30.039424
433.717523	18498.680894	30.044442
434.105401	18522.587463	30.049460
434.301604	18543.279018	30.054477
434.717809	18561.127345	30.059495
434.860690	18602.409690	30.064512
435.223297	18633.897470	30.069530
435.675378	18671.109941	30.074548
436.164223	18701.765947	30.079565
437.008555	18728.259913	30.084583
437.190288	18770.881774	30.089600
437.968621	18785.578598	30.094618
438.425844	18819.931578	30.099636
438.354915	18850.984939	30.104653
438.802398	18877.981759	30.109671
439.365636	18911.432619	30.114688
439.789172	18944.001477	30.119706
440.517344	18983.121105	30.124724
440.789080	19013.478065	30.129741
441.320392	19036.340127	30.134759
441.622219	19065.340417	30.139776
442.230675	19092.962364	30.144794
442.633772	19128.254187	30.149812
442.844424	19172.534767	30.154829
443.446129	19206.708887	30.159847
443.818059	19231.481705	30.164864
444.285381	19264.079692	30.169882
444.825437	19304.434459	30.174900
445.052009	19331.972789	30.179917
445.951829	19366.637574	30.184935
446.272910	19399.657582	30.189952
446.855769	19436.606949	30.194970
447.547111	19461.554842	30.199988
447.884489	19492.007006	30.205005
448.470943	19529.665103	30.210023
448.737366	19547.212433	30.215040
449.115563	19574.800661	30.220058
449.697417	19592.405666	30.225076
449.563062	19633.541205	30.230093
450.229624	19653.050193	30.235111
450.534791	19702.828112	30.240128
451.009687	19727.675871	30.245146
451.487443	19769.082768	30.250164
451.993042	19797.797218	30.255181
452.793098	19826.411656	30.260199
453.192299	19861.517563	30.265216
453.551722	19886.852112	30.270234
453.800663	19924.759833	30.275252
454.166991	19961.754394	30.280269
455.077142	19985.782384	30.285287
455.505939	20015.377248	30.290304
455.401447	20050.580365	30.295322
456.197122	20077.264721	30.300340
456.449858	20105.743234	30.305357
456.756646	20137.114987	30.310375
457.382416	20159.506139	30.315392
457.792138	20194.667030	30.320410
458.311180	20210.425899	30.325428
458.315338	20251.811491	30.330445
459.351632	20273.999596	30.335463
459.877763	20304.831973	30.340480
460.172565	20337.172266	30.345498
460.775794	20358.106139	30.350516
461.066645	20407.496029	30.355533
461.480670	20423.867966	30.360551
461.690255	20461.217455	30.365568
462.474126	20498.474752	30.370586
462.974642	20521.439980	30.375604
463.083428	20568.969822	30.380621
463.574631	20588.845361	30.385639
464.019949	20638.923654	30.390656
464.348925	20679.717623	30.395674
465.176949	20706.630215	30.400692
465.563643	20743.542666	30.405709
466.340591	20781.493948	30.410727
466.375719	20815.284248	30.415744
466.889360	20836.820510	30.420762
467.680097	20873.555498	30.425780
468.182924	20899.197232	30.430797
468.820077	20938.836340	30.435815
468.952964	20980.582530	30.440832
469.298601	21005.984487	30.445850
470.258158	21043.804152	30.450868
470.400136	21077.923710	30.455885
470.781524	21109.381212	30.460903
471.272398	21142.092380	30.465920
472.022175	21181.938997	30.470938
472.598082	21198.884863	30.475956
472.921103	21240.134456	30.480973
473.508532	21256.832843	30.485991
474.107029	21303.466693	30.491008
474.112568	21332.934209	30.496026
474.893375	21351.602593	30.501044
475.178074	21396.850268	30.506061
475.920029	21419.089266	30.511079
476.386193	21464.689391	30.516096
476.961767	21482.168382	30.521114
477.548590	21519.478801	30.526132
478.032322	21558.134303	30.531149
478.068692	21576.530149	30.536167
478.589567	21605.616027	30.541184
478.850042	21649.480650	30.546202
479.660830	21681.760417	30.551220
479.930233	21719.473911	30.556237
480.476210	21752.325240	30.561255
480.772214	21786.610416	30.566272
481.089725	21826.410586	30.571290
482.012202	21852.949806	30.576308
482.086449	21888.932262	30.581325
482.496695	21913.594549	30.586343
483.230950	21934.045401	30.591360
483.364182	21981.441345	30.596378
484.059084	21995.157074	30.601396
484.476393	22027.563244	30.606413
484.762180	22061.365511	30.611431
485.286484	22114.795266	30.616448
485.647207	22138.304929	30.621466
486.181133	22180.850042	30.626484
486.397446	22221.593510	30.631501
487.132807	22262.527682	30.636519
487.946160	22295.919567	30.641536
488.103923	22346.717370	30.646554
488.777820	22368.943360	30.651572
489.085308	22417.817122	30.656589
489.565210	22459.888024	30.661607
490.127258	22494.265460	30.666624
490.623151	22541.613188	30.671642
491.233437	22572.972968	30.676660
491.392821	22625.008705	30.681677
492.020810	22655.362442	30.686695
492.750389	22697.733655	30.691712
492.955093	22746.252278	30.696730
493.860491	22779.136705	30.701748
494.220116	22821.556947	30.706765
494.729292	22857.408529	30.711783
495.431465	22895.848221	30.716800
495.840197	22932.705202	30.721818
496.516672	22963.381028	30.726836
497.057646	23002.694910	30.731853
497.841856	23033.630947	30.736871
498.594120	23060.121355	30.741888
498.641956	23093.117060	30.746906
499.257647	23116.345770	30.751924
499.791215	23157.065528	30.756941
500.303493	23180.877102	30.761959
501.006176	23205.069515	30.766976
501.288925	23245.993283	30.771994
501.984048	23275.503434	30.777012
502.066564	23302.667240	30.782029
502.363914	23341.141002	30.787047
503.040234	23372.105131	30.792064
503.356685	23417.289749	30.797082
504.023718	23445.124684	30.802100
504.300794	23494.654840	30.807117
504.759266	23531.178427	30.812135
505.210989	23575.473189	30.817152
506.116328	23607.351184	30.822170
506.562090	23638.557349	30.827188
506.991362	23688.604974	30.832205
507.292172	23719.395673	30.837223
508.162323	23750.521852	30.842240
508.526048	23783.107932	30.847258
508.986477	23819.149045	30.852276
509.369682	23846.810149	30.857293
510.338841	23875.465704	30.862311
510.797258	23908.418967	30.867328
510.879732	23945.492537	30.872346
511.641951	23970.540698	30.877364
511.740127	24001.034196	30.882381
512.275546	24045.179099	30.887399
513.033213	24082.054064	30.892416
512.791946	24121.593793	30.897434
513.610438	24147.453226	30.902452
514.383556	24202.728194	30.907469
515.009992	24239.299912	30.912487
515.553555	24266.209973	30.917504
515.862497	24300.693099	30.922522
516.644885	24332.110877	30.927540
517.283765	24376.891628	30.932557
517.033288	24411.932773	30.937575
517.899371	24449.326155	30.942592
518.412542	24498.944714	30.947610
518.972247	24532.154101	30.952628
519.457489	24574.920575	30.957645
519.754736	24630.826579	30.962663
520.268444	24658.744001	30.967680
520.872115	24699.117063	30.972698
521.297517	24750.189497	30.977716
522.115022	24798.528561	30.982733
522.350832	24841.801012	30.987751
523.083323	24872.655942	30.992768
523.466654	24922.322498	30.997786
524.081648	24962.775559	31.002804
524.859806	25004.369325	31.007821
525.395800	25037.895478	31.012839
526.125907	25087.142601	31.017856
526.436092	25127.161768	31.022874
527.105287	25171.579944	31.027892
527.896851	25205.184684	31.032909
528.345689	25241.686960	31.037927
529.083879	25273.796596	31.042944
529.300484	25309.302531	31.047962
529.623499	25338.502423	31.052980
530.194109	25383.545803	31.057997
530.594695	25426.775477	31.063015
531.062237	25462.003099	31.068032
531.942885	25494.690738	31.073050
532.198695	25535.968931	31.078068
532.935904	25580.664936	31.083085
533.155755	25627.248967	31.088103
533.753884	25658.902746	31.093120
534.609938	25698.141610	31.098138
534.942159	25755.218928	31.103156
535.572032	25776.906098	31.108173
535.910451	25840.580874	31.113191
536.655942	25858.006935	31.118208
536.968999	25919.538666	31.123226
537.582083	25944.544380	31.128244
538.426288	25978.415719	31.133261
538.265051	26020.820333	31.138279
539.180275	26044.233289	31.143296
539.879757	26083.445262	31.148314
539.811423	26115.424314	31.153332
540.371652	26156.594961	31.158349
540.857845	26204.198575	31.163367
541.856886	26232.213970	31.168384
542.217498	26284.425775	31.173402
542.948655	26322.396493	31.178420
543.128446	26357.159085	31.183437
543.604487	26414.012598	31.188455
544.254659	26444.356666	31.193472
544.898348	26491.907689	31.198490
545.168095	26535.477100	31.203508
545.867472	26578.589031	31.208525
546.211605	26625.045090	31.213543
547.298967	26663.178884	31.218560
547.216098	26722.096707	31.223578
547.724421	26758.345606	31.228596
548.704735	26819.737483	31.233613
549.169715	26860.183008	31.238631
549.538021	26904.460131	31.243648
550.482650	26952.308066	31.248666
551.041360	26998.314280	31.253684
551.714859	27045.023972	31.258701
551.995185	27081.196471	31.263719
552.793761	27119.174885	31.268736
553.351419	27165.561470	31.273754
553.628819	27225.849692	31.278772
554.730116	27254.035732	31.283789
555.207277	27311.722604	31.288807
555.516843	27346.646290	31.293824
556.168871	27384.112954	31.298842
556.753446	27427.863107	31.303860
557.256210	27471.365639	31.308877
557.675366	27512.422005	31.313895
558.215581	27552.067884	31.318912
558.929387	27596.795307	31.323930
559.304248	27653.322674	31.328948
560.031690	27683.549637	31.333965
560.442293	27728.971746	31.338983
561.195941	27776.072596	31.344000
561.729760	27826.662504	31.349018
562.079979	27862.738965	31.354036
562.808205	27907.788760	31.359053
563.033437	27963.526412	31.364071
564.057522	28001.829467	31.369088
564.733244	28046.508268	31.374106
565.331091	28097.269246	31.379124
566.120207	28132.491700	31.384141
566.233144	28181.283319	31.389159
566.896600	28224.886774	31.394176
567.719031	28255.153257	31.399194
567.996506	28301.853252	31.404212
568.345256	28337.723012	31.409229
569.089753	28368.016302	31.414247
569.943117	28406.782419	31.419264
570.168511	28452.457456	31.424282
570.386068	28485.408092	31.429300
571.116582	28522.147150	31.434317
571.390001	28565.166012	31.439335
571.868709	28621.840957	31.444352
572.536617	28671.045179	31.449370
572.782239	28709.447118	31.454388
573.380236	28771.109821	31.459405
574.003653	28828.701607	31.464423
574.699327	28876.442855	31.469440
575.417639	28924.328763	31.474458
575.808115	28980.647129	31.479476
576.615897	29007.368658	31.484493
576.999217	29068.385938	31.489511
577.678019	29122.038305	31.494528
578.464490	29171.228316	31.499546
578.748048	29223.509974	31.504564
579.617373	29265.253917	31.509581
580.258834	29318.923914	31.514599
580.752821	29368.493609	31.519616
581.439109	29412.063538	31.524634
581.834249	29463.806595	31.529652
582.472582	29516.084694	31.534669
583.115947	29568.122630	31.539687
583.530625	29617.332238	31.544704
584.184535	29665.701777	31.549722
584.602411	29721.142167	31.554740
585.231367	29767.968479	31.559757
586.069466	29816.501390	31.564775
586.270934	29875.104895	31.569792
587.127115	29928.235274	31.574810
587.335035	29984.445941	31.579828
588.527880	30026.903056	31.584845
589.040743	30084.827361	31.589863
589.377397	30145.268303	31.594880
590.423939	30174.475196	31.599898
591.045655	30233.547297	31.604916
591.744731	30272.591453	31.609933
592.053945	30329.105514	31.614951
592.953469	30374.440626	31.619968
593.675447	30416.934355	31.624986
593.976869	30469.270753	31.630004
594.896523	30497.658461	31.635021
595.181104	30558.293613	31.640039
595.545451	30610.016850	31.645056
596.394845	30664.915790	31.650074
597.078331	30706.715103	31.655092
598.075069	30743.820248	31.660109
598.344866	30802.264910	31.665127
599.074468	30843.097459	31.670144
599.465114	30890.666267	31.675162
599.961154	30924.943875	31.680180
600.719884	30964.713026	31.685197
600.863754	31003.601503	31.690215
601.320612	31056.657323	31.695232
601.981799	31092.915232	31.700250
602.695081	31137.594992	31.705268
603.196051	31185.334632	31.710285
603.501975	31250.570912	31.715303
603.954966	31289.817452	31.720320
604.936170	31338.240701	31.725338
605.248668	31407.057292	31.730356
606.159316	31441.834177	31.735373
606.793412	31500.726072	31.740391
607.092635	31544.144281	31.745408
607.981357	31598.630326	31.750426
608.015945	31648.097294	31.755444
609.296878	31698.869487	31.760461
609.439673	31756.626976	31.765479
610.020648	31816.062752	31.770496
611.240013	31864.188003	31.775514
611.299223	31930.484425	31.780532
612.172397	31983.968687	31.785549
612.402166	32045.287912	31.790567
613.195009	32096.235211	31.795584
613.962580	32153.491116	31.800602
614.605169	32208.190182	31.805620
615.026060	32262.916856	31.810637
615.665455	32322.463371	31.815655
616.652734	32377.818941	31.820672
617.794188	32425.974014	31.825690
618.077817	32480.757948	31.830708
619.008609	32517.146302	31.835725
619.594314	32567.024752	31.840743
620.210636	32619.733973	31.845760
620.859939	32663.078900	31.850778
621.312655	32716.375596	31.855796
621.971139	32748.279522	31.860813
622.618166	32803.700171	31.865831
622.960395	32868.147433	31.870848
623.762891	32911.955659	31.875866
623.862905	32966.890240	31.880884
624.594544	33030.703968	31.885901
625.478812	33083.518590	31.890919
626.121159	33136.215863	31.895936
626.713450	33193.392969	31.900954
627.180399	33257.150426	31.905972
627.778479	33311.718391	31.910989
628.371741	33350.211425	31.916007
628.776928	33418.961774	31.921024
629.906825	33473.723001	31.926042
630.102014	33534.583557	31.931060
630.818480	33599.295629	31.936077
631.632877	33650.989876	31.941095
632.081442	33708.175891	31.946112
632.316703	33778.466424	31.951130
633.318051	33812.707425	31.956148
633.934700	33862.565953	31.961165
634.869075	33898.628932	31.966183
635.460977	33962.615111	31.971200
636.375717	33996.449421	31.976218
636.715860	34045.662121	31.981236
637.312840	34087.201668	31.986253
638.100303	34142.851929	31.991271
638.651032	34192.950514	31.996288
639.357966	34247.570440	32.001306
639.789998	34294.165190	32.006324
640.251778	34353.528215	32.011341
640.795329	34400.980361	32.016359
641.411093	34463.312690	32.021376
642.151646	34517.474171	32.026394
642.857978	34573.037913	32.031412
643.155069	34628.440016	32.036429
643.979751	34686.825860	32.041447
644.709498	34750.000226	32.046464
645.289681	34810.895587	32.051482
645.944992	34874.876766	32.056500
646.363055	34932.826943	32.061517
647.256294	34998.131116	32.066535
647.685226	35067.924932	32.071552
648.320948	35127.147948	32.076570
649.016816	35187.543893	32.081588
649.587665	35246.615295	32.086605
650.293686	35312.562160	32.091623
651.105378	35377.165120	32.096640
651.859949	35434.792317	32.101658
652.807314	35500.603758	32.106676
653.597421	35554.863199	32.111693
654.466971	35614.295062	32.116711
654.502710	35671.900394	32.121728
655.527142	35729.280701	32.126746
656.258954	35780.816604	32.131764
656.601491	35846.181847	32.136781
657.347706	35894.367414	32.141799
657.916857	35954.841496	32.146816
658.899524	36014.006114	32.151834
659.609491	36078.979548	32.156852
660.330186	36120.320033	32.161869
661.409463	36175.906992	32.166887
661.898794	36228.115061	32.171904
662.456139	36288.046764	32.176922
663.312145	36332.402566	32.181940
663.586955	36392.105319	32.186957
664.249784	36426.383562	32.191975
664.846335	36487.239878	32.196992
665.714701	36546.125046	32.202010
666.487799	36613.972392	32.207028
666.961558	36652.881519	32.212045
667.254951	36710.290169	32.217063
667.683853	36779.012791	32.222080
668.538046	36840.940832	32.227098
669.204074	36880.259730	32.232116
669.760190	36944.567342	32.237133
670.573847	36985.466342	32.242151
671.171127	37051.420048	32.247168
671.758756	37093.843586	32.252186
672.109697	37169.933367	32.257204
672.657181	37216.568351	32.262221
673.380870	37275.644664	32.267239
673.678984	37340.696458	32.272256
674.492966	37415.608428	32.277274
675.137105	37484.447866	32.282292
675.797515	37543.412222	32.287309
676.578983	37614.678813	32.292327
677.387420	37684.481453	32.297344
678.099438	37752.667917	32.302362
678.944557	37812.453613	32.307380
679.528424	37879.098543	32.312397
680.418537	37928.580404	32.317415
680.675046	38001.305485	32.322432
681.558001	38055.490457	32.327450
682.958371	38129.563325	32.332468
683.265141	38192.617813	32.337485
684.119514	38245.820951	32.342503
684.776041	38310.743743	32.347520
685.624369	38365.736186	32.352538
686.205276	38423.374518	32.357556
686.803100	38488.622682	32.362573
687.814118	38545.806657	32.367591
687.988513	38619.868760	32.372608
688.954974	38674.408227	32.377626
689.936550	38736.835409	32.382644
690.340386	38798.113921	32.387661
691.235271	38858.951820	32.392679
691.793700	38923.604046	32.397696
692.320839	38977.809221	32.402714
693.410934	39028.509683	32.407732
693.875810	39103.197772	32.412749
694.941310	39149.326751	32.417767
695.280635	39223.429883	32.422784
696.013862	39284.263517	32.427802
696.687477	39334.473030	32.432820
697.396321	39410.104388	32.437837
698.006910	39467.177062	32.442855
698.479618	39528.795725	32.447872
699.178816	39591.972703	32.452890
699.884330	39673.903537	32.457908
700.370349	39731.369062	32.462925
701.256915	39797.535008	32.467943
701.869245	39861.849522	32.472960
702.438322	39947.381231	32.477978
703.295768	40007.213734	32.482996
703.901583	40076.490856	32.488013
704.997646	40147.852078	32.493031
705.438722	40229.122837	32.498048
706.081700	40280.276687	32.503066
706.826772	40354.044196	32.508084
706.972458	40408.863430	32.513101
708.328527	40456.922393	32.518119
708.530004	40541.717712	32.523136
708.760954	40602.789000	32.528154
709.969256	40655.602755	32.533172
710.723761	40742.203309	32.538189
711.461983	40805.462161	32.543207
711.529368	40887.814246	32.548224
712.615909	40951.544877	32.553242
713.566882	41013.838662	32.558260
713.975876	41101.904257	32.563277
715.054175	41158.455559	32.568295
715.962080	41230.623987	32.573312
716.255679	41305.151891	32.578330
717.706991	41364.205482	32.583348
718.051365	41435.688626	32.588365
718.932480	41510.309970	32.593383
719.678664	41564.045382	32.598400
720.113870	41632.130666	32.603418
721.040382	41694.634264	32.608436
721.503182	41772.638209	32.613453
722.601429	41832.311048	32.618471
722.909950	41916.272938	32.623488
723.636754	41987.095074	32.628506
724.616802	42058.416531	32.633524
725.155921	42127.938113	32.638541
726.040243	42216.250748	32.643559
726.444169	42286.204527	32.648576
727.428895	42348.010492	32.653594
728.193093	42423.786761	32.658612
728.582308	42513.580186	32.663629
729.578726	42574.937218	32.668647
730.240653	42655.452575	32.673664
730.529470	42734.822808	32.678682
731.594072	42818.504716	32.683700
732.370529	42891.757729	32.688717
733.009637	42971.158448	32.693735
733.905033	43048.938451	32.698752
734.792641	43131.139172	32.703770
735.676232	43205.890514	32.708788
735.972901	43285.700478	32.713805
736.989697	43364.301621	32.718823
737.600941	43446.550998	32.723840
738.071203	43512.117841	32.728858
739.235879	43598.216446	32.733876
739.658347	43682.020550	32.738893
740.760784	43757.761459	32.743911
741.524030	43835.111816	32.748928
742.107067	43912.103217	32.753946
743.175050	43968.649661	32.758964
743.756795	44061.158525	32.763981
744.595774	44132.170358	32.768999
745.591257	44197.605716	32.774016
745.975065	44272.283518	32.779034
746.727615	44333.868599	32.784052
747.463619	44405.749659	32.789069
748.381398	44460.864250	32.794087
749.101612	44534.514883	32.799104
749.838516	44602.592264	32.804122
750.569098	44658.084283	32.809140
751.120571	44738.630091	32.814157
751.853014	44797.472401	32.819175
752.615803	44858.379485	32.824192
753.160200	44934.880004	32.829210
753.870055	45003.332351	32.834228
754.573631	45077.609397	32.839245
755.205057	45161.444171	32.844263
756.077380	45233.786465	32.849280
756.661938	45317.206728	32.854298
757.661867	45394.529521	32.859316
758.216211	45475.702913	32.864333
759.273873	45550.562859	32.869351
759.889331	45617.982136	32.874368
760.669543	45707.994879	32.879386
761.406955	45785.263402	32.884404
762.230568	45856.341521	32.889421
763.260700	45939.706452	32.894439
763.940730	46014.022789	32.899456
764.732539	46093.896187	32.904474
765.733037	46167.994960	32.909492
766.341396	46249.917358	32.914509
766.982679	46323.840518	32.919527
767.609060	46392.015056	32.924544
768.401905	46474.051105	32.929562
769.175544	46570.413790	32.934580
769.885117	46644.365293	32.939597
770.794835	46721.802980	32.944615
771.417076	46808.600132	32.949632
772.104949	46895.740620	32.954650
773.118867	46961.918549	32.959668
773.743829	47039.683763	32.964685
774.697299	47130.947708	32.969703
775.632765	47212.544900	32.974720
776.356412	47296.028187	32.979738
777.448886	47371.354185	32.984756
777.917325	47446.085733	32.989773
778.530318	47544.489110	32.994791
779.355822	47619.038352	32.999808
780.215775	47706.694992	33.004826
781.081368	47774.726401	33.009844
781.583454	47866.258481	33.014861
782.573766	47943.682423	33.019879
783.546217	48016.149654	33.024896
784.023324	48108.586187	33.029914
784.745755	48179.207099	33.034932
786.029224	48259.706238	33.039949
786.657282	48342.742740	33.044967
787.465219	48414.423754	33.049984
788.271303	48507.403192	33.055002
789.277278	48572.266411	33.060020
790.066843	48638.546320	33.065037
790.462199	48703.349456	33.070055
791.140697	48765.438389	33.075072
791.768624	48849.944504	33.080090
792.549964	48923.783734	33.085108
793.218345	48998.755083	33.090125
793.971175	49076.379568	33.095143
794.649892	49161.576416	33.100160
795.222057	49255.442658	33.105178
795.849650	49338.026380	33.110196
796.698808	49426.201297	33.115213
797.516228	49516.883950	33.120231
798.679192	49595.354186	33.125248
799.184474	49687.090822	33.130266
800.204226	49760.788308	33.135284
800.850171	49852.569672	33.140301
802.080419	49932.643141	33.145319
802.624787	50021.860357	33.150336
803.277161	50105.153693	33.155354
804.460906	50199.044331	33.160372
805.121976	50298.749149	33.165389
805.671395	50379.103400	33.170407
806.915179	50472.010851	33.175424
807.663191	50558.298359	33.180442
808.839964	50639.405940	33.185460
809.872314	50736.034184	33.190477
810.697694	50798.775849	33.195495
811.536462	50879.439732	33.200512
811.993161	50970.938263	33.205530
813.241235	51037.728488	33.210548
813.803883	51132.600190	33.215565
814.380299	51210.312566	33.220583
815.366271	51276.236557	33.225600
816.021202	51377.942804	33.230618
816.792646	51468.248246	33.235636
817.843892	51560.996362	33.240653
818.718569	51637.855242	33.245671
819.528044	51721.090091	33.250688
820.162143	51818.658583	33.255706
821.131928	51883.299815	33.260724
822.060814	51971.717639	33.265741
822.643161	52067.616810	33.270759
823.665134	52144.410238	33.275776
824.563387	52228.744184	33.280794
825.611141	52323.188363	33.285812
826.397550	52398.309867	33.290829
827.204526	52471.853599	33.295847
828.339693	52533.712565	33.300864
828.937068	52617.982615	33.305882
829.627409	52709.288719	33.310900
830.787222	52784.371342	33.315917
831.151534	52856.983500	33.320935
831.961775	52934.255847	33.325952
832.718941	53019.237694	33.330970
833.428652	53104.647250	33.335988
834.196654	53173.226121	33.341005
834.931500	53251.376589	33.346023
835.809758	53342.715960	33.351040
836.308484	53419.986317	33.356058
837.174202	53501.995893	33.361076
838.414991	53575.279408	33.366093
839.101865	53666.994899	33.371111
839.997013	53735.255836	33.376128
840.710300	53825.172071	33.381146
841.559538	53901.385036	33.386164
842.234380	53989.171466	33.391181
842.709063	54078.262134	33.396199
843.978628	54167.195167	33.401216
844.482671	54266.044321	33.406234
845.488841	54363.362212	33.411252
846.486116	54444.588151	33.416269
847.142898	54537.594291	33.421287
847.994532	54629.967039	33.426304
848.796541	54727.281501	33.431322
849.590816	54828.925069	33.436340
850.260753	54915.586789	33.441357
851.311347	54996.822496	33.446375
852.787081	55097.083931	33.451392
853.384661	55198.489419	33.456410
853.930706	55288.616282	33.461428
854.981665	55366.883385	33.466445
855.661975	55484.716058	33.471463
856.821991	55566.028430	33.476480
857.616783	55665.122995	33.481498
858.509461	55767.535795	33.486516
859.561603	55852.083098	33.491533
860.268610	55958.475333	33.496551
861.172435	56037.864056	33.501568
861.739870	56143.714558	33.506586
862.760258	56236.352688	33.511604
863.604195	56336.860385	33.516621
864.612551	56437.891720	33.521639
865.549706	56527.236424	33.526656
866.642400	56629.331809	33.531674
867.782986	56719.901429	33.536692
868.572735	56808.873226	33.541709
869.153526	56898.241730	33.546727
870.196368	56982.227531	33.551744
870.930190	57087.539301	33.556762
871.551297	57175.018164	33.561780
872.920219	57256.876185	33.566797
873.568245	57357.212306	33.571815
874.535136	57446.607265	33.576832
875.557262	57532.461392	33.581850
876.199132	57635.366500	33.586868
877.576269	57720.884052	33.591885
878.018489	57823.013828	33.596903
878.955121	57905.912694	33.601920
879.603276	57993.776282	33.606938
880.041288	58074.554903	33.611956
881.299366	58162.372741	33.616973
881.962364	58257.972843	33.621991
883.062234	58340.175256	33.627008
884.143235	58433.720867	33.632026
884.762708	58513.916905	33.637044
885.693991	58597.602663	33.642061
886.345125	58690.255097	33.647079
887.124025	58774.275291	33.652096
888.147458	58870.642029	33.657114
888.555386	58979.789130	33.662132
889.546196	59057.787943	33.667149
890.101053	59168.731249	33.672167
891.042354	59284.772444	33.677184
892.018657	59374.301522	33.682202
892.890781	59478.657779	33.687220
894.219182	59571.102650	33.692237
894.776957	59685.057351	33.697255
895.774045	59770.884818	33.702272
896.754571	59880.583843	33.707290
897.748125	59989.053279	33.712308
898.918248	60088.954885	33.717325
899.548989	60197.205431	33.722343
900.326995	60292.576704	33.727360
901.403039	60400.650220	33.732378
902.175078	60503.231643	33.737396
903.092432	60606.993450	33.742413
904.181163	60717.463201	33.747431
905.226908	60811.073759	33.752448
906.254289	60914.024106	33.757466
906.991973	61011.981899	33.762484
908.280689	61115.460102	33.767501
909.116614	61225.518416	33.772519
909.911063	61318.268473	33.777536
910.774014	61413.909806	33.782554
911.895825	61505.194149	33.787572
912.825883	61604.621079	33.792589
913.880694	61707.423020	33.797607
914.755936	61804.832604	33.802624
915.850172	61903.423505	33.807642
916.464878	62006.511830	33.812660
917.605424	62104.638570	33.817677
918.409549	62195.765265	33.822695
919.241499	62281.122162	33.827712
920.093141	62387.834554	33.832730
921.034644	62500.848561	33.837748
922.226488	62601.483223	33.842765
923.066529	62706.070992	33.847783
923.860300	62812.324500	33.852800
924.737542	62898.182218	33.857818
925.560447	63010.261359	33.862836
926.700678	63104.679856	33.867853
927.524908	63204.905728	33.872871
928.360357	63315.892096	33.877888
929.527592	63399.653384	33.882906
930.226786	63501.880669	33.887924
931.127993	63584.185140	33.892941
931.975592	63675.567846	33.897959
933.087391	63769.368932	33.902976
934.116467	63844.830041	33.907994
934.481499	63957.562381	33.913012
935.576276	64043.270681	33.918029
936.530834	64150.876652	33.923047
937.321715	64251.163890	33.928064
938.161167	64340.773173	33.933082
938.762614	64447.480146	33.938100
940.008964	64545.972210	33.943117
941.021621	64670.451372	33.948135
941.717703	64781.815867	33.953152
942.439641	64874.364384	33.958170
943.383124	65001.920027	33.963188
944.096997	65101.153408	33.968205
945.195720	65213.703803	33.973223
945.982111	65336.919018	33.978240
946.760837	65459.419347	33.983258
947.817993	65584.412168	33.988276
949.139010	65695.739403	33.993293
950.204329	65812.713784	33.998311
950.754574	65937.884314	34.003328
952.211240	66051.595447	34.008346
952.866813	66162.759668	34.013364
953.961593	66278.323618	34.018381
955.315487	66389.902321	34.023399
956.415499	66510.526434	34.028416
957.314273	66616.553901	34.033434
958.150468	66732.900781	34.038452
959.344437	66842.593595	34.043469
960.129357	66962.013642	34.048487
961.083512	67068.682259	34.053504
962.308202	67178.135217	34.058522
962.861768	67301.450618	34.063540
964.023891	67408.264898	34.068557
965.007133	67517.173880	34.073575
966.156197	67642.572908	34.078592
966.843926	67755.721588	34.083610
967.725967	67874.885464	34.088628
968.703230	67983.030496	34.093645
969.740674	68094.388307	34.098663
970.780737	68223.383954	34.103680
971.756196	68334.917257	34.108698
972.988003	68450.409250	34.113716
974.057687	68561.094983	34.118733
975.139163	68671.817375	34.123751
976.012897	68788.240143	34.128768
977.158587	68887.449598	34.133786
978.176792	69002.157594	34.138804
978.906650	69110.809449	34.143821
979.827137	69218.130172	34.148839
980.787918	69332.274355	34.153856
982.095728	69437.013956	34.158874
982.935488	69543.294276	34.163892
983.499092	69647.237352	34.168909
984.665381	69741.873900	34.173927
985.362804	69842.353583	34.178944
986.641492	69946.253978	34.183962
987.071444	70063.317245	34.188980
988.296710	70168.598283	34.193997
989.445229	70269.867620	34.199015
989.629469	70378.556473	34.204032
990.967702	70491.642835	34.209050
991.744727	70613.481072	34.214068
992.766187	70727.149899	34.219085
993.882827	70858.892814	34.224103
994.790329	70975.575966	34.229120
995.852180	71094.724596	34.234138
996.959223	71210.202224	34.239156
997.724046	71330.227216	34.244173
998.924373	71456.798854	34.249191
999.794462	71567.906145	34.254208
1001.219455	71708.906205	34.259226
1002.040798	71826.637995	34.264244
1002.770160	71944.909548	34.269261
1004.083591	72063.708096	34.274279
1004.964575	72199.092657	34.279296
1005.921611	72325.392648	34.284314
1007.317251	72426.437903	34.289332
1008.185997	72560.038730	34.294349
1009.238713	72681.485729	34.299367
1009.951281	72793.800238	34.304384
1011.591300	72930.692947	34.309402
1012.264575	73053.194624	34.314420
1013.042978	73166.991997	34.319437
1014.304528	73273.237992	34.324455
1015.241263	73422.390753	34.329472
1016.434062	73539.037330	34.334490
1017.505663	73672.095217	34.339508
1018.646717	73792.504967	34.344525
1019.713123	73910.014251	34.349543
1020.815509	74033.502655	34.354560
1022.333874	74142.644484	34.359578
1022.793732	74273.857422	34.364596
1023.790095	74390.780361	34.369613
1024.792247	74506.350752	34.374631
1025.763327	74627.664632	34.379648
1026.913848	74751.130857	34.384666
1027.961414	74878.165683	34.389684
1029.096455	74997.964363	34.394701
1030.558523	75112.327604	34.399719
1031.149341	75246.989113	34.404736
1032.351033	75353.489525	34.409754
1033.556617	75478.796760	34.414772
1034.444490	75597.911595	34.419789
1035.418095	75713.051113	34.424807
1036.522781	75830.805724	34.429824
1037.376552	75935.582432	34.434842
1038.437067	76044.371401	34.439860
1039.314705	76147.571811	34.444877
1040.354984	76266.678996	34.449895
1041.324105	76372.021042	34.454912
1042.553335	76482.624599	34.459930
1043.239866	76574.210143	34.464948
1044.005423	76717.044217	34.469965
1045.146042	76833.560263	34.474983
1046.029520	76943.418708	34.480000
1047.186875	77059.914436	34.485018
1048.207982	77186.569866	34.490036
1049.261370	77303.835619	34.495053
1050.391446	77420.969770	34.500071
1051.250604	77550.453048	34.505088
1052.646011	77674.245830	34.510106
1053.568084	77795.466478	34.515124
1054.455447	77924.227142	34.520141
1055.513430	78051.280275	34.525159
1056.739992	78188.988795	34.530176
1057.927572	78293.181046	34.535194
1058.817120	78427.323199	34.540212
1059.978749	78554.198649	34.545229
1061.159109	78684.194242	34.550247
1061.736689	78808.294658	34.555264
1063.145149	78930.399089	34.560282
1064.594827	79057.983999	34.565300
1065.448577	79184.090649	34.570317
1066.485673	79318.246779	34.575335
1067.808842	79448.041209	34.580352
1068.840462	79564.596538	34.585370
1069.548715	79692.031535	34.590388
1070.816877	79837.310565	34.595405
1072.197052	79945.013961	34.600423
1072.831776	80077.696753	34.605440
1073.922195	80207.716312	34.610458
1075.355307	80344.546817	34.615476
1076.241186	80473.336381	34.620493
1077.399682	80589.782522	34.625511
1078.507568	80724.271580	34.630528
1079.914442	80845.369944	34.635546
1081.150578	80966.483534	34.640564
1082.069039	81101.542480	34.645581
1083.713941	81216.467221	34.650599
1084.478933	81350.073017	34.655616
1085.113898	81470.147334	34.660634
1086.601735	81576.129034	34.665652
1087.429674	81695.895823	34.670669
1088.606626	81833.320570	34.675687
1089.780449	81959.450168	34.680704
1090.829216	82073.159602	34.685722
1091.604582	82203.469387	34.690740
1092.524489	82327.201467	34.695757
1093.944707	82472.171379	34.700775
1094.921034	82608.628010	34.705792
1095.729219	82712.719623	34.710810
1097.009654	82838.591042	34.715828
1097.944640	82958.683122	34.720845
1098.891476	83085.532073	34.725863
1099.810298	83214.700064	34.730880
1100.648921	83325.212935	34.735898
1101.909735	83461.750006	34.740916
1102.871028	83595.768867	34.745933
1103.971723	83724.841534	34.750951
1105.171628	83853.058378	34.755968
1106.063198	83993.950340	34.760986
1107.367674	84123.087877	34.766004
1108.164257	84255.385902	34.771021
1109.453476	84402.735558	34.776039
1110.587622	84545.445052	34.781056
1111.759261	84677.066490	34.786074
1112.752992	84824.434478	34.791092
1113.637952	84969.253890	34.796109
1115.047089	85101.750633	34.801127
1116.260494	85238.091807	34.806144
1117.329043	85387.032446	34.811162
1118.376748	85522.485036	34.816180
1119.752421	85663.153083	34.821197
1120.805582	85808.899883	34.826215
1121.736644	85950.664821	34.831232
1122.879335	86097.284542	34.836250
1124.294833	86247.484854	34.841268
1125.027378	86391.136883	34.846285
1126.512944	86513.652845	34.851303
1127.824041	86689.303535	34.856320
1129.244939	86816.586374	34.861338
1130.233879	86951.058382	34.866356
1131.288669	87088.302908	34.871373
1132.219598	87234.104193	34.876391
1133.396842	87384.116449	34.881408
1134.503011	87525.712256	34.886426
1135.927221	87670.951184	34.891444
1137.119201	87817.840462	34.896461
1138.310141	87950.882861	34.901479
1139.450070	88094.519485	34.906496
1140.184400	88243.027350	34.911514
1141.625034	88386.339873	34.916532
1142.755157	88536.234886	34.921549
1144.012095	88684.264305	34.926567
1145.030002	88826.926106	34.931584
1145.991270	88967.081061	34.936602
1147.459455	89103.349477	34.941620
1148.600203	89261.323136	34.946637
1150.161096	89393.082493	34.951655
1151.128043	89540.759183	34.956672
1152.288776	89680.861750	34.961690
1153.491865	89819.820194	34.966708
1154.431881	89960.155705	34.971725
1155.257100	90098.366565	34.976743
1156.716680	90247.228187	34.981760
1157.798380	90398.427569	34.986778
1159.243093	90524.760973	34.991796
1160.196131	90653.468946	34.996813
1161.379785	90767.627123	35.001831
1162.591008	90895.017991	35.006848
1163.666754	91022.576605	35.011866
1165.015595	91152.173212	35.016884
1166.091448	91286.399102	35.021901
1167.281632	91407.434082	35.026919
1168.265315	91541.088031	35.031936
1169.349243	91676.099248	35.036954
1170.725512	91801.306214	35.041972
1171.376649	91947.658060	35.046989
1172.463360	92085.909487	35.052007
1173.990957	92223.478195	35.057024
1174.911147	92376.184232	35.062042
1176.061412	92527.558193	35.067060
1177.175392	92673.373245	35.072077
1178.352833	92816.971844	35.077095
1179.446888	92969.527853	35.082112
1180.473485	93121.735128	35.087130
1181.873240	93260.367912	35.092148
1183.100309	93417.206758	35.097165
1183.983476	93571.742199	35.102183
1185.219020	93728.132830	35.107200
1186.422389	93881.386143	35.112218
1187.928530	94049.260208	35.117236
1188.884109	94204.749955	35.122253
1190.233806	94343.985717	35.127271
1191.295069	94512.408408	35.132288
1192.532951	94668.463728	35.137306
1194.040101	94812.060779	35.142324
1195.343816	94972.851729	35.147341
1196.299808	95129.663536	35.152359
1197.733330	95284.774880	35.157376
1198.751681	95431.799790	35.162394
1200.062235	95573.655546	35.167412
1201.189014	95749.863849	35.172429
1202.607779	95898.377915	35.177447
1204.078242	96060.054726	35.182464
1205.144536	96203.123547	35.187482
1206.479439	96357.018161	35.192500
1207.663483	96521.957305	35.197517
1208.519270	96677.473779	35.202535
1209.934417	96826.038831	35.207552
1210.925001	96992.429170	35.212570
1212.213917	97136.986742	35.217588
1213.366471	97299.045619	35.222605
1214.893040	97446.376122	35.227623
1216.141962	97607.093418	35.232640
1216.900386	97763.739908	35.237658
1218.662499	97920.784597	35.242676
1219.781520	98078.736053	35.247693
1220.641162	98242.765089	35.252711
1221.945363	98399.556932	35.257728
1222.989155	98551.007546	35.262746
1224.385674	98692.204966	35.267764
1225.563466	98844.022132	35.272781
1226.878298	98987.878814	35.277799
1228.094852	99136.636084	35.282816
1228.747834	99281.321066	35.287834
1230.602621	99422.462796	35.292852
1231.623682	99577.561615	35.297869
1232.225041	99739.295290	35.302887
1233.932250	99886.524291	35.307904
1234.902788	100041.564687	35.312922
1235.622096	100194.615171	35.317940
1237.050448	100366.933036	35.322957
1238.012157	100533.537284	35.327975
1239.637946	100683.087319	35.332992
1240.404281	100860.752825	35.338010
1241.935058	101024.486275	35.343028
1243.184797	101196.149089	35.348045
1244.369265	101372.138644	35.353063
1245.936228	101539.236011	35.358080
1247.118018	101711.906815	35.363098
1248.476548	101878.944861	35.368116
1249.574221	102049.891559	35.373133
1250.952787	102222.471602	35.378151
1252.301812	102397.177298	35.383168
1253.481074	102571.303859	35.388186
1254.896941	102739.990432	35.393204
1256.017450	102904.871717	35.398221
1257.043273	103089.574530	35.403239
1258.368531	103253.406981	35.408256
1259.717452	103441.383205	35.413274
1261.190908	103618.147398	35.418292
1262.683194	103787.430508	35.423309
1263.916704	103956.812929	35.428327
1265.439578	104133.598458	35.433344
1266.123283	104314.302813	35.438362
1267.536229	104476.516242	35.443380
1269.123115	104656.554414	35.448397
1270.590746	104831.809932	35.453415
1272.146956	104994.080080	35.458432
1273.099105	105171.286850	35.463450
1274.755841	105332.176459	35.468468
1276.163064	105510.636012	35.473485
1277.316686	105675.126426	35.478503
1278.809533	105837.064368	35.483520
1279.472508	106007.254624	35.488538
1281.074316	106171.727852	35.493556
1282.825813	106348.139188	35.498573
1283.645504	106515.295817	35.503591
1285.096702	106677.378992	35.508608
1286.495795	106851.647743	35.513626
1287.548008	107011.005703	35.518644
1288.798398	107175.617658	35.523661
1290.268647	107344.182881	35.528679
1291.419827	107501.452553	35.533696
1292.305467	107672.682492	35.538714
1293.847516	107833.955294	35.543732
1294.915066	107982.545580	35.548749
1295.612988	108151.884789	35.553767
1297.338681	108302.157181	35.558784
1298.376430	108466.261154	35.563802
1299.825825	108626.402110	35.568820
1300.969318	108814.016722	35.573837
1302.004824	108971.054875	35.578855
1303.537561	109127.451708	35.583872
1304.475896	109316.710436	35.588890
1305.812072	109494.495710	35.593908
1307.150591	109661.332188	35.598925
1308.405207	109830.993384	35.603943
1309.923051	110022.450384	35.608960
1311.081961	110202.940023	35.613978
1311.932399	110377.637897	35.618996
1313.217842	110565.616894	35.624013
1314.442957	110754.714606	35.629031
1316.236117	110929.361509	35.634048
1317.321761	111133.118458	35.639066
1318.620109	111323.284961	35.644084
1320.356446	111519.789071	35.649101
1321.465050	111703.665207	35.654119
1323.231824	111891.850033	35.659136
1324.632559	112076.688970	35.664154
1326.305629	112257.833599	35.669172
1327.486945	112432.461827	35.674189
1328.650288	112623.204195	35.679207
1330.478967	112799.415913	35.684224
1332.017885	112989.069588	35.689242
1333.032914	113179.409356	35.694260
1334.762517	113339.416301	35.699277
1335.832693	113525.426380	35.704295
1337.113237	113704.523310	35.709312
1338.383567	113882.414044	35.714330
1339.845222	114066.789663	35.719348
1341.239843	114247.581577	35.724365
1342.296985	114427.447205	35.729383
1344.115766	114614.637832	35.734400
1345.272547	114801.966732	35.739418
1346.574205	114983.259855	35.744436
1348.209165	115160.120448	35.749453
1349.136116	115343.678817	35.754471
1351.171441	115529.626334	35.759488
1352.131921	115713.156738	35.764506
1353.527350	115896.657329	35.769524
1355.199818	116073.758943	35.774541
1356.340061	116260.943033	35.779559
1358.159223	116431.173691	35.784576
1359.396381	116613.261152	35.789594
1360.606186	116774.315923	35.794612
1362.120449	116949.321537	35.799629
1363.371779	117136.608383	35.804647
1364.744525	117307.029822	35.809664
1366.390907	117478.719488	35.814682
1367.436048	117644.320146	35.819700
1368.984393	117802.472170	35.824717
1370.081931	117980.925717	35.829735
1371.434528	118129.392136	35.834752
1372.823085	118292.707399	35.839770
1373.756098	118455.627568	35.844788
1375.282588	118628.452017	35.849805
1376.287642	118801.689744	35.854823
1377.437865	118975.924962	35.859840
1378.607099	119158.503533	35.864858
1379.820316	119344.394246	35.869876
1381.087834	119532.816720	35.874893
1382.453857	119734.160885	35.879911
1383.926362	119912.207290	35.884928
1385.259941	120109.532439	35.889946
1386.701617	120310.204195	35.894964
1388.152642	120494.881275	35.899981
1389.193783	120703.357471	35.904999
1390.582310	120900.458257	35.910016
1392.095568	121101.086731	35.915034
1393.400168	121311.514214	35.920052
1394.812965	121507.817857	35.925069
1396.235356	121719.319046	35.930087
1397.910756	121915.786642	35.935104
1399.564111	122124.645447	35.940122
1400.884343	122333.799484	35.945140
1402.804366	122521.215268	35.950157
1404.203068	122722.950863	35.955175
1405.071274	122926.266802	35.960192
1406.712171	123127.536373	35.965210
1408.361110	123324.702591	35.970228
1409.970241	123533.934193	35.975245
1411.243528	123728.351356	35.980263
1412.712845	123932.200085	35.985280
1414.082425	124127.478795	35.990298
1415.245290	124324.603009	35.995316
1417.083651	124536.427899	36.000333
1418.564516	124742.700190	36.005351
1419.923000	124934.465376	36.010368
1421.350570	125124.346344	36.015386
1423.335460	125319.219308	36.020404
1425.008279	125506.556061	36.025421
1426.142931	125710.066174	36.030439
1427.662218	125891.109381	36.035456
1429.222519	126084.332690	36.040474
1430.181614	126290.155085	36.045492
1431.723344	126481.230817	36.050509
1433.074072	126668.880152	36.055527
1434.689255	126861.403597	36.060544
1435.952630	127071.249704	36.065562
1437.546773	127269.707635	36.070580
1439.078888	127458.777668	36.075597
1440.627365	127650.949943	36.080615
1442.030972	127848.416295	36.085632
1443.393413	128022.214777	36.090650
1444.726383	128215.920047	36.095668
1446.334858	128379.838875	36.100685
1447.606174	128554.313936	36.105703
1449.038279	128726.066277	36.110720
1450.502314	128892.810738	36.115738
1451.698325	129087.950068	36.120756
1453.516066	129259.416430	36.125773
1454.744129	129445.052033	36.130791
1455.998160	129632.230297	36.135808
1457.381726	129815.753393	36.140826
1458.570241	130003.159936	36.145844
1459.886491	130207.599438	36.150861
1461.595794	130390.593166	36.155879
1462.952275	130585.527507	36.160896
1464.463396	130785.227485	36.165914
1465.279996	131002.421119	36.170932
1467.077957	131199.215283	36.175949
1468.108802	131400.858327	36.180967
1469.469253	131631.387090	36.185984
1471.020245	131812.299506	36.191002
1472.166244	132058.145108	36.196020
1473.880891	132266.134471	36.201037
1475.047416	132484.639599	36.206055
1476.570410	132720.472705	36.211072
1478.241806	132940.206119	36.216090
1479.470021	133169.982924	36.221108
1481.370530	133391.964030	36.226125
1482.642909	133640.349968	36.231143
1484.154488	133872.570779	36.236160
1485.898259	134093.061817	36.241178
1487.330303	134319.495862	36.246196
1488.993653	134532.451454	36.251213
1490.549822	134772.186139	36.256231
1491.796054	134994.068243	36.261248
1493.636941	135221.204689	36.266266
1495.016968	135451.026372	36.271284
1496.532751	135668.448665	36.276301
1497.936419	135919.494387	36.281319
1499.732263	136150.598710	36.286336
1501.526503	136355.678100	36.291354
1502.679001	136605.160393	36.296372
1504.522211	136837.086298	36.301389
1505.872184	137056.889577	36.306407
1507.624606	137282.725697	36.311424
1509.402144	137504.618616	36.316442
1511.159180	137736.552680	36.321460
1512.756227	137955.689855	36.326477
1514.369803	138168.401248	36.331495
1516.052757	138378.251899	36.336512
1517.649207	138586.622450	36.341530
1519.022963	138803.457022	36.346548
1520.446166	139021.603270	36.351565
1521.569849	139248.124625	36.356583
1523.696209	139451.728207	36.361600
1525.107799	139668.347657	36.366618
1526.340090	139864.213621	36.371636
1527.809233	140048.206689	36.376653
1529.247560	140249.795980	36.381671
1530.225324	140459.608627	36.386688
1531.976003	140651.456050	36.391706
1533.322332	140863.012566	36.396724
1534.177488	141067.804966	36.401741
1536.265624	141277.611684	36.406759
1537.688577	141511.326522	36.411776
1539.191235	141724.068242	36.416794
1540.343531	141944.078492	36.421812
1541.849660	142163.387761	36.426829
1543.381398	142389.779286	36.431847
1544.693993	142625.383321	36.436864
1546.641854	142847.225532	36.441882
1547.744710	143090.825847	36.446900
1549.676544	143328.352145	36.451917
1550.859948	143568.939652	36.456935
1552.195204	143805.664538	36.461952
1553.856441	144044.278682	36.466970
1555.333945	144296.688628	36.471988
1556.889936	144534.943050	36.477005
1558.543907	144779.090266	36.482023
1560.122093	145031.502896	36.487040
1561.975280	145271.363533	36.492058
1563.522942	145519.893717	36.497076
1565.312318	145772.849210	36.502093
1567.018900	146011.838894	36.507111
1568.806980	146248.244327	36.512128
1570.490430	146483.311874	36.517146
1572.054787	146739.568570	36.522164
1574.094652	146968.967790	36.527181
1575.777400	147190.338177	36.532199
1577.268580	147434.227787	36.537216
1579.155503	147670.488780	36.542234
1580.905797	147896.239320	36.547252
1581.951995	148132.599277	36.552269
1583.572628	148357.131415	36.557287
1585.381254	148600.599281	36.562304
1586.926305	148830.001850	36.567322
1588.680019	149071.821404	36.572340
1590.313095	149305.536146	36.577357
1591.909894	149532.260734	36.582375
1593.215932	149771.824139	36.587392
1595.208952	150002.076679	36.592410
1596.549068	150239.039354	36.597428
1598.093144	150477.581375	36.602445
1599.903768	150702.860385	36.607463
1601.423333	150948.851349	36.612480
1602.663800	151180.677036	36.617498
1604.128727	151435.110888	36.622516
1605.772083	151666.597131	36.627533
1607.817504	151903.333138	36.632551
1609.061061	152152.280227	36.637568
1610.687584	152386.436586	36.642586
1612.525129	152610.279201	36.647604
1614.215168	152828.251437	36.652621
1615.770038	153043.355952	36.657639
1616.955580	153258.190893	36.662656
1619.069312	153471.079473	36.667674
1620.392590	153708.551718	36.672692
1621.570829	153928.945331	36.677709
1623.561875	154151.747031	36.682727
1624.926161	154385.452037	36.687744
1625.860950	154618.237945	36.692762
1627.663511	154862.577590	36.697780
1629.174631	155109.513782	36.702797
1631.078985	155345.421923	36.707815
1632.437355	155600.627384	36.712832
1633.999032	155846.090160	36.717850
1635.489381	156099.199023	36.722868
1636.949276	156357.551230	36.727885
1639.123496	156602.732008	36.732903
1640.649243	156869.902618	36.737920
1642.456785	157118.822447	36.742938
1644.014585	157374.085632	36.747956
1645.553520	157625.714573	36.752973
1647.358261	157880.232229	36.757991
1648.515425	158141.042514	36.763008
1650.330947	158407.824035	36.768026
1652.459716	158676.345791	36.773044
1653.870197	158947.874840	36.778061
1655.558153	159201.533143	36.783079
1657.031658	159486.168033	36.788096
1658.638372	159732.741963	36.793114
1660.511750	160015.681851	36.798132
1662.149162	160279.082184	36.803149
1664.061206	160545.699892	36.808167
1665.616131	160815.686099	36.813184
1667.288699	161076.170160	36.818202
1669.080278	161362.304155	36.823220
1670.362268	161639.023026	36.828237
1672.486685	161901.660634	36.833255
1674.111307	162177.872747	36.838272
1676.198429	162439.429623	36.843290
1677.913092	162713.285463	36.848308
1679.527360	162972.423013	36.853325
1681.492318	163241.804482	36.858343
1682.964366	163519.230567	36.863360
1684.645774	163784.070209	36.868378
1686.956901	164040.885390	36.873396
1688.134161	164308.472189	36.878413
1690.067923	164557.716188	36.883431
1691.529312	164834.710126	36.888448
1693.268600	165095.174649	36.893466
1695.286643	165358.919620	36.898484
1697.076878	165629.132831	36.903501
1699.244312	165883.155511	36.908519
1700.722060	166144.227038	36.913536
1702.390597	166394.831962	36.918554
1703.946447	166632.557731	36.923572
1705.226918	166878.674299	36.928589
1706.779520	167123.239966	36.933607
1708.380574	167355.851804	36.938624
1709.813531	167617.955444	36.943642
1711.373603	167872.392551	36.948660
1712.844850	168129.280740	36.953677
1714.485643	168387.437496	36.958695
1715.914258	168658.097888	36.963712
1717.760384	168926.017613	36.968730
1719.581418	169186.700657	36.973748
1720.905655	169457.370631	36.978765
1722.710462	169732.786197	36.983783
1724.572678	170011.860380	36.988800
1726.152370	170287.759628	36.993818
1727.967829	170562.672084	36.998836
1729.616736	170851.058548	37.003853
1731.712219	171122.531069	37.008871
1733.306117	171421.116263	37.013888
1734.869563	171711.882052	37.018906
1736.956212	171978.262654	37.023924
1738.418118	172279.589943	37.028941
1740.287767	172555.230919	37.033959
1742.067231	172835.366014	37.038976
1743.677400	173134.342235	37.043994
1745.525341	173418.796272	37.049012
1747.214627	173715.899570	37.054029
1749.465948	173995.650814	37.059047
1750.863675	174298.881129	37.064064
1752.809105	174577.314965	37.069082
1754.840836	174882.694408	37.074100
1756.534853	175176.560226	37.079117
1758.500730	175458.295252	37.084135
1760.231420	175753.783252	37.089152
1761.999564	176048.430168	37.094170
1763.820393	176328.468940	37.099188
1765.460207	176631.411897	37.104205
1767.241809	176923.170493	37.109223
1768.799466	177220.929396	37.114240
1770.682771	177510.760341	37.119258
1772.450152	177808.667799	37.124276
1774.306596	178096.451859	37.129293
1776.239250	178386.763194	37.134311
1778.227070	178686.659164	37.139328
1780.192033	178986.472104	37.144346
1782.124634	179271.422948	37.149364
1783.714533	179557.267489	37.154381
1785.452751	179853.100739	37.159399
1787.211794	180147.841629	37.164416
1788.929581	180442.426176	37.169434
1791.310693	180729.129943	37.174452
1792.850799	181034.112565	37.179469
1794.826292	181315.860328	37.184487
1796.536473	181602.270443	37.189504
1798.063190	181884.803695	37.194522
1800.262859	182150.521816	37.199540
1801.504969	182432.190281	37.204557
1803.577193	182696.130260	37.209575
1804.994807	182960.315329	37.214592
1806.780363	183226.511780	37.219610
1808.684217	183490.483281	37.224628
1810.302976	183772.899949	37.229645
1812.314779	184044.787948	37.234663
1813.880720	184315.403400	37.239680
1815.341544	184609.942768	37.244698
1817.468445	184892.628495	37.249716
1818.836584	185184.217181	37.254733
1820.773480	185466.733674	37.259751
1822.309143	185762.283859	37.264768
1824.154281	186064.055291	37.269786
1826.287281	186358.854716	37.274804
1827.493615	186670.946425	37.279821
1829.032000	186978.660470	37.284839
1831.167759	187289.289164	37.289856
1832.868897	187601.397496	37.294874
1834.900552	187912.732164	37.299892
1836.471858	188225.994707	37.304909
1838.451686	188544.524247	37.309927
1840.165156	188859.849625	37.314944
1841.961343	189184.668816	37.319962
1844.238295	189501.609531	37.324980
1846.039986	189831.229171	37.329997
1847.958408	190154.842771	37.335015
1849.814369	190472.516717	37.340032
1851.567961	190793.153211	37.345050
1853.471041	191117.169188	37.350068
1855.219961	191458.636032	37.355085
1857.195734	191780.690585	37.360103
1859.321218	192104.563682	37.365120
1861.297139	192430.848562	37.370138
1863.531965	192759.378903	37.375156
1864.970482	193083.101031	37.380173
1867.226049	193408.891167	37.385191
1869.338513	193728.538244	37.390208
1871.216078	194042.577048	37.395226
1873.244113	194358.548422	37.400244
1874.884335	194680.027981	37.405261
1876.996655	195003.211484	37.410279
1879.028259	195318.896442	37.415296
1880.791741	195631.440318	37.420314
1883.217080	195937.801717	37.425332
1884.893237	196259.107938	37.430349
1886.776079	196579.824930	37.435367
1889.189309	196883.592081	37.440384
1890.668856	197197.218649	37.445402
1892.460447	197510.937205	37.450420
1894.221634	197832.239741	37.455437
1896.291513	198130.776042	37.460455
1898.091071	198449.334747	37.465472
1899.639435	198763.264428	37.470490
1902.218580	199049.692682	37.475508
1903.772458	199344.789244	37.480525
1905.262002	199633.614786	37.485543
1907.311552	199916.641286	37.490560
1909.090359	200224.018955	37.495578
1911.165215	200519.140855	37.500596
1912.479809	200809.688641	37.505613
1914.645051	201109.648119	37.510631
1916.468394	201420.566867	37.515648
1917.978927	201740.612631	37.520666
1920.004379	202038.733501	37.525684
1921.685464	202358.362301	37.530701
1923.613460	202685.531701	37.535719
1925.724231	202996.236013	37.540736
1927.537774	203316.674373	37.545754
1929.286432	203637.264491	37.550772
1931.030482	203982.901753	37.555789
1933.238570	204322.260245	37.560807
1935.162674	204648.159614	37.565824
1936.996594	204980.218993	37.570842
1939.211131	205297.545677	37.575860
1941.324187	205635.670333	37.580877
1943.189569	205984.854748	37.585895
1945.087642	206323.715701	37.590912
1946.872326	206652.910897	37.595930
1949.055700	206989.762814	37.600948
1950.904062	207336.330249	37.605965
1953.246690	207685.017415	37.610983
1955.120363	208015.094670	37.616000
1956.827631	208350.544580	37.621018
1958.751211	208690.265526	37.626036
1961.056395	209042.457543	37.631053
1962.903489	209382.537257	37.636071
1965.024895	209713.638123	37.641088
1966.899384	210061.423052	37.646106
1969.266941	210393.961127	37.651124
1970.871883	210746.121674	37.656141
1972.799549	211089.955740	37.661159
1974.852034	211435.599995	37.666176
1976.722731	211789.374598	37.671194
1979.045683	212131.348872	37.676212
1980.910535	212474.806865	37.681229
1982.742995	212837.543633	37.686247
1985.215295	213178.509537	37.691264
1987.063845	213542.466478	37.696282
1989.296052	213881.709465	37.701300
1991.209802	214220.979346	37.706317
1992.977395	214572.804971	37.711335
1995.307263	214905.410486	37.716352
1997.421217	215258.022705	37.721370
1999.442442	215595.720930	37.726388
2001.460331	215943.502089	37.731405
2003.406912	216293.035720	37.736423
2005.673176	216625.926424	37.741440
2007.349881	216957.210980	37.746458
2009.454193	217275.631342	37.751476
2011.219486	217588.457049	37.756493
2013.172462	217921.708404	37.761511
2015.419409	218226.931529	37.766528
2017.257193	218550.097693	37.771546
2018.967042	218869.984498	37.776564
2021.311351	219199.523142	37.781581
2023.325884	219521.243627	37.786599
2025.586849	219847.814722	37.791616
2027.157614	220178.953397	37.796634
2029.037440	220507.124241	37.801652
2031.157890	220839.003985	37.806669
2032.851184	221186.151359	37.811687
2034.800476	221505.630828	37.816704
2036.719301	221865.722023	37.821722
2039.006500	222204.564824	37.826740
2040.653616	222563.381937	37.831757
2042.501097	222921.610263	37.836775
2044.804077	223268.441910	37.841792
2046.495044	223638.087962	37.846810
2048.546444	224001.659958	37.851828
2050.493609	224369.554655	37.856845
2052.027058	224800.065281	37.861863
2054.539624	225169.943702	37.866880
2056.698062	225551.358788	37.871898
2058.803873	225930.447622	37.876916
2061.056041	226303.737463	37.881933
2063.036459	226682.544924	37.886951
2065.369463	227053.565104	37.891968
2067.435732	227434.940069	37.896986
2069.535548	227807.854501	37.902004
2071.984424	228180.842181	37.907021
2073.882849	228572.788375	37.912039
2076.430757	228941.471656	37.917056
2078.257274	229316.162972	37.922074
2080.571470	229688.137264	37.927092
2082.823998	230056.541950	37.932109
2084.883001	230436.331315	37.937127
2086.864742	230808.159859	37.942144
2088.742365	231190.927245	37.947162
2090.802276	231553.324082	37.952180
2093.345398	231947.240066	37.957197
2095.246684	232337.881670	37.962215
2097.552448	232701.361489	37.967232
2099.939220	233078.468429	37.972250
2101.930721	233457.061843	37.977268
2104.108875	233828.617319	37.982285
2106.277728	234190.676842	37.987303
2108.304073	234570.792965	37.992320
2110.416375	234942.718698	37.997338
2112.404649	235320.253120	38.002356
2114.585203	235702.787343	38.007373
2116.579057	236078.825214	38.012391
2118.685470	236453.678279	38.017408
2120.657498	236819.943872	38.022426
2122.431566	237181.187801	38.027444
2124.513477	237537.304372	38.032461
2126.614840	237903.223038	38.037479
2128.682835	238250.657766	38.042496
2130.512232	238625.994259	38.047514
2132.320579	238982.844777	38.052532
2134.737033	239344.070264	38.057549
2136.557702	239716.592532	38.062567
2139.091310	240094.057437	38.067584
2141.123467	240462.510108	38.072602
2143.165023	240845.414836	38.077620
2145.525351	241224.155519	38.082637
2147.322923	241599.557714	38.087655
2149.524773	241990.670272	38.092672
2151.908420	242378.478681	38.097690
2153.823232	242764.432287	38.102708
2156.112006	243137.348353	38.107725
2157.950274	243545.363806	38.112743
2160.132216	243932.701077	38.117760
2162.748359	244338.436691	38.122778
2164.862360	244739.808152	38.127796
2167.368453	245123.770138	38.132813
2169.186866	245523.539842	38.137831
2171.598327	245923.369083	38.142848
2173.597109	246320.216868	38.147866
2175.571637	246728.957203	38.152884
2178.020250	247133.102196	38.157901
2179.722660	247547.603256	38.162919
2182.114364	247952.166011	38.167936
2184.636404	248362.348254	38.172954
2186.902218	248773.461310	38.177972
2188.876383	249192.445314	38.182989
2190.880688	249603.805309	38.188007
2193.465619	250008.673179	38.193024
2195.813474	250421.555729	38.198042
2197.930692	250840.775485	38.203060
2200.683034	251241.987523	38.208077
2203.111131	251660.575842	38.213095
2205.381614	252057.065362	38.218112
2207.922808	252450.820293	38.223130
2210.015258	252856.205083	38.228148
2212.450806	253249.470528	38.233165
2214.673092	253656.970304	38.238183
2216.939507	254050.619936	38.243200
2218.945839	254458.409745	38.248218
2220.956379	254857.385256	38.253236
2223.668482	255258.079287	38.258253
2225.798119	255671.719984	38.263271
2227.674573	256059.110409	38.268288
2230.277306	256465.641295	38.273306
2232.237481	256869.582220	38.278324
2234.503730	257272.103648	38.283341
2236.505014	257671.187706	38.288359
2239.043575	258063.100005	38.293376
2241.164383	258471.235192	38.298394
2243.062402	258853.749882	38.303412
2245.683920	259214.888525	38.308429
2247.338361	259607.680261	38.313447
2249.490211	259984.593307	38.318464
2252.051416	260362.559717	38.323482
2253.913252	260747.826534	38.328500
2256.504999	261139.481267	38.333517
2258.159681	261521.555880	38.338535
2260.350207	261918.686117	38.343552
2262.499641	262314.578673	38.348570
2264.565885	262711.323238	38.353588
2267.530565	263108.484723	38.358605
2269.691689	263513.039358	38.363623
2271.989480	263906.268500	38.368640
2274.403481	264303.594959	38.373658
2276.377711	264725.403907	38.378676
2278.797582	265126.439195	38.383693
2281.017967	265538.125028	38.388711
2283.578560	265948.588810	38.393728
2285.780690	266358.779600	38.398746
2287.650150	266780.073905	38.403764
2290.113721	267192.535717	38.408781
2292.151750	267616.573015	38.413799
2294.220003	268042.866775	38.418816
2296.756395	268473.608443	38.423834
2299.135659	268906.890287	38.428852
2301.541801	269326.323406	38.433869
2303.611945	269769.333536	38.438887
2306.019479	270194.279521	38.443904
2308.511574	270628.941830	38.448922
2311.069465	271069.970195	38.453940
2313.861587	271495.313191	38.458957
2315.979656	271933.998403	38.463975
2318.329070	272366.347091	38.468992
2320.962762	272781.376571	38.474010
2323.248589	273217.952607	38.479028
2325.652742	273645.517209	38.484045
2327.994846	274080.509545	38.489063
2330.411511	274509.215506	38.494080
2332.656789	274930.200662	38.499098
2334.637137	275370.458248	38.504116
2337.245721	275801.013775	38.509133
2339.977422	276239.653483	38.514151
2342.154088	276670.099653	38.519168
2344.651104	277097.853052	38.524186
2346.740390	277533.622303	38.529204
2349.284859	277971.935873	38.534221
2351.334515	278408.016079	38.539239
2354.097442	278841.620586	38.544256
2356.563554	279274.179667	38.549274
2358.470623	279715.718397	38.554292
2361.208499	280136.396104	38.559309
2363.870398	280573.750272	38.564327
2366.125119	281000.118319	38.569344
2368.612027	281408.412976	38.574362
2370.503537	281823.940121	38.579380
2373.231156	282220.663061	38.584397
2375.277381	282622.676040	38.589415
2377.603074	283017.937995	38.594432
2379.842013	283424.340052	38.599450
2382.008400	283835.325887	38.604468
2384.587766	284226.914098	38.609485
2387.054622	284641.230278	38.614503
2389.049488	285063.419676	38.619520
2391.704939	285469.703220	38.624538
2393.625869	285893.630951	38.629556
2396.433087	286304.665416	38.634573
2398.731906	286738.160128	38.639591
2400.695321	287164.645466	38.644608
2403.141261	287588.081672	38.649626
2404.932051	288024.830750	38.654644
2407.402826	288471.912089	38.659661
2409.806507	288914.049885	38.664679
2412.199857	289365.054295	38.669696
2414.776207	289816.486283	38.674714
2417.147504	290276.104371	38.679732
2419.389457	290731.499961	38.684749
2421.706445	291200.549556	38.689767
2424.263933	291659.043516	38.694784
2426.934214	292113.937024	38.699802
2428.935487	292584.253486	38.704820
2431.446882	293047.934351	38.709837
2434.194397	293517.089225	38.714855
2436.492950	293999.548959	38.719872
2439.098384	294472.001308	38.724890
2441.880479	294951.435679	38.729908
2444.364271	295414.303196	38.734925
2447.089992	295873.879871	38.739943
2449.467153	296346.211818	38.744960
2452.382428	296815.815554	38.749978
2454.903772	297282.660973	38.754996
2457.569146	297744.173423	38.760013
2460.291115	298208.647787	38.765031
2462.527524	298678.710118	38.770048
2465.305388	299144.798944	38.775066
2467.372485	299602.540419	38.780084
2470.027074	300059.603341	38.785101
2472.614519	300525.490003	38.790119
2475.006721	300982.693597	38.795136
2477.502440	301442.292638	38.800154
2480.171945	301913.928444	38.805172
2482.686822	302374.004376	38.810189
2485.541861	302838.114620	38.815207
2487.676735	303299.213235	38.820224
2490.533248	303754.404640	38.825242
2492.951861	304216.471476	38.830260
2495.348418	304667.084547	38.835277
2497.866210	305123.239746	38.840295
2500.201183	305584.908976	38.845312
2503.010822	306039.160669	38.850330
2505.141141	306475.814332	38.855348
2507.211830	306903.611268	38.860365
2510.184483	307332.762513	38.865383
2512.357020	307756.222466	38.870400
2514.968876	308184.666045	38.875418
2517.602348	308621.029578	38.880436
2519.858588	309044.624361	38.885453
2521.955203	309482.238335	38.890471
2524.367871	309936.818535	38.895488
2527.014530	310374.748520	38.900506
2529.055061	310828.850894	38.905524
2531.409439	311288.921465	38.910541
2534.213561	311745.159827	38.915559
2536.598142	312204.586956	38.920576
2539.268419	312679.587460	38.925594
2541.522423	313154.042312	38.930612
2544.074309	313629.362279	38.935629
2546.595301	314110.983977	38.940647
2548.912229	314585.244798	38.945664
2552.015326	315066.261962	38.950682
2553.953538	315553.658716	38.955700
2556.636804	316051.424662	38.960717
2559.329824	316531.382430	38.965735
2561.753437	317035.508846	38.970752
2564.470030	317519.902811	38.975770
2567.368540	318022.323474	38.980788
2569.701217	318525.821695	38.985805
2572.329460	319021.930528	38.990823
2574.695692	319526.586437	38.995840
2577.692843	320021.107710	39.000858
2579.839353	320535.266180	39.005876
2582.544012	321047.123790	39.010893
2585.971573	321550.736955	39.015911
2588.082345	322061.184465	39.020928
2590.726665	322568.547698	39.025946
2593.315284	323062.939202	39.030964
2596.654279	323575.011853	39.035981
2599.150758	324072.383534	39.040999
2601.645035	324593.167806	39.046016
2604.351189	325082.906893	39.051034
2607.352594	325600.861781	39.056052
2609.793522	326109.023314	39.061069
2613.042603	326600.572016	39.066087
2615.770565	327098.904624	39.071104
2618.303608	327603.359823	39.076122
2621.073296	328096.143427	39.081140
2623.778918	328589.238813	39.086157
2626.407985	329075.943744	39.091175
2628.840329	329565.851061	39.096192
2631.823597	330050.360543	39.101210
2634.358304	330545.324170	39.106228
2636.602096	331034.947081	39.111245
2639.617673	331530.792949	39.116263
2642.228981	332019.944801	39.121280
2644.477135	332506.941658	39.126298
2647.085722	332974.756987	39.131316
2649.597374	333429.532545	39.136333
2652.286359	333884.454849	39.141351
2654.709838	334366.738919	39.146368
2656.906141	334825.161187	39.151386
2659.624790	335297.895204	39.156404
2662.184478	335769.051436	39.161421
2664.797961	336240.043538	39.166439
2667.229708	336729.571856	39.171456
2669.755711	337214.511162	39.176474
2672.396085	337705.649748	39.181492
2674.708590	338194.805306	39.186509
2677.525629	338691.621603	39.191527
2680.203461	339215.040487	39.196544
2682.935248	339705.565548	39.201562
2686.101992	340212.344088	39.206580
2688.609403	340725.443647	39.211597
2691.219222	341232.886192	39.216615
2693.934929	341746.909228	39.221632
2696.624165	342263.623504	39.226650
2699.276882	342783.868365	39.231668
2702.260453	343292.478870	39.236685
2704.993379	343810.188703	39.241703
2707.748965	344338.680750	39.246720
2710.214195	344861.374714	39.251738
2713.434182	345379.247669	39.256756
2715.533674	345911.003134	39.261773
2718.741838	346444.507647	39.266791
2721.504048	346975.335993	39.271808
2724.224431	347498.346711	39.276826
2727.015533	348040.001051	39.281844
2729.683366	348567.783038	39.286861
2732.731615	349089.000807	39.291879
2735.022175	349637.624203	39.296896
2737.999005	350167.195323	39.301914
2741.363221	350699.086275	39.306932
2743.491009	351237.539674	39.311949
2746.346668	351775.897836	39.316967
2749.266977	352315.230394	39.321984
2752.149840	352858.244258	39.327002
2754.993605	353399.304124	39.332020
2757.708294	353926.493556	39.337037
2760.574239	354461.675134	39.342055
2763.509953	355005.724533	39.347072
2766.068929	355547.695619	39.352090
2768.915851	356080.731173	39.357108
2771.796584	356632.082424	39.362125
2774.893178	357159.888930	39.367143
2777.502245	357704.544991	39.372160
2780.238735	358232.651023	39.377178
2783.269169	358771.568403	39.382196
2786.134997	359300.987774	39.387213
2789.180503	359834.814726	39.392231
2791.860774	360372.805403	39.397248
2794.288862	360890.043016	39.402266
2797.411521	361391.758998	39.407284
2799.734628	361905.550479	39.412301
2802.435520	362386.383901	39.417319
2805.358672	362895.983400	39.422336
2808.035889	363387.850570	39.427354
2810.620329	363883.965589	39.432372
2812.785726	364400.571792	39.437389
2815.917313	364912.019601	39.442407
2818.796565	365421.674399	39.447424
2821.581257	365952.047077	39.452442
2824.690281	366461.729952	39.457460
2827.129496	366996.941475	39.462477
2829.986503	367516.930194	39.467495
2832.501852	368052.117004	39.472512
2834.941653	368584.187964	39.477530
2837.987332	369126.535504	39.482548
2840.571191	369683.363038	39.487565
2843.547710	370229.945598	39.492583
2845.991620	370789.318648	39.497600
2848.848675	371342.478233	39.502618
2851.987036	371913.323065	39.507636
2854.694612	372479.102789	39.512653
2857.704692	373047.364440	39.517671
2860.743164	373629.061964	39.522688
2863.798843	374187.937994	39.527706
2866.959996	374763.662849	39.532724
2869.331462	375339.022596	39.537741
2872.667661	375900.799585	39.542759
2875.442263	376480.950911	39.547776
2878.338797	377063.028235	39.552794
2881.607318	377635.067367	39.557812
2884.153709	378218.832494	39.562829
2887.335891	378792.949111	39.567847
2890.360447	379367.462904	39.572864
2893.238514	379953.661582	39.577882
2896.212018	380533.747725	39.582900
2899.096699	381112.646941	39.587917
2902.223843	381692.488493	39.592935
2905.140088	382276.388239	39.597952
2907.879574	382863.325831	39.602970
2911.406803	383432.879818	39.607988
2914.294924	384018.406180	39.613005
2917.216917	384592.173313	39.618023
2920.383325	385179.007329	39.623040
2923.181308	385747.373333	39.628058
2925.796422	386326.108684	39.633076
2928.693693	386917.726477	39.638093
2931.874627	387491.788202	39.643111
2934.981964	388071.635596	39.648128
2937.741460	388658.757481	39.653146
2940.782414	389230.429652	39.658164
2943.676110	389816.750509	39.663181
2946.619021	390411.296805	39.668199
2949.546652	390980.245110	39.673216
2952.195584	391562.517956	39.678234
2955.325429	392096.543768	39.683252
2958.146184	392662.996364	39.688269
2961.008891	393196.058569	39.693287
2964.007343	393737.181005	39.698304
2966.807708	394280.963732	39.703322
2969.443457	394833.056435	39.708340
2972.640081	395386.877304	39.713357
2975.264005	395935.784164	39.718375
2977.869762	396512.934000	39.723392
2980.510915	397092.933779	39.728410
2983.798873	397652.307129	39.733428
2986.361895	398244.369396	39.738445
2989.151525	398822.768875	39.743463
2992.270638	399417.131056	39.748480
2994.565762	400022.490414	39.753498
2997.793169	400615.292446	39.758516
3001.205019	401221.416356	39.763533
3004.326946	401828.918591	39.768551
3007.247427	402447.850388	39.773568
3010.288254	403055.012736	39.778586
3013.559348	403667.501868	39.783604
3016.361990	404303.630809	39.788621
3019.317988	404913.078166	39.793639
3022.443827	405537.317263	39.798656
3025.122138	406177.256074	39.803674
3027.975107	406799.611868	39.808692
3031.428676	407442.874938	39.813709
3034.512607	408069.047159	39.818727
3037.164526	408715.553810	39.823744
3040.407036	409368.721256	39.828762
3043.605201	410013.364971	39.833780
3046.853534	410666.757056	39.838797
3049.782528	411300.111210	39.843815
3053.279431	411955.793171	39.848832
3056.209314	412613.121864	39.853850
3059.433902	413244.715218	39.858868
3062.838988	413913.927916	39.863885
3065.834147	414549.838137	39.868903
3069.032796	415189.782585	39.873920
3072.261103	415852.009655	39.878938
3075.715843	416497.966990	39.883956
3078.829937	417141.024186	39.888973
3081.720018	417783.139498	39.893991
3085.314061	418429.766274	39.899008
3087.758252	419078.004664	39.904026
3091.178522	419726.707279	39.909044
3094.801834	420366.418393	39.914061
3097.233807	421027.207167	39.919079
3100.658917	421660.839026	39.924096
3103.573895	422303.683725	39.929114
3107.036490	422943.513228	39.934132
3109.851315	423594.096636	39.939149
3112.802443	424249.000681	39.944167
3116.223544	424885.624673	39.949184
3119.086267	425528.579553	39.954202
3122.219507	426139.987331	39.959220
3125.250811	426742.885655	39.964237
3128.463903	427352.733337	39.969255
3131.261861	427950.625722	39.974272
3134.161508	428574.579393	39.979290
3137.279529	429182.677795	39.984308
3140.173617	429805.868801	39.989325
3143.068095	430424.815061	39.994343
3146.419317	431051.323665	39.999360
3149.160914	431684.448281	40.004378
3152.278405	432324.690968	40.009396
3155.494991	432960.470016	40.014413
3158.317070	433608.123044	40.019431
3161.771317	434253.608406	40.024448
3164.582517	434910.448703	40.029466
3167.635689	435560.295024	40.034484
3171.052950	436230.857604	40.039501
3173.787753	436907.790384	40.044519
3177.349879	437570.596353	40.049536
3180.259804	438254.757883	40.054554
3183.551767	438932.484761	40.059572
3186.685116	439631.664231	40.064589
3189.864193	440296.205355	40.069607
3193.362019	440989.389365	40.074624
3196.332964	441704.714257	40.079642
3199.626875	442392.725982	40.084660
3202.856278	443087.614509	40.089677
3205.904428	443791.777296	40.094695
3209.212980	444483.119653	40.099712
3212.538856	445202.335560	40.104730
3215.748767	445924.788303	40.109748
3219.283943	446624.690105	40.114765
3222.787929	447334.346569	40.119783
3226.145463	448039.448884	40.124800
3229.383133	448753.053297	40.129818
3232.808606	449461.594980	40.134836
3235.966416	450169.043893	40.139853
3238.618566	450890.065724	40.144871
3242.398477	451598.131882	40.149888
3245.852656	452315.236892	40.154906
3249.117036	453025.618208	40.159924
3252.562494	453745.564652	40.164941
3255.770673	454470.434836	40.169959
3259.232355	455179.907978	40.174976
3262.524719	455897.431781	40.179994
3265.886152	456612.796423	40.185012
3269.277243	457313.509633	40.190029
3272.366925	458030.238127	40.195047
3276.172127	458756.241647	40.200064
3279.298061	459477.977444	40.205082
3282.369995	460188.719003	40.210100
3285.699831	460905.720950	40.215117
3288.699524	461626.950712	40.220135
3291.883901	462336.643421	40.225152
3294.869549	463053.022020	40.230170
3298.192449	463735.228005	40.235188
3301.024880	464422.093191	40.240205
3304.333592	465110.985577	40.245223
3307.566461	465791.825205	40.250240
3310.996289	466487.179064	40.255258
3313.664534	467175.802429	40.260276
3316.845872	467865.384341	40.265293
3319.936025	468578.930819	40.270311
3322.914138	469281.445685	40.275328
3326.305173	469999.194940	40.280346
3329.495621	470730.149978	40.285364
3332.799554	471455.144810	40.290381
3335.992167	472195.655742	40.295399
3339.514055	472923.042259	40.300416
3342.758033	473675.222752	40.305434
3345.839914	474402.980175	40.310452
3349.720614	475183.419656	40.315469
3352.767577	475942.372964	40.320487
3355.994649	476694.343177	40.325504
3359.268560	477460.938371	40.330522
3362.869594	478224.672173	40.335540
3366.265325	478998.013620	40.340557
3369.537462	479782.818819	40.345575
3372.995918	480564.480171	40.350592
3376.455060	481346.514780	40.355610
3379.907763	482135.948878	40.360628
3383.527851	482910.112271	40.365645
3386.312366	483709.847910	40.370663
3390.192397	484497.097311	40.375680
3393.397560	485295.791356	40.380698
3396.498614	486116.601403	40.385716
3400.279057	486910.690669	40.390733
3403.828137	487713.575203	40.395751
3407.163052	488523.684780	40.400768
3410.710039	489329.431803	40.405786
3413.641334	490154.843724	40.410804
3417.449479	490971.290653	40.415821
3420.720868	491786.473453	40.420839
3424.243287	492608.703424	40.425856
3427.879442	493429.767807	40.430874
3431.318757	494255.019189	40.435892
3435.313425	495067.620123	40.440909
3438.291666	495897.062905	40.445927
3441.871557	496716.019999	40.450944
3445.273055	497541.988060	40.455962
3448.659536	498362.568172	40.460980
3452.517564	499196.973348	40.465997
3455.366133	500016.704945	40.471015
3459.054542	500856.917205	40.476032
3462.889532	501690.907239	40.481050
3466.099106	502508.650054	40.486068
3470.105310	503352.733361	40.491085
3473.203640	504192.174646	40.496103
3476.980116	504989.116770	40.501120
3480.433933	505826.376592	40.506125
3483.703929	506581.085801	40.511130
3486.937315	507293.667628	40.516135
3490.084924	507952.851187	40.521140
3493.175380	508551.200061	40.526144
3495.976302	509083.242224	40.531149
3498.640550	509572.739256	40.536154
3501.134583	509982.210116	40.541159
3503.034333	510363.888621	40.546164
3505.323053	510650.688393	40.551168
3507.320729	510934.544493	40.556173
3509.207673	511135.850117	40.561178
3511.003280	511298.365412	40.566183
3512.129587	511440.698585	40.571188
3513.517510	511493.800523	40.576192
3515.001225	511548.101295	40.581197
3515.755070	511571.152059	40.586202
3517.112016	511512.304864	40.591207
3517.574918	511510.107056	40.596212
3518.409632	511422.000304	40.601216
3519.263370	511293.721771	40.606221
3519.764978	511205.767735	40.611226
3520.296095	511032.108222	40.616231
3520.582306	510897.137269	40.621236
3520.907313	510717.891540	40.626240
3521.279492	510513.846327	40.631245
3521.352486	510323.506023	40.636250
3521.715253	510122.999146	40.641255
3521.692753	509892.548596	40.646260
3521.825382	509657.263944	40.651264
3521.834466	509442.031372	40.656269
3521.760501	509183.600224	40.661274
3522.091734	508957.078347	40.666279
3521.824599	508693.003548	40.671284
3521.689815	508450.408065	40.676288
3522.083991	508165.728397	40.681293
3521.878026	507939.531104	40.686298
3521.728541	507637.218772	40.691303
3521.281631	507415.960998	40.696308
3521.202189	507107.809242	40.701312
3521.127514	506885.777463	40.706317
3520.943055	506585.375294	40.711322
3520.861393	506336.720078	40.716327
3520.399444	506074.559255	40.721332
3520.324238	505814.863672	40.726336
3520.059164	505557.775187	40.731341
3519.619908	505303.493868	40.736346
3519.491901	505047.489603	40.741351
3519.571652	504796.459049	40.746356
3518.916747	504552.322709	40.751360
3518.843479	504306.724577	40.756365
3518.942986	504064.233596	40.761370
3518.611275	503809.103915	40.766375
3518.194081	503576.911465	40.771380
3518.196918	503341.511574	40.776384
3518.067300	503094.893248	40.781389
3517.437383	502891.119698	40.786394
3517.272157	502635.390036	40.791399
3516.734036	502413.628153	40.796404
3516.409125	502206.862836	40.801408
3516.706174	501994.277109	40.806413
3516.153066	501777.571354	40.811418
3516.093607	501576.020976	40.816423
3515.243483	501374.188343	40.821428
3515.596951	501161.887497	40.826432
3515.580698	500956.678721	40.831437
3514.809662	500792.690585	40.836442
3515.101227	500571.382116	40.841447
3515.088805	500383.073531	40.846452
3514.848838	500199.608021	40.851456
3514.497861	500015.955692	40.856461
3513.645645	499831.823859	40.861466
3514.099003	499659.886534	40.866471
3513.335809	499482.773715	40.871476
3513.303866	499309.542906	40.876480
3513.236865	499154.743434	40.881485
3512.890871	499004.543007	40.886490
3513.175780	498822.954900	40.891495
3512.573687	498664.742625	40.896500
3512.295641	498518.172505	40.901504
3512.327619	498377.374307	40.906509
3512.378693	498216.472896	40.911514
3512.144538	498064.576283	40.916519
3511.329248	497926.693037	40.921524
3511.199801	497779.485917	40.926528
3511.502559	497657.878236	40.931533
3511.322750	497523.283629	40.936538
3511.220559	497392.169214	40.941543
3510.916414	497261.187035	40.946548
3510.971869	497137.792282	40.951552
3510.620108	497027.878223	40.956557
3510.332435	496889.599932	40.961562
3510.628747	496762.620388	40.966567
3510.119738	496655.108618	40.971572
3509.906935	496535.195154	40.976576
3510.083026	496418.206751	40.981581
3509.532155	496320.522328	40.986586
3509.772918	496216.535028	40.991591
3509.168581	496114.098446	40.996596
3509.483228	496007.262812	41.001600
3509.059702	495902.669856	41.006605
3509.218060	495814.440438	41.011610
3509.203640	495705.477790	41.016615
3508.712872	495612.590362	41.021620
3509.063718	495505.138466	41.026624
3508.959489	495423.784400	41.031629
3508.497700	495335.549430	41.036634
3508.680180	495249.237633	41.041639
3508.376447	495163.052916	41.046644
3508.144194	495076.400772	41.051648
3508.242622	494991.316318	41.056653
3507.836320	494921.806059	41.061658
3508.021753	494839.846623	41.066663
3508.111799	494758.003173	41.071668
3507.761276	494688.483218	41.076672
3507.986919	494606.769576	41.081677
3507.802828	494537.324019	41.086682
3507.582808	494447.274256	41.091687
3507.469282	494383.792240	41.096692
3507.589301	494314.550967	41.101696
3507.276419	494254.847251	41.106701
3506.979315	494190.785927	41.111706
3507.206453	494110.589012	41.116711
3507.077760	494060.628849	41.121716
3506.863167	493998.933849	41.126720
3507.165535	493936.549261	41.131725
3506.719089	493877.422469	41.136730
3506.625803	493817.328153	41.141735
3506.413092	493762.873536	41.146740
3506.616384	493704.301810	41.151744
3506.289653	493651.080245	41.156749
3506.324778	493621.551593	41.161754
3506.696975	493564.978336	41.166759
3506.584500	493515.672463	41.171764
3506.154067	493472.645509	41.176768
3506.797289	493422.257770	41.181773
3506.228110	493361.173739	41.186778
3506.070634	493304.379563	41.191783
3505.952036	493266.873356	41.196788
3505.662961	493217.138832	41.201792
3505.903388	493169.143572	41.206797
3505.628661	493114.696853	41.211802
3505.852326	493111.015410	41.216807
3505.830233	493045.843181	41.221812
3505.529832	493024.621217	41.226816
3505.949577	492988.700537	41.231821
3505.817187	492947.499005	41.236826
3505.887918	492907.531330	41.241831
3505.689192	492861.529090	41.246836
3505.778010	492819.380749	41.251840
3505.945471	492774.738400	41.256845
3505.253801	492749.172068	41.261850
3505.521535	492707.096478	41.266855
3505.306807	492681.555952	41.271860
3505.082201	492652.066812	41.276864
3505.280103	492611.116185	41.281869
3505.154165	492586.624996	41.286874
3505.139771	492552.038169	41.291879
3505.073325	492545.870316	41.296884
3505.289486	492494.281489	41.301888
3505.176750	492463.660216	41.306893
3504.958480	492463.036456	41.311898
3505.497081	492415.397269	41.316903
3505.132444	492376.104989	41.321908
3504.884310	492354.519492	41.326912
3504.964431	492321.132745	41.331917
3505.061039	492306.278961	41.336922
3505.114538	492266.565852	41.341927
3504.949516	492264.718215	41.346932
3504.981326	492223.185262	41.351936
3505.094595	492190.653990	41.356941
3504.814372	492177.328344	41.361946
3505.024740	492157.847844	41.366951
3505.107450	492128.106723	41.371956
3504.936791	492097.595292	41.376960
3504.734062	492081.623822	41.381965
3505.047215	492065.317576	41.386970
3504.996872	492025.924235	41.391975
3504.739096	492011.379453	41.396980
3504.812345	491983.361511	41.401984
3504.807549	491952.519759	41.406989
3504.630882	491934.265031	41.411994
3504.874555	491912.246772	41.416999
3504.584437	491888.692223	41.422004
3504.635796	491871.768804	41.427008
3504.607080	491845.640636	41.432013
3504.603141	491831.156881	41.437018
3504.496196	491808.788759	41.442023
3504.450573	491791.880597	41.447028
3504.157891	491775.365986	41.452032
3504.694068	491755.985506	41.457037
3504.364661	491744.034745	41.462042
3504.623102	491721.710057	41.467047
3504.521683	491706.735160	41.472052
3504.570102	491687.330414	41.477056
3504.620071	491667.469593	41.482061
3504.501286	491665.563943	41.487066
3504.858750	491633.195684	41.492071
3504.566945	491631.114796	41.497076
3504.502377	491594.356364	41.502080
3504.781574	491580.941868	41.507085
3504.572743	491562.236048	41.512090
3504.523491	491538.845569	41.517095
3504.673208	491524.235997	41.522100
3504.577921	491507.538011	41.527104
3504.646798	491476.683829	41.532109
3504.508156	491472.704810	41.537114
3504.665183	491445.128634	41.542119
3504.353702	491435.656501	41.547124
3504.465863	491413.000043	41.552128
3504.708690	491396.045930	41.557133
3504.512223	491386.353008	41.562138
3504.732663	491360.438010	41.567143
3504.244712	491333.318140	41.572148
3504.231857	491315.948551	41.577152
3504.468554	491306.389706	41.582157
3504.207680	491299.695060	41.587162
3504.342692	491273.945386	41.592167
3504.712053	491256.971147	41.597172
3504.310645	491249.437704	41.602176
3504.546653	491223.266824	41.607181
3504.391577	491219.594229	41.612186
3504.420699	491194.114416	41.617191
3504.325351	491174.985097	41.622196
3504.256645	491174.135064	41.627200
3504.341418	491145.050462	41.632205
3504.291959	491144.045444	41.637210
3504.465931	491124.215094	41.642215
3504.224155	491104.349143	41.647220
3503.864820	491103.696985	41.652224
3504.440873	491076.864388	41.657229
3504.393201	491066.843898	41.662234
3504.220083	491074.113902	41.667239
3504.249446	491045.746964	41.672244
3504.255415	491030.754552	41.677248
3504.306741	491013.881010	41.682253
3503.933568	491007.710483	41.687258
3504.483027	490995.316443	41.692263
3504.421178	490982.816431	41.697268
3504.205302	490965.326664	41.702272
3504.444962	490949.385596	41.707277
3504.264806	490935.790008	41.712282
3504.378863	490926.655535	41.717287
3504.140710	490903.192825	41.722292
3504.530817	490891.988799	41.727296
3504.557999	490876.385140	41.732301
3504.308106	490853.683938	41.737306
3504.470160	490845.605440	41.742311
3504.469718	490818.255824	41.747316
3504.497758	490812.072463	41.752320
3504.730401	490792.890912	41.757325
3504.571633	490768.959655	41.762330
3504.367906	490740.629098	41.767335
3504.306431	490737.650686	41.772340
3504.135939	490727.700076	41.777344
3504.168294	490701.104826	41.782349
3504.052599	490702.085530	41.787354
3504.240829	490686.506905	41.792359
3504.297536	490668.416646	41.797364
3503.921425	490665.437306	41.802368
3504.234625	490642.748142	41.807373
3504.072041	490632.796232	41.812378
3504.456503	490634.558905	41.817383
3504.351193	490605.300919	41.822388
3503.943928	490590.879956	41.827392
3504.399258	490588.680855	41.832397
3504.063332	490562.650104	41.837402
3504.462318	490555.648299	41.842407
3504.313705	490538.400744	41.847412
3503.812694	490515.941420	41.852416
3504.255231	490509.793741	41.857421
3504.058722	490516.561171	41.862426
3503.840290	490496.640237	41.867431
3504.005873	490495.196005	41.872436
3504.051742	490496.049886	41.877440
3504.088855	490483.685844	41.882445
3503.821534	490472.889377	41.887450
3504.242415	490452.259560	41.892455
3504.320757	490450.575871	41.897460
3504.063975	490426.963563	41.902464
3504.406815	490421.793942	41.907469
3504.267907	490411.281034	41.912474
3504.366477	490384.624221	41.917479
3504.271505	490387.627624	41.922484
3504.012590	490364.724661	41.927488
3504.093947	490355.949623	41.932493
3504.128172	490353.006672	41.937498
3504.411322	490329.815390	41.942503
3504.323108	490314.381451	41.947508
3504.138526	490312.536711	41.952512
3504.341613	490282.013896	41.957517
3504.320325	490286.879690	41.962522
3503.963042	490259.788261	41.967527
3504.038533	490246.658259	41.972532
3503.744729	490246.350256	41.977536
3504.105292	490231.351807	41.982541
3503.936385	490226.566917	41.987546
3503.719133	490208.013024	41.992551
3504.044162	490200.820180	41.997556
3504.157758	490202.473760	42.002560
3504.029546	490202.240881	42.007565
3504.203015	490177.496616	42.012570
3504.056462	490162.173072	42.017575
3504.015722	490163.091307	42.022580
3503.487337	490136.077393	42.027584
3503.937694	490137.627100	42.032589
3504.045645	490139.636125	42.037594
3504.187082	490126.850163	42.042599
3504.302784	490100.088940	42.047604
3503.997241	490100.542536	42.052608
3504.174538	490088.915824	42.057613
3504.243443	490073.152954	42.062618
3504.281086	490068.183426	42.067623
3504.159912	490050.981737	42.072628
3504.343543	490030.388960	42.077632
3504.194702	490017.902056	42.082637
3504.073996	490012.602993	42.087642
3504.029324	489989.209859	42.092647
3504.222349	489992.218453	42.097652
3503.840071	489967.055253	42.102656
3504.067130	489956.332296	42.107661
3504.009187	489958.722113	42.112666
3504.250214	489941.969575	42.117671
3504.131018	489938.797559	42.122676
3503.818832	489945.532827	42.127680
3504.044439	489929.441167	42.132685
3503.814625	489907.849953	42.137690
3503.868830	489897.964688	42.142695
3504.180393	489896.041484	42.147700
3504.316124	489900.730609	42.152704
3504.059082	489862.378400	42.157709
3503.989664	489866.390854	42.162714
3504.032386	489854.987871	42.167719
3503.735973	489840.346208	42.172724
3503.818940	489820.934073	42.177728
3504.167534	489824.070057	42.182733
3503.999346	489824.501948	42.187738
3503.672785	489802.571351	42.192743
3504.186188	489786.788634	42.197748
3503.852233	489796.870333	42.202752
3503.862372	489791.955730	42.207757
3503.624870	489775.076080	42.212762
3503.805301	489768.159181	42.217767
3503.987834	489759.317222	42.222772
3503.893184	489766.879230	42.227776
3504.178671	489759.692469	42.232781
3503.781415	489738.937937	42.237786
3503.865463	489732.390814	42.242791
3504.110105	489727.185875	42.247796
3503.802047	489715.686300	42.252800
3503.868648	489702.152118	42.257805
3503.968767	489700.262316	42.262810
3504.191827	489690.552856	42.267815
3504.021918	489687.287511	42.272820
3503.459703	489679.373645	42.277824
3504.053753	489663.730031	42.282829
3504.007500	489671.740286	42.287834
3504.038649	489660.845523	42.292839
3503.976802	489641.405443	42.297844
3503.701584	489626.810914	42.302848
3504.184893	489614.375776	42.307853
3503.848536	489619.899356	42.312858
3504.110297	489607.043372	42.317863
3504.365729	489594.948147	42.322868
3504.210218	489580.587916	42.327872
3504.349041	489561.673198	42.332877
3504.067643	489548.244562	42.337882
3503.939033	489541.680335	42.342887
3504.115671	489527.267564	42.347892
3504.102022	489526.864614	42.352896
3504.096756	489517.545714	42.357901
3503.858589	489500.412667	42.362906
3503.623052	489477.403626	42.367911
3503.805525	489478.742475	42.372916
3503.547047	489480.404278	42.377920
3504.029919	489475.566826	42.382925
3503.868458	489463.284154	42.387930
3503.864923	489453.863646	42.392935
3504.032917	489453.178726	42.397940
3503.993515	489452.070725	42.402944
3503.971084	489423.354969	42.407949
3504.212368	489422.607813	42.412954
3504.149404	489422.516565	42.417959
3504.318036	489388.705401	42.422964
3503.843064	489392.376846	42.427968
3504.222281	489386.947935	42.432973
3503.938575	489371.341517	42.437978
3503.828645	489358.544116	42.442983
3503.834783	489348.970071	42.447988
3504.035744	489347.520161	42.452992
3503.958626	489336.085155	42.457997
3503.598358	489324.239031	42.463002
3503.875378	489314.115634	42.468007
3503.989113	489313.034072	42.473012
3503.867363	489318.777076	42.478016
3504.104923	489278.268778	42.483021
3503.915125	489278.653444	42.488026
3503.666595	489277.223924	42.493031
3503.635395	489278.191346	42.498036
3503.505036	489278.060098	42.503040
3503.611950	489269.027255	42.508045
3503.619187	489265.987097	42.513050
3503.749167	489254.164743	42.518055
3503.836277	489248.022184	42.523060
3503.825778	489252.937192	42.528064
3503.799290	489253.701262	42.533069
3503.984679	489235.487985	42.538074
3503.970020	489208.239583	42.543079
3504.150114	489208.768393	42.548084
3504.146633	489204.311660	42.553088
3503.956908	489183.776974	42.558093
3503.527678	489191.290792	42.563098
3504.070652	489180.517462	42.568103
3504.273684	489170.253727	42.573108
3503.778509	489164.811005	42.578112
3503.875014	489144.433644	42.583117
3504.124373	489143.431939	42.588122
3503.968727	489141.886423	42.593127
3503.733260	489124.448693	42.598132
3503.968491	489120.258122	42.603136
3504.252139	489115.857288	42.608141
3503.772921	489107.676799	42.613146
3503.671388	489086.570892	42.618151
3503.712827	489075.218294	42.623156
3503.683189	489077.603748	42.628160
3503.791730	489082.499984	42.633165
3503.914292	489068.044758	42.638170
3503.762801	489050.745644	42.643175
3504.279690	489038.507432	42.648180
3503.973202	489044.178415	42.653184
3504.347924	489019.704739	42.658189
3503.842619	489004.386307	42.663194
3503.744031	489002.781108	42.668199
3504.074950	488996.751889	42.673204
3503.873159	488993.238199	42.678208
3504.014647	488974.069209	42.683213
3503.591691	488970.185250	42.688218
3503.713769	488981.056398	42.693223
3503.553551	488971.305846	42.698228
3503.604943	488961.268577	42.703232
3503.841439	488945.073055	42.708237
3503.573014	488937.213743	42.713242
3503.587254	488942.479491	42.718247
3504.009760	488935.777289	42.723252
3503.842762	488933.777675	42.728256
3503.976166	488924.335258	42.733261
3504.026739	488909.232803	42.738266
3504.193884	488902.267035	42.743271
3504.075945	488902.235127	42.748276
3503.968593	488884.270396	42.753280
3504.338166	488867.597896	42.758285
3504.012125	488869.473043	42.763290
3503.889105	488864.528594	42.768295
3503.910045	488836.311622	42.773300
3504.222852	488835.654445	42.778304
3504.149388	488827.511006	42.783309
3504.160662	488802.587966	42.788314
3503.922235	488808.552179	42.793319
3503.963553	488786.663561	42.798324
3503.897897	488778.670827	42.803329
3504.213313	488767.122778	42.808333
3504.174740	488767.280938	42.813338
3503.829156	488755.888016	42.818343
3504.183821	488729.644269	42.823348
3504.082880	488729.710981	42.828353
3504.313357	488716.960646	42.833357
3503.968741	488698.425400	42.838362
3503.938905	488681.562601	42.843367
3503.925782	488689.821302	42.848372
3503.620597	488669.557576	42.853377
3504.176806	488652.602120	42.858381
3503.859219	488649.866473	42.863386
3503.906620	488656.596013	42.868391
3503.791082	488637.163388	42.873396
3503.353269	488611.652583	42.878401
3503.541686	488612.180095	42.883405
3503.332015	488629.435595	42.888410
3503.392539	488622.587885	42.893415
3503.449764	488622.629596	42.898420
3503.391113	488628.616104	42.903425
3503.855029	488620.336983	42.908429
3503.549158	488625.704070	42.913434
3503.714622	488630.743386	42.918439
3503.667005	488607.399662	42.923444
3503.701009	488599.745676	42.928449
3503.826315	488592.482485	42.933453
3503.349499	488595.799796	42.938458
3503.607122	488598.038597	42.943463
3503.542420	488600.581615	42.948468
3503.464753	488607.634863	42.953473
3503.479207	488607.531374	42.958477
3503.550383	488607.874803	42.963482
3503.532309	488593.998637	42.968487
3503.415586	488575.731172	42.973492
3503.443383	488566.761155	42.978497
3503.570805	488565.120194	42.983501
3503.559724	488575.961968	42.988506
3503.706036	488576.597444	42.993511
3503.832458	488575.209911	42.998516
3503.420062	488588.749108	43.003521
3503.391385	488586.524978	43.008525
3503.533164	488588.984706	43.013530
3503.430906	488577.806485	43.018535
3503.566302	488557.776922	43.023540
3503.490809	488548.924530	43.028545
3503.724749	488541.644149	43.033549
3503.450877	488547.715355	43.038554
3503.390763	488559.071427	43.043559
3503.776351	488554.705005	43.048564
3503.793750	488561.489975	43.053569
3503.809580	488545.430299	43.058573
3503.673559	488533.700195	43.063578
3503.596520	488524.037573	43.068583
3503.773043	488514.841407	43.073588
3503.907661	488518.062086	43.078593
3503.700629	488507.356269	43.083597
3503.593932	488506.056233	43.088602
3503.568973	488495.676209	43.093607
3503.959045	488483.255070	43.098612
3503.740564	488489.266885	43.103617
3503.767162	488486.527465	43.108621
3503.882668	488495.373767	43.113626
3503.830839	488478.412956	43.118631
3503.839410	488461.999778	43.123636
3503.487237	488456.179668	43.128641
3503.781028	488449.649604	43.133645
3503.454226	488462.770128	43.138650
3503.157666	488467.274668	43.143655
3503.516533	488462.405907	43.148660
3503.692428	488469.925669	43.153665
3503.622024	488450.840297	43.158669
3503.775557	488434.860070	43.163674
3503.598974	488425.314440	43.168679
3503.549836	488428.868105	43.173684
3503.297258	488434.834672	43.178689
3503.653027	488436.551438	43.183693
3503.540664	488437.531731	43.188698
3503.463893	488445.749944	43.193703
3504.013126	488434.316699	43.198708
3503.742122	488407.664861	43.203713
3503.780074	488405.379523	43.208717
3503.792789	488402.237052	43.213722
3503.764056	488401.988425	43.218727
3503.421873	488401.839998	43.223732
3503.671764	488394.354422	43.228737
3504.107972	488375.087589	43.233741
3504.092923	488375.545960	43.238746
3503.613014	488377.242858	43.243751
3503.988538	488369.838723	43.248756
3503.861584	488354.459961	43.253761
3503.901133	488346.602379	43.258765
3503.985542	488342.030241	43.263770
3503.617431	488343.962743	43.268775
3503.808244	488320.682288	43.273780
3503.601692	488311.141338	43.278785
3503.663178	488305.357106	43.283789
3504.015713	488315.128464	43.288794
3503.632943	488307.742854	43.293799
3503.920583	488297.921166	43.298804
3503.892046	488274.675325	43.303809
3503.868055	488269.765722	43.308813
3503.876631	488276.045643	43.313818
3503.874517	488270.778000	43.318823
3503.891452	488246.106607	43.323828
3503.926481	488235.007793	43.328833
3503.850202	488233.652275	43.333837
3503.785900	488229.914092	43.338842
3503.717662	488240.967710	43.343847
3503.982469	488209.621324	43.348852
3503.408447	488216.449244	43.353857
3503.683080	488208.047899	43.358861
3503.591508	488204.010092	43.363866
3503.715930	488197.456058	43.368871
3503.972373	488192.654073	43.373876
3503.903252	488179.190911	43.378881
3503.876993	488169.520082	43.383885
3503.676213	488161.953685	43.388890
3503.623817	488169.813580	43.393895
3503.516799	488176.567699	43.398900
3503.275752	488160.649610	43.403905
3503.613021	488144.994681	43.408909
3503.335442	488142.809841	43.413914
3503.620458	488130.658353	43.418919
3503.712834	488122.842983	43.423924
3503.468757	488137.368996	43.428929
3503.770016	488139.702265	43.433933
3503.644349	488146.965891	43.438938
3503.660452	488140.580924	43.443943
3503.921944	488128.129222	43.448948
3503.562961	488116.231482	43.453953
3503.924528	488098.445164	43.458957
3503.881127	488098.350817	43.463962
3503.630082	488097.580119	43.468967
3504.111134	488093.603744	43.473972
3503.967210	488086.281605	43.478977
3504.121196	488068.983966	43.483981
3503.888963	488068.716846	43.488986
3503.761152	488056.529253	43.493991
3504.007742	488044.586404	43.498996
3503.950511	488036.440060	43.504001
3503.891616	488033.967365	43.509005
3503.910640	488025.049134	43.514010
3503.866182	487997.550427	43.519015
3504.155949	487995.225238	43.524020
3503.618279	488011.925277	43.529025
3503.763788	487995.490051	43.534029
3503.927684	487970.744417	43.539034
3503.750729	487963.022209	43.544039
3503.983505	487949.308544	43.549044
3504.102058	487957.951993	43.554049
3504.196976	487951.959748	43.559053
3504.217648	487931.086517	43.564058
3504.093806	487922.342786	43.569063
3504.156715	487895.485484	43.574068
3503.786128	487889.820076	43.579073
3503.977392	487872.161777	43.584077
3503.986216	487873.021632	43.589082
3503.764065	487869.460295	43.594087
3503.909893	487846.237026	43.599092
3503.795329	487848.028188	43.604097
3503.796912	487836.529182	43.609101
3503.726016	487827.017202	43.614106
3503.578163	487813.667537	43.619111
3503.930438	487808.698342	43.624116
3503.565160	487815.797344	43.629121
3503.770864	487808.419835	43.634125
3503.964747	487806.970929	43.639130
3503.469022	487797.323460	43.644135
3503.854696	487785.257153	43.649140
3503.665380	487786.806858	43.654145
3503.886146	487781.199915	43.659149
3503.736011	487786.441308	43.664154
3503.835321	487793.973444	43.669159
3503.855061	487760.638819	43.674164
3503.500981	487752.032714	43.679169
3503.797125	487749.503863	43.684173
3503.910554	487744.471091	43.689178
3503.643643	487750.085545	43.694183
3503.432878	487722.967321	43.699188
3503.578140	487717.625574	43.704193
3503.866495	487714.287452	43.709197
3503.738541	487711.774975	43.714202
3503.494569	487712.269545	43.719207
3503.918550	487713.418380	43.724212
3503.758686	487720.788886	43.729217
3503.749162	487697.741959	43.734221
3503.871957	487677.257557	43.739226
3503.554115	487683.741236	43.744231
3503.600873	487675.679613	43.749236
3503.421254	487686.497877	43.754241
3503.475027	487670.330152	43.759245
3503.586660	487676.847262	43.764250
3503.201125	487676.806991	43.769255
3503.518738	487682.734323	43.774260
3503.742793	487674.036801	43.779265
3503.553141	487652.132727	43.784269
3503.590761	487643.414003	43.789274
3503.444650	487662.737240	43.794279
3503.481106	487647.585358	43.799284
3503.655409	487652.471569	43.804289
3503.895885	487659.880132	43.809293
3503.895880	487644.480729	43.814298
3503.465846	487624.843497	43.819303
3503.895457	487612.415542	43.824308
3503.659982	487617.062595	43.829313
3503.873527	487609.785083	43.834317
3504.019179	487620.248033	43.839322
3503.682701	487598.215136	43.844327
3503.957570	487582.518954	43.849332
3503.570853	487582.377557	43.854337
3503.728055	487575.970097	43.859341
3503.802237	487573.020399	43.864346
3503.435314	487561.174222	43.869351
3503.609588	487546.557698	43.874356
3503.802377	487537.307833	43.879361
3503.359587	487548.978278	43.884365
3503.689683	487532.209537	43.889370
3503.770969	487543.087956	43.894375
3503.452434	487541.162801	43.899380
3503.472442	487567.957047	43.904385
3503.680436	487550.802371	43.909389
3503.539643	487531.169980	43.914394
3503.217701	487527.472382	43.919399
3503.580940	487518.499506	43.924404
3503.627487	487514.541034	43.929409
3503.634156	487518.035391	43.934413
3503.743231	487522.121440	43.939418
3503.561928	487522.251513	43.944423
3503.599427	487526.956754	43.949428
3503.817462	487521.704763	43.954433
3503.726347	487496.796195	43.959437
3504.100092	487481.996123	43.964442
3503.514176	487491.713612	43.969447
3503.727256	487483.878902	43.974452
3503.598877	487490.839266	43.979457
3503.611749	487472.955511	43.984461
3503.499687	487455.192800	43.989466
3503.606289	487450.414314	43.994471
3503.726876	487451.560464	43.999476
3503.192577	487460.003390	44.004481
3503.599284	487445.704647	44.009485
3503.623524	487447.169966	44.014490
3503.348719	487466.007176	44.019495
3503.309241	487456.186103	44.024500
3503.630325	487459.377490	44.029505
3503.513364	487455.343537	44.034509
3503.514884	487466.639861	44.039514
3503.538416	487440.801277	44.044519
3503.842334	487420.186657	44.049524
3503.640313	487428.374449	44.054529
3503.527065	487424.390560	44.059533
3503.776699	487424.857774	44.064538
3503.674396	487424.468792	44.069543
3503.799713	487419.079458	44.074548
3503.747039	487412.857088	44.079553
3503.594147	487397.684279	44.084557
3503.708400	487389.510553	44.089562
3503.421308	487402.372243	44.094567
3503.672516	487393.518331	44.099572
3503.230270	487407.518995	44.104577
3503.716410	487398.982550	44.109581
3503.859746	487404.127005	44.114586
3503.359850	487385.665677	44.119591
3503.454650	487362.196600	44.124596
3503.554780	487349.567269	44.129601
3503.801558	487353.732902	44.134605
3503.535070	487356.814550	44.139610
3503.454486	487365.135146	44.144615
3504.057012	487353.034292	44.149620
3503.605258	487361.261586	44.154625
3503.475277	487345.426573	44.159629
3503.787850	487325.570339	44.164634
3503.382357	487336.221874	44.169639
3503.216785	487337.109319	44.174644
3503.183209	487330.326675	44.179649
3503.693996	487331.107213	44.184653
3503.953063	487334.308423	44.189658
3503.546602	487333.815544	44.194663
3503.846294	487330.323593	44.199668
3503.338692	487317.233072	44.204673
3503.399165	487298.480457	44.209677
3503.693423	487291.240724	44.214682
3503.496007	487296.236439	44.219687
3503.536617	487301.903730	44.224692
3503.712546	487296.759648	44.229697
3503.627205	487303.459991	44.234701
3503.685333	487307.807425	44.239706
3503.315559	487304.066686	44.244711
3503.809390	487289.551427	44.249716
3503.635491	487279.092966	44.254721
3503.321646	487273.215776	44.259725
3503.868716	487260.009168	44.264730
3503.377660	487266.621681	44.269735
3503.816767	487263.766226	44.274740
3503.647240	487261.817490	44.279745
3503.415322	487268.642329	44.284749
3503.546243	487265.480986	44.289754
3503.204608	487236.761722	44.294759
3503.601466	487219.728868	44.299764
3503.512561	487226.784404	44.304769
3503.066645	487225.537898	44.309773
3503.659120	487229.294315	44.314778
3503.243886	487234.527104	44.319783
3503.254826	487241.009622	44.324788
3503.118243	487234.547170	44.329793
3503.567302	487233.007229	44.334797
3503.380186	487228.072484	44.339802
3503.392488	487247.624388	44.344807
3503.959293	487238.568548	44.349812
3503.708045	487239.368225	44.354817
3503.811764	487235.805918	44.359821
3503.683596	487220.375773	44.364826
3503.557696	487209.707058	44.369831
3503.349218	487199.304677	44.374836
3503.536883	487200.338924	44.379841
3503.354973	487191.300091	44.384845
3503.573008	487197.395287	44.389850
3503.371801	487200.567957	44.394855
3503.895189	487190.455150	44.399860
3503.635923	487200.881017	44.404865
3503.849901	487205.558442	44.409869
3504.082223	487169.200393	44.414874
3503.499443	487171.014968	44.419879
3503.329400	487169.218277	44.424884
3503.435077	487167.732607	44.429889
3503.568420	487155.857762	44.434893
3503.837679	487175.774385	44.439898
3503.496420	487173.599496	44.444903
3503.689435	487142.566650	44.449908
3503.493571	487140.166146	44.454913
3503.660064	487133.554440	44.459917
3503.745708	487139.721237	44.464922
3503.543791	487146.490720	44.469927
3503.932621	487137.209676	44.474932
3503.989994	487137.656629	44.479937
3503.865979	487107.737647	44.484941
3503.781655	487107.852394	44.489946
3503.346560	487106.604169	44.494951
3503.666852	487107.212196	44.499956
3503.682574	487112.123612	44.504961
3503.340927	487099.817233	44.509965
3503.392886	487083.244036	44.514970
3503.626904	487077.736108	44.519975
3503.692618	487066.175843	44.524980
3503.469419	487074.924370	44.529985
3503.721387	487074.378068	44.534989
3503.953468	487064.868476	44.539994
3503.747593	487070.068218	44.544999
3503.957385	487065.323984	44.550004
3503.911997	487049.323380	44.555009
3503.421015	487035.014248	44.560013
3503.816572	487036.978145	44.565018
3503.581299	487046.995040	44.570023
3503.748667	487030.859477	44.575028
3503.267391	487028.959993	44.580033
3503.434558	487013.128394	44.585037
3503.467627	486994.278497	44.590042
3503.622095	487013.453563	44.595047
3503.558732	486995.682727	44.600052
3503.638537	486999.976147	44.605057
3503.557581	487004.446949	44.610061
3503.754460	487009.177784	44.615066
3503.509141	487015.498251	44.620071
3503.638408	487008.537780	44.625076
3503.428260	486993.728306	44.630081
3503.706632	486969.571176	44.635085
3504.022880	486969.369318	44.640090
3503.174323	486970.314076	44.645095
3503.365863	486966.737838	44.650100
3503.578963	486969.591768	44.655105
3503.443709	486976.249458	44.660109
3503.524265	486980.036182	44.665114
3503.283226	486979.871753	44.670119
3503.700091	486976.665165	44.675124
3503.668582	486969.274170	44.680129
3503.554448	486960.325830	44.685133
3503.746274	486950.012014	44.690138
3503.743751	486942.211162	44.695143
3503.585619	486943.806663	44.700148
3503.648223	486936.958019	44.705153
3503.337111	486936.399399	44.710157
3503.366650	486936.141542	44.715162
3503.823499	486941.084593	44.720167
3503.630765	486920.699911	44.725172
3503.313032	486906.211324	44.730177
3503.550536	486909.922596	44.735181
3503.668488	486906.864561	44.740186
3503.655803	486913.198949	44.745191
3503.413649	486907.158339	44.750196
3503.685779	486918.310898	44.755201
3503.714526	486915.469597	44.760205
3503.718427	486896.674872	44.765210
3503.606180	486879.823504	44.770215
3503.725283	486875.650799	44.775220
3503.851633	486869.957197	44.780225
3503.735184	486879.651448	44.785229
3503.894226	486876.130988	44.790234
3503.497823	486862.921260	44.795239
3503.788139	486842.105534	44.800244
3503.747020	486836.033125	44.805249
3503.184612	486841.035992	44.810253
3503.530530	486840.018908	44.815258
3503.547844	486853.238119	44.820263
3503.634852	486841.573036	44.825268
3503.535956	486837.282805	44.830273
3503.757590	486848.646020	44.835277
3503.718243	486815.926986	44.840282
3503.681386	486815.375671	44.845287
3503.423822	486813.136854	44.850292
3503.359183	486811.171492	44.855297
3503.354077	486804.130869	44.860301
3503.928448	486803.786893	44.865306
3503.531069	486818.540772	44.870311
3503.964985	486814.723561	44.875316
3503.846673	486799.494153	44.880321
3503.529370	486779.939548	44.885325
3503.817202	486772.346024	44.890330
3503.556703	486783.380217	44.895335
3503.823086	486783.692825	44.900340
3503.511187	486784.958033	44.905345
3503.315571	486777.136976	44.910349
3503.578687	486772.941485	44.915354
3503.276205	486776.332867	44.920359
3503.338380	486756.262328	44.925364
3503.487440	486755.884260	44.930369
3503.217525	486764.792288	44.935373
3503.570207	486749.741686	44.940378
3503.535169	486754.002655	44.945383
3503.766775	486753.408904	44.950388
3503.825074	486756.236677	44.955393
3503.730488	486764.965016	44.960397
3503.940526	486749.126423	44.965402
3503.530692	486728.522558	44.970407
3503.971571	486722.981832	44.975412
3503.827958	486724.017810	44.980417
3503.417976	486726.970264	44.985421
3503.776330	486714.046404	44.990426
3503.362924	486708.944657	44.995431
3503.701101	486683.713880	45.000436
3503.781271	486694.390323	45.005441
3503.752539	486675.853834	45.010445
3504.076155	486684.668084	45.015450
3503.517295	486688.707911	45.020455
3503.814728	486670.981062	45.025460
3503.881731	486651.162945	45.030465
3503.729142	486646.881158	45.035469
3503.962271	486637.675142	45.040474
3503.755241	486645.256153	45.045479
3503.760819	486634.009086	45.050484
3503.656988	486626.477413	45.055489
3503.442627	486618.051345	45.060493
3503.702950	486600.431615	45.065498
3503.410465	486606.962308	45.070503
3503.472144	486597.732714	45.075508
3503.799531	486609.028697	45.080513
3503.457775	486612.021043	45.085517
3503.858885	486598.634416	45.090522
3503.615227	486576.585668	45.095527
3503.940197	486577.040996	45.100532
3503.906357	486569.396920	45.105537
3503.882095	486566.158672	45.110541
3503.896859	486550.452099	45.115546
3503.872640	486537.689910	45.120551
3503.628006	486525.317166	45.125556
3503.813582	486523.210907	45.130561
3503.644343	486531.545878	45.135565
3503.783361	486520.530949	45.140570
3503.700477	486505.852958	45.145575
3503.914831	486494.826107	45.150580
3503.547191	486496.049485	45.155585
3503.561552	486493.565010	45.160589
3503.873437	486493.667794	45.165594
3503.567299	486482.419250	45.170599
3503.715546	486457.420834	45.175604
3503.607873	486454.449049	45.180609
3503.621855	486456.321342	45.185613
3503.806528	486449.909164	45.190618
3503.923652	486456.932418	45.195623
3503.765257	486439.378724	45.200628
3503.556802	486432.724723	45.205633
3503.402503	486420.945547	45.210637
3503.777525	486413.034144	45.215642
3503.649838	486422.730402	45.220647
3503.568465	486421.527538	45.225652
3503.405662	486420.742822	45.230657
3503.770742	486431.678335	45.235661
3503.427128	486408.480024	45.240666
3503.199673	486403.500782	45.245671
3503.805781	486383.445197	45.250676
3503.415726	486392.777663	45.255681
3503.619895	486392.137580	45.260685
3503.827180	486384.252677	45.265690
3503.466975	486394.390979	45.270695
3503.452181	486386.895798	45.275700
3503.519392	486393.876304	45.280705
3503.750410	486389.128548	45.285709
3503.602800	486372.890239	45.290714
3503.246974	486365.043676	45.295719
3503.705468	486341.009264	45.300724
3503.334122	486352.263864	45.305729
3503.123414	486359.744248	45.310733
3503.484402	486345.350593	45.315738
3503.283712	486348.371342	45.320743
3503.285165	486359.769651	45.325748
3503.447162	486365.012755	45.330753
3503.737877	486356.202780	45.335757
3503.701586	486356.056640	45.340762
3503.415494	486368.665567	45.345767
3503.541018	486360.438961	45.350772
3503.512475	486358.011910	45.355777
3503.288378	486372.536103	45.360781
3503.769330	486354.830615	45.365786
3503.970434	486331.090173	45.370791
3503.770232	486320.128747	45.375796
3503.920279	486330.237091	45.380801
3503.482041	486328.077433	45.385805
3503.658159	486320.754689	45.390810
3503.702977	486309.957167	45.395815
3503.535566	486289.669131	45.400820
3503.616649	486289.504438	45.405825
3503.189681	486288.558831	45.410829
3503.546233	486288.451917	45.415834
3503.347718	486293.853345	45.420839
3503.408848	486290.500234	45.425844
3503.472197	486297.025447	45.430849
3503.359586	486297.752588	45.435853
3503.679627	486298.107383	45.440858
3503.506451	486297.273641	45.445863
3503.712946	486292.479077	45.450868
3503.637353	486278.103720	45.455873
3503.165770	486269.718156	45.460877
3503.784796	486255.942227	45.465882
3503.534854	486260.439913	45.470887
3503.468764	486271.393010	45.475892
3503.702493	486255.600925	45.480897
3503.711115	486269.379172	45.485901
3503.401706	486267.503104	45.490906
3503.488843	486275.189743	45.495911
3503.434904	486251.337535	45.500916
3503.809968	486228.228049	45.505921
3503.317063	486230.079164	45.510925
3503.687309	486221.205896	45.515930
3503.382085	486223.078006	45.520935
3503.438503	486225.602194	45.525940
3503.441798	486232.947482	45.530945
3503.459083	486226.663008	45.535949
3503.429682	486227.427659	45.540954
3503.132591	486238.417288	45.545959
3503.323896	486229.521648	45.550964
3503.761935	486227.020831	45.555969
3503.385597	486237.009786	45.560973
3503.816308	486235.523329	45.565978
3503.890888	486214.943663	45.570983
3503.531354	486211.454390	45.575988
3503.689633	486206.566105	45.580993
3503.260353	486204.708978	45.585997
3503.766399	486203.210611	45.591002
3503.244794	486210.081614	45.596007
3503.523386	486201.982726	45.601012
3503.693696	486199.676204	45.606017
3503.132447	486213.645887	45.611021
3503.897667	486211.042693	45.616026
3503.587582	486188.750697	45.621031
3503.405741	486166.995667	45.626036
3503.554422	486165.300483	45.631041
3503.132120	486174.942113	45.636045
3503.557396	486175.381597	45.641050
3503.336480	486183.826208	45.646055
3503.667334	486175.364427	45.651060
3503.777068	486169.622583	45.656065
3503.484717	486175.950760	45.661069
3503.623788	486175.574259	45.666074
3503.449078	486146.168390	45.671079
3503.122866	486152.096644	45.676084
3503.305259	486144.722181	45.681089
3503.350770	486142.334058	45.686093
3503.235470	486133.892119	45.691098
3503.237886	486146.354268	45.696103
3503.376992	486133.312692	45.701108
3503.184186	486145.197776	45.706113
3503.190789	486154.467661	45.711117
3503.254507	486142.147251	45.716122
3503.226547	486163.429075	45.721127
3503.389614	486191.013200	45.726132
3503.716322	486164.871672	45.731137
3503.374959	486152.767278	45.736141
3503.242601	486160.083375	45.741146
3503.231239	486163.783470	45.746151
3503.329929	486141.984070	45.751156
3503.436571	486158.583878	45.756161
3503.197462	486153.606413	45.761165
3503.514379	486145.450783	45.766170
3503.703165	486162.442886	45.771175
3503.542155	486175.336129	45.776180
3503.760986	486164.460361	45.781185
3503.326528	486156.575481	45.786189
3503.679434	486174.605497	45.791194
3503.449502	486156.353609	45.796199
3503.089540	486169.278303	45.801204
3503.294620	486157.796783	45.806209
3502.897419	486175.438760	45.811213
3503.383011	486158.897542	45.816218
3503.231121	486173.106512	45.821223
3503.377216	486179.112084	45.826228
3503.642768	486166.810447	45.831233
3503.181971	486171.088182	45.836237
3503.855059	486173.768205	45.841242
3503.632759	486123.143193	45.846247
3503.388202	486143.446069	45.851252
3503.786124	486120.383500	45.856257
3503.136568	486117.446654	45.861261
3503.369504	486123.033235	45.866266
3503.204116	486135.623235	45.871271
3503.719958	486131.894262	45.876276
3503.383224	486137.368241	45.881281
3503.036610	486145.832736	45.886285
3503.502113	486133.246172	45.891290
3503.290410	486145.387543	45.896295
3503.105403	486148.608486	45.901300
3503.441750	486146.326373	45.906305
3503.252784	486142.303524	45.911309
3503.531290	486158.926827	45.916314
3503.591526	486136.120294	45.921319
3503.501488	486149.306298	45.926324
3503.676518	486149.937319	45.931329
3503.397357	486136.911198	45.936333
3503.655212	486120.507265	45.941338
3503.407553	486124.700661	45.946343
3503.123430	486124.239070	45.951348
3503.572022	486122.141854	45.956353
3503.200220	486135.980328	45.961357
3503.135502	486126.567845	45.966362
3503.377532	486136.661752	45.971367
3503.575256	486130.652688	45.976372
3503.411198	486114.112797	45.981377
3503.357959	486125.773191	45.986381
3503.792646	486125.197983	45.991386
3503.395209	486119.232327	45.996391
3503.209983	486147.378171	46.001396
3503.605636	486132.168313	46.006401
3503.559898	486134.354038	46.011405
3503.694617	486130.482665	46.016410
3503.589388	486116.871775	46.021415
3503.632730	486103.895977	46.026420
3503.751878	486071.910527	46.031425
3503.339303	486103.385299	46.036429
3503.753095	486090.958862	46.041434
3503.347734	486097.000964	46.046439
3503.372769	486099.783432	46.051444
3503.441245	486094.757333	46.056449
3503.196414	486094.036229	46.061453
3503.336453	486110.478819	46.066458
3503.543557	486113.587128	46.071463
3503.656415	486092.393356	46.076468
3503.947436	486093.208686	46.081473
3503.536586	486073.516164	46.086477
3503.652753	486047.306435	46.091482
3503.982634	486065.542835	46.096487
3503.486154	486071.548687	46.101492
3503.784155	486052.959951	46.106497
3503.800437	486048.195393	46.111501
3503.788473	486028.845060	46.116506
3503.527103	486018.501056	46.121511
3503.415230	486035.135511	46.126516
3503.908438	486022.189871	46.131521
3503.230632	486029.896197	46.136525
3503.638073	486020.155728	46.141530
3503.375261	486007.582881	46.146535
3503.473151	485998.347275	46.151540
3503.858199	485989.116937	46.156545
3503.374574	486000.237506	46.161549
3503.570435	485993.266142	46.166554
3503.786749	485995.663765	46.171559
3503.639294	485995.585854	46.176564
3503.904880	485988.907431	46.181569
3503.425377	485972.974546	46.186573
3503.751382	485977.533244	46.191578
3503.766068	485960.053075	46.196583
3503.694290	485951.249552	46.201588
3503.758336	485940.955392	46.206593
3503.704031	485958.644689	46.211597
3503.602912	485945.742279	46.216602
3503.454282	485937.356183	46.221607
3503.468470	485919.369447	46.226612
3503.573102	485921.987376	46.231617
3503.431758	485927.785157	46.236621
3503.823884	485911.613127	46.241626
3503.718245	485919.431701	46.246631
3503.313751	485931.097072	46.251636
3503.768615	485918.866676	46.256641
3503.424746	485921.910123	46.261645
3503.684562	485900.642250	46.266650
3503.554282	485890.936049	46.271655
3503.489059	485883.549964	46.276660
3503.293178	485881.807896	46.281665
3503.109625	485889.132188	46.286669
3503.279751	485880.797005	46.291674
3503.397328	485886.503211	46.296679
3503.045503	485888.990650	46.301684
3503.666465	485890.564412	46.306689
3503.169153	485890.896427	46.311693
3503.319491	485886.059978	46.316698
3503.123994	485895.716559	46.321703
3503.280580	485900.960646	46.326708
3503.790968	485888.468150	46.331713
3503.351528	485888.132425	46.336717
3503.850944	485887.850945	46.341722
3503.693114	485894.664560	46.346727
3503.459111	485891.408690	46.351732
3503.697881	485888.787345	46.356737
3503.627199	485880.844851	46.361741
3503.655446	485866.148806	46.366746
3503.279504	485878.063001	46.371751
3503.443772	485862.838844	46.376756
3503.763836	485872.616589	46.381761
3503.693158	485869.081595	46.386765
3503.631217	485866.811744	46.391770
3503.743708	485857.523102	46.396775
3503.783415	485834.922101	46.401780
3503.619390	485836.619946	46.406785
3503.161956	485829.498478	46.411789
3503.713866	485822.825401	46.416794
3503.294231	485825.272905	46.421799
3503.247159	485822.544749	46.426804
3503.600945	485817.169514	46.431809
3503.525201	485833.291821	46.436813
3503.725804	485821.658824	46.441818
3503.612612	485821.372852	46.446823
3503.539334	485824.930815	46.451828
3503.609967	485798.981250	46.456833
3503.420083	485784.370282	46.461837
3503.556858	485795.038279	46.466842
3503.421373	485795.110458	46.471847
3503.161540	485795.050309	46.476852
3503.595537	485790.472967	46.481857
3503.247890	485793.567692	46.486861
3503.459738	485785.073889	46.491866
3503.651087	485801.964584	46.496871
3503.622562	485793.204812	46.501876
3503.758175	485808.787120	46.506881
3503.403297	485771.759320	46.511885
3503.652612	485760.726522	46.516890
3503.696763	485762.290146	46.521895
3503.525960	485770.473709	46.526900
3503.655832	485755.660194	46.531905
3503.455180	485763.037898	46.536909
3503.585960	485762.612040	46.541914
3503.525744	485768.447706	46.546919
3503.325535	485772.633677	46.551924
3503.653880	485767.971707	46.556929
3503.676721	485763.358025	46.561933
3503.640698	485738.843753	46.566938
3503.859507	485729.892874	46.571943
3503.689412	485752.768120	46.576948
3504.146751	485736.788281	46.581953
3503.803093	485706.091248	46.586957
3503.638761	485722.126327	46.591962
3503.848695	485707.705411	46.596967
3503.880915	485695.187048	46.601972
3503.884057	485697.719727	46.606977
3503.485068	485682.128504	46.611981
3503.865434	485661.702558	46.616986
3503.611277	485673.850938	46.621991
3503.608019	485667.164236	46.626996
3503.737040	485658.683470	46.632001
3503.531115	485664.592860	46.637005
3503.734394	485660.254602	46.642010
3503.832270	485632.122060	46.647015
3503.702998	485619.629173	46.652020
3503.866351	485622.187200	46.657025
3503.592878	485623.243762	46.662029
3503.878222	485606.176445	46.667034
3503.788394	485598.236861	46.672039
3502.966233	485598.924197	46.677044
3503.201807	485577.811785	46.682049
3503.039730	485585.386107	46.687053
3503.397476	485604.277143	46.692058
3503.386162	485602.860507	46.697063
3503.244430	485598.526107	46.702068
3503.575993	485592.141088	46.707073
3503.313976	485604.848032	46.712077
3503.278476	485595.937288	46.717082
3503.677893	485591.416027	46.722087
3503.645642	485593.346373	46.727092
3504.000842	485594.658198	46.732097
3503.599601	485591.935328	46.737101
3503.615873	485590.970287	46.742106
3503.415666	485588.215640	46.747111
3503.507953	485558.462698	46.752116
3503.771297	485549.504696	46.757121
3503.600780	485550.950283	46.762125
3503.649715	485538.327852	46.767130
3503.554077	485548.019485	46.772135
3503.537516	485553.291036	46.777140
3503.743075	485561.263214	46.782145
3503.612655	485554.292602	46.787149
3504.003412	485527.582806	46.792154
3503.878325	485524.512305	46.797159
3503.524016	485516.259859	46.802164
3503.927927	485512.497798	46.807169
3503.687753	485519.223237	46.812173
3503.493924	485486.627679	46.817178
3503.727430	485473.064116	46.822183
3503.606462	485479.517417	46.827188
3503.846273	485461.443929	46.832193
3503.424960	485468.957948	46.837197
3503.523453	485470.158372	46.842202
3503.434203	485475.846729	46.847207
3503.342325	485480.471599	46.852212
3503.569041	485471.519350	46.857217
3503.483821	485453.446568	46.862221
3503.667175	485435.787276	46.867226
3503.770909	485438.506738	46.872231
3503.387407	485444.849561	46.877236
3503.260898	485444.565688	46.882241
3503.229959	485453.335223	46.887245
3503.778136	485441.596397	46.892250
3503.661352	485446.123887	46.897255
3503.447783	485447.221652	46.902260
3503.935487	485437.569527	46.907265
3503.206305	485439.255413	46.912269
3503.481832	485413.728902	46.917274
3503.691730	485406.299147	46.922279
3503.643442	485397.846292	46.927284
3503.696144	485401.587070	46.932289
3503.506264	485397.057585	46.937293
3503.574803	485417.159750	46.942298
3503.511880	485403.136371	46.947303
3503.493265	485416.564899	46.952308
3503.622631	485403.777680	46.957313
3503.343267	485380.973268	46.962317
3503.666346	485377.983892	46.967322
3503.704014	485369.821412	46.972327
3503.572658	485364.269424	46.977332
3503.362779	485367.342440	46.982337
3503.446660	485378.069691	46.987341
3503.440584	485361.149545	46.992346
3503.796459	485358.914917	46.997351
3503.570378	485368.880570	47.002356
3503.807659	485356.532223	47.007361
3503.471504	485340.322843	47.012365
3503.341230	485335.023987	47.017370
3503.395247	485338.663244	47.022375
3503.388024	485332.939638	47.027380
3503.395733	485327.922945	47.032385
3503.413506	485331.618594	47.037389
3503.357845	485322.356273	47.042394
3503.519690	485339.809324	47.047399
3503.421236	485326.652765	47.052404
3503.758827	485325.636922	47.057409
3503.443924	485330.195754	47.062413
3503.386016	485326.861291	47.067418
3503.521032	485335.148688	47.072423
3503.399256	485327.062054	47.077428
3503.688816	485296.669578	47.082433
3503.477052	485300.705490	47.087437
3503.577168	485293.141056	47.092442
3503.522685	485309.209779	47.097447
3502.974036	485313.552249	47.102452
3503.335238	485310.810149	47.107457
3503.276467	485300.585723	47.112461
3503.276447	485302.865641	47.117466
3503.351851	485308.781334	47.122471
3503.450217	485301.977118	47.127476
3503.360056	485300.218285	47.132481
3503.136989	485315.705699	47.137485
3503.564586	485313.257080	47.142490
3503.578615	485298.664174	47.147495
3503.060261	485305.028357	47.152500
3503.356505	485312.429017	47.157505
3503.453330	485314.896276	47.162509
3503.379405	485317.542511	47.167514
3503.389252	485321.898027	47.172519
3503.459682	485314.540944	47.177524
3503.489618	485309.267420	47.182529
3503.247346	485328.000257	47.187533
3503.407569	485330.254843	47.192538
3503.643255	485310.864643	47.197543
3503.183344	485303.084759	47.202548
3503.362544	485282.892860	47.207553
3503.346625	485278.994464	47.212557
3503.340502	485278.539572	47.217562
3503.000330	485282.291809	47.222567
3503.247761	485283.570028	47.227572
3503.445334	485277.155422	47.232577
3503.393660	485288.968063	47.237581
3503.533154	485291.732555	47.242586
3503.564541	485279.214054	47.247591
3503.471000	485295.187636	47.252596
3503.873007	485281.698629	47.257601
3503.554447	485289.905752	47.262605
3503.727399	485300.618967	47.267610
3503.761495	485278.322175	47.272615
3503.614322	485267.098452	47.277620
3503.686559	485257.005283	47.282625
3503.234816	485251.351915	47.287629
3503.570188	485251.805634	47.292634
3503.403822	485251.376070	47.297639
3502.969300	485273.229767	47.302644
3503.417003	485249.145038	47.307649
3503.333815	485260.152076	47.312653
3503.710452	485263.031076	47.317658
3503.855427	485258.752606	47.322663
3503.641060	485271.148262	47.327668
3503.533738	485244.314152	47.332673
3503.412771	485226.804097	47.337677
3503.284689	485223.227394	47.342682
3503.768022	485216.412961	47.347687
3503.519164	485221.164031	47.352692
3503.360456	485214.805720	47.357697
3502.969030	485221.808483	47.362701
3503.209329	485219.389457	47.367706
3503.635354	485219.322221	47.372711
3502.990144	485223.679974	47.377716
3503.213559	485215.944034	47.382721
3503.162486	485221.170468	47.387725
3503.193457	485238.289658	47.392730
3503.510670	485225.269979	47.397735
3503.142960	485234.802123	47.402740
3503.358576	485230.056517	47.407745
3503.367802	485235.982694	47.412749
3503.254956	485225.716112	47.417754
3503.317729	485229.961958	47.422759
3503.089928	485236.229575	47.427764
3503.300244	485227.533119	47.432769
3503.280104	485232.552010	47.437773
3503.249537	485239.497728	47.442778
3503.649518	485224.033159	47.447783
3503.338882	485238.521222	47.452788
3503.680315	485238.619345	47.457793
3503.235014	485245.275977	47.462797
3503.374403	485238.110615	47.467802
3503.345174	485248.703829	47.472807
3503.270643	485242.180234	47.477812
3503.455418	485234.349083	47.482817
3503.557382	485244.161622	47.487821
3503.313486	485248.962563	47.492826
3503.489141	485245.489843	47.497831
3503.162431	485239.563396	47.502836
3503.477755	485247.062391	47.507841
3503.592558	485250.033442	47.512845
3503.647287	485231.786343	47.517850
3503.397149	485223.973269	47.522855
3503.248491	485225.719401	47.527860
3503.560495	485218.070784	47.532865
3503.697926	485214.502775	47.537869
3503.297349	485218.973850	47.542874
3503.547652	485205.812746	47.547879
3503.581974	485215.332015	47.552884
3503.470099	485220.618723	47.557889
3503.629962	485226.571754	47.562893
3503.562108	485213.714258	47.567898
3503.832264	485209.567979	47.572903
3503.622353	485188.728208	47.577908
3503.581394	485184.935076	47.582913
3503.520643	485185.907375	47.587917
3503.424364	485175.131519	47.592922
3503.465970	485181.812536	47.597927
3503.327595	485185.634221	47.602932
3503.236676	485186.915265	47.607937
3503.253223	485194.360180	47.612941
3503.524210	485184.539534	47.617946
3503.325287	485187.408196	47.622951
3503.218716	485195.379199	47.627956
3503.466246	485185.156959	47.632961
3503.339569	485185.126422	47.637965
3503.016339	485190.953173	47.642970
3503.391086	485179.038949	47.647975
3503.454845	485188.097615	47.652980
3503.592926	485184.174857	47.657985
3503.410585	485192.816455	47.662989
3503.268099	485190.255278	47.667994
3503.511736	485190.976813	47.672999
3503.035682	485181.172919	47.678004
3503.365989	485182.995336	47.683009
3503.399344	485192.717421	47.688013
3503.058635	485180.257670	47.693018
3503.168329	485188.447807	47.698023
3503.263022	485208.647381	47.703028
3503.162151	485208.612765	47.708033
3503.218048	485212.555725	47.713037
3503.739449	485202.290205	47.718042
3503.586664	485180.022838	47.723047
3503.410858	485173.717878	47.728052
3503.605388	485160.565559	47.733057
3503.827925	485163.620921	47.738061
3503.346843	485159.542712	47.743066
3503.472829	485170.162098	47.748071
3503.450972	485170.216318	47.753076
3503.317457	485168.565652	47.758081
3503.433750	485162.974461	47.763085
3503.528256	485167.063316	47.768090
3503.772725	485167.784720	47.773095
3503.432565	485155.122214	47.778100
3503.382942	485130.406666	47.783105
3503.163186	485129.529572	47.788109
3503.370681	485117.540421	47.793114
3503.704678	485121.338117	47.798119
3503.591186	485121.508147	47.803124
3503.400888	485118.245237	47.808129
3503.340944	485122.409178	47.813133
3503.470002	485123.959433	47.818138
3503.658882	485130.718515	47.823143
3503.808830	485139.712917	47.828148
3503.509100	485136.416644	47.833153
3503.547633	485116.854761	47.838157
3503.387922	485106.342208	47.843162
3503.549515	485095.170907	47.848167
3503.425101	485089.820394	47.853172
3503.499423	485089.808750	47.858177
3503.269664	485099.673796	47.863181
3503.769437	485101.368109	47.868186
3503.620254	485094.450959	47.873191
3503.351103	485104.727534	47.878196
3503.501662	485097.661680	47.883201
3503.211718	485101.608665	47.888205
3503.059898	485097.427735	47.893210
3503.257242	485107.123943	47.898215
3503.262536	485108.288458	47.903220
3503.471592	485097.717612	47.908225
3503.527982	485116.048805	47.913229
3503.301726	485117.452572	47.918234
3503.599792	485098.761581	47.923239
3503.309102	485113.297248	47.928244
3503.400944	485093.676252	47.933249
3503.308166	485081.379900	47.938253
3503.156772	485073.399168	47.943258
3503.417114	485089.164995	47.948263
3503.023770	485091.507109	47.953268
3503.417401	485101.425608	47.958273
3503.502380	485077.701977	47.963277
3503.427852	485069.911746	47.968282
3503.561917	485073.335748	47.973287
3503.450124	485084.803374	47.978292
3503.590144	485066.593301	47.983297
3503.605885	485076.520881	47.988301
3503.611461	485077.888006	47.993306
3503.592022	485064.820105	47.998311
3503.446248	485071.024147	48.003316
3503.545284	485074.555012	48.008321
3503.336564	485073.980149	48.013325
3503.182793	485070.863447	48.018330
3503.647309	485059.137613	48.023335
3503.564145	485049.930171	48.028340
3503.642034	485042.622469	48.033345
3503.784441	485039.712262	48.038349
3503.660477	485034.311000	48.043354
3503.710540	485040.788076	48.048359
3503.476472	485043.307672	48.053364
3503.526285	485026.834367	48.058369
3503.424609	485010.992952	48.063373
3503.445629	485002.832948	48.068378
3503.793498	484999.484953	48.073383
3503.465359	485004.552587	48.078388
3503.324828	485005.334852	48.083393
3503.705564	485007.047988	48.088397
3503.264186	484992.628161	48.093402
3503.418924	485003.192431	48.098407
3503.332825	485001.584918	48.103412
3503.542320	485000.437316	48.108417
3503.497817	485002.015015	48.113421
3503.141431	485010.785530	48.118426
3503.364861	484997.983174	48.123431
3503.519834	485008.192762	48.128436
3503.322884	485008.072006	48.133441
3503.643003	485003.259163	48.138445
3503.562837	484981.942691	48.143450
3503.618518	484968.558871	48.148455
3503.101023	484977.405530	48.153460
3503.061306	484981.819621	48.158465
3503.400843	484975.331812	48.163469
3503.172013	484956.673304	48.168474
3503.747446	484972.997383	48.173479
3503.835006	484978.151306	48.178484
3503.687944	484957.301351	48.183489
3503.579352	484979.053199	48.188493
3503.573235	484959.042243	48.193498
3503.858376	484966.242138	48.198503
3503.755423	484960.533553	48.203508
3503.745962	484945.589450	48.208513
3503.628559	484927.723916	48.213517
3503.292330	484932.438202	48.218522
3503.744687	484928.415055	48.223527
3503.597219	484933.403486	48.228532
3503.542767	484932.398927	48.233537
3503.477929	484906.773555	48.238541
3503.397224	484887.534267	48.243546
3503.506676	484887.263752	48.248551
3503.391562	484901.873153	48.253556
3503.252734	484907.012216	48.258561
3503.416742	484889.659465	48.263565
3503.272467	484901.790960	48.268570
3503.672284	484896.661513	48.273575
3503.309765	484895.806973	48.278580
3503.339644	484881.160583	48.283585
3503.473867	484910.828309	48.288589
3503.571183	484892.371504	48.293594
3503.750035	484883.426549	48.298599
3503.662120	484905.377866	48.303604
3503.857288	484878.647425	48.308609
3503.870879	484865.979478	48.313613
3503.512445	484874.699714	48.318618
3503.897141	484865.367569	48.323623
3503.682226	484859.676652	48.328628
3503.547863	484846.069468	48.333633
3503.407440	484844.166547	48.338637
3503.402833	484837.631762	48.343642
3503.683992	484828.163974	48.348647
3503.287158	484828.226802	48.353652
3503.341263	484824.165255	48.358657
3503.439678	484823.592501	48.363661
3503.309731	484825.994339	48.368666
3503.867659	484827.223511	48.373671
3503.748850	484824.101242	48.378676
3503.585086	484827.927010	48.383681
3503.603658	484831.673293	48.388685
3503.561508	484813.289121	48.393690
3503.786269	484795.318717	48.398695
3503.528369	484789.178599	48.403700
3503.350215	484788.953542	48.408705
3503.290260	484791.242994	48.413709
3503.301478	484799.195542	48.418714
3503.781460	484781.691422	48.423719
3503.621078	484790.481719	48.428724
3503.535600	484787.303512	48.433729
3503.282543	484793.372610	48.438733
3503.235598	484798.649169	48.443738
3503.725046	484789.503085	48.448743
3503.352007	484788.194229	48.453748
3503.373160	484762.808393	48.458753
3503.601254	484749.245178	48.463757
3503.673706	484745.130050	48.468762
3503.489448	484749.111065	48.473767
3503.402423	484750.796833	48.478772
3503.526215	484742.671139	48.483777
3503.615536	484748.939452	48.488781
3503.358500	484755.363838	48.493786
3503.453395	484751.295828	48.498791
3503.307083	484759.577276	48.503796
3503.144961	484759.653668	48.508801
3503.538305	484759.287615	48.513805
3503.163383	484764.616025	48.518810
3503.511187	484754.428372	48.523815
3503.333209	484762.765487	48.528820
3503.503737	484765.170503	48.533825
3503.687407	484747.662525	48.538829
3503.710489	484734.486351	48.543834
3503.910400	484720.116947	48.548839
3503.609934	484717.935326	48.553844
3503.660945	484724.868335	48.558849
3503.744111	484717.762332	48.563853
3503.708143	484709.560548	48.568858
3503.732663	484694.205567	48.573863
3503.613181	484693.363266	48.578868
3503.877020	484697.526784	48.583873
3503.663867	484698.624524	48.588877
3503.423631	484698.510608	48.593882
3503.413237	484689.392820	48.598887
3503.384291	484700.188946	48.603892
3503.490308	484695.663190	48.608897
3503.710229	484664.216781	48.613901
3503.530570	484660.597462	48.618906
3503.764968	484655.139449	48.623911
3503.308645	484650.753232	48.628916
3503.385086	484660.772760	48.633921
3503.395280	484648.206535	48.638925
3503.159167	484662.024615	48.643930
3503.860944	484649.602398	48.648935
3503.549765	484656.086039	48.653940
3503.402434	484659.605257	48.658945
3503.676540	484665.236420	48.663949
3503.612774	484643.663661	48.668954
3503.561126	484622.646270	48.673959
3503.495395	484618.552957	48.678964
3503.602106	484598.473130	48.683969
3503.632170	484612.553159	48.688973
3503.257560	484613.625760	48.693978
3503.570320	484608.611326	48.698983
3503.639094	484610.069823	48.703988
3503.593766	484609.114470	48.708993
3503.811192	484611.714749	48.713997
3503.316669	484592.692571	48.719002
3503.471991	484567.690586	48.724007
3502.977293	484564.070381	48.729012
3503.047465	484582.957211	48.734017
3503.440618	484579.095343	48.739021
3503.279470	484570.761294	48.744026
3503.503032	484593.069047	48.749031
3503.740484	484573.525836	48.754036
3503.222379	484568.794715	48.759041
3503.446547	484583.249400	48.764045
3503.516023	484583.643836	48.769050
3503.426229	484569.978749	48.774055
3503.220949	484578.066937	48.779060
3503.282509	484575.321433	48.784065
3503.629568	484581.397069	48.789069
3503.409734	484584.421117	48.794074
3503.727827	484577.632580	48.799079
3503.595743	484570.661875	48.804084
3503.518776	484589.267969	48.809089
3503.422971	484587.864614	48.814093
3503.587621	484572.690043	48.819098
3503.611126	484551.306045	48.824103
3503.672575	484546.837963	48.829108
3503.495533	484542.407577	48.834113
3503.733383	484546.220584	48.839117
3503.461747	484564.046842	48.844122
3503.550386	484552.430779	48.849127
3503.449608	484543.428538	48.854132
3503.252781	484546.904936	48.859137
3503.594506	484543.405841	48.864141
3503.557605	484529.681700	48.869146
3503.886590	484515.849052	48.874151
3503.744260	484499.810986	48.879156
3503.283265	484528.357431	48.884161
3503.766954	484489.472027	48.889165
3503.494601	484519.103290	48.894170
3503.560546	484502.778982	48.899175
3503.895514	484492.491892	48.904180
3503.183222	484464.181719	48.909185
3503.141964	484477.867802	48.914189
3503.122688	484460.138319	48.919194
3503.305097	484470.394519	48.924199
3503.444442	484484.102715	48.929204
3503.411466	484489.022498	48.934209
3503.621596	484475.563260	48.939213
3503.485154	484478.979461	48.944218
3503.460234	484467.279968	48.949223
3503.507834	484485.055838	48.954228
3503.404138	484471.646202	48.959233
3503.690818	484463.899961	48.964237
3503.813534	484471.277709	48.969242
3503.676700	484460.153212	48.974247
3503.366154	484461.266360	48.979252
3503.405461	484456.295110	48.984257
3503.692617	484445.306246	48.989261
3503.365960	484432.995785	48.994266
3503.346693	484424.081933	48.999271
3503.401877	484432.888984	49.004276
3502.790725	484434.201643	49.009281
3503.209537	484422.989297	49.014285
3502.926050	484445.529361	49.019290
3503.176375	484447.465821	49.024295
3503.057943	484463.950671	49.029300
3503.578871	484478.358527	49.034305
3503.553115	484462.251339	49.039309
3503.355842	484464.511870	49.044314
3503.502692	484444.780191	49.049319
3503.810068	484436.574687	49.054324
3503.459469	484447.928443	49.059329
3503.593730	484452.315154	49.064333
3503.534365	484446.143545	49.069338
3503.824530	484430.594371	49.074343
3503.618076	484447.397138	49.079348
3503.237820	484437.476393	49.084353
3503.518276	484434.746934	49.089357
3503.173912	484425.935134	49.094362
3503.321375	484412.840412	49.099367
3503.603158	484411.884008	49.104372
3503.260065	484406.821195	49.109377
3503.393560	484416.781166	49.114381
3503.281426	484414.265753	49.119386
3503.812584	484408.760764	49.124391
3503.918293	484412.898673	49.129396
3503.963499	484412.232988	49.134401
3503.863051	484398.316140	49.139405
3503.613880	484390.299915	49.144410
3503.548045	484376.276250	49.149415
3503.689916	484368.502196	49.154420
3503.620105	484370.590595	49.159425
3503.602358	484365.679005	49.164429
3503.393685	484383.951460	49.169434
3503.713130	484370.069551	49.174439
3503.827691	484364.579734	49.179444
3503.303135	484351.337867	49.184449
3503.888814	484341.416388	49.189453
3503.334752	484335.677593	49.194458
3503.466340	484331.502365	49.199463
3503.798723	484334.591161	49.204468
3503.740239	484334.651174	49.209473
3503.699804	484322.498060	49.214477
3503.479062	484311.133415	49.219482
3503.527715	484286.958571	49.224487
3503.209611	484299.523240	49.229492
3503.148987	484297.151666	49.234497
3503.473293	484289.146083	49.239501
3503.491218	484286.306105	49.244506
3503.536557	484279.763237	49.249511
3503.486521	484294.768131	49.254516
3503.612705	484282.385995	49.259521
3503.559799	484276.517302	49.264525
3503.296067	484289.934691	49.269530
3503.745487	484287.837152	49.274535
3503.517953	484288.025215	49.279540
3503.175727	484288.586063	49.284545
3503.812937	484271.208627	49.289549
3503.360041	484267.936414	49.294554
3503.372276	484257.953538	49.299559
3503.801106	484266.245618	49.304564
3503.378534	484254.862177	49.309569
3503.612709	484268.656867	49.314573
3503.513190	484261.528907	49.319578
3503.629055	484254.062909	49.324583
3503.366259	484266.061541	49.329588
3503.481463	484262.750196	49.334593
3503.421850	484273.348747	49.339597
3503.363920	484271.939381	49.344602
3503.334194	484241.038398	49.349607
3503.664491	484228.370639	49.354612
3503.022293	484228.168259	49.359617
3503.522761	484213.041657	49.364621
3503.418803	484227.143150	49.369626
3503.363207	484224.720107	49.374631
3503.586447	484219.770388	49.379636
3503.298964	484219.359944	49.384641
3503.838956	484221.909290	49.389645
3503.401089	484226.133159	49.394650
3503.537806	484221.754436	49.399655
3503.372824	484226.796482	49.404660
3503.641818	484220.623565	49.409665
3503.660360	484217.479487	49.414669
3503.499074	484204.940080	49.419674
3503.595392	484198.085134	49.424679
3503.739035	484187.625463	49.429684
3503.566661	484186.842165	49.434689
3503.625955	484190.683466	49.439693
3503.382252	484192.039390	49.444698
3503.570980	484181.369928	49.449703
3503.471995	484191.721419	49.454708
3503.234070	484181.170060	49.459713
3503.832721	484175.553007	49.464717
3503.605789	484174.828998	49.469722
3503.624438	484151.976029	49.474727
3503.504644	484149.715120	49.479732
3503.419827	484148.056668	49.484737
3503.548844	484146.516413	49.489741
3503.360030	484154.247516	49.494746
3503.353011	484141.278359	49.499751
3503.202077	484159.085910	49.504756
3503.151115	484160.360705	49.509761
3503.438816	484150.435563	49.514765
3503.253971	484150.262222	49.519770
3503.380966	484156.828765	49.524775
3503.265837	484153.807137	49.529780
3503.498424	484152.351842	49.534785
3503.513004	484148.904387	49.539789
3503.221853	484150.267814	49.544794
3503.572931	484147.729814	49.549799
3503.801394	484150.632405	49.554804
3503.316862	484131.608193	49.559809
3503.614902	484121.782733	49.564813
3503.198776	484127.117830	49.569818
3503.389971	484115.231967	49.574823
3503.573765	484118.344286	49.579828
3503.317739	484120.715474	49.584833
3503.471607	484126.923121	49.589837
3503.350539	484133.528882	49.594842
3503.238679	484128.074786	49.599847
3503.539470	484122.910124	49.604852
3503.372425	484121.619326	49.609857
3503.683283	484123.900909	49.614861
3503.456091	484132.398071	49.619866
3503.409373	484128.504311	49.624871
3503.592003	484119.507742	49.629876
3503.363957	484129.930332	49.634881
3503.279204	484129.437176	49.639885
3503.579786	484127.109817	49.644890
3503.763415	484100.836118	49.649895
3503.737036	484110.264195	49.654900
3503.219798	484094.133055	49.659905
3503.609468	484085.458404	49.664909
3503.509968	484071.997162	49.669914
3503.479725	484099.260174	49.674919
3503.466872	484094.499739	49.679924
3503.408214	484103.020940	49.684929
3503.738013	484089.846513	49.689933
3503.248139	484099.094529	49.694938
3503.636010	484079.273717	49.699943
3503.547402	484070.117335	49.704948
3503.152636	484052.548162	49.709953
3503.774233	484044.951480	49.714957
3503.256641	484053.950570	49.719962
3503.383130	484056.869293	49.724967
3503.654024	484061.690488	49.729972
3503.418341	484059.093226	49.734977
3503.514455	484059.483463	49.739981
3503.463501	484069.574099	49.744986
3503.708098	484048.661256	49.749991
3503.813569	484048.746020	49.754996
3503.432957	484035.582515	49.760001
3503.748321	484005.183933	49.765005
3503.531267	484008.410295	49.770010
3503.731241	484006.554818	49.775015
3503.626725	484006.368778	49.780020
3503.411273	484008.429571	49.785025
3503.495907	484006.035000	49.790029
3503.496054	484013.736292	49.795034
3503.450190	484007.917070	49.800039
3503.474168	483995.905568	49.805044
3502.944271	483988.237544	49.810049
3503.676931	483997.748363	49.815053
3503.256691	483992.292307	49.820058
3503.492060	483978.423408	49.825063
3503.579203	483977.903077	49.830068
3503.727685	483969.570493	49.835073
3503.630341	483970.497971	49.840077
3503.183196	483971.126077	49.845082
3503.388176	483976.819033	49.850087
3503.394569	483977.578115	49.855092
3503.108807	483975.191421	49.860097
3503.551912	483968.788240	49.865101
3503.735761	483969.924600	49.870106
3503.452485	483965.662871	49.875111
3503.498442	483975.839570	49.880116
3503.557211	483965.342528	49.885121
3503.730594	483941.350201	49.890125
3503.087484	483951.990491	49.895130
3503.466063	483932.373662	49.900135
3503.351294	483931.327919	49.905140
3503.345061	483940.499564	49.910145
3503.700097	483945.206156	49.915149
3503.481794	483942.758129	49.920154
3503.225854	483927.345539	49.925159
3503.337995	483929.303893	49.930164
3503.382681	483935.731524	49.935169
3503.469645	483927.915306	49.940173
3503.478139	483950.713789	49.945178
3503.602990	483944.766232	49.950183
3503.601620	483941.523925	49.955188
3503.584122	483936.865518	49.960193
3503.635217	483914.665799	49.965197
3503.284544	483917.305303	49.970202
3503.214841	483911.033825	49.975207
3502.990423	483910.917402	49.980212
3503.230891	483912.652810	49.985217
3503.642806	483897.387963	49.990221
3503.434720	483908.466176	49.995226
3503.422376	483900.412314	50.000231
3503.554596	483902.215499	50.005236
3503.682878	483913.139210	50.010241
3503.569896	483910.015872	50.015245
3503.389031	483909.487236	50.020250
3503.869369	483912.248718	50.025255
3503.623841	483905.650367	50.030260
3503.290622	483883.106029	50.035265
3503.633836	483865.369372	50.040269
3503.314316	483878.187869	50.045274
3503.496110	483876.132588	50.050279
3503.317545	483868.966312	50.055284
3503.258359	483870.090428	50.060289
3503.250267	483871.358466	50.065293
3503.273718	483874.648166	50.070298
3503.452235	483877.558693	50.075303
3503.327071	483872.714623	50.080308
3503.548115	483867.309166	50.085313
3503.428872	483870.520090	50.090317
3503.579595	483875.816323	50.095322
3503.497767	483882.871963	50.100327
3503.615200	483885.640144	50.105332
3503.649209	483882.392235	50.110337
3503.730614	483874.171545	50.115341
3503.333636	483855.538552	50.120346
3503.607011	483848.402166	50.125351
3503.570735	483843.189375	50.130356
3503.441529	483843.209901	50.135361
3503.464497	483840.926390	50.140365
3503.381628	483845.144894	50.145370
3503.620837	483845.005854	50.150375
3503.533891	483842.790383	50.155380
3503.369224	483842.309851	50.160385
3503.749690	483844.428467	50.165389
3503.495370	483827.191554	50.170394
3503.681451	483804.767708	50.175399
3503.382233	483803.852445	50.180404
3503.355292	483794.584853	50.185409
3503.692496	483787.843687	50.190413
3503.377737	483789.666867	50.195418
3503.316047	483798.999344	50.200423
3503.425222	483790.318231	50.205428
3503.146641	483797.861000	50.210433
3503.330564	483802.037343	50.215437
3503.414183	483799.288243	50.220442
3503.152194	483803.129738	50.225447
3503.501543	483799.426640	50.230452
3503.036874	483803.908168	50.235457
3503.472884	483803.839354	50.240461
3503.524994	483804.692549	50.245466
3503.499235	483806.875378	50.250471
3503.496602	483803.025251	50.255476
3503.605905	483802.349414	50.260481
3503.366673	483800.715340	50.265485
3503.417255	483788.750171	50.270490
3503.193375	483786.556338	50.275495
3503.575820	483771.802715	50.280500
3503.370031	483771.835346	50.285505
3503.556547	483760.102005	50.290509
3503.342021	483770.218651	50.295514
3503.181436	483774.905454	50.300519
3503.320627	483772.451565	50.305524
3503.399598	483765.396543	50.310529
3503.585290	483762.479303	50.315533
3503.527940	483773.432435	50.320538
3503.417627	483774.463304	50.325543
3503.397011	483765.701363	50.330548
3503.380056	483774.722781	50.335553
3503.519916	483771.255456	50.340557
3503.622909	483787.705882	50.345562
3503.360823	483779.083447	50.350567
3503.662266	483772.297261	50.355572
3503.472512	483765.690047	50.360577
3503.366739	483745.338924	50.365581
3503.383017	483736.165806	50.370586
3503.493724	483733.361748	50.375591
3503.655692	483730.448254	50.380596
3502.980787	483745.755008	50.385601
3503.418599	483732.867266	50.390605
3503.244914	483730.918825	50.395610
3503.137626	483733.671883	50.400615
3503.428147	483727.039407	50.405620
3503.188270	483735.842747	50.410625
3503.418808	483728.662421	50.415629
3503.290201	483740.386833	50.420634
3503.286654	483747.379482	50.425639
3503.245476	483738.874111	50.430644
3503.161987	483738.988744	50.435649
3503.287335	483739.222367	50.440653
3503.415229	483740.012920	50.445658
3502.728218	483745.289604	50.450663
3503.523746	483741.515970	50.455668
3503.147172	483754.394233	50.460673
3503.264203	483740.746536	50.465677
3502.990654	483746.971198	50.470682
3503.620671	483734.813075	50.475687
3503.503404	483733.767715	50.480692
3503.026193	483751.576545	50.485697
3503.517619	483748.256312	50.490701
3503.745780	483745.940357	50.495706
3503.243011	483746.982594	50.500711
3503.531686	483745.670404	50.505716
3503.434565	483744.368528	50.510721
3503.222161	483740.551546	50.515725
3503.289906	483752.396914	50.520730
3503.139796	483738.690108	50.525735
3503.634944	483708.921311	50.530740
3503.420643	483681.493943	50.535745
3503.436136	483627.480797	50.540749
3503.156857	483582.482151	50.545754
3502.820662	483524.724284	50.550759
3502.799168	483463.065788	50.555764
3502.563477	483383.555335	50.560769
3502.780162	483290.799445	50.565773
3502.363651	483195.204456	50.570778
3502.350715	483082.115325	50.575783
3502.467120	482963.482219	50.580788
3502.014628	482847.370420	50.585793
3501.871704	482711.802688	50.590797
3501.889138	482564.047960	50.595802
3501.467774	482411.497152	50.600807
3501.443553	482253.713996	50.605812
3501.268630	482097.270830	50.610817
3501.274186	481897.524600	50.615821
3500.364450	481736.482266	50.620826
3499.748428	481562.977492	50.625831
3500.016593	481352.492364	50.630836
3499.630809	481153.611185	50.635841
3499.494636	480952.965633	50.640845
3498.977479	480741.280582	50.645850
3498.682872	480513.342112	50.650855
3498.549282	480303.111977	50.655860
3498.159883	480066.213773	50.660865
3498.068032	479817.964798	50.665869
3497.321147	479565.964774	50.670874
3496.893932	479325.212205	50.675879
3497.000877	479060.756054	50.680884
3496.237134	478806.569875	50.685889
3495.727691	478539.720945	50.690893
3495.575198	478264.196311	50.695898
3494.767153	477995.816204	50.700903
3494.566332	477717.858969	50.705908
3493.798622	477443.231178	50.710913
3493.520803	477148.907689	50.715917
3493.234530	476854.783959	50.720922
3492.628346	476569.981841	50.725927
3492.338921	476275.596718	50.730932
3491.810703	475965.988425	50.735937
3491.415729	475651.843159	50.740941
3490.697727	475339.771598	50.745946
3490.143032	475028.683191	50.750951
3489.911853	474706.589924	50.755956
3488.946221	474401.538240	50.760961
3488.744196	474075.628597	50.765965
3488.395752	473750.902808	50.770970
3487.641080	473421.927182	50.775975
3487.280795	473072.910631	50.780980
3486.573696	472744.372844	50.785985
3485.917393	472410.752241	50.790989
3485.404282	472068.231769	50.795994
3484.913643	471722.558838	50.800999
3484.277920	471379.843527	50.806004
3483.179344	471042.417664	50.811009
3483.158561	470687.172503	50.816013
3482.570958	470332.720670	50.821018
3481.479127	469988.888358	50.826023
3481.349347	469639.929491	50.831028
3480.693668	469287.143796	50.836033
3480.225325	468932.953533	50.841037
3479.532383	468574.229366	50.846042
3478.721913	468213.286603	50.851047
3478.213647	467859.084528	50.856052
3477.528149	467507.389169	50.861057
3476.925748	467132.551920	50.866061
3476.377755	466770.478098	50.871066
3475.897858	466413.661149	50.876071
3475.212794	466039.274016	50.881076
3474.057389	465680.320264	50.886081
3473.945933	465314.349256	50.891085
3473.244996	464946.385917	50.896090
3472.730947	464568.852434	50.901095
3471.938167	464193.182110	50.906100
3470.976777	463827.776501	50.911105
3470.818755	463456.100953	50.916109
3470.348396	463082.997563	50.921114
3469.409152	462705.498619	50.926119
3468.659256	462331.716404	50.931124
3467.698009	461956.693153	50.936129
3467.645054	461567.672946	50.941133
3466.470463	461206.415956	50.946138
3465.644512	460834.446051	50.951143
3465.346438	460464.466052	50.956148
3464.530784	460098.974679	50.961153
3464.085335	459703.947157	50.966157
3463.306693	459330.929784	50.971162
3462.229744	458959.221444	50.976167
3462.112133	458583.094032	50.981172
3461.492582	458190.299005	50.986177
3460.866341	457820.884583	50.991181
3460.140873	457434.789296	50.996186
3459.431190	457057.562866	51.001191
3458.884509	456667.215314	51.006196
3458.050879	456290.604337	51.011201
3457.168337	455909.327223	51.016205
3456.783552	455536.539186	51.021210
3455.978039	455145.089936	51.026215
3455.325694	454772.433047	51.031220
3454.451052	454394.985090	51.036225
3454.045059	454015.275010	51.041229
3453.011253	453629.416902	51.046234
3452.191461	453264.068197	51.051239
3452.165970	452879.509465	51.056244
3450.919319	452516.804089	51.061249
3450.725706	452127.946268	51.066253
3449.790388	451749.855264	51.071258
3448.988093	451366.865567	51.076263
3448.547809	450985.588366	51.081268
3447.504145	450608.459953	51.086273
3446.788943	450233.455592	51.091277
3446.255236	449867.703304	51.096282
3445.071472	449482.306895	51.101287
3444.808594	449116.500006	51.106292
3443.809724	448745.931748	51.111297
3443.130936	448369.369175	51.116301
3442.272474	448014.855195	51.121306
3441.900114	447642.901697	51.126311
3441.065977	447278.019287	51.131316
3440.299632	446895.508881	51.136321
3439.879781	446533.137949	51.141325
3438.917011	446167.192919	51.146330
3438.096099	445801.219834	51.151335
3437.898663	445435.244079	51.156340
3436.920507	445060.503513	51.161345
3436.391719	444696.852962	51.166349
3435.784708	444347.117368	51.171354
3434.814065	443970.480500	51.176359
3434.296808	443608.283725	51.181364
3433.240991	443230.278227	51.186369
3432.693434	442876.197173	51.191373
3432.127067	442522.266219	51.196378
3431.205101	442166.457304	51.201383
3430.670707	441788.042352	51.206388
3429.792680	441436.886217	51.211393
3429.288620	441068.608450	51.216397
3428.884864	440716.605524	51.221402
3428.164484	440355.357119	51.226407
3427.146349	439971.406188	51.231412
3426.397670	439621.549058	51.236417
3426.151262	439255.488096	51.241421
3425.205815	438899.432557	51.246426
3424.316216	438528.715513	51.251431
3423.882360	438167.542247	51.256436
3422.850346	437823.594210	51.261441
3422.131958	437454.992019	51.266445
3421.661042	437107.772095	51.271450
3420.893938	436761.330447	51.276455
3419.819463	436403.635020	51.281460
3419.160689	436058.791428	51.286465
3418.513648	435697.438691	51.291469
3417.744108	435364.180371	51.296474
3417.097160	435007.743267	51.301479
3416.506407	434660.051727	51.306484
3416.074934	434318.017631	51.311489
3415.449010	433963.771571	51.316493
3414.885513	433618.905306	51.321498
3414.145593	433266.648132	51.326503
3413.062608	432909.362111	51.331508
3412.110395	432574.471360	51.336513
3411.527720	432212.703848	51.341517
3411.008538	431869.406927	51.346522
3410.108180	431542.924941	51.351527
3409.952755	431190.953434	51.356532
3408.669854	430841.161531	51.361537
3408.121206	430508.516595	51.366541
3407.418825	430160.579141	51.371546
3406.519943	429831.282236	51.376551
3406.158765	429476.069789	51.381556
3405.087921	429150.296046	51.386561
3404.767909	428798.242368	51.391565
3404.172155	428470.861438	51.396570
3403.174598	428134.879976	51.401575
3402.808467	427785.308996	51.406580
3402.088253	427450.595678	51.411585
3401.106300	427107.386181	51.416589
3400.548414	426772.435556	51.421594
3400.388079	426435.513084	51.426599
3399.551615	426091.124727	51.431604
3398.326820	425765.003923	51.436609
3397.841941	425428.450391	51.441613
3397.508620	425086.534962	51.446618
3396.503302	424752.341247	51.451623
3395.816206	424416.035761	51.456628
3395.001778	424083.048246	51.461633
3394.587543	423742.170172	51.466637
3393.774282	423402.392378	51.471642
3392.753994	423065.742015	51.476647
3392.345752	422737.220709	51.481652
3391.495033	422412.651870	51.486657
3390.985147	422074.994293	51.491661
3390.256797	421748.975850	51.496666
3389.442319	421426.218694	51.501671
3388.971566	421077.162624	51.506676
3388.209802	420755.811933	51.511681
3387.665195	420423.550674	51.516685
3386.643766	420089.989096	51.521690
3385.736929	419767.379867	51.526695
3385.468272	419422.691544	51.531700
3384.411328	419111.479577	51.536705
3384.211444	418777.239112	51.541709
3383.506243	418454.024142	51.546714
3382.515853	418130.190065	51.551719
3382.180585	417794.485979	51.556724
3380.957542	417481.783549	51.561729
3380.640589	417150.464225	51.566733
3380.182598	416816.165435	51.571738
3379.651853	416491.325551	51.576743
3378.778170	416168.975309	51.581748
3377.617036	415848.826546	51.586753
3377.204175	415511.050157	51.591757
3376.658762	415203.424456	51.596762
3375.891037	414879.925220	51.601767
3375.083051	414543.114793	51.606772
3374.446951	414231.199190	51.611777
3373.877239	413899.323786	51.616781
3373.449140	413577.738383	51.621786
3372.355944	413253.002235	51.626791
3371.842018	412928.577478	51.631796
3370.924327	412613.182757	51.636801
3370.211835	412291.094745	51.641805
3369.790270	411957.751186	51.646810
3369.246908	411647.089646	51.651815
3368.272933	411319.391296	51.656820
3367.834653	411004.462822	51.661825
3367.024895	410695.637766	51.666829
3366.645265	410361.761617	51.671834
3365.753605	410045.420929	51.676839
3365.066294	409721.141349	51.681844
3364.339394	409406.470580	51.686849
3363.580799	409081.890502	51.691853
3363.023787	408766.779657	51.696858
3362.072003	408437.674312	51.701863
3361.507643	408124.896071	51.706868
3360.632429	407818.974768	51.711873
3360.138145	407495.759293	51.716877
3359.433093	407184.569443	51.721882
3358.829864	406875.291891	51.726887
3358.507784	406544.338566	51.731892
3357.699619	406240.780086	51.736897
3356.553642	405910.636528	51.741901
3356.275697	405592.805995	51.746906
3355.212703	405280.535432	51.751911
3354.787624	404956.418525	51.756916
3353.957186	404647.612365	51.761921
3353.384551	404330.451098	51.766925
3352.708080	404023.266590	51.771930
3351.719567	403717.221401	51.776935
3351.729187	403402.627612	51.781940
3350.633147	403094.534616	51.786945
3349.648876	402775.796202	51.791949
3349.269781	402460.136213	51.796954
3348.600120	402158.423057	51.801959
3348.072806	401844.432676	51.806964
3347.146132	401527.884230	51.811969
3346.600586	401223.270349	51.816973
3345.996639	400913.324732	51.821978
3345.020860	400600.054126	51.826983
3344.670669	400275.267964	51.831988
3343.663605	399969.749383	51.836993
3342.968262	399671.118470	51.841997
3342.527537	399356.327798	51.847002
3341.780366	399053.123729	51.852007
3341.338307	398737.844367	51.857012
3340.507820	398433.071670	51.862017
3339.634544	398118.210509	51.867021
3339.144109	397813.912216	51.872026
3338.319835	397511.087585	51.877031
3337.686677	397190.078362	51.882036
3337.096343	396889.194064	51.887041
3336.583152	396585.396663	51.892045
3336.041529	396272.423266	51.897050
3334.915804	395963.607083	51.902055
3334.242019	395661.377599	51.907060
3334.075599	395353.522793	51.912065
3333.107326	395042.283494	51.917069
3332.155767	394729.030195	51.922074
3331.345036	394431.591236	51.927079
3331.067952	394123.946259	51.932084
3330.434580	393830.414886	51.937089
3329.475920	393522.923181	51.942093
3328.857830	393217.586894	51.947098
3328.230436	392915.020785	51.952103
3327.718802	392605.797588	51.957108
3326.942701	392302.537750	51.962113
3326.269506	392006.429223	51.967117
3325.930621	391691.093731	51.972122
3324.952557	391396.070756	51.977127
3324.366918	391078.760088	51.982132
3323.824639	390771.305463	51.987137
3322.760303	390467.897408	51.992141
3322.277136	390169.734650	51.997146
3321.547961	389859.657219	52.002151
3321.048361	389551.778458	52.007156
3320.166304	389261.197903	52.012161
3319.777887	388947.295298	52.017165
3319.266455	388641.622884	52.022170
3318.106409	388337.881342	52.027175
3317.901432	388025.569163	52.032180
3317.141021	387728.879471	52.037185
3316.526391	387420.949873	52.042189
3315.730146	387103.027069	52.047194
3314.634464	386805.696293	52.052199
3314.223438	386504.058845	52.057204
3313.519746	386198.904956	52.062209
3312.694528	385891.555300	52.067213
3312.185111	385589.188448	52.072218
3311.120723	385284.160354	52.077223
3310.939959	384983.669357	52.082228
3310.104190	384687.933487	52.087233
3309.189983	384389.562794	52.092237
3308.650889	384093.164949	52.097242
3307.610121	383789.545117	52.102247
3307.361399	383496.987762	52.107252
3306.580783	383213.413619	52.112257
3305.796582	382912.620036	52.117261
3305.266171	382611.911100	52.122266
3304.555769	382329.616339	52.127271
3304.141303	382011.869649	52.132276
3303.542893	381712.232593	52.137281
3302.837290	381415.763927	52.142285
3302.259263	381119.247372	52.147290
3301.245174	380822.517738	52.152295
3301.065339	380513.114823	52.157300
3299.855740	380214.274992	52.162305
3299.225939	379920.072008	52.167309
3298.836173	379620.334933	52.172314
3297.489173	379330.819222	52.177319
3297.012429	379042.028537	52.182324
3296.566011	378746.948410	52.187329
3295.787317	378443.601211	52.192333
3295.384572	378159.777757	52.197338
3294.563868	377858.416726	52.202343
3294.211534	377559.904496	52.207348
3293.300032	377257.663035	52.212353
3292.800344	376958.355674	52.217357
3291.974846	376659.886159	52.222362
3291.154714	376370.291060	52.227367
3290.997619	376068.023117	52.232372
3290.052294	375772.389533	52.237377
3289.441727	375475.581612	52.242381
3288.836404	375178.389143	52.247386
3287.648129	374887.111979	52.252391
3287.573527	374579.452616	52.257396
3286.649527	374291.207437	52.262401
3285.944045	373986.568834	52.267405
3285.284994	373694.665355	52.272410
3284.465333	373400.037854	52.277415
3283.906259	373108.343408	52.282420
3283.325468	372812.427482	52.287425
3282.513353	372513.315277	52.292429
3281.755651	372218.618804	52.297434
3281.017354	371937.323873	52.302439
3280.683852	371636.806908	52.307444
3279.930901	371345.003747	52.312449
3279.257651	371052.651742	52.317453
3278.893391	370742.109937	52.322458
3278.116935	370454.476634	52.327463
3277.344337	370160.378876	52.332468
3276.866909	369853.919073	52.337473
3276.171583	369557.922379	52.342477
3275.583219	369261.601459	52.347482
3274.364467	368973.315935	52.352487
3273.935809	368667.247132	52.357492
3273.321303	368372.170960	52.362497
3272.441283	368078.534112	52.367501
3272.155277	367779.738392	52.372506
3271.325926	367486.751097	52.377511
3270.596228	367195.069112	52.382516
3270.035119	366892.749019	52.387521
3269.427397	366601.908916	52.392525
3268.885523	366296.884838	52.397530
3267.846610	366018.779718	52.402535
3267.309746	365704.922116	52.407540
3266.274603	365408.544427	52.412545
3265.598098	365124.422751	52.417549
3265.222135	364827.937022	52.422554
3264.495477	364532.980590	52.427559
3263.691111	364244.395562	52.432564
3263.015548	363962.022178	52.437569
3262.352793	363669.060203	52.442573
3261.553916	363377.848136	52.447578
3260.857087	363100.663552	52.452583
3260.694001	362802.579052	52.457588
3260.024404	362509.941664	52.462593
3259.225254	362218.544314	52.467597
3258.714596	361916.030834	52.472602
3258.078778	361620.685391	52.477607
3257.739804	361325.469278	52.482612
3257.033605	361016.594161	52.487617
3255.873263	360722.572969	52.492621
3255.398946	360429.204844	52.497626
3254.328753	360145.853219	52.502631
3253.853105	359845.076905	52.507636
3253.002004	359560.745686	52.512641
3252.489520	359276.155671	52.517645
3251.974417	358972.886439	52.522650
3251.275277	358682.953219	52.527655
3250.574869	358385.511587	52.532660
3250.121113	358093.754789	52.537665
3249.466709	357797.091210	52.542669
3248.851299	357486.652544	52.547674
3247.741435	357205.631421	52.552679
3247.310081	356903.863152	52.557684
3246.693255	356616.984072	52.562689
3245.690367	356326.169065	52.567693
3245.519687	356027.077279	52.572698
3244.649657	355747.002585	52.577703
3244.314497	355446.101117	52.582708
3243.548049	355145.622390	52.587713
3242.589098	354846.164866	52.592717
3241.947904	354553.475691	52.597722
3241.434409	354264.225756	52.602727
3240.973136	353960.027180	52.607732
3240.102653	353666.860300	52.612737
3239.338220	353369.043169	52.617741
3238.641833	353066.276329	52.622746
3237.820355	352780.044549	52.627751
3237.498513	352489.838326	52.632756
3236.331573	352197.346436	52.637761
3235.970121	351898.591992	52.642765
3235.233204	351602.542129	52.647770
3234.640231	351318.022453	52.652775
3234.107606	351024.482164	52.657780
3233.462930	350736.531759	52.662785
3232.498704	350438.297262	52.667789
3231.865311	350144.590014	52.672794
3230.872586	349854.959346	52.677799
3230.185234	349558.101542	52.682804
3229.799818	349273.054816	52.687809
3228.908972	348993.278730	52.692813
3228.359092	348705.175458	52.697818
3227.468047	348420.687948	52.702823
3227.301775	348134.506315	52.707828
3226.988740	347834.169559	52.712833
3225.912738	347548.128872	52.717837
3225.649974	347251.522579	52.722842
3224.965244	346961.446464	52.727847
3224.273332	346666.533997	52.732852
3223.330437	346368.198132	52.737857
3222.510400	346074.321023	52.742861
3222.284888	345777.904876	52.747866
3221.172974	345506.724362	52.752871
3220.875825	345201.229811	52.757876
3220.243073	344904.160973	52.762881
3219.274471	344611.496343	52.767885
3218.640616	344310.453932	52.772890
3217.786708	344028.331602	52.777895
3217.382132	343729.006307	52.782900
3216.553712	343440.360950	52.787905
3216.035793	343144.206994	52.792909
3215.306884	342841.925007	52.797914
3214.503954	342560.602293	52.802919
3214.060238	342265.883233	52.807924
3213.755099	341972.540849	52.812929
3212.596160	341673.375700	52.817933
3211.783716	341380.085306	52.822938
3210.940154	341096.216845	52.827943
3210.782373	340807.936671	52.832948
3209.914380	340510.781793	52.837953
3208.780589	340227.668071	52.842957
3208.697920	339933.771820	52.847962
3207.858525	339645.517813	52.852967
3207.085352	339356.310166	52.857972
3206.543835	339075.872318	52.862977
3206.076107	338781.751688	52.867981
3205.271558	338487.275712	52.872986
3204.613499	338198.528345	52.877991
3204.295629	337906.925685	52.882996
3203.498489	337614.455663	52.888001
3202.559098	337324.323402	52.893005
3201.993382	337029.650375	52.898010
3201.035639	336737.787403	52.903015
3200.573421	336446.684845	52.908020
3199.947411	336152.195697	52.913025
3199.102855	335866.217075	52.918029
3198.784522	335563.403120	52.923034
3198.142650	335284.161624	52.928039
3197.519808	334990.557964	52.933044
3196.761111	334695.268891	52.938049
3195.948280	334407.802636	52.943053
3195.724529	334115.150439	52.948058
3194.773551	333831.369592	52.953063
3194.311784	333526.430972	52.958068
3193.510392	333238.016173	52.963073
3192.817102	332940.519974	52.968077
3192.430119	332643.661453	52.973082
3191.394331	332362.026658	52.978087
3190.826729	332056.487510	52.983092
3189.875700	331764.679027	52.988097
3189.230583	331476.614331	52.993101
3189.123862	331178.356166	52.998106
3188.078739	330895.826131	53.003111
3187.339085	330603.241289	53.008116
3186.942873	330310.346372	53.013121
3185.909203	330012.382938	53.018125
3185.520469	329723.889000	53.023130
3184.716616	329431.768023	53.028135
3184.486322	329131.484510	53.033140
3183.562776	328835.230284	53.038145
3182.712687	328545.277310	53.043149
3182.086552	328241.106696	53.048154
3181.505124	327944.031139	53.053159
3180.789896	327658.534473	53.058164
3180.268313	327373.922699	53.063169
3179.645685	327082.069733	53.068173
3178.975008	326776.882104	53.073178
3178.316092	326479.660556	53.078183
3177.712663	326195.210296	53.083188
3176.805708	325894.665057	53.088193
3176.110828	325606.688187	53.093197
3175.679172	325307.847838	53.098202
3174.796759	325021.706305	53.103207
3174.063942	324717.666540	53.108212
3173.515953	324436.027591	53.113217
3172.407816	324142.331372	53.118221
3172.098101	323839.214470	53.123226
3171.504257	323559.794981	53.128231
3170.757278	323259.647789	53.133236
3170.125671	322970.811647	53.138241
3169.120781	322687.355066	53.143245
3168.989345	322389.526315	53.148250
3168.113338	322103.832288	53.153255
3167.234858	321800.518163	53.158260
3166.677527	321514.237115	53.163265
3166.174539	321231.129298	53.168269
3165.590868	320943.271953	53.173274
3164.459119	320652.164871	53.178279
3164.127472	320354.666563	53.183284
3163.575411	320057.915109	53.188289
3162.733825	319775.467437	53.193293
3162.224589	319484.258165	53.198298
3161.835680	319191.806747	53.203303
3160.852365	318897.793400	53.208308
3160.362707	318605.228794	53.213313
3159.437269	318311.560955	53.218317
3159.093224	318015.279408	53.223322
3158.109773	317733.459208	53.228327
3157.637735	317429.939196	53.233332
3157.065281	317132.086936	53.238337
3156.209846	316849.963851	53.243341
3155.586658	316548.527563	53.248346
3155.087659	316255.702777	53.253351
3154.252561	315965.425731	53.258356
3153.625233	315674.682104	53.263361
3152.606089	315386.673316	53.268365
3152.104047	315080.884715	53.273370
3151.217714	314811.696367	53.278375
3150.647730	314505.764050	53.283380
3150.175574	314224.489786	53.288385
3149.305587	313941.877214	53.293389
3148.942934	313642.428356	53.298394
3148.151910	313352.086168	53.303399
3147.297127	313069.723548	53.308404
3146.818264	312779.152197	53.313409
3145.842691	312481.808806	53.318413
3145.426352	312192.066343	53.323418
3144.243271	311918.105018	53.328423
3143.446122	311630.815015	53.333428
3143.416020	311342.995487	53.338433
3142.353942	311062.366736	53.343437
3141.809095	310773.124830	53.348442
3141.462173	310500.810341	53.353447
3140.878290	310206.607610	53.358452
3139.946833	309920.455084	53.363457
3139.306394	309639.043213	53.368461
3138.796240	309347.551441	53.373466
3138.324875	309051.978443	53.378471
3137.620549	308771.211301	53.383476
3137.121805	308478.162297	53.388481
3136.169041	308176.577235	53.393485
3135.916193	307884.964916	53.398490
3134.954541	307600.008654	53.403495
3134.185530	307304.147595	53.408500
3133.773058	307006.752453	53.413505
3132.864134	306717.991573	53.418509
3132.595593	306419.375454	53.423514
3131.431629	306136.790845	53.428519
3130.810272	305841.641649	53.433524
3130.294830	305544.412337	53.438529
3129.348789	305261.027456	53.443533
3128.689443	304981.976739	53.448538
3128.259018	304701.768746	53.453543
3127.716237	304395.704682	53.458548
3127.230524	304113.798068	53.463553
3126.064267	303825.351980	53.468557
3125.976226	303524.179971	53.473562
3124.884129	303229.609137	53.478567
3124.366524	302947.654396	53.483572
3123.647915	302648.464888	53.488577
3123.137951	302362.484198	53.493581
3122.323811	302068.529243	53.498586
3121.499705	301772.716270	53.503591
3120.722075	301483.796765	53.508596
3120.256024	301195.413157	53.513601
3119.264583	300914.344637	53.518605
3118.727271	300618.305883	53.523610
3118.335802	300333.830784	53.528615
3117.212253	300032.994181	53.533620
3116.978654	299743.119654	53.538625
3116.300634	299456.676558	53.543629
3115.557634	299173.171940	53.548634
3114.525752	298888.719374	53.553639
3114.029379	298603.595874	53.558644
3113.693110	298316.587508	53.563649
3112.801640	298031.831228	53.568653
3112.178984	297738.220424	53.573658
3111.200412	297452.229158	53.578663
3110.697822	297169.014438	53.583668
3109.959437	296890.522541	53.588673
3109.465582	296605.395584	53.593677
3108.747143	296312.408958	53.598682
3108.188673	296032.817758	53.603687
3107.461522	295737.335894	53.608692
3106.905189	295451.376769	53.613697
3106.121035	295168.127361	53.618701
3105.556467	294866.379062	53.623706
3104.724381	294594.189265	53.628711
3103.700249	294309.474129	53.633716
3103.156839	294024.708019	53.638721
3102.737702	293739.539870	53.643725
3102.088039	293463.703454	53.648730
3101.239794	293183.364929	53.653735
3100.688832	292896.866829	53.658740
3100.267608	292611.111880	53.663745
3099.054342	292330.269835	53.668749
3099.092004	292038.558598	53.673754
3098.605509	291758.084780	53.678759
3097.805464	291469.485167	53.683764
3097.169415	291173.702870	53.688769
3096.353520	290879.604106	53.693773
3095.732324	290584.582841	53.698778
3094.999230	290299.511387	53.703783
3094.576041	290010.494033	53.708788
3093.940107	289717.715357	53.713793
3092.895384	289437.352970	53.718797
3092.645264	289135.573461	53.723802
3091.665073	288845.420665	53.728807
3090.677013	288560.922717	53.733812
3090.176768	288266.796852	53.738817
3089.444169	287991.095339	53.743821
3088.723275	287699.550682	53.748826
3088.148439	287419.188571	53.753831
3087.614725	287137.469925	53.758836
3087.209449	286847.759246	53.763841
3086.236230	286563.461039	53.768845
3085.488356	286270.111268	53.773850
3085.070588	285987.405623	53.778855
3084.452220	285698.899334	53.783860
3083.751464	285410.202137	53.788865
3082.932640	285117.575871	53.793869
3082.657253	284830.262651	53.798874
3081.658789	284537.791775	53.803879
3080.710412	284247.350243	53.808884
3080.372107	283963.026224	53.813889
3079.620516	283688.572706	53.818893
3079.020573	283393.567665	53.823898
3078.101183	283116.415307	53.828903
3077.496431	282826.198748	53.833908
3077.100628	282532.892786	53.838913
3076.508784	282250.772807	53.843917
3075.973189	281957.565101	53.848922
3075.337424	281666.614328	53.853927
3074.473755	281376.081526	53.858932
3073.956631	281081.291494	53.863937
3072.947504	280795.060165	53.868941
3072.187220	280501.199793	53.873946
3071.715084	280216.793405	53.878951
3070.827408	279930.644443	53.883956
3070.204243	279648.299257	53.888961
3069.516603	279366.906528	53.893965
3069.270185	279067.819797	53.898970
3068.683639	278779.636347	53.903975
3067.589501	278490.998336	53.908980
3067.187058	278204.059053	53.913985
3066.551441	277911.095151	53.918989
3065.363751	277622.268052	53.923994
3064.929325	277339.204896	53.928999
3064.611707	277053.168891	53.934004
3064.015908	276758.950598	53.939009
3063.063782	276488.270535	53.944013
3062.242260	276183.671361	53.949018
3061.683725	275897.087646	53.954023
3061.094478	275612.444388	53.959028
3060.678650	275316.312910	53.964033
3059.825036	275045.922868	53.969037
3058.890590	274747.886963	53.974042
3058.377237	274463.231743	53.979047
3057.538692	274182.601085	53.984052
3057.058976	273890.962263	53.989057
3056.084983	273602.636194	53.994061
3055.885954	273314.111110	53.999066
3055.010504	273031.016024	54.004071
3054.218487	272747.143737	54.009076
3054.063670	272453.823772	54.014081
3053.161276	272172.006550	54.019085
3052.644137	271874.923823	54.024090
3051.978744	271583.263932	54.029095
3051.311175	271299.932617	54.034100
3050.745109	271000.998713	54.039105
3049.845487	270711.260830	54.044109
3049.265943	270429.622250	54.049114
3048.664885	270137.876266	54.054119
3047.855055	269852.810665	54.059124
3047.146089	269545.571823	54.064129
3046.354093	269253.601754	54.069133
3045.844355	268966.095026	54.074138
3045.102325	268682.598248	54.079143
3044.492382	268384.258198	54.084148
3043.858823	268101.610464	54.089153
3043.151850	267817.777495	54.094157
3042.738478	267526.232290	54.099162
3041.963270	267234.005952	54.104167
3041.195009	266942.568205	54.109172
3040.932041	266657.417700	54.114177
3039.761757	266362.147333	54.119181
3039.425705	266067.152617	54.124186
3038.680679	265777.596604	54.129191
3037.978945	265490.911836	54.134196
3037.411833	265188.670462	54.139201
3036.314556	264910.962541	54.144205
3036.133333	264616.912182	54.149210
3035.246108	264326.182771	54.154215
3034.307290	264044.553826	54.159220
3034.166789	263742.195188	54.164225
3033.520331	263465.384820	54.169229
3032.965381	263165.486285	54.174234
3031.995610	262874.898525	54.179239
3031.538675	262579.110821	54.184244
3031.066001	262285.821738	54.189249
3030.103011	261993.782067	54.194253
3029.364591	261696.842794	54.199258
3029.156164	261404.480533	54.204263
3028.188555	261110.048516	54.209268
3027.748306	260810.363396	54.214273
3026.818126	260522.038329	54.219277
3026.182064	260223.276223	54.224282
3025.465478	259935.376404	54.229287
3024.678832	259643.744261	54.234292
3024.044382	259338.794304	54.239297
3023.342504	259054.382215	54.244301
3022.681396	258770.371483	54.249306
3022.150998	258479.846195	54.254311
3021.579066	258190.091862	54.259316
3020.700912	257897.126536	54.264321
3020.184559	257598.526964	54.269325
3019.570211	257305.240506	54.274330
3018.783937	257014.375576	54.279335
3018.231729	256707.327743	54.284340
3017.874397	256429.027465	54.289345
3016.650400	256138.946092	54.294349
3016.183732	255848.617912	54.299354
3015.659238	255552.976670	54.304359
3014.551296	255254.117494	54.309364
3014.048211	254964.356626	54.314369
3013.540690	254681.320176	54.319373
3012.658070	254389.582880	54.324378
3011.876873	254106.183127	54.329383
3011.230047	253806.310921	54.334388
3010.859998	253509.655144	54.339393
3009.729777	253230.819605	54.344397
3009.464547	252940.489397	54.349402
3008.633477	252647.931756	54.354407
3007.912608	252360.450493	54.359412
3007.356257	252078.622722	54.364417
3006.678517	251785.456525	54.369421
3006.118830	251482.951388	54.374426
3005.256769	251203.490915	54.379431
3004.867952	250920.874558	54.384436
3004.342590	250618.492893	54.389441
3003.311252	250340.002943	54.394445
3002.930641	250045.595879	54.399450
3002.649918	249749.900236	54.404455
3001.606231	249458.757047	54.409460
3000.977864	249163.677802	54.414465
3000.132589	248873.293763	54.419469
2999.826624	248581.959062	54.424474
2998.952139	248287.506200	54.429479
2998.156531	247998.491157	54.434484
2997.773831	247690.337335	54.439489
2996.619013	247392.492743	54.444493
2996.380975	247108.127861	54.449498
2995.687877	246818.895220	54.454503
2994.982284	246531.651478	54.459508
2994.506925	246239.609799	54.464513
2993.724862	245943.313600	54.469517
2992.796578	245643.195888	54.474522
2992.223086	245358.607568	54.479527
2991.364477	245071.594836	54.484532
2990.794696	244770.098122	54.489537
2990.139692	244482.850713	54.494541
2989.326265	244199.601599	54.499546
2989.083951	243910.456626	54.504551
2988.500200	243613.828665	54.509556
2987.993088	243315.966940	54.514561
2986.943854	243036.602969	54.519565
2986.460921	242732.881842	54.524570
2986.116243	242437.517534	54.529575
2984.982700	242145.309138	54.534580
2984.480044	241842.611934	54.539585
2983.533436	241549.051217	54.544589
2983.038119	241256.591158	54.549594
2982.745007	240962.215429	54.554599
2981.649701	240677.414778	54.559604
2981.149390	240379.355494	54.564609
2980.432752	240091.440601	54.569613
2980.133429	239783.267135	54.574618
2979.206975	239486.856426	54.579623
2978.372148	239199.140757	54.584628
2977.960398	238901.886189	54.589633
2977.165302	238611.110053	54.594637
2976.485235	238316.165843	54.599642
2975.873423	238010.083880	54.604647
2975.397592	237715.159898	54.609652
2974.878718	237410.134409	54.614657
2974.023641	237124.286282	54.619661
2973.663564	236816.563669	54.624666
2972.883398	236520.799959	54.629671
2971.987995	236217.619986	54.634676
2971.632441	235918.124030	54.639681
2970.527511	235616.710513	54.644685
2969.931840	235318.247401	54.649690
2969.362542	235021.257863	54.654695
2968.584921	234726.084604	54.659700
2968.002522	234421.969243	54.664705
2967.242713	234131.836621	54.669709
2966.570955	233821.906238	54.674714
2965.930517	233530.432433	54.679719
2965.247210	233237.387602	54.684724
2964.807398	232938.194077	54.689729
2964.243538	232638.664652	54.694733
2963.340023	232340.997785	54.699738
2962.874782	232038.297302	54.704743
2962.014616	231738.359331	54.709748
2961.500418	231437.043521	54.714753
2960.534826	231149.371503	54.719757
2959.958358	230843.255148	54.724762
2959.325303	230548.199296	54.729767
2958.511492	230254.013269	54.734772
2958.118798	229951.893827	54.739777
2957.429938	229652.292087	54.744781
2956.729956	229358.880308	54.749786
2956.076422	229060.369837	54.754791
2955.448436	228762.696571	54.759796
2954.800079	228460.750031	54.764801
2953.869465	228165.367334	54.769805
2953.324075	227860.554931	54.774810
2952.892494	227565.935520	54.779815
2951.946635	227274.224731	54.784820
2951.568093	226973.933902	54.789825
2950.890766	226674.506202	54.794829
2950.465374	226375.548909	54.799834
2949.648987	226066.559436	54.804839
2948.787438	225770.155809	54.809844
2948.350311	225466.404360	54.814849
2947.535033	225172.707127	54.819853
2946.820273	224866.659526	54.824858
2946.105143	224561.809781	54.829863
2945.025634	224266.871959	54.834868
2944.657012	223967.290801	54.839873
2944.030239	223676.688087	54.844877
2943.458814	223369.376037	54.849882
2943.318402	223082.975781	54.854887
2942.325608	222781.575777	54.859892
2941.760022	222475.475680	54.864897
2940.879840	222187.961086	54.869901
2939.995578	221880.284424	54.874906
2939.951752	221573.685263	54.879911
2938.901242	221277.583141	54.884916
2938.212922	220979.897304	54.889921
2937.593585	220668.059299	54.894925
2936.762466	220377.170561	54.899930
2936.112576	220083.402900	54.904935
2935.345382	219780.388051	54.909940
2935.172901	219473.588818	54.914945
2934.418575	219178.071973	54.919949
2933.864543	218875.880010	54.924954
2933.539334	218563.940790	54.929959
2932.304444	218264.952376	54.934964
2932.271327	217954.700729	54.939969
2931.193548	217654.238915	54.944973
2930.312190	217346.695491	54.949978
2930.089748	217037.190687	54.954983
2929.057577	216739.818689	54.959988
2928.317481	216422.188538	54.964993
2927.403504	216125.207796	54.969997
2926.991524	215824.317555	54.975002
2926.216836	215529.010257	54.980007
2925.221376	215238.817866	54.985012
2924.699105	214936.905292	54.990017
2924.342779	214639.550014	54.995021
2923.684388	214331.195711	55.000026
2922.777802	214036.259532	55.005031
2922.163103	213737.638188	55.010036
2922.117317	213440.340946	55.015041
2921.419976	213140.208028	55.020045
2920.658023	212830.069769	55.025050
2919.854390	212525.998102	55.030055
2919.017077	212217.758448	55.035060
2918.604611	211915.791471	55.040065
2917.858026	211616.908035	55.045069
2917.216655	211311.072736	55.050074
2916.820923	211007.605548	55.055079
2915.967341	210697.708513	55.060084
2915.226740	210398.575342	55.065089
2914.486661	210086.741504	55.070093
2913.842291	209784.859637	55.075098
2913.446986	209470.734282	55.080103
2912.427067	209176.398536	55.085108
2911.880759	208866.487457	55.090113
2910.929408	208557.367534	55.095117
2910.333119	208259.838254	55.100122
2909.612840	207961.350089	55.105127
2908.526581	207668.470312	55.110132
2908.203853	207364.869558	55.115137
2907.546468	207072.739313	55.120141
2906.639381	206784.442623	55.125146
2906.416405	206480.270616	55.130151
2905.333189	206185.972276	55.135156
2904.872316	205878.417583	55.140161
2904.392594	205581.863205	55.145165
2903.726992	205285.288866	55.150170
2903.183579	204989.269386	55.155175
2902.487694	204687.154208	55.160180
2901.851536	204379.864303	55.165185
2901.133108	204076.165135	55.170189
2900.247873	203776.808154	55.175194
2899.942698	203476.151931	55.180199
2899.019481	203176.651429	55.185204
2898.262666	202877.202530	55.190209
2897.516830	202576.811781	55.195213
2896.963460	202279.000960	55.200218
2896.409356	201980.428310	55.205223
2895.471833	201686.346508	55.210228
2895.285786	201381.483254	55.215233
2894.389969	201082.562362	55.220237
2893.419216	200786.798153	55.225242
2893.127397	200487.275867	55.230247
2892.405045	200192.137283	55.235252
2891.889906	199889.141490	55.240257
2891.403071	199594.070690	55.245261
2890.568025	199290.314524	55.250266
2889.883999	198997.352431	55.255271
2889.037152	198691.425574	55.260276
2888.435225	198385.105407	55.265281
2887.900241	198078.343776	55.270285
2887.106256	197782.670003	55.275290
2886.790219	197480.369027	55.280295
2885.951231	197177.630905	55.285300
2885.256843	196880.979410	55.290305
2884.428754	196581.818628	55.295309
2883.697980	196275.085912	55.300314
2883.457876	195971.280258	55.305319
2882.250486	195684.883593	55.310324
2881.900740	195370.970413	55.315329
2881.509343	195076.266354	55.320333
2880.550650	194779.363530	55.325338
2880.244541	194472.727129	55.330343
2879.408294	194167.181731	55.335348
2878.700898	193857.075423	55.340353
2878.246532	193548.050659	55.345357
2877.694998	193252.670163	55.350362
2877.075016	192941.843212	55.355367
2876.216992	192644.250109	55.360372
2875.595817	192330.857078	55.365377
2874.701089	192026.810081	55.370381
2874.114656	191720.998533	55.375386
2873.505826	191420.281700	55.380391
2872.834890	191111.446559	55.385396
2871.974774	190810.811485	55.390401
2871.148978	190514.002444	55.395405
2870.502371	190201.568732	55.400410
2869.834945	189891.214166	55.405415
2869.001034	189606.727635	55.410420
2868.588020	189309.758957	55.415425
2867.911968	188998.699147	55.420429
2866.882172	188710.025190	55.425434
2866.468473	188400.314540	55.430439
2865.724203	188104.220176	55.435444
2865.751288	187803.298355	55.440449
2864.723370	187508.054204	55.445453
2863.900101	187207.512637	55.450458
2863.542208	186902.319455	55.455463
2862.834385	186596.814785	55.460468
2862.205510	186290.218309	55.465473
2861.644932	185991.767645	55.470477
2860.691601	185691.434742	55.475482
2860.172200	185377.639415	55.480487
2859.120367	185086.740013	55.485492
2858.680609	184783.342302	55.490497
2858.104625	184487.575500	55.495501
2857.493083	184176.716315	55.500506
2857.147667	183860.817792	55.505511
2856.104927	183570.613763	55.510516
2855.398170	183258.567600	55.515521
2855.109435	182955.247497	55.520525
2854.212695	182652.038495	55.525530
2853.462137	182354.965210	55.530535
2852.679633	182054.260942	55.535540
2852.158540	181746.241275	55.540545
2851.742947	181447.047716	55.545549
2850.643847	181147.646466	55.550554
2850.287356	180835.409543	55.555559
2849.555764	180535.356508	55.560564
2848.844265	180227.441454	55.565569
2848.239176	179920.071445	55.570573
2847.640739	179615.170241	55.575578
2846.833325	179317.172961	55.580583
2846.265456	179002.337250	55.585588
2845.700186	178694.855356	55.590593
2844.948263	178402.465061	55.595597
2844.044882	178100.688492	55.600602
2843.750594	177785.793150	55.605607
2842.896504	177486.468036	55.610612
2842.280519	177190.655988	55.615617
2841.360198	176875.714072	55.620621
2840.968415	176581.282687	55.625626
2840.387747	176275.868874	55.630631
2839.541578	175980.890539	55.635636
2839.076627	175668.811066	55.640641
2838.420176	175360.999566	55.645645
2837.505331	175067.285139	55.650650
2837.307520	174744.181781	55.655655
2836.553146	174448.716750	55.660660
2835.896253	174140.978205	55.665665
2835.303483	173825.740967	55.670669
2834.550029	173510.099254	55.675674
2833.736172	173209.502043	55.680679
2833.078637	172900.259748	55.685684
2832.414879	172598.575108	55.690689
2831.512104	172294.183646	55.695693
2830.833021	171991.285199	55.700698
2830.573936	171687.712140	55.705703
2829.605247	171372.884634	55.710708
2829.188011	171067.586463	55.715713
2828.330867	170773.093513	55.720717
2827.820547	170456.509465	55.725722
2827.298053	170155.240967	55.730727
2826.615149	169851.914687	55.735732
2825.954342	169474.996368	55.740737
2825.623917	169165.452143	55.745741
2824.819297	168854.116220	55.750746
2824.442629	168541.303557	55.755751
2823.390750	168227.875586	55.760756
2822.765620	167908.520517	55.765761
2822.032366	167606.313663	55.770765
2821.029519	167291.347070	55.775770
2820.844117	166979.623323	55.780775
2819.631477	166679.152904	55.785780
2818.941102	166365.924797	55.790785
2818.391670	166066.066350	55.795789
2817.344045	165768.857727	55.800794
2816.901277	165452.826163	55.805799
2816.316629	165149.306020	55.810804
2815.719833	164847.900994	55.815809
2815.143190	164545.427198	55.820813
2814.486676	164224.824529	55.825818
2814.254655	163924.221222	55.830823
2813.211726	163624.982146	55.835828
2812.609952	163308.587402	55.840833
2811.959745	163001.649870	55.845837
2811.034635	162691.287493	55.850842
2810.701981	162396.510506	55.855847
2809.812928	162078.544642	55.860852
2809.082004	161776.728679	55.865857
2808.344709	161466.398011	55.870861
2807.487779	161168.739143	55.875866
2807.042912	160856.600270	55.880871
2806.210079	160563.189012	55.885876
2805.683400	160245.906801	55.890881
2805.307339	159949.872903	55.895885
2804.347406	159657.900486	55.900890
2803.800564	159344.863088	55.905895
2803.347711	159040.471122	55.910900
2802.466562	158737.586201	55.915905
2801.889027	158432.214985	55.920909
2801.324652	158119.445629	55.925914
2800.877869	157819.665363	55.930919
2799.681162	157518.620830	55.935924
2799.201705	157204.435239	55.940929
2798.681233	156902.259301	55.945933
2797.667543	156607.232052	55.950938
2797.233739	156294.712853	55.955943
2796.393207	155996.180392	55.960948
2796.079270	155679.414819	55.965953
2795.215383	155382.442283	55.970957
2794.465637	155082.378098	55.975962
2793.937853	154763.125395	55.980967
2793.121174	154474.873372	55.985972
2792.612131	154166.720294	55.990977
2792.327273	153851.670592	55.995981
2791.036638	153558.989119	56.000986
2790.585499	153245.217153	56.005991
2789.985655	152951.211377	56.010996
2789.468398	152640.493453	56.016001
2788.688718	152330.709747	56.021005
2787.920604	152030.358177	56.026010
2787.583030	151716.252267	56.031015
2786.229509	151404.267637	56.036020
2785.771171	151105.832817	56.041025
2784.943473	150808.692085	56.046029
2784.372613	150499.655206	56.051034
2783.880322	150199.416579	56.056039
2783.217012	149910.150695	56.061044
2782.720888	149600.691137	56.066049
2781.788309	149297.073682	56.071053
2781.172832	148996.141328	56.076058
2780.897748	148683.274951	56.081063
2779.938127	148385.567385	56.086068
2779.477335	148075.240023	56.091073
2778.962067	147775.396237	56.096077
2777.947748	147465.975850	56.101082
2777.281741	147158.307902	56.106087
2776.620371	146858.661137	56.111092
2775.831082	146556.711886	56.116097
2775.325783	146249.942326	56.121101
2774.617360	145947.045726	56.126106
2774.163986	145644.950367	56.131111
2773.348239	145336.129435	56.136116
2772.846648	145046.323112	56.141121
2772.167964	144727.218810	56.146125
2771.106631	144418.966889	56.151130
2770.728320	144110.940230	56.156135
2770.194082	143811.099259	56.161140
2769.464117	143509.576775	56.166145
2769.000880	143186.756545	56.171149
2768.192237	142892.304848	56.176154
2767.918560	142581.151098	56.181159
2766.933168	142270.062431	56.186164
2766.318433	141968.168394	56.191169
2765.472890	141661.993826	56.196173
2764.771738	141348.201281	56.201178
2764.354233	141037.581648	56.206183
2763.659624	140743.336003	56.211188
2763.028836	140430.088204	56.216193
2762.270783	140123.597743	56.221197
2761.525593	139812.661501	56.226202
2760.858560	139499.848442	56.231207
2760.311914	139187.578616	56.236212
2759.610555	138881.053808	56.241217
2759.108316	138579.201413	56.246221
2758.243237	138258.873402	56.251226
2758.017053	137944.113891	56.256231
2756.811669	137643.233642	56.261236
2756.256234	137338.683602	56.266241
2755.624672	137028.571647	56.271245
2754.399288	136716.689549	56.276250
2754.167033	136412.402837	56.281255
2753.728715	136113.360488	56.286260
2752.934366	135805.599394	56.291265
2752.119839	135494.592662	56.296269
2751.371875	135197.387286	56.301274
2750.702082	134873.838774	56.306279
2750.023967	134579.194748	56.311284
2749.381596	134283.023720	56.316289
2748.627709	133972.900291	56.321293
2747.923067	133679.006466	56.326298
2747.611022	133361.591828	56.331303
2746.737379	133056.286176	56.336308
2745.847787	132765.759091	56.341313
2745.513758	132460.996758	56.346317
2744.604894	132168.992682	56.351322
2744.354365	131862.381766	56.356327
2743.316378	131556.813451	56.361332
2742.906756	131248.837213	56.366337
2742.443344	130937.799112	56.371341
2741.240773	130643.596513	56.376346
2740.715954	130334.784866	56.381351
2740.214855	130041.404666	56.386356
2739.245692	129731.222168	56.391361
2738.556174	129429.559158	56.396365
2738.088335	129132.157128	56.401370
2737.762874	128825.743770	56.406375
2736.982988	128528.854874	56.411380
2736.477757	128212.329203	56.416385
2736.239902	127918.510670	56.421389
2734.850721	127609.015429	56.426394
2734.095829	127293.085998	56.431399
2733.729830	127000.516783	56.436404
2733.061745	126689.622344	56.441409
2732.465172	126373.106999	56.446413
2731.302536	126079.340446	56.451418
2731.178985	125775.215085	56.456423
2730.375620	125467.010182	56.461428
2729.815820	125156.814593	56.466433
2729.183117	124841.211795	56.471437
2728.489133	124538.295519	56.476442
2728.152820	124225.218097	56.481447
2727.543673	123921.546141	56.486452
2726.231969	123608.211420	56.491457
2725.975004	123295.805303	56.496461
2725.166148	122987.223430	56.501466
2724.680881	122690.669322	56.506471
2723.654383	122381.798827	56.511476
2723.222173	122060.610254	56.516481
2722.841064	121762.208932	56.521485
2721.824737	121445.475521	56.526490
2721.395347	121131.928732	56.531495
2720.595216	120829.604854	56.536500
2719.972997	120515.131037	56.541505
2719.109153	120209.155107	56.546509
2718.023901	119906.728367	56.551514
2718.013052	119590.975375	56.556519
2716.973319	119301.016073	56.561524
2716.440284	118993.618166	56.566529
2715.746068	118678.054376	56.571533
2715.330347	118372.657529	56.576538
2714.754049	118060.059715	56.581543
2713.984969	117758.998121	56.586548
2713.181690	117442.755808	56.591553
2712.525769	117130.581816	56.596557
2712.038137	116830.210152	56.601562
2711.172086	116516.420284	56.606567
2710.406696	116220.460408	56.611572
2709.817820	115915.697887	56.616577
2709.019794	115595.935924	56.621581
2708.439979	115296.872735	56.626586
2707.709495	114988.138847	56.631591
2707.107414	114681.495547	56.636596
2706.138484	114377.744762	56.641601
2705.743305	114076.997588	56.646605
2704.885442	113788.462067	56.651610
2704.578897	113476.791857	56.656615
2703.687326	113162.324232	56.661620
2702.959914	112864.024198	56.666625
2702.414192	112557.201239	56.671629
2701.369581	112264.245132	56.676634
2701.071628	111959.617829	56.681639
2700.289115	111664.685358	56.686644
2699.634558	111356.853743	56.691649
2698.786966	111052.216823	56.696653
2698.420986	110760.510011	56.701658
2697.768344	110451.052186	56.706663
2696.943301	110152.349797	56.711668
2696.380804	109855.976371	56.716673
2696.137342	109548.343423	56.721677
2695.187367	109250.484080	56.726682
2694.755767	108932.374290	56.731687
2693.689626	108627.085169	56.736692
2693.291749	108333.654748	56.741697
2692.699651	108022.060790	56.746701
2691.876558	107724.231809	56.751706
2691.386585	107408.188049	56.756711
2690.443684	107115.962801	56.761716
2689.678056	106818.751368	56.766721
2689.191406	106503.328079	56.771725
2688.588339	106209.023373	56.776730
2687.988720	105905.744161	56.781735
2687.202932	105594.656501	56.786740
2686.325928	105294.061986	56.791745
2685.940760	104991.451976	56.796749
2685.268764	104696.434588	56.801754
2684.640229	104394.429050	56.806759
2683.739505	104072.835529	56.811764
2683.126202	103783.453783	56.816769
2682.611473	103464.306941	56.821773
2681.727782	103159.509219	56.826778
2681.322261	102859.600513	56.831783
2680.252860	102568.244273	56.836788
2679.726689	102262.703762	56.841793
2679.305024	101969.114565	56.846797
2678.291494	101664.509137	56.851802
2677.948643	101355.443546	56.856807
2677.336952	101060.551126	56.861812
2676.510306	100757.672377	56.866817
2675.728810	100448.999182	56.871821
2674.822349	100154.387020	56.876826
2674.206635	99856.859198	56.881831
2673.904439	99557.591999	56.886836
2673.108393	99252.844329	56.891841
2672.936064	98954.014750	56.896845
2672.088237	98648.858350	56.901850
2671.255290	98343.703665	56.906855
2670.485960	98046.090483	56.911860
2669.260726	97756.272079	56.916865
2669.084499	97459.612730	56.921869
2668.946700	97161.695410	56.926874
2667.893749	96854.388475	56.931879
2667.277507	96556.485158	56.936884
2666.501705	96260.589736	56.941889
2665.919845	95944.411575	56.946893
2664.953097	95648.015393	56.951898
2664.496392	95353.806284	56.956903
2664.033099	95058.314728	56.961908
2663.307042	94740.299246	56.966913
2662.993919	94447.645634	56.971917
2662.048237	94151.303963	56.976922
2661.626662	93833.938004	56.981927
2660.663588	93551.450037	56.986932
2659.944233	93236.467001	56.991937
2659.667478	92926.915949	56.996941
2658.757596	92636.473257	57.001946
2658.029732	92321.263633	57.006951
2657.372722	92018.887272	57.011956
2656.572913	91733.207262	57.016961
2655.920969	91411.905249	57.021965
2655.401246	91117.489612	57.026970
2654.717158	90816.738221	57.031975
2653.813378	90523.380528	57.036980
2653.445160	90211.618683	57.041985
2653.267434	89912.302133	57.046989
2652.146560	89611.782377	57.051994
2651.203948	89311.580888	57.056999
2651.014672	89008.493657	57.062004
2650.202223	88705.122685	57.067009
2649.896511	88397.573893	57.072013
2648.677903	88098.111311	57.077018
2648.328631	87790.229399	57.082023
2647.587440	87484.702521	57.087028
2646.721199	87198.414308	57.092033
2646.306991	86877.528436	57.097037
2645.624063	86583.263649	57.102042
2645.007359	86260.644149	57.107047
2644.354149	85972.062863	57.112052
2643.345693	85671.605666	57.117057
2642.970776	85360.060861	57.122061
2642.075197	85061.337567	57.127066
2641.488560	84747.648448	57.132071
2640.620963	84451.610544	57.137076
2640.024422	84156.072600	57.142081
2639.856515	83840.695266	57.147085
2638.814802	83547.518191	57.152090
2638.050694	83243.038315	57.157095
2637.355747	82933.912434	57.162100
2636.584883	82636.560066	57.167105
2636.101794	82338.767032	57.172109
2634.914587	82044.556588	57.177114
2634.766143	81737.263118	57.182119
2634.019277	81449.893035	57.187124
2633.057298	81144.892011	57.192129
2632.437069	80853.409733	57.197133
2631.878085	80559.253826	57.202138
2631.364409	80258.409123	57.207143
2630.834706	79970.587849	57.212148
2630.093831	79663.552049	57.217153
2629.358305	79367.818790	57.222157
2628.731290	79068.511258	57.227162
2628.189833	78769.739490	57.232167
2627.318211	78461.842526	57.237172
2626.448069	78182.375943	57.242177
2626.080365	77879.432810	57.247181
2624.970572	77588.885411	57.252186
2624.559580	77280.204562	57.257191
2623.652869	76997.363733	57.262196
2623.108781	76707.632670	57.267201
2622.385467	76409.754299	57.272205
2621.664935	76123.937199	57.277210
2621.190340	75824.672119	57.282215
2620.769982	75543.979378	57.287220
2619.814799	75235.770697	57.292225
2619.427830	74958.312015	57.297229
2618.450626	74659.086860	57.302234
2617.992253	74364.681213	57.307239
2617.298871	74063.436975	57.312244
2616.738545	73775.847592	57.317249
2616.330642	73483.201756	57.322253
2615.189124	73183.954994	57.327258
2614.713432	72885.785505	57.332263
2614.265918	72591.854027	57.337268
2613.151012	72307.382762	57.342273
2612.892116	72006.740545	57.347277
2612.246054	71716.451580	57.352282
2611.338151	71416.827011	57.357287
2611.133179	71128.345443	57.362292
2609.803329	70842.998139	57.367297
2609.337178	70527.918406	57.372301
2608.473437	70249.017389	57.377306
2608.170059	69938.842892	57.382311
2607.507297	69642.626830	57.387316
2606.605789	69355.282412	57.392321
2606.184247	69057.105168	57.397325
2605.482510	68766.159203	57.402330
2604.831499	68467.184964	57.407335
2604.081626	68177.864124	57.412340
2603.246894	67876.356707	57.417345
2602.720966	67588.092155	57.422349
2601.904171	67290.707598	57.427354
2601.163111	67008.090596	57.432359
2601.118924	66718.166715	57.437364
2599.612622	66432.607929	57.442369
2599.182169	66141.734335	57.447373
2598.522204	65842.007280	57.452378
2597.881086	65556.900640	57.457383
2597.262725	65259.842085	57.462388
2596.538178	64981.665942	57.467393
2596.214980	64677.828813	57.472397
2595.365349	64397.129085	57.477402
2594.659561	64101.188344	57.482407
2593.825249	63803.553431	57.487412
2593.207321	63522.772868	57.492417
2592.740847	63222.720616	57.497421
2591.876870	62954.419932	57.502426
2591.291672	62660.980354	57.507431
2590.613547	62373.220422	57.512436
2589.908539	62089.916950	57.517441
2589.101344	61801.306118	57.522445
2588.390077	61521.874273	57.527450
2587.752055	61223.428918	57.532455
2587.298333	60937.883882	57.537460
2586.428683	60662.614574	57.542465
2585.629418	60375.797029	57.547469
2585.206164	60081.637600	57.552474
2584.535472	59799.575556	57.557479
2583.764824	59520.717882	57.562484
2582.645546	59240.897264	57.567489
2582.318486	58944.258975	57.572493
2581.832130	58674.427652	57.577498
2581.274983	58393.634955	57.582503
2580.403504	58106.208610	57.587508
2579.725313	57832.435160	57.592513
2579.067504	57537.796090	57.597517
2578.239682	57269.947799	57.602522
2577.747929	56980.181065	57.607527
2577.093024	56708.686612	57.612532
2576.424343	56416.788899	57.617537
2575.870426	56137.409826	57.622541
2575.140036	55859.588335	57.627546
2574.630637	55574.068203	57.632551
2573.884600	55282.441310	57.637556
2573.239386	55019.448150	57.642561
2572.332852	54730.833299	57.647565
2571.625739	54449.684718	57.652570
2571.108007	54171.193834	57.657575
2570.483209	53895.435994	57.662580
2569.464136	53627.263117	57.667585
2569.064380	53337.662922	57.672589
2568.310815	53060.011188	57.677594
2567.599829	52789.156647	57.682599
2566.677388	52506.585175	57.687604
2566.159893	52237.163715	57.692609
2565.924589	51956.099275	57.697613
2564.675168	51684.267757	57.702618
2563.975677	51406.670870	57.707623
2563.682527	51137.587832	57.712628
2562.654431	50866.932700	57.717633
2562.535425	50584.795600	57.722637
2561.563320	50315.006800	57.727642
2560.945168	50033.659848	57.732647
2560.475187	49764.220545	57.737652
2559.634091	49487.963453	57.742657
2558.919996	49220.045281	57.747661
2558.186984	48942.646999	57.752666
2557.632052	48665.610757	57.757671
2557.042486	48402.904765	57.762676
2556.097239	48127.526797	57.767681
2555.670365	47844.722745	57.772685
2554.924325	47582.101192	57.777690
2554.183102	47309.063386	57.782695
2553.807466	47042.446717	57.787700
2552.887380	46765.890362	57.792705
2552.329659	46482.499457	57.797709
2551.380003	46221.375970	57.802714
2550.549854	45951.792485	57.807719
2550.244879	45680.697133	57.812724
2549.475619	45418.304535	57.817729
2548.866438	45141.626480	57.822733
2548.020527	44880.949342	57.827738
2547.388395	44617.174438	57.832743
2546.858943	44341.657136	57.837748
2546.212079	44080.830758	57.842753
2545.624040	43810.299548	57.847757
2544.457721	43530.497008	57.852762
2543.752889	43273.733578	57.857767
2543.357854	43012.823261	57.862772
2542.153873	42750.729583	57.867777
2542.082490	42496.568416	57.872781
2541.362447	42222.860598	57.877786
2540.471907	41974.876810	57.882791
2539.960128	41701.409890	57.887796
2539.308780	41452.453407	57.892801
2538.357795	41183.529207	57.897805
2537.679140	40916.561267	57.902810
2536.857168	40671.658881	57.907815
2536.356300	40411.705939	57.912820
2535.573917	40164.363566	57.917825
2534.838192	39903.236700	57.922829
2534.136735	39651.471910	57.927834
2533.362873	39405.002358	57.932839
2532.973404	39154.491759	57.937844
2531.843711	38909.453211	57.942849
2531.319859	38641.225381	57.947853
2530.490233	38399.874106	57.952858
2529.939499	38159.258201	57.957863
2529.387039	37910.634943	57.962868
2528.363324	37670.769604	57.967873
2527.887137	37415.385680	57.972877
2527.024382	37176.755315	57.977882
2526.116393	36947.900575	57.982887
2525.419294	36704.009311	57.987892
2524.674869	36478.689792	57.992897
2524.174723	36237.753460	57.997901
2523.139682	36015.753229	58.002906
2521.989630	35795.470060	58.007911
2521.560156	35561.889525	58.012916
2520.560931	35340.676491	58.017921
2519.690621	35133.592553	58.022925
2518.805012	34920.939431	58.027930
2517.687481	34726.472061	58.032935
2516.728042	34515.675412	58.037940
2515.807297	34321.284304	58.042945
2514.843906	34138.381929	58.047949
2513.615223	33962.970179	58.052954
2512.897511	33786.700182	58.057959
2511.967730	33617.300499	58.062964
2510.685926	33463.031165	58.067969
2509.987729	33295.979554	58.072973
2509.199055	33149.120738	58.077978
2508.212187	32993.119730	58.082983
2507.438626	32848.385041	58.087988
2506.522897	32707.771665	58.092993
2505.973425	32574.846017	58.097997
2505.241330	32443.571668	58.103002
2504.581536	32305.902970	58.108007
2503.940592	32175.935753	58.113012
2502.948514	32057.901684	58.118017
2502.422907	31920.723741	58.123021
2501.564230	31794.368339	58.128026
2501.053711	31672.469957	58.133031
2500.576291	31546.684905	58.138036
2499.979641	31424.026186	58.143041
2499.290821	31300.376480	58.148045
2498.392922	31179.100939	58.153050
2497.671046	31056.795051	58.158055
2497.273767	30923.994494	58.163060
2496.290062	30808.984387	58.168065
2495.702449	30695.169995	58.173069
2495.364466	30576.301852	58.178074
2494.747277	30466.677618	58.183079
2493.910023	30352.952582	58.188084
2493.114294	30224.448927	58.193089
2492.764581	30109.614986	58.198093
2491.889482	30002.622742	58.203098
2491.446142	29887.140045	58.208103
2491.157536	29758.485402	58.213108
2490.309685	29645.228318	58.218113
2489.795062	29519.001822	58.223117
2489.258150	29405.924614	58.228122
2488.509984	29282.283778	58.233127
2487.551971	29160.956913	58.238132
2486.888155	29055.789009	58.243137
2486.612742	28922.789497	58.248141
2485.777890	28821.138546	58.253146
2485.118206	28694.099388	58.258151
2484.600110	28568.169929	58.263156
2483.506480	28452.366054	58.268161
2483.093129	28335.873792	58.273165
2482.780459	28221.214755	58.278170
2482.210414	28104.012819	58.283175
2481.499009	27990.993661	58.288180
2480.575108	27863.067683	58.293185
2480.091248	27744.049034	58.298189
2479.386274	27625.055257	58.303194
2478.742037	27515.916482	58.308199
2478.275953	27381.850875	58.313204
2477.502522	27263.473272	58.318209
2476.901353	27151.594893	58.323213
2475.828442	27030.127654	58.328218
2475.536715	26923.767765	58.333223
2475.098692	26799.704955	58.338228
2474.110809	26683.175889	58.343233
2473.837131	26566.351989	58.348237
2473.214193	26437.487634	58.353242
2472.251806	26328.598470	58.358247
2472.033544	26194.064322	58.363252
2471.451003	26070.253558	58.368257
2470.489064	25943.208928	58.373261
2469.907275	25831.395098	58.378266
2469.100244	25710.265294	58.383271
2468.470658	25592.137808	58.388276
2467.632784	25483.382327	58.393281
2467.275481	25349.554122	58.398285
2466.765105	25236.426869	58.403290
2465.724954	25112.329611	58.408295
2465.030559	24996.186411	58.413300
2464.557611	24878.235214	58.418305
2463.895866	24760.751536	58.423309
2463.037541	24639.287334	58.428314
2462.596146	24517.910369	58.433319
2462.252436	24406.631021	58.438324
2461.172732	24282.529900	58.443329
2460.939083	24148.228593	58.448333
2460.218192	24037.280120	58.453338
2459.598093	23909.226933	58.458343
2459.045235	23779.281530	58.463348
2458.474469	23662.727284	58.468353
2457.669003	23531.847132	58.473357
2456.962589	23408.366437	58.478362
2456.004459	23286.351931	58.483367
2455.933783	23157.593073	58.488372
2454.531019	23050.031887	58.493377
2454.313055	22921.983699	58.498381
2453.765980	22784.566119	58.503386
2452.868407	22671.440300	58.508391
2452.380869	22539.430621	58.513396
2451.763866	22422.998621	58.518401
2451.049250	22294.504420	58.523405
2450.130508	22167.870750	58.528410
2449.406411	22054.381525	58.533415
2448.886473	21916.498954	58.538420
2448.042485	21811.593506	58.543425
2447.505467	21682.103369	58.548429
2447.050886	21558.931161	58.553434
2446.178787	21447.899254	58.558439
2445.785038	21330.663775	58.563444
2445.037880	21209.043999	58.568449
2444.170547	21081.441340	58.573453
2443.461267	20963.053392	58.578458
2443.027844	20846.586945	58.583463
2442.399743	20716.429535	58.588468
2441.580221	20607.638257	58.593473
2441.075627	20474.055324	58.598477
2440.420546	20362.298749	58.603482
2439.615313	20238.751537	58.608487
2438.980961	20120.592936	58.613492
2438.314627	19998.413128	58.618497
2437.593647	19875.938592	58.623501
2436.727498	19763.494222	58.628506
2435.932111	19640.060303	58.633511
2435.696990	19518.081133	58.638516
2434.810525	19407.699091	58.643521
2434.166679	19288.970393	58.648525
2433.653228	19173.856524	58.653530
2432.817481	19057.250464	58.658535
2432.097521	18940.780067	58.663540
2431.402647	18819.418431	58.668545
2430.882262	18704.834091	58.673549
2430.200332	18593.236514	58.678554
2429.388185	18483.393137	58.683559
2429.276219	18344.147127	58.688564
2428.397166	18243.848878	58.693569
2427.333408	18130.409557	58.698573
2427.071634	18011.984048	58.703578
2426.622370	17899.000763	58.708583
2425.921023	17771.254352	58.713588
2425.078595	17661.106036	58.718593
2424.484267	17535.527593	58.723597
2423.626574	17416.663163	58.728602
2422.612398	17303.753064	58.733607
2422.123642	17183.787611	58.738612
2421.230416	17083.177656	58.743617
2420.909927	16970.026008	58.748621
2420.226451	16861.483017	58.753626
2419.509225	16746.608677	58.758631
2418.779900	16633.206025	58.763636
2418.196760	16521.961691	58.768641
2417.791109	16404.172732	58.773645
2416.528929	16287.910834	58.778650
2415.768945	16185.381418	58.783655
2415.777716	16068.131343	58.788660
2414.862575	15968.936560	58.793665
2413.751958	15851.089275	58.798669
2413.110902	15743.926677	58.803674
2412.588700	15632.846321	58.808679
2411.649547	15538.835497	58.813684
2411.325490	15426.136730	58.818689
2410.493459	15322.253849	58.823693
2410.027574	15217.688728	58.828698
2408.946850	15102.087546	58.833703
2408.741563	14996.845493	58.838708
2407.852438	14905.161316	58.843713
2407.218851	14802.346229	58.848717
2406.572895	14681.423677	58.853722
2405.690258	14593.050408	58.858727
2404.989311	14478.630005	58.863732
2404.306589	14397.817135	58.868737
2404.038944	14277.134992	58.873741
2403.134971	14183.637508	58.878746
2402.128296	14084.606938	58.883751
2401.693900	13980.478327	58.888756
2401.063422	13883.621279	58.893761
2399.900847	13790.345070	58.898765
2399.295867	13700.465669	58.903770
2398.535098	13610.532289	58.908775
2398.082772	13511.729152	58.913780
2397.165827	13432.331562	58.918785
2396.643982	13325.192030	58.923789
2396.204008	13233.294355	58.928794
2395.440524	13145.629377	58.933799
2395.227408	13041.672817	58.938804
2394.355973	12951.440488	58.943809
2393.524210	12856.069958	58.948813
2393.090583	12760.194591	58.953818
2392.102421	12668.837836	58.958823
2391.826494	12580.114583	58.963828
2390.681908	12493.438238	58.968833
2390.360636	12392.854973	58.973837
2389.555890	12304.057594	58.978842
2388.547726	12218.691004	58.983847
2388.091817	12125.376863	58.988852
2387.301316	12031.257837	58.993857
2386.240038	11950.198307	58.998861
2385.617462	11867.098153	59.003866
2384.819943	11781.137427	59.008871
2384.618970	11703.158632	59.013876
2383.551159	11618.292723	59.018881
2382.946613	11541.619156	59.023885
2382.590438	11455.856989	59.028890
2381.665844	11375.729667	59.033895
2381.258495	11295.064681	59.038900
2380.586460	11218.867014	59.043905
2379.606462	11127.153729	59.048909
2379.244064	11057.706070	59.053914
2378.185010	10975.251880	59.058919
2377.937717	10885.039400	59.063924
2376.972887	10814.092604	59.068929
2376.645996	10741.442890	59.073933
2376.066150	10657.374098	59.078938
2374.705272	10575.135850	59.083943
2374.457149	10494.311815	59.088948
2373.617656	10416.476025	59.093953
2372.786886	10346.663683	59.098957
2372.388945	10270.525570	59.103962
2371.641581	10196.752608	59.108967
2371.079235	10118.052291	59.113972
2370.364559	10044.720663	59.118977
2369.566522	9967.810823	59.123981
2369.109063	9885.698174	59.128986
2368.475243	9819.765192	59.133991
2367.683208	9737.526923	59.138996
2366.924877	9668.548062	59.144001
2366.192975	9590.754714	59.149005
2365.423132	9521.745613	59.154010
2365.092251	9452.068802	59.159015
2364.685083	9363.097875	59.164020
2363.731202	9311.930027	59.169025
2362.879404	9227.244524	59.174029
2362.613181	9156.399102	59.179034
2361.845394	9091.178514	59.184039
2361.529231	9004.836600	59.189044
2360.619646	8932.797279	59.194049
2359.635522	8844.448319	59.199053
2359.071562	8773.271275	59.204058
2358.241753	8707.143120	59.209063
2357.386657	8632.505448	59.214068
2356.719435	8569.815390	59.219073
2356.387342	8502.011298	59.224077
2355.789895	8422.275823	59.229082
2354.985984	8360.025252	59.234087
2354.209639	8278.491855	59.239092
2353.711361	8218.353364	59.244097
2353.102004	8156.682590	59.249101
2352.336307	8086.509156	59.254106
2351.560911	8022.295915	59.259111
2351.224928	7945.421402	59.264116
2350.298404	7883.548043	59.269121
2349.714749	7804.813167	59.274125
2349.477654	7741.080983	59.279130
2348.539945	7674.944933	59.284135
2347.694701	7594.220578	59.289140
2347.093323	7544.229153	59.294145
2346.574099	7462.799855	59.299149
2345.692598	7393.948057	59.304154
2344.772480	7329.920888	59.309159
2344.490261	7262.147651	59.314164
2343.494449	7206.056015	59.319169
2342.802184	7142.711348	59.324173
2342.421967	7081.699694	59.329178
2341.565524	7014.257668	59.334183
2341.077484	6942.430102	59.339188
2340.250466	6880.988449	59.344193
2339.767289	6814.287196	59.349197
2339.184092	6744.297818	59.354202
2338.258532	6690.460061	59.359207
2337.544252	6608.693275	59.364212
2336.844466	6562.412319	59.369217
2336.198396	6495.930797	59.374221
2335.573057	6426.138124	59.379226
2334.978597	6370.746385	59.384231
2334.245437	6300.758432	59.389236
2333.451328	6250.080992	59.394241
2333.009468	6182.623537	59.399245
2332.595876	6113.540987	59.404250
2331.566495	6049.142297	59.409255
2331.407656	5988.634810	59.414260
2330.702566	5928.588076	59.419265
2329.751134	5868.467075	59.424269
2329.370931	5797.507413	59.429274
2328.444008	5736.475999	59.434279
2327.837262	5665.414082	59.439284
2327.272938	5607.492499	59.444289
2326.548203	5541.037208	59.449293
2325.974425	5478.719632	59.454298
2324.824433	5415.481768	59.459303
2324.354437	5351.997510	59.464308
2323.875616	5300.012940	59.469313
2323.029459	5235.901075	59.474317
2322.966947	5167.424268	59.479322
2321.878045	5104.055011	59.484327
2321.033648	5033.550436	59.489332
2320.248071	4986.920486	59.494337
2319.915501	4919.368648	59.499341
2319.405407	4861.733213	59.504346
2318.657118	4804.192568	59.509351
2317.653906	4734.642121	59.514356
2317.178320	4673.425223	59.519361
2316.201990	4611.851856	59.524365
2315.672761	4552.021020	59.529370
2314.770299	4497.144967	59.534375
2314.837870	4436.951002	59.539380
2313.812894	4384.191897	59.544385
2313.317279	4311.521813	59.549389
2312.697235	4248.859511	59.554394
2311.925402	4191.469326	59.559399
2311.164552	4126.808529	59.564404
2310.442390	4082.810253	59.569409
2309.342387	4015.819623	59.574413
2308.899469	3950.095756	59.579418
2308.212611	3905.682314	59.584423
2307.879399	3841.650537	59.589428
2306.980298	3795.495061	59.594433
2306.621723	3736.192531	59.599437
2306.013157	3675.537158	59.604442
2304.965156	3620.317600	59.609447
2304.832702	3554.222135	59.614452
2304.316234	3503.215173	59.619457
2303.359193	3443.146780	59.624461
2302.877644	3381.683852	59.629466
2302.246341	3315.559756	59.634471
2301.287024	3252.097509	59.639476
2300.460544	3195.844457	59.644481
2300.008223	3132.557035	59.649485
2299.508386	3074.482215	59.654490
2298.509639	3020.859556	59.659495
2297.884844	2959.886395	59.664500
2297.548491	2903.153755	59.669505
2296.421430	2859.224171	59.674509
2296.078529	2784.957090	59.679514
2295.525628	2726.168145	59.684519
2294.909092	2678.918617	59.689524
2294.001723	2619.836193	59.694529
2293.099427	2558.695018	59.699533
2292.699349	2485.569346	59.704538
2291.374351	2443.903286	59.709543
2291.187990	2381.497194	59.714548
2290.393244	2339.670047	59.719553
2289.751216	2283.025363	59.724557
2289.297180	2224.266918	59.729562
2288.553178	2171.728309	59.734567
2287.946043	2110.907297	59.739572
2287.163747	2060.855950	59.744577
2286.636498	2013.185949	59.749581
2286.208525	1944.912250	59.754586
2285.304746	1897.333106	59.759591
2284.320963	1853.029783	59.764596
2283.835090	1790.117020	59.769601
2282.959658	1754.530634	59.774605
2282.656870	1687.567752	59.779610
2281.738120	1646.482986	59.784615
2281.435356	1581.361013	59.789620
2280.391742	1537.265276	59.794625
2279.585324	1485.762548	59.799629
2279.602774	1430.355482	59.804634
2278.419376	1385.271502	59.809639
2277.753886	1330.566107	59.814644
2277.508109	1275.844807	59.819649
2276.763991	1226.701794	59.824653
2276.138051	1167.625576	59.829658
2275.294668	1119.127109	59.834663
2274.812735	1064.650650	59.839668
2273.834796	1004.744660	59.844673
2273.512490	951.165845	59.849677
2272.626685	900.198193	59.854682
2271.630210	854.674627	59.859687
2271.029457	801.154726	59.864692
2270.428008	761.797802	59.869697
2269.766804	718.132760	59.874701
2269.213087	663.872622	59.879706
2268.379337	627.053954	59.884711
2267.556649	570.362605	59.889716
2266.839770	519.970312	59.894721
2266.304112	497.022712	59.899725
2265.781839	435.078792	59.904730
2264.532322	398.009699	59.909735
2264.163325	354.059713	59.914740
2263.495031	302.465170	59.919745
2262.562850	268.826312	59.924750
2262.369989	223.828524	59.929754
2261.064118	196.066304	59.934759
2260.933251	145.747933	59.939764
2260.031350	111.806606	59.944769
2258.768797	86.456675	59.949774
2258.435940	50.171858	59.954778
2257.502327	23.122019	59.959783
2256.621889	-8.986938	59.964788
2253.594015	34.209527	59.969793
2250.790058	82.019259	59.974798
2251.171515	80.309429	59.979802
2251.314228	84.065112	59.984807
2252.198624	69.676190	59.989812
2251.518941	76.607291	59.994817
2250.871544	79.546908	59.999822
2249.666054	83.289386	60.004826
2249.287568	89.967720	60.009831
2249.113513	95.123470	60.014836
2248.357195	88.414053	60.019841
2247.204400	99.695157	60.024846
2246.385062	97.393674	60.029850
2245.854667	89.054186	60.034855
2245.639854	100.441952	60.039860
2244.864215	93.087498	60.044865
2243.926684	92.698607	60.049870
2243.656239	100.411591	60.054874
2243.016362	96.378602	60.059879
2242.491722	93.063740	60.064884
2241.544793	103.195754	60.069889
2240.278570	100.499982	60.074894
2240.435741	95.436998	60.079898
2240.182115	98.888142	60.084903
2239.474422	92.817537	60.089908
2238.916630	92.961317	60.094913
2237.252443	98.102731	60.099918
2236.831937	101.118321	60.104922
2235.945682	101.725775	60.109927
2235.369786	93.760921	60.114932
2235.119359	107.350944	60.119937
2234.705970	103.961665	60.124942
2234.059880	98.797458	60.129946
2233.486747	100.381794	60.134951
2232.776459	103.908537	60.139956
2231.678727	102.444396	60.144961
2231.038099	103.373994	60.149966
2230.592191	97.492086	60.154970
2229.703791	99.538003	60.159975
2228.919259	101.420793	60.164980
2228.585084	104.674992	60.169985
2228.112246	99.060696	60.174990
2227.778962	98.471878	60.179994
2226.991271	107.030135	60.184999
2225.754661	106.447432	60.190004
2225.269314	98.589633	60.195009
2224.652396	97.949622	60.200014
2224.054712	101.231431	60.205018
2223.391202	100.701309	60.210023
2222.654656	104.164414	60.215028
2222.026832	99.478263	60.220033
2220.999026	95.741779	60.225038
2220.326017	96.525134	60.230042
2219.874283	103.265557	60.235047
2220.089196	98.636517	60.240052
2219.252377	96.858189	60.245057
2217.698977	98.539695	60.250062
2217.334865	87.308634	60.255066
2216.919468	98.266190	60.260071
2216.642664	99.472373	60.265076
2216.077725	90.618000	60.270081
2214.206966	102.249549	60.275086
2214.066393	90.421652	60.280090
2213.866071	96.764234	60.285095
2213.261376	88.906456	60.290100
2212.341932	101.347407	60.295105
2211.103437	96.327651	60.300110
2211.162307	91.078422	60.305114
2210.138666	100.486207	60.310119
2209.637954	94.157279	60.315124
2209.056625	99.576331	60.320129
2208.250291	100.981635	60.325134
2207.881803	96.418343	60.330138
2207.168092	99.709101	60.335143
2206.442654	103.309214	60.340148
2205.886916	91.178190	60.345153
2205.051820	105.627333	60.350158
2204.367180	95.454752	60.355162
2203.422293	105.365689	60.360167
2202.881074	102.441379	60.365172
2202.437198	92.992239	60.370177
2201.648061	108.317150	60.375182
2201.150884	101.044682	60.380186
2200.367455	102.741233	60.385191
2199.665549	95.062874	60.390196
2199.302653	101.394982	60.395201
2198.312194	99.322504	60.400206
2197.833727	86.173175	60.405210
2197.515940	106.492991	60.410215
2196.628189	98.508239	60.415220
2196.030154	98.133309	60.420225
2194.523283	98.303097	60.425230
2194.580590	86.681922	60.430234
2194.238314	104.201919	60.435239
2193.157849	93.237468	60.440244
2192.315208	91.786489	60.445249
2191.829953	104.544899	60.450254
2191.524002	100.091531	60.455258
2190.218920	100.189885	60.460263
2189.820517	96.118601	60.465268
2189.767444	95.819631	60.470273
2188.107149	104.032232	60.475278
2187.849596	85.508520	60.480282
2187.470254	96.222246	60.485287
2186.251024	91.029144	60.490292
2186.164747	93.020350	60.495297
2185.262583	101.368125	60.500302
2184.400064	88.945176	60.505306
2183.968951	87.685941	60.510311
2183.003247	93.793578	60.515316
2183.467326	95.719544	60.520321
2182.047361	100.364946	60.525326
2181.721458	99.981535	60.530330
2180.892941	98.436859	60.535335
2180.242618	95.066261	60.540340
2179.808086	91.522661	60.545345
2179.011834	99.729059	60.550350
2178.171674	99.010942	60.555354
2176.982692	96.124759	60.560359
2176.273801	89.226502	60.565364
2176.588759	81.959233	60.570369
2175.250915	91.992436	60.575374
2174.505586	97.912155	60.580378
2174.025626	95.254089	60.585383
2173.785489	95.281254	60.590388
2172.703518	84.963583	60.595393
2171.741331	95.832859	60.600398
2171.520163	90.197573	60.605402
2171.125202	89.721047	60.610407
2170.249092	88.668029	60.615412
2169.651926	93.378423	60.620417
2169.086932	93.622704	60.625422
2168.563994	100.610960	60.630426
2168.243261	91.817200	60.635431
2166.820062	91.614198	60.640436
2165.904703	94.572698	60.645441
2164.863045	95.597477	60.650446
2165.271035	93.872387	60.655450
2164.328204	93.572670	60.660455
2163.366925	90.057459	60.665460
2162.816568	94.973306	60.670465
2162.077989	100.740578	60.675470
2161.448538	95.805556	60.680474
2160.866441	93.329271	60.685479
2160.576098	86.528608	60.690484
2159.890808	83.278679	60.695489
2159.343632	101.477703	60.700494
2159.018520	88.125864	60.705498
2158.051692	91.201337	60.710503
2156.684924	96.685097	60.715508
2156.053775	92.489907	60.720513
2155.466213	85.856247	60.725518
2155.042198	88.315761	60.730522
2154.414359	92.209466	60.735527
2153.746820	96.401196	60.740532
2153.584839	94.034865	60.745537
2152.800680	87.878657	60.750542
2152.275213	79.461153	60.755546
2151.033903	95.083296	60.760551
2149.868583	90.979172	60.765556
2149.611157	91.076889	60.770561
2148.832284	94.401652	60.775566
2148.739379	82.153065	60.780570
2147.960719	87.657047	60.785575
2147.193788	95.346309	60.790580
2146.971316	88.005045	60.795585
2146.578307	91.531923	60.800590
2145.335290	91.111117	60.805594
2144.203342	87.638763	60.810599
2143.334611	94.358625	60.815604
2143.061856	90.890284	60.820609
2142.032514	95.951520	60.825614
2142.055412	84.690611	60.830618
2141.354360	92.364689	60.835623
2140.683289	96.389832	60.840628
2140.494658	84.547502	60.845633
2140.018046	92.577035	60.850638
2138.790979	96.753475	60.855642
2137.592007	84.562126	60.860647
2136.636176	91.767297	60.865652
2136.537550	83.212685	60.870657
2135.451567	102.470141	60.875662
2135.129338	84.212165	60.880666
2134.806778	86.406436	60.885671
2134.126586	90.581253	60.890676
2133.876847	92.167907	60.895681
2133.019316	94.480180	60.900686
2132.270367	88.137050	60.905690
2131.213582	99.361956	60.910695
2130.439831	88.844016	60.915700
2129.959153	92.485727	60.920705
2129.051949	107.755268	60.925710
2128.727441	82.999310	60.930714
2128.027093	94.068310	60.935719
2127.445600	95.247157	60.940724
2127.232746	90.835797	60.945729
2126.358747	97.588039	60.950734
2125.100853	89.428677	60.955738
2124.350189	90.110842	60.960743
2123.741681	86.113912	60.965748
2123.493980	91.495803	60.970753
2122.743900	91.928728	60.975758
2122.201113	94.962158	60.980762
2121.610236	85.459104	60.985767
2121.242179	93.674832	60.990772
2120.706149	78.374338	60.995777
2119.503049	96.980199	61.000782
2118.687178	82.430551	61.005786
2118.124877	91.366199	61.010791
2117.342355	96.738345	61.015796
2117.332475	85.269761	61.020801
2116.433482	96.322979	61.025806
2115.655346	86.337153	61.030810
2114.378899	85.237300	61.035815
2113.714463	89.374929	61.040820
2113.467003	85.066832	61.045825
2112.458266	87.902976	61.050830
2112.294149	83.234739	61.055834
2112.017325	87.892731	61.060839
2111.426601	89.443613	61.065844
2110.915024	88.261811	61.070849
2109.408751	95.740411	61.075854
2108.764731	90.170657	61.080858
2108.203306	90.980486	61.085863
2107.710680	97.878787	61.090868
2107.223886	90.333478	61.095873
2106.783927	89.741105	61.100878
2105.542119	91.128812	61.105882
2104.448397	85.688767	61.110887
2104.044637	93.216333	61.115892
2103.654161	83.110654	61.120897
2102.881533	95.427405	61.125902
2102.671766	80.161871	61.130906
2102.082974	88.816307	61.135911
2101.320909	85.764650	61.140916
2100.582446	91.210228	61.145921
2100.064288	93.826609	61.150926
2099.677990	84.887161	61.155930
2098.475617	90.191899	61.160935
2096.989100	92.864181	61.165940
2096.820871	82.611277	61.170945
2096.112253	93.358333	61.175950
2095.844340	89.547047	61.180954
2095.056434	93.289554	61.185959
2094.465959	93.946307	61.190964
2094.337016	80.889778	61.195969
2093.436221	96.760666	61.200974
2092.456320	86.035771	61.205978
2091.748677	86.611774	61.210983
2090.940127	83.026627	61.215988
2090.532027	85.344859	61.220993
2089.878687	92.156704	61.225998
2089.668067	85.693471	61.231002
2088.844060	89.342364	61.236007
2087.428333	84.000734	61.241012
2086.866427	83.796707	61.246017
2086.233392	86.044983	61.251022
2085.731395	81.080302	61.256026
2085.224536	87.223955	61.261031
2084.678569	81.578730	61.266036
2084.536657	86.317811	61.271041
2083.187151	93.506628	61.276046
2082.543860	89.505766	61.281050
2081.975847	85.497690	61.286055
2081.339845	81.678593	61.291060
2081.105340	81.509339	61.296065
2079.849250	91.165346	61.301070
2078.713404	81.299381	61.306074
2078.195618	86.588521	61.311079
2077.163636	86.383405	61.316084
2077.892683	87.649162	61.321089
2077.082472	88.569438	61.326094
2076.285935	83.112206	61.331098
2075.734124	89.490066	61.336103
2074.282655	93.011469	61.341108
2073.960574	84.093374	61.346113
2073.086048	89.021256	61.351118
2072.764104	83.638513	61.356122
2072.031474	84.209025	61.361127
2071.372052	85.408134	61.366132
2071.144167	80.843059	61.371137
2069.835673	91.513437	61.376142
2069.258100	83.372294	61.381146
2068.662474	83.271390	61.386151
2068.117557	84.233141	61.391156
2067.820514	87.251232	61.396161
2067.064376	86.090906	61.401166
2066.117375	93.714148	61.406170
2065.124577	88.485175	61.411175
2064.720927	96.011150	61.416180
2064.320920	81.196844	61.421185
2063.719822	86.300521	61.426190
2062.710265	90.910806	61.431194
2061.982168	77.214546	61.436199
2060.913718	85.087284	61.441204
2060.530058	84.776131	61.446209
2059.751739	90.488228	61.451214
2059.620319	78.742491	61.456218
2059.447649	84.636000	61.461223
2058.678015	85.297540	61.466228
2057.826573	78.445605	61.471233
2056.755784	89.909278	61.476238
2056.266897	88.293398	61.481242
2055.395947	87.966544	61.486247
2054.996834	83.674639	61.491252
2054.035284	81.064647	61.496257
2053.314098	80.018621	61.501262
2052.552914	80.388675	61.506266
2052.476002	86.380523	61.511271
2051.955138	83.391523	61.516276
2051.532939	78.579759	61.521281
2050.001356	82.361457	61.526286
2049.097256	78.737876	61.531290
2048.651728	79.379519	61.536295
2047.997029	87.916694	61.541300
2047.993226	84.074538	61.546305
2047.184561	92.878992	61.551310
2046.737197	85.095642	61.556314
2045.551967	89.399514	61.561319
2044.773270	93.938475	61.566324
2044.529003	81.862157	61.571329
2043.874178	81.272359	61.576334
2043.211901	83.880083	61.581338
2042.200045	77.239686	61.586343
2041.538368	86.426067	61.591348
2041.071974	81.337479	61.596353
2040.618146	87.116346	61.601358
2040.009669	93.583627	61.606362
2039.270569	88.014794	61.611367
2037.993638	94.290136	61.616372
2037.499049	86.460669	61.621377
2036.751791	85.795660	61.626382
2036.437744	81.655830	61.631386
2036.090883	86.742816	61.636391
2035.177202	90.916866	61.641396
2034.194499	86.916274	61.646401
2032.822053	89.089536	61.651406
2032.291713	87.484970	61.656410
2032.072500	89.188207	61.661415
2031.516920	87.828910	61.666420
2031.007601	84.907465	61.671425
2030.730738	95.469318	61.676430
2030.237610	80.478999	61.681434
2029.728142	89.004166	61.686439
2028.768305	91.532971	61.691444
2027.801377	87.993481	61.696449
2027.138572	84.661178	61.701454
2026.693790	83.030420	61.706458
2025.716027	82.848256	61.711463
2024.593611	84.439391	61.716468
2024.198895	89.191789	61.721473
2023.679458	94.788695	61.726478
2023.413402	84.634904	61.731482
2023.002817	89.142251	61.736487
2022.139235	91.663665	61.741492
2021.283882	79.857801	61.746497
2020.155006	82.567971	61.751502
2019.911328	85.238566	61.756506
2019.580980	82.184645	61.761511
2018.842623	93.092543	61.766516
2017.937044	92.009563	61.771521
2017.262007	84.232397	61.776526
2016.702672	83.044003	61.781530
2016.133015	90.646788	61.786535
2015.298362	96.118692	61.791540
2014.027222	88.962816	61.796545
2013.353527	76.688174	61.801550
2013.198917	83.953856	61.806554
2012.981309	77.663628	61.811559
2011.897229	84.233204	61.816564
2011.610292	90.181120	61.821569
2011.011895	87.791035	61.826574
2009.944628	79.497413	61.831578
2009.224730	85.559776	61.836583
2008.406535	91.694512	61.841588
2008.350082	80.425717	61.846593
2007.427531	82.735731	61.851598
2006.863987	85.491788	61.856602
2006.115053	82.627305	61.861607
2004.722628	86.205599	61.866612
2004.728944	80.739229	61.871617
2004.377786	83.108354	61.876622
2003.942256	81.894005	61.881626
2002.888735	77.769058	61.886631
2002.128729	82.368134	61.891636
2001.358055	81.962308	61.896641
2000.697002	83.636333	61.901646
2000.175112	85.605224	61.906650
1999.194435	77.657393	61.911655
1998.382606	91.049505	61.916660
1998.297318	84.238401	61.921665
1997.435695	82.774732	61.926670
1997.037202	85.266484	61.931674
1996.764649	83.788158	61.936679
1995.555703	82.302352	61.941684
1995.012745	73.245883	61.946689
1994.218029	80.053373	61.951694
1993.361385	81.047272	61.956698
1992.406027	77.781917	61.961703
1991.891596	79.082604	61.966708
1991.553404	78.048340	61.971713
1990.818733	88.572473	61.976718
1990.378163	70.766987	61.981722
1990.083879	76.077427	61.986727
1989.115533	80.692231	61.991732
1988.211900	72.588683	61.996737
1987.482168	81.883638	62.001742
1987.241234	75.499350	62.006746
1986.180360	75.852341	62.011751
1985.059665	76.553857	62.016756
1984.502486	77.273154	62.021761
1984.326713	79.283297	62.026766
1983.469622	72.326640	62.031770
1983.248618	74.988906	62.036775
1982.381998	85.593904	62.041780
1981.598420	83.726785	62.046785
1980.725215	88.755403	62.051790
1980.225310	83.055588	62.056794
1979.639599	92.160541	62.061799
1979.158667	86.990699	62.066804
1978.618628	72.362652	62.071809
1977.535249	85.737944	62.076814
1976.893454	77.706371	62.081818
1976.804697	83.644904	62.086823
1975.867428	87.392226	62.091828
1975.062965	86.711086	62.096833
1974.292445	84.424023	62.101838
1973.906217	87.112518	62.106842
1973.494637	81.510644	62.111847
1972.121572	94.848354	62.116852
1971.375513	86.037003	62.121857
1970.951149	91.721321	62.126862
1970.229856	90.230654	62.131866
1969.835063	78.512548	62.136871
1969.476906	89.749589	62.141876
1968.651834	89.213641	62.146881
1967.843141	88.153146	62.151886
1966.853224	86.449666	62.156890
1966.886864	81.925090	62.161895
1965.479997	86.795584	62.166900
1964.610749	77.259508	62.171905
1964.036684	78.779391	62.176910
1963.583042	81.532202	62.181914
1963.344886	83.454482	62.186919
1962.867463	85.504626	62.191924
1962.471782	80.146224	62.196929
1961.378700	86.616328	62.201934
1960.384189	83.847609	62.206938
1960.179138	81.073415	62.211943
1959.121916	86.162787	62.216948
1958.389583	75.961613	62.221953
1957.356305	71.565404	62.226958
1957.009044	78.792281	62.231962
1956.736385	87.555817	62.236967
1956.054631	84.172929	62.241972
1955.618732	75.025363	62.246977
1954.225982	84.826102	62.251982
1953.655716	88.124106	62.256986
1953.343364	79.207650	62.261991
1952.891975	86.071033	62.266996
1952.332104	82.343961	62.272001
1950.988746	88.335004	62.277006
1950.538859	87.952383	62.282010
1950.229339	77.247297	62.287015
1949.285990	77.397151	62.292020
1948.718292	84.305803	62.297025
1947.764569	80.264380	62.302030
1946.876163	80.621547	62.307034
1947.044880	71.907837	62.312039
1946.366672	78.165433	62.317044
1945.419322	81.925402	62.322049
1944.367334	78.628099	62.327054
1943.825407	76.402526	62.332058
1943.529925	83.673223	62.337063
1942.683267	78.093118	62.342068
1942.096243	88.174369	62.347073
1941.188732	83.912733	62.352078
1940.064138	91.682467	62.357082
1939.959179	73.019510	62.362087
1939.308489	93.043637	62.367092
1939.068541	67.859637	62.372097
1938.567751	79.912484	62.377102
1936.827837	75.587462	62.382106
1936.798744	78.321763	62.387111
1935.978804	88.351685	62.392116
1935.887201	83.075896	62.397121
1934.613967	82.041851	62.402126
1934.020481	84.531451	62.407130
1933.530156	82.001234	62.412135
1932.761855	95.372258	62.417140
1932.298373	78.322594	62.422145
1931.114345	86.604788	62.427150
1930.142138	83.980767	62.432154
1929.833628	81.774909	62.437159
1929.376920	93.696196	62.442164
1929.130191	82.549078	62.447169
1928.497041	86.030526	62.452174
1927.551045	81.073294	62.457178
1926.548326	84.875174	62.462183
1925.951626	85.439916	62.467188
1925.662143	76.828906	62.472193
1925.295574	84.790525	62.477198
1924.575204	82.254254	62.482202
1923.463278	80.365168	62.487207
1922.757268	82.852134	62.492212
1922.265123	83.761384	62.497217
1921.985436	80.238987	62.502222
1920.819455	74.378440	62.507226
1920.197720	81.164793	62.512231
1919.694437	89.003045	62.517236
1919.004007	76.627024	62.522241
1917.476909	78.884815	62.527246
1917.090108	75.205968	62.532250
1917.391154	70.735133	62.537255
1916.409578	81.828302	62.542260
1915.827050	79.658064	62.547265
1915.292857	80.198692	62.552270
1913.916018	87.652104	62.557274
1913.526844	80.113431	62.562279
1912.882427	81.477344	62.567284
1912.738796	74.757515	62.572289
1912.127702	82.280159	62.577294
1910.767076	82.021633	62.582298
1910.240403	76.799152	62.587303
1909.673906	90.213826	62.592308
1909.173255	80.426874	62.597313
1908.040339	84.381889	62.602318
1907.307584	77.714589	62.607322
1907.038264	72.845473	62.612327
1906.392200	82.972366	62.617332
1906.229374	68.002202	62.622337
1905.598047	82.570398	62.627342
1904.202924	86.749961	62.632346
1903.746107	80.288001	62.637351
1902.991865	83.180003	62.642356
1902.459601	75.891123	62.647361
1901.354326	80.371582	62.652366
1900.535095	80.921198	62.657370
1900.140065	77.331966	62.662375
1899.549673	79.087832	62.667380
1899.067552	75.510850	62.672385
1898.894576	80.289552	62.677390
1898.316320	79.848477	62.682394
1897.439048	76.875100	62.687399
1896.494010	80.115925	62.692404
1895.833795	83.749903	62.697409
1894.888941	75.525211	62.702414
1894.227740	80.663687	62.707418
1893.951674	71.739911	62.712423
1893.388074	82.107591	62.717428
1892.805061	73.970526	62.722433
1891.895926	80.741014	62.727438
1890.911013	84.707228	62.732442
1890.495135	77.895012	62.737447
1889.834293	77.542741	62.742452
1889.467206	72.736456	62.747457
1888.373063	79.173635	62.752462
1887.881341	90.824527	62.757466
1887.288708	84.850887	62.762471
1886.860438	88.118475	62.767476
1885.980914	83.063978	62.772481
1884.784697	76.169086	62.777486
1884.192493	88.857747	62.782490
1883.630269	78.528673	62.787495
1883.501158	85.952723	62.792500
1883.077525	79.722031	62.797505
1881.914691	85.138842	62.802510
1881.112328	82.082617	62.807514
1881.072066	80.597386	62.812519
1880.189690	82.409076	62.817524
1879.448305	83.435172	62.822529
1878.555144	77.953933	62.827534
1877.768566	86.482111	62.832538
1877.300770	76.871297	62.837543
1876.784426	82.947097	62.842548
1875.809075	75.697037	62.847553
1875.288851	74.592348	62.852558
1874.666965	80.662829	62.857562
1874.433781	77.144094	62.862567
1873.268233	82.424150	62.867572
1872.587999	74.237876	62.872577
1871.951775	72.803115	62.877582
1870.800964	74.454011	62.882586
1871.039362	71.417041	62.887591
1870.432816	76.053280	62.892596
1869.593135	70.524135	62.897601
1868.757572	75.564149	62.902606
1868.004215	81.130405	62.907610
1867.888991	66.911171	62.912615
1866.697427	75.601414	62.917620
1865.943057	75.252960	62.922625
1865.412318	72.710253	62.927630
1864.788233	83.423415	62.932634
1864.257226	68.849171	62.937639
1863.173658	81.959604	62.942644
1862.635095	81.332470	62.947649
1862.077990	74.578954	62.952654
1861.738755	77.461839	62.957658
1861.143233	70.433741	62.962663
1859.801893	77.785346	62.967668
1859.158417	74.981433	62.972673
1858.947241	79.845045	62.977678
1858.392131	88.136212	62.982682
1857.895403	75.172822	62.987687
1856.668058	86.558910	62.992692
1856.087903	88.634844	62.997697
1855.773538	77.500061	63.002702
1854.943988	87.241379	63.007706
1854.007084	82.943446	63.012711
1853.043441	89.303153	63.017716
1852.588942	82.069742	63.022721
1852.352212	74.647223	63.027726
1852.100505	78.717793	63.032730
1851.359052	78.826164	63.037735
1850.066833	72.244566	63.042740
1849.703567	77.983840	63.047745
1849.075959	76.716444	63.052750
1847.875713	90.089831	63.057754
1847.325882	78.626601	63.062759
1846.773525	89.657948	63.067764
1846.419276	78.015437	63.072769
1846.094090	75.845354	63.077774
1845.138875	84.447621	63.082778
1844.424822	77.936638	63.087783
1843.752084	76.025158	63.092788
1843.271573	78.388032	63.097793
1842.205425	79.032064	63.102798
1840.894525	85.328647	63.107802
1840.781463	84.045778	63.112807
1840.261629	86.900576	63.117812
1839.805516	83.420396	63.122817
1839.315390	79.217100	63.127822
1838.159314	86.137197	63.132826
1837.532534	85.560344	63.137831
1836.859112	87.223758	63.142836
1836.464763	81.630215	63.147841
1836.192026	82.767979	63.152846
1835.036418	80.307154	63.157850
1834.224159	83.318768	63.162855
1833.601507	83.356243	63.167860
1833.021306	75.690236	63.172865
1832.635483	82.079615	63.177870
1831.474409	74.881142	63.182874
1830.989167	81.986441	63.187879
1830.242332	79.840737	63.192884
1829.941232	77.936477	63.197889
1829.855667	66.732263	63.202894
1828.556904	76.585931	63.207898
1827.863309	67.198640	63.212903
1827.425115	78.309618	63.217908
1826.343990	74.457203	63.222913
1825.280168	81.723758	63.227918
1824.576688	81.740956	63.232922
1824.541847	74.556030	63.237927
1824.107780	76.939916	63.242932
1823.623402	74.686310	63.247937
1822.823189	77.585631	63.252942
1821.859109	76.218713	63.257946
1821.392909	66.964042	63.262951
1820.527798	72.415594	63.267956
1819.552796	74.558963	63.272961
1819.141268	71.431239	63.277966
1818.808238	68.800381	63.282970
1818.101115	81.849472	63.287975
1816.867752	75.506116	63.292980
1816.219236	80.636285	63.297985
1815.596070	82.195534	63.302990
1814.796114	81.663531	63.307994
1814.585382	71.647659	63.312999
1814.289063	80.588404	63.318004
1814.077566	72.977391	63.323009
1812.687798	74.139580	63.328014
1811.823791	87.330278	63.333018
1811.710847	62.268087	63.338023
1810.419164	72.842844	63.343028
1809.569585	62.327636	63.348033
1809.400017	60.240076	63.353038
1808.772462	72.226326	63.358042
1808.486400	66.888399	63.363047
1807.071336	78.473032	63.368052
1806.725244	68.309933	63.373057
1806.176125	75.917361	63.378062
1805.227276	76.525434	63.383066
1804.372875	75.230989	63.388071
1803.629183	74.756284	63.393076
1803.181104	71.724249	63.398081
1803.175593	64.268180	63.403086
1802.141975	67.086305	63.408090
1801.612622	73.383363	63.413095
1800.459829	76.415947	63.418100
1799.706583	73.035000	63.423105
1799.714579	70.614905	63.428110
1799.045576	71.454494	63.433114
1798.404146	73.436095	63.438119
1797.122222	78.736237	63.443124
1796.597541	69.897692	63.448129
1796.771751	69.390760	63.453134
1795.189324	69.787230	63.458138
1794.676910	69.116536	63.463143
1794.019734	68.241761	63.468148
1793.308127	80.809043	63.473153
1793.205807	72.015383	63.478158
1791.618640	79.030760	63.483162
1791.505353	67.577077	63.488167
1790.931199	67.805547	63.493172
1790.296231	73.734621	63.498177
1789.590029	68.811907	63.503182
1788.361480	82.916740	63.508186
1788.166517	68.970369	63.513191
1787.352772	85.213805	63.518196
1787.209567	67.477863	63.523201
1786.238130	71.408855	63.528206
1784.983046	76.010913	63.533210
1784.791701	66.542301	63.538215
1784.487687	77.285059	63.543220
1783.453896	78.706107	63.548225
1783.122390	63.944104	63.553230
1781.964386	70.749409	63.558234
1781.458712	64.914957	63.563239
1780.952257	72.703259	63.568244
1780.685350	71.389636	63.573249
1779.657858	75.745828	63.578254
1778.788979	71.747770	63.583258
1778.327479	59.940984	63.588263
1777.795015	81.035944	63.593268
1776.992031	70.492845	63.598273
1776.066800	67.328445	63.603278
1775.579143	75.891164	63.608282
1775.343992	68.141998	63.613287
1774.414699	70.527269	63.618292
1773.160868	74.012705	63.623297
1773.036507	72.520334	63.628302
1772.283167	76.967025	63.633306
1772.095361	66.515460	63.638311
1771.213228	72.097454	63.643316
1770.305765	70.674259	63.648321
1770.216919	67.610411	63.653326
1769.197696	72.611812	63.658330
1768.165462	66.247582	63.663335
1767.306445	72.907644	63.668340
1766.986912	71.156124	63.673345
1766.791033	72.325841	63.678350
1765.873019	67.655959	63.683354
1764.664003	70.508260	63.688359
1764.493861	72.482827	63.693364
1763.687573	66.439089	63.698369
1763.509631	67.175470	63.703374
1762.137071	68.514715	63.708378
1761.809275	73.704339	63.713383
1760.935519	76.640587	63.718388
1760.285626	76.783326	63.723393
1760.140621	75.499228	63.728398
1758.895529	87.698683	63.733402
1758.101934	76.151203	63.738407
1758.094984	78.963981	63.743412
1757.195878	76.820407	63.748417
1756.633191	69.836009	63.753422
1755.569268	84.266352	63.758426
1755.249406	76.215263	63.763431
1754.450277	74.948324	63.768436
1753.917722	75.174926	63.773441
1753.242973	70.748674	63.778446
1751.993464	72.323836	63.783450
1751.816476	62.931796	63.788455
1751.257344	70.488781	63.793460
1750.809876	74.866399	63.798465
1749.882412	78.456123	63.803470
1748.984894	71.499675	63.808474
1748.660394	64.901633	63.813479
1748.207718	70.342891	63.818484
1747.205508	63.486649	63.823489
1746.771859	62.489658	63.828494
1746.089088	71.513852	63.833498
1745.337530	70.989954	63.838503
1744.223483	73.212200	63.843508
1743.262924	74.165915	63.848513
1743.120525	77.042780	63.853518
1742.233276	65.782989	63.858522
1742.052427	75.938510	63.863527
1741.915496	74.262066	63.868532
1740.969235	72.848197	63.873537
1740.101949	68.663830	63.878542
1739.281830	68.247013	63.883546
1738.975357	76.645348	63.888551
1737.539419	63.714489	63.893556
1737.055058	68.727140	63.898561
1736.850973	67.471350	63.903566
1736.041813	71.616270	63.908570
1735.717968	68.424176	63.913575
1734.596001	75.301043	63.918580
1734.017920	73.128567	63.923585
1733.727241	68.803740	63.928590
1732.326566	64.070191	63.933594
1731.606548	63.738397	63.938599
1730.911891	70.988920	63.943604
1730.519515	68.455807	63.948609
1730.303600	69.598747	63.953614
1729.637390	67.948025	63.958618
1729.338820	71.240758	63.963623
1727.869892	76.119644	63.968628
1727.569642	79.477299	63.973633
1727.282592	68.431252	63.978638
1725.875061	76.668592	63.983642
1725.167919	62.474024	63.988647
1724.582357	74.802104	63.993652
1724.091991	73.440405	63.998657
1723.597041	67.214775	64.003662
1722.842411	75.258534	64.008666
1722.569005	72.148312	64.013671
1722.001080	70.204451	64.018676
1720.383297	66.390018	64.023681
1720.091473	70.058554	64.028686
1719.120285	64.988727	64.033690
1718.787190	67.168940	64.038695
1718.411277	77.659780	64.043700
1717.758147	64.357030	64.048705
1716.953677	64.049693	64.053710
1716.156935	73.172415	64.058714
1715.764173	69.420442	64.063719
1714.729629	65.287882	64.068724
1714.153048	67.804799	64.073729
1713.723324	69.716524	64.078734
1712.900758	68.890116	64.083738
1712.228043	59.195220	64.088743
1711.204058	60.237863	64.093748
1710.589605	83.485665	64.098753
1710.498076	71.492399	64.103758
1709.781800	78.091960	64.108762
1709.465529	73.460556	64.113767
1708.350167	73.133219	64.118772
1707.387174	75.659477	64.123777
1707.172132	71.182298	64.128782
1706.044689	71.784083	64.133786
1705.309837	68.649393	64.138791
1704.501336	73.934297	64.143796
1703.960507	75.795866	64.148801
1703.857279	73.456514	64.153806
1703.534765	77.062122	64.158810
1702.639020	68.490693	64.163815
1701.721565	76.662817	64.168820
1701.145751	71.881838	64.173825
1700.895678	69.532698	64.178830
1699.370678	82.128271	64.183834
1698.686724	67.187318	64.188839
1698.672015	64.357692	64.193844
1697.575024	71.129683	64.198849
1696.773715	71.179800	64.203854
1695.747626	78.065106	64.208858
1695.364930	67.851081	64.213863
1695.048250	62.647343	64.218868
1694.707817	79.138862	64.223873
1694.269087	68.061725	64.228878
1692.919503	69.173440	64.233882
1692.336106	69.721928	64.238887
1691.958404	69.356271	64.243892
1691.478622	72.018658	64.248897
1690.616318	61.992779	64.253902
1689.712613	69.959301	64.258906
1689.441709	61.914650	64.263911
1688.323616	68.451887	64.268916
1687.124440	73.562321	64.273921
1686.857464	62.060536	64.278926
1686.415063	68.391102	64.283930
1686.006197	73.631453	64.288935
1685.677832	69.383579	64.293940
1684.458535	70.214419	64.298945
1683.358189	59.866829	64.303950
1682.687205	72.001909	64.308954
1682.561171	71.925843	64.313959
1682.609538	69.852558	64.318964
1681.232556	67.280323	64.323969
1680.534595	64.377889	64.328974
1679.681493	64.748459	64.333978
1679.564283	60.627889	64.338983
1678.652087	66.030188	64.343988
1677.732025	63.473680	64.348993
1677.706037	69.037968	64.353998
1676.685902	77.677396	64.359002
1675.704174	66.664444	64.364007
1675.215491	59.281986	64.369012
1674.650222	71.002901	64.374017
1674.478648	61.018688	64.379022
1673.092818	70.731709	64.384026
1672.405117	75.958011	64.389031
1671.986404	71.943676	64.394036
1671.420016	71.087626	64.399041
1670.658517	63.863616	64.404046
1669.340580	60.864137	64.409050
1669.317289	58.616166	64.414055
1668.870572	61.628099	64.419060
1668.210209	74.553086	64.424065
1667.137525	62.253669	64.429070
1666.507556	65.178024	64.434074
1665.784386	70.755296	64.439079
1665.782290	64.978067	64.444084
1664.661308	71.827994	64.449089
1663.687401	68.354419	64.454094
1662.990784	70.381084	64.459098
1662.889435	66.483486	64.464103
1662.884576	66.755584	64.469108
1661.566946	79.557915	64.474113
1660.928165	70.396931	64.479118
1660.067719	70.270383	64.484122
1659.408645	65.149424	64.489127
1658.334607	69.295442	64.494132
1657.528343	74.084864	64.499137
1657.444073	72.275488	64.504142
1656.589474	72.643150	64.509146
1656.557429	76.827061	64.514151
1655.820583	65.923445	64.519156
1654.415766	66.160904	64.524161
1654.148201	61.860804	64.529166
1653.586693	72.360625	64.534170
1652.830280	64.412028	64.539175
1651.963140	65.183786	64.544180
1651.391726	77.034988	64.549185
1651.583261	74.861693	64.554190
1649.558742	70.977885	64.559194
1648.712762	63.328932	64.564199
1648.344556	60.558619	64.569204
1647.839787	72.725643	64.574209
1647.846773	64.991649	64.579214
1647.448994	72.862045	64.584218
1646.501324	68.337264	64.589223
1645.990060	67.366812	64.594228
1645.015632	78.548793	64.599233
1644.314808	60.376381	64.604238
1643.091845	66.685878	64.609242
1642.759553	62.951121	64.614247
1642.340844	59.687386	64.619252
1641.729341	77.048244	64.624257
1641.020895	63.615548	64.629262
1640.122872	75.256874	64.634266
1639.501457	59.192747	64.639271
1639.320535	68.410030	64.644276
1638.426122	72.114380	64.649281
1637.394255	67.276566	64.654286
1636.654234	73.763224	64.659290
1636.365456	65.625231	64.664295
1635.782639	70.000711	64.669300
1634.487262	73.697801	64.674305
1634.114087	66.710141	64.679310
1633.380885	66.618577	64.684314
1633.350050	78.295599	64.689319
1632.913510	63.575556	64.694324
1631.434623	80.720996	64.699329
1630.839057	64.066163	64.704334
1630.338690	64.688202	64.709338
1629.847528	71.244129	64.714343
1629.260230	68.161712	64.719348
1628.150651	69.978038	64.724353
1627.691856	69.746692	64.729358
1627.234394	75.573483	64.734362
1626.510509	71.979782	64.739367
1626.115325	70.416910	64.744372
1625.051385	70.209167	64.749377
1624.429249	62.794309	64.754382
1623.209621	71.766624	64.759386
1622.351116	70.914418	64.764391
1622.232907	72.109649	64.769396
1621.484535	64.659655	64.774401
1621.283403	64.155575	64.779406
1621.087239	71.654914	64.784410
1620.033260	62.003275	64.789415
1619.215633	67.571909	64.794420
1618.490795	77.287173	64.799425
1618.133983	68.556048	64.804430
1617.029439	69.088004	64.809434
1616.180258	72.800943	64.814439
1615.954907	64.282313	64.819444
1615.035720	79.659468	64.824449
1614.066637	60.083696	64.829454
1613.418170	76.490112	64.834458
1612.877266	59.741456	64.839463
1612.802620	74.448295	64.844468
1611.998789	69.736682	64.849473
1611.528367	67.326371	64.854478
1610.445753	73.840656	64.859482
1610.202640	70.509606	64.864487
1609.853340	67.819869	64.869492
1608.595633	66.979053	64.874497
1607.753726	63.473492	64.879502
1607.466980	61.664751	64.884506
1606.150044	74.200496	64.889511
1605.293785	70.725599	64.894516
1604.701742	71.884153	64.899521
1604.341484	60.353057	64.904526
1603.834298	66.482622	64.909530
1603.616502	63.316277	64.914535
1603.397347	71.527284	64.919540
1602.023593	64.004777	64.924545
1601.131976	61.968877	64.929550
1600.742118	71.700302	64.934554
1599.953418	64.042269	64.939559
1599.284074	63.112712	64.944564
1598.192958	75.199443	64.949569
1598.137455	65.259874	64.954574
1597.515483	72.063658	64.959578
1596.733941	72.840757	64.964583
1595.913706	63.934122	64.969588
1595.426298	78.026910	64.974593
1595.072217	69.594962	64.979598
1593.948354	64.896358	64.984602
1593.061302	69.064728	64.989607
1592.976038	61.369051	64.994612
1592.078490	67.786131	64.999617
1590.939003	72.513401	65.004622
1590.316816	71.617351	65.009626
1589.987195	64.028302	65.014631
1589.582484	69.605452	65.019636
1588.845926	60.669759	65.024641
1588.259728	66.119632	65.029646
1587.084482	62.971377	65.034650
1586.339325	63.357941	65.039655
1586.354415	57.007163	65.044660
1585.756957	70.218612	65.049665
1584.741804	61.141113	65.054670
1584.055500	63.041585	65.059674
1583.776973	62.516692	65.064679
1582.957452	63.823350	65.069684
1581.551551	70.537235	65.074689
1581.512279	63.960137	65.079694
1581.103926	70.126040	65.084698
1580.543151	64.428121	65.089703
1579.861069	61.825955	65.094708
1578.654086	73.339773	65.099713
1578.289517	65.959694	65.104718
1577.513778	78.600267	65.109722
1576.357133	67.898993	65.114727
1575.794074	68.795918	65.119732
1575.174576	66.412455	65.124737
1574.986441	58.116569	65.129742
1574.699640	66.428202	65.134746
1573.683735	72.274345	65.139751
1573.000519	70.199035	65.144756
1572.176648	68.256454	65.149761
1571.612462	59.089964	65.154766
1570.509138	78.200454	65.159770
1570.247832	60.937480	65.164775
1569.657571	60.242934	65.169780
1569.192851	65.553667	65.174785
1568.521432	66.750070	65.179790
1567.568708	65.107072	65.184794
1566.907544	66.300270	65.189799
1566.414594	65.344270	65.194804
1565.533056	62.043708	65.199809
1564.355222	63.728987	65.204814
1564.088051	69.030409	65.209818
1563.794911	62.764872	65.214823
1563.387029	63.947787	65.219828
1562.331804	66.782047	65.224833
1561.606318	59.295327	65.229838
1560.821199	61.451190	65.234842
1560.420516	67.261079	65.239847
1559.878854	60.051065	65.244852
1558.973145	63.011371	65.249857
1558.508404	69.030125	65.254862
1558.116331	58.700944	65.259866
1557.045061	57.344855	65.264871
1556.164046	65.137502	65.269876
1555.074355	66.260028	65.274881
1554.847248	61.797404	65.279886
1554.382477	65.397242	65.284890
1554.055608	64.323397	65.289895
1553.078996	58.667910	65.294900
1551.999044	66.801236	65.299905
1551.803576	67.180887	65.304910
1551.540829	65.816170	65.309914
1550.285435	68.474094	65.314919
1549.825097	61.654839	65.319924
1548.791725	71.889044	65.324929
1548.571554	66.867105	65.329934
1548.369205	64.021570	65.334938
1547.071133	63.715451	65.339943
1546.363746	58.107070	65.344948
1545.723571	58.691418	65.349953
1545.235577	65.861829	65.354958
1544.141613	63.033400	65.359962
1543.714174	65.376848	65.364967
1543.390891	53.940818	65.369972
1542.708706	65.429596	65.374977
1541.926486	61.490397	65.379982
1541.050363	66.360330	65.384986
1540.139421	71.847624	65.389991
1540.003625	66.891122	65.394996
1539.149892	70.759339	65.400001
1538.464649	50.905145	65.405006
1537.626714	63.752703	65.410010
1537.433895	62.011043	65.415015
1536.813784	56.470794	65.420020
1535.828460	67.922593	65.425025
1535.080267	61.529109	65.430030
1534.578749	60.689589	65.435034
1534.328971	58.348309	65.440039
1533.503964	57.851914	65.445044
1532.277779	64.300732	65.450049
1531.810738	55.312775	65.455054
1531.521581	61.119134	65.460058
1530.685806	63.927995	65.465063
1529.907826	54.289319	65.470068
1529.165304	67.285714	65.475073
1528.900580	60.911596	65.480078
1527.825482	62.591603	65.485082
1526.740544	63.055830	65.490087
1526.402521	62.841580	65.495092
1525.745308	56.480950	65.500097
1525.548298	51.803826	65.505102
1525.351064	61.744323	65.510106
1524.164029	56.779842	65.515111
1523.754373	57.100495	65.520116
1522.735916	63.029054	65.525121
1521.856539	51.906891	65.530126
1520.862592	72.239422	65.535130
1520.026080	66.951171	65.540135
1520.286339	67.143294	65.545140
1519.770962	72.485738	65.550145
1519.105181	59.292310	65.555150
1517.799974	67.106647	65.560154
1517.357869	60.757564	65.565159
1517.426176	61.287680	65.570164
1515.914989	56.589168	65.575169
1515.223845	56.405804	65.580174
1514.647094	67.248661	65.585178
1514.244779	70.146335	65.590183
1514.022850	65.388017	65.595188
1512.712563	68.557703	65.600193
1512.111826	65.483760	65.605198
1511.685387	62.115628	65.610202
1510.238014	65.718663	65.615207
1509.720089	60.703049	65.620212
1509.069450	65.604964	65.625217
1508.786133	59.530256	65.630222
1508.052656	63.956505	65.635226
1507.887749	62.812776	65.640231
1507.428160	59.418377	65.645236
1506.253873	68.265263	65.650241
1505.662175	52.779919	65.655246
1505.034876	59.586136	65.660250
1503.880255	59.148438	65.665255
1503.636229	60.587582	65.670260
1502.684491	54.399914	65.675265
1502.484161	56.044991	65.680270
1501.657694	54.323611	65.685274
1500.607107	52.699345	65.690279
1500.444845	59.975681	65.695284
1499.552183	60.508707	65.700289
1498.592730	59.226332	65.705294
1498.036104	60.161671	65.710298
1497.090423	65.334391	65.715303
1496.876100	67.093651	65.720308
1496.449502	64.657478	65.725313
1495.962314	60.936324	65.730318
1494.797421	65.003804	65.735322
1494.397187	67.937416	65.740327
1493.986178	57.409423	65.745332
1492.814101	68.663843	65.750337
1492.005508	54.222169	65.755342
1491.699019	59.726948	65.760346
1491.126010	63.186308	65.765351
1490.844240	52.341329	65.770356
1489.560721	56.861300	65.775361
1489.170718	54.245859	65.780366
1488.826273	68.864673	65.785370
1487.353016	63.639782	65.790375
1487.051834	63.602598	65.795380
1486.230100	66.019755	65.800385
1485.892276	61.308244	65.805390
1484.937124	61.720326	65.810394
1483.755552	65.755770	65.815399
1483.696752	60.268249	65.820404
1483.148413	60.528952	65.825409
1482.730989	57.909985	65.830414
1481.958527	56.454404	65.835418
1480.742625	61.659034	65.840423
1480.432380	49.311098	65.845428
1479.885805	56.225907	65.850433
1479.445356	56.862105	65.855438
1478.344162	72.597769	65.860442
1477.531919	68.780050	65.865447
1477.239110	57.328153	65.870452
1476.449510	66.992229	65.875457
1475.520798	51.640878	65.880462
1474.969733	64.767693	65.885466
1474.072361	55.310430	65.890471
1474.021817	60.900684	65.895476
1473.238010	59.333374	65.900481
1472.753243	51.447332	65.905486
1472.066799	59.978587	65.910490
1471.140801	62.276706	65.915495
1471.105840	57.909707	65.920500
1469.787103	55.257377	65.925505
1468.891655	57.208461	65.930510
1468.525347	58.490432	65.935514
1467.970964	57.449604	65.940519
1466.979241	54.511927	65.945524
1466.108801	70.098960	65.950529
1465.729098	59.422503	65.955534
1465.505127	63.461874	65.960538
1464.830243	65.701164	65.965543
1463.880168	66.705350	65.970548
1462.994974	61.241942	65.975553
1462.818701	61.270061	65.980558
1462.048693	56.262987	65.985562
1460.795860	58.743933	65.990567
1460.721033	55.840299	65.995572
1459.867821	51.587579	66.000577
1459.202553	59.773291	66.005582
1458.802461	55.820696	66.010586
1457.956371	52.582349	66.015591
1457.405327	49.029042	66.020596
1456.741259	66.582743	66.025601
1456.295024	64.927095	66.030606
1454.989584	70.882368	66.035610
1454.284933	61.840735	66.040615
1454.096867	63.622630	66.045620
1453.633664	65.353642	66.050625
1452.497805	66.294324	66.055630
1452.085983	64.634785	66.060634
1451.017501	78.903505	66.065639
1450.924538	61.919723	66.070644
1450.214779	73.058107	66.075649
1449.342706	64.598141	66.080654
1448.635777	60.293790	66.085658
1448.222218	68.106783	66.090663
1447.577523	69.399889	66.095668
1446.523711	70.180884	66.100673
1445.974458	59.018897	66.105678
1445.629327	66.770554	66.110682
1444.747399	62.120299	66.115687
1444.519905	55.418599	66.120692
1443.523857	68.594067	66.125697
1443.035106	56.976213	66.130702
1442.121189	56.151798	66.135706
1440.886781	66.350178	66.140711
1440.647130	61.947907	66.145716
1440.172955	66.104313	66.150721
1439.719935	66.745669	66.155726
1438.885544	53.402469	66.160730
1438.014713	71.706515	66.165735
1437.745300	54.712944	66.170740
1436.951012	61.892625	66.175745
1435.880128	57.644549	66.180750
1435.110430	60.460281	66.185754
1434.515969	62.035549	66.190759
1434.590159	57.312177	66.195764
1433.814078	68.568328	66.200769
1433.045464	60.454608	66.205774
1432.200245	69.162491	66.210778
1431.462394	67.799190	66.215783
1431.199462	58.996426	66.220788
1429.958859	61.976887	66.225793
1429.484417	62.870795	66.230798
1429.003981	62.923608	66.235802
1428.460773	63.800062	66.240807
1427.509865	50.314549	66.245812
1426.724292	56.783255	66.250817
1426.309570	60.253735	66.255822
1426.061293	67.720355	66.260826
1424.823011	67.874701	66.265831
1424.027506	48.474885	66.270836
1423.553646	55.340299	66.275841
1423.057866	64.407355	66.280846
1422.682007	57.391790	66.285850
1421.374758	62.842764	66.290855
1420.961396	56.834473	66.295860
1420.506473	51.149740	66.300865
1419.493152	54.158731	66.305870
1419.051921	49.446327	66.310874
1417.943132	65.003443	66.315879
1417.795651	51.267235	66.320884
1417.340354	58.569647	66.325889
1416.308313	59.585300	66.330894
1415.708035	55.210396	66.335898
1414.689456	66.238603	66.340903
1414.547135	54.613000	66.345908
1413.450760	65.060670	66.350913
1412.555878	58.641664	66.355918
1412.156137	59.944725	66.360922
1411.570489	70.024228	66.365927
1411.133966	54.493756	66.370932
1410.875904	54.498611	66.375937
1410.149798	65.902930	66.380942
1409.281612	51.317814	66.385946
1408.513772	60.844407	66.390951
1408.027195	59.147876	66.395956
1406.599716	60.910750	66.400961
1406.075935	52.332374	66.405966
1405.758002	57.476297	66.410970
1405.295405	68.457131	66.415975
1404.596887	54.851088	66.420980
1403.932504	62.713411	66.425985
1403.284901	60.662451	66.430990
1402.811489	47.728647	66.435994
1401.778826	64.735422	66.440999
1401.360603	54.396250	66.446004
1400.701003	55.035758	66.451009
1399.506195	61.605790	66.456014
1398.822960	49.695612	66.461018
1398.355405	62.020721	66.466023
1398.218332	45.572232	66.471028
1397.503028	59.313325	66.476033
1396.347742	53.795114	66.481038
1395.976215	51.492127	66.486042
1394.819484	56.863994	66.491047
1394.581153	62.368984	66.496052
1394.126082	65.722887	66.501057
1392.939197	65.954230	66.506062
1392.461627	58.136445	66.511066
1391.994491	67.378716	66.516071
1391.535386	45.850287	66.521076
1390.329540	53.759257	66.526081
1389.776828	59.963888	66.531086
1389.408523	58.387325	66.536090
1388.467152	46.984939	66.541095
1388.438341	47.596716	66.546100
1387.173917	61.204338	66.551105
1386.386050	60.331523	66.556110
1386.254804	48.095500	66.561114
1385.603312	62.603849	66.566119
1384.525083	53.963811	66.571124
1383.824418	50.591994	66.576129
1383.484051	54.457490	66.581134
1382.761196	55.570657	66.586138
1381.759749	65.189583	66.591143
1381.078775	57.429364	66.596148
1380.581663	58.818866	66.601153
1380.407890	63.898878	66.606158
1379.588853	52.642617	66.611162
1378.451395	61.266083	66.616167
1377.837843	46.247870	66.621172
1377.716866	56.911056	66.626177
1377.167612	52.991651	66.631182
1376.178809	54.055637	66.636186
1374.956817	52.526478	66.641191
1374.824253	42.924039	66.646196
1374.509104	53.878272	66.651201
1373.261567	47.051749	66.656206
1372.753734	53.566196	66.661210
1371.977244	51.081597	66.666215
1371.903588	32.218327	66.671220
1370.602449	52.077745	66.676225
1369.732263	52.063222	66.681230
1369.449962	47.987850	66.686234
1368.620952	51.942063	66.691239
1368.221305	48.954460	66.696244
1367.109746	51.338879	66.701249
1366.623650	52.234649	66.706254
1366.212007	55.031325	66.711258
1365.678609	54.438168	66.716263
1365.058924	51.280552	66.721268
1364.004006	55.926656	66.726273
1363.610964	47.912530	66.731278
1363.243582	50.621749	66.736282
1361.981018	60.517139	66.741287
1361.187815	42.526718	66.746292
1360.772728	64.205344	66.751297
1360.457825	51.274737	66.756302
1359.817479	54.036810	66.761306
1358.735646	65.423574	66.766311
1358.444999	44.267330	66.771316
1357.802919	61.450125	66.776321
1356.932285	54.797068	66.781326
1356.055989	51.151997	66.786330
1355.293855	56.197814	66.791335
1355.116949	52.432099	66.796340
1354.751265	56.943408	66.801345
1353.957538	48.489961	66.806350
1353.268526	54.356738	66.811354
1352.301131	59.821520	66.816359
1351.334421	59.298828	66.821364
1350.531110	51.137048	66.826369
1350.164098	53.959744	66.831374
1349.779625	55.340807	66.836378
1349.260301	50.257655	66.841383
1348.476850	60.381219	66.846388
1347.513051	58.587112	66.851393
1346.812653	52.616586	66.856398
1346.531426	51.324215	66.861402
1345.507945	46.368520	66.866407
1344.780085	58.465367	66.871412
1344.248538	51.472996	66.876417
1343.867119	53.831231	66.881422
1343.693336	52.176445	66.886426
1342.654606	54.240230	66.891431
1341.668244	53.219223	66.896436
1341.165409	57.295046	66.901441
1339.942330	51.062284	66.906446
1339.543425	51.417525	66.911450
1338.627080	52.208246	66.916455
1338.591601	44.340699	66.921460
1338.294501	54.106260	66.926465
1336.949804	51.171140	66.931470
1336.502589	42.908606	66.936474
1335.884782	52.602157	66.941479
1335.453362	43.349994	66.946484
1334.233900	36.671990	66.951489
1333.623845	52.611847	66.956494
1333.289437	43.915087	66.961498
1332.486116	51.425788	66.966503
1331.408383	43.905280	66.971508
1330.625563	45.784889	66.976513
1330.055251	52.979442	66.981518
1329.959561	43.366417	66.986522
1329.511269	52.266661	66.991527
1329.192469	43.491732	66.996532
1328.038083	46.773902	67.001537
1327.112563	59.722147	67.006542
1326.932134	41.516059	67.011546
1325.709902	47.828714	67.016551
1325.090369	47.192494	67.021556
1324.590092	42.524192	67.026561
1323.852086	42.266333	67.031566
1322.961975	48.713835	67.036570
1322.252594	52.204366	67.041575
1321.785032	58.728188	67.046580
1321.129445	56.342648	67.051585
1320.925878	50.271067	67.056590
1320.062483	57.177924	67.061594
1318.818710	63.989150	67.066599
1318.786960	51.721549	67.071604
1318.471243	51.948456	67.076609
1317.053106	62.029440	67.081614
1316.607432	50.291248	67.086618
1315.622037	44.369201	67.091623
1315.255150	47.141420	67.096628
1314.931015	45.259820	67.101633
1313.877563	54.461273	67.106638
1313.482704	48.178847	67.111642
1312.683501	61.400310	67.116647
1312.578925	53.493287	67.121652
1311.200015	56.292375	67.126657
1310.498670	41.501030	67.131662
1310.348194	49.220159	67.136666
1309.124684	62.649425	67.141671
1308.299787	50.381780	67.146676
1307.513462	63.348901	67.151681
1307.340876	64.907582	67.156686
1307.310277	49.661100	67.161690
1306.534558	61.440730	67.166695
1305.640919	52.951148	67.171700
1304.920796	51.160892	67.176705
1304.046445	60.562521	67.181710
1303.338608	45.127269	67.186714
1302.545256	51.430091	67.191719
1302.166188	58.457057	67.196724
1301.605123	53.678580	67.201729
1300.070788	57.256127	67.206734
1299.756821	46.220785	67.211738
1299.092975	47.211057	67.216743
1298.796170	48.598686	67.221748
1298.533638	50.116477	67.226753
1297.687353	50.520779	67.231758
1297.185828	49.755422	67.236762
1296.350606	60.057530	67.241767
1295.941361	40.946442	67.246772
1294.513795	50.789243	67.251777
1293.744521	51.671707	67.256782
1293.467957	46.578357	67.261786
1292.956184	62.601943	67.266791
1292.122263	38.747362	67.271796
1291.068091	44.344220	67.276801
1290.833377	44.015810	67.281806
1290.456761	42.418510	67.286810
1289.887268	49.242373	67.291815
1288.844836	42.034802	67.296820
1288.387859	41.986145	67.301825
1287.692199	41.686873	67.306830
1286.877908	42.051400	67.311834
1285.525647	48.238098	67.316839
1285.144056	43.046338	67.321844
1284.675486	44.470740	67.326849
1284.453387	45.493275	67.331854
1284.211101	41.783695	67.336858
1282.937140	45.868598	67.341863
1282.093082	44.903833	67.346868
1281.783635	41.955520	67.351873
1281.135127	47.721257	67.356878
1280.367838	38.273371	67.361882
1279.154331	46.240364	67.366887
1279.196983	50.765596	67.371892
1278.812642	43.570079	67.376897
1277.444904	55.976821	67.381902
1277.303322	33.544888	67.386906
1276.173910	46.117144	67.391911
1275.849439	44.265564	67.396916
1274.965899	46.801411	67.401921
1274.275037	44.911899	67.406926
1274.011469	46.830380	67.411930
1273.019827	47.737169	67.416935
1272.140255	48.006431	67.421940
1271.310131	45.855228	67.426945
1270.707463	55.973713	67.431950
1270.743069	37.091511	67.436954
1269.634468	56.008921	67.441959
1269.019997	46.226093	67.446964
1268.392208	45.472935	67.451969
1267.632765	50.888906	67.456974
1267.376052	49.874906	67.461978
1266.502607	53.306387	67.466983
1265.441336	50.129133	67.471988
1265.028177	55.677691	67.476993
1264.169078	41.732997	67.481998
1264.185201	48.031686	67.487002
1263.089012	54.417363	67.492007
1262.469711	48.899148	67.497012
1261.882981	52.274002	67.502017
1261.396593	53.554593	67.507022
1260.365618	51.000116	67.512026
1259.591170	53.195364	67.517031
1258.987287	51.601091	67.522036
1258.751738	48.904366	67.527041
1257.884880	54.829403	67.532046
1257.201037	55.445995	67.537050
1256.414562	55.446584	67.542055
1255.851749	51.120959	67.547060
1255.435887	53.994008	67.552065
1254.589770	53.925238	67.557070
1253.844986	45.298481	67.562074
1253.670376	52.504236	67.567079
1252.541723	49.970025	67.572084
1251.544600	47.645122	67.577089
1250.925406	59.390409	67.582094
1250.634255	46.173799	67.587098
1249.955372	54.197714	67.592103
1249.615010	59.171759	67.597108
1248.802715	48.799108	67.602113
1247.922935	53.953538	67.607118
1247.382014	53.681707	67.612122
1246.410313	47.587211	67.617127
1245.309751	52.138119	67.622132
1245.408217	50.755424	67.627137
1244.465246	47.612981	67.632142
1244.373681	51.049440	67.637146
1243.214690	43.798927	67.642151
1242.345622	53.838357	67.647156
1241.818598	39.978058	67.652161
1241.443185	51.629384	67.657166
1241.225582	39.131177	67.662170
1239.825587	53.276034	67.667175
1239.335891	48.535110	67.672180
1238.874763	46.352049	67.677185
1237.920248	53.336490	67.682190
1237.093306	46.058407	67.687194
1236.493538	51.387496	67.692199
1236.112991	42.963009	67.697204
1235.778147	48.300430	67.702209
1234.515365	47.894247	67.707214
1233.821332	41.826563	67.712218
1233.280641	42.529201	67.717223
1232.856212	56.008026	67.722228
1232.212497	48.044832	67.727233
1231.278225	49.204273	67.732238
1231.010221	44.959502	67.737242
1230.337536	55.508571	67.742247
1229.354724	50.327276	67.747252
1228.512215	54.944382	67.752257
1227.830807	52.712777	67.757262
1227.992846	46.660339	67.762266
1226.809151	44.841328	67.767271
1225.639663	50.623696	67.772276
1225.355969	50.966941	67.777281
1224.684179	51.529588	67.782286
1224.571264	48.931630	67.787290
1223.570859	46.932095	67.792295
1222.699414	37.842976	67.797300
1222.535571	46.136627	67.802305
1221.424081	53.907661	67.807310
1221.040780	44.766142	67.812314
1219.972519	44.040466	67.817319
1219.620305	49.120468	67.822324
1219.275217	46.502665	67.827329
1217.968379	49.284031	67.832334
1217.672853	48.378705	67.837338
1216.908572	51.018600	67.842343
1216.384560	43.892615	67.847348
1215.519952	39.998176	67.852353
1214.552110	46.980009	67.857358
1214.329558	42.046808	67.862362
1213.681782	45.943859	67.867367
1212.783321	47.535980	67.872372
1212.359361	51.108873	67.877377
1211.778523	51.453644	67.882382
1211.303858	43.909828	67.887386
1210.106551	46.829888	67.892391
1209.364015	52.506520	67.897396
1208.847726	51.683609	67.902401
1208.134443	56.400012	67.907406
1208.035789	49.556446	67.912410
1206.901565	51.695390	67.917415
1206.238713	58.050019	67.922420
1205.464838	46.832387	67.927425
1205.233286	49.986774	67.932430
1204.476549	49.350327	67.937434
1203.553673	56.441705	67.942439
1202.939755	51.226986	67.947444
1202.483232	54.019781	67.952449
1201.612655	52.490012	67.957454
1200.935602	51.293723	67.962458
1200.150952	55.209392	67.967463
1199.671648	59.710402	67.972468
1199.563740	43.364552	67.977473
1198.711450	53.169523	67.982478
1197.882593	46.057332	67.987482
1197.061796	42.840290	67.992487
1196.270955	53.073858	67.997492
1195.842641	44.122419	68.002497
1194.929174	47.572901	68.007502
1194.408712	50.677046	68.012506
1193.723338	55.950377	68.017511
1192.945497	53.327287	68.022516
1192.028778	43.155766	68.027521
1191.300168	55.126603	68.032526
1191.290712	46.911175	68.037530
1190.886504	52.237555	68.042535
1190.237331	47.889415	68.047540
1189.586391	43.748127	68.052545
1188.707039	49.444945	68.057550
1187.625753	50.878504	68.062554
1186.677940	51.339987	68.067559
1186.193071	43.290052	68.072564
1185.655065	50.734938	68.077569
1184.953247	51.884234	68.082574
1184.917521	45.700831	68.087578
1184.099051	51.460505	68.092583
1183.194476	58.894312	68.097588
1182.904482	44.147981	68.102593
1181.706241	42.047471	68.107598
1181.162995	44.455113	68.112602
1180.395661	56.361153	68.117607
1180.135163	49.565406	68.122612
1179.496570	54.653114	68.127617
1178.072477	53.624523	68.132622
1177.960932	54.582178	68.137626
1177.564706	57.780103	68.142631
1176.728533	60.089265	68.147636
1175.775435	53.192370	68.152641
1174.927498	56.004845	68.157646
1174.623619	50.561063	68.162650
1174.246518	53.278157	68.167655
1173.505907	43.947486	68.172660
1172.882036	41.634213	68.177665
1172.055289	56.328135	68.182670
1171.346933	45.819147	68.187674
1170.360743	48.874372	68.192679
1169.620179	48.172290	68.197684
1169.389585	41.915810	68.202689
1168.506922	58.397328	68.207694
1168.512485	42.288891	68.212698
1167.513884	49.319784	68.217703
1166.411041	51.472676	68.222708
1166.099022	40.435484	68.227713
1165.197373	44.852288	68.232718
1164.494066	44.082784	68.237722
1163.615867	55.705278	68.242727
1163.145179	41.153264	68.247732
1162.935285	40.078217	68.252737
1162.376279	49.760859	68.257742
1161.745168	45.493430	68.262746
1160.824961	52.690044	68.267751
1160.378562	47.782990	68.272756
1159.481110	38.469390	68.277761
1158.245853	53.759686	68.282766
1157.896359	52.481350	68.287770
1157.423184	49.775126	68.292775
1156.926290	51.435853	68.297780
1156.244195	48.926852	68.302785
1155.115130	57.515944	68.307790
1154.787204	47.096257	68.312794
1154.323521	49.216877	68.317799
1153.670432	40.542463	68.322804
1152.649976	51.753945	68.327809
1152.142023	45.434354	68.332814
1151.759269	49.998855	68.337818
1150.814428	47.571066	68.342823
1150.062735	51.509889	68.347828
1149.581700	41.563966	68.352833
1149.029449	54.093351	68.357838
1148.497796	48.417736	68.362842
1147.634623	54.141954	68.367847
1146.565700	56.522836	68.372852
1146.448815	43.324268	68.377857
1145.308994	53.476165	68.382862
1144.567167	41.892364	68.387866
1143.903998	51.038099	68.392871
1143.533569	54.916283	68.397876
1143.263869	51.028164	68.402881
1142.293192	59.978401	68.407886
1141.496207	50.282990	68.412890
1140.933078	49.629960	68.417895
1140.418416	62.826694	68.422900
1140.208265	49.195128	68.427905
1138.763307	59.352990	68.432910
1137.949276	56.945397	68.437914
1137.612484	49.499511	68.442919
1136.987878	67.117914	68.447924
1136.264271	56.472595	68.452929
1135.406785	63.599324	68.457934
1134.800558	58.339247	68.462938
1134.225248	51.424857	68.467943
1133.741716	57.727325	68.472948
1133.165847	55.999325	68.477953
1132.040612	55.358439	68.482958
1131.615165	44.227337	68.487962
1131.641365	49.466340	68.492967
1130.375169	55.685152	68.497972
1129.965517	54.055287	68.502977
1128.904891	59.547583	68.507982
1128.671524	53.266317	68.512986
1127.590334	55.888840	68.517991
1126.942145	64.742060	68.522996
1126.849682	55.420263	68.528001
1125.683128	53.090824	68.533006
1124.787459	48.849717	68.538010
1124.577036	57.950251	68.543015
1124.102245	56.010645	68.548020
1123.396456	45.704684	68.553025
1122.006977	55.628235	68.558030
1121.956768	52.228725	68.563034
1121.490424	57.311123	68.568039
1120.515127	54.306328	68.573044
1119.728576	50.656534	68.578049
1118.923503	58.985959	68.583054
1118.869871	52.729718	68.588058
1117.937788	58.548481	68.593063
1116.826592	64.056712	68.598068
1116.444546	52.226462	68.603073
1115.854570	62.081191	68.608078
1115.262804	57.939970	68.613082
1114.189244	60.302680	68.618087
1113.547270	69.118649	68.623092
1113.041749	55.004240	68.628097
1112.430764	66.387141	68.633102
1112.200324	66.854384	68.638106
1111.341002	66.469235	68.643111
1110.010974	57.669129	68.648116
1110.178710	52.683319	68.653121
1109.574296	54.747490	68.658126
1108.346969	53.749137	68.663130
1107.809050	52.237445	68.668135
1107.553690	59.530159	68.673140
1106.725989	50.268555	68.678145
1105.888839	65.850348	68.683150
1105.223862	58.213831	68.688154
1104.807341	62.154543	68.693159
1104.048690	62.164945	68.698164
1103.052948	55.052527	68.703169
1102.402555	61.231741	68.708174
1102.018297	46.626573	68.713178
1101.647708	49.680087	68.718183
1100.461643	54.962124	68.723188
1099.898113	52.697614	68.728193
1099.369456	60.719738	68.733198
1098.766457	56.999754	68.738202
1097.669686	58.215053	68.743207
1096.900852	53.911204	68.748212
1096.710858	50.067181	68.753217
1096.048970	57.620093	68.758222
1095.878058	53.331512	68.763226
1094.635278	61.080903	68.768231
1094.070561	61.889888	68.773236
1093.353862	54.119688	68.778241
1092.797401	66.559876	68.783246
1092.346168	61.272002	68.788250
1091.508301	59.508423	68.793255
1090.484876	62.919665	68.798260
1090.335048	55.161786	68.803265
1089.254363	58.714593	68.808270
1088.531950	49.120876	68.813274
1088.074759	51.644151	68.818279
1087.603898	56.936994	68.823284
1086.900699	55.371179	68.828289
1085.804239	60.591664	68.833294
1085.349478	54.497001	68.838298
1084.932930	56.094501	68.843303
1084.063229	51.895007	68.848308
1083.563911	50.206880	68.853313
1082.821164	59.712198	68.858318
1082.323336	54.534237	68.863322
1081.634925	52.259637	68.868327
1080.395236	55.522368	68.873332
1079.647724	51.853764	68.878337
1079.173077	56.740380	68.883342
1079.297363	51.324691	68.888346
1078.694390	54.506634	68.893351
1077.590014	57.588579	68.898356
1077.246094	51.889424	68.903361
1076.343376	56.336389	68.908366
1075.009023	53.987939	68.913370
1074.344930	56.378561	68.918375
1073.990968	52.913841	68.923380
1073.879399	49.705434	68.928385
1073.360874	52.426115	68.933390
1072.463230	50.460754	68.938394
1071.736508	56.193248	68.943399
1071.028943	55.798164	68.948404
1070.400942	47.460386	68.953409
1068.952145	58.358438	68.958414
1068.550282	53.868494	68.963418
1068.338063	58.393262	68.968423
1067.963686	56.188549	68.973428
1067.438110	45.497570	68.978433
1066.190823	57.372756	68.983438
1065.732666	47.861582	68.988442
1065.136682	52.299173	68.993447
1063.906552	52.439783	68.998452
1063.576301	44.024682	69.003457
1062.702434	51.292793	69.008462
1062.522421	59.002428	69.013466
1062.068016	46.300667	69.018471
1060.739949	50.107291	69.023476
1060.149571	52.270159	69.028481
1059.577582	51.320530	69.033486
1059.216665	52.265824	69.038490
1058.726004	53.684318	69.043495
1057.665633	59.004721	69.048500
1057.132091	52.403812	69.053505
1056.517881	60.385938	69.058510
1055.222360	61.358500	69.063514
1054.537551	60.019990	69.068519
1053.973937	62.501859	69.073524
1054.024423	52.569162	69.078529
1053.550599	61.910286	69.083534
1052.417794	56.410751	69.088538
1051.911584	56.679035	69.093543
1050.849259	58.855489	69.098548
1050.950002	52.576272	69.103553
1049.835655	56.878728	69.108558
1049.253535	61.446576	69.113562
1048.748577	57.362522	69.118567
1047.405752	58.363112	69.123572
1046.690799	52.650456	69.128577
1046.178087	52.287454	69.133582
1045.699839	59.092111	69.138586
1045.454777	49.099211	69.143591
1044.464079	63.450259	69.148596
1044.189146	49.232967	69.153601
1042.966497	57.501116	69.158606
1042.586233	46.381773	69.163610
1041.991507	58.343950	69.168615
1040.984479	49.226015	69.173620
1040.420777	45.121352	69.178625
1040.007520	59.260687	69.183630
1039.667054	49.710296	69.188634
1038.926367	51.504443	69.193639
1037.813502	58.657633	69.198644
1037.606261	52.618215	69.203649
1036.715039	51.795070	69.208654
1035.622365	48.175087	69.213658
1035.273275	59.749700	69.218663
1034.838130	56.974376	69.223668
1034.028036	48.304480	69.228673
1032.839624	59.265195	69.233678
1032.486171	43.442544	69.238682
1032.039509	46.996995	69.243687
1031.384757	54.723813	69.248692
1030.560586	51.332334	69.253697
1029.877791	47.129934	69.258702
1029.693517	52.698866	69.263706
1028.828780	55.121421	69.268711
1028.031679	53.414453	69.273716
1027.305468	51.306724	69.278721
1026.781463	58.888171	69.283726
1025.694722	61.243552	69.288730
1025.034575	54.926130	69.293735
1024.361020	54.082550	69.298740
1023.975674	54.454604	69.303745
1023.613174	49.901641	69.308750
1023.044196	52.663472	69.313754
1021.887178	52.691551	69.318759
1021.460979	58.073485	69.323764
1020.828821	50.198405	69.328769
1020.171869	57.009420	69.333774
1019.308737	56.471954	69.338778
1018.767233	51.649446	69.343783
1017.809337	61.119626	69.348788
1017.783718	52.066316	69.353793
1016.824526	53.614553	69.358798
1016.409885	49.547676	69.363802
1015.678594	48.427873	69.368807
1014.538464	54.505259	69.373812
1013.780797	47.600998	69.378817
1012.944867	56.621289	69.383822
1012.562711	55.300866	69.388826
1012.399329	50.277857	69.393831
1011.590274	55.080501	69.398836
1010.820592	44.759521	69.403841
1009.933457	55.323820	69.408846
1009.542980	51.164795	69.413850
1009.401684	47.934318	69.418855
1008.256115	51.817581	69.423860
1007.558798	45.051947	69.428865
1007.206381	58.063607	69.433870
1006.103854	54.891457	69.438874
1005.404625	54.130810	69.443879
1004.579493	55.525265	69.448884
1004.280170	54.272083	69.453889
1003.658042	59.149062	69.458894
1002.645597	51.249344	69.463898
1001.956528	57.384269	69.468903
1001.314066	77.009723	69.473908
1001.797080	55.448232	69.478913
1000.315060	62.128771	69.483918
999.653621	64.138966	69.488922
999.217024	56.316347	69.493927
998.344582	58.336461	69.498932
997.333448	59.642249	69.503937
996.613112	55.683936	69.508942
996.124686	50.345239	69.513946
995.752613	59.791595	69.518951
994.830031	56.191872	69.523956
994.417355	54.196681	69.528961
993.926968	60.498681	69.533966
993.182729	66.814268	69.538970
992.173871	56.690607	69.543975
991.020343	59.249005	69.548980
990.714414	53.209528	69.553985
990.445203	61.409567	69.558990
989.877373	62.023539	69.563994
989.530268	58.396902	69.568999
988.096520	66.958849	69.574004
988.013296	51.828023	69.579009
987.343733	50.780404	69.584014
985.805381	66.997306	69.589018
985.388025	53.584812	69.594023
984.947984	55.996571	69.599028
984.882806	61.756280	69.604033
984.124304	65.024489	69.609038
983.071372	54.385905	69.614042
982.563114	55.674757	69.619047
981.674280	67.235917	69.624052
981.005826	54.662846	69.629057
979.839253	59.817260	69.634062
979.451460	62.851452	69.639066
979.195999	57.671218	69.644071
978.404561	53.389931	69.649076
978.373789	57.721835	69.654081
976.910406	60.663839	69.659086
976.693255	59.891143	69.664090
976.040975	59.326449	69.669095
975.024807	69.127598	69.674100
974.494301	52.237210	69.679105
973.742686	58.758964	69.684110
973.289983	50.737080	69.689114
972.418247	55.649050	69.694119
971.743881	57.047909	69.699124
971.296151	43.972978	69.704129
970.806319	45.850221	69.709134
969.475514	55.767657	69.714138
969.155669	45.540685	69.719143
968.397393	49.835394	69.724148
967.732415	46.314535	69.729153
967.650578	50.741290	69.734158
966.831238	57.308512	69.739162
966.065955	53.075104	69.744167
965.201981	55.568516	69.749172
964.735080	51.792223	69.754177
963.694366	57.491132	69.759182
962.972610	58.427630	69.764186
962.823583	60.184417	69.769191
962.021752	61.904742	69.774196
961.122561	57.831405	69.779201
960.696221	54.439720	69.784206
960.024988	55.506943	69.789210
959.733583	56.005975	69.794215
958.264810	61.235294	69.799220
957.646004	59.540976	69.804225
956.856927	57.436964	69.809230
956.617849	59.644871	69.814234
956.665297	51.179148	69.819239
954.770832	53.598438	69.824244
954.608510	58.821702	69.829249
954.137932	45.217432	69.834254
953.621359	54.940655	69.839258
952.698750	52.435295	69.844263
951.489913	54.614604	69.849268
951.241407	51.339694	69.854273
950.889777	48.538484	69.859278
950.365216	45.041015	69.864282
949.817359	47.788460	69.869287
948.819093	54.868254	69.874292
948.376969	54.434118	69.879297
947.513745	49.781090	69.884302
946.648708	62.718219	69.889306
946.379330	48.430688	69.894311
945.116626	63.080494	69.899316
944.695164	51.756431	69.904321
943.688414	55.057846	69.909326
943.070303	59.830124	69.914330
943.348138	44.107304	69.919335
942.202236	53.046056	69.924340
941.264405	47.759967	69.929345
940.619947	55.381091	69.934350
939.849608	52.233375	69.939354
939.732530	53.833700	69.944359
938.857704	63.752704	69.949364
938.034405	54.328053	69.954369
937.503322	53.986919	69.959374
937.179414	54.976799	69.964378
936.437796	47.899713	69.969383
935.320433	51.387456	69.974388
934.927222	51.079572	69.979393
934.216110	55.281636	69.984398
933.411173	47.746300	69.989402
932.748331	47.429289	69.994407
932.165986	54.330942	69.999412
931.925003	53.927875	70.004417
930.838645	50.051486	70.009422
930.178312	53.986864	70.014426
929.855112	46.513631	70.019431
929.089177	58.417916	70.024436
928.358929	43.451575	70.029441
927.206577	53.700152	70.034446
926.610561	57.245274	70.039450
926.152482	50.192450	70.044455
925.690616	55.677835	70.049460
925.251916	53.259470	70.054465
924.613980	54.203138	70.059470
923.570063	53.476869	70.064474
923.383421	52.342953	70.069479
922.006867	56.259858	70.074484
921.221155	55.552420	70.079489
920.506851	53.573708	70.084494
920.539228	56.801220	70.089498
920.117036	47.937184	70.094503
918.619122	52.852633	70.099508
918.215055	53.615589	70.104513
917.811329	47.683150	70.109518
916.986444	51.362460	70.114522
916.201878	46.490359	70.119527
915.341232	55.546142	70.124532
914.810015	45.037450	70.129537
914.276562	50.280353	70.134542
914.210955	54.884287	70.139546
913.385240	50.584826	70.144551
912.181966	60.313269	70.149556
911.677508	50.684934	70.154561
911.454025	54.102966	70.159566
910.184375	48.866544	70.164570
909.606904	49.146197	70.169575
909.120771	55.024930	70.174580
908.890003	48.476798	70.179585
907.885012	46.424511	70.184590
907.296941	48.566544	70.189594
906.923563	44.284980	70.194599
905.375697	57.130522	70.199604
904.998184	51.089840	70.204609
904.843401	53.631243	70.209614
904.008928	52.182563	70.214618
903.196299	45.452663	70.219623
902.204418	53.879668	70.224628
901.446124	53.822269	70.229633
901.220170	51.122484	70.234638
900.674668	58.018280	70.239642
899.984577	45.470770	70.244647
898.935572	46.561862	70.249652
898.551194	49.095653	70.254657
898.226644	48.108260	70.259662
897.375581	53.321295	70.264666
896.392759	40.672153	70.269671
895.978949	47.029777	70.274676
895.364219	44.533786	70.279681
894.244323	46.810921	70.284686
893.584950	44.618484	70.289690
893.221783	47.785951	70.294695
892.768948	52.732193	70.299700
892.210279	54.293997	70.304705
891.458866	51.310433	70.309710
890.321511	57.228163	70.314714
890.214582	48.459030	70.319719
888.944681	55.643573	70.324724
888.242084	53.486399	70.329729
887.852967	39.768273	70.334734
887.378949	48.415616	70.339738
887.192647	48.696091	70.344743
886.053230	49.140875	70.349748
885.147777	44.198144	70.354753
884.863086	45.271670	70.359758
884.019695	48.253809	70.364762
883.383847	50.654172	70.369767
882.441043	45.488742	70.374772
882.132049	37.674238	70.379777
881.852788	40.415214	70.384782
880.394240	53.667570	70.389786
879.770230	39.392357	70.394791
878.963987	47.302571	70.399796
878.729732	52.912574	70.404801
878.303787	54.877431	70.409806
877.516225	46.235553	70.414810
876.671182	44.377006	70.419815
876.082183	54.307293	70.424820
875.644607	43.633910	70.429825
874.492156	42.969089	70.434830
873.812406	48.320432	70.439834
873.534775	53.560471	70.444839
872.989755	58.657000	70.449844
872.214989	48.590759	70.454849
871.446774	45.903173	70.459854
870.365246	42.240498	70.464858
870.117319	42.023035	70.469863
869.804531	46.177482	70.474868
868.826526	45.068608	70.479873
868.261124	50.185724	70.484878
867.234666	45.904041	70.489882
867.012466	45.017049	70.494887
865.690839	48.124195	70.499892
865.082739	47.528846	70.504897
864.573907	49.738695	70.509902
864.269810	53.100179	70.514906
863.929248	54.876417	70.519911
862.760395	51.415288	70.524916
862.088514	52.345452	70.529921
861.748218	45.079947	70.534926
861.040857	47.884334	70.539930
860.485155	49.472477	70.544935
859.466490	55.711928	70.549940
859.225263	54.022191	70.554945
858.329389	49.664536	70.559950
857.451786	52.226379	70.564954
856.898887	48.354996	70.569959
856.428087	52.288607	70.574964
855.482650	41.516304	70.579969
854.763020	44.428294	70.584974
853.831833	45.437577	70.589978
853.846332	39.282479	70.594983
853.288321	49.357635	70.599988
852.426243	46.976713	70.604993
851.768390	44.025579	70.609998
851.056734	46.004378	70.615002
850.610924	45.460467	70.620007
849.170078	50.311679	70.625012
848.457646	43.603697	70.630017
848.222158	40.661025	70.635022
847.714102	51.672769	70.640026
847.764441	40.630016	70.645031
846.069137	44.402162	70.650036
845.673029	47.639527	70.655041
845.304819	50.612272	70.660046
844.099318	57.214184	70.665050
843.462337	41.230158	70.670055
842.546792	55.719084	70.675060
842.144237	48.975970	70.680065
842.095840	39.290840	70.685070
841.485175	53.862114	70.690074
840.956621	29.262241	70.695079
840.068603	56.423129	70.700084
838.693840	52.729876	70.705089
837.959219	53.783566	70.710094
837.217774	46.654454	70.715098
837.208542	41.865537	70.720103
836.844790	49.235426	70.725108
836.220578	46.075526	70.730113
835.227743	43.098874	70.735118
834.198513	50.809643	70.740122
834.160466	52.622882	70.745127
832.907643	47.079492	70.750132
832.144751	44.077278	70.755137
831.896208	42.429708	70.760142
831.308233	46.159635	70.765146
831.181160	45.752638	70.770151
829.767997	58.381245	70.775156
828.931979	46.388392	70.780161
828.800717	42.449904	70.785166
827.803428	57.421749	70.790170
827.180608	47.274575	70.795175
826.493214	57.154305	70.800180
825.907930	45.725479	70.805185
825.407137	47.095168	70.810190
824.150198	51.615939	70.815194
824.067752	40.419294	70.820199
823.279071	49.394258	70.825204
822.647108	50.661832	70.830209
821.547747	43.731618	70.835214
820.526194	39.967963	70.840218
820.461938	43.207696	70.845223
820.122035	49.094698	70.850228
819.900220	47.742477	70.855233
819.025874	46.981376	70.860238
818.016326	41.112284	70.865242
817.764370	37.265546	70.870247
816.660737	46.749510	70.875252
815.530110	46.508571	70.880257
815.613617	51.889808	70.885262
814.801180	51.235541	70.890266
813.660490	51.444031	70.895271
813.096267	46.476972	70.900276
812.568855	41.317985	70.905281
812.288570	38.417140	70.910286
811.151231	38.521025	70.915290
810.229507	33.058981	70.920295
809.967597	41.846017	70.925300
809.193724	37.153594	70.930305
809.567763	44.465955	70.935310
808.288645	48.234950	70.940314
807.482511	33.156184	70.945319
806.869413	39.297971	70.950324
806.090065	44.162165	70.955329
805.152432	39.393316	70.960334
804.339957	46.300082	70.965338
804.048682	35.377946	70.970343
803.823300	44.409888	70.975348
802.730193	40.588250	70.980353
801.977052	41.594438	70.985358
801.421172	46.290605	70.990362
801.090329	42.226205	70.995367
799.791564	43.776540	71.000372
799.330517	44.346747	71.005377
798.703229	37.465970	71.010382
797.946370	46.609327	71.015386
797.827764	37.126180	71.020391
796.743473	44.717998	71.025396
795.916868	45.944028	71.030401
795.312983	40.674226	71.035406
794.942016	46.796395	71.040410
794.387005	37.869969	71.045415
793.211743	49.971887	71.050420
792.671387	57.133368	71.055425
792.368319	45.594976	71.060430
791.624192	60.198545	71.065434
790.628026	43.010234	71.070439
789.956685	58.482099	71.075444
789.486832	48.983904	71.080449
789.300589	46.910131	71.085454
787.939339	48.224430	71.090458
787.459926	43.343219	71.095463
786.775820	53.484188	71.100468
785.995362	54.031134	71.105473
786.284845	44.888270	71.110478
785.113911	56.713558	71.115482
784.489143	54.758478	71.120487
783.847064	54.340436	71.125492
782.666434	51.251784	71.130497
782.034050	53.445050	71.135502
781.311603	53.807732	71.140506
780.992234	59.598438	71.145511
780.482203	61.633463	71.150516
779.744715	52.693507	71.155521
778.994856	58.800313	71.160526
778.376783	57.856510	71.165530
777.800543	54.036169	71.170535
776.695231	51.739727	71.175540
775.874935	52.236252	71.180545
775.787555	49.798255	71.185550
775.057002	53.850496	71.190554
774.619449	52.289789	71.195559
773.265648	52.418691	71.200564
772.706891	53.009190	71.205569
772.734023	40.051105	71.210574
771.939567	55.757022	71.215578
771.464130	48.643928	71.220583
770.724742	56.239196	71.225588
769.899548	54.333374	71.230593
769.141225	44.950494	71.235598
767.935954	52.230446	71.240602
767.986374	44.729304	71.245607
767.223948	47.752203	71.250612
766.497384	52.004071	71.255617
765.801018	50.014666	71.260622
764.750251	56.584092	71.265626
764.764813	44.151523	71.270631
763.704421	49.267041	71.275636
762.971042	52.761528	71.280641
762.344746	39.697752	71.285646
761.524136	48.207909	71.290650
761.516095	49.033989	71.295655
760.384761	51.798674	71.300660
759.562082	46.178961	71.305665
759.076923	48.922767	71.310670
758.726146	55.467479	71.315674
758.269251	43.788018	71.320679
757.190977	50.148948	71.325684
756.490241	51.149961	71.330689
756.185116	46.557957	71.335694
754.730388	50.509466	71.340698
754.084233	50.309687	71.345703
753.635762	54.283910	71.350708
753.397868	42.894416	71.355713
753.088381	43.688069	71.360718
752.212807	55.319695	71.365722
751.547174	47.615607	71.370727
750.712868	39.943108	71.375732
749.602821	42.688639	71.380737
748.770082	30.190722	71.385742
748.143593	50.851175	71.390746
747.923966	45.129147	71.395751
747.627733	45.611627	71.400756
746.617586	47.634823	71.405761
745.971659	47.149599	71.410766
744.993008	48.379354	71.415770
744.575947	46.779123	71.420775
744.232585	44.613682	71.425780
743.289111	49.347916	71.430785
742.798343	47.100295	71.435790
741.771861	52.943661	71.440794
741.691661	39.662069	71.445799
740.692522	50.996420	71.450804
739.806868	49.631635	71.455809
739.461775	38.998761	71.460814
738.730113	48.731016	71.465818
738.243958	48.160435	71.470823
737.662241	51.665472	71.475828
736.956074	53.643428	71.480833
735.637216	45.838359	71.485838
734.495407	45.053645	71.490842
734.332742	39.464469	71.495847
733.707482	49.722222	71.500852
733.310515	44.884664	71.505857
732.988004	38.325944	71.510862
732.641670	51.817569	71.515866
732.068990	46.604312	71.520871
731.279953	51.990433	71.525876
729.968919	55.867043	71.530881
729.183172	43.943501	71.535886
728.577546	51.642049	71.540890
728.336922	50.628702	71.545895
727.834181	56.730863	71.550900
726.760653	48.864661	71.555905
726.315175	45.972783	71.560910
725.879367	44.476459	71.565914
724.977402	50.694219	71.570919
724.215729	52.942774	71.575924
723.594166	50.263424	71.580929
722.748771	38.674219	71.585934
721.550548	54.414469	71.590938
720.685404	36.975124	71.595943
720.558167	36.974988	71.600948
719.833510	43.654916	71.605953
719.878228	49.706175	71.610958
719.491060	48.596322	71.615962
718.433744	40.951460	71.620967
717.799398	50.275588	71.625972
717.177331	50.873025	71.630977
716.248582	42.222159	71.635982
714.925489	49.781072	71.640986
714.898100	44.135667	71.645991
714.650971	48.079411	71.650996
713.500374	37.431307	71.656001
712.990220	43.742790	71.661006
712.065829	44.576011	71.666010
711.726638	38.685383	71.671015
711.207006	45.791533	71.676020
709.858731	43.450236	71.681025
709.503032	50.238568	71.686030
708.824221	46.781488	71.691034
708.795947	44.945905	71.696039
707.587236	42.210249	71.701044
706.932009	47.459958	71.706049
706.608622	47.262411	71.711054
705.905857	50.502894	71.716058
704.684392	39.981187	71.721063
704.197648	52.829738	71.726068
703.829053	43.394291	71.731073
703.292795	52.289669	71.736078
701.919163	53.933971	71.741082
701.285914	49.373724	71.746087
700.536092	46.210210	71.751092
700.454986	50.384548	71.756097
700.315041	35.116182	71.761102
699.172598	54.256714	71.766106
698.371387	46.295130	71.771111
698.096661	42.739021	71.776116
696.845612	42.597730	71.781121
696.017831	36.660333	71.786126
695.507945	48.834519	71.791130
694.881924	42.005608	71.796135
694.365234	37.347964	71.801140
694.057178	43.583117	71.806145
693.818874	46.552538	71.811150
692.952229	55.106313	71.816154
691.975223	45.789823	71.821159
690.731766	50.273816	71.826164
689.939247	51.429802	71.831169
689.646899	40.048996	71.836174
688.979513	50.280350	71.841178
688.624186	46.718153	71.846183
688.170673	42.619694	71.851188
686.991034	45.472520	71.856193
686.735020	40.746561	71.861198
686.129696	50.742543	71.866202
685.058156	42.838205	71.871207
684.467333	46.913945	71.876212
683.634254	57.758279	71.881217
683.480893	38.166737	71.886222
682.445298	54.800409	71.891226
681.704291	45.843711	71.896231
681.291443	48.028847	71.901236
681.111672	58.587813	71.906241
680.077899	44.108285	71.911246
678.981708	52.652886	71.916250
678.541910	56.201564	71.921255
678.363906	49.282392	71.926260
677.174285	50.116862	71.931265
676.607880	40.690847	71.936270
676.065663	48.907551	71.941274
675.402837	42.461376	71.946279
674.554485	46.918727	71.951284
673.659290	49.567003	71.956289
673.493164	41.933205	71.961294
673.013683	46.413813	71.966298
671.956320	48.032998	71.971303
671.389369	50.572238	71.976308
670.374129	47.607109	71.981313
670.271698	44.640117	71.986318
668.738371	55.581769	71.991322
667.931535	51.484385	71.996327
667.751027	40.978274	72.001332
667.163338	47.824050	72.006337
667.180280	44.115850	72.011342
666.377691	47.168824	72.016346
665.454993	38.520173	72.021351
664.906829	42.245369	72.026356
664.125955	44.492266	72.031361
663.059177	41.978444	72.036366
662.229820	51.082916	72.041370
661.975238	39.323966	72.046375
661.778428	42.427121	72.051380
661.114640	47.414868	72.056385
660.165022	47.534657	72.061390
659.220001	45.633765	72.066394
659.066785	45.607809	72.071399
658.395714	40.679886	72.076404
656.778629	47.967117	72.081409
656.521123	45.589335	72.086414
655.920168	47.936886	72.091418
655.373085	38.979281	72.096423
655.178172	41.691074	72.101428
653.933911	52.842149	72.106433
653.302172	50.036714	72.111438
653.041543	51.167929	72.116442
652.579958	47.148027	72.121447
651.631252	44.743132	72.126452
650.422411	49.152249	72.131457
650.501662	36.149617	72.136462
649.900175	54.147523	72.141466
648.681812	45.869216	72.146471
648.199878	45.564469	72.151476
647.603730	44.385413	72.156481
646.964599	41.724652	72.161486
645.834267	49.363279	72.166490
644.918254	41.904096	72.171495
644.690545	40.054547	72.176500
644.250308	45.670551	72.181505
644.091730	48.860654	72.186510
642.842671	52.634401	72.191514
642.675790	42.504568	72.196519
642.068229	42.618773	72.201524
640.534641	47.041766	72.206529
639.984342	45.521117	72.211534
639.737313	49.520040	72.216538
639.199766	38.550434	72.221543
638.788559	42.146597	72.226548
637.494550	51.195771	72.231553
637.511427	42.646642	72.236558
636.313845	42.523673	72.241562
635.213202	43.552138	72.246567
634.594192	33.929528	72.251572
634.338733	43.316319	72.256577
634.088886	31.865690	72.261582
633.128960	38.026474	72.266586
632.452462	35.351171	72.271591
631.996754	33.635700	72.276596
631.021361	49.685816	72.281601
630.334388	39.463785	72.286606
629.605664	40.704240	72.291610
628.876021	37.176439	72.296615
628.490649	38.677583	72.301620
627.437256	48.379100	72.306625
627.087422	34.276360	72.311630
626.260354	41.480363	72.316634
625.837511	46.734077	72.321639
625.272492	47.874350	72.326644
623.906400	43.003513	72.331649
623.506253	39.781184	72.336654
622.942624	37.595654	72.341658
622.663146	41.475173	72.346663
622.226875	39.960021	72.351668
621.395584	49.908425	72.356673
620.702417	34.346588	72.361678
619.792452	37.717853	72.366682
618.815247	36.914862	72.371687
618.226582	39.394495	72.376692
617.515686	42.087548	72.381697
617.131589	44.173503	72.386702
617.082003	45.062965	72.391706
615.831319	45.512976	72.396711
615.415266	42.994881	72.401716
614.756387	49.524018	72.406721
613.909396	42.632561	72.411726
612.626451	40.213111	72.416730
612.170735	44.776669	72.421735
611.884347	45.595043	72.426740
611.269569	48.223908	72.431745
611.076179	37.625251	72.436750
610.111255	50.373354	72.441754
609.280604	39.734272	72.446759
608.658101	42.987224	72.451764
607.366258	45.493703	72.456769
607.021532	38.530141	72.461774
606.463241	51.793765	72.466778
606.014143	46.362179	72.471783
605.618531	35.116108	72.476788
604.087331	39.018379	72.481793
603.875515	35.389192	72.486798
603.178789	38.925184	72.491802
602.795292	40.164275	72.496807
602.252810	43.063883	72.501812
601.279548	40.180404	72.506817
601.029116	42.044811	72.511822
600.299347	41.410564	72.516826
599.129963	39.759883	72.521831
598.472835	40.057023	72.526836
597.874771	38.417844	72.531841
597.492623	33.935904	72.536846
596.313078	44.018620	72.541850
595.719248	40.910717	72.546855
595.447312	38.380711	72.551860
595.079515	45.457962	72.556865
594.614948	35.162681	72.561870
593.503346	44.682679	72.566874
592.904554	50.344443	72.571879
592.453572	35.507240	72.576884
591.047130	38.028825	72.581889
590.858821	38.271796	72.586894
590.409034	36.430818	72.591898
589.164388	39.207314	72.596903
588.360071	38.186000	72.601908
587.678896	40.475383	72.606913
587.413174	35.952825	72.611918
587.033013	40.837068	72.616922
586.030380	34.536506	72.621927
585.302382	37.506663	72.626932
584.613855	33.697957	72.631937
584.197254	34.623800	72.636942
583.837876	35.155776	72.641946
582.783639	33.103589	72.646951
582.472495	32.071531	72.651956
581.574329	35.218593	72.656961
580.737922	33.571653	72.661966
579.987066	37.931504	72.666970
579.044305	47.025671	72.671975
579.071279	34.269481	72.676980
578.572653	44.841374	72.681985
577.739275	32.468209	72.686990
576.894020	31.934360	72.691994
576.680624	35.699282	72.696999
575.377575	35.924280	72.702004
574.049037	40.268920	72.707009
573.589308	28.919543	72.712014
573.423198	33.785459	72.717018
572.955199	41.134120	72.722023
572.817183	37.953622	72.727028
571.754202	41.883829	72.732033
571.139121	41.551423	72.737038
570.554370	37.185331	72.742042
569.608541	36.235447	72.747047
568.714431	30.903141	72.752052
568.286396	43.064293	72.757057
567.982318	28.911713	72.762062
566.802589	32.267619	72.767066
565.865456	31.743678	72.772071
565.521349	28.938186	72.777076
564.821635	37.301401	72.782081
564.430690	30.267949	72.787086
563.588707	37.231507	72.792090
562.641858	41.600506	72.797095
562.456793	34.524798	72.802100
561.544728	41.676128	72.807105
561.586071	33.031658	72.812110
560.328179	41.490093	72.817114
559.537970	37.847392	72.822119
559.348226	37.868259	72.827124
558.204736	41.904329	72.832129
557.440467	42.122358	72.837134
556.687766	45.777659	72.842138
556.387410	39.586005	72.847143
556.125726	32.738531	72.852148
555.310754	43.233090	72.857153
554.371607	38.486666	72.862158
553.628307	34.085915	72.867162
553.096385	50.872757	72.872167
552.705971	35.690050	72.877172
551.141707	41.299040	72.882177
550.934203	42.360304	72.887182
550.533377	47.894353	72.892186
550.178929	39.863246	72.897191
549.419257	30.720362	72.902196
548.356584	46.792279	72.907201
547.803227	35.688039	72.912206
547.681547	37.378987	72.917210
546.190206	44.755053	72.922215
545.888002	35.236541	72.927220
545.295877	39.746147	72.932225
544.705502	39.144901	72.937230
543.739462	38.280242	72.942234
542.956120	35.475338	72.947239
542.240634	39.564654	72.952244
542.019802	53.446268	72.957249
541.335750	41.962324	72.962254
540.719412	48.677074	72.967258
540.089974	37.036210	72.972263
539.260774	39.655094	72.977268
538.090983	50.523130	72.982273
537.643134	37.386868	72.987278
537.050749	46.043637	72.992282
536.619399	48.588109	72.997287
536.089917	40.826146	73.002292
534.839823	50.156930	73.007297
534.433338	43.384557	73.012302
533.962071	43.565381	73.017306
533.520628	45.395571	73.022311
532.923320	47.980672	73.027316
531.803821	38.193411	73.032321
531.599055	46.244420	73.037326
530.959697	42.304903	73.042330
529.737650	47.419451	73.047335
529.338062	38.848373	73.052340
528.849497	49.243641	73.057345
528.217279	36.970907	73.062350
527.154074	38.080181	73.067354
526.534146	42.939550	73.072359
526.304851	38.870062	73.077364
525.248003	45.159856	73.082369
524.314886	36.527124	73.087374
523.517269	41.968274	73.092378
522.748736	48.948531	73.097383
522.936444	37.888661	73.102388
522.325237	45.584974	73.107393
521.947254	48.679153	73.112398
520.990826	40.895326	73.117402
520.049145	51.446351	73.122407
519.788314	31.093021	73.127412
518.238169	40.539409	73.132417
517.785474	41.010571	73.137422
517.309690	38.265484	73.142426
517.090170	42.824542	73.147431
516.408807	29.927330	73.152436
515.234991	42.265633	73.157441
514.753314	41.069951	73.162446
514.497885	40.891564	73.167450
513.249051	43.689262	73.172455
512.598019	40.319277	73.177460
511.981563	46.180974	73.182465
511.529200	38.788331	73.187470
511.090710	35.023390	73.192474
509.892975	40.544053	73.197479
509.647572	39.976163	73.202484
508.975403	44.014436	73.207489
508.183808	42.934356	73.212494
507.370495	39.032019	73.217498
506.642705	39.871840	73.222503
506.313985	33.700485	73.227508
505.651171	43.305124	73.232513
505.018639	35.373521	73.237518
504.341146	40.119070	73.242522
503.794809	50.696998	73.247527
502.618377	38.826341	73.252532
501.720944	50.300662	73.257537
500.916546	36.647241	73.262542
500.624605	37.614735	73.267546
500.417232	47.220933	73.272551
500.170495	47.470066	73.277556
498.912836	44.125767	73.282561
498.301823	34.443588	73.287566
497.983279	44.922149	73.292570
497.012746	43.985689	73.297575
496.179048	36.573383	73.302580
495.179206	43.100093	73.307585
494.973856	38.564777	73.312590
494.662806	36.469919	73.317594
493.324061	41.475348	73.322599
493.117694	38.487085	73.327604
492.187791	48.738214	73.332609
491.955307	40.966792	73.337614
491.055945	40.686004	73.342618
489.825442	40.683461	73.347623
489.611040	36.323041	73.352628
489.255359	40.265168	73.357633
488.623852	38.292323	73.362638
487.986020	38.515460	73.367642
486.985206	37.982771	73.372647
486.449743	33.422784	73.377652
485.201943	39.979539	73.382657
484.494616	32.174971	73.387662
484.303119	36.245471	73.392666
483.642908	45.766128	73.397671
483.540722	38.953174	73.402676
482.793058	36.837998	73.407681
481.754904	39.963244	73.412686
481.170639	36.689857	73.417690
480.645758	45.700131	73.422695
479.680787	46.383794	73.427700
478.854676	48.585917	73.432705
478.370426	46.559652	73.437710
478.067470	45.810136	73.442714
476.821944	44.113302	73.447719
476.246171	40.324510	73.452724
475.378728	43.584977	73.457729
475.488828	46.533595	73.462734
474.952248	40.040569	73.467738
473.842599	35.781785	73.472743
473.355913	35.011083	73.477748
472.793289	37.193304	73.482753
471.778122	40.103594	73.487758
470.992122	39.503573	73.492762
469.992649	46.988959	73.497767
469.966351	43.473724	73.502772
469.498731	40.937067	73.507777
468.720942	43.932533	73.512782
467.745748	46.686657	73.517786
466.986286	40.407327	73.522791
466.800921	26.600115	73.527796
465.814125	44.490683	73.532801
465.044309	37.902365	73.537806
464.637291	43.350681	73.542810
463.698292	55.364613	73.547815
463.640953	37.290535	73.552820
462.697316	37.863579	73.557825
461.718489	28.943294	73.562830
461.632346	42.194769	73.567834
460.418303	33.679363	73.572839
460.033248	36.667448	73.577844
459.289790	44.392725	73.582849
459.096639	33.778294	73.587854
458.272015	33.919243	73.592858
457.100941	41.643269	73.597863
456.813219	33.899581	73.602868
456.012862	44.101693	73.607873
454.936427	43.957933	73.612878
454.204116	43.458166	73.617882
453.566849	38.148058	73.622887
453.742219	37.019580	73.627892
452.980904	34.900281	73.632897
452.014558	45.362215	73.637902
451.474187	36.135544	73.642906
450.951489	37.087773	73.647911
450.312417	39.463517	73.652916
449.083446	46.331083	73.657921
448.209786	34.645595	73.662926
447.993745	36.567609	73.667930
447.624494	46.456624	73.672935
447.209339	42.143964	73.677940
445.865928	40.161564	73.682945
445.455839	39.266707	73.687950
444.948007	44.827277	73.692954
443.730822	46.229184	73.697959
443.160281	42.122620	73.702964
442.624876	38.975491	73.707969
442.485481	44.251867	73.712974
441.757250	36.442759	73.717978
440.695832	44.510419	73.722983
440.270982	42.604001	73.727988
439.565614	49.438604	73.732993
438.709724	39.251447	73.737998
438.113042	39.067521	73.743002
437.227153	46.020767	73.748007
437.140537	37.842940	73.753012
436.467834	35.851444	73.758017
435.377404	38.677551	73.763022
434.577505	42.222140	73.768026
433.898785	46.904829	73.773031
433.733845	41.636153	73.778036
432.898018	44.210398	73.783041
431.959299	48.746870	73.788046
431.378569	46.608263	73.793050
430.774174	45.846864	73.798055
430.814658	44.608998	73.803060
429.552856	47.306308	73.808065
428.831629	49.930099	73.813070
428.326167	44.605302	73.818074
427.607735	52.856424	73.823079
426.942003	46.535366	73.828084
426.216336	52.212646	73.833089
425.627391	46.549514	73.838094
425.520974	43.755052	73.843098
424.067044	54.390879	73.848103
423.716652	44.425935	73.853108
422.786382	44.878601	73.858113
422.615388	47.572403	73.863118
421.844246	34.754184	73.868122
420.966147	55.927797	73.873127
420.422436	42.103570	73.878132
419.350621	46.478339	73.883137
418.245318	46.192548	73.888142
417.920534	36.855846	73.893146
417.534985	45.705162	73.898151
417.307347	43.108201	73.903156
416.726710	43.388470	73.908161
415.757743	37.282884	73.913166
415.464613	41.565111	73.918170
414.866856	46.864066	73.923175
414.000096	41.074908	73.928180
412.972849	34.644319	73.933185
412.357221	39.946119	73.938190
411.779902	46.314074	73.943194
410.871070	46.427460	73.948199
410.132788	41.798891	73.953204
409.496798	44.726050	73.958209
409.348761	42.214170	73.963214
408.867561	33.488985	73.968218
407.423921	50.973007	73.973223
407.114088	42.419193	73.978228
406.631593	44.289058	73.983233
405.444571	39.922795	73.988238
404.749707	45.896348	73.993242
403.956814	39.103586	73.998247
403.853046	43.404523	74.003252
403.370423	39.328113	74.008257
402.633418	45.141235	74.013262
401.982050	34.484721	74.018266
400.937478	40.901903	74.023271
400.951680	42.534936	74.028276
400.045274	45.240278	74.033281
398.876016	33.748565	74.038286
398.500512	36.079167	74.043290
397.768662	43.971330	74.048295
397.257297	42.848209	74.053300
396.370394	43.128404	74.058305
395.429713	43.641083	74.063310
395.480522	42.750055	74.068314
394.895980	46.629321	74.073319
394.126534	40.105621	74.078324
393.148082	36.310063	74.083329
392.240515	45.781848	74.088334
391.989243	44.587320	74.093338
391.288298	43.874431	74.098343
390.383366	39.523144	74.103348
389.850322	46.664588	74.108353
389.630865	42.825346	74.113358
389.062741	41.566201	74.118362
387.780032	40.838794	74.123367
387.396981	42.339601	74.128372
386.711292	46.864149	74.133377
385.776295	56.103786	74.138382
385.135599	44.177784	74.143386
384.418503	44.601224	74.148391
384.201904	45.061593	74.153396
383.643225	47.993785	74.158401
382.592114	50.994988	74.163406
381.774924	47.977927	74.168410
381.490544	58.813729	74.173415
381.023108	45.393647	74.178420
379.996292	53.470010	74.183425
378.996637	56.108225	74.188430
378.640991	46.901015	74.193434
377.998031	50.767519	74.198439
377.382369	42.825383	74.203444
376.512257	49.873898	74.208449
376.145030	47.144654	74.213454
375.739877	39.098016	74.218458
374.807261	54.695128	74.223463
374.026269	38.761065	74.228468
373.408799	42.202487	74.233473
372.612333	46.033533	74.238478
372.377505	45.831379	74.243482
371.449087	55.103085	74.248487
370.860010	46.316252	74.253492
370.463526	48.549284	74.258497
369.258390	43.807482	74.263502
368.533499	45.093128	74.268506
367.962018	44.134124	74.273511
367.736016	51.497860	74.278516
367.375831	41.829363	74.283521
366.140722	39.460767	74.288526
365.449084	48.242180	74.293530
365.025860	50.392748	74.298535
363.975877	49.445350	74.303540
363.280481	40.550896	74.308545
362.456055	51.141619	74.313550
362.298368	41.174365	74.318554
361.841737	44.721036	74.323559
361.035421	45.119280	74.328564
359.936195	44.976040	74.333569
359.400253	46.846548	74.338574
359.369574	43.852376	74.343578
358.093569	56.788885	74.348583
357.350684	44.811375	74.353588
356.834196	49.223815	74.358593
356.118853	45.991850	74.363598
356.164709	45.197798	74.368602
354.633015	62.798383	74.373607
354.275834	43.709310	74.378612
353.616569	51.536307	74.383617
353.024656	50.861241	74.388622
352.623834	49.900272	74.393626
351.255412	62.648105	74.398631
351.079308	44.914648	74.403636
350.679422	48.698267	74.408641
349.431493	56.144450	74.413646
348.890859	40.572612	74.418650
348.219229	48.712217	74.423655
348.000081	53.126155	74.428660
346.767595	40.905004	74.433665
345.970494	52.093732	74.438670
345.459159	53.689103	74.443674
345.143309	53.245991	74.448679
344.737231	54.130774	74.453684
343.568368	47.707014	74.458689
342.553580	49.075137	74.463694
342.375690	50.065469	74.468698
341.912389	50.282904	74.473703
341.305573	42.732006	74.478708
340.519555	50.714814	74.483713
339.557735	49.397008	74.488718
339.211971	42.610275	74.493722
338.506387	50.580265	74.498727
337.655813	55.485896	74.503732
337.310792	53.735496	74.508737
336.521416	48.381859	74.513742
335.710298	50.135390	74.518746
334.843611	45.022719	74.523751
334.506389	43.772515	74.528756
333.769312	49.041654	74.533761
333.552411	47.625627	74.538766
332.466174	45.378391	74.543770
331.621300	54.010783	74.548775
331.341280	48.555470	74.553780
330.699886	57.779866	74.558785
329.536646	49.179165	74.563790
329.082618	51.413491	74.568794
328.306874	45.171497	74.573799
328.446250	45.414298	74.578804
327.069899	53.324051	74.583809
326.216463	56.523992	74.588814
326.250640	47.568458	74.593818
325.463659	58.375562	74.598823
324.119484	54.497979	74.603828
323.857117	50.621431	74.608833
322.887415	54.046471	74.613838
322.777880	47.490153	74.618842
321.882910	52.136376	74.623847
321.690270	44.752845	74.628852
320.876429	52.000552	74.633857
319.893603	48.271947	74.638862
319.037711	34.344567	74.643866
318.254549	50.504452	74.648871
317.846345	49.814307	74.653876
317.591403	53.164848	74.658881
316.796720	52.340772	74.663886
315.977033	45.112373	74.668890
315.400823	50.431566	74.673895
314.852283	50.744588	74.678900
314.092844	48.224514	74.683905
313.068115	48.999762	74.688910
312.761164	40.112796	74.693914
311.910298	51.863574	74.698919
311.270174	40.848930	74.703924
310.698808	41.320122	74.708929
309.794006	43.760328	74.713934
309.669255	38.128897	74.718938
308.732276	46.268226	74.723943
308.174155	51.297551	74.728948
307.197014	45.250081	74.733953
306.740402	45.363961	74.738958
306.063349	38.664731	74.743962
305.225968	50.965257	74.748967
304.634901	39.493396	74.753972
304.214227	40.535042	74.758977
303.678235	39.132034	74.763982
302.402724	39.824263	74.768986
301.809118	48.214774	74.773991
301.617107	44.845800	74.778996
301.126419	35.101937	74.784001
299.842476	55.990193	74.789006
299.257627	36.365043	74.794010
298.495812	52.344923	74.799015
298.051111	47.991274	74.804020
297.693021	47.744123	74.809025
297.162473	52.895203	74.814030
296.261699	39.530034	74.819034
295.615808	36.140374	74.824039
294.842603	44.803921	74.829044
294.016135	38.213661	74.834049
293.153754	51.598314	74.839054
292.951699	29.020223	74.844058
292.342692	47.276360	74.849063
291.484899	42.654267	74.854068
290.911682	38.679051	74.859073
289.779970	50.502981	74.864078
289.541573	37.478486	74.869082
289.230060	56.502444	74.874087
288.059209	36.614337	74.879092
287.310251	34.439510	74.884097
286.872450	50.443432	74.889102
286.717723	32.444845	74.894106
285.761940	49.638275	74.899111
284.891559	42.009567	74.904116
284.398708	47.939909	74.909121
283.829867	45.993398	74.914126
283.012984	48.359680	74.919130
282.437405	48.017897	74.924135
281.692409	41.119784	74.929140
280.863791	35.453905	74.934145
279.774762	52.854648	74.939150
279.633548	40.227796	74.944154
278.950746	39.991408	74.949159
278.449432	44.016691	74.954164
277.806721	37.171659	74.959169
276.938161	47.775740	74.964174
276.654167	47.289715	74.969178
276.118531	39.364820	74.974183
274.726543	42.267446	74.979188
274.485690	46.538198	74.984193
273.859977	50.870299	74.989198
273.219906	38.827559	74.994202
271.678887	46.170689	74.999207
271.415656	48.683671	75.004212
270.922698	35.171517	75.009217
270.472348	54.277521	75.014222
270.240732	44.564901	75.019226
268.910431	46.349175	75.024231
268.494847	43.540933	75.029236
268.155584	46.870227	75.034241
266.641476	55.349135	75.039246
265.881786	41.329174	75.044250
265.318236	51.167176	75.049255
264.851913	46.533149	75.054260
264.819150	50.422250	75.059265
264.227658	43.562747	75.064270
263.717253	44.227645	75.069274
262.441451	48.406349	75.074279
261.771463	42.418742	75.079284
261.042803	45.385937	75.084289
260.075354	46.093732	75.089294
259.866157	41.798740	75.094298
259.306482	44.573429	75.099303
258.643908	40.907336	75.104308
257.692040	46.322688	75.109313
257.056379	48.628553	75.114318
256.674993	40.798914	75.119322
256.167814	42.768928	75.124327
254.861121	38.516433	75.129332
254.536418	35.827741	75.134337
253.628776	50.531550	75.139342
253.621499	31.798309	75.144346
252.397310	47.703674	75.149351
251.407930	46.070198	75.154356
251.202919	50.212244	75.159361
250.547013	40.195131	75.164366
250.493342	36.411477	75.169370
249.200834	46.417718	75.174375
248.633981	37.999525	75.179380
248.210899	49.109725	75.184385
247.095250	43.295661	75.189390
246.407310	37.571102	75.194394
245.880896	44.148573	75.199399
245.550121	43.315220	75.204404
244.657411	41.636376	75.209409
243.350645	40.127611	75.214414
242.925664	41.841690	75.219418
242.521802	36.156997	75.224423
242.014550	38.319399	75.229428
242.108676	33.198674	75.234433
240.533175	44.144101	75.239438
240.312412	42.664049	75.244442
239.556473	36.723267	75.249447
238.600698	51.955113	75.254452
238.095896	45.510700	75.259457
237.605447	44.374818	75.264462
236.914360	38.575075	75.269466
235.695804	41.260853	75.274471
235.188989	39.112092	75.279476
234.913505	36.935915	75.284481
234.169399	36.477517	75.289486
233.508303	36.910995	75.294490
232.693236	38.226823	75.299495
231.867951	40.275936	75.304500
231.648453	46.738255	75.309505
230.548580	40.600009	75.314510
229.701600	38.650548	75.319514
229.077920	46.370973	75.324519
228.801226	32.520028	75.329524
228.613830	43.226824	75.334529
227.844456	42.986907	75.339534
227.104804	44.448399	75.344538
226.376559	43.388273	75.349543
225.045831	41.569546	75.354548
224.592449	44.598513	75.359553
223.650571	54.922585	75.364558
223.379261	37.850857	75.369562
223.090020	50.407765	75.374567
222.034520	57.069593	75.379572
221.460906	41.859429	75.384577
221.144158	48.146454	75.389582
220.824064	45.977390	75.394586
219.761366	40.211666	75.399591
218.901874	47.487172	75.404596
218.522323	45.655571	75.409601
217.040888	41.145546	75.414606
216.344710	46.912783	75.419610
215.914162	51.046636	75.424615
215.365885	44.210219	75.429620
215.367375	42.940725	75.434625
214.515487	49.805041	75.439630
213.520697	39.586520	75.444634
212.995841	56.296562	75.449639
212.464516	50.843489	75.454644
211.740947	40.362546	75.459649
210.323104	58.878529	75.464654
210.004133	43.982561	75.469658
209.760090	48.345282	75.474663
208.806045	50.216249	75.479668
208.729362	49.359737	75.484673
207.436995	41.328439	75.489678
207.125062	45.287274	75.494682
206.582757	41.753400	75.499687
205.686080	52.634778	75.504692
205.085685	48.603997	75.509697
204.274168	54.643500	75.514702
204.044959	52.529328	75.519706
202.768422	51.316942	75.524711
201.654698	53.008380	75.529716
201.449087	53.258869	75.534721
200.745704	54.083849	75.539726
200.538586	48.013003	75.544730
200.496879	44.577503	75.549735
199.242576	56.446241	75.554740
198.739387	44.099447	75.559745
197.326525	52.820851	75.564750
197.007323	45.700352	75.569754
196.521001	47.151424	75.574759
195.622877	41.886139	75.579764
195.428505	33.727103	75.584769
194.097927	48.138832	75.589774
193.596812	42.515382	75.594778
192.987823	51.591137	75.599783
192.298478	41.049556	75.604788
192.363259	43.459789	75.609793
190.788714	46.478293	75.614798
190.312479	37.597847	75.619802
190.095857	42.265257	75.624807
189.250096	53.614730	75.629812
188.136723	43.883449	75.634817
187.661115	46.359340	75.639822
187.267299	34.316797	75.644826
186.977900	39.855190	75.649831
185.985627	44.580041	75.654836
185.230128	38.446834	75.659841
184.516830	43.363733	75.664846
184.052456	54.652400	75.669850
182.705883	43.072395	75.674855
181.901564	50.706522	75.679860
181.921754	34.624321	75.684865
181.459163	46.913994	75.689870
181.001418	24.819808	75.694874
180.252963	46.163564	75.699879
179.520300	43.585656	75.704884
178.644933	39.664953	75.709889
177.308806	44.301139	75.714894
176.678829	48.414757	75.719898
176.387205	45.066410	75.724903
176.022705	42.742018	75.729908
175.660517	46.748289	75.734913
174.761596	44.136970	75.739918
173.966380	54.030844	75.744922
173.275837	44.229001	75.749927
172.827446	47.339177	75.754932
172.158094	33.708537	75.759937
171.236903	58.731823	75.764942
170.766129	35.539064	75.769946
170.164079	50.238318	75.774951
169.115853	41.603607	75.779956
168.408163	45.529358	75.784961
167.863864	41.573218	75.789966
167.545696	39.142099	75.794970
166.385421	52.820264	75.799975
165.848555	47.446930	75.804980
165.347272	45.929618	75.809985
164.544903	45.851089	75.814990
164.595003	50.819728	75.819994
163.607051	44.335686	75.824999
162.956504	46.531990	75.830004
162.319761	32.732163	75.835009
160.853348	53.126037	75.840014
160.180531	35.008252	75.845018
159.739538	45.411730	75.850023
159.784109	46.464367	75.855028
159.493356	33.251150	75.860033
158.477163	53.637889	75.865038
157.478127	40.668479	75.870042
156.760157	40.601725	75.875047
155.882898	49.608304	75.880052
155.001575	42.662595	75.885057
154.430886	48.050315	75.890062
154.079218	42.352587	75.895066
153.800440	42.967960	75.900071
153.279109	42.399953	75.905076
152.502956	35.894764	75.910081
151.408507	43.436393	75.915086
151.175281	32.801607	75.920090
150.451213	40.798229	75.925095
149.704255	38.011314	75.930100
149.212735	36.541331	75.935105
147.903497	43.901182	75.940110
147.218924	33.866608	75.945114
146.720381	40.594178	75.950119
146.386241	46.466117	75.955124
145.942881	34.718471	75.960129
144.517653	47.055994	75.965134
143.996559	36.355153	75.970138
143.720876	29.856894	75.975143
143.053887	37.450203	75.980148
142.069657	32.947675	75.985153
141.329509	44.493185	75.990158
141.173558	33.543325	75.995162
140.449196	37.151640	76.000167
139.536610	38.408936	76.005172
138.946005	38.438564	76.010177
138.328985	34.257504	76.015182
137.642429	32.217847	76.020186
136.884607	38.628817	76.025191
135.920552	29.433545	76.030196
135.584943	35.114916	76.035201
134.754333	40.009534	76.040206
134.683037	37.203188	76.045210
134.013125	40.694021	76.050215
132.562895	44.414931	76.055220
132.293252	32.488214	76.060225
131.891699	43.483027	76.065230
131.118198	33.152002	76.070234
130.215991	43.356231	76.075239
129.567429	32.964286	76.080244
129.431904	30.407863	76.085249
128.234458	34.561518	76.090254
127.498318	38.922292	76.095258
127.161324	40.590821	76.100263
126.145985	45.313064	76.105268
126.324439	27.800676	76.110273
124.836601	48.086017	76.115278
124.194310	41.748712	76.120282
123.801420	34.740902	76.125287
123.221292	43.577110	76.130292
122.198866	45.569392	76.135297
121.377143	39.585531	76.140302
120.966597	53.197769	76.145306
121.073842	35.446009	76.150311
119.759140	53.966071	76.155316
119.081406	32.564525	76.160321
118.055834	47.973092	76.165326
117.864464	37.902453	76.170330
117.760890	38.556118	76.175335
116.613085	41.374162	76.180340
115.696184	43.277084	76.185345
115.079080	41.846056	76.190350
114.561866	47.561124	76.195354
113.633620	39.645274	76.200359
112.931958	49.633042	76.205364
112.598688	48.172521	76.210369
112.033303	37.202805	76.215374
111.614511	41.238606	76.220378
110.419395	53.165742	76.225383
109.771630	46.630630	76.230388
109.506094	43.295479	76.235393
108.495004	40.558582	76.240398
107.579783	44.916384	76.245402
107.082879	43.243855	76.250407
106.365412	46.518368	76.255412
106.328683	35.588922	76.260417
105.337677	47.913983	76.265422
104.678468	44.014029	76.270426
104.453378	43.294720	76.275431
103.440848	48.942131	76.280436
102.669007	38.809532	76.285441
101.914680	47.600991	76.290446
101.484531	52.923736	76.295450
100.490413	38.080284	76.300455
99.114576	38.977838	76.305460
98.938614	40.000990	76.310465
98.494371	39.666690	76.315470
98.502337	43.326954	76.320474
97.860998	45.572264	76.325479
96.867828	45.301850	76.330484
95.904556	39.053588	76.335489
95.636912	40.184395	76.340494
94.694453	44.180717	76.345498
94.015947	31.519754	76.350503
93.037626	43.191557	76.355508
92.914445	37.960418	76.360513
91.975332	43.058420	76.365518
91.287904	41.480930	76.370522
90.468030	45.273214	76.375527
90.044964	42.377899	76.380532
89.695510	37.274303	76.385537
88.645000	45.363997	76.390542
88.215526	43.587686	76.395546
87.792599	36.807009	76.400551
86.411822	44.162529	76.405556
85.682961	34.163424	76.410561
85.215429	48.303527	76.415566
84.824349	37.504706	76.420570
84.416189	37.845850	76.425575
83.672847	47.348293	76.430580
82.992704	31.114469	76.435585
82.235207	38.737993	76.440590
81.686790	29.282510	76.445594
80.664459	36.533559	76.450599
79.759528	42.789824	76.455604
79.644324	36.545082	76.460609
79.089790	44.971967	76.465614
78.240989	49.719705	76.470618
77.290051	33.590565	76.475623
76.762022	48.546083	76.480628
76.095698	40.907000	76.485633
75.857798	46.161241	76.490638
74.687289	38.490613	76.495642
74.267390	39.472252	76.500647
73.460285	49.871054	76.505652
73.340879	45.088713	76.510657
71.946368	55.062419	76.515662
71.404726	40.320272	76.520666
70.890898	41.163938	76.525671
70.297806	52.799546	76.530676
69.816873	44.339321	76.535681
68.860230	38.175164	76.540686
68.181554	45.628439	76.545690
67.976206	44.568541	76.550695
66.588966	47.295493	76.555700
65.963552	46.526501	76.560705
65.507036	44.079618	76.565710
65.034888	48.125514	76.570714
64.973747	43.501028	76.575719
63.299622	42.512966	76.580724
63.104250	49.684174	76.585729
62.368294	48.177505	76.590734
61.752400	51.435830	76.595738
61.180362	37.375004	76.600743
60.328749	53.927441	76.605748
60.177258	43.741646	76.610753
58.849886	41.849943	76.615758
58.022745	49.591810	76.620762
57.757045	41.754807	76.625767
57.077567	61.561209	76.630772
56.936909	33.739853	76.635777
55.751121	47.021599	76.640782
55.143453	52.599727	76.645786
54.735712	40.166806	76.650791
53.554245	48.159137	76.655796
53.014046	37.488179	76.660801
52.371799	34.077512	76.665806
51.907454	32.513337	76.670810
51.274693	39.298593	76.675815
50.077672	43.887426	76.680820
49.677510	42.100140	76.685825
49.173356	51.747358	76.690830
48.430032	39.418421	76.695834
47.698082	43.020087	76.700839
46.758879	43.832262	76.705844
46.326906	37.456709	76.710849
45.907963	44.494851	76.715854
45.429453	47.236139	76.720858
44.507606	40.194448	76.725863
43.740381	54.298785	76.730868
43.208388	38.624774	76.735873
42.640430	44.292755	76.740878
41.266978	47.408579	76.745882
40.945786	38.978077	76.750887
40.366129	40.283226	76.755892
40.049403	37.367807	76.760897
39.623632	41.275430	76.765902
38.339953	48.397884	76.770906
38.271236	44.222432	76.775911
37.366344	44.721653	76.780916
36.494639	36.694328	76.785921
35.625478	45.694913	76.790926
35.004128	38.993202	76.795930
34.547156	39.857767	76.800935
34.171765	49.724128	76.805940
33.283364	36.330318	76.810945
32.517663	39.628310	76.815950
32.070751	38.769360	76.820954
31.857365	32.786273	76.825959
30.318930	35.576779	76.830964
29.843441	46.104031	76.835969
29.311064	39.694037	76.840974
28.891634	42.640354	76.845978
28.191658	31.111862	76.850983
27.202806	42.290234	76.855988
27.004730	36.449773	76.860993
25.967208	40.352478	76.865998
25.058494	35.722849	76.871002
24.507417	30.665620	76.876007
23.828884	48.070326	76.881012
23.577027	37.782288	76.886017
22.717676	45.552952	76.891022
21.884893	38.861317	76.896026
21.492325	35.519637	76.901031
20.767411	45.876954	76.906036
20.304476	37.435953	76.911041
19.035048	36.758660	76.916046
18.589507	52.306534	76.921050
18.239699	30.844853	76.926055
17.551855	35.396632	76.931060
16.481107	36.966185	76.936065
15.920316	42.998854	76.941070
15.388438	35.918629	76.946074
15.321112	41.930930	76.951079
14.422030	42.462347	76.956084
13.670854	42.334705	76.961089
12.848738	42.893267	76.966094
11.935011	43.542130	76.971098
11.184185	35.539687	76.976103
10.296914	31.723449	76.981108
10.417147	39.593309	76.986113
9.546913	43.114548	76.991118
8.703659	41.367987	76.996122
8.413676	38.560263	77.001127
7.296222	37.354146	77.006132
7.235861	30.362705	77.011137
6.247470	43.537290	77.016142
5.437697	48.789721	77.021147
4.828692	38.333167	77.026151
4.453057	37.647343	77.031156
3.284798	49.638034	77.036161