Mon Mar 08 19:40:04 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.554302	96.669145	0.000000
-0.895905	80.982062	0.005005
-1.928117	37.381512	0.010010
-4.180983	20.069287	0.015014
-8.796025	4.338558	0.020019
-13.845903	8.092795	0.025024
-18.642225	13.433896	0.030029
-22.897469	19.235865	0.035034
-27.399989	25.514070	0.040038
-30.926495	11.465687	0.045043
-34.404326	25.691708	0.050048
-38.122495	22.478400	0.055053
-41.389663	7.470950	0.060058
-45.517609	25.258691	0.065062
-49.303673	7.574559	0.070067
-52.889634	24.373903	0.075072
-56.578384	11.746944	0.080077
-60.339366	11.773019	0.085082
-64.315162	15.918951	0.090086
-68.008237	20.153821	0.095091
-71.670965	25.195927	0.100096
-75.868154	19.275977	0.105101
-79.161734	27.318270	0.110106
-83.124113	15.685837	0.115110
-86.779952	9.706354	0.120115
-90.324886	23.564709	0.125120
-94.160803	17.140913	0.130125
-98.031271	10.484536	0.135130
-102.120861	19.486417	0.140134
-105.575677	9.070790	0.145139
-109.673077	20.450220	0.150144
-113.249478	21.593288	0.155149
-116.950588	18.022595	0.160154
-120.875595	26.335980	0.165158
-124.160157	13.849633	0.170163
-127.892910	26.802943	0.175168
-132.114048	18.215754	0.180173
-135.769348	17.187526	0.185178
-139.674435	19.482130	0.190182
-143.152437	16.276397	0.195187
-146.732120	13.976229	0.200192
-150.485267	14.660310	0.205197
-154.542086	2.256243	0.210202
-158.803494	17.984020	0.215206
-162.389074	21.593219	0.220211
-166.232074	20.541374	0.225216
-170.061706	21.478946	0.230221
-173.746548	16.557552	0.235226
-177.403988	15.641684	0.240230
-180.916696	19.963049	0.245235
-184.775270	15.140353	0.250240
-188.477618	22.664582	0.255245
-191.991200	14.052901	0.260250
-195.955206	18.685981	0.265254
-199.284665	18.268123	0.270259
-203.496874	21.739276	0.275264
-207.461294	18.951857	0.280269
-211.068588	18.270870	0.285274
-214.831351	22.860829	0.290278
-218.478146	22.280767	0.295283
-222.381903	23.878330	0.300288
-226.319511	19.337953	0.305293
-229.719022	15.935332	0.310298
-233.683092	18.737779	0.315302
-237.161345	22.184888	0.320307
-241.275487	23.543265	0.325312
-245.196999	23.672512	0.330317
-248.137939	14.911182	0.335322
-252.340451	15.900511	0.340326
-256.293440	9.088850	0.345331
-260.028401	15.205542	0.350336
-263.865322	25.260102	0.355341
-267.255175	13.621767	0.360346
-270.966503	15.040472	0.365350
-275.082526	11.077395	0.370355
-278.895619	17.558220	0.375360
-282.864884	25.614009	0.380365
-286.037720	14.239086	0.385370
-290.111160	17.536861	0.390374
-293.618635	18.558814	0.395379
-297.146161	15.805880	0.400384
-301.377263	20.879125	0.405389
-305.064574	18.016101	0.410394
-309.116530	16.617824	0.415398
-312.350874	12.454154	0.420403
-316.523236	19.916410	0.425408
-320.144139	21.196186	0.430413
-323.835964	5.165789	0.435418
-327.630584	18.903472	0.440422
-331.381633	17.004647	0.445427
-335.147134	10.226265	0.450432
-339.361989	10.938616	0.455437
-342.698759	7.600257	0.460442
-346.727039	16.204838	0.465446
-350.232399	11.456908	0.470451
-353.544988	15.986245	0.475456
-357.865536	14.906876	0.480461
-361.428338	9.497981	0.485466
-365.376267	19.677635	0.490470
-369.009891	11.703513	0.495475
-372.980522	22.351970	0.500480
-376.833814	13.323340	0.505485
-380.133830	8.408642	0.510490
-384.019303	10.516014	0.515494
-387.877695	18.286201	0.520499
-391.470758	8.575858	0.525504
-395.487119	11.222923	0.530509
-398.878567	9.703575	0.535514
-403.000243	15.601548	0.540518
-406.884438	13.146982	0.545523
-410.663425	14.242416	0.550528
-414.346343	18.034665	0.555533
-417.735597	-1.963875	0.560538
-421.732057	18.277476	0.565542
-425.447215	13.881678	0.570547
-429.197371	14.950461	0.575552
-433.196308	21.128486	0.580557
-436.519168	11.417643	0.585562
-440.497483	13.615619	0.590566
-444.271075	14.153622	0.595571
-447.806916	7.009197	0.600576
-452.111861	20.125284	0.605581
-455.317774	11.368699	0.610586
-459.314623	15.616390	0.615590
-462.925610	16.524242	0.620595
-466.803861	21.268631	0.625600
-470.893661	28.658043	0.630605
-474.316236	14.932798	0.635610
-478.421663	24.343058	0.640614
-481.943093	15.141771	0.645619
-485.635348	20.277500	0.650624
-489.528298	23.873188	0.655629
-493.205430	10.095597	0.660634
-496.929986	14.517467	0.665638
-500.603228	8.623417	0.670643
-504.535533	18.725100	0.675648
-508.403401	16.983975	0.680653
-511.899614	9.961043	0.685658
-515.983348	22.567282	0.690662
-519.645034	8.553901	0.695667
-523.206913	17.115809	0.700672
-526.913277	24.644328	0.705677
-531.007511	14.757227	0.710682
-534.552573	16.659097	0.715686
-538.191581	16.776815	0.720691
-541.934187	19.965403	0.725696
-546.125522	16.111019	0.730701
-549.658253	19.526273	0.735706
-553.516863	13.163636	0.740710
-556.981948	9.748315	0.745715
-560.795560	7.667478	0.750720
-564.858411	11.779238	0.755725
-568.286434	13.796492	0.760730
-572.612972	14.418291	0.765734
-576.064176	12.760521	0.770739
-579.615023	17.988910	0.775744
-583.310199	12.265639	0.780749
-587.124601	0.351880	0.785754
-591.187590	20.608837	0.790758
-594.797360	8.203539	0.795763
-598.578282	15.745646	0.800768
-602.202168	16.491778	0.805773
-605.807482	19.806754	0.810778
-609.895334	8.978993	0.815782
-613.745587	19.602282	0.820787
-617.098698	7.860862	0.825792
-621.369599	15.892830	0.830797
-625.012769	8.962932	0.835802
-628.901379	20.968941	0.840806
-632.086280	15.208379	0.845811
-635.855208	13.582533	0.850816
-639.829536	15.469566	0.855821
-643.667390	7.452831	0.860826
-647.662375	17.798119	0.865830
-651.285246	11.793769	0.870835
-654.714703	4.848698	0.875840
-659.013268	15.174701	0.880845
-662.324418	14.957976	0.885850
-666.121191	10.465228	0.890854
-669.881252	15.254126	0.895859
-673.700154	6.770828	0.900864
-677.770605	8.309034	0.905869
-681.087282	8.657722	0.910874
-684.862183	10.956052	0.915878
-688.514741	13.684235	0.920883
-692.469322	11.348614	0.925888
-696.718936	6.835243	0.930893
-700.506892	-3.352764	0.935898
-704.097070	16.661663	0.940902
-707.435430	8.169440	0.945907
-711.123487	2.175606	0.950912
-714.960405	5.776888	0.955917
-718.680484	1.016531	0.960922
-722.829705	20.312986	0.965926
-726.432517	9.146179	0.970931
-730.265768	9.115474	0.975936
-734.170619	21.300842	0.980941
-737.484849	3.086839	0.985946
-741.574344	7.281991	0.990950
-745.072888	4.957156	0.995955
-748.819570	12.549205	1.000960
-753.096178	11.520302	1.005965
-756.903131	9.482871	1.010970
-760.139290	3.260793	1.015974
-764.022012	2.840689	1.020979
-767.487690	7.800289	1.025984
-771.180824	13.371788	1.030989
-774.947091	1.770758	1.035994
-779.152826	15.511720	1.040998
-782.920250	3.584484	1.046003
-786.803061	15.340662	1.051008
-791.040429	12.933720	1.056013
-794.203593	2.376375	1.061018
-797.615346	12.297545	1.066022
-801.397847	8.187487	1.071027
-805.313451	7.044215	1.076032
-809.493799	8.248580	1.081037
-812.700005	6.268172	1.086042
-816.559384	8.305845	1.091046
-820.500742	6.636902	1.096051
-824.009647	8.681640	1.101056
-828.431255	5.525267	1.106061
-831.617287	7.862154	1.111066
-835.779218	6.878145	1.116070
-839.631451	12.576095	1.121075
-842.990983	9.875977	1.126080
-846.848654	4.631661	1.131085
-850.409911	-3.148253	1.136090
-854.271162	7.131825	1.141094
-858.236114	18.606379	1.146099
-861.743611	3.033113	1.151104
-865.595837	14.800289	1.156109
-869.110058	3.629022	1.161114
-872.663063	11.128800	1.166118
-876.690918	18.794376	1.171123
-880.914282	8.280494	1.176128
-884.646530	3.758875	1.181133
-888.175407	7.066779	1.186138
-892.021379	6.921686	1.191142
-895.610006	7.192736	1.196147
-899.349711	8.534954	1.201152
-903.232428	14.595816	1.206157
-906.831324	2.870492	1.211162
-910.879073	8.197721	1.216166
-914.787006	4.243512	1.221171
-918.187731	8.484949	1.226176
-922.250778	9.509922	1.231181
-925.917445	6.217266	1.236186
-929.589358	15.910575	1.241190
-933.184060	7.508560	1.246195
-936.590543	0.508215	1.251200
-940.779586	19.049769	1.256205
-944.389546	0.126513	1.261210
-948.524466	10.180857	1.266214
-952.122453	12.452898	1.271219
-955.648143	16.238171	1.276224
-959.523077	16.796351	1.281229
-963.304610	11.281458	1.286234
-967.440092	8.506917	1.291238
-971.054053	22.401134	1.296243
-974.688838	3.425130	1.301248
-978.484195	15.894530	1.306253
-981.943599	3.218278	1.311258
-985.835483	13.632759	1.316262
-989.634225	8.593708	1.321267
-993.747055	4.489488	1.326272
-997.379054	17.621864	1.331277
-1001.157394	15.093020	1.336282
-1004.783783	12.741717	1.341286
-1008.642376	5.458995	1.346291
-1012.133728	10.785718	1.351296
-1016.194797	6.113489	1.356301
-1020.003143	8.496537	1.361306
-1023.913319	16.747455	1.366310
-1027.384600	14.229467	1.371315
-1030.975174	7.482613	1.376320
-1034.692911	14.534347	1.381325
-1038.290378	7.588351	1.386330
-1042.602228	21.269455	1.391334
-1046.317397	18.864611	1.396339
-1050.121614	11.508612	1.401344
-1053.627206	14.590706	1.406349
-1057.255762	3.217277	1.411354
-1061.360024	13.853484	1.416358
-1065.232497	5.898202	1.421363
-1068.686941	1.526402	1.426368
-1072.268761	11.319037	1.431373
-1076.215254	10.108627	1.436378
-1079.984149	12.706217	1.441382
-1083.744691	4.037688	1.446387
-1087.518907	7.736759	1.451392
-1091.386680	15.804397	1.456397
-1094.727973	7.858810	1.461402
-1098.456542	13.501121	1.466406
-1102.294536	12.262363	1.471411
-1106.276034	3.452613	1.476416
-1110.402222	13.234619	1.481421
-1113.978406	11.430497	1.486426
-1117.590368	16.525952	1.491430
-1121.461203	8.737647	1.496435
-1125.157330	5.379067	1.501440
-1128.802618	10.345838	1.506445
-1132.552702	7.536749	1.511450
-1136.482533	-0.207396	1.516454
-1140.391294	6.553383	1.521459
-1143.610720	10.646296	1.526464
-1147.748124	19.824665	1.531469
-1151.467645	9.292194	1.536474
-1155.501639	6.971649	1.541478
-1159.310086	15.946033	1.546483
-1162.758717	9.153030	1.551488
-1166.684415	8.759393	1.556493
-1170.023355	5.181329	1.561498
-1173.604863	9.172952	1.566502
-1177.478377	19.036062	1.571507
-1181.309335	12.044081	1.576512
-1185.516326	21.511166	1.581517
-1189.287887	6.396974	1.586522
-1193.224458	23.747464	1.591526
-1196.919176	9.324248	1.596531
-1200.282918	8.068116	1.601536
-1203.941727	14.964035	1.606541
-1207.597942	10.793448	1.611546
-1211.876586	18.288407	1.616550
-1215.359794	13.804746	1.621555
-1219.012636	12.331570	1.626560
-1223.230853	7.908766	1.631565
-1226.723437	-3.771531	1.636570
-1230.235388	3.097769	1.641574
-1234.152673	12.644720	1.646579
-1237.710303	12.441444	1.651584
-1241.816314	14.055691	1.656589
-1245.639685	3.445396	1.661594
-1249.597959	2.886817	1.666598
-1252.962042	3.097255	1.671603
-1256.503263	5.595619	1.676608
-1260.531127	16.180509	1.681613
-1264.467468	8.639460	1.686618
-1268.033997	9.866249	1.691622
-1271.669482	6.327907	1.696627
-1275.369463	-1.432275	1.701632
-1279.417197	2.506395	1.706637
-1282.892510	1.096367	1.711642
-1286.980095	22.033185	1.716646
-1291.033851	8.933779	1.721651
-1294.431540	2.216404	1.726656
-1298.239994	14.007191	1.731661
-1302.074095	-3.222325	1.736666
-1305.826083	6.004994	1.741670
-1309.369153	9.951249	1.746675
-1312.963316	2.757613	1.751680
-1316.795502	2.763967	1.756685
-1320.310650	-3.527748	1.761690
-1324.165755	8.464489	1.766694
-1328.476541	-3.360628	1.771699
-1332.212239	13.986291	1.776704
-1336.186221	12.266685	1.781709
-1339.679788	2.057893	1.786714
-1343.386949	-0.238945	1.791718
-1347.098650	5.727447	1.796723
-1350.467597	-0.895101	1.801728
-1354.851527	4.750011	1.806733
-1358.210978	9.568884	1.811738
-1362.054593	3.512720	1.816742
-1366.036321	1.625689	1.821747
-1369.393024	-4.543089	1.826752
-1373.030301	4.013168	1.831757
-1377.081522	1.079240	1.836762
-1380.837159	5.925297	1.841766
-1384.875163	7.642439	1.846771
-1388.520820	6.513706	1.851776
-1392.531498	2.426972	1.856781
-1395.677922	6.620491	1.861786
-1399.621145	6.327818	1.866790
-1403.372425	5.611798	1.871795
-1406.921958	0.522524	1.876800
-1410.953118	7.736958	1.881805
-1414.568751	1.141385	1.886810
-1418.706496	-0.961828	1.891814
-1422.688288	4.882356	1.896819
-1425.916475	-7.916902	1.901824
-1429.616442	15.599226	1.906829
-1433.807786	-6.500384	1.911834
-1437.363216	-2.536195	1.916838
-1440.745510	0.242903	1.921843
-1444.683419	-10.766544	1.926848
-1448.992670	4.546821	1.931853
-1452.369304	-3.192298	1.936858
-1455.776826	5.666312	1.941862
-1459.851922	4.198057	1.946867
-1463.599794	-2.535518	1.951872
-1467.803426	-4.252811	1.956877
-1471.246840	-8.326159	1.961882
-1475.043319	-0.349756	1.966886
-1479.024573	-3.477614	1.971891
-1482.083741	-1.935957	1.976896
-1485.998759	-0.719260	1.981901
-1489.846122	-3.532677	1.986906
-1493.637604	2.596512	1.991910
-1497.785307	2.631615	1.996915
-1501.687295	-2.535788	2.006912
-1502.358240	-2.369761	2.016909
-1499.684162	5.236869	2.026906
-1497.204948	2.026572	2.036902
-1494.703514	5.319075	2.046899
-1492.869892	1.189079	2.056896
-1491.131263	1.311873	2.066893
-1489.643593	3.855726	2.076890
-1487.285624	-1.236055	2.086886
-1485.246914	7.257010	2.096883
-1483.553126	2.581033	2.106880
-1481.725227	-3.559465	2.116877
-1479.920001	2.822203	2.126874
-1477.908901	4.729662	2.136870
-1475.979844	4.624622	2.146867
-1474.046946	7.251923	2.156864
-1472.008303	-0.832697	2.166861
-1470.172487	0.733389	2.176858
-1468.307014	3.583053	2.186854
-1466.348435	8.798687	2.196851
-1464.611882	-0.732710	2.206848
-1462.710627	7.577138	2.216845
-1460.741868	-4.926478	2.226842
-1459.039764	6.260309	2.236838
-1456.926694	3.667584	2.246835
-1455.204527	7.626440	2.256832
-1453.274785	2.162760	2.266829
-1451.463333	10.684352	2.276826
-1449.510320	10.157109	2.286822
-1447.921821	15.048359	2.296819
-1445.751703	4.094496	2.306816
-1443.586206	2.630147	2.316813
-1442.144825	3.256851	2.326810
-1440.176071	3.412307	2.336806
-1438.005778	9.415063	2.346803
-1436.281586	2.200227	2.356800
-1434.484766	5.315103	2.366797
-1432.708992	-3.401559	2.376794
-1430.763406	4.129171	2.386790
-1429.020582	0.441623	2.396787
-1426.971172	9.992428	2.406784
-1424.896302	-1.961352	2.416781
-1423.007648	-5.233327	2.426778
-1421.312775	3.115913	2.436774
-1419.373664	-1.150907	2.446771
-1417.689977	7.203287	2.456768
-1415.588438	4.921895	2.466765
-1413.484065	0.832292	2.476762
-1411.936037	2.098734	2.486758
-1410.037056	-3.146843	2.496755
-1408.066156	3.045744	2.506752
-1406.275197	4.724845	2.516749
-1404.389275	-1.271740	2.526746
-1402.383499	6.928279	2.536742
-1401.057959	9.937064	2.546739
-1398.596566	6.344488	2.556736
-1396.548168	12.118923	2.566733
-1395.168876	11.598313	2.576730
-1393.098547	12.196990	2.586726
-1391.295711	12.015918	2.596723
-1389.324632	7.448761	2.606720
-1387.211297	12.347611	2.616717
-1385.432230	15.478002	2.626714
-1383.474848	9.918377	2.636710
-1382.194753	10.345164	2.646707
-1380.212625	1.418672	2.656704
-1377.894192	9.544985	2.666701
-1376.105062	8.578282	2.676698
-1374.414209	8.189376	2.686694
-1372.464962	10.354708	2.696691
-1370.467050	3.288718	2.706688
-1368.439610	13.555154	2.716685
-1366.923469	15.346169	2.726682
-1364.951495	8.795874	2.736678
-1362.953527	15.206790	2.746675
-1361.150106	9.943387	2.756672
-1359.286004	-2.085546	2.766669
-1357.408371	9.213751	2.776666
-1355.545324	6.168540	2.786662
-1353.875551	5.306217	2.796659
-1351.750700	7.056644	2.806656
-1349.812283	3.063128	2.816653
-1348.116624	8.101496	2.826650
-1346.398841	11.281197	2.836646
-1344.282553	10.388459	2.846643
-1342.228334	8.711505	2.856640
-1340.359154	12.533246	2.866637
-1338.423884	7.496632	2.876634
-1336.967405	10.223991	2.886630
-1335.037183	16.565257	2.896627
-1333.113773	8.944417	2.906624
-1330.886833	11.055866	2.916621
-1329.155465	13.480304	2.926618
-1327.369318	8.369679	2.936614
-1325.585451	9.186359	2.946611
-1323.398741	7.977654	2.956608
-1321.737906	14.016283	2.966605
-1319.935259	9.618234	2.976602
-1317.895844	9.085166	2.986598
-1315.993610	7.184684	2.996595
-1314.220688	5.366474	3.006592
-1312.221129	10.612003	3.016589
-1310.362134	1.351612	3.026586
-1308.929719	6.972103	3.036582
-1306.862644	11.043232	3.046579
-1304.715196	7.766241	3.056576
-1302.558717	4.249403	3.066573
-1301.066949	2.821965	3.076570
-1299.352016	16.179318	3.086566
-1297.579910	9.874205	3.096563
-1295.489902	9.907755	3.106560
-1293.323202	11.833107	3.116557
-1291.718740	7.762038	3.126554
-1289.956937	6.280338	3.136550
-1288.018688	12.525631	3.146547
-1286.167691	4.981149	3.156544
-1284.136455	7.948114	3.166541
-1282.261995	3.884366	3.176538
-1280.430754	10.580968	3.186534
-1278.638487	9.432271	3.196531
-1276.574897	13.466095	3.206528
-1274.737160	1.927716	3.216525
-1272.892414	4.154065	3.226522
-1271.080761	10.310692	3.236518
-1269.262062	8.267310	3.246515
-1266.870567	8.663136	3.256512
-1265.528995	13.930328	3.266509
-1263.761029	9.760486	3.276506
-1261.667736	12.984365	3.286502
-1260.052676	11.734575	3.296499
-1258.152630	16.928192	3.306496
-1255.981829	8.762593	3.316493
-1254.115534	6.758971	3.326490
-1252.238761	10.833764	3.336486
-1250.321426	5.839560	3.346483
-1248.591059	13.924341	3.356480
-1246.458054	7.278902	3.366477
-1244.948826	14.507031	3.376474
-1242.966941	9.271993	3.386470
-1241.203555	4.007190	3.396467
-1239.124571	12.445110	3.406464
-1237.064762	8.594877	3.416461
-1235.352695	6.945925	3.426458
-1233.639008	6.529785	3.436454
-1231.489582	8.266921	3.446451
-1229.964350	12.221155	3.456448
-1227.700669	16.267215	3.466445
-1226.022053	16.794521	3.476442
-1224.056035	9.271147	3.486438
-1222.434696	11.424346	3.496435
-1220.259359	11.941644	3.506432
-1218.348061	10.753422	3.516429
-1216.728847	5.279615	3.526426
-1214.810734	10.895083	3.536422
-1212.892648	15.380113	3.546419
-1211.253707	6.914418	3.556416
-1208.985349	10.479781	3.566413
-1207.139244	9.693551	3.576410
-1205.429998	4.420068	3.586406
-1203.757069	14.018705	3.596403
-1201.618378	6.013017	3.606400
-1199.527835	7.686978	3.616397
-1197.744811	10.134829	3.626394
-1196.309901	15.169252	3.636390
-1193.977560	11.109672	3.646387
-1192.027329	13.657082	3.656384
-1190.243961	13.310345	3.666381
-1188.563593	15.604115	3.676378
-1186.306791	10.513017	3.686374
-1184.834094	13.302614	3.696371
-1183.201153	13.268878	3.706368
-1180.805814	7.917217	3.716365
-1179.443233	3.471266	3.726362
-1177.107714	12.128712	3.736358
-1175.388532	4.603819	3.746355
-1173.419616	13.389391	3.756352
-1171.456715	15.500613	3.766349
-1169.665673	12.500220	3.776346
-1167.841913	9.911407	3.786342
-1166.188504	13.311533	3.796339
-1163.895507	8.809887	3.806336
-1161.871680	16.292042	3.816333
-1160.480693	17.849026	3.826330
-1158.571821	11.981570	3.836326
-1156.802172	14.875247	3.846323
-1154.654215	18.414143	3.856320
-1152.761054	10.904057	3.866317
-1150.953619	13.930631	3.876314
-1148.882772	17.497658	3.886310
-1147.153192	21.611879	3.896307
-1145.349766	12.560999	3.906304
-1143.633505	18.654057	3.916301
-1141.455201	17.983669	3.926298
-1139.754460	14.775127	3.936294
-1137.963927	7.144113	3.946291
-1136.018646	7.557777	3.956288
-1133.837223	10.890825	3.966285
-1132.030616	8.277944	3.976282
-1130.378506	9.493194	3.986278
-1128.369408	6.001667	3.996275
-1126.580629	6.148289	4.006272
-1124.633475	10.085625	4.016269
-1122.772567	10.700678	4.026266
-1121.082613	9.598465	4.036262
-1118.956149	6.422884	4.046259
-1117.061137	9.113392	4.056256
-1115.374770	8.690657	4.066253
-1113.495034	2.922629	4.076250
-1111.384002	6.262222	4.086246
-1109.884760	14.050955	4.096243
-1107.888359	14.451729	4.106240
-1105.796259	8.840774	4.116237
-1104.068489	9.290836	4.126234
-1102.252963	13.317137	4.136230
-1100.105565	9.378803	4.146227
-1098.327983	11.260800	4.156224
-1096.671842	15.577847	4.166221
-1094.483619	8.434263	4.176218
-1092.452101	7.193757	4.186214
-1091.039989	14.483319	4.196211
-1089.186239	9.638347	4.206208
-1087.184039	1.754055	4.216205
-1085.135565	6.695146	4.226202
-1083.506733	1.458291	4.236198
-1081.738276	7.771976	4.246195
-1079.461181	8.993079	4.256192
-1077.646737	5.449050	4.266189
-1075.752302	13.621408	4.276186
-1074.077903	10.233982	4.286182
-1072.225778	11.887776	4.296179
-1070.221076	14.035028	4.306176
-1068.487209	12.089045	4.316173
-1066.552745	8.587401	4.326170
-1064.488808	7.681184	4.336166
-1062.591008	11.058087	4.346163
-1060.805252	11.118407	4.356160
-1059.252145	6.490479	4.366157
-1057.232448	10.616783	4.376154
-1055.323207	9.018524	4.386150
-1053.343854	7.309587	4.396147
-1051.299178	9.093643	4.406144
-1049.702030	8.633123	4.416141
-1047.710364	1.816262	4.426138
-1045.726290	11.425260	4.436134
-1043.854107	11.370725	4.446131
-1042.236459	10.479066	4.456128
-1040.168621	9.147540	4.466125
-1038.415694	9.438901	4.476122
-1036.522163	12.567053	4.486118
-1034.491526	11.650400	4.496115
-1032.896753	10.236652	4.506112
-1030.921593	12.977569	4.516109
-1028.955070	14.219974	4.526106
-1027.012844	9.638773	4.536102
-1025.444107	8.792839	4.546099
-1023.128652	10.764127	4.556096
-1021.266760	12.179576	4.566093
-1019.603495	9.690747	4.576090
-1017.656870	10.860558	4.586086
-1016.121852	11.276779	4.596083
-1013.765868	13.083711	4.606080
-1011.843613	22.042682	4.616077
-1010.090776	12.093728	4.626074
-1008.415850	15.335806	4.636070
-1006.557607	7.973507	4.646067
-1004.869660	9.854124	4.656064
-1002.716036	11.210303	4.666061
-1000.656758	5.539953	4.676058
-999.128319	7.701853	4.686054
-996.668530	6.408731	4.696051
-995.288781	11.924182	4.706048
-993.489500	8.805768	4.716045
-991.316695	11.892456	4.726042
-989.649077	9.508734	4.736038
-987.640544	6.636316	4.746035
-985.948931	9.446297	4.756032
-983.972660	12.847032	4.766029
-981.741586	5.976148	4.776026
-980.344807	11.556775	4.786022
-978.598591	9.864655	4.796019
-976.354538	7.871891	4.806016
-974.504473	6.298947	4.816013
-972.561831	4.804354	4.826010
-971.028040	3.037267	4.836006
-968.993827	11.728911	4.846003
-966.985439	12.015791	4.856000
-965.117278	16.177464	4.865997
-963.237577	5.336740	4.875994
-961.515004	9.322759	4.885990
-959.645945	9.807175	4.895987
-957.677998	14.246562	4.905984
-955.729288	10.052774	4.915981
-954.001043	10.482347	4.925978
-952.429142	12.327878	4.935974
-950.196359	12.255231	4.945971
-948.051279	9.675201	4.955968
-946.391312	12.431855	4.965965
-944.391453	10.326597	4.975962
-942.488507	12.326031	4.985958
-941.025562	15.947819	4.995955
-938.977059	17.150352	5.005952
-936.751431	8.755217	5.015949
-935.027925	11.879062	5.025946
-933.408537	10.477234	5.035942
-931.284201	8.030002	5.045939
-929.564936	6.710096	5.055936
-927.770451	7.400657	5.065933
-925.903430	11.733059	5.075930
-923.936935	9.408957	5.085926
-922.114562	10.685551	5.095923
-919.990765	9.343602	5.105920
-918.126454	11.854463	5.115917
-916.509588	7.279581	5.125914
-914.297246	11.072078	5.135910
-912.683384	8.681215	5.145907
-910.761733	8.702555	5.155904
-908.843649	8.067671	5.165901
-906.942124	8.153807	5.175898
-905.136427	8.214215	5.185894
-903.602647	7.708666	5.195891
-901.452755	16.132427	5.205888
-899.316193	9.406188	5.215885
-897.456603	2.443201	5.225882
-895.914021	9.495734	5.235878
-893.946773	12.845890	5.245875
-892.074611	10.150079	5.255872
-890.317940	6.681734	5.265869
-887.914475	7.273391	5.275866
-886.207414	10.688830	5.285862
-884.663858	11.591635	5.295859
-882.497091	14.472565	5.305856
-880.760994	9.414465	5.315853
-878.745179	7.909828	5.325850
-877.078984	8.721984	5.335846
-875.047956	12.338256	5.345843
-873.308675	16.042221	5.355840
-871.386474	10.033911	5.365837
-869.687097	12.001216	5.375834
-867.364760	4.234850	5.385830
-865.902946	9.674112	5.395827
-863.921219	10.112174	5.405824
-862.100558	14.077856	5.415821
-859.930576	10.232430	5.425818
-858.175398	6.041237	5.435814
-856.347637	11.586208	5.445811
-854.320738	12.197045	5.455808
-852.408109	8.916940	5.465805
-850.780872	3.337879	5.475802
-849.174426	6.087370	5.485798
-846.895970	10.423539	5.495795
-845.240061	7.917058	5.505792
-843.253347	7.397563	5.515789
-841.097276	1.915542	5.525786
-839.416937	1.591856	5.535782
-837.846091	12.089683	5.545779
-835.496346	6.431454	5.555776
-833.773925	15.743031	5.565773
-831.906942	10.032505	5.575770
-830.112582	13.020378	5.585766
-828.093853	8.326057	5.595763
-826.267260	15.080633	5.605760
-824.717378	9.954448	5.615757
-822.742998	9.067492	5.625754
-820.455415	12.513342	5.635750
-818.720933	9.970637	5.645747
-817.135338	15.614345	5.655744
-815.103431	8.369677	5.665741
-813.283450	10.767717	5.675738
-811.363086	12.590803	5.685734
-809.441741	11.750228	5.695731
-807.467608	7.934573	5.705728
-805.721740	16.508265	5.715725
-803.858890	4.247805	5.725722
-801.757443	9.245427	5.735718
-800.353052	9.990542	5.745715
-798.214648	10.394145	5.755712
-796.277697	10.645224	5.765709
-794.596197	5.799580	5.775706
-792.385289	11.343362	5.785702
-790.588741	9.423874	5.795699
-788.838358	13.953442	5.805696
-786.849047	19.396870	5.815693
-785.095122	11.307763	5.825690
-783.001154	14.669340	5.835686
-781.245207	6.041530	5.845683
-779.240436	13.901277	5.855680
-777.489971	16.102049	5.865677
-775.925392	16.493179	5.875674
-773.931086	9.786622	5.885670
-771.770986	19.541428	5.895667
-769.940459	11.795328	5.905664
-768.168969	11.663953	5.915661
-766.478168	9.177211	5.925658
-764.212423	13.035527	5.935654
-762.636980	9.435193	5.945651
-760.804881	14.172763	5.955648
-758.830001	15.262492	5.965645
-756.898839	22.753528	5.975642
-755.117391	12.699117	5.985638
-753.274931	20.234328	5.995635
-751.374067	13.874277	6.005632
-749.545928	13.858592	6.015629
-747.392204	15.571812	6.025626
-745.416801	14.962633	6.035622
-743.756636	14.130694	6.045619
-742.033317	19.092493	6.055616
-739.959193	16.931327	6.065613
-737.995204	16.680797	6.075610
-736.323697	11.034734	6.085606
-734.556988	9.080585	6.095603
-732.382702	15.473383	6.105600
-730.479170	14.100489	6.115597
-728.747446	9.046349	6.125594
-726.833478	11.502065	6.135590
-725.137472	8.076687	6.145587
-723.059139	17.069395	6.155584
-721.156743	4.182184	6.165581
-719.431559	6.784907	6.175578
-717.636878	6.815643	6.185574
-715.697702	11.675077	6.195571
-713.495557	5.688464	6.205568
-712.042530	8.803599	6.215565
-709.925566	12.163147	6.225562
-708.123581	9.887610	6.235558
-706.358751	8.930032	6.245555
-704.391420	19.074106	6.255552
-702.446205	8.977775	6.265549
-700.263779	11.209050	6.275546
-698.795168	12.949688	6.285542
-696.778644	4.982882	6.295539
-695.078042	11.096164	6.305536
-693.141382	4.395725	6.315533
-691.272209	11.951978	6.325530
-689.153336	14.166579	6.335526
-687.418118	12.007508	6.345523
-685.642497	13.478062	6.355520
-683.729916	12.905813	6.365517
-682.127577	9.198606	6.375514
-679.980333	15.126861	6.385510
-677.909551	11.003778	6.395507
-675.962192	12.945814	6.405504
-674.337702	14.956807	6.415501
-672.592755	19.152622	6.425498
-670.593618	18.590236	6.435494
-668.611706	14.822391	6.445491
-667.123778	14.755344	6.455488
-664.950109	6.714509	6.465485
-663.223238	17.702251	6.475482
-661.055739	10.549715	6.485478
-658.989391	16.058312	6.495475
-657.510611	21.460275	6.505472
-655.639763	8.928647	6.515469
-653.943525	13.927995	6.525466
-651.763843	10.572222	6.535462
-649.673556	22.848673	6.545459
-648.303868	13.898996	6.555456
-646.258392	15.872747	6.565453
-644.276052	14.476278	6.575450
-642.664218	8.141961	6.585446
-640.447532	11.397225	6.595443
-638.832445	16.109571	6.605440
-636.685550	13.889502	6.615437
-634.976736	17.344325	6.625434
-632.947277	12.105322	6.635430
-631.146489	12.071994	6.645427
-629.394437	17.412950	6.655424
-627.548330	17.299757	6.665421
-625.384992	10.029502	6.675418
-623.540406	4.968455	6.685414
-621.958914	13.194372	6.695411
-620.040982	13.304959	6.705408
-618.070758	13.756119	6.715405
-616.145143	4.761859	6.725402
-614.332233	6.299136	6.735398
-612.645995	12.602661	6.745395
-610.410277	11.059960	6.755392
-608.502007	0.380694	6.765389
-606.975652	14.120863	6.775386
-604.844487	10.851824	6.785382
-602.949909	16.147928	6.795379
-601.059623	7.189319	6.805376
-599.295833	12.503160	6.815373
-597.637042	4.407272	6.825370
-595.349039	7.253318	6.835366
-593.662646	-0.979597	6.845363
-591.974664	11.662728	6.855360
-589.931011	7.978235	6.865357
-588.398322	11.238610	6.875354
-586.225420	13.732024	6.885350
-584.155741	8.693465	6.895347
-582.442850	7.038530	6.905344
-580.617770	15.337667	6.915341
-578.707312	3.238686	6.925338
-576.916137	12.812633	6.935334
-574.615864	14.766271	6.945331
-572.957503	13.925265	6.955328
-571.171415	9.298308	6.965325
-569.186747	2.471879	6.975322
-567.374085	6.619064	6.985318
-565.397271	13.004098	6.995315
-563.712263	9.913722	7.005312
-561.909022	12.541989	7.015309
-559.869827	15.116781	7.025306
-557.966695	13.362006	7.035302
-556.169631	9.559044	7.045299
-554.330140	16.179168	7.055296
-552.441503	16.926027	7.065293
-550.235668	14.518210	7.075290
-548.608296	14.591586	7.085286
-546.776773	12.639849	7.095283
-544.851600	19.407340	7.105280
-543.017085	11.779172	7.115277
-541.055430	7.427333	7.125274
-538.907950	12.934134	7.135270
-537.721020	9.678607	7.145267
-535.623179	17.024803	7.155264
-533.788493	8.113013	7.165261
-531.723525	6.599236	7.175258
-529.811653	8.152350	7.185254
-528.092016	2.277698	7.195251
-526.202840	13.812753	7.205248
-524.291182	8.469502	7.215245
-522.328507	7.903590	7.225242
-520.480044	7.791683	7.235238
-518.455642	6.844887	7.245235
-516.581436	9.444488	7.255232
-514.723991	3.195752	7.265229
-513.204533	-0.292858	7.275226
-511.010808	8.100606	7.285222
-509.126890	4.721148	7.295219
-507.603536	7.675192	7.305216
-505.507659	11.399853	7.315213
-503.674581	14.148130	7.325210
-501.657211	12.013598	7.335206
-499.931315	4.573326	7.345203
-497.773141	8.395406	7.355200
-496.269837	5.193577	7.365197
-494.377856	13.194753	7.375194
-492.346336	0.863352	7.385190
-490.063138	10.174070	7.395187
-488.415596	9.015922	7.405184
-486.604677	8.968454	7.415181
-484.672257	6.129128	7.425178
-483.115950	6.136534	7.435174
-481.377925	6.416480	7.445171
-479.433207	9.559027	7.455168
-477.170548	8.695787	7.465165
-475.394462	7.772894	7.475162
-473.527831	3.207351	7.485158
-471.662479	3.069101	7.495155
-469.635909	9.804672	7.505152
-468.210321	8.489363	7.515149
-466.030433	16.968767	7.525146
-464.106443	6.547594	7.535142
-462.306891	9.542821	7.545139
-460.447583	16.358794	7.555136
-458.475418	9.021317	7.565133
-456.794969	7.619529	7.575130
-455.283915	5.652725	7.585126
-452.975385	13.110608	7.595123
-450.934655	8.640429	7.605120
-449.207289	11.031443	7.615117
-447.340953	5.038686	7.625114
-445.251269	14.740332	7.635110
-443.412719	17.855657	7.645107
-441.715960	12.865708	7.655104
-439.789107	15.809050	7.665101
-437.518405	14.845096	7.675098
-436.225698	8.343979	7.685094
-434.234368	5.612121	7.695091
-432.433405	12.004828	7.705088
-430.334863	11.104684	7.715085
-428.765101	11.329437	7.725082
-426.646524	13.245922	7.735078
-424.817962	19.645284	7.745075
-422.955643	12.922176	7.755072
-420.849715	4.742368	7.765069
-419.195948	7.749854	7.775066
-417.145683	4.350219	7.785062
-415.211527	7.815012	7.795059
-413.705350	11.528132	7.805056
-411.749850	14.594809	7.815053
-409.699917	8.200155	7.825050
-407.670759	10.048834	7.835046
-406.134167	5.802860	7.845043
-404.026050	10.652958	7.855040
-402.456452	11.613498	7.865037
-400.583185	10.850394	7.875034
-398.333841	8.980470	7.885030
-396.785564	6.807245	7.895027
-394.728798	11.256628	7.905024
-392.813573	13.276659	7.915021
-390.842228	9.974902	7.925018
-389.137232	11.940086	7.935014
-387.411551	14.465618	7.945011
-385.323354	10.742602	7.955008
-383.882343	14.439306	7.965005
-381.370882	14.226391	7.975002
-379.546795	11.222874	7.984998
-377.900207	12.430069	7.994995
-376.024501	8.515212	8.004992
-374.256926	11.572452	8.014989
-372.477174	9.701738	8.024986
-370.427833	11.278823	8.034982
-368.518269	16.294857	8.044979
-366.541910	14.541170	8.054976
-364.488188	9.625329	8.064973
-362.759436	14.127109	8.074970
-360.924271	14.352164	8.084966
-359.168417	13.416797	8.094963
-357.419599	12.144680	8.104960
-355.525325	18.550976	8.114957
-353.121054	18.527298	8.124954
-351.530539	10.802433	8.134950
-349.576501	13.837819	8.144947
-348.306676	15.141497	8.154944
-346.345292	13.251279	8.164941
-344.233746	9.486678	8.174938
-342.177888	14.132032	8.184934
-340.103428	12.713211	8.194931
-338.522913	14.253068	8.204928
-336.801952	7.790995	8.214925
-334.505927	10.449714	8.224922
-332.849972	8.145661	8.234918
-330.763288	10.504665	8.244915
-329.141377	7.127695	8.254912
-327.290609	11.414246	8.264909
-325.065109	4.690073	8.274906
-323.572143	9.171103	8.284902
-321.562527	8.349982	8.294899
-319.933418	13.863956	8.304896
-318.008352	10.015467	8.314893
-315.903126	16.528640	8.324890
-314.164470	8.240183	8.334886
-311.851615	10.537839	8.344883
-310.245259	7.787010	8.354880
-308.600596	12.025955	8.364877
-306.462689	9.728667	8.374874
-304.927836	12.395240	8.384870
-302.732310	12.420721	8.394867
-300.818488	17.410872	8.404864
-299.006808	9.173922	8.414861
-297.280453	11.281017	8.424858
-295.312050	8.515036	8.434854
-293.838358	5.925911	8.444851
-291.717418	14.986442	8.454848
-289.551565	17.380213	8.464845
-287.693233	8.613224	8.474842
-285.990643	15.064385	8.484838
-284.043893	4.887583	8.494835
-282.114075	6.914847	8.504832
-280.244309	9.199579	8.514829
-278.371748	6.063669	8.524826
-276.476662	14.228742	8.534822
-274.957180	10.055045	8.544819
-272.830828	12.613021	8.554816
-270.732962	15.447108	8.564813
-269.103907	15.881962	8.574810
-267.222122	11.282570	8.584807
-265.318410	15.213376	8.594803
-263.520605	10.346355	8.604800
-261.575474	9.267171	8.614797
-259.664976	10.403908	8.624794
-257.746859	13.535100	8.634791
-256.177476	5.248436	8.644787
-254.017979	10.813587	8.654784
-251.997686	8.948777	8.664781
-250.247756	8.188107	8.674778
-248.244736	8.043848	8.684775
-246.827667	7.394723	8.694771
-244.963501	10.346652	8.704768
-242.623124	13.312575	8.714765
-240.341160	4.226973	8.724762
-238.902103	5.978934	8.734759
-237.263439	2.277263	8.744755
-235.255982	-0.603843	8.754752
-233.255577	8.472821	8.764749
-231.627227	5.781686	8.774746
-229.519212	5.295442	8.784743
-227.892742	4.295560	8.794739
-225.720621	0.039843	8.804736
-224.271137	7.101406	8.814733
-222.170333	-1.914216	8.824730
-219.991026	-0.959286	8.834727
-218.391660	3.697453	8.844723
-216.670430	4.155525	8.854720
-214.775934	8.449398	8.864717
-212.894345	-0.796481	8.874714
-210.924965	-1.873179	8.884711
-208.837443	4.653967	8.894707
-207.122399	7.310795	8.904704
-205.141210	4.430747	8.914701
-203.559793	-2.716294	8.924698
-201.590220	2.268197	8.934695
-199.643082	3.238092	8.944691
-197.676981	4.978600	8.954688
-195.891283	5.145363	8.964685
-193.851407	8.124553	8.974682
-192.158924	-0.153297	8.984679
-190.344561	0.888316	8.994675
-188.258660	4.235933	9.004672
-186.627460	1.762254	9.014669
-184.687807	0.909781	9.024666
-183.101471	5.101285	9.034663
-180.838440	4.186160	9.044659
-179.022479	6.729017	9.054656
-177.194145	2.840812	9.064653
-175.158487	-2.076729	9.074650
-173.034372	2.669981	9.084647
-171.415323	-3.201017	9.094643
-169.817356	3.255870	9.104640
-167.719999	6.933237	9.114637
-165.836551	-2.870241	9.124634
-164.012169	4.420471	9.134631
-162.056833	-3.722469	9.144627
-160.209706	10.933124	9.154624
-158.756477	2.382435	9.164621
-156.563822	-1.767558	9.174618
-154.684420	5.853837	9.184615
-152.731547	-8.168350	9.194611
-150.860124	5.487114	9.204608
-148.969190	-0.556719	9.214605
-146.764622	3.280390	9.224602
-145.192771	9.245706	9.234599
-143.350058	6.394116	9.244595
-141.600403	10.725371	9.254592
-139.719515	11.511687	9.264589
-137.726885	10.044518	9.274586
-135.939525	5.258197	9.284583
-133.635565	3.749252	9.294579
-132.151078	4.777231	9.304576
-130.359898	7.827734	9.314573
-128.257627	6.253085	9.324570
-126.546566	7.961717	9.334567
-124.747571	4.199802	9.344563
-122.667793	-0.001622	9.354560
-120.906009	8.481676	9.364557
-118.935858	4.665617	9.374554
-116.861197	-3.925777	9.384551
-115.339512	12.270641	9.394547
-113.284010	4.544356	9.404544
-111.832301	17.512139	9.414541
-109.254283	10.438237	9.424538
-107.602770	5.711500	9.434535
-105.543820	15.055246	9.444531
-104.328746	-2.698453	9.454528
-102.179661	-2.092257	9.464525
-100.138259	5.718063	9.474522
-98.341761	-1.079571	9.484519
-96.720011	7.558712	9.494515
-94.805176	2.115804	9.504512
-92.388352	-2.224625	9.514509
-90.828699	7.249308	9.524506
-88.841993	1.149188	9.534503
-87.016685	3.761672	9.544499
-85.180624	12.234732	9.554496
-83.585028	6.692768	9.564493
-81.288454	15.321300	9.574490
-79.540291	3.521680	9.584487
-77.597579	6.595415	9.594483
-76.090969	11.930174	9.604480
-73.878417	10.456392	9.614477
-72.142606	2.777982	9.624474
-70.320436	11.728504	9.634471
-68.194290	2.478442	9.644467
-66.406720	14.787977	9.654464
-64.404099	8.483239	9.664461
-62.809365	13.233983	9.674458
-60.812024	2.725601	9.684455
-58.846462	4.777344	9.694451
-57.043925	13.036315	9.704448
-55.278632	8.949843	9.714445
-53.142535	7.112508	9.724442
-51.424174	9.085278	9.734439
-49.809234	3.121854	9.744435
-47.785393	10.519787	9.754432
-45.435605	-0.305315	9.764429
-43.859143	0.528058	9.774426
-42.177551	3.094033	9.784423
-40.214238	4.064635	9.794419
-38.247667	6.286752	9.804416
-36.510824	6.361958	9.814413
-34.701450	10.876390	9.824410
-32.606111	7.392512	9.834407
-30.622164	9.270831	9.844403
-28.846759	8.839394	9.854400
-27.040182	9.148207	9.864397
-25.092590	9.699775	9.874394
-23.077315	6.075528	9.884391
-21.636842	6.867452	9.894387
-19.647686	9.709631	9.904384
-17.606357	6.070180	9.914381
-15.766635	11.708668	9.924378
-13.590278	0.244978	9.934375
-11.904287	11.487665	9.944371
-10.143951	12.146477	9.954368
-8.439975	12.187475	9.964365
-6.323792	12.178514	9.974362
-4.583153	5.915609	9.984359
-3.198312	29.841940	9.994355
-2.031441	65.654016	10.004352
-1.338284	123.429578	10.014349
0.000000	171.294436	10.019354
0.806990	216.454731	10.024359
1.345282	253.751626	10.029363
1.775640	291.292902	10.034368
2.076912	320.609402	10.039373
2.481666	339.241905	10.044378
2.811030	362.829961	10.049383
2.969748	371.176368	10.054387
3.395063	388.127858	10.059392
3.469437	410.083593	10.064397
3.801509	414.838626	10.069402
3.561326	419.818967	10.074407
3.810047	415.805640	10.079411
3.607375	426.568734	10.084416
3.705902	426.661910	10.089421
4.001439	437.662504	10.094426
4.169952	454.497342	10.099431
4.607040	454.845589	10.104435
4.633890	461.633041	10.109440
4.406383	448.631720	10.114445
4.401462	437.255368	10.119450
4.287225	446.627753	10.124455
4.460383	446.603374	10.129459
4.235467	450.550008	10.134464
4.319351	455.641094	10.139469
4.687357	467.346058	10.144474
4.452846	473.550754	10.149479
4.834361	477.066372	10.154483
4.791722	474.953920	10.159488
4.717104	480.776741	10.164493
4.722168	476.371769	10.169498
4.509315	489.052453	10.174503
4.912170	479.878596	10.179507
5.125518	485.264421	10.184512
4.868289	480.461331	10.189517
5.112726	482.942298	10.194522
4.853976	481.671681	10.199527
5.277010	491.038823	10.204531
5.205494	495.844061	10.209536
5.100133	491.767345	10.214541
5.161063	483.753421	10.219546
5.032137	515.379691	10.224551
5.347747	503.338753	10.229555
4.952907	493.396443	10.234560
5.122303	508.895578	10.239565
5.222046	507.148328	10.244570
5.228929	507.353888	10.249575
5.531359	534.928174	10.254579
5.637629	535.570452	10.259584
6.031822	539.527170	10.264589
5.825919	515.889343	10.269594
5.522384	511.259202	10.274599
5.628789	516.608481	10.279603
5.752479	533.830592	10.284608
5.821632	531.774416	10.289613
5.804177	534.476929	10.294618
5.438411	551.695129	10.299623
5.936530	533.248089	10.304627
5.699497	538.360428	10.309632
5.872312	552.364168	10.314637
6.041545	547.239156	10.319642
5.682994	548.611560	10.324647
6.226322	545.159892	10.329651
6.137510	543.020103	10.334656
6.183334	560.349279	10.339661
6.413581	546.273531	10.344666
6.280519	560.836980	10.349671
6.542829	543.608633	10.354675
6.162513	553.400403	10.359680
6.503829	563.807186	10.364685
6.836032	576.970273	10.369690
6.770192	584.225136	10.374695
7.000711	582.017064	10.379699
6.751813	573.178905	10.384704
6.690676	563.486087	10.389709
6.780553	574.232591	10.394714
6.436657	559.537222	10.399719
6.660168	588.817785	10.404723
6.981309	561.035305	10.409728
6.735994	589.744118	10.414733
7.075795	591.397791	10.419738
7.237303	595.524097	10.424743
7.242994	598.763807	10.429747
7.127989	603.156560	10.434752
7.149578	605.638400	10.439757
7.656447	598.501007	10.444762
7.108808	580.632272	10.449767
6.835198	577.312470	10.454771
6.983214	606.792762	10.459776
7.045877	599.838177	10.464781
7.377237	604.459349	10.469786
7.296221	612.606020	10.474791
7.481263	609.315557	10.479795
7.591148	608.165900	10.484800
7.125336	617.342165	10.489805
7.138523	612.909049	10.494810
7.240732	633.211243	10.499815
7.889240	637.392347	10.504819
7.777836	619.138606	10.509824
7.724740	635.324625	10.514829
7.874868	637.049554	10.519834
7.794250	649.504289	10.524839
8.242024	628.769181	10.529843
8.054682	642.078268	10.534848
8.202495	646.083775	10.539853
8.008105	640.603576	10.544858
8.075169	642.944133	10.549863
8.290560	644.013699	10.554867
8.278229	653.686922	10.559872
8.400614	654.471711	10.564877
8.284551	645.732165	10.569882
8.095448	644.521386	10.574887
8.393350	653.181639	10.579891
8.346331	649.108187	10.584896
8.221467	646.337063	10.589901
8.474309	641.004724	10.594906
8.156549	653.005290	10.599911
8.393658	649.410055	10.604915
8.844524	649.778187	10.609920
8.516052	652.222830	10.614925
8.617045	649.813063	10.619930
8.113481	657.246584	10.624935
8.694034	682.130740	10.629939
9.026550	680.095615	10.634944
9.113449	684.306384	10.639949
9.169298	681.537968	10.644954
9.068341	668.327036	10.649959
9.101234	658.593926	10.654963
9.047979	659.056655	10.659968
8.905880	659.068366	10.664973
9.596515	652.231211	10.669978
9.320386	664.999409	10.674983
9.407655	664.968229	10.679987
9.454321	657.694478	10.684992
9.375037	677.949991	10.689997
9.607433	661.853766	10.695002
9.271006	655.475302	10.700007
9.406923	655.404825	10.705011
9.317108	665.831561	10.710016
9.427874	669.488178	10.715021
9.498414	670.246545	10.720026
9.370214	694.628770	10.725031
9.984476	688.092355	10.730035
10.042390	690.790760	10.735040
9.640694	693.669701	10.740045
9.695617	686.164390	10.745050
10.152956	693.922475	10.750055
9.961483	690.157473	10.755059
10.024405	685.266982	10.760064
9.953591	702.512433	10.765069
10.244993	686.648037	10.770074
9.986331	686.455995	10.775079
10.152011	689.178212	10.780083
10.035564	693.296840	10.785088
10.063508	694.744805	10.790093
10.517130	699.540469	10.795098
10.097634	693.777616	10.800103
10.339959	697.019030	10.805107
10.431700	697.580056	10.810112
10.594949	692.935329	10.815117
10.828199	689.053702	10.820122
10.227661	705.883763	10.825127
10.490423	701.489660	10.830131
10.421263	697.809224	10.835136
10.334117	699.280276	10.840141
10.412653	692.834034	10.845146
10.297932	704.160456	10.850151
10.613709	699.251708	10.855155
10.727202	704.918463	10.860160
10.593813	718.744128	10.865165
11.256186	720.360560	10.870170
10.883594	731.934708	10.875175
10.915215	732.724516	10.880179
10.982863	719.447222	10.885184
11.311597	718.238999	10.890189
11.546730	725.013855	10.895194
11.151440	732.912680	10.900199
11.258003	729.434439	10.905203
11.503465	724.242015	10.910208
11.057463	714.432288	10.915213
11.216726	713.374093	10.920218
11.502016	716.596043	10.925223
11.255068	726.893347	10.930227
11.387409	729.789619	10.935232
11.297095	738.513418	10.940237
11.510572	742.491132	10.945242
11.507758	738.971988	10.950247
11.750455	725.692000	10.955251
11.839746	741.016509	10.960256
11.336167	739.859032	10.965261
11.959942	722.605937	10.970266
11.849826	734.321146	10.975271
11.964393	727.310914	10.980275
11.941025	724.236587	10.985280
11.801284	735.406179	10.990285
11.928618	734.837188	10.995290
11.863643	739.550002	11.000295
11.987159	728.804203	11.005299
12.048493	734.917671	11.010304
11.827203	735.806163	11.015309
11.963197	752.813690	11.020314
12.158111	768.955571	11.025319
12.422756	761.714809	11.030323
12.617768	767.887394	11.035328
12.583055	766.040135	11.040333
12.995208	756.323739	11.045338
12.559215	755.898210	11.050343
12.608572	747.006066	11.055347
12.775506	733.099504	11.060352
12.340518	731.152091	11.065357
12.628243	738.057334	11.070362
12.752280	762.131368	11.075367
12.941032	754.459599	11.080371
13.033455	761.356580	11.085376
13.079885	751.987093	11.090381
13.177953	738.052087	11.095386
12.855621	728.722507	11.100391
12.748777	731.794119	11.105395
13.089724	732.961936	11.110400
13.003048	733.718574	11.115405
13.079061	744.604608	11.120410
13.116858	761.821768	11.125415
13.145118	765.248723	11.130419
13.260410	763.281348	11.135424
12.745498	768.236240	11.140429
13.235801	762.900676	11.145434
13.104205	769.093814	11.150439
13.500954	766.756702	11.155443
13.601039	778.006345	11.160448
13.442945	774.004190	11.165453
13.703947	769.831116	11.170458
13.614912	770.476170	11.175463
13.721046	768.877677	11.180467
13.564767	778.088250	11.185472
13.246878	773.075544	11.190477
13.542453	765.634309	11.195482
13.338256	776.229174	11.200487
13.623844	785.146932	11.205491
13.850077	791.905893	11.210496
13.752297	789.838459	11.215501
14.237084	797.778301	11.220506
13.858790	789.738069	11.225511
14.061149	798.289071	11.230515
13.973623	799.102616	11.235520
13.963331	793.406920	11.240525
14.797126	789.497292	11.245530
14.254678	803.009817	11.250535
14.428515	794.608714	11.255539
14.895785	794.712466	11.260544
14.538739	792.539729	11.265549
14.760627	782.554046	11.270554
14.546943	789.100900	11.275559
14.194224	776.691676	11.280563
14.373129	781.485452	11.285568
14.373320	797.972231	11.290573
14.725408	794.546277	11.295578
14.664689	798.947778	11.300583
14.471299	796.849861	11.305587
14.675990	796.956069	11.310592
14.682205	787.124627	11.315597
14.955867	801.837911	11.320602
14.662181	804.354300	11.325607
14.723033	790.324255	11.330611
15.019525	790.094130	11.335616
15.026775	793.428250	11.340621
14.965941	798.004808	11.345626
14.580946	786.606800	11.350631
15.111813	814.370686	11.355635
15.566655	817.343271	11.360640
15.479260	816.729679	11.365645
15.191209	805.795579	11.370650
15.190770	817.095978	11.375655
15.529530	815.447762	11.380659
15.893469	823.540932	11.385664
15.410122	810.122779	11.390669
15.218688	797.692544	11.395674
15.410779	811.980463	11.400679
15.325400	815.679440	11.405683
15.660529	810.939454	11.410688
15.725957	823.131353	11.415693
16.347434	817.987733	11.420698
16.133138	819.319806	11.425703
15.728343	813.357445	11.430707
16.379594	809.763927	11.435712
15.730520	794.494104	11.440717
15.906172	787.029408	11.445722
15.587987	795.964623	11.450727
16.060693	808.711284	11.455731
16.402596	814.584499	11.460736
16.020947	810.389334	11.465741
16.419327	811.734075	11.470746
16.288506	810.608601	11.475751
16.301005	818.268972	11.480755
16.481540	810.775100	11.485760
16.218179	817.684699	11.490765
16.484839	822.136492	11.495770
16.453556	821.231681	11.500775
16.563043	819.468648	11.505779
16.382636	817.341849	11.510784
16.441772	818.191927	11.515789
16.437466	810.793767	11.520794
16.145456	826.729528	11.525799
16.583823	822.744190	11.530803
16.379145	830.377705	11.535808
16.130284	828.823209	11.540813
16.512975	831.837266	11.545818
16.607168	842.195358	11.550823
16.825221	840.481237	11.555827
16.953928	837.839941	11.560832
16.893577	846.595296	11.565837
17.297553	848.060572	11.570842
17.054558	854.806092	11.575847
17.158936	839.911208	11.580851
17.290871	847.114160	11.585856
16.887468	845.177462	11.590861
17.249115	835.874340	11.595866
17.353208	841.056954	11.600871
17.272452	842.662617	11.605875
17.364014	841.044363	11.610880
17.172429	847.256564	11.615885
17.597242	836.800093	11.620890
17.357151	844.057647	11.625895
17.398386	849.928369	11.630899
17.811872	851.723284	11.635904
17.950772	858.198166	11.640909
17.994428	833.386203	11.645914
18.041025	831.134889	11.650919
17.943805	841.720626	11.655923
18.152738	837.864915	11.660928
18.238874	835.873796	11.665933
18.346011	820.483336	11.670938
18.211760	836.830755	11.675943
18.192054	824.522915	11.680947
18.372261	829.810079	11.685952
17.969477	830.613983	11.690957
18.281591	825.144393	11.695962
18.175220	836.087970	11.700967
18.305221	833.943200	11.705971
18.192219	827.920102	11.710976
18.116533	837.805399	11.715981
18.357199	830.074850	11.720986
18.176633	835.553594	11.725991
18.246228	834.066576	11.730995
18.347308	816.800543	11.736000
18.340150	833.370535	11.741005
18.886860	831.014227	11.746010
18.361185	832.594656	11.751015
18.334185	825.198531	11.756019
18.429153	840.525394	11.761024
18.297584	863.861363	11.766029
18.872303	862.044624	11.771034
19.038941	873.155996	11.776039
18.977093	859.616956	11.781043
19.147229	862.973999	11.786048
18.945235	866.533894	11.791053
19.225959	869.333991	11.796058
19.182847	877.753882	11.801063
19.092126	873.580106	11.806067
19.024458	863.948050	11.811072
19.185922	865.709046	11.816077
19.340524	864.358276	11.821082
18.978929	867.831664	11.826087
19.280782	864.405821	11.831091
19.398855	863.144454	11.836096
19.165318	862.923170	11.841101
19.269777	865.096952	11.846106
19.435018	869.730514	11.851111
19.321536	860.749155	11.856115
19.699780	865.602630	11.861120
19.353589	870.294107	11.866125
19.605842	853.607884	11.871130
19.674723	865.482305	11.876135
20.016356	884.059352	11.881139
19.901090	875.322694	11.886144
19.634917	875.429885	11.891149
19.804208	882.524396	11.896154
19.944432	885.767945	11.901159
20.125710	889.435450	11.906163
20.656942	887.210911	11.911168
20.278125	883.617661	11.916173
20.506263	865.404069	11.921178
20.447939	861.261398	11.926183
20.612854	857.795897	11.931187
20.675944	857.569881	11.936192
20.175881	865.769336	11.941197
20.295784	855.596444	11.946202
20.155608	861.272180	11.951207
20.305961	866.360695	11.956211
20.493981	856.131208	11.961216
20.300531	856.565841	11.966221
20.636243	852.188443	11.971226
20.233202	857.056137	11.976231
20.173545	863.529574	11.981235
20.543745	875.661871	11.986240
20.541576	892.040326	11.991245
21.154208	888.053986	11.996250
20.832177	878.236987	12.001255
20.968782	883.281969	12.006259
21.229453	880.860889	12.011264
20.871009	891.832096	12.016269
21.440164	883.727433	12.021274
21.046481	883.008148	12.026279
20.765069	871.817475	12.031283
20.921437	884.986813	12.036288
21.083290	884.932700	12.041293
21.314185	880.963090	12.046298
21.167500	869.484430	12.051303
21.221661	860.684489	12.056307
21.260123	853.568064	12.061312
20.996921	858.993765	12.066317
21.240779	857.486836	12.071322
21.277880	853.660104	12.076327
20.886316	866.923122	12.081331
21.226133	850.188245	12.086336
20.874186	851.315197	12.091341
21.027075	850.108202	12.096346
20.865220	860.385721	12.101351
21.026298	859.049687	12.106355
21.427130	851.790315	12.111360
21.027526	863.725261	12.116365
20.983668	857.312658	12.121370
21.139139	852.192889	12.126375
21.382111	861.852341	12.131379
21.333246	858.111857	12.136384
21.027621	859.048498	12.141389
21.132529	839.670318	12.146394
20.999385	834.689624	12.151399
20.767788	829.068632	12.156403
21.095674	834.094129	12.161408
21.000137	835.987572	12.166413
21.305583	820.983369	12.171418
21.079970	828.397875	12.176423
20.617566	832.338334	12.181427
21.077628	827.431764	12.186432
20.828324	833.903896	12.191437
20.968381	833.719220	12.196442
20.949512	832.421350	12.201447
21.076578	849.465109	12.206451
21.369947	838.023521	12.211456
20.864421	836.076303	12.216461
21.055838	817.015511	12.221466
21.066121	823.122967	12.226471
20.886113	820.382680	12.231475
21.020069	819.618669	12.236480
20.972489	824.983160	12.241485
21.391145	822.644124	12.246490
21.026808	825.353131	12.251495
20.942978	830.384367	12.256499
21.277576	822.785494	12.261504
20.806563	832.399530	12.266509
20.910561	820.540311	12.271514
20.947552	829.160284	12.276519
20.696570	825.895160	12.281523
20.908362	825.080889	12.286528
20.696959	839.209265	12.291533
21.072768	830.567774	12.296538
20.621077	835.466874	12.301543
20.879447	845.127013	12.306547
21.516740	856.578040	12.311552
21.065290	854.970697	12.316557
20.772497	838.921768	12.321562
21.118920	830.597196	12.326567
21.167776	826.152018	12.331571
21.118060	823.701604	12.336576
20.825162	831.142613	12.341581
21.100898	831.682184	12.346586
21.009504	835.894627	12.351591
21.105335	840.091402	12.356595
21.335528	833.502640	12.361600
20.790567	833.591218	12.366605
21.241838	834.637372	12.371610
21.161624	841.557195	12.376615
20.855642	843.036355	12.381619
21.057751	844.614250	12.386624
21.040796	841.644530	12.391629
21.279205	831.202023	12.396634
21.175398	840.713346	12.401639
21.072134	835.895040	12.406643
21.168591	828.092876	12.411648
21.252386	828.424944	12.416653
21.221371	836.934344	12.421658
21.486587	837.450363	12.426663
21.345940	832.786252	12.431667
21.203053	809.412277	12.436672
20.926996	823.263949	12.441677
21.475146	812.600171	12.446682
21.064152	808.638339	12.451687
20.904011	818.775210	12.456691
21.079919	798.654067	12.461696
20.952575	809.444854	12.466701
20.794948	796.126149	12.471706
20.995071	797.029432	12.476711
20.686689	809.511170	12.481715
20.992535	804.952473	12.486720
20.856424	811.835465	12.491725
21.125957	811.948678	12.496730
20.858450	807.934001	12.501735
20.813016	812.504953	12.506739
20.890475	802.788292	12.511744
20.917115	804.987091	12.516749
20.923870	812.757184	12.521754
21.036438	817.383361	12.526759
20.681639	824.059968	12.531763
21.086415	831.698783	12.536768
20.887409	844.235645	12.541773
21.525054	836.735086	12.546778
21.297887	835.451514	12.551783
21.151772	823.108643	12.556787
21.171950	817.907963	12.561792
21.238408	817.492180	12.566797
21.165874	804.178819	12.571802
20.816855	824.203173	12.576807
21.125318	813.222813	12.581811
20.970796	813.616543	12.586816
20.920779	817.762458	12.591821
20.776453	810.077552	12.596826
21.053474	818.493659	12.601831
20.763616	827.468530	12.606835
21.022799	823.617424	12.611840
20.962878	824.349299	12.616845
20.829254	820.095649	12.621850
21.160397	823.871698	12.626855
20.898479	823.667556	12.631859
21.085122	826.575687	12.636864
20.905138	823.799126	12.641869
20.873148	819.051459	12.646874
20.982559	823.548834	12.651879
20.688671	827.579107	12.656883
20.895918	823.827747	12.661888
21.051859	837.643649	12.666893
21.198731	817.309496	12.671898
20.574612	829.273914	12.676903
20.668646	838.651181	12.681907
21.220784	851.415174	12.686912
21.112814	863.549608	12.691917
21.159036	849.588070	12.696922
21.041382	840.785582	12.701927
20.796931	839.903729	12.706931
21.024602	835.907838	12.711936
20.753862	835.563180	12.716941
20.974803	836.851070	12.721946
21.120076	853.322658	12.726951
21.055658	860.869165	12.731955
20.998227	839.408521	12.736960
20.669716	836.955262	12.741965
20.641286	845.232447	12.746970
20.974546	853.168103	12.751975
21.255824	863.729759	12.756979
21.349072	853.422350	12.761984
20.827898	865.360918	12.766989
20.849057	863.585158	12.771994
20.927961	865.187437	12.776999
21.159505	863.917434	12.782003
21.523765	859.267403	12.787008
20.960592	841.514355	12.792013
21.211592	837.782821	12.797018
20.985138	839.104220	12.802023
20.867041	839.567834	12.807027
20.620897	833.886083	12.812032
20.799138	843.383962	12.817037
21.467799	849.058424	12.822042
20.971752	838.889166	12.827047
20.747458	835.711246	12.832051
20.927867	837.011908	12.837056
21.108563	862.439539	12.842061
21.048879	846.848580	12.847066
20.941467	840.947584	12.852071
21.015560	837.558073	12.857075
20.903116	829.458071	12.862080
21.106602	837.545301	12.867085
21.183540	847.038839	12.872090
21.218268	833.299920	12.877095
20.503532	842.575948	12.882099
21.016844	833.120907	12.887104
20.990114	841.277972	12.892109
20.950229	847.264132	12.897114
20.942880	855.526921	12.902119
20.772068	857.273103	12.907123
21.219115	859.806977	12.912128
20.995275	868.219418	12.917133
20.959962	854.999421	12.922138
21.162777	861.647035	12.927143
20.935273	863.332875	12.932147
21.006567	849.449338	12.937152
20.804116	859.837409	12.942157
21.234308	864.578521	12.947162
21.133602	853.428427	12.952167
20.814054	850.901197	12.957171
20.955448	845.006249	12.962176
21.214905	849.336201	12.967181
21.022645	838.143950	12.972186
21.211002	840.911465	12.977191
21.004951	848.158861	12.982195
21.108471	838.250365	12.987200
21.060048	838.753329	12.992205
21.143189	848.670072	12.997210
21.201556	848.233501	13.002215
21.340701	848.203510	13.007219
21.179005	843.504906	13.012224
20.840396	850.210481	13.017229
20.883246	849.953001	13.022234
21.065088	849.083582	13.027239
20.798060	856.622977	13.032243
21.311812	839.134985	13.037248
21.117825	855.118220	13.042253
20.684514	849.362237	13.047258
21.253846	849.582176	13.052263
20.956326	850.517523	13.057267
20.942475	841.618056	13.062272
21.225571	855.565081	13.067277
21.381482	843.639217	13.072282
21.378785	847.310822	13.077287
21.033017	851.355684	13.082291
21.273299	842.986533	13.087296
20.919799	832.960122	13.092301
20.568635	831.674249	13.097306
20.960783	828.973593	13.102311
21.158939	847.593976	13.107315
20.923872	848.457863	13.112320
20.892958	856.815874	13.117325
21.168690	857.360178	13.122330
21.443402	849.628919	13.127335
21.142348	843.638959	13.132339
21.081143	819.301053	13.137344
21.024300	826.422141	13.142349
21.110217	819.853242	13.147354
21.252786	817.091469	13.152359
21.203508	816.433952	13.157363
21.488604	818.755533	13.162368
21.016916	815.885150	13.167373
20.775857	820.916229	13.172378
20.965503	816.819177	13.177383
21.046843	825.780575	13.182387
20.956829	818.079118	13.187392
21.022465	823.819784	13.192397
21.038051	824.348807	13.197402
21.345601	818.435254	13.202407
21.113421	814.925865	13.207411
21.363196	817.961118	13.212416
20.969015	817.997264	13.217421
21.406360	813.129014	13.222426
21.227277	813.898816	13.227431
21.031435	803.221242	13.232435
21.134564	801.273147	13.237440
21.133936	796.897370	13.242445
21.109645	801.359293	13.247450
20.759963	783.092883	13.252455
20.464725	800.221283	13.257459
20.832597	806.058815	13.262464
20.761388	807.931029	13.267469
20.878434	816.823650	13.272474
21.043909	817.420229	13.277479
20.786400	830.185602	13.282483
21.110151	807.093592	13.287488
20.872883	816.203568	13.292493
20.983578	813.844265	13.297498
21.381580	820.695692	13.302503
20.910505	823.036952	13.307507
21.241114	814.112525	13.312512
21.188811	820.494885	13.317517
20.695764	805.782049	13.322522
21.138601	818.377368	13.327527
21.136805	815.771082	13.332531
21.049014	812.068357	13.337536
20.827333	809.842488	13.342541
20.968535	814.061981	13.347546
20.986482	812.242587	13.352551
20.811939	825.780033	13.357555
21.074646	823.957869	13.362560
20.726771	826.284211	13.367565
21.020735	829.903767	13.372570
21.170005	834.178749	13.377575
20.782076	837.023982	13.382579
20.865984	829.815166	13.387584
21.030762	835.152100	13.392589
20.637432	835.129764	13.397594
20.713630	822.410821	13.402599
20.724680	838.408645	13.407603
20.973356	838.195607	13.412608
20.654453	834.693736	13.417613
20.524590	833.337876	13.422618
20.948844	828.654632	13.427623
20.971723	827.957221	13.432627
20.621390	831.551805	13.437632
20.874257	833.585220	13.442637
21.022665	853.902435	13.447642
21.363005	842.514852	13.452647
21.128985	846.704314	13.457651
21.369338	843.140054	13.462656
21.022990	844.379651	13.467661
20.993666	826.997211	13.472666
21.357038	816.323477	13.477671
21.037303	827.588078	13.482675
21.074520	829.725271	13.487680
20.733270	836.749801	13.492685
20.974245	829.785589	13.497690
21.110089	832.301284	13.502695
20.928587	836.736253	13.507699
21.253544	827.779603	13.512704
20.825083	841.688715	13.517709
20.872836	837.686827	13.522714
21.075916	825.513762	13.527719
21.346995	835.566099	13.532723
21.132405	839.787153	13.537728
21.186216	837.657688	13.542733
21.279874	830.412624	13.547738
21.228880	839.723138	13.552743
21.205854	848.407887	13.557747
21.133065	841.621442	13.562752
20.813374	834.399724	13.567757
20.899068	830.625171	13.572762
21.004788	832.119092	13.577767
20.933412	841.612627	13.582771
21.011941	832.729970	13.587776
20.834689	841.778351	13.592781
20.921551	836.234297	13.597786
20.802309	837.205865	13.602791
20.521212	839.046903	13.607795
21.225219	832.915575	13.612800
21.058832	830.412806	13.617805
21.121054	842.554772	13.622810
20.983577	839.227388	13.627815
20.854221	842.015613	13.632819
21.083504	838.032080	13.637824
20.968191	834.278546	13.642829
20.968589	838.172002	13.647834
21.385105	829.251211	13.652839
20.906706	846.372608	13.657843
20.867877	836.023200	13.662848
20.874693	846.155538	13.667853
20.889394	843.114538	13.672858
20.927234	843.078626	13.677863
20.681198	844.600265	13.682867
20.902737	838.842345	13.687872
20.635374	839.522151	13.692877
21.006553	841.577698	13.697882
20.912085	843.079893	13.702887
20.923742	850.789301	13.707891
21.238935	844.347824	13.712896
21.104391	848.855730	13.717901
21.122058	848.687421	13.722906
21.390556	845.459288	13.727911
21.431978	849.820859	13.732915
21.566061	837.813328	13.737920
21.081683	841.889755	13.742925
20.964937	829.255195	13.747930
21.147507	817.459139	13.752935
20.977614	819.041169	13.757939
20.947824	822.010627	13.762944
20.998637	819.512642	13.767949
20.888068	806.113884	13.772954
20.861330	816.740400	13.777959
20.927038	821.143821	13.782963
21.146292	834.812430	13.787968
20.733774	836.844737	13.792973
20.908197	844.759990	13.797978
21.518668	831.768174	13.802983
21.045688	834.540240	13.807987
20.918156	828.424842	13.812992
21.012083	812.175496	13.817997
20.790056	827.666442	13.823002
21.226987	818.512171	13.828007
20.979933	826.486751	13.833011
21.116490	823.008434	13.838016
20.678576	825.454790	13.843021
20.663655	816.948163	13.848026
21.278209	823.555323	13.853031
21.175456	837.609600	13.858035
21.070515	824.280889	13.863040
21.099728	828.721671	13.868045
20.962468	825.066256	13.873050
21.087051	821.310733	13.878055
20.365347	833.779566	13.883059
21.027450	829.739620	13.888064
21.282657	845.419395	13.893069
20.935832	846.154452	13.898074
21.381476	833.622577	13.903079
20.687852	831.785783	13.908083
20.898366	826.769206	13.913088
21.303634	823.837803	13.918093
21.266911	834.857002	13.923098
21.115238	837.074784	13.928103
20.924986	837.576714	13.933107
21.185843	833.643339	13.938112
20.888416	838.123604	13.943117
20.694340	834.595517	13.948122
20.934813	829.621468	13.953127
20.939064	828.904951	13.958131
20.863648	833.466499	13.963136
20.824984	832.690595	13.968141
20.930225	827.542575	13.973146
20.918122	824.589431	13.978151
21.012177	842.529410	13.983155
21.212949	843.678594	13.988160
20.987202	841.473868	13.993165
20.857528	842.287830	13.998170
21.191248	831.104736	14.003175
21.096087	838.569404	14.008179
20.990455	828.743156	14.013184
21.070519	833.499100	14.018189
21.381151	831.410616	14.023207
21.497900	817.011025	14.028224
21.126862	836.177922	14.033242
21.232467	831.313473	14.038259
21.281122	836.798382	14.043277
21.195380	838.916689	14.048295
21.288977	828.975247	14.053312
20.862511	834.137986	14.058330
20.913676	830.919614	14.063347
20.826575	830.199045	14.068365
20.870353	828.373871	14.073383
20.911760	836.266479	14.078400
20.883607	839.317772	14.083418
21.084516	834.584402	14.088435
21.031817	835.631010	14.093453
20.850389	849.223195	14.098471
21.237053	861.900584	14.103488
21.528923	858.980418	14.108506
21.437369	860.105578	14.113523
21.530217	859.873795	14.118541
21.534336	861.795316	14.123559
21.563991	858.099059	14.128576
21.074555	841.084433	14.133594
21.442875	848.487640	14.138611
21.272276	853.019738	14.143629
21.119652	860.938586	14.148647
21.277524	852.820886	14.153664
21.442953	868.775328	14.158682
21.233824	863.095965	14.163699
21.339206	856.119129	14.168717
21.379186	868.623745	14.173735
21.385801	849.617338	14.178752
21.322094	855.095007	14.183770
21.292212	859.540175	14.188787
21.641318	854.411957	14.193805
21.476503	861.203403	14.198823
21.579830	853.666940	14.203840
21.521550	874.194903	14.208858
21.763754	874.260172	14.213875
22.009185	887.809481	14.218893
21.448464	868.564794	14.223911
21.413567	879.384194	14.228928
21.815877	889.182261	14.233946
21.983512	894.445310	14.238963
22.009044	881.071585	14.243981
21.722068	874.531669	14.248999
22.005315	871.203920	14.254016
21.720426	873.748794	14.259034
21.614790	872.939951	14.264051
21.854789	888.594678	14.269069
21.831288	889.496644	14.274087
22.151577	880.262998	14.279104
21.840279	895.875108	14.284122
22.060868	890.721760	14.289139
21.776183	886.833401	14.294157
21.647786	893.564001	14.299175
21.780754	882.762152	14.304192
21.636462	898.877700	14.309210
21.605140	890.807456	14.314227
21.929092	894.395590	14.319245
21.517906	907.024102	14.324263
21.955124	900.676964	14.329280
22.096414	906.663040	14.334298
22.234031	909.639149	14.339315
22.173764	908.679932	14.344333
22.076642	931.715102	14.349351
22.577176	913.951085	14.354368
22.301416	901.438590	14.359386
22.163561	896.776531	14.364403
22.319022	888.640321	14.369421
22.248047	889.205391	14.374439
22.582922	882.371253	14.379456
22.320743	890.925743	14.384474
22.295889	875.504266	14.389491
22.481377	883.115962	14.394509
22.399180	893.335773	14.399527
22.396550	894.460910	14.404544
21.946703	888.499055	14.409562
22.175245	897.017754	14.414579
22.305817	894.746179	14.419597
22.401741	914.349899	14.424615
22.399394	915.047160	14.429632
22.372400	912.667015	14.434650
22.397378	924.629844	14.439667
22.908791	917.330263	14.444685
22.586704	913.767163	14.449703
22.747708	911.931148	14.454720
22.898061	915.210372	14.459738
22.583864	911.940148	14.464755
22.681317	910.855111	14.469773
22.568913	923.973921	14.474791
22.728590	911.900021	14.479808
22.868499	916.303971	14.484826
22.692570	920.335181	14.489843
22.850398	904.939588	14.494861
22.491773	910.192201	14.499879
22.975733	910.193746	14.504896
22.774368	917.242713	14.509914
22.872341	911.696810	14.514931
23.104668	903.458676	14.519949
22.363420	894.391179	14.524967
23.056832	896.726550	14.529984
23.152371	898.542268	14.535002
22.744945	895.669135	14.540019
23.171876	893.889802	14.545037
22.787087	887.340314	14.550055
22.940998	888.902919	14.555072
23.056252	898.817557	14.560090
22.829654	906.128500	14.565107
23.006296	909.996518	14.570125
22.680514	924.278711	14.575143
22.922956	917.861964	14.580160
22.972421	929.470133	14.585178
22.516896	924.759636	14.590195
22.584326	921.395514	14.595213
22.898589	916.395519	14.600231
23.062139	920.501565	14.605248
23.082313	928.720056	14.610266
23.218603	915.336500	14.615283
23.226789	918.446503	14.620301
22.905944	931.372065	14.625319
23.381121	931.209855	14.630336
23.506862	946.058660	14.635354
23.388022	939.531222	14.640371
23.490251	926.311952	14.645389
23.288013	927.333656	14.650407
23.078935	909.322621	14.655424
23.275947	934.995848	14.660442
23.301178	941.676802	14.665459
23.550552	949.256324	14.670477
23.695348	954.831329	14.675495
23.768580	937.777183	14.680512
23.509707	922.946644	14.685530
23.345059	927.032682	14.690547
23.552340	917.548067	14.695565
23.565298	918.327825	14.700583
23.267648	921.829501	14.705600
23.501986	921.570432	14.710618
23.645375	941.525244	14.715635
23.495513	945.255022	14.720653
23.616453	945.331767	14.725671
23.825098	949.704316	14.730688
23.606302	957.441875	14.735706
23.290985	954.640550	14.740723
23.990237	950.584236	14.745741
23.782163	955.548603	14.750759
24.086529	944.725664	14.755776
23.910444	955.114638	14.760794
23.626620	942.567217	14.765811
23.735817	929.813989	14.770829
24.014924	951.139199	14.775847
24.031842	939.792711	14.780864
23.916708	941.122972	14.785882
23.375864	951.768306	14.790899
23.796098	947.890191	14.795917
23.804289	942.418367	14.800935
23.978183	954.126252	14.805952
23.990809	944.384821	14.810970
24.041625	958.844496	14.815987
24.336340	945.496989	14.821005
24.321807	957.308855	14.826023
23.971540	953.566208	14.831040
24.080641	947.082631	14.836058
24.108457	949.846614	14.841075
24.106307	941.671022	14.846093
23.972973	944.853935	14.851111
23.682884	944.247526	14.856128
24.019853	945.269744	14.861146
24.310449	941.838567	14.866163
24.084419	937.261339	14.871181
24.191483	939.989088	14.876199
24.192400	938.189612	14.881216
24.490345	943.221125	14.886234
24.187278	945.130307	14.891251
24.375985	950.317661	14.896269
24.214632	946.958563	14.901287
24.444840	943.159517	14.906304
24.572928	938.530530	14.911322
24.247240	939.192851	14.916339
24.317798	933.539635	14.921357
24.234970	942.263738	14.926375
24.275963	934.861436	14.931392
24.482315	943.935794	14.936410
24.216898	937.793505	14.941427
24.336717	942.018208	14.946445
24.639139	958.641410	14.951463
24.650978	961.115381	14.956480
24.672417	962.518237	14.961498
24.840286	969.882695	14.966515
24.963795	951.368710	14.971533
24.654839	940.151268	14.976551
24.490773	954.376240	14.981568
24.357045	936.107780	14.986586
24.566553	951.424543	14.991603
24.585817	974.496272	14.996621
24.849915	963.445376	15.001639
25.084301	959.441179	15.006656
25.194569	969.564286	15.011674
24.747124	966.074645	15.016691
25.191800	955.790851	15.021709
24.872387	956.741589	15.026727
24.697122	960.988193	15.031744
25.147877	957.416646	15.036762
24.971890	956.631601	15.041779
25.074416	958.888202	15.046797
24.888601	946.046739	15.051815
24.940227	951.930739	15.056832
25.125589	964.638752	15.061850
24.798622	972.134038	15.066867
25.225102	960.025412	15.071885
25.067488	976.722005	15.076903
25.169919	968.097165	15.081920
25.553619	969.363599	15.086938
25.078163	965.441154	15.091955
25.204547	953.595884	15.096973
25.356270	968.276986	15.101991
25.301396	956.693414	15.107008
25.554047	943.390367	15.112026
25.380907	937.066631	15.117043
25.187790	927.938431	15.122061
25.324783	935.540588	15.127079
24.843704	942.590137	15.132096
25.180919	951.816650	15.137114
24.986563	956.816580	15.142131
25.190138	961.526546	15.147149
25.278078	961.383627	15.152167
25.488446	966.825492	15.157184
25.502379	960.003181	15.162202
25.158206	970.296286	15.167219
25.558624	954.805325	15.172237
25.244950	970.331384	15.177255
25.497060	972.545254	15.182272
25.692601	962.482076	15.187290
25.419048	972.337659	15.192307
25.493607	970.422621	15.197325
25.741262	978.162870	15.202343
25.715226	965.756773	15.207360
25.264573	963.448906	15.212378
25.208633	979.204411	15.217395
25.763472	988.191760	15.222413
26.137771	993.904772	15.227431
25.712812	1009.008201	15.232448
26.032120	993.926512	15.237466
25.713763	984.698708	15.242483
25.926145	988.315672	15.247501
26.228234	982.175655	15.252519
25.897233	967.606668	15.257536
25.920167	964.295248	15.262554
25.833012	964.875484	15.267571
25.924086	962.435604	15.272589
26.103405	963.478249	15.277607
25.673857	973.287930	15.282624
26.470846	971.823925	15.287642
26.242176	968.791715	15.292659
25.903346	963.636332	15.297677
25.767234	974.701592	15.302695
25.767602	988.431643	15.307712
25.849736	989.738310	15.312730
25.828506	999.446710	15.317747
25.802858	999.925909	15.322765
26.280175	985.514260	15.327783
26.125942	988.511765	15.332800
26.304773	995.193413	15.337818
26.290234	998.439183	15.342835
26.149485	1000.605610	15.347853
26.335715	999.750210	15.352871
26.368059	999.329886	15.357888
26.610411	983.261675	15.362906
26.341956	995.187997	15.367923
26.167965	992.601636	15.372941
26.092374	990.359781	15.377959
26.248919	1007.534807	15.382976
26.786236	1014.904857	15.387994
26.566097	1012.420227	15.393011
26.545195	1004.483529	15.398029
26.661072	988.960839	15.403047
26.447987	997.836303	15.408064
26.655084	1000.887861	15.413082
26.761548	989.829054	15.418099
26.363050	991.786492	15.423117
26.388620	993.054994	15.428135
26.901171	1003.653477	15.433152
26.864031	1009.295271	15.438170
26.915690	1011.456179	15.443187
26.822888	1015.692794	15.448205
26.732404	1000.492422	15.453223
26.625050	1010.854745	15.458240
26.758985	1012.068215	15.463258
26.749527	1016.189298	15.468275
27.273314	1015.890356	15.473293
27.164778	998.644917	15.478311
26.785482	996.003215	15.483328
27.085793	988.885122	15.488346
26.922309	986.300232	15.493363
27.013272	982.804936	15.498381
27.069145	983.480331	15.503399
26.936049	989.974215	15.508416
27.434290	989.185450	15.513434
27.273045	985.656450	15.518451
27.004001	982.552030	15.523469
27.234475	973.456911	15.528487
27.034941	982.622768	15.533504
26.858312	987.706391	15.538522
27.073186	1005.922824	15.543539
27.127755	1013.473678	15.548557
27.289403	1002.096195	15.553575
27.458800	1018.174429	15.558592
27.449441	1013.570485	15.563610
27.470046	1012.563760	15.568627
27.444654	1015.103448	15.573645
27.455136	1008.610406	15.578663
27.310407	1018.030222	15.583680
27.563251	1017.914482	15.588698
27.630692	1018.212105	15.593715
27.289413	1008.187323	15.598733
27.197272	996.722913	15.603751
27.215168	1015.743079	15.608768
27.350515	1019.718380	15.613786
27.244042	1016.495222	15.618803
26.941935	1010.814900	15.623821
27.533769	1015.205002	15.628839
27.364011	1020.900982	15.633856
27.505125	1000.215063	15.638874
27.757960	1024.611772	15.643891
27.759871	1044.578280	15.648909
28.237741	1030.562875	15.653927
27.451084	1029.008538	15.658944
27.649637	1016.835548	15.663962
27.580829	1039.836489	15.668979
27.640534	1045.730249	15.673997
28.013328	1040.258436	15.679015
28.206325	1042.629601	15.684032
28.196561	1038.639155	15.689050
28.127798	1023.600452	15.694067
27.731528	1014.825474	15.699085
28.243989	1023.118080	15.704103
27.811743	1014.955988	15.709120
27.798637	1016.029326	15.714138
27.874765	1033.788180	15.719155
27.705515	1052.187049	15.724173
28.261789	1046.767764	15.729191
27.964785	1048.049966	15.734208
28.100889	1044.755083	15.739226
28.060704	1023.162154	15.744243
27.730630	1043.930320	15.749261
28.290023	1035.009206	15.754279
28.144499	1039.507477	15.759296
28.409794	1040.127454	15.764314
28.133647	1039.205804	15.769331
27.744492	1042.923438	15.774349
28.098167	1025.997482	15.779367
28.283679	1045.834043	15.784384
28.354768	1061.427814	15.789402
28.793707	1059.855747	15.794419
28.797834	1054.417560	15.799437
28.808873	1038.505722	15.804455
28.563332	1042.656599	15.809472
28.711021	1029.157869	15.814490
29.136559	1024.619833	15.819507
28.561606	1023.217337	15.824525
28.731444	1017.807787	15.829543
28.879578	1022.009124	15.834560
28.625315	1023.449664	15.839578
28.709427	1031.562069	15.844595
28.746573	1023.866197	15.849613
28.779317	1021.614923	15.854631
28.792500	1024.502370	15.859648
28.703463	1024.257123	15.864666
28.910869	1021.946535	15.869683
28.785016	1034.611442	15.874701
29.078823	1027.555712	15.879719
29.055460	1023.347229	15.884736
29.002353	1021.333003	15.889754
29.136722	1030.466085	15.894771
28.957402	1024.925040	15.899789
29.209911	1016.746541	15.904807
29.342114	1018.138028	15.909824
29.260583	1013.869617	15.914842
29.520889	1013.477426	15.919859
29.137987	1002.814386	15.924877
29.222929	986.395348	15.929895
29.253871	992.999915	15.934912
29.130594	988.286741	15.939930
29.033755	993.738288	15.944947
28.848333	1002.341946	15.949965
29.374598	1011.774287	15.954983
29.376373	1022.147526	15.960000
29.393913	1020.884901	15.965018
29.626331	1028.449868	15.970035
29.334568	1014.437682	15.975053
28.894241	998.917178	15.980071
29.063634	1016.228583	15.985088
29.283313	1022.271414	15.990106
29.351617	1023.712416	15.995123
29.204263	1023.632190	16.000141
29.494757	1032.620831	16.005159
29.396560	1036.455643	16.010176
29.188028	1033.525593	16.015194
29.355556	1025.491195	16.020211
29.216389	1035.054845	16.025229
29.113019	1025.904404	16.030247
29.412942	1036.530532	16.035264
29.610068	1058.370740	16.040282
29.962473	1051.952126	16.045299
29.569252	1044.672497	16.050317
29.706901	1052.513697	16.055335
29.723411	1055.260628	16.060352
29.884372	1053.503249	16.065370
30.128469	1038.474404	16.070387
29.987054	1056.341909	16.075405
30.199951	1046.939680	16.080423
30.172166	1054.330668	16.085440
29.902376	1065.819987	16.090458
30.042412	1054.120313	16.095475
29.822739	1041.120581	16.100493
30.177979	1052.455153	16.105511
29.774797	1057.818737	16.110528
30.014954	1051.208826	16.115546
30.184010	1038.411351	16.120563
30.108152	1054.943995	16.125581
29.973262	1043.327500	16.130599
30.399737	1044.723964	16.135616
30.367112	1037.399413	16.140634
30.585079	1047.264740	16.145651
30.314741	1048.558418	16.150669
30.391161	1052.403136	16.155687
30.510628	1048.594985	16.160704
30.411951	1051.929686	16.165722
30.470133	1045.433738	16.170739
30.238683	1055.178849	16.175757
30.427511	1045.497333	16.180775
30.130343	1048.245529	16.185792
30.213017	1060.987307	16.190810
30.117095	1055.248917	16.195827
30.437287	1060.890367	16.200845
30.338832	1052.865342	16.205863
30.348448	1048.909553	16.210880
29.939997	1054.906294	16.215898
30.632408	1064.942916	16.220915
30.404397	1086.624467	16.225933
30.503081	1080.008793	16.230951
30.282130	1079.968616	16.235968
30.074662	1081.549555	16.240986
30.561630	1078.261623	16.246003
30.528121	1082.075120	16.251021
30.586022	1091.929828	16.256039
31.251832	1106.752438	16.261056
31.047410	1098.816644	16.266074
31.069556	1074.651388	16.271091
30.741258	1075.567372	16.276109
30.746927	1083.717483	16.281127
31.124597	1091.693446	16.286144
31.139794	1097.655670	16.291162
31.463458	1095.592355	16.296179
31.201752	1089.929152	16.301197
31.307556	1078.651745	16.306215
31.292544	1071.588620	16.311232
31.153661	1084.392493	16.316250
31.465210	1078.636296	16.321267
31.326816	1073.551147	16.326285
31.314361	1061.389752	16.331303
31.665651	1061.565033	16.336320
31.234913	1063.351454	16.341338
31.275746	1067.219153	16.346355
31.291894	1060.715745	16.351373
31.191000	1077.208365	16.356391
31.583192	1070.533302	16.361408
31.055703	1069.470848	16.366426
31.295325	1063.675794	16.371443
31.033902	1075.958116	16.376461
31.482475	1084.300271	16.381479
31.725850	1089.969712	16.386496
31.718275	1097.362218	16.391514
31.936875	1086.672394	16.396531
31.779993	1098.573142	16.401549
31.622044	1086.368867	16.406567
31.729622	1085.876770	16.411584
31.621215	1096.604243	16.416602
32.037063	1088.387070	16.421619
31.840353	1089.587216	16.426637
31.632343	1089.537111	16.431655
31.615036	1098.198952	16.436672
31.836552	1105.139671	16.441690
31.743310	1089.214522	16.446707
31.692274	1098.759439	16.451725
31.912031	1108.364989	16.456743
32.221007	1090.585692	16.461760
31.879168	1089.965508	16.466778
32.089461	1097.987044	16.471795
32.347548	1099.740686	16.476813
32.190505	1104.536525	16.481831
32.174738	1085.141717	16.486848
32.186980	1096.806290	16.491866
32.131806	1095.473464	16.496883
32.179364	1105.075016	16.501901
32.136804	1098.104355	16.506919
32.393903	1089.105585	16.511936
31.886505	1099.243926	16.516954
32.360059	1091.789858	16.521971
32.003968	1089.490482	16.526989
32.025319	1098.377379	16.532007
32.152062	1094.572774	16.537024
32.187529	1101.670570	16.542042
32.639441	1111.084949	16.547059
32.865127	1120.285317	16.552077
32.624468	1099.877207	16.557095
32.826779	1093.046811	16.562112
32.580624	1093.216708	16.567130
32.826884	1085.942030	16.572147
32.873220	1083.921373	16.577165
32.736841	1086.805945	16.582183
32.880637	1090.237257	16.587200
32.981834	1083.492200	16.592218
32.930790	1082.025016	16.597235
32.601553	1090.481786	16.602253
32.840856	1090.072495	16.607271
32.719772	1082.032188	16.612288
32.664787	1091.436166	16.617306
32.571700	1081.398489	16.622323
32.672411	1087.638063	16.627341
32.608654	1111.558479	16.632359
33.377764	1108.301044	16.637376
32.898981	1121.626321	16.642394
33.104027	1119.226437	16.647411
33.395960	1113.798952	16.652429
33.081590	1124.227404	16.657447
33.346750	1121.391667	16.662464
33.188448	1121.969100	16.667482
33.182955	1116.406588	16.672499
32.938424	1116.563643	16.677517
33.019504	1131.724913	16.682535
33.044808	1118.698624	16.687552
33.289424	1132.290763	16.692570
33.051607	1129.624898	16.697587
33.003631	1119.834816	16.702605
33.385797	1118.559646	16.707623
33.365659	1118.037583	16.712640
33.143605	1131.911775	16.717658
33.522778	1136.395604	16.722675
33.530411	1141.569438	16.727693
33.715753	1143.301655	16.732711
33.811901	1145.431895	16.737728
33.792856	1139.578969	16.742746
33.939795	1133.350382	16.747763
33.689697	1124.791110	16.752781
33.566942	1125.405343	16.757799
33.942613	1116.824922	16.762816
33.789633	1110.560811	16.767834
33.882828	1115.941201	16.772851
33.760945	1120.133723	16.777869
33.745312	1122.585363	16.782887
33.873959	1129.372600	16.787904
34.074755	1155.462445	16.792922
33.899050	1156.682841	16.797939
34.006314	1139.520788	16.802957
33.884363	1151.165911	16.807975
34.172778	1136.372130	16.812992
34.078429	1150.295183	16.818010
34.331560	1153.438527	16.823027
34.115461	1137.463709	16.828045
34.037604	1147.222137	16.833063
34.082632	1158.209886	16.838080
33.757597	1149.270889	16.843098
34.151436	1138.886542	16.848115
34.362715	1155.219359	16.853133
34.073886	1151.444839	16.858151
34.104611	1152.254807	16.863168
34.328912	1148.857749	16.868186
33.959899	1147.752712	16.873203
34.128205	1156.922931	16.878221
34.339825	1160.489726	16.883239
34.510744	1164.476697	16.888256
34.597699	1171.962697	16.893274
34.756216	1176.366905	16.898291
35.301911	1172.320867	16.903309
34.976220	1158.246316	16.908327
35.158578	1137.553623	16.913344
34.864083	1136.235366	16.918362
34.390282	1137.105349	16.923379
34.822708	1124.607122	16.928397
34.739418	1129.122235	16.933415
34.609347	1138.369915	16.938432
34.705818	1133.887473	16.943450
34.805712	1145.042631	16.948467
34.992489	1144.602392	16.953485
34.461437	1148.916804	16.958503
34.787471	1154.299397	16.963520
35.198283	1150.053093	16.968538
35.114950	1168.108090	16.973555
35.112468	1164.108583	16.978573
34.857352	1174.173709	16.983591
35.077403	1161.292492	16.988608
35.023166	1163.437281	16.993626
35.140166	1160.924024	16.998643
35.449103	1157.912993	17.003661
35.370402	1172.624760	17.008679
35.429698	1169.345244	17.013696
35.447506	1157.877327	17.018714
34.978613	1183.155430	17.023731
35.333703	1169.014764	17.028749
35.030909	1181.495672	17.033767
35.241348	1173.378847	17.038784
35.356922	1175.477680	17.043802
35.416091	1190.763623	17.048819
36.026520	1187.863370	17.053837
35.703739	1184.076954	17.058855
35.802561	1167.457306	17.063872
35.770479	1162.982773	17.068890
35.593482	1160.030365	17.073907
35.695272	1163.414914	17.078925
35.544074	1165.472926	17.083943
35.729890	1178.741023	17.088960
35.964169	1187.178760	17.093978
35.697073	1193.343338	17.098995
35.940019	1186.199693	17.104013
35.609344	1196.822696	17.109031
35.609085	1201.705242	17.114048
36.022068	1194.172698	17.119066
36.181294	1197.505625	17.124083
35.946698	1197.302465	17.129101
36.089367	1198.770948	17.134119
36.290937	1194.295320	17.139136
36.270780	1193.801570	17.144154
35.981762	1185.407336	17.149171
36.193289	1185.444469	17.154189
36.322909	1187.084910	17.159207
36.420950	1192.475566	17.164224
36.528658	1184.442756	17.169242
36.612422	1183.289100	17.174259
36.621685	1188.443815	17.179277
36.262683	1196.661587	17.184295
36.375396	1185.946108	17.189312
36.616714	1189.844784	17.194330
36.575174	1191.125579	17.199347
36.734987	1178.868974	17.204365
36.404995	1184.780899	17.209383
36.447140	1190.337763	17.214400
36.992824	1188.769108	17.219418
36.235703	1185.258017	17.224435
36.495576	1180.642540	17.229453
36.658606	1186.787279	17.234471
36.482941	1197.741047	17.239488
36.686831	1193.425489	17.244506
36.458681	1189.578363	17.249523
37.088086	1199.582661	17.254541
36.784918	1199.149776	17.259559
36.829787	1216.504875	17.264576
36.900374	1218.167318	17.269594
37.401195	1223.327017	17.274611
37.231661	1226.215331	17.279629
37.161829	1220.137676	17.284647
37.125717	1200.942575	17.289664
37.075787	1201.460258	17.294682
36.817103	1212.026175	17.299699
37.280572	1218.654669	17.304717
37.180025	1221.140316	17.309735
37.247712	1229.647116	17.314752
37.375714	1209.241401	17.319770
37.610090	1217.537575	17.324787
37.351359	1217.147936	17.329805
37.275445	1221.509326	17.334823
37.546692	1216.814950	17.339840
37.543014	1218.302056	17.344858
36.974701	1221.483618	17.349875
37.619468	1213.115042	17.354893
37.499675	1214.136199	17.359911
37.457580	1228.507148	17.364928
37.716610	1222.723093	17.369946
37.410278	1222.182178	17.374963
37.537460	1215.269329	17.379981
37.742477	1219.047967	17.384999
37.434969	1212.939011	17.390016
37.683320	1214.760284	17.395034
37.554956	1237.343196	17.400051
38.156052	1227.773552	17.405069
38.011804	1230.321224	17.410087
37.707068	1239.610980	17.415104
37.992379	1234.433033	17.420122
37.984210	1239.049452	17.425139
37.907115	1231.725603	17.430157
38.033422	1234.714594	17.435175
38.000261	1233.098259	17.440192
38.278336	1229.085450	17.445210
38.143198	1226.404764	17.450227
38.342441	1235.260229	17.455245
38.398095	1228.925042	17.460263
38.364763	1237.367737	17.465280
38.622271	1224.091972	17.470298
38.597001	1227.669824	17.475315
38.923033	1226.944692	17.480333
38.720711	1226.833907	17.485351
38.523664	1223.629865	17.490368
38.476889	1227.940995	17.495386
38.522420	1235.719911	17.500403
38.679215	1226.814127	17.505421
38.458551	1223.870243	17.510439
38.382345	1234.798739	17.515456
38.541711	1219.548851	17.520474
38.396013	1224.294159	17.525491
38.293101	1229.136460	17.530509
38.593514	1229.252221	17.535527
38.597633	1234.851345	17.540544
39.023277	1236.325037	17.545562
38.717228	1252.499808	17.550579
39.087777	1256.601251	17.555597
39.264779	1255.056784	17.560615
39.233077	1250.004891	17.565632
39.211625	1236.772031	17.570650
38.817838	1241.333552	17.575667
39.152611	1242.066722	17.580685
39.376746	1259.758208	17.585703
39.192731	1260.083355	17.590720
39.247699	1252.337331	17.595738
39.132390	1258.812768	17.600755
39.173241	1251.632112	17.605773
39.248155	1246.740960	17.610791
39.277938	1258.778802	17.615808
39.548465	1249.055808	17.620826
39.514712	1253.235886	17.625843
39.539890	1257.552851	17.630861
39.698312	1258.435264	17.635879
39.692590	1250.768129	17.640896
39.711543	1243.691638	17.645914
39.193112	1255.805898	17.650931
39.656989	1254.478362	17.655949
39.658930	1258.476578	17.660967
39.284125	1252.650458	17.665984
39.482766	1250.169781	17.671002
39.587056	1252.220091	17.676019
39.358157	1254.400613	17.681037
39.365102	1276.542029	17.686055
39.638994	1280.095778	17.691072
40.065200	1278.272476	17.696090
39.848624	1286.280402	17.701107
39.754285	1279.357235	17.706125
40.183183	1284.481239	17.711143
39.711802	1282.878160	17.716160
40.017214	1274.200318	17.721178
40.263350	1287.960668	17.726195
40.080127	1288.307711	17.731213
40.273076	1284.652939	17.736231
40.332674	1287.043848	17.741248
40.388909	1276.154848	17.746266
39.970018	1293.022456	17.751283
39.904312	1306.415723	17.756301
40.756993	1295.426430	17.761319
40.756703	1310.155718	17.766336
40.314973	1308.950584	17.771354
40.414855	1309.106193	17.776371
40.557443	1300.905741	17.781389
40.707647	1304.441471	17.786407
40.617191	1312.457610	17.791424
40.790294	1303.349414	17.796442
40.799478	1300.047974	17.801459
41.049373	1310.564313	17.806477
41.019992	1297.095146	17.811495
40.626776	1308.134026	17.816512
40.924788	1304.545861	17.821530
40.888211	1300.754665	17.826547
41.017324	1306.846666	17.831565
40.773609	1306.970559	17.836583
40.690032	1319.265619	17.841600
41.080340	1308.137708	17.846618
41.240185	1312.991612	17.851635
40.914529	1303.741171	17.856653
41.173781	1300.080540	17.861671
40.991426	1307.686636	17.866688
41.142184	1299.359046	17.871706
40.816313	1311.260178	17.876723
40.985245	1326.846497	17.881741
41.384036	1323.692120	17.886759
41.177717	1332.080664	17.891776
41.290015	1323.224388	17.896794
41.581947	1328.851576	17.901811
41.325691	1338.174560	17.906829
41.823978	1320.248392	17.911847
41.475468	1311.322474	17.916864
41.447911	1334.290565	17.921882
41.898397	1316.513591	17.926899
41.533799	1317.263925	17.931917
41.650913	1331.735421	17.936935
41.774749	1328.673656	17.941952
42.152117	1313.881238	17.946970
42.165458	1331.233638	17.951987
41.681262	1318.411116	17.957005
41.891281	1321.971915	17.962023
41.761329	1326.129605	17.967040
41.811651	1322.975750	17.972058
41.837857	1320.835580	17.977075
41.767190	1346.643462	17.982093
42.161958	1339.788548	17.987111
41.990009	1352.451647	17.992128
42.476546	1349.880996	17.997146
42.478751	1355.930338	18.002163
42.297462	1350.892828	18.007181
42.681097	1348.657900	18.012199
42.699822	1350.501655	18.017216
42.838630	1344.357642	18.022234
42.469500	1322.568198	18.027251
42.406526	1324.470595	18.032269
42.660791	1308.769770	18.037287
42.544047	1310.065714	18.042304
42.393796	1321.701331	18.047322
42.824959	1325.857619	18.052339
42.925385	1346.016463	18.057357
43.229222	1339.736026	18.062375
42.942923	1316.173239	18.067392
42.539283	1313.595130	18.072410
42.623964	1306.158930	18.077427
42.694871	1342.866837	18.082445
43.059782	1342.052133	18.087463
42.697922	1358.250078	18.092480
42.891330	1345.328905	18.097498
42.937049	1350.375621	18.102515
42.648602	1348.442924	18.107533
42.959358	1352.503597	18.112551
42.972496	1353.012800	18.117568
42.905849	1345.780031	18.122586
42.898015	1347.439266	18.127603
42.813360	1365.040133	18.132621
43.556888	1363.883486	18.137639
43.457074	1372.601120	18.142656
43.505037	1380.371861	18.147674
43.766669	1365.763009	18.152691
43.647477	1378.115707	18.157709
43.789809	1370.308499	18.162727
43.807633	1375.968409	18.167744
43.727709	1353.324293	18.172762
43.344204	1342.286731	18.177779
43.432394	1363.834902	18.182797
43.834512	1355.651229	18.187815
43.758800	1362.151856	18.192832
43.622485	1366.146984	18.197850
44.054377	1363.078552	18.202867
43.941774	1362.997500	18.207885
44.044379	1365.155056	18.212903
43.850249	1362.420834	18.217920
43.842614	1365.003368	18.222938
43.831426	1369.293134	18.227955
43.843805	1369.726956	18.232973
43.994377	1364.136314	18.237991
43.811407	1371.442105	18.243008
43.597346	1375.630525	18.248026
44.187946	1375.880901	18.253043
44.129145	1394.734479	18.258061
44.678203	1402.802830	18.263079
44.394784	1396.921179	18.268096
44.415961	1393.825437	18.273114
44.548357	1391.273507	18.278131
44.548463	1401.727506	18.283149
44.945995	1390.697477	18.288167
44.784032	1371.073926	18.293184
44.585348	1362.986065	18.298202
44.831903	1363.873304	18.303219
44.576529	1363.277068	18.308237
44.528588	1369.351715	18.313255
44.779065	1381.447268	18.318272
44.805196	1392.895943	18.323290
44.968707	1397.102802	18.328307
44.733551	1395.273280	18.333325
44.966883	1394.146089	18.338343
44.953580	1399.191225	18.343360
44.884989	1392.451081	18.348378
44.788615	1393.504693	18.353395
44.571370	1386.590066	18.358413
44.666244	1391.886923	18.363431
44.846705	1403.488739	18.368448
45.225942	1414.053737	18.373466
45.443042	1415.469476	18.378483
45.476163	1416.327839	18.383501
45.169416	1428.639707	18.388519
45.590962	1408.177460	18.393536
45.418166	1411.091498	18.398554
45.543359	1414.554168	18.403571
45.342694	1431.517690	18.408589
45.566919	1409.888307	18.413607
45.649971	1412.272350	18.418624
45.521243	1410.894597	18.423642
45.686090	1424.104919	18.428659
45.627777	1421.391496	18.433677
45.276629	1402.971507	18.438695
45.607643	1416.775071	18.443712
45.417245	1430.433722	18.448730
46.235273	1419.325599	18.453747
45.961086	1444.779163	18.458765
46.076481	1459.413078	18.463783
46.414820	1451.094810	18.468800
46.010655	1426.020140	18.473818
45.952037	1429.895933	18.478835
45.983029	1452.356242	18.483853
45.975590	1441.165824	18.488871
46.320840	1437.077753	18.493888
46.105975	1444.928196	18.498906
46.348782	1453.948302	18.503923
46.393594	1445.670557	18.508941
46.350175	1448.567115	18.513959
46.479996	1440.118519	18.518976
46.542063	1442.447714	18.523994
46.680029	1438.809537	18.529011
46.582568	1439.059539	18.534029
46.739608	1445.724425	18.539047
46.531638	1438.226293	18.544064
46.278666	1449.909854	18.549082
46.753208	1441.036633	18.554099
46.425666	1454.224838	18.559117
46.366796	1456.030646	18.564135
46.449649	1464.843468	18.569152
46.742786	1473.562987	18.574170
46.887325	1480.791434	18.579187
46.586652	1469.193169	18.584205
46.800766	1467.787476	18.589223
47.206952	1484.081717	18.594240
47.242570	1503.209805	18.599258
47.682872	1492.317593	18.604275
47.454500	1475.301474	18.609293
47.105898	1455.466908	18.614311
47.416093	1465.294220	18.619328
47.212497	1471.993037	18.624346
47.385560	1481.332586	18.629363
47.615647	1496.154306	18.634381
47.874694	1491.600211	18.639399
47.883113	1491.908830	18.644416
47.301250	1477.574381	18.649434
47.661183	1476.971243	18.654451
48.014182	1489.325807	18.659469
47.782606	1489.414732	18.664487
47.665306	1497.669628	18.669504
47.889418	1504.394629	18.674522
48.053142	1481.332367	18.679539
47.955383	1474.681777	18.684557
47.694807	1504.007510	18.689575
48.624388	1474.587841	18.694592
48.328198	1492.944594	18.699610
48.202155	1481.368805	18.704627
48.271048	1470.907062	18.709645
48.044005	1466.576781	18.714663
48.257863	1466.786572	18.719680
48.259581	1487.049441	18.724698
48.479014	1481.263735	18.729715
48.059529	1500.217442	18.734733
48.185655	1492.469379	18.739751
48.574542	1479.851955	18.744768
48.051366	1485.626500	18.749786
48.439269	1489.201444	18.754803
48.445374	1494.241944	18.759821
48.305530	1487.651541	18.764839
48.452349	1475.502148	18.769856
48.545456	1477.356079	18.774874
48.719972	1496.748290	18.779891
48.872186	1467.850570	18.784909
48.635313	1515.165801	18.789927
48.858459	1509.879698	18.794944
48.636601	1502.592954	18.799962
49.168714	1511.861105	18.804979
48.896766	1513.087440	18.809997
48.862083	1508.872757	18.815015
49.014609	1504.003747	18.820032
48.938665	1496.151059	18.825050
48.941928	1506.722604	18.830067
49.484638	1496.262355	18.835085
49.374056	1498.011923	18.840103
49.513463	1509.346673	18.845120
49.574325	1486.552484	18.850138
49.476348	1487.579619	18.855155
49.474095	1504.058566	18.860173
49.619401	1501.554893	18.865191
49.843280	1496.386652	18.870208
49.331118	1490.365268	18.875226
49.824898	1505.041129	18.880243
49.895658	1483.174996	18.885261
49.440689	1513.008360	18.890279
49.912481	1510.768788	18.895296
50.212193	1524.239257	18.900314
49.897126	1520.962737	18.905331
49.905781	1518.463552	18.910349
49.741434	1535.519714	18.915367
50.104321	1521.875312	18.920384
50.036061	1531.781900	18.925402
50.007275	1524.756929	18.930419
50.168479	1518.993077	18.935437
49.936388	1525.981172	18.940455
50.417474	1518.239407	18.945472
50.447853	1534.279829	18.950490
50.555202	1530.483709	18.955507
50.771847	1532.603442	18.960525
50.429292	1521.967399	18.965543
50.336725	1522.148983	18.970560
50.111870	1536.548597	18.975578
50.225742	1537.570263	18.980595
50.598597	1545.578709	18.985613
50.465969	1552.552527	18.990631
50.857586	1557.860323	18.995648
51.084185	1554.700327	19.000666
51.052179	1552.553676	19.005683
51.236585	1555.741104	19.010701
51.333994	1563.331030	19.015719
51.080361	1541.700582	19.020736
51.123278	1526.493324	19.025754
51.174556	1512.094046	19.030771
51.217065	1515.882950	19.035789
50.791026	1522.702205	19.040807
51.061918	1538.188338	19.045824
51.081026	1554.155863	19.050842
50.782686	1553.709611	19.055859
51.277163	1555.085848	19.060877
51.002979	1556.016822	19.065895
51.328577	1547.420541	19.070912
51.105773	1553.811008	19.075930
51.322188	1574.656369	19.080947
51.770898	1570.647715	19.085965
51.696378	1581.461375	19.090983
51.871001	1582.320776	19.096000
51.771892	1583.835723	19.101018
51.764702	1579.618208	19.106035
51.868158	1582.947535	19.111053
52.152073	1582.380112	19.116071
52.155377	1576.963881	19.121088
52.351771	1581.591830	19.126106
52.111259	1579.281804	19.131123
52.343653	1582.044743	19.136141
52.016217	1585.249311	19.141159
51.882881	1572.466559	19.146176
52.227557	1570.497354	19.151194
52.196269	1568.487436	19.156211
52.377333	1580.416479	19.161229
52.255493	1577.168905	19.166247
52.453020	1571.504630	19.171264
52.675462	1572.195960	19.176282
52.427287	1566.793098	19.181299
52.874966	1570.478076	19.186317
52.620031	1582.668556	19.191335
52.617948	1571.936495	19.196352
52.889193	1561.167144	19.201370
52.721620	1564.728448	19.206387
52.684447	1571.635145	19.211405
52.677948	1579.845677	19.216423
52.788606	1585.740970	19.221440
52.597772	1587.792777	19.226458
52.440570	1597.693145	19.231475
52.745154	1586.638467	19.236493
52.749812	1597.546474	19.241511
53.108777	1608.234396	19.246528
53.434843	1616.089899	19.251546
53.729213	1621.738836	19.256563
53.820126	1614.671137	19.261581
53.592949	1595.828445	19.266599
53.577877	1580.274097	19.271616
53.809219	1584.635358	19.276634
53.715920	1581.021444	19.281651
53.986247	1566.744477	19.286669
53.665373	1575.926911	19.291687
53.921298	1578.569696	19.296704
53.978847	1575.499575	19.301722
53.741623	1585.354496	19.306739
53.810011	1574.436593	19.311757
53.569332	1591.976104	19.316775
53.790385	1592.324746	19.321792
54.066642	1583.764626	19.326810
53.558366	1579.181866	19.331827
54.173608	1592.394446	19.336845
54.078578	1613.454696	19.341863
54.407870	1605.398900	19.346880
54.700614	1609.840037	19.351898
53.975800	1595.201084	19.356915
54.209108	1602.711158	19.361933
54.541402	1602.359383	19.366951
54.373614	1596.441906	19.371968
54.533781	1608.183973	19.376986
54.425951	1614.334340	19.382003
54.573991	1599.120466	19.387021
54.379157	1606.003559	19.392039
54.291266	1607.670872	19.397056
54.390996	1594.594534	19.402074
54.530644	1604.348469	19.407091
55.042208	1621.511654	19.412109
54.924198	1629.607866	19.417127
55.104105	1634.719797	19.422144
55.328256	1632.828006	19.427162
55.211451	1637.874001	19.432179
55.577408	1619.600490	19.437197
55.088605	1614.907650	19.442215
55.015159	1603.263601	19.447232
55.607449	1623.083276	19.452250
55.325433	1630.966549	19.457267
55.682566	1638.315326	19.462285
55.376746	1638.159693	19.467303
55.404357	1624.092834	19.472320
55.651816	1621.190613	19.477338
55.351393	1631.236538	19.482355
55.598609	1622.577210	19.487373
55.651644	1630.021668	19.492391
55.230672	1626.691227	19.497408
55.523647	1622.210331	19.502426
55.612816	1628.812195	19.507443
55.987052	1628.625187	19.512461
55.838805	1633.528333	19.517479
55.536319	1635.671883	19.522496
56.013215	1640.434439	19.527514
55.939314	1660.108727	19.532531
55.955058	1661.572332	19.537549
55.832527	1659.364599	19.542567
55.992650	1656.474726	19.547584
56.070841	1655.208667	19.552602
56.189038	1666.836354	19.557619
56.592512	1675.033468	19.562637
56.619456	1674.230175	19.567655
56.888422	1675.500819	19.572672
57.227371	1662.625366	19.577690
56.685115	1651.925908	19.582707
56.904941	1650.465804	19.587725
56.832244	1637.684334	19.592743
56.926916	1640.851485	19.597760
57.073836	1639.590196	19.602778
56.740233	1632.519403	19.607795
56.848362	1632.448763	19.612813
56.775224	1643.614599	19.617831
56.709852	1663.842798	19.622848
57.315273	1668.679247	19.627866
56.862929	1667.543410	19.632883
56.977141	1674.183772	19.637901
56.940434	1677.933442	19.642919
56.937087	1675.242665	19.647936
57.073722	1678.538410	19.652954
57.316187	1690.559997	19.657971
57.306055	1695.699110	19.662989
57.471455	1704.418692	19.668007
57.554600	1699.323158	19.673024
57.974144	1702.781428	19.678042
57.753924	1708.915152	19.683059
57.861816	1698.179616	19.688077
57.850877	1697.190457	19.693095
57.571508	1702.281274	19.698112
57.825721	1695.278728	19.703130
57.599140	1697.573773	19.708147
57.726698	1692.570258	19.713165
57.525907	1717.049919	19.718183
57.800132	1731.182161	19.723200
58.374024	1728.665157	19.728218
58.115286	1738.026543	19.733235
58.261253	1725.958873	19.738253
58.501065	1726.076443	19.743271
58.256300	1737.543423	19.748288
58.226090	1728.997486	19.753306
58.270968	1727.974255	19.758323
58.536960	1739.882021	19.763341
59.032278	1753.505553	19.768359
58.955140	1758.479197	19.773376
58.951482	1755.034985	19.778394
58.751885	1765.448736	19.783411
58.773151	1752.420948	19.788429
58.987337	1755.834903	19.793447
58.818605	1747.664972	19.798464
58.795358	1760.422686	19.803482
59.136956	1748.441774	19.808499
59.203634	1737.668738	19.813517
59.106246	1759.846408	19.818535
59.011155	1750.363856	19.823552
59.292614	1738.839276	19.828570
58.683560	1744.797500	19.833587
59.125569	1759.555809	19.838605
59.447466	1770.075159	19.843623
59.389819	1773.696061	19.848640
59.309271	1774.033031	19.853658
59.330552	1778.135272	19.858675
59.556512	1779.639297	19.863693
59.499175	1784.015195	19.868711
59.258837	1780.195021	19.873728
59.874516	1794.011752	19.878746
59.796704	1801.230202	19.883763
59.947938	1800.789323	19.888781
60.309339	1801.691311	19.893799
60.084391	1805.180026	19.898816
60.094792	1796.361734	19.903834
60.245218	1800.820908	19.908851
60.353423	1799.414770	19.913869
60.470175	1793.635878	19.918887
60.468867	1803.783656	19.923904
60.886800	1790.093260	19.928922
60.757271	1793.582486	19.933939
60.653384	1793.750148	19.938957
61.037270	1788.765497	19.943975
60.693060	1794.074324	19.948992
60.861630	1790.646682	19.954010
60.754565	1799.304380	19.959027
60.851710	1801.179732	19.964045
61.012648	1794.613579	19.969063
60.906076	1791.497227	19.974080
61.208222	1786.616847	19.979098
61.223710	1800.721206	19.984115
60.964409	1794.997564	19.989133
61.087986	1782.554323	19.994151
60.981869	1779.974296	19.999168
61.113697	1785.658658	20.004186
61.328642	1807.533337	20.009203
61.345685	1813.155792	20.014221
62.119307	1818.020524	20.019239
61.714667	1834.021328	20.024256
62.006256	1805.931260	20.029274
61.720562	1791.187471	20.034291
61.177195	1802.971106	20.039309
61.823454	1810.899922	20.044327
61.628169	1812.324838	20.049344
61.564532	1804.190024	20.054362
61.702892	1831.834171	20.059379
61.951960	1811.810994	20.064397
61.972586	1818.129722	20.069415
61.900625	1828.733947	20.074432
61.970827	1824.875249	20.079450
62.345214	1833.062936	20.084467
62.078695	1844.399763	20.089485
62.303609	1847.497426	20.094503
62.381976	1837.392556	20.099520
62.646308	1837.125547	20.104538
62.533301	1854.785012	20.109555
62.517564	1843.913356	20.114573
62.525905	1833.314717	20.119591
62.657334	1846.957043	20.124608
62.990873	1841.075920	20.129626
63.094408	1835.722259	20.134643
62.930732	1833.359040	20.139661
63.369710	1836.804806	20.144679
63.137352	1839.261241	20.149696
63.158784	1832.108563	20.154714
62.979613	1832.393622	20.159731
63.258441	1835.894815	20.164749
63.521005	1822.381748	20.169767
63.160769	1837.260208	20.174784
63.202437	1828.850612	20.179802
63.512959	1834.566271	20.184819
63.138543	1824.370023	20.189837
63.526062	1842.072348	20.194855
63.424294	1854.954351	20.199872
63.605296	1862.101671	20.204890
63.810772	1867.698815	20.209907
63.836698	1856.186579	20.214925
64.271346	1851.492685	20.219943
63.510780	1865.212782	20.224960
63.708219	1870.735705	20.229978
64.068463	1851.350692	20.234995
63.706708	1857.500756	20.240013
63.847612	1869.041616	20.245031
63.908247	1878.454407	20.250048
64.262371	1891.622389	20.255066
64.522360	1895.491541	20.260083
64.478794	1896.152950	20.265101
64.733205	1897.446386	20.270119
64.586555	1899.915905	20.275136
64.752372	1894.539706	20.280154
64.729424	1893.366832	20.285171
64.807060	1877.021883	20.290189
64.324038	1895.372758	20.295207
64.476716	1897.651397	20.300224
64.851857	1890.006557	20.305242
64.715601	1900.006037	20.310259
64.807309	1906.447175	20.315277
65.423852	1890.813792	20.320295
64.906982	1923.689076	20.325312
65.113425	1918.023246	20.330330
65.367421	1906.469881	20.335347
65.562796	1927.375736	20.340365
65.446769	1904.274045	20.345383
65.603550	1926.068518	20.350400
65.726899	1902.949105	20.355418
66.002160	1893.484476	20.360435
65.830950	1920.910749	20.365453
65.945487	1906.241443	20.370471
65.420550	1903.552005	20.375488
65.590721	1901.384072	20.380506
65.933556	1905.933718	20.385523
66.244639	1903.457023	20.390541
65.801094	1888.942800	20.395559
65.980990	1906.347980	20.400576
66.150526	1906.366648	20.405594
65.918456	1899.803347	20.410611
65.974738	1903.560268	20.415629
66.429097	1905.771924	20.420647
66.530519	1926.903546	20.425664
66.336471	1935.019919	20.430682
66.695794	1928.068139	20.435699
66.555742	1929.113025	20.440717
66.414203	1928.734561	20.445735
66.489051	1934.994357	20.450752
66.521941	1926.408353	20.455770
66.712119	1920.883541	20.460787
66.709090	1926.287444	20.465805
67.005524	1919.054689	20.470823
67.095895	1922.623709	20.475840
67.031526	1922.945518	20.480858
67.244146	1927.528520	20.485875
66.970712	1935.849462	20.490893
66.874239	1932.129000	20.495911
67.139878	1944.598562	20.500928
67.503931	1939.061746	20.505946
67.491019	1931.258544	20.510963
67.314750	1952.868643	20.515981
67.537690	1944.266478	20.520999
67.379034	1942.866704	20.526016
67.239813	1950.002212	20.531034
67.764475	1960.874759	20.536051
67.684837	1974.530414	20.541069
67.875412	1967.180809	20.546087
67.779655	1972.176372	20.551104
67.933022	1979.543662	20.556122
68.080955	1968.189633	20.561139
67.777376	1973.171147	20.566157
68.243027	1984.013796	20.571175
68.286744	1997.008005	20.576192
68.615322	1993.764013	20.581210
68.734125	2000.815927	20.586227
68.874339	1999.933205	20.591245
68.967693	1992.858641	20.596263
68.824743	1983.586489	20.601280
69.027163	1984.024630	20.606298
68.718802	1981.544459	20.611315
68.566062	1980.980589	20.616333
68.891625	1988.432109	20.621351
69.192914	1984.877865	20.626368
69.068094	1992.245478	20.631386
69.193088	1989.917996	20.636403
69.083959	1990.666944	20.641421
69.270848	1984.005332	20.646439
69.346825	1988.555088	20.651456
69.465769	1989.269238	20.656474
69.591655	1978.239615	20.661491
69.327992	1987.677452	20.666509
69.340687	1982.734627	20.671527
69.572345	1984.209452	20.676544
69.704845	1993.790183	20.681562
69.686973	1978.798999	20.686579
69.792998	1989.285295	20.691597
69.838434	1988.647350	20.696615
69.888870	1993.913764	20.701632
69.973147	2010.395218	20.706650
70.433089	2004.166683	20.711667
69.964036	2019.701332	20.716685
70.074187	2012.908799	20.721703
70.571616	2014.824166	20.726720
70.138028	2013.381711	20.731738
70.373541	2011.469185	20.736755
70.277655	2014.205908	20.741773
70.744652	2010.768378	20.746791
70.715194	2009.654735	20.751808
70.368460	2001.594843	20.756826
70.389711	1998.393567	20.761843
70.633756	2019.087300	20.766861
70.952716	2032.874502	20.771879
71.138516	2025.415517	20.776896
70.799975	2033.122402	20.781914
71.020678	2027.918301	20.786931
71.072102	2039.039408	20.791949
71.488637	2026.294409	20.796967
71.045709	2021.844229	20.801984
71.241020	2028.157214	20.807002
71.455828	2015.957202	20.812019
71.225682	2038.321637	20.817037
71.496857	2044.869499	20.822055
71.789475	2048.333938	20.827072
71.527322	2056.703487	20.832090
71.615302	2058.998761	20.837107
71.699549	2058.371928	20.842125
71.841342	2051.426465	20.847143
71.544701	2055.684876	20.852160
71.444928	2055.732333	20.857178
71.891298	2070.076558	20.862195
72.096786	2076.902326	20.867213
72.346119	2084.686952	20.872231
72.632653	2081.444927	20.877248
72.520923	2083.679243	20.882266
72.659812	2072.556239	20.887283
72.633259	2076.843946	20.892301
72.736675	2076.582146	20.897319
72.958036	2070.386910	20.902336
72.773648	2072.429889	20.907354
72.957642	2073.838392	20.912371
72.926138	2083.176346	20.917389
72.861707	2067.659234	20.922407
72.656182	2082.123158	20.927424
72.696086	2084.967229	20.932442
72.985323	2089.884135	20.937459
73.021181	2101.309796	20.942477
73.243093	2090.604552	20.947495
73.374573	2115.215942	20.952512
73.495356	2104.570860	20.957530
74.033218	2100.384253	20.962547
73.659267	2110.267623	20.967565
73.859731	2103.877502	20.972583
73.673039	2099.606661	20.977600
73.604428	2097.774083	20.982618
73.780128	2103.174719	20.987635
73.849238	2097.302629	20.992653
73.686079	2097.811657	20.997671
73.694181	2102.279463	21.002688
74.031383	2126.425480	21.007706
74.267160	2125.348184	21.012723
73.983905	2132.597987	21.017741
73.929489	2142.340760	21.022759
74.400134	2130.946154	21.027776
74.115393	2134.320211	21.032794
74.316111	2152.054279	21.037811
74.494871	2165.071148	21.042829
74.890150	2162.491322	21.047847
75.343009	2159.671075	21.052864
75.160342	2160.326364	21.057882
75.242904	2151.228931	21.062899
75.295696	2152.927354	21.067917
75.113916	2158.366141	21.072935
75.385163	2151.338638	21.077952
75.445180	2151.893877	21.082970
75.514434	2147.030068	21.087987
75.471065	2153.513306	21.093005
75.387582	2154.607389	21.098023
75.778274	2144.277891	21.103040
75.313952	2158.742261	21.108058
75.575742	2146.437119	21.113075
75.503435	2151.427431	21.118093
75.381362	2155.851517	21.123111
75.582804	2147.984129	21.128128
76.002258	2161.469134	21.133146
75.779917	2173.222321	21.138163
75.854030	2179.376946	21.143181
76.130287	2183.141334	21.148199
76.144168	2156.796916	21.153216
76.143569	2181.800721	21.158234
76.416334	2173.700145	21.163251
76.324676	2174.926096	21.168269
76.514685	2172.130459	21.173287
76.520288	2191.412110	21.178304
76.545847	2211.093306	21.183322
76.717318	2206.976107	21.188339
76.703363	2206.879316	21.193357
77.031028	2208.725826	21.198375
76.930356	2201.551538	21.203392
77.100310	2209.537657	21.208410
77.119646	2208.013516	21.213427
77.378862	2197.163817	21.218445
76.901348	2208.325356	21.223463
77.104382	2207.851037	21.228480
77.401099	2195.323203	21.233498
77.192464	2201.010110	21.238515
77.527444	2223.635501	21.243533
77.786175	2217.196713	21.248551
78.023942	2218.016198	21.253568
77.858480	2226.908409	21.258586
77.972420	2225.411653	21.263603
78.033360	2225.795285	21.268621
78.021810	2223.278750	21.273639
78.371410	2222.530942	21.278656
77.986996	2224.966070	21.283674
78.208883	2217.987306	21.288691
78.313752	2209.403814	21.293709
78.410976	2214.854760	21.298727
78.465785	2204.923281	21.303744
78.100040	2220.734256	21.308762
78.169573	2211.774146	21.313779
78.657465	2234.313820	21.318797
78.335066	2244.491087	21.323815
78.725453	2243.214519	21.328832
78.570697	2246.912373	21.333850
78.737854	2244.434978	21.338867
79.022155	2254.399098	21.343885
79.226471	2264.242269	21.348903
79.357090	2261.984634	21.353920
79.058836	2273.562813	21.358938
79.388452	2277.364336	21.363955
79.291423	2270.795061	21.368973
79.338412	2272.711507	21.373991
79.410953	2267.773199	21.379008
79.750324	2266.599148	21.384026
79.855657	2272.018934	21.389043
79.961933	2279.688049	21.394061
79.761326	2271.979091	21.399079
79.969494	2274.761760	21.404096
80.107110	2297.440762	21.409114
80.016133	2307.433300	21.414131
80.263956	2302.825688	21.419149
79.979117	2303.877957	21.424167
80.399817	2310.597156	21.429184
80.236579	2308.762337	21.434202
80.361344	2299.445718	21.439219
80.236791	2313.745944	21.444237
80.180000	2317.281899	21.449255
80.780930	2314.384528	21.454272
80.698788	2322.019216	21.459290
80.767506	2314.295602	21.464307
81.455641	2306.717043	21.469325
81.555058	2312.524761	21.474343
81.641702	2304.600087	21.479360
81.566228	2296.004403	21.484378
81.435301	2305.256106	21.489395
81.674694	2308.523026	21.494413
81.610459	2308.630884	21.499431
81.886789	2300.048313	21.504448
81.767682	2315.898714	21.509466
81.861860	2308.814427	21.514483
82.129516	2297.444197	21.519501
81.995348	2304.253448	21.524519
82.066597	2289.019638	21.529536
81.762283	2292.615507	21.534554
81.778727	2304.052289	21.539571
81.730374	2305.829783	21.544589
81.500182	2311.082858	21.549607
82.128541	2300.946592	21.554624
82.175509	2310.248583	21.559642
82.268288	2328.566384	21.564659
82.712354	2320.726282	21.569677
82.422579	2325.573574	21.574695
83.008693	2324.308261	21.579712
82.656423	2331.938838	21.584730
82.675975	2331.312872	21.589747
83.091399	2320.306034	21.594765
82.698926	2347.184786	21.599783
83.061417	2336.725939	21.604800
83.063654	2351.308014	21.609818
82.791909	2358.244624	21.614835
83.289855	2363.126769	21.619853
83.410841	2355.865147	21.624871
83.565458	2354.014243	21.629888
83.296752	2353.895151	21.634906
83.220683	2357.228118	21.639923
83.991237	2369.389436	21.644941
83.811387	2385.366007	21.649959
83.639561	2390.410810	21.654976
83.962839	2376.872605	21.659994
83.771987	2380.108259	21.665011
83.999405	2381.918867	21.670029
83.841912	2393.431435	21.675047
84.365499	2406.036447	21.680064
84.460349	2412.640123	21.685082
84.237135	2415.891171	21.690099
84.877651	2413.090506	21.695117
84.408934	2419.460786	21.700135
84.638428	2415.676421	21.705152
84.889601	2410.907001	21.710170
84.753023	2414.012095	21.715187
85.073728	2401.927013	21.720205
84.828833	2408.614752	21.725223
85.187926	2436.401825	21.730240
85.357880	2438.276662	21.735258
85.571248	2438.096427	21.740275
85.889433	2423.704809	21.745293
85.396039	2429.470248	21.750311
85.565186	2430.118211	21.755328
85.852096	2427.575285	21.760346
85.682499	2434.140127	21.765363
85.859541	2426.502217	21.770381
85.873776	2432.708184	21.775399
85.554603	2430.618993	21.780416
85.762205	2431.823200	21.785434
85.955812	2433.398525	21.790451
86.085531	2426.387954	21.795469
85.809367	2433.884534	21.800487
86.189514	2448.155537	21.805504
86.558992	2450.409919	21.810522
86.344912	2453.295350	21.815539
86.526472	2471.900419	21.820557
86.638516	2443.877866	21.825575
86.716977	2460.612453	21.830592
87.021246	2461.182240	21.835610
86.941008	2458.572794	21.840627
86.802067	2449.324086	21.845645
86.802606	2467.703177	21.850663
87.336669	2476.708943	21.855680
87.426803	2473.305449	21.860698
87.367310	2484.606612	21.865715
87.951668	2473.781942	21.870733
88.097088	2478.522134	21.875751
87.896451	2478.191618	21.880768
87.970673	2479.291251	21.885786
87.951555	2482.113351	21.890803
87.956866	2469.978615	21.895821
87.730801	2481.215885	21.900839
87.612602	2474.851249	21.905856
88.015568	2469.261625	21.910874
87.786329	2471.828568	21.915891
88.422182	2479.794814	21.920909
88.328209	2497.995525	21.925927
88.291674	2490.442765	21.930944
88.550786	2488.361242	21.935962
88.586516	2498.763945	21.940979
88.649244	2498.897179	21.945997
88.569074	2498.633972	21.951015
88.327480	2499.086304	21.956032
89.088352	2506.356203	21.961050
88.853997	2522.800170	21.966067
89.306013	2518.878045	21.971085
89.314490	2517.877868	21.976103
89.491314	2525.283383	21.981120
89.482578	2511.149099	21.986138
89.593274	2517.033755	21.991155
89.660046	2514.717048	21.996173
89.708529	2509.474170	22.001191
89.110594	2517.977752	22.006208
89.530989	2528.879943	22.011226
89.702966	2548.531956	22.016243
90.009719	2549.026630	22.021261
90.119636	2543.837653	22.026279
90.144871	2545.632543	22.031296
90.368452	2537.342187	22.036314
90.288491	2533.086446	22.041331
90.391912	2527.936265	22.046349
90.467287	2541.996401	22.051367
90.534843	2565.453089	22.056384
91.193470	2557.316728	22.061402
90.920158	2566.603099	22.066419
90.854832	2564.681844	22.071437
90.938947	2560.597354	22.076455
90.978878	2560.959176	22.081472
91.628732	2558.765783	22.086490
91.288303	2577.832554	22.091507
91.536992	2559.689044	22.096525
91.566489	2552.576412	22.101543
91.301082	2563.363823	22.106560
91.271387	2556.474568	22.111578
91.165633	2556.983109	22.116595
91.291915	2551.510723	22.121613
91.478895	2561.916096	22.126631
91.624061	2579.301667	22.131648
91.877433	2585.928124	22.136666
92.138042	2592.618714	22.141683
92.475463	2572.390059	22.146701
92.290992	2575.741934	22.151719
91.865443	2591.421267	22.156736
92.376450	2604.753657	22.161754
92.640684	2607.178224	22.166771
92.570327	2619.005065	22.171789
92.626545	2617.975246	22.176807
92.907137	2605.421317	22.181824
93.211388	2601.138111	22.186842
92.879706	2617.974461	22.191859
92.858093	2611.094904	22.196877
93.676261	2627.183955	22.201895
93.361030	2633.798852	22.206912
93.447630	2629.628999	22.211930
93.745623	2631.152307	22.216947
93.514061	2628.644829	22.221965
93.887814	2626.904459	22.226983
93.648837	2630.729102	22.232000
93.793704	2621.612002	22.237018
93.635086	2634.811301	22.242035
94.022611	2630.586384	22.247053
93.991620	2629.336078	22.252071
93.593920	2644.478533	22.257088
94.144769	2656.281069	22.262106
94.244686	2660.120896	22.267123
94.306749	2671.070110	22.272141
94.381695	2658.822648	22.277159
94.351060	2666.837859	22.282176
94.775248	2668.342621	22.287194
94.883167	2688.246509	22.292211
95.193414	2681.014324	22.297229
95.116173	2686.111003	22.302247
95.070101	2679.523978	22.307264
95.462433	2669.248124	22.312282
95.189324	2678.214406	22.317299
95.406838	2681.580860	22.322317
95.212114	2669.823938	22.327335
95.466674	2674.660055	22.332352
95.517608	2680.412728	22.337370
95.528673	2673.039481	22.342387
95.779965	2685.279939	22.347405
95.923413	2694.248237	22.352423
96.048820	2701.137411	22.357440
96.344980	2698.095076	22.362458
96.412714	2695.550872	22.367475
96.318044	2696.416318	22.372493
96.420290	2697.957475	22.377511
96.505610	2690.827223	22.382528
96.617617	2686.156201	22.387546
96.547452	2685.434408	22.392563
96.452934	2694.648302	22.397581
96.801715	2695.216509	22.402599
96.684137	2717.309977	22.407616
97.172919	2714.097704	22.412634
96.914577	2712.939489	22.417651
97.060933	2723.629896	22.422669
96.869054	2718.588874	22.427687
97.179422	2730.788488	22.432704
97.341002	2749.052587	22.437722
97.154888	2763.462177	22.442739
97.493522	2743.866271	22.447757
97.640385	2752.564272	22.452775
97.498372	2776.138879	22.457792
98.114253	2767.867640	22.462810
98.273865	2771.958328	22.467827
98.267196	2777.974283	22.472845
98.412951	2772.420841	22.477863
98.517895	2787.033381	22.482880
98.826121	2781.649881	22.487898
98.723204	2780.301700	22.492915
98.528657	2771.945744	22.497933
98.687456	2773.591156	22.502951
98.777793	2780.922499	22.507968
98.711330	2785.618709	22.512986
98.907837	2798.763888	22.518003
99.094066	2807.870948	22.523021
99.012446	2802.442632	22.528039
99.339339	2809.221860	22.533056
99.108593	2800.560181	22.538074
99.301728	2807.784692	22.543091
99.507426	2826.613683	22.548109
99.740812	2834.131467	22.553127
99.879760	2841.344184	22.558144
99.875987	2835.619494	22.563162
100.060406	2838.894516	22.568179
99.883570	2829.436090	22.573197
99.907877	2832.641467	22.578215
100.085074	2845.630882	22.583232
100.232733	2845.774960	22.588250
100.479672	2853.594207	22.593267
100.829456	2855.109281	22.598285
100.879372	2837.896949	22.603303
100.951872	2844.067058	22.608320
101.122321	2845.224526	22.613338
101.085102	2842.377689	22.618355
101.200223	2839.122719	22.623373
101.228421	2841.334051	22.628391
100.926299	2845.217585	22.633408
100.926003	2836.675664	22.638426
101.337255	2844.332630	22.643443
101.190898	2862.226737	22.648461
101.656591	2865.835250	22.653479
101.590357	2875.085649	22.658496
101.617533	2875.169497	22.663514
101.676141	2879.102491	22.668531
101.998057	2894.658240	22.673549
101.989051	2896.862141	22.678567
102.127613	2907.116597	22.683584
102.504639	2890.648046	22.688602
102.729423	2892.824107	22.693619
102.478322	2901.511718	22.698637
102.837400	2896.308057	22.703655
102.806363	2893.898340	22.708672
102.534830	2902.904623	22.713690
102.992838	2914.486993	22.718707
103.259963	2916.241786	22.723725
103.361045	2910.975432	22.728743
102.809297	2927.841723	22.733760
103.334366	2929.740229	22.738778
103.497966	2926.571111	22.743795
103.381841	2924.394408	22.748813
103.557506	2920.104872	22.753831
103.796962	2938.045311	22.758848
103.854465	2952.235331	22.763866
103.986860	2953.450789	22.768883
104.440830	2958.904122	22.773901
104.206570	2949.425672	22.778919
104.186502	2957.358341	22.783936
104.365079	2951.109778	22.788954
104.494709	2950.387576	22.793971
104.303487	2959.041290	22.798989
104.764249	2950.528038	22.804007
104.880593	2966.261372	22.809024
104.492649	2975.151758	22.814042
105.242021	2971.801917	22.819059
104.914930	2971.832135	22.824077
104.970227	2959.949375	22.829095
105.329472	2971.660805	22.834112
105.348384	2967.107579	22.839130
105.804792	2982.355667	22.844147
105.759293	2987.150853	22.849165
105.965334	2987.091341	22.854183
106.124862	2993.773851	22.859200
106.125015	2978.423232	22.864218
106.243693	2958.755925	22.869235
106.087391	2963.521577	22.874253
106.373375	2971.029474	22.879271
106.216193	2990.609507	22.884288
106.286245	2983.336031	22.889306
106.712528	2979.274734	22.894323
106.325269	2987.119669	22.899341
106.546541	2986.045414	22.904359
106.488902	2992.074304	22.909376
106.201228	2991.207053	22.914394
106.532677	3009.496308	22.919411
106.626747	3017.306983	22.924429
107.117562	3020.876921	22.929447
106.910594	3025.192888	22.934464
107.252674	3035.956143	22.939482
107.485476	3045.605741	22.944499
107.131501	3043.462227	22.949517
107.575615	3046.706112	22.954535
107.700482	3049.530533	22.959552
107.582039	3069.244504	22.964570
108.075577	3069.919430	22.969587
107.992843	3071.071667	22.974605
108.321610	3065.240375	22.979623
108.100199	3071.827135	22.984640
108.412863	3089.169304	22.989658
108.636806	3085.279467	22.994675
108.535627	3102.122093	22.999693
108.558384	3080.713495	23.004711
108.920762	3091.370514	23.009728
109.060600	3092.348038	23.014746
109.207650	3089.752578	23.019763
109.113644	3098.177710	23.024781
109.448590	3098.921975	23.029799
109.747194	3120.414034	23.034816
109.739298	3113.580820	23.039834
110.116520	3110.331979	23.044851
109.822985	3112.203725	23.049869
110.053918	3111.209725	23.054887
109.939082	3116.876523	23.059904
109.955906	3115.487193	23.064922
110.008048	3110.838953	23.069939
110.218245	3117.976735	23.074957
110.457085	3116.034436	23.079975
110.635028	3137.723527	23.084992
110.365552	3146.039016	23.090010
111.085362	3129.923774	23.095027
111.036083	3131.863550	23.100045
110.879527	3124.748842	23.105063
111.242415	3124.836581	23.110080
111.139010	3132.792073	23.115098
111.668385	3124.540724	23.120115
111.363741	3132.208167	23.125133
111.563936	3125.086916	23.130151
111.519983	3133.664550	23.135168
111.887120	3145.702080	23.140186
112.193821	3150.032139	23.145203
111.975959	3148.777762	23.150221
111.914936	3148.900059	23.155239
112.323662	3142.051528	23.160256
112.236088	3146.856621	23.165274
112.380638	3149.280701	23.170291
112.174259	3151.464198	23.175309
112.436868	3142.930518	23.180327
112.537112	3165.908656	23.185344
112.319518	3150.766410	23.190362
112.680451	3161.176726	23.195379
112.655494	3172.840247	23.200397
112.498422	3167.729805	23.205415
112.996109	3180.531553	23.210432
113.270610	3188.302538	23.215450
113.627545	3197.421167	23.220467
113.453162	3212.408252	23.225485
113.442288	3217.441832	23.230503
113.541778	3206.017481	23.235520
113.532680	3203.457910	23.240538
113.994797	3212.551912	23.245555
113.832428	3252.236578	23.250573
113.886873	3234.295467	23.255591
114.468312	3229.296928	23.260608
114.362852	3223.203661	23.265626
114.531817	3237.666435	23.270643
114.706262	3256.084077	23.275661
114.821380	3263.882876	23.280679
115.047880	3256.136753	23.285696
114.819424	3264.798943	23.290714
115.368200	3255.365338	23.295731
115.416665	3261.194934	23.300749
115.259602	3257.291078	23.305767
115.430741	3250.076863	23.310784
115.357168	3253.276702	23.315802
115.565099	3273.665711	23.320819
115.630811	3280.327916	23.325837
116.007262	3283.175195	23.330855
116.087273	3273.076933	23.335872
116.027712	3283.237392	23.340890
115.958441	3271.338058	23.345907
115.914831	3295.328860	23.350925
116.227215	3299.642327	23.355943
116.517326	3296.028202	23.360960
116.603021	3306.735790	23.365978
116.606858	3316.444888	23.370995
117.038385	3326.553030	23.376013
117.291969	3328.030795	23.381031
117.482942	3332.443863	23.386048
117.216554	3340.961909	23.391066
117.431697	3338.172272	23.396083
117.392219	3326.482881	23.401101
117.664850	3337.100904	23.406119
117.730693	3330.084355	23.411136
117.922117	3333.814593	23.416154
117.938425	3325.854960	23.421171
117.784848	3332.600137	23.426189
118.274795	3348.580296	23.431207
118.753493	3339.932601	23.436224
118.581353	3351.512758	23.441242
119.088871	3347.003427	23.446259
119.002074	3345.722628	23.451277
118.798582	3341.065521	23.456295
119.063003	3345.740615	23.461312
118.868228	3338.907989	23.466330
119.170634	3348.542757	23.471347
119.007311	3345.537373	23.476365
119.036478	3345.060855	23.481383
119.165847	3341.079841	23.486400
119.050932	3364.014726	23.491418
119.361468	3372.364500	23.496435
119.299977	3374.415592	23.501453
119.546376	3389.238226	23.506471
119.783790	3391.933073	23.511488
119.544696	3397.090416	23.516506
120.050993	3396.889425	23.521523
120.168049	3412.790672	23.526541
120.148194	3436.334281	23.531559
120.748983	3426.576063	23.536576
120.567381	3436.553147	23.541594
120.922216	3429.272584	23.546611
120.926653	3428.267483	23.551629
120.737123	3429.417111	23.556647
121.093947	3433.832082	23.561664
121.396688	3442.969734	23.566682
121.713464	3435.744792	23.571699
121.326524	3445.491113	23.576717
121.471663	3454.391965	23.581735
121.642478	3451.357666	23.586752
121.615120	3474.012106	23.591770
121.694908	3472.836096	23.596787
121.893412	3469.526002	23.601805
122.062844	3472.264741	23.606823
122.441510	3482.817195	23.611840
122.661584	3490.954922	23.616858
122.824522	3491.277490	23.621875
123.037196	3491.016339	23.626893
122.518278	3513.178150	23.631911
123.150533	3493.759392	23.636928
122.791061	3501.106185	23.641946
122.981016	3514.428468	23.646963
123.306400	3533.393464	23.651981
123.162331	3515.916289	23.656999
123.636057	3520.957658	23.662016
123.618006	3531.961196	23.667034
123.823192	3546.724489	23.672051
123.986169	3551.893290	23.677069
123.825312	3552.496388	23.682087
124.398613	3542.734612	23.687104
124.040000	3553.678411	23.692122
124.325185	3553.876870	23.697139
124.220496	3538.021651	23.702157
124.405684	3586.763770	23.707175
124.860529	3568.935391	23.712192
124.670985	3581.131265	23.717210
124.878191	3585.482041	23.722227
124.872650	3577.531260	23.727245
124.718650	3588.580902	23.732263
125.201763	3603.926073	23.737280
125.040073	3604.561556	23.742298
125.236052	3606.311261	23.747315
125.458318	3618.491061	23.752333
125.894781	3632.197339	23.757351
127.025860	3620.701788	23.762368
127.066556	3630.953481	23.767386
126.861450	3612.785844	23.772403
126.885034	3587.674619	23.777421
126.594870	3597.865771	23.782439
126.852891	3596.327027	23.787456
127.166779	3588.594326	23.792474
126.840612	3598.172951	23.797491
127.356809	3605.079691	23.802509
127.442952	3618.797765	23.807527
127.091968	3614.492100	23.812544
127.085060	3612.289226	23.817562
127.111546	3609.748296	23.822579
127.311134	3621.968684	23.827597
127.324829	3635.131971	23.832615
127.997253	3634.565465	23.837632
127.928940	3646.947368	23.842650
128.040124	3639.886470	23.847667
128.471105	3633.716937	23.852685
128.249317	3656.758994	23.857703
128.538865	3669.974294	23.862720
128.783596	3673.866815	23.867738
128.893300	3666.598476	23.872755
128.740513	3658.642811	23.877773
128.782407	3668.305171	23.882791
129.306224	3663.679090	23.887808
129.223657	3682.946095	23.892826
129.236297	3691.578748	23.897843
129.645765	3698.397145	23.902861
129.712774	3703.107765	23.907879
129.853856	3686.297586	23.912896
129.743551	3694.880622	23.917914
130.033905	3687.265680	23.922931
130.468535	3701.322357	23.927949
130.319489	3728.148310	23.932967
130.724634	3726.812637	23.937984
130.689396	3724.628423	23.943002
130.941117	3711.807559	23.948019
131.166029	3710.185196	23.953037
130.604053	3715.405144	23.958055
130.908714	3724.117898	23.963072
130.767580	3719.342174	23.968090
130.961950	3722.316900	23.973107
131.162655	3737.759158	23.978125
131.322102	3740.934535	23.983143
131.277980	3744.856612	23.988160
131.538891	3746.307296	23.993178
131.441224	3767.610994	23.998195
131.891831	3766.047819	24.003213
131.729202	3776.675781	24.008231
132.180072	3777.168766	24.013248
132.057286	3793.625474	24.018266
131.988170	3802.316851	24.023283
132.530830	3802.257944	24.028301
132.246102	3809.098192	24.033319
132.596630	3814.519578	24.038336
132.855647	3826.201272	24.043354
132.962433	3831.939202	24.048371
133.211631	3835.206482	24.053389
133.278293	3849.025419	24.058407
133.321266	3849.701435	24.063424
133.711790	3846.014530	24.068442
133.494326	3844.103203	24.073459
133.727745	3874.957269	24.078477
134.093054	3880.055383	24.083495
134.155617	3858.405673	24.088512
134.368218	3872.994272	24.093530
134.296719	3877.939418	24.098547
134.718018	3881.567858	24.103565
134.891589	3896.450606	24.108583
134.948609	3894.232777	24.113600
135.248885	3904.702070	24.118618
135.325881	3900.413822	24.123635
135.976434	3880.334814	24.128653
135.591392	3903.078414	24.133671
135.488413	3894.424027	24.138688
135.872567	3921.239260	24.143706
135.613062	3909.466491	24.148723
135.930979	3918.953642	24.153741
136.029475	3929.901139	24.158759
136.348696	3932.510676	24.163776
136.242237	3914.416610	24.168794
136.393918	3950.209676	24.173811
136.897303	3942.260934	24.178829
136.825566	3961.049887	24.183847
136.945321	3958.176229	24.188864
137.180066	3955.158379	24.193882
136.729003	3949.205653	24.198899
137.165902	3961.084854	24.203917
137.159114	3975.861140	24.208935
137.386085	3990.751202	24.213952
137.397581	3990.085545	24.218970
137.199028	3987.707076	24.223987
137.941060	4000.668035	24.229005
138.188396	4007.996990	24.234023
138.182677	4003.991713	24.239040
138.735972	3998.893575	24.244058
138.577848	4005.134772	24.249075
138.894676	4013.832388	24.254093
138.681248	4036.441065	24.259111
139.093081	4036.044318	24.264128
139.226504	4027.176743	24.269146
139.038372	4039.653597	24.274163
139.448786	4024.246694	24.279181
139.318224	4029.182429	24.284199
139.021210	4037.451679	24.289216
139.987218	4042.078068	24.294234
139.932416	4048.692190	24.299251
140.068380	4048.234807	24.304269
140.401972	4052.377569	24.309287
140.444706	4049.741936	24.314304
140.698398	4041.318500	24.319322
140.719622	4036.946283	24.324339
140.806449	4053.320304	24.329357
140.877636	4029.641043	24.334375
140.744667	4083.581649	24.339392
141.070241	4069.228148	24.344410
141.012484	4068.057502	24.349427
141.391716	4065.577457	24.354445
141.347120	4073.889865	24.359463
141.657100	4090.520187	24.364480
142.015409	4095.225393	24.369498
141.852363	4113.823789	24.374515
142.116712	4101.516603	24.379533
142.046509	4097.134559	24.384551
142.166451	4118.504760	24.389568
142.545954	4122.975327	24.394586
142.621264	4137.185685	24.399603
142.705898	4120.105543	24.404621
143.075090	4124.262315	24.409639
143.001198	4126.696217	24.414656
143.248821	4138.509773	24.419674
143.174987	4145.759424	24.424691
143.571832	4139.896406	24.429709
143.869377	4150.857170	24.434727
143.588872	4157.390905	24.439744
143.572756	4155.651171	24.444762
144.056000	4173.357607	24.449779
144.004461	4184.832662	24.454797
144.400530	4192.409385	24.459815
144.168136	4183.667692	24.464832
144.866009	4199.845337	24.469850
144.571496	4209.210065	24.474867
144.793681	4203.175064	24.479885
145.257589	4201.144825	24.484903
144.974039	4201.254624	24.489920
145.270652	4211.179585	24.494938
145.442933	4231.718000	24.499955
145.405233	4233.256463	24.504973
145.492195	4235.944779	24.509991
145.902089	4226.259741	24.515008
146.187526	4231.054487	24.520026
145.847799	4257.428815	24.525043
146.397427	4259.160761	24.530061
146.392799	4248.597047	24.535079
146.332845	4248.300690	24.540096
146.511041	4254.973726	24.545114
146.739408	4267.774540	24.550131
146.777901	4272.794319	24.555149
146.919509	4263.796288	24.560167
147.000477	4282.923946	24.565184
147.524565	4292.710432	24.570202
147.603629	4306.140797	24.575219
147.634209	4321.923880	24.580237
147.914280	4304.202716	24.585255
147.889503	4303.326502	24.590272
148.188358	4315.995765	24.595290
147.977218	4333.890198	24.600307
148.101081	4332.163523	24.605325
148.090349	4334.526031	24.610343
148.631179	4356.959879	24.615360
148.745260	4354.117729	24.620378
148.532964	4363.954018	24.625395
148.940837	4376.961514	24.630413
149.279613	4392.902423	24.635431
149.388220	4397.128355	24.640448
149.291795	4379.751107	24.645466
149.477212	4397.559579	24.650483
149.894136	4414.023757	24.655501
150.183345	4415.568330	24.660519
149.988607	4413.509346	24.665536
150.592153	4414.494842	24.670554
150.653616	4437.433178	24.675571
150.951414	4441.905072	24.680589
151.151260	4437.854314	24.685607
151.209317	4448.789768	24.690624
151.367723	4444.998917	24.695642
151.230414	4449.104382	24.700659
151.324024	4447.856079	24.705677
151.427154	4455.480432	24.710695
151.144474	4460.380779	24.715712
151.913938	4458.874471	24.720730
151.590783	4467.474587	24.725747
151.717133	4493.862346	24.730765
152.435077	4499.310370	24.735783
152.494109	4500.186026	24.740800
152.685356	4496.906754	24.745818
153.069404	4498.215954	24.750835
153.294357	4513.755858	24.755853
153.435885	4509.793831	24.760871
153.152893	4523.743097	24.765888
153.741122	4528.340990	24.770906
153.722460	4516.970642	24.775923
153.377505	4512.002958	24.780941
153.747785	4508.427678	24.785959
153.847736	4542.940334	24.790976
154.097049	4533.834501	24.795994
154.172537	4552.690416	24.801011
154.281654	4558.602111	24.806029
154.541413	4544.703887	24.811047
154.437802	4555.374135	24.816064
154.833934	4570.260631	24.821082
154.540170	4582.136476	24.826099
154.882184	4573.576724	24.831117
155.079365	4598.094514	24.836135
155.100171	4598.037790	24.841152
155.190719	4596.529581	24.846170
155.267969	4623.752177	24.851187
155.652693	4624.048067	24.856205
156.114296	4631.701105	24.861223
155.914208	4647.543340	24.866240
156.228170	4636.126162	24.871258
156.258637	4671.702747	24.876275
156.515224	4661.389727	24.881293
156.759658	4656.004708	24.886311
157.060068	4685.967959	24.891328
157.279923	4668.780661	24.896346
157.618516	4682.580629	24.901363
157.468926	4694.249499	24.906381
157.659314	4667.761493	24.911399
157.378665	4698.991893	24.916416
157.926282	4684.227943	24.921434
158.205873	4708.954618	24.926451
157.903223	4710.985344	24.931469
158.353682	4699.976658	24.936487
158.587494	4732.762151	24.941504
158.684895	4725.778450	24.946522
158.920772	4727.233228	24.951539
159.053888	4724.991342	24.956557
159.382953	4749.556799	24.961575
159.171269	4740.046832	24.966592
159.422106	4745.812502	24.971610
159.924443	4770.241023	24.976627
159.820923	4751.339122	24.981645
160.116948	4773.243096	24.986663
160.351786	4759.111857	24.991680
160.378209	4754.222546	24.996698
160.865550	4778.080779	25.001715
160.899344	4784.095827	25.006733
161.113182	4782.164383	25.011751
160.944469	4800.731511	25.016768
160.982043	4777.722710	25.021786
161.058477	4770.629837	25.026803
161.016064	4797.694835	25.031821
161.620223	4813.770107	25.036839
161.338578	4801.128520	25.041856
161.258640	4834.777675	25.046874
161.541714	4838.300171	25.051891
161.694719	4853.745707	25.056909
161.854441	4867.598754	25.061927
162.378725	4868.598498	25.066944
162.415419	4889.837561	25.071962
162.764345	4890.455408	25.076979
162.780393	4890.251548	25.081997
163.051283	4899.978119	25.087015
163.529253	4913.526376	25.092032
163.348131	4912.878800	25.097050
163.930405	4904.498461	25.102067
163.744860	4895.837765	25.107085
164.105941	4914.828761	25.112103
163.705688	4897.961902	25.117120
164.048218	4947.512618	25.122138
164.328188	4929.996041	25.127155
164.470242	4943.649016	25.132173
164.675046	4939.474611	25.137191
164.796180	4954.169341	25.142208
165.524428	4947.793753	25.147226
165.124412	4951.405514	25.152243
165.096437	4959.047099	25.157261
165.859643	4959.790849	25.162279
165.922291	4969.910964	25.167296
165.701803	5008.059108	25.172314
165.789738	4979.864837	25.177331
166.151415	4982.021754	25.182349
166.346195	5005.301594	25.187367
166.835319	5009.326222	25.192384
166.575522	5002.802903	25.197402
166.955147	5002.293273	25.202419
167.061061	5022.884285	25.207437
166.816445	5009.300467	25.212455
166.854684	5033.106421	25.217472
167.365587	5038.468873	25.222490
167.590007	5045.046793	25.227507
167.325514	5068.933323	25.232525
167.677381	5071.246794	25.237543
168.060830	5071.078758	25.242560
168.068840	5090.411837	25.247578
168.323384	5104.076135	25.252595
168.452175	5103.495569	25.257613
169.139500	5097.844684	25.262631
168.858419	5111.300949	25.267648
168.971103	5111.827455	25.272666
169.255155	5108.987956	25.277683
169.287856	5132.603791	25.282701
169.657095	5134.353596	25.287719
169.955855	5150.924767	25.292736
169.843848	5149.772909	25.297754
170.489098	5163.738421	25.302771
170.368121	5165.141575	25.307789
171.033011	5160.387918	25.312807
170.742489	5164.843695	25.317824
170.636310	5164.671904	25.322842
171.114498	5159.539724	25.327859
170.732822	5173.350358	25.332877
171.532273	5190.351523	25.337895
171.496103	5196.919922	25.342912
171.633872	5191.325149	25.347930
171.861962	5194.805364	25.352947
172.035494	5204.920550	25.357965
172.246237	5208.934549	25.362983
172.399112	5224.598409	25.368000
172.354165	5223.616792	25.373018
172.620930	5215.099349	25.378035
172.942748	5217.589920	25.383053
173.272901	5235.657971	25.388071
173.358649	5248.797844	25.393088
173.036987	5250.151184	25.398106
173.477402	5242.176392	25.403123
173.471088	5251.331413	25.408141
173.665061	5248.873634	25.413159
173.697003	5271.190200	25.418176
173.890641	5285.182199	25.423194
174.297991	5284.390439	25.428211
174.439950	5304.334945	25.433229
174.880284	5319.789446	25.438247
174.769305	5308.490632	25.443264
175.004554	5321.979630	25.448282
175.342982	5329.969713	25.453299
175.109230	5342.819969	25.458317
175.120727	5336.025894	25.463335
175.781505	5355.934959	25.468352
175.855400	5356.380334	25.473370
175.939342	5361.223314	25.478387
175.978391	5382.581505	25.483405
176.427313	5387.485098	25.488423
176.862046	5388.138065	25.493440
176.975427	5394.976935	25.498458
177.315199	5383.770622	25.503475
177.234166	5388.410983	25.508493
177.503200	5397.316083	25.513511
177.757955	5408.237414	25.518528
177.439394	5415.911401	25.523546
177.598840	5409.366691	25.528563
178.104908	5413.535059	25.533581
177.943043	5435.184968	25.538599
178.298197	5449.728814	25.543616
178.111604	5449.981283	25.548634
178.363687	5456.367744	25.553651
178.269539	5477.199763	25.558669
178.826923	5485.785174	25.563687
179.496501	5492.389879	25.568704
179.179999	5506.748992	25.573722
179.713194	5506.616871	25.578739
180.116722	5516.549279	25.583757
180.087323	5527.570282	25.588775
180.279261	5538.021834	25.593792
180.486386	5534.048290	25.598810
180.470809	5538.842684	25.603827
180.562916	5548.487264	25.608845
180.658673	5552.602293	25.613863
181.259152	5553.547462	25.618880
181.035341	5559.903631	25.623898
181.126734	5554.689014	25.628915
181.247954	5566.825186	25.633933
181.610215	5580.427126	25.638951
181.536608	5587.301404	25.643968
181.561333	5593.576270	25.648986
182.262035	5593.515783	25.654003
182.103493	5603.990215	25.659021
182.132300	5613.891170	25.664039
182.819759	5624.088349	25.669056
182.555418	5637.890150	25.674074
182.883978	5640.015472	25.679092
183.013601	5666.403243	25.684109
183.237369	5661.745718	25.689127
183.516749	5672.165331	25.694144
183.527998	5698.858395	25.699162
183.981038	5700.015891	25.704180
184.217433	5697.077674	25.709197
184.326467	5705.608031	25.714215
184.773705	5729.050169	25.719232
184.922028	5728.334298	25.724250
185.157650	5714.305869	25.729268
185.359250	5722.393506	25.734285
185.568042	5740.433538	25.739303
185.596988	5740.314148	25.744320
185.563802	5750.939417	25.749338
186.204005	5750.598278	25.754356
185.666999	5753.188096	25.759373
186.248499	5752.263131	25.764391
186.667619	5793.790990	25.769408
186.627599	5762.035262	25.774426
186.708068	5790.548149	25.779444
187.037265	5784.365638	25.784461
187.077347	5807.844489	25.789479
187.588079	5812.362321	25.794496
187.507004	5796.207447	25.799514
187.844404	5815.617988	25.804532
188.067158	5837.038812	25.809549
188.140989	5831.458711	25.814567
188.922468	5815.761068	25.819584
188.610802	5816.625883	25.824602
188.647460	5857.559556	25.829620
188.986040	5835.940032	25.834637
188.761797	5874.817945	25.839655
189.173591	5840.383604	25.844672
189.308981	5898.515926	25.849690
189.489044	5870.565671	25.854708
189.420524	5910.198496	25.859725
189.718755	5911.697740	25.864743
189.945532	5925.802290	25.869760
190.148449	5914.736191	25.874778
190.162710	5965.075897	25.879796
190.630314	5936.842873	25.884813
190.785771	5976.838253	25.889831
191.014657	5961.994039	25.894848
191.126534	5969.905728	25.899866
191.535764	5993.329959	25.904884
191.678997	5975.808768	25.909901
191.641178	5978.733649	25.914919
191.608566	5992.168410	25.919936
191.764255	6010.963846	25.924954
192.032723	6012.188557	25.929972
192.549920	6021.659471	25.934989
192.412556	6030.689536	25.940007
192.526562	6037.829924	25.945024
192.750890	6056.877245	25.950042
192.858088	6053.483581	25.955060
192.939142	6071.305215	25.960077
193.311676	6098.827269	25.965095
193.746283	6092.398100	25.970112
193.708585	6108.630622	25.975130
194.013293	6123.634765	25.980148
194.261524	6119.962914	25.985165
194.428575	6128.907532	25.990183
194.907452	6153.526197	25.995200
194.690298	6149.760166	26.000218
195.440434	6153.402851	26.005236
195.416446	6173.391511	26.010253
195.554002	6173.063626	26.015271
196.019947	6163.318044	26.020288
196.064749	6204.180572	26.025306
196.370137	6189.954114	26.030324
196.779577	6186.103920	26.035341
196.770543	6216.550758	26.040359
197.341069	6189.402285	26.045376
197.160440	6218.597242	26.050394
197.522032	6219.790604	26.055412
197.867638	6219.449221	26.060429
197.227639	6224.703708	26.065447
197.988015	6217.759162	26.070464
198.284906	6237.264046	26.075482
198.135018	6257.902285	26.080500
198.224038	6257.527064	26.085517
198.047860	6264.031715	26.090535
198.542039	6278.979063	26.095552
198.532400	6277.226243	26.100570
198.805675	6296.945819	26.105588
199.334394	6303.718114	26.110605
199.373469	6314.014423	26.115623
199.756432	6318.404874	26.120640
199.849573	6335.091197	26.125658
200.202051	6342.746015	26.130676
200.313672	6354.736457	26.135693
201.029685	6367.200955	26.140711
201.112226	6363.154215	26.145728
201.174791	6368.522550	26.150746
200.733576	6365.704812	26.155764
201.094161	6372.117649	26.160781
201.475614	6394.749969	26.165799
201.883477	6406.805734	26.170816
202.176387	6398.012805	26.175834
202.146906	6407.925158	26.180852
202.310546	6426.960602	26.185869
202.202342	6429.817330	26.190887
202.665106	6422.473258	26.195904
202.521972	6434.097626	26.200922
202.588446	6448.262848	26.205940
203.153709	6452.431525	26.210957
202.942090	6472.148385	26.215975
203.399708	6484.871320	26.220992
203.773829	6486.732237	26.226010
203.882569	6500.640584	26.231028
203.990333	6523.387540	26.236045
204.304487	6502.038437	26.241063
204.701772	6541.174635	26.246080
204.768584	6545.017618	26.251098
204.879525	6544.552352	26.256116
205.174675	6553.228191	26.261133
205.220025	6571.190656	26.266151
205.607347	6582.496910	26.271168
205.880672	6576.407163	26.276186
205.720615	6616.120199	26.281204
206.246575	6596.451554	26.286221
206.459558	6630.273679	26.291239
206.954002	6627.696182	26.296256
206.942847	6624.559645	26.301274
206.885900	6649.101696	26.306292
207.556787	6651.493600	26.311309
207.308789	6662.536922	26.316327
207.777006	6660.451395	26.321344
208.100427	6676.593143	26.326362
207.896117	6680.317307	26.331380
208.373003	6688.405651	26.336397
208.337187	6718.954565	26.341415
208.578450	6720.974378	26.346432
208.681664	6716.276736	26.351450
208.978804	6744.029949	26.356468
209.377501	6741.798140	26.361485
209.736968	6760.981394	26.366503
209.822279	6766.237673	26.371520
209.907642	6767.736326	26.376538
209.892102	6782.283151	26.381556
210.685899	6791.051945	26.386573
210.718876	6798.325995	26.391591
211.126403	6806.028928	26.396608
211.412929	6789.767948	26.401626
211.453025	6834.094767	26.406644
211.907873	6832.661224	26.411661
211.508028	6823.530015	26.416679
212.000904	6839.304255	26.421696
212.360708	6854.309016	26.426714
212.147713	6849.103915	26.431732
212.293951	6856.499985	26.436749
212.498472	6888.441295	26.441767
212.814722	6874.988214	26.446784
213.077475	6909.471805	26.451802
212.953992	6888.851232	26.456820
213.680999	6909.298664	26.461837
213.715348	6887.509744	26.466855
213.783735	6917.186441	26.471872
213.929085	6903.851057	26.476890
214.357858	6930.899141	26.481908
214.002476	6937.800865	26.486925
214.210117	6956.432654	26.491943
214.589944	6960.735682	26.496960
215.257250	6998.053493	26.501978
215.185376	6997.367946	26.506996
215.485780	6994.439730	26.512013
215.610185	7015.296510	26.517031
215.892363	7030.170628	26.522048
216.285729	7036.049025	26.527066
216.702911	7047.549934	26.532084
216.862451	7050.747265	26.537101
216.933534	7055.488210	26.542119
217.020431	7084.110357	26.547136
217.470318	7074.276263	26.552154
217.273916	7090.531226	26.557172
217.839679	7094.039896	26.562189
218.058419	7105.677914	26.567207
218.235038	7118.574438	26.572224
218.351572	7114.560628	26.577242
218.459254	7139.905738	26.582260
218.609659	7144.681275	26.587277
218.813336	7170.556381	26.592295
218.880672	7189.564098	26.597312
219.697981	7186.099467	26.602330
219.476258	7201.460857	26.607348
219.963764	7192.296545	26.612365
220.097454	7227.306571	26.617383
220.098841	7245.647443	26.622400
220.814857	7233.741673	26.627418
221.202990	7250.024011	26.632436
221.520472	7248.229160	26.637453
221.568436	7256.107666	26.642471
221.928754	7259.334407	26.647488
222.246071	7238.165496	26.652506
221.853066	7261.556758	26.657524
222.401069	7283.418009	26.662541
222.667797	7277.561922	26.667559
222.264039	7276.762465	26.672576
222.496080	7298.928241	26.677594
222.789469	7317.694734	26.682612
223.202329	7332.096703	26.687629
223.183532	7338.084196	26.692647
223.397410	7352.195315	26.697664
224.070763	7363.248860	26.702682
223.865198	7362.704200	26.707700
224.161009	7393.753976	26.712717
224.556905	7383.567929	26.717735
224.469461	7418.733252	26.722752
225.161316	7404.215070	26.727770
225.077439	7421.707412	26.732788
225.336609	7442.033460	26.737805
225.561436	7437.108488	26.742823
225.703706	7455.448405	26.747840
226.414658	7447.581959	26.752858
226.038216	7475.302292	26.757876
226.426715	7473.880056	26.762893
226.443362	7470.326621	26.767911
226.723485	7494.485880	26.772928
227.298364	7508.781940	26.777946
227.580757	7513.556227	26.782964
228.040850	7507.942250	26.787981
228.081587	7528.002674	26.792999
228.165220	7537.047207	26.798016
229.023609	7533.996897	26.803034
228.874056	7540.582835	26.808052
228.957581	7526.483312	26.813069
229.398694	7532.458158	26.818087
229.198124	7580.764351	26.823104
229.577919	7561.875438	26.828122
229.372718	7560.764207	26.833140
229.571207	7593.302829	26.838157
230.138035	7592.825448	26.843175
230.189997	7606.921705	26.848192
230.640058	7627.562991	26.853210
230.448437	7625.503049	26.858228
230.754912	7674.771255	26.863245
231.364014	7655.642672	26.868263
231.457612	7701.119388	26.873280
231.836409	7683.751405	26.878298
231.613724	7700.538393	26.883316
232.553345	7713.075405	26.888333
232.870249	7710.972158	26.893351
232.361593	7720.613207	26.898368
233.007264	7735.648045	26.903386
233.253104	7740.617070	26.908404
233.297822	7748.515240	26.913421
233.936562	7767.924381	26.918439
233.774834	7772.092877	26.923456
233.933847	7778.574656	26.928474
234.182989	7798.173405	26.933492
234.521104	7800.743659	26.938509
234.726480	7815.497838	26.943527
235.189070	7822.088611	26.948544
235.757869	7816.209343	26.953562
235.660995	7817.806393	26.958580
235.859954	7839.832689	26.963597
235.889089	7851.712388	26.968615
236.049543	7851.107791	26.973632
236.414724	7865.431330	26.978650
236.430928	7872.366310	26.983668
236.825605	7903.343956	26.988685
236.942903	7906.785043	26.993703
237.216745	7919.641589	26.998720
237.606272	7925.299857	27.003738
237.392313	7943.575201	27.008756
237.433910	7941.480400	27.013773
238.034209	7965.183384	27.018791
238.000631	7973.932133	27.023808
238.120451	7990.729372	27.028826
238.669676	8010.847090	27.033844
239.015418	8015.375392	27.038861
239.386410	8034.403457	27.043879
239.483897	8047.007323	27.048896
239.647135	8053.232040	27.053914
239.929862	8062.450523	27.058932
240.575903	8072.075336	27.063949
240.597634	8089.040968	27.068967
240.686308	8101.504261	27.073984
241.019693	8117.400501	27.079002
241.454864	8111.584909	27.084020
241.645784	8127.402366	27.089037
241.906794	8136.404828	27.094055
242.304716	8148.997087	27.099072
242.846124	8152.766412	27.104090
242.698366	8155.382704	27.109108
242.762508	8154.712403	27.114125
242.892797	8174.059918	27.119143
243.011103	8188.250802	27.124160
243.582706	8186.763910	27.129178
243.671717	8204.853582	27.134196
243.788221	8226.684294	27.139213
244.356330	8239.085838	27.144231
244.419082	8245.431304	27.149248
244.559353	8272.969250	27.154266
244.763840	8271.918556	27.159284
244.845760	8282.350248	27.164301
245.308726	8300.695957	27.169319
245.508112	8312.284504	27.174336
245.706944	8327.166131	27.179354
246.011054	8340.815301	27.184372
246.356150	8356.167002	27.189389
246.786540	8353.941714	27.194407
246.602351	8374.940868	27.199424
247.109754	8392.223646	27.204442
247.456445	8390.440532	27.209460
247.609002	8417.773779	27.214477
248.034536	8415.550044	27.219495
248.061114	8430.082325	27.224512
248.507448	8435.608986	27.229530
248.563562	8452.014815	27.234548
248.735666	8459.549199	27.239565
249.010595	8467.116770	27.244583
249.153520	8490.640916	27.249600
249.609838	8506.813840	27.254618
249.594963	8517.896911	27.259636
250.009257	8537.622176	27.264653
250.378551	8542.094167	27.269671
250.418490	8548.653492	27.274688
250.547186	8565.519209	27.279706
250.943277	8564.975385	27.284724
251.246097	8581.824382	27.289741
252.025454	8592.001127	27.294759
252.225673	8607.251855	27.299776
252.475431	8603.887611	27.304794
252.644890	8599.486484	27.309812
252.648525	8624.241674	27.314829
252.821027	8628.726961	27.319847
252.757909	8625.786346	27.324864
253.401780	8649.840721	27.329882
253.566291	8661.527950	27.334900
253.498798	8670.122778	27.339917
254.151926	8680.156821	27.344935
253.801776	8704.735621	27.349952
254.121088	8717.466794	27.354970
254.556695	8720.874646	27.359988
254.833531	8746.430808	27.365005
255.103609	8767.503678	27.370023
255.667134	8769.747820	27.375040
255.855719	8789.136416	27.380058
255.917449	8783.541401	27.385076
256.166616	8805.624862	27.390093
256.499205	8803.157791	27.395111
256.759245	8833.309793	27.400128
256.804839	8848.483119	27.405146
257.228834	8857.226337	27.410164
257.161068	8879.729471	27.415181
257.587039	8883.027947	27.420199
257.651216	8900.722686	27.425216
258.185188	8912.174961	27.430234
258.593613	8927.336961	27.435252
258.221759	8950.424933	27.440269
259.261368	8959.012645	27.445287
259.452715	8970.545151	27.450304
259.866889	8986.818955	27.455322
260.182692	8991.393250	27.460340
260.359735	8991.469380	27.465357
260.714349	9009.639269	27.470375
260.949537	9025.920399	27.475392
261.294248	9022.285189	27.480410
261.765436	9030.719609	27.485428
261.412153	9045.289035	27.490445
262.061259	9044.300013	27.495463
262.226760	9072.910310	27.500480
262.154547	9078.834622	27.505498
262.762610	9081.135454	27.510516
263.094733	9092.897422	27.515533
263.283047	9102.898430	27.520551
263.480715	9108.543276	27.525568
263.835146	9114.733638	27.530586
264.088168	9131.000237	27.535604
264.143107	9127.110200	27.540621
264.709908	9145.311354	27.545639
264.771687	9158.056413	27.550656
264.907960	9161.010432	27.555674
265.222269	9170.320966	27.560692
265.215362	9177.920052	27.565709
265.662302	9189.982097	27.570727
265.859025	9194.610059	27.575744
266.231928	9218.226569	27.580762
266.261649	9234.140537	27.585780
266.284767	9253.922414	27.590797
266.568483	9244.552091	27.595815
266.871368	9273.633082	27.600832
266.673225	9282.599651	27.605850
267.437972	9292.965708	27.610868
267.519296	9319.050158	27.615885
268.016808	9336.720806	27.620903
268.259719	9357.276334	27.625920
268.466275	9371.555790	27.630938
268.879949	9370.224985	27.635956
269.000335	9397.257866	27.640973
269.264131	9421.758870	27.645991
269.709650	9431.087607	27.651008
269.849946	9440.226958	27.656026
270.230077	9466.410011	27.661044
270.236141	9483.807019	27.666061
270.866433	9500.347148	27.671079
271.084319	9529.374510	27.676096
271.322528	9515.336985	27.681114
271.590927	9552.508010	27.686132
271.837383	9546.838808	27.691149
272.081509	9555.746065	27.696167
272.364607	9585.374971	27.701184
272.611333	9600.163282	27.706202
273.169852	9605.199564	27.711220
273.541224	9621.351437	27.716237
273.635084	9630.902390	27.721255
273.793702	9650.331113	27.726272
274.132991	9668.462541	27.731290
274.418151	9680.247805	27.736308
274.457595	9681.432615	27.741325
274.916021	9706.822194	27.746343
275.317310	9730.425547	27.751360
275.738936	9739.170845	27.756378
276.267448	9740.602712	27.761396
276.525264	9743.507966	27.766413
276.753316	9758.375349	27.771431
276.873616	9764.686321	27.776448
277.004622	9779.322490	27.781466
277.532630	9786.435686	27.786484
277.456240	9806.039386	27.791501
277.721622	9810.984355	27.796519
278.133557	9828.289139	27.801536
277.782038	9838.891335	27.806554
278.243660	9857.003102	27.811572
278.551902	9886.602628	27.816589
278.995717	9891.199296	27.821607
279.222659	9896.709144	27.826624
279.262137	9940.800562	27.831642
279.884002	9933.357035	27.836660
279.800738	9944.965146	27.841677
279.854164	9967.922762	27.846695
280.538847	9972.080512	27.851712
280.544147	10005.365009	27.856730
281.331501	10008.604570	27.861748
281.772316	10020.216955	27.866765
281.792455	10026.109215	27.871783
282.137768	10051.101115	27.876800
281.995228	10048.196092	27.881818
282.751497	10092.412549	27.886836
283.039520	10075.342327	27.891853
283.214990	10118.350608	27.896871
284.080060	10092.230963	27.901888
284.012082	10138.359393	27.906906
284.545534	10112.721059	27.911924
284.619837	10151.915880	27.916941
284.789950	10135.540766	27.921959
285.228471	10169.056407	27.926976
285.225178	10167.496101	27.931994
285.582430	10184.230817	27.937012
285.757357	10207.203273	27.942029
285.721537	10224.242276	27.947047
286.708650	10197.336899	27.952064
286.690089	10260.641334	27.957082
286.980993	10249.037044	27.962100
287.189910	10264.697296	27.967117
287.439965	10270.802473	27.972135
287.539752	10293.482092	27.977152
287.746474	10317.378653	27.982170
288.258483	10325.479538	27.987188
288.509493	10351.006756	27.992205
288.667644	10366.264805	27.997223
289.189093	10387.070499	28.002240
289.225966	10395.840912	28.007258
289.486813	10419.967460	28.012276
290.056527	10441.293589	28.017293
290.260068	10457.742652	28.022311
290.501231	10461.373530	28.027328
290.524013	10498.859127	28.032346
290.888702	10485.938496	28.037364
291.479290	10518.604367	28.042381
291.836411	10550.294687	28.047399
292.070273	10547.809235	28.052416
292.179566	10583.096230	28.057434
292.494753	10589.952554	28.062452
292.940859	10610.788273	28.067469
293.082277	10624.404871	28.072487
293.605378	10637.825682	28.077504
293.658703	10669.540670	28.082522
294.567273	10672.128728	28.087540
294.525970	10690.109177	28.092557
294.559193	10701.956254	28.097575
294.953992	10703.575979	28.102592
295.282370	10732.189063	28.107610
295.783263	10732.630693	28.112628
295.670973	10730.512023	28.117645
295.965224	10759.283665	28.122663
296.658655	10741.724682	28.127680
296.508255	10794.893639	28.132698
296.342751	10788.707262	28.137716
297.200947	10784.183142	28.142733
297.073377	10848.175570	28.147751
297.819661	10836.467561	28.152768
298.043478	10849.218531	28.157786
298.352558	10883.761774	28.162804
298.751317	10895.355574	28.167821
298.904266	10909.922455	28.172839
299.602267	10906.330050	28.177856
299.321361	10948.560739	28.182874
300.168255	10951.369200	28.187892
300.356189	10959.575991	28.192909
300.523744	10990.068170	28.197927
300.842884	11006.922814	28.202944
301.231443	11025.391166	28.207962
301.087553	11015.908461	28.212980
301.457026	11043.655403	28.217997
301.698466	11068.994126	28.223015
302.119070	11078.194080	28.228032
302.140081	11118.367920	28.233050
302.761325	11125.535766	28.238068
303.262727	11148.572926	28.243085
303.551979	11164.078080	28.248103
304.066546	11175.765001	28.253120
304.349145	11185.395471	28.258138
304.779313	11207.122695	28.263156
305.131594	11217.972169	28.268173
305.046776	11240.504380	28.273191
305.581742	11237.250718	28.278208
305.430979	11256.586804	28.283226
305.980831	11265.152017	28.288244
306.324353	11286.823121	28.293261
306.368882	11306.096666	28.298279
306.692792	11331.705225	28.303296
307.081371	11352.625910	28.308314
307.480626	11358.600722	28.313332
307.669320	11401.271164	28.318349
308.057360	11408.281527	28.323367
308.781352	11416.942243	28.328384
308.748538	11447.833243	28.333402
309.185740	11451.561012	28.338420
309.664215	11444.313539	28.343437
309.539622	11482.914303	28.348455
310.088298	11494.515369	28.353472
310.377996	11513.052413	28.358490
310.683691	11517.172631	28.363508
310.899256	11544.917087	28.368525
311.173455	11557.478433	28.373543
311.669084	11570.899741	28.378560
311.751172	11594.648984	28.383578
311.857261	11595.537635	28.388596
312.690869	11616.146541	28.393613
312.299283	11632.074311	28.398631
312.785011	11648.227857	28.403648
313.136776	11661.121253	28.408666
313.487655	11672.902336	28.413684
313.942050	11704.619332	28.418701
313.820424	11730.125638	28.423719
314.945967	11727.047709	28.428736
314.803205	11735.472510	28.433754
314.673771	11771.582250	28.438772
315.291614	11772.945001	28.443789
315.500600	11800.849957	28.448807
315.776092	11809.011384	28.453824
316.165501	11845.905142	28.458842
316.462052	11857.762713	28.463860
316.956646	11872.782538	28.468877
317.014838	11911.875106	28.473895
317.542397	11917.464507	28.478912
317.899336	11929.903974	28.483930
318.353446	11953.483520	28.488948
319.018304	11970.803599	28.493965
319.165792	11994.910992	28.498983
319.338161	11997.281344	28.504000
319.795671	12009.578134	28.509018
320.347730	12033.309050	28.514036
320.301832	12037.371323	28.519053
320.624315	12060.288069	28.524071
321.137687	12055.476174	28.529088
321.293700	12088.769587	28.534106
321.333072	12107.274060	28.539124
321.761420	12120.798274	28.544141
322.218624	12137.255578	28.549159
322.738746	12152.917787	28.554176
322.860920	12172.417754	28.559194
323.253890	12192.901306	28.564212
323.331170	12209.215782	28.569229
323.587427	12234.270368	28.574247
324.385970	12239.375167	28.579264
324.527289	12255.651940	28.584282
324.983244	12270.333392	28.589300
325.550449	12279.744088	28.594317
325.528984	12300.804635	28.599335
325.771840	12310.567501	28.604352
325.970510	12334.485468	28.609370
326.119042	12358.253263	28.614388
326.451858	12372.902296	28.619405
326.460943	12411.517180	28.624423
327.340889	12411.173185	28.629440
327.855348	12431.765403	28.634458
327.788164	12461.935912	28.639476
328.082035	12480.352665	28.644493
328.192689	12508.721655	28.649511
328.569699	12514.123355	28.654528
329.245091	12540.118911	28.659546
329.395315	12558.873482	28.664564
330.282313	12561.381707	28.669581
330.388244	12576.037186	28.674599
330.641390	12596.005404	28.679616
331.161460	12600.749954	28.684634
331.102625	12618.269735	28.689652
331.816145	12638.083378	28.694669
331.973554	12644.728289	28.699687
332.229623	12654.134889	28.704704
332.209943	12689.677975	28.709722
332.508519	12702.208844	28.714740
333.054524	12720.464106	28.719757
332.881822	12753.350133	28.724775
333.354548	12761.085136	28.729792
333.513163	12785.550139	28.734810
333.662708	12815.164383	28.739828
334.555187	12833.968856	28.744845
334.927731	12854.760575	28.749863
335.296096	12889.252917	28.754880
335.729786	12908.260858	28.759898
335.964864	12923.699322	28.764916
336.387264	12943.855707	28.769933
336.831949	12967.083754	28.774951
337.074933	12982.824640	28.779968
337.283593	13011.281471	28.784986
337.431008	13037.989931	28.790004
337.964188	13056.064642	28.795021
338.545324	13075.152014	28.800039
338.465066	13094.430406	28.805056
338.952124	13125.912002	28.810074
339.083736	13158.151029	28.815092
339.885609	13171.863815	28.820109
339.801597	13194.372629	28.825127
340.326838	13213.440747	28.830144
340.952119	13245.470432	28.835162
341.363179	13264.416705	28.840180
341.883587	13268.713744	28.845197
342.204842	13297.260413	28.850215
342.470861	13301.445695	28.855232
342.822444	13325.792269	28.860250
343.039046	13358.193309	28.865268
343.595915	13342.867263	28.870285
343.475903	13392.905806	28.875303
343.973210	13403.976378	28.880320
344.558610	13410.506195	28.885338
344.329498	13431.838322	28.890356
344.700858	13452.011783	28.895373
345.349754	13475.310000	28.900391
345.766625	13496.523534	28.905408
346.009122	13509.344619	28.910426
346.225888	13548.874241	28.915444
346.882769	13557.628762	28.920461
347.171436	13579.087370	28.925479
347.302954	13586.923613	28.930496
347.882800	13601.891633	28.935514
347.757611	13640.123696	28.940532
348.324817	13654.598677	28.945549
348.246516	13661.081270	28.950567
348.848464	13680.634632	28.955584
349.243818	13691.490047	28.960602
349.010712	13750.787561	28.965620
349.913402	13753.056966	28.970637
350.147729	13777.041974	28.975655
350.404892	13803.265746	28.980672
351.150841	13810.949684	28.985690
351.381689	13847.577227	28.990708
351.878181	13859.930518	28.995725
352.379588	13875.891499	29.000743
352.402286	13898.802617	29.005760
352.900188	13921.304787	29.010778
353.240599	13940.519772	29.015796
353.693993	13960.468504	29.020813
353.834610	13987.685655	29.025831
354.012055	14002.083063	29.030848
354.907432	14017.941958	29.035866
355.063204	14049.215058	29.040884
354.903540	14068.447117	29.045901
355.008327	14087.326331	29.050919
355.322984	14117.327301	29.055936
355.967821	14139.489156	29.060954
356.579238	14175.452406	29.065972
357.048980	14198.895407	29.070989
357.189072	14217.089245	29.076007
357.292779	14246.204090	29.081024
358.277499	14274.095488	29.086042
358.675539	14290.750239	29.091060
359.485986	14311.308379	29.096077
359.870655	14321.211512	29.101095
360.205555	14332.839884	29.106112
360.311669	14350.944149	29.111130
360.713285	14391.663956	29.116148
361.278412	14371.307916	29.121165
361.429539	14417.001191	29.126183
361.518135	14422.350454	29.131200
361.833548	14434.037997	29.136218
361.944146	14463.772253	29.141236
362.296208	14504.669600	29.146253
362.784279	14511.425781	29.151271
363.102900	14539.135186	29.156288
363.369410	14564.747732	29.161306
363.553129	14595.449844	29.166324
364.149556	14613.655668	29.171341
364.759356	14647.217321	29.176359
364.601825	14677.938059	29.181376
365.302228	14695.809589	29.186394
365.578627	14726.095435	29.191412
365.978805	14745.688522	29.196429
366.534487	14769.151277	29.201447
366.872835	14787.864648	29.206464
367.451571	14804.651461	29.211482
367.643030	14826.092779	29.216500
368.123249	14833.723157	29.221517
368.406245	14852.797007	29.226535
368.640608	14875.553158	29.231552
368.849724	14878.841098	29.236570
369.387977	14899.255762	29.241588
369.600858	14925.089510	29.246605
370.419083	14935.196624	29.251623
370.445016	14960.582392	29.256640
370.579664	14978.452991	29.261658
370.953691	15005.759338	29.266676
371.075828	15026.619811	29.271693
371.398751	15062.582122	29.276711
371.397500	15094.768973	29.281728
372.103197	15119.413552	29.286746
372.562640	15148.722976	29.291764
372.842546	15174.949713	29.296781
373.260682	15211.582961	29.301799
373.428935	15246.091866	29.306816
374.349264	15255.057309	29.311834
375.201405	15282.603049	29.316852
376.214500	15292.277479	29.321869
376.885605	15307.964363	29.326887
376.969582	15317.873452	29.331904
377.462778	15316.948495	29.336922
377.592571	15337.274733	29.341940
377.633927	15352.805966	29.346957
378.052720	15367.588255	29.351975
378.489966	15381.434171	29.356992
378.480741	15391.313975	29.362010
378.674250	15417.043890	29.367028
379.288913	15442.119078	29.372045
379.891268	15457.595370	29.377063
379.469442	15482.191631	29.382080
379.825348	15502.603785	29.387098
380.250407	15532.468122	29.392116
380.538971	15567.712549	29.397133
381.338115	15590.870414	29.402151
381.531247	15625.776715	29.407168
381.856184	15645.218906	29.412186
382.331820	15681.985133	29.417204
382.823393	15701.975134	29.422221
383.072852	15726.467578	29.427239
382.864141	15758.551307	29.432256
383.765034	15781.100752	29.437274
384.198169	15823.315798	29.442292
384.551831	15854.518546	29.447309
384.770611	15878.824035	29.452327
385.169305	15905.671750	29.457344
385.763730	15941.804831	29.462362
386.040008	15964.977299	29.467380
386.199231	15986.173261	29.472397
386.901645	15999.950425	29.477415
387.500500	16031.841297	29.482432
388.141728	16036.385193	29.487450
388.617958	16066.145486	29.492468
388.588703	16087.947793	29.497485
389.018130	16107.554500	29.502503
389.359565	16124.141254	29.507520
389.567751	16157.140508	29.512538
390.218407	16168.297508	29.517556
390.137152	16192.729632	29.522573
390.699811	16210.698697	29.527591
390.788672	16243.931089	29.532608
390.998018	16278.861777	29.537626
391.608587	16297.948119	29.542644
391.721537	16326.619850	29.547661
392.593703	16358.397786	29.552679
392.992082	16398.044000	29.557696
393.655776	16409.126080	29.562714
394.112062	16439.657572	29.567732
394.479788	16459.423060	29.572749
395.317256	16483.610852	29.577767
394.958971	16503.986880	29.582784
395.317597	16526.488713	29.587802
396.188742	16545.109894	29.592820
396.283906	16579.854865	29.597837
396.826063	16594.533659	29.602855
396.962392	16618.502524	29.607872
397.459621	16643.522813	29.612890
397.744383	16673.534937	29.617908
398.335769	16706.994612	29.622925
398.595699	16721.812381	29.627943
399.050719	16760.431162	29.632960
399.232126	16777.524368	29.637978
399.824657	16805.573410	29.642996
400.044746	16840.223089	29.648013
400.752918	16863.818977	29.653031
401.098841	16893.309450	29.658048
401.474819	16915.343991	29.663066
402.141508	16950.209534	29.668084
401.839225	16970.471163	29.673101
402.850164	16991.104217	29.678119
403.149953	17037.679131	29.683136
403.554818	17058.951297	29.688154
403.889335	17081.165101	29.693172
404.276792	17103.020545	29.698189
405.017373	17120.544269	29.703207
405.107241	17153.498671	29.708224
405.531707	17181.937931	29.713242
406.010151	17207.217025	29.718260
405.984700	17244.136603	29.723277
406.945542	17253.502254	29.728295
407.084192	17282.571034	29.733312
407.231929	17313.842523	29.738330
408.114860	17341.758882	29.743348
408.410827	17370.802370	29.748365
409.164028	17395.042032	29.753383
409.078866	17429.064570	29.758400
409.521770	17445.559427	29.763418
410.136084	17457.879352	29.768436
409.965768	17475.955662	29.773453
410.639368	17518.848400	29.778471
411.144057	17553.533856	29.783488
411.683311	17565.338117	29.788506
411.991070	17591.271753	29.793524
412.076596	17609.928073	29.798541
412.674589	17637.166807	29.803559
412.901099	17665.808958	29.808576
413.202429	17690.431096	29.813594
413.485982	17714.960837	29.818612
413.970762	17747.886654	29.823629
414.756085	17770.194181	29.828647
414.819886	17805.798220	29.833664
415.267986	17853.765839	29.838682
415.837056	17869.563931	29.843700
415.913904	17895.229375	29.848717
416.466403	17947.198297	29.853735
416.626719	17979.087001	29.858752
417.305730	17999.093042	29.863770
417.859945	18026.354792	29.868788
418.432989	18082.837170	29.873805
419.026081	18110.177515	29.878823
419.408680	18114.891196	29.883840
419.706250	18169.808417	29.888858
420.430723	18192.218766	29.893876
420.543108	18213.190518	29.898893
421.264644	18237.601703	29.903911
421.538972	18250.335079	29.908928
422.184106	18279.935839	29.913946
422.787070	18305.860056	29.918964
423.161430	18347.648880	29.923981
423.463492	18365.056892	29.928999
423.937256	18387.704313	29.934016
423.840774	18413.065368	29.939034
424.493096	18446.536827	29.944052
425.022686	18474.298551	29.949069
425.606566	18497.212832	29.954087
425.863926	18523.383810	29.959104
426.377167	18558.722898	29.964122
427.114615	18576.277919	29.969140
427.136489	18604.155017	29.974157
427.674990	18628.262131	29.979175
428.221657	18648.600726	29.984192
428.442496	18690.795635	29.989210
429.111323	18698.067793	29.994228
429.193315	18722.098574	29.999245
429.538504	18755.280662	30.004263
429.908729	18777.562871	30.009280
430.402153	18811.007679	30.014298
430.916769	18839.377951	30.019316
431.153417	18884.659434	30.024333
431.525208	18910.720314	30.029351
432.394450	18930.147652	30.034368
432.559945	18957.909590	30.039386
433.004272	18988.346849	30.044404
433.374186	19000.057342	30.049421
433.367294	19045.720615	30.054439
434.291481	19064.243299	30.059456
434.230572	19093.448254	30.064474
435.155827	19120.192578	30.069492
435.525294	19136.276135	30.074509
435.696305	19160.602864	30.079527
435.945844	19194.970439	30.084544
436.354029	19240.865798	30.089562
436.950018	19259.030759	30.094580
437.337484	19297.003434	30.099597
437.798599	19327.835938	30.104615
438.391915	19357.434415	30.109632
438.601119	19393.939623	30.114650
439.414384	19419.610542	30.119668
439.559011	19465.489102	30.124685
440.390848	19486.375513	30.129703
440.661442	19519.578204	30.134720
441.015112	19551.019628	30.139738
441.369459	19580.206977	30.144756
441.930227	19618.594579	30.149773
442.286156	19645.390353	30.154791
443.117518	19676.855146	30.159808
443.295837	19720.846716	30.164826
444.077360	19744.273510	30.169844
444.413474	19780.211737	30.174861
444.541161	19811.214073	30.179879
445.148187	19838.520996	30.184896
445.723764	19866.785790	30.189914
445.960036	19896.708334	30.194932
446.114332	19932.865655	30.199949
446.640570	19962.159414	30.204967
447.229980	20002.656138	30.209984
447.519914	20042.216355	30.215002
447.885193	20057.327054	30.220020
448.364553	20108.504565	30.225037
448.711884	20153.271275	30.230055
450.079290	20178.783905	30.235072
449.964057	20199.348890	30.240090
450.883839	20240.706667	30.245108
451.018941	20272.776150	30.250125
451.551811	20294.511742	30.255143
452.066675	20332.470582	30.260160
452.253609	20363.431501	30.265178
453.134390	20401.231417	30.270196
453.469315	20416.886722	30.275213
453.572556	20457.908185	30.280231
454.381581	20471.715796	30.285248
454.484977	20534.625047	30.290266
455.281154	20549.473857	30.295284
455.511182	20574.137912	30.300301
455.982885	20620.986370	30.305319
456.687102	20625.246790	30.310336
456.773041	20678.968248	30.315354
457.385777	20666.990259	30.320372
457.682722	20720.545159	30.325389
457.990033	20748.564099	30.330407
458.791069	20763.456441	30.335424
458.711596	20799.884530	30.340442
459.154360	20834.063889	30.345460
459.657792	20874.645478	30.350477
460.182499	20903.888094	30.355495
460.639151	20939.156553	30.360512
461.084201	20969.882644	30.365530
461.157531	21005.845078	30.370548
461.723129	21051.800223	30.375565
462.082258	21088.582395	30.380583
463.040955	21126.422844	30.385600
463.439686	21165.890213	30.390618
463.873674	21198.643214	30.395636
464.407924	21228.204649	30.400653
464.639979	21269.490432	30.405671
465.248522	21300.792398	30.410688
465.926361	21342.639739	30.415706
466.318350	21381.274736	30.420724
466.775942	21415.152953	30.425741
467.123797	21454.292091	30.430759
467.580021	21482.872968	30.435776
468.019724	21516.823557	30.440794
468.567498	21571.396696	30.445812
469.098710	21589.612896	30.450829
469.407542	21633.807588	30.455847
470.228640	21661.432085	30.460864
470.519936	21703.931833	30.465882
471.036585	21739.308697	30.470900
471.496019	21774.110396	30.475917
472.025402	21804.949910	30.480935
472.729202	21833.329752	30.485952
472.892820	21878.773690	30.490970
473.499133	21909.828756	30.495988
473.982746	21953.488533	30.501005
474.678074	21992.264149	30.506023
475.442194	22009.168683	30.511040
475.365122	22049.321274	30.516058
476.084457	22073.858942	30.521076
476.668403	22113.015665	30.526093
477.165317	22145.144745	30.531111
477.459789	22170.566949	30.536128
477.949259	22198.001077	30.541146
478.709291	22232.192009	30.546164
479.103584	22258.795557	30.551181
479.372477	22294.708519	30.556199
480.134160	22330.098872	30.561216
480.483877	22356.641955	30.566234
480.730382	22378.542231	30.571252
481.323204	22407.970153	30.576269
481.769028	22454.847502	30.581287
482.164616	22479.503535	30.586304
482.367268	22507.620257	30.591322
482.552070	22536.969289	30.596340
483.386447	22574.107284	30.601357
483.897246	22606.138221	30.606375
484.479415	22633.292138	30.611392
484.818596	22667.212394	30.616410
485.442311	22692.888579	30.621428
485.832304	22718.664256	30.626445
485.943042	22759.439285	30.631463
486.329663	22794.014624	30.636480
486.823915	22838.842378	30.641498
487.348335	22882.217056	30.646516
488.051715	22912.594696	30.651533
488.341937	22959.246298	30.656551
488.969136	22993.192260	30.661568
489.015718	23042.670255	30.666586
489.468543	23077.753127	30.671604
490.453792	23117.479297	30.676621
490.756060	23169.245139	30.681639
491.499282	23210.586113	30.686656
491.886037	23251.132564	30.691674
492.027191	23297.463932	30.696692
492.683859	23334.731269	30.701709
493.093914	23374.402425	30.706727
494.173862	23404.685586	30.711744
494.443141	23447.443216	30.716762
494.860191	23490.045888	30.721780
495.387968	23528.388062	30.726797
495.854165	23569.063659	30.731815
496.373013	23616.024187	30.736832
496.671688	23667.111710	30.741850
497.556815	23692.658092	30.746868
497.920296	23745.139118	30.751885
498.304986	23791.304750	30.756903
499.227478	23813.118240	30.761920
499.781839	23860.386532	30.766938
499.941299	23892.521727	30.771956
500.864456	23923.181364	30.776973
501.257106	23964.677036	30.781991
501.993214	23999.679021	30.787008
502.079519	24024.635632	30.792026
502.935882	24066.773686	30.797044
503.518111	24113.644464	30.802061
504.017992	24130.378347	30.807079
504.708407	24155.953346	30.812096
504.906179	24198.899253	30.817114
505.401231	24231.566127	30.822132
506.172206	24265.413941	30.827149
506.270524	24300.452808	30.832167
506.825561	24339.367603	30.837184
507.352326	24378.091653	30.842202
507.397538	24417.367472	30.847220
508.032442	24450.851395	30.852237
508.403530	24500.461834	30.857255
509.428113	24522.620803	30.862272
509.938809	24556.200351	30.867290
509.957229	24589.351113	30.872308
510.612883	24608.629330	30.877325
510.830896	24667.643648	30.882343
511.349078	24705.874408	30.887360
511.847634	24738.188881	30.892378
512.092865	24768.263397	30.897396
513.064539	24825.139393	30.902413
513.254939	24854.687173	30.907431
513.905469	24886.672902	30.912448
514.414150	24943.007874	30.917466
514.902896	24971.761608	30.922484
515.701286	25025.639567	30.927501
516.328839	25053.111008	30.932519
516.403462	25089.637063	30.937536
516.905497	25140.073061	30.942554
517.566597	25178.204209	30.947572
518.416148	25201.316787	30.952589
518.299117	25268.789252	30.957607
519.308593	25294.286122	30.962624
520.007804	25328.794353	30.967642
519.986522	25390.135426	30.972660
521.070389	25424.669247	30.977677
521.572304	25443.346725	30.982695
521.976090	25509.879417	30.987712
522.743473	25533.342715	30.992730
523.214104	25557.622930	30.997748
524.166915	25582.960716	31.002765
524.280612	25626.691902	31.007783
524.849446	25669.420395	31.012800
525.635386	25685.696796	31.017818
525.931355	25731.162195	31.022836
526.668141	25766.590199	31.027853
527.118044	25779.260367	31.032871
527.850029	25845.335706	31.037888
528.186828	25857.229115	31.042906
528.849929	25899.797477	31.047924
529.359177	25940.614080	31.052941
529.853778	25964.275075	31.057959
530.350722	25996.685313	31.062976
530.741898	26049.169521	31.067994
530.901718	26066.068322	31.073012
531.549844	26123.970221	31.078029
532.155707	26156.144437	31.083047
532.113906	26189.551529	31.088064
533.041300	26238.744754	31.093082
532.964941	26298.687190	31.098100
533.969275	26312.477913	31.103117
534.370424	26392.909381	31.108135
534.799710	26419.642741	31.113152
535.233939	26458.566199	31.118170
535.698743	26529.870490	31.123188
536.568198	26548.834197	31.128205
536.865661	26631.431654	31.133223
537.299370	26647.788777	31.138240
538.303020	26670.045471	31.143258
538.512227	26743.716970	31.148276
539.009713	26761.832642	31.153293
539.927268	26776.820855	31.158311
540.243775	26867.470094	31.163328
541.019286	26883.706844	31.168346
541.496393	26904.429594	31.173364
541.805921	26979.834322	31.178381
542.645936	26985.668219	31.183399
543.160816	27018.038279	31.188416
543.679068	27092.035571	31.193434
543.962744	27126.680836	31.198452
545.126182	27131.974046	31.203469
545.422928	27212.003191	31.208487
545.321775	27243.097086	31.213504
546.724992	27245.453775	31.218522
546.823216	27284.381543	31.223540
547.392251	27340.491604	31.228557
547.697540	27418.655645	31.233575
548.312717	27447.905784	31.238592
549.290753	27454.990213	31.243610
549.562007	27523.235160	31.248628
550.435469	27595.307887	31.253645
550.502120	27605.826739	31.258663
551.299052	27632.747797	31.263680
552.219941	27712.925039	31.268698
552.509400	27725.310324	31.273716
553.387827	27775.132944	31.278733
553.695393	27804.364183	31.283751
554.324757	27868.740401	31.288768
555.226009	27871.701059	31.293786
554.917620	27946.193978	31.298804
556.080449	27951.331575	31.303821
556.361250	28027.276791	31.308839
556.756054	28044.876103	31.313856
557.267929	28117.556315	31.318874
557.994694	28151.230330	31.323892
558.625955	28195.547874	31.328909
559.360016	28257.538294	31.333927
559.567896	28289.005703	31.338944
560.429829	28331.915997	31.343962
560.766504	28381.030239	31.348980
561.479408	28414.826769	31.353997
561.912391	28459.472857	31.359015
562.457572	28535.844776	31.364032
563.350047	28533.740907	31.369050
563.707568	28612.782469	31.374068
564.138324	28633.755137	31.379085
564.573439	28683.796928	31.384103
565.321329	28731.039332	31.389120
565.725460	28770.219783	31.394138
566.129428	28833.021355	31.399156
566.657771	28878.353061	31.404173
567.561460	28893.743363	31.409191
568.061456	28972.195128	31.414208
568.836811	29004.917708	31.419226
568.839582	29048.275596	31.424244
569.748517	29055.742068	31.429261
570.102802	29144.638686	31.434279
570.709763	29190.196692	31.439296
571.146071	29195.412591	31.444314
571.786663	29257.678590	31.449332
572.035917	29302.756524	31.454349
573.007493	29340.817391	31.459367
573.310384	29399.350985	31.464384
574.052826	29409.414336	31.469402
574.206989	29482.947142	31.474420
574.949403	29539.805455	31.479437
575.508209	29582.094457	31.484455
576.129314	29638.245964	31.489472
576.840985	29681.426456	31.494490
577.318090	29742.956057	31.499508
577.678605	29791.695717	31.504525
578.705977	29824.014216	31.509543
579.330535	29878.650007	31.514560
580.144915	29931.081021	31.519578
580.666099	29976.281410	31.524596
581.661330	30020.429371	31.529613
582.146446	30037.865186	31.534631
582.446372	30103.387761	31.539648
583.382115	30144.195153	31.544666
583.864097	30192.224844	31.549684
584.290772	30225.637365	31.554701
584.807410	30285.134511	31.559719
585.153669	30329.675060	31.564736
586.216617	30370.924511	31.569754
586.510246	30416.479124	31.574772
586.773829	30454.658511	31.579789
587.465369	30516.131670	31.584807
588.181297	30564.032219	31.589824
588.930362	30593.719033	31.594842
589.045966	30655.585444	31.599860
589.942220	30703.399376	31.604877
590.468924	30751.373161	31.609895
590.915201	30812.943233	31.614912
591.864207	30858.358462	31.619930
592.195253	30913.678013	31.624948
593.327165	30952.642234	31.629965
593.854680	31000.640264	31.634983
594.408746	31065.005694	31.640000
595.157073	31090.945804	31.645018
595.992284	31135.350797	31.650036
596.400048	31165.493313	31.655053
597.144675	31225.354736	31.660071
597.237873	31238.751884	31.665088
597.856511	31314.806798	31.670106
598.354204	31329.275919	31.675124
599.113605	31414.755586	31.680141
599.471336	31433.365266	31.685159
599.943564	31456.899191	31.690176
600.779485	31491.664417	31.695194
601.473131	31586.978926	31.700212
601.453195	31613.076884	31.705229
602.425504	31624.537651	31.710247
602.811894	31731.389796	31.715264
603.132485	31742.309820	31.720282
603.874608	31780.189143	31.725300
604.255666	31866.829939	31.730317
605.005418	31895.623804	31.735335
605.160712	31972.437999	31.740352
605.979921	32020.274361	31.745370
606.814716	32075.263864	31.750388
607.138881	32138.612562	31.755405
607.939602	32177.567833	31.760423
608.604000	32243.434963	31.765440
609.365070	32306.798270	31.770458
610.177870	32334.856277	31.775476
610.454629	32387.606182	31.780493
611.635165	32442.973720	31.785511
612.080562	32501.078054	31.790528
612.894499	32545.896908	31.795546
613.188548	32576.151544	31.800564
613.627391	32667.575689	31.805581
614.571558	32698.436294	31.810599
615.135330	32755.625842	31.815616
615.071497	32816.242822	31.820634
616.052401	32845.602070	31.825652
616.399122	32935.111558	31.830669
617.509327	32965.460762	31.835687
617.813907	33060.990783	31.840704
618.645526	33082.769102	31.845722
619.472655	33155.657985	31.850740
620.055092	33204.290502	31.855757
620.449717	33264.306516	31.860775
621.396773	33295.791964	31.865792
621.896147	33368.153931	31.870810
623.000812	33443.889109	31.875828
623.634926	33478.239884	31.880845
624.219626	33498.863292	31.885863
624.694375	33554.408437	31.890880
625.400860	33632.945816	31.895898
626.020642	33655.803681	31.900916
626.752561	33701.970676	31.905933
627.223512	33741.133486	31.910951
627.736469	33799.107111	31.915968
627.865587	33870.105293	31.920986
628.953292	33916.238301	31.926004
629.528631	33965.849905	31.931021
629.957092	34000.493025	31.936039
630.635919	34091.448631	31.941056
631.436890	34113.025129	31.946074
631.982417	34189.365055	31.951092
632.325661	34228.837818	31.956109
632.993270	34293.736895	31.961127
633.834069	34328.833650	31.966144
634.329539	34409.652985	31.971162
635.235443	34422.422043	31.976180
635.421622	34498.051365	31.981197
636.443370	34508.842667	31.986215
636.461610	34608.784191	31.991232
637.322967	34628.767528	31.996250
637.944198	34690.133504	32.001268
638.332654	34749.744459	32.006285
639.048107	34795.124222	32.011303
640.347864	34857.342775	32.016320
640.464890	34903.611034	32.021338
641.152043	34962.350750	32.026356
641.684592	35030.114838	32.031373
642.758871	35062.313269	32.036391
642.891013	35128.760605	32.041408
643.740793	35179.889615	32.046426
644.558317	35229.436486	32.051444
644.987497	35308.609224	32.056461
645.552655	35355.300797	32.061479
645.773494	35405.521745	32.066496
646.944952	35464.078922	32.071514
647.916596	35539.848020	32.076532
648.615600	35564.694822	32.081549
649.464189	35650.919988	32.086567
649.760435	35685.366976	32.091584
650.553284	35745.282841	32.096602
651.239366	35803.272156	32.101620
651.998768	35835.104466	32.106637
652.909971	35920.042549	32.111655
653.486952	35963.647231	32.116672
654.188136	35995.085542	32.121690
655.036866	36061.461906	32.126708
655.694337	36092.677196	32.131725
656.217839	36149.629479	32.136743
656.831219	36195.961022	32.141760
657.056952	36247.416538	32.146778
658.075375	36301.667250	32.151796
658.545879	36341.692303	32.156813
659.604666	36419.739032	32.161831
660.194861	36445.831002	32.166848
660.481525	36536.688996	32.171866
661.739110	36540.048632	32.176884
661.739288	36631.684262	32.181901
662.401157	36651.366007	32.186919
662.814464	36732.532877	32.191936
663.039870	36810.353093	32.196954
664.048933	36875.166874	32.201972
664.434003	36920.344902	32.206989
665.595974	36950.456708	32.212007
665.983043	37049.237898	32.217024
666.755752	37136.137084	32.222042
667.511494	37173.657674	32.227060
668.015976	37215.191347	32.232077
668.668621	37283.367979	32.237095
668.902956	37358.758211	32.242112
669.645225	37408.096504	32.247130
670.679144	37442.719754	32.252148
671.361439	37530.007454	32.257165
671.807328	37565.550729	32.262183
673.384202	37590.047938	32.267200
673.300984	37687.403661	32.272218
674.089880	37720.303826	32.277236
675.074675	37782.630749	32.282253
675.369478	37856.293470	32.287271
675.939720	37884.416851	32.292288
676.230836	37951.359327	32.297306
677.208251	38033.511636	32.302324
677.733834	38066.526931	32.307341
678.370946	38171.860630	32.312359
679.468161	38226.417215	32.317376
680.068573	38266.719440	32.322394
680.780734	38338.386381	32.327412
681.348596	38409.549984	32.332429
682.848850	38434.588830	32.337447
683.064105	38515.543563	32.342464
683.535359	38593.977753	32.347482
684.215558	38606.990961	32.352500
685.068972	38661.665033	32.357517
685.486900	38751.962234	32.362535
686.592045	38795.829186	32.367552
686.932037	38876.174511	32.372570
687.990667	38915.434062	32.377588
688.284837	39007.346418	32.382605
689.042202	39042.608284	32.387623
689.722233	39118.712759	32.392640
690.305824	39184.579200	32.397658
691.039789	39230.690205	32.402676
692.059624	39326.320317	32.407693
692.377534	39365.042904	32.412711
693.165533	39451.196310	32.417728
693.981254	39476.888119	32.422746
694.688460	39593.126214	32.427764
695.173733	39628.227637	32.432781
696.261139	39704.028632	32.437799
696.888597	39753.961303	32.442816
697.432273	39818.792707	32.447834
698.335897	39880.028638	32.452852
698.775189	39922.024024	32.457869
699.505050	40011.368435	32.462887
700.394926	40061.443147	32.467904
700.818828	40147.700631	32.472922
701.764290	40184.988003	32.477940
702.515232	40267.046880	32.482957
702.888800	40338.459242	32.487975
703.622088	40386.941968	32.492992
704.282526	40457.150150	32.498010
705.390901	40538.245143	32.503028
706.223268	40585.627760	32.508045
706.446450	40644.795504	32.513063
707.180014	40721.212443	32.518080
708.244312	40755.840826	32.523098
708.827314	40828.893430	32.528116
709.306138	40877.547375	32.533133
710.073716	40909.843729	32.538151
711.221332	40998.059232	32.543168
711.361986	41045.594252	32.548186
712.143079	41104.228494	32.553204
712.939193	41156.119078	32.558221
713.591415	41208.067420	32.563239
714.498291	41278.104132	32.568256
715.301133	41329.675627	32.573274
715.854426	41391.146238	32.578292
716.151252	41465.604900	32.583309
717.083443	41517.017594	32.588327
717.899030	41575.166982	32.593344
718.612122	41655.615844	32.598362
719.389787	41699.808965	32.603380
719.926878	41784.626360	32.608397
720.785486	41837.966225	32.613415
721.086775	41919.229388	32.618432
721.522249	41965.903131	32.623450
722.430243	42071.280947	32.628468
722.795259	42129.888746	32.633485
723.631455	42183.965003	32.638503
724.745923	42296.736069	32.643520
725.553334	42339.024175	32.648538
726.483206	42440.858702	32.653556
726.956320	42483.490564	32.658573
728.139131	42562.960513	32.663591
728.790857	42625.637389	32.668608
729.433496	42683.613052	32.673626
730.322629	42752.384330	32.678644
730.954535	42826.634689	32.683661
731.893822	42876.088418	32.688679
732.605645	42958.587525	32.693696
733.496287	43032.497931	32.698714
734.203129	43070.829502	32.703732
734.921105	43148.953592	32.708749
735.309625	43240.980943	32.713767
736.049691	43275.793808	32.718784
736.530048	43367.860840	32.723802
737.886156	43409.067475	32.728820
738.166277	43529.865238	32.733837
738.616239	43581.780418	32.738855
740.083122	43607.914202	32.743872
740.391794	43708.864652	32.748890
741.034893	43809.349229	32.753908
741.666872	43847.855320	32.758925
742.411819	43943.075547	32.763943
743.011716	43995.712544	32.768960
744.417836	44054.864598	32.773978
744.965933	44130.572333	32.778996
745.701633	44233.675443	32.784013
746.460492	44274.597537	32.789031
747.560189	44360.798579	32.794048
747.881562	44394.500576	32.799066
748.939547	44439.217620	32.804084
749.531066	44536.626371	32.809101
749.530828	44582.146297	32.814119
750.903469	44629.312132	32.819136
751.158645	44693.110104	32.824154
752.275525	44787.834132	32.829172
752.879566	44879.845353	32.834189
753.402110	44925.346051	32.839207
755.100430	44962.012948	32.844224
755.246974	45052.451208	32.849242
755.695855	45154.144859	32.854260
756.515369	45227.678491	32.859277
757.141854	45290.643506	32.864295
758.096083	45332.543338	32.869312
758.915502	45429.649516	32.874330
759.546486	45516.615479	32.879348
759.831506	45574.648299	32.884365
761.066629	45630.776049	32.889383
761.899763	45745.324258	32.894400
762.314477	45831.070629	32.899418
762.833119	45897.329641	32.904436
764.042051	45937.748661	32.909453
764.807073	46022.478005	32.914471
765.725461	46148.337835	32.919488
766.283488	46211.616783	32.924506
767.513908	46254.023813	32.929524
768.140963	46342.086089	32.934541
768.632479	46471.660045	32.939559
769.252356	46516.398547	32.944576
770.331877	46570.651705	32.949594
770.821409	46690.926989	32.954612
771.601351	46769.133223	32.959629
772.276435	46839.898224	32.964647
773.575864	46899.808909	32.969664
774.090360	47009.387133	32.974682
774.782978	47109.049960	32.979700
775.553517	47160.883778	32.984717
776.666441	47223.749941	32.989735
777.675761	47298.221204	32.994752
778.508372	47412.509080	32.999770
778.572288	47498.830570	33.004788
779.938570	47586.920257	33.009805
780.449338	47645.514005	33.014823
780.815514	47721.124300	33.019840
781.849050	47809.473149	33.024858
782.574180	47874.731843	33.029876
783.913737	47929.452643	33.034893
784.605435	48058.937033	33.039911
785.542939	48157.301606	33.044928
785.878758	48234.575403	33.049946
786.840900	48309.178357	33.054964
787.370849	48357.239364	33.059981
788.312511	48424.693210	33.064999
789.283873	48501.374802	33.070016
790.105954	48591.080118	33.075034
790.526226	48643.920638	33.080052
791.589900	48738.485214	33.085069
791.946574	48834.708922	33.090087
792.659002	48905.750800	33.095104
793.398615	48992.290729	33.100122
794.349686	49065.276808	33.105140
794.926102	49100.897270	33.110157
795.778902	49190.944674	33.115175
796.690641	49291.512640	33.120192
797.182722	49379.763056	33.125210
798.101892	49482.643826	33.130228
799.267879	49554.146225	33.135245
799.491104	49630.790867	33.140263
800.568089	49686.824250	33.145280
801.103493	49812.973183	33.150298
801.621802	49878.764451	33.155316
803.084366	49945.828800	33.160333
803.152174	50087.904148	33.165351
803.849930	50162.793664	33.170368
804.617473	50253.951845	33.175386
805.220574	50358.894924	33.180404
806.182600	50449.928487	33.185421
807.557276	50529.467268	33.190439
808.138067	50627.567840	33.195456
809.277635	50767.590966	33.200474
809.471685	50857.663304	33.205492
810.232758	50942.659893	33.210509
811.743999	51017.467708	33.215527
812.449917	51139.221958	33.220544
813.035081	51252.917603	33.225562
813.962461	51325.061533	33.230580
815.219211	51444.142487	33.235597
815.608626	51509.363849	33.240615
816.782759	51621.775219	33.245632
817.439805	51736.282998	33.250650
818.182582	51792.385673	33.255668
819.428583	51910.565721	33.260685
819.829551	51994.046699	33.265703
821.481168	52044.915128	33.270720
821.906297	52175.611177	33.275738
822.652302	52288.489354	33.280756
824.004001	52334.101264	33.285773
824.994968	52432.048610	33.290791
825.889996	52504.047800	33.295808
826.697779	52573.896179	33.300826
827.107021	52679.391823	33.305844
827.899520	52788.434387	33.310861
828.595589	52859.936460	33.315879
829.839585	52927.084679	33.320896
830.365995	53052.285818	33.325914
830.959819	53118.490421	33.330932
831.935352	53188.140904	33.335949
833.005165	53253.007823	33.340967
833.517004	53375.657105	33.345984
834.280728	53440.847995	33.351002
835.481958	53499.537324	33.356020
835.868759	53618.130449	33.361037
836.491512	53720.666148	33.366055
837.523309	53781.561108	33.371072
838.695369	53857.993908	33.376090
839.127855	53968.401242	33.381108
839.531502	54030.056654	33.386125
840.634240	54104.307963	33.391143
841.084038	54184.183746	33.396160
842.539626	54305.672828	33.401178
843.264281	54431.379057	33.406196
844.088063	54491.956011	33.411213
844.885672	54574.940765	33.416231
845.570276	54699.099163	33.421248
846.374781	54771.648909	33.426266
847.170666	54847.407170	33.431284
848.130911	54984.799270	33.436301
848.776738	55095.005900	33.441319
849.334256	55170.746627	33.446336
850.610178	55233.605625	33.451354
851.152872	55370.653596	33.456372
851.738041	55495.126796	33.461389
852.674400	55563.978283	33.466407
853.558657	55675.416225	33.471424
854.597194	55809.535111	33.476442
855.307803	55939.995077	33.481460
856.100972	56024.275011	33.486477
857.244610	56097.195890	33.491495
858.230346	56219.517475	33.496512
859.618600	56347.179937	33.501530
859.683149	56428.960859	33.506548
861.242559	56502.600034	33.511565
861.856884	56648.320621	33.516583
862.515155	56729.929483	33.521600
864.136055	56833.747525	33.526618
864.509675	56930.551559	33.531636
865.786373	57044.874286	33.536653
866.593535	57157.375239	33.541671
866.964425	57226.888033	33.546688
868.503056	57352.494299	33.551706
869.317980	57422.439100	33.556724
870.068103	57538.174548	33.561741
870.810483	57623.110747	33.566759
871.807762	57731.815706	33.571776
872.635861	57839.784267	33.576794
872.869522	57933.531588	33.581812
874.468183	58023.166556	33.586829
875.415841	58139.900339	33.591847
876.058800	58246.672702	33.596864
877.282163	58325.471125	33.601882
877.943053	58456.263087	33.606900
878.991828	58523.409348	33.611917
879.607372	58654.487741	33.616935
880.704625	58707.392025	33.621952
881.359096	58817.114501	33.626970
881.815720	58906.004167	33.631988
882.792197	58990.262208	33.637005
884.309257	59061.923120	33.642023
884.632251	59188.679297	33.647040
885.524698	59249.229483	33.652058
886.250864	59382.309652	33.657076
887.235916	59460.412066	33.662093
888.260027	59534.836822	33.667111
888.905500	59645.307557	33.672128
890.021528	59738.333207	33.677146
890.350963	59854.124822	33.682164
891.216590	59960.925294	33.687181
892.682135	60044.204173	33.692199
893.440195	60166.026154	33.697216
894.270281	60290.947393	33.702234
895.208011	60345.889773	33.707252
896.547321	60452.785028	33.712269
897.154135	60551.607345	33.717287
897.705889	60671.580530	33.722304
898.631727	60808.093247	33.727322
899.462351	60928.557301	33.732340
900.259647	61021.213823	33.737357
901.892306	61080.847049	33.742375
902.313202	61183.298584	33.747392
903.315935	61287.224192	33.752410
904.065592	61397.833960	33.757428
905.189756	61523.761763	33.762445
906.246938	61661.775397	33.767463
906.707840	61750.504270	33.772480
908.163916	61842.245386	33.777498
908.672167	61993.064233	33.782516
910.038274	62089.187791	33.787533
910.923920	62191.160386	33.792551
911.517654	62290.183402	33.797568
912.674075	62384.611460	33.802586
914.058223	62478.135403	33.807604
914.878374	62580.098424	33.812621
915.919486	62726.559716	33.817639
916.491322	62810.078370	33.822656
918.026308	62878.028160	33.827674
918.549696	63045.453142	33.832692
918.964312	63112.495779	33.837709
920.221270	63183.601299	33.842727
920.929040	63341.191534	33.847744
922.241343	63451.818572	33.852762
922.743419	63541.787181	33.857780
923.765964	63638.159615	33.862797
924.769681	63781.575077	33.867815
925.693807	63901.891691	33.872832
926.732777	63995.620177	33.877850
927.390422	64087.979262	33.882868
927.893218	64177.508661	33.887885
929.226920	64265.696783	33.892903
929.865500	64374.630056	33.897920
931.067707	64513.440411	33.902938
931.657333	64625.013511	33.907956
932.529845	64701.491353	33.912973
933.638887	64781.042532	33.917991
934.771907	64874.239312	33.923008
935.590055	65019.550568	33.928026
936.240979	65132.654866	33.933044
937.264113	65242.498289	33.938061
938.336523	65324.571422	33.943079
939.077012	65428.444661	33.948096
940.150039	65505.907591	33.953114
941.183860	65660.057499	33.958132
942.088353	65770.222858	33.963149
942.946159	65871.562755	33.968167
943.540034	65970.623881	33.973184
945.236370	66053.693624	33.978202
945.867960	66176.436653	33.983220
946.549219	66335.581295	33.988237
947.598487	66426.935579	33.993255
948.530478	66517.102479	33.998272
949.161118	66661.669600	34.003290
950.695003	66739.923268	34.008308
951.532708	66893.406811	34.013325
952.383659	66978.712229	34.018343
953.044406	67102.372462	34.023360
954.023692	67233.837839	34.028378
955.122112	67335.333519	34.033396
955.645356	67489.686717	34.038413
957.195230	67590.107517	34.043431
957.993686	67716.762979	34.048448
959.027592	67842.649031	34.053466
959.581993	67978.820648	34.058484
961.071013	68078.362955	34.063501
962.353618	68221.697783	34.068519
962.547469	68329.192319	34.073536
964.113237	68418.003825	34.078554
965.285824	68581.864655	34.083572
965.541948	68669.666430	34.088589
967.191780	68819.340401	34.093607
967.837026	68916.026808	34.098624
968.710886	69055.642369	34.103642
969.824097	69157.145244	34.108660
970.520100	69308.983695	34.113677
971.695318	69396.768878	34.118695
972.722721	69565.392953	34.123712
973.568008	69650.256163	34.128730
974.425024	69796.949173	34.133748
975.674545	69901.782626	34.138765
977.019778	70039.934020	34.143783
978.164687	70155.228777	34.148800
979.101194	70247.554056	34.153818
979.817512	70405.721965	34.158836
980.518951	70498.205862	34.163853
982.053573	70574.705886	34.168871
982.774577	70737.525742	34.173888
983.696205	70841.961499	34.178906
985.051965	70909.999840	34.183924
985.543374	71069.617807	34.188941
986.496924	71170.764813	34.193959
987.014553	71270.920234	34.198976
988.332277	71357.769094	34.203994
989.265412	71500.987723	34.209012
989.924550	71633.585694	34.214029
991.138285	71715.132669	34.219047
991.747591	71834.389305	34.224064
992.885448	71997.608187	34.229082
994.083384	72079.070724	34.234100
994.676863	72232.205459	34.239117
996.070692	72323.589465	34.244135
996.823541	72475.942511	34.249152
997.775586	72576.420878	34.254170
998.904474	72734.187996	34.259188
999.556673	72832.952461	34.264205
1000.743799	72988.905198	34.269223
1001.565616	73105.311209	34.274240
1002.918656	73270.958032	34.279258
1004.031633	73364.040728	34.284276
1004.854754	73496.403920	34.289293
1006.178348	73646.242379	34.294311
1006.856167	73763.029006	34.299328
1008.096348	73854.754141	34.304346
1009.288970	73983.377811	34.309364
1010.286193	74135.906911	34.314381
1011.518432	74284.772604	34.319399
1012.507239	74432.799763	34.324416
1013.322357	74538.497873	34.329434
1014.302936	74652.726492	34.334452
1015.316238	74811.817577	34.339469
1016.610889	74945.202283	34.344487
1017.669811	75066.681733	34.349504
1018.352840	75168.271300	34.354522
1019.485398	75291.155945	34.359540
1020.929723	75397.194539	34.364557
1021.886747	75524.987184	34.369575
1023.077395	75682.736179	34.374592
1024.069756	75831.702073	34.379610
1025.250964	75917.992211	34.384628
1026.487163	76008.628233	34.389645
1027.207601	76173.363279	34.394663
1028.165988	76268.923497	34.399680
1029.534480	76419.647677	34.404698
1030.185171	76526.513643	34.409716
1031.539230	76626.303789	34.414733
1032.795244	76780.840480	34.419751
1033.460688	76872.171562	34.424768
1034.246373	77019.599105	34.429786
1035.828693	77111.885105	34.434804
1036.688473	77266.829813	34.439821
1037.606435	77368.197164	34.444839
1039.044870	77450.768317	34.449856
1039.668977	77572.066570	34.454874
1040.514660	77711.374499	34.459892
1041.255924	77785.430821	34.464909
1042.429390	77928.151586	34.469927
1043.062243	78031.906101	34.474944
1044.320251	78124.962494	34.479962
1045.411457	78279.391438	34.484980
1045.797294	78406.168091	34.489997
1047.478165	78504.316426	34.495015
1048.300899	78654.404513	34.500032
1048.816057	78795.776023	34.505050
1049.912575	78887.894541	34.510068
1050.675724	79061.615097	34.515085
1051.838274	79189.530867	34.520103
1053.235551	79306.317260	34.525120
1053.870422	79486.749129	34.530138
1054.636688	79603.928338	34.535156
1056.215810	79739.739165	34.540173
1057.730666	79848.855414	34.545191
1058.727284	80001.700567	34.550208
1059.868630	80187.177968	34.555226
1060.931101	80306.336779	34.560244
1062.112536	80447.778028	34.565261
1063.105350	80566.310995	34.570279
1064.704465	80673.850588	34.575296
1065.259131	80853.036632	34.580314
1066.475051	80986.132131	34.585332
1067.337566	81101.471392	34.590349
1068.827995	81206.439332	34.595367
1069.652817	81391.883073	34.600384
1070.697978	81497.884156	34.605402
1072.003790	81628.238651	34.610420
1072.948722	81794.746901	34.615437
1074.068094	81885.914332	34.620455
1075.141062	82027.029621	34.625472
1075.811852	82211.278794	34.630490
1077.412636	82322.101270	34.635508
1078.301747	82446.667028	34.640525
1079.479440	82563.165395	34.645543
1080.940404	82708.680392	34.650560
1082.027219	82878.929858	34.655578
1083.312534	83031.264648	34.660596
1084.014217	83160.138036	34.665613
1085.244222	83265.391704	34.670631
1086.221811	83393.084702	34.675648
1087.324163	83515.783231	34.680666
1088.562492	83694.316002	34.685684
1089.689675	83814.009359	34.690701
1090.516438	83929.433176	34.695719
1092.264183	84042.055853	34.700736
1092.831092	84219.587174	34.705754
1094.183009	84355.179817	34.710772
1094.867596	84462.505097	34.715789
1095.817761	84579.992884	34.720807
1097.798439	84675.777231	34.725824
1098.412509	84796.101503	34.730842
1099.623161	84958.691747	34.735860
1100.711436	85062.763057	34.740877
1101.521287	85168.725325	34.745895
1102.473689	85332.314208	34.750912
1103.260658	85429.113752	34.755930
1104.597696	85552.223080	34.760948
1105.176498	85706.276567	34.765965
1106.290344	85808.121907	34.770983
1107.635847	85946.868156	34.776000
1108.221060	86121.497754	34.781018
1109.311952	86235.311469	34.786036
1111.053760	86382.046459	34.791053
1111.889322	86541.192988	34.796071
1113.117410	86652.868951	34.801088
1114.301710	86818.556899	34.806106
1115.424610	86940.785173	34.811124
1115.913706	87111.631715	34.816141
1117.482919	87228.466644	34.821159
1118.330123	87387.959078	34.826176
1119.635727	87515.093631	34.831194
1120.736339	87710.084451	34.836212
1121.747065	87836.818858	34.841229
1122.725306	88012.786202	34.846247
1124.070605	88132.975098	34.851264
1124.963347	88306.321601	34.856282
1126.384727	88427.410617	34.861300
1127.558997	88622.707853	34.866317
1128.082913	88743.972987	34.871335
1129.971935	88910.228995	34.876352
1130.991741	89072.128407	34.881370
1132.230774	89205.822185	34.886388
1133.676687	89352.264119	34.891405
1134.750003	89528.892706	34.896423
1136.019487	89662.224010	34.901440
1136.677149	89807.630793	34.906458
1138.129874	89971.017428	34.911476
1139.207710	90109.972286	34.916493
1139.966725	90282.242878	34.921511
1141.238730	90408.748462	34.926528
1142.586404	90596.086620	34.931546
1143.924870	90712.755789	34.936564
1145.131868	90890.866678	34.941581
1146.421665	91023.861600	34.946599
1147.526572	91171.343952	34.951616
1148.367396	91344.552238	34.956634
1149.910053	91481.253719	34.961652
1150.838098	91622.430255	34.966669
1151.347419	91799.957484	34.971687
1153.029139	91916.938995	34.976704
1153.960006	92119.370756	34.981722
1155.456674	92254.806824	34.986740
1156.491597	92408.974715	34.991757
1157.795803	92572.847148	34.996775
1159.029157	92698.885124	35.001792
1159.939448	92840.502387	35.006810
1161.096592	92988.741285	35.011828
1162.723359	93111.948819	35.016845
1162.986343	93256.214247	35.021863
1164.452006	93415.317308	35.026880
1165.335712	93554.641116	35.031898
1166.483016	93695.625302	35.036916
1167.704252	93854.991763	35.041933
1168.718848	93983.272955	35.046951
1169.671814	94157.364693	35.051968
1170.633217	94314.359578	35.056986
1172.406801	94450.138258	35.062004
1173.342583	94657.728515	35.067021
1174.454643	94784.253063	35.072039
1175.833529	94952.691751	35.077056
1177.280130	95107.546696	35.082074
1177.817378	95253.464014	35.087092
1179.115083	95436.815608	35.092109
1180.467654	95577.228755	35.097127
1181.853485	95742.667678	35.102144
1182.698080	95916.733435	35.107162
1184.192396	96072.346541	35.112180
1185.253961	96237.834348	35.117197
1186.164640	96406.371066	35.122215
1187.802894	96572.636268	35.127232
1188.547001	96729.682643	35.132250
1189.736242	96899.557788	35.137268
1191.304799	97067.665903	35.142285
1192.279517	97247.408256	35.147303
1193.458313	97416.479225	35.152320
1194.354246	97588.917615	35.157338
1195.728442	97743.802228	35.162356
1197.215600	97937.088695	35.167373
1198.145955	98126.024333	35.172391
1199.684028	98274.971505	35.177408
1200.875054	98442.934757	35.182426
1201.788629	98626.436597	35.187444
1203.130522	98785.274763	35.192461
1204.397181	98987.044624	35.197479
1205.573725	99149.207695	35.202496
1206.573682	99320.567157	35.207514
1208.022099	99497.348084	35.212532
1209.369635	99681.124705	35.217549
1210.275062	99844.316435	35.222567
1211.682644	100008.859329	35.227584
1213.110305	100207.912828	35.232602
1214.369514	100364.883386	35.237620
1215.537695	100529.980546	35.242637
1217.002065	100714.284637	35.247655
1218.214008	100874.315762	35.252672
1219.326142	101057.008271	35.257690
1220.601512	101232.868340	35.262708
1222.259093	101395.299781	35.267725
1222.876608	101570.166084	35.272743
1224.185075	101727.467085	35.277760
1225.312582	101873.972001	35.282778
1226.180311	102033.888702	35.287796
1227.321327	102197.667018	35.292813
1228.651448	102367.984243	35.297831
1230.265718	102518.927260	35.302848
1231.266643	102695.949340	35.307866
1232.174461	102859.490973	35.312884
1233.699824	103027.744518	35.317901
1234.466912	103174.549032	35.322919
1235.922629	103372.941848	35.327936
1236.895853	103535.130016	35.332954
1238.175773	103701.915107	35.337972
1239.585664	103894.997996	35.342989
1240.809575	104061.984383	35.348007
1242.229603	104229.864648	35.353024
1243.171577	104429.588328	35.358042
1244.618558	104590.063191	35.363060
1246.237457	104783.784578	35.368077
1247.041664	104930.746024	35.373095
1248.506922	105139.036659	35.378112
1250.050886	105291.793215	35.383130
1250.855513	105490.098535	35.388148
1252.479513	105660.146100	35.393165
1253.566316	105832.254716	35.398183
1255.277910	106034.742637	35.403200
1256.362573	106197.766708	35.408218
1257.449239	106380.650262	35.413236
1258.878135	106564.461732	35.418253
1259.746070	106738.060910	35.423271
1261.335267	106898.566743	35.428288
1262.330165	107109.253000	35.433306
1264.015238	107268.632231	35.438324
1264.998845	107457.502028	35.443341
1266.325633	107643.413841	35.448359
1267.570282	107820.220295	35.453376
1269.026476	108007.386447	35.458394
1269.903363	108196.608113	35.463412
1272.004517	108364.580127	35.468429
1272.527187	108583.398492	35.473447
1274.250549	108722.091659	35.478464
1275.863499	108939.670318	35.483482
1276.527700	109099.932812	35.488500
1277.718208	109302.037439	35.493517
1278.735409	109482.246695	35.498535
1280.256970	109686.858922	35.503552
1281.749250	109857.317906	35.508570
1282.807556	110050.139265	35.513588
1284.364679	110247.338801	35.518605
1285.690710	110425.455194	35.523623
1286.974051	110629.309348	35.528640
1288.197666	110803.685012	35.533658
1289.021411	110990.151831	35.538676
1290.598310	111198.337849	35.543693
1292.001264	111368.258220	35.548711
1293.328748	111567.808920	35.553728
1294.541850	111723.576826	35.558746
1295.314187	111919.965079	35.563764
1297.435461	112077.920270	35.568781
1298.330594	112250.351813	35.573799
1299.485126	112444.214787	35.578816
1301.137924	112599.475227	35.583834
1302.100993	112801.397964	35.588852
1303.416354	112960.107247	35.593869
1304.441000	113172.069183	35.598887
1305.920065	113325.279140	35.603904
1307.206855	113532.910568	35.608922
1308.098545	113699.541496	35.613940
1309.387004	113904.681595	35.618957
1310.970935	114076.028774	35.623975
1312.191869	114300.629998	35.628992
1313.944933	114481.790679	35.634010
1314.678456	114677.187642	35.639028
1315.854065	114875.250696	35.644045
1317.152504	115081.487713	35.649063
1318.441893	115290.323467	35.654080
1320.095050	115481.940324	35.659098
1320.908171	115705.283113	35.664116
1322.679860	115900.492897	35.669133
1323.790451	116100.057335	35.674151
1324.955263	116310.909244	35.679168
1326.706561	116522.258477	35.684186
1328.350978	116729.150360	35.689204
1329.364036	116921.892829	35.694221
1330.712436	117154.755006	35.699239
1332.410803	117323.921778	35.704256
1333.616867	117555.936525	35.709274
1335.008671	117749.099893	35.714292
1336.516104	117969.427111	35.719309
1338.026545	118141.294690	35.724327
1339.222887	118357.192008	35.729344
1341.022070	118593.458964	35.734362
1342.024442	118771.008617	35.739380
1343.632043	118954.801293	35.744397
1345.002712	119156.652981	35.749415
1346.315366	119363.511226	35.754432
1347.720593	119544.611276	35.759450
1349.249691	119768.255640	35.764468
1350.572075	119954.874111	35.769485
1352.208242	120120.934872	35.774503
1353.341233	120364.352348	35.779520
1354.917417	120526.049814	35.784538
1356.294631	120746.035147	35.789556
1357.668923	120944.480827	35.794573
1359.194445	121118.043796	35.799591
1360.527932	121341.853072	35.804608
1361.773826	121492.932859	35.809626
1362.994606	121699.412661	35.814644
1364.277281	121903.110667	35.819661
1365.910002	122089.530426	35.824679
1366.798209	122258.427579	35.829696
1368.333650	122463.558882	35.834714
1369.468985	122623.832215	35.839732
1370.738681	122812.024564	35.844749
1372.052116	123003.288964	35.849767
1373.578156	123172.014598	35.854784
1374.764712	123382.261951	35.859802
1376.083343	123539.725296	35.864820
1377.414652	123759.705097	35.869837
1378.771340	123927.018559	35.874855
1379.973171	124161.245861	35.879872
1381.610881	124316.294580	35.884890
1382.896892	124553.627759	35.889908
1383.852186	124713.929636	35.894925
1385.117802	124936.399456	35.899943
1386.357224	125148.438250	35.904960
1387.745300	125351.917941	35.909978
1388.872402	125578.189670	35.914996
1390.420876	125763.394559	35.920013
1391.973370	126003.206171	35.925031
1393.208123	126206.336673	35.930048
1394.881651	126432.440055	35.935066
1395.969199	126658.701778	35.940084
1398.001417	126847.168637	35.945101
1399.135966	127113.695401	35.950119
1400.603745	127316.746511	35.955136
1401.548241	127512.826544	35.960154
1403.404360	127719.999189	35.965172
1404.617759	127929.669713	35.970189
1406.397283	128203.439154	35.975207
1407.877357	128402.240016	35.980224
1409.012165	128625.191548	35.985242
1410.345897	128871.181748	35.990260
1411.985946	129057.990642	35.995277
1413.350207	129301.116831	36.000295
1414.708717	129511.498437	36.005312
1416.904691	129758.195631	36.010330
1418.120077	129957.024417	36.015348
1419.726697	130194.026368	36.020365
1421.220279	130376.952828	36.025383
1422.256186	130630.455175	36.030400
1424.064929	130812.688306	36.035418
1425.252964	131069.172994	36.040436
1427.004332	131255.434212	36.045453
1428.480586	131482.091812	36.050471
1429.427463	131694.734410	36.055488
1431.448802	131906.739120	36.060506
1432.672783	132144.793940	36.065524
1433.904962	132331.436189	36.070541
1435.946131	132540.756564	36.075559
1437.004858	132802.003388	36.080576
1438.424449	132977.850789	36.085594
1439.916597	133210.373236	36.090612
1441.031455	133439.270537	36.095629
1442.823576	133622.968880	36.100647
1443.924280	133871.498011	36.105664
1445.651015	134028.614443	36.110682
1446.806233	134259.615193	36.115700
1448.001404	134441.247005	36.120717
1449.604894	134647.079332	36.125735
1451.006370	134852.463746	36.130752
1452.399715	135059.662846	36.135770
1453.585880	135282.278832	36.140788
1454.888628	135497.351437	36.145805
1456.472316	135699.266425	36.150823
1457.744072	135911.179261	36.155840
1459.463940	136155.803055	36.160858
1460.716349	136359.916733	36.165876
1461.940760	136586.033966	36.170893
1463.694198	136813.336060	36.175911
1465.068258	137044.413003	36.180928
1466.589158	137265.483088	36.185946
1468.067971	137477.881303	36.190964
1469.728649	137727.558420	36.195981
1471.540478	137946.471202	36.200999
1472.337676	138167.181528	36.206016
1474.256076	138405.557910	36.211034
1475.955800	138601.163748	36.216052
1476.741193	138875.738766	36.221069
1478.532581	139072.511698	36.226087
1479.945625	139336.473052	36.231104
1481.546609	139552.960071	36.236122
1482.703635	139800.985887	36.241140
1484.495069	140012.693670	36.246157
1485.944705	140294.425178	36.251175
1487.014357	140500.206035	36.256192
1488.599184	140764.862430	36.261210
1490.186386	140976.394033	36.266228
1491.603055	141249.952765	36.271245
1493.443919	141453.881366	36.276263
1495.023728	141730.612277	36.281280
1496.819190	141947.034990	36.286298
1498.596566	142190.280007	36.291316
1499.918298	142415.158750	36.296333
1501.804876	142654.106338	36.301351
1502.785812	142893.541881	36.306368
1504.371969	143116.241860	36.311386
1506.158381	143378.189455	36.316404
1507.531814	143594.259999	36.321421
1508.988652	143832.689378	36.326439
1510.553675	144090.635049	36.331456
1512.332562	144305.885709	36.336474
1513.455887	144552.168608	36.341492
1515.036430	144786.073470	36.346509
1516.715332	145028.989099	36.351527
1518.194843	145266.703476	36.356544
1519.687230	145491.133992	36.361562
1521.669645	145747.708945	36.366580
1522.536971	145968.072011	36.371597
1524.008044	146218.064794	36.376615
1525.964332	146408.990222	36.381632
1526.627708	146671.334206	36.386650
1528.407853	146875.130941	36.391668
1529.985954	147100.649505	36.396685
1531.468142	147335.805977	36.401703
1532.690536	147549.405469	36.406720
1534.132433	147791.746382	36.411738
1535.646700	148023.619750	36.416756
1537.240088	148260.210518	36.421773
1538.525246	148484.784048	36.426791
1540.006766	148750.247787	36.431808
1541.933517	148975.787687	36.436826
1543.100021	149206.064267	36.441844
1544.571566	149485.492754	36.446861
1546.369916	149709.220076	36.451879
1547.788753	149964.448210	36.456896
1549.353114	150198.167554	36.461914
1551.015662	150464.136467	36.466932
1552.513470	150715.085770	36.471949
1553.932760	150948.668773	36.476967
1555.415006	151234.411353	36.481984
1557.005216	151468.173776	36.487002
1558.328422	151746.390258	36.492020
1559.966170	152004.883184	36.497037
1562.096952	152250.926201	36.502055
1563.584235	152523.621011	36.507072
1564.929543	152788.302709	36.512090
1566.813638	153030.739450	36.517108
1567.890237	153308.982967	36.522125
1570.101045	153538.135384	36.527143
1571.352903	153834.802542	36.532160
1573.352008	154061.836854	36.537178
1575.024985	154359.025007	36.542196
1576.535542	154589.893411	36.547213
1578.645322	154860.771553	36.552231
1579.617012	155108.439907	36.557248
1581.703902	155386.185258	36.562266
1583.439788	155617.379951	36.567284
1584.650947	155877.365443	36.572301
1586.343685	156141.143652	36.577319
1587.882783	156392.852100	36.582336
1589.276789	156648.668276	36.587354
1590.698524	156909.617231	36.592372
1592.591531	157189.398855	36.597389
1594.458402	157425.124402	36.602407
1595.905548	157691.692463	36.607424
1597.193180	157964.982993	36.612442
1599.507187	158220.271706	36.617460
1600.636138	158477.348236	36.622477
1602.495537	158732.649539	36.627495
1604.021563	159010.690960	36.632512
1605.571805	159265.715595	36.637530
1607.712685	159507.625296	36.642548
1608.838687	159773.017681	36.647565
1610.424118	160026.292347	36.652583
1612.060146	160275.490239	36.657600
1613.178929	160516.542091	36.662618
1615.054944	160744.489920	36.667636
1616.175766	160993.039215	36.672653
1618.113109	161240.382672	36.677671
1619.662357	161479.216917	36.682688
1621.338626	161727.175894	36.687706
1623.002131	161985.207739	36.692724
1624.358363	162240.614434	36.697741
1626.136926	162476.946040	36.702759
1627.543425	162740.591413	36.707776
1628.849677	163018.471014	36.712794
1630.812405	163262.400348	36.717812
1632.133506	163533.965952	36.722829
1633.967267	163800.341274	36.727847
1635.194074	164054.196122	36.732864
1636.817156	164330.982864	36.737882
1638.630904	164602.364083	36.742900
1640.159027	164890.368733	36.747917
1641.821071	165159.089482	36.752935
1643.820094	165435.190753	36.757952
1645.515571	165708.539402	36.762970
1647.710676	165972.349293	36.767988
1649.064099	166256.650928	36.773005
1650.975744	166527.003481	36.778023
1652.644408	166792.133071	36.783040
1653.921051	167057.009720	36.788058
1655.722225	167336.061043	36.793076
1657.311149	167622.859694	36.798093
1659.118722	167883.611856	36.803111
1660.427897	168163.825565	36.808128
1662.300086	168447.097514	36.813146
1663.871296	168706.903571	36.818164
1665.370448	169028.772573	36.823181
1667.214565	169278.392061	36.828199
1668.811093	169580.590053	36.833216
1670.458571	169868.905817	36.838234
1672.283791	170162.789303	36.843252
1673.972233	170444.951002	36.848269
1675.686541	170725.804157	36.853287
1677.272174	171014.290535	36.858304
1678.858710	171305.785185	36.863322
1680.655973	171586.390394	36.868340
1682.561746	171890.003423	36.873357
1684.217564	172175.290674	36.878375
1685.844236	172452.034906	36.883392
1687.583882	172745.025498	36.888410
1689.756059	173030.490668	36.893428
1691.315301	173322.651599	36.898445
1693.313441	173593.928220	36.903463
1695.024629	173874.360449	36.908480
1696.335296	174166.605110	36.913498
1698.580408	174431.784507	36.918516
1699.958389	174723.248717	36.923533
1701.682947	174994.743206	36.928551
1703.599973	175263.215082	36.933568
1705.093536	175519.894548	36.938586
1706.919718	175769.710389	36.943604
1708.146152	176029.683138	36.948621
1709.970599	176286.543263	36.953639
1711.823876	176548.792123	36.958656
1713.350194	176820.545966	36.963674
1715.136679	177079.193195	36.968692
1716.885953	177345.853196	36.973709
1718.224805	177617.502514	36.978727
1720.099440	177889.791691	36.983744
1721.673456	178171.988061	36.988762
1723.049657	178437.407577	36.993780
1724.696984	178728.997089	36.998797
1726.248624	179007.333122	37.003815
1728.038923	179293.397662	37.008832
1729.572292	179590.796608	37.013850
1731.483052	179873.179336	37.018868
1733.250476	180175.404489	37.023885
1734.920767	180476.492648	37.028903
1736.453543	180761.897491	37.033920
1738.222243	181072.857888	37.038938
1740.476761	181375.889658	37.043956
1742.013412	181685.952437	37.048973
1743.958644	181976.628781	37.053991
1745.962043	182272.956717	37.059008
1747.438969	182571.819074	37.064026
1749.311431	182882.255797	37.069044
1750.889784	183182.704950	37.074061
1752.764867	183484.910805	37.079079
1754.593573	183780.451947	37.084096
1756.273950	184084.735674	37.089114
1758.352772	184393.754553	37.094132
1760.272875	184685.049204	37.099149
1762.102241	184985.356551	37.104167
1764.162342	185288.750760	37.109184
1765.846347	185594.579574	37.114202
1767.684530	185876.695441	37.119220
1769.290471	186170.498603	37.124237
1771.182119	186477.861198	37.129255
1772.977437	186774.759762	37.134272
1774.426510	187082.831165	37.139290
1776.264274	187380.069536	37.144308
1778.360856	187685.072843	37.149325
1779.934248	187983.093073	37.154343
1781.992709	188279.515447	37.159360
1783.651433	188578.718797	37.164378
1785.390377	188890.537807	37.169396
1787.195679	189184.442763	37.174413
1789.046645	189490.550173	37.179431
1790.621691	189789.393837	37.184448
1792.328329	190102.507722	37.189466
1794.473545	190392.013487	37.194484
1796.137501	190701.572114	37.199501
1798.067865	191001.242635	37.204519
1799.946665	191275.377108	37.209536
1801.610800	191563.050057	37.214554
1803.406782	191847.239227	37.219572
1804.859871	192128.705214	37.224589
1806.587195	192408.314507	37.229607
1808.407978	192687.339477	37.234624
1809.996388	192986.213587	37.239642
1812.054015	193277.869953	37.244660
1813.807964	193556.428214	37.249677
1814.970743	193864.931658	37.254695
1816.971802	194157.338286	37.259712
1818.769666	194466.366527	37.264730
1820.585677	194767.816994	37.269748
1822.556311	195074.790933	37.274765
1824.008236	195397.523229	37.279783
1825.533478	195698.644674	37.284800
1827.153268	196008.725980	37.289818
1829.032611	196336.790408	37.294836
1831.088188	196677.406678	37.299853
1832.491636	196989.901663	37.304871
1834.721340	197322.714358	37.309888
1836.485444	197655.983861	37.314906
1838.396377	197977.415699	37.319924
1840.680878	198331.117612	37.324941
1842.300006	198637.559395	37.329959
1844.474738	198963.867373	37.334976
1846.166453	199299.570381	37.339994
1848.114142	199625.194990	37.345012
1850.415422	199943.822541	37.350029
1851.894750	200287.714207	37.355047
1854.059469	200603.371844	37.360064
1856.079971	200931.950262	37.365082
1857.937339	201256.748650	37.370100
1859.947771	201573.972277	37.375117
1861.714416	201906.468258	37.380135
1863.728968	202238.051066	37.385152
1865.474121	202564.055473	37.390170
1867.546156	202881.962290	37.395188
1869.579325	203219.044252	37.400205
1870.921655	203539.126966	37.405223
1873.405330	203874.123086	37.410240
1875.383476	204202.143723	37.415258
1876.743590	204525.834214	37.420276
1879.017084	204848.264520	37.425293
1880.894402	205176.954153	37.430311
1882.868137	205486.995577	37.435328
1884.847805	205825.383565	37.440346
1886.722917	206145.751748	37.445364
1889.200585	206455.553344	37.450381
1890.802996	206784.016427	37.455399
1892.534275	207104.323815	37.460416
1894.821112	207418.806896	37.465434
1896.276203	207746.245062	37.470452
1898.307244	208059.350337	37.475469
1900.172406	208373.994231	37.480487
1902.029259	208670.817759	37.485504
1903.924611	208970.264444	37.490522
1905.686604	209264.846269	37.495540
1908.094557	209547.863547	37.500557
1909.440453	209863.867040	37.505575
1911.352640	210166.579500	37.510592
1913.136403	210444.507705	37.515610
1914.535336	210773.481753	37.520628
1916.731166	211059.294445	37.525645
1918.374217	211389.553284	37.530663
1920.340757	211708.349444	37.535680
1921.909699	212025.407560	37.540698
1923.914322	212345.026068	37.545716
1926.021439	212651.134607	37.550733
1927.511283	212999.263251	37.555751
1929.303014	213334.497895	37.560768
1931.067732	213667.808809	37.565786
1933.226079	213982.281952	37.570804
1935.167159	214326.359607	37.575821
1936.385906	214683.820864	37.580839
1938.705440	215029.010130	37.585856
1941.070911	215376.161770	37.590874
1942.650146	215715.365262	37.595892
1945.081630	216067.689984	37.600909
1946.561953	216415.711093	37.605927
1948.685260	216769.408744	37.610944
1950.685490	217131.824730	37.615962
1952.528522	217485.634003	37.620980
1954.332246	217848.681637	37.625997
1956.481144	218209.213252	37.631015
1958.576545	218555.725464	37.636032
1960.453787	218920.074691	37.641050
1962.160960	219292.807203	37.646068
1964.827505	219644.655570	37.651085
1966.581005	220015.695792	37.656103
1968.484468	220378.448418	37.661120
1970.566260	220749.643425	37.666138
1972.544694	221111.460889	37.671156
1974.870333	221475.231166	37.676173
1976.631499	221841.733784	37.681191
1978.999167	222188.588234	37.686208
1980.940275	222561.160455	37.691226
1982.521409	222919.481706	37.696244
1985.040124	223275.852835	37.701261
1986.830977	223636.797899	37.706279
1988.792425	224064.582712	37.711296
1990.568782	224433.279240	37.716314
1992.631995	224799.646395	37.721332
1994.783496	225158.560375	37.726349
1996.838159	225533.020682	37.731367
1998.964642	225889.529314	37.736384
2001.084968	226258.535189	37.741402
2002.874365	226626.427019	37.746420
2005.417277	226987.229743	37.751437
2007.410760	227338.978614	37.756455
2009.175799	227677.990925	37.761472
2011.302766	228009.226707	37.766490
2013.101811	228338.484095	37.771508
2015.246621	228673.275118	37.776525
2016.772625	229015.708397	37.781543
2018.869299	229347.639853	37.786560
2020.935598	229687.704353	37.791578
2022.658828	230046.211927	37.796596
2024.758740	230374.641970	37.801613
2026.457789	230738.768894	37.806631
2028.266994	231089.698681	37.811648
2030.538372	231444.670859	37.816666
2032.148401	231808.181256	37.821684
2034.400165	232173.699266	37.826701
2036.141369	232545.725291	37.831719
2038.488663	232911.586596	37.836736
2040.660596	233285.629815	37.841754
2042.453482	233661.004525	37.846772
2044.579893	234022.003336	37.851789
2046.663913	234400.001510	37.856807
2048.651452	234779.260954	37.861824
2050.735192	235156.550925	37.866842
2052.933922	235541.367387	37.871860
2055.221076	235911.744976	37.876877
2057.054817	236300.863761	37.881895
2059.061837	236676.393661	37.886912
2061.350761	237061.074537	37.891930
2063.307877	237455.080028	37.896948
2065.300947	237827.644603	37.901965
2067.617002	238217.455955	37.906983
2069.736942	238598.918126	37.912000
2071.930191	238978.896848	37.917018
2073.788786	239378.690591	37.922036
2076.062577	239752.512567	37.927053
2078.490844	240152.498099	37.932071
2080.804724	240528.576828	37.937088
2083.302884	240910.571064	37.942106
2084.959531	241300.446942	37.947124
2087.176270	241676.392393	37.952141
2089.642349	242049.937296	37.957159
2091.321793	242437.781296	37.962176
2093.734204	242818.703066	37.967194
2095.709345	243204.292791	37.972212
2097.661341	243578.939910	37.977229
2099.621843	243975.608802	37.982247
2101.657704	244367.085309	37.987264
2104.238930	244737.190970	37.992282
2106.092567	245132.229342	37.997300
2108.090375	245516.171388	38.002317
2110.721055	245908.675764	38.007335
2112.445839	246286.821168	38.012352
2114.488850	246675.280646	38.017370
2116.604261	247060.554621	38.022388
2118.963900	247448.762816	38.027405
2120.852659	247832.042760	38.032423
2122.852995	248191.378252	38.037440
2125.196756	248548.424859	38.042458
2126.965737	248917.222613	38.047476
2129.117686	249264.293298	38.052493
2131.193755	249646.074937	38.057511
2133.314497	249995.717749	38.062528
2135.302628	250372.003024	38.067546
2137.360854	250744.874276	38.072564
2139.817755	251115.244614	38.077581
2141.757159	251484.580194	38.082599
2143.591367	251853.323637	38.087616
2145.746543	252237.689811	38.092634
2147.656559	252621.816306	38.097652
2149.737664	253004.570217	38.102669
2151.880594	253401.438569	38.107687
2153.820807	253799.127401	38.112704
2156.281061	254189.850689	38.117722
2158.565677	254569.019336	38.122740
2161.101530	254957.446044	38.127757
2163.151148	255347.169942	38.132775
2165.278817	255755.705224	38.137792
2167.538521	256134.271198	38.142810
2169.626706	256547.945573	38.147828
2171.584520	256950.566036	38.152845
2174.199578	257357.680850	38.157863
2176.132833	257754.032320	38.162880
2178.647428	258167.769176	38.167898
2180.455853	258573.362959	38.172916
2182.842533	258971.143375	38.177933
2185.242585	259381.750625	38.182951
2187.537077	259791.664029	38.187968
2189.599251	260191.733309	38.192986
2191.940060	260595.137580	38.198004
2194.436178	261007.484998	38.203021
2196.193240	261418.400668	38.208039
2198.464888	261828.371644	38.213056
2201.041315	262232.630040	38.218074
2203.237691	262633.443658	38.223092
2205.634660	263030.669586	38.228109
2207.988444	263445.430887	38.233127
2210.103437	263850.755275	38.238144
2212.863248	264249.804976	38.243162
2214.137358	264655.238251	38.248180
2216.530647	265063.365060	38.253197
2218.914669	265484.982818	38.258215
2221.052464	265877.248685	38.263232
2223.206548	266302.841254	38.268250
2225.548016	266711.257411	38.273268
2227.686782	267114.701663	38.278285
2230.270626	267525.518832	38.283303
2232.170425	267944.091183	38.288320
2234.682373	268354.945844	38.293338
2236.601373	268759.493217	38.298356
2238.892925	269182.881845	38.303373
2241.148778	269584.404197	38.308391
2243.269668	269979.851407	38.313408
2245.259973	270361.957404	38.318426
2247.301052	270765.648386	38.323444
2249.369511	271141.620184	38.328461
2251.694314	271541.811710	38.333479
2253.327273	271935.838473	38.338496
2255.895286	272328.497772	38.343514
2257.962617	272744.429884	38.348532
2260.152487	273153.001124	38.353549
2262.335492	273563.936084	38.358567
2264.154958	273989.738966	38.363584
2266.786058	274396.868766	38.368602
2268.996723	274837.140532	38.373620
2271.132949	275254.383256	38.378637
2273.429133	275678.027715	38.383655
2275.544236	276124.284533	38.388672
2278.053360	276548.936779	38.393690
2280.111171	276994.237316	38.398708
2282.577776	277424.866032	38.403725
2284.995571	277864.698454	38.408743
2287.051478	278311.828128	38.413760
2289.347520	278753.000627	38.418778
2291.430208	279203.936313	38.423796
2294.127814	279644.638406	38.428813
2296.710936	280104.283980	38.433831
2298.298384	280552.681083	38.438848
2300.883801	281004.628637	38.443866
2303.399575	281470.533404	38.448884
2305.446619	281921.625849	38.453901
2308.293527	282382.879528	38.458919
2311.039287	282837.874300	38.463936
2313.243227	283279.033638	38.468954
2315.636295	283749.198536	38.473972
2318.561178	284183.714220	38.478989
2321.004115	284632.734933	38.484007
2322.859053	285074.202079	38.489024
2325.508967	285520.293155	38.494042
2327.798919	285976.221022	38.499060
2329.965973	286425.740884	38.504077
2332.580238	286864.977313	38.509095
2334.823833	287318.396061	38.514112
2337.576129	287763.807871	38.519130
2339.942833	288221.676868	38.524148
2342.218822	288667.391622	38.529165
2344.852332	289106.571352	38.534183
2346.710003	289559.463962	38.539200
2349.479540	289984.166654	38.544218
2351.721472	290440.604203	38.549236
2353.753928	290879.571742	38.554253
2356.490370	291323.482123	38.559271
2358.568977	291771.865289	38.564288
2361.365012	292227.322892	38.569306
2363.401967	292676.574756	38.574324
2365.621573	293126.711332	38.579341
2368.476029	293551.293175	38.584359
2370.805300	293980.758541	38.589376
2372.637396	294397.575316	38.594394
2375.057719	294812.723129	38.599412
2377.099791	295235.881007	38.604429
2379.399186	295647.871087	38.609447
2381.476880	296085.170633	38.614464
2384.086754	296509.099590	38.619482
2386.124305	296951.204610	38.624500
2388.454909	297394.786296	38.629517
2390.911045	297819.803648	38.634535
2393.151478	298274.752219	38.639552
2395.230445	298717.989617	38.644570
2397.998171	299160.888141	38.649588
2400.231945	299611.160459	38.654605
2402.652087	300063.637407	38.659623
2404.930387	300526.448651	38.664640
2407.378812	300993.626097	38.669658
2409.493158	301459.153259	38.674676
2411.997273	301934.447603	38.679693
2414.468325	302400.017077	38.684711
2416.796556	302874.269578	38.689728
2419.087841	303353.403460	38.694746
2421.618872	303831.913582	38.699764
2424.003160	304318.802298	38.704781
2426.773889	304808.727025	38.709799
2429.113207	305294.019290	38.714816
2431.393625	305774.391472	38.719834
2433.975861	306257.482799	38.724852
2436.445091	306754.611358	38.729869
2438.899801	307245.110859	38.734887
2441.142290	307737.064564	38.739904
2443.943669	308239.214885	38.744922
2446.498304	308722.733263	38.749940
2448.752857	309225.347298	38.754957
2451.064718	309721.092229	38.759975
2453.574444	310223.585509	38.764992
2456.251131	310720.995681	38.770010
2459.080778	311220.817863	38.775028
2461.615605	311722.995956	38.780045
2464.382426	312213.959375	38.785063
2466.846232	312712.182046	38.790080
2469.240186	313209.575381	38.795098
2471.902781	313712.029085	38.800116
2474.130757	314198.243255	38.805133
2477.142813	314695.785800	38.810151
2479.526428	315198.556099	38.815168
2482.027453	315691.450747	38.820186
2484.318898	316171.702447	38.825204
2486.573282	316673.216090	38.830221
2489.339526	317171.572944	38.835239
2491.929916	317672.367966	38.840256
2494.253697	318160.122766	38.845274
2497.055255	318663.317423	38.850292
2499.291216	319156.287621	38.855309
2501.630095	319638.876770	38.860327
2503.932651	320120.377097	38.865344
2506.619378	320583.731228	38.870362
2509.065093	321042.676708	38.875380
2511.266934	321513.391897	38.880397
2513.822704	321986.207265	38.885415
2516.335079	322450.544494	38.890432
2518.417950	322936.864541	38.895450
2521.498694	323406.998630	38.900468
2523.691347	323885.753212	38.905485
2526.367672	324373.672657	38.910503
2528.794621	324851.064064	38.915520
2530.944552	325352.292519	38.920538
2533.536969	325830.820286	38.925556
2535.491538	326337.762316	38.930573
2538.553148	326835.688197	38.935591
2540.487920	327339.655806	38.940608
2542.823366	327859.327055	38.945626
2545.789085	328373.536697	38.950644
2548.353203	328890.447617	38.955661
2550.836837	329410.085036	38.960679
2553.320172	329938.378438	38.965696
2555.932896	330465.606489	38.970714
2558.771191	330991.601572	38.975732
2561.412127	331519.376364	38.980749
2564.229618	332040.237719	38.985767
2567.058396	332545.349620	38.990784
2569.742211	333087.783653	38.995802
2572.682676	333591.930943	39.000820
2574.971406	334127.157216	39.005837
2578.054858	334634.778611	39.010855
2580.537683	335161.612009	39.015872
2582.961299	335692.640490	39.020890
2585.738551	336204.031501	39.025908
2588.190103	336729.765897	39.030925
2590.679122	337260.670153	39.035943
2593.141332	337786.039068	39.040960
2595.908704	338320.267811	39.045978
2598.593879	338851.661408	39.050996
2601.222587	339377.473598	39.056013
2603.679296	339909.021641	39.061031
2606.264976	340446.460804	39.066048
2608.783675	340992.360966	39.071066
2611.816129	341520.478142	39.076084
2614.407186	342057.547190	39.081101
2616.801359	342592.408465	39.086119
2619.758122	343130.527350	39.091136
2622.103803	343668.408201	39.096154
2624.895914	344205.578813	39.101172
2627.560733	344763.837368	39.106189
2629.987333	345286.863841	39.111207
2632.646904	345823.253748	39.116224
2635.194778	346371.461831	39.121242
2638.213124	346903.240497	39.126260
2640.586204	347443.316614	39.131277
2643.002076	347987.392029	39.136295
2646.147030	348502.050102	39.141312
2648.449841	349012.571865	39.146330
2651.095042	349521.993879	39.151348
2654.092123	350010.970243	39.156365
2656.295002	350517.482932	39.161383
2658.640352	351034.503503	39.166400
2661.081908	351552.747811	39.171418
2663.883575	352066.233806	39.176436
2666.282206	352592.166662	39.181453
2668.825077	353130.332373	39.186471
2671.693780	353655.697915	39.191488
2673.813070	354193.716764	39.196506
2676.669980	354729.633278	39.201524
2679.179828	355286.921629	39.206541
2681.915097	355822.262224	39.211559
2684.553417	356372.030268	39.216576
2687.368883	356930.496052	39.221594
2690.082628	357476.229618	39.226612
2692.818950	358045.381654	39.231629
2695.470808	358600.656504	39.236647
2698.400225	359160.094535	39.241664
2700.810195	359729.354966	39.246682
2703.556357	360299.621509	39.251700
2706.093357	360874.203831	39.256717
2708.922308	361439.925946	39.261735
2711.599194	362020.386043	39.266752
2714.469729	362602.737241	39.271770
2717.702981	363170.379679	39.276788
2720.353913	363762.953895	39.281805
2722.702237	364333.133339	39.286823
2725.996878	364911.936938	39.291840
2728.338059	365493.117513	39.296858
2731.438302	366070.211475	39.301876
2734.224332	366662.498382	39.306893
2737.380591	367245.659094	39.311911
2740.309351	367822.706939	39.316928
2742.851156	368406.888682	39.321946
2745.875326	368974.085562	39.326964
2748.298542	369557.966258	39.331981
2751.051551	370137.092376	39.336999
2754.426234	370722.202412	39.342016
2756.941873	371303.964115	39.347034
2759.742641	371879.861925	39.352052
2762.393692	372464.352188	39.357069
2765.081091	373028.275595	39.362087
2768.143573	373623.392474	39.367104
2770.752228	374209.844280	39.372122
2773.868310	374781.541843	39.377140
2776.795095	375359.224022	39.382157
2779.300516	375948.458422	39.387175
2782.319854	376528.164570	39.392192
2785.519210	377093.676576	39.397210
2788.268628	377663.945553	39.402228
2790.886320	378250.540719	39.407245
2793.597762	378805.323186	39.412263
2796.555399	379347.652900	39.417280
2798.893458	379886.343882	39.422298
2802.018159	380416.074342	39.427316
2804.693029	380957.817667	39.432333
2807.277845	381502.789508	39.437351
2809.855812	382040.702324	39.442368
2812.740655	382576.275891	39.447386
2815.343275	383122.084430	39.452404
2817.874916	383677.256894	39.457421
2820.483465	384230.531874	39.462439
2823.560022	384785.246610	39.467456
2826.110465	385366.036724	39.472474
2829.340827	385931.439942	39.477492
2832.071242	386483.875861	39.482509
2834.814434	387079.650237	39.487527
2838.138856	387628.728176	39.492544
2840.832517	388198.975348	39.497562
2843.276502	388763.850587	39.502580
2846.017395	389372.903723	39.507597
2848.651893	389946.049423	39.512615
2851.892021	390522.006739	39.517632
2854.457577	391127.811281	39.522650
2857.189542	391732.640708	39.527668
2860.186449	392326.842142	39.532685
2863.001197	392918.526228	39.537703
2865.988304	393532.185779	39.542720
2868.929961	394134.049270	39.547738
2872.089201	394734.473023	39.552756
2875.066142	395342.598894	39.557773
2877.820794	395958.255236	39.562791
2880.895370	396561.449631	39.567808
2883.309923	397178.481568	39.572826
2886.456622	397791.608044	39.577844
2889.392915	398411.780374	39.582861
2891.909013	399033.681147	39.587879
2894.971511	399645.721752	39.592896
2898.027576	400281.408472	39.597914
2900.786249	400907.469731	39.602932
2903.664790	401535.528315	39.607949
2906.475531	402158.692159	39.612967
2909.540987	402784.998151	39.617984
2912.738033	403418.750160	39.623002
2915.877964	404059.622617	39.628020
2918.874786	404680.045868	39.633037
2921.641832	405313.599926	39.638055
2924.775523	405933.596551	39.643072
2927.885213	406583.193822	39.648090
2930.929151	407199.731845	39.653108
2933.552290	407835.006598	39.658125
2936.458906	408462.492025	39.663143
2939.550555	409087.273764	39.668160
2942.257588	409724.802780	39.673178
2945.155542	410353.213915	39.678196
2948.389991	410991.925505	39.683213
2951.291943	411615.138999	39.688231
2954.424396	412215.035797	39.693248
2957.233998	412814.236610	39.698266
2959.921665	413395.272559	39.703284
2962.983906	413986.603536	39.708301
2965.781981	414580.397417	39.713319
2968.546556	415170.535166	39.718336
2971.216822	415780.214994	39.723354
2974.275161	416379.785180	39.728372
2977.309380	416984.060265	39.733389
2980.007832	417601.477065	39.738407
2982.839960	418211.358660	39.743424
2985.787292	418841.075422	39.748442
2988.178181	419464.151380	39.753460
2991.444330	420101.138090	39.758477
2994.261782	420751.230527	39.763495
2997.269555	421380.070258	39.768512
2999.837653	422040.889962	39.773530
3002.931786	422697.683579	39.778548
3005.793864	423357.690623	39.783565
3009.231430	424025.926036	39.788583
3012.011216	424695.515968	39.793600
3015.092919	425352.830762	39.798618
3018.326394	426024.165596	39.803636
3021.630579	426693.192636	39.808653
3024.401711	427371.964216	39.813671
3027.878082	428031.760480	39.818688
3031.001345	428711.379597	39.823706
3034.057167	429398.641674	39.828724
3037.615709	430064.149689	39.833741
3040.350504	430742.764877	39.838759
3043.557382	431417.843173	39.843776
3046.795217	432095.685123	39.848794
3050.070610	432764.411117	39.853812
3053.287882	433432.926405	39.858829
3056.062214	434122.438592	39.863847
3059.472024	434783.543885	39.868864
3062.411329	435469.144301	39.873882
3065.398370	436133.953434	39.878900
3068.968281	436808.756681	39.883917
3071.985791	437482.844270	39.888935
3074.855796	438172.332518	39.893952
3078.183413	438844.030152	39.898970
3081.516160	439517.506564	39.903988
3084.778086	440183.025593	39.909005
3087.302489	440881.076570	39.914023
3090.581445	441560.556882	39.919040
3093.640049	442237.217652	39.924058
3096.438205	442911.571714	39.929076
3099.485768	443603.943086	39.934093
3102.661131	444285.338278	39.939111
3105.657658	444960.565756	39.944128
3108.776340	445673.522875	39.949146
3112.031072	446354.239158	39.954164
3115.213264	447031.454337	39.959181
3118.096492	447712.595404	39.964199
3121.348861	448369.056348	39.969216
3124.530595	449035.431656	39.974234
3127.389920	449655.269782	39.979252
3130.604937	450307.227802	39.984269
3133.339336	450955.953511	39.989287
3136.105503	451635.075293	39.994304
3139.424340	452274.409063	39.999322
3142.161369	452942.058319	40.004340
3145.460978	453613.293628	40.009357
3148.130417	454290.074565	40.014375
3151.046101	454969.731577	40.019392
3154.363445	455663.423553	40.024410
3157.331932	456331.088306	40.029428
3160.480401	457052.495077	40.034445
3163.687114	457735.362166	40.039463
3166.518931	458474.280893	40.044480
3169.444770	459161.854266	40.049498
3172.877446	459858.585120	40.054516
3176.346066	460634.063458	40.059533
3178.915861	461365.641105	40.064551
3181.880326	462072.999986	40.069568
3185.575251	462838.043649	40.074586
3188.319665	463590.968481	40.079604
3192.196059	464300.437318	40.084621
3195.118995	465029.811811	40.089639
3197.939260	465837.023462	40.094656
3201.238760	466563.554538	40.099674
3204.599326	467316.351870	40.104692
3207.807039	468086.190865	40.109709
3211.498595	468842.522849	40.114727
3214.373823	469617.314604	40.119744
3218.318610	470351.906716	40.124762
3221.284005	471161.116243	40.129780
3224.856912	471893.184112	40.134797
3228.221386	472688.819756	40.139815
3231.471019	473417.496626	40.144832
3234.715839	474211.372916	40.149850
3237.618350	474955.774430	40.154868
3241.675852	475697.842547	40.159885
3244.742123	476500.201819	40.164903
3248.206701	477254.945396	40.169920
3251.227902	478022.874231	40.174938
3254.347802	478776.401695	40.179956
3258.353017	479512.523658	40.184973
3261.369545	480286.684420	40.189991
3264.427240	481084.008173	40.195008
3267.600270	481843.627371	40.200026
3270.840518	482624.635603	40.205044
3274.546454	483380.421402	40.210061
3277.499225	484148.829947	40.215079
3280.906507	484959.837629	40.220096
3284.114356	485728.951597	40.225114
3287.141119	486490.534432	40.230132
3290.417748	487264.376357	40.235149
3293.538367	488020.325313	40.240167
3296.279563	488753.871470	40.245184
3299.726154	489491.723648	40.250202
3302.901463	490236.814277	40.255220
3306.441704	490956.204920	40.260237
3309.929819	491690.023873	40.265255
3312.948079	492449.195962	40.270272
3316.159954	493226.137281	40.275290
3319.489912	493975.095300	40.280308
3322.545761	494709.115907	40.285325
3325.358142	495458.398591	40.290343
3328.441309	496226.041822	40.295360
3331.803014	496990.275669	40.300378
3334.981888	497765.868800	40.305396
3338.967670	498527.414396	40.310413
3342.138390	499348.338334	40.315431
3345.155513	500158.292192	40.320448
3348.664578	500927.486672	40.325466
3352.200482	501691.998882	40.330484
3355.454765	502538.967098	40.335501
3358.934123	503314.676967	40.340519
3362.524093	504109.619404	40.345536
3365.322476	504943.217457	40.350554
3368.721952	505717.218930	40.355572
3372.457702	506568.309035	40.360589
3375.381324	507398.590478	40.365607
3378.884032	508201.436475	40.370624
3382.450694	509021.949267	40.375642
3385.515103	509858.701751	40.380660
3389.208574	510689.813631	40.385677
3393.238745	511508.216887	40.390695
3396.355522	512341.509424	40.395712
3399.617482	513185.686980	40.400730
3402.573666	514031.838470	40.405748
3405.913469	514884.092285	40.410765
3409.406857	515742.080113	40.415783
3412.577626	516602.395477	40.420800
3416.706202	517435.780581	40.425818
3419.964434	518319.197024	40.430836
3423.063568	519208.643983	40.435853
3426.595217	520048.447988	40.440871
3430.537597	520875.435325	40.445888
3434.021590	521771.440774	40.450906
3437.057700	522668.930227	40.455924
3440.670470	523526.091283	40.460941
3444.516695	524394.464449	40.465959
3448.113822	525259.956447	40.470976
3451.628802	526107.315634	40.475994
3454.671093	526971.643553	40.481012
3458.046083	527842.727945	40.486029
3461.787353	528728.224153	40.491047
3465.369462	529599.683589	40.496064
3468.687535	530471.943146	40.501082
3472.161111	531356.578409	40.506100
3475.814192	532197.744212	40.511117
3480.072831	533011.665109	40.516122
3483.149945	533827.047755	40.521127
3486.557507	534557.516532	40.526132
3489.710476	535254.448946	40.531136
3492.398860	535904.850223	40.536141
3495.375386	536499.111098	40.541146
3498.279380	537028.657886	40.546151
3501.117177	537463.696487	40.551156
3503.353226	537829.067964	40.556160
3505.501011	538173.686804	40.561165
3507.850175	538464.933071	40.566170
3509.496606	538647.044665	40.571175
3511.135741	538840.872060	40.576180
3512.687221	539005.419128	40.581184
3513.958104	539098.042595	40.586189
3515.662079	539096.561324	40.591194
3515.947563	539136.059850	40.596199
3517.251214	539134.288331	40.601204
3517.834465	539130.156035	40.606208
3518.865806	539011.715623	40.611213
3520.033669	538892.091140	40.616218
3520.194889	538783.634624	40.621223
3520.931876	538663.924939	40.626228
3521.031880	538529.618158	40.631232
3521.401940	538350.772536	40.636237
3521.742427	538157.434337	40.641242
3521.885653	537932.406793	40.646247
3522.260316	537686.025277	40.651252
3522.230796	537503.192309	40.656256
3522.227086	537276.208536	40.661261
3522.572260	537055.580969	40.666266
3522.507440	536800.061959	40.671271
3522.535237	536567.607624	40.676276
3522.632520	536286.647395	40.681280
3523.002763	535995.233248	40.686285
3522.955767	535728.479767	40.691290
3521.547823	535481.687973	40.696295
3522.245179	535229.609009	40.701300
3521.860029	534978.101145	40.706304
3522.004010	534661.085845	40.711309
3522.420972	534373.321511	40.716314
3521.384784	534133.572530	40.721319
3521.419378	533892.084510	40.726324
3521.479501	533564.602480	40.731328
3520.978600	533311.216631	40.736333
3520.935656	533064.827432	40.741338
3520.652807	532766.837406	40.746343
3521.100029	532488.733959	40.751348
3520.155306	532268.141039	40.756352
3520.096841	531992.281261	40.761357
3519.899330	531747.310453	40.766362
3519.160019	531490.547476	40.771367
3519.309998	531252.133126	40.776372
3519.299326	530985.242129	40.781376
3518.851880	530736.050597	40.786381
3518.911358	530480.206009	40.791386
3518.362682	530257.602076	40.796391
3518.506928	529980.563277	40.801396
3517.677349	529776.693924	40.806400
3517.793002	529519.005693	40.811405
3517.109838	529293.276327	40.816410
3516.549178	529086.323501	40.821415
3516.887564	528871.544430	40.826420
3516.308887	528684.955177	40.831424
3516.588220	528430.963096	40.836429
3516.142015	528237.322960	40.841434
3515.701959	528060.862592	40.846439
3516.023056	527803.518356	40.851444
3515.358203	527635.225627	40.856448
3515.310924	527449.043295	40.861453
3515.332014	527213.519867	40.866458
3514.715733	527048.599533	40.871463
3514.850326	526851.161228	40.876468
3514.463531	526660.878900	40.881472
3513.782360	526508.497893	40.886477
3514.145049	526354.029795	40.891482
3513.536556	526177.322518	40.896487
3513.502201	526004.363977	40.901492
3513.303192	525837.393969	40.906496
3512.897708	525664.086053	40.911501
3513.129341	525482.992491	40.916506
3513.133741	525315.024525	40.921511
3512.859801	525201.033095	40.926516
3512.343112	525066.910605	40.931520
3512.309801	524862.094384	40.936525
3512.519520	524697.170995	40.941530
3512.295712	524556.426587	40.946535
3512.558109	524407.566663	40.951540
3511.718725	524264.692800	40.956544
3511.240020	524158.814439	40.961549
3511.640554	524049.813912	40.966554
3511.559127	523912.226115	40.971559
3511.505049	523773.571235	40.976564
3511.337847	523613.296597	40.981568
3511.688336	523448.287683	40.986573
3510.925350	523354.935581	40.991578
3510.381552	523264.429855	40.996583
3510.820117	523105.368857	41.001588
3510.227240	522974.425965	41.006592
3509.889672	522899.456383	41.011597
3510.449941	522745.225881	41.016602
3509.726824	522662.126195	41.021607
3509.893409	522574.537682	41.026612
3509.984178	522452.329791	41.031616
3509.623428	522325.440033	41.036621
3509.580035	522241.876881	41.041626
3509.296052	522150.059972	41.046631
3509.441905	522008.729481	41.051636
3508.861775	521962.561098	41.056640
3508.890819	521886.568319	41.061645
3509.362296	521754.587924	41.066650
3509.104796	521649.770539	41.071655
3508.909773	521577.704746	41.076660
3508.708884	521522.728507	41.081664
3508.558031	521384.371930	41.086669
3508.487582	521286.297612	41.091674
3507.684234	521238.999587	41.096679
3508.153677	521172.540258	41.101684
3508.102623	521118.246820	41.106688
3507.939265	521045.516397	41.111693
3507.852514	520972.773544	41.116698
3507.778492	520882.635398	41.121703
3508.202731	520769.867686	41.126708
3507.873870	520734.071746	41.131712
3507.569440	520636.030517	41.136717
3507.913291	520548.554827	41.141722
3507.364949	520503.439101	41.146727
3507.277428	520447.632343	41.151732
3507.242678	520370.530245	41.156736
3507.321789	520293.106414	41.161741
3506.769160	520255.120032	41.166746
3506.937880	520206.553012	41.171751
3506.896848	520145.277072	41.176756
3506.274044	520094.407782	41.181760
3506.429268	520049.887503	41.186765
3507.035220	520018.796357	41.191770
3507.005195	519971.119635	41.196775
3507.066843	519914.478473	41.201780
3506.678869	519828.227022	41.206784
3507.004156	519749.952703	41.211789
3507.052859	519685.171923	41.216794
3507.098675	519625.397263	41.221799
3506.169027	519590.351124	41.226804
3506.220233	519558.992834	41.231808
3505.940869	519514.438663	41.236813
3506.676166	519483.528329	41.241818
3506.302435	519408.497912	41.246823
3506.387762	519391.039411	41.251828
3506.552626	519360.926920	41.256832
3506.338611	519303.771006	41.261837
3506.556484	519249.479463	41.266842
3506.263596	519158.557412	41.271847
3505.982839	519123.053759	41.276852
3505.374961	519098.776915	41.281856
3505.694295	519073.038765	41.286861
3506.186866	519054.150250	41.291866
3505.979300	519031.377603	41.296871
3505.903524	518976.069673	41.301876
3505.780763	518925.724546	41.306880
3505.916003	518846.515211	41.311885
3506.045401	518824.093560	41.316890
3505.411127	518801.337468	41.321895
3505.206745	518764.910763	41.326900
3505.161816	518742.971661	41.331904
3504.767742	518727.155819	41.336909
3505.255461	518697.951879	41.341914
3504.989496	518673.468668	41.346919
3505.643901	518619.409473	41.351924
3505.342976	518586.082274	41.356928
3505.496704	518564.010402	41.361933
3505.648273	518549.625196	41.366938
3505.401695	518558.210259	41.371943
3505.485556	518505.757908	41.376948
3505.201542	518467.623814	41.381952
3505.254730	518436.414787	41.386957
3505.814791	518384.645318	41.391962
3505.569534	518389.336476	41.396967
3505.226005	518383.980014	41.401972
3505.375337	518338.292978	41.406976
3504.933170	518298.211308	41.411981
3505.260419	518233.987648	41.416986
3505.129560	518245.740434	41.421991
3505.294327	518237.218878	41.426996
3504.722874	518191.190232	41.432000
3504.554739	518173.011968	41.437005
3504.706345	518144.062453	41.442010
3504.879778	518141.961784	41.447015
3505.428319	518132.873828	41.452020
3505.070314	518107.190660	41.457024
3504.817044	518069.151930	41.462029
3504.964486	518052.187897	41.467034
3504.734949	518035.586845	41.472039
3505.084216	518014.949859	41.477044
3505.272680	518006.475010	41.482048
3505.445376	517938.633611	41.487053
3504.995811	517936.884229	41.492058
3504.901491	517924.812992	41.497063
3504.805778	517897.823796	41.502068
3504.863400	517898.371045	41.507072
3505.166618	517869.295950	41.512077
3505.324053	517828.359827	41.517082
3504.834767	517806.691996	41.522087
3505.089327	517786.373118	41.527092
3504.984767	517784.771474	41.532096
3504.561953	517757.631465	41.537101
3504.654495	517725.454042	41.542106
3504.527910	517708.027261	41.547111
3505.306805	517658.344914	41.552116
3505.396974	517632.286755	41.557120
3504.718597	517629.056374	41.562125
3505.024034	517607.970674	41.567130
3504.847312	517609.111250	41.572135
3504.911218	517583.107735	41.577140
3505.102657	517578.323884	41.582144
3504.619748	517557.716712	41.587149
3504.990801	517500.917252	41.592154
3504.799710	517500.492396	41.597159
3505.146922	517484.861638	41.602164
3505.064438	517452.964207	41.607168
3505.137063	517432.673652	41.612173
3505.262355	517416.471045	41.617178
3504.950949	517390.829976	41.622183
3505.201485	517366.516062	41.627188
3505.281418	517336.413320	41.632192
3504.789836	517302.456242	41.637197
3505.235716	517254.645913	41.642202
3504.895510	517255.610062	41.647207
3504.577096	517239.325693	41.652212
3504.746449	517236.466974	41.657216
3504.847564	517229.775559	41.662221
3505.064705	517198.032575	41.667226
3504.669728	517198.095084	41.672231
3504.833563	517155.032261	41.677236
3504.794799	517131.320023	41.682240
3504.647015	517103.124029	41.687245
3504.666498	517083.246027	41.692250
3504.961225	517051.895083	41.697255
3505.281708	517014.319559	41.702260
3504.137292	517025.929957	41.707264
3504.106841	517012.330782	41.712269
3504.429748	517000.091787	41.717274
3504.059110	516996.711497	41.722279
3505.045942	516974.455276	41.727284
3504.821809	516964.173910	41.732288
3504.811923	516951.582893	41.737293
3504.661762	516942.756438	41.742298
3504.714309	516929.548662	41.747303
3504.648120	516882.425074	41.752308
3504.856485	516838.747519	41.757312
3505.018614	516834.220955	41.762317
3504.241485	516822.307406	41.767322
3504.696257	516840.492589	41.772327
3504.650164	516829.778414	41.777332
3504.844374	516819.531988	41.782336
3504.649037	516807.880493	41.787341
3504.723899	516750.771277	41.792346
3504.871041	516711.553540	41.797351
3504.734322	516700.651311	41.802356
3504.106977	516707.780292	41.807360
3503.972105	516698.496128	41.812365
3504.080999	516668.033587	41.817370
3503.900002	516678.177040	41.822375
3504.904976	516661.227784	41.827380
3504.940500	516639.121469	41.832384
3504.943676	516611.153654	41.837389
3504.475688	516615.880510	41.842394
3504.258084	516605.800186	41.847399
3504.372277	516595.060529	41.852404
3504.213297	516581.936482	41.857408
3504.110853	516580.283813	41.862413
3504.664476	516588.085956	41.867418
3504.138351	516582.504896	41.872423
3504.409686	516557.579629	41.877428
3504.326834	516507.322018	41.882432
3504.399900	516492.037105	41.887437
3504.674109	516472.219266	41.892442
3504.329758	516517.942412	41.897447
3504.115822	516472.661692	41.902452
3504.237345	516438.201357	41.907456
3504.121143	516427.750878	41.912461
3504.411189	516440.702777	41.917466
3504.237960	516434.661297	41.922471
3504.684077	516393.423155	41.927476
3504.756277	516400.896876	41.932480
3504.381918	516413.245758	41.937485
3504.707139	516391.194479	41.942490
3504.289213	516361.067514	41.947495
3504.344915	516365.155350	41.952500
3504.480180	516372.315669	41.957504
3503.977333	516369.310168	41.962509
3504.369546	516337.841328	41.967514
3504.220046	516333.060432	41.972519
3504.299713	516314.082350	41.977524
3504.620324	516278.831598	41.982528
3504.651919	516245.649455	41.987533
3504.598478	516248.591341	41.992538
3504.045460	516253.483462	41.997543
3504.448695	516245.681828	42.002548
3504.878393	516248.243906	42.007552
3504.264913	516238.782253	42.012557
3504.484075	516169.914814	42.017562
3504.923378	516164.231606	42.022567
3504.347433	516154.662822	42.027572
3504.549888	516165.352886	42.032576
3504.305524	516144.099357	42.037581
3504.221988	516127.675628	42.042586
3503.531349	516123.485951	42.047591
3504.313324	516103.182822	42.052596
3504.568932	516104.609199	42.057600
3504.119631	516130.220917	42.062605
3504.544330	516123.326192	42.067610
3504.456609	516099.367350	42.072615
3504.286834	516088.722823	42.077620
3504.312965	516089.679714	42.082624
3504.358850	516065.750283	42.087629
3504.775943	516012.984541	42.092634
3504.544913	515984.142329	42.097639
3504.734176	515963.730404	42.102644
3504.752978	515965.699979	42.107648
3503.829039	515955.478016	42.112653
3504.745945	515930.045178	42.117658
3504.262697	515938.972446	42.122663
3503.571665	515931.596492	42.127668
3503.796974	515947.391264	42.132672
3504.077293	515906.329856	42.137677
3504.580323	515880.406017	42.142682
3504.116328	515910.622826	42.147687
3503.585162	515904.485996	42.152692
3503.784064	515895.957853	42.157696
3503.388736	515879.532581	42.162701
3503.528183	515874.048396	42.167706
3503.615585	515881.823404	42.172711
3504.090722	515865.361697	42.177716
3504.250958	515866.853745	42.182720
3504.197593	515907.525517	42.187725
3503.910496	515887.947429	42.192730
3504.014235	515874.123814	42.197735
3504.754476	515823.076570	42.202740
3504.543943	515828.774482	42.207744
3504.083585	515865.464571	42.212749
3504.111472	515839.160577	42.217754
3504.261273	515836.911627	42.222759
3504.129481	515828.638020	42.227764
3504.428378	515824.393027	42.232768
3504.026148	515822.838238	42.237773
3504.280190	515781.224336	42.242778
3503.778901	515773.970053	42.247783
3504.069870	515770.383794	42.252788
3504.371074	515749.397575	42.257792
3504.123546	515729.155551	42.262797
3504.271954	515711.986683	42.267802
3504.148907	515702.447213	42.272807
3504.098023	515688.900767	42.277812
3504.630117	515692.104247	42.282816
3503.713095	515711.771887	42.287821
3504.057257	515727.244623	42.292826
3504.137943	515695.368624	42.297831
3504.621261	515645.069520	42.302836
3504.485639	515657.735263	42.307840
3503.910269	515655.499746	42.312845
3504.488754	515607.967219	42.317850
3504.342145	515639.803395	42.322855
3504.462333	515639.531600	42.327860
3504.452968	515592.091935	42.332864
3504.093183	515571.007651	42.337869
3504.296379	515575.527563	42.342874
3503.611329	515576.748614	42.347879
3503.596507	515569.113895	42.352884
3503.604735	515559.351287	42.357888
3503.486399	515561.595470	42.362893
3503.779320	515566.404667	42.367898
3504.322714	515562.576160	42.372903
3504.075656	515572.528413	42.377908
3504.021432	515608.193910	42.382912
3504.344191	515551.395463	42.387917
3504.382573	515555.233348	42.392922
3503.938263	515595.360739	42.397927
3504.182579	515586.774684	42.402932
3504.579283	515526.424069	42.407936
3504.457610	515489.572511	42.412941
3503.867397	515512.982035	42.417946
3503.705620	515511.035173	42.422951
3504.140012	515502.064993	42.427956
3504.492079	515499.885186	42.432960
3504.285082	515492.027917	42.437965
3504.831078	515433.170694	42.442970
3504.907118	515422.840936	42.447975
3504.126925	515426.302448	42.452980
3503.843211	515406.015175	42.457984
3504.042115	515406.944799	42.462989
3504.470113	515397.570953	42.467994
3503.737512	515414.073977	42.472999
3503.867698	515399.284817	42.478004
3504.100391	515378.663006	42.483008
3504.009949	515391.625276	42.488013
3504.441270	515398.031134	42.493018
3504.204517	515409.398029	42.498023
3504.388727	515361.320186	42.503028
3504.969597	515312.066801	42.508032
3504.656546	515319.197270	42.513037
3504.745846	515284.992547	42.518042
3504.799778	515270.316482	42.523047
3504.747734	515242.759735	42.528052
3504.423309	515250.094343	42.533056
3503.685796	515245.658959	42.538061
3504.280159	515233.982713	42.543066
3504.044041	515244.388634	42.548071
3503.898847	515212.901466	42.553076
3504.241685	515233.533845	42.558080
3504.236005	515194.387289	42.563085
3504.005786	515191.439641	42.568090
3504.092517	515202.755550	42.573095
3504.635786	515161.903655	42.578100
3504.453332	515177.409550	42.583104
3504.167112	515183.625426	42.588109
3504.638552	515135.552120	42.593114
3504.436348	515161.429731	42.598119
3504.204317	515135.368027	42.603124
3504.184000	515105.782903	42.608128
3504.061448	515120.723019	42.613133
3504.361597	515061.599880	42.618138
3503.938542	515077.093316	42.623143
3504.329437	515099.336780	42.628148
3504.255449	515048.264136	42.633152
3503.860598	515056.975583	42.638157
3504.056101	515039.090483	42.643162
3503.855868	515051.261108	42.648167
3504.000105	515070.053664	42.653172
3504.332511	515021.344484	42.658176
3504.261439	515032.078502	42.663181
3504.610665	514983.113659	42.668186
3503.931581	515003.047991	42.673191
3504.281493	515004.763033	42.678196
3504.206864	514958.444628	42.683200
3504.119178	514986.782778	42.688205
3504.185643	514965.731524	42.693210
3504.334755	514935.512375	42.698215
3504.034340	514945.574589	42.703220
3504.147475	514919.407418	42.708224
3504.395287	514932.013108	42.713229
3504.024685	514928.581809	42.718234
3503.862354	514898.462395	42.723239
3504.198780	514887.180731	42.728244
3504.049448	514914.314845	42.733248
3503.948164	514906.491173	42.738253
3504.224460	514850.709286	42.743258
3504.045011	514883.108457	42.748263
3504.195313	514868.113335	42.753268
3504.565394	514836.746342	42.758272
3504.043072	514851.901617	42.763277
3504.271839	514849.842374	42.768282
3504.153582	514802.771746	42.773287
3504.168899	514817.589182	42.778292
3504.151504	514804.390786	42.783296
3504.060478	514828.329318	42.788301
3504.245052	514771.499499	42.793306
3503.831242	514775.510189	42.798311
3503.584392	514770.643072	42.803316
3504.001351	514779.883892	42.808321
3503.948729	514791.677317	42.813325
3504.418553	514733.436641	42.818330
3503.805618	514762.262820	42.823335
3504.135173	514777.789321	42.828340
3504.239702	514759.614825	42.833345
3503.848761	514750.420631	42.838349
3504.109348	514719.070725	42.843354
3504.464800	514692.207368	42.848359
3503.946102	514701.242051	42.853364
3504.121959	514691.047808	42.858369
3503.899692	514693.713170	42.863373
3504.121855	514697.876263	42.868378
3504.236316	514706.912034	42.873383
3504.155683	514645.723267	42.878388
3504.080466	514666.523575	42.883393
3504.140490	514643.247422	42.888397
3503.695212	514653.939663	42.893402
3504.273796	514678.784176	42.898407
3504.246378	514622.746057	42.903412
3504.773093	514583.008137	42.908417
3504.750525	514587.108777	42.913421
3505.015361	514554.999193	42.918426
3504.016776	514563.907471	42.923431
3503.658216	514549.801772	42.928436
3503.999804	514538.266159	42.933441
3503.560491	514547.490697	42.938445
3504.057335	514545.439629	42.943450
3503.843610	514538.948642	42.948455
3504.100618	514569.155066	42.953460
3504.126182	514538.802992	42.958465
3503.924090	514526.038210	42.963469
3504.082639	514509.271155	42.968474
3504.251152	514530.387172	42.973479
3504.234843	514536.358305	42.978484
3504.318449	514522.132120	42.983489
3504.200086	514500.451952	42.988493
3504.334629	514478.428303	42.993498
3504.152500	514478.305431	42.998503
3504.095931	514459.498528	43.003508
3503.946070	514442.021442	43.008513
3503.792841	514427.124480	43.013517
3504.019529	514413.077912	43.018522
3503.946030	514462.810289	43.023527
3503.853724	514433.184780	43.028532
3504.119059	514411.039211	43.033537
3504.388465	514405.432847	43.038541
3504.047531	514407.510041	43.043546
3503.699332	514413.027865	43.048551
3503.969815	514399.480170	43.053556
3503.806670	514379.425505	43.058561
3503.898237	514375.212917	43.063565
3504.718583	514351.006903	43.068570
3504.692570	514353.388397	43.073575
3504.238925	514347.744547	43.078580
3504.545750	514321.394095	43.083585
3505.045308	514290.005623	43.088589
3504.749644	514286.562348	43.093594
3504.418711	514282.315350	43.098599
3503.952012	514276.268891	43.103604
3504.111175	514291.367542	43.108609
3503.968637	514276.671082	43.113613
3504.035544	514229.721332	43.118618
3504.064409	514238.517976	43.123623
3504.276317	514198.930069	43.128628
3504.441287	514197.032574	43.133633
3503.805785	514217.163267	43.138637
3503.760410	514196.533378	43.143642
3503.621640	514189.372853	43.148647
3503.932964	514181.433051	43.153652
3503.872851	514181.240311	43.158657
3503.534465	514194.596758	43.163661
3503.973175	514180.971719	43.168666
3504.413043	514162.440093	43.173671
3503.967379	514185.069890	43.178676
3504.085167	514185.911241	43.183681
3504.257656	514178.296868	43.188685
3504.105190	514155.306531	43.193690
3503.646031	514161.803020	43.198695
3504.043717	514143.480366	43.203700
3504.649926	514106.915393	43.208705
3504.227546	514117.604353	43.213709
3504.226421	514135.257551	43.218714
3504.339392	514097.354231	43.223719
3504.308687	514067.111365	43.228724
3504.034975	514072.668109	43.233729
3504.272025	514097.162806	43.238733
3504.598993	514033.985302	43.243738
3504.240153	514038.594457	43.248743
3504.078369	514052.428921	43.253748
3504.671619	513986.932980	43.258753
3503.970448	514022.046518	43.263757
3504.467559	513988.685184	43.268762
3504.444086	513975.234190	43.273767
3504.171841	513990.553039	43.278772
3504.674310	513980.610240	43.283777
3504.319160	513927.909435	43.288781
3504.390309	513945.804319	43.293786
3504.472319	513940.935568	43.298791
3503.805996	513908.112026	43.303796
3503.954983	513893.217411	43.308801
3503.746299	513889.810889	43.313805
3504.641989	513870.650500	43.318810
3504.646255	513860.584040	43.323815
3504.362636	513865.383683	43.328820
3504.522169	513878.661684	43.333825
3504.433549	513856.065507	43.338829
3504.333362	513839.642174	43.343834
3504.192741	513823.933369	43.348839
3504.376695	513791.379876	43.353844
3504.477480	513761.216847	43.358849
3504.125866	513756.770653	43.363853
3504.406492	513753.084439	43.368858
3504.650459	513722.949295	43.373863
3504.187482	513711.894357	43.378868
3504.076086	513747.775157	43.383873
3504.131856	513739.774373	43.388877
3503.926180	513719.826811	43.393882
3504.312905	513713.695851	43.398887
3503.942954	513700.451146	43.403892
3503.716603	513696.693298	43.408897
3504.147419	513672.952543	43.413901
3504.299121	513667.819785	43.418906
3504.057481	513684.702141	43.423911
3504.204412	513643.909217	43.428916
3504.139983	513666.024207	43.433921
3503.794668	513670.327828	43.438925
3503.722190	513654.810427	43.443930
3503.578847	513634.397667	43.448935
3503.443670	513619.901802	43.453940
3503.888472	513617.858851	43.458945
3503.769726	513627.033224	43.463949
3504.140448	513609.827080	43.468954
3503.705607	513634.985052	43.473959
3504.005226	513645.408450	43.478964
3503.840266	513635.672100	43.483969
3504.019349	513607.974987	43.488973
3504.381396	513559.762738	43.493978
3504.192143	513548.360932	43.498983
3503.964029	513573.132240	43.503988
3503.713893	513561.891816	43.508993
3503.376090	513565.536694	43.513997
3503.701417	513547.730664	43.519002
3503.441734	513549.693953	43.524007
3503.595711	513527.868327	43.529012
3504.417944	513528.547793	43.534017
3503.673732	513550.669205	43.539021
3503.892265	513563.482879	43.544026
3503.879185	513600.511866	43.549031
3503.694738	513583.089940	43.554036
3504.404968	513571.191908	43.559041
3504.033551	513538.725704	43.564045
3504.285963	513517.238590	43.569050
3504.744180	513499.917340	43.574055
3504.372428	513519.046092	43.579060
3504.254049	513507.481308	43.584065
3503.908774	513486.493284	43.589069
3504.369362	513454.856507	43.594074
3504.070187	513481.966020	43.599079
3503.692450	513445.201045	43.604084
3504.567748	513419.720431	43.609089
3504.160437	513432.177865	43.614093
3503.890247	513443.753699	43.619098
3504.107358	513440.431541	43.624103
3504.018520	513429.519620	43.629108
3504.086268	513428.598494	43.634113
3504.132795	513441.540613	43.639117
3503.934264	513421.490403	43.644122
3504.038345	513402.100513	43.649127
3503.726178	513390.869778	43.654132
3504.137428	513396.773739	43.659137
3503.997786	513363.815315	43.664141
3503.435328	513342.659102	43.669146
3503.313942	513367.818513	43.674151
3503.754121	513370.885221	43.679156
3503.822947	513352.563104	43.684161
3503.235087	513356.652218	43.689165
3503.777938	513375.080160	43.694170
3503.893828	513354.828427	43.699175
3503.942255	513366.151622	43.704180
3503.782396	513373.916284	43.709185
3503.527115	513372.995625	43.714189
3503.249807	513369.498676	43.719194
3503.628451	513374.345539	43.724199
3503.649317	513366.248928	43.729204
3503.761785	513350.550267	43.734209
3503.667869	513359.316189	43.739213
3503.648749	513353.148075	43.744218
3503.443602	513356.367361	43.749223
3504.103502	513357.021907	43.754228
3504.396064	513345.341480	43.759233
3504.153841	513322.111277	43.764237
3504.097207	513292.680467	43.769242
3503.897884	513298.428042	43.774247
3504.037719	513289.199744	43.779252
3504.234518	513273.133595	43.784257
3504.152871	513274.664105	43.789261
3503.821127	513299.401607	43.794266
3504.236169	513288.207623	43.799271
3503.853926	513257.007188	43.804276
3504.411008	513240.631147	43.809281
3504.276368	513244.243984	43.814285
3503.754829	513261.373335	43.819290
3503.667101	513263.916487	43.824295
3503.815048	513284.025633	43.829300
3504.032252	513284.345477	43.834305
3503.548471	513268.235135	43.839309
3503.924060	513247.436388	43.844314
3503.860552	513196.255317	43.849319
3503.531595	513187.758651	43.854324
3503.795301	513223.581277	43.859329
3503.939706	513250.317548	43.864333
3503.848148	513242.896239	43.869338
3503.832023	513247.957284	43.874343
3503.989299	513255.823630	43.879348
3504.377557	513228.446926	43.884353
3504.046859	513214.386289	43.889357
3504.121425	513179.167946	43.894362
3504.535685	513157.806550	43.899367
3504.553260	513145.865941	43.904372
3504.635837	513130.677645	43.909377
3503.932642	513131.648803	43.914381
3503.206451	513113.856755	43.919386
3503.704478	513118.836578	43.924391
3503.551505	513131.304619	43.929396
3503.894233	513094.070923	43.934401
3503.577650	513125.483444	43.939405
3503.880707	513130.696415	43.944410
3504.315459	513103.514499	43.949415
3503.858450	513109.909879	43.954420
3503.909986	513124.723075	43.959425
3503.709925	513113.929699	43.964429
3503.708488	513088.536570	43.969434
3503.521997	513079.258564	43.974439
3503.589659	513089.820134	43.979444
3504.283149	513089.407108	43.984449
3503.879870	513091.342559	43.989453
3504.070490	513065.716704	43.994458
3504.517124	513063.420475	43.999463
3503.890063	513086.535667	44.004468
3504.152977	513057.964468	44.009473
3504.136779	513026.554003	44.014477
3504.103376	513027.520477	44.019482
3503.954603	513048.132061	44.024487
3503.869620	513022.549699	44.029492
3504.642667	512988.636941	44.034497
3504.045844	513023.331373	44.039501
3504.199621	512992.349244	44.044506
3504.460371	512963.272379	44.049511
3504.356030	512952.514356	44.054516
3503.671675	512970.984941	44.059521
3504.080045	512975.574297	44.064525
3504.320726	512968.707378	44.069530
3504.243252	512963.914137	44.074535
3503.828576	512939.597796	44.079540
3504.270989	512901.437393	44.084545
3504.255527	512878.373083	44.089549
3503.991321	512886.559141	44.094554
3503.404909	512891.609253	44.099559
3503.891043	512898.209747	44.104564
3503.909110	512890.568617	44.109569
3504.107636	512867.470472	44.114573
3504.064675	512897.423782	44.119578
3504.023349	512885.795809	44.124583
3503.681062	512862.176109	44.129588
3503.758389	512849.264727	44.134593
3503.652240	512854.491873	44.139597
3503.467451	512862.817147	44.144602
3503.537654	512857.545269	44.149607
3503.400268	512860.905695	44.154612
3504.383776	512832.928423	44.159617
3503.739544	512877.646540	44.164621
3503.778262	512859.530991	44.169626
3503.587407	512841.097609	44.174631
3503.560616	512850.966062	44.179636
3504.039521	512848.968216	44.184641
3503.782971	512820.326962	44.189645
3504.082025	512799.438593	44.194650
3504.460929	512808.939439	44.199655
3503.428832	512828.274504	44.204660
3503.492074	512832.918446	44.209665
3503.979062	512847.056039	44.214669
3504.098705	512823.009180	44.219674
3504.217985	512817.173094	44.224679
3503.714789	512829.848464	44.229684
3504.163210	512813.489187	44.234689
3503.905757	512826.580989	44.239693
3503.748586	512810.722104	44.244698
3503.997742	512793.534348	44.249703
3503.790553	512763.266461	44.254708
3503.295851	512756.768609	44.259713
3503.415316	512768.940931	44.264717
3503.057186	512760.499245	44.269722
3503.423461	512762.009593	44.274727
3503.152954	512774.698815	44.279732
3503.693869	512794.797018	44.284737
3504.149146	512811.570096	44.289741
3503.941285	512814.486401	44.294746
3503.792188	512799.637937	44.299751
3503.795765	512793.769544	44.304756
3503.791278	512780.567528	44.309761
3503.148148	512775.054266	44.314765
3504.086570	512750.422629	44.319770
3504.210077	512786.116582	44.324775
3503.900968	512779.083551	44.329780
3503.619487	512741.543053	44.334785
3504.277741	512720.091960	44.339789
3504.249970	512698.648093	44.344794
3504.157953	512707.059952	44.349799
3503.699863	512703.743193	44.354804
3504.240281	512673.508746	44.359809
3504.362024	512678.446999	44.364813
3504.212518	512698.907365	44.369818
3504.007510	512738.497854	44.374823
3503.742214	512721.846604	44.379828
3503.958038	512700.920682	44.384833
3504.227489	512697.134837	44.389837
3504.257840	512682.864938	44.394842
3504.239220	512686.661899	44.399847
3504.135622	512669.732113	44.404852
3504.081312	512634.887110	44.409857
3503.805421	512640.596422	44.414861
3504.169041	512637.301539	44.419866
3504.733930	512592.696673	44.424871
3504.130134	512585.608964	44.429876
3504.107110	512563.911247	44.434881
3504.233106	512575.020366	44.439885
3503.906195	512597.481750	44.444890
3504.121164	512590.466984	44.449895
3503.697898	512565.291500	44.454900
3504.327870	512536.863758	44.459905
3503.980176	512570.002153	44.464909
3503.871842	512567.186536	44.469914
3503.921148	512541.228122	44.474919
3503.860885	512551.354970	44.479924
3503.964297	512543.700196	44.484929
3503.767126	512527.897954	44.489933
3503.318130	512524.680895	44.494938
3503.897314	512513.915737	44.499943
3504.114312	512507.608825	44.504948
3504.212341	512483.514316	44.509953
3503.951784	512520.230668	44.514957
3503.943788	512504.145574	44.519962
3503.753135	512484.143596	44.524967
3503.783419	512480.699020	44.529972
3504.108555	512477.056084	44.534977
3503.975959	512503.432620	44.539981
3504.042996	512460.069576	44.544986
3503.521982	512443.610228	44.549991
3504.262170	512429.834967	44.554996
3504.597538	512412.582615	44.560001
3504.251431	512392.858032	44.565005
3504.123729	512380.282219	44.570010
3504.634357	512378.785173	44.575015
3504.173828	512360.242130	44.580020
3504.075629	512350.899183	44.585025
3503.867275	512389.883971	44.590029
3503.858076	512356.700628	44.595034
3504.194113	512337.171690	44.600039
3503.697813	512319.848339	44.605044
3503.928122	512340.046760	44.610049
3503.871257	512359.531742	44.615053
3503.678011	512346.612156	44.620058
3504.200434	512331.657150	44.625063
3503.900257	512311.722866	44.630068
3503.946134	512343.939521	44.635073
3503.849646	512337.682091	44.640077
3503.731313	512299.558376	44.645082
3503.702940	512289.749078	44.650087
3503.485078	512289.530661	44.655092
3504.032668	512271.131711	44.660097
3504.331619	512271.843353	44.665101
3503.876609	512308.641481	44.670106
3504.089879	512281.493258	44.675111
3503.944870	512291.987763	44.680116
3504.068760	512248.261086	44.685121
3504.077052	512270.568748	44.690125
3503.873797	512238.124062	44.695130
3504.632252	512245.238231	44.700135
3503.906081	512255.166977	44.705140
3504.143161	512210.865856	44.710145
3504.861706	512194.564468	44.715149
3504.555977	512167.902788	44.720154
3504.695084	512155.992863	44.725159
3503.457402	512171.465935	44.730164
3503.886417	512157.385524	44.735169
3503.485128	512146.218636	44.740173
3503.715145	512132.169656	44.745178
3504.078556	512104.592722	44.750183
3503.855761	512105.538594	44.755188
3504.104555	512155.125628	44.760193
3504.311501	512145.127293	44.765197
3503.931538	512126.874786	44.770202
3504.706095	512085.624815	44.775207
3504.497595	512082.572010	44.780212
3504.029585	512076.626141	44.785217
3503.564681	512105.079317	44.790221
3503.913540	512095.766749	44.795226
3504.007706	512071.216980	44.800231
3503.138858	512072.163785	44.805236
3503.136798	512071.051268	44.810241
3504.062336	512041.968938	44.815245
3503.488475	512050.710213	44.820250
3503.756979	512093.768500	44.825255
3503.703844	512093.726395	44.830260
3503.911354	512074.672758	44.835265
3503.517845	512081.362010	44.840269
3503.546366	512086.264581	44.845274
3503.405512	512072.172992	44.850279
3503.646724	512084.680675	44.855284
3503.872524	512102.249537	44.860289
3503.788335	512110.154578	44.865293
3503.649597	512114.931813	44.870298
3503.724539	512103.740217	44.875303
3503.631972	512093.435077	44.880308
3503.727299	512061.448739	44.885313
3503.450830	512064.881891	44.890317
3503.646222	512062.928764	44.895322
3503.752030	512066.149734	44.900327
3503.255179	512061.017819	44.905332
3503.898292	512029.703661	44.910337
3503.770374	512057.193078	44.915341
3503.502205	512075.801203	44.920346
3503.628404	512035.513570	44.925351
3503.677971	512070.967771	44.930356
3503.684769	512081.033713	44.935361
3503.742995	512048.496751	44.940365
3503.775002	512089.113632	44.945370
3503.882187	512056.821886	44.950375
3503.868423	512053.890062	44.955380
3503.985748	512081.290093	44.960385
3503.945236	512051.399296	44.965389
3503.463546	512022.033464	44.970394
3504.137239	511997.999049	44.975399
3503.549475	512044.835114	44.980404
3504.031295	512051.031920	44.985409
3503.644147	512047.450880	44.990413
3503.326865	512030.098940	44.995418
3503.740744	512025.076015	45.000423
3503.804251	512000.935691	45.005428
3503.973055	512034.853487	45.010433
3503.976169	512027.163746	45.015437
3503.621384	512009.868300	45.020442
3504.100690	511966.894133	45.025447
3503.695680	512018.760176	45.030452
3503.872677	511993.590150	45.035457
3503.574425	511997.229109	45.040461
3503.269908	512004.056089	45.045466
3504.322066	511989.371177	45.050471
3503.751083	511999.427307	45.055476
3503.814602	511978.423395	45.060481
3503.994584	511950.622264	45.065485
3503.769958	511951.821373	45.070490
3503.801257	511958.190593	45.075495
3503.547975	511997.132792	45.080500
3503.504551	511956.517666	45.085505
3503.915036	511930.147122	45.090509
3503.525225	511936.279377	45.095514
3503.807129	511962.186536	45.100519
3503.618299	511987.358648	45.105524
3503.676631	511931.955721	45.110529
3504.333309	511945.055488	45.115533
3503.566439	511937.183871	45.120538
3503.264001	511945.275246	45.125543
3503.608196	511935.457449	45.130548
3503.546436	511925.147337	45.135553
3503.564806	511945.430311	45.140557
3503.598251	511943.502766	45.145562
3503.692728	511912.173927	45.150567
3503.701533	511955.779489	45.155572
3503.574031	511953.624443	45.160577
3503.976031	511912.989403	45.165581
3503.673390	511913.189084	45.170586
3504.272679	511908.541525	45.175591
3503.991481	511921.030718	45.180596
3503.496735	511911.446675	45.185601
3503.440034	511913.023952	45.190605
3504.070031	511897.798626	45.195610
3503.868629	511873.902343	45.200615
3503.944928	511926.249068	45.205620
3503.885955	511912.346757	45.210625
3504.054010	511896.941499	45.215629
3503.768393	511912.972564	45.220634
3503.947046	511922.505557	45.225639
3503.480820	511917.014642	45.230644
3503.647010	511900.648508	45.235649
3503.655146	511868.321471	45.240653
3503.479541	511872.194014	45.245658
3503.770851	511860.512768	45.250663
3503.774821	511868.555752	45.255668
3503.891892	511859.127925	45.260673
3503.860667	511842.287054	45.265677
3503.959013	511846.723364	45.270682
3503.949534	511860.636716	45.275687
3503.347363	511880.107254	45.280692
3503.476985	511873.105683	45.285697
3503.535899	511876.738806	45.290701
3503.799144	511897.489017	45.295706
3504.334196	511869.075166	45.300711
3503.954858	511826.539881	45.305716
3503.775519	511822.824773	45.310721
3503.852236	511806.422101	45.315725
3503.931081	511801.300296	45.320730
3504.323734	511812.671299	45.325735
3503.640171	511818.597082	45.330740
3504.040150	511781.654999	45.335745
3504.222578	511774.746219	45.340749
3504.035713	511790.002964	45.345754
3504.096628	511782.405154	45.350759
3503.795641	511759.283277	45.355764
3504.022519	511740.529737	45.360769
3504.204677	511735.290406	45.365773
3504.298949	511726.979059	45.370778
3504.064504	511753.777560	45.375783
3503.793457	511780.531216	45.380788
3503.764478	511745.781567	45.385793
3503.578889	511725.676720	45.390797
3502.945271	511730.987575	45.395802
3503.747498	511719.073718	45.400807
3503.862307	511717.487409	45.405812
3503.855968	511697.000077	45.410817
3503.776811	511722.509367	45.415821
3503.747378	511757.824939	45.420826
3503.814616	511743.801366	45.425831
3503.433313	511740.826400	45.430836
3503.947487	511708.722615	45.435841
3503.870070	511749.256422	45.440845
3503.407851	511747.154251	45.445850
3503.870156	511712.276299	45.450855
3503.657715	511706.998148	45.455860
3503.513463	511713.192850	45.460865
3503.924898	511676.552261	45.465869
3503.519481	511723.360388	45.470874
3503.596675	511681.005529	45.475879
3503.566886	511661.988935	45.480884
3503.467555	511692.206219	45.485889
3503.612711	511715.909460	45.490893
3503.331672	511704.824454	45.495898
3503.725510	511713.767079	45.500903
3503.639501	511695.417061	45.505908
3503.397977	511723.481446	45.510913
3503.557195	511713.895112	45.515917
3503.529479	511699.937099	45.520922
3504.101511	511683.607793	45.525927
3503.814242	511731.156056	45.530932
3503.586191	511700.333100	45.535937
3503.956399	511699.667610	45.540941
3503.730061	511728.690772	45.545946
3503.730867	511697.376343	45.550951
3503.467642	511727.417112	45.555956
3503.800901	511744.261119	45.560961
3503.396813	511705.169466	45.565965
3503.579785	511681.667462	45.570970
3503.815431	511705.761127	45.575975
3503.598062	511719.302741	45.580980
3503.460542	511713.405687	45.585985
3503.717701	511709.318035	45.590989
3503.771961	511679.006897	45.595994
3504.146028	511690.785630	45.600999
3503.694384	511697.888929	45.606004
3504.017942	511672.037612	45.611009
3504.046995	511686.855614	45.616013
3503.866373	511703.376170	45.621018
3504.243991	511654.903120	45.626023
3504.001077	511638.399037	45.631028
3503.661292	511672.802646	45.636033
3503.905078	511650.505120	45.641037
3503.971858	511621.406034	45.646042
3503.591120	511657.940881	45.651047
3503.667161	511666.529047	45.656052
3503.871286	511641.253037	45.661057
3503.738293	511617.143227	45.666061
3503.904480	511603.306256	45.671066
3503.816420	511644.196117	45.676071
3503.622023	511624.193720	45.681076
3503.973351	511592.216632	45.686081
3504.156433	511630.989521	45.691085
3503.948373	511634.209590	45.696090
3504.332981	511568.838490	45.701095
3504.062976	511599.689981	45.706100
3503.829925	511571.397032	45.711105
3504.436201	511541.656064	45.716109
3504.148621	511575.798672	45.721114
3503.941856	511552.459266	45.726119
3504.315735	511519.112570	45.731124
3503.712193	511560.842940	45.736129
3503.655576	511561.661399	45.741133
3503.885077	511537.038882	45.746138
3504.280402	511514.717228	45.751143
3503.944335	511498.075965	45.756148
3504.416117	511472.807993	45.761153
3503.806780	511475.383261	45.766157
3503.888971	511500.513256	45.771162
3503.922961	511500.912683	45.776167
3503.854036	511454.786159	45.781172
3504.045295	511444.587536	45.786177
3504.370651	511438.718410	45.791181
3504.009582	511434.728402	45.796186
3504.153602	511422.311294	45.801191
3503.854227	511411.886658	45.806196
3503.695936	511409.078745	45.811201
3503.939713	511410.760346	45.816205
3503.574027	511438.996591	45.821210
3503.390879	511462.499125	45.826215
3503.248343	511449.064949	45.831220
3503.670295	511426.131898	45.836225
3503.602595	511422.297878	45.841229
3503.207306	511467.638008	45.846234
3503.495497	511468.250207	45.851239
3503.442117	511474.885937	45.856244
3503.244339	511465.052349	45.861249
3503.699015	511460.022811	45.866253
3503.203818	511462.478863	45.871258
3503.425414	511463.708661	45.876263
3503.181330	511460.964905	45.881268
3503.271932	511465.149591	45.886273
3503.328045	511470.503283	45.891277
3503.145360	511486.366712	45.896282
3502.449498	511491.383942	45.901287
3503.115329	511484.297465	45.906292
3503.486849	511465.874889	45.911297
3503.567729	511458.931441	45.916301
3503.297266	511485.432519	45.921306
3503.531493	511520.504554	45.926311
3503.831006	511522.885585	45.931316
3503.207269	511505.025062	45.936321
3503.688608	511469.688304	45.941325
3503.483376	511523.497262	45.946330
3503.614939	511501.571403	45.951335
3503.630820	511487.151022	45.956340
3503.647843	511515.781958	45.961345
3504.085553	511480.958011	45.966349
3503.389733	511526.901964	45.971354
3503.835949	511493.695554	45.976359
3503.690104	511477.074795	45.981364
3503.686424	511479.048446	45.986369
3503.812898	511472.401334	45.991373
3503.949272	511481.030648	45.996378
3503.123914	511506.911142	46.001383
3503.258574	511523.179684	46.006388
3503.429982	511532.966987	46.011393
3503.857262	511520.252235	46.016397
3503.721253	511507.019430	46.021402
3504.259803	511486.546906	46.026407
3503.414269	511498.214991	46.031412
3503.605007	511500.157913	46.036417
3503.628576	511498.687183	46.041421
3503.589757	511463.078495	46.046426
3503.061144	511472.015271	46.051431
3503.141522	511504.936309	46.056436
3503.555594	511531.784430	46.061441
3503.894620	511555.659610	46.066445
3503.373724	511569.299904	46.071450
3503.626281	511568.400059	46.076455
3503.508391	511564.928127	46.081460
3503.590281	511551.407972	46.086465
3503.984947	511495.393991	46.091469
3503.876384	511490.402891	46.096474
3504.217477	511465.104973	46.101479
3503.848228	511482.970878	46.106484
3503.409014	511486.379276	46.111489
3503.784120	511494.060244	46.116493
3503.610531	511526.414307	46.121498
3504.029008	511500.547730	46.126503
3503.800203	511482.220051	46.131508
3503.852084	511479.480111	46.136513
3503.769977	511487.385111	46.141517
3503.937057	511438.135293	46.146522
3503.635410	511451.336313	46.151527
3503.623682	511456.043069	46.156532
3503.339351	511461.298802	46.161537
3503.827511	511478.068001	46.166541
3503.654233	511494.182883	46.171546
3503.837582	511465.065107	46.176551
3503.991594	511481.027095	46.181556
3503.764449	511446.308156	46.186561
3504.147491	511410.430327	46.191565
3504.053824	511409.989909	46.196570
3503.386938	511422.186296	46.201575
3504.123606	511409.321385	46.206580
3504.202129	511388.921451	46.211585
3504.261802	511386.989699	46.216589
3503.712070	511377.464634	46.221594
3503.618563	511361.644925	46.226599
3503.964952	511364.271519	46.231604
3503.995244	511404.333813	46.236609
3503.730375	511421.727978	46.241613
3503.565621	511419.882289	46.246618
3503.870598	511410.829233	46.251623
3504.013209	511413.791562	46.256628
3503.847161	511408.860113	46.261633
3504.037796	511374.378536	46.266637
3503.640810	511341.558045	46.271642
3504.071819	511338.960521	46.276647
3503.991246	511355.263241	46.281652
3503.982431	511322.128414	46.286657
3503.907792	511306.103313	46.291661
3503.715619	511309.219752	46.296666
3503.228361	511314.153473	46.301671
3503.181376	511330.653267	46.306676
3503.431367	511368.960869	46.311681
3503.788104	511347.707479	46.316685
3503.922744	511318.597153	46.321690
3503.815047	511304.094969	46.326695
3503.891326	511290.879034	46.331700
3503.977981	511285.907611	46.336705
3503.904739	511309.392984	46.341709
3503.344920	511336.597693	46.346714
3503.560550	511350.020576	46.351719
3503.527663	511350.835294	46.356724
3503.420697	511318.828948	46.361729
3504.063413	511285.591077	46.366733
3503.532221	511311.678322	46.371738
3503.149320	511328.787697	46.376743
3503.380623	511331.078356	46.381748
3503.456661	511340.931432	46.386753
3503.772269	511356.766816	46.391757
3503.716111	511352.475650	46.396762
3503.936172	511298.006310	46.401767
3504.382549	511297.986436	46.406772
3504.109527	511281.689126	46.411777
3504.227673	511257.387347	46.416781
3503.870279	511257.292146	46.421786
3503.809938	511264.384369	46.426791
3503.836864	511266.656748	46.431796
3503.885740	511259.010018	46.436801
3503.833785	511279.254307	46.441805
3503.521639	511297.010201	46.446810
3503.486292	511295.245225	46.451815
3503.548432	511292.098915	46.456820
3503.686864	511303.915157	46.461825
3503.883800	511294.575576	46.466829
3503.523726	511284.666354	46.471834
3503.672271	511245.840435	46.476839
3503.728274	511246.944650	46.481844
3503.611876	511256.979958	46.486849
3503.693316	511292.076609	46.491853
3503.477137	511272.279602	46.496858
3503.983906	511246.348097	46.501863
3503.748015	511233.080274	46.506868
3503.504745	511212.073317	46.511873
3503.975566	511202.133907	46.516877
3503.735588	511251.193736	46.521882
3503.755535	511245.119862	46.526887
3503.257475	511227.947447	46.531892
3503.695357	511217.456760	46.536897
3503.623467	511258.446169	46.541901
3503.592847	511248.889578	46.546906
3504.148594	511221.280822	46.551911
3504.327026	511223.579851	46.556916
3503.772405	511210.109435	46.561921
3503.851678	511189.203243	46.566925
3503.803071	511180.408309	46.571930
3503.557371	511225.523077	46.576935
3503.824243	511218.701906	46.581940
3503.462564	511193.565249	46.586945
3504.205095	511169.923515	46.591949
3503.723518	511182.647277	46.596954
3503.895060	511230.073829	46.601959
3503.893612	511221.726774	46.606964
3503.350530	511200.868368	46.611969
3504.164556	511174.230519	46.616973
3503.546753	511210.449657	46.621978
3503.703045	511178.806162	46.626983
3503.993436	511150.227426	46.631988
3503.821325	511175.296911	46.636993
3503.612800	511168.500265	46.641997
3504.115689	511152.231972	46.647002
3503.990523	511147.799889	46.652007
3504.044463	511176.627920	46.657012
3503.310053	511150.487713	46.662017
3503.544006	511131.732387	46.667021
3504.078232	511117.179181	46.672026
3504.180667	511116.050087	46.677031
3503.843973	511124.956709	46.682036
3504.022465	511112.028025	46.687041
3504.373689	511101.652145	46.692045
3503.877388	511086.857061	46.697050
3503.710882	511068.114367	46.702055
3504.350579	511067.203900	46.707060
3504.174297	511077.147597	46.712065
3504.392686	511056.118074	46.717069
3503.977969	511048.898654	46.722074
3503.968405	511073.031966	46.727079
3503.815976	511070.172480	46.732084
3503.438064	511062.694296	46.737089
3503.644290	511063.875961	46.742093
3503.494266	511076.294447	46.747098
3503.267705	511061.507300	46.752103
3503.310175	511059.780592	46.757108
3504.061753	511042.612850	46.762113
3504.129679	511035.114781	46.767117
3503.543837	511059.490964	46.772122
3503.938822	511078.045954	46.777127
3503.619032	511038.635907	46.782132
3503.256188	511032.926002	46.787137
3503.793211	511027.377417	46.792141
3503.386711	511045.553209	46.797146
3503.362732	511037.917894	46.802151
3503.684837	511042.015505	46.807156
3503.804849	511064.711812	46.812161
3503.818730	511061.522495	46.817165
3503.484818	511061.170629	46.822170
3503.461181	511057.430745	46.827175
3503.698457	511053.194308	46.832180
3503.438121	511059.306411	46.837185
3503.781035	511038.813683	46.842189
3503.196726	511044.471089	46.847194
3502.948040	511035.454749	46.852199
3503.684093	511029.824118	46.857204
3503.342287	511030.080587	46.862209
3503.262470	511032.622821	46.867213
3502.972152	511053.259186	46.872218
3503.302792	511061.453283	46.877223
3503.717958	511071.505869	46.882228
3503.921524	511060.950939	46.887233
3504.068872	511049.797800	46.892237
3504.051431	511026.579525	46.897242
3503.997430	511017.127681	46.902247
3503.980376	511019.811769	46.907252
3503.853641	511036.678586	46.912257
3503.729651	511064.523114	46.917261
3503.494033	511076.702175	46.922266
3503.670779	511071.463497	46.927271
3503.910495	511071.729239	46.932276
3503.608238	511062.519018	46.937281
3503.772948	511045.241669	46.942285
3503.737775	511048.889839	46.947290
3503.829653	511028.436774	46.952295
3503.449619	511015.343336	46.957300
3503.754490	510990.050442	46.962305
3503.994320	510982.575771	46.967309
3503.967033	511028.516582	46.972314
3504.079547	511044.283174	46.977319
3503.635687	511000.491261	46.982324
3503.132846	510984.887670	46.987329
3504.325764	510968.206600	46.992333
3504.020721	510951.863445	46.997338
3503.814336	510950.024284	47.002343
3503.592126	510999.284391	47.007348
3503.761469	510980.033203	47.012353
3503.683311	510957.988021	47.017357
3503.697763	510951.409003	47.022362
3503.907946	510966.148412	47.027367
3504.013537	510950.145082	47.032372
3503.832790	510933.428129	47.037377
3503.833807	510906.210086	47.042381
3503.659922	510917.570046	47.047386
3503.832974	510910.358853	47.052391
3503.655048	510927.840960	47.057396
3503.213926	510937.927777	47.062401
3503.463172	510944.566475	47.067405
3503.291041	510952.637723	47.072410
3503.228525	510946.627368	47.077415
3504.068041	510960.204907	47.082420
3503.740651	510972.044410	47.087425
3504.039119	510971.592596	47.092429
3504.009184	510979.287221	47.097434
3503.905259	510960.332156	47.102439
3503.833891	510968.994561	47.107444
3503.462951	510945.275546	47.112449
3504.227366	510891.629517	47.117453
3503.674190	510919.491521	47.122458
3503.604461	510914.949434	47.127463
3504.381566	510879.918852	47.132468
3503.698088	510905.271916	47.137473
3503.551383	510905.092823	47.142477
3503.483339	510917.549058	47.147482
3503.680622	510928.496212	47.152487
3503.735141	510940.680104	47.157492
3503.689538	510890.754051	47.162497
3504.079053	510885.431098	47.167501
3503.836304	510899.584465	47.172506
3503.899138	510908.630419	47.177511
3504.115107	510909.557601	47.182516
3503.848414	510903.225363	47.187521
3504.001130	510898.445750	47.192525
3503.716166	510884.477138	47.197530
3503.723615	510845.622020	47.202535
3503.617116	510850.748651	47.207540
3503.634889	510869.414077	47.212545
3503.855422	510830.626430	47.217549
3503.690778	510804.648599	47.222554
3503.473946	510835.037741	47.227559
3503.682391	510833.487143	47.232564
3503.635504	510860.560947	47.237569
3504.015559	510836.773680	47.242573
3503.983053	510810.522017	47.247578
3503.793127	510814.650017	47.252583
3503.507697	510839.231990	47.257588
3503.619048	510862.435846	47.262593
3504.148050	510806.600745	47.267597
3503.427499	510825.686458	47.272602
3503.565552	510825.462358	47.277607
3504.086374	510780.758548	47.282612
3503.433482	510800.137143	47.287617
3503.618434	510806.431917	47.292621
3503.517417	510829.112878	47.297626
3503.626288	510832.738328	47.302631
3503.712738	510830.599916	47.307636
3503.760208	510826.342830	47.312641
3503.764878	510786.020869	47.317645
3504.004078	510776.977875	47.322650
3503.475285	510803.217288	47.327655
3503.879992	510813.979957	47.332660
3503.889901	510825.007382	47.337665
3503.908389	510758.072129	47.342669
3504.088980	510753.945760	47.347674
3503.591325	510771.478559	47.352679
3504.325617	510755.274500	47.357684
3503.922066	510753.213522	47.362689
3503.907072	510787.466394	47.367693
3503.805994	510759.151242	47.372698
3503.036969	510741.312881	47.377703
3503.288260	510749.266712	47.382708
3503.537470	510766.681475	47.387713
3503.522750	510768.353405	47.392717
3503.421615	510782.383303	47.397722
3503.846177	510770.629664	47.402727
3503.857110	510758.030744	47.407732
3503.646538	510741.723048	47.412737
3504.054112	510722.282145	47.417741
3504.339839	510703.922903	47.422746
3503.766898	510711.905836	47.427751
3504.110345	510729.710476	47.432756
3503.719881	510748.187597	47.437761
3503.931490	510727.968207	47.442765
3503.623848	510703.581162	47.447770
3503.460206	510695.006527	47.452775
3504.088448	510672.343415	47.457780
3504.069742	510686.360364	47.462785
3504.274157	510676.412165	47.467789
3504.221710	510701.817571	47.472794
3503.634236	510707.222628	47.477799
3503.907315	510674.598503	47.482804
3503.356126	510662.240129	47.487809
3503.685094	510645.847069	47.492813
3503.285891	510663.060868	47.497818
3503.783609	510679.222241	47.502823
3504.275308	510681.168283	47.507828
3503.896756	510667.720202	47.512833
3504.112183	510635.408665	47.517837
3504.046675	510616.902474	47.522842
3504.018292	510603.955511	47.527847
3503.983856	510605.225837	47.532852
3503.493361	510623.263574	47.537857
3503.658817	510645.852070	47.542861
3503.527754	510652.247438	47.547866
3503.733012	510635.975104	47.552871
3503.887750	510626.237094	47.557876
3503.850104	510615.972974	47.562881
3504.142391	510597.764356	47.567885
3503.841806	510594.219918	47.572890
3503.796112	510605.610416	47.577895
3504.052217	510613.209406	47.582900
3503.979638	510619.291991	47.587905
3504.200175	510607.621078	47.592909
3504.083640	510590.741866	47.597914
3504.133410	510585.523109	47.602919
3504.328062	510577.751851	47.607924
3503.980972	510580.336394	47.612929
3503.782182	510549.962067	47.617933
3504.015644	510536.366563	47.622938
3503.747942	510517.689852	47.627943
3503.642632	510509.662419	47.632948
3504.257555	510495.197118	47.637953
3504.736732	510468.813469	47.642957
3504.195695	510449.269222	47.647962
3503.833116	510444.419147	47.652967
3504.239768	510456.648915	47.657972
3503.998876	510485.018784	47.662977
3504.092880	510467.650844	47.667981
3503.902828	510458.726117	47.672986
3503.569518	510438.541918	47.677991
3503.338694	510433.367462	47.682996
3503.777156	510433.348841	47.688001
3504.032523	510444.590679	47.693005
3503.764893	510459.861374	47.698010
3503.658533	510452.795334	47.703015
3504.080925	510453.791101	47.708020
3503.712932	510412.363535	47.713025
3504.166804	510381.430425	47.718029
3503.853957	510390.788992	47.723034
3503.921955	510398.316622	47.728039
3503.848677	510413.657825	47.733044
3503.738495	510392.831197	47.738049
3503.841482	510380.773969	47.743053
3504.163588	510356.489270	47.748058
3503.792582	510361.253110	47.753063
3503.891735	510370.141830	47.758068
3503.397206	510335.007562	47.763073
3503.777992	510368.136271	47.768077
3503.688979	510373.260280	47.773082
3503.430817	510355.897294	47.778087
3503.984516	510326.972015	47.783092
3503.728223	510354.079715	47.788097
3503.911491	510361.032624	47.793101
3503.823355	510340.860153	47.798106
3503.667160	510349.384500	47.803111
3503.876471	510347.783129	47.808116
3503.780287	510330.343924	47.813121
3503.618790	510305.275508	47.818125
3504.019976	510310.018504	47.823130
3503.865686	510323.854807	47.828135
3504.050841	510290.737922	47.833140
3503.665317	510340.835216	47.838145
3503.871342	510332.859679	47.843149
3503.688940	510311.083104	47.848154
3503.671016	510278.504219	47.853159
3504.272174	510241.375244	47.858164
3503.768727	510248.133174	47.863169
3503.814389	510296.442287	47.868173
3503.793936	510291.032168	47.873178
3503.642427	510286.148689	47.878183
3503.821459	510296.997945	47.883188
3503.631638	510298.444630	47.888193
3504.052300	510269.894433	47.893197
3503.851426	510278.628247	47.898202
3503.751231	510269.790407	47.903207
3503.799109	510232.748857	47.908212
3504.242386	510203.992603	47.913217
3504.047075	510230.787300	47.918221
3503.850285	510274.328454	47.923226
3503.868930	510241.844906	47.928231
3503.519608	510199.250235	47.933236
3503.047977	510211.416616	47.938241
3503.835011	510190.346753	47.943245
3504.119374	510179.727920	47.948250
3503.947321	510181.374179	47.953255
3503.866739	510193.276397	47.958260
3503.722848	510193.248630	47.963265
3504.248857	510172.219999	47.968269
3503.785791	510180.236404	47.973274
3503.845517	510166.870440	47.978279
3503.859689	510187.206754	47.983284
3503.676610	510171.501289	47.988289
3503.698272	510156.522349	47.993293
3503.591451	510146.370067	47.998298
3503.293860	510155.321604	48.003303
3504.248359	510139.739877	48.008308
3504.252582	510136.045982	48.013313
3504.188773	510117.488390	48.018317
3503.841784	510148.304065	48.023322
3503.700966	510143.621229	48.028327
3503.655177	510114.790342	48.033332
3504.123000	510094.883868	48.038337
3504.330176	510095.255957	48.043341
3504.022100	510080.986780	48.048346
3503.838507	510054.707247	48.053351
3504.079578	510060.487490	48.058356
3503.945333	510095.671273	48.063361
3503.948784	510076.748853	48.068365
3503.517683	510079.852682	48.073370
3504.072001	510058.819439	48.078375
3504.143381	510075.099360	48.083380
3503.691844	510052.403716	48.088385
3504.076380	510027.501562	48.093389
3504.208862	510050.854958	48.098394
3503.755773	510029.879711	48.103399
3504.409755	510009.842529	48.108404
3504.293455	509983.147501	48.113409
3504.283305	509970.956085	48.118413
3504.070040	509971.344033	48.123418
3503.712018	509960.219466	48.128423
3503.872617	509951.694400	48.133428
3503.328501	509998.630342	48.138433
3503.535486	509975.324580	48.143437
3503.574020	509977.038764	48.148442
3503.356216	509964.121255	48.153447
3503.957187	509946.824446	48.158452
3503.469395	509999.873341	48.163457
3503.745844	509972.863255	48.168461
3503.809537	509957.270373	48.173466
3503.474965	509991.980091	48.178471
3503.104131	509985.765159	48.183476
3503.549834	509977.296233	48.188481
3503.454363	509952.469836	48.193485
3503.530968	509961.463519	48.198490
3503.208822	509957.163448	48.203495
3503.522268	509941.581673	48.208500
3503.327327	509985.477423	48.213505
3503.690638	510002.824336	48.218509
3503.367848	510004.545029	48.223514
3503.624675	510017.355322	48.228519
3503.704384	510003.986073	48.233524
3503.570007	510001.528303	48.238529
3503.721972	509987.793466	48.243533
3503.650877	510001.718066	48.248538
3503.197530	509967.891974	48.253543
3503.588098	509959.077597	48.258548
3503.533614	509959.187480	48.263553
3503.749398	509959.760587	48.268557
3503.751075	509955.510523	48.273562
3503.066471	509989.516660	48.278567
3503.554541	510007.046226	48.283572
3503.777362	510020.924358	48.288577
3503.579234	510012.253644	48.293581
3503.702784	510020.126816	48.298586
3503.425143	510010.203825	48.303591
3503.419028	509957.840319	48.308596
3503.513891	509963.137764	48.313601
3503.977802	509951.680912	48.318605
3503.917217	509983.109337	48.323610
3502.974443	510002.737019	48.328615
3503.598006	509987.156865	48.333620
3503.894923	509977.699580	48.338625
3504.140350	509977.509094	48.343629
3503.708524	509986.127777	48.348634
3503.129849	510008.480564	48.353639
3503.670197	510004.195970	48.358644
3503.331821	510015.025992	48.363649
3504.126408	509970.529776	48.368653
3504.247045	509959.481339	48.373658
3503.882258	509941.578252	48.378663
3503.842379	509951.096291	48.383668
3503.451256	509957.330643	48.388673
3503.886316	509941.021333	48.393677
3503.890679	509961.713621	48.398682
3503.975510	509970.857781	48.403687
3504.056403	509984.707780	48.408692
3503.697126	509977.377956	48.413697
3503.833207	509943.559845	48.418701
3503.996421	509934.224855	48.423706
3503.570804	509934.696959	48.428711
3503.668462	509913.685119	48.433716
3503.964924	509897.347079	48.438721
3503.911696	509893.662212	48.443725
3503.901927	509901.708291	48.448730
3503.065192	509913.932586	48.453735
3503.773508	509921.308630	48.458740
3503.690488	509955.826882	48.463745
3503.715525	509915.550252	48.468749
3503.845344	509872.929638	48.473754
3503.562076	509899.283405	48.478759
3503.862972	509908.393450	48.483764
3503.736809	509912.410400	48.488769
3503.710616	509867.132947	48.493773
3504.012836	509853.424849	48.498778
3504.147611	509860.689191	48.503783
3503.564762	509879.905967	48.508788
3503.160800	509895.502273	48.513793
3503.568672	509903.988284	48.518797
3503.879112	509911.882563	48.523802
3503.401813	509918.130549	48.528807
3503.760795	509907.347972	48.533812
3503.571877	509897.967429	48.538817
3503.787885	509857.205133	48.543821
3503.789363	509851.993786	48.548826
3503.069912	509863.744232	48.553831
3503.760567	509885.896563	48.558836
3503.644450	509887.938762	48.563841
3503.997348	509880.698714	48.568845
3503.907477	509880.814191	48.573850
3503.536997	509872.170646	48.578855
3503.312766	509858.899915	48.583860
3502.912192	509861.796581	48.588865
3503.044908	509856.412712	48.593869
3503.466427	509877.646300	48.598874
3503.460660	509910.533422	48.603879
3503.671936	509862.435756	48.608884
3503.530107	509864.330240	48.613889
3503.141089	509867.376861	48.618893
3503.335537	509897.753252	48.623898
3503.426332	509905.429278	48.628903
3503.962844	509867.854368	48.633908
3503.700310	509865.315646	48.638913
3503.891539	509862.098077	48.643917
3503.349413	509867.546821	48.648922
3503.623594	509869.830901	48.653927
3504.002320	509880.851236	48.658932
3503.666969	509885.204818	48.663937
3503.705259	509884.136376	48.668941
3503.790854	509856.802114	48.673946
3503.690330	509836.479226	48.678951
3503.715710	509828.481413	48.683956
3503.892149	509835.688585	48.688961
3503.145849	509859.737667	48.693965
3503.481629	509879.062227	48.698970
3503.447424	509900.165438	48.703975
3503.860680	509896.710409	48.708980
3503.796399	509900.312829	48.713985
3503.906818	509857.442273	48.718989
3504.278841	509827.532987	48.723994
3503.283817	509843.070974	48.728999
3503.399496	509829.442933	48.734004
3503.694125	509841.741440	48.739009
3504.045602	509846.745393	48.744013
3504.083955	509819.722104	48.749018
3503.835212	509805.746887	48.754023
3503.451756	509817.393667	48.759028
3503.169600	509827.557196	48.764033
3503.608847	509835.178180	48.769037
3503.630460	509856.222029	48.774042
3503.204155	509851.432451	48.779047
3503.776238	509840.059617	48.784052
3503.649590	509854.903812	48.789057
3503.581047	509857.393843	48.794061
3503.639844	509823.992465	48.799066
3504.197681	509808.979076	48.804071
3503.809593	509821.334905	48.809076
3503.617464	509828.802709	48.814081
3503.975117	509779.669793	48.819085
3503.816330	509794.013176	48.824090
3503.740816	509820.941360	48.829095
3503.974457	509781.845709	48.834100
3503.606234	509813.930197	48.839105
3503.742688	509804.144018	48.844109
3503.743588	509796.656002	48.849114
3503.530814	509829.727778	48.854119
3503.996619	509801.523829	48.859124
3503.421591	509777.987236	48.864129
3503.609521	509793.641870	48.869133
3503.485092	509769.173945	48.874138
3503.811110	509819.059110	48.879143
3503.966790	509758.068399	48.884148
3503.725108	509771.868363	48.889153
3503.595701	509756.204629	48.894157
3503.804176	509755.868198	48.899162
3503.179428	509767.300175	48.904167
3503.986519	509778.910601	48.909172
3503.628074	509753.923101	48.914177
3503.286000	509765.310404	48.919181
3504.168555	509779.893972	48.924186
3503.563819	509755.957289	48.929191
3503.641152	509748.710144	48.934196
3503.544300	509789.049279	48.939201
3503.836464	509745.795560	48.944205
3503.472274	509767.355843	48.949210
3503.566652	509801.138046	48.954215
3503.944755	509751.293496	48.959220
3504.171492	509717.612397	48.964225
3504.166548	509700.056943	48.969229
3504.442154	509706.489577	48.974234
3503.767422	509722.381807	48.979239
3504.207883	509731.318105	48.984244
3503.892494	509682.088905	48.989249
3503.533323	509690.999820	48.994253
3503.844056	509711.694582	48.999258
3503.776581	509675.985524	49.004263
3504.298349	509651.921249	49.009268
3503.516683	509691.711113	49.014273
3503.251072	509696.357289	49.019277
3503.929559	509706.672629	49.024282
3503.897015	509701.921965	49.029287
3503.856553	509646.729642	49.034292
3503.223921	509680.829363	49.039297
3503.919332	509659.823929	49.044301
3503.849295	509632.412719	49.049306
3503.814049	509667.075783	49.054311
3504.251656	509614.742293	49.059316
3503.921970	509635.740744	49.064321
3503.333901	509659.714500	49.069325
3503.884409	509663.371588	49.074330
3503.564974	509679.561866	49.079335
3503.817948	509658.474573	49.084340
3503.734123	509649.431447	49.089345
3503.407330	509627.575636	49.094349
3503.094940	509615.431737	49.099354
3503.038447	509649.491057	49.104359
3503.964579	509673.731425	49.109364
3504.030051	509669.319423	49.114369
3503.664435	509659.612513	49.119373
3503.648994	509645.347319	49.124378
3503.645200	509636.139752	49.129383
3503.785065	509582.082403	49.134388
3503.962599	509591.414493	49.139393
3503.392285	509604.254632	49.144397
3503.234058	509622.797445	49.149402
3503.322673	509629.360852	49.154407
3503.832049	509624.069164	49.159412
3503.442115	509626.610023	49.164417
3503.348296	509637.755794	49.169421
3503.287457	509625.420360	49.174426
3503.050108	509629.505544	49.179431
3503.184633	509627.055815	49.184436
3503.303217	509655.066668	49.189441
3503.253135	509661.753173	49.194445
3503.924119	509658.206769	49.199450
3504.047242	509662.943298	49.204455
3503.822242	509669.758635	49.209460
3503.457771	509643.810629	49.214465
3503.694857	509624.091864	49.219469
3504.133035	509596.752058	49.224474
3504.073572	509634.049952	49.229479
3503.947641	509629.516407	49.234484
3503.896400	509641.110799	49.239489
3503.931083	509645.507148	49.244493
3504.135161	509599.484271	49.249498
3502.936938	509602.507047	49.254503
3503.682145	509568.490739	49.259508
3504.096908	509560.228880	49.264513
3504.152128	509561.889873	49.269517
3504.073054	509559.524489	49.274522
3503.779160	509577.380462	49.279527
3503.832995	509561.586400	49.284532
3503.669054	509562.927866	49.289537
3503.611715	509585.654159	49.294541
3503.493781	509551.976616	49.299546
3503.962243	509536.774736	49.304551
3503.984277	509574.211664	49.309556
3503.943981	509564.807449	49.314561
3504.060265	509530.080945	49.319565
3503.748027	509544.195813	49.324570
3503.555436	509586.422571	49.329575
3503.667126	509549.824820	49.334580
3503.381761	509529.530784	49.339585
3503.597311	509530.458108	49.344589
3503.870421	509526.165039	49.349594
3503.658429	509504.442713	49.354599
3504.035246	509484.296942	49.359604
3503.854542	509490.852372	49.364609
3503.806292	509487.824369	49.369613
3504.085693	509513.735630	49.374618
3503.856037	509544.635030	49.379623
3503.809751	509542.416247	49.384628
3503.797394	509507.710030	49.389633
3503.408433	509479.134696	49.394637
3503.839378	509472.843453	49.399642
3503.415302	509496.842112	49.404647
3503.437914	509490.514221	49.409652
3503.481737	509468.447847	49.414657
3503.535322	509507.903744	49.419661
3503.649004	509502.978129	49.424666
3503.260712	509491.048518	49.429671
3503.528619	509444.812759	49.434676
3503.280363	509484.974154	49.439681
3503.157621	509522.282291	49.444685
3503.851031	509503.047813	49.449690
3503.912758	509487.910174	49.454695
3503.599912	509479.611488	49.459700
3503.804069	509509.784648	49.464705
3503.081798	509498.059613	49.469709
3503.440798	509485.354153	49.474714
3503.178376	509495.261782	49.479719
3503.866849	509489.182819	49.484724
3503.437492	509477.664451	49.489729
3503.387729	509464.315246	49.494733
3503.552430	509479.214908	49.499738
3503.088258	509502.157396	49.504743
3503.690203	509497.255801	49.509748
3503.687878	509504.744342	49.514753
3503.549630	509497.429973	49.519757
3503.743114	509536.205957	49.524762
3503.476856	509521.018994	49.529767
3503.960948	509528.177672	49.534772
3503.788279	509530.127661	49.539777
3503.516058	509516.408894	49.544781
3503.528045	509528.701702	49.549786
3503.500460	509526.530556	49.554791
3503.463945	509526.536412	49.559796
3503.544572	509493.485109	49.564801
3503.392499	509478.735419	49.569805
3503.539763	509476.536632	49.574810
3503.662650	509473.430984	49.579815
3504.133944	509467.183956	49.584820
3503.566709	509481.035606	49.589825
3503.153961	509493.547353	49.594829
3503.366028	509504.796650	49.599834
3503.222595	509510.384874	49.604839
3503.656029	509499.691467	49.609844
3503.940518	509473.741827	49.614849
3503.920304	509465.447480	49.619853
3503.870903	509463.532751	49.624858
3503.048312	509473.883093	49.629863
3503.552164	509483.264859	49.634868
3503.558820	509533.909659	49.639873
3503.106495	509543.948465	49.644877
3503.658437	509518.310787	49.649882
3503.255145	509504.511536	49.654887
3502.849075	509508.168058	49.659892
3502.641472	509527.730680	49.664897
3503.068909	509553.871459	49.669901
3503.406571	509554.577103	49.674906
3503.386716	509568.443360	49.679911
3503.475128	509586.036522	49.684916
3503.664272	509593.545358	49.689921
3503.374059	509574.921773	49.694925
3503.709088	509558.172557	49.699930
3503.588572	509552.373260	49.704935
3503.936225	509535.419646	49.709940
3503.739064	509553.665115	49.714945
3503.915613	509536.738545	49.719949
3504.076412	509573.951162	49.724954
3503.345362	509581.200678	49.729959
3503.654249	509554.235405	49.734964
3503.720235	509550.936383	49.739969
3503.696995	509558.579991	49.744973
3503.952090	509562.030815	49.749978
3503.499902	509559.876186	49.754983
3503.501020	509532.504166	49.759988
3503.461070	509525.730819	49.764993
3503.526865	509554.256131	49.769997
3504.108655	509507.363791	49.775002
3503.426867	509530.795991	49.780007
3503.503465	509543.584527	49.785012
3504.278696	509511.384784	49.790017
3503.658537	509535.414379	49.795021
3503.826318	509541.864117	49.800026
3503.343493	509519.273903	49.805031
3503.619015	509544.123234	49.810036
3503.695835	509516.840414	49.815041
3503.414597	509516.783758	49.820045
3503.624990	509533.092815	49.825050
3503.318503	509544.171068	49.830055
3503.500962	509500.630502	49.835060
3503.553404	509537.404967	49.840065
3503.693610	509552.207247	49.845069
3503.796051	509510.703154	49.850074
3503.593119	509533.907883	49.855079
3504.259934	509497.576450	49.860084
3503.385313	509511.071896	49.865089
3503.602868	509526.620900	49.870093
3504.033179	509521.291082	49.875098
3503.822974	509486.767877	49.880103
3503.469357	509518.800011	49.885108
3503.926887	509526.468839	49.890113
3503.833731	509493.090835	49.895117
3503.313345	509522.366582	49.900122
3503.653182	509553.833695	49.905127
3503.671871	509506.777374	49.910132
3503.188688	509508.068110	49.915137
3503.312172	509533.700412	49.920141
3503.794478	509533.472484	49.925146
3503.530559	509505.282192	49.930151
3503.912062	509490.650562	49.935156
3503.644399	509488.314975	49.940161
3503.637536	509509.616724	49.945165
3503.732092	509463.661389	49.950170
3503.658760	509471.515334	49.955175
3503.892057	509493.487480	49.960180
3503.923670	509482.351617	49.965185
3503.477612	509460.818016	49.970189
3503.921220	509459.938464	49.975194
3503.336833	509492.209500	49.980199
3503.701575	509500.449553	49.985204
3504.004199	509483.604195	49.990209
3503.972750	509453.859220	49.995213
3504.141935	509439.261103	50.000218
3503.197825	509452.716982	50.005223
3503.732830	509464.724791	50.010228
3503.881062	509461.058586	50.015233
3503.996288	509431.088009	50.020237
3504.332865	509434.070622	50.025242
3503.878911	509459.187153	50.030247
3503.818051	509431.116433	50.035252
3503.819538	509384.264879	50.040257
3503.494004	509384.468200	50.045261
3503.738351	509409.879203	50.050266
3503.651479	509437.619308	50.055271
3503.879172	509427.717305	50.060276
3503.693686	509426.380629	50.065281
3503.770081	509413.618591	50.070285
3503.772217	509385.335457	50.075290
3503.717552	509366.168464	50.080295
3503.829742	509366.656773	50.085300
3503.922237	509373.017282	50.090305
3503.743119	509414.382207	50.095309
3503.501939	509390.842915	50.100314
3503.251621	509374.843775	50.105319
3503.193950	509369.692226	50.110324
3503.344006	509388.490140	50.115329
3503.679700	509390.916350	50.120333
3504.472133	509367.972599	50.125338
3503.809397	509344.246891	50.130343
3503.496976	509340.349891	50.135348
3504.001420	509345.683985	50.140353
3503.655971	509400.027715	50.145357
3503.971569	509400.736852	50.150362
3503.642583	509412.476487	50.155367
3503.686287	509400.680919	50.160372
3503.443589	509378.811501	50.165377
3503.133836	509363.934847	50.170381
3503.131451	509377.191350	50.175386
3503.431699	509393.587530	50.180391
3503.610375	509351.362668	50.185396
3503.539377	509367.665760	50.190401
3503.226815	509386.688579	50.195405
3503.682981	509392.637435	50.200410
3503.418546	509410.640711	50.205415
3503.550102	509401.968178	50.210420
3503.827515	509403.138709	50.215425
3503.606372	509404.742205	50.220429
3503.940032	509399.528816	50.225434
3503.779508	509398.845935	50.230439
3503.806766	509382.954719	50.235444
3503.599256	509396.698986	50.240449
3503.705178	509363.795223	50.245453
3504.094016	509317.236436	50.250458
3503.930506	509328.646400	50.255463
3503.996644	509315.025783	50.260468
3504.356668	509308.340923	50.265473
3503.187440	509346.270198	50.270477
3503.381471	509367.186202	50.275482
3503.709811	509375.077899	50.280487
3504.095851	509365.555598	50.285492
3504.090916	509306.359518	50.290497
3503.956365	509271.368563	50.295501
3504.296605	509273.844666	50.300506
3502.925243	509298.904042	50.305511
3503.261153	509300.368911	50.310516
3503.927039	509269.855660	50.315521
3503.413372	509267.508327	50.320525
3503.821223	509268.455870	50.325530
3503.956634	509273.494140	50.330535
3503.630010	509296.162182	50.335540
3503.494294	509325.377466	50.340545
3503.624547	509318.678330	50.345549
3504.047316	509266.750896	50.350554
3503.225531	509300.476495	50.355559
3503.818713	509324.618192	50.360564
3504.183898	509263.440831	50.365569
3503.486878	509266.435044	50.370573
3503.594324	509283.570143	50.375578
3503.932282	509259.230797	50.380583
3503.869155	509241.532283	50.385588
3503.716939	509268.625241	50.390593
3503.525039	509297.191706	50.395597
3503.876547	509247.906459	50.400602
3504.103234	509232.590736	50.405607
3504.172998	509221.043907	50.410612
3504.038520	509201.079808	50.415617
3503.961396	509188.190078	50.420621
3503.746743	509183.113880	50.425626
3503.922377	509211.723591	50.430631
3503.959136	509228.110976	50.435636
3503.995588	509229.825563	50.440641
3503.982050	509222.137196	50.445645
3504.120857	509182.296234	50.450650
3504.026111	509162.679984	50.455655
3503.819419	509156.894173	50.460660
3503.673670	509172.298533	50.465665
3503.526902	509170.955718	50.470669
3503.535230	509171.764025	50.475674
3503.547386	509182.539167	50.480679
3503.508864	509169.187957	50.485684
3503.962860	509151.306428	50.490689
3503.682799	509153.880587	50.495693
3503.534983	509142.772863	50.500698
3503.703486	509127.314454	50.505703
3503.366845	509109.659034	50.510708
3503.948917	509126.668678	50.515713
3503.638085	509155.051790	50.520717
3503.888647	509160.324875	50.525722
3503.661103	509147.661274	50.530727
3503.627149	509121.710839	50.535732
3503.763339	509092.141130	50.540737
3503.779636	509042.402312	50.545741
3503.577014	509051.895971	50.550746
3503.185391	509014.111719	50.555751
3503.287748	508954.442105	50.560756
3503.189449	508856.957422	50.565761
3502.868192	508769.323313	50.570765
3503.235295	508651.626163	50.575770
3502.937319	508564.037932	50.580775
3502.938528	508434.354819	50.585780
3502.872607	508326.286976	50.590785
3502.333474	508249.006785	50.595789
3502.544466	508085.285435	50.600794
3502.118399	507965.988609	50.605799
3501.972350	507769.936883	50.610804
3502.035904	507581.743544	50.615809
3502.091937	507426.389604	50.620813
3501.495359	507237.487251	50.625818
3500.615169	507067.097522	50.630823
3500.737606	506872.308902	50.635828
3500.209554	506679.240226	50.640833
3500.082042	506480.337251	50.645837
3500.265169	506239.634084	50.650842
3499.914467	506028.869136	50.655847
3499.389585	505788.119842	50.660852
3498.606027	505564.057718	50.665857
3498.057426	505332.769356	50.670861
3498.633103	505068.050771	50.675866
3497.936916	504816.940561	50.680871
3497.544202	504592.905488	50.685876
3497.471385	504350.243089	50.690881
3496.386315	504095.540121	50.695885
3496.290896	503810.816183	50.700890
3495.897582	503499.411317	50.705895
3495.267879	503203.728503	50.710900
3495.315061	502955.207440	50.715905
3494.609499	502663.475508	50.720909
3493.992857	502358.109072	50.725914
3493.630589	502048.242918	50.730919
3492.925459	501752.092311	50.735924
3492.745205	501483.035889	50.740929
3491.819230	501159.525818	50.745933
3491.717696	500813.454843	50.750938
3490.992818	500515.717642	50.755943
3490.782264	500216.274307	50.760948
3490.253782	499870.708224	50.765953
3489.745965	499520.322970	50.770957
3489.067422	499215.469568	50.775962
3488.537427	498908.157508	50.780967
3488.363860	498530.615502	50.785972
3487.579407	498221.661316	50.790977
3487.093619	497858.735370	50.795981
3486.402248	497538.667192	50.800986
3486.346645	497172.216743	50.805991
3485.241880	496832.151821	50.810996
3485.254330	496481.777507	50.816001
3484.444125	496136.843002	50.821005
3483.872715	495778.193000	50.826010
3483.539467	495377.774825	50.831015
3482.966658	495019.363392	50.836020
3482.067277	494665.807143	50.841025
3481.715740	494325.272838	50.846029
3481.068173	493933.228248	50.851034
3480.823997	493561.823512	50.856039
3479.964363	493195.370183	50.861044
3479.750166	492773.506045	50.866049
3478.551449	492417.016887	50.871053
3478.200090	492057.956034	50.876058
3477.585513	491641.193984	50.881063
3476.825090	491250.579389	50.886068
3476.400314	490893.685586	50.891073
3475.445581	490515.646994	50.896077
3475.345674	490090.260140	50.901082
3474.368762	489685.313315	50.906087
3473.887152	489297.906382	50.911092
3473.592027	488908.537223	50.916097
3472.714268	488552.633106	50.921101
3472.223259	488118.956479	50.926106
3471.747801	487699.552550	50.931111
3470.874994	487317.891182	50.936116
3469.694714	486923.555569	50.941121
3468.982615	486534.862316	50.946125
3468.456289	486140.863142	50.951130
3467.794038	485763.038329	50.956135
3467.152802	485374.816998	50.961140
3466.367546	484976.579266	50.966145
3465.584186	484560.347145	50.971149
3465.241152	484133.295368	50.976154
3464.263559	483754.771784	50.981159
3463.534614	483356.998507	50.986164
3463.395421	482958.414517	50.991169
3462.391840	482570.751651	50.996173
3461.949359	482187.856780	51.001178
3461.414131	481801.118037	51.006183
3460.325593	481397.838500	51.011188
3460.130938	480984.325316	51.016193
3458.939091	480581.248059	51.021197
3458.344776	480158.608593	51.026202
3457.940817	479760.254921	51.031207
3457.557163	479349.423265	51.036212
3456.763043	478930.083243	51.041217
3455.931740	478555.744105	51.046221
3455.181051	478179.053872	51.051226
3454.372596	477777.683583	51.056231
3453.573853	477367.282142	51.061236
3452.428897	476963.262527	51.066241
3451.630913	476568.759402	51.071245
3451.867426	476187.263367	51.076250
3451.073262	475750.420823	51.081255
3450.085009	475342.897236	51.086260
3449.712427	474952.553093	51.091265
3448.711394	474586.479905	51.096269
3448.286077	474198.512042	51.101274
3447.221066	473776.218108	51.106279
3446.258258	473369.918267	51.111284
3446.337197	472964.307480	51.116289
3445.126108	472630.372377	51.121293
3444.094717	472200.689900	51.126298
3443.668220	471785.554235	51.131303
3443.011152	471419.724956	51.136308
3442.428916	471059.657021	51.141313
3441.342567	470636.389411	51.146317
3440.785587	470219.164273	51.151322
3440.282212	469874.527024	51.156327
3439.300929	469471.753218	51.161332
3438.980551	469082.455700	51.166337
3438.005616	468684.583961	51.171341
3437.567001	468320.643177	51.176346
3436.591307	467918.903445	51.181351
3436.188818	467533.646695	51.186356
3435.407545	467153.767143	51.191361
3434.619620	466744.267733	51.196365
3433.920768	466394.584122	51.201370
3433.069557	465986.449254	51.206375
3432.675739	465612.667583	51.211380
3432.093741	465227.143765	51.216385
3430.940575	464835.972644	51.221389
3430.388701	464459.660108	51.226394
3429.885419	464085.361908	51.231399
3428.687316	463689.206869	51.236404
3428.372760	463328.356210	51.241409
3427.772239	462932.498539	51.246413
3426.814300	462550.029232	51.251418
3426.116228	462190.437479	51.256423
3425.455159	461779.200201	51.261428
3425.029783	461430.609907	51.266433
3423.536374	461056.568044	51.271437
3423.438790	460654.401250	51.276442
3422.608479	460311.183079	51.281447
3421.893893	459909.861035	51.286452
3421.416665	459551.002548	51.291457
3420.336015	459180.617173	51.296461
3419.438382	458819.073993	51.301466
3419.009914	458424.172830	51.306471
3418.537921	458083.247591	51.311476
3417.524041	457697.455868	51.316481
3417.227041	457324.582014	51.321485
3416.334717	456971.429286	51.326490
3415.492821	456581.583262	51.331495
3415.100891	456195.007739	51.336500
3414.400305	455815.424984	51.341505
3413.616333	455488.461483	51.346509
3412.800124	455129.686877	51.351514
3412.306183	454726.917495	51.356519
3411.222244	454393.186819	51.361524
3410.933520	453998.997462	51.366529
3409.793980	453665.721532	51.371533
3409.495967	453279.943913	51.376538
3408.628196	452928.144818	51.381543
3407.900540	452553.738091	51.386548
3407.005906	452213.044700	51.391553
3406.187425	451820.626775	51.396557
3405.715105	451492.288064	51.401562
3405.054494	451101.406001	51.406567
3404.341273	450778.271211	51.411572
3404.030229	450376.360573	51.416577
3402.889444	450057.698288	51.421581
3402.301344	449666.628339	51.426586
3401.953148	449330.474943	51.431591
3400.953285	448953.972310	51.436596
3400.568489	448602.081839	51.441601
3399.806818	448237.101121	51.446605
3399.006445	447898.004350	51.451610
3398.239449	447508.347727	51.456615
3397.568788	447196.423823	51.461620
3396.835268	446810.252385	51.466625
3396.235634	446441.767007	51.471629
3395.570752	446119.220213	51.476634
3394.677305	445747.928218	51.481639
3394.300996	445362.438148	51.486644
3393.504388	445060.556098	51.491649
3392.990730	444679.035863	51.496653
3392.595609	444347.895050	51.501658
3391.616264	443967.553859	51.506663
3390.850856	443624.736021	51.511668
3390.429012	443231.401793	51.516673
3389.224385	442920.877165	51.521677
3389.135445	442530.981555	51.526682
3387.789679	442201.839916	51.531687
3387.394257	441832.134868	51.536692
3386.400961	441488.764514	51.541697
3385.966911	441140.427371	51.546701
3385.107353	440777.785520	51.551706
3384.327131	440454.978376	51.556711
3383.536462	440081.857255	51.561716
3383.265270	439748.248255	51.566721
3382.607815	439387.508623	51.571725
3381.821557	439057.500261	51.576730
3381.017281	438688.650414	51.581735
3380.501156	438328.634640	51.586740
3379.898693	438023.207900	51.591745
3378.641052	437662.792048	51.596749
3378.319385	437298.592685	51.601754
3377.598064	436979.869228	51.606759
3376.531105	436624.790452	51.611764
3375.748852	436293.831080	51.616769
3375.253139	435934.437868	51.621773
3374.596069	435626.756516	51.626778
3374.091279	435248.998996	51.631783
3373.312154	434964.991542	51.636788
3372.712242	434583.329233	51.641793
3371.912264	434261.638855	51.646797
3371.206244	433918.550877	51.651802
3370.598397	433588.620580	51.656807
3370.044386	433221.225718	51.661812
3369.422682	432904.746125	51.666817
3368.575099	432549.398248	51.671821
3367.858432	432228.151746	51.676826
3367.300451	431885.698930	51.681831
3366.688632	431534.743554	51.686836
3365.859510	431219.495062	51.691841
3365.153817	430856.458319	51.696845
3364.473772	430543.387332	51.701850
3363.874745	430198.277948	51.706855
3362.896419	429877.958107	51.711860
3362.370551	429520.283462	51.716865
3361.777439	429203.398991	51.721869
3360.732544	428881.299940	51.726874
3360.240222	428521.320921	51.731879
3359.413911	428202.531301	51.736884
3358.901087	427883.078790	51.741889
3358.241430	427539.188785	51.746893
3357.789870	427194.321774	51.751898
3357.119825	426896.418913	51.756903
3355.958022	426561.307004	51.761908
3355.643811	426223.771102	51.766913
3354.570630	425889.830535	51.771917
3354.034015	425587.574440	51.776922
3353.585832	425237.627599	51.781927
3352.832704	424913.860101	51.786932
3352.182811	424592.409171	51.791937
3351.561213	424261.475915	51.796941
3350.929033	423911.312559	51.801946
3350.129883	423604.402407	51.806951
3349.167531	423243.716237	51.811956
3348.777901	422948.697695	51.816961
3347.948218	422606.829652	51.821965
3347.197580	422293.216732	51.826970
3346.481084	421983.938566	51.831975
3345.761465	421638.459539	51.836980
3345.399801	421325.028213	51.841985
3344.522916	421008.118470	51.846989
3344.054034	420656.236987	51.851994
3343.338631	420363.605036	51.856999
3342.197758	420020.331922	51.862004
3342.093876	419707.451450	51.867009
3341.039620	419394.819408	51.872013
3340.501292	419059.390815	51.877018
3339.707536	418731.848696	51.882023
3339.507116	418421.027070	51.887028
3338.833487	418085.938657	51.892033
3337.684048	417782.805507	51.897037
3337.244310	417449.806720	51.902042
3336.409243	417121.922400	51.907047
3335.838435	416820.008700	51.912052
3335.472070	416467.169957	51.917057
3334.704345	416178.974893	51.922061
3334.011048	415814.543508	51.927066
3333.261472	415515.871191	51.932071
3332.124629	415196.270211	51.937076
3331.772970	414865.260378	51.942081
3330.718428	414543.784452	51.947085
3330.361123	414237.084208	51.952090
3329.554214	413922.676735	51.957095
3328.722593	413584.639268	51.962100
3327.779867	413295.935272	51.967105
3327.603610	412980.681162	51.972109
3327.121744	412660.593311	51.977114
3326.348710	412331.425770	51.982119
3325.597776	412029.237089	51.987124
3325.006220	411702.193800	51.992129
3324.092291	411398.881035	51.997133
3323.378522	411073.781453	52.002138
3323.066549	410775.271588	52.007143
3322.128042	410434.292981	52.012148
3321.432895	410147.120366	52.017153
3320.594897	409819.485704	52.022157
3319.827130	409509.498196	52.027162
3319.510661	409205.230307	52.032167
3318.396959	408877.883232	52.037172
3317.982278	408579.495082	52.042177
3317.288479	408273.956095	52.047181
3316.753686	407951.666553	52.052186
3316.073674	407644.772196	52.057191
3315.299116	407333.798011	52.062196
3314.846223	407032.884884	52.067201
3314.321316	406710.123364	52.072205
3313.597594	406394.557027	52.077210
3312.602480	406085.968836	52.082215
3312.010420	405776.195565	52.087220
3311.602064	405455.054651	52.092225
3310.511995	405161.925282	52.097229
3309.959348	404822.678953	52.102234
3309.455250	404521.953095	52.107239
3308.560514	404224.412442	52.112244
3307.956806	403890.145908	52.117249
3307.214957	403609.045676	52.122253
3306.721933	403256.937335	52.127258
3305.809245	402986.635756	52.132263
3304.845320	402666.799927	52.137268
3304.414894	402359.636610	52.142273
3303.945817	402061.932229	52.147277
3303.091124	401751.017398	52.152282
3302.790162	401434.699396	52.157287
3301.741453	401136.340997	52.162292
3300.907811	400814.966469	52.167297
3300.304372	400535.774830	52.172301
3299.995039	400191.865471	52.177306
3299.292180	399922.928642	52.182311
3298.154012	399602.149593	52.187316
3297.686230	399305.055315	52.192321
3296.847261	399000.619528	52.197325
3295.922284	398685.492163	52.202330
3295.521834	398412.936204	52.207335
3295.008064	398078.519359	52.212340
3294.372161	397805.766864	52.217345
3293.807530	397481.063270	52.222349
3293.318957	397192.215608	52.227354
3292.960544	396883.057570	52.232359
3291.970381	396570.437391	52.237364
3291.409267	396261.204009	52.242369
3290.495593	395949.176136	52.247373
3289.527155	395649.001460	52.252378
3289.124405	395337.802413	52.257383
3288.172434	395043.543548	52.262388
3287.566723	394742.744191	52.267393
3286.792965	394437.214382	52.272397
3286.420408	394122.465493	52.277402
3285.722839	393834.334229	52.282407
3284.890420	393533.356743	52.287412
3284.627174	393223.591130	52.292417
3283.372502	392917.183178	52.297421
3283.086619	392629.764981	52.302426
3282.536108	392320.291013	52.307431
3281.996493	392007.532590	52.312436
3281.207070	391689.928989	52.317441
3279.944403	391401.994104	52.322445
3279.329248	391085.374556	52.327450
3279.094266	390800.170901	52.332455
3278.245430	390510.307114	52.337460
3277.733081	390194.044751	52.342465
3277.353550	389896.854872	52.347469
3276.390123	389615.723667	52.352474
3275.918171	389294.920763	52.357479
3275.626381	388990.691290	52.362484
3274.720901	388680.326277	52.367489
3274.024734	388376.359003	52.372493
3273.182284	388059.265459	52.377498
3272.515117	387742.217710	52.382503
3271.748194	387456.105311	52.387508
3271.291058	387139.959998	52.392513
3270.504344	386832.866292	52.397517
3269.543287	386542.581508	52.402522
3268.868208	386221.198703	52.407527
3268.460483	385942.875685	52.412532
3268.061893	385630.573594	52.417537
3266.640060	385347.396625	52.422541
3266.156188	384996.905322	52.427546
3265.678684	384744.397057	52.432551
3264.665005	384436.988778	52.437556
3264.302998	384105.162080	52.442561
3263.592485	383842.562725	52.447565
3263.084314	383524.512749	52.452570
3262.365556	383239.174083	52.457575
3261.601669	382932.222681	52.462580
3261.099087	382620.827593	52.467585
3260.295522	382323.033378	52.472589
3259.626403	382031.116089	52.477594
3259.366967	381705.661387	52.482599
3258.284553	381441.451129	52.487604
3257.688890	381116.298965	52.492609
3257.207934	380806.157444	52.497613
3256.316627	380528.074606	52.502618
3255.856557	380219.654629	52.507623
3254.685881	379917.423482	52.512628
3254.310086	379608.451227	52.517633
3253.659185	379319.206751	52.522637
3252.899279	379014.512793	52.527642
3252.325321	378710.651877	52.532647
3251.432460	378419.887526	52.537652
3251.111267	378116.312741	52.542657
3250.437004	377812.155590	52.547661
3249.628840	377506.363952	52.552666
3248.706761	377213.967520	52.557671
3248.178483	376931.554102	52.562676
3247.444219	376629.610457	52.567681
3246.835398	376335.835399	52.572685
3246.222183	376034.249723	52.577690
3245.854614	375729.239799	52.582695
3244.927983	375433.727885	52.587700
3244.241460	375130.595439	52.592705
3243.630749	374842.864091	52.597709
3242.743622	374537.240654	52.602714
3241.861157	374243.442982	52.607719
3241.254010	373957.256629	52.612724
3241.111729	373654.510594	52.617729
3240.048584	373354.477328	52.622733
3239.206497	373071.272946	52.627738
3239.323175	372767.563727	52.632743
3238.216579	372474.246955	52.637748
3237.612049	372158.334810	52.642753
3237.032554	371874.343101	52.647757
3236.651766	371573.069870	52.652762
3236.088862	371265.208916	52.657767
3235.107978	370970.869710	52.662772
3234.498475	370660.009832	52.667777
3233.807467	370361.906307	52.672781
3233.138029	370063.848192	52.677786
3232.663821	369760.058384	52.682791
3231.888345	369463.488484	52.687796
3231.036297	369161.509693	52.692801
3230.523110	368863.316867	52.697805
3229.798317	368553.528680	52.702810
3229.278902	368247.165904	52.707815
3228.221784	367955.184423	52.712820
3227.748263	367653.542473	52.717825
3227.125464	367352.838008	52.722829
3226.238949	367064.767241	52.727834
3225.978879	366739.220319	52.732839
3224.808555	366443.277787	52.737844
3224.197666	366148.466079	52.742849
3223.474834	365856.545228	52.747853
3222.629219	365561.919484	52.752858
3222.422916	365267.546913	52.757863
3221.199008	364966.031087	52.762868
3220.795548	364663.365743	52.767873
3220.053444	364378.664516	52.772877
3219.507687	364096.576657	52.777882
3218.933713	363793.703574	52.782887
3218.487800	363508.822915	52.787892
3217.634072	363202.020895	52.792897
3217.069260	362897.868302	52.797901
3216.173429	362592.595629	52.802906
3215.822891	362294.715574	52.807911
3214.902774	362016.821916	52.812916
3214.164078	361714.444905	52.817921
3213.682998	361407.394126	52.822925
3212.929340	361106.313342	52.827930
3212.534343	360805.988196	52.832935
3211.342995	360525.151576	52.837940
3211.124261	360230.800219	52.842945
3210.252105	359933.776780	52.847949
3209.481293	359632.307800	52.852954
3208.960227	359351.282002	52.857959
3208.306281	359055.821826	52.862964
3207.277765	358751.665368	52.867969
3206.658421	358468.588853	52.872973
3205.994824	358175.822311	52.877978
3205.491951	357877.328396	52.882983
3204.870923	357586.129382	52.887988
3204.085565	357289.152586	52.892993
3203.714713	357002.007675	52.897997
3203.020513	356705.318378	52.903002
3202.372188	356402.665211	52.908007
3201.657575	356121.193709	52.913012
3201.118630	355818.265270	52.918017
3200.393849	355514.473728	52.923021
3199.578988	355224.513303	52.928026
3198.978312	354921.411182	52.933031
3198.189818	354634.293539	52.938036
3197.744867	354329.254633	52.943041
3197.024927	354046.474702	52.948045
3196.030902	353745.591128	52.953050
3195.786136	353442.958522	52.958055
3195.030894	353159.594046	52.963060
3194.486584	352861.713691	52.968065
3193.574969	352568.725273	52.973069
3193.064083	352277.453361	52.978074
3192.632489	351967.944888	52.983079
3191.528683	351668.670254	52.988084
3191.100370	351372.442971	52.993089
3190.439333	351075.970921	52.998093
3189.616218	350779.777399	53.003098
3189.046261	350477.408521	53.008103
3188.263536	350189.222476	53.013108
3187.473298	349894.189708	53.018113
3186.980289	349599.159242	53.023117
3186.157727	349313.494610	53.028122
3185.495789	349010.266880	53.033127
3184.694340	348723.450552	53.038132
3184.380919	348427.418296	53.043137
3183.733298	348143.399836	53.048141
3182.987941	347852.752379	53.053146
3182.721592	347545.789048	53.058151
3181.745809	347250.822609	53.063156
3181.061843	346953.975894	53.068161
3180.665290	346654.995048	53.073165
3179.848718	346345.872489	53.078170
3179.242133	346051.299643	53.083175
3178.638172	345761.560988	53.088180
3178.113733	345463.917798	53.093185
3177.213442	345162.183652	53.098189
3176.512510	344861.536376	53.103194
3175.863074	344554.566914	53.108199
3174.910280	344270.781360	53.113204
3174.541206	343972.978817	53.118209
3174.332754	343668.276791	53.123213
3173.146952	343365.255092	53.128218
3172.665986	343064.054894	53.133223
3172.001575	342763.467675	53.138228
3171.514338	342460.458217	53.143233
3170.635210	342173.291159	53.148237
3169.972045	341872.724827	53.153242
3169.448709	341563.429329	53.158247
3168.181340	341274.028571	53.163252
3167.502250	340963.660167	53.168257
3167.184086	340675.557415	53.173261
3166.641657	340385.783313	53.178266
3165.774352	340092.088219	53.183271
3164.933315	339790.674553	53.188276
3164.538516	339491.047136	53.193281
3163.808508	339205.675731	53.198285
3162.764117	338911.188644	53.203290
3162.925767	338600.421152	53.208295
3161.744861	338314.709857	53.213300
3161.033790	338010.110747	53.218305
3160.527718	337711.841905	53.223309
3159.851746	337410.671090	53.228314
3159.235399	337128.581986	53.233319
3158.158322	336825.842751	53.238324
3157.749960	336514.748310	53.243329
3157.244312	336224.669870	53.248333
3156.154089	335945.654694	53.253338
3155.786544	335641.270457	53.258343
3155.003483	335348.355496	53.263348
3154.084766	335062.919782	53.268353
3153.709737	334766.119168	53.273357
3152.804561	334472.761572	53.278362
3152.561415	334176.726762	53.283367
3151.561657	333889.618834	53.288372
3150.808243	333583.275433	53.293377
3150.507879	333302.266211	53.298381
3149.474300	333018.647856	53.303386
3149.587913	332707.733779	53.308391
3148.626843	332419.900959	53.313396
3147.625521	332126.421569	53.318401
3147.060285	331829.893339	53.323405
3146.355136	331525.926633	53.328410
3145.703059	331237.123731	53.333415
3144.923919	330951.598542	53.338420
3144.415012	330650.855921	53.343425
3143.705497	330356.050343	53.348429
3142.893305	330079.132222	53.353434
3142.305382	329778.042169	53.358439
3141.591974	329486.645351	53.363444
3140.937181	329202.010374	53.368449
3140.651419	328909.627150	53.373453
3139.645303	328616.618456	53.378458
3139.226084	328316.463429	53.383463
3138.568485	328024.161150	53.388468
3137.586243	327731.476324	53.393473
3137.351434	327429.812039	53.398477
3136.090473	327151.426811	53.403482
3135.986378	326840.955844	53.408487
3135.223380	326549.326761	53.413492
3134.490768	326267.621396	53.418497
3133.730881	325970.668495	53.423501
3133.132527	325669.131498	53.428506
3132.832233	325386.870933	53.433511
3131.828427	325094.256313	53.438516
3131.194929	324785.007011	53.443521
3130.859426	324488.210772	53.448525
3129.477487	324203.393003	53.453530
3129.081606	323906.935261	53.458535
3128.359072	323605.003073	53.463540
3127.905645	323329.736208	53.468545
3127.062376	323025.300407	53.473549
3126.348046	322741.135976	53.478554
3125.567360	322447.509397	53.483559
3125.286918	322161.619424	53.488564
3124.489438	321860.762419	53.493569
3123.713256	321568.507135	53.498573
3123.047448	321276.869981	53.503578
3122.666251	320979.585199	53.508583
3121.693773	320695.607836	53.513588
3121.050544	320403.098580	53.518593
3120.259553	320113.208923	53.523597
3119.580798	319811.053200	53.528602
3119.099998	319518.871913	53.533607
3118.214434	319247.836722	53.538612
3117.770923	318953.228834	53.543617
3117.155686	318657.323142	53.548621
3116.419448	318365.611570	53.553626
3115.951732	318071.233952	53.558631
3115.237822	317772.107366	53.563636
3114.775282	317483.099819	53.568641
3113.940896	317191.782192	53.573645
3113.166882	316903.917140	53.578650
3112.737222	316604.079986	53.583655
3111.829882	316307.042090	53.588660
3111.054048	316018.818296	53.593665
3110.368459	315719.579204	53.598669
3109.587648	315442.685797	53.603674
3109.039993	315145.663996	53.608679
3108.594709	314855.704041	53.613684
3107.672791	314572.642977	53.618689
3106.931806	314275.038167	53.623693
3106.528502	313979.314345	53.628698
3106.012655	313689.438753	53.633703
3105.386695	313406.760651	53.638708
3104.538522	313098.118172	53.643713
3104.332111	312804.524433	53.648717
3103.248516	312514.455453	53.653722
3102.454010	312206.234882	53.658727
3101.637816	311928.370381	53.663732
3101.260048	311624.793178	53.668737
3100.456117	311336.535815	53.673741
3099.447835	311066.288019	53.678746
3099.118602	310766.495084	53.683751
3098.388942	310480.744836	53.688756
3097.738113	310190.576027	53.693761
3097.428599	309904.910694	53.698765
3096.766398	309614.385777	53.703770
3096.281000	309318.688277	53.708775
3095.270977	309018.463918	53.713780
3094.715364	308722.954345	53.718785
3094.384746	308429.063696	53.723789
3093.229724	308148.086310	53.728794
3092.779487	307841.251463	53.733799
3092.092873	307538.120280	53.738804
3091.075762	307261.269954	53.743809
3090.928784	306958.765051	53.748813
3089.986295	306661.249229	53.753818
3089.273032	306357.049974	53.758823
3088.831881	306073.561386	53.763828
3088.072675	305774.257466	53.768833
3087.321490	305486.691285	53.773837
3086.445345	305186.742481	53.778842
3086.222050	304889.287229	53.783847
3085.440432	304601.978693	53.788852
3084.855957	304313.848938	53.793857
3084.301995	304002.743522	53.798861
3083.234100	303721.895936	53.803866
3082.538272	303426.549704	53.808871
3081.842204	303132.832749	53.813876
3081.481932	302837.457714	53.818881
3080.752432	302539.110057	53.823885
3079.911708	302260.362937	53.828890
3079.446001	301954.459869	53.833895
3078.573839	301673.093647	53.838900
3077.790033	301376.000201	53.843905
3077.407492	301085.489435	53.848909
3076.827921	300787.496725	53.853914
3075.805127	300498.130354	53.858919
3075.266668	300206.980573	53.863924
3074.631299	299916.889753	53.868929
3073.976032	299620.511329	53.873933
3073.241969	299342.990197	53.878938
3072.824718	299042.269248	53.883943
3072.167032	298745.176647	53.888948
3071.495853	298464.766436	53.893953
3070.772095	298149.041609	53.898957
3070.166253	297867.041193	53.903962
3069.338297	297567.834394	53.908967
3068.817952	297283.858614	53.913972
3068.289488	296978.262217	53.918977
3067.508538	296685.769881	53.923981
3066.403414	296392.487996	53.928986
3065.928764	296100.251925	53.933991
3065.431621	295810.056361	53.938996
3064.724371	295517.143180	53.944001
3063.908672	295227.710289	53.949005
3063.438078	294938.145984	53.954010
3062.778577	294644.536417	53.959015
3062.007180	294352.090190	53.964020
3061.651317	294063.372451	53.969025
3061.013327	293754.783491	53.974029
3060.026691	293481.878209	53.979034
3059.314452	293182.137424	53.984039
3058.786740	292881.144615	53.989044
3057.815649	292599.169426	53.994049
3057.502835	292304.941717	53.999053
3056.384315	292012.649364	54.004058
3055.856141	291723.064682	54.009063
3055.173649	291439.871005	54.014068
3054.795280	291143.207434	54.019073
3054.343828	290846.707906	54.024077
3053.155668	290574.544440	54.029082
3052.712502	290270.530003	54.034087
3052.333391	289975.011336	54.039092
3051.354078	289684.859187	54.044097
3050.528580	289397.254659	54.049101
3050.261851	289106.123268	54.054106
3049.529979	288803.579207	54.059111
3048.535414	288530.924794	54.064116
3047.820136	288227.129632	54.069121
3047.525361	287942.699675	54.074125
3046.369939	287661.258095	54.079130
3046.178455	287367.337232	54.084135
3045.430063	287076.051061	54.089140
3044.650241	286789.048257	54.094145
3044.053597	286495.267213	54.099149
3043.077131	286196.528848	54.104154
3042.769607	285911.971978	54.109159
3042.272731	285632.258345	54.114164
3041.723463	285328.281707	54.119169
3041.243090	285038.021271	54.124173
3040.269562	284755.606477	54.129178
3039.594089	284451.903894	54.134183
3038.877511	284166.519239	54.139188
3038.576708	283861.127022	54.144193
3037.821600	283573.201306	54.149197
3036.905421	283278.067951	54.154202
3036.385621	282970.952571	54.159207
3035.348902	282671.915866	54.164212
3035.036403	282394.947244	54.169217
3034.726031	282093.401283	54.174221
3033.468026	281809.323590	54.179226
3032.955772	281508.395086	54.184231
3032.304906	281220.884719	54.189236
3031.771133	280919.908443	54.194241
3031.322835	280619.453361	54.199245
3030.318050	280327.388922	54.204250
3030.105561	280037.109118	54.209255
3029.084290	279735.496478	54.214260
3028.227483	279442.236808	54.219265
3027.661092	279129.167654	54.224269
3026.861868	278849.804446	54.229274
3025.872328	278558.577574	54.234279
3025.497606	278260.376877	54.239284
3024.413869	277969.317615	54.244289
3024.117580	277691.097085	54.249293
3023.636282	277387.946784	54.254298
3023.259314	277090.026423	54.259303
3022.641225	276807.603509	54.264308
3021.738325	276508.900414	54.269313
3020.951571	276203.811825	54.274317
3020.236564	275905.588337	54.279322
3019.965954	275607.956689	54.284327
3019.318592	275304.603350	54.289332
3018.505455	275005.605887	54.294337
3018.122109	274709.851308	54.299341
3016.894083	274415.834951	54.304346
3016.181597	274106.303187	54.309351
3015.615543	273827.386748	54.314356
3015.062712	273527.813400	54.319361
3014.473068	273230.639957	54.324365
3013.862352	272935.252690	54.329370
3013.056184	272646.492725	54.334375
3012.525099	272344.140121	54.339380
3012.033240	272053.955256	54.344385
3011.304469	271747.177140	54.349389
3010.347069	271454.595697	54.354394
3009.900538	271151.644284	54.359399
3008.929674	270862.528856	54.364404
3008.217876	270562.726773	54.369409
3007.955050	270264.050753	54.374413
3007.196646	269979.613660	54.379418
3006.299035	269676.887026	54.384423
3005.507354	269390.137833	54.389428
3005.198751	269092.386428	54.394433
3004.551085	268795.936779	54.399437
3003.814564	268514.807749	54.404442
3003.358323	268205.899613	54.409447
3002.499496	267916.054652	54.414452
3001.815989	267619.305694	54.419457
3001.421075	267319.225840	54.424461
3000.699056	267026.838394	54.429466
3000.054776	266733.471037	54.434471
2999.289398	266416.997988	54.439476
2998.439501	266126.235859	54.444481
2998.137782	265818.731039	54.449485
2997.398047	265531.873974	54.454490
2996.903375	265236.039043	54.459495
2996.377238	264927.602648	54.464500
2995.356957	264632.564486	54.469505
2994.653070	264320.311062	54.474509
2993.990800	264037.314011	54.479514
2993.510159	263732.182271	54.484519
2992.967873	263438.826740	54.489524
2992.016000	263132.496741	54.494529
2991.808389	262830.633442	54.499533
2990.937706	262528.773517	54.504538
2990.349658	262223.150849	54.509543
2989.935838	261919.156320	54.514548
2988.749687	261617.474583	54.519553
2988.348454	261313.886178	54.524557
2987.745413	261010.915801	54.529562
2986.763532	260706.808741	54.534567
2986.152465	260403.458293	54.539572
2985.487924	260108.928453	54.544577
2984.974941	259807.040289	54.549581
2983.707713	259505.857626	54.554586
2983.110967	259208.465727	54.559591
2982.717628	258909.284732	54.564596
2981.762532	258623.690788	54.569601
2981.637530	258308.474495	54.574605
2980.790710	258022.711336	54.579610
2980.469621	257723.953355	54.584615
2979.663378	257412.513427	54.589620
2978.694126	257110.115165	54.594625
2978.472184	256803.040387	54.599629
2977.675813	256508.688721	54.604634
2977.239906	256194.314125	54.609639
2976.383688	255892.714647	54.614644
2975.253253	255591.617427	54.619649
2975.076828	255284.028338	54.624653
2974.252438	254995.133235	54.629658
2973.528215	254681.927178	54.634663
2972.941461	254390.219452	54.639668
2972.232294	254079.329489	54.644673
2971.751415	253775.381828	54.649677
2970.928382	253495.147520	54.654682
2970.082022	253171.165373	54.659687
2969.887314	252872.471005	54.664692
2969.074888	252572.423318	54.669697
2968.294589	252272.676657	54.674701
2967.637962	251969.498409	54.679706
2967.146074	251655.904257	54.684711
2966.345665	251356.518914	54.689716
2965.602130	251064.510385	54.694721
2965.485198	250746.554747	54.699725
2963.924719	250453.148641	54.704730
2963.560539	250134.418418	54.709735
2962.762321	249846.826416	54.714740
2962.260692	249539.247919	54.719745
2961.618371	249242.082510	54.724749
2960.792865	248944.386417	54.729754
2960.584652	248651.762806	54.734759
2959.791697	248344.309227	54.739764
2958.994675	248043.656347	54.744769
2958.538937	247733.120203	54.749773
2957.772497	247431.343239	54.754778
2956.830460	247131.988492	54.759783
2956.417887	246820.097794	54.764788
2955.472715	246522.374641	54.769793
2955.253509	246219.444068	54.774797
2954.373980	245923.341612	54.779802
2953.704724	245601.791887	54.784807
2953.225686	245308.403115	54.789812
2952.315185	245010.295786	54.794817
2951.994997	244701.578475	54.799821
2950.937606	244398.198982	54.804826
2950.135212	244098.268571	54.809831
2949.534071	243802.865270	54.814836
2948.907110	243500.769407	54.819841
2948.084571	243200.003946	54.824845
2947.569897	242908.561597	54.829850
2947.139230	242602.820791	54.834855
2946.209556	242296.192074	54.839860
2945.400045	242006.479220	54.844865
2944.933749	241696.366375	54.849869
2944.271923	241393.797373	54.854874
2943.585954	241102.080902	54.859879
2943.138007	240796.194632	54.864884
2942.419450	240508.049839	54.869889
2941.760812	240199.422862	54.874893
2941.140897	239902.427805	54.879898
2940.411054	239598.142669	54.884903
2940.164038	239298.518265	54.889908
2938.980744	238995.299653	54.894913
2938.208570	238683.002493	54.899917
2937.676577	238394.044176	54.904922
2936.885681	238093.185011	54.909927
2936.553194	237789.402155	54.914932
2935.890609	237481.801915	54.919937
2935.431929	237184.712272	54.924941
2934.316164	236886.581623	54.929946
2933.742642	236578.995372	54.934951
2932.868986	236280.573487	54.939956
2932.176884	235974.433759	54.944961
2932.042598	235673.503016	54.949965
2931.222210	235375.355428	54.954970
2930.500216	235077.498702	54.959975
2929.825694	234776.758009	54.964980
2929.011677	234467.102770	54.969985
2928.348900	234162.389841	54.974989
2927.213260	233873.157784	54.979994
2926.877214	233571.068577	54.984999
2926.389758	233269.335301	54.990004
2925.560981	232976.441632	54.995009
2925.193201	232679.147238	55.000013
2924.795512	232375.085481	55.005018
2923.710781	232074.672756	55.010023
2923.466436	231772.982144	55.015028
2922.361778	231468.271394	55.020033
2922.272941	231156.882510	55.025037
2921.333243	230858.284054	55.030042
2920.509258	230556.943825	55.035047
2920.023759	230246.028252	55.040052
2919.366350	229945.834946	55.045057
2918.820321	229645.064859	55.050061
2918.315584	229338.840460	55.055066
2917.037044	229025.966857	55.060071
2916.547662	228722.848492	55.065076
2915.775634	228421.914692	55.070081
2915.366509	228101.370204	55.075085
2914.432358	227820.196692	55.080090
2913.757079	227521.414942	55.085095
2913.746402	227208.347228	55.090100
2912.690653	226910.646320	55.095105
2912.356349	226601.629477	55.100109
2911.578821	226299.672934	55.105114
2910.995042	225983.390659	55.110119
2910.191031	225685.183283	55.115124
2909.640220	225378.573145	55.120129
2909.413189	225063.281837	55.125133
2908.126821	224757.427024	55.130138
2907.292075	224450.610771	55.135143
2906.869359	224142.572033	55.140148
2906.013083	223841.413684	55.145153
2905.505534	223530.157352	55.150157
2904.731801	223223.794493	55.155162
2904.195215	222916.389637	55.160167
2903.492843	222607.955681	55.165172
2902.945545	222304.246604	55.170177
2902.262637	221991.433020	55.175181
2901.555501	221688.986484	55.180186
2900.746254	221377.506593	55.185191
2900.260781	221070.495716	55.190196
2899.412991	220772.886904	55.195201
2898.929286	220464.465275	55.200205
2898.183803	220153.655071	55.205210
2897.431329	219847.798995	55.210215
2896.777728	219540.210096	55.215220
2896.170971	219239.450671	55.220225
2895.975571	218927.756666	55.225229
2894.810156	218622.098442	55.230234
2894.078604	218313.445152	55.235239
2893.542874	218007.358914	55.240244
2892.629037	217702.632219	55.245249
2892.176662	217399.501264	55.250253
2891.584557	217093.529762	55.255258
2891.007081	216780.454634	55.260263
2890.250296	216474.321005	55.265268
2889.553201	216175.625552	55.270273
2889.218785	215862.554300	55.275277
2888.109674	215552.636540	55.280282
2887.461887	215247.636720	55.285287
2887.078421	214936.754081	55.290292
2886.548060	214633.265865	55.295297
2885.628095	214321.618229	55.300301
2885.016251	214015.510971	55.305306
2884.348683	213701.624301	55.310311
2883.638380	213395.408230	55.315316
2882.972209	213097.612588	55.320321
2882.365078	212773.729265	55.325325
2881.686266	212476.282129	55.330330
2880.980198	212172.464008	55.335335
2880.584033	211851.390233	55.340340
2879.702739	211551.497519	55.345345
2878.991634	211235.262357	55.350349
2878.459229	210928.049833	55.355354
2877.612739	210612.462883	55.360359
2877.024586	210298.147554	55.365364
2876.119318	210008.282544	55.370369
2875.895000	209687.192597	55.375373
2874.983670	209391.476839	55.380378
2874.095318	209081.657057	55.385383
2873.633705	208768.220385	55.390388
2872.875980	208469.379326	55.395393
2872.351193	208160.092113	55.400397
2871.478012	207852.414344	55.405402
2870.977771	207545.468170	55.410407
2870.839744	207242.322459	55.415412
2869.876176	206937.387261	55.420417
2869.418101	206609.847258	55.425421
2868.727677	206303.803031	55.430426
2868.019705	205988.600021	55.435431
2867.298494	205672.140880	55.440436
2866.573931	205368.295919	55.445441
2865.886065	205059.661614	55.450445
2865.007212	204742.481654	55.455450
2864.589203	204431.428162	55.460455
2863.876389	204122.357424	55.465460
2862.872844	203822.280865	55.470465
2862.578493	203498.244968	55.475469
2862.223213	203199.418024	55.480474
2861.077661	202878.078402	55.485479
2860.874572	202570.068054	55.490484
2860.005581	202256.209191	55.495489
2859.297102	201946.271653	55.500493
2858.550587	201630.628070	55.505498
2858.056071	201316.384381	55.510503
2857.354592	201002.137090	55.515508
2856.222597	200696.091317	55.520513
2856.109813	200385.495635	55.525517
2855.524161	200074.518504	55.530522
2854.442944	199764.321526	55.535527
2853.980359	199451.279755	55.540532
2853.278521	199138.252253	55.545537
2852.740414	198827.389359	55.550541
2851.515327	198513.214076	55.555546
2850.893590	198206.160093	55.560551
2850.373502	197907.528311	55.565556
2849.572301	197604.616358	55.570561
2849.331303	197290.139868	55.575565
2848.438517	196980.514738	55.580570
2848.046895	196679.159334	55.585575
2847.582174	196366.276263	55.590580
2846.673982	196053.681637	55.595585
2846.167779	195742.832102	55.600589
2845.413875	195442.940994	55.605594
2844.879337	195119.222932	55.610599
2844.177607	194795.482521	55.615604
2843.117636	194497.185091	55.620609
2842.875356	194175.284502	55.625613
2841.792434	193869.767317	55.630618
2841.118879	193561.693344	55.635623
2840.775705	193252.207543	55.640628
2839.872982	192942.087048	55.645633
2839.302900	192632.144853	55.650637
2838.305014	192319.498673	55.655642
2837.886851	192002.627633	55.660647
2837.773489	191699.884003	55.665652
2836.640711	191392.239902	55.670657
2836.296222	191077.882407	55.675661
2835.448262	190765.744145	55.680666
2834.968295	190450.992346	55.685671
2834.087696	190136.280618	55.690676
2833.501399	189819.615963	55.695681
2832.931425	189503.307069	55.700685
2832.137816	189194.770992	55.705690
2831.145005	188883.329602	55.710695
2830.914310	188567.774775	55.715700
2830.051700	188268.504858	55.720705
2829.175213	187948.260195	55.725709
2828.912889	187636.749608	55.730714
2827.897707	187336.682924	55.735719
2827.499086	187022.895378	55.740724
2826.788860	186709.731804	55.745729
2826.430980	186391.909303	55.750733
2825.480388	186086.815482	55.755738
2825.062799	185769.184885	55.760743
2824.443479	185448.102776	55.765748
2823.561166	185139.277132	55.770753
2823.043482	184824.098821	55.775757
2822.173555	184509.067556	55.780762
2821.504061	184200.087469	55.785767
2820.976470	183876.114397	55.790772
2820.561997	183565.711741	55.795777
2819.860831	183252.074685	55.800781
2819.035487	182937.251056	55.805786
2818.156106	182618.418511	55.810791
2817.790835	182300.575399	55.815796
2816.830092	181992.814486	55.820801
2816.176194	181673.431600	55.825805
2815.707257	181350.294730	55.830810
2815.029053	181048.944968	55.835815
2814.531646	180733.220394	55.840820
2813.799778	180418.527435	55.845825
2813.354083	180097.813108	55.850829
2812.624307	179784.981599	55.855834
2811.675905	179467.378958	55.860839
2811.277263	179134.949575	55.865844
2810.222683	178830.291691	55.870849
2809.562579	178517.255023	55.875853
2809.060742	178201.397369	55.880858
2808.130610	177888.141066	55.885863
2807.568683	177578.084912	55.890868
2806.710310	177260.815436	55.895873
2806.146539	176939.775079	55.900877
2805.776618	176640.354039	55.905882
2804.760680	176329.272620	55.910887
2804.771213	176011.340971	55.915892
2803.613432	175698.289981	55.920897
2803.038182	175377.123779	55.925901
2802.524808	175069.406367	55.930906
2801.641056	174753.050645	55.935911
2801.063940	174438.492978	55.940916
2800.495083	174127.726453	55.945921
2799.779390	173803.746168	55.950925
2798.811216	173498.122250	55.955930
2797.898767	173184.555952	55.960935
2797.660681	172859.083316	55.965940
2796.804570	172558.586825	55.970945
2796.263964	172244.549400	55.975949
2795.911121	171930.611916	55.980954
2794.951978	171618.260890	55.985959
2794.446874	171311.881110	55.990964
2793.607919	170998.600368	55.995969
2793.244188	170688.642318	56.000973
2792.767017	170372.549743	56.005978
2791.676311	170059.634383	56.010983
2791.639314	169731.014913	56.015988
2790.612467	169426.665619	56.020993
2789.865351	169097.769828	56.025997
2789.322080	168775.304487	56.031002
2788.473666	168463.266657	56.036007
2787.930943	168145.626026	56.041012
2787.002855	167813.298505	56.046017
2786.742315	167455.474519	56.051021
2786.024682	167131.474030	56.056026
2785.144415	166832.017943	56.061031
2784.470692	166507.316537	56.066036
2784.302797	166172.098446	56.071041
2783.453611	165891.387595	56.076045
2782.682337	165536.511130	56.081050
2782.004770	165229.572002	56.086055
2781.501129	164907.311698	56.091060
2780.661484	164587.739427	56.096065
2780.024965	164265.009930	56.101069
2779.396343	163951.004315	56.106074
2778.702010	163640.050602	56.111079
2777.822458	163320.190609	56.116084
2777.150121	163003.504642	56.121089
2776.563894	162687.341812	56.126093
2775.972492	162372.759131	56.131098
2775.138260	162065.744375	56.136103
2774.380114	161747.493806	56.141108
2773.421609	161426.366345	56.146113
2773.142715	161117.123153	56.151117
2772.671047	160800.399457	56.156122
2771.866494	160495.465853	56.161127
2771.191143	160173.389520	56.166132
2770.642092	159860.500516	56.171137
2770.013718	159557.504967	56.176141
2769.187550	159232.715111	56.181146
2768.270866	158914.731299	56.186151
2767.763642	158600.537510	56.191156
2766.798681	158305.589778	56.196161
2766.317887	157981.443382	56.201165
2765.710448	157662.443199	56.206170
2764.850179	157382.487448	56.211175
2764.432327	157056.992266	56.216180
2763.869775	156743.319921	56.221185
2763.477909	156439.246391	56.226189
2762.632475	156126.819441	56.231194
2761.688331	155805.423786	56.236199
2761.255496	155486.365397	56.241204
2760.330024	155189.963701	56.246209
2759.824893	154864.528740	56.251213
2759.505091	154558.452269	56.256218
2758.497139	154247.936989	56.261223
2758.094343	153926.003195	56.266228
2757.521756	153633.868384	56.271233
2756.669103	153286.094441	56.276237
2755.811915	153005.983798	56.281242
2755.174192	152665.935832	56.286247
2754.581825	152369.963981	56.291252
2753.781942	152038.146405	56.296257
2753.566754	151741.535782	56.301261
2752.958076	151409.516326	56.306266
2751.825852	151115.713030	56.311271
2751.243264	150781.776616	56.316276
2750.754929	150499.277606	56.321281
2750.329337	150146.156597	56.326285
2749.377868	149863.622097	56.331290
2748.682269	149522.993233	56.336295
2748.217427	149230.613715	56.341300
2747.444420	148896.383773	56.346305
2746.338578	148608.445256	56.351309
2746.201156	148266.101851	56.356314
2745.524321	147963.498739	56.361319
2745.015482	147644.452388	56.366324
2744.022731	147323.045871	56.371329
2743.230420	147032.530257	56.376333
2743.261068	146703.711458	56.381338
2741.885031	146401.068823	56.386343
2741.304351	146047.433158	56.391348
2740.580864	145764.822687	56.396353
2740.019603	145430.646608	56.401357
2739.499843	145131.959772	56.406362
2738.805498	144822.133606	56.411367
2738.411614	144491.245032	56.416372
2737.395857	144201.045253	56.421377
2736.582040	143867.396164	56.426381
2736.193954	143547.787932	56.431386
2735.209743	143238.646196	56.436391
2734.698342	142939.242230	56.441396
2734.018467	142606.297193	56.446401
2733.330113	142293.725491	56.451405
2732.881855	141982.618302	56.456410
2731.994183	141678.864526	56.461415
2731.359110	141348.861270	56.466420
2730.858600	141041.139110	56.471425
2729.976918	140715.184192	56.476429
2729.671910	140420.105030	56.481434
2728.735623	140107.366491	56.486439
2728.200762	139794.707385	56.491444
2727.488912	139468.942390	56.496449
2726.874077	139163.455598	56.501453
2726.138073	138833.584929	56.506458
2725.467696	138533.335143	56.511463
2724.689940	138218.507730	56.516468
2724.008875	137909.410809	56.521473
2723.629335	137595.124076	56.526477
2722.957441	137280.289910	56.531482
2721.979605	136975.480338	56.536487
2721.491306	136653.102971	56.541492
2721.020115	136347.406628	56.546497
2720.205098	136037.728169	56.551501
2719.487673	135715.499096	56.556506
2718.718503	135392.125784	56.561511
2718.260392	135084.801907	56.566516
2717.405566	134777.849021	56.571521
2717.040143	134446.609876	56.576525
2716.630474	134138.564340	56.581530
2715.323011	133849.096052	56.586535
2714.968406	133515.261874	56.591540
2714.224337	133195.885202	56.596545
2713.424465	132874.628301	56.601549
2712.728173	132568.067767	56.606554
2712.187856	132273.857650	56.611559
2711.480326	131936.109463	56.616564
2710.681922	131635.214859	56.621569
2710.183995	131329.411135	56.626573
2709.646453	131010.979014	56.631578
2708.663661	130712.638388	56.636583
2708.254128	130382.533272	56.641588
2707.840209	130066.594443	56.646593
2707.032684	129755.141471	56.651597
2706.362390	129444.343389	56.656602
2705.617766	129125.292440	56.661607
2704.968300	128802.369141	56.666612
2704.208132	128505.007561	56.671617
2703.792072	128193.599032	56.676621
2703.376859	127869.011221	56.681626
2702.260705	127566.153553	56.686631
2701.611665	127243.248478	56.691636
2700.931651	126936.594949	56.696641
2700.102863	126613.611497	56.701645
2699.289563	126297.233075	56.706650
2698.857078	125991.338335	56.711655
2698.549996	125687.713007	56.716660
2697.681732	125385.119708	56.721665
2696.998048	125057.141138	56.726669
2696.930263	124734.161124	56.731674
2695.782812	124421.844954	56.736679
2695.134310	124100.082028	56.741684
2694.110323	123781.722068	56.746689
2693.490422	123476.761766	56.751693
2692.906684	123172.129368	56.756698
2692.147321	122853.662381	56.761703
2691.763851	122534.936502	56.766708
2690.901867	122235.450652	56.771713
2690.145272	121914.696281	56.776717
2689.721908	121603.199994	56.781722
2688.654562	121307.413980	56.786727
2688.541988	120982.188483	56.791732
2687.893596	120665.977652	56.796737
2686.954846	120360.119854	56.801741
2686.327685	120053.714768	56.806746
2685.933796	119746.438376	56.811751
2685.406502	119411.471272	56.816756
2684.267033	119098.543964	56.821761
2683.715308	118807.497302	56.826765
2683.251513	118461.506165	56.831770
2682.547935	118176.997149	56.836775
2681.455852	117842.419151	56.841780
2680.825819	117548.568064	56.846785
2679.676339	117232.104025	56.851789
2679.745393	116916.637809	56.856794
2678.677544	116635.561384	56.861799
2678.692578	116298.625636	56.866804
2677.353019	116005.329978	56.871809
2676.852654	115692.888830	56.876813
2676.205712	115394.654010	56.881818
2675.208580	115056.581279	56.886823
2674.934942	114783.218981	56.891828
2674.126570	114452.835888	56.896833
2673.534491	114172.314376	56.901837
2672.740889	113841.486365	56.906842
2671.932754	113560.237988	56.911847
2671.682456	113214.589118	56.916852
2671.079142	112896.017554	56.921857
2670.161839	112626.169743	56.926861
2669.526602	112324.675829	56.931866
2668.861825	111994.689614	56.936871
2668.369382	111724.175067	56.941876
2667.698785	111394.254895	56.946881
2667.244568	111074.597946	56.951885
2666.536506	110803.962654	56.956890
2665.333313	110461.453994	56.961895
2665.177682	110144.592043	56.966900
2664.270508	109834.440005	56.971905
2663.706794	109536.090934	56.976909
2663.325003	109257.622382	56.981914
2662.074421	108931.253799	56.986919
2661.663619	108608.474883	56.991924
2661.272115	108297.156645	56.996929
2660.317255	108017.993609	57.001933
2659.974092	107689.162972	57.006938
2659.027293	107389.041904	57.011943
2658.513656	107073.095245	57.016948
2657.998250	106753.574552	57.021953
2657.031955	106471.753753	57.026957
2656.486700	106130.483694	57.031962
2655.850845	105855.749168	57.036967
2655.470677	105515.407082	57.041972
2654.350001	105227.135042	57.046977
2654.048852	104897.295598	57.051981
2653.497515	104584.680530	57.056986
2652.492269	104283.066122	57.061991
2651.997320	103963.909513	57.066996
2651.105875	103652.661194	57.072001
2650.435722	103346.691763	57.077005
2650.176606	103032.071673	57.082010
2648.964601	102724.515095	57.087015
2648.655355	102401.347387	57.092020
2647.733234	102096.563366	57.097025
2647.053290	101782.305873	57.102029
2646.442771	101489.317331	57.107034
2645.624616	101187.922440	57.112039
2645.118085	100876.364649	57.117044
2644.499042	100559.380124	57.122049
2643.645924	100256.524941	57.127053
2643.148938	99944.921098	57.132058
2642.410183	99650.967612	57.137063
2642.043019	99317.322869	57.142068
2641.085696	99014.018492	57.147073
2640.478322	98730.102830	57.152077
2640.208378	98381.874597	57.157082
2638.888372	98102.938022	57.162087
2638.591246	97788.395268	57.167092
2637.871444	97482.682523	57.172097
2637.045224	97168.587345	57.177101
2636.548519	96864.756572	57.182106
2635.651595	96557.657389	57.187111
2635.263547	96235.051818	57.192116
2634.285060	95962.042547	57.197121
2633.879390	95631.096189	57.202125
2633.111091	95351.351440	57.207130
2632.558924	95024.559324	57.212135
2632.050360	94701.810942	57.217140
2631.439420	94422.769442	57.222145
2630.234303	94088.858902	57.227149
2630.037608	93817.489411	57.232154
2629.283943	93484.328080	57.237159
2629.007932	93172.281545	57.242164
2627.902825	92881.543302	57.247169
2627.339869	92576.785683	57.252173
2626.913203	92253.926697	57.257178
2625.837425	91946.950980	57.262183
2625.292273	91637.143631	57.267188
2624.537727	91336.047681	57.272193
2623.882376	91029.867783	57.277197
2623.331325	90710.868114	57.282202
2622.458662	90420.404542	57.287207
2621.990419	90091.110538	57.292212
2621.338505	89796.651340	57.297217
2620.399004	89501.715478	57.302221
2620.325876	89182.738515	57.307226
2618.960363	88856.122340	57.312231
2618.494725	88569.853990	57.317236
2618.211019	88255.767602	57.322241
2617.149468	87954.297954	57.327245
2616.283496	87653.784152	57.332250
2616.158746	87320.414251	57.337255
2614.904639	87046.006238	57.342260
2614.290359	86744.045285	57.347265
2613.820097	86412.880552	57.352269
2613.205958	86144.512596	57.357274
2612.127658	85819.691010	57.362279
2611.579848	85544.087397	57.367284
2611.128541	85210.510564	57.372289
2610.379166	84934.927777	57.377293
2610.020672	84635.960695	57.382298
2609.096280	84315.175409	57.387303
2608.620025	84028.183600	57.392308
2608.084953	83715.167303	57.397313
2607.309428	83399.145091	57.402317
2606.964270	83109.406926	57.407322
2606.086852	82798.847987	57.412327
2605.503040	82478.981088	57.417332
2604.787848	82174.204901	57.422337
2603.455957	81884.583008	57.427341
2603.255003	81565.360240	57.432346
2602.402824	81296.711474	57.437351
2602.339830	80949.933275	57.442356
2601.130333	80687.046389	57.447361
2600.366533	80360.858815	57.452365
2600.077677	80073.467030	57.457370
2599.601576	79756.913935	57.462375
2598.700289	79436.947734	57.467380
2597.982227	79154.750715	57.472385
2597.340258	78851.754434	57.477389
2596.886671	78528.645396	57.482394
2595.858645	78242.441875	57.487399
2595.307059	77921.411012	57.492404
2594.354191	77640.868853	57.497409
2593.797734	77315.970386	57.502413
2593.327125	77041.835780	57.507418
2592.471345	76733.728077	57.512423
2591.577638	76427.411492	57.517428
2590.886074	76127.675909	57.522433
2590.424853	75834.960082	57.527437
2590.182396	75532.393371	57.532442
2589.236062	75243.906586	57.537447
2588.849264	74936.676944	57.542452
2588.109169	74632.922812	57.547457
2587.442984	74322.306662	57.552461
2586.841809	74028.321514	57.557466
2586.005433	73725.318610	57.562471
2585.120021	73414.662589	57.567476
2584.682415	73119.378856	57.572481
2583.639174	72822.016264	57.577485
2583.314262	72518.665561	57.582490
2582.345091	72227.970682	57.587495
2581.931417	71929.609470	57.592500
2581.244581	71633.462452	57.597505
2580.283112	71328.001084	57.602509
2579.798734	71020.416504	57.607514
2578.708303	70736.451829	57.612519
2578.469661	70447.567632	57.617524
2577.481957	70165.007441	57.622529
2577.488937	69854.322856	57.627533
2576.741241	69541.583942	57.632538
2575.450726	69274.925574	57.637543
2575.318838	68967.576960	57.642548
2574.664400	68651.822666	57.647553
2573.943450	68376.795651	57.652557
2573.360878	68067.904935	57.657562
2572.765833	67777.292646	57.662567
2571.870830	67473.229873	57.667572
2571.493619	67183.516603	57.672577
2570.554023	66879.476553	57.677581
2569.955014	66604.284356	57.682586
2569.179542	66282.429061	57.687591
2568.713634	65986.997612	57.692596
2567.623071	65703.423025	57.697601
2566.905047	65412.786651	57.702605
2566.617925	65104.216300	57.707610
2565.941337	64815.868409	57.712615
2565.308861	64518.868056	57.717620
2564.477475	64217.987427	57.722625
2563.951364	63936.872904	57.727629
2563.208122	63636.949945	57.732634
2562.062500	63340.558999	57.737639
2561.625761	63052.288418	57.742644
2561.231318	62749.978276	57.747649
2559.892241	62475.887211	57.752653
2559.963135	62192.886742	57.757658
2558.884784	61891.585113	57.762663
2558.218565	61601.375472	57.767668
2557.628293	61321.205804	57.772673
2556.915458	61026.580605	57.777677
2556.237916	60727.905788	57.782682
2555.330611	60449.603690	57.787687
2555.027457	60162.897680	57.792692
2554.355733	59877.947931	57.797697
2553.537022	59583.656583	57.802701
2553.127472	59299.921226	57.807706
2552.615227	59006.036721	57.812711
2551.548558	58725.313580	57.817716
2551.275408	58443.835896	57.822721
2550.489079	58143.681457	57.827725
2550.096023	57858.123447	57.832730
2548.774019	57579.654629	57.837735
2548.264034	57283.011924	57.842740
2547.967258	56982.311352	57.847745
2547.024410	56712.951406	57.852749
2546.348660	56431.064982	57.857754
2545.342221	56137.994295	57.862759
2545.047543	55849.144710	57.867764
2544.375410	55573.059026	57.872769
2543.639244	55285.174395	57.877773
2543.225499	54975.977783	57.882778
2542.146632	54708.890327	57.887783
2541.614478	54425.258924	57.892788
2540.979166	54135.325921	57.897793
2540.244333	53844.214047	57.902797
2539.691081	53569.427727	57.907802
2539.211830	53282.590894	57.912807
2538.312708	52997.141439	57.917812
2537.715156	52720.077854	57.922817
2537.130154	52438.387520	57.927821
2536.454158	52136.975807	57.932826
2535.639513	51857.403368	57.937831
2534.897455	51574.802244	57.942836
2534.326948	51291.817694	57.947841
2533.627884	51004.751370	57.952845
2533.238939	50724.977224	57.957850
2532.501380	50436.840936	57.962855
2531.733010	50156.623298	57.967860
2531.023362	49876.868964	57.972865
2530.282785	49595.833194	57.977869
2529.563525	49303.770521	57.982874
2529.069437	49028.247094	57.987879
2528.254557	48749.754575	57.992884
2527.485751	48464.622420	57.997889
2526.269685	48195.559389	58.002893
2525.820953	47916.376622	58.007898
2525.137398	47643.432197	58.012903
2524.360945	47363.671145	58.017908
2523.595505	47098.501018	58.022913
2522.820121	46824.018099	58.027917
2522.632048	46552.631518	58.032922
2521.799174	46290.856023	58.037927
2521.164572	46027.575927	58.042932
2520.804492	45754.185717	58.047937
2519.630797	45481.700467	58.052941
2518.975160	45208.419403	58.057946
2518.277025	44951.389896	58.062951
2517.845782	44677.041052	58.067956
2516.944896	44409.576924	58.072961
2516.255127	44154.901345	58.077965
2515.952228	43883.697750	58.082970
2515.242849	43613.100442	58.087975
2514.702697	43350.598478	58.092980
2513.663505	43087.019005	58.097985
2512.883727	42819.319864	58.102989
2511.985540	42550.337620	58.107994
2511.396971	42299.322563	58.112999
2510.764183	42037.155654	58.118004
2509.822419	41774.203748	58.123009
2508.782499	41524.308719	58.128013
2508.862093	41267.596415	58.133018
2507.767986	41024.164665	58.138023
2506.851149	40765.377551	58.143028
2506.120678	40516.211777	58.148033
2505.659108	40271.653361	58.153037
2505.011860	40027.078871	58.158042
2504.031059	39776.464871	58.163047
2503.315883	39537.294246	58.168052
2502.707757	39297.238970	58.173057
2501.424328	39063.789708	58.178061
2500.914398	38828.769873	58.183066
2500.428055	38594.279111	58.188071
2499.642192	38357.216604	58.193076
2498.729367	38128.098580	58.198081
2497.793095	37902.008112	58.203085
2497.111987	37690.060582	58.208090
2496.130163	37465.491156	58.213095
2495.672075	37232.614430	58.218100
2495.027623	37022.664251	58.223105
2493.579389	36820.249252	58.228109
2492.821653	36603.165274	58.233114
2491.646252	36406.887364	58.238119
2490.767770	36214.609312	58.243124
2489.791940	36036.056865	58.248129
2488.860786	35857.967073	58.253133
2488.269164	35668.056947	58.258138
2487.138280	35505.044193	58.263143
2486.302118	35331.841283	58.268148
2485.564673	35167.231661	58.273153
2484.208983	35004.809427	58.278157
2483.373334	34853.364549	58.283162
2482.852142	34718.067229	58.288167
2482.256722	34555.841770	58.293172
2481.352135	34417.604920	58.298177
2480.300865	34291.591337	58.303181
2480.002754	34128.363630	58.308186
2478.845115	34006.634447	58.313191
2478.326238	33862.862021	58.318196
2477.934651	33731.258052	58.323201
2476.975267	33611.088561	58.328205
2476.537663	33479.206272	58.333210
2475.745261	33352.956504	58.338215
2475.027278	33222.097322	58.343220
2474.471244	33088.394327	58.348225
2474.084599	32960.575664	58.353229
2473.425879	32834.950235	58.358234
2472.390017	32706.948852	58.363239
2471.657673	32588.504840	58.368244
2471.304451	32463.190935	58.373249
2470.291995	32344.132562	58.378253
2469.701268	32216.777079	58.383258
2469.004873	32082.643067	58.388263
2468.278416	31977.812421	58.393268
2467.623056	31865.896894	58.398273
2467.030339	31744.703174	58.403277
2466.617968	31620.901430	58.408282
2465.989527	31513.217161	58.413287
2465.260750	31386.302396	58.418292
2464.525059	31262.997030	58.423297
2463.726130	31148.009036	58.428301
2463.150807	31029.243243	58.433306
2462.536689	30918.634338	58.438311
2461.953520	30805.515337	58.443316
2461.411046	30689.491320	58.448321
2460.646386	30575.739069	58.453325
2460.367278	30448.188313	58.458330
2459.659358	30339.726452	58.463335
2458.896444	30220.220491	58.468340
2458.508962	30095.631587	58.473345
2457.825678	29972.983314	58.478349
2457.355312	29849.608613	58.483354
2456.801952	29727.614642	58.488359
2455.763300	29607.807714	58.493364
2455.296501	29490.291930	58.498369
2454.489682	29365.479638	58.503373
2453.811635	29257.432590	58.508378
2453.376910	29120.080513	58.513383
2452.676949	28999.624015	58.518388
2452.060114	28880.717702	58.523393
2451.307016	28763.288893	58.528397
2450.847819	28630.532681	58.533402
2450.217987	28511.961312	58.538407
2449.623719	28395.754875	58.543412
2449.045764	28279.834205	58.548417
2447.974870	28163.986197	58.553421
2447.866104	28029.621681	58.558426
2446.851607	27908.957747	58.563431
2446.170862	27777.567478	58.568436
2445.946429	27655.353671	58.573441
2445.073511	27532.050910	58.578445
2444.592271	27408.360785	58.583450
2443.772847	27285.887088	58.588455
2443.122823	27147.973721	58.593460
2442.646661	27030.352451	58.598465
2441.829854	26902.057804	58.603469
2441.355522	26780.422580	58.608474
2440.744599	26653.901222	58.613479
2439.901337	26516.968510	58.618484
2439.542979	26393.974352	58.623489
2438.583146	26276.828590	58.628493
2438.204985	26154.475980	58.633498
2437.606123	26028.453618	58.638503
2436.382843	25883.693438	58.643508
2436.024694	25766.650290	58.648513
2435.196298	25640.988800	58.653517
2434.999543	25509.996780	58.658522
2434.204571	25387.443632	58.663527
2433.300429	25254.718618	58.668532
2432.595754	25118.467686	58.673537
2431.763881	25008.108999	58.678541
2431.361828	24874.502794	58.683546
2430.535933	24760.098303	58.688551
2429.978095	24630.716214	58.693556
2429.656929	24509.533539	58.698561
2428.597401	24390.473121	58.703565
2428.379458	24260.363366	58.708570
2427.331256	24129.156759	58.713575
2426.444175	24012.525397	58.718580
2426.029327	23898.337518	58.723585
2425.269806	23768.400563	58.728589
2424.481147	23647.627856	58.733594
2424.048244	23527.691190	58.738599
2423.700848	23402.541988	58.743604
2422.615496	23277.699499	58.748609
2421.872253	23163.746634	58.753613
2421.303424	23030.462659	58.758618
2420.630263	22912.181174	58.763623
2419.601078	22797.874352	58.768628
2419.412218	22668.718190	58.773633
2418.865686	22558.527081	58.778637
2417.885588	22426.726800	58.783642
2417.254279	22316.914034	58.788647
2416.399163	22202.572861	58.793652
2416.414390	22064.102835	58.798657
2415.174159	21949.103663	58.803661
2414.744941	21821.139003	58.808666
2414.113266	21708.159586	58.813671
2413.093974	21594.566568	58.818676
2413.018872	21471.756571	58.823681
2412.069122	21354.650192	58.828685
2410.916294	21228.492349	58.833690
2410.608603	21110.723036	58.838695
2410.091138	20979.671958	58.843700
2409.598516	20864.088453	58.848705
2408.833074	20763.901737	58.853709
2408.139950	20625.371908	58.858714
2407.808352	20512.601401	58.863719
2407.095785	20391.045305	58.868724
2406.400756	20257.916079	58.873729
2405.717367	20139.019895	58.878733
2404.644192	20014.091580	58.883738
2404.200555	19888.670493	58.888743
2403.492990	19777.687134	58.893748
2402.967421	19642.720870	58.898753
2402.014714	19534.589401	58.903757
2401.196926	19419.456122	58.908762
2400.680725	19296.552286	58.913767
2399.622244	19185.035505	58.918772
2399.486929	19058.524989	58.923777
2398.368121	18941.599627	58.928781
2397.740887	18838.893322	58.933786
2396.940503	18724.920499	58.938791
2396.255269	18611.401532	58.943796
2395.850321	18498.628755	58.948801
2394.789286	18394.793075	58.953805
2394.396586	18292.830746	58.958810
2393.869684	18174.942241	58.963815
2392.914122	18068.121138	58.968820
2392.801171	17951.470391	58.973825
2392.027039	17842.750050	58.978829
2391.449883	17727.309319	58.983834
2390.522689	17620.012192	58.988839
2389.413597	17504.106097	58.993844
2389.259173	17395.955265	58.998849
2388.252610	17291.504017	59.003853
2387.674234	17175.441438	59.008858
2387.152625	17080.188905	59.013863
2386.165214	16973.605751	59.018868
2385.399573	16868.950237	59.023873
2384.841178	16763.861594	59.028877
2384.190737	16649.577139	59.033882
2383.635209	16551.397777	59.038887
2382.756702	16451.623958	59.043892
2382.288119	16346.643885	59.048897
2381.430470	16254.008445	59.053901
2380.679577	16152.038070	59.058906
2380.080660	16053.413533	59.063911
2379.355200	15944.776562	59.068916
2378.697139	15840.208935	59.073921
2377.970771	15751.074091	59.078925
2377.241479	15653.258409	59.083930
2376.415536	15556.357840	59.088935
2375.656595	15471.625466	59.093940
2375.031805	15361.024035	59.098945
2374.606321	15277.609597	59.103949
2373.912544	15192.844158	59.108954
2373.189278	15095.304446	59.113959
2372.749452	15009.896673	59.118964
2372.241845	14893.528007	59.123969
2371.236231	14816.578797	59.128973
2370.265560	14709.182280	59.133978
2369.699093	14618.931345	59.138983
2369.074362	14539.517121	59.143988
2368.776495	14440.778052	59.148993
2367.923571	14356.114885	59.153997
2367.351693	14266.584563	59.159002
2366.720803	14165.917226	59.164007
2366.146015	14070.187763	59.169012
2365.221057	13984.149018	59.174017
2364.186213	13898.486444	59.179021
2363.924375	13800.761064	59.184026
2363.054802	13704.525457	59.189031
2362.214052	13632.702112	59.194036
2361.907356	13532.378964	59.199041
2360.816862	13451.135780	59.204045
2359.947058	13365.901448	59.209050
2359.414764	13289.520535	59.214055
2358.760864	13196.926113	59.219060
2358.286646	13121.866135	59.224065
2357.776925	13043.145660	59.229069
2357.033796	12945.868234	59.234074
2356.369694	12864.378674	59.239079
2355.344168	12797.182345	59.244084
2354.980676	12701.756337	59.249089
2354.593336	12634.973630	59.254093
2353.623059	12553.405469	59.259098
2353.263762	12465.996204	59.264103
2352.344777	12381.044078	59.269108
2351.556992	12285.906742	59.274113
2350.959130	12214.631660	59.279117
2350.419149	12128.100473	59.284122
2349.923547	12061.134664	59.289127
2349.046390	11966.548697	59.294132
2348.579841	11883.048555	59.299137
2347.532607	11794.507690	59.304141
2346.829851	11707.342101	59.309146
2346.015082	11639.405555	59.314151
2345.387838	11580.216621	59.319156
2344.879200	11496.190702	59.324161
2344.086377	11414.379009	59.329165
2343.239182	11341.271622	59.334170
2342.784468	11266.724687	59.339175
2342.183481	11195.877823	59.344180
2341.394197	11116.222431	59.349185
2340.892217	11046.486709	59.354189
2340.449370	10962.091557	59.359194
2339.446969	10883.776626	59.364199
2339.087969	10814.092091	59.369204
2338.295441	10731.888753	59.374209
2337.395918	10668.815724	59.379213
2336.799405	10589.979145	59.384218
2336.377646	10507.372650	59.389223
2335.302869	10449.477733	59.394228
2334.730870	10374.099720	59.399233
2334.058059	10307.235471	59.404237
2333.562736	10225.585423	59.409242
2332.773094	10157.793980	59.414247
2332.149615	10091.751689	59.419252
2331.799507	10017.368705	59.424257
2330.710926	9948.602316	59.429261
2330.386795	9867.335749	59.434266
2329.965915	9790.300382	59.439271
2328.960164	9714.064280	59.444276
2328.540141	9645.103315	59.449281
2327.848723	9565.897016	59.454285
2326.813889	9496.913525	59.459290
2326.155610	9414.338314	59.464295
2325.416978	9351.743912	59.469300
2325.198599	9278.847803	59.474305
2324.092690	9215.814793	59.479309
2323.363482	9148.950051	59.484314
2323.089003	9063.660769	59.489319
2322.256021	9009.188552	59.494324
2321.577674	8933.330123	59.499329
2320.880792	8869.953638	59.504333
2320.206491	8794.843552	59.509338
2319.736749	8719.473015	59.514343
2318.606393	8659.213708	59.519348
2318.354548	8575.859184	59.524353
2317.357153	8527.681009	59.529357
2316.834690	8449.172111	59.534362
2316.443521	8374.640091	59.539367
2315.467178	8314.565229	59.544372
2315.144191	8240.370962	59.549377
2314.265208	8178.260888	59.554381
2313.448618	8106.529554	59.559386
2312.576796	8036.708498	59.564391
2312.017132	7972.143380	59.569396
2311.666770	7913.843623	59.574401
2310.432958	7848.125358	59.579405
2309.941446	7773.332209	59.584410
2309.785255	7714.883712	59.589415
2308.873039	7656.984085	59.594420
2308.173072	7579.658055	59.599425
2307.597577	7524.125719	59.604429
2306.973805	7451.848688	59.609434
2306.397756	7389.048594	59.614439
2305.835832	7322.954733	59.619444
2304.983823	7251.907584	59.624449
2304.179335	7198.761908	59.629453
2303.203357	7137.648916	59.634458
2302.919653	7058.920157	59.639463
2301.979127	7005.907970	59.644468
2301.433096	6941.982522	59.649473
2301.072672	6877.749462	59.654477
2300.318293	6817.385141	59.659482
2299.780880	6746.655732	59.664487
2299.055882	6684.234046	59.669492
2298.401750	6612.451024	59.674497
2297.890949	6553.225238	59.679501
2296.869539	6486.737066	59.684506
2296.484265	6426.468032	59.689511
2295.861860	6364.686900	59.694516
2295.216245	6294.383030	59.699521
2294.364651	6234.049914	59.704525
2294.222144	6151.156203	59.709530
2293.256938	6101.302303	59.714535
2292.144514	6041.685735	59.719540
2291.677603	5970.302063	59.724545
2290.919196	5909.258229	59.729549
2290.245617	5847.030684	59.734554
2289.543026	5787.567837	59.739559
2289.135593	5736.565047	59.744564
2288.698201	5654.803834	59.749569
2287.675161	5605.251040	59.754573
2287.273291	5528.975307	59.759578
2286.476404	5470.098161	59.764583
2285.969192	5404.882036	59.769588
2285.241904	5339.806793	59.774593
2284.659240	5267.206576	59.779597
2283.597676	5223.015812	59.784602
2283.109538	5153.260271	59.789607
2282.633284	5084.851085	59.794612
2282.041411	5036.208246	59.799617
2280.923657	4974.200743	59.804621
2280.079265	4906.842964	59.809626
2279.509130	4842.133035	59.814631
2278.820713	4796.235990	59.819636
2278.183740	4727.949384	59.824641
2277.376555	4679.139970	59.829645
2276.872189	4614.661949	59.834650
2276.812715	4560.162265	59.839655
2276.047486	4505.840971	59.844660
2275.237195	4428.681404	59.849665
2274.382692	4374.202036	59.854669
2273.784045	4314.660821	59.859674
2273.377216	4250.960749	59.864679
2272.391769	4190.814174	59.869684
2272.117390	4128.031349	59.874689
2271.381752	4067.612213	59.879693
2270.433933	4010.391851	59.884698
2269.749636	3951.460340	59.889703
2269.057120	3899.369527	59.894708
2268.526521	3844.732707	59.899713
2267.695783	3779.276992	59.904718
2267.025481	3732.240024	59.909722
2266.268611	3664.092522	59.914727
2265.634099	3600.909297	59.919732
2265.261804	3548.582823	59.924737
2264.636093	3498.907875	59.929742
2263.750707	3437.656275	59.934746
2263.148346	3365.094600	59.939751
2262.556946	3315.246857	59.944756
2261.950256	3257.990312	59.949761
2261.057936	3201.655444	59.954766
2260.441216	3147.123998	59.959770
2259.939465	3083.779209	59.964775
2258.961904	3034.928170	59.969780
2258.764371	2966.839509	59.974785
2257.847468	2910.342480	59.979790
2256.886346	2864.688736	59.984794
2256.476168	2796.786794	59.989799
2255.559664	2747.821361	59.994804
2255.126728	2695.064372	59.999809
2254.312457	2637.862109	60.004814
2253.533755	2589.180533	60.009818
2253.397955	2534.280164	60.014823
2252.404188	2481.351099	60.019828
2251.604462	2422.106551	60.024833
2251.010194	2365.451636	60.029838
2250.314207	2318.148876	60.034842
2249.941252	2265.644151	60.039847
2249.135828	2204.446550	60.044852
2248.809498	2148.697823	60.049857
2248.047035	2110.403689	60.054862
2247.216909	2049.835978	60.059866
2246.858515	1978.403238	60.064871
2246.132634	1933.372749	60.069876
2245.050117	1882.708864	60.074881
2244.611749	1817.645231	60.079886
2243.922106	1758.909508	60.084890
2243.361800	1713.872360	60.089895
2242.475440	1661.179997	60.094900
2241.904632	1600.866355	60.099905
2241.135108	1553.987777	60.104910
2240.381942	1501.675435	60.109914
2239.958138	1438.279694	60.114919
2239.330780	1387.542186	60.119924
2238.499819	1342.050783	60.124929
2237.979592	1289.360042	60.129934
2237.180415	1226.299171	60.134938
2236.320083	1187.267611	60.139943
2235.606191	1142.254233	60.144948
2235.322943	1081.182754	60.149953
2234.492307	1030.245345	60.154958
2233.878777	979.185366	60.159962
2233.006972	918.886033	60.164967
2232.099054	880.244478	60.169972
2231.522012	825.702031	60.174977
2230.831397	789.759130	60.179982
2230.038322	738.731633	60.184986
2229.483024	695.556083	60.189991
2228.868872	649.841653	60.194996
2228.533936	599.101519	60.200001
2227.920759	558.780360	60.205006
2226.791653	515.292675	60.210010
2226.194891	465.709432	60.215015
2225.272987	422.124506	60.220020
2224.654465	389.299778	60.225025
2223.897707	345.692040	60.230030
2223.547068	300.047299	60.235034
2222.491741	261.497015	60.240039
2221.718708	218.236009	60.245044
2221.029274	186.194096	60.250049
2220.223066	146.418778	60.255054
2219.471213	122.244561	60.260058
2219.071251	80.228876	60.265063
2218.349943	67.804006	60.270068
2217.360994	40.412852	60.275073
2216.472146	7.974059	60.280078
2213.264909	63.287360	60.285082
2211.191702	102.937517	60.290087
2211.132967	99.167123	60.295092
2211.548799	103.130188	60.300097
2211.968318	102.757807	60.305102
2211.404131	91.880149	60.310106
2211.087976	84.495375	60.315111
2209.659917	92.425083	60.320116
2209.233206	104.082972	60.325121
2209.070250	104.137292	60.330126
2208.139971	109.597485	60.335130
2207.367775	107.610193	60.340135
2206.134584	109.794362	60.345140
2205.442925	99.955591	60.350145
2205.367348	98.625736	60.355150
2204.343321	107.054308	60.360154
2204.437327	100.801317	60.365159
2203.951334	113.097795	60.370164
2203.088174	107.365636	60.375169
2202.327466	101.112623	60.380174
2201.493149	104.092919	60.385178
2200.920352	103.204626	60.390183
2199.689308	106.585313	60.395188
2199.407063	109.616797	60.400193
2199.512523	107.837192	60.405198
2198.497059	112.087238	60.410202
2197.653661	101.413138	60.415207
2196.571054	110.730911	60.420212
2196.139502	104.829364	60.425217
2195.656228	102.444596	60.430222
2195.566242	112.349190	60.435226
2194.945106	100.529703	60.440231
2193.880579	107.433548	60.445236
2193.171613	106.443861	60.450241
2192.886782	104.055996	60.455246
2191.414532	116.840086	60.460250
2191.021877	110.661142	60.465255
2189.977868	112.094669	60.470260
2189.133178	112.187759	60.475265
2189.059793	111.291199	60.480270
2188.670431	108.241856	60.485274
2188.615707	110.882447	60.490279
2187.722905	106.541080	60.495284
2186.572524	110.752611	60.500289
2186.054405	100.709705	60.505294
2185.038455	112.702345	60.510298
2184.645364	100.972834	60.515303
2183.635752	109.613584	60.520308
2182.913356	99.733968	60.525313
2182.046436	107.998858	60.530318
2181.904840	99.436838	60.535322
2182.122748	97.536897	60.540327
2181.077208	107.624620	60.545332
2179.781979	106.849365	60.550337
2179.057386	106.565452	60.555342
2178.612407	116.723477	60.560346
2178.459144	109.628232	60.565351
2177.414266	110.022733	60.570356
2176.655568	113.405762	60.575361
2176.381735	103.136452	60.580366
2175.276218	109.362438	60.585370
2175.054482	103.112233	60.590375
2174.012019	110.487227	60.595380
2173.518768	99.633015	60.600385
2172.727062	110.025809	60.605390
2171.917874	100.137890	60.610394
2171.375951	105.038183	60.615399
2170.541325	109.382545	60.620404
2169.794426	108.039352	60.625409
2170.340403	103.602189	60.630414
2168.956525	109.440272	60.635418
2167.849621	103.510265	60.640423
2167.509933	103.865428	60.645428
2167.273932	103.655383	60.650433
2166.307872	98.256521	60.655438
2165.468711	105.772719	60.660442
2165.181729	102.363378	60.665447
2164.279534	100.000927	60.670452
2163.825231	108.140436	60.675457
2163.237849	103.386363	60.680462
2161.866436	106.034009	60.685466
2162.015976	101.033717	60.690471
2161.051119	106.338566	60.695476
2160.270011	100.153457	60.700481
2159.639262	103.133006	60.705486
2159.229584	110.407611	60.710490
2158.357304	95.206144	60.715495
2157.613741	106.989997	60.720500
2157.082961	103.819601	60.725505
2156.626198	103.247207	60.730510
2155.883884	101.305652	60.735514
2155.187308	102.404960	60.740519
2154.209257	105.319769	60.745524
2153.590216	94.342027	60.750529
2153.240752	101.454117	60.755534
2152.760136	113.344485	60.760538
2152.192302	95.256323	60.765543
2151.297063	93.080423	60.770548
2150.345395	108.440556	60.775553
2149.737243	85.979791	60.780558
2148.813458	97.770155	60.785562
2148.274375	94.134323	60.790567
2147.633661	99.821388	60.795572
2146.968458	93.356135	60.800577
2147.417116	90.325225	60.805582
2146.312085	98.023949	60.810586
2145.436951	95.996242	60.815591
2144.787964	91.788093	60.820596
2144.046993	100.375188	60.825601
2143.778144	92.626542	60.830606
2142.945813	100.595802	60.835610
2141.405003	90.828712	60.840615
2141.060731	97.600947	60.845620
2140.972227	107.803331	60.850625
2140.312703	94.649606	60.855630
2138.875471	96.967097	60.860634
2138.443170	99.948278	60.865639
2138.685967	101.390536	60.870644
2137.348144	100.886977	60.875649
2136.881496	92.318197	60.880654
2135.740727	101.287257	60.885658
2135.409541	104.463699	60.890663
2134.403981	103.746582	60.895668
2134.088251	105.332648	60.900673
2133.658246	95.504429	60.905678
2133.097790	102.515963	60.910682
2132.451314	96.460885	60.915687
2131.909719	104.207409	60.920692
2130.611365	101.981940	60.925697
2129.700929	99.343278	60.930702
2129.407253	110.549577	60.935706
2129.071871	97.036932	60.940711
2127.847634	98.519576	60.945716
2127.033512	103.975552	60.950721
2127.230452	95.687821	60.955726
2125.967632	98.917468	60.960730
2125.650529	104.480657	60.965735
2124.542973	101.294556	60.970740
2123.971789	92.195187	60.975745
2123.551614	104.304607	60.980750
2122.502558	107.894562	60.985754
2122.479448	105.692251	60.990759
2121.765872	105.986900	60.995764
2121.157026	100.351612	61.000769
2120.746418	102.965094	61.005774
2120.084535	102.258104	61.010778
2119.066871	97.600701	61.015783
2117.693333	100.989840	61.020788
2117.339666	98.390567	61.025793
2117.286980	99.231607	61.030798
2116.238043	104.581348	61.035802
2115.517036	97.480011	61.040807
2114.831220	103.770303	61.045812
2114.093217	96.871928	61.050817
2113.933606	104.490038	61.055822
2113.312032	108.215585	61.060826
2113.102069	98.614219	61.065831
2112.524172	100.379074	61.070836
2110.940533	98.649872	61.075841
2110.376568	96.774645	61.080846
2109.338831	97.076579	61.085850
2108.695722	103.536707	61.090855
2108.286659	102.617723	61.095860
2107.628556	98.141382	61.100865
2107.352679	89.927102	61.105870
2106.232721	105.746009	61.110874
2105.925437	97.121987	61.115879
2105.899267	97.689172	61.120884
2104.737303	94.885436	61.125889
2103.671354	93.111940	61.130894
2102.626638	99.697290	61.135898
2102.222538	95.647405	61.140903
2101.731331	100.154901	61.145908
2100.718693	96.182654	61.150913
2100.659076	96.938065	61.155918
2100.278901	109.008028	61.160922
2099.662658	103.500070	61.165927
2099.034427	99.328061	61.170932
2097.946570	102.761761	61.175937
2097.317259	90.886847	61.180942
2096.217794	104.447561	61.185946
2095.812697	96.326320	61.190951
2095.250462	95.660292	61.195956
2094.387607	93.578618	61.200961
2094.471255	92.942561	61.205966
2093.789195	98.680350	61.210970
2092.959903	95.625144	61.215975
2091.657084	90.104719	61.220980
2090.612839	102.965996	61.225985
2090.301564	93.584131	61.230990
2089.679008	105.186373	61.235994
2089.478105	103.726604	61.240999
2088.896304	94.721966	61.246004
2088.114963	100.710466	61.251009
2087.992866	92.046027	61.256014
2087.026765	99.989219	61.261018
2086.071033	92.854182	61.266023
2085.080692	93.911816	61.271028
2084.476462	105.205235	61.276033
2084.011802	96.382274	61.281038
2083.328076	103.474873	61.286042
2082.911820	89.878891	61.291047
2082.258088	100.148880	61.296052
2081.678782	97.380424	61.301057
2080.527401	86.944484	61.306062
2079.440434	94.851664	61.311066
2079.554474	99.884411	61.316071
2078.591936	96.281099	61.321076
2077.755883	102.357128	61.326081
2077.747795	94.234391	61.331086
2076.819996	101.586486	61.336090
2076.573768	94.662125	61.341095
2075.822033	94.535506	61.346100
2074.776038	100.250629	61.351105
2073.896933	91.815124	61.356110
2072.946992	102.840140	61.361114
2072.362365	92.610718	61.366119
2072.604809	103.765051	61.371124
2071.831415	94.108031	61.376129
2071.220226	102.941039	61.381134
2070.762662	96.520126	61.386138
2069.976299	103.411406	61.391143
2068.887788	101.937957	61.396148
2067.775394	102.387367	61.401153
2067.575999	99.937079	61.406158
2066.733557	103.327116	61.411162
2066.349489	107.719849	61.416167
2065.827786	105.645545	61.421172
2065.237766	109.241521	61.426177
2064.234020	87.204678	61.431182
2062.997209	105.464230	61.436186
2062.559761	102.256969	61.441191
2062.509978	100.599765	61.446196
2061.620460	108.056174	61.451201
2061.382789	87.585030	61.456206
2060.708765	101.950253	61.461210
2059.781666	110.279913	61.466215
2058.892517	92.898767	61.471220
2057.943098	103.281913	61.476225
2057.549931	113.395452	61.481230
2057.053570	106.624319	61.486234
2057.023006	100.777439	61.491239
2056.228176	101.916017	61.496244
2054.946863	107.941293	61.501249
2054.552838	98.802790	61.506254
2053.766668	100.550249	61.511258
2053.466643	106.028734	61.516263
2052.447552	98.645154	61.521268
2051.332852	97.174293	61.526273
2050.610147	99.376861	61.531278
2050.054948	108.260912	61.536282
2050.053543	106.217578	61.541287
2049.420523	88.445727	61.546292
2048.668417	102.807575	61.551297
2048.366394	96.997468	61.556302
2046.891140	106.601512	61.561306
2045.987861	97.668403	61.566311
2045.563874	90.970946	61.571316
2044.522179	102.967699	61.576321
2044.582467	92.815704	61.581326
2043.606752	99.566734	61.586330
2043.353653	101.895043	61.591335
2042.887544	94.851048	61.596340
2042.233587	104.490328	61.601345
2041.591341	89.536258	61.606350
2040.137907	95.472162	61.611354
2039.738933	96.388658	61.616359
2038.976239	93.844850	61.621364
2038.322039	95.156648	61.626369
2038.281221	99.244184	61.631374
2037.604249	103.286028	61.636378
2037.094339	99.702359	61.641383
2036.070869	102.871986	61.646388
2034.981215	100.406874	61.651393
2034.632457	98.160058	61.656398
2034.274007	106.859928	61.661402
2033.373238	99.853376	61.666407
2032.072897	102.619109	61.671412
2031.418962	101.084593	61.676417
2031.438297	96.901293	61.681422
2030.674255	108.305234	61.686426
2030.085431	108.439766	61.691431
2030.076880	106.009654	61.696436
2028.782076	99.808351	61.701441
2027.997225	96.657809	61.706446
2027.055832	104.535600	61.711450
2026.605070	101.109696	61.716455
2026.067362	106.684249	61.721460
2025.479375	99.347376	61.726465
2025.304538	100.900054	61.731470
2024.019792	95.723711	61.736474
2023.040884	98.802694	61.741479
2022.670342	100.946225	61.746484
2021.950939	98.365591	61.751489
2021.894282	94.684763	61.756494
2020.563357	104.076686	61.761498
2019.566247	93.652559	61.766503
2019.070797	93.179366	61.771508
2018.458858	96.635330	61.776513
2018.022312	96.630584	61.781518
2017.505938	91.734404	61.786522
2016.898747	90.499967	61.791527
2016.796270	92.077429	61.796532
2015.835056	96.456111	61.801537
2014.918311	95.767520	61.806542
2013.858926	95.032185	61.811546
2013.410894	98.747553	61.816551
2012.995950	95.315968	61.821556
2012.437082	93.159270	61.826561
2011.674856	95.735534	61.831566
2010.542222	100.739063	61.836570
2009.987789	97.482574	61.841575
2009.762106	97.608359	61.846580
2009.070279	103.805012	61.851585
2008.589087	95.489298	61.856590
2007.342588	105.479658	61.861594
2006.456507	99.525722	61.866599
2006.471834	95.805086	61.871604
2005.705729	90.601631	61.876609
2005.488072	91.658080	61.881614
2004.272912	102.171720	61.886618
2003.174614	108.812917	61.891623
2002.657284	96.103436	61.896628
2002.108877	103.698098	61.901633
2001.614765	104.404205	61.906638
2001.240181	105.282144	61.911642
2000.885322	95.583954	61.916647
1999.652347	105.118028	61.921652
1998.545960	114.102185	61.926657
1998.219500	95.647785	61.931662
1997.728985	103.383063	61.936666
1997.207923	102.587525	61.941671
1996.756114	95.908685	61.946676
1995.549683	105.143671	61.951681
1994.694349	95.695219	61.956686
1994.048411	91.026181	61.961690
1993.673385	105.061696	61.966695
1993.510478	98.562497	61.971700
1992.578646	112.851966	61.976705
1991.664406	95.512680	61.981710
1990.666604	104.507983	61.986714
1989.925272	99.895082	61.991719
1989.895230	93.904630	61.996724
1988.906761	104.349183	62.001729
1989.103254	97.704636	62.006734
1988.152172	95.734769	62.011738
1987.018482	97.015456	62.016743
1986.777377	95.025939	62.021748
1985.850076	109.368301	62.026753
1985.542182	95.840296	62.031758
1984.374265	103.544327	62.036762
1983.504451	100.568127	62.041767
1982.937545	96.438455	62.046772
1982.212648	108.093222	62.051777
1981.991522	99.512318	62.056782
1981.291445	98.481857	62.061786
1980.327660	94.039882	62.066791
1979.724536	99.962274	62.071796
1978.662026	105.605939	62.076801
1978.490800	89.315628	62.081806
1978.177428	93.454305	62.086810
1977.669327	91.814660	62.091815
1976.859200	86.906773	62.096820
1975.559174	88.108213	62.101825
1975.080172	87.857913	62.106830
1974.370186	90.682925	62.111834
1973.726354	101.023894	62.116839
1973.986974	91.229599	62.121844
1972.511175	100.953603	62.126849
1971.874699	92.066487	62.131854
1971.330964	95.872740	62.136858
1970.649156	97.135322	62.141863
1970.323173	94.873864	62.146868
1969.033431	103.004072	62.151873
1968.255360	81.363544	62.156878
1967.547824	97.340931	62.161882
1966.819069	95.029869	62.166887
1966.349985	100.971987	62.171892
1966.128099	99.185993	62.176897
1965.872943	97.988726	62.181902
1964.904040	87.758840	62.186906
1963.874766	90.541498	62.191911
1963.641523	89.779127	62.196916
1962.689789	88.432242	62.201921
1962.821685	87.440033	62.206926
1961.466427	88.448407	62.211930
1960.559439	93.435058	62.216935
1959.962143	95.635088	62.221940
1959.272686	91.756678	62.226945
1958.891998	97.691072	62.231950
1957.851641	90.555333	62.236954
1956.723383	85.217002	62.241959
1956.319090	87.695464	62.246964
1955.738889	96.403722	62.251969
1955.664865	81.093009	62.256974
1955.130053	92.023768	62.261978
1954.632559	92.497041	62.266983
1953.864669	78.591089	62.271988
1952.532460	92.756450	62.276993
1952.171675	86.621394	62.281998
1952.040868	93.208373	62.287002
1950.602478	92.676720	62.292007
1949.749202	79.902331	62.297012
1949.074153	89.138127	62.302017
1948.421621	89.793699	62.307022
1948.152156	87.908032	62.312026
1947.618038	85.998146	62.317031
1947.568365	91.709693	62.322036
1946.235224	90.562122	62.327041
1945.337112	89.719218	62.332046
1944.670778	85.160662	62.337050
1944.079896	85.837986	62.342055
1943.914788	81.516822	62.347060
1942.966700	92.905827	62.352065
1942.058764	90.788788	62.357070
1941.381404	91.128196	62.362074
1940.623010	84.737727	62.367079
1940.538824	92.309163	62.372084
1939.825661	95.226147	62.377089
1939.233497	86.669464	62.382094
1938.314488	93.894046	62.387098
1937.327448	89.638700	62.392103
1936.907362	85.619772	62.397108
1936.121851	102.297065	62.402113
1935.918790	88.872282	62.407118
1934.693225	88.027748	62.412122
1933.725177	92.391770	62.417127
1933.781242	79.238085	62.422132
1933.077732	104.315017	62.427137
1932.964500	96.753007	62.432142
1931.757981	85.767687	62.437146
1930.641407	98.531677	62.442151
1930.152730	79.549585	62.447156
1929.485230	91.808641	62.452161
1929.412661	82.409427	62.457166
1929.154748	84.244942	62.462170
1928.151657	86.350129	62.467175
1927.308157	81.382907	62.472180
1926.228870	93.114426	62.477185
1925.085069	88.049800	62.482190
1924.703124	91.046667	62.487194
1924.563746	95.715944	62.492199
1923.749940	86.880651	62.497204
1923.082287	98.169957	62.502209
1922.816811	86.579538	62.507214
1921.983230	88.421286	62.512218
1920.977327	91.127714	62.517223
1920.262055	86.805581	62.522228
1919.919354	96.354463	62.527233
1919.402400	89.145117	62.532238
1918.262945	95.633606	62.537242
1917.492596	92.603796	62.542247
1916.916756	85.604065	62.547252
1916.192753	94.541726	62.552257
1916.090541	90.224770	62.557262
1915.713719	88.608450	62.562266
1914.822931	85.053739	62.567271
1914.070533	83.490734	62.572276
1913.086290	97.665528	62.577281
1912.862879	96.450612	62.582286
1911.579039	92.068935	62.587290
1910.662117	94.534171	62.592295
1910.471093	89.075461	62.597300
1909.779315	96.547818	62.602305
1909.285193	95.265496	62.607310
1909.086545	87.043727	62.612314
1908.269370	94.654255	62.617319
1907.354438	85.421881	62.622324
1906.383485	85.131424	62.627329
1906.122752	88.191048	62.632334
1904.819137	92.698233	62.637338
1904.017320	84.545412	62.642343
1903.829462	88.621592	62.647348
1903.122375	90.705027	62.652353
1902.644682	75.769058	62.657358
1902.263487	88.304347	62.662362
1901.766632	86.844274	62.667367
1901.065137	88.562563	62.672372
1900.204171	94.119064	62.677377
1899.440690	85.811931	62.682382
1898.203888	90.021519	62.687386
1897.137373	88.338083	62.692391
1897.353214	83.313081	62.697396
1896.467371	97.339798	62.702401
1895.712871	91.018108	62.707406
1895.470724	88.976730	62.712410
1894.979939	92.673668	62.717415
1894.752550	85.702200	62.722420
1893.521823	101.932961	62.727425
1893.005887	92.083761	62.732430
1892.398600	90.556069	62.737434
1891.055129	92.776805	62.742439
1890.515809	84.758927	62.747444
1889.512747	90.968740	62.752449
1889.414082	89.399725	62.757454
1889.125927	94.840061	62.762458
1888.406305	91.128881	62.767463
1887.769612	81.901228	62.772468
1886.473278	91.815960	62.777473
1886.014373	84.602140	62.782478
1885.838512	90.453559	62.787482
1885.175776	90.826928	62.792487
1884.209401	85.076597	62.797492
1883.245612	82.263583	62.802497
1882.848837	83.626007	62.807502
1882.383990	86.678615	62.812506
1881.159016	86.885791	62.817511
1880.409457	89.382809	62.822516
1879.479356	97.184730	62.827521
1879.313247	83.293650	62.832526
1878.737612	88.044799	62.837530
1878.559224	89.648508	62.842535
1878.562522	76.127913	62.847540
1876.901832	94.883707	62.852545
1876.282967	80.507871	62.857550
1875.700686	84.145223	62.862554
1874.544145	81.577269	62.867559
1873.821637	80.484172	62.872564
1872.942173	91.912758	62.877569
1872.745460	88.306213	62.882574
1872.657854	79.956443	62.887578
1871.622441	87.451821	62.892583
1871.521505	81.251876	62.897588
1870.301124	86.466493	62.902593
1869.542836	87.340715	62.907598
1869.185790	82.711003	62.912602
1868.343066	89.548193	62.917607
1867.553696	79.655693	62.922612
1866.886309	90.317360	62.927617
1866.233704	82.320630	62.932622
1865.658200	91.310411	62.937626
1865.454736	91.725981	62.942631
1864.590874	75.236612	62.947636
1863.487688	87.802953	62.952641
1863.206914	85.250497	62.957646
1862.348731	85.071456	62.962650
1861.686142	82.899726	62.967655
1861.032771	84.812224	62.972660
1859.806525	93.449606	62.977665
1859.754888	96.578534	62.982670
1859.834941	85.625522	62.987674
1858.474926	95.332768	62.992679
1857.223492	91.138355	62.997684
1856.903720	85.463563	63.002689
1856.436244	82.671104	63.007694
1856.243800	84.455232	63.012698
1855.259508	84.371906	63.017703
1854.526664	83.531179	63.022708
1853.289824	89.014910	63.027713
1853.029191	85.222984	63.032718
1852.630581	79.538636	63.037722
1851.799748	84.686681	63.042727
1850.972013	80.171127	63.047732
1850.304100	92.368760	63.052737
1849.586993	82.658748	63.057742
1849.055756	81.303489	63.062746
1848.678408	96.312295	63.067751
1848.233829	86.869656	63.072756
1847.242051	83.901835	63.077761
1846.918349	92.306041	63.082766
1846.237680	89.637313	63.087770
1844.459333	92.471141	63.092775
1844.206687	85.937333	63.097780
1843.742498	85.694166	63.102785
1843.026863	89.360582	63.107790
1842.926791	89.349749	63.112794
1842.001977	96.978961	63.117799
1841.193409	88.398324	63.122804
1840.338000	88.573648	63.127809
1839.992282	91.780805	63.132814
1839.806681	78.252361	63.137818
1838.156448	91.183100	63.142823
1837.397682	85.576436	63.147828
1836.982625	88.699989	63.152833
1836.647079	87.707880	63.157838
1836.242808	83.203938	63.162842
1835.670550	94.303073	63.167847
1835.036771	89.113359	63.172852
1833.988184	90.852083	63.177857
1833.714868	90.156009	63.182862
1832.506045	90.172994	63.187866
1831.528162	97.427454	63.192871
1831.239198	85.605831	63.197876
1830.255425	84.377619	63.202881
1829.968261	95.962896	63.207886
1829.778875	87.569366	63.212890
1828.981636	83.704958	63.217895
1827.913459	80.353480	63.222900
1827.320417	88.152352	63.227905
1827.022959	99.168437	63.232910
1826.346616	85.112388	63.237914
1825.007238	83.946948	63.242919
1824.525121	77.988874	63.247924
1824.171230	90.527714	63.252929
1823.492267	94.150468	63.257934
1822.744573	89.929703	63.262938
1821.737266	95.208278	63.267943
1821.538803	87.519479	63.272948
1820.666024	89.930427	63.277953
1820.349200	88.003412	63.282958
1819.572633	85.873444	63.287962
1818.392590	84.771013	63.292967
1818.415703	82.293308	63.297972
1817.500763	84.534340	63.302977
1816.909052	92.870721	63.307982
1816.314197	85.445127	63.312986
1815.479219	85.998820	63.317991
1815.288609	78.245704	63.322996
1814.139691	92.872419	63.328001
1812.910254	90.782824	63.333006
1812.394497	77.380924	63.338010
1812.010333	89.175553	63.343015
1811.367961	84.102325	63.348020
1810.853234	80.968888	63.353025
1810.933159	75.147068	63.358030
1809.775321	94.010693	63.363034
1808.413206	93.318781	63.368039
1808.205195	82.085104	63.373044
1807.774546	85.324671	63.378049
1806.831895	90.466832	63.383054
1805.745239	90.484930	63.388058
1805.032945	86.889302	63.393063
1804.583662	81.675035	63.398068
1804.244908	93.125006	63.403073
1803.991109	90.937262	63.408078
1803.618629	81.953100	63.413082
1802.360346	94.471555	63.418087
1801.832690	80.497562	63.423092
1801.174686	87.360627	63.428097
1799.955206	86.529383	63.433102
1799.022008	81.158580	63.438106
1798.371747	88.752088	63.443111
1798.610268	80.240159	63.448116
1797.667195	91.090686	63.453121
1797.445267	81.063956	63.458126
1796.381772	89.640825	63.463130
1795.417461	82.308597	63.468135
1795.059131	81.775830	63.473140
1794.644345	75.346625	63.478145
1793.884138	85.341827	63.483150
1793.038130	86.636834	63.488154
1792.276467	82.678484	63.493159
1791.884790	70.482128	63.498164
1791.272908	84.041170	63.503169
1790.407533	79.870643	63.508174
1789.629313	82.359620	63.513178
1788.949155	85.556812	63.518183
1788.569294	73.509959	63.523188
1787.425142	75.643901	63.528193
1786.399079	81.732822	63.533198
1786.122367	85.077251	63.538202
1785.369462	79.102265	63.543207
1785.318535	86.171692	63.548212
1784.794375	81.924907	63.553217
1784.156485	79.578974	63.558222
1783.444097	79.403615	63.563226
1782.410732	92.244310	63.568231
1781.931792	86.050784	63.573236
1780.989887	84.103194	63.578241
1780.338205	82.155248	63.583246
1779.662295	74.007719	63.588250
1779.061367	80.377620	63.593255
1778.924575	78.852512	63.598260
1777.967897	83.771414	63.603265
1776.921434	76.714004	63.608270
1776.525497	79.746222	63.613274
1775.854377	83.648422	63.618279
1775.694398	82.432910	63.623284
1774.626472	79.313216	63.628289
1773.621841	77.946420	63.633294
1773.348322	79.599931	63.638298
1772.395353	83.308781	63.643303
1772.010701	82.944192	63.648308
1771.048870	83.302011	63.653313
1770.537555	92.636409	63.658318
1770.340355	80.658314	63.663322
1769.424268	91.329529	63.668327
1767.989270	84.739077	63.673332
1767.589792	78.870391	63.678337
1767.002867	90.842294	63.683342
1767.001296	78.487799	63.688346
1766.505097	91.060277	63.693351
1765.770915	92.323342	63.698356
1764.758234	87.703152	63.703361
1764.058411	87.294002	63.708366
1762.893589	75.028050	63.713370
1761.736983	87.640748	63.718375
1761.857926	84.928321	63.723380
1761.387091	93.300705	63.728385
1760.717656	89.783435	63.733390
1760.319596	87.394690	63.738394
1759.763807	97.010531	63.743399
1758.597696	84.265407	63.748404
1757.826158	81.248456	63.753409
1757.450503	83.481133	63.758414
1757.075535	85.295829	63.763418
1755.696159	92.872676	63.768423
1755.066169	89.949934	63.773428
1754.451423	81.969306	63.778433
1754.108593	80.495842	63.783438
1753.578893	82.954823	63.788442
1753.208766	86.777692	63.793447
1752.234773	84.616023	63.798452
1751.786776	79.575021	63.803457
1750.584555	79.980484	63.808462
1750.026913	81.267553	63.813466
1748.840183	92.424856	63.818471
1748.639240	77.460758	63.823476
1748.125078	92.473940	63.828481
1747.662227	83.843171	63.833486
1747.232613	85.171407	63.838490
1745.963577	84.893658	63.843495
1745.712772	82.060505	63.848500
1745.058764	85.750270	63.853505
1744.380511	90.117213	63.858510
1743.435876	79.006843	63.863514
1742.478588	83.970005	63.868519
1742.368579	84.200439	63.873524
1741.824488	89.255670	63.878529
1740.501791	86.416137	63.883534
1740.019591	84.135371	63.888538
1739.291654	86.715720	63.893543
1739.266550	91.366848	63.898548
1738.740212	87.572982	63.903553
1737.094973	87.257217	63.908558
1736.885533	65.919172	63.913562
1736.400337	82.496734	63.918567
1735.817183	82.110062	63.923572
1734.655531	90.890188	63.928577
1733.647721	89.176999	63.933582
1733.454085	82.449344	63.938586
1732.415081	76.407857	63.943591
1732.598044	80.410955	63.948596
1731.916853	84.966014	63.953601
1730.907641	82.920329	63.958606
1730.287061	79.587691	63.963610
1729.411308	81.141317	63.968615
1729.127097	77.364194	63.973620
1728.745024	77.002356	63.978625
1727.844446	81.368341	63.983630
1726.891994	76.675531	63.988634
1726.306583	77.903940	63.993639
1725.976388	80.394315	63.998644
1724.906991	79.454120	64.003649
1724.007666	75.118709	64.008654
1723.723499	79.997048	64.013658
1722.998556	81.898868	64.018663
1722.624993	76.128574	64.023668
1721.731784	81.199830	64.028673
1721.327569	85.818130	64.033678
1720.719590	82.108196	64.038682
1719.584566	79.950040	64.043687
1718.943586	76.518148	64.048692
1718.245729	76.583338	64.053697
1717.181767	87.391583	64.058702
1717.577018	74.959882	64.063706
1716.367902	84.389337	64.068711
1715.568698	78.882177	64.073716
1714.806407	81.486909	64.078721
1714.265492	82.511145	64.083726
1714.250981	81.687252	64.088730
1713.626389	80.815181	64.093735
1712.416978	71.471986	64.098740
1712.178731	82.029243	64.103745
1711.220244	82.913229	64.108750
1709.808199	80.988299	64.113754
1709.101612	81.296140	64.118759
1708.587764	78.020670	64.123764
1708.597074	75.917302	64.128769
1708.206250	72.735829	64.133774
1708.155811	70.400690	64.138778
1706.752546	81.329051	64.143783
1706.174337	73.635939	64.148788
1705.360508	67.998653	64.153793
1704.402668	82.891492	64.158798
1703.519886	79.177903	64.163802
1702.800972	72.724488	64.168807
1702.574851	77.364961	64.173812
1701.968971	75.570604	64.178817
1701.461301	74.164328	64.183822
1700.892166	75.754415	64.188826
1699.810731	79.046898	64.193831
1699.353414	70.978215	64.198836
1698.759777	82.356701	64.203841
1697.449819	85.072077	64.208846
1697.258385	76.951700	64.213850
1696.545977	90.525145	64.218855
1696.141862	82.668769	64.223860
1695.751792	77.776267	64.228865
1694.113916	80.119548	64.233870
1693.850579	85.849248	64.238874
1692.985230	85.035921	64.243879
1692.724884	73.804279	64.248884
1692.360501	82.840964	64.253889
1691.081540	90.271009	64.258894
1690.816391	73.270342	64.263898
1690.043869	76.039123	64.268903
1689.662694	73.234571	64.273908
1688.594157	71.409628	64.278913
1687.541202	72.715460	64.283918
1687.485641	69.450780	64.288922
1686.736661	87.544622	64.293927
1686.172537	72.933104	64.298932
1685.565771	66.994869	64.303937
1684.826191	82.048576	64.308942
1684.506502	81.199043	64.313946
1683.405917	86.348980	64.318951
1682.272529	74.089121	64.323956
1681.813895	84.884801	64.328961
1681.280365	81.128362	64.333966
1681.158526	73.875255	64.338970
1680.194482	84.741750	64.343975
1679.319919	87.451054	64.348980
1678.974838	79.722495	64.353985
1678.292531	74.553157	64.358990
1677.774404	75.446053	64.363994
1676.658934	80.855385	64.368999
1675.888904	79.967003	64.374004
1675.333848	68.462074	64.379009
1674.924260	75.208431	64.384014
1674.521861	76.034062	64.389018
1672.959089	82.417994	64.394023
1672.574038	79.341259	64.399028
1672.173392	76.900906	64.404033
1671.940969	77.491392	64.409038
1671.287548	76.459916	64.414042
1670.002526	86.527464	64.419047
1669.556346	79.135072	64.424052
1669.414607	75.325867	64.429057
1668.003426	80.808980	64.434062
1667.289855	72.129759	64.439066
1666.407103	84.260613	64.444071
1666.420097	74.707506	64.449076
1666.035126	84.587937	64.454081
1664.817810	74.173748	64.459086
1664.063037	78.231177	64.464090
1663.150980	82.594274	64.469095
1663.221131	80.897537	64.474100
1662.752324	79.234373	64.479105
1661.547894	82.896474	64.484110
1660.767963	85.950279	64.489114
1659.880481	86.666894	64.494119
1659.909327	84.164627	64.499124
1659.254562	74.690783	64.504129
1657.991483	79.641045	64.509134
1657.759077	90.184764	64.514138
1656.992528	87.285318	64.519143
1656.415979	77.390638	64.524148
1655.694981	73.220884	64.529153
1654.433337	89.093930	64.534158
1654.256745	74.733086	64.539162
1654.057651	72.718015	64.544167
1653.410497	84.688452	64.549172
1652.145313	79.857700	64.554177
1651.340397	73.621381	64.559182
1651.265705	75.132937	64.564186
1650.616842	81.633470	64.569191
1649.445797	80.230083	64.574196
1648.926885	73.774877	64.579201
1647.996931	79.304553	64.584206
1647.722456	61.029704	64.589210
1647.557264	77.876534	64.594215
1646.722227	79.414258	64.599220
1645.933563	72.211889	64.604225
1645.264112	80.738821	64.609230
1644.454921	70.475849	64.614234
1642.969681	69.871390	64.619239
1642.508396	71.206249	64.624244
1641.940430	65.175135	64.629249
1641.613153	68.514988	64.634254
1641.553415	66.015758	64.639258
1640.979930	73.945577	64.644263
1640.373156	75.152167	64.649268
1639.651205	67.579679	64.654273
1638.697076	78.143423	64.659278
1637.665712	70.913382	64.664282
1636.787443	69.075584	64.669287
1636.273482	75.073741	64.674292
1636.127180	74.501008	64.679297
1635.320772	81.848121	64.684302
1634.762032	70.581898	64.689306
1633.629738	74.659882	64.694311
1633.079562	80.871941	64.699316
1632.716608	71.197220	64.704321
1631.708444	74.236826	64.709326
1631.336435	66.484179	64.714330
1630.416243	74.795488	64.719335
1630.084653	74.769404	64.724340
1629.700756	65.776070	64.729345
1628.730047	73.604996	64.734350
1627.997651	74.494094	64.739354
1627.168495	71.025895	64.744359
1626.770326	76.833780	64.749364
1626.045609	76.043866	64.754369
1625.113358	64.781794	64.759374
1625.153244	62.318777	64.764378
1624.429900	70.023256	64.769383
1623.290747	74.059758	64.774388
1622.623037	75.141998	64.779393
1621.764738	65.555434	64.784398
1621.315364	75.662123	64.789402
1619.932504	68.785960	64.794407
1619.510828	75.452245	64.799412
1619.252419	73.924392	64.804417
1618.524110	66.212580	64.809422
1618.373965	80.188688	64.814426
1617.952877	76.031223	64.819431
1617.157538	77.326119	64.824436
1616.305138	72.519696	64.829441
1615.396648	76.295642	64.834446
1614.202543	75.490417	64.839450
1613.549334	78.273379	64.844455
1613.047868	73.543665	64.849460
1613.331943	78.169319	64.854465
1612.497536	81.545588	64.859470
1611.390920	73.703072	64.864474
1610.487924	83.490766	64.869479
1610.021009	82.956353	64.874484
1609.625142	79.137064	64.879489
1608.523038	93.688594	64.884494
1607.580606	75.668079	64.889498
1607.182470	78.402636	64.894503
1606.630028	84.476296	64.899508
1606.429082	79.780837	64.904513
1606.079878	84.787782	64.909518
1605.560540	80.466163	64.914522
1604.137727	80.939851	64.919527
1603.496177	77.310974	64.924532
1602.738689	84.117341	64.929537
1601.335789	83.037801	64.934542
1601.055238	73.491914	64.939546
1600.602893	79.502365	64.944551
1600.313827	72.301065	64.949556
1600.243681	82.494163	64.954561
1598.981748	79.679745	64.959566
1598.363039	77.504271	64.964570
1597.758463	76.903426	64.969575
1596.878648	74.682706	64.974580
1596.031036	79.581183	64.979585
1595.031112	72.398204	64.984590
1594.890523	75.038233	64.989594
1594.216501	82.162484	64.994599
1594.009181	80.319026	64.999604
1593.454629	76.624294	65.004609
1592.475186	81.915858	65.009614
1591.759743	76.661929	65.014618
1590.644164	72.710994	65.019623
1589.581431	76.900940	65.024628
1589.545514	67.538534	65.029633
1588.702250	80.822128	65.034638
1588.570743	71.574248	65.039642
1588.154981	78.116601	65.044647
1587.182803	69.973635	65.049652
1586.739884	72.950262	65.054657
1585.648026	74.732222	65.059662
1584.513314	75.622174	65.064666
1583.991848	72.783161	65.069671
1583.350761	79.151589	65.074676
1583.134274	70.104860	65.079681
1582.348024	73.454562	65.084686
1582.104948	73.021781	65.089690
1580.887841	73.961093	65.094695
1580.106376	66.352352	65.099700
1579.997237	75.397369	65.104705
1579.286117	75.489933	65.109710
1578.749643	65.609420	65.114714
1577.912552	71.501233	65.119719
1577.340203	84.311305	65.124724
1576.369119	74.624408	65.129729
1575.196014	75.421120	65.134734
1574.797479	72.690306	65.139738
1574.286077	78.878867	65.144743
1573.957153	79.984561	65.149748
1573.395858	67.994982	65.154753
1572.172884	77.939169	65.159758
1571.772416	78.149529	65.164762
1571.087240	76.880286	65.169767
1570.739739	78.818367	65.174772
1570.348224	62.985788	65.179777
1568.975624	78.592640	65.184782
1568.492485	65.589334	65.189786
1568.013240	80.223242	65.194791
1567.134359	77.493055	65.199796
1566.082336	70.693664	65.204801
1565.491138	79.222367	65.209806
1565.064530	74.356198	65.214810
1564.853638	71.780067	65.219815
1564.060202	76.859168	65.224820
1563.322142	76.907134	65.229825
1562.482980	75.518864	65.234830
1562.034779	80.407505	65.239834
1561.408891	71.969846	65.244839
1560.310264	72.510317	65.249844
1559.773688	64.758603	65.254849
1559.124289	73.331242	65.259854
1558.917318	69.795751	65.264858
1557.474513	71.474217	65.269863
1556.689603	69.907028	65.274868
1556.712459	75.830942	65.279873
1556.123826	74.943737	65.284878
1555.751227	72.740211	65.289882
1555.112195	76.189527	65.294887
1553.825300	70.209588	65.299892
1553.780156	66.150095	65.304897
1552.602487	76.011399	65.309902
1551.523533	68.580816	65.314906
1550.991160	70.037365	65.319911
1550.347919	69.340178	65.324916
1550.332365	57.705429	65.329921
1549.455421	77.667694	65.334926
1548.446871	74.748393	65.339930
1547.802863	70.884970	65.344935
1547.191877	67.908811	65.349940
1547.187944	72.197034	65.354945
1545.842434	75.041125	65.359950
1545.483719	64.881656	65.364954
1544.961867	62.850074	65.369959
1544.385924	65.163480	65.374964
1543.421927	71.165347	65.379969
1542.170917	65.618085	65.384974
1541.860946	70.407495	65.389978
1541.440489	71.234438	65.394983
1541.058301	71.200636	65.399988
1540.350724	69.331020	65.404993
1539.034364	85.230137	65.409998
1538.631984	76.064723	65.415002
1538.669678	71.298244	65.420007
1537.511163	75.924452	65.425012
1536.822313	71.163033	65.430017
1535.729833	81.928551	65.435022
1535.690610	68.906755	65.440026
1535.193543	66.629975	65.445031
1533.689294	84.167354	65.450036
1533.404005	67.731306	65.455041
1533.030909	68.236928	65.460046
1532.560478	75.905973	65.465050
1531.871630	79.249675	65.470055
1530.743585	68.837153	65.475060
1530.612456	69.036260	65.480065
1529.047906	62.537512	65.485070
1528.004875	64.281776	65.490074
1528.006038	62.089827	65.495079
1527.551061	65.615551	65.500084
1527.477602	74.049376	65.505089
1526.499382	73.220927	65.510094
1525.414656	72.980229	65.515098
1524.907484	67.444087	65.520103
1524.152405	67.518421	65.525108
1524.218059	57.633714	65.530113
1522.933770	74.833377	65.535118
1522.345085	76.103348	65.540122
1521.489462	72.715081	65.545127
1520.739047	70.095380	65.550132
1519.885853	71.732216	65.555137
1518.782691	71.568563	65.560142
1518.438773	73.241166	65.565146
1518.044343	67.020095	65.570151
1518.011793	76.798799	65.575156
1517.963580	68.095909	65.580161
1516.669493	76.017252	65.585166
1516.091463	68.011953	65.590170
1515.219928	67.683770	65.595175
1513.499129	75.330737	65.600180
1513.194542	77.023898	65.605185
1512.718980	69.599951	65.610190
1512.576279	68.734933	65.615194
1512.166456	68.481612	65.620199
1510.956560	73.074996	65.625204
1510.215693	72.215145	65.630209
1509.430203	79.379199	65.635214
1509.506926	66.990232	65.640218
1508.970698	67.701542	65.645223
1507.793655	74.702320	65.650228
1507.178251	73.098750	65.655233
1506.187063	81.582218	65.660238
1505.873306	79.814027	65.665242
1504.978425	78.953420	65.670247
1503.956006	80.774840	65.675252
1503.950791	75.212552	65.680257
1503.101125	74.762632	65.685262
1502.312823	73.213345	65.690266
1501.641668	72.321920	65.695271
1500.756049	79.192819	65.700276
1500.404325	64.828313	65.705281
1499.832584	72.846178	65.710286
1499.754414	74.784044	65.715290
1498.497093	68.842012	65.720295
1497.585687	75.089414	65.725300
1497.733052	72.350711	65.730305
1496.447920	76.919790	65.735310
1495.350867	71.504196	65.740314
1495.179159	69.926313	65.745319
1494.618680	81.395740	65.750324
1494.354355	70.563726	65.755329
1492.988955	76.384981	65.760334
1492.077478	75.347254	65.765338
1491.644104	82.316594	65.770343
1490.989088	78.773463	65.775348
1490.905417	65.467019	65.780353
1489.811255	66.910356	65.785358
1489.434594	81.061212	65.790362
1488.725674	72.313513	65.795367
1488.124898	72.260842	65.800372
1487.630826	72.530241	65.805377
1486.759564	75.783097	65.810382
1486.183754	64.603216	65.815386
1485.308139	70.121149	65.820391
1484.233757	70.829677	65.825396
1484.037677	62.136101	65.830401
1483.378101	75.486709	65.835406
1482.962667	66.487384	65.840410
1482.069410	55.320112	65.845415
1481.243840	77.524413	65.850420
1480.636775	67.809680	65.855425
1480.057038	78.755492	65.860430
1479.224985	70.459428	65.865434
1478.523321	68.174174	65.870439
1477.703713	63.378365	65.875444
1477.713329	65.136708	65.880449
1476.456927	61.208209	65.885454
1475.579715	66.754781	65.890458
1475.009600	73.703273	65.895463
1474.353059	71.349351	65.900468
1474.321802	63.667164	65.905473
1473.830864	66.709781	65.910478
1473.091634	74.219707	65.915482
1472.348869	64.129174	65.920487
1471.439334	71.524245	65.925492
1470.429127	64.525880	65.930497
1469.477972	77.907059	65.935502
1468.886499	79.398246	65.940506
1468.855469	68.272135	65.945511
1468.087936	76.505614	65.950516
1467.950169	65.133131	65.955521
1466.806262	76.439820	65.960526
1466.379051	74.189797	65.965530
1465.691449	64.349106	65.970535
1464.955663	63.603574	65.975540
1464.024544	69.644392	65.980545
1463.116143	70.438509	65.985550
1462.883123	60.049366	65.990554
1462.726872	64.279792	65.995559
1461.637438	74.407788	66.000564
1460.771918	66.724147	66.005569
1460.298259	71.583729	66.010574
1459.449916	62.708401	66.015578
1458.733478	71.168712	66.020583
1457.912162	69.139010	66.025588
1457.705783	57.492025	66.030593
1457.114796	60.804419	66.035598
1456.348736	64.422166	66.040602
1455.480181	57.664637	66.045607
1454.677883	64.077623	66.050612
1454.335783	67.579111	66.055617
1453.945188	61.411061	66.060622
1452.681936	70.669443	66.065626
1452.230220	59.696925	66.070631
1451.680962	67.454190	66.075636
1451.101640	59.956873	66.080641
1449.960325	66.305475	66.085646
1449.439167	68.108749	66.090650
1449.091889	66.443660	66.095655
1448.488122	66.219595	66.100660
1447.929418	63.490607	66.105665
1446.835444	78.190675	66.110670
1446.228972	70.910546	66.115674
1445.749137	68.448129	66.120679
1444.764159	66.319869	66.125684
1443.909277	55.707882	66.130689
1443.212336	67.012919	66.135694
1442.527753	66.423250	66.140698
1442.446319	65.288317	66.145703
1441.735533	67.799783	66.150708
1441.459730	67.690744	66.155713
1440.131680	62.376545	66.160718
1439.778908	65.969612	66.165722
1439.509718	62.671094	66.170727
1438.585045	76.574744	66.175732
1438.072013	67.991466	66.180737
1437.322865	75.304291	66.185742
1436.446040	70.709967	66.190746
1435.535972	61.894919	66.195751
1434.767559	81.045212	66.200756
1434.335349	62.943721	66.205761
1433.970249	78.412576	66.210766
1433.270704	70.161699	66.215770
1432.576724	58.448718	66.220775
1431.654289	72.752535	66.225780
1431.261390	70.793517	66.230785
1430.384245	69.223682	66.235790
1429.220563	68.150372	66.240794
1429.179237	57.129984	66.245799
1428.628378	74.274608	66.250804
1428.320081	69.463780	66.255809
1426.966920	80.674439	66.260814
1426.387774	64.382896	66.265818
1425.866839	67.843428	66.270823
1425.326383	81.031619	66.275828
1424.974167	65.227531	66.280833
1423.673871	73.315468	66.285838
1422.992248	69.628363	66.290842
1422.695339	74.258019	66.295847
1421.602408	75.888837	66.300852
1420.834687	68.670613	66.305857
1419.867454	82.107975	66.310862
1419.486435	82.670063	66.315866
1419.450670	68.192285	66.320871
1418.973577	79.708385	66.325876
1418.607295	65.390369	66.330881
1417.356791	66.983156	66.335886
1416.748442	78.252049	66.340890
1416.090292	70.068713	66.345895
1415.008990	73.388088	66.350900
1414.731768	71.787560	66.355905
1413.981499	72.302685	66.360910
1413.172108	72.456644	66.365914
1412.421330	66.932443	66.370919
1411.834967	75.316901	66.375924
1411.362266	78.974764	66.380929
1410.912857	72.778222	66.385934
1410.050508	65.114599	66.390938
1409.106402	80.221343	66.395943
1408.223777	65.457146	66.400948
1408.080996	62.395571	66.405953
1407.354708	68.190972	66.410958
1406.663489	64.278329	66.415962
1406.165305	65.015150	66.420967
1405.296016	70.391758	66.425972
1405.038923	63.753091	66.430977
1404.056132	67.433683	66.435982
1402.905508	77.924644	66.440986
1402.318338	62.780772	66.445991
1401.788571	71.695523	66.450996
1401.764173	77.841392	66.456001
1401.345260	77.589532	66.461006
1399.961679	72.638974	66.466010
1399.360075	70.700519	66.471015
1398.898745	70.841736	66.476020
1398.084986	65.340165	66.481025
1397.157836	72.867361	66.486030
1396.685172	69.101321	66.491034
1396.186341	66.531554	66.496039
1395.557809	80.607331	66.501044
1395.004236	70.429985	66.506049
1394.039545	67.880651	66.511054
1393.306100	74.706891	66.516058
1393.052398	58.623824	66.521063
1392.275973	69.796432	66.526068
1391.436958	67.268122	66.531073
1390.953582	62.396827	66.536078
1390.357688	77.296846	66.541082
1389.992058	66.449423	66.546087
1388.601486	62.961743	66.551092
1388.257368	63.563698	66.556097
1387.618599	62.813805	66.561102
1386.367004	73.305048	66.566106
1385.716302	59.639350	66.571111
1385.230922	68.378321	66.576116
1384.971010	59.247079	66.581121
1384.466951	67.142240	66.586126
1384.013994	65.213277	66.591130
1382.733315	57.182524	66.596135
1382.229793	64.896259	66.601140
1381.957521	68.918060	66.606145
1380.985212	60.064049	66.611150
1380.373789	82.431434	66.616154
1379.852604	66.685753	66.621159
1378.820662	76.266925	66.626164
1378.162255	75.570616	66.631169
1377.432591	65.630993	66.636174
1376.659718	74.653773	66.641178
1376.399571	65.902591	66.646183
1375.799100	77.286924	66.651188
1375.411422	71.378607	66.656193
1374.125134	66.385794	66.661198
1373.807224	73.842962	66.666202
1373.439125	63.084243	66.671207
1371.997121	81.963164	66.676212
1371.424812	70.550962	66.681217
1370.926891	66.738484	66.686222
1370.343200	78.780858	66.691226
1370.032048	61.749767	66.696231
1368.797744	76.667691	66.701236
1368.036956	64.971657	66.706241
1367.692777	79.386992	66.711246
1367.260200	73.328125	66.716250
1366.934628	62.654107	66.721255
1365.389580	67.229866	66.726260
1365.061240	61.996483	66.731265
1364.348073	68.095720	66.736270
1363.457690	63.041560	66.741274
1362.932674	67.461486	66.746279
1362.128239	65.517438	66.751284
1361.890211	63.601621	66.756289
1361.560236	68.919320	66.761294
1360.603542	80.030715	66.766298
1359.795678	60.979772	66.771303
1358.935318	68.769156	66.776308
1358.803122	68.971595	66.781313
1357.711364	62.766797	66.786318
1356.900056	76.863743	66.791322
1356.664270	69.704482	66.796327
1356.037444	68.441794	66.801332
1355.002153	66.003041	66.806337
1354.111128	66.354488	66.811342
1353.664390	62.595377	66.816346
1353.562780	63.587695	66.821351
1352.883292	65.250584	66.826356
1351.951919	69.709877	66.831361
1350.907169	65.528614	66.836366
1350.255644	79.406210	66.841370
1350.089293	66.887176	66.846375
1349.372264	75.853779	66.851380
1348.455087	63.179727	66.856385
1347.710086	66.177599	66.861390
1347.251774	75.025809	66.866394
1346.965163	63.675432	66.871399
1345.813570	71.388122	66.876404
1345.356155	68.966315	66.881409
1344.764689	64.429163	66.886414
1344.387564	68.704164	66.891418
1343.251970	74.529956	66.896423
1342.564459	76.645108	66.901428
1342.079714	76.588217	66.906433
1340.940854	70.029809	66.911438
1340.016587	72.524777	66.916442
1339.626466	64.270480	66.921447
1339.128086	69.389459	66.926452
1339.015771	74.216845	66.931457
1338.595447	71.431194	66.936462
1337.343897	66.402919	66.941466
1336.847503	68.523958	66.946471
1336.027973	64.262747	66.951476
1335.741924	68.835491	66.956481
1334.619578	68.334364	66.961486
1333.666915	64.319810	66.966490
1333.701827	60.592940	66.971495
1332.392974	70.538246	66.976500
1331.841227	62.940392	66.981505
1331.197842	67.719743	66.986510
1330.539343	65.645280	66.991514
1330.217309	61.524170	66.996519
1329.522837	68.084041	67.001524
1328.786332	63.323960	67.006529
1328.211135	73.299288	67.011534
1327.528488	71.258624	67.016538
1326.932831	63.267227	67.021543
1325.685881	66.926765	67.026548
1324.908002	68.471269	67.031553
1325.058401	52.803354	67.036558
1324.103672	74.955659	67.041562
1323.955841	64.182435	67.046567
1322.740343	72.302662	67.051572
1322.416836	74.159690	67.056577
1321.869297	67.685474	67.061582
1320.781051	61.562134	67.066586
1319.990615	71.015045	67.071591
1319.150835	80.229816	67.076596
1318.974037	73.680891	67.081601
1318.023739	74.924819	67.086606
1316.919721	67.947746	67.091610
1316.550490	68.435437	67.096615
1315.950713	64.279640	67.101620
1315.613700	64.927781	67.106625
1315.281941	68.154840	67.111630
1314.515376	65.663923	67.116634
1313.781345	70.913404	67.121639
1312.983065	69.375226	67.126644
1312.489950	64.801948	67.131649
1311.297979	68.419638	67.136654
1310.615178	72.317485	67.141658
1310.224768	65.249044	67.146663
1309.891235	63.745787	67.151668
1309.107839	68.824930	67.156673
1308.463819	58.609964	67.161678
1307.524464	69.415850	67.166682
1307.147066	66.200782	67.171687
1306.012784	77.318345	67.176692
1305.312556	70.469460	67.181697
1304.991947	66.756534	67.186702
1304.325766	75.271962	67.191706
1303.972263	61.278364	67.196711
1303.006908	71.236878	67.201716
1301.736853	64.363477	67.206721
1301.754804	65.250061	67.211726
1301.239257	61.874041	67.216730
1300.302649	58.675344	67.221735
1299.626653	70.319254	67.226740
1298.788552	64.780594	67.231745
1298.864682	66.769619	67.236750
1297.246830	75.578265	67.241754
1296.769845	71.442370	67.246759
1295.970572	74.658609	67.251764
1295.707242	67.246710	67.256769
1295.266791	68.504200	67.261774
1294.811226	72.211391	67.266778
1293.989986	65.962038	67.271783
1293.013425	72.550997	67.276788
1292.580006	65.647085	67.281793
1291.995892	63.329008	67.286798
1290.887138	57.645736	67.291802
1290.387623	67.847139	67.296807
1289.859136	75.465516	67.301812
1289.324191	66.221906	67.306817
1288.295937	70.613049	67.311822
1287.742959	74.446110	67.316826
1287.253362	67.778198	67.321831
1286.780333	72.574628	67.326836
1285.788189	75.581850	67.331841
1284.959289	69.865121	67.336846
1284.272691	75.373560	67.341850
1284.129045	65.763404	67.346855
1283.099196	72.630483	67.351860
1282.101591	72.175775	67.356865
1281.890097	63.114121	67.361870
1281.212046	71.808046	67.366874
1280.869785	65.044177	67.371879
1279.849941	81.577439	67.376884
1279.120627	73.140549	67.381889
1278.735073	70.005625	67.386894
1278.017105	74.754272	67.391898
1276.841911	67.656078	67.396903
1276.193628	74.046202	67.401908
1275.761889	68.395635	67.406913
1275.559342	64.383262	67.411918
1274.977158	75.362596	67.416922
1273.928553	72.948069	67.421927
1273.212446	83.589176	67.426932
1272.571860	70.286162	67.431937
1272.234307	63.857420	67.436942
1271.034613	73.506292	67.441946
1270.638529	64.672672	67.446951
1270.215252	72.253823	67.451956
1269.146476	63.896145	67.456961
1268.314512	63.593293	67.461966
1267.439857	67.871716	67.466970
1267.427191	58.751648	67.471975
1266.838953	72.138239	67.476980
1266.448005	64.216810	67.481985
1265.294638	75.009431	67.486990
1264.335159	72.752617	67.491994
1264.160002	66.924071	67.496999
1263.473845	74.400372	67.502004
1262.833543	65.693888	67.507009
1261.880215	73.972717	67.512014
1261.317049	64.897598	67.517018
1261.124516	57.518606	67.522023
1259.971813	62.416795	67.527028
1258.854928	72.542909	67.532033
1258.603098	69.503415	67.537038
1257.887107	70.795261	67.542042
1257.753191	66.934394	67.547047
1256.782559	72.981558	67.552052
1256.301016	69.768865	67.557057
1255.698309	56.199665	67.562062
1254.961502	76.660046	67.567066
1254.020207	61.213016	67.572071
1253.363881	70.655655	67.577076
1252.936168	73.885364	67.582081
1252.562688	61.244756	67.587086
1251.087423	79.126117	67.592090
1250.831588	67.305692	67.597095
1250.167910	75.519548	67.602100
1249.325860	69.606239	67.607105
1248.816094	65.204349	67.612110
1247.699165	73.676343	67.617114
1247.515931	71.444337	67.622119
1246.950741	74.820478	67.627124
1246.457193	73.120333	67.632129
1245.845248	68.037715	67.637134
1244.526842	74.506013	67.642138
1244.001408	66.610702	67.647143
1243.514297	71.902935	67.652148
1242.924399	74.945556	67.657153
1242.291107	72.491815	67.662158
1241.355946	81.340168	67.667162
1241.306797	74.838762	67.672167
1240.395681	72.046018	67.677172
1239.247196	54.706593	67.682177
1239.041490	66.094390	67.687182
1238.251227	75.370685	67.692186
1237.772621	65.947831	67.697191
1236.337900	61.049658	67.702196
1235.985556	66.016127	67.707201
1235.855311	67.777781	67.712206
1234.881889	67.133177	67.717210
1234.705048	61.435784	67.722215
1233.794837	62.294919	67.727220
1233.003353	66.651586	67.732225
1232.766234	64.316193	67.737230
1231.372726	72.633485	67.742234
1230.819321	56.394706	67.747239
1230.177896	79.358179	67.752244
1229.807148	68.867982	67.757249
1229.520241	62.681917	67.762254
1228.178967	65.006700	67.767258
1227.645591	54.370496	67.772263
1227.096320	61.008215	67.777268
1226.401693	66.727662	67.782273
1225.667978	62.293583	67.787278
1224.610593	63.220277	67.792282
1224.453378	60.638804	67.797287
1223.946279	69.682424	67.802292
1223.226999	66.318319	67.807297
1222.594016	63.534970	67.812302
1221.591511	60.636925	67.817306
1221.627538	63.234685	67.822311
1220.260659	67.922534	67.827316
1219.194491	74.787526	67.832321
1218.836770	64.426144	67.837326
1218.559522	72.755165	67.842330
1218.332542	67.485191	67.847335
1217.170568	65.910265	67.852340
1216.084901	73.860088	67.857345
1215.809358	80.231952	67.862350
1215.117149	66.888290	67.867354
1214.877051	72.210630	67.872359
1213.818975	66.257575	67.877364
1213.005049	70.102182	67.882369
1212.932321	65.276010	67.887374
1211.666955	78.574754	67.892378
1210.892494	67.861771	67.897383
1210.487204	69.525245	67.902388
1210.320092	71.434681	67.907393
1209.394991	70.941666	67.912398
1208.729712	68.253337	67.917402
1207.878021	79.811672	67.922407
1207.487837	65.413946	67.927412
1205.858638	71.974257	67.932417
1205.674891	67.507919	67.937422
1204.808338	74.978226	67.942426
1204.560724	69.418238	67.947431
1204.245205	70.739450	67.952436
1203.487566	70.525719	67.957441
1202.797334	53.042490	67.962446
1201.781778	67.660759	67.967450
1201.622166	66.894640	67.972455
1200.682861	67.570767	67.977460
1199.820192	71.681735	67.982465
1199.515198	65.742964	67.987470
1198.473434	73.655850	67.992474
1197.488880	74.794888	67.997479
1196.709279	65.177075	68.002484
1196.489554	63.215791	68.007489
1196.219454	68.213337	68.012494
1195.606493	78.636211	68.017498
1194.988199	66.176464	68.022503
1194.318179	69.540901	68.027508
1193.552103	59.277581	68.032513
1193.010238	69.761680	68.037518
1191.807942	80.677221	68.042522
1191.147070	68.344086	68.047527
1190.643611	72.675462	68.052532
1190.263039	73.519770	68.057537
1189.513005	67.473587	68.062542
1188.436027	80.546852	68.067546
1187.948840	71.387134	68.072551
1187.430482	72.299082	68.077556
1186.814072	73.762758	68.082561
1185.914250	77.319852	68.087566
1185.307032	81.587312	68.092570
1184.987243	72.106100	68.097575
1184.485331	77.224087	68.102580
1183.266295	69.024379	68.107585
1182.627512	67.877172	68.112590
1181.797358	78.629462	68.117594
1181.418164	69.370576	68.122599
1181.113573	72.793591	68.127604
1179.676395	74.372025	68.132609
1179.318474	68.809083	68.137614
1178.866761	66.638703	68.142618
1178.388170	61.845542	68.147623
1177.642589	67.111081	68.152628
1176.348428	67.555083	68.157633
1176.147013	65.149367	68.162638
1175.549542	70.813954	68.167642
1174.834815	70.224421	68.172647
1173.936175	71.491723	68.177652
1173.204849	76.248826	68.182657
1172.900960	64.391910	68.187662
1172.373787	65.123924	68.192666
1171.799276	66.987770	68.197671
1171.051106	70.656360	68.202676
1169.988125	71.408934	68.207681
1169.841573	75.060692	68.212686
1168.725671	74.273201	68.217690
1167.962932	69.080553	68.222695
1167.534859	66.444394	68.227700
1166.978501	73.652503	68.232705
1166.666792	70.570507	68.237710
1165.878257	71.042907	68.242714
1164.967309	73.087986	68.247719
1164.492931	75.609231	68.252724
1163.742825	81.031608	68.257729
1163.010321	67.841024	68.262734
1162.115486	68.412327	68.267738
1161.623012	78.551131	68.272743
1161.469188	68.467976	68.277748
1160.082703	75.902719	68.282753
1159.569107	72.234700	68.287758
1158.939017	81.611690	68.292762
1158.642542	64.764398	68.297767
1158.077049	79.057237	68.302772
1156.622904	70.795591	68.307777
1156.362821	66.306709	68.312782
1155.780946	70.142810	68.317786
1154.798799	71.812884	68.322791
1154.109040	65.134268	68.327796
1153.440209	78.142629	68.332801
1153.242874	73.320508	68.337806
1152.769972	77.998671	68.342810
1151.459574	76.158814	68.347815
1150.832238	77.703080	68.352820
1150.540975	85.181254	68.357825
1150.133559	74.857747	68.362830
1148.433196	75.729044	68.367834
1148.224473	76.408840	68.372839
1147.464413	71.663602	68.377844
1147.235901	81.897615	68.382849
1146.867243	72.920896	68.387854
1145.861199	82.416026	68.392858
1145.166015	74.118830	68.397863
1144.748298	74.473916	68.402868
1144.191335	74.690309	68.407873
1143.212508	73.313357	68.412878
1142.132872	82.291942	68.417882
1141.760451	81.513943	68.422887
1141.497174	77.572740	68.427892
1140.615089	73.277395	68.432897
1139.940738	65.030506	68.437902
1138.980717	75.447086	68.442906
1138.785844	66.308700	68.447911
1137.859412	71.038496	68.452916
1136.883029	74.074802	68.457921
1136.864099	66.423800	68.462926
1136.041922	79.743542	68.467930
1134.986301	75.327574	68.472935
1134.193307	69.830685	68.477940
1133.594622	68.323895	68.482945
1133.749801	66.168957	68.487950
1132.755544	79.616988	68.492954
1131.661211	76.320444	68.497959
1131.144508	73.190637	68.502964
1130.279521	77.138002	68.507969
1130.321356	65.946737	68.512974
1129.192230	74.538976	68.517978
1128.545322	69.368918	68.522983
1127.797603	75.806422	68.527988
1127.389585	70.212037	68.532993
1127.232795	72.730081	68.537998
1125.781458	84.235584	68.543002
1125.179628	83.836255	68.548007
1124.924936	66.936595	68.553012
1123.858452	66.109728	68.558017
1122.886586	71.739260	68.563022
1122.292201	69.982644	68.568026
1121.896561	69.181536	68.573031
1121.595970	67.362424	68.578036
1121.085129	75.216121	68.583041
1120.369762	71.074031	68.588046
1119.260643	75.474943	68.593050
1118.540419	84.278107	68.598055
1118.384719	78.350292	68.603060
1117.325472	85.206338	68.608065
1116.789526	79.744256	68.613070
1115.945234	86.518808	68.618074
1115.709207	69.220386	68.623079
1114.776230	73.579091	68.628084
1114.049205	81.580712	68.633089
1113.513767	71.036319	68.638094
1112.937537	77.116986	68.643098
1111.855262	79.312330	68.648103
1111.674025	71.236160	68.653108
1110.890417	73.387153	68.658113
1110.223630	69.995811	68.663118
1109.088371	74.514419	68.668122
1108.561219	79.297406	68.673127
1108.478612	77.766881	68.678132
1107.710443	85.644170	68.683137
1106.924468	75.940672	68.688142
1105.459651	74.771916	68.693146
1105.517421	72.848500	68.698151
1105.240671	75.811379	68.703156
1103.932459	68.253493	68.708161
1103.209393	75.912304	68.713166
1102.661996	75.507476	68.718170
1102.237236	71.875801	68.723175
1101.957352	67.218198	68.728180
1100.913687	73.556131	68.733185
1099.831721	65.523894	68.738190
1099.366826	68.251786	68.743194
1099.117350	66.426125	68.748199
1098.945741	68.544426	68.753204
1097.540027	76.362281	68.758209
1096.905794	68.306133	68.763214
1096.381898	73.798191	68.768218
1095.720980	77.094976	68.773223
1094.636108	68.577528	68.778228
1094.230315	67.809576	68.783233
1093.706388	62.222600	68.788238
1092.998254	68.382591	68.793242
1091.525350	71.646115	68.798247
1091.113372	71.599774	68.803252
1090.889495	73.092492	68.808257
1090.488504	61.351965	68.813262
1089.876538	70.357089	68.818266
1089.376705	72.849281	68.823271
1088.537645	73.807531	68.828276
1087.590717	68.641056	68.833281
1087.249657	70.698008	68.838286
1086.015626	72.919077	68.843290
1085.410657	74.447184	68.848295
1085.048931	69.455692	68.853300
1084.588320	67.625771	68.858305
1083.952102	65.763863	68.863310
1082.801316	68.145146	68.868314
1082.489099	70.457694	68.873319
1082.180793	61.274290	68.878324
1080.683137	68.800862	68.883329
1080.166074	60.320832	68.888334
1079.460420	75.203638	68.893338
1079.066733	69.157578	68.898343
1078.790830	65.347698	68.903348
1078.128112	73.356438	68.908353
1077.476835	65.891179	68.913358
1076.469007	65.860778	68.918362
1075.844812	55.740512	68.923367
1075.010606	69.271891	68.928372
1074.125872	65.929422	68.933377
1073.784539	61.026148	68.938382
1073.633515	60.468395	68.943386
1072.629024	65.325737	68.948391
1072.030661	63.121940	68.953396
1071.292952	79.608788	68.958401
1070.697810	64.488392	68.963406
1069.569125	75.010662	68.968410
1069.014674	66.933949	68.973415
1068.339105	66.639399	68.978420
1067.754111	76.384519	68.983425
1066.774820	69.733065	68.988430
1065.972286	70.627167	68.993434
1065.351130	75.776754	68.998439
1065.103387	72.038085	69.003444
1064.979933	73.655171	69.008449
1064.411850	59.654781	69.013454
1063.199683	62.473166	69.018458
1062.891410	70.013962	69.023463
1062.344681	62.653498	69.028468
1061.087168	69.858044	69.033473
1060.208658	69.595779	69.038478
1059.732341	71.270574	69.043482
1059.662532	73.287533	69.048487
1059.150915	68.433424	69.053492
1057.740226	81.930374	69.058497
1057.224958	67.768622	69.063502
1056.644258	69.221916	69.068506
1055.285716	66.855214	69.073511
1055.060692	65.225929	69.078516
1054.129544	72.388023	69.083521
1053.833449	70.788966	69.088526
1053.584519	78.161064	69.093530
1053.108418	73.974625	69.098535
1052.519494	69.355153	69.103540
1051.304390	79.257281	69.108545
1050.904041	64.249400	69.113550
1049.556676	71.638547	69.118554
1048.847592	76.488330	69.123559
1048.319555	70.589798	69.128564
1047.813845	71.698446	69.133569
1047.822727	71.427475	69.138574
1047.507606	68.360233	69.143578
1046.186232	63.641253	69.148583
1045.647904	60.358800	69.153588
1044.630118	70.204305	69.158593
1043.797827	66.271642	69.163598
1042.975315	66.088779	69.168602
1042.677348	72.312835	69.173607
1042.676567	65.647648	69.178612
1041.893160	68.710054	69.183617
1040.732988	64.195654	69.188622
1040.077142	66.400454	69.193626
1039.520240	65.930924	69.198631
1038.790088	62.568608	69.203636
1037.996501	73.665170	69.208641
1037.496192	64.793000	69.213646
1037.015032	69.595486	69.218650
1036.108235	74.071470	69.223655
1035.508989	67.261806	69.228660
1034.345804	73.580932	69.233665
1034.211394	68.332526	69.238670
1033.927117	70.544444	69.243674
1032.968162	71.804044	69.248679
1031.972609	73.468412	69.253684
1031.562838	77.772293	69.258689
1031.095921	65.974462	69.263694
1030.018968	74.077494	69.268698
1029.370272	65.526960	69.273703
1028.922137	63.635145	69.278708
1028.343334	82.810500	69.283713
1027.872505	63.348164	69.288718
1026.809620	72.442380	69.293722
1026.243598	75.359828	69.298727
1026.078300	60.013384	69.303732
1025.060602	79.841998	69.308737
1024.160837	69.454938	69.313742
1023.550795	66.710570	69.318746
1022.968518	72.626641	69.323751
1021.907915	70.278786	69.328756
1021.118178	66.411898	69.333761
1020.562011	64.947256	69.338766
1020.526006	72.064716	69.343770
1020.131607	67.357539	69.348775
1019.369433	59.474733	69.353780
1018.208315	68.436352	69.358785
1017.584727	63.991131	69.363790
1017.161298	72.352873	69.368794
1016.000391	69.271969	69.373799
1015.411483	62.396018	69.378804
1014.795697	75.219345	69.383809
1014.684875	58.383566	69.388814
1014.014779	68.142226	69.393818
1012.864672	69.768115	69.398823
1012.241943	64.056538	69.403828
1011.442942	68.744024	69.408833
1011.399290	71.988351	69.413838
1010.458246	66.142924	69.418842
1009.178623	59.323253	69.423847
1008.870808	78.721979	69.428852
1008.130480	60.102000	69.433857
1007.900801	70.591640	69.438862
1007.884969	56.426148	69.443866
1006.718850	67.547288	69.448871
1006.299347	60.116141	69.453876
1004.901556	64.788512	69.458881
1004.050431	57.597915	69.463886
1003.620204	73.231645	69.468890
1003.186017	75.074778	69.473895
1003.071951	68.736681	69.478900
1001.520543	69.336810	69.483905
1000.901020	64.413157	69.488910
1000.554685	53.763039	69.493914
999.983290	65.603220	69.498919
999.184751	61.040769	69.503924
997.996872	74.319371	69.508929
997.650468	66.876592	69.513934
997.337615	55.603017	69.518938
996.723030	65.491610	69.523943
996.082911	60.266903	69.528948
995.154629	70.495551	69.533953
994.839588	58.835991	69.538958
994.071560	59.420291	69.543962
993.038930	69.454242	69.548967
992.441881	62.078151	69.553972
991.889881	76.122861	69.558977
991.514194	59.887435	69.563982
990.351704	60.772602	69.568986
989.473955	62.520738	69.573991
989.466921	64.097226	69.578996
988.597846	65.698911	69.584001
988.268350	61.121758	69.589006
987.143996	66.726710	69.594010
986.348833	62.728242	69.599015
986.208586	67.016050	69.604020
985.014612	71.766385	69.609025
984.494240	70.709193	69.614030
984.011205	74.305687	69.619034
983.440689	70.694074	69.624039
982.979411	72.249801	69.629044
982.070272	66.594841	69.634049
981.586799	66.537816	69.639054
981.093212	70.060299	69.644058
979.712438	70.981779	69.649063
979.067931	69.436590	69.654068
978.384235	68.526804	69.659073
978.022551	58.341151	69.664078
977.693423	64.994340	69.669082
976.643442	66.875534	69.674087
975.875219	58.635759	69.679092
975.195900	72.142515	69.684097
974.915768	69.497047	69.689102
974.181392	60.075549	69.694106
973.040597	67.887574	69.699111
972.643375	67.048897	69.704116
971.878180	66.621985	69.709121
971.748066	63.616777	69.714126
971.044377	62.139352	69.719130
970.039469	69.387317	69.724135
969.942799	65.796503	69.729140
968.462847	72.471966	69.734145
967.548712	59.076999	69.739150
966.895676	70.540693	69.744154
966.040938	76.605777	69.749159
966.310469	62.286078	69.754164
965.771879	80.283425	69.759169
965.496352	67.598925	69.764174
964.452465	70.901483	69.769178
963.533136	66.035005	69.774183
963.429936	62.451539	69.779188
961.875583	73.762199	69.784193
961.191313	74.471945	69.789198
961.093491	68.927584	69.794202
960.192443	67.311262	69.799207
959.546686	62.234111	69.804212
958.750189	71.013165	69.809217
958.270130	58.490522	69.814222
958.017962	60.517574	69.819226
956.806052	69.941434	69.824231
955.931971	54.712523	69.829236
955.482549	65.030553	69.834241
955.155344	58.341626	69.839246
954.442873	61.026936	69.844250
952.994899	74.529855	69.849255
952.784933	59.616289	69.854260
952.011730	70.873615	69.859265
951.836854	69.567502	69.864270
951.374333	64.513233	69.869274
950.178525	70.648358	69.874279
950.010153	59.490565	69.879284
948.996432	67.962005	69.884289
948.140779	67.546341	69.889294
947.576675	60.013645	69.894298
947.051656	76.723688	69.899303
946.573628	54.387924	69.904308
945.323376	68.274092	69.909313
944.760667	53.698922	69.914318
944.657418	57.632354	69.919322
943.854370	61.631412	69.924327
943.111242	68.197525	69.929332
942.160965	69.022140	69.934337
941.818159	55.110527	69.939342
941.374177	64.055824	69.944346
940.173969	73.900430	69.949351
939.748337	58.761004	69.954356
938.659546	71.670639	69.959361
938.563581	73.228165	69.964366
938.061476	71.963084	69.969370
936.697519	78.976479	69.974375
936.311509	60.691217	69.979380
935.731624	70.962208	69.984385
935.468959	61.139253	69.989390
934.389444	71.172799	69.994394
933.143768	64.076548	69.999399
932.652331	69.550849	70.004404
932.304461	59.020829	70.009409
931.941778	70.318484	70.014414
931.345279	60.665340	70.019418
930.561694	68.054707	70.024423
930.271751	59.398242	70.029428
929.379073	65.808393	70.034433
928.258612	73.049531	70.039438
927.502158	65.320379	70.044442
926.713698	71.475844	70.049447
926.559659	69.554596	70.054452
926.275963	66.898664	70.059457
925.496467	66.281665	70.064462
924.508648	65.453403	70.069466
923.939688	74.081148	70.074471
923.616444	57.179852	70.079476
922.274899	68.158636	70.084481
921.754348	69.591349	70.089486
921.256647	61.748490	70.094490
920.233968	72.988756	70.099495
919.780396	57.629870	70.104500
918.853953	60.910600	70.109505
918.134643	68.064251	70.114510
918.100980	59.926791	70.119514
917.338968	65.031012	70.124519
917.144719	55.441591	70.129524
915.875328	70.302162	70.134529
915.432174	63.904489	70.139534
915.078159	64.608999	70.144538
913.523713	62.059100	70.149543
913.224941	61.890700	70.154548
912.635721	61.730676	70.159553
912.278318	60.161894	70.164558
911.524362	64.853274	70.169562
910.300653	70.529259	70.174567
909.977401	63.581105	70.179572
909.284818	74.808266	70.184577
908.720823	64.266913	70.189582
907.776656	66.703695	70.194586
907.175084	69.224723	70.199591
907.018910	54.502875	70.204596
906.397434	62.464077	70.209601
905.483977	56.097100	70.214606
904.549103	59.938961	70.219610
904.090187	63.883266	70.224615
903.593307	51.804844	70.229620
902.265358	68.439240	70.234625
901.892626	67.270268	70.239630
901.302978	62.889062	70.244634
900.809912	67.914220	70.249639
900.394850	62.907602	70.254644
899.556688	61.793776	70.259649
898.831655	61.702673	70.264654
898.237608	66.478990	70.269658
897.157626	67.158692	70.274663
896.449659	72.131325	70.279668
895.832000	66.966147	70.284673
895.409582	73.746148	70.289678
895.312152	63.356042	70.294682
894.435593	71.028281	70.299687
893.591713	61.947497	70.304692
892.703564	69.274671	70.309697
892.079655	63.101300	70.314702
891.556095	73.593555	70.319706
890.293792	73.748798	70.324711
889.887030	53.125227	70.329716
889.591791	77.962100	70.334721
889.191620	77.018256	70.339726
888.811738	69.435757	70.344730
887.367811	76.006187	70.349735
886.939646	62.488191	70.354740
886.377567	75.140567	70.359745
885.409199	71.224887	70.364750
884.801797	69.134533	70.369754
884.175692	74.374822	70.374759
884.013042	70.125926	70.379764
882.686701	71.016719	70.384769
882.035382	68.748862	70.389774
881.758264	66.154964	70.394778
881.047474	69.964327	70.399783
880.392676	68.036049	70.404788
879.198721	72.926767	70.409793
878.935546	76.404714	70.414798
878.762054	63.874301	70.419802
877.669589	65.166242	70.424807
876.876465	66.467312	70.429812
876.077931	67.939543	70.434817
875.807956	60.101454	70.439822
875.170334	64.318617	70.444826
873.823682	64.602402	70.449831
873.420765	61.093450	70.454836
873.267421	63.771793	70.459841
872.602471	69.868192	70.464846
872.071085	68.850622	70.469850
870.621686	68.534210	70.474855
870.784360	64.462185	70.479860
869.957393	76.320986	70.484865
868.706824	61.473710	70.489870
868.352659	64.442619	70.494874
867.725753	64.216068	70.499879
867.222482	68.205282	70.504884
866.093042	61.402790	70.509889
865.200382	64.716007	70.514894
864.703252	62.504036	70.519898
864.310866	57.906955	70.524903
864.149554	64.024117	70.529908
863.561924	58.688603	70.534913
862.315705	61.435231	70.539918
862.136350	67.090092	70.544922
861.343528	68.071016	70.549927
860.759595	55.916578	70.554932
859.814699	71.085048	70.559937
859.357127	70.749551	70.564942
857.982596	64.085411	70.569946
857.138644	70.289146	70.574951
856.800853	64.557498	70.579956
856.552112	66.618704	70.584961
856.061148	66.851462	70.589966
855.772431	55.347013	70.594970
854.347006	62.835394	70.599975
853.827688	65.882626	70.604980
853.137959	61.479519	70.609985
852.714987	60.648114	70.614990
852.007153	63.914573	70.619994
851.206509	70.658586	70.624999
850.982085	54.425945	70.630004
850.017473	68.679821	70.635009
848.922647	71.427591	70.640014
848.820043	55.957682	70.645018
848.089747	62.400354	70.650023
847.450359	57.134580	70.655028
846.500232	61.833545	70.660033
845.702502	59.270477	70.665038
845.786135	68.038775	70.670042
844.387448	65.443630	70.675047
843.615438	53.580894	70.680052
843.216338	66.046486	70.685057
842.323044	55.103439	70.690062
842.140040	58.913956	70.695066
841.288275	72.779315	70.700071
840.728917	58.733471	70.705076
839.887186	70.999875	70.710081
839.579860	56.857153	70.715086
838.875180	57.920242	70.720090
837.568464	68.045168	70.725095
837.207785	56.914854	70.730100
836.918915	66.707475	70.735105
836.466990	60.404253	70.740110
835.379696	55.613450	70.745114
834.342233	63.047976	70.750119
834.093190	59.451466	70.755124
833.618013	59.978164	70.760129
832.579857	69.719747	70.765134
832.178944	68.919525	70.770138
831.411888	70.659557	70.775143
830.697669	68.944165	70.780148
829.720228	64.555321	70.785153
828.810351	73.932735	70.790158
828.484499	58.250795	70.795162
828.200422	73.162714	70.800167
828.036232	62.084697	70.805172
826.963914	68.059875	70.810177
826.082446	73.952641	70.815182
825.949400	66.340331	70.820186
824.734531	64.729860	70.825191
824.287995	63.913249	70.830196
823.639778	62.313504	70.835201
822.814416	68.466982	70.840206
821.857142	59.550927	70.845210
820.553581	66.376571	70.850215
820.617750	52.728205	70.855220
820.180702	58.556536	70.860225
819.460002	67.985834	70.865230
819.438972	51.250927	70.870234
818.643730	66.159050	70.875239
817.770952	56.496311	70.880244
816.642485	69.845931	70.885249
816.008424	56.736028	70.890254
815.198257	58.465579	70.895258
814.378366	55.172812	70.900263
814.232538	60.768722	70.905268
813.749699	56.952402	70.910273
813.274183	77.864778	70.915278
812.609841	64.955220	70.920282
811.613032	71.582243	70.925287
811.379012	58.875414	70.930292
810.113020	64.515593	70.935297
809.183550	64.252067	70.940302
808.867589	63.302717	70.945306
808.235761	59.216818	70.950311
808.026582	63.230187	70.955316
807.001273	53.801456	70.960321
806.152264	69.998551	70.965326
805.523317	57.860759	70.970330
805.020226	58.838156	70.975335
803.817278	66.623867	70.980340
803.402409	57.455914	70.985345
802.700259	63.616589	70.990350
802.917184	64.301192	70.995354
801.916694	64.261849	71.000359
801.065137	62.136270	71.005364
800.747345	59.048995	71.010369
800.030005	61.072839	71.015374
799.106140	63.537964	71.020378
798.132263	56.565677	71.025383
797.759969	61.962684	71.030388
797.007487	54.267647	71.035393
796.154341	58.299948	71.040398
795.681012	57.463955	71.045402
794.493811	71.157226	71.050407
794.484592	60.002512	71.055412
793.955003	62.903164	71.060417
793.122793	59.945082	71.065422
792.398675	62.419411	71.070426
791.601368	69.579197	71.075431
791.319084	63.362516	71.080436
790.344080	63.125167	71.085441
789.098602	68.856703	71.090446
789.177680	57.300030	71.095450
788.425132	78.182392	71.100455
788.444270	62.347778	71.105460
787.312417	68.846503	71.110465
786.550776	61.531370	71.115470
786.085562	60.801313	71.120474
785.003011	65.492995	71.125479
784.094933	63.951972	71.130484
783.547421	70.606824	71.135489
783.089902	63.172322	71.140494
783.076426	55.999855	71.145498
781.638316	72.131470	71.150503
781.216751	53.454564	71.155508
780.310729	66.127001	71.160513
779.634478	59.160956	71.165518
779.642283	55.556682	71.170522
778.722633	53.080852	71.175527
777.764590	61.860427	71.180532
777.525192	63.568512	71.185537
776.541582	62.936748	71.190542
775.956937	57.980807	71.195546
775.118855	66.556796	71.200551
774.315375	65.935779	71.205556
774.379311	66.195329	71.210561
773.288327	76.397901	71.215566
772.907246	51.990562	71.220570
772.100032	65.691149	71.225575
771.021400	59.673779	71.230580
770.459157	68.970635	71.235585
769.547744	62.753191	71.240590
769.177809	53.581250	71.245594
768.535354	57.234688	71.250599
768.186722	62.713081	71.255604
767.303189	64.903731	71.260609
766.699329	63.191291	71.265614
766.364192	54.403294	71.270618
765.329655	65.612372	71.275623
764.362654	54.767823	71.280628
763.756381	66.608849	71.285633
763.093336	65.691106	71.290638
763.025924	52.574595	71.295642
762.339637	67.120052	71.300647
761.403567	53.894258	71.305652
760.675620	59.958129	71.310657
759.901764	57.798120	71.315662
759.811311	56.134830	71.320666
758.598742	61.818563	71.325671
758.082867	56.501618	71.330676
757.581240	59.232254	71.335681
756.874392	58.053421	71.340686
756.326956	52.411940	71.345690
755.329960	63.652886	71.350695
755.077570	59.177035	71.355700
754.391924	64.169796	71.360705
753.112355	60.321064	71.365710
752.546812	62.382252	71.370714
752.188461	55.485452	71.375719
751.815782	62.889862	71.380724
750.511039	61.416730	71.385729
750.015589	65.942426	71.390734
749.814703	56.291018	71.395738
749.035993	64.048633	71.400743
747.741713	65.282877	71.405748
747.657691	56.357141	71.410753
746.722534	69.064186	71.415758
746.556783	60.509406	71.420762
745.455487	58.278535	71.425767
744.722997	60.243308	71.430772
744.523333	67.271692	71.435777
743.555293	60.697444	71.440782
742.858431	60.549866	71.445786
741.660792	56.189811	71.450791
741.160690	61.640284	71.455796
741.056794	56.907420	71.460801
740.498727	52.655268	71.465806
739.662580	58.632296	71.470810
738.857928	60.107119	71.475815
738.483099	63.416778	71.480820
737.971428	58.020326	71.485825
736.782976	60.792506	71.490830
736.083062	60.383658	71.495834
735.489221	64.690068	71.500839
735.399720	56.671898	71.505844
734.374482	57.852278	71.510849
733.394032	64.019430	71.515854
733.105778	60.862812	71.520858
732.708912	59.317688	71.525863
731.739312	50.299572	71.530868
730.916752	59.226312	71.535873
729.880184	61.576947	71.540878
729.963934	61.412321	71.545882
728.936687	58.292937	71.550887
727.728118	54.631600	71.555892
727.586831	58.424440	71.560897
726.718998	58.215783	71.565902
726.668541	55.240491	71.570906
726.241082	58.105973	71.575911
725.195851	50.181624	71.580916
724.539237	58.323477	71.585921
723.831219	59.180561	71.590926
722.464133	55.058793	71.595930
721.806685	59.547208	71.600935
721.564349	62.152996	71.605940
721.009847	53.858801	71.610945
720.596306	65.289124	71.615950
720.275397	58.572436	71.620954
718.845666	59.312627	71.625959
718.536184	53.805148	71.630964
718.179195	46.217480	71.635969
717.291968	64.375966	71.640974
716.500525	48.508017	71.645978
715.601974	62.857049	71.650983
715.183487	60.821814	71.655988
715.055716	56.499583	71.660993
713.742996	68.885149	71.665998
713.209782	64.179640	71.671002
712.417193	68.599695	71.676007
712.061161	60.821069	71.681012
711.647865	54.639456	71.686017
710.849188	69.532378	71.691022
710.077665	53.162969	71.696026
708.604088	57.552681	71.701031
708.169589	60.062917	71.706036
707.948421	49.146959	71.711041
707.203318	58.189097	71.716046
707.012597	49.281936	71.721050
706.005432	60.434632	71.726055
705.149099	65.227514	71.731060
704.751369	57.710980	71.736065
703.469699	61.464629	71.741070
703.275289	56.919634	71.746074
702.470398	61.554524	71.751079
702.091367	67.681122	71.756084
701.272390	59.110513	71.761089
700.449259	66.714374	71.766094
699.951746	62.301211	71.771098
699.171389	58.179072	71.776103
698.747293	59.784115	71.781108
697.989746	63.072719	71.786113
696.947533	62.018258	71.791118
696.785144	63.275723	71.796122
696.311772	61.799553	71.801127
695.531235	51.811545	71.806132
694.597102	59.808369	71.811137
693.782755	59.102382	71.816142
693.756611	52.628911	71.821146
692.721932	62.423591	71.826151
691.637704	59.682280	71.831156
691.438477	51.355181	71.836161
690.610716	62.362631	71.841166
690.153995	61.607587	71.846170
689.184728	63.657381	71.851175
688.462949	58.496233	71.856180
687.875418	59.728356	71.861185
687.441004	62.211775	71.866190
687.135399	57.110512	71.871194
685.723096	62.830808	71.876199
685.142682	58.233743	71.881204
684.694983	54.943259	71.886209
684.196209	61.169341	71.891214
683.757383	59.247730	71.896218
682.664501	58.620787	71.901223
682.142513	51.903013	71.906228
681.664181	50.616860	71.911233
680.892509	56.943159	71.916238
680.001067	46.069284	71.921242
679.051943	55.965452	71.926247
678.578744	61.725444	71.931252
678.744149	56.257467	71.936257
677.489493	63.878006	71.941262
676.823906	55.115840	71.946266
676.333296	58.887037	71.951271
675.557165	69.547250	71.956276
674.860214	57.727824	71.961281
673.727390	62.200485	71.966286
673.356467	57.398189	71.971290
672.825848	56.410504	71.976295
672.466740	62.090833	71.981300
671.728487	57.347027	71.986305
670.786761	65.993157	71.991310
670.629109	57.653130	71.996314
669.633920	56.004604	72.001319
668.779680	60.445523	72.006324
668.315082	53.228213	72.011329
667.409617	61.261478	72.016334
667.069618	65.156921	72.021338
666.220767	58.987904	72.026343
665.675372	68.091291	72.031348
665.615841	57.923834	72.036353
664.118294	63.585180	72.041358
663.255058	58.265226	72.046362
662.942352	57.838895	72.051367
662.523162	62.054433	72.056372
662.002236	63.717476	72.061377
660.770427	66.569130	72.066382
660.355217	58.594949	72.071386
659.677299	63.711072	72.076391
659.179147	67.899765	72.081396
658.249399	57.295326	72.086401
657.187404	52.134752	72.091406
656.653899	60.550310	72.096410
656.212236	63.063271	72.101415
655.898157	59.808282	72.106420
655.791382	68.176393	72.111425
654.603690	63.493120	72.116430
654.177731	65.664558	72.121434
652.746711	54.616428	72.126439
651.942702	63.305283	72.131444
651.497542	58.804954	72.136449
650.961243	64.084597	72.141454
650.769861	64.939853	72.146458
649.929579	61.983107	72.151463
648.978347	58.119994	72.156468
648.766801	50.051892	72.161473
647.786217	66.000318	72.166478
646.919684	54.731425	72.171482
646.343431	57.656879	72.176487
645.577245	64.613058	72.181492
645.256543	47.988983	72.186497
644.748359	55.121680	72.191502
644.206551	58.919957	72.196506
643.174972	62.124486	72.201511
642.617583	61.166300	72.206516
641.679208	52.704614	72.211521
640.513767	65.077791	72.216526
640.241203	58.191005	72.221530
640.260083	58.771520	72.226535
639.567087	59.744499	72.231540
638.483068	52.401921	72.236545
637.271724	62.816071	72.241550
637.007917	59.942563	72.246554
636.798959	57.850324	72.251559
635.959983	51.815360	72.256564
635.271840	51.636464	72.261569
634.305425	63.534852	72.266574
633.663936	53.127360	72.271578
633.531141	54.069475	72.276583
632.992871	51.342171	72.281588
632.101886	50.131201	72.286593
631.448830	59.732671	72.291598
630.743061	54.223664	72.296602
629.490603	57.956927	72.301607
628.760829	69.098591	72.306612
628.778572	50.429055	72.311617
628.011961	66.813313	72.316622
627.729048	64.545206	72.321626
626.585933	60.540781	72.326631
625.827743	65.418976	72.331636
625.673979	59.905636	72.336641
624.238502	64.708772	72.341646
623.378370	60.009621	72.346650
622.714772	65.911899	72.351655
622.624377	60.601343	72.356660
622.463178	49.090841	72.361665
622.187142	63.556786	72.366670
621.061388	54.289217	72.371674
620.567892	60.273208	72.376679
619.583497	63.801372	72.381684
618.995471	55.140409	72.386689
617.968767	58.651657	72.391694
617.405475	61.862041	72.396698
616.084451	52.496270	72.401703
615.380257	63.225454	72.406708
615.165626	51.278788	72.411713
614.666924	59.017068	72.416718
614.567019	58.257252	72.421722
614.010929	56.743813	72.426727
612.736859	61.391948	72.431732
612.439587	53.793212	72.436737
611.395519	57.789745	72.441742
610.680036	56.058856	72.446746
609.826154	55.589414	72.451751
609.585903	65.208722	72.456756
609.590905	54.742434	72.461761
608.103892	60.187679	72.466766
607.525103	62.274660	72.471770
606.882086	61.779521	72.476775
606.014992	57.931410	72.481780
605.372752	51.336882	72.486785
604.395979	48.419239	72.491790
604.114643	42.602970	72.496794
603.572149	56.321340	72.501799
603.009043	58.109375	72.506804
602.288271	52.126558	72.511809
601.570338	54.182085	72.516814
600.954819	60.163435	72.521818
600.254360	56.719270	72.526823
599.188720	65.178586	72.531828
598.660910	52.979043	72.536833
598.003828	63.992445	72.541838
597.679054	58.649837	72.546842
597.481392	59.269568	72.551847
596.164828	58.243076	72.556852
595.815853	50.113297	72.561857
594.901699	64.647754	72.566862
593.701728	62.122028	72.571866
593.256149	53.618150	72.576871
592.769432	59.350345	72.581876
592.379448	50.474938	72.586881
591.767100	59.114358	72.591886
591.767774	53.973796	72.596890
590.565400	45.265620	72.601895
589.434031	60.941618	72.606900
589.365948	53.924513	72.611905
587.933697	56.893273	72.616910
587.390686	50.528936	72.621914
586.851350	63.262854	72.626919
586.566850	56.131992	72.631924
586.081469	53.711646	72.636929
585.094044	56.048203	72.641934
584.129700	61.653054	72.646938
583.499021	52.499035	72.651943
583.274363	58.291990	72.656948
582.389139	50.085203	72.661953
581.255367	53.474753	72.666958
580.921669	50.618693	72.671962
580.494974	46.861294	72.676967
580.134690	59.626613	72.681972
579.221534	48.149154	72.686977
578.198190	59.361229	72.691982
578.056576	55.252514	72.696986
577.082903	57.806067	72.701991
576.134782	63.577061	72.706996
575.909205	49.820344	72.712001
575.242243	59.939667	72.717006
574.230248	60.168736	72.722010
573.711158	55.869422	72.727015
572.810493	64.989980	72.732020
572.159381	52.351220	72.737025
572.119475	53.209161	72.742030
571.463090	54.731379	72.747034
570.581318	52.509779	72.752039
569.372734	60.898835	72.757044
569.262451	59.886800	72.762049
568.741933	54.081821	72.767054
567.816997	67.968342	72.772058
567.024159	67.896020	72.777063
566.400918	57.458837	72.782068
566.170134	57.781090	72.787073
565.135778	63.635204	72.792078
564.292383	63.745966	72.797082
564.266102	63.690317	72.802087
563.565353	60.977869	72.807092
562.636808	64.358395	72.812097
561.528266	59.364541	72.817102
561.247652	68.621296	72.822106
560.913043	59.823800	72.827111
560.007058	67.270591	72.832116
559.469943	64.475314	72.837121
558.581708	73.399947	72.842126
558.083754	61.826397	72.847130
556.867280	68.778629	72.852135
556.024062	58.836928	72.857140
555.520880	66.295252	72.862145
555.153040	62.254108	72.867150
555.027023	56.742666	72.872154
554.239266	63.880486	72.877159
553.150605	68.320935	72.882164
552.948785	56.846870	72.887169
552.219292	71.884907	72.892174
551.614720	57.925219	72.897178
550.662188	65.721603	72.902183
549.957964	62.218132	72.907188
549.688765	65.310729	72.912193
548.490187	66.220767	72.917198
547.488182	63.947366	72.922202
547.283182	65.933824	72.927207
546.635779	68.824904	72.932212
546.453549	54.805835	72.937217
545.428628	63.853156	72.942222
544.531555	65.352220	72.947226
544.019369	66.793134	72.952231
543.856551	62.817101	72.957236
543.100719	66.061321	72.962241
541.929187	66.763640	72.967246
541.630585	66.354000	72.972250
541.168097	61.545815	72.977255
539.453999	63.348472	72.982260
539.327157	62.807402	72.987265
538.646819	66.348662	72.992270
538.327033	73.393028	72.997274
537.676254	59.275134	73.002279
536.874449	63.198418	73.007284
536.011701	63.317002	73.012289
535.675654	61.725957	73.017294
534.660973	62.778587	73.022298
534.226796	58.256036	73.027303
533.115667	69.866866	73.032308
533.128397	55.089816	73.037313
532.722472	69.401421	73.042318
531.707132	62.858456	73.047322
531.050863	64.503661	73.052327
530.297142	52.333819	73.057332
529.053566	62.519768	73.062337
528.091429	70.320846	73.067342
527.906387	60.602302	73.072346
527.592943	64.239655	73.077351
527.132069	70.618986	73.082356
527.072536	65.489590	73.087361
525.624416	67.626758	73.092366
524.950903	73.257843	73.097370
524.606758	61.792259	73.102375
523.273360	60.243396	73.107380
522.669186	61.903957	73.112385
522.120337	66.023480	73.117390
521.723668	66.359546	73.122394
521.183083	61.661570	73.127399
519.991732	69.264210	73.132404
519.493963	60.096922	73.137409
519.215350	56.593471	73.142414
518.802175	62.231966	73.147418
517.699235	65.324917	73.152423
516.556187	67.575910	73.157428
516.255857	69.870851	73.162433
515.822486	65.450669	73.167438
515.026672	59.262228	73.172442
514.087495	53.378883	73.177447
513.527379	62.296983	73.182452
513.313055	57.537580	73.187457
512.694730	62.221645	73.192462
511.668393	55.317769	73.197466
510.981001	61.132401	73.202471
510.330737	63.694382	73.207476
509.952623	55.689102	73.212481
509.027913	53.822849	73.217486
508.152212	61.515548	73.222490
508.127978	59.608350	73.227495
507.267514	65.173027	73.232500
505.956007	54.134346	73.237505
505.313906	69.013395	73.242510
504.873251	54.732746	73.247514
504.640211	56.168620	73.252519
504.078237	50.709288	73.257524
503.113046	48.619266	73.262529
502.395349	51.122608	73.267534
501.903834	58.460812	73.272538
501.651210	51.373773	73.277543
500.416439	52.317982	73.282548
499.996614	47.170300	73.287553
499.227799	58.138436	73.292558
498.407566	58.289683	73.297562
497.443419	59.610226	73.302567
497.040172	58.933428	73.307572
496.381690	48.170753	73.312577
495.931902	65.026494	73.317582
495.492796	52.142694	73.322586
494.635824	48.844915	73.327591
493.505673	63.893163	73.332596
493.313040	43.571522	73.337601
492.662839	64.652032	73.342606
491.402310	59.154179	73.347610
491.306873	62.856147	73.352615
490.490308	57.525676	73.357620
490.252377	47.925953	73.362625
489.702936	54.374580	73.367630
488.827705	57.849132	73.372634
488.368040	57.670147	73.377639
487.323525	61.341967	73.382644
486.648840	48.093606	73.387649
486.060049	63.664280	73.392654
485.201486	62.867641	73.397658
484.428316	53.454100	73.402663
483.303882	58.739156	73.407668
482.847322	57.578876	73.412673
482.589419	64.707994	73.417678
482.383602	58.225317	73.422682
481.957496	65.144703	73.427687
480.280882	63.056066	73.432692
479.890634	56.317361	73.437697
479.637461	55.055300	73.442702
478.507359	61.596435	73.447706
477.788946	57.991177	73.452711
477.075317	66.858051	73.457716
476.806921	51.704779	73.462721
476.480014	53.742198	73.467726
475.415608	58.122043	73.472730
475.095829	53.060922	73.477735
474.124814	67.506701	73.482740
473.326198	65.942050	73.487745
472.248978	68.830663	73.492750
471.626739	56.321373	73.497754
471.326657	62.088503	73.502759
470.873607	64.297397	73.507764
470.470253	57.745273	73.512769
469.560868	58.948300	73.517774
468.323654	62.811665	73.522778
468.233485	46.236072	73.527783
467.618844	56.741287	73.532788
466.582165	53.714982	73.537793
465.898282	64.418879	73.542798
465.584561	60.071106	73.547802
465.217029	54.708531	73.552807
464.323485	76.316650	73.557812
463.639592	57.486122	73.562817
463.106301	64.269631	73.567822
462.263023	61.483733	73.572826
461.063314	55.440080	73.577831
460.383140	65.495303	73.582836
460.303444	47.844205	73.587841
459.896152	55.930614	73.592846
458.536919	62.475147	73.597850
457.857735	50.107395	73.602855
457.315999	63.562326	73.607860
457.278996	52.681730	73.612865
456.752776	52.486548	73.617870
455.326849	51.720390	73.622874
454.862412	54.017827	73.627879
454.184730	62.809595	73.632884
453.755457	53.719722	73.637889
452.886399	56.821165	73.642894
451.950408	70.184382	73.647898
451.846100	59.035402	73.652903
451.236132	65.036396	73.657908
450.133233	65.216924	73.662913
449.311966	61.233847	73.667918
448.723237	70.798298	73.672922
448.637268	57.736830	73.677927
447.941956	61.258419	73.682932
446.945210	62.016509	73.687937
446.459674	63.066867	73.692942
445.894984	60.864177	73.697946
445.128024	63.329655	73.702951
443.951696	65.210692	73.707956
443.557397	51.222283	73.712961
443.091754	64.031198	73.717966
442.389299	66.101649	73.722970
441.825156	63.096256	73.727975
440.817545	59.445627	73.732980
440.590909	58.739124	73.737985
440.254467	65.503889	73.742990
439.106239	61.826782	73.747994
438.553623	62.317009	73.752999
437.715254	59.719560	73.758004
437.036530	54.207888	73.763009
436.125817	67.622269	73.768014
435.605732	70.576663	73.773018
435.422407	51.067201	73.778023
434.496501	61.651977	73.783028
433.722465	56.462976	73.788033
433.023694	61.647121	73.793038
432.213028	62.701977	73.798042
432.040141	53.252738	73.803047
430.775144	67.713829	73.808052
430.165221	61.476881	73.813057
429.539760	56.614271	73.818062
429.206877	64.185816	73.823066
428.838420	66.537348	73.828071
427.722007	65.305603	73.833076
427.301423	53.035423	73.838081
426.738147	64.825482	73.843086
425.993830	68.868940	73.848090
425.187960	62.723133	73.853095
424.060498	65.960369	73.858100
423.934592	60.475730	73.863105
423.506508	58.355353	73.868110
422.581556	60.229461	73.873114
422.157787	54.041702	73.878119
421.351658	68.029165	73.883124
420.752772	53.754834	73.888129
419.829333	55.827384	73.893134
418.760540	63.844168	73.898138
418.760950	49.256750	73.903143
417.988577	66.319998	73.908148
416.819355	51.638258	73.913153
416.050039	57.927978	73.918158
415.654589	70.443460	73.923162
415.496159	58.828477	73.928167
415.069605	56.895504	73.933172
414.064604	63.145514	73.938177
413.222387	51.833439	73.943182
412.619741	66.712515	73.948186
412.270283	51.430261	73.953191
411.136772	61.537222	73.958196
410.533131	63.159879	73.963201
410.157752	57.604612	73.968206
409.517022	57.547526	73.973210
408.645853	65.515480	73.978215
407.901795	63.163195	73.983220
407.188601	65.776225	73.988225
406.965531	68.375813	73.993230
406.243867	59.200083	73.998234
405.107342	55.476978	74.003239
404.293906	70.839047	74.008244
404.196176	60.866933	74.013249
403.753642	67.191319	74.018254
402.330757	67.602614	74.023258
402.194935	66.090065	74.028263
401.536411	61.035625	74.033268
400.640734	64.346317	74.038273
399.880003	59.002254	74.043278
398.950810	65.087236	74.048282
399.002154	59.527051	74.053287
398.450600	64.818626	74.058292
397.769417	57.181764	74.063297
396.884731	61.118292	74.068302
395.941139	66.887046	74.073306
395.968345	57.262435	74.078311
394.570749	66.276152	74.083316
393.808935	49.079087	74.088321
393.555371	59.741232	74.093326
392.852171	65.799667	74.098330
392.443637	61.301445	74.103335
391.107526	56.017531	74.108340
390.505845	59.733936	74.113345
390.303140	52.451317	74.118350
389.783496	56.238222	74.123354
388.793831	56.779178	74.128359
387.884058	53.258055	74.133364
387.339085	58.499698	74.138369
387.354859	58.806333	74.143374
386.701163	61.323160	74.148378
385.649191	56.567947	74.153383
385.025781	55.074752	74.158388
384.396249	54.241655	74.163393
383.281870	59.112014	74.168398
382.245229	60.720101	74.173402
382.297689	58.385974	74.178407
381.811784	61.584072	74.183412
380.977051	57.713547	74.188417
380.225082	45.420504	74.193422
379.566714	61.226181	74.198426
379.174488	51.780367	74.203431
378.642506	53.397919	74.208436
377.680594	50.181556	74.213441
376.831834	54.061905	74.218446
376.049542	55.736690	74.223450
375.864488	56.218819	74.228455
374.775005	57.950438	74.233460
374.280947	53.842717	74.238465
373.823649	50.676826	74.243470
372.788933	60.559912	74.248474
372.057766	50.061162	74.253479
371.370574	56.659483	74.258484
370.637911	48.439521	74.263489
370.495192	46.346218	74.268494
370.253374	58.975973	74.273498
369.609574	46.626275	74.278503
368.529175	46.983015	74.283508
367.852229	51.627564	74.288513
366.937854	42.985583	74.293518
365.882140	47.832406	74.298522
365.415568	50.144388	74.303527
364.882380	41.359670	74.308532
364.545396	55.387481	74.313537
364.161306	48.457027	74.318542
363.081941	62.087516	74.323546
362.478026	49.682581	74.328551
361.851498	64.158637	74.333556
361.160017	58.868203	74.338561
360.584952	58.162042	74.343566
359.636084	63.696697	74.348570
359.378146	55.230785	74.353575
358.015591	62.206376	74.358580
357.411171	56.757001	74.363585
356.865896	46.640194	74.368590
356.489367	55.369792	74.373594
356.154702	51.142065	74.378599
355.330023	51.981573	74.383604
354.596361	58.951557	74.388609
354.200786	46.076640	74.393614
353.554847	66.632964	74.398618
352.479880	51.570416	74.403623
351.865544	56.260183	74.408628
351.361053	53.319421	74.413633
350.759388	53.590417	74.418638
349.627670	60.540262	74.423642
349.061429	45.309926	74.428647
348.338014	52.808096	74.433652
348.021455	54.414977	74.438657
347.096885	61.429578	74.443662
346.061944	58.428279	74.448666
345.733710	60.499038	74.453671
345.321264	53.533683	74.458676
344.729139	48.008244	74.463681
344.348158	51.225892	74.468686
343.304264	49.512731	74.473690
342.921388	48.222474	74.478695
342.024284	57.985873	74.483700
340.710841	63.439871	74.488705
340.460447	49.756548	74.493710
339.838842	48.310383	74.498714
339.389778	56.236312	74.503719
339.212317	52.675772	74.508724
337.971501	49.062357	74.513729
336.851291	53.509490	74.518734
336.636311	51.413514	74.523738
336.257388	54.009557	74.528743
335.745775	55.795749	74.533748
334.799225	58.086464	74.538753
334.344401	52.610103	74.543758
333.285819	52.346833	74.548762
332.178125	55.122093	74.553767
331.745906	53.563752	74.558772
331.033142	46.297781	74.563777
330.899072	47.166000	74.568782
330.538147	54.518102	74.573786
329.725440	46.074385	74.578791
328.785821	61.313072	74.583796
328.200146	49.819816	74.588801
327.401059	42.914511	74.593806
326.379074	58.669337	74.598810
326.039137	42.855781	74.603815
325.486362	51.684425	74.608820
324.986623	58.926197	74.613825
324.014208	53.754662	74.618830
323.076977	49.436904	74.623834
322.696001	49.048304	74.628839
322.072926	53.649588	74.633844
321.827218	43.997529	74.638849
321.475343	51.211002	74.643854
320.036638	46.161090	74.648858
319.596729	48.930846	74.653863
318.668624	52.986272	74.658868
317.559246	51.113259	74.663873
317.521339	52.749846	74.668878
316.754777	52.042678	74.673882
316.736873	43.063897	74.678887
315.393418	56.219277	74.683892
314.615829	52.547816	74.688897
314.426653	49.559965	74.693902
313.708309	54.583261	74.698906
313.221507	42.290565	74.703911
312.094518	53.634339	74.708916
311.694091	59.382779	74.713921
311.195599	50.046954	74.718926
310.030781	55.972406	74.723930
309.341914	58.209448	74.728935
308.568178	57.367816	74.733940
308.359227	53.591539	74.738945
308.014689	55.895120	74.743950
306.569923	54.097641	74.748954
306.274675	61.713652	74.753959
305.787698	63.265703	74.758964
305.338460	56.859694	74.763969
304.447689	58.643247	74.768974
303.565784	62.998803	74.773978
303.253750	50.528448	74.778983
301.980060	61.548706	74.783988
301.040470	56.121231	74.788993
300.612496	49.516308	74.793998
299.921244	60.361742	74.799002
300.020645	48.384021	74.804007
299.641201	59.310637	74.809012
298.502267	55.703079	74.814017
298.092595	52.143286	74.819022
297.002170	69.804409	74.824026
296.670196	55.577466	74.829031
295.715295	62.330429	74.834036
294.873321	61.643171	74.839041
294.637156	52.375919	74.844046
293.594740	56.400691	74.849050
292.766812	52.907561	74.854055
292.001196	65.750103	74.859060
291.636693	47.920525	74.864065
291.437413	46.758699	74.869070
290.310337	65.895282	74.874074
289.613661	57.972364	74.879079
289.098878	63.603425	74.884084
288.708048	54.915874	74.889089
288.233738	47.216125	74.894094
287.200149	49.016137	74.899098
286.980675	55.082643	74.904103
285.818703	57.018229	74.909108
284.730658	56.461652	74.914113
284.328444	56.429657	74.919118
283.468997	55.259519	74.924122
283.228339	56.521595	74.929127
282.999037	52.882598	74.934132
281.889159	71.906069	74.939137
281.421930	52.284217	74.944142
280.487667	68.534404	74.949146
280.125998	51.382418	74.954151
279.100715	56.688019	74.959156
278.464403	65.660870	74.964161
278.350839	49.073276	74.969166
276.753465	60.000065	74.974170
276.205671	45.597816	74.979175
275.598314	53.779200	74.984180
275.168680	63.349847	74.989185
274.948112	53.879852	74.994190
274.126659	54.286816	74.999194
273.344649	45.380946	75.004199
272.962240	53.532782	75.009204
271.738647	61.672053	75.014209
271.067958	46.510431	75.019214
270.154587	68.123298	75.024218
269.829065	61.448435	75.029223
269.421463	57.347457	75.034228
268.925885	63.524203	75.039233
268.278874	56.796513	75.044238
267.312473	56.677840	75.049242
267.064325	61.952612	75.054247
266.029666	59.473241	75.059252
264.822140	56.898430	75.064257
264.392653	60.147474	75.069262
264.152386	55.948868	75.074266
263.651901	53.597230	75.079271
262.532899	65.777062	75.084276
261.687348	52.377843	75.089281
261.661334	56.931278	75.094286
261.087178	62.885600	75.099290
260.701492	44.070730	75.104295
259.496782	70.517344	75.109300
258.758289	58.543872	75.114305
257.813823	47.438971	75.119310
256.847312	63.596533	75.124314
256.471264	58.490806	75.129319
255.841066	47.293238	75.134324
255.532652	61.496259	75.139329
255.379065	51.458966	75.144334
254.137937	63.041719	75.149338
253.717936	47.048568	75.154343
252.789515	54.740274	75.159348
251.590347	58.137234	75.164353
251.276801	60.448497	75.169358
250.364083	67.745073	75.174362
250.036202	57.339769	75.179367
249.663934	57.607338	75.184372
249.155804	58.312850	75.189377
248.376238	52.079353	75.194382
247.414307	60.170616	75.199386
247.119490	47.650229	75.204391
246.557707	53.402317	75.209396
245.134920	58.682990	75.214401
245.304008	45.609296	75.219406
244.360671	57.541946	75.224410
243.591134	57.065494	75.229415
242.877102	56.135525	75.234420
242.241910	61.213391	75.239425
242.190485	58.764946	75.244430
240.561525	57.941398	75.249434
239.840043	54.795571	75.254439
239.269431	51.832262	75.259444
238.823573	51.722082	75.264449
238.669139	51.608022	75.269454
237.533735	58.210014	75.274458
236.880850	59.386428	75.279463
236.338553	52.899085	75.284468
235.673653	53.840887	75.289473
234.946706	50.405794	75.294478
233.803730	57.459972	75.299482
233.858336	54.248778	75.304487
233.128012	60.865043	75.309492
232.277370	60.387332	75.314497
231.479617	46.196822	75.319502
230.661837	59.896027	75.324506
230.659520	49.460914	75.329511
230.319994	49.396859	75.334516
228.942618	61.157446	75.339521
228.414768	61.115527	75.344526
227.803519	66.916507	75.349530
226.864043	55.968504	75.354535
225.918116	57.265745	75.359540
224.954617	60.599921	75.364545
225.035948	55.014466	75.369550
224.508061	59.972734	75.374554
224.213348	51.064890	75.379559
223.166054	58.401843	75.384564
222.567467	57.350982	75.389569
222.200759	54.232180	75.394574
221.043688	50.834120	75.399578
220.313431	47.618742	75.404583
219.871812	57.169224	75.409588
219.244815	61.066306	75.414593
218.296809	54.526956	75.419598
217.462721	57.395833	75.424602
216.944333	65.224027	75.429607
216.834645	58.838023	75.434612
215.836382	59.609061	75.439617
215.089481	59.520069	75.444622
213.960977	62.122089	75.449626
213.500150	58.997792	75.454631
213.321155	56.792020	75.459636
213.006656	54.536892	75.464641
211.952318	56.695034	75.469646
211.181151	56.515300	75.474650
210.852236	57.665305	75.479655
209.589703	51.895142	75.484660
208.869896	62.453428	75.489665
208.745204	54.218601	75.494670
208.149179	61.683881	75.499674
207.215213	53.667947	75.504679
206.158766	62.780319	75.509684
205.501401	52.534781	75.514689
205.548714	51.749940	75.519694
204.929372	63.824905	75.524698
203.894130	54.361803	75.529703
203.333804	61.871853	75.534708
202.477276	75.522066	75.539713
202.155639	57.070703	75.544718
200.886126	63.232075	75.549722
200.335343	57.531363	75.554727
200.091029	57.185646	75.559732
199.143280	65.222630	75.564737
199.109074	55.153698	75.569742
197.765131	58.554840	75.574746
197.311144	53.759577	75.579751
196.673505	61.647781	75.584756
196.148184	62.889019	75.589761
195.368038	56.781780	75.594766
194.640053	58.946245	75.599770
194.092216	54.970135	75.604775
193.864114	55.897503	75.609780
192.325194	57.259333	75.614785
191.908480	53.806333	75.619790
191.393305	58.146032	75.624794
190.923199	48.299552	75.629799
189.690475	59.128831	75.634804
188.746506	60.320126	75.639809
188.693926	42.442440	75.644814
188.075285	59.720879	75.649818
187.571573	62.697935	75.654823
186.947777	50.911206	75.659828
185.730188	59.763864	75.664833
185.297460	47.410549	75.669838
184.699829	70.993033	75.674842
184.874828	59.917832	75.679847
183.428516	55.129396	75.684852
182.709612	59.618264	75.689857
182.335896	50.073364	75.694862
181.168899	61.016740	75.699866
180.478742	56.390011	75.704871
179.883454	48.178181	75.709876
179.313067	58.793067	75.714881
179.109568	58.133361	75.719886
178.617367	57.245311	75.724890
177.638094	54.268328	75.729895
177.045610	50.433374	75.734900
176.373415	50.586355	75.739905
175.648883	43.990902	75.744910
174.556616	58.583797	75.749914
174.086300	57.753756	75.754919
173.958655	51.586651	75.759924
173.084304	55.647748	75.764929
172.555225	51.662347	75.769934
171.762546	56.153518	75.774938
170.632025	54.996678	75.779943
170.091740	64.316911	75.784948
169.591665	60.658022	75.789953
169.251969	53.714226	75.794958
167.882392	47.245267	75.799962
166.846503	52.727627	75.804967
166.780767	52.340829	75.809972
166.364607	65.379972	75.814977
166.042219	59.269143	75.819982
165.103465	65.109734	75.824986
164.115962	55.087145	75.829991
163.850848	51.939541	75.834996
162.980777	64.368279	75.840001
162.290601	54.998407	75.845006
161.406804	63.655943	75.850010
160.797906	63.904486	75.855015
160.750934	59.676652	75.860020
159.629081	57.823047	75.865025
158.926023	47.102302	75.870030
157.981681	51.652346	75.875034
157.444656	58.568945	75.880039
157.253184	58.176964	75.885044
156.312898	52.912080	75.890049
155.731922	39.160104	75.895054
154.969832	52.770019	75.900058
154.753538	48.200204	75.905063
154.141430	50.901252	75.910068
152.890172	60.831547	75.915073
152.564183	45.476258	75.920078
151.682383	58.581753	75.925082
150.668834	53.762184	75.930087
149.876034	57.406614	75.935092
149.277273	58.355240	75.940097
149.157453	42.828320	75.945102
148.970046	53.501984	75.950106
147.894919	57.207197	75.955111
147.029110	53.504134	75.960116
146.262830	51.414083	75.965121
145.885720	54.545989	75.970126
145.474294	65.427254	75.975130
144.334323	62.955268	75.980135
144.172989	50.112445	75.985140
143.315042	60.344284	75.990145
142.231789	49.392446	75.995150
141.563153	43.194920	76.000154
141.091089	56.254007	76.005159
140.664908	56.329929	76.010164
140.324158	63.388691	76.015169
139.085437	45.919316	76.020174
138.425513	54.812375	76.025178
137.680373	63.782100	76.030183
137.487042	55.189245	76.035188
136.524646	55.372740	76.040193
135.705239	51.529828	76.045198
135.167152	51.590480	76.050202
134.582768	52.978332	76.055207
133.868468	57.037575	76.060212
133.030338	60.695546	76.065217
132.455774	52.135097	76.070222
132.099858	52.710714	76.075226
131.463475	50.566842	76.080231
130.934656	51.357673	76.085236
129.871711	49.117825	76.090241
129.598817	55.405726	76.095246
128.374561	50.583498	76.100250
127.823758	52.751266	76.105255
127.382678	57.033433	76.110260
126.834600	64.910523	76.115265
126.502632	56.257779	76.120270
125.193477	47.395025	76.125274
124.498612	70.012213	76.130279
124.323990	42.932607	76.135284
122.665726	53.082336	76.140289
122.361991	59.425615	76.145294
121.559139	53.981148	76.150298
121.138948	62.282516	76.155303
121.256608	50.715032	76.160308
120.723492	61.765500	76.165313
119.829871	59.922827	76.170318
118.799673	61.041171	76.175322
117.778375	60.975462	76.180327
117.077378	49.932727	76.185332
116.382610	54.033011	76.190337
116.014853	57.869856	76.195342
115.687427	57.122690	76.200346
114.818734	63.027813	76.205351
114.364536	56.532764	76.210356
113.202657	60.631845	76.215361
113.065701	60.064029	76.220366
112.060742	64.798787	76.225370
111.006910	67.414176	76.230375
110.864029	57.395696	76.235380
110.338391	57.179997	76.240385
109.709886	53.090626	76.245390
108.624019	52.666236	76.250394
107.831637	54.831532	76.255399
107.534797	59.379264	76.260404
106.881731	53.206069	76.265409
106.550950	45.291109	76.270414
105.509656	47.406215	76.275418
104.875155	61.038375	76.280423
104.389081	58.660822	76.285428
103.150800	55.786669	76.290433
102.382364	48.750418	76.295438
102.237116	48.477218	76.300442
101.706183	52.649145	76.305447
101.197674	56.022767	76.310452
100.165454	62.884308	76.315457
99.265681	60.746177	76.320462
98.809152	55.408909	76.325466
98.021270	60.673566	76.330471
97.471412	62.831729	76.335476
96.191978	60.979629	76.340481
96.157575	61.087696	76.345486
95.555418	61.409291	76.350490
94.907834	60.534998	76.355495
94.815272	52.933687	76.360500
93.493777	62.020557	76.365505
93.342388	55.095631	76.370510
92.908956	68.850267	76.375514
91.547969	62.860918	76.380519
91.227656	55.116163	76.385524
90.336169	61.401794	76.390529
89.591377	54.284509	76.395534
88.535503	62.723517	76.400538
88.050536	58.761062	76.405543
87.721241	53.581691	76.410548
87.111855	55.087073	76.415553
86.684620	65.627111	76.420558
85.737876	53.716888	76.425562
85.054803	57.547252	76.430567
84.730267	53.767360	76.435572
83.499855	56.451914	76.440577
83.171026	53.040111	76.445582
82.534222	54.352762	76.450586
81.642397	51.412335	76.455591
81.119957	44.071957	76.460596
80.063572	60.759513	76.465601
80.089661	52.754533	76.470606
79.308614	60.118460	76.475610
78.174962	55.084705	76.480615
77.436146	59.901604	76.485620
76.915944	60.251132	76.490625
76.669060	53.090720	76.495630
76.186308	60.580532	76.500634
74.897971	61.476726	76.505639
74.735152	57.161725	76.510644
73.809611	57.479706	76.515649
72.805375	54.203996	76.520654
72.496910	53.146329	76.525658
71.487425	56.610885	76.530663
71.266316	52.179034	76.535668
70.630082	55.170935	76.540673
69.665608	51.876271	76.545678
68.847686	53.788625	76.550682
68.301385	66.709764	76.555687
68.025007	61.271237	76.560692
67.679823	60.589984	76.565697
66.673703	62.696344	76.570702
65.924704	60.929970	76.575706
65.283073	57.399331	76.580711
64.239256	62.605471	76.585716
63.381077	64.148960	76.590721
63.144962	52.995840	76.595726
62.934914	55.162892	76.600730
62.416807	57.338074	76.605735
61.542041	59.466063	76.610740
60.459174	53.873900	76.615745
60.318463	55.394427	76.620750
59.267102	57.351897	76.625754
58.207939	53.947768	76.630759
57.780338	45.529479	76.635764
57.035175	60.136434	76.640769
57.011489	53.848692	76.645774
56.040764	55.263484	76.650778
54.710277	60.141633	76.655783
54.799977	58.921128	76.660788
54.148286	60.890550	76.665793
53.550089	53.048206	76.670798
52.606971	54.433367	76.675802
51.780037	62.791725	76.680807
51.389528	49.789942	76.685812
50.628645	56.337008	76.690817
49.980567	60.232758	76.695822
49.133437	63.598897	76.700826
48.515812	63.121934	76.705831
48.396799	55.121174	76.710836
47.381419	64.113517	76.715841
46.886226	58.683085	76.720846
46.223265	65.506255	76.725850
45.657480	60.192730	76.730855
44.484241	62.773575	76.735860
43.767021	62.173734	76.740865
43.487421	55.556248	76.745870
43.291803	65.382884	76.750874
41.934178	63.678892	76.755879
41.169112	55.768553	76.760884
40.313581	49.845275	76.765889
40.385092	61.431636	76.770894
39.798447	55.832878	76.775898
38.645738	59.317136	76.780903
37.996204	65.509006	76.785908
37.676390	58.437495	76.790913
37.190679	49.747798	76.795918
36.088569	61.336844	76.800922
35.306397	58.520862	76.805927
34.979821	56.792776	76.810932
34.166619	67.845353	76.815937
33.397840	53.350710	76.820942
32.722276	53.584687	76.825946
31.990993	60.882346	76.830951
31.712846	58.241429	76.835956
30.834798	61.968871	76.840961
30.145968	51.622771	76.845966
29.806188	66.237618	76.850970
29.033045	52.252995	76.855975
28.314169	57.974986	76.860980
27.246650	65.155976	76.865985
26.699436	56.389361	76.870990
26.630571	58.395136	76.875994
25.715317	65.744216	76.880999
24.868123	44.886915	76.886004
24.141171	59.196100	76.891009
23.956996	52.954456	76.896014
22.916980	52.899658	76.901018
21.934277	64.252061	76.906023
21.660726	55.908547	76.911028
20.914711	59.835692	76.916033
20.188748	61.627748	76.921038
19.238309	58.505895	76.926042
18.347087	65.130527	76.931047
18.327897	63.093238	76.936052
17.666868	61.068438	76.941057
17.583350	45.991463	76.946062
16.672479	55.391313	76.951066
15.503788	58.841862	76.956071
15.401994	55.496355	76.961076
14.248825	63.685996	76.966081
13.343470	48.801595	76.971086
12.715615	60.397002	76.976090
11.916326	59.171639	76.981095
11.814877	51.623792	76.986100
11.297280	69.294539	76.991105
10.745490	56.512439	76.996110
9.804511	55.123609	77.001114
9.329789	65.549808	77.006119
8.791179	51.226612	77.011124
7.430583	63.162803	77.016129
6.694559	61.895815	77.021134
6.795901	55.263305	77.026139
5.975912	60.902088	77.031143
5.297135	61.308461	77.036148
4.485907	52.457819	77.041153
3.997934	67.030075	77.046158