Mon Mar 08 19:43:33 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.613624	85.907638	0.000000
-0.641190	67.084566	0.005005
-1.304202	45.130354	0.010010
-2.672723	-1.423514	0.015014
-7.799526	-18.830699	0.020019
-12.982059	-23.899688	0.025024
-18.070203	-25.634523	0.030029
-22.756982	-14.260488	0.035034
-26.669999	-14.156534	0.040038
-30.268493	-22.907801	0.045043
-33.939168	-11.717917	0.050048
-37.438617	-16.858252	0.055053
-41.405240	-19.525684	0.060058
-44.610359	-27.388849	0.065062
-48.819013	-16.360685	0.070067
-52.617596	-8.105357	0.075072
-56.130079	-16.045623	0.080077
-60.032041	-10.317228	0.085082
-63.599832	-10.211526	0.090086
-67.768760	-16.736692	0.095091
-71.110734	-22.345189	0.100096
-75.088756	-2.506147	0.105101
-79.093859	-19.954944	0.110106
-82.499704	-17.888240	0.115110
-86.467464	-9.392998	0.120115
-90.160838	-17.834166	0.125120
-93.924921	-18.326257	0.130125
-97.225541	-16.889710	0.135130
-101.096149	-16.330390	0.140134
-105.039164	-22.393253	0.145139
-109.091865	-28.864349	0.150144
-112.954868	-34.386492	0.155149
-116.775774	-33.619051	0.160154
-120.327544	-17.416350	0.165158
-124.311369	-39.236265	0.170163
-128.084645	-16.941596	0.175168
-131.957722	-11.247659	0.180173
-135.959384	-20.211949	0.185178
-139.160849	-21.493861	0.190182
-142.930770	-13.440080	0.195187
-146.434064	-11.983740	0.200192
-149.919756	-13.759560	0.205197
-154.346158	-7.229869	0.210202
-157.723090	-30.043802	0.215206
-161.888063	-23.270417	0.220211
-165.642631	-5.606671	0.225216
-169.226140	-16.517222	0.230221
-172.712551	-17.501323	0.235226
-176.398631	-13.659980	0.240230
-180.611899	-7.567926	0.245235
-184.362753	-14.323596	0.250240
-187.777764	-24.824219	0.255245
-192.158727	-6.746680	0.260250
-195.649261	-10.352366	0.265254
-199.406598	-10.299784	0.270259
-203.233383	-12.697550	0.275264
-206.480446	-10.995034	0.280269
-210.243303	-4.553801	0.285274
-214.293564	-9.735262	0.290278
-218.172172	4.564480	0.295283
-221.806832	-12.405486	0.300288
-225.362097	-17.189726	0.305293
-229.548470	-2.877119	0.310298
-233.027774	-15.841470	0.315302
-237.004245	-10.455695	0.320307
-240.556225	-9.783019	0.325312
-244.519114	-6.249023	0.330317
-248.363248	-2.387073	0.335322
-251.722322	-11.775407	0.340326
-255.706827	-3.146350	0.345331
-259.462719	-8.762621	0.350336
-263.369576	0.167846	0.355341
-267.268077	-0.933251	0.360346
-270.883283	-9.758741	0.365350
-274.492241	-11.976714	0.370355
-278.252767	-8.517542	0.375360
-282.083856	-6.977143	0.380365
-286.379464	-11.748757	0.385370
-289.453221	-4.945936	0.390374
-293.191565	-8.718482	0.395379
-297.005036	-12.382842	0.400384
-300.638500	-15.544538	0.405389
-304.856805	-4.260540	0.410394
-308.237481	-10.521636	0.415398
-312.197723	-22.541818	0.420403
-316.058759	-2.259096	0.425408
-319.458424	-8.687442	0.430413
-323.342626	-4.396388	0.435418
-327.281293	-6.776093	0.440422
-331.070008	-9.690624	0.445427
-335.179068	-5.724746	0.450432
-338.188869	-12.043432	0.455437
-342.737212	-10.522454	0.460442
-346.216325	-5.673192	0.465446
-349.508954	-21.284696	0.470451
-353.557649	-12.415025	0.475456
-357.283718	-2.587681	0.480461
-361.237923	-11.672688	0.485466
-364.656802	-26.341559	0.490470
-368.737160	-11.610463	0.495475
-372.607501	-4.038583	0.500480
-376.071563	-7.307631	0.505485
-380.070206	-5.700902	0.510490
-383.221828	-10.921485	0.515494
-386.730779	-11.821256	0.520499
-391.035912	-10.324831	0.525504
-394.891041	-22.336420	0.530509
-399.023052	7.259879	0.535514
-402.490474	-16.754956	0.540518
-406.561872	-3.994685	0.545523
-409.932443	-6.827638	0.550528
-413.466395	-4.219660	0.555533
-417.662486	-14.875884	0.560538
-421.414439	-11.950831	0.565542
-425.014806	-14.666646	0.570547
-428.886470	-8.636609	0.575552
-432.270141	-5.409257	0.580557
-436.479949	-13.918766	0.585562
-440.153761	-14.798437	0.590566
-444.138228	-10.850699	0.595571
-447.935455	-4.203363	0.600576
-451.211015	-13.577927	0.605581
-455.131264	-17.127210	0.610586
-458.777541	-9.994652	0.615590
-462.448328	-3.481019	0.620595
-466.426490	-6.811318	0.625600
-469.755064	-12.188009	0.630605
-474.145351	-8.290517	0.635610
-477.475832	-15.363559	0.640614
-481.511988	-8.373685	0.645619
-485.799862	-4.970307	0.650624
-488.783849	-14.470225	0.655629
-492.977546	-9.110841	0.660634
-496.251522	-19.135240	0.665638
-500.166836	12.279372	0.670643
-504.018392	-19.720494	0.675648
-507.877942	-2.752234	0.680653
-511.866928	-0.987570	0.685658
-515.338004	-11.146031	0.690662
-518.925698	-21.721057	0.695667
-522.801879	6.457981	0.700672
-526.287455	-21.617223	0.705677
-530.791409	-1.456992	0.710682
-534.285574	-22.297892	0.715686
-538.091435	-9.513609	0.720691
-541.540181	-7.199732	0.725696
-545.598104	5.279514	0.730701
-549.511701	4.597574	0.735706
-552.534172	-11.548753	0.740710
-556.514075	-21.430332	0.745715
-560.585746	-3.284913	0.750720
-563.935165	-13.680333	0.755725
-568.172535	-14.173334	0.760730
-571.828202	-14.811291	0.765734
-575.895559	2.423640	0.770739
-579.350729	-15.747544	0.775744
-582.902523	-22.999519	0.780749
-586.742145	-13.068559	0.785754
-590.247766	-27.656983	0.790758
-594.307609	-11.142273	0.795763
-597.914516	-9.999858	0.800768
-601.870291	-26.187783	0.805773
-606.009191	-13.933622	0.810778
-609.444784	-6.774585	0.815782
-612.834597	-23.641072	0.820787
-617.104634	-16.143721	0.825792
-620.685049	-11.408766	0.830797
-624.584993	-4.850397	0.835802
-628.255628	-16.993553	0.840806
-631.706009	-20.716951	0.845811
-635.434314	-24.555195	0.850816
-639.059983	-18.863735	0.855821
-643.260429	-18.995100	0.860826
-647.100267	-14.527713	0.865830
-650.985774	-22.508363	0.870835
-654.574356	-13.722768	0.875840
-658.511661	-23.465902	0.880845
-662.228236	-10.914885	0.885850
-665.693924	-9.580485	0.890854
-669.622464	-14.987159	0.895859
-673.395295	-2.174837	0.900864
-676.646012	-13.536682	0.905869
-680.689335	-15.438634	0.910874
-684.600228	-23.681652	0.915878
-688.367624	-9.883091	0.920883
-692.236926	-11.199448	0.925888
-695.594947	-27.708206	0.930893
-700.146007	-17.445785	0.935898
-703.427211	-10.869489	0.940902
-707.160542	-14.881844	0.945907
-711.004041	-4.379261	0.950912
-714.370152	-21.298255	0.955917
-718.599411	-14.269255	0.960922
-722.043251	-8.308710	0.965926
-725.733954	-13.833715	0.970931
-729.598810	-20.155558	0.975936
-733.425803	-25.087954	0.980941
-737.790989	-10.058471	0.985946
-741.209815	-21.681903	0.990950
-744.889949	-6.984225	0.995955
-748.770341	-12.062595	1.000960
-752.267355	-20.685433	1.005965
-756.173150	-2.793291	1.010970
-759.654854	-11.120551	1.015974
-763.962667	-20.646598	1.020979
-767.744940	-2.696918	1.025984
-770.870091	-16.407659	1.030989
-774.469499	-12.916710	1.035994
-778.576594	-15.930997	1.040998
-782.203625	-28.809344	1.046003
-786.314779	-14.312356	1.051008
-790.181186	-0.835254	1.056013
-793.734035	-3.625900	1.061018
-797.337822	-26.667411	1.066022
-801.300454	-10.809688	1.071027
-805.182959	-8.837648	1.076032
-808.525330	-15.223956	1.081037
-812.426825	-24.389116	1.086042
-816.406283	-18.907323	1.091046
-820.212916	-5.575343	1.096051
-823.789232	-43.477992	1.101056
-827.334627	-6.127062	1.106061
-831.283713	-11.807693	1.111066
-834.990854	-2.214471	1.116070
-838.678387	-14.849693	1.121075
-842.409867	-20.479941	1.126080
-846.302529	-21.926336	1.131085
-850.182302	-13.458156	1.136090
-853.855489	-13.014327	1.141094
-857.861143	-9.750018	1.146099
-861.786959	-15.100029	1.151104
-865.347050	-20.923206	1.156109
-869.289371	-10.663187	1.161114
-872.447451	-18.196829	1.166118
-876.335067	-27.097610	1.171123
-880.361034	-18.788923	1.176128
-883.665803	-30.362555	1.181133
-887.589045	-31.075500	1.186138
-891.638074	-12.873290	1.191142
-895.306216	-17.020329	1.196147
-899.309615	-22.485590	1.201152
-902.852506	-17.412475	1.206157
-906.374488	-2.432374	1.211162
-909.961883	-21.028098	1.216166
-913.962468	-27.610169	1.221171
-917.700048	-24.264058	1.226176
-921.456906	-15.911608	1.231181
-925.702491	-16.278081	1.236186
-928.961644	-19.609021	1.241190
-932.871943	-8.545113	1.246195
-936.735119	-15.084472	1.251200
-940.123394	-16.062633	1.256205
-943.889051	-25.037988	1.261210
-947.602392	-24.171311	1.266214
-951.558196	-22.467986	1.271219
-955.634662	-9.523131	1.276224
-959.297218	-14.421528	1.281229
-963.197461	-12.290288	1.286234
-966.911898	-18.642086	1.291238
-970.416800	-18.294368	1.296243
-974.142257	-13.713879	1.301248
-977.739937	-23.521795	1.306253
-982.099484	-23.715412	1.311258
-985.431196	-13.533943	1.316262
-989.078462	-23.228264	1.321267
-993.304977	-14.915700	1.326272
-996.918947	-12.599974	1.331277
-1000.601685	-20.402728	1.336282
-1004.364177	-16.800205	1.341286
-1008.235442	-16.261382	1.346291
-1012.262746	-8.038986	1.351296
-1015.691456	-22.580671	1.356301
-1019.391618	-12.885806	1.361306
-1023.063141	-15.977206	1.366310
-1026.899725	-11.101341	1.371315
-1030.825276	-14.912126	1.376320
-1034.097993	-16.671812	1.381325
-1038.401655	3.701652	1.386330
-1041.809553	-9.630758	1.391334
-1045.428643	-16.909078	1.396339
-1049.329778	-5.702963	1.401344
-1052.972334	-13.614554	1.406349
-1057.295754	-9.792923	1.411354
-1060.947831	-9.011555	1.416358
-1064.459344	-14.126313	1.421363
-1068.337763	-14.529184	1.426368
-1071.920840	-15.567446	1.431373
-1075.856580	-16.396336	1.436378
-1079.446301	-13.125658	1.441382
-1082.949500	-13.008259	1.446387
-1087.334910	-14.693942	1.451392
-1090.826941	-15.341497	1.456397
-1094.933379	-10.956895	1.461402
-1098.607457	-11.673079	1.466406
-1101.675495	-21.522947	1.471411
-1105.792464	-7.939068	1.476416
-1109.782929	-22.783357	1.481421
-1113.677154	-11.699667	1.486426
-1117.571542	-17.216672	1.491430
-1121.176514	-12.131728	1.496435
-1124.659779	-20.973774	1.501440
-1127.906023	-27.477468	1.506445
-1132.146596	-21.158668	1.511450
-1135.990818	-20.303867	1.516454
-1139.758657	-9.710247	1.521459
-1143.765872	2.479582	1.526464
-1147.332960	-12.194286	1.531469
-1151.226794	-4.789308	1.536474
-1154.282196	-17.217646	1.541478
-1158.350678	-12.436920	1.546483
-1162.220267	-10.838490	1.551488
-1166.040323	-16.001483	1.556493
-1170.004271	-7.278078	1.561498
-1173.650666	-19.821538	1.566502
-1177.051385	-20.163480	1.571507
-1181.672427	-12.443417	1.576512
-1185.011516	-21.929701	1.581517
-1188.763234	-9.192541	1.586522
-1192.348154	-15.553652	1.591526
-1195.859825	-19.665322	1.596531
-1200.135965	-17.949739	1.601536
-1203.658431	-5.370654	1.606541
-1207.658641	-14.046277	1.611546
-1211.300376	-19.811688	1.616550
-1214.806318	-8.689057	1.621555
-1218.904016	-14.986989	1.626560
-1222.304151	-21.628332	1.631565
-1226.399372	-28.871152	1.636570
-1229.979350	-4.600210	1.641574
-1233.729033	-15.982273	1.646579
-1237.652545	-17.847235	1.651584
-1240.922328	-23.093430	1.656589
-1244.823596	-21.852462	1.661594
-1248.667154	-19.143248	1.666598
-1252.518297	-26.636376	1.671603
-1256.864157	-18.403598	1.676608
-1260.487458	-21.951723	1.681613
-1264.282312	-13.311997	1.686618
-1267.311184	-25.246135	1.691622
-1270.764846	-27.749159	1.696627
-1274.732244	-25.737533	1.701632
-1278.728919	-25.346908	1.706637
-1282.870897	-22.091603	1.711642
-1286.744444	-21.966654	1.716646
-1290.406210	-30.297353	1.721651
-1294.099333	-21.325392	1.726656
-1297.529258	-20.997067	1.731661
-1301.684857	-25.305096	1.736666
-1305.087817	-26.638304	1.741670
-1309.027181	-25.345403	1.746675
-1313.003477	-14.062204	1.751680
-1316.722591	-27.850492	1.756685
-1320.297545	-14.532787	1.761690
-1323.626860	-25.858982	1.766694
-1327.312079	-18.856096	1.771699
-1331.422608	-19.486275	1.776704
-1335.168593	-22.079591	1.781709
-1339.102050	-19.778424	1.786714
-1343.052271	-12.531259	1.791718
-1346.706717	-5.128023	1.796723
-1350.834369	-17.693479	1.801728
-1354.003618	-27.427439	1.806733
-1357.653382	-16.910740	1.811738
-1361.279800	-23.391074	1.816742
-1365.474774	-20.633295	1.821747
-1369.362299	-7.538264	1.826752
-1373.157166	-21.735340	1.831757
-1376.944520	-21.641384	1.836762
-1380.409758	-28.658375	1.841766
-1384.128332	-25.604707	1.846771
-1387.876113	-20.616340	1.851776
-1391.676306	-27.089299	1.856781
-1395.540335	-11.924487	1.861786
-1399.795478	-8.485290	1.866790
-1403.203573	-22.206542	1.871795
-1407.010114	-18.342463	1.876800
-1410.385833	-22.552826	1.881805
-1414.474004	-17.654983	1.886810
-1417.837230	-28.348027	1.891814
-1421.573137	-24.015885	1.896819
-1425.756652	-22.153885	1.901824
-1429.275897	-20.494424	1.906829
-1433.250583	-14.269699	1.911834
-1437.152384	-10.279939	1.916838
-1440.323392	-20.037147	1.921843
-1444.085680	-12.313752	1.926848
-1447.824672	-19.084975	1.931853
-1451.747900	-8.622105	1.936858
-1455.740472	-23.940019	1.941862
-1459.583003	-17.674918	1.946867
-1463.761614	-11.572013	1.951872
-1467.109502	-21.614640	1.956877
-1470.635930	-8.487400	1.961882
-1474.678543	-10.134204	1.966886
-1478.206507	-16.185454	1.971891
-1482.173416	-12.063779	1.976896
-1485.757871	-17.106272	1.981901
-1489.845041	-0.216808	1.986906
-1493.456068	-5.899953	1.991910
-1496.540140	-33.577247	1.996915
-1500.606673	-14.103298	2.006912
-1501.804309	-18.357314	2.016909
-1499.690643	-15.689563	2.026906
-1496.662474	-17.742133	2.036902
-1494.525266	-23.891169	2.046899
-1492.878564	-9.419508	2.056896
-1490.820286	-19.758746	2.066893
-1488.706195	-11.375690	2.076890
-1486.681495	-25.388216	2.086886
-1484.873884	-21.359433	2.096883
-1483.189331	-13.027577	2.106880
-1481.196379	-18.881943	2.116877
-1479.500531	-11.797587	2.126874
-1477.372419	-18.287760	2.136870
-1475.447351	-14.674063	2.146867
-1473.319851	-20.129999	2.156864
-1471.389820	-8.147717	2.166861
-1470.120311	-22.988176	2.176858
-1468.002612	-18.314350	2.186854
-1466.089328	-22.131885	2.196851
-1464.225150	-17.101692	2.206848
-1462.120528	-13.110976	2.216845
-1460.544120	-12.951171	2.226842
-1458.340617	-17.764052	2.236838
-1456.649200	-11.989397	2.246835
-1454.941774	-14.640361	2.256832
-1452.750355	-21.644295	2.266829
-1450.933856	-9.670654	2.276826
-1448.964027	-21.004568	2.286822
-1447.039023	-9.327751	2.296819
-1445.559841	-17.079674	2.306816
-1443.347470	-15.480754	2.316813
-1441.402707	-15.381498	2.326810
-1439.596086	-19.775574	2.336806
-1437.852007	-19.282629	2.346803
-1435.906775	-19.762875	2.356800
-1434.219547	-19.322398	2.366797
-1431.868618	-25.642958	2.376794
-1430.175813	-25.062857	2.386790
-1428.194993	-30.675251	2.396787
-1426.712012	-24.398290	2.406784
-1424.523206	-16.960225	2.416781
-1422.758912	-20.035503	2.426778
-1420.674414	-22.146862	2.436774
-1418.814845	-22.453915	2.446771
-1417.262534	-16.538545	2.456768
-1415.508346	-23.589272	2.466765
-1413.299738	-19.114672	2.476762
-1411.191956	-31.954738	2.486758
-1409.575746	-25.484376	2.496755
-1407.636162	-22.806034	2.506752
-1405.725907	-25.473648	2.516749
-1404.111879	-19.233439	2.526746
-1401.790316	-14.221162	2.536742
-1400.463116	-14.509275	2.546739
-1398.263893	-18.498846	2.556736
-1396.069037	-18.240660	2.566733
-1394.458428	-23.645347	2.576730
-1392.856323	-18.563660	2.586726
-1390.870398	-18.846714	2.596723
-1388.818765	-20.180735	2.606720
-1387.089121	-21.033761	2.616717
-1385.126555	-24.680715	2.626714
-1383.040749	-26.593316	2.636710
-1381.372582	-13.190708	2.646707
-1379.643514	-21.522559	2.656704
-1377.452500	-21.020601	2.666701
-1375.764548	-24.107304	2.676698
-1373.799160	-23.247139	2.686694
-1372.120422	-18.378217	2.696691
-1370.225354	-23.945262	2.706688
-1368.364220	-15.741048	2.716685
-1366.491987	-20.663431	2.726682
-1364.453900	-22.742049	2.736678
-1362.189099	-21.775082	2.746675
-1360.673126	-30.233842	2.756672
-1358.976650	-26.435041	2.766669
-1356.966668	-22.217512	2.776666
-1354.915812	-20.302145	2.786662
-1353.087517	-19.137405	2.796659
-1351.549757	-26.391844	2.806656
-1349.419506	-16.964473	2.816653
-1347.333429	-28.099038	2.826650
-1345.857054	-23.706085	2.836646
-1344.189905	-28.666666	2.846643
-1341.775629	-22.573461	2.856640
-1340.074913	-26.022156	2.866637
-1338.091146	-18.096476	2.876634
-1336.345202	-25.543694	2.886630
-1334.337213	-21.395295	2.896627
-1332.591957	-19.206793	2.906624
-1330.869910	-19.515444	2.916621
-1328.801510	-16.769237	2.926618
-1326.828088	-23.297671	2.936614
-1325.107355	-15.413550	2.946611
-1322.943994	-14.108223	2.956608
-1321.612994	-14.003770	2.966605
-1319.490908	-18.175118	2.976602
-1317.251106	-16.998856	2.986598
-1315.691038	-16.026396	2.996595
-1313.646202	-27.058026	3.006592
-1311.915251	-11.267160	3.016589
-1309.959345	-20.039457	3.026586
-1308.297407	-21.235245	3.036582
-1306.118365	-12.833984	3.046579
-1304.397086	-15.068668	3.056576
-1302.587354	-21.133545	3.066573
-1300.582776	-18.280789	3.076570
-1298.591151	-27.380872	3.086566
-1296.998014	-17.766431	3.096563
-1295.172178	-23.739150	3.106560
-1293.227334	-12.917932	3.116557
-1291.252439	-18.385599	3.126554
-1289.250719	-24.304367	3.136550
-1287.449087	-17.762540	3.146547
-1285.537545	-14.692787	3.156544
-1283.949240	-18.183449	3.166541
-1281.901414	-7.403959	3.176538
-1280.151647	-20.660283	3.186534
-1278.034994	-26.471129	3.196531
-1276.181156	-11.183021	3.206528
-1274.055297	-18.673640	3.216525
-1272.560625	-27.289984	3.226522
-1270.736297	-19.482396	3.236518
-1268.591381	-26.503986	3.246515
-1266.886109	-21.945522	3.256512
-1265.017280	-19.382038	3.266509
-1262.922947	-15.318437	3.276506
-1261.031381	-17.911899	3.286502
-1259.369461	-16.867286	3.296499
-1257.796221	-15.276413	3.306496
-1255.448191	-16.979837	3.316493
-1253.491234	-17.476015	3.326490
-1251.805529	-18.244547	3.336486
-1250.031304	-24.107928	3.346483
-1248.231302	-22.745958	3.356480
-1246.512214	-7.054173	3.366477
-1244.306654	-14.055456	3.376474
-1242.117792	-17.602732	3.386470
-1240.492046	-13.694628	3.396467
-1239.039223	-14.274313	3.406464
-1236.735413	-8.073313	3.416461
-1235.094606	-12.273348	3.426458
-1232.907880	-25.725874	3.436454
-1230.991582	-10.327725	3.446451
-1229.423097	-20.458912	3.456448
-1227.211395	-14.397890	3.466445
-1225.585942	-23.137764	3.476442
-1223.807972	-10.982499	3.486438
-1221.962782	-30.038897	3.496435
-1220.026352	-14.457662	3.506432
-1218.304982	-13.798295	3.516429
-1215.984737	-13.654734	3.526426
-1214.173438	-12.836084	3.536422
-1212.460737	-9.874964	3.546419
-1210.531177	-18.957159	3.556416
-1208.651881	-16.355831	3.566413
-1206.694808	-17.125127	3.576410
-1205.036569	-26.441771	3.586406
-1202.990867	-12.894172	3.596403
-1201.296877	-16.652726	3.606400
-1199.259838	-10.581092	3.616397
-1197.454204	-23.939453	3.626394
-1195.557998	-15.004959	3.636390
-1193.563109	-22.843999	3.646387
-1191.773177	-19.590509	3.656384
-1190.146550	-22.103627	3.666381
-1187.930016	-18.646837	3.676378
-1186.113092	-22.077708	3.686374
-1184.328511	-15.424124	3.696371
-1182.326285	-18.278371	3.706368
-1180.568667	-20.610353	3.716365
-1178.543889	-21.014696	3.726362
-1176.746911	-24.454999	3.736358
-1174.786252	-27.462049	3.746355
-1173.086904	-21.708966	3.756352
-1171.355754	-19.052325	3.766349
-1169.369188	-20.997804	3.776346
-1167.173760	-27.621630	3.786342
-1165.532625	-23.619626	3.796339
-1163.615819	-13.494799	3.806336
-1161.548428	-23.246333	3.816333
-1159.870497	-13.995848	3.826330
-1158.251093	-12.238620	3.836326
-1156.047822	-17.051192	3.846323
-1154.040421	-18.531078	3.856320
-1152.450704	-22.830243	3.866317
-1150.844151	-16.069205	3.876314
-1148.591714	-19.667618	3.886310
-1146.473450	-18.432272	3.896307
-1144.832664	-17.142634	3.906304
-1142.980705	-9.367768	3.916301
-1141.062607	-25.031820	3.926298
-1139.448717	-20.638622	3.936294
-1137.177754	-17.889913	3.946291
-1135.452383	-17.898973	3.956288
-1133.788637	-18.289723	3.966285
-1131.718486	-15.638344	3.976282
-1129.761597	-22.819196	3.986278
-1128.025306	-18.510305	3.996275
-1125.916223	-16.233018	4.006272
-1124.397779	-20.410245	4.016269
-1122.320932	-22.796414	4.026266
-1120.467956	-22.145399	4.036262
-1118.772701	-24.899959	4.046259
-1116.776112	-18.832830	4.056256
-1114.922868	-18.462887	4.066253
-1112.865601	-18.962365	4.076250
-1110.846287	-22.817109	4.086246
-1109.204546	-14.951748	4.096243
-1107.298870	-26.846685	4.106240
-1105.629366	-14.680279	4.116237
-1103.390700	-22.978219	4.126234
-1101.763260	-26.190832	4.136230
-1099.740380	-16.902333	4.146227
-1097.992597	-25.713800	4.156224
-1096.283971	-26.334319	4.166221
-1094.297431	-16.678447	4.176218
-1091.949738	-30.245023	4.186214
-1090.641046	-16.950435	4.196211
-1088.582957	-25.397882	4.206208
-1086.555432	-26.476748	4.216205
-1084.734353	-22.994487	4.226202
-1082.981355	-15.020596	4.236198
-1081.018181	-20.817778	4.246195
-1079.071882	-18.061282	4.256192
-1077.453702	-22.604935	4.266189
-1075.498609	-16.027481	4.276186
-1073.479392	-23.695069	4.286182
-1071.584958	-17.733127	4.296179
-1069.895362	-19.436822	4.306176
-1068.093241	-13.673251	4.316173
-1066.101010	-16.832098	4.326170
-1064.141618	-20.154625	4.336166
-1062.284476	-17.191234	4.346163
-1060.185427	-16.304816	4.356160
-1058.795254	-18.705818	4.366157
-1056.653803	-22.254815	4.376154
-1054.831185	-13.130011	4.386150
-1052.820790	-25.207442	4.396147
-1050.882975	-21.117027	4.406144
-1048.929442	-20.076279	4.416141
-1047.627327	-19.286570	4.426138
-1045.442537	-19.953219	4.436134
-1043.594832	-19.334455	4.446131
-1041.649870	-17.324502	4.456128
-1039.660430	-22.928498	4.466125
-1038.203135	-18.195988	4.476122
-1035.809664	-28.828466	4.486118
-1033.965854	-17.217212	4.496115
-1032.311955	-23.796934	4.506112
-1030.380763	-14.065835	4.516109
-1028.380765	-21.986087	4.526106
-1027.007630	-19.980969	4.536102
-1024.665655	-19.314940	4.546099
-1022.813556	-17.574309	4.556096
-1021.119736	-16.146232	4.566093
-1019.214156	-22.207292	4.576090
-1017.299452	-18.885202	4.586086
-1015.345027	-22.058485	4.596083
-1013.677271	-12.684681	4.606080
-1011.674058	-28.730128	4.616077
-1009.615923	-14.554364	4.626074
-1007.649374	-20.063102	4.636070
-1006.170131	-27.290614	4.646067
-1004.212301	-23.165468	4.656064
-1002.103204	-21.393298	4.666061
-1000.279800	-22.003685	4.676058
-998.444979	-27.677647	4.686054
-996.741987	-27.452515	4.696051
-994.932753	-23.546737	4.706048
-992.805182	-21.480691	4.716045
-990.915564	-23.435778	4.726042
-989.185660	-28.467735	4.736038
-986.990143	-25.547348	4.746035
-985.522876	-26.454426	4.756032
-983.695798	-15.192529	4.766029
-981.606464	-14.659724	4.776026
-979.649475	-22.091514	4.786022
-977.605276	-16.486575	4.796019
-975.873031	-17.469180	4.806016
-974.316769	-27.402489	4.816013
-972.102735	-32.630270	4.826010
-970.552409	-17.643835	4.836006
-968.603069	-20.544707	4.846003
-966.807457	-18.555014	4.856000
-964.828183	-20.374429	4.865997
-962.504384	-23.336757	4.875994
-960.845713	-22.302461	4.885990
-959.073034	-14.672642	4.895987
-957.251530	-13.894892	4.905984
-955.508015	-15.668704	4.915981
-953.385766	-11.842943	4.925978
-951.415634	-20.225696	4.935974
-949.430546	-20.727698	4.945971
-947.896801	-28.985401	4.955968
-946.114765	-15.736406	4.965965
-943.954060	-12.600422	4.975962
-942.211964	-15.605492	4.985958
-940.471075	-19.183485	4.995955
-938.490811	-20.652535	5.005952
-936.462641	-23.902278	5.015949
-934.777439	-18.625131	5.025946
-932.481059	-21.901971	5.035942
-931.177999	-21.928607	5.045939
-929.404043	-22.916269	5.055936
-927.159274	-17.387563	5.065933
-925.250492	-13.939718	5.075930
-923.268705	-29.552234	5.085926
-921.512500	-14.456581	5.095923
-919.547119	-18.545687	5.105920
-918.092406	-16.319879	5.115917
-916.278035	-19.693304	5.125914
-914.207806	-19.015288	5.135910
-911.728722	-15.459688	5.145907
-910.530572	-14.833265	5.155904
-908.442903	-22.131171	5.165901
-906.697008	-10.622551	5.175898
-904.512716	-14.129323	5.185894
-902.619275	-18.642673	5.195891
-901.067460	-18.027008	5.205888
-899.229784	-17.289691	5.215885
-897.016238	-22.212614	5.225882
-895.204417	-21.262754	5.235878
-893.169967	-15.883530	5.245875
-891.479901	-19.533884	5.255872
-889.754563	-27.776402	5.265869
-887.995567	-10.093442	5.275866
-885.700240	-16.581433	5.285862
-884.246558	-23.184309	5.295859
-882.068293	-15.748737	5.305856
-880.330165	-12.661964	5.315853
-878.485520	-23.244447	5.325850
-876.436789	-18.342723	5.335846
-874.955119	-13.484533	5.345843
-872.572354	-15.388908	5.355840
-870.794290	-14.024712	5.365837
-869.143573	-17.411409	5.375834
-866.961963	-19.529917	5.385830
-865.075225	-14.251778	5.395827
-863.384651	-20.542015	5.405824
-861.717570	-19.280061	5.415821
-859.871563	-19.308203	5.425818
-857.629062	-13.341723	5.435814
-855.860265	-18.368759	5.445811
-854.170939	-17.699262	5.455808
-852.000163	-15.216862	5.465805
-850.305927	-18.245792	5.475802
-848.173300	-16.459874	5.485798
-846.740249	-15.564677	5.495795
-844.830582	-20.150045	5.505792
-842.417476	-17.107997	5.515789
-840.618343	-15.276651	5.525786
-839.111639	-20.847524	5.535782
-837.329430	-17.721979	5.545779
-835.409432	-15.767855	5.555776
-833.377284	-18.863424	5.565773
-831.525279	-16.360043	5.575770
-829.595349	-23.215854	5.585766
-827.636655	-18.662824	5.595763
-825.828950	-9.963298	5.605760
-824.172119	-15.616581	5.615757
-822.233125	-18.940390	5.625754
-819.912714	-17.662854	5.635750
-818.268722	-17.178703	5.645747
-816.707457	-15.871380	5.655744
-814.656307	-17.994248	5.665741
-812.926579	-17.866407	5.675738
-810.803293	-13.180208	5.685734
-809.009706	-14.474056	5.695731
-807.318413	-18.276118	5.705728
-805.294551	-14.238713	5.715725
-803.196706	-12.333516	5.725722
-801.454488	-19.899779	5.735718
-799.559252	-17.460121	5.745715
-797.521633	-20.643370	5.755712
-796.271027	-16.019753	5.765709
-793.938762	-14.879866	5.775706
-791.902754	-20.369541	5.785702
-790.085755	-20.088276	5.795699
-788.505482	-17.740359	5.805696
-786.344816	-14.103726	5.815693
-784.666522	-18.514707	5.825690
-782.966711	-13.964463	5.835686
-780.960370	-16.987973	5.845683
-778.896020	-22.352702	5.855680
-777.071448	-22.268414	5.865677
-774.957449	-16.033433	5.875674
-773.184010	-22.674728	5.885670
-771.501644	-23.218188	5.895667
-769.613046	-16.146702	5.905664
-767.981626	-18.832399	5.915661
-765.730887	-20.423480	5.925658
-763.874839	-23.763983	5.935654
-761.914070	-17.141365	5.945651
-760.379896	-17.713233	5.955648
-758.513164	-20.018141	5.965645
-756.572173	-21.176047	5.975642
-754.243736	-19.233456	5.985638
-752.550894	-20.607470	5.995635
-750.847423	-22.167905	6.005632
-748.909600	-23.235304	6.015629
-747.163326	-21.153874	6.025626
-745.224163	-20.500547	6.035622
-743.176735	-14.005437	6.045619
-741.351629	-11.503998	6.055616
-739.850519	-22.694599	6.065613
-737.744158	-13.717491	6.075610
-735.809414	-18.368360	6.085606
-733.443059	-19.532655	6.095603
-732.321786	-24.495585	6.105600
-730.369527	-15.234912	6.115597
-728.333096	-22.262396	6.125594
-726.396695	-14.541712	6.135590
-724.679057	-28.480937	6.145587
-722.593930	-19.942500	6.155584
-720.608405	-20.529637	6.165581
-718.982529	-19.968316	6.175578
-717.074939	-23.372281	6.185574
-714.985999	-15.532291	6.195571
-713.230100	-19.991939	6.205568
-711.513060	-27.868305	6.215565
-709.784360	-16.710431	6.225562
-707.678069	-22.754392	6.235558
-706.025462	-17.222400	6.245555
-704.116852	-16.987286	6.255552
-702.111438	-21.603636	6.265549
-699.874603	-11.355846	6.275546
-698.085102	-16.297666	6.285542
-696.320330	-20.401902	6.295539
-694.477604	-16.684375	6.305536
-692.599918	-19.447270	6.315533
-690.688882	-17.692106	6.325530
-689.247082	-15.121478	6.335526
-687.030647	-17.625891	6.345523
-684.957858	-12.677308	6.355520
-683.212110	-17.018481	6.365517
-681.488258	-13.820332	6.375514
-679.924001	-18.154604	6.385510
-677.519809	-16.388241	6.395507
-675.762662	-19.509204	6.405504
-673.909149	-19.457880	6.415501
-671.984212	-27.335864	6.425498
-670.081176	-20.325017	6.435494
-668.020745	-26.795797	6.445491
-666.630561	-12.871339	6.455488
-664.536354	-25.197131	6.465485
-662.650831	-17.157229	6.475482
-660.889289	-20.512553	6.485478
-658.531962	-18.105566	6.495475
-656.955144	-16.590635	6.505472
-655.315767	-14.463634	6.515469
-653.171053	-17.444418	6.525466
-651.705786	-20.438204	6.535462
-649.423075	-15.988892	6.545459
-647.299496	-21.034579	6.555456
-645.758267	-16.741503	6.565453
-644.043064	-16.786469	6.575450
-642.185656	-15.820013	6.585446
-640.081621	-16.749683	6.595443
-638.054874	-22.809296	6.605440
-636.262776	-16.915880	6.615437
-634.496602	-23.068057	6.625434
-632.726917	-28.387162	6.635430
-630.724928	-21.215261	6.645427
-628.906278	-23.600803	6.655424
-626.905798	-16.496545	6.665421
-625.282644	-9.991951	6.675418
-623.155276	-28.728381	6.685414
-621.351296	-20.951714	6.695411
-619.362194	-27.003717	6.705408
-617.528486	-16.489343	6.715405
-615.929170	-15.268485	6.725402
-614.009917	-21.768770	6.735398
-611.798646	-24.243869	6.745395
-609.981723	-18.709638	6.755392
-608.176282	-18.978982	6.765389
-606.427867	-23.320526	6.775386
-604.523521	-19.249637	6.785382
-602.709145	-14.591250	6.795379
-600.815615	-25.850789	6.805376
-598.936085	-21.973287	6.815373
-596.792432	-25.575916	6.825370
-595.122262	-13.882836	6.835366
-593.057533	-21.358391	6.845363
-591.373071	-20.234799	6.855360
-589.600111	-11.259537	6.865357
-587.474313	-21.825172	6.875354
-585.529041	-20.612199	6.885350
-583.947147	-16.852912	6.895347
-582.188119	-14.749710	6.905344
-579.805581	-22.637582	6.915341
-578.035177	-19.333116	6.925338
-576.115703	-19.188050	6.935334
-574.607511	-14.916487	6.945331
-572.789849	-24.376635	6.955328
-570.766128	-19.336431	6.965325
-568.532315	-15.678121	6.975322
-567.084143	-23.107260	6.985318
-565.208095	-14.421588	6.995315
-563.124660	-16.472038	7.005312
-561.229584	-23.067888	7.015309
-559.592679	-16.548077	7.025306
-557.563877	-20.111801	7.035302
-555.491875	-21.781494	7.045299
-553.697932	-21.813712	7.055296
-552.006180	-18.709805	7.065293
-550.280346	-14.592986	7.075290
-548.433358	-17.791365	7.085286
-546.216458	-24.624917	7.095283
-544.260620	-21.334258	7.105280
-542.662857	-16.366502	7.115277
-540.997184	-21.253696	7.125274
-538.583335	-20.349203	7.135270
-536.573813	-26.014430	7.145267
-535.298956	-11.394126	7.155264
-533.263657	-19.321221	7.165261
-531.312469	-17.251834	7.175258
-529.261287	-17.326703	7.185254
-527.682446	-23.793072	7.195251
-525.658277	-15.898345	7.205248
-523.745445	-19.181429	7.215245
-521.881424	-14.560905	7.225242
-520.030807	-18.964502	7.235238
-518.272288	-20.873019	7.245235
-516.095419	-17.671322	7.255232
-514.353597	-24.801570	7.265229
-512.465146	-28.833858	7.275226
-511.065027	-17.577545	7.285222
-508.786440	-16.520373	7.295219
-506.897042	-16.967250	7.305216
-504.871327	-18.258478	7.315213
-503.075647	-8.828905	7.325210
-501.231936	-14.598669	7.335206
-499.365206	-17.255462	7.345203
-497.452154	-20.278051	7.355200
-495.938697	-15.227326	7.365197
-493.759536	-16.145184	7.375194
-491.605548	-20.489853	7.385190
-489.788846	-15.694387	7.395187
-488.387686	-12.982938	7.405184
-486.292090	-18.093491	7.415181
-484.352128	-12.618277	7.425178
-482.331270	-20.702489	7.435174
-480.958166	-19.435937	7.445171
-478.791608	-16.788311	7.455168
-476.818371	-19.927858	7.465165
-474.911758	-20.030113	7.475162
-472.901863	-21.074067	7.485158
-471.288171	-25.417683	7.495155
-469.238760	-26.248485	7.505152
-467.421417	-24.389759	7.515149
-466.045349	-17.575604	7.525146
-463.682510	-24.178199	7.535142
-461.732642	-27.070858	7.545139
-459.605134	-28.441459	7.555136
-458.451566	-24.809455	7.565133
-456.295203	-20.832371	7.575130
-454.370262	-18.850301	7.585126
-452.487810	-21.026443	7.595123
-450.755887	-16.747898	7.605120
-448.666437	-15.287853	7.615117
-446.758920	-23.472350	7.625114
-444.823150	-10.738470	7.635110
-442.873371	-17.958724	7.645107
-441.554455	-28.251708	7.655104
-439.396372	-9.304248	7.665101
-437.548763	-14.694087	7.675098
-435.619695	-17.313423	7.685094
-433.577654	-23.260062	7.695091
-431.927206	-20.080001	7.705088
-430.061298	-27.310530	7.715085
-428.007336	-15.665971	7.725082
-426.066833	-15.795703	7.735078
-424.439554	-21.459799	7.745075
-422.476986	-16.967028	7.755072
-420.564694	-29.347265	7.765069
-418.702268	-16.353773	7.775066
-416.581269	-28.830490	7.785062
-414.936037	-21.089873	7.795059
-413.149376	-30.376025	7.805056
-411.348137	-10.263201	7.815053
-409.190881	-23.588812	7.825050
-407.433465	-20.296349	7.835046
-405.596306	-21.408973	7.845043
-403.707583	-23.426614	7.855040
-401.587415	-17.118055	7.865037
-399.911998	-16.840722	7.875034
-398.116582	-13.349067	7.885030
-396.156543	-19.115227	7.895027
-394.239541	-27.015428	7.905024
-392.656125	-17.068744	7.915021
-390.533347	-21.788845	7.925018
-388.539090	-16.739035	7.935014
-386.860760	-9.589428	7.945011
-385.223935	-14.263509	7.955008
-383.353404	-17.670776	7.965005
-381.267816	-9.921498	7.975002
-379.143510	-22.798169	7.984998
-377.050099	-8.417392	7.994995
-375.456377	-22.341376	8.004992
-373.875572	-12.987905	8.014989
-371.842948	-26.464100	8.024986
-369.976268	-11.488206	8.034982
-368.061191	-14.656274	8.044979
-366.222734	-23.008097	8.054976
-364.179294	-18.376619	8.064973
-362.287859	-17.454846	8.074970
-360.697219	-23.982998	8.084966
-358.622372	-23.911508	8.094963
-356.843371	-22.861259	8.104960
-354.961814	-15.387259	8.114957
-353.262298	-21.290199	8.124954
-351.080350	-19.080674	8.134950
-349.067427	-21.773326	8.144947
-347.401279	-18.671495	8.154944
-345.386117	-19.766706	8.164941
-343.772370	-19.316867	8.174938
-341.643820	-20.531225	8.184934
-339.863174	-27.746500	8.194931
-338.146954	-20.658170	8.204928
-335.951218	-19.339724	8.214925
-334.450003	-24.716811	8.224922
-332.729917	-17.248590	8.234918
-330.460448	-22.086792	8.244915
-328.597409	-23.970810	8.254912
-326.863513	-14.016520	8.264909
-325.083107	-19.333973	8.274906
-322.673536	-22.944087	8.284902
-320.998968	-17.371102	8.294899
-319.356591	-16.930553	8.304896
-317.507177	-11.412318	8.314893
-315.538380	-22.461067	8.324890
-313.555587	-19.117675	8.334886
-311.652284	-19.113490	8.344883
-309.810106	-15.949738	8.354880
-307.831674	-18.125304	8.364877
-306.391205	-16.788882	8.374874
-304.563706	-12.113401	8.384870
-302.319318	-18.660628	8.394867
-300.579787	-22.836345	8.404864
-298.573183	-11.083047	8.414861
-296.667273	-11.014532	8.424858
-294.726822	-17.870053	8.434854
-293.078510	-11.201868	8.444851
-291.245036	-12.839575	8.454848
-289.088939	-14.012499	8.464845
-287.192862	-15.999650	8.474842
-285.563878	-14.233862	8.484838
-283.542100	-16.531585	8.494835
-281.655076	-15.714826	8.504832
-280.000499	-25.642928	8.514829
-278.331525	-16.882899	8.524826
-276.081070	-15.991527	8.534822
-274.141999	-23.967794	8.544819
-272.297765	-18.200817	8.554816
-270.331483	-20.718603	8.564813
-268.670702	-21.431939	8.574810
-266.732710	-17.794004	8.584807
-264.979594	-18.526813	8.594803
-262.977810	-20.702913	8.604800
-260.957146	-7.287712	8.614797
-259.293629	-11.962818	8.624794
-257.374840	-13.358344	8.634791
-255.435758	-13.568233	8.644787
-253.697333	-17.565332	8.654784
-251.871231	-7.186773	8.664781
-249.901520	-3.391261	8.674778
-247.873635	-10.417014	8.684775
-246.052443	-4.739484	8.694771
-244.118081	-9.806739	8.704768
-242.212704	-8.939197	8.714765
-240.617484	-9.127344	8.724762
-238.590303	-11.185907	8.734759
-236.677366	-17.970683	8.744755
-234.795098	-13.817014	8.754752
-232.590611	-15.730199	8.764749
-231.222350	-7.989433	8.774746
-229.597411	-13.744612	8.784743
-227.242649	-17.487984	8.794739
-225.728099	-14.167667	8.804736
-223.510537	-11.122178	8.814733
-221.640852	-13.376629	8.824730
-219.976992	-17.807040	8.834727
-217.874331	-13.506966	8.844723
-215.808864	-16.597874	8.854720
-214.282512	-18.688581	8.864717
-212.501643	-7.636492	8.874714
-210.398186	-21.535966	8.884711
-208.622897	-12.990204	8.894707
-206.408401	-14.669713	8.904704
-204.643014	-20.486762	8.914701
-203.005140	-13.434761	8.924698
-201.189594	-19.103507	8.934695
-198.789515	-23.237744	8.944691
-197.263419	-27.091975	8.954688
-195.517738	-18.814621	8.964685
-193.468147	-23.080800	8.974682
-191.692253	-22.462537	8.984679
-189.709594	-35.666955	8.994675
-187.898958	-20.116724	9.004672
-186.184349	-27.154001	9.014669
-184.398419	-18.273625	9.024666
-181.950879	-25.124730	9.034663
-180.192674	-26.917699	9.044659
-178.412440	-28.917855	9.054656
-176.680977	-20.802418	9.064653
-174.758935	-19.135425	9.074650
-172.925456	-21.922449	9.084647
-171.208381	-31.168922	9.094643
-169.533102	-27.375305	9.104640
-167.246031	-27.544347	9.114637
-165.553979	-35.585314	9.124634
-163.669484	-23.419276	9.134631
-161.480871	-36.269723	9.144627
-159.656104	-28.028649	9.154624
-157.689971	-31.411531	9.164621
-156.250089	-24.195281	9.174618
-154.070787	-27.659544	9.184615
-152.089842	-26.352439	9.194611
-150.467977	-24.724362	9.204608
-148.567094	-22.324542	9.214605
-146.788428	-21.291450	9.224602
-144.625240	-25.878856	9.234599
-143.288072	-26.082599	9.244595
-141.015136	-32.368990	9.254592
-139.363442	-22.938243	9.264589
-137.176994	-26.979913	9.274586
-135.349282	-23.908447	9.284583
-133.378833	-33.274269	9.294579
-131.614669	-30.824202	9.304576
-129.951703	-26.013388	9.314573
-127.846851	-25.273896	9.324570
-126.045891	-26.896818	9.334567
-124.159573	-23.986264	9.344563
-122.176715	-26.113443	9.354560
-120.487636	-21.395204	9.364557
-118.456626	-28.866585	9.374554
-116.737323	-29.350749	9.384551
-114.777079	-14.233239	9.394547
-112.840726	-27.948088	9.404544
-111.080506	-20.328210	9.414541
-109.177249	-23.107375	9.424538
-107.089085	-27.270697	9.434535
-105.242155	-29.344596	9.444531
-103.717799	-28.897700	9.454528
-101.796871	-23.905407	9.464525
-99.694762	-23.230185	9.474522
-97.718875	-25.282026	9.484519
-95.850083	-27.122579	9.494515
-94.160893	-22.053833	9.504512
-92.472324	-19.695876	9.514509
-90.392250	-25.932508	9.524506
-88.344888	-21.854007	9.534503
-86.696665	-24.568780	9.544499
-84.507654	-15.187401	9.554496
-83.141699	-17.542945	9.564493
-81.167169	-19.615083	9.574490
-79.002303	-21.408131	9.584487
-77.165727	-17.016530	9.594483
-75.490434	-17.544167	9.604480
-73.272706	-19.453006	9.614477
-71.627557	-20.905776	9.624474
-69.592817	-15.678994	9.634471
-67.906439	-24.257392	9.644467
-65.994503	-20.806173	9.654464
-64.080897	-22.300189	9.664461
-62.280340	-17.061301	9.674458
-60.461404	-22.435244	9.684455
-58.498407	-27.394825	9.694451
-56.716136	-22.585622	9.704448
-54.937009	-20.347870	9.714445
-52.970271	-21.021455	9.724442
-50.748339	-26.263905	9.734439
-48.905656	-30.520640	9.744435
-47.327655	-26.817196	9.754432
-45.189448	-16.851392	9.764429
-43.371982	-18.408998	9.774426
-41.620958	-16.312005	9.784423
-39.692341	-31.407067	9.794419
-37.959314	-10.567778	9.804416
-35.992796	-20.349730	9.814413
-34.188700	-24.799236	9.824410
-31.982299	-23.224857	9.834407
-30.495610	-22.152993	9.844403
-28.629133	-25.169373	9.854400
-26.687879	-19.806070	9.864397
-24.646105	-18.028589	9.874394
-22.419766	-20.616085	9.884391
-21.066046	-21.880234	9.894387
-19.351421	-18.244351	9.904384
-16.997396	-20.013839	9.914381
-15.359971	-17.289268	9.924378
-13.460191	-20.056754	9.934375
-11.517576	-20.098074	9.944371
-9.497530	-18.219226	9.954368
-7.743248	-16.683222	9.964365
-6.353974	-18.745619	9.974362
-4.652989	2.163565	9.984359
-3.436653	33.605305	9.994355
-2.211661	94.960510	10.004352
-1.221160	165.070352	10.014349
0.000000	239.297694	10.019354
0.560721	287.695419	10.024359
1.173177	333.808045	10.029363
2.081658	376.937449	10.034368
2.648428	390.409869	10.039373
3.282535	413.553622	10.044378
3.134898	442.869471	10.049383
3.410294	448.600183	10.054387
3.331549	485.226618	10.059392
3.947507	486.777874	10.064397
3.655075	498.592948	10.069402
3.809545	514.485554	10.074407
4.131144	522.631035	10.079411
4.287299	531.061523	10.084416
4.469334	528.511111	10.089421
4.601422	543.950019	10.094426
4.216035	544.405800	10.099431
4.585473	529.166166	10.104435
4.547592	541.924654	10.109440
4.468122	550.190896	10.114445
4.760238	567.416159	10.119450
4.876940	577.937630	10.124455
5.285088	576.466010	10.129459
5.200677	584.852905	10.134464
5.039408	561.176315	10.139469
4.830327	564.529122	10.144474
4.683330	585.508090	10.149479
4.977979	587.848601	10.154483
4.979475	585.133019	10.159488
5.067517	594.892699	10.164493
5.071934	597.569659	10.169498
5.088542	603.868399	10.174503
5.465122	593.766689	10.179507
5.133797	610.500112	10.184512
5.219204	599.703698	10.189517
5.660902	597.723693	10.194522
5.273877	604.339123	10.199527
5.545605	608.271237	10.204531
5.511204	608.393497	10.209536
5.700282	606.220405	10.214541
6.057676	610.462120	10.219546
5.912720	623.438027	10.224551
5.810185	608.961126	10.229555
5.561078	616.495974	10.234560
5.710076	612.452757	10.239565
5.461513	628.983771	10.244570
5.463615	636.394982	10.249575
5.922201	651.788232	10.254579
5.946760	659.542792	10.259584
6.098687	662.107927	10.264589
6.159765	664.854706	10.269594
6.077228	676.538675	10.274599
6.320053	661.667595	10.279603
6.076647	678.975261	10.284608
5.852700	681.527817	10.289613
6.231128	672.311983	10.294618
6.147372	667.432269	10.299623
6.408344	677.844070	10.304627
6.088783	687.796561	10.309632
6.285610	686.158372	10.314637
6.042372	689.709040	10.319642
5.915130	696.710416	10.324647
6.261219	714.400319	10.329651
6.242432	726.458927	10.334656
6.598743	716.388750	10.339661
6.733010	724.846496	10.344666
6.679788	717.889825	10.349671
6.960203	716.028570	10.354675
6.851353	712.346569	10.359680
7.234306	723.282981	10.364685
6.929314	723.431059	10.369690
6.844959	715.776050	10.374695
7.220610	723.045720	10.379699
7.179593	734.418768	10.384704
6.746200	748.683408	10.389709
7.211701	756.061761	10.394714
7.649582	762.331218	10.399719
7.722259	758.550865	10.404723
7.389769	742.672360	10.409728
7.345725	750.038951	10.414733
7.446852	747.338984	10.419738
7.235038	738.870104	10.424743
7.612779	734.383521	10.429747
7.484808	771.945760	10.434752
7.787413	767.152614	10.439757
7.734377	753.776248	10.444762
7.628619	757.681886	10.449767
7.627247	758.084302	10.454771
7.848357	774.890639	10.459776
7.706296	779.793959	10.464781
7.779039	779.596360	10.469786
7.688450	794.888133	10.474791
7.724289	784.323412	10.479795
7.735477	791.471484	10.484800
7.763234	791.926023	10.489805
7.624152	798.453106	10.494810
7.650754	790.837128	10.499815
7.945694	797.657671	10.504819
8.213937	819.152625	10.509824
8.198462	822.510878	10.514829
8.254920	817.529901	10.519834
8.137347	812.333840	10.524839
8.577106	818.216674	10.529843
8.271022	822.469670	10.534848
8.571330	826.069284	10.539853
8.689869	826.447843	10.544858
8.383812	831.886687	10.549863
8.594456	817.911546	10.554867
8.071537	831.569238	10.559872
8.088540	828.679251	10.564877
8.405753	833.667021	10.569882
8.182228	849.076249	10.574887
8.808835	857.849771	10.579891
8.477277	865.103013	10.584896
8.830446	864.712451	10.589901
8.863221	858.790655	10.594906
8.700604	866.606722	10.599911
8.929240	858.512209	10.604915
9.105919	862.860095	10.609920
9.310576	873.913370	10.614925
9.526567	867.795191	10.619930
8.866379	869.718784	10.624935
9.395156	872.066151	10.629939
9.334965	878.121797	10.634944
9.148605	876.495825	10.639949
9.385404	870.763828	10.644954
9.221917	876.214639	10.649959
9.242839	873.524289	10.654963
9.142364	898.883318	10.659968
9.517676	900.540817	10.664973
9.915291	905.230361	10.669978
9.539707	912.903807	10.674983
9.843034	900.884975	10.679987
9.621588	910.686351	10.684992
9.954842	907.332745	10.689997
9.912815	905.505553	10.695002
9.605624	906.521298	10.700007
10.251263	907.336170	10.705011
10.060766	903.383295	10.710016
9.941420	907.008869	10.715021
10.107642	912.471756	10.720026
10.086134	920.060341	10.725031
10.064184	913.590593	10.730035
10.133353	906.535462	10.735040
10.347159	913.548773	10.740045
10.394262	921.515918	10.745050
10.575457	915.341768	10.750055
10.398424	915.537244	10.755059
10.052973	918.058761	10.760064
10.471971	919.811795	10.765069
10.493794	914.528806	10.770074
10.531731	917.971601	10.775079
10.393955	915.150440	10.780083
10.523542	915.976667	10.785088
10.395719	918.942859	10.790093
10.318893	919.515008	10.795098
10.475576	913.655426	10.800103
10.814021	930.671884	10.805107
10.675037	951.776258	10.810112
10.991218	948.518406	10.815117
11.100162	951.162988	10.820122
10.732913	958.477162	10.825127
11.002506	961.979208	10.830131
11.050396	955.252298	10.835136
10.912775	957.105162	10.840141
10.898041	960.567407	10.845146
11.090876	950.259796	10.850151
11.358855	943.934597	10.855155
11.030614	955.971795	10.860160
10.970882	958.875094	10.865165
11.068567	960.168457	10.870170
11.289028	973.058002	10.875175
11.067181	960.140457	10.880179
11.281627	973.552930	10.885184
11.839461	987.125107	10.890189
11.714301	986.055484	10.895194
11.340752	996.773731	10.900199
12.189932	988.709472	10.905203
11.990386	993.554224	10.910208
11.621449	975.189701	10.915213
12.069459	967.361331	10.920218
11.916269	962.117281	10.925223
11.594320	952.344365	10.930227
11.695928	972.243454	10.935232
11.721769	981.738929	10.940237
11.942355	983.394311	10.945242
11.903170	989.534962	10.950247
11.898022	987.064791	10.955251
12.050913	989.409058	10.960256
11.928347	997.909509	10.965261
12.261664	990.786971	10.970266
12.321663	995.172433	10.975271
12.369448	991.060100	10.980275
12.257432	999.532062	10.985280
12.449246	988.319419	10.990285
12.482290	993.038761	10.995290
12.286930	995.222537	11.000295
12.380436	991.801499	11.005299
12.291328	1006.071397	11.010304
12.618019	1016.354688	11.015309
12.794752	1025.537541	11.020314
12.859941	1039.245120	11.025319
13.097573	1026.123336	11.030323
12.631576	1033.294026	11.035328
13.023877	1025.182777	11.040333
12.893965	1036.220158	11.045338
12.778081	1037.050855	11.050343
13.154552	1036.968808	11.055347
13.032512	1037.305324	11.060352
12.950548	1033.385564	11.065357
13.316173	1030.097729	11.070362
12.886540	1039.861437	11.075367
13.090637	1044.408432	11.080371
13.167667	1031.583497	11.085376
13.042663	1030.274149	11.090381
13.409742	1034.602754	11.095386
13.004052	1051.050502	11.100391
13.175991	1039.266979	11.105395
13.502305	1035.394057	11.110400
13.071282	1039.898856	11.115405
13.470686	1051.715987	11.120410
13.646102	1061.667049	11.125415
13.691317	1065.132372	11.130419
13.299154	1074.585774	11.135424
13.551716	1074.441491	11.140429
13.713166	1065.047131	11.145434
13.348915	1078.854786	11.150439
13.776283	1075.307934	11.155443
13.693296	1077.847536	11.160448
13.550422	1074.153524	11.165453
13.678801	1073.131761	11.170458
13.549234	1098.375931	11.175463
13.819321	1092.545496	11.180467
14.077695	1105.692465	11.185472
14.171232	1103.452538	11.190477
14.546584	1096.479363	11.195482
14.381863	1111.155665	11.200487
14.294246	1103.524625	11.205491
14.367568	1113.503047	11.210496
13.969118	1105.475309	11.215501
14.159710	1104.710126	11.220506
14.047449	1104.958351	11.225511
14.268339	1107.386408	11.230515
14.301594	1116.697862	11.235520
14.552139	1125.749156	11.240525
14.912707	1121.538009	11.245530
14.825945	1133.478488	11.250535
15.100967	1128.768472	11.255539
14.762745	1117.861050	11.260544
14.925293	1112.943474	11.265549
14.746573	1112.005388	11.270554
14.659820	1104.292208	11.275559
15.100245	1110.427371	11.280563
15.114529	1139.890689	11.285568
15.183679	1129.186362	11.290573
15.280051	1125.107243	11.295578
14.787194	1133.684185	11.300583
14.816619	1121.794017	11.305587
15.009128	1121.807547	11.310592
15.352603	1128.767163	11.315597
15.225753	1127.795570	11.320602
15.402405	1138.334695	11.325607
15.484236	1120.691296	11.330611
15.370186	1131.013433	11.335616
15.433838	1123.728840	11.340621
15.646185	1131.740706	11.345626
15.495909	1128.210287	11.350631
15.358687	1130.679702	11.355635
15.693298	1132.657536	11.360640
15.579144	1133.317650	11.365645
15.617181	1128.019382	11.370650
15.514973	1133.902064	11.375655
15.504837	1145.127004	11.380659
15.723979	1157.572222	11.385664
15.788046	1163.161886	11.390669
15.933180	1162.536417	11.395674
15.912242	1177.852176	11.400679
15.688560	1168.930770	11.405683
16.202911	1162.490484	11.410688
16.317225	1164.372575	11.415693
16.228853	1159.110228	11.420698
15.983272	1176.002513	11.425703
16.226947	1166.008341	11.430707
16.123420	1170.207049	11.435712
16.318586	1173.563323	11.440717
16.463717	1153.303062	11.445722
16.056625	1181.680917	11.450727
16.382618	1169.713442	11.455731
16.264485	1178.856694	11.460736
16.227001	1194.693933	11.465741
16.631672	1192.407517	11.470746
16.664861	1201.818385	11.475751
17.113780	1198.777428	11.480755
16.808838	1200.041994	11.485760
16.869225	1198.933296	11.490765
17.250871	1195.937763	11.495770
16.697886	1207.225686	11.500775
17.231797	1204.297328	11.505779
17.164757	1204.767002	11.510784
17.157112	1187.667655	11.515789
17.206525	1173.725776	11.520794
16.674476	1169.250139	11.525799
16.890712	1198.377007	11.530803
17.267882	1196.025592	11.535808
17.218009	1210.992761	11.540813
17.504942	1200.518574	11.545818
17.086695	1205.284738	11.550823
17.409676	1206.477531	11.555827
17.370321	1214.100656	11.560832
17.483202	1200.970228	11.565837
17.728314	1198.622530	11.570842
17.443523	1218.454280	11.575847
17.798482	1205.567513	11.580851
17.465414	1202.799523	11.585856
17.420592	1207.657513	11.590861
17.768926	1207.264561	11.595866
17.920240	1205.870120	11.600871
17.615132	1206.155415	11.605875
17.513551	1207.403313	11.610880
17.675455	1205.922027	11.615885
17.740363	1194.281609	11.620890
17.288005	1212.678231	11.625895
17.945586	1222.462607	11.630899
18.057731	1226.404577	11.635904
17.998987	1235.170956	11.640909
17.919064	1244.112610	11.645914
18.124505	1241.725500	11.650919
18.120255	1244.031795	11.655923
18.235456	1244.571750	11.660928
17.830265	1239.374103	11.665933
18.196152	1236.936170	11.670938
18.333752	1248.957652	11.675943
18.385341	1243.994652	11.680947
18.576443	1259.651996	11.685952
18.046698	1272.543200	11.690957
18.627169	1260.456210	11.695962
18.625338	1270.145526	11.700967
18.630443	1270.553230	11.705971
18.944013	1263.916265	11.710976
18.768487	1271.632104	11.715981
19.189607	1267.758193	11.720986
19.022299	1278.979921	11.725991
19.054349	1270.478138	11.730995
19.315667	1273.043280	11.736000
19.033248	1274.543960	11.741005
19.141160	1266.488979	11.746010
19.105007	1275.396861	11.751015
19.286417	1270.141905	11.756019
19.147912	1259.819116	11.761024
19.131717	1270.404868	11.766029
19.181560	1261.949138	11.771034
18.969167	1273.968119	11.776039
19.184776	1273.362944	11.781043
19.327438	1276.487917	11.786048
18.823277	1275.161752	11.791053
19.544333	1263.664203	11.796058
19.103267	1272.307082	11.801063
18.932099	1275.876358	11.806067
19.309399	1290.521577	11.811072
19.273785	1309.662414	11.816077
19.610958	1301.635501	11.821082
19.473175	1312.313218	11.826087
19.503535	1312.510311	11.831091
19.734918	1312.557065	11.836096
19.634661	1314.251047	11.841101
19.814887	1314.474699	11.846106
19.778611	1318.659568	11.851111
19.920275	1317.159422	11.856115
20.217808	1327.460203	11.861120
20.266429	1335.586609	11.866125
20.386778	1318.509271	11.871130
20.156102	1315.262872	11.876135
20.104520	1309.493122	11.881139
20.376755	1316.388498	11.886144
20.402654	1314.752273	11.891149
20.303849	1306.880055	11.896154
20.208437	1323.329081	11.901159
20.420990	1331.039822	11.906163
20.811492	1334.282973	11.911168
20.344669	1331.615142	11.916173
21.097139	1332.684245	11.921178
20.215048	1315.973392	11.926183
20.250610	1340.204452	11.931187
20.590575	1350.047463	11.936192
20.768929	1332.240175	11.941197
20.929462	1334.069183	11.946202
20.821144	1347.976621	11.951207
20.388677	1344.811288	11.956211
20.704196	1335.226595	11.961216
20.486542	1346.620413	11.966221
20.559413	1340.100656	11.971226
20.836327	1355.865844	11.976231
21.242028	1366.770732	11.981235
21.327020	1378.715555	11.986240
21.470156	1377.442254	11.991245
21.585768	1362.633329	11.996250
21.497089	1348.011550	12.001255
21.344409	1337.064904	12.006259
21.560968	1343.619083	12.011264
21.228559	1338.610067	12.016269
21.418521	1333.905668	12.021274
21.560668	1339.041391	12.026279
21.559235	1338.308404	12.031283
21.554377	1321.894442	12.036288
21.582675	1328.899699	12.041293
21.729666	1321.786220	12.046298
21.432949	1337.579807	12.051303
21.532766	1339.336498	12.056307
21.707708	1316.879246	12.061312
21.311067	1340.447527	12.066317
21.549671	1325.876070	12.071322
21.449067	1325.639882	12.076327
21.613783	1335.862504	12.081331
21.793602	1329.339886	12.086336
21.771098	1331.070354	12.091341
21.512472	1333.341543	12.096346
21.425516	1338.204720	12.101351
21.589758	1343.008907	12.106355
21.663666	1333.691417	12.111360
21.375403	1331.764673	12.116365
22.042298	1326.241443	12.121370
21.455941	1323.001312	12.126375
21.417335	1317.212143	12.131379
21.402350	1314.915376	12.136384
21.210266	1308.433164	12.141389
21.510749	1304.447596	12.146394
21.481407	1307.945370	12.151399
21.375142	1316.285709	12.156403
21.609891	1296.507703	12.161408
21.351750	1296.815470	12.166413
21.856608	1303.564924	12.171418
21.708299	1310.547878	12.176423
21.360259	1310.806905	12.181427
21.561854	1305.662259	12.186432
21.245381	1312.107478	12.191437
21.416152	1307.018212	12.196442
21.124246	1316.749097	12.201447
21.362812	1307.145158	12.206451
21.370856	1306.782828	12.211456
21.430992	1323.243313	12.216461
21.529069	1314.133296	12.221466
21.468762	1305.625723	12.226471
21.256736	1315.854807	12.231475
21.534546	1305.713166	12.236480
21.314691	1313.073393	12.241485
21.546403	1301.578173	12.246490
21.263585	1309.815781	12.251495
21.589107	1308.401428	12.256499
21.685187	1307.228680	12.261504
21.653895	1321.046534	12.266509
21.596626	1314.072875	12.271514
21.563085	1315.341469	12.276519
21.513696	1307.475562	12.281523
21.517131	1317.780669	12.286528
21.562898	1316.729489	12.291533
21.669589	1304.390022	12.296538
21.487471	1314.723147	12.301543
21.451870	1316.655979	12.306547
21.842032	1310.598144	12.311552
21.664727	1309.956290	12.316557
21.702732	1316.983647	12.321562
21.840412	1316.613255	12.326567
22.074733	1302.394171	12.331571
21.831852	1284.491702	12.336576
21.625267	1285.248568	12.341581
21.668548	1276.916881	12.346586
21.667241	1291.950504	12.351591
21.286707	1289.887094	12.356595
21.416240	1277.307460	12.361600
21.367013	1299.886690	12.366605
21.301032	1288.927828	12.371610
21.364201	1300.792489	12.376615
21.326922	1297.903182	12.381619
21.197095	1275.655459	12.386624
20.996472	1298.069597	12.391629
21.411424	1283.911608	12.396634
21.326780	1295.091777	12.401639
21.555671	1282.961500	12.406643
21.700866	1274.886374	12.411648
21.421126	1294.417797	12.416653
21.475371	1289.115308	12.421658
21.484047	1287.795651	12.426663
21.263030	1287.096115	12.431667
21.256796	1296.092280	12.436672
21.194088	1287.539368	12.441677
21.405809	1305.106347	12.446682
21.663822	1280.767179	12.451687
21.390839	1290.061359	12.456691
21.697447	1286.615722	12.461696
21.458657	1295.660020	12.466701
21.524613	1292.252768	12.471706
21.712007	1292.667667	12.476711
21.686487	1290.374161	12.481715
21.933380	1296.388885	12.486720
21.498385	1305.642684	12.491725
21.715425	1296.737633	12.496730
21.596952	1296.567375	12.501735
21.626745	1295.168654	12.506739
21.773890	1286.596463	12.511744
21.446622	1293.437640	12.516749
21.401817	1277.399114	12.521754
21.425542	1280.284435	12.526759
21.392774	1281.608097	12.531763
21.734880	1294.349215	12.536768
21.477734	1287.013206	12.541773
21.765415	1260.688654	12.546778
21.633632	1268.410131	12.551783
21.191919	1265.747769	12.556787
21.486739	1260.522036	12.561792
21.318883	1256.611185	12.566797
21.576189	1256.667997	12.571802
21.438477	1267.235282	12.576807
21.212043	1260.014238	12.581811
21.375474	1253.770238	12.586816
21.253037	1270.655606	12.591821
21.621895	1263.730697	12.596826
21.557884	1270.656031	12.601831
21.437700	1265.714115	12.606835
21.367814	1265.581839	12.611840
21.356047	1264.547725	12.616845
21.364226	1266.435720	12.621850
21.410270	1268.647263	12.626855
21.533923	1267.433850	12.631859
21.644766	1265.989088	12.636864
21.406492	1280.388706	12.641869
21.843471	1258.635658	12.646874
22.026183	1269.826781	12.651879
21.602120	1274.791017	12.656883
21.620864	1279.085373	12.661888
21.617469	1271.503889	12.666893
21.840313	1266.081474	12.671898
21.481176	1274.561474	12.676903
21.193567	1281.465707	12.681907
21.489211	1278.673113	12.686912
21.272597	1274.986079	12.691917
21.526753	1271.222379	12.696922
21.397805	1277.103076	12.701927
21.421010	1272.184018	12.706931
21.832989	1273.578667	12.711936
21.359219	1275.294375	12.716941
21.695223	1276.412556	12.721946
21.388617	1274.044038	12.726951
21.626672	1275.035914	12.731955
21.727853	1263.678241	12.736960
21.433887	1256.889023	12.741965
21.725216	1237.311811	12.746970
21.500132	1247.684858	12.751975
21.224086	1240.752439	12.756979
21.399387	1238.619299	12.761984
21.378412	1246.625868	12.766989
21.146569	1242.688957	12.771994
21.437497	1259.319140	12.776999
21.141727	1277.359701	12.782003
21.451845	1271.051295	12.787008
21.703395	1284.738842	12.792013
21.378688	1277.880400	12.797018
21.376300	1289.641966	12.802023
21.517811	1285.921461	12.807027
21.610027	1274.644058	12.812032
21.655331	1264.474876	12.817037
21.184154	1262.261922	12.822042
20.899309	1258.841246	12.827047
21.152133	1265.687654	12.832051
21.536471	1275.816855	12.837056
21.139701	1297.126856	12.842061
21.326512	1281.237464	12.847066
21.585303	1282.725936	12.852071
21.645670	1284.105706	12.857075
21.553039	1293.885216	12.862080
21.664633	1292.528642	12.867085
21.518445	1280.339921	12.872090
21.695805	1295.956918	12.877095
21.421250	1296.584276	12.882099
21.688419	1281.696064	12.887104
21.634748	1279.091655	12.892109
21.439661	1256.291390	12.897114
21.391982	1263.021724	12.902119
21.601451	1256.994310	12.907123
21.441434	1244.889827	12.912128
21.477870	1249.383204	12.917133
21.508882	1251.048355	12.922138
21.344023	1249.962966	12.927143
21.098831	1257.659948	12.932147
21.622086	1269.676704	12.937152
21.186129	1273.024859	12.942157
21.379692	1280.047886	12.947162
21.635915	1286.655638	12.952167
21.660392	1281.036196	12.957171
21.133443	1266.350363	12.962176
21.019705	1284.786105	12.967181
21.514056	1285.357049	12.972186
21.607388	1290.803321	12.977191
21.437992	1297.818018	12.982195
21.773169	1292.823960	12.987200
21.488071	1278.736637	12.992205
21.270921	1273.406479	12.997210
21.526692	1280.698708	13.002215
21.467813	1282.302507	13.007219
21.594070	1268.550132	13.012224
21.085348	1269.213263	13.017229
21.270563	1274.154432	13.022234
21.068162	1295.580086	13.027239
21.202106	1299.641603	13.032243
21.616502	1297.374122	13.037248
21.381507	1300.668151	13.042253
21.413082	1292.885533	13.047258
21.686711	1303.809863	13.052263
21.527350	1295.620876	13.057267
21.572628	1308.814637	13.062272
21.470844	1304.227747	13.067277
21.472620	1296.177063	13.072282
21.432925	1292.037598	13.077287
21.290909	1301.761911	13.082291
21.726259	1294.752264	13.087296
21.346939	1304.352001	13.092301
21.473265	1311.363690	13.097306
21.641200	1293.386220	13.102311
21.321064	1312.745912	13.107315
21.319243	1302.779766	13.112320
21.178441	1306.981305	13.117325
21.638346	1297.138637	13.122330
21.773519	1296.883765	13.127335
21.524767	1313.655287	13.132339
21.847787	1291.481967	13.137344
21.576498	1281.022645	13.142349
21.751354	1270.971568	13.147354
21.368931	1260.722378	13.152359
21.496921	1259.074606	13.157363
21.718308	1271.817613	13.162368
21.005605	1274.651662	13.167373
21.412308	1260.715787	13.172378
21.395218	1270.200953	13.177383
21.128911	1265.698666	13.182387
21.528523	1274.781472	13.187392
21.475064	1274.312257	13.192397
21.389114	1264.148242	13.197402
21.488100	1272.074188	13.202407
21.337704	1267.488756	13.207411
21.569705	1261.692716	13.212416
21.284542	1262.435306	13.217421
21.320334	1269.133405	13.222426
21.635195	1264.230908	13.227431
21.223262	1277.825580	13.232435
21.777472	1271.177037	13.237440
21.355819	1272.491764	13.242445
21.229365	1270.911384	13.247450
21.438041	1282.044758	13.252455
21.280399	1278.616403	13.257459
21.610322	1286.492906	13.262464
21.563061	1291.362351	13.267469
21.586745	1278.351739	13.272474
21.768801	1279.488168	13.277479
21.461134	1282.410578	13.282483
21.619494	1272.802108	13.287488
21.319216	1276.805146	13.292493
21.187579	1275.712879	13.297498
21.377078	1280.301701	13.302503
21.389576	1280.556837	13.307507
21.425635	1278.256665	13.312512
21.234247	1273.174714	13.317517
21.268110	1280.339911	13.322522
21.558846	1289.895839	13.327527
21.246450	1302.438582	13.332531
21.589532	1297.741311	13.337536
21.744136	1288.914034	13.342541
21.311748	1289.309520	13.347546
21.315538	1288.026913	13.352551
21.271700	1284.026886	13.357555
21.659774	1284.815058	13.362560
21.340712	1300.091766	13.367565
21.259089	1293.192966	13.372570
21.824242	1303.107261	13.377575
21.335593	1297.905557	13.382579
21.625956	1288.384833	13.387584
21.202450	1285.142389	13.392589
21.602478	1288.686791	13.397594
21.577998	1295.866032	13.402599
21.614962	1283.602362	13.407603
21.860881	1271.450453	13.412608
21.176429	1285.492307	13.417613
21.133546	1292.321239	13.422618
21.186278	1281.945853	13.427623
21.043398	1297.889904	13.432627
21.393481	1307.135174	13.437632
21.395714	1322.942563	13.442637
21.628892	1322.730406	13.447642
21.648531	1323.213066	13.452647
21.726082	1316.970122	13.457651
21.693101	1286.699023	13.462656
21.412644	1293.815013	13.467661
21.322215	1290.437437	13.472666
21.535809	1283.068922	13.477671
21.682197	1289.145406	13.482675
21.562156	1281.532060	13.487680
21.384475	1285.143378	13.492685
21.461011	1282.891943	13.497690
21.527578	1284.698086	13.502695
21.242502	1287.765130	13.507699
21.581671	1273.037333	13.512704
21.269031	1289.632936	13.517709
21.729924	1286.886523	13.522714
21.765564	1282.766584	13.527719
21.232373	1288.587184	13.532723
21.233981	1289.383383	13.537728
21.414067	1292.275305	13.542733
21.542237	1285.445549	13.547738
21.763416	1294.820184	13.552743
21.602542	1290.151260	13.557747
21.893512	1285.850241	13.562752
21.758616	1283.556836	13.567757
21.575043	1288.730303	13.572762
21.674518	1283.639801	13.577767
21.502117	1290.298577	13.582771
21.190030	1292.554632	13.587776
21.250690	1295.945006	13.592781
21.611496	1286.488742	13.597786
21.698662	1289.001240	13.602791
21.621718	1293.424405	13.607795
21.656759	1295.123612	13.612800
21.614234	1274.402675	13.617805
21.396389	1263.988458	13.622810
21.370754	1258.186204	13.627815
21.119503	1262.788553	13.632819
21.169339	1272.758215	13.637824
21.443189	1279.662778	13.642829
21.289960	1286.736393	13.647834
21.620281	1286.642785	13.652839
21.525684	1298.173057	13.657843
21.787645	1289.949986	13.662848
21.493445	1281.060259	13.667853
21.569363	1273.608051	13.672858
21.803791	1261.680338	13.677863
21.335375	1260.195507	13.682867
21.481546	1259.235550	13.687872
21.494983	1267.887932	13.692877
21.464875	1268.864234	13.697882
21.440057	1258.141684	13.702887
21.343399	1264.201732	13.707891
21.264059	1258.753402	13.712896
21.576093	1254.452187	13.717901
21.407699	1262.405007	13.722906
21.380503	1257.741579	13.727911
21.447628	1270.977553	13.732915
21.399407	1256.432992	13.737920
21.509093	1267.788728	13.742925
21.265425	1258.444670	13.747930
21.516966	1261.098103	13.752935
21.002309	1270.754100	13.757939
21.213782	1277.646533	13.762944
21.702687	1299.972768	13.767949
21.621854	1291.876915	13.772954
21.580928	1273.644196	13.777959
21.030697	1273.366185	13.782963
21.744692	1277.494449	13.787968
21.448689	1272.564805	13.792973
21.523101	1274.759208	13.797978
21.487899	1263.812803	13.802983
21.263723	1269.128359	13.807987
21.434989	1255.923913	13.812992
21.260129	1268.763238	13.817997
21.485260	1274.604802	13.823002
21.531352	1281.654506	13.828007
21.398102	1271.958508	13.833011
21.280424	1275.495596	13.838016
21.229978	1290.101810	13.843021
21.275026	1293.822685	13.848026
21.590842	1291.156184	13.853031
21.219736	1309.180415	13.858035
21.729273	1303.928303	13.863040
21.646184	1299.250122	13.868045
21.672675	1295.489613	13.873050
21.488545	1280.637118	13.878055
21.379670	1268.380953	13.883059
21.655586	1274.611815	13.888064
21.748689	1273.038993	13.893069
21.716551	1279.546078	13.898074
21.562133	1262.640368	13.903079
21.408092	1274.626388	13.908083
21.280721	1267.070990	13.913088
21.610411	1277.754543	13.918093
21.244886	1263.998612	13.923098
21.093988	1263.857181	13.928103
21.309307	1271.061239	13.933107
21.605705	1267.126796	13.938112
21.215993	1267.922334	13.943117
21.282036	1264.384186	13.948122
21.480206	1271.792833	13.953127
21.357154	1293.292560	13.958131
21.749532	1290.014595	13.963136
21.500109	1273.431537	13.968141
21.482524	1270.163774	13.973146
21.508347	1278.464098	13.978151
21.437595	1283.326249	13.983155
21.349062	1275.848232	13.988160
21.037105	1280.362497	13.993165
21.006002	1285.301904	13.998170
21.364493	1291.628414	14.003175
21.388326	1302.942677	14.008179
21.630168	1312.925896	14.013184
21.197482	1312.543978	14.018189
21.257576	1312.688564	14.023207
21.399432	1305.463444	14.028224
21.490167	1308.349587	14.033242
21.704079	1296.026034	14.038259
21.619132	1314.089354	14.043277
21.357659	1313.102428	14.048295
21.617529	1302.160461	14.053312
21.279847	1321.135521	14.058330
21.595800	1302.359138	14.063347
21.839456	1304.964496	14.068365
21.480477	1314.575985	14.073383
21.349791	1317.456552	14.078400
21.320389	1319.930870	14.083418
21.599024	1311.167597	14.088435
21.707107	1308.584945	14.093453
21.405905	1312.692876	14.098471
21.637255	1307.005990	14.103488
21.801007	1315.582461	14.108506
21.682816	1315.448819	14.113523
21.731401	1314.856011	14.118541
21.749595	1318.680200	14.123559
21.703845	1310.413817	14.128576
21.510794	1314.731004	14.133594
21.729694	1331.580317	14.138611
21.663420	1334.821831	14.143629
21.813920	1343.884905	14.148647
21.977523	1335.545790	14.153664
21.660451	1355.127916	14.158682
21.541295	1347.884636	14.163699
21.810197	1351.420316	14.168717
21.957632	1343.090068	14.173735
21.639299	1346.216067	14.178752
21.319574	1356.349837	14.183770
21.828478	1357.451614	14.188787
21.966437	1367.150606	14.193805
22.114204	1379.131987	14.198823
22.457015	1378.437191	14.203840
22.085959	1378.183439	14.208858
22.051049	1375.532351	14.213875
22.209545	1365.136596	14.218893
22.193012	1383.618509	14.223911
22.133537	1381.455812	14.228928
22.359040	1384.630348	14.233946
22.281958	1378.533326	14.238963
22.240638	1374.574553	14.243981
22.002908	1392.709530	14.248999
22.212358	1383.474349	14.254016
22.385331	1384.201864	14.259034
22.126736	1394.769487	14.264051
22.523737	1384.209838	14.269069
22.438304	1385.867297	14.274087
22.532160	1386.475303	14.279104
22.231768	1383.231081	14.284122
22.141483	1387.343142	14.289139
22.701489	1385.713965	14.294157
22.331864	1389.412849	14.299175
22.669275	1384.655942	14.304192
22.423412	1390.623752	14.309210
22.586766	1387.560379	14.314227
22.849679	1387.930642	14.319245
22.342146	1375.283239	14.324263
22.781572	1370.237942	14.329280
22.535756	1360.216555	14.334298
22.462408	1355.808310	14.339315
22.885419	1363.390240	14.344333
22.748536	1362.188390	14.349351
22.689701	1346.811134	14.354368
22.671707	1352.814937	14.359386
22.958306	1352.803910	14.364403
22.859329	1339.474770	14.369421
22.430212	1343.928716	14.374439
22.625034	1353.182919	14.379456
22.564849	1359.441983	14.384474
22.619854	1360.142698	14.389491
22.827418	1374.580944	14.394509
22.414679	1384.830240	14.399527
22.793014	1381.738870	14.404544
22.464617	1380.518804	14.409562
22.702648	1380.630351	14.414579
22.988687	1381.468814	14.419597
22.879312	1385.118321	14.424615
22.860213	1380.550410	14.429632
22.990116	1380.418091	14.434650
22.949207	1388.081898	14.439667
23.226246	1379.293672	14.444685
22.825466	1388.564252	14.449703
23.082340	1377.267216	14.454720
23.195858	1376.248785	14.459738
22.892737	1386.932039	14.464755
22.978359	1379.201493	14.469773
22.782297	1383.179419	14.474791
22.855895	1387.543754	14.479808
22.824411	1385.824887	14.484826
22.690249	1390.296291	14.489843
22.983337	1397.596954	14.494861
23.145746	1416.781796	14.499879
23.316242	1411.469506	14.504896
23.315779	1415.398939	14.509914
23.767679	1409.824694	14.514931
23.466872	1399.859240	14.519949
23.044884	1402.080025	14.524967
23.270570	1402.530156	14.529984
23.606112	1411.628248	14.535002
23.173243	1400.947709	14.540019
23.493464	1397.750778	14.545037
23.044569	1394.210928	14.550055
23.261231	1413.231389	14.555072
23.535408	1407.556509	14.560090
23.482346	1417.715425	14.565107
23.691258	1422.766023	14.570125
23.602248	1421.271825	14.575143
23.716762	1404.050077	14.580160
23.565946	1395.795685	14.585178
23.175354	1415.342430	14.590195
23.875343	1397.534963	14.595213
23.930311	1394.619433	14.600231
23.204803	1379.183319	14.605248
23.319603	1403.159127	14.610266
23.802566	1412.966709	14.615283
24.043281	1412.687731	14.620301
23.497952	1407.099525	14.625319
23.693629	1393.020219	14.630336
23.675338	1419.065285	14.635354
23.221321	1419.611250	14.640371
23.613811	1408.544234	14.645389
23.566302	1417.637364	14.650407
23.779107	1425.361391	14.655424
23.821328	1425.840787	14.660442
23.689898	1421.273478	14.665459
23.854333	1420.248496	14.670477
23.917182	1418.860631	14.675495
23.881623	1415.967402	14.680512
23.879100	1415.672168	14.685530
23.648340	1420.794470	14.690547
23.971547	1413.074771	14.695565
23.867354	1407.645854	14.700583
23.885867	1424.456455	14.705600
23.591172	1412.575712	14.710618
23.933346	1425.095537	14.715635
24.364437	1431.461881	14.720653
24.227843	1427.372004	14.725671
23.963651	1421.924560	14.730688
23.966314	1418.669742	14.735706
23.944321	1433.180840	14.740723
24.277576	1433.502133	14.745741
24.018530	1453.318946	14.750759
24.261991	1448.880588	14.755776
24.359902	1440.897946	14.760794
24.274154	1457.723642	14.765811
24.676048	1450.781006	14.770829
24.074511	1439.741963	14.775847
24.248112	1437.073334	14.780864
24.522198	1438.885805	14.785882
24.188066	1452.471468	14.790899
24.396486	1447.249067	14.795917
24.680842	1442.072756	14.800935
24.090818	1449.099041	14.805952
24.360345	1450.471808	14.810970
24.569135	1453.260501	14.815987
24.348193	1445.954759	14.821005
24.614889	1451.617475	14.826023
24.684992	1447.809218	14.831040
24.729647	1447.050296	14.836058
24.554743	1454.475970	14.841075
25.114028	1445.383144	14.846093
24.479785	1430.020504	14.851111
24.352792	1417.505841	14.856128
24.625968	1434.165726	14.861146
24.866086	1447.038464	14.866163
24.890657	1442.425816	14.871181
24.544476	1430.185196	14.876199
24.425562	1420.123077	14.881216
24.750044	1422.718711	14.886234
24.515960	1457.363092	14.891251
24.815126	1446.889787	14.896269
25.057377	1452.858414	14.901287
24.808120	1449.269404	14.906304
25.138389	1443.097942	14.911322
24.852164	1436.746401	14.916339
24.772221	1434.981776	14.921357
24.597661	1438.212272	14.926375
25.011551	1442.481448	14.931392
25.301167	1448.928566	14.936410
24.908996	1457.390881	14.941427
24.964849	1447.011440	14.946445
24.977418	1448.338679	14.951463
24.885756	1453.309821	14.956480
25.152280	1449.438774	14.961498
24.878954	1455.379531	14.966515
24.784897	1446.837640	14.971533
24.962881	1459.569295	14.976551
24.958338	1458.660922	14.981568
25.335753	1448.403216	14.986586
24.884512	1464.326132	14.991603
24.958348	1454.862435	14.996621
25.390573	1449.720735	15.001639
25.120969	1457.367575	15.006656
25.331572	1453.738246	15.011674
25.086608	1450.990092	15.016691
25.058317	1445.657589	15.021709
25.214357	1446.332755	15.026727
25.017671	1448.802318	15.031744
25.722719	1464.978087	15.036762
25.370353	1459.656373	15.041779
25.440112	1447.799263	15.046797
25.402413	1451.822732	15.051815
25.495913	1452.973474	15.056832
25.287315	1455.124051	15.061850
25.525667	1473.123417	15.066867
25.483480	1471.701966	15.071885
25.552118	1484.808150	15.076903
25.478258	1482.397628	15.081920
25.991862	1471.504722	15.086938
25.719621	1478.247533	15.091955
26.032544	1467.749997	15.096973
26.028883	1453.261996	15.101991
25.715448	1440.380662	15.107008
25.955957	1439.194112	15.112026
25.750999	1437.053039	15.117043
25.779951	1444.169348	15.122061
25.667888	1443.315878	15.127079
25.256270	1434.711393	15.132096
25.751815	1424.241386	15.137114
25.678405	1439.515718	15.142131
25.806874	1451.355524	15.147149
26.071501	1457.709108	15.152167
25.865642	1456.931944	15.157184
25.893097	1445.499995	15.162202
25.871207	1450.058898	15.167219
25.732484	1458.988858	15.172237
25.976394	1461.221410	15.177255
25.714299	1463.611749	15.182272
26.128453	1461.364055	15.187290
26.269277	1469.178236	15.192307
26.074770	1472.017105	15.197325
25.916511	1470.139130	15.202343
25.914779	1464.970691	15.207360
26.032249	1472.661188	15.212378
26.347418	1467.333667	15.217395
26.214279	1465.351015	15.222413
26.593583	1473.053229	15.227431
26.122862	1481.749877	15.232448
26.357022	1471.818589	15.237466
26.562784	1464.506121	15.242483
26.314214	1467.218336	15.247501
26.662990	1470.970960	15.252519
26.536904	1463.201781	15.257536
26.426567	1446.262804	15.262554
26.025731	1442.134850	15.267571
26.266140	1447.222903	15.272589
26.716559	1456.153269	15.277607
26.546680	1473.104084	15.282624
26.586549	1464.904178	15.287642
26.349410	1451.519896	15.292659
26.287901	1463.456079	15.297677
26.344723	1465.079846	15.302695
26.417289	1478.356851	15.307712
26.672902	1472.656594	15.312730
26.701843	1472.442854	15.317747
26.685234	1472.673667	15.322765
26.806649	1473.162454	15.327783
26.365819	1473.303634	15.332800
26.669767	1473.958355	15.337818
26.759002	1477.898666	15.342835
26.590128	1482.306424	15.347853
26.778776	1475.210606	15.352871
26.468445	1475.991621	15.357888
26.519672	1468.949185	15.362906
26.865498	1477.172677	15.367923
26.852800	1472.701241	15.372941
26.755556	1465.312839	15.377959
26.530405	1477.846125	15.382976
26.533373	1476.577915	15.387994
26.865361	1488.624381	15.393011
26.955636	1495.888232	15.398029
26.794347	1499.822892	15.403047
26.936099	1490.315306	15.408064
27.040797	1495.316488	15.413082
27.046154	1500.224981	15.418099
27.083574	1503.081916	15.423117
27.290541	1501.293541	15.428135
27.053945	1501.779661	15.433152
27.201639	1499.185937	15.438170
27.185482	1492.610402	15.443187
27.023038	1500.743525	15.448205
27.393997	1499.051685	15.453223
27.043387	1498.409289	15.458240
27.266724	1496.306854	15.463258
27.387258	1494.458336	15.468275
26.982854	1494.507193	15.473293
27.439720	1499.795113	15.478311
26.649396	1495.597138	15.483328
27.131233	1492.435755	15.488346
27.383432	1505.377402	15.493363
27.287372	1518.235402	15.498381
27.596394	1528.347652	15.503399
27.556565	1530.699403	15.508416
27.654319	1522.957407	15.513434
28.060391	1521.944211	15.518451
27.571731	1512.508064	15.523469
27.831462	1491.999115	15.528487
27.588416	1501.032254	15.533504
27.858425	1491.889589	15.538522
27.963540	1491.361687	15.543539
27.555773	1490.380780	15.548557
27.658738	1495.561558	15.553575
27.665545	1495.823241	15.558592
27.582182	1490.666242	15.563610
27.575591	1492.860106	15.568627
27.601131	1484.330576	15.573645
27.871151	1488.640017	15.578663
27.513380	1507.418755	15.583680
27.949297	1502.817553	15.588698
28.199365	1516.542108	15.593715
27.954468	1525.929478	15.598733
27.992413	1519.420804	15.603751
27.873265	1515.829113	15.608768
27.962492	1517.335249	15.613786
27.820815	1517.266696	15.618803
28.113411	1524.106619	15.623821
28.398497	1517.835369	15.628839
28.037641	1530.264508	15.633856
28.255943	1529.671361	15.638874
28.153223	1536.700183	15.643891
27.912080	1530.602524	15.648909
28.181401	1527.401101	15.653927
28.169459	1525.458882	15.658944
27.935271	1529.641125	15.663962
28.132840	1527.399655	15.668979
28.110747	1531.041568	15.673997
28.273028	1518.593931	15.679015
28.060379	1521.976808	15.684032
28.090098	1524.259265	15.689050
28.313616	1520.660892	15.694067
28.013732	1530.096361	15.699085
28.244125	1524.651783	15.704103
28.025585	1543.084325	15.709120
28.335116	1551.203540	15.714138
28.571125	1556.842879	15.719155
28.326331	1559.950901	15.724173
28.844386	1552.127693	15.729191
28.925956	1556.663835	15.734208
28.544761	1561.948603	15.739226
29.025685	1555.282742	15.744243
28.980161	1549.119267	15.749261
28.653127	1524.994768	15.754279
28.612795	1529.331702	15.759296
28.659423	1520.687105	15.764314
28.701844	1523.315164	15.769331
28.752727	1542.510098	15.774349
29.074355	1554.344346	15.779367
28.684257	1527.812224	15.784384
28.664304	1525.762748	15.789402
28.796970	1536.145372	15.794419
29.143448	1554.410730	15.799437
29.110456	1552.525347	15.804455
29.155616	1555.901716	15.809472
29.233821	1545.944918	15.814490
29.130394	1527.103007	15.819507
28.897598	1527.950307	15.824525
29.043935	1512.721827	15.829543
29.118265	1517.207991	15.834560
28.862976	1531.317538	15.839578
29.300329	1530.669003	15.844595
28.897725	1535.329556	15.849613
29.092467	1534.924206	15.854631
28.966926	1545.915870	15.859648
29.145319	1548.242254	15.864666
29.092338	1549.704224	15.869683
28.855493	1550.561609	15.874701
29.092215	1544.103013	15.879719
29.064937	1554.375886	15.884736
28.988145	1555.179428	15.889754
29.166858	1544.775601	15.894771
29.093571	1584.351109	15.899789
29.379516	1573.107486	15.904807
29.247221	1585.761330	15.909824
29.377959	1597.843134	15.914842
29.939915	1592.081383	15.919859
29.698020	1588.343303	15.924877
29.620715	1581.352774	15.929895
29.950339	1585.973626	15.934912
29.697549	1603.640944	15.939930
29.988259	1586.405032	15.944947
29.765758	1566.751526	15.949965
29.796852	1553.481664	15.954983
29.546203	1560.559260	15.960000
29.123017	1557.218183	15.965018
29.497452	1563.738339	15.970035
29.535005	1582.314122	15.975053
29.618597	1588.685629	15.980071
29.827612	1580.125205	15.985088
29.880309	1586.776912	15.990106
29.798885	1595.822082	15.995123
29.844455	1596.129493	16.000141
29.712497	1583.780642	16.005159
29.995220	1583.545297	16.010176
30.080193	1579.253300	16.015194
30.112472	1582.554653	16.020211
29.951592	1589.537722	16.025229
30.026962	1586.324751	16.030247
30.114890	1582.453842	16.035264
30.094691	1589.348407	16.040282
29.911676	1593.133977	16.045299
29.814073	1593.632535	16.050317
30.195746	1601.433539	16.055335
30.374856	1614.920186	16.060352
30.178243	1612.368777	16.065370
30.498291	1614.357980	16.070387
30.254582	1620.714068	16.075405
30.637387	1612.108603	16.080423
30.530858	1593.067331	16.085440
30.183025	1588.205732	16.090458
30.472823	1582.149203	16.095475
30.446995	1597.571838	16.100493
30.522326	1593.194860	16.105511
30.717699	1600.408967	16.110528
30.325345	1590.756851	16.115546
30.868107	1604.286156	16.120563
30.398352	1610.272463	16.125581
30.672483	1604.688748	16.130599
30.939342	1608.899631	16.135616
30.645081	1600.010493	16.140634
30.691797	1591.233709	16.145651
30.560729	1593.455308	16.150669
30.835869	1609.608580	16.155687
31.025791	1611.613818	16.160704
30.737028	1598.067752	16.165722
30.898839	1588.784985	16.170739
30.749072	1594.847659	16.175757
30.785173	1607.053102	16.180775
30.856106	1597.094282	16.185792
30.698821	1610.873676	16.190810
30.883962	1604.203062	16.195827
31.075785	1608.226144	16.200845
31.121032	1606.573661	16.205863
31.166385	1602.311571	16.210880
30.835441	1606.144335	16.215898
31.091923	1606.485744	16.220915
30.821262	1602.247318	16.225933
30.783078	1608.227708	16.230951
31.313092	1592.094038	16.235968
31.104531	1600.297492	16.240986
31.240319	1604.730622	16.246003
31.189562	1596.697677	16.251021
31.086711	1597.799527	16.256039
31.290506	1594.702920	16.261056
31.314600	1598.161308	16.266074
31.417969	1599.060383	16.271091
31.093442	1604.188266	16.276109
31.048184	1612.315343	16.281127
31.520480	1617.511186	16.286144
31.442364	1637.462981	16.291162
31.352804	1634.343946	16.296179
31.799775	1635.056085	16.301197
31.800569	1635.856694	16.306215
31.697398	1631.319417	16.311232
31.342894	1627.987817	16.316250
31.673736	1620.973065	16.321267
31.684923	1625.619555	16.326285
31.577952	1639.085790	16.331303
31.707970	1619.199808	16.336320
31.791097	1650.767619	16.341338
32.191361	1631.634451	16.346355
32.090978	1636.341210	16.351373
31.580873	1621.414733	16.356391
31.605439	1641.301392	16.361408
31.717314	1636.659028	16.366426
31.713098	1629.133011	16.371443
31.785189	1640.686241	16.376461
31.651372	1633.600882	16.381479
31.891113	1632.371969	16.386496
32.003147	1632.387214	16.391514
32.074042	1629.834032	16.396531
32.145203	1636.674722	16.401549
31.888532	1629.604242	16.406567
32.181378	1631.180943	16.411584
32.059844	1632.424198	16.416602
32.229851	1626.644729	16.421619
32.445700	1629.778390	16.426637
32.208268	1641.313352	16.431655
32.608409	1628.491061	16.436672
32.213293	1626.687023	16.441690
32.132530	1624.933517	16.446707
32.275381	1629.686419	16.451725
32.223272	1646.969430	16.456743
32.785679	1655.237129	16.461760
32.573281	1654.555376	16.466778
32.625889	1633.177939	16.471795
32.425496	1633.900529	16.476813
32.631951	1646.369836	16.481831
32.717650	1637.306814	16.486848
32.384998	1652.292391	16.491866
32.799765	1632.003904	16.496883
32.409438	1667.027630	16.501901
32.632831	1652.608604	16.506919
32.983127	1649.186604	16.511936
32.847993	1664.911457	16.516954
33.081338	1668.478055	16.521971
33.374533	1629.119084	16.526989
32.596653	1632.952358	16.532007
32.735740	1628.714634	16.537024
32.633888	1630.749111	16.542042
32.652169	1636.893535	16.547059
32.697135	1636.891164	16.552077
32.585616	1659.695436	16.557095
32.825824	1670.005949	16.562112
32.864291	1656.585382	16.567130
33.046198	1668.289429	16.572147
33.068927	1657.897818	16.577165
32.941766	1661.542365	16.582183
33.256656	1654.213970	16.587200
33.193610	1659.901049	16.592218
33.186905	1667.166299	16.597235
33.251355	1654.787632	16.602253
33.431596	1657.996190	16.607271
33.187437	1660.127301	16.612288
33.100083	1668.360223	16.617306
33.124832	1659.805549	16.622323
33.645462	1661.578724	16.627341
32.946533	1665.791089	16.632359
33.234305	1675.057414	16.637376
33.033506	1681.291855	16.642394
33.279813	1694.607413	16.647411
33.761493	1701.517933	16.652429
33.495444	1690.282041	16.657447
33.736717	1691.634171	16.662464
33.239840	1695.841057	16.667482
33.304692	1703.669056	16.672499
33.504176	1682.620471	16.677517
33.669707	1692.197310	16.682535
33.653046	1691.281418	16.687552
33.844972	1697.602660	16.692570
33.679984	1694.884173	16.697587
33.909227	1702.218770	16.702605
33.970242	1713.413608	16.707623
34.034171	1707.946751	16.712640
33.992338	1701.085783	16.717658
34.015156	1701.580867	16.722675
34.051896	1680.981380	16.727693
34.029352	1686.528305	16.732711
34.176698	1684.475717	16.737728
34.171099	1680.268921	16.742746
34.339969	1674.991401	16.747763
34.378183	1677.873411	16.752781
34.067634	1681.405645	16.757799
34.322240	1683.375409	16.762816
34.405565	1684.033871	16.767834
34.518640	1684.923537	16.772851
34.662345	1684.713511	16.777869
34.062175	1686.228167	16.782887
34.339041	1678.960879	16.787904
34.588620	1684.874952	16.792922
34.206024	1686.134684	16.797939
34.737768	1673.524167	16.802957
34.321702	1682.635351	16.807975
34.563050	1671.631569	16.812992
34.448542	1681.817774	16.818010
34.522067	1680.181221	16.823027
34.856356	1672.854441	16.828045
34.826106	1679.056960	16.833063
34.686248	1677.446577	16.838080
34.584822	1667.812498	16.843098
34.669816	1680.636257	16.848115
34.542428	1673.601762	16.853133
34.491659	1683.953977	16.858151
34.717854	1692.234427	16.863168
35.098933	1694.835242	16.868186
34.827872	1682.618603	16.873203
34.902942	1681.090341	16.878221
34.839543	1694.659787	16.883239
34.869718	1699.926180	16.888256
34.880506	1692.932556	16.893274
34.833410	1695.269763	16.898291
34.994499	1689.538881	16.903309
34.968788	1693.761849	16.908327
34.979474	1689.371558	16.913344
35.254683	1693.189457	16.918362
35.209090	1696.923248	16.923379
35.312778	1686.322078	16.928397
35.457855	1686.484634	16.933415
35.023352	1699.037345	16.938432
35.040500	1694.652314	16.943450
35.123296	1694.887724	16.948467
35.434120	1690.053164	16.953485
35.114370	1696.501637	16.958503
35.385297	1704.358114	16.963520
35.396282	1689.719678	16.968538
35.517726	1708.544933	16.973555
35.637817	1720.848759	16.978573
35.534550	1727.471925	16.983591
35.653679	1721.640759	16.988608
35.612266	1714.142652	16.993626
35.653643	1726.927792	16.998643
35.795449	1712.454082	17.003661
35.724774	1728.475457	17.008679
35.567087	1730.610088	17.013696
35.644150	1719.939209	17.018714
35.332203	1735.380886	17.023731
35.542830	1720.720014	17.028749
35.723202	1726.182679	17.033767
35.688318	1727.162015	17.038784
36.048436	1718.665497	17.043802
36.138020	1717.188398	17.048819
36.317910	1717.262032	17.053837
35.871905	1728.868083	17.058855
36.084928	1719.149208	17.063872
36.289424	1713.777903	17.068890
35.716053	1724.883603	17.073907
36.245383	1711.041777	17.078925
36.228338	1720.503040	17.083943
36.451933	1714.359490	17.088960
36.172639	1717.062494	17.093978
36.089768	1729.519820	17.098995
36.125683	1727.313542	17.104013
36.452818	1732.057533	17.109031
36.316604	1737.168010	17.114048
36.209428	1738.693698	17.119066
36.022256	1751.213297	17.124083
36.522195	1752.516310	17.129101
36.408214	1753.330513	17.134119
36.688674	1750.421418	17.139136
36.780325	1745.813705	17.144154
36.750792	1753.378363	17.149171
37.039266	1733.430773	17.154189
36.743626	1747.427416	17.159207
36.747841	1749.168143	17.164224
36.888913	1746.828687	17.169242
36.563111	1755.093399	17.174259
36.619603	1758.447558	17.179277
36.819617	1751.297884	17.184295
36.765558	1747.040597	17.189312
36.987894	1744.030663	17.194330
36.724605	1757.993843	17.199347
36.858647	1752.835106	17.204365
37.185283	1753.437460	17.209383
36.973953	1745.005332	17.214400
37.271294	1748.360399	17.219418
36.927033	1751.528370	17.224435
37.021391	1741.595602	17.229453
37.260405	1751.277162	17.234471
36.823151	1745.946858	17.239488
37.052498	1745.784519	17.244506
37.238995	1770.136458	17.249523
37.483399	1776.551611	17.254541
37.560556	1792.681611	17.259559
37.250184	1794.708471	17.264576
37.816155	1775.567561	17.269594
37.510784	1778.589337	17.274611
37.548910	1770.584589	17.279629
37.492059	1768.108387	17.284647
37.334521	1770.014914	17.289664
37.669603	1767.619341	17.294682
37.510197	1780.927332	17.299699
37.803320	1764.958670	17.304717
37.710175	1769.714655	17.309735
37.266763	1777.386238	17.314752
37.695645	1776.146021	17.319770
37.740097	1779.374692	17.324787
37.875013	1766.770762	17.329805
37.996451	1766.015307	17.334823
37.663933	1775.880850	17.339840
37.926984	1769.963789	17.344858
37.740282	1779.318445	17.349875
38.052182	1765.515968	17.354893
37.755992	1772.994181	17.359911
37.659473	1771.840913	17.364928
38.282165	1774.524327	17.369946
38.219433	1774.834860	17.374963
38.026752	1769.983057	17.379981
38.110183	1783.953880	17.384999
38.242446	1790.064458	17.390016
38.416564	1785.416838	17.395034
38.487844	1800.654315	17.400051
38.324612	1792.816951	17.405069
38.448248	1797.305562	17.410087
38.238287	1808.836274	17.415104
38.698988	1798.577624	17.420122
38.643406	1805.197939	17.425139
38.581604	1790.629212	17.430157
38.656449	1785.770912	17.435175
38.492144	1774.660297	17.440192
38.592170	1789.204199	17.445210
38.304526	1798.428677	17.450227
38.318194	1789.520193	17.455245
38.624151	1795.744640	17.460263
38.218424	1802.644170	17.465280
38.791924	1791.694284	17.470298
38.970522	1783.932962	17.475315
38.538461	1800.115877	17.480333
38.654081	1795.930611	17.485351
38.570803	1797.981025	17.490368
38.839294	1810.766194	17.495386
39.087943	1816.877096	17.500403
38.875090	1825.441581	17.505421
39.179111	1817.457318	17.510439
39.117876	1826.519860	17.515456
39.421234	1826.888406	17.520474
39.109239	1817.898141	17.525491
38.940992	1827.454376	17.530509
39.306635	1824.072359	17.535527
39.465200	1820.948313	17.540544
39.676080	1823.057204	17.545562
39.273952	1818.374071	17.550579
39.737556	1826.989536	17.555597
39.731801	1815.671131	17.560615
39.553797	1828.988424	17.565632
39.709253	1815.879383	17.570650
39.967913	1816.621569	17.575667
39.421301	1798.180326	17.580685
39.537820	1808.554712	17.585703
39.567052	1821.374905	17.590720
39.716603	1815.990305	17.595738
39.785972	1808.408413	17.600755
39.825745	1817.503602	17.605773
40.139994	1818.516919	17.610791
39.730612	1812.578107	17.615808
39.614998	1812.187646	17.620826
39.723013	1815.854496	17.625843
39.834195	1818.394563	17.630861
39.976891	1819.723104	17.635879
39.857157	1802.308587	17.640896
39.892363	1809.751265	17.645914
39.930821	1830.634831	17.650931
39.979583	1813.863529	17.655949
40.118226	1820.108382	17.660967
39.866874	1824.548274	17.665984
39.889091	1829.627221	17.671002
40.062710	1825.739434	17.676019
40.269661	1816.656961	17.681037
40.229905	1853.180928	17.686055
40.218863	1862.119084	17.691072
40.496170	1849.305181	17.696090
40.494464	1839.198907	17.701107
40.212960	1852.584640	17.706125
40.262145	1853.541136	17.711143
40.412949	1852.381447	17.716160
40.765785	1831.671554	17.721178
40.595706	1863.594818	17.726195
40.640986	1837.404814	17.731213
40.793940	1848.907561	17.736231
40.667503	1852.670017	17.741248
40.919563	1835.248068	17.746266
40.684190	1847.314543	17.751283
40.842271	1842.477555	17.756301
41.252260	1845.388391	17.761319
40.529035	1841.039607	17.766336
40.402896	1860.271062	17.771354
40.597792	1844.962918	17.776371
40.823397	1862.727277	17.781389
40.990065	1869.371947	17.786407
41.021036	1877.107917	17.791424
41.219072	1863.167779	17.796442
41.482203	1873.059505	17.801459
41.372609	1878.241290	17.806477
41.733332	1862.728926	17.811495
41.361481	1875.842801	17.816512
41.338399	1879.755519	17.821530
41.724029	1871.816412	17.826547
41.656349	1873.497835	17.831565
41.701785	1839.724278	17.836583
41.094207	1829.146789	17.841600
41.393109	1839.948281	17.846618
41.198430	1858.934265	17.851635
41.134737	1870.495179	17.856653
41.738761	1869.648589	17.861671
41.770346	1865.434236	17.866688
41.824348	1867.665683	17.871706
41.876119	1856.133578	17.876723
41.784811	1875.246240	17.881741
41.975630	1858.771551	17.886759
41.778498	1868.002085	17.891776
41.885116	1861.540506	17.896794
42.129790	1860.213261	17.901811
41.903112	1865.224954	17.906829
41.797226	1872.134893	17.911847
41.719476	1867.031919	17.916864
41.703674	1861.138849	17.921882
42.233006	1860.801248	17.926899
41.789964	1861.765469	17.931917
42.129814	1876.655023	17.936935
42.174113	1886.241889	17.941952
42.394671	1885.939379	17.946970
42.783002	1897.179680	17.951987
42.431690	1881.618844	17.957005
42.589351	1863.950796	17.962023
42.541618	1858.677871	17.967040
42.667643	1865.675085	17.972058
42.751911	1847.767080	17.977075
42.577742	1855.268345	17.982093
42.593193	1852.231613	17.987111
42.695724	1859.311223	17.992128
42.495937	1854.193111	17.997146
42.480817	1849.715653	18.002163
42.439034	1856.245701	18.007181
42.718262	1871.143346	18.012199
42.482962	1883.093436	18.017216
42.291216	1881.713102	18.022234
42.858740	1879.845152	18.027251
42.640561	1891.570722	18.032269
42.451716	1885.794905	18.037287
42.734532	1890.357256	18.042304
42.777024	1906.356059	18.047322
43.284196	1917.556972	18.052339
42.945495	1933.095933	18.057357
43.345463	1912.011894	18.062375
43.387665	1916.203645	18.067392
43.141524	1928.658869	18.072410
43.285858	1916.487461	18.077427
43.070935	1913.482741	18.082445
43.147778	1908.049928	18.087463
43.269593	1915.304241	18.092480
43.357386	1915.324927	18.097498
43.435322	1908.235546	18.102515
43.313691	1915.733182	18.107533
43.305076	1916.094860	18.112551
43.575650	1935.535273	18.117568
43.505477	1939.768549	18.122586
43.960712	1942.717806	18.127603
43.840553	1945.533895	18.132621
44.256287	1940.979823	18.137639
44.041047	1932.329559	18.142656
43.954977	1912.888201	18.147674
44.285049	1899.740222	18.152691
43.495960	1908.211047	18.157709
43.906918	1905.992114	18.162727
43.964272	1911.719863	18.167744
43.997963	1922.684841	18.172762
44.296536	1942.567536	18.177779
43.984735	1933.264136	18.182797
44.241183	1930.023781	18.187815
44.225429	1928.955146	18.192832
43.791582	1936.796745	18.197850
44.243925	1931.881333	18.202867
44.230136	1932.734621	18.207885
44.309891	1930.239748	18.212903
44.183598	1931.328058	18.217920
44.497460	1935.393115	18.222938
44.592862	1932.458445	18.227955
44.311150	1931.449532	18.232973
44.150839	1932.647088	18.237991
44.463371	1932.603614	18.243008
44.526556	1935.620120	18.248026
44.571859	1942.461933	18.253043
44.578303	1949.398036	18.258061
44.869338	1963.559290	18.263079
44.954636	1968.585753	18.268096
44.865414	1961.266604	18.273114
45.117242	1966.252348	18.278131
45.079383	1966.835770	18.283149
45.483010	1962.261600	18.288167
45.266609	1949.243210	18.293184
44.900848	1935.970228	18.298202
45.227930	1916.333981	18.303219
44.859893	1935.901420	18.308237
45.149409	1949.915038	18.313255
45.094534	1956.686319	18.318272
45.105605	1970.082123	18.323290
45.658355	1961.225978	18.328307
45.355591	1978.639025	18.333325
45.636969	1962.123034	18.338343
45.468904	1966.493055	18.343360
45.022227	1965.600114	18.348378
45.359876	1969.142287	18.353395
45.350033	1971.365057	18.358413
45.468794	1967.328679	18.363431
45.661788	1956.138913	18.368448
45.315560	1962.253524	18.373466
45.424078	1961.490682	18.378483
45.300357	1977.050456	18.383501
45.696895	1981.992675	18.388519
45.496660	1981.220876	18.393536
45.430098	1993.452457	18.398554
45.742223	1992.806576	18.403571
45.718745	2003.440958	18.408589
45.556216	2004.321120	18.413607
46.008296	2012.060783	18.418624
45.949857	2027.905930	18.423642
46.028907	2028.928461	18.428659
45.999753	2026.119032	18.433677
46.421258	2032.425828	18.438695
46.260774	2019.184523	18.443712
46.309611	2015.774342	18.448730
46.604389	2019.370556	18.453747
46.996005	2017.080759	18.458765
46.529976	2021.009107	18.463783
46.807179	2013.269690	18.468800
46.694367	2009.850686	18.473818
46.817043	2015.805586	18.478835
46.840757	2008.820759	18.483853
46.741135	1989.090449	18.488871
46.711597	1992.986924	18.493888
46.604358	1995.818265	18.498906
47.285993	1991.311430	18.503923
47.094377	1977.477377	18.508941
46.858055	1982.391547	18.513959
46.773364	1970.654600	18.518976
46.741319	1975.899556	18.523994
47.042245	1988.552294	18.529011
46.930068	2001.314976	18.534029
46.939601	2007.245447	18.539047
47.163333	1999.697037	18.544064
46.559534	2006.623534	18.549082
47.177398	2000.766194	18.554099
47.265993	2003.248549	18.559117
47.213714	2012.207531	18.564135
47.507888	2013.049458	18.569152
47.373547	2004.284000	18.574170
47.233474	2001.753390	18.579187
47.507939	2001.840258	18.584205
47.287855	2004.194093	18.589223
47.576034	1996.973608	18.594240
47.423598	2016.849689	18.599258
47.896140	2024.211712	18.604275
48.178868	2031.375924	18.609293
47.643634	2022.584733	18.614311
47.893249	2010.111736	18.619328
47.905817	2011.443746	18.624346
47.897716	2015.925122	18.629363
48.099152	2016.443638	18.634381
47.775670	2024.824536	18.639399
47.992732	2022.487073	18.644416
47.746090	2030.788078	18.649434
47.947847	2032.044297	18.654451
48.236482	2031.482387	18.659469
48.130347	2037.538285	18.664487
47.914772	2037.959718	18.669504
48.018109	2037.701071	18.674522
47.996073	2041.251866	18.679539
48.225246	2040.158315	18.684557
48.232853	2047.783271	18.689575
48.601858	2060.164088	18.694592
48.989539	2058.946153	18.699610
48.903452	2052.996575	18.704627
49.061846	2037.903264	18.709645
48.358366	2043.986798	18.714663
48.847874	2036.671261	18.719680
48.365456	2037.253231	18.724698
48.736637	2029.192074	18.729715
48.722218	2039.571779	18.734733
48.678822	2066.913477	18.739751
48.901166	2067.596975	18.744768
48.631578	2073.922780	18.749786
48.652682	2065.994518	18.754803
48.793950	2068.276572	18.759821
48.879719	2075.042780	18.764839
49.170520	2071.202306	18.769856
49.061992	2067.411366	18.774874
48.706389	2063.224104	18.779891
49.003206	2075.987687	18.784909
48.987057	2085.313762	18.789927
49.413433	2081.805596	18.794944
49.248200	2085.550704	18.799962
49.139460	2082.082268	18.804979
49.640369	2075.866022	18.809997
49.497831	2090.538578	18.815015
49.297234	2085.407930	18.820032
49.731560	2088.225271	18.825050
49.215986	2090.050516	18.830067
49.177694	2086.389944	18.835085
49.294959	2112.793738	18.840103
49.487728	2105.626170	18.845120
49.573810	2109.469628	18.850138
49.878758	2108.691179	18.855155
50.192963	2100.011426	18.860173
49.800628	2113.507884	18.865191
49.987010	2108.671014	18.870208
50.255233	2105.977735	18.875226
50.225217	2099.574023	18.880243
50.280406	2096.338990	18.885261
50.059132	2107.837136	18.890279
50.578559	2098.064420	18.895296
50.338188	2096.858563	18.900314
50.293467	2099.263096	18.905331
50.794230	2101.849618	18.910349
50.764200	2097.915588	18.915367
50.943472	2095.280544	18.920384
50.424548	2098.501614	18.925402
50.610106	2102.263136	18.930419
51.008043	2096.536792	18.935437
50.730698	2099.912816	18.940455
50.971379	2085.064310	18.945472
50.738360	2104.560103	18.950490
50.721037	2099.744714	18.955507
50.869055	2093.026315	18.960525
50.675695	2109.992628	18.965543
50.842489	2100.545145	18.970560
51.097746	2110.150423	18.975578
50.970207	2118.017197	18.980595
51.269641	2125.597221	18.985613
51.190174	2130.434513	18.990631
51.076198	2122.648889	18.995648
51.138143	2128.773973	19.000666
50.761424	2123.504658	19.005683
51.251115	2126.947114	19.010701
51.278737	2138.537723	19.015719
51.357161	2125.818221	19.020736
51.499388	2118.078254	19.025754
51.395505	2121.942575	19.030771
51.570028	2124.055738	19.035789
51.452056	2125.998472	19.040807
51.760529	2111.312162	19.045824
51.538229	2129.261548	19.050842
51.524215	2139.026198	19.055859
51.866781	2144.942934	19.060877
52.126720	2159.705525	19.065895
52.423563	2150.394572	19.070912
52.310432	2145.001410	19.075930
52.252168	2139.756803	19.080947
52.281560	2118.048869	19.085965
51.852503	2124.714739	19.090983
52.115613	2126.099609	19.096000
52.113134	2136.759055	19.101018
52.060120	2145.604977	19.106035
52.514057	2140.767895	19.111053
52.325754	2152.518797	19.116071
52.436075	2142.908831	19.121088
52.387515	2145.005667	19.126106
52.501276	2152.228349	19.131123
52.330311	2143.833595	19.136141
52.380062	2152.513692	19.141159
52.396054	2148.658826	19.146176
52.793963	2140.533569	19.151194
52.521991	2152.909732	19.156211
52.929493	2141.273472	19.161229
52.862699	2148.952820	19.166247
53.017101	2150.935487	19.171264
53.015852	2157.283023	19.176282
52.862884	2152.235991	19.181299
53.147561	2158.912310	19.186317
52.958454	2173.104731	19.191335
53.452509	2178.522258	19.196352
53.561843	2178.981537	19.201370
53.054922	2177.472114	19.206387
53.447522	2170.046123	19.211405
53.567716	2174.872034	19.216423
53.417932	2178.471553	19.221440
53.629837	2171.713041	19.226458
53.231510	2174.678934	19.231475
53.604182	2168.053660	19.236493
53.643087	2176.021336	19.241511
53.418091	2169.881502	19.246528
53.763787	2166.164385	19.251546
53.560061	2176.786743	19.256563
53.729889	2170.094718	19.261581
53.536277	2172.741665	19.266599
53.405027	2175.204057	19.271616
53.567733	2179.302731	19.276634
53.579247	2187.131634	19.281651
54.050678	2187.640128	19.286669
53.895940	2201.194728	19.291687
53.849793	2205.757737	19.296704
54.322578	2191.968524	19.301722
54.054044	2207.704228	19.306739
54.418828	2211.810008	19.311757
54.275090	2198.899355	19.316775
54.373872	2201.875632	19.321792
54.290292	2192.121951	19.326810
54.094825	2208.599495	19.331827
54.357400	2213.251696	19.336845
54.325814	2221.471317	19.341863
54.559114	2233.738646	19.346880
54.764099	2225.219387	19.351898
54.784988	2229.867669	19.356915
55.124854	2223.964916	19.361933
54.976214	2224.605344	19.366951
54.766161	2227.663918	19.371968
54.838785	2226.184754	19.376986
55.041330	2220.138734	19.382003
55.074120	2221.451808	19.387021
54.901473	2222.947089	19.392039
54.618784	2218.487023	19.397056
55.129981	2210.187927	19.402074
55.046932	2235.145221	19.407091
55.052551	2245.783005	19.412109
55.076410	2261.851240	19.417127
55.239145	2262.235935	19.422144
55.461952	2251.211079	19.427162
55.453391	2260.062565	19.432179
55.693610	2243.477314	19.437197
55.691996	2244.253172	19.442215
55.492014	2244.299307	19.447232
56.001655	2245.710938	19.452250
55.958935	2249.980826	19.457267
55.975578	2243.915681	19.462285
55.877588	2238.845692	19.467303
55.893251	2248.962767	19.472320
55.745974	2243.861311	19.477338
55.842967	2248.325997	19.482355
56.299630	2260.199065	19.487373
56.141983	2263.460078	19.492391
56.213039	2269.256571	19.497408
56.647300	2263.634484	19.502426
56.618487	2271.326715	19.507443
56.600622	2259.983152	19.512461
56.948697	2240.426493	19.517479
56.752432	2240.961257	19.522496
56.779193	2228.138218	19.527514
56.388372	2239.311144	19.532531
56.829445	2219.695634	19.537549
56.809793	2231.879035	19.542567
56.603469	2231.732695	19.547584
56.845239	2232.397374	19.552602
56.551418	2231.324301	19.557619
56.720632	2235.366896	19.562637
56.862841	2246.033233	19.567655
56.788890	2247.407379	19.572672
57.056874	2251.220290	19.577690
56.800670	2264.187076	19.582707
56.871246	2264.586471	19.587725
56.822898	2257.787628	19.592743
57.234556	2268.042910	19.597760
57.304929	2269.976072	19.602778
56.905189	2264.041825	19.607795
56.949876	2273.049999	19.612813
57.354978	2273.643010	19.617831
57.297253	2289.625185	19.622848
57.394830	2288.307207	19.627866
57.246603	2298.115393	19.632883
57.555652	2298.498777	19.637901
57.854174	2285.438857	19.642919
57.567722	2291.567665	19.647936
57.904967	2288.422887	19.652954
57.699654	2294.092006	19.657971
57.484308	2314.961692	19.662989
57.768544	2318.647756	19.668007
58.104168	2328.984423	19.673024
58.307774	2331.137024	19.678042
58.102126	2314.040769	19.683059
58.335064	2317.068034	19.688077
58.733041	2323.564334	19.693095
58.055200	2331.139882	19.698112
58.707602	2312.226739	19.703130
58.565767	2327.045717	19.708147
58.382238	2321.751808	19.713165
58.851175	2321.165851	19.718183
58.698776	2307.897823	19.723200
58.776712	2313.070303	19.728218
58.343401	2316.351697	19.733235
58.489633	2312.353316	19.738253
58.692642	2316.635943	19.743271
58.598172	2322.152109	19.748288
58.879991	2341.751728	19.753306
58.737059	2341.085602	19.758323
59.152972	2341.230140	19.763341
59.653929	2344.798273	19.768359
59.326968	2349.835564	19.773376
59.484541	2345.800757	19.778394
59.537445	2346.034654	19.783411
59.698436	2340.497022	19.788429
59.949519	2334.407033	19.793447
59.495691	2318.553753	19.798464
59.618953	2310.167033	19.803482
59.320848	2300.876940	19.808499
59.242380	2312.766186	19.813517
59.311393	2319.211129	19.818535
59.444522	2330.168421	19.823552
59.869564	2321.382768	19.828570
59.707397	2330.261943	19.833587
59.608311	2336.647185	19.838605
59.828986	2333.763243	19.843623
59.419748	2336.084376	19.848640
59.866465	2342.225263	19.853658
60.473809	2351.176780	19.858675
60.276538	2356.902843	19.863693
60.260861	2364.287066	19.868711
60.033098	2368.447284	19.873728
60.371609	2359.719455	19.878746
60.454341	2357.626742	19.883763
60.339429	2361.044559	19.888781
60.597388	2350.663700	19.893799
60.555991	2367.624167	19.898816
60.541418	2363.537371	19.903834
60.593427	2370.026735	19.908851
60.491261	2356.581545	19.913869
60.566754	2350.760235	19.918887
60.628117	2365.122113	19.923904
61.090149	2356.638862	19.928922
60.802561	2353.455296	19.933939
60.753584	2374.551798	19.938957
61.017149	2377.723633	19.943975
60.673956	2380.403912	19.948992
60.809136	2382.130906	19.954010
60.936096	2382.840646	19.959027
61.072093	2385.780350	19.964045
61.055499	2390.880629	19.969063
61.263501	2415.774508	19.974080
61.446828	2410.691839	19.979098
61.359151	2410.812088	19.984115
61.487250	2423.268608	19.989133
61.662354	2419.623469	19.994151
61.576105	2413.904223	19.999168
61.906869	2409.573567	20.004186
62.218612	2405.891694	20.009203
62.100825	2407.539484	20.014221
62.324484	2408.712804	20.019239
62.233913	2409.542972	20.024256
62.510520	2408.881505	20.029274
62.472456	2408.542367	20.034291
62.161767	2406.062493	20.039309
62.318181	2402.564275	20.044327
62.511921	2402.528739	20.049344
62.538889	2415.115430	20.054362
62.537516	2405.726032	20.059379
62.198288	2402.392597	20.064397
62.346786	2399.867017	20.069415
62.213098	2407.234689	20.074432
62.368362	2398.130996	20.079450
62.582925	2411.862066	20.084467
62.249857	2426.142190	20.089485
62.896154	2422.633478	20.094503
62.813456	2429.907296	20.099520
62.739856	2440.541340	20.104538
63.015279	2438.001016	20.109555
63.051064	2437.229301	20.114573
62.861627	2434.752106	20.119591
62.898202	2440.131795	20.124608
62.939117	2431.586673	20.129626
63.107969	2437.414828	20.134643
62.950981	2453.139299	20.139661
63.130401	2447.855885	20.144679
63.178943	2458.374504	20.149696
63.167151	2457.423178	20.154714
63.408376	2462.605849	20.159731
63.360906	2458.145947	20.164749
63.406197	2461.342389	20.169767
63.861439	2476.634173	20.174784
63.873223	2486.506631	20.179802
63.762559	2489.607611	20.184819
63.597934	2486.280916	20.189837
64.269135	2475.669673	20.194855
64.126085	2477.623532	20.199872
64.116976	2492.203636	20.204890
64.300322	2479.750247	20.209907
64.314619	2474.790472	20.214925
64.422757	2467.276776	20.219943
64.329479	2480.780146	20.224960
64.403882	2485.187158	20.229978
64.444899	2477.711690	20.234995
64.153884	2482.160464	20.240013
64.664424	2478.586872	20.245031
64.950963	2487.381993	20.250048
64.913745	2490.660030	20.255066
64.751017	2494.255398	20.260083
64.435065	2499.739313	20.265101
64.974276	2491.922462	20.270119
65.140976	2503.466011	20.275136
65.009979	2507.977364	20.280154
65.376629	2504.403905	20.285171
64.959528	2506.363721	20.290189
65.435934	2493.272099	20.295207
65.445118	2508.307857	20.300224
65.120364	2502.629762	20.305242
65.248826	2493.719842	20.310259
65.144752	2503.982824	20.315277
65.192171	2497.830865	20.320295
65.271692	2521.430317	20.325312
65.549486	2541.028488	20.330330
66.107833	2529.945974	20.335347
66.090567	2537.288851	20.340365
66.205209	2533.396126	20.345383
66.295837	2515.671909	20.350400
66.378208	2520.255420	20.355418
66.216441	2508.918883	20.360435
65.756664	2505.718698	20.365453
66.153657	2510.067976	20.370471
66.415256	2506.436549	20.375488
66.617322	2518.290660	20.380506
66.718613	2518.705614	20.385523
66.195168	2513.983393	20.390541
66.689127	2508.598668	20.395559
66.519384	2520.368929	20.400576
66.499085	2509.034998	20.405594
66.861981	2513.605228	20.410611
66.850463	2513.463996	20.415629
66.641001	2510.698174	20.420647
66.737202	2511.476536	20.425664
66.680725	2508.412598	20.430682
67.088990	2500.586739	20.435699
66.779232	2511.375694	20.440717
66.648676	2511.542109	20.445735
66.934990	2510.885382	20.450752
66.941201	2501.029865	20.455770
66.959956	2512.588365	20.460787
66.846481	2538.317126	20.465805
66.835020	2547.888153	20.470823
66.900980	2539.368075	20.475840
66.924263	2563.663219	20.480858
67.576225	2560.181889	20.485875
67.350174	2571.525424	20.490893
67.514212	2572.408593	20.495911
67.851660	2573.895703	20.500928
67.441465	2576.403436	20.505946
67.928116	2579.649854	20.510963
67.994112	2589.447665	20.515981
68.104332	2592.258597	20.520999
68.332857	2609.348550	20.526016
68.142700	2601.828087	20.531034
68.902638	2587.863711	20.536051
68.385165	2596.125642	20.541069
68.508484	2592.564228	20.546087
68.526844	2597.372700	20.551104
68.561956	2597.621237	20.556122
68.771039	2585.376021	20.561139
68.721441	2597.610910	20.566157
68.823529	2590.697465	20.571175
69.028622	2593.071676	20.576192
68.605257	2588.581231	20.581210
69.020330	2593.721278	20.586227
68.901791	2591.600067	20.591245
68.661474	2589.034215	20.596263
69.345080	2579.266460	20.601280
69.404296	2588.314985	20.606298
69.333945	2579.324245	20.611315
69.520752	2584.908126	20.616333
69.503013	2589.292898	20.621351
69.301407	2592.992023	20.626368
69.070216	2582.722048	20.631386
69.394459	2588.299743	20.636403
69.442323	2609.648567	20.641421
69.200415	2609.492952	20.646439
69.858146	2608.311348	20.651456
69.704566	2616.409856	20.656474
69.773210	2618.522675	20.661491
69.645544	2619.204607	20.666509
69.852457	2622.498796	20.671527
69.786140	2628.219023	20.676544
69.849166	2632.719135	20.681562
69.939829	2634.542140	20.686579
70.184535	2644.269012	20.691597
70.176692	2653.258270	20.696615
70.557109	2657.018750	20.701632
70.481422	2651.211992	20.706650
70.655215	2648.345692	20.711667
70.890104	2649.676125	20.716685
70.695241	2641.930652	20.721703
70.840583	2636.850817	20.726720
70.505944	2654.703141	20.731738
70.797794	2639.547023	20.736755
70.946414	2642.974002	20.741773
70.553197	2639.342366	20.746791
70.858446	2660.228623	20.751808
70.837938	2668.809331	20.756826
70.976984	2661.020031	20.761843
71.123654	2672.301841	20.766861
71.055137	2672.778490	20.771879
71.325954	2669.895138	20.776896
71.009686	2684.408013	20.781914
71.225126	2695.610443	20.786931
71.720382	2689.513614	20.791949
71.769699	2697.639585	20.796967
71.958991	2700.689624	20.801984
71.877048	2698.235354	20.807002
72.041525	2694.787694	20.812019
72.100169	2692.455729	20.817037
72.165538	2699.533812	20.822055
72.283903	2682.659953	20.827072
72.097273	2697.957596	20.832090
72.324143	2693.068457	20.837107
72.632651	2688.200907	20.842125
72.468135	2696.940672	20.847143
72.480984	2680.701876	20.852160
72.459124	2695.004991	20.857178
72.505558	2687.899805	20.862195
72.704740	2685.765662	20.867213
72.312434	2689.319037	20.872231
72.896001	2697.638243	20.877248
72.700448	2716.656158	20.882266
73.018656	2717.917464	20.887283
73.085771	2719.899974	20.892301
72.809910	2727.081258	20.897319
73.610121	2718.285088	20.902336
73.524399	2710.530037	20.907354
73.387154	2713.471700	20.912371
73.489087	2725.170481	20.917389
73.377666	2719.607721	20.922407
73.461664	2711.934146	20.927424
73.166496	2711.618701	20.932442
73.537545	2706.314858	20.937459
73.612550	2707.367973	20.942477
73.330150	2714.654906	20.947495
73.458811	2731.178878	20.952512
73.684342	2734.446527	20.957530
73.827098	2738.189873	20.962547
73.820970	2747.029470	20.967565
73.608534	2736.504696	20.972583
74.137577	2736.801097	20.977600
74.006425	2747.657700	20.982618
74.138022	2760.959501	20.987635
74.409835	2765.150274	20.992653
74.087523	2771.661761	20.997671
74.526091	2765.728894	21.002688
74.788287	2758.767811	21.007706
75.034456	2765.066715	21.012723
74.882356	2767.239931	21.017741
74.600372	2770.218061	21.022759
75.114022	2768.119488	21.027776
74.867891	2773.121220	21.032794
75.096716	2767.726773	21.037811
75.408238	2753.403511	21.042829
74.895070	2771.028033	21.047847
75.067659	2776.119511	21.052864
74.938594	2786.262401	21.057882
75.048033	2795.164611	21.062899
75.178669	2794.000988	21.067917
75.171456	2800.809107	21.072935
75.338964	2790.325166	21.077952
75.595484	2793.192246	21.082970
75.694924	2812.346507	21.087987
75.893975	2827.567831	21.093005
75.798628	2820.920161	21.098023
75.944967	2835.161979	21.103040
76.052917	2830.398732	21.108058
76.315705	2823.771813	21.113075
76.263942	2822.133092	21.118093
76.097760	2818.691731	21.123111
76.318909	2817.580528	21.128128
76.108125	2820.470229	21.133146
75.905880	2822.672688	21.138163
76.152557	2824.529827	21.143181
76.386158	2838.852119	21.148199
76.449269	2833.429018	21.153216
76.492963	2836.602201	21.158234
76.425910	2844.657146	21.163251
76.865276	2855.901070	21.168269
76.630046	2863.980488	21.173287
76.857855	2862.579550	21.178304
76.936793	2873.600168	21.183322
76.859638	2870.011667	21.188339
77.704598	2857.149612	21.193357
77.344956	2857.737195	21.198375
77.593757	2868.630039	21.203392
77.699958	2866.518565	21.208410
77.637332	2854.389608	21.213427
77.660880	2858.690006	21.218445
77.755802	2860.193016	21.223463
77.890709	2853.785479	21.228480
77.941569	2866.926423	21.233498
78.019938	2886.160438	21.238515
78.522321	2879.105147	21.243533
78.303097	2873.952803	21.248551
77.935397	2854.898041	21.253568
78.331025	2854.020934	21.258586
78.148274	2872.004253	21.263603
78.427704	2875.692015	21.268621
78.272386	2882.734592	21.273639
78.208428	2884.872531	21.278656
78.497135	2876.954635	21.283674
78.598604	2879.564085	21.288691
78.948240	2869.976826	21.293709
78.893395	2884.032113	21.298727
78.798690	2883.758630	21.303744
78.672238	2881.363341	21.308762
78.636733	2905.312904	21.313779
78.993078	2907.611918	21.318797
78.661615	2913.272290	21.323815
79.071107	2906.091792	21.328832
78.894998	2907.885800	21.333850
79.137646	2926.882083	21.338867
79.348672	2928.867626	21.343885
79.541460	2935.212873	21.348903
79.660336	2940.848628	21.353920
79.476177	2938.912449	21.358938
79.576814	2940.332752	21.363955
80.299319	2926.838103	21.368973
79.742987	2943.685508	21.373991
79.961502	2961.274583	21.379008
80.353704	2961.923173	21.384026
80.326005	2971.596962	21.389043
80.495083	2963.644612	21.394061
80.462856	2963.028445	21.399079
80.424053	2965.027094	21.404096
80.744579	2964.028242	21.409114
80.426433	2964.204914	21.414131
80.702384	2960.920324	21.419149
80.563537	2968.727220	21.424167
80.335728	2958.203164	21.429184
80.799041	2955.233998	21.434202
80.570981	2979.388223	21.439219
80.952914	2983.349124	21.444237
81.043652	2987.519286	21.449255
81.106471	2992.342822	21.454272
81.128155	2992.118419	21.459290
80.977037	2994.016212	21.464307
81.583058	2985.524583	21.469325
81.577770	2996.766381	21.474343
81.686793	3011.209393	21.479360
82.189266	3007.714048	21.484378
81.441379	3010.985195	21.489395
81.757522	3001.932554	21.494413
81.858548	3022.367375	21.499431
81.822644	3011.396578	21.504448
82.013154	3013.849483	21.509466
82.375044	3007.759636	21.514483
82.446319	3010.796314	21.519501
82.072963	3010.092965	21.524519
82.224692	3011.280169	21.529536
82.716248	3004.728377	21.534554
82.269591	3015.860456	21.539571
82.416141	3012.645260	21.544589
82.464817	3011.946969	21.549607
82.189079	3017.688163	21.554624
82.618181	3028.587768	21.559642
82.668220	3046.651374	21.564659
83.183580	3038.335421	21.569677
82.787470	3029.228815	21.574695
83.122851	3037.583082	21.579712
83.367364	3029.266281	21.584730
83.080998	3058.456133	21.589747
83.385336	3057.495253	21.594765
83.519382	3058.526392	21.599783
83.665159	3062.609141	21.604800
83.552195	3066.718997	21.609818
83.684246	3079.349283	21.614835
84.217449	3066.055384	21.619853
83.979472	3069.701435	21.624871
83.620814	3069.995475	21.629888
84.000301	3067.876571	21.634906
83.715682	3069.917584	21.639923
83.972998	3076.504305	21.644941
84.345638	3077.410872	21.649959
84.513713	3095.485604	21.654976
85.081474	3084.962003	21.659994
84.866861	3088.730971	21.665011
85.096793	3073.110761	21.670029
84.988774	3072.177101	21.675047
84.503564	3087.810656	21.680064
84.848281	3072.224842	21.685082
84.584050	3094.823676	21.690099
84.991846	3091.466117	21.695117
85.209022	3081.699269	21.700135
85.264754	3087.463137	21.705152
85.085224	3082.176176	21.710170
85.186253	3090.360193	21.715187
85.326937	3080.111575	21.720205
85.161798	3095.897029	21.725223
85.360063	3117.232050	21.730240
85.461379	3111.506214	21.735258
85.737665	3116.306759	21.740275
85.702946	3109.664233	21.745293
85.879125	3120.362765	21.750311
85.870624	3111.972215	21.755328
85.825577	3101.378792	21.760346
85.982906	3123.488049	21.765363
86.244475	3126.086956	21.770381
86.262861	3133.310393	21.775399
85.988027	3137.668686	21.780416
86.184088	3137.843583	21.785434
86.759727	3143.571753	21.790451
86.272365	3136.730033	21.795469
86.623200	3131.481963	21.800487
86.736712	3164.856561	21.805504
87.292736	3154.980564	21.810522
87.051628	3158.461954	21.815539
86.957453	3163.500150	21.820557
87.220786	3148.730331	21.825575
87.037865	3168.178650	21.830592
87.544628	3145.962793	21.835610
87.422374	3162.918989	21.840627
87.255794	3151.483608	21.845645
87.523994	3158.739583	21.850663
87.299509	3156.635184	21.855680
87.729249	3164.144635	21.860698
87.617063	3179.322361	21.865715
87.726921	3192.506891	21.870733
87.873074	3178.876608	21.875751
87.532505	3198.298980	21.880768
87.698613	3188.735277	21.885786
88.005231	3197.811586	21.890803
88.288694	3206.447174	21.895821
88.330795	3205.914318	21.900839
88.332160	3224.228175	21.905856
88.494865	3212.470433	21.910874
88.281715	3221.364571	21.915891
88.406802	3210.251536	21.920909
88.586284	3236.778022	21.925927
88.842780	3238.497572	21.930944
89.207310	3234.560876	21.935962
89.133675	3241.553629	21.940979
89.114803	3245.201750	21.945997
89.165635	3235.116804	21.951015
89.275718	3249.188615	21.956032
89.150117	3243.036405	21.961050
89.557367	3260.130871	21.966067
89.601279	3275.231101	21.971085
89.937926	3257.193018	21.976103
89.914414	3271.544943	21.981120
90.118981	3272.317864	21.986138
89.914460	3269.359966	21.991155
90.123979	3258.953941	21.996173
90.073981	3265.659765	22.001191
89.821268	3249.964528	22.006208
90.219097	3251.933698	22.011226
90.175440	3266.181855	22.016243
90.508444	3279.391444	22.021261
90.902154	3292.504838	22.026279
90.663101	3289.188254	22.031296
90.849169	3284.915031	22.036314
91.114257	3290.772232	22.041331
90.887581	3284.626685	22.046349
91.286727	3279.705158	22.051367
91.099005	3292.944316	22.056384
91.271415	3278.737904	22.061402
91.384047	3276.699285	22.066419
91.348029	3278.148496	22.071437
91.805792	3276.297105	22.076455
91.395489	3286.204382	22.081472
91.424523	3287.096542	22.086490
91.560795	3281.092119	22.091507
91.447796	3284.020590	22.096525
91.733873	3275.230576	22.101543
91.593112	3295.720859	22.106560
91.815528	3306.206855	22.111578
91.598472	3312.435141	22.116595
92.008303	3312.154339	22.121613
92.037464	3305.503108	22.126631
91.886842	3323.782334	22.131648
92.290100	3327.335624	22.136666
92.750080	3335.607266	22.141683
92.214534	3334.355555	22.146701
92.401118	3344.004856	22.151719
92.457165	3351.747838	22.156736
92.816442	3359.462129	22.161754
92.954618	3368.951623	22.166771
92.890214	3370.530438	22.171789
93.274729	3363.283696	22.176807
93.183118	3364.431864	22.181824
93.416564	3371.686410	22.186842
93.655353	3370.844514	22.191859
93.360348	3371.438324	22.196877
93.614969	3380.913188	22.201895
93.556125	3396.118816	22.206912
93.844152	3392.955700	22.211930
93.653670	3393.218991	22.216947
93.641416	3395.414832	22.221965
94.062722	3377.757182	22.226983
94.226581	3402.240539	22.232000
94.223676	3407.420795	22.237018
94.960703	3402.673455	22.242035
94.839222	3411.097651	22.247053
94.854125	3410.123915	22.252071
94.808068	3414.531542	22.257088
95.211398	3411.864466	22.262106
95.253507	3403.973029	22.267123
94.911190	3390.487309	22.272141
95.243711	3392.196327	22.277159
95.196393	3391.162508	22.282176
95.226509	3401.443263	22.287194
95.394519	3397.586634	22.292211
95.393385	3403.760859	22.297229
95.368489	3399.382020	22.302247
95.306053	3406.552408	22.307264
95.343634	3395.720629	22.312282
95.665845	3391.001691	22.317299
95.394236	3411.269159	22.322317
95.879535	3414.272931	22.327335
95.940663	3424.120850	22.332352
95.719662	3433.865889	22.337370
95.817188	3430.218714	22.342387
95.989342	3429.886143	22.347405
96.077268	3439.559894	22.352423
96.315869	3456.163122	22.357440
96.174119	3464.669241	22.362458
96.403138	3463.936663	22.367475
96.233188	3463.714497	22.372493
96.799345	3466.724264	22.377511
96.852391	3487.592150	22.382528
96.965725	3494.298776	22.387546
97.389292	3485.482778	22.392563
97.133434	3488.006163	22.397581
97.519854	3482.793985	22.402599
97.237827	3491.888053	22.407616
97.143506	3499.588232	22.412634
97.412386	3481.342794	22.417651
97.436127	3508.634013	22.422669
97.869817	3515.111788	22.427687
97.872311	3515.787947	22.432704
98.013542	3528.007341	22.437722
98.118735	3517.646874	22.442739
97.891176	3525.072554	22.447757
98.076892	3513.996816	22.452775
98.311882	3509.123418	22.457792
98.260619	3533.668046	22.462810
98.462259	3535.220969	22.467827
98.521960	3547.231560	22.472845
98.815127	3537.523871	22.477863
99.029666	3536.685835	22.482880
99.010446	3545.758476	22.487898
99.253380	3533.753276	22.492915
98.847150	3532.552504	22.497933
98.967092	3532.925971	22.502951
98.675727	3556.164630	22.507968
98.709030	3561.616049	22.512986
99.259796	3573.261240	22.518003
99.607007	3569.882560	22.523021
99.724487	3587.463333	22.528039
99.622383	3591.025701	22.533056
99.623241	3590.505703	22.538074
100.099596	3589.932685	22.543091
100.493062	3589.984077	22.548109
100.646868	3584.381048	22.553127
100.663410	3584.601100	22.558144
100.515483	3585.305970	22.563162
100.807877	3576.775135	22.568179
100.776947	3585.213308	22.573197
100.682899	3585.144222	22.578215
100.557543	3581.055874	22.583232
100.857652	3574.313329	22.588250
100.941068	3573.672400	22.593267
100.534637	3581.345309	22.598285
101.149527	3591.407085	22.603303
101.002889	3603.636267	22.608320
100.931440	3612.207560	22.613338
101.738552	3610.368852	22.618355
101.442555	3613.661664	22.623373
101.619065	3607.966906	22.628391
101.646129	3598.369262	22.633408
101.800944	3598.591648	22.638426
101.710697	3606.238531	22.643443
101.781905	3628.997078	22.648461
101.699303	3627.511851	22.653479
102.051191	3621.957453	22.658496
101.750958	3631.668062	22.663514
102.451254	3638.531289	22.668531
102.309674	3654.120870	22.673549
102.400308	3658.473734	22.678567
102.560630	3660.153611	22.683584
102.659273	3662.172912	22.688602
102.934375	3652.895942	22.693619
102.945448	3655.275313	22.698637
103.051771	3670.163055	22.703655
103.178743	3684.393847	22.708672
103.089021	3687.569613	22.713690
103.559037	3675.792384	22.718707
103.520437	3679.922016	22.723725
103.627502	3686.335539	22.728743
103.903008	3676.449655	22.733760
103.790987	3681.555377	22.738778
103.646853	3670.381094	22.743795
103.674566	3690.432094	22.748813
104.108521	3700.215237	22.753831
104.093256	3710.646609	22.758848
103.838720	3707.470840	22.763866
104.491339	3706.950730	22.768883
104.413609	3712.784113	22.773901
104.342889	3719.022271	22.778919
104.890374	3718.522074	22.783936
104.949046	3735.774163	22.788954
104.704411	3731.071572	22.793971
104.699069	3747.296344	22.798989
104.990594	3731.520089	22.804007
105.304826	3741.377415	22.809024
105.167338	3766.688971	22.814042
105.607349	3761.177890	22.819059
105.497301	3755.940958	22.824077
105.452923	3763.925144	22.829095
105.757913	3760.830828	22.834112
105.489953	3766.963590	22.839130
105.759794	3764.440453	22.844147
105.806367	3773.069320	22.849165
106.047357	3778.730764	22.854183
105.872893	3775.524905	22.859200
106.033699	3786.281441	22.864218
106.556048	3772.416772	22.869235
106.628212	3779.029408	22.874253
106.605877	3779.342977	22.879271
107.152000	3779.695685	22.884288
107.414335	3789.776065	22.889306
107.370916	3786.503682	22.894323
107.197194	3776.045921	22.899341
106.945586	3785.578182	22.904359
107.661682	3775.896498	22.909376
107.453045	3777.905822	22.914394
107.702127	3787.239459	22.919411
107.858396	3777.917645	22.924429
107.867529	3801.616923	22.929447
108.276972	3794.649177	22.934464
108.020125	3786.386731	22.939482
108.289265	3786.159825	22.944499
108.294091	3784.528489	22.949517
108.298912	3786.580862	22.954535
108.508521	3792.009758	22.959552
108.300493	3796.771348	22.964570
108.360278	3793.959979	22.969587
108.663492	3787.441027	22.974605
108.348675	3799.622464	22.979623
108.593861	3791.581228	22.984640
108.615744	3804.538851	22.989658
108.633757	3820.909437	22.994675
108.505391	3829.946171	22.999693
108.615334	3824.652106	23.004711
109.125624	3843.778388	23.009728
109.069617	3853.450982	23.014746
109.321307	3849.035767	23.019763
109.486621	3862.768984	23.024781
109.723516	3864.842568	23.029799
110.001302	3879.702394	23.034816
110.236574	3876.885836	23.039834
110.260801	3876.490319	23.044851
110.395986	3869.711798	23.049869
110.556892	3887.675384	23.054887
110.688994	3861.063577	23.059904
110.559354	3880.603458	23.064922
110.477874	3874.959179	23.069939
110.785800	3871.110793	23.074957
110.395726	3894.386966	23.079975
110.887538	3891.284857	23.084992
111.175480	3909.139323	23.090010
111.173298	3904.648156	23.095027
111.407182	3902.711256	23.100045
111.482473	3910.716556	23.105063
111.583322	3902.052462	23.110080
111.811200	3899.414855	23.115098
111.741633	3896.548579	23.120115
111.827541	3905.621198	23.125133
112.179928	3929.984129	23.130151
112.091317	3919.214563	23.135168
112.185569	3926.671721	23.140186
112.021632	3928.334903	23.145203
112.249890	3941.051282	23.150221
111.819829	3931.786689	23.155239
112.028027	3924.660612	23.160256
112.209095	3952.513603	23.165274
112.424903	3955.913662	23.170291
112.543681	3956.842682	23.175309
112.622331	3964.660259	23.180327
113.090845	3977.265201	23.185344
113.315284	3983.518545	23.190362
113.366144	3985.657212	23.195379
113.208492	3987.596290	23.200397
113.648517	3985.781471	23.205415
113.749224	3966.306798	23.210432
113.455023	3980.314780	23.215450
113.718323	3998.756960	23.220467
113.777825	4014.757726	23.225485
114.113036	4003.888261	23.230503
114.202191	4004.367339	23.235520
114.026205	4007.126646	23.240538
114.281541	4010.679312	23.245555
114.503991	4023.626384	23.250573
114.760085	4017.453882	23.255591
114.988096	4021.976097	23.260608
115.179076	4017.663335	23.265626
115.447981	4025.166634	23.270643
115.467515	4011.053115	23.275661
115.401303	4028.833625	23.280679
115.389647	4021.541186	23.285696
115.449949	4009.374359	23.290714
115.863550	4005.947237	23.295731
115.872564	4021.251246	23.300749
115.170963	4022.715421	23.305767
115.866501	4025.870656	23.310784
115.920364	4047.966350	23.315802
115.780694	4048.386738	23.320819
116.005597	4046.592844	23.325837
115.913557	4060.618222	23.330855
116.071596	4069.459971	23.335872
116.094345	4081.108752	23.340890
116.315973	4079.374373	23.345907
116.461939	4089.353951	23.350925
116.581889	4111.796332	23.355943
116.937318	4102.162513	23.360960
117.067821	4111.065315	23.365978
117.011837	4114.571684	23.370995
117.531201	4113.874586	23.376013
117.458202	4134.583358	23.381031
117.611479	4128.586892	23.386048
117.680478	4138.777795	23.391066
117.726078	4136.635687	23.396083
118.199990	4132.512976	23.401101
118.142952	4138.841952	23.406119
118.128164	4133.844562	23.411136
118.496932	4121.161979	23.416154
118.305187	4146.564653	23.421171
118.648653	4136.684143	23.426189
118.535921	4158.778252	23.431207
118.700447	4160.245126	23.436224
118.715556	4156.513373	23.441242
118.909385	4161.370682	23.446259
119.011746	4161.452770	23.451277
118.688216	4163.515865	23.456295
119.023297	4171.242317	23.461312
119.284199	4172.503459	23.466330
118.889586	4179.339386	23.471347
119.470684	4177.017482	23.476365
119.245496	4205.300737	23.481383
119.715596	4205.737953	23.486400
119.902582	4217.290641	23.491418
119.911904	4222.325282	23.496435
120.390047	4214.256107	23.501453
120.111380	4227.988884	23.506471
120.265682	4237.598302	23.511488
120.683077	4238.246876	23.516506
120.290638	4244.232132	23.521523
121.073352	4241.558692	23.526541
120.936711	4247.183782	23.531559
120.997888	4239.821409	23.536576
121.377143	4259.050944	23.541594
121.300890	4274.884850	23.546611
121.547673	4262.009993	23.551629
121.482448	4268.487432	23.556647
121.347664	4267.622466	23.561664
121.889137	4259.185247	23.566682
121.645672	4277.168957	23.571699
121.820456	4286.383395	23.576717
122.016345	4297.930007	23.581735
122.013630	4288.119547	23.586752
121.898857	4291.245159	23.591770
122.267272	4312.197661	23.596787
122.685681	4307.644807	23.601805
122.672151	4331.375302	23.606823
122.795276	4323.282444	23.611840
123.404609	4321.096038	23.616858
122.937795	4327.021602	23.621875
123.511303	4316.622077	23.626893
123.373657	4318.864798	23.631911
123.538958	4314.266560	23.636928
124.065439	4326.107387	23.641946
123.659509	4337.812931	23.646963
123.747563	4328.942167	23.651981
123.878969	4341.389576	23.656999
123.877516	4333.342537	23.662016
124.322191	4328.212813	23.667034
123.815694	4339.117862	23.672051
124.740116	4339.886969	23.677069
124.605489	4364.513148	23.682087
124.522319	4361.415316	23.687104
124.478000	4361.948731	23.692122
124.694337	4363.351513	23.697139
124.909837	4367.250450	23.702157
124.592574	4370.824504	23.707175
125.146981	4379.571768	23.712192
125.362264	4380.123571	23.717210
125.133541	4399.044333	23.722227
125.110498	4391.848709	23.727245
125.315781	4401.424146	23.732263
125.552797	4425.416124	23.737280
125.520669	4418.506703	23.742298
125.617832	4433.823832	23.747315
126.052183	4432.091677	23.752333
126.104675	4440.341617	23.757351
126.337693	4434.857792	23.762368
126.819657	4432.061577	23.767386
126.709689	4437.703726	23.772403
127.097390	4433.134492	23.777421
127.390656	4435.625534	23.782439
127.157622	4432.889057	23.787456
127.143914	4436.056795	23.792474
126.780182	4459.788277	23.797491
127.346797	4461.083293	23.802509
127.330776	4470.205556	23.807527
126.891329	4484.887738	23.812544
127.736940	4483.784609	23.817562
127.556547	4493.194265	23.822579
127.634936	4498.971598	23.827597
127.990575	4514.798251	23.832615
128.487787	4519.546730	23.837632
128.588465	4523.414460	23.842650
128.499457	4534.060347	23.847667
128.741830	4518.083412	23.852685
129.067273	4518.395031	23.857703
129.126788	4524.585230	23.862720
129.068025	4520.039965	23.867738
129.137092	4533.815907	23.872755
129.306941	4549.296990	23.877773
129.329794	4548.538241	23.882791
129.601121	4543.838853	23.887808
129.768745	4543.086124	23.892826
129.859355	4551.180584	23.897843
130.173870	4552.123270	23.902861
130.232674	4574.097037	23.907879
130.183289	4582.302730	23.912896
130.687722	4555.288884	23.917914
130.725971	4570.418101	23.922931
130.637306	4575.639192	23.927949
130.733541	4569.086038	23.932967
130.994069	4566.047420	23.937984
130.762455	4550.120073	23.943002
130.586537	4573.574779	23.948019
130.695385	4589.576172	23.953037
131.040446	4589.581802	23.958055
131.031551	4595.261387	23.963072
131.362132	4618.433226	23.968090
131.233041	4628.534126	23.973107
131.587881	4625.980772	23.978125
131.713834	4641.800922	23.983143
131.637984	4660.692923	23.988160
132.252278	4655.954543	23.993178
132.394047	4673.548483	23.998195
132.265864	4657.761858	24.003213
132.931087	4660.420971	24.008231
132.484008	4668.257466	24.013248
132.961515	4675.926863	24.018266
133.042605	4693.547809	24.023283
133.160071	4684.239476	24.028301
133.241685	4682.684689	24.033319
133.232111	4688.165392	24.038336
133.557509	4679.984230	24.043354
133.485008	4706.056397	24.048371
133.662977	4705.567116	24.053389
134.123669	4699.504091	24.058407
134.047017	4712.257177	24.063424
134.396824	4703.859711	24.068442
134.331664	4707.779108	24.073459
134.088637	4706.682003	24.078477
134.383638	4723.727652	24.083495
134.800876	4740.614589	24.088512
134.850098	4746.472977	24.093530
134.788484	4738.890788	24.098547
135.114682	4745.435034	24.103565
135.422188	4738.634929	24.108583
135.044956	4753.374322	24.113600
135.307570	4756.993666	24.118618
135.686287	4757.495823	24.123635
135.520427	4760.800386	24.128653
135.954478	4777.956085	24.133671
135.765298	4778.603080	24.138688
136.351043	4784.061263	24.143706
136.106718	4795.956160	24.148723
136.169967	4801.395400	24.153741
136.459372	4809.769036	24.158759
136.464672	4827.029348	24.163776
136.508813	4822.203259	24.168794
136.670226	4823.521232	24.173811
136.915343	4840.174557	24.178829
137.182861	4851.075343	24.183847
137.360136	4857.773187	24.188864
137.949253	4853.232282	24.193882
137.735669	4858.986301	24.198899
137.674611	4859.138507	24.203917
138.109215	4852.182776	24.208935
138.165779	4867.753061	24.213952
138.492301	4877.495918	24.218970
138.301104	4875.064994	24.223987
138.188405	4867.674178	24.229005
138.397362	4871.715109	24.234023
138.466583	4875.461295	24.239040
138.650637	4874.342488	24.244058
138.775327	4895.763428	24.249075
138.911431	4892.539264	24.254093
139.368460	4892.054253	24.259111
139.195465	4898.810329	24.264128
139.386387	4890.962804	24.269146
139.732473	4893.127688	24.274163
139.847302	4908.657259	24.279181
139.787890	4918.569459	24.284199
140.135245	4929.843043	24.289216
140.192961	4920.383607	24.294234
140.248629	4922.606606	24.299251
140.074224	4922.918488	24.304269
140.291650	4937.417706	24.309287
140.389340	4953.181339	24.314304
140.431930	4949.482762	24.319322
140.509047	4958.423701	24.324339
140.525833	4971.762346	24.329357
140.980120	4975.442436	24.334375
141.025234	5001.009417	24.339392
141.402199	4990.709992	24.344410
141.450291	5010.540064	24.349427
141.759645	5007.090793	24.354445
142.237591	5021.499779	24.359463
142.364423	5040.908263	24.364480
142.371011	5030.479853	24.369498
142.632544	5033.308826	24.374515
142.631098	5042.407880	24.379533
142.783984	5035.821098	24.384551
142.859912	5035.537668	24.389568
143.065818	5027.054404	24.394586
143.080197	5047.717489	24.399603
143.163851	5057.788693	24.404621
143.732361	5058.771942	24.409639
143.561995	5061.535267	24.414656
143.763227	5057.686285	24.419674
143.777235	5051.947656	24.424691
143.648824	5064.677834	24.429709
143.742198	5078.404784	24.434727
143.912861	5087.781654	24.439744
143.970388	5082.287813	24.444762
144.462145	5099.071240	24.449779
144.438386	5119.916725	24.454797
144.730818	5112.702698	24.459815
145.105406	5113.374665	24.464832
144.753380	5122.973361	24.469850
145.092357	5134.705503	24.474867
145.156063	5144.362217	24.479885
145.369810	5144.841135	24.484903
145.021279	5145.464780	24.489920
145.836342	5163.863716	24.494938
145.969407	5171.381401	24.499955
146.105752	5181.285377	24.504973
146.169147	5175.481397	24.509991
146.383807	5170.901771	24.515008
146.259079	5171.919261	24.520026
146.655420	5184.987532	24.525043
146.801410	5190.082527	24.530061
146.948312	5195.021615	24.535079
146.996732	5195.974522	24.540096
146.882681	5197.972885	24.545114
147.240268	5193.772460	24.550131
147.169496	5231.923313	24.555149
147.703650	5218.804341	24.560167
147.425743	5216.590938	24.565184
147.399799	5227.265031	24.570202
147.726994	5238.475200	24.575219
147.835844	5244.693238	24.580237
148.351884	5244.316812	24.585255
148.099196	5260.269594	24.590272
148.622414	5273.531694	24.595290
149.042417	5278.948053	24.600307
148.955504	5279.045383	24.605325
149.008081	5288.408957	24.610343
149.234285	5276.150906	24.615360
149.113894	5285.300544	24.620378
149.704772	5300.233042	24.625395
149.796133	5303.536832	24.630413
150.041530	5297.743118	24.635431
149.751079	5294.918868	24.640448
149.791029	5297.674661	24.645466
150.220743	5307.994520	24.650483
150.282767	5328.783354	24.655501
150.501583	5327.721907	24.660519
150.671850	5329.134493	24.665536
150.609792	5324.662666	24.670554
151.145278	5345.091244	24.675571
150.895879	5354.827917	24.680589
151.085647	5358.559725	24.685607
151.433736	5355.286712	24.690624
151.698264	5378.117059	24.695642
152.176097	5364.565602	24.700659
151.727463	5384.462010	24.705677
151.878143	5381.235416	24.710695
152.063802	5385.066224	24.715712
152.094470	5394.534843	24.720730
152.177326	5402.145615	24.725747
152.259779	5406.692261	24.730765
152.613860	5411.503195	24.735783
153.124254	5418.484887	24.740800
152.979830	5439.530219	24.745818
153.422370	5431.658808	24.750835
153.244934	5424.278034	24.755853
153.491965	5434.404475	24.760871
153.587754	5437.130151	24.765888
153.782415	5459.193717	24.770906
154.189120	5463.949076	24.775923
154.123367	5469.976346	24.780941
154.059374	5462.306839	24.785959
154.051817	5470.858799	24.790976
154.247093	5500.572233	24.795994
154.933540	5498.212097	24.801011
154.916740	5498.706548	24.806029
154.702210	5492.369318	24.811047
155.008698	5490.858834	24.816064
155.185880	5521.023615	24.821082
155.501347	5523.069180	24.826099
155.523500	5525.829428	24.831117
155.650610	5515.420005	24.836135
155.721210	5525.672193	24.841152
155.915913	5550.128262	24.846170
156.251268	5545.331027	24.851187
156.306344	5552.139933	24.856205
156.420982	5547.146598	24.861223
156.629191	5559.721256	24.866240
156.837354	5563.786108	24.871258
156.988879	5564.189212	24.876275
156.978996	5567.686214	24.881293
157.172232	5573.531410	24.886311
157.461051	5577.963385	24.891328
157.448637	5601.230019	24.896346
157.731245	5597.912325	24.901363
157.435920	5606.122402	24.906381
157.830389	5608.597513	24.911399
158.245758	5613.726014	24.916416
158.405562	5623.651723	24.921434
158.727613	5625.538911	24.926451
158.714611	5634.987112	24.931469
158.695135	5632.181739	24.936487
159.219093	5655.420363	24.941504
159.167083	5655.330399	24.946522
159.416824	5654.015398	24.951539
159.452130	5654.007491	24.956557
159.378818	5659.226516	24.961575
159.728236	5672.359349	24.966592
159.805000	5680.629717	24.971610
160.211326	5673.730038	24.976627
160.209793	5680.508693	24.981645
160.402352	5693.517081	24.986663
160.663147	5699.969913	24.991680
160.610746	5709.051541	24.996698
160.857651	5707.134364	25.001715
160.989828	5714.797225	25.006733
160.989302	5724.953900	25.011751
161.421712	5717.762103	25.016768
161.615549	5730.061488	25.021786
161.506363	5735.700860	25.026803
161.524473	5751.943775	25.031821
161.737650	5758.228787	25.036839
161.876770	5756.599421	25.041856
162.196933	5782.199428	25.046874
162.286731	5798.914796	25.051891
162.639380	5788.778401	25.056909
162.240695	5796.680934	25.061927
162.411910	5804.033156	25.066944
162.622739	5824.911465	25.071962
163.332675	5822.575859	25.076979
163.520885	5813.987973	25.081997
163.501683	5825.474894	25.087015
163.795639	5838.080174	25.092032
163.871420	5850.293849	25.097050
164.209903	5842.015557	25.102067
163.973402	5844.427678	25.107085
163.910806	5846.891531	25.112103
164.589914	5864.309173	25.117120
164.869408	5873.088591	25.122138
164.657028	5875.725808	25.127155
164.745924	5882.779652	25.132173
164.753911	5893.522770	25.137191
165.719018	5898.061787	25.142208
165.315861	5911.498924	25.147226
165.450152	5903.708671	25.152243
166.123199	5907.030777	25.157261
166.058829	5924.438013	25.162279
166.197838	5931.564924	25.167296
166.015433	5934.136794	25.172314
166.149000	5934.799246	25.177331
166.806980	5951.149624	25.182349
166.808008	5958.952320	25.187367
166.805610	5957.236928	25.192384
166.573396	5967.857119	25.197402
166.978435	5973.971594	25.202419
167.407012	5982.424416	25.207437
167.523942	5993.586084	25.212455
167.680644	5992.293756	25.217472
167.664743	6008.584860	25.222490
168.036782	6023.028243	25.227507
168.223382	6018.113750	25.232525
168.383127	6031.825501	25.237543
168.908304	6037.343385	25.242560
168.645691	6046.210917	25.247578
168.796477	6062.464488	25.252595
169.192867	6044.920134	25.257613
169.078037	6064.004242	25.262631
169.595230	6070.591012	25.267648
169.649493	6081.092440	25.272666
169.516173	6076.705700	25.277683
169.966989	6094.381090	25.282701
169.779917	6111.371472	25.287719
170.276399	6092.955131	25.292736
170.264820	6113.729272	25.297754
170.500304	6132.821340	25.302771
171.022177	6129.874484	25.307789
170.793877	6135.779249	25.312807
171.044165	6141.022374	25.317824
171.399186	6155.522099	25.322842
171.310415	6164.542147	25.327859
171.545159	6156.562661	25.332877
171.414180	6164.563529	25.337895
171.865368	6166.975410	25.342912
171.714706	6172.925243	25.347930
171.746717	6185.270480	25.352947
172.226717	6180.804800	25.357965
172.305150	6208.623364	25.362983
172.279583	6208.912323	25.368000
172.474095	6215.312225	25.373018
172.947902	6231.265868	25.378035
173.365816	6235.066948	25.383053
173.324519	6242.027645	25.388071
173.805403	6228.875370	25.393088
173.808247	6262.122031	25.398106
174.113210	6267.893831	25.403123
174.476426	6265.086325	25.408141
174.248648	6267.738653	25.413159
174.970889	6270.149032	25.418176
174.856895	6256.086908	25.423194
175.009032	6272.757471	25.428211
175.464659	6273.365441	25.433229
175.321820	6294.426685	25.438247
175.294328	6281.696869	25.443264
175.449371	6284.157562	25.448282
175.319698	6293.851371	25.453299
176.090365	6296.450720	25.458317
175.635849	6316.556227	25.463335
175.975875	6312.114400	25.468352
176.040090	6325.928198	25.473370
176.520219	6342.131140	25.478387
176.534421	6336.104031	25.483405
176.520312	6350.904336	25.488423
177.037475	6368.615896	25.493440
177.154997	6372.765447	25.498458
176.894728	6384.185027	25.503475
177.030859	6396.915083	25.508493
176.980255	6414.298672	25.513511
177.951969	6429.808089	25.518528
178.235833	6436.913722	25.523546
178.505613	6432.261195	25.528563
178.802754	6432.739452	25.533581
178.850086	6440.262015	25.538599
179.072308	6435.340133	25.543616
179.080580	6449.330545	25.548634
179.101220	6467.874316	25.553651
179.318006	6456.477504	25.558669
179.411465	6465.216131	25.563687
179.680816	6475.928227	25.568704
179.871829	6481.516870	25.573722
179.933456	6495.578282	25.578739
180.473570	6496.924146	25.583757
180.453963	6516.379167	25.588775
180.679844	6508.367862	25.593792
180.668554	6517.673165	25.598810
180.631894	6510.248943	25.603827
180.949675	6523.595287	25.608845
181.001333	6545.406342	25.613863
181.182321	6546.571083	25.618880
181.384095	6556.700008	25.623898
181.263605	6575.764436	25.628915
181.646518	6575.017409	25.633933
181.493856	6593.789594	25.638951
182.303241	6606.433728	25.643968
182.599258	6595.142979	25.648986
182.529768	6616.618624	25.654003
182.581097	6613.184165	25.659021
183.105298	6626.400132	25.664039
183.379276	6630.113333	25.669056
183.306895	6628.999095	25.674074
183.400629	6641.002069	25.679092
184.008558	6645.054624	25.684109
183.946894	6658.351443	25.689127
184.229006	6653.421513	25.694144
184.211276	6658.997087	25.699162
184.261111	6694.606181	25.704180
184.242636	6691.503048	25.709197
184.258090	6697.064691	25.714215
184.713272	6714.334159	25.719232
185.170057	6719.369905	25.724250
185.052521	6733.953413	25.729268
185.637793	6740.470626	25.734285
185.567252	6741.470926	25.739303
185.908518	6753.579291	25.744320
186.251415	6761.992725	25.749338
186.288636	6770.127603	25.754356
186.415298	6780.058590	25.759373
186.363664	6789.189538	25.764391
186.517090	6796.573418	25.769408
186.830198	6813.344022	25.774426
186.902554	6824.640883	25.779444
187.385711	6820.381435	25.784461
187.466750	6835.686326	25.789479
187.515418	6853.450351	25.794496
187.984759	6855.416501	25.799514
188.209043	6862.104619	25.804532
188.443835	6867.585723	25.809549
188.765961	6879.282612	25.814567
189.024749	6888.865306	25.819584
189.346994	6886.898204	25.824602
189.350741	6888.130570	25.829620
189.425352	6880.073948	25.834637
189.774913	6896.795563	25.839655
189.893396	6911.766476	25.844672
190.106158	6905.268454	25.849690
189.947378	6914.905153	25.854708
190.371499	6915.515032	25.859725
190.231635	6921.011043	25.864743
190.642683	6936.524634	25.869760
191.073384	6941.881690	25.874778
190.579555	6947.910936	25.879796
191.114908	6954.086873	25.884813
191.320062	6966.475180	25.889831
191.343088	6977.730455	25.894848
191.693303	6973.852507	25.899866
191.516403	6985.193953	25.904884
191.911925	6996.038947	25.909901
191.951040	7003.760590	25.914919
192.029815	7007.789039	25.919936
192.480435	7022.204354	25.924954
192.347431	7036.919658	25.929972
192.942489	7038.469250	25.934989
193.046892	7063.744748	25.940007
193.069984	7072.448532	25.945024
193.467612	7056.816259	25.950042
193.553009	7082.689631	25.955060
193.795544	7092.392280	25.960077
194.061085	7092.984964	25.965095
194.139893	7104.321924	25.970112
194.559990	7111.049747	25.975130
194.669875	7115.760134	25.980148
195.046669	7120.666365	25.985165
195.275519	7129.039971	25.990183
195.270202	7141.553249	25.995200
195.722821	7127.210340	26.000218
195.800403	7145.310786	26.005236
196.081324	7149.580848	26.010253
196.500509	7163.829793	26.015271
196.458705	7161.740523	26.020288
196.606237	7154.777570	26.025306
196.649120	7167.827646	26.030324
196.765453	7173.806121	26.035341
196.809292	7184.180173	26.040359
197.093413	7201.996771	26.045376
197.218101	7197.769193	26.050394
197.542151	7211.488103	26.055412
197.657000	7224.621170	26.060429
197.855629	7238.328629	26.065447
198.055579	7245.130954	26.070464
198.483644	7249.615199	26.075482
198.334524	7270.347587	26.080500
198.737190	7282.663755	26.085517
199.049160	7285.265613	26.090535
198.666718	7294.136467	26.095552
199.353320	7307.838577	26.100570
199.581003	7310.634842	26.105588
199.777784	7312.433650	26.110605
200.259024	7327.089863	26.115623
200.215923	7339.225372	26.120640
200.671706	7342.184338	26.125658
200.747657	7335.785835	26.130676
200.766543	7353.317593	26.135693
200.938201	7356.400540	26.140711
200.714286	7373.974180	26.145728
201.233855	7375.929249	26.150746
201.428915	7388.922211	26.155764
201.549048	7387.924355	26.160781
202.181089	7403.392976	26.165799
202.346949	7415.263124	26.170816
202.405815	7423.718288	26.175834
202.501566	7420.426053	26.180852
202.726762	7414.737026	26.185869
203.179851	7430.375045	26.190887
203.039766	7453.351795	26.195904
203.238795	7449.301128	26.200922
203.588129	7451.710586	26.205940
203.788126	7448.646423	26.210957
203.694627	7466.022347	26.215975
203.953163	7479.712610	26.220992
204.394208	7462.106753	26.226010
204.511329	7481.615988	26.231028
204.925188	7491.716464	26.236045
205.116875	7509.829061	26.241063
204.906805	7514.998155	26.246080
205.357506	7523.230395	26.251098
205.442445	7530.192814	26.256116
205.715855	7536.066138	26.261133
205.906380	7542.453879	26.266151
206.062841	7550.181489	26.271168
206.334127	7551.916519	26.276186
206.265475	7581.918556	26.281204
206.645062	7582.644149	26.286221
207.107753	7583.755408	26.291239
207.205788	7590.496246	26.296256
207.284718	7601.662041	26.301274
207.644679	7614.963309	26.306292
207.716434	7622.284301	26.311309
208.014645	7635.957369	26.316327
208.243394	7639.613520	26.321344
208.403851	7643.743209	26.326362
208.396543	7658.048038	26.331380
208.547858	7676.028008	26.336397
208.955032	7677.884590	26.341415
209.247171	7699.535472	26.346432
209.441114	7709.335973	26.351450
209.681105	7710.677092	26.356468
209.844242	7714.427125	26.361485
209.906144	7730.547992	26.366503
209.903286	7747.920023	26.371520
210.146025	7747.552513	26.376538
210.477656	7771.908601	26.381556
210.436775	7772.091449	26.386573
211.291921	7786.802599	26.391591
211.347133	7798.347639	26.396608
211.576524	7792.456372	26.401626
212.013316	7805.857293	26.406644
211.896140	7824.767002	26.411661
212.401693	7821.048978	26.416679
212.400653	7834.441045	26.421696
212.427469	7837.507844	26.426714
212.848108	7858.221030	26.431732
212.799357	7858.064436	26.436749
213.378286	7864.576086	26.441767
213.652670	7878.808680	26.446784
213.884244	7879.426486	26.451802
214.173422	7874.925428	26.456820
214.204820	7888.218738	26.461837
214.406618	7876.319660	26.466855
214.228609	7883.163652	26.471872
214.547752	7890.896978	26.476890
214.832762	7896.390918	26.481908
214.816402	7915.827584	26.486925
215.385308	7917.918855	26.491943
215.285474	7943.656451	26.496960
215.552821	7945.258394	26.501978
215.669921	7942.744755	26.506996
216.015485	7965.632281	26.512013
216.192926	7973.474007	26.517031
216.066081	7984.954583	26.522048
216.355030	7997.974814	26.527066
216.675226	8000.441728	26.532084
217.068982	8022.667010	26.537101
217.294301	8024.187537	26.542119
217.219665	8033.817838	26.547136
217.510469	8045.258629	26.552154
217.965215	8044.976913	26.557172
218.198481	8068.795236	26.562189
218.394080	8081.011321	26.567207
218.249137	8100.289721	26.572224
218.756226	8102.867702	26.577242
218.956932	8117.157907	26.582260
218.858033	8130.439159	26.587277
219.554049	8137.402011	26.592295
219.816198	8150.573002	26.597312
219.959569	8163.443482	26.602330
220.128960	8172.452702	26.607348
220.363849	8177.876840	26.612365
220.735842	8188.946783	26.617383
220.776122	8202.274366	26.622400
221.244451	8202.277683	26.627418
221.546268	8216.666744	26.632436
221.642436	8229.933510	26.637453
222.100299	8218.820315	26.642471
222.025125	8229.262069	26.647488
222.122694	8251.442852	26.652506
222.707625	8242.791896	26.657524
222.680372	8257.885759	26.662541
222.907535	8256.626072	26.667559
222.974430	8281.136148	26.672576
223.038906	8292.142674	26.677594
223.599262	8282.716629	26.682612
223.593039	8316.225849	26.687629
223.855207	8312.212097	26.692647
224.318967	8325.286580	26.697664
224.022574	8341.018295	26.702682
224.205126	8341.132482	26.707700
224.487971	8364.656959	26.712717
224.923431	8367.881402	26.717735
225.170851	8388.670155	26.722752
225.201050	8397.653705	26.727770
225.593659	8408.167364	26.732788
225.781102	8426.627974	26.737805
226.064637	8425.810945	26.742823
226.307257	8444.064492	26.747840
226.263774	8448.183642	26.752858
226.673758	8458.131175	26.757876
226.450999	8465.303606	26.762893
227.035490	8463.480198	26.767911
227.272522	8486.524317	26.772928
227.588228	8495.834596	26.777946
227.995672	8505.958823	26.782964
227.772671	8519.625310	26.787981
228.016002	8531.901827	26.792999
228.337300	8533.968930	26.798016
228.336702	8551.598055	26.803034
228.543875	8559.794162	26.808052
228.638499	8577.860587	26.813069
229.165448	8599.465906	26.818087
229.458845	8610.698987	26.823104
229.886122	8631.252460	26.828122
230.215833	8646.334659	26.833140
229.710770	8658.120765	26.838157
230.018507	8672.157593	26.843175
230.703736	8684.517228	26.848192
230.671912	8708.987090	26.853210
231.206831	8714.850670	26.858228
231.334861	8726.457213	26.863245
231.694708	8744.941094	26.868263
231.770771	8746.983585	26.873280
232.158340	8768.845073	26.878298
232.484850	8774.068334	26.883316
232.708753	8791.266153	26.888333
232.631244	8805.237835	26.893351
233.326413	8812.370325	26.898368
233.679111	8830.657158	26.903386
234.000170	8825.749427	26.908404
234.128330	8843.296206	26.913421
234.190426	8839.521946	26.918439
234.268482	8850.811571	26.923456
234.422795	8864.300189	26.928474
234.935867	8868.947646	26.933492
235.041495	8886.294265	26.938509
235.165587	8895.288326	26.943527
235.591141	8897.632369	26.948544
235.871747	8922.135395	26.953562
236.373273	8924.661692	26.958580
236.476826	8929.211567	26.963597
236.843397	8925.264418	26.968615
236.912420	8930.620849	26.973632
236.833984	8936.180199	26.978650
237.679473	8940.035799	26.983668
237.453042	8952.744406	26.988685
237.570734	8959.174272	26.993703
237.689501	8975.014370	26.998720
237.781513	8978.652916	27.003738
237.882751	8981.804875	27.008756
238.104691	9000.765881	27.013773
238.576903	9004.793137	27.018791
238.904572	9020.551194	27.023808
239.113524	9046.928027	27.028826
239.484713	9044.581832	27.033844
239.437560	9041.989931	27.038861
239.836648	9068.510789	27.043879
240.246810	9065.989982	27.048896
240.044200	9090.431825	27.053914
240.156714	9093.672896	27.058932
240.448023	9106.881399	27.063949
240.687791	9123.366506	27.068967
241.288189	9135.563386	27.073984
240.806982	9165.105579	27.079002
241.539958	9161.630723	27.084020
241.983073	9182.780084	27.089037
241.872371	9194.296391	27.094055
242.269624	9210.117918	27.099072
242.421541	9221.118273	27.104090
242.615109	9232.791879	27.109108
243.219954	9235.810100	27.114125
243.580225	9261.064279	27.119143
244.026510	9271.289071	27.124160
243.888271	9284.048818	27.129178
244.363304	9283.834678	27.134196
244.700319	9298.947065	27.139213
244.821182	9312.848251	27.144231
245.033172	9312.560368	27.149248
245.021206	9329.017371	27.154266
245.539147	9336.164994	27.159284
245.395235	9348.931996	27.164301
245.601892	9364.084116	27.169319
245.971689	9370.007726	27.174336
246.110311	9398.707546	27.179354
246.247955	9401.904153	27.184372
246.684538	9418.257092	27.189389
246.732036	9435.382657	27.194407
247.471359	9449.326631	27.199424
247.271548	9464.606996	27.204442
247.669216	9477.372365	27.209460
248.089280	9488.097637	27.214477
248.056205	9503.420710	27.219495
248.910328	9500.439536	27.224512
248.480607	9532.885442	27.229530
248.928882	9543.802200	27.234548
249.153841	9552.086515	27.239565
249.413147	9569.659670	27.244583
249.501016	9586.948948	27.249600
249.677087	9604.296582	27.254618
250.284159	9624.843620	27.259636
250.542277	9641.768625	27.264653
250.503610	9650.842598	27.269671
250.879153	9637.043120	27.274688
250.844758	9669.085169	27.279706
251.302574	9672.916600	27.284724
252.091876	9677.413653	27.289741
252.001918	9699.190130	27.294759
252.297641	9710.661324	27.299776
252.550405	9711.169601	27.304794
252.763073	9713.553617	27.309812
252.952093	9732.142681	27.314829
253.194150	9742.743455	27.319847
253.824583	9750.001616	27.324864
253.764906	9768.829071	27.329882
253.952466	9768.779187	27.334900
253.907108	9781.858603	27.339917
254.256209	9789.736877	27.344935
254.352037	9802.333449	27.349952
254.835152	9824.278835	27.354970
255.148274	9832.702311	27.359988
255.079817	9856.246190	27.365005
255.271464	9870.859805	27.370023
256.096887	9879.543172	27.375040
255.752824	9908.516074	27.380058
256.106765	9922.562848	27.385076
256.763096	9913.908219	27.390093
256.845155	9946.142801	27.395111
257.117570	9947.558838	27.400128
257.495333	9974.583624	27.405146
258.041820	9976.583560	27.410164
258.204805	9973.297756	27.415181
258.554099	10006.662411	27.420199
258.931957	10002.883167	27.425216
259.012669	10010.174395	27.430234
259.274805	10036.984398	27.435252
259.771360	10025.101160	27.440269
259.643084	10037.461765	27.445287
260.274112	10057.358713	27.450304
260.218588	10063.757647	27.455322
260.511062	10069.139855	27.460340
261.080317	10080.821914	27.465357
261.145032	10097.632681	27.470375
261.326051	10086.655893	27.475392
261.015621	10111.264136	27.480410
260.990906	10126.183201	27.485428
261.805664	10146.175319	27.490445
261.874613	10168.838041	27.495463
262.398204	10176.114625	27.500480
262.496200	10202.610733	27.505498
262.816638	10202.431461	27.510516
263.118097	10223.650523	27.515533
263.028160	10251.520006	27.520551
263.663963	10249.486760	27.525568
263.796705	10257.686618	27.530586
264.350085	10292.219092	27.535604
264.621316	10292.999096	27.540621
264.579714	10312.649870	27.545639
265.132769	10319.464211	27.550656
265.260629	10328.928743	27.555674
265.857961	10343.492710	27.560692
266.114678	10340.507063	27.565709
266.120816	10343.028376	27.570727
266.565770	10344.350056	27.575744
266.567239	10377.253163	27.580762
266.314185	10386.060741	27.585780
266.889937	10398.980695	27.590797
266.988643	10410.911155	27.595815
267.294806	10412.749574	27.600832
267.402565	10439.179618	27.605850
267.609662	10454.950148	27.610868
268.132274	10469.879104	27.615885
267.812336	10506.415609	27.620903
268.671835	10517.571301	27.625920
269.063080	10527.903711	27.630938
269.219738	10542.812772	27.635956
269.928447	10559.175919	27.640973
270.080615	10575.983117	27.645991
270.798670	10588.007406	27.651008
270.582687	10595.840826	27.656026
271.122003	10602.655128	27.661044
271.320248	10610.990722	27.666061
271.372257	10629.886838	27.671079
271.698786	10631.553625	27.676096
272.039891	10658.983307	27.681114
271.867296	10666.094878	27.686132
272.386050	10684.443689	27.691149
272.668438	10695.334615	27.696167
272.902154	10706.364733	27.701184
273.123268	10710.724851	27.706202
273.345997	10749.443125	27.711220
273.907423	10749.766486	27.716237
273.883568	10768.287280	27.721255
273.987547	10775.918296	27.726272
274.367785	10798.045204	27.731290
274.536426	10816.891878	27.736308
275.076024	10836.800112	27.741325
275.082863	10852.980736	27.746343
275.729084	10875.740202	27.751360
275.719097	10881.836709	27.756378
276.008357	10906.864955	27.761396
276.182868	10916.821767	27.766413
276.293216	10939.342115	27.771431
276.840411	10957.566318	27.776448
277.218748	10977.680273	27.781466
277.052009	11004.125552	27.786484
277.702413	11004.613780	27.791501
278.006505	11036.620133	27.796519
278.224642	11040.597162	27.801536
278.564468	11060.178273	27.806554
278.962171	11077.948743	27.811572
279.728721	11097.545698	27.816589
279.637634	11114.875492	27.821607
279.797407	11116.496906	27.826624
280.104941	11122.439408	27.831642
280.291052	11145.501250	27.836660
280.512075	11150.018911	27.841677
281.101778	11165.210565	27.846695
281.315682	11167.020501	27.851712
281.786861	11172.856663	27.856730
281.573889	11203.091610	27.861748
282.109645	11200.648030	27.866765
282.267777	11213.349184	27.871783
282.450579	11235.295716	27.876800
282.926444	11230.355848	27.881818
282.870014	11255.291033	27.886836
283.586592	11261.073554	27.891853
283.767522	11276.044008	27.896871
283.987236	11291.141692	27.901888
284.155191	11301.233990	27.906906
284.201643	11322.424030	27.911924
284.853420	11334.382755	27.916941
284.938700	11351.955441	27.921959
285.128484	11368.234952	27.926976
285.604165	11383.221687	27.931994
285.879147	11401.697986	27.937012
286.114256	11402.065512	27.942029
286.181525	11428.524604	27.947047
286.862855	11433.756785	27.952064
287.150797	11458.367859	27.957082
287.413825	11465.516222	27.962100
287.902229	11474.734335	27.967117
288.153514	11502.129897	27.972135
288.174096	11506.079907	27.977152
288.666072	11517.252832	27.982170
288.919597	11542.483800	27.987188
289.122417	11553.746129	27.992205
289.492118	11564.914969	27.997223
289.538869	11574.614369	28.002240
289.933436	11598.416143	28.007258
289.995455	11614.429021	28.012276
290.400718	11619.572658	28.017293
290.622198	11644.283171	28.022311
290.978662	11662.019587	28.027328
291.263485	11684.007964	28.032346
291.314563	11701.876530	28.037364
292.057046	11718.788064	28.042381
292.156553	11734.446045	28.047399
292.361508	11749.842467	28.052416
292.764932	11760.239506	28.057434
292.777204	11785.370030	28.062452
293.187076	11793.359702	28.067469
293.430134	11816.060508	28.072487
293.844047	11842.472155	28.077504
294.694478	11857.817353	28.082522
294.624215	11870.573961	28.087540
294.830716	11889.770898	28.092557
295.525292	11895.862943	28.097575
295.653012	11895.772228	28.102592
295.840531	11906.920778	28.107610
295.967997	11928.075143	28.112628
296.376380	11932.201531	28.117645
296.387574	11946.696786	28.122663
296.653313	11962.035726	28.127680
296.946632	11972.399698	28.132698
296.750100	11999.778607	28.137716
297.009971	12009.285726	28.142733
297.640748	12048.254754	28.147751
298.012995	12060.512047	28.152768
298.244186	12085.255183	28.157786
298.293345	12114.625337	28.162804
298.646383	12120.405934	28.167821
299.381579	12137.381673	28.172839
299.550792	12173.820626	28.177856
300.083046	12176.798700	28.182874
300.050001	12205.559179	28.187892
300.313702	12223.998735	28.192909
300.596315	12234.644590	28.197927
301.093634	12259.881974	28.202944
301.820773	12278.044077	28.207962
301.843333	12294.951967	28.212980
302.213868	12302.460400	28.217997
302.843411	12318.798349	28.223015
302.688642	12345.467589	28.228032
303.282945	12340.348913	28.233050
303.508943	12369.294104	28.238068
303.683433	12373.206035	28.243085
304.278451	12382.962598	28.248103
304.320525	12416.936450	28.253120
304.945215	12422.235272	28.258138
304.900674	12431.598346	28.263156
305.684641	12443.452872	28.268173
306.092579	12451.982741	28.273191
306.017375	12459.947767	28.278208
306.051858	12474.745002	28.283226
306.161633	12503.086793	28.288244
306.609254	12514.077258	28.293261
306.762715	12543.720672	28.298279
307.288121	12560.801166	28.303296
307.103197	12570.569220	28.308314
307.491764	12608.456322	28.313332
308.250005	12626.180208	28.318349
308.479095	12635.729228	28.323367
308.484942	12673.056093	28.328384
308.846748	12680.321127	28.333402
309.528451	12708.488517	28.338420
309.833164	12727.404043	28.343437
310.181604	12748.791156	28.348455
310.753104	12758.639080	28.353472
311.065290	12767.465774	28.358490
311.424942	12787.822631	28.363508
311.784094	12800.348256	28.368525
312.184030	12802.625199	28.373543
312.270356	12813.735058	28.378560
312.597975	12824.954440	28.383578
312.652213	12836.822085	28.388596
312.668160	12842.892620	28.393613
312.447744	12873.290091	28.398631
312.982566	12890.865917	28.403648
313.254604	12905.306739	28.408666
313.384389	12947.520089	28.413684
313.682000	12948.986322	28.418701
314.465266	12971.803471	28.423719
314.516731	13000.146237	28.428736
314.949994	13014.528408	28.433754
315.381487	13020.548918	28.438772
315.700472	13046.089755	28.443789
316.057813	13062.605311	28.448807
316.182804	13094.907072	28.453824
316.691109	13104.821968	28.458842
316.742571	13124.580611	28.463860
317.107155	13163.261405	28.468877
317.708268	13173.697968	28.473895
317.548471	13192.008442	28.478912
318.204413	13220.007925	28.483930
318.892142	13239.122200	28.488948
319.123496	13252.634356	28.493965
319.546739	13280.993953	28.498983
319.498406	13292.416070	28.504000
320.105888	13304.263791	28.509018
320.668276	13329.213559	28.514036
321.220888	13346.887242	28.519053
321.404823	13345.115725	28.524071
321.843391	13366.223891	28.529088
322.030048	13378.738921	28.534106
322.146064	13381.693459	28.539124
322.622070	13400.080934	28.544141
322.763984	13406.752852	28.549159
322.727632	13431.929471	28.554176
323.534298	13441.467428	28.559194
323.793339	13458.453253	28.564212
323.812751	13478.913085	28.569229
324.405215	13473.045581	28.574247
324.774186	13500.207381	28.579264
325.720054	13513.634424	28.584282
325.572203	13518.740147	28.589300
325.575055	13537.291162	28.594317
326.266614	13548.209067	28.599335
326.684800	13568.313438	28.604352
326.868482	13575.527599	28.609370
327.179677	13593.279207	28.614388
327.218216	13610.534124	28.619405
327.584491	13614.791273	28.624423
327.718337	13650.878905	28.629440
327.672385	13662.370187	28.634458
328.192931	13682.035704	28.639476
328.440730	13709.933288	28.644493
328.983103	13727.217645	28.649511
328.827202	13761.697354	28.654528
329.197714	13769.360607	28.659546
329.896163	13793.188052	28.664564
330.051730	13829.508984	28.669581
330.514340	13836.327945	28.674599
330.674702	13867.838372	28.679616
330.878599	13880.027157	28.684634
331.312215	13891.504364	28.689652
331.234916	13922.259831	28.694669
331.676424	13951.239616	28.699687
332.097125	13968.789329	28.704704
332.557034	13995.667332	28.709722
333.175847	14012.535729	28.714740
333.010531	14039.180787	28.719757
333.529116	14058.170645	28.724775
333.856152	14086.314574	28.729792
334.281763	14112.391515	28.734810
334.569907	14128.274581	28.739828
335.044023	14153.280904	28.744845
335.551847	14173.858353	28.749863
335.826333	14201.849011	28.754880
336.138085	14205.289779	28.759898
336.633622	14232.216640	28.764916
336.428046	14268.303768	28.769933
337.177132	14273.160328	28.774951
337.506966	14293.396634	28.779968
337.761752	14332.830263	28.784986
338.217267	14338.168248	28.790004
338.124796	14366.131497	28.795021
338.838130	14380.983566	28.800039
338.919062	14419.935632	28.805056
339.414589	14433.392174	28.810074
340.061241	14464.595394	28.815092
340.003574	14496.285034	28.820109
340.720230	14498.756380	28.825127
341.066577	14524.673875	28.830144
341.112243	14550.778961	28.835162
341.475259	14557.579979	28.840180
341.974056	14579.599266	28.845197
342.300552	14592.638328	28.850215
342.432911	14628.550606	28.855232
343.135777	14645.798918	28.860250
343.755372	14657.878880	28.865268
344.027865	14691.373569	28.870285
344.351866	14695.924892	28.875303
344.847420	14720.420405	28.880320
345.229595	14721.531701	28.885338
345.651737	14741.877579	28.890356
345.805951	14752.046987	28.895373
346.239232	14756.746810	28.900391
346.350944	14777.302895	28.905408
346.635543	14798.600638	28.910426
347.386026	14817.389572	28.915444
347.129600	14833.524588	28.920461
347.547709	14855.079209	28.925479
347.836043	14864.584375	28.930496
347.909443	14884.270364	28.935514
348.190444	14903.659779	28.940532
348.160775	14921.160058	28.945549
349.034376	14940.006569	28.950567
349.198809	14970.299546	28.955584
349.128508	14999.031678	28.960602
350.122133	15002.982404	28.965620
350.126906	15027.219311	28.970637
350.617819	15061.238228	28.975655
350.836643	15081.549041	28.980672
351.226113	15099.868923	28.985690
351.777931	15131.225893	28.990708
352.143230	15149.345800	28.995725
352.392052	15170.857686	29.000743
352.994657	15194.017534	29.005760
353.378035	15216.666424	29.010778
353.909867	15221.851158	29.015796
353.838700	15255.576024	29.020813
354.211858	15276.527722	29.025831
354.382323	15302.602590	29.030848
355.003358	15328.543800	29.035866
355.351164	15357.222269	29.040884
355.653760	15374.609202	29.045901
355.945357	15389.018861	29.050919
356.343387	15421.401692	29.055936
356.713856	15442.755334	29.060954
357.222524	15462.188094	29.065972
357.590154	15486.621976	29.070989
357.934846	15508.980974	29.076007
358.264500	15518.526312	29.081024
358.455411	15539.411767	29.086042
359.190021	15554.120585	29.091060
359.573808	15586.001124	29.096077
359.877471	15601.785931	29.101095
360.411263	15624.912233	29.106112
360.544021	15649.204612	29.111130
361.254454	15657.596671	29.116148
361.110939	15674.485966	29.121165
361.451115	15698.792307	29.126183
362.012609	15719.241960	29.131200
361.996697	15740.447499	29.136218
362.590179	15768.906523	29.141236
362.779998	15796.367742	29.146253
363.472172	15805.434016	29.151271
363.666815	15831.727442	29.156288
363.947896	15870.693614	29.161306
364.482760	15887.310794	29.166324
364.710427	15907.766172	29.171341
364.825102	15925.089504	29.176359
365.798204	15950.498689	29.181376
366.013433	15966.477557	29.186394
366.600783	15990.752450	29.191412
366.867265	16018.699688	29.196429
367.208913	16018.702105	29.201447
367.611580	16034.291988	29.206464
367.734212	16057.979457	29.211482
368.270102	16079.204199	29.216500
368.554008	16097.947047	29.221517
368.550259	16103.178470	29.226535
368.958058	16115.910460	29.231552
369.327188	16147.945166	29.236570
369.303411	16158.968826	29.241588
369.894211	16182.950317	29.246605
370.422969	16208.858229	29.251623
370.497174	16235.941877	29.256640
370.803497	16274.747599	29.261658
371.165167	16281.261959	29.266676
371.665644	16323.017163	29.271693
372.199754	16346.964743	29.276711
372.539906	16366.443420	29.281728
372.827051	16402.392852	29.286746
373.103579	16418.825340	29.291764
373.230016	16450.261856	29.296781
373.515563	16489.861561	29.301799
374.487438	16503.728004	29.306816
374.486434	16541.634999	29.311834
375.128025	16564.821024	29.316852
375.708382	16593.617381	29.321869
375.854826	16614.389454	29.326887
376.473852	16638.625095	29.331904
376.791231	16661.930836	29.336922
377.291436	16682.032344	29.341940
377.507392	16711.674282	29.346957
377.642882	16723.262940	29.351975
378.295765	16753.922579	29.356992
379.004292	16776.402095	29.362010
379.443099	16795.000358	29.367028
379.735804	16816.411707	29.372045
379.614926	16844.405052	29.377063
380.364514	16866.075901	29.382080
380.642636	16897.306307	29.387098
381.048610	16915.319277	29.392116
381.452293	16940.489005	29.397133
382.138446	16961.288517	29.402151
382.564176	16975.158773	29.407168
382.851020	17014.057936	29.412186
383.279892	17021.943427	29.417204
383.592903	17039.616480	29.422221
383.708368	17061.910051	29.427239
384.507094	17081.611011	29.432256
384.722389	17098.768073	29.437274
385.155284	17128.810444	29.442292
385.445704	17146.337236	29.447309
385.517995	17173.881939	29.452327
386.123997	17183.541054	29.457344
386.207161	17210.575485	29.462362
386.800296	17226.228738	29.467380
387.376693	17252.513260	29.472397
387.567012	17268.225826	29.477415
387.898889	17290.482880	29.482432
388.253780	17312.254852	29.487450
388.542270	17325.349542	29.492468
389.015193	17357.388138	29.497485
389.421508	17373.697038	29.502503
389.850489	17397.415398	29.507520
390.196288	17425.603315	29.512538
390.671929	17448.621865	29.517556
391.125501	17454.734126	29.522573
390.985676	17485.633741	29.527591
391.607030	17503.999462	29.532608
391.971962	17543.727992	29.537626
392.245218	17555.358309	29.542644
392.464750	17582.079558	29.547661
392.539759	17625.160514	29.552679
393.247774	17636.259248	29.557696
393.707187	17670.375871	29.562714
393.945024	17700.065233	29.567732
394.850205	17725.576966	29.572749
394.853942	17753.850107	29.577767
395.253667	17777.715829	29.582784
395.863484	17811.138569	29.587802
396.081618	17837.532356	29.592820
396.814389	17866.412512	29.597837
397.021190	17896.471148	29.602855
397.484660	17903.586475	29.607872
398.129343	17943.143509	29.612890
398.547859	17966.798865	29.617908
398.993808	17983.276887	29.622925
399.202825	18009.984608	29.627943
399.694895	18032.724263	29.632960
400.227097	18052.378199	29.637978
400.591084	18076.386291	29.642996
400.986480	18105.610797	29.648013
401.175447	18123.405837	29.653031
401.933352	18141.265743	29.658048
402.441852	18174.741831	29.663066
402.064625	18194.450317	29.668084
402.898313	18211.706917	29.673101
403.087442	18247.680401	29.678119
403.863232	18263.021170	29.683136
403.706139	18293.049000	29.688154
404.272153	18319.217315	29.693172
404.625649	18338.261140	29.698189
405.010028	18385.428224	29.703207
405.793217	18399.401068	29.708224
406.190820	18428.992357	29.713242
406.306694	18456.841639	29.718260
406.902043	18482.793358	29.723277
406.973101	18513.457680	29.728295
407.279840	18549.320212	29.733312
407.761151	18568.759692	29.738330
408.087115	18611.112861	29.743348
408.467507	18629.950401	29.748365
408.929388	18666.555397	29.753383
409.290536	18688.762952	29.758400
409.694716	18723.145025	29.763418
410.245196	18744.643758	29.768436
410.809246	18773.834383	29.773453
411.413964	18792.993460	29.778471
411.967331	18805.217875	29.783488
412.071567	18828.602386	29.788506
412.322036	18846.577433	29.793524
413.094310	18871.016579	29.798541
413.057391	18897.029978	29.803559
413.570587	18916.091587	29.808576
414.053563	18937.958826	29.813594
414.532895	18971.489709	29.818612
415.142984	18992.362751	29.823629
415.363002	19019.639358	29.828647
415.451032	19045.476402	29.833664
415.829652	19078.086547	29.838682
416.397131	19094.750724	29.843700
417.034266	19131.156449	29.848717
416.753362	19174.349203	29.853735
417.523107	19187.922538	29.858752
418.173238	19219.385367	29.863770
418.212865	19262.065864	29.868788
418.885884	19278.505937	29.873805
419.236266	19324.439529	29.878823
419.598669	19344.791080	29.883840
419.850182	19383.316773	29.888858
420.438966	19404.575667	29.893876
421.067260	19435.984145	29.898893
421.332790	19470.471070	29.903911
421.994497	19502.848803	29.908928
422.479141	19524.693769	29.913946
422.794346	19567.443006	29.918964
423.491584	19587.756484	29.923981
423.669220	19621.544332	29.928999
424.044225	19636.333770	29.934016
424.293620	19667.027068	29.939034
424.976495	19704.203263	29.944052
425.473356	19725.980813	29.949069
425.700959	19768.817400	29.954087
426.363646	19793.602254	29.959104
426.936184	19805.130274	29.964122
427.066109	19842.431522	29.969140
427.523044	19858.385746	29.974157
427.963794	19898.866932	29.979175
428.508789	19918.972412	29.984192
428.871132	19943.142326	29.989210
429.239896	19979.693988	29.994228
430.008058	19994.553021	29.999245
429.994531	20034.252946	30.004263
430.595418	20053.214966	30.009280
431.222225	20075.901111	30.014298
431.175130	20105.043968	30.019316
431.791813	20130.789914	30.024333
432.162898	20158.926010	30.029351
432.896615	20187.921774	30.034368
433.176641	20205.399547	30.039386
433.720944	20232.731341	30.044404
434.296564	20248.237884	30.049421
434.533113	20267.720463	30.054439
434.778001	20296.678166	30.059456
435.204121	20313.915047	30.064474
435.642694	20350.365895	30.069492
435.530211	20366.797625	30.074509
436.162677	20417.797448	30.079527
436.235732	20440.553851	30.084544
437.001474	20464.058664	30.089562
437.209914	20505.254490	30.094580
437.941910	20523.390601	30.099597
437.988390	20559.389396	30.104615
438.609238	20609.586099	30.109632
439.208878	20626.813791	30.114650
439.141337	20670.965369	30.119668
440.050323	20698.576132	30.124685
440.472266	20745.509705	30.129703
440.836364	20768.301716	30.134720
441.272569	20799.772296	30.139738
442.104688	20840.682602	30.144756
442.875358	20869.059892	30.149773
443.063883	20903.592569	30.154791
443.020077	20926.520285	30.159808
443.849532	20948.144177	30.164826
443.855765	20998.446356	30.169844
444.656331	21026.995177	30.174861
444.862960	21064.815141	30.179879
445.667020	21086.851990	30.184896
445.956778	21133.853070	30.189914
446.094744	21171.290474	30.194932
446.754492	21200.693665	30.199949
447.161379	21232.391078	30.204967
447.520846	21275.743929	30.209984
448.512117	21306.538024	30.215002
448.629526	21338.270748	30.220020
449.384055	21370.280824	30.225037
450.351420	21389.405408	30.230055
450.256448	21427.200665	30.235072
450.721165	21448.693178	30.240090
451.059861	21484.219907	30.245108
451.611811	21506.227034	30.250125
452.261548	21534.871693	30.255143
452.214423	21577.568385	30.260160
452.905077	21598.278522	30.265178
453.271092	21620.679276	30.270196
453.572874	21666.691281	30.275213
453.991202	21688.460853	30.280231
454.616731	21725.546650	30.285248
455.158749	21755.254732	30.290266
454.981442	21793.711348	30.295284
455.993863	21829.406369	30.300301
456.387049	21857.338810	30.305319
456.461950	21896.976984	30.310336
457.570617	21912.178956	30.315354
457.671338	21940.955145	30.320372
458.386697	21966.051659	30.325389
458.520393	22007.524411	30.330407
459.235711	22022.861616	30.335424
459.604673	22056.797101	30.340442
459.758389	22099.882979	30.345460
460.389105	22111.954344	30.350477
460.815767	22155.533217	30.355495
460.901324	22188.858099	30.360512
461.449201	22222.018822	30.365530
462.031778	22249.294093	30.370548
462.475969	22288.438102	30.375565
462.909623	22311.604823	30.380583
463.558544	22360.005810	30.385600
464.199382	22385.026659	30.390618
464.372028	22427.700876	30.395636
464.856953	22457.972264	30.400653
465.537072	22484.921310	30.405671
465.644944	22532.360758	30.410688
466.290345	22549.256434	30.415706
466.703823	22601.785601	30.420724
467.715106	22633.204464	30.425741
467.846218	22668.781117	30.430759
468.148226	22700.993596	30.435776
469.252914	22730.980896	30.440794
469.142412	22768.945660	30.445812
469.740240	22784.225936	30.450829
470.507052	22806.420395	30.455847
470.479485	22860.026450	30.460864
471.169178	22877.431301	30.465882
471.231198	22905.884624	30.470900
471.801246	22950.983401	30.475917
472.240108	22981.055206	30.480935
473.016863	23032.441820	30.485952
473.501076	23052.784302	30.490970
473.900700	23100.538911	30.495988
474.041154	23131.802157	30.501005
474.748408	23173.007014	30.506023
475.500874	23201.011405	30.511040
475.712959	23249.079882	30.516058
476.312571	23286.279815	30.521076
476.674211	23315.415477	30.526093
477.181317	23352.702765	30.531111
477.525379	23390.045260	30.536128
477.857104	23426.418663	30.541146
478.371273	23470.215636	30.546164
479.161402	23505.084277	30.551181
479.957777	23537.871073	30.556199
480.183042	23562.296815	30.561216
480.701867	23606.426594	30.566234
481.255183	23635.164481	30.571252
481.527520	23669.374810	30.576269
482.102347	23698.706416	30.581287
482.405946	23740.849771	30.586304
483.214642	23759.914322	30.591322
483.620131	23789.001337	30.596340
483.920822	23820.810670	30.601357
484.528702	23852.918480	30.606375
485.150105	23886.660939	30.611392
485.610815	23904.590965	30.616410
486.230857	23925.657265	30.621428
486.499091	23959.957093	30.626445
487.090233	23985.493290	30.631463
487.302504	24014.880092	30.636480
487.891224	24036.718709	30.641498
488.195735	24075.046603	30.646516
488.308510	24113.865131	30.651533
489.171831	24142.389931	30.656551
489.441708	24179.125425	30.661568
489.826487	24218.730286	30.666586
490.242691	24248.820714	30.671604
490.696504	24305.495397	30.676621
491.376087	24340.843494	30.681639
491.672721	24386.203378	30.686656
492.216201	24415.172675	30.691674
493.024690	24471.514972	30.696692
493.136922	24508.706415	30.701709
494.091453	24535.497885	30.706727
494.499256	24574.650987	30.711744
494.924658	24617.865057	30.716762
495.407528	24652.662299	30.721780
496.148727	24696.697458	30.726797
496.726523	24730.235984	30.731815
497.330651	24770.580790	30.736832
497.845304	24803.938121	30.741850
498.173028	24830.484149	30.746868
498.486727	24885.655087	30.751885
499.265583	24910.759569	30.756903
499.662781	24952.489498	30.761920
499.833852	24997.633242	30.766938
500.263270	25031.105454	30.771956
500.914292	25064.335267	30.776973
501.462433	25103.510636	30.781991
501.880824	25147.552782	30.787008
502.199065	25178.651520	30.792026
502.705063	25225.153347	30.797044
503.058315	25268.346017	30.802061
503.883532	25308.055148	30.807079
504.770522	25351.271721	30.812096
505.211567	25380.671863	30.817114
505.873558	25412.069983	30.822132
506.352889	25457.212395	30.827149
506.998190	25489.325433	30.832167
507.364162	25521.869022	30.837184
508.075620	25558.225410	30.842202
508.358650	25594.763565	30.847220
508.851811	25630.026856	30.852237
509.457303	25657.335867	30.857255
509.869373	25688.873601	30.862272
510.193434	25712.415667	30.867290
510.602962	25756.412854	30.872308
510.873856	25781.850924	30.877325
511.643428	25814.993309	30.882343
511.992636	25842.230816	30.887360
512.572280	25887.830326	30.892378
513.422575	25905.617840	30.897396
513.321587	25947.558137	30.902413
514.525967	25979.514566	30.907431
514.856763	26014.993634	30.912448
515.229968	26041.531282	30.917466
515.656580	26085.482539	30.922484
516.006078	26112.296645	30.927501
516.475991	26155.790598	30.932519
517.074655	26208.249406	30.937536
517.436837	26237.978010	30.942554
518.475039	26266.108521	30.947572
518.631742	26314.629132	30.952589
519.685722	26353.287415	30.957607
519.911550	26378.202655	30.962624
520.282434	26419.341901	30.967642
520.877222	26459.265494	30.972660
521.569718	26498.655263	30.977677
522.191399	26527.343375	30.982695
522.426827	26580.742794	30.987712
522.775041	26614.449478	30.992730
523.663527	26651.916143	30.997748
523.779632	26693.123463	31.002765
524.591607	26730.978277	31.007783
525.018379	26778.426050	31.012800
525.143159	26816.325935	31.017818
525.897028	26856.185787	31.022836
526.496640	26910.968383	31.027853
526.714653	26947.744504	31.032871
527.679577	26986.219192	31.037888
528.041321	27030.180221	31.042906
528.729475	27063.918781	31.047924
529.158683	27123.678252	31.052941
529.696513	27151.624542	31.057959
530.297346	27198.438426	31.062976
530.369117	27242.907098	31.067994
531.075934	27288.953574	31.073012
531.973761	27332.028035	31.078029
532.769528	27374.853372	31.083047
532.917027	27416.453029	31.088064
533.443541	27454.193521	31.093082
534.029758	27489.989685	31.098100
534.232001	27532.240332	31.103117
534.742935	27583.761187	31.108135
535.466518	27622.884054	31.113152
535.883485	27666.806512	31.118170
536.532766	27721.399604	31.123188
536.923371	27763.470375	31.128205
537.107196	27815.196128	31.133223
538.105636	27849.728331	31.138240
538.302581	27890.182897	31.143258
539.244704	27915.396888	31.148276
539.556996	27974.098785	31.153293
539.821185	28003.648516	31.158311
540.387291	28047.832671	31.163328
541.102568	28087.297556	31.168346
541.668827	28133.717860	31.173364
542.238340	28175.213645	31.178381
542.944450	28222.436031	31.183399
543.213926	28266.114953	31.188416
543.690740	28309.148006	31.193434
544.685439	28350.658453	31.198452
544.972451	28388.674857	31.203469
545.189582	28441.593300	31.208487
546.218462	28478.049933	31.213504
546.731616	28526.285637	31.218522
547.508559	28574.416437	31.223540
547.747767	28608.646539	31.228557
548.334381	28656.240624	31.233575
548.818260	28702.124165	31.238592
548.976820	28740.522709	31.243610
550.025659	28788.590352	31.248628
550.115647	28831.298768	31.253645
550.729012	28883.870324	31.258663
551.289920	28938.467425	31.263680
551.951552	28985.538396	31.268698
552.712178	29042.458283	31.273716
552.986245	29085.363388	31.278733
553.967774	29134.646702	31.283751
554.503702	29176.705096	31.288768
555.254147	29222.026054	31.293786
555.997244	29248.978883	31.298804
556.538551	29297.655209	31.303821
557.121815	29339.323558	31.308839
557.603965	29380.503852	31.313856
558.277975	29421.166754	31.318874
559.153352	29451.832026	31.323892
559.012427	29508.749025	31.328909
559.630000	29543.945139	31.333927
560.310043	29591.468784	31.338944
560.544495	29630.486114	31.343962
561.234571	29676.341145	31.348980
561.987755	29723.724307	31.353997
562.189520	29780.300862	31.359015
562.841211	29817.931596	31.364032
563.502689	29853.034714	31.369050
563.937938	29908.753490	31.374068
564.636375	29955.495205	31.379085
565.075776	29986.486228	31.384103
565.618678	30035.266945	31.389120
565.907591	30091.383142	31.394138
566.885175	30141.880448	31.399156
567.506000	30184.506291	31.404173
568.088745	30223.351372	31.409191
568.960359	30264.741356	31.414208
568.960300	30317.256092	31.419226
569.695118	30335.973089	31.424244
570.117450	30386.703004	31.429261
570.307922	30432.132293	31.434279
570.955925	30474.185652	31.439296
571.664518	30528.966298	31.444314
571.914565	30568.982544	31.449332
572.636077	30609.116062	31.454349
573.214481	30657.034090	31.459367
574.221889	30701.782423	31.464384
574.329148	30745.411899	31.469402
575.110665	30791.797647	31.474420
575.578217	30845.368000	31.479437
576.043436	30898.786029	31.484455
576.450943	30946.189986	31.489472
577.031698	30999.181759	31.494490
577.550623	31049.940903	31.499508
578.370172	31095.303360	31.504525
578.538473	31149.751352	31.509543
579.037972	31212.736062	31.514560
579.907772	31263.140540	31.519578
581.104963	31305.731100	31.524596
581.874730	31346.619969	31.529613
582.345384	31393.071122	31.534631
583.189417	31449.346279	31.539648
583.598312	31489.765009	31.544666
584.255869	31526.057545	31.549684
584.774880	31579.193421	31.554701
584.950608	31627.321851	31.559719
585.863431	31664.256469	31.564736
586.366984	31706.388020	31.569754
586.800911	31761.779203	31.574772
587.377703	31824.541187	31.579789
588.082026	31869.947788	31.584807
589.190114	31908.687993	31.589824
589.014363	31969.140067	31.594842
589.740052	32019.084392	31.599860
590.439120	32057.716724	31.604877
591.105542	32113.839626	31.609895
591.498734	32163.332995	31.614912
591.928378	32209.253965	31.619930
592.463372	32254.211037	31.624948
593.350762	32313.776343	31.629965
593.709847	32364.531920	31.634983
594.576715	32417.076072	31.640000
594.951574	32470.995914	31.645018
595.380601	32516.640441	31.650036
596.291647	32572.371317	31.655053
596.686966	32639.578530	31.660071
597.024850	32678.194193	31.665088
597.611340	32742.327819	31.670106
598.011682	32809.309533	31.675124
599.155669	32852.829931	31.680141
599.392793	32912.516733	31.685159
600.569855	32947.761904	31.690176
600.575057	33003.389474	31.695194
601.645898	33043.383485	31.700212
602.107966	33094.351880	31.705229
602.508504	33142.609709	31.710247
603.111929	33192.195633	31.715264
604.012850	33235.066954	31.720282
604.495810	33292.525046	31.725300
604.971600	33335.018267	31.730317
605.547338	33392.132500	31.735335
606.407851	33433.522817	31.740352
606.871334	33500.825138	31.745370
607.507966	33541.951899	31.750388
608.133288	33590.378573	31.755405
608.662328	33649.387898	31.760423
609.353357	33689.291074	31.765440
609.928026	33740.677002	31.770458
610.646275	33808.233185	31.775476
611.126785	33854.683416	31.780493
611.534724	33908.996757	31.785511
612.560837	33964.009423	31.790528
612.851763	34019.719431	31.795546
613.302430	34074.496243	31.800564
614.590244	34114.349539	31.805581
615.016872	34168.656026	31.810599
615.726534	34213.596931	31.815616
616.080201	34265.286082	31.820634
616.843452	34320.069095	31.825652
617.556313	34370.019440	31.830669
617.872194	34424.842521	31.835687
618.604527	34474.821608	31.840704
619.344712	34533.824104	31.845722
619.732095	34584.881500	31.850740
620.674985	34639.386323	31.855757
621.021888	34701.346215	31.860775
621.828718	34752.889050	31.865792
622.259930	34795.369475	31.870810
622.701872	34848.658999	31.875828
623.461245	34902.000604	31.880845
623.985355	34975.962573	31.885863
624.851099	35030.536140	31.890880
625.297966	35083.759425	31.895898
625.790019	35143.564999	31.900916
626.706500	35193.866885	31.905933
627.384508	35264.726927	31.910951
627.907593	35309.512924	31.915968
628.334829	35375.274286	31.920986
629.235357	35426.402305	31.926004
630.214475	35483.949773	31.931021
630.463428	35531.967554	31.936039
631.128861	35581.314291	31.941056
631.709780	35636.920480	31.946074
631.874877	35697.582519	31.951092
633.021428	35751.224620	31.956109
633.570696	35810.509554	31.961127
634.293909	35852.306136	31.966144
634.728761	35916.406832	31.971162
635.065108	35968.589583	31.976180
635.962761	36008.153295	31.981197
636.332508	36062.638978	31.986215
637.352133	36105.650174	31.991232
637.955249	36167.041864	31.996250
638.265156	36228.540378	32.001268
639.332360	36265.925789	32.006285
639.742303	36324.733411	32.011303
640.311242	36386.251162	32.016320
640.819972	36445.489629	32.021338
641.385920	36495.553310	32.026356
642.390597	36551.434014	32.031373
642.881512	36606.919033	32.036391
643.426769	36662.507515	32.041408
644.112391	36726.897726	32.046426
644.517467	36790.643910	32.051444
645.468999	36836.035808	32.056461
646.184122	36902.501467	32.061479
646.521100	36962.390276	32.066496
647.391154	37027.901589	32.071514
648.012588	37086.224153	32.076532
649.133118	37140.144460	32.081549
649.401403	37210.614487	32.086567
650.003728	37269.604475	32.091584
650.869119	37323.761500	32.096602
651.009165	37381.821206	32.101620
651.954272	37429.642128	32.106637
652.496367	37502.388964	32.111655
653.443489	37555.786409	32.116672
654.055328	37626.233425	32.121690
654.504096	37684.126765	32.126708
655.017896	37737.008859	32.131725
655.833026	37805.847620	32.136743
656.388267	37871.008734	32.141760
656.996820	37931.691797	32.146778
657.481875	38014.606736	32.151796
658.220964	38067.017257	32.156813
658.965148	38131.405105	32.161831
659.885588	38192.080435	32.166848
660.498763	38258.093111	32.171866
661.033425	38327.396487	32.176884
661.895164	38385.975404	32.181901
662.555729	38463.879092	32.186919
663.332837	38522.722657	32.191936
664.215686	38577.645647	32.196954
664.636795	38628.282714	32.201972
665.213655	38686.594273	32.206989
666.044008	38743.547522	32.212007
666.805520	38811.287334	32.217024
668.001351	38867.053860	32.222042
668.336867	38929.256667	32.227060
669.050087	38970.507601	32.232077
669.512188	39025.516391	32.237095
669.947823	39071.401709	32.242112
670.736373	39120.363985	32.247130
671.092058	39185.248173	32.252148
671.796590	39231.072185	32.257165
672.561764	39293.318287	32.262183
672.912742	39346.882563	32.267200
673.877820	39400.388643	32.272218
674.409886	39467.563709	32.277236
675.136399	39512.110930	32.282253
675.856052	39576.902396	32.287271
676.148101	39637.310856	32.292288
677.182956	39697.128206	32.297306
677.693392	39771.253803	32.302324
678.043076	39818.187650	32.307341
678.977240	39886.594924	32.312359
679.755161	39946.827778	32.317376
680.521683	40000.953957	32.322394
681.097792	40075.289606	32.327412
681.867957	40136.216605	32.332429
682.299556	40198.132813	32.337447
682.873735	40269.251237	32.342464
683.969024	40328.665397	32.347482
684.409873	40404.884737	32.352500
685.242418	40464.869467	32.357517
685.965524	40530.676384	32.362535
686.486937	40598.075227	32.367552
687.504679	40653.183738	32.372570
687.806350	40726.137249	32.377588
688.587082	40788.351663	32.382605
689.070871	40847.540160	32.387623
689.633213	40923.103817	32.392640
690.630509	40991.999067	32.397658
691.152693	41060.722666	32.402676
691.749672	41141.673348	32.407693
692.685294	41206.800910	32.412711
693.632804	41272.390455	32.417728
694.076019	41342.621147	32.422746
694.500516	41415.365653	32.427764
695.913525	41485.902994	32.432781
696.313700	41546.272616	32.437799
697.091206	41625.768095	32.442816
698.243167	41689.364905	32.447834
698.412396	41758.701036	32.452852
699.509838	41813.832150	32.457869
700.286583	41894.511758	32.462887
700.794682	41940.328614	32.467904
701.673027	42006.178005	32.472922
702.133156	42080.370531	32.477940
702.711459	42131.847750	32.482957
703.594671	42200.191993	32.487975
703.664969	42280.336154	32.492992
705.007331	42344.822932	32.498010
705.517013	42406.736286	32.503028
706.021177	42479.475777	32.508045
707.173337	42546.592619	32.513063
707.225914	42603.119608	32.518080
708.282551	42656.184488	32.523098
708.659461	42724.788068	32.528116
709.560675	42777.001202	32.533133
710.642624	42834.831761	32.538151
711.297964	42907.523760	32.543168
712.243016	42953.668028	32.548186
712.586284	43014.171734	32.553204
713.237541	43083.218816	32.558221
713.691772	43128.255700	32.563239
714.244722	43203.457121	32.568256
715.285967	43252.848405	32.573274
715.879645	43342.679863	32.578292
716.582290	43406.528070	32.583309
717.461151	43460.689901	32.588327
718.058549	43547.364350	32.593344
718.876750	43599.886555	32.598362
719.482887	43673.330890	32.603380
720.148331	43749.254902	32.608397
721.339252	43807.090307	32.613415
721.737035	43865.061649	32.618432
722.337678	43935.773108	32.623450
722.797819	44021.153241	32.628468
723.519849	44091.394927	32.633485
724.627464	44152.383425	32.638503
724.931658	44231.518369	32.643520
725.845866	44301.162505	32.648538
726.779439	44384.566901	32.653556
727.291417	44457.919151	32.658573
728.416041	44519.041879	32.663591
728.986441	44596.227620	32.668608
729.810454	44672.067343	32.673626
730.226290	44747.054407	32.678644
731.012702	44807.235158	32.683661
732.386733	44884.521364	32.688679
732.651009	44968.763840	32.693696
733.425813	45026.855699	32.698714
734.568153	45090.772613	32.703732
734.955631	45165.658740	32.708749
735.633886	45223.536341	32.713767
736.462077	45306.659102	32.718784
737.485461	45371.084960	32.723802
738.374603	45440.680880	32.728820
738.777760	45512.761487	32.733837
739.815664	45566.298887	32.738855
740.648342	45640.204465	32.743872
741.441417	45707.630524	32.748890
741.714570	45767.375783	32.753908
742.366411	45845.629873	32.758925
743.386452	45904.114669	32.763943
743.807321	45986.327544	32.768960
744.671314	46053.462874	32.773978
745.349563	46126.208895	32.778996
746.303792	46198.248768	32.784013
747.059947	46258.868416	32.789031
747.219856	46325.211446	32.794048
748.270079	46392.208012	32.799066
749.242304	46449.329886	32.804084
749.675975	46510.948210	32.809101
750.588862	46579.181987	32.814119
751.078189	46643.912109	32.819136
752.431047	46704.359435	32.824154
752.806680	46776.351835	32.829172
753.370879	46847.103014	32.834189
754.357416	46896.147423	32.839207
754.766118	46978.385826	32.844224
755.799677	47049.795053	32.849242
756.279210	47112.155921	32.854260
756.799058	47167.623228	32.859277
757.760878	47244.307208	32.864295
758.529371	47331.907147	32.869312
759.303665	47395.947899	32.874330
759.986765	47472.554202	32.879348
760.741122	47553.270015	32.884365
761.435980	47613.304649	32.889383
761.857113	47712.462051	32.894400
762.529215	47781.123763	32.899418
763.782919	47852.829344	32.904436
764.448124	47943.042283	32.909453
765.175619	48027.553870	32.914471
765.856554	48103.797269	32.919488
766.558944	48182.022191	32.924506
767.422707	48264.531768	32.929524
768.264215	48357.369125	32.934541
769.043573	48429.843564	32.939559
769.763462	48514.838292	32.944576
770.780735	48604.957552	32.949594
771.307545	48678.299892	32.954612
772.236463	48756.977214	32.959629
773.370037	48837.187334	32.964647
773.735643	48928.172411	32.969664
774.577536	49014.336517	32.974682
775.459448	49078.057031	32.979700
776.423772	49159.794346	32.984717
777.468362	49234.476478	32.989735
777.970284	49320.939161	32.994752
778.842207	49394.904786	32.999770
779.880196	49467.301288	33.004788
780.374064	49547.509182	33.009805
781.234681	49617.691029	33.014823
781.654443	49700.565133	33.019840
782.875611	49766.436625	33.024858
783.779838	49846.940271	33.029876
784.593146	49922.324771	33.034893
784.862860	50002.223297	33.039911
785.995822	50077.380862	33.044928
786.576803	50154.974329	33.049946
787.604407	50233.352191	33.054964
788.415049	50312.815737	33.059981
789.261653	50378.449351	33.064999
789.763294	50451.866144	33.070016
790.700722	50516.633801	33.075034
791.343409	50569.750781	33.080052
791.884344	50646.469196	33.085069
792.944426	50707.734222	33.090087
793.477615	50790.039953	33.095104
793.920731	50872.089015	33.100122
794.769315	50933.549423	33.105140
795.428243	51012.598448	33.110157
796.436852	51082.913994	33.115175
797.165793	51172.924942	33.120192
797.878876	51256.172988	33.125210
798.884182	51331.523424	33.130228
799.213603	51425.723793	33.135245
799.949445	51506.536294	33.140263
800.958093	51594.096985	33.145280
801.630056	51679.319601	33.150298
802.494602	51769.649636	33.155316
803.198677	51850.579200	33.160333
804.123583	51935.709123	33.165351
804.858996	52027.074037	33.170368
805.473059	52119.979866	33.175386
806.458646	52203.128975	33.180404
806.978071	52303.921619	33.185421
808.198084	52385.478394	33.190439
808.844301	52487.596309	33.195456
809.535011	52567.890578	33.200474
811.162041	52657.425182	33.205492
811.795183	52752.275321	33.210509
812.761005	52829.721295	33.215527
813.629462	52925.336514	33.220544
814.260861	53008.062856	33.225562
815.097179	53090.788520	33.230580
815.683546	53176.457927	33.235597
816.626051	53269.566740	33.240615
817.533417	53344.467808	33.245632
818.325895	53436.976460	33.250650
819.124521	53536.194529	33.255668
820.045503	53620.064286	33.260685
820.929571	53700.733655	33.265703
821.488634	53790.854189	33.270720
822.426502	53884.897984	33.275738
823.361987	53966.545085	33.280756
824.186718	54053.370597	33.285773
824.901379	54138.171963	33.290791
826.098531	54228.764390	33.295808
826.642321	54313.723181	33.300826
827.569705	54395.373507	33.305844
828.338412	54487.035960	33.310861
829.000893	54564.682846	33.315879
830.084304	54660.093118	33.320896
830.945896	54746.587826	33.325914
832.211160	54827.719180	33.330932
832.627881	54911.791967	33.335949
833.445421	54994.822867	33.340967
834.567156	55070.426080	33.345984
835.307154	55148.972168	33.351002
836.456659	55201.008948	33.356020
836.888231	55282.319219	33.361037
837.498850	55348.661914	33.366055
838.080690	55422.878469	33.371072
838.887444	55503.823836	33.376090
839.761113	55596.763016	33.381108
840.719592	55680.743653	33.386125
841.320898	55761.227293	33.391143
842.031175	55844.203382	33.396160
842.876102	55935.128684	33.401178
843.699603	56026.487140	33.406196
844.283367	56115.087487	33.411213
845.302406	56205.954858	33.416231
845.725618	56298.751502	33.421248
846.707385	56401.743988	33.426266
847.957712	56486.038575	33.431284
848.521054	56588.360055	33.436301
849.239383	56688.779218	33.441319
850.647887	56782.393746	33.446336
851.373920	56874.857851	33.451354
852.240130	56968.146111	33.456372
853.379460	57065.416215	33.461389
854.024678	57148.481174	33.466407
855.186911	57252.980744	33.471424
855.621051	57347.763403	33.476442
856.664393	57420.440386	33.481460
857.211420	57525.364569	33.486477
858.054533	57615.506134	33.491495
859.217093	57714.638507	33.496512
859.690133	57823.222321	33.501530
860.665791	57917.160919	33.506548
861.572774	58011.631813	33.511565
862.658376	58104.167987	33.516583
863.341330	58210.248805	33.521600
864.187869	58322.381328	33.526618
865.129105	58414.298015	33.531636
865.629059	58521.584137	33.536653
866.573686	58614.543085	33.541671
867.676334	58714.599584	33.546688
868.688509	58821.098748	33.551706
869.141366	58913.487115	33.556724
870.228386	59026.166527	33.561741
871.154080	59123.213137	33.566759
872.482854	59225.850480	33.571776
872.807830	59333.292274	33.576794
873.897286	59412.132467	33.581812
874.972585	59514.284505	33.586829
875.629141	59611.783776	33.591847
876.922752	59713.535934	33.596864
877.678370	59818.124196	33.601882
878.615672	59903.835516	33.606900
879.236317	60005.854236	33.611917
880.333376	60092.983860	33.616935
881.216686	60173.628155	33.621952
881.726228	60270.194462	33.626970
882.956087	60347.216628	33.631988
883.805765	60440.016704	33.637005
884.190961	60537.630310	33.642023
885.101690	60618.685776	33.647040
886.246750	60716.993985	33.652058
887.117696	60797.946054	33.657076
887.667113	60907.486110	33.662093
888.498024	60992.404759	33.667111
889.407491	61094.531860	33.672128
890.003875	61192.099484	33.677146
891.229855	61299.781787	33.682164
892.311736	61395.896558	33.687181
892.749284	61498.681939	33.692199
894.037866	61595.386864	33.697216
894.615605	61693.503154	33.702234
895.369869	61802.166464	33.707252
896.336916	61908.977785	33.712269
897.523774	62011.308867	33.717287
898.819745	62108.608886	33.722304
899.527573	62211.847738	33.727322
900.526725	62312.599951	33.732340
901.478142	62406.170350	33.737357
902.612827	62504.407485	33.742375
903.628737	62600.150525	33.747392
904.987382	62696.291060	33.752410
905.603926	62785.628492	33.757428
906.825163	62879.161459	33.762445
907.303039	62973.946813	33.767463
908.462113	63047.644146	33.772480
909.121695	63152.559959	33.777498
909.975055	63256.093987	33.782516
911.079838	63349.205725	33.787533
912.168717	63439.920515	33.792551
912.783592	63529.378565	33.797568
913.604062	63637.164034	33.802586
914.251187	63732.639926	33.807604
915.603787	63822.089330	33.812621
916.064070	63933.107465	33.817639
917.141998	64018.903611	33.822656
918.125931	64128.759555	33.827674
918.761456	64244.314829	33.832692
919.967756	64345.884928	33.837709
920.411972	64428.868969	33.842727
921.113698	64558.816003	33.847744
921.986130	64651.465829	33.852762
922.733463	64765.967490	33.857780
923.989228	64878.351987	33.862797
924.835589	64995.738362	33.867815
925.968295	65094.841924	33.872832
926.889450	65216.689610	33.877850
927.621101	65322.938656	33.882868
928.354705	65439.183509	33.887885
929.109727	65553.811837	33.892903
930.628404	65655.781353	33.897920
931.208238	65747.305056	33.902938
931.934700	65846.041328	33.907956
932.829696	65950.252925	33.912973
933.961587	66058.722609	33.917991
935.223511	66151.472486	33.923008
936.132996	66260.281894	33.928026
936.925090	66369.382212	33.933044
938.082275	66463.634666	33.938061
938.737124	66571.046162	33.943079
939.723678	66666.103711	33.948096
940.520106	66784.706006	33.953114
941.314064	66889.794697	33.958132
942.444450	67001.283043	33.963149
943.150266	67114.140861	33.968167
944.198227	67218.578194	33.973184
945.324338	67328.568856	33.978202
946.336543	67437.877089	33.983220
947.290628	67534.125357	33.988237
948.171524	67666.661211	33.993255
948.859080	67776.405197	33.998272
950.375583	67885.127195	34.003290
951.393532	67993.815426	34.008308
952.505053	68098.263197	34.013325
953.120240	68219.025706	34.018343
954.347794	68320.367100	34.023360
955.277807	68425.433019	34.028378
955.794024	68544.463418	34.033396
957.140500	68650.677213	34.038413
957.734937	68761.597666	34.043431
958.949987	68864.687491	34.048448
959.822043	68989.166459	34.053466
960.983595	69095.020427	34.058484
962.141558	69210.029630	34.063501
962.932091	69333.481380	34.068519
964.106465	69435.374048	34.073536
965.149953	69550.567734	34.078554
966.059090	69648.536245	34.083572
967.160706	69757.713808	34.088589
968.131621	69871.272015	34.093607
968.744449	69970.451751	34.098624
970.100209	70089.339050	34.103642
970.982334	70195.603568	34.108660
971.961921	70295.453149	34.113677
972.942917	70416.000483	34.118695
973.851774	70524.353761	34.123712
974.707102	70641.656100	34.128730
975.310872	70755.846472	34.133748
976.632943	70861.741338	34.138765
977.359291	70968.483411	34.143783
978.312873	71070.805133	34.148800
979.610909	71196.512953	34.153818
980.409471	71315.382614	34.158836
981.476379	71421.832872	34.163853
982.255165	71545.395199	34.168871
983.343591	71638.391603	34.173888
984.270091	71736.171914	34.178906
985.009169	71844.054010	34.183924
986.017214	71945.992512	34.188941
986.897733	72066.591224	34.193959
987.844079	72174.442147	34.198976
989.099109	72280.955571	34.203994
989.633094	72383.173945	34.209012
990.694742	72499.569923	34.214029
991.191087	72614.413686	34.219047
992.613879	72741.312036	34.224064
993.836962	72863.611370	34.229082
994.686574	72977.459545	34.234100
996.035882	73085.592531	34.239117
996.991768	73204.391650	34.244135
997.736952	73313.633002	34.249152
998.715788	73434.079058	34.254170
999.732854	73555.221161	34.259188
1001.345885	73663.631284	34.264205
1001.981168	73780.260578	34.269223
1003.146379	73904.635516	34.274240
1004.155888	74000.884589	34.279258
1004.829580	74123.506563	34.284276
1006.102550	74238.274055	34.289293
1006.988331	74352.364464	34.294311
1008.212975	74484.860012	34.299328
1009.040755	74592.458554	34.304346
1009.864644	74711.515144	34.309364
1011.287701	74827.241629	34.314381
1011.922979	74960.004708	34.319399
1012.800641	75075.358081	34.324416
1014.376660	75190.133377	34.329434
1015.239748	75336.234621	34.334452
1016.601410	75433.401441	34.339469
1017.468641	75555.356798	34.344487
1018.474958	75678.839065	34.349504
1019.246706	75788.146581	34.354522
1020.271990	75926.105597	34.359540
1021.414448	76033.396373	34.364557
1022.649388	76162.242254	34.369575
1023.502071	76281.625869	34.374592
1024.702109	76403.533415	34.379610
1025.666123	76526.414582	34.384628
1026.965010	76638.038066	34.389645
1027.718623	76757.629851	34.394663
1028.457542	76878.513953	34.399680
1029.672573	76990.121120	34.404698
1031.031575	77119.332567	34.409716
1031.914744	77233.964289	34.414733
1033.003021	77360.572232	34.419751
1033.665969	77470.727768	34.424768
1035.000259	77593.019288	34.429786
1035.485843	77722.620009	34.434804
1036.663648	77850.626174	34.439821
1037.816528	77963.961376	34.444839
1038.639083	78079.176334	34.449856
1040.096420	78197.786126	34.454874
1040.924571	78310.100451	34.459892
1042.180842	78412.487408	34.464909
1043.095347	78513.709398	34.469927
1043.716822	78635.570695	34.474944
1044.792488	78759.850760	34.479962
1045.501932	78867.547756	34.484980
1046.794597	78993.861552	34.489997
1047.989265	79123.642795	34.495015
1048.803373	79230.781476	34.500032
1049.743898	79354.991842	34.505050
1050.786440	79491.278357	34.510068
1052.053156	79616.260116	34.515085
1052.978495	79749.324415	34.520103
1053.690780	79881.184572	34.525120
1055.030520	79998.641508	34.530138
1055.480974	80145.190591	34.535156
1056.612081	80271.424172	34.540173
1057.969326	80400.675620	34.545191
1059.008760	80551.659770	34.550208
1060.079748	80688.177244	34.555226
1060.864240	80826.738686	34.560244
1062.189779	80960.897599	34.565261
1063.307946	81103.131012	34.570279
1064.510993	81253.183998	34.575296
1065.600880	81371.636691	34.580314
1066.886592	81512.518783	34.585332
1067.792357	81650.111913	34.590349
1068.639447	81790.819129	34.595367
1070.031357	81936.889779	34.600384
1071.223072	82068.415791	34.605402
1072.167569	82210.956250	34.610420
1072.951464	82344.375818	34.615437
1074.294839	82487.518493	34.620455
1075.020060	82632.081719	34.625472
1076.553957	82763.140455	34.630490
1077.568995	82905.042260	34.635508
1078.994691	83037.738315	34.640525
1080.270551	83172.779179	34.645543
1081.383538	83309.541099	34.650560
1082.486015	83441.254331	34.655578
1083.364966	83590.029121	34.660596
1084.802390	83712.466963	34.665613
1086.111667	83836.481138	34.670631
1087.001674	83969.780396	34.675648
1088.220111	84084.535924	34.680666
1089.648429	84210.980054	34.685684
1090.623749	84337.914265	34.690701
1091.591326	84466.715545	34.695719
1092.563742	84579.553001	34.700736
1093.925719	84707.192936	34.705754
1094.638664	84843.383590	34.710772
1095.748311	84966.272857	34.715789
1097.254331	85087.487565	34.720807
1098.094872	85209.428423	34.725824
1099.253515	85314.931382	34.730842
1100.160267	85427.334912	34.735860
1101.064571	85555.805156	34.740877
1102.308851	85655.700691	34.745895
1103.089034	85770.977683	34.750912
1104.339722	85897.624559	34.755930
1105.144410	86024.570746	34.760948
1106.051208	86138.824281	34.765965
1107.176503	86266.568173	34.770983
1108.128983	86413.511214	34.776000
1109.157224	86541.999324	34.781018
1110.376698	86684.545295	34.786036
1111.148261	86820.992231	34.791053
1112.259300	86959.295597	34.796071
1113.329361	87094.868492	34.801088
1114.694611	87237.666863	34.806106
1115.759762	87373.918880	34.811124
1116.861231	87513.820788	34.816141
1117.868147	87656.211029	34.821159
1118.839718	87807.707020	34.826176
1120.030560	87953.648953	34.831194
1121.163963	88103.274884	34.836212
1122.206610	88242.836793	34.841229
1123.267464	88393.114943	34.846247
1124.317663	88546.582873	34.851264
1125.676624	88694.779553	34.856282
1126.929801	88861.243917	34.861300
1127.846259	89006.199560	34.866317
1129.439435	89146.033885	34.871335
1130.485187	89302.619141	34.876352
1131.752001	89444.176760	34.881370
1133.121046	89588.956826	34.886388
1134.015464	89738.353859	34.891405
1135.567900	89880.134503	34.896423
1136.878622	90021.328450	34.901440
1138.097249	90151.388827	34.906458
1139.032492	90308.776772	34.911476
1140.044031	90447.542063	34.916493
1141.722079	90578.227574	34.921511
1142.701039	90725.625862	34.926528
1143.712915	90858.986598	34.931546
1145.005833	91011.851559	34.936564
1146.128505	91145.367177	34.941581
1146.959633	91284.577562	34.946599
1148.104305	91427.407075	34.951616
1149.456173	91570.704195	34.956634
1150.250342	91715.918699	34.961652
1151.289462	91856.895775	34.966669
1153.059135	91993.526493	34.971687
1153.967618	92163.233179	34.976704
1155.071655	92297.935150	34.981722
1156.057512	92426.408023	34.986740
1157.120985	92593.569861	34.991757
1158.492803	92721.002752	34.996775
1159.181437	92863.142515	35.001792
1160.431721	93006.737119	35.006810
1161.319843	93143.142011	35.011828
1162.170543	93286.839931	35.016845
1163.800806	93425.531991	35.021863
1164.578969	93573.531589	35.026880
1165.886776	93712.833324	35.031898
1166.876875	93854.166190	35.036916
1167.960467	94017.559559	35.041933
1169.205028	94171.820371	35.046951
1170.281968	94324.938756	35.051968
1171.997265	94456.039886	35.056986
1172.896873	94609.770350	35.062004
1174.084519	94770.034359	35.067021
1175.572656	94906.854371	35.072039
1176.470544	95058.292110	35.077056
1177.763686	95218.776605	35.082074
1178.890132	95371.141580	35.087092
1180.142497	95515.606007	35.092109
1181.047440	95675.560914	35.097127
1181.802212	95841.265493	35.102144
1183.445661	95996.215576	35.107162
1184.432788	96152.782932	35.112180
1185.443435	96316.356530	35.117197
1186.699842	96486.312886	35.122215
1188.025138	96642.734990	35.127232
1189.482961	96814.009187	35.132250
1190.961021	96961.445478	35.137268
1192.190190	97141.867817	35.142285
1193.373213	97297.077197	35.147303
1194.523482	97461.769250	35.152320
1196.102343	97607.333873	35.157338
1197.549685	97766.217848	35.162356
1198.342202	97933.601885	35.167373
1199.625985	98068.468234	35.172391
1200.742937	98226.269249	35.177408
1201.794948	98388.560701	35.182426
1203.238711	98544.939154	35.187444
1204.490859	98712.369709	35.192461
1205.615249	98859.589892	35.197479
1206.658748	99028.049189	35.202496
1207.883851	99180.898643	35.207514
1209.084985	99331.152716	35.212532
1210.003809	99521.715160	35.217549
1211.785702	99659.055011	35.222567
1212.441897	99814.384301	35.227584
1213.694484	99985.006424	35.232602
1215.733694	100150.924148	35.237620
1216.559384	100309.646296	35.242637
1218.167552	100453.269429	35.247655
1219.323030	100624.038272	35.252672
1220.641276	100776.864564	35.257690
1221.929639	100924.932393	35.262708
1222.890442	101081.094916	35.267725
1224.397088	101227.870900	35.272743
1225.544835	101373.983591	35.277760
1226.307968	101528.712674	35.282778
1227.604715	101649.956680	35.287796
1229.042652	101789.679681	35.292813
1230.382815	101934.183502	35.297831
1231.020278	102079.742721	35.302848
1232.199851	102218.522322	35.307866
1233.794386	102366.430463	35.312884
1234.800054	102520.899802	35.317901
1236.079306	102662.608457	35.322919
1237.543616	102829.895971	35.327936
1238.331681	102973.551227	35.332954
1239.466062	103127.757342	35.337972
1240.449950	103293.669215	35.342989
1241.672373	103455.437672	35.348007
1242.640722	103631.940621	35.353024
1244.171787	103795.870731	35.358042
1245.153788	103967.792727	35.363060
1246.176218	104132.249000	35.368077
1247.763337	104296.002835	35.373095
1249.012688	104460.975854	35.378112
1250.386626	104651.077681	35.383130
1251.704663	104820.199788	35.388148
1252.697241	105005.865862	35.393165
1254.291363	105169.649959	35.398183
1255.457553	105358.113543	35.403200
1256.623622	105530.707424	35.408218
1258.179718	105689.748658	35.413236
1259.163130	105877.644240	35.418253
1260.491401	106051.810857	35.423271
1262.071294	106225.565367	35.428288
1263.038310	106413.625994	35.433306
1264.509351	106574.933274	35.438324
1265.914906	106755.737686	35.443341
1267.310490	106917.673148	35.448359
1268.474668	107098.259052	35.453376
1269.637796	107279.833760	35.458394
1271.335057	107444.724629	35.463412
1272.641770	107623.323587	35.468429
1273.571710	107794.743585	35.473447
1275.283462	107961.255878	35.478464
1276.181636	108136.322462	35.483482
1277.501932	108310.500443	35.488500
1278.842549	108487.296662	35.493517
1280.428240	108652.637589	35.498535
1281.520381	108834.368213	35.503552
1282.751926	109012.027380	35.508570
1284.162500	109171.956624	35.513588
1285.248661	109345.489395	35.518605
1286.342920	109526.553969	35.523623
1287.921261	109705.656793	35.528640
1289.124219	109884.067415	35.533658
1290.447457	110051.535635	35.538676
1291.459212	110236.485880	35.543693
1293.129784	110416.313483	35.548711
1294.538704	110577.081389	35.553728
1295.549090	110723.349301	35.558746
1296.964239	110893.891197	35.563764
1298.057560	111043.154414	35.568781
1299.258622	111207.282581	35.573799
1300.268440	111363.131269	35.578816
1301.453481	111550.950257	35.583834
1302.566671	111706.658091	35.588852
1303.936865	111895.969440	35.593869
1305.043187	112070.777975	35.598887
1306.583042	112244.873172	35.603904
1307.546329	112426.176207	35.608922
1309.409246	112595.063536	35.613940
1310.295505	112779.318556	35.618957
1311.692759	112973.533366	35.623975
1313.095325	113150.448358	35.628992
1314.377886	113339.138988	35.634010
1315.704845	113517.480258	35.639028
1316.918419	113721.681359	35.644045
1318.039406	113909.711981	35.649063
1319.579564	114094.119669	35.654080
1321.034761	114277.402733	35.659098
1322.452707	114459.635858	35.664116
1323.681297	114666.551759	35.669133
1324.834644	114854.514694	35.674151
1326.759501	115031.397964	35.679168
1327.705247	115222.220137	35.684186
1329.225442	115411.705276	35.689204
1330.392444	115615.555676	35.694221
1331.838406	115795.717511	35.699239
1333.373371	116000.018993	35.704256
1334.358065	116187.581835	35.709274
1335.848471	116379.035234	35.714292
1337.482093	116574.968711	35.719309
1338.877053	116776.247122	35.724327
1340.018918	116960.188273	35.729344
1341.212643	117163.306116	35.734362
1342.685774	117352.610642	35.739380
1343.915773	117552.154976	35.744397
1345.230395	117741.038052	35.749415
1346.633793	117943.900841	35.754432
1347.719608	118145.454450	35.759450
1349.473636	118336.133520	35.764468
1350.952447	118536.785643	35.769485
1352.096180	118742.823810	35.774503
1353.379894	118928.567389	35.779520
1354.743245	119127.298644	35.784538
1356.266420	119333.217897	35.789556
1357.331073	119532.328994	35.794573
1358.831904	119737.507863	35.799591
1360.260672	119931.878580	35.804608
1361.127077	120140.023491	35.809626
1363.149074	120346.321075	35.814644
1364.511809	120548.634573	35.819661
1365.476759	120721.980182	35.824679
1366.881875	120923.232389	35.829696
1367.981329	121114.314567	35.834714
1369.871805	121293.608433	35.839732
1371.032986	121477.211412	35.844749
1372.463458	121667.371159	35.849767
1373.832097	121855.338445	35.854784
1374.644616	122048.765353	35.859802
1376.311274	122242.488533	35.864820
1377.725494	122415.913244	35.869837
1378.813904	122639.975315	35.874855
1380.472936	122815.022869	35.879872
1381.984999	123016.628728	35.884890
1383.232936	123212.528012	35.889908
1384.650648	123422.865748	35.894925
1386.053109	123622.923114	35.899943
1387.666033	123809.814226	35.904960
1388.722685	124018.402864	35.909978
1390.251332	124214.226913	35.914996
1391.829591	124409.791196	35.920013
1392.913340	124617.607582	35.925031
1394.473926	124826.388420	35.930048
1396.018125	125026.611102	35.935066
1397.578603	125230.049942	35.940084
1398.968621	125425.676886	35.945101
1400.335469	125626.730209	35.950119
1402.018104	125828.976174	35.955136
1403.275772	126038.929229	35.960154
1404.582992	126240.047264	35.965172
1405.966506	126447.513459	35.970189
1407.264383	126657.262247	35.975207
1408.696270	126863.279894	35.980224
1410.188717	127074.736377	35.985242
1411.697640	127268.685671	35.990260
1412.643979	127498.688494	35.995277
1414.342000	127699.552539	36.000295
1416.112743	127899.823794	36.005312
1417.170029	128128.281500	36.010330
1418.553525	128336.002753	36.015348
1420.310228	128545.262422	36.020365
1421.299786	128751.985320	36.025383
1422.957694	128984.104412	36.030400
1424.217149	129196.032338	36.035418
1425.551010	129404.808330	36.040436
1427.280880	129627.027460	36.045453
1428.134804	129841.267077	36.050471
1430.034465	130052.035663	36.055488
1431.260444	130287.566158	36.060506
1432.684711	130498.768400	36.065524
1434.479424	130707.708990	36.070541
1435.557958	130932.715193	36.075559
1437.068245	131152.333582	36.080576
1438.594046	131370.760325	36.085594
1440.012615	131584.543518	36.090612
1441.549668	131803.934709	36.095629
1442.367826	132031.056203	36.100647
1444.422090	132222.749031	36.105664
1446.078361	132425.655698	36.110682
1447.115596	132629.206992	36.115700
1448.789094	132835.788091	36.120717
1450.117552	133033.987356	36.125735
1451.239045	133234.995627	36.130752
1452.631012	133444.121884	36.135770
1454.226526	133651.342145	36.140788
1455.753513	133857.789245	36.145805
1456.905695	134075.536024	36.150823
1458.527967	134284.403780	36.155840
1460.112347	134506.139712	36.160858
1461.507652	134723.992165	36.165876
1463.076509	134929.680102	36.170893
1464.447615	135158.246487	36.175911
1465.785237	135373.794260	36.180928
1467.220221	135594.789395	36.185946
1468.474888	135814.091595	36.190964
1469.903903	136032.417409	36.195981
1471.442302	136267.707087	36.200999
1473.104122	136485.695208	36.206016
1474.533867	136717.242371	36.211034
1475.864219	136950.796615	36.216052
1477.227684	137160.828717	36.221069
1478.949302	137402.282251	36.226087
1480.647305	137632.488845	36.231104
1482.035211	137878.649930	36.236122
1483.686526	138102.873755	36.241140
1485.397544	138332.044648	36.246157
1486.119721	138569.472065	36.251175
1488.013505	138794.891844	36.256192
1489.768836	139027.001095	36.261210
1491.046018	139260.252638	36.266228
1492.645713	139503.428215	36.271245
1494.081476	139735.517745	36.276263
1495.480790	139971.454774	36.281280
1497.348628	140201.730417	36.286298
1499.208121	140425.495170	36.291316
1500.655546	140654.903289	36.296333
1502.139959	140893.330693	36.301351
1504.201915	141125.711715	36.306368
1505.563702	141335.076607	36.311386
1506.851104	141563.642610	36.316404
1508.792702	141791.447370	36.321421
1509.867771	142014.119221	36.326439
1511.544615	142233.706059	36.331456
1513.085952	142456.712643	36.336474
1514.784732	142692.686778	36.341492
1516.219614	142908.565407	36.346509
1517.664422	143141.642961	36.351527
1519.339752	143366.789541	36.356544
1521.362777	143572.503303	36.361562
1522.288585	143800.357738	36.366580
1524.041985	144016.345669	36.371597
1525.744091	144235.752766	36.376615
1527.040227	144448.951895	36.381632
1528.372034	144642.817622	36.386650
1529.954221	144841.435923	36.391668
1531.573995	145046.944755	36.396685
1532.565357	145256.762931	36.401703
1533.749303	145454.206264	36.406720
1535.620029	145680.403404	36.411738
1536.491190	145898.927592	36.416756
1538.230840	146113.145097	36.421773
1539.647954	146337.796605	36.426791
1541.009818	146556.969939	36.431808
1542.150734	146797.437147	36.436826
1543.711953	147039.259117	36.441844
1545.540416	147269.632131	36.446861
1546.610418	147513.525900	36.451879
1547.806000	147757.376246	36.456896
1549.634315	147988.071423	36.461914
1550.971190	148244.668042	36.466932
1552.828861	148493.540103	36.471949
1554.079809	148758.939290	36.476967
1555.681598	149010.175839	36.481984
1556.940902	149262.964625	36.487002
1558.396733	149527.209403	36.492020
1560.225643	149781.420328	36.497037
1561.698160	150060.105879	36.502055
1563.380605	150319.427816	36.507072
1565.329573	150581.473136	36.512090
1566.524165	150851.297543	36.517108
1568.441253	151107.812173	36.522125
1569.735572	151373.454184	36.527143
1571.619128	151644.912551	36.532160
1573.147403	151909.989299	36.537178
1574.935836	152184.979003	36.542196
1576.767124	152443.419432	36.547213
1578.501036	152702.561977	36.552231
1579.765930	152970.820608	36.557248
1581.460644	153236.743726	36.562266
1583.091040	153496.035722	36.567284
1584.810694	153758.333045	36.572301
1586.360249	154023.664283	36.577319
1588.024444	154296.928961	36.582336
1589.553859	154557.513135	36.587354
1590.997394	154824.908863	36.592372
1592.900313	155081.190352	36.597389
1594.303880	155341.027184	36.602407
1595.776826	155616.019304	36.607424
1597.686049	155882.081540	36.612442
1599.167046	156144.321318	36.617460
1601.180034	156400.772853	36.622477
1602.719909	156678.628529	36.627495
1604.291336	156944.042687	36.632512
1605.924602	157202.576644	36.637530
1607.242499	157470.964192	36.642548
1609.101153	157727.767209	36.647565
1610.933110	157980.430003	36.652583
1612.560190	158224.923133	36.657600
1614.308163	158467.915204	36.662618
1615.510363	158705.936218	36.667636
1617.268232	158937.720604	36.672653
1619.171692	159176.470369	36.677671
1620.382693	159408.053101	36.682688
1622.121764	159664.090602	36.687706
1623.581084	159916.256055	36.692724
1624.977704	160145.037098	36.697741
1627.055934	160393.823342	36.702759
1628.538947	160647.385187	36.707776
1630.286928	160886.386886	36.712794
1631.425579	161129.811273	36.717812
1632.776275	161394.216565	36.722829
1634.634413	161662.334967	36.727847
1636.475834	161924.206071	36.732864
1638.026031	162172.264386	36.737882
1639.366931	162446.672132	36.742900
1640.909319	162702.280959	36.747917
1642.845279	162969.255452	36.752935
1644.199391	163253.495707	36.757952
1646.251815	163522.053726	36.762970
1647.761972	163783.851506	36.767988
1649.207758	164049.580212	36.773005
1650.936174	164332.336394	36.778023
1652.546486	164607.427973	36.783040
1654.222590	164872.783678	36.788058
1655.850858	165157.946473	36.793076
1657.544540	165430.849588	36.798093
1659.235343	165712.493642	36.803111
1660.850214	166001.939213	36.808128
1662.743084	166279.509650	36.813146
1664.235157	166561.597587	36.818164
1665.908297	166834.184560	36.823181
1667.848415	167123.396971	36.828199
1669.518419	167403.294177	36.833216
1671.232303	167686.826665	36.838234
1673.118876	167971.094883	36.843252
1674.643546	168251.757139	36.848269
1676.391715	168523.152204	36.853287
1677.894050	168811.051905	36.858304
1679.714133	169097.609563	36.863322
1681.213832	169382.127391	36.868340
1682.748052	169664.612392	36.873357
1685.115893	169935.754228	36.878375
1686.806671	170236.039935	36.883392
1688.590249	170490.040464	36.888410
1689.968258	170779.852013	36.893428
1691.904773	171050.321810	36.898445
1693.847910	171328.174933	36.903463
1695.145604	171623.155523	36.908480
1697.281063	171886.978090	36.913498
1698.983199	172162.883910	36.918516
1700.522914	172441.747713	36.923533
1702.290661	172710.746297	36.928551
1704.234326	172966.348557	36.933568
1706.046396	173214.184594	36.938586
1707.518392	173474.203411	36.943604
1709.204986	173716.810768	36.948621
1711.079655	173972.278248	36.953639
1712.267600	174226.016998	36.958656
1713.852616	174476.840021	36.963674
1715.558115	174748.640455	36.968692
1717.252003	175014.494896	36.973709
1719.126379	175262.536726	36.978727
1720.407144	175540.803666	36.983744
1722.284249	175810.224397	36.988762
1723.794660	176079.984240	36.993780
1725.116520	176359.975586	36.998797
1727.166676	176631.632431	37.003815
1728.202317	176920.325168	37.008832
1730.008530	177203.036385	37.013850
1731.876682	177492.463626	37.018868
1733.836245	177790.492669	37.023885
1735.563542	178081.836721	37.028903
1737.091484	178376.804864	37.033920
1739.066138	178665.753959	37.038938
1740.337028	178979.188695	37.043956
1741.906751	179274.245338	37.048973
1743.792330	179565.485778	37.053991
1745.584846	179878.628699	37.059008
1747.575673	180181.148421	37.064026
1749.166338	180492.412116	37.069044
1750.610188	180808.332382	37.074061
1752.798811	181108.556192	37.079079
1754.582755	181432.420328	37.084096
1756.576224	181739.239135	37.089114
1758.497721	182052.136415	37.094132
1759.912436	182364.596207	37.099149
1762.471178	182664.734006	37.104167
1764.128905	182986.422048	37.109184
1765.749211	183290.989097	37.114202
1767.871691	183580.138189	37.119220
1769.531510	183893.191706	37.124237
1771.233843	184198.348362	37.129255
1773.081198	184497.951813	37.134272
1774.531916	184801.452271	37.139290
1776.739353	185104.263648	37.144308
1778.334977	185417.947144	37.149325
1780.570125	185722.331724	37.154343
1781.902778	186029.196447	37.159360
1784.025270	186336.153566	37.164378
1785.971932	186639.549600	37.169396
1787.802828	186933.410918	37.174413
1789.393683	187239.037311	37.179431
1791.287746	187544.046570	37.184448
1793.301012	187834.864591	37.189466
1795.033511	188139.548128	37.194484
1796.990650	188445.974577	37.199501
1798.990388	188727.638305	37.204519
1800.262824	189021.157416	37.209536
1801.878756	189289.053398	37.214554
1803.668044	189565.628803	37.219572
1805.473746	189855.248739	37.224589
1807.090664	190134.177144	37.229607
1808.535754	190418.312126	37.234624
1810.177382	190709.536926	37.239642
1812.181190	191002.761864	37.244660
1813.346190	191306.553412	37.249677
1815.660206	191597.384979	37.254695
1817.384338	191918.985446	37.259712
1819.342886	192215.156507	37.264730
1820.933968	192513.037523	37.269748
1823.005385	192817.735300	37.274765
1824.790758	193123.089553	37.279783
1826.300083	193436.294568	37.284800
1828.201242	193749.477441	37.289818
1829.907314	194068.302813	37.294836
1831.523377	194386.928764	37.299853
1833.650249	194695.449411	37.304871
1835.349141	195019.688555	37.309888
1837.427950	195341.521529	37.314906
1839.349367	195658.444469	37.319924
1840.990695	195997.992519	37.324941
1843.004192	196307.150211	37.329959
1844.374199	196645.501834	37.334976
1846.665183	196967.806388	37.339994
1848.510330	197305.503091	37.345012
1850.458874	197630.671093	37.350029
1852.594142	197968.605285	37.355047
1854.112617	198298.326087	37.360064
1856.149360	198623.537038	37.365082
1858.423226	198942.315339	37.370100
1860.151632	199273.950874	37.375117
1862.021869	199593.837954	37.380135
1863.745467	199934.705925	37.385152
1865.793669	200250.887795	37.390170
1868.097242	200580.840844	37.395188
1869.605959	200920.073701	37.400205
1871.530394	201245.661136	37.405223
1873.573758	201571.866293	37.410240
1875.119133	201897.289300	37.415258
1877.098517	202224.244694	37.420276
1879.201878	202576.480177	37.425293
1881.383607	202893.278114	37.430311
1883.301399	203223.638313	37.435328
1885.185034	203546.783242	37.440346
1886.974694	203868.853290	37.445364
1888.489342	204199.486302	37.450381
1890.493180	204519.558528	37.455399
1892.672780	204856.677890	37.460416
1894.744956	205184.524328	37.465434
1896.197007	205508.891349	37.470452
1898.244562	205850.531165	37.475469
1900.261748	206166.167499	37.480487
1901.884939	206472.410886	37.485504
1903.885099	206793.435652	37.490522
1905.640007	207087.208248	37.495540
1907.304424	207398.832308	37.500557
1909.577324	207706.286500	37.505575
1911.346338	208008.642877	37.510592
1913.014438	208325.374392	37.515610
1915.078670	208640.952959	37.520628
1916.616138	208950.015511	37.525645
1918.927703	209267.513072	37.530663
1920.317888	209595.987239	37.535680
1921.827302	209911.622352	37.540698
1924.299794	210238.988752	37.545716
1925.752050	210579.163091	37.550733
1927.566912	210918.075697	37.555751
1929.850079	211251.583827	37.560768
1931.786708	211592.537370	37.565786
1933.794457	211927.705080	37.570804
1935.423540	212274.842946	37.575821
1937.407177	212614.943911	37.580839
1939.524290	212955.469834	37.585856
1941.251487	213308.831217	37.590874
1943.519574	213658.134931	37.595892
1945.286406	214013.068101	37.600909
1947.257125	214345.651580	37.605927
1949.504096	214704.130578	37.610944
1951.177089	215061.534566	37.615962
1953.053881	215416.622836	37.620980
1955.120830	215774.539421	37.625997
1956.995072	216116.808731	37.631015
1959.064693	216490.052914	37.636032
1960.785556	216857.196775	37.641050
1963.197372	217202.522179	37.646068
1965.027857	217572.128225	37.651085
1967.072149	217937.969530	37.656103
1969.118030	218296.486580	37.661120
1970.976514	218657.384057	37.666138
1973.247318	219020.858844	37.671156
1974.784016	219393.834860	37.676173
1976.906876	219749.693371	37.681191
1978.985829	220113.077141	37.686208
1980.857847	220483.555050	37.691226
1983.071741	220844.026133	37.696244
1984.954818	221222.098799	37.701261
1987.291538	221595.543132	37.706279
1989.446221	221952.651540	37.711296
1991.143094	222315.192519	37.716314
1993.212690	222676.977730	37.721332
1995.059093	223057.401706	37.726349
1997.264105	223416.819902	37.731367
1998.997726	223826.456938	37.736384
2001.080381	224219.038707	37.741402
2003.273445	224574.350110	37.746420
2005.109838	224953.400852	37.751437
2006.960708	225296.884755	37.756455
2009.284667	225647.431210	37.761472
2011.416276	225986.645140	37.766490
2013.312394	226333.237225	37.771508
2015.156146	226675.890020	37.776525
2017.104322	227019.568899	37.781543
2019.088487	227361.008630	37.786560
2020.829323	227721.052977	37.791578
2023.114655	228067.730196	37.796596
2024.817686	228421.713797	37.801613
2026.669498	228776.691111	37.806631
2028.838040	229139.416391	37.811648
2030.799867	229499.458529	37.816666
2032.555579	229868.957068	37.821684
2034.506590	230241.753160	37.826701
2036.575143	230613.770250	37.831719
2038.638495	230983.148400	37.836736
2040.470450	231371.663496	37.841754
2042.579233	231746.955094	37.846772
2044.799688	232119.182806	37.851789
2046.444976	232515.122991	37.856807
2048.948345	232891.118525	37.861824
2050.896182	233282.213770	37.866842
2052.911064	233669.439501	37.871860
2054.741569	234058.016731	37.876877
2056.775883	234446.385391	37.881895
2059.079662	234844.567325	37.886912
2061.247235	235239.546885	37.891930
2063.432423	235622.206997	37.896948
2065.590789	236028.772772	37.901965
2067.769704	236426.041027	37.906983
2070.065134	236817.298241	37.912000
2071.886522	237218.867829	37.917018
2074.033263	237608.449869	37.922036
2076.306118	238005.480619	37.927053
2078.381213	238404.195146	37.932071
2080.927688	238786.225323	37.937088
2082.802646	239189.647908	37.942106
2085.123732	239576.085241	37.947124
2087.234170	239963.801894	37.952141
2089.341126	240359.343468	37.957159
2091.311115	240749.040832	37.962176
2093.256670	241150.300227	37.967194
2095.703093	241532.584130	37.972212
2097.710652	241930.864576	37.977229
2099.743435	242322.716166	37.982247
2102.341133	242717.451206	37.987264
2104.239736	243109.860008	37.992282
2106.366958	243504.418195	37.997300
2108.297215	243897.510252	38.002317
2110.251515	244300.277226	38.007335
2112.981139	244677.826888	38.012352
2115.085290	245073.358784	38.017370
2116.952462	245472.637933	38.022388
2119.233198	245859.634977	38.027405
2121.134519	246256.447172	38.032423
2123.315404	246611.254124	38.037440
2125.015719	246984.096587	38.042458
2127.299234	247347.830215	38.047476
2129.777792	247710.517796	38.052493
2131.501561	248076.602742	38.057511
2133.298496	248440.797319	38.062528
2135.355486	248822.452922	38.067546
2137.506105	249190.530402	38.072564
2140.081377	249581.300943	38.077581
2141.858742	249956.678824	38.082599
2144.158289	250332.101782	38.087616
2146.227228	250717.113147	38.092634
2148.404035	251097.485245	38.097652
2150.334445	251477.109857	38.102669
2152.401509	251874.469392	38.107687
2154.559237	252263.382119	38.112704
2156.602442	252667.123102	38.117722
2158.761651	253065.740855	38.122740
2160.881980	253472.900687	38.127757
2162.883926	253877.692429	38.132775
2164.872623	254282.690374	38.137792
2166.919959	254706.604393	38.142810
2169.162667	255124.696687	38.147828
2171.478936	255523.548797	38.152845
2173.585387	255946.490842	38.157863
2176.009270	256367.351240	38.162880
2178.067785	256792.690433	38.167898
2180.351205	257210.450313	38.172916
2182.818496	257635.497717	38.177933
2184.692779	258061.198836	38.182951
2187.125079	258480.868070	38.187968
2188.875783	258915.201800	38.192986
2191.406312	259339.988288	38.198004
2194.079722	259765.083086	38.203021
2195.779582	260203.135934	38.208039
2198.173403	260631.019999	38.213056
2200.243150	261061.750447	38.218074
2202.565589	261495.794663	38.223092
2204.693425	261918.972603	38.228109
2207.078493	262359.155675	38.233127
2209.476360	262776.906617	38.238144
2211.420904	263217.033773	38.243162
2213.657055	263644.515425	38.248180
2216.235738	264072.527577	38.253197
2218.861317	264511.786360	38.258215
2221.024389	264941.211844	38.263232
2222.860138	265367.717572	38.268250
2225.472954	265791.661846	38.273268
2227.712462	266228.799184	38.278285
2229.991721	266651.247651	38.283303
2232.518986	267074.241471	38.288320
2234.368812	267502.753987	38.293338
2236.599406	267939.335532	38.298356
2239.113424	268366.422501	38.303373
2240.950108	268794.455526	38.308391
2243.356937	269193.464128	38.313408
2245.586256	269593.618888	38.318426
2247.654474	269989.353865	38.323444
2250.307693	270378.467653	38.328461
2252.193233	270790.693398	38.333479
2254.449235	271180.581877	38.338496
2256.720873	271592.950028	38.343514
2258.619223	271998.391625	38.348532
2260.921406	272404.480641	38.353549
2262.866569	272822.591408	38.358567
2264.962873	273231.075859	38.363584
2266.894215	273660.264946	38.368602
2269.264179	274083.541804	38.373620
2271.130312	274507.584525	38.378637
2273.321216	274968.004308	38.383655
2275.517051	275400.454199	38.388672
2277.902444	275842.374938	38.393690
2280.035047	276294.116078	38.398708
2282.668711	276736.403895	38.403725
2284.815813	277192.486665	38.408743
2287.539213	277650.408655	38.413760
2289.736829	278098.023932	38.418778
2292.321267	278553.529035	38.423796
2294.681311	278995.123125	38.428813
2296.771943	279466.684964	38.433831
2299.434260	279906.020711	38.438848
2301.709879	280356.086993	38.443866
2303.577156	280831.570332	38.448884
2306.263967	281276.414070	38.453901
2308.495564	281740.407610	38.458919
2311.354049	282182.734059	38.463936
2313.489430	282656.776528	38.468954
2315.713025	283104.436064	38.473972
2318.727850	283552.630289	38.478989
2320.974462	284016.060847	38.484007
2323.475252	284464.716833	38.489024
2325.890803	284912.318980	38.494042
2327.926306	285364.807537	38.499060
2330.780745	285818.969410	38.504077
2333.137825	286274.352774	38.509095
2335.571862	286714.202147	38.514112
2337.896520	287166.490430	38.519130
2340.402506	287614.684925	38.524148
2342.948414	288056.089929	38.529165
2345.244816	288513.385333	38.534183
2347.492103	288939.797970	38.539200
2350.153165	289380.293822	38.544218
2352.229176	289828.807461	38.549236
2354.569218	290268.895644	38.554253
2356.854261	290716.942923	38.559271
2359.342786	291151.061946	38.564288
2361.182118	291609.872946	38.569306
2364.039515	292051.425799	38.574324
2366.300362	292498.381584	38.579341
2368.272999	292941.216235	38.584359
2370.982698	293367.980481	38.589376
2373.400923	293777.491104	38.594394
2375.576491	294200.528124	38.599412
2377.971240	294616.442349	38.604429
2380.351053	295021.384367	38.609447
2382.688805	295442.107072	38.614464
2384.756415	295862.465319	38.619482
2387.028839	296296.863016	38.624500
2389.393523	296720.017433	38.629517
2391.483582	297160.183015	38.634535
2393.693499	297595.934055	38.639552
2396.254343	298033.940034	38.644570
2398.376042	298483.115185	38.649588
2400.925877	298923.610160	38.654605
2402.969821	299386.563133	38.659623
2405.568409	299832.560274	38.664640
2408.036954	300293.538388	38.669658
2409.959688	300758.818397	38.674676
2412.891627	301208.366054	38.679693
2415.121919	301681.240511	38.684711
2417.247090	302154.384232	38.689728
2419.925796	302629.191464	38.694746
2421.940931	303112.611772	38.699764
2424.312221	303586.728098	38.704781
2427.101670	304069.920968	38.709799
2429.679508	304545.677915	38.714816
2432.036629	305038.385178	38.719834
2434.739549	305516.328906	38.724852
2437.410256	305997.628963	38.729869
2439.903710	306478.676004	38.734887
2442.156898	306960.089598	38.739904
2445.082874	307441.725007	38.744922
2447.536663	307931.332934	38.749940
2449.853461	308404.577608	38.754957
2452.324493	308893.798080	38.759975
2454.689363	309377.343861	38.764992
2457.461269	309864.506194	38.770010
2459.933194	310355.117660	38.775028
2462.450276	310837.922257	38.780045
2465.005131	311333.469432	38.785063
2467.468099	311813.560801	38.790080
2470.144590	312279.748288	38.795098
2472.534480	312777.118672	38.800116
2475.148360	313262.208972	38.805133
2477.872540	313741.285484	38.810151
2480.370420	314239.419474	38.815168
2483.053694	314721.368163	38.820186
2485.486840	315189.181855	38.825204
2488.066912	315672.260057	38.830221
2490.926530	316153.183624	38.835239
2493.222711	316622.790379	38.840256
2495.847329	317084.825040	38.845274
2498.371794	317566.988655	38.850292
2500.423853	318046.532582	38.855309
2503.015952	318511.892796	38.860327
2505.625831	318963.507804	38.865344
2508.158954	319392.300443	38.870362
2510.188571	319846.187367	38.875380
2512.989389	320292.787834	38.880397
2515.332597	320731.763305	38.885415
2517.628902	321181.944190	38.890432
2520.369149	321626.312779	38.895450
2522.347963	322085.707727	38.900468
2524.954118	322539.870759	38.905485
2527.668233	323003.487231	38.910503
2530.041333	323445.695313	38.915520
2532.715129	323920.005131	38.920538
2534.900891	324388.345359	38.925556
2537.504468	324861.822954	38.930573
2539.594234	325332.763505	38.935591
2541.802429	325824.761015	38.940608
2544.445676	326298.935165	38.945626
2546.441335	326788.395580	38.950644
2549.164316	327289.292589	38.955661
2552.006787	327783.463216	38.960679
2554.635934	328283.099045	38.965696
2557.302191	328779.678426	38.970714
2559.349779	329284.478896	38.975732
2562.148113	329799.060896	38.980749
2564.827509	330303.475166	38.985767
2567.436591	330823.336764	38.990784
2570.189223	331337.509152	38.995802
2572.561505	331844.729554	39.000820
2574.991528	332363.846838	39.005837
2577.791968	332887.675653	39.010855
2580.428348	333417.214692	39.015872
2583.080305	333933.238267	39.020890
2585.630702	334460.193032	39.025908
2588.404681	334978.906594	39.030925
2591.053647	335507.234384	39.035943
2593.865569	336026.746589	39.040960
2596.558278	336551.453669	39.045978
2599.417790	337067.776336	39.050996
2602.182539	337594.723704	39.056013
2604.337544	338121.052514	39.061031
2607.179550	338637.949702	39.066048
2610.336056	339154.488268	39.071066
2612.699961	339676.911968	39.076084
2615.459663	340206.987433	39.081101
2618.116258	340719.073045	39.086119
2621.186036	341240.000979	39.091136
2623.656831	341744.515998	39.096154
2626.167676	342265.904734	39.101172
2628.636400	342777.469983	39.106189
2631.550173	343294.622254	39.111207
2633.973080	343824.542404	39.116224
2636.713667	344341.230742	39.121242
2639.234289	344850.739076	39.126260
2642.186983	345378.682731	39.131277
2645.134019	345870.317429	39.136295
2647.445596	346375.631210	39.141312
2650.310354	346845.894009	39.146330
2652.772415	347309.590598	39.151348
2655.476772	347793.097951	39.156365
2658.090691	348266.232173	39.161383
2660.377417	348741.470593	39.166400
2663.230634	349226.566834	39.171418
2665.663075	349716.802791	39.176436
2668.093462	350208.354809	39.181453
2670.908192	350690.169473	39.186471
2673.135814	351202.840455	39.191488
2675.603241	351690.387678	39.196506
2678.316547	352210.511672	39.201524
2680.841126	352714.769447	39.206541
2683.321737	353230.097180	39.211559
2686.199828	353757.109978	39.216576
2688.596869	354270.460752	39.221594
2691.230722	354797.654037	39.226612
2693.903685	355323.820398	39.231629
2697.185546	355847.727326	39.236647
2699.743949	356392.633892	39.241664
2702.275111	356930.761651	39.246682
2705.210296	357457.625883	39.251700
2707.929991	357994.747824	39.256717
2710.284270	358544.815978	39.261735
2712.971768	359100.891497	39.266752
2716.267522	359626.431823	39.271770
2718.926326	360177.423309	39.276788
2721.350612	360731.186814	39.281805
2724.424439	361271.313129	39.286823
2727.058574	361828.076409	39.291840
2729.794661	362377.406004	39.296858
2732.820694	362927.749233	39.301876
2735.479785	363489.514150	39.306893
2738.212186	364037.225950	39.311911
2741.112991	364595.030796	39.316928
2743.385158	365156.735222	39.321946
2746.623384	365710.057172	39.326964
2749.259138	366277.019645	39.331981
2752.172205	366833.551597	39.336999
2754.662013	367397.934522	39.342016
2757.812275	367954.288064	39.347034
2760.473361	368529.541618	39.352052
2763.201012	369092.850200	39.357069
2765.958918	369663.581925	39.362087
2768.425880	370242.396336	39.367104
2771.391345	370794.073873	39.372122
2774.439929	371363.798214	39.377140
2777.151510	371935.065424	39.382157
2780.373361	372490.207524	39.387175
2783.350570	373069.587905	39.392192
2785.652599	373625.495023	39.397210
2788.848411	374190.412987	39.402228
2791.630287	374745.772419	39.407245
2794.211228	375301.003949	39.412263
2796.760712	375845.804906	39.417280
2799.308859	376375.197982	39.422298
2802.076640	376907.873059	39.427316
2804.350368	377453.431854	39.432333
2807.685651	377977.985554	39.437351
2810.001793	378525.146763	39.442368
2812.736475	379074.568225	39.447386
2815.624702	379614.824545	39.452404
2817.983914	380170.810236	39.457421
2821.036254	380724.166713	39.462439
2822.966054	381307.070186	39.467456
2826.106059	381867.347518	39.472474
2828.996218	382438.970415	39.477492
2831.468627	383020.366742	39.482509
2834.894111	383592.141262	39.487527
2837.625401	384180.759228	39.492544
2840.223301	384771.316956	39.497562
2843.040087	385358.888230	39.502580
2845.618942	385954.706392	39.507597
2848.545234	386548.050243	39.512615
2851.806305	387151.249203	39.517632
2854.556540	387746.199540	39.522650
2857.492974	388357.064675	39.527668
2860.032257	388968.895468	39.532685
2863.121295	389569.088565	39.537703
2865.914481	390183.876678	39.542720
2868.854129	390804.083892	39.547738
2871.606089	391420.201333	39.552756
2875.086796	392040.275822	39.557773
2878.144389	392653.660294	39.562791
2881.135953	393278.938520	39.567808
2884.056730	393897.648411	39.572826
2887.122790	394511.708747	39.577844
2889.643285	395135.480945	39.582861
2892.618496	395749.051629	39.587879
2895.701421	396372.965697	39.592896
2898.442015	396994.133073	39.597914
2901.822022	397608.949842	39.602932
2904.528022	398238.923963	39.607949
2907.512820	398853.577482	39.612967
2910.475143	399483.614166	39.617984
2913.659160	400100.976702	39.623002
2917.165815	400721.192342	39.628020
2919.717640	401347.353486	39.633037
2923.009978	401950.642816	39.638055
2925.738721	402572.594180	39.643072
2928.707679	403193.912352	39.648090
2931.597209	403801.667424	39.653108
2934.790712	404426.196497	39.658125
2937.675522	405045.717151	39.663143
2940.792671	405664.681817	39.668160
2943.477680	406278.379047	39.673178
2946.901375	406894.102028	39.678196
2949.416087	407514.874469	39.683213
2952.497347	408107.888998	39.688231
2955.370554	408686.780539	39.693248
2958.088106	409268.600794	39.698266
2960.915525	409851.305063	39.703284
2964.192786	410419.048201	39.708301
2966.882647	410994.274849	39.713319
2969.641154	411571.456629	39.718336
2972.325454	412148.410920	39.723354
2975.393343	412744.428912	39.728372
2977.868134	413334.547479	39.733389
2980.847110	413937.069115	39.738407
2983.679022	414547.635605	39.743424
2986.700985	415144.144586	39.748442
2989.440621	415763.164875	39.753460
2992.048080	416383.307937	39.758477
2995.215741	417003.754502	39.763495
2998.143967	417641.862838	39.768512
3000.843353	418271.529516	39.773530
3004.132638	418907.322517	39.778548
3006.658223	419566.179430	39.783565
3009.589066	420217.684683	39.788583
3012.736844	420868.355042	39.793600
3015.344302	421523.149775	39.798618
3018.393976	422189.843452	39.803636
3021.570038	422859.440108	39.808653
3024.801073	423530.481296	39.813671
3027.718724	424203.303811	39.818688
3030.774552	424885.613621	39.823706
3034.277229	425554.738121	39.828724
3037.371756	426240.098514	39.833741
3040.644984	426914.317639	39.838759
3043.718512	427584.118389	39.843776
3046.615997	428273.181883	39.848794
3049.806606	428946.982884	39.853812
3052.815071	429631.738067	39.858829
3056.102596	430318.179037	39.863847
3059.439621	431008.748113	39.868864
3062.175622	431690.453335	39.873882
3065.731024	432370.136843	39.878900
3068.807040	433054.107909	39.883917
3071.674337	433737.840618	39.888935
3075.320968	434420.798690	39.893952
3078.625492	435108.781581	39.898970
3081.829778	435782.631073	39.903988
3085.238001	436451.087211	39.909005
3088.268101	437125.156425	39.914023
3091.814245	437808.773514	39.919040
3094.647675	438472.582335	39.924058
3098.042457	439119.952993	39.929076
3101.234775	439802.710506	39.934093
3103.936741	440475.424455	39.939111
3107.542670	441133.140448	39.944128
3110.321278	441794.058455	39.949146
3113.308053	442484.597155	39.954164
3116.397859	443134.543286	39.959181
3119.396336	443787.524305	39.964199
3122.156084	444437.943305	39.969216
3125.181026	445074.886200	39.974234
3128.729043	445690.871000	39.979252
3131.499555	446325.947603	39.984269
3134.086483	446973.338034	39.989287
3137.271545	447612.769558	39.994304
3139.858805	448237.901746	39.999322
3143.243455	448893.820209	40.004340
3145.670294	449584.697616	40.009357
3148.833792	450232.818169	40.014375
3151.537467	450899.012679	40.019392
3154.763245	451600.434328	40.024410
3157.799295	452292.096347	40.029428
3160.732236	452979.502476	40.034445
3163.333452	453669.622739	40.039463
3166.502920	454385.341221	40.044480
3170.144413	455086.185286	40.049498
3173.061409	455841.522682	40.054516
3176.028567	456542.934173	40.059533
3179.276294	457292.452240	40.064551
3182.643256	458002.002789	40.069568
3185.113624	458745.573491	40.074586
3188.712370	459496.378439	40.079604
3192.281617	460215.489978	40.084621
3195.075784	461019.747914	40.089639
3198.577571	461743.474520	40.094656
3201.670238	462516.162102	40.099674
3205.169738	463266.246144	40.104692
3208.203452	464062.006517	40.109709
3211.379788	464807.484661	40.114727
3215.093573	465555.937369	40.119744
3217.952868	466344.609494	40.124762
3221.544813	467114.169368	40.129780
3224.916703	467878.374867	40.134797
3228.068969	468661.654208	40.139815
3231.586196	469426.893047	40.144832
3234.657233	470184.133552	40.149850
3237.956132	470969.123728	40.154868
3241.268658	471760.605225	40.159885
3244.485651	472503.629483	40.164903
3247.942220	473318.844770	40.169920
3250.785419	474102.422331	40.174938
3254.459924	474847.008244	40.179956
3257.789417	475651.178820	40.184973
3261.010342	476411.553050	40.189991
3264.340294	477213.436825	40.195008
3267.694344	477973.933107	40.200026
3271.250339	478787.749477	40.205044
3274.579136	479555.418091	40.210061
3277.898083	480307.389207	40.215079
3281.696773	481093.676452	40.220096
3284.175049	481886.408307	40.225114
3287.819724	482640.108784	40.230132
3290.988662	483439.087083	40.235149
3294.187395	484194.314088	40.240167
3297.394800	484930.256731	40.245184
3300.480532	485698.076425	40.250202
3303.452531	486431.724979	40.255220
3306.370942	487153.732384	40.260237
3309.367944	487890.554840	40.265255
3312.722689	488637.548656	40.270272
3315.631186	489408.228101	40.275290
3318.661838	490220.687584	40.280308
3321.780068	490974.699172	40.285325
3324.979923	491750.894624	40.290343
3328.095942	492559.400009	40.295360
3331.584832	493327.603919	40.300378
3334.624190	494150.144959	40.305396
3337.915143	494955.336058	40.310413
3341.023606	495762.641983	40.315431
3344.556238	496597.722873	40.320448
3347.876743	497403.811761	40.325466
3350.980457	498260.195518	40.330484
3354.606807	499066.212706	40.335501
3357.996187	499933.631636	40.340519
3361.329103	500759.210935	40.345536
3364.313556	501608.991437	40.350554
3367.834169	502455.213608	40.355572
3371.378799	503298.514088	40.360589
3374.685885	504183.307801	40.365607
3378.154003	505000.844002	40.370624
3381.380319	505882.637252	40.375642
3384.647047	506795.724052	40.380660
3388.130872	507642.712038	40.385677
3391.855336	508507.991383	40.390695
3395.215038	509380.602734	40.395712
3398.259460	510298.031619	40.400730
3402.142469	511136.660339	40.405748
3405.506415	512060.504255	40.410765
3408.630695	512933.425919	40.415783
3412.785263	513794.838212	40.420800
3415.696384	514703.776429	40.425818
3419.116966	515627.921201	40.430836
3422.690409	516538.118440	40.435853
3426.010839	517413.803404	40.440871
3430.079099	518273.031961	40.445888
3433.276521	519188.944188	40.450906
3436.801490	520136.174383	40.455924
3440.479341	521024.825405	40.460941
3444.154245	521928.809447	40.465959
3448.094095	522820.095044	40.470976
3451.659850	523679.825960	40.475994
3454.882122	524601.784453	40.481012
3458.809019	525473.010033	40.486029
3462.026384	526351.156988	40.491047
3465.108402	527227.008658	40.496064
3469.108602	528094.601631	40.501082
3472.905869	528981.233060	40.506100
3476.605839	529900.391074	40.511117
3479.548717	530746.154503	40.516122
3483.160319	531533.122796	40.521127
3486.535312	532275.222891	40.526132
3489.626268	532980.602712	40.531136
3492.756440	533629.209914	40.536141
3495.597049	534201.502234	40.541146
3498.791667	534714.865242	40.546151
3500.759551	535179.506162	40.551156
3503.090000	535589.874181	40.556160
3505.441732	535976.890968	40.561165
3507.009583	536279.717755	40.566170
3508.877979	536496.117148	40.571175
3510.038158	536697.775334	40.576180
3511.346300	536863.191854	40.581184
3512.700251	536978.140317	40.586189
3513.918464	537069.218478	40.591194
3515.365705	537113.488470	40.596199
3516.226620	537144.314577	40.601204
3516.868497	537125.474328	40.606208
3518.479814	537081.377742	40.611213
3519.185866	537006.310271	40.616218
3520.254288	536887.999241	40.621223
3520.662133	536770.953445	40.626228
3520.531528	536641.667249	40.631232
3521.155547	536477.104895	40.636237
3521.466186	536289.758959	40.641242
3522.089610	536104.028223	40.646247
3522.123645	535905.659097	40.651252
3521.933464	535734.196172	40.656256
3522.305200	535531.222626	40.661261
3522.010446	535322.694070	40.666266
3522.326398	535063.600883	40.671271
3521.921195	534821.237338	40.676276
3522.469786	534567.251780	40.681280
3522.576732	534313.281350	40.686285
3522.169797	534060.297329	40.691290
3522.246813	533840.323253	40.696295
3522.082888	533559.708801	40.701300
3521.700444	533324.492246	40.706304
3521.981179	533068.301594	40.711309
3521.815310	532795.049947	40.716314
3521.792172	532513.030279	40.721319
3521.557139	532294.751020	40.726324
3521.280780	532041.966234	40.731328
3520.531760	531761.159309	40.736333
3520.959535	531493.450085	40.741338
3520.452901	531225.681871	40.746343
3520.428252	530994.517061	40.751348
3520.016324	530773.718143	40.756352
3519.893634	530498.752170	40.761357
3519.743428	530235.205874	40.766362
3519.360778	530020.506085	40.771367
3519.782556	529785.210406	40.776372
3519.185356	529516.568406	40.781376
3518.939121	529285.009303	40.786381
3518.323644	529067.402370	40.791386
3518.796972	528793.727525	40.796391
3518.488798	528583.494188	40.801396
3518.124237	528383.020705	40.806400
3517.897580	528123.696498	40.811405
3517.563906	527914.266954	40.816410
3517.205588	527694.882253	40.821415
3517.538474	527441.017851	40.826420
3517.474622	527266.106742	40.831424
3516.952392	527071.201176	40.836429
3516.316796	526833.653488	40.841434
3516.338933	526617.378019	40.846439
3516.059050	526456.998041	40.851444
3515.211733	526240.703276	40.856448
3515.822235	526031.605271	40.861453
3515.421666	525881.297033	40.866458
3515.636617	525654.767952	40.871463
3515.315835	525493.929900	40.876468
3515.161532	525287.066049	40.881472
3515.319264	525098.044148	40.886477
3514.910647	524934.080424	40.891482
3514.578228	524765.654692	40.896487
3514.455509	524565.802879	40.901492
3513.756181	524422.959015	40.906496
3513.690903	524214.904697	40.911501
3513.736555	524063.902371	40.916506
3513.050840	523894.765136	40.921511
3512.838172	523770.037131	40.926516
3512.806283	523611.662260	40.931520
3512.721271	523473.869267	40.936525
3512.429496	523305.674675	40.941530
3512.244726	523189.127438	40.946535
3512.427446	523049.266374	40.951540
3511.958809	522927.706711	40.956544
3512.300468	522739.993183	40.961549
3511.949632	522651.829753	40.966554
3511.835112	522487.491446	40.971559
3511.676390	522345.352729	40.976564
3511.331522	522266.438082	40.981568
3511.291435	522109.768805	40.986573
3511.034876	521973.355260	40.991578
3510.878869	521903.408241	40.996583
3510.684575	521760.309452	41.001588
3510.430256	521632.487595	41.006592
3510.742142	521554.830783	41.011597
3510.501561	521448.442238	41.016602
3510.477645	521303.846310	41.021607
3510.307325	521232.887494	41.026612
3510.278247	521089.807286	41.031616
3510.107020	521024.004852	41.036621
3509.787602	520912.215315	41.041626
3509.658894	520793.973606	41.046631
3509.812075	520719.674959	41.051636
3509.694540	520612.250309	41.056640
3509.723281	520518.403022	41.061645
3509.416295	520423.091396	41.066650
3509.485429	520328.579331	41.071655
3509.215249	520260.109657	41.076660
3509.088915	520159.711668	41.081664
3509.195489	520068.377666	41.086669
3508.658170	519993.527554	41.091674
3508.964472	519909.189442	41.096679
3508.906791	519826.475919	41.101684
3508.330254	519747.990270	41.106688
3508.801829	519664.838331	41.111693
3508.415204	519589.305222	41.116698
3508.115875	519500.054822	41.121703
3507.951137	519464.786437	41.126708
3508.329868	519355.201968	41.131712
3508.345691	519327.590717	41.136717
3507.765946	519249.558293	41.141722
3507.999849	519150.057967	41.146727
3507.999601	519125.988553	41.151732
3507.679209	519050.998740	41.156736
3507.900451	518988.969190	41.161741
3507.805229	518928.455868	41.166746
3507.526188	518857.655692	41.171751
3507.393461	518804.783476	41.176756
3507.203131	518772.349424	41.181760
3507.576361	518667.312329	41.186765
3507.046602	518652.276399	41.191770
3507.503397	518565.025280	41.196775
3507.364289	518547.045131	41.201780
3506.807154	518473.860002	41.206784
3507.718390	518378.445146	41.211789
3507.272606	518354.091052	41.216794
3506.935345	518316.015641	41.221799
3507.214151	518237.387618	41.226804
3506.860621	518232.791230	41.231808
3506.853216	518166.597513	41.236813
3506.667836	518101.443051	41.241818
3506.672011	518071.303076	41.246823
3506.802430	518032.748536	41.251828
3506.352503	517978.103313	41.256832
3506.519327	517963.209501	41.261837
3506.355604	517890.465312	41.266842
3506.574951	517826.257199	41.271847
3506.666537	517833.929481	41.276852
3506.576738	517799.252544	41.281856
3506.171740	517728.872018	41.286861
3506.405181	517700.060536	41.291866
3506.264766	517658.210273	41.296871
3507.029844	517591.285317	41.301876
3506.585665	517595.401281	41.306880
3506.151499	517555.974027	41.311885
3506.415600	517490.796696	41.316890
3506.388096	517479.018014	41.321895
3506.186110	517430.198069	41.326900
3506.285257	517385.426682	41.331904
3506.519065	517376.236347	41.336909
3505.917305	517323.382975	41.341914
3506.374788	517262.826789	41.346919
3506.456542	517255.127008	41.351924
3505.830262	517210.419240	41.356928
3506.485781	517158.782638	41.361933
3506.140412	517163.894536	41.366938
3505.824785	517105.027716	41.371943
3505.818954	517066.087893	41.376948
3506.054549	517013.202328	41.381952
3506.234289	517009.633909	41.386957
3505.894960	516997.398446	41.391962
3505.724923	516949.988081	41.396967
3505.922160	516906.666518	41.401972
3506.075059	516856.119886	41.406976
3505.921270	516878.042454	41.411981
3505.818673	516862.128209	41.416986
3505.610482	516811.992529	41.421991
3506.069430	516761.194942	41.426996
3505.895607	516717.628099	41.432000
3506.030988	516688.577501	41.437005
3506.181958	516705.900491	41.442010
3505.680576	516652.927977	41.447015
3506.217649	516595.998108	41.452020
3506.328927	516614.187224	41.457024
3505.790700	516552.723794	41.462029
3505.087359	516518.849207	41.467034
3505.931295	516481.240358	41.472039
3506.129693	516450.662156	41.477044
3505.380879	516469.290824	41.482048
3506.035914	516436.668020	41.487053
3505.363093	516390.599898	41.492058
3505.561738	516352.081262	41.497063
3505.920066	516328.254570	41.502068
3505.357774	516331.630889	41.507072
3505.051203	516295.619567	41.512077
3506.018953	516248.229669	41.517082
3505.588121	516219.520628	41.522087
3505.700549	516236.597321	41.527092
3505.263417	516212.390444	41.532096
3505.682162	516149.358166	41.537101
3505.444502	516121.174752	41.542106
3505.261037	516109.874934	41.547111
3505.433499	516136.248121	41.552116
3505.430158	516111.820807	41.557120
3505.133100	516072.115493	41.562125
3504.951124	516037.752916	41.567130
3505.736139	516009.964002	41.572135
3505.450222	516025.890055	41.577140
3505.094415	516003.945928	41.582144
3505.631342	515944.080471	41.587149
3505.338630	515952.016666	41.592154
3505.328148	515937.149074	41.597159
3505.470228	515894.794553	41.602164
3504.805776	515874.517476	41.607168
3505.374025	515857.990478	41.612173
3505.401494	515808.320302	41.617178
3505.525808	515796.668166	41.622183
3505.338606	515761.395473	41.627188
3505.192344	515744.172076	41.632192
3505.411101	515714.904304	41.637197
3505.249354	515746.995514	41.642202
3505.149836	515732.091236	41.647207
3504.827759	515701.290475	41.652212
3504.607815	515682.207322	41.657216
3505.313975	515657.869509	41.662221
3505.481871	515638.826158	41.667226
3505.118316	515668.976916	41.672231
3504.980108	515615.589674	41.677236
3505.169797	515576.767211	41.682240
3505.163438	515613.032011	41.687245
3505.120560	515577.887851	41.692250
3504.969983	515553.331264	41.697255
3505.257608	515546.457969	41.702260
3504.975013	515548.525803	41.707264
3504.980707	515508.518413	41.712269
3504.775977	515501.065417	41.717274
3504.805288	515493.373115	41.722279
3504.874674	515494.323198	41.727284
3504.799259	515453.620415	41.732288
3504.893675	515459.523132	41.737293
3505.178066	515455.027448	41.742298
3504.266167	515419.362808	41.747303
3505.025951	515384.394838	41.752308
3504.455018	515419.788318	41.757312
3504.877430	515401.007933	41.762317
3504.487803	515385.542272	41.767322
3504.840864	515363.384105	41.772327
3504.837847	515354.230096	41.777332
3504.686486	515378.784284	41.782336
3505.115729	515338.304921	41.787341
3505.137380	515322.673038	41.792346
3504.529956	515318.773481	41.797351
3505.072794	515275.797698	41.802356
3504.703752	515302.915302	41.807360
3504.792296	515258.443366	41.812365
3504.825271	515288.076929	41.817370
3504.174563	515255.809955	41.822375
3505.137063	515225.816838	41.827380
3504.530318	515261.873826	41.832384
3504.467849	515244.434359	41.837389
3504.901621	515222.313827	41.842394
3504.831192	515224.499900	41.847399
3504.803697	515218.384373	41.852404
3504.401012	515196.851223	41.857408
3504.340803	515171.571698	41.862413
3504.334704	515163.935421	41.867418
3505.149013	515146.610159	41.872423
3505.075484	515160.429748	41.877428
3504.963288	515170.411488	41.882432
3504.820991	515171.142157	41.887437
3505.006505	515139.906086	41.892442
3504.501497	515100.635966	41.897447
3505.062908	515070.503656	41.902452
3505.076237	515063.066576	41.907456
3505.041622	515034.950399	41.912461
3504.956219	515088.830201	41.917466
3504.806951	515067.964929	41.922471
3504.847757	515028.355475	41.927476
3504.969257	515016.551508	41.932480
3505.235917	514973.972659	41.937485
3504.988705	515011.338984	41.942490
3504.806727	515007.877894	41.947495
3505.055512	514981.031880	41.952500
3504.859176	514972.211692	41.957504
3504.847370	514924.669424	41.962509
3504.851449	514894.675472	41.967514
3504.517148	514952.388485	41.972519
3504.638690	514926.017706	41.977524
3504.715470	514897.479059	41.982528
3505.214153	514857.088722	41.987533
3504.956226	514862.136914	41.992538
3504.692854	514877.959331	41.997543
3505.023176	514864.402558	42.002548
3504.722145	514833.242822	42.007552
3505.295977	514784.292529	42.012557
3505.206146	514808.938981	42.017562
3504.993141	514802.043354	42.022567
3505.156360	514762.970300	42.027572
3505.304338	514719.246239	42.032576
3505.380053	514737.088956	42.037581
3505.224812	514705.096665	42.042586
3505.134989	514678.657749	42.047591
3505.273035	514677.725574	42.052596
3505.054437	514651.559868	42.057600
3504.988856	514623.700798	42.062605
3504.892133	514648.702633	42.067610
3504.544960	514642.688006	42.072615
3504.737854	514589.548649	42.077620
3504.819781	514596.718143	42.082624
3504.535245	514586.596614	42.087629
3504.979941	514553.598767	42.092634
3505.080346	514552.318475	42.097639
3505.080576	514561.574683	42.102644
3504.771390	514557.273744	42.107648
3504.854691	514531.464774	42.112653
3504.815872	514527.373993	42.117658
3504.468851	514501.582414	42.122663
3505.082915	514455.356143	42.127668
3505.201691	514449.571280	42.132672
3504.717216	514473.774796	42.137677
3504.468503	514447.208889	42.142682
3504.792673	514419.641940	42.147687
3505.129079	514410.737251	42.152692
3504.643371	514445.006533	42.157696
3504.549181	514440.317518	42.162701
3504.714161	514413.079203	42.167706
3504.450465	514386.515568	42.172711
3505.255801	514349.363287	42.177716
3504.963976	514337.674756	42.182720
3504.776220	514363.146631	42.187725
3504.836215	514336.076528	42.192730
3504.281582	514325.339982	42.197735
3504.591606	514322.357372	42.202740
3504.625695	514296.707564	42.207744
3505.236636	514265.301467	42.212749
3505.432382	514257.025902	42.217754
3504.927452	514258.623224	42.222759
3504.777910	514252.678381	42.227764
3504.916773	514213.304417	42.232768
3504.746485	514208.526203	42.237773
3504.642554	514241.926253	42.242778
3504.315281	514215.220655	42.247783
3504.684228	514209.345586	42.252788
3504.378364	514210.102149	42.257792
3504.420215	514190.975922	42.262797
3504.202467	514184.333698	42.267802
3504.328694	514182.391740	42.272807
3505.109526	514143.270211	42.277812
3504.713385	514168.572991	42.282816
3504.794570	514171.190467	42.287821
3504.828881	514151.508993	42.292826
3504.839691	514091.770693	42.297831
3504.936686	514079.261802	42.302836
3504.966708	514074.907123	42.307840
3504.594667	514066.215395	42.312845
3504.172323	514073.211911	42.317850
3504.368652	514072.877470	42.322855
3504.398502	514071.304804	42.327860
3505.049743	514042.522166	42.332864
3505.058931	514014.245617	42.337869
3504.897343	514013.310186	42.342874
3504.612986	514006.071438	42.347879
3505.000725	514002.621253	42.352884
3504.783325	514005.538859	42.357888
3504.894919	513984.782758	42.362893
3504.608583	513995.045627	42.367898
3504.881090	514006.029467	42.372903
3504.858322	513973.205540	42.377908
3504.487902	513924.857244	42.382912
3504.929393	513933.285320	42.387917
3504.905843	513945.782872	42.392922
3504.933297	513888.570320	42.397927
3504.897357	513903.447222	42.402932
3504.630229	513916.135043	42.407936
3504.820977	513890.206945	42.412941
3504.644579	513858.115227	42.417946
3504.900620	513832.884872	42.422951
3505.181613	513809.572666	42.427956
3505.018960	513790.073651	42.432960
3505.204164	513773.807492	42.437965
3505.256245	513769.449248	42.442970
3504.820258	513761.172130	42.447975
3504.656110	513740.155818	42.452980
3504.058455	513759.926976	42.457984
3504.401754	513749.402210	42.462989
3504.782310	513740.439609	42.467994
3504.721220	513725.325150	42.472999
3505.093889	513695.523720	42.478004
3505.012044	513686.634179	42.483008
3504.900471	513655.948147	42.488013
3504.423236	513663.509918	42.493018
3504.166129	513704.522660	42.498023
3504.733640	513651.270556	42.503028
3504.731421	513643.430646	42.508032
3504.860588	513672.343685	42.513037
3504.685543	513647.029443	42.518042
3504.608009	513638.543858	42.523047
3504.764326	513614.340598	42.528052
3504.656199	513611.221626	42.533056
3504.255966	513598.588641	42.538061
3504.754673	513571.397387	42.543066
3504.601816	513548.406312	42.548071
3504.472805	513558.644578	42.553076
3504.107410	513595.375135	42.558080
3504.227954	513596.367822	42.563085
3504.649172	513564.889249	42.568090
3504.761109	513529.109349	42.573095
3504.554141	513545.227595	42.578100
3504.116061	513563.456264	42.583104
3504.419342	513559.968757	42.588109
3504.868855	513541.738439	42.593114
3504.192316	513509.522780	42.598119
3505.277856	513470.907954	42.603124
3504.834899	513478.869055	42.608128
3504.590872	513513.304355	42.613133
3504.572742	513493.630405	42.618138
3504.522051	513490.502332	42.623143
3504.330600	513488.155258	42.628148
3504.204682	513482.358159	42.633152
3504.533072	513431.368828	42.638157
3504.269822	513435.659532	42.643162
3503.671595	513432.972079	42.648167
3504.211372	513431.824588	42.653172
3504.613345	513454.726024	42.658176
3504.400407	513448.993251	42.663181
3504.616630	513430.496188	42.668186
3504.568271	513418.161534	42.673191
3504.579459	513379.918649	42.678196
3504.469563	513406.593664	42.683200
3504.378399	513432.001089	42.688205
3504.369421	513405.395649	42.693210
3504.528248	513392.522393	42.698215
3504.512617	513353.929603	42.703220
3504.513579	513336.225218	42.708224
3504.651293	513342.728838	42.713229
3504.771549	513337.853869	42.718234
3504.416626	513328.450881	42.723239
3504.892163	513344.562608	42.728244
3504.286760	513367.876309	42.733248
3504.394036	513323.396314	42.738253
3504.538509	513312.093364	42.743258
3504.240964	513343.755355	42.748263
3504.413188	513314.996614	42.753268
3504.434520	513309.934938	42.758272
3503.920207	513302.428732	42.763277
3504.531724	513290.950778	42.768282
3504.731014	513273.518482	42.773287
3504.797264	513295.613272	42.778292
3504.329738	513284.052949	42.783296
3504.468801	513263.291623	42.788301
3504.706267	513290.164836	42.793306
3503.998206	513281.121143	42.798311
3504.609378	513239.899822	42.803316
3504.536472	513259.082778	42.808321
3504.392182	513240.136651	42.813325
3504.451093	513223.535838	42.818330
3504.028296	513260.225609	42.823335
3504.104949	513237.551923	42.828340
3503.802409	513233.907187	42.833345
3503.961651	513230.492963	42.838349
3503.864519	513232.784682	42.843354
3504.047900	513238.825867	42.848359
3504.445519	513220.401071	42.853364
3504.373941	513268.467319	42.858369
3504.246643	513234.495050	42.863373
3504.810047	513187.463981	42.868378
3504.349404	513217.179203	42.873383
3504.304127	513239.898704	42.878388
3504.454519	513251.155257	42.883393
3504.484338	513248.368503	42.888397
3504.689731	513216.012884	42.893402
3504.368396	513193.553798	42.898407
3504.023195	513176.359219	42.903412
3504.087567	513177.967822	42.908417
3504.742065	513160.008200	42.913421
3505.114416	513158.431897	42.918426
3504.299621	513159.774790	42.923431
3504.372439	513140.389560	42.928436
3504.472986	513133.848364	42.933441
3504.744628	513116.505640	42.938445
3505.325592	513099.619851	42.943450
3504.027347	513113.381773	42.948455
3503.805775	513104.969272	42.953460
3503.609119	513109.249532	42.958465
3504.337088	513097.247196	42.963469
3504.690459	513077.766965	42.968474
3504.187551	513087.659938	42.973479
3504.619826	513081.673302	42.978484
3504.518762	513076.681488	42.983489
3504.242453	513066.709498	42.988493
3504.467129	513095.304917	42.993498
3504.474991	513110.023839	42.998503
3504.492733	513111.032805	43.003508
3504.492259	513095.503527	43.008513
3504.340778	513031.335699	43.013517
3504.833541	513013.148564	43.018522
3504.537289	513038.437240	43.023527
3504.100093	513038.304087	43.028532
3504.060565	513048.528516	43.033537
3504.171045	513035.763801	43.038541
3505.130992	513014.670081	43.043546
3504.544884	513001.813105	43.048551
3504.218430	513028.725282	43.053556
3504.519051	513050.075161	43.058561
3504.343796	513031.386618	43.063565
3504.535799	512984.009013	43.068570
3504.208990	512950.927653	43.073575
3504.354358	512959.706533	43.078580
3504.129214	513001.474696	43.083585
3504.148954	513011.436856	43.088589
3504.514323	513012.239127	43.093594
3504.363403	513005.231781	43.098599
3504.599129	512964.119720	43.103604
3504.856636	512937.926690	43.108609
3504.633940	512979.138087	43.113613
3504.520918	512967.673268	43.118618
3504.209917	512947.842637	43.123623
3504.806795	512921.343014	43.128628
3504.840823	512910.917200	43.133633
3504.759605	512887.205713	43.138637
3505.056070	512878.913558	43.143642
3504.355770	512912.966928	43.148647
3504.236689	512892.397706	43.153652
3504.163057	512889.981341	43.158657
3505.091930	512863.631493	43.163661
3505.004927	512861.925430	43.168666
3504.691228	512869.512287	43.173671
3504.445614	512835.102652	43.178676
3505.376534	512810.067616	43.183681
3504.701799	512802.232445	43.188685
3504.557520	512786.422102	43.193690
3504.431048	512810.470232	43.198695
3504.543486	512801.043663	43.203700
3504.637582	512763.292137	43.208705
3504.273379	512803.261690	43.213709
3504.636187	512785.246609	43.218714
3504.644201	512735.418707	43.223719
3504.569880	512718.282017	43.228724
3504.639047	512710.733906	43.233729
3504.776167	512714.354480	43.238733
3504.711432	512699.087924	43.243738
3504.532502	512704.883054	43.248743
3504.675184	512689.988391	43.253748
3505.050990	512674.348666	43.258753
3504.883318	512695.874182	43.263757
3504.818236	512696.896264	43.268762
3504.454500	512673.734991	43.273767
3503.799464	512630.385388	43.278772
3503.721783	512629.689545	43.283777
3503.816087	512640.803612	43.288781
3504.221447	512648.479255	43.293786
3504.787507	512632.101218	43.298791
3505.055276	512602.972069	43.303796
3504.791649	512612.878080	43.308801
3504.439407	512613.287939	43.313805
3504.825428	512618.740871	43.318810
3504.608160	512614.526076	43.323815
3505.237915	512563.435920	43.328820
3504.856605	512571.944146	43.333825
3504.378624	512570.552782	43.338829
3505.098432	512534.978221	43.343834
3504.786672	512556.020827	43.348839
3504.566928	512513.310327	43.353844
3504.704931	512525.682218	43.358849
3504.589346	512531.973256	43.363853
3504.613907	512491.753395	43.368858
3504.429484	512479.388979	43.373863
3504.628870	512454.873741	43.378868
3504.985609	512477.581303	43.383873
3504.351669	512467.210211	43.388877
3504.105793	512440.134839	43.393882
3504.950385	512417.895128	43.398887
3504.736935	512419.244197	43.403892
3505.220149	512433.180359	43.408897
3504.792756	512433.956205	43.413901
3504.699823	512407.817751	43.418906
3504.118817	512384.083386	43.423911
3504.813899	512340.570227	43.428916
3505.037390	512352.675798	43.433921
3504.555493	512370.457388	43.438925
3504.866184	512357.002891	43.443930
3504.597821	512353.909015	43.448935
3504.554961	512347.744291	43.453940
3504.869479	512344.254761	43.458945
3504.368896	512313.425441	43.463949
3504.412702	512282.510018	43.468954
3504.318620	512265.679517	43.473959
3504.092769	512311.041162	43.478964
3504.176248	512288.112196	43.483969
3504.612240	512270.186177	43.488973
3504.295490	512280.505473	43.493978
3503.607789	512265.842865	43.498983
3504.620005	512226.073309	43.503988
3504.668358	512221.057625	43.508993
3504.538601	512274.042830	43.513997
3504.708990	512238.605081	43.519002
3504.285024	512241.757985	43.524007
3504.023895	512225.813828	43.529012
3504.815831	512202.013960	43.534017
3504.632604	512199.817167	43.539021
3504.256917	512247.732022	43.544026
3504.083975	512247.607677	43.549031
3504.193512	512231.857873	43.554036
3504.343791	512222.475590	43.559041
3503.959110	512202.048688	43.564045
3504.649286	512190.557563	43.569050
3504.138498	512186.540817	43.574055
3503.975721	512190.563016	43.579060
3504.391741	512186.500951	43.584065
3504.618551	512186.009897	43.589069
3504.877873	512160.220082	43.594074
3504.569047	512196.995305	43.599079
3504.520687	512158.809670	43.604084
3504.696435	512168.848840	43.609089
3504.180630	512168.019880	43.614093
3504.752602	512114.306973	43.619098
3504.443489	512153.409356	43.624103
3504.554330	512126.226514	43.629108
3504.491906	512121.329485	43.634113
3504.033202	512130.457212	43.639117
3504.504153	512094.870481	43.644122
3504.276133	512116.406268	43.649127
3504.620369	512076.084309	43.654132
3504.641955	512113.515712	43.659137
3504.684587	512078.704873	43.664141
3504.757831	512071.914647	43.669146
3504.648453	512061.865092	43.674151
3504.812911	512029.108986	43.679156
3504.532297	512060.973038	43.684161
3504.574582	512015.336379	43.689165
3504.469745	512025.521158	43.694170
3504.111204	512003.319316	43.699175
3504.262102	512010.023715	43.704180
3504.435797	512022.542094	43.709185
3503.990810	512014.670241	43.714189
3504.272514	512001.624747	43.719194
3504.157496	512016.515802	43.724199
3504.318297	511980.471978	43.729204
3504.647641	511962.714257	43.734209
3504.333881	511985.528458	43.739213
3504.460422	511975.542738	43.744218
3504.335051	511997.922443	43.749223
3504.728164	511949.751355	43.754228
3504.349263	511971.007646	43.759233
3504.245450	511958.832461	43.764237
3504.450602	511922.427390	43.769242
3504.518871	511940.830698	43.774247
3504.430428	511970.944554	43.779252
3503.971604	511929.180958	43.784257
3504.087647	511906.094567	43.789261
3504.376471	511931.444173	43.794266
3504.005731	511916.377046	43.799271
3504.411191	511888.590789	43.804276
3504.407853	511926.583010	43.809281
3504.080516	511893.044381	43.814285
3504.067764	511926.383988	43.819290
3503.922015	511923.523592	43.824295
3504.622420	511890.227214	43.829300
3504.685517	511888.092622	43.834305
3504.556168	511866.056726	43.839309
3504.264513	511873.033483	43.844314
3504.147133	511904.113205	43.849319
3504.068754	511903.215090	43.854324
3504.161923	511888.934609	43.859329
3504.260346	511887.502667	43.864333
3504.629577	511861.644440	43.869338
3504.201553	511889.232117	43.874343
3504.222770	511866.059485	43.879348
3504.232473	511866.007444	43.884353
3504.226661	511847.847286	43.889357
3504.199307	511864.849321	43.894362
3504.497396	511841.481127	43.899367
3504.131915	511880.238929	43.904372
3504.773422	511837.188249	43.909377
3504.318400	511853.347305	43.914381
3504.197416	511827.465334	43.919386
3504.063602	511842.460688	43.924391
3504.251510	511822.094589	43.929396
3504.087451	511843.822963	43.934401
3503.879063	511819.219500	43.939405
3504.406236	511843.469207	43.944410
3504.290824	511829.322822	43.949415
3504.070749	511840.082398	43.954420
3504.324608	511840.851765	43.959425
3503.938278	511838.687029	43.964429
3504.275052	511826.695050	43.969434
3504.348920	511851.117574	43.974439
3503.911388	511836.364463	43.979444
3503.825755	511806.733342	43.984449
3504.512449	511786.642479	43.989453
3504.723235	511799.711632	43.994458
3504.005979	511822.893358	43.999463
3504.005400	511837.159421	44.004468
3504.324543	511834.225527	44.009473
3503.754537	511840.487471	44.014477
3504.286538	511829.678753	44.019482
3503.786723	511826.064893	44.024487
3504.251832	511815.722035	44.029492
3504.088955	511819.896101	44.034497
3504.311783	511793.909147	44.039501
3504.453620	511785.337372	44.044506
3504.126895	511771.679636	44.049511
3504.355779	511800.833042	44.054516
3504.511829	511759.376548	44.059521
3504.047792	511806.851310	44.064525
3504.122449	511775.221853	44.069530
3504.158863	511779.465606	44.074535
3504.178700	511808.196746	44.079540
3504.100689	511771.431404	44.084545
3504.134846	511763.331934	44.089549
3504.453005	511796.568901	44.094554
3504.041922	511758.136172	44.099559
3503.967674	511738.367883	44.104564
3504.702114	511719.078810	44.109569
3504.181136	511742.482564	44.114573
3504.676769	511728.138334	44.119578
3504.645506	511734.669281	44.124583
3504.087406	511730.457550	44.129588
3504.165054	511763.024358	44.134593
3503.917255	511750.214133	44.139597
3503.993727	511735.379690	44.144602
3504.234440	511715.713357	44.149607
3503.988232	511759.764382	44.154612
3504.182395	511741.268970	44.159617
3503.693414	511739.525154	44.164621
3504.265174	511744.139594	44.169626
3503.854714	511754.575197	44.174631
3504.282516	511717.527434	44.179636
3504.297611	511735.787603	44.184641
3503.578979	511766.102607	44.189645
3504.207954	511719.967715	44.194650
3503.898909	511758.969815	44.199655
3503.738567	511760.563483	44.204660
3504.466516	511722.102399	44.209665
3504.185773	511769.295350	44.214669
3504.483080	511754.678960	44.219674
3504.188024	511738.436178	44.224679
3503.979177	511780.103583	44.229684
3504.297323	511750.307366	44.234689
3504.004989	511782.274967	44.239693
3504.594428	511752.537049	44.244698
3504.004531	511748.583291	44.249703
3504.359589	511716.454108	44.254708
3504.310910	511750.002092	44.259713
3504.225562	511754.619217	44.264717
3504.112350	511730.202936	44.269722
3504.461425	511719.119532	44.274727
3504.606200	511759.061671	44.279732
3504.477543	511723.366587	44.284737
3503.891161	511700.846244	44.289741
3504.268219	511716.722142	44.294746
3504.800394	511728.981720	44.299751
3504.476445	511734.445981	44.304756
3504.307905	511713.781974	44.309761
3504.461808	511698.277607	44.314765
3504.103843	511671.421084	44.319770
3504.862386	511645.248050	44.324775
3504.539531	511644.641508	44.329780
3504.468294	511625.985567	44.334785
3504.088387	511686.600465	44.339789
3504.069804	511687.159959	44.344794
3504.082445	511656.804803	44.349799
3503.805057	511638.383815	44.354804
3504.070777	511635.053621	44.359809
3504.287745	511626.773424	44.364813
3504.313211	511654.542745	44.369818
3504.211932	511649.247012	44.374823
3504.063793	511624.785512	44.379828
3504.419698	511602.723164	44.384833
3504.268665	511655.157176	44.389837
3503.911114	511647.220743	44.394842
3503.854786	511624.262395	44.399847
3504.047960	511644.467480	44.404852
3504.201345	511638.575013	44.409857
3504.172376	511629.018381	44.414861
3504.144064	511668.279847	44.419866
3504.325292	511667.492452	44.424871
3504.201410	511642.217723	44.429876
3504.159377	511612.731140	44.434881
3504.204522	511596.181504	44.439885
3504.389584	511583.909802	44.444890
3504.199140	511630.481796	44.449895
3503.901138	511614.289950	44.454900
3504.383940	511597.317016	44.459905
3504.086229	511637.430558	44.464909
3504.126254	511625.485343	44.469914
3503.990291	511588.880534	44.474919
3504.181075	511640.451139	44.479924
3504.526044	511626.130639	44.484929
3503.968517	511618.529335	44.489933
3504.277628	511577.199972	44.494938
3504.297185	511569.153307	44.499943
3504.076131	511621.750257	44.504948
3504.096106	511604.243419	44.509953
3503.714412	511598.840226	44.514957
3504.264999	511583.829533	44.519962
3503.892297	511611.459504	44.524967
3503.988238	511592.979458	44.529972
3504.469595	511591.436374	44.534977
3503.936963	511616.106867	44.539981
3504.080480	511590.486261	44.544986
3504.331572	511567.074532	44.549991
3504.232518	511617.679238	44.554996
3504.352405	511595.704776	44.560001
3504.124060	511604.492838	44.565005
3504.079700	511599.339859	44.570010
3504.344360	511558.523366	44.575015
3503.846880	511596.139128	44.580020
3504.377170	511583.509324	44.585025
3504.196740	511564.465863	44.590029
3504.252936	511540.629602	44.595034
3504.412830	511561.447115	44.600039
3504.211518	511598.004278	44.605044
3504.006972	511583.972956	44.610049
3504.119480	511555.524216	44.615053
3505.235627	511561.317386	44.620058
3504.880010	511524.595391	44.625063
3504.829022	511520.657576	44.630068
3505.212269	511496.263667	44.635073
3504.838935	511496.474526	44.640077
3504.765259	511490.972023	44.645082
3505.496754	511445.882564	44.650087
3504.812336	511463.444160	44.655092
3505.148500	511413.914651	44.660097
3504.929115	511376.968447	44.665101
3504.795699	511392.621797	44.670106
3504.721909	511403.054988	44.675111
3504.497059	511385.738392	44.680116
3504.490436	511347.999652	44.685121
3504.688882	511327.428939	44.690125
3504.344578	511365.628072	44.695130
3504.258967	511350.464787	44.700135
3504.352964	511312.861834	44.705140
3504.824668	511301.354058	44.710145
3504.515143	511347.389157	44.715149
3504.344124	511308.411572	44.720154
3504.658219	511307.451389	44.725159
3504.279725	511307.916015	44.730164
3504.559414	511278.378003	44.735169
3504.700566	511279.671110	44.740173
3504.336023	511280.437071	44.745178
3504.325676	511231.315932	44.750183
3504.074578	511255.031823	44.755188
3504.083770	511234.946223	44.760193
3504.063580	511266.315283	44.765197
3504.369827	511233.737599	44.770202
3504.414617	511263.123383	44.775207
3504.305717	511239.110437	44.780212
3504.601794	511257.883194	44.785217
3504.560896	511244.331626	44.790221
3504.393744	511220.934942	44.795226
3504.451395	511228.312059	44.800231
3504.394513	511216.280696	44.805236
3504.515303	511244.642697	44.810241
3504.300928	511208.302416	44.815245
3504.291665	511219.332601	44.820250
3504.371503	511185.525860	44.825255
3504.026846	511182.646189	44.830260
3503.913966	511202.495452	44.835265
3503.904447	511181.755075	44.840269
3504.080042	511157.342915	44.845274
3504.179223	511211.509397	44.850279
3503.884430	511215.046790	44.855284
3504.021347	511202.580065	44.860289
3503.998877	511181.285243	44.865293
3504.243409	511175.378210	44.870298
3504.170631	511222.742159	44.875303
3503.984975	511212.248849	44.880308
3504.193073	511193.447102	44.885313
3504.409493	511184.104385	44.890317
3504.173013	511224.765709	44.895322
3503.621338	511205.780528	44.900327
3504.194750	511189.602310	44.905332
3504.021643	511215.582485	44.910337
3503.461689	511225.536138	44.915341
3504.204635	511195.874170	44.920346
3503.989301	511234.761472	44.925351
3503.574976	511213.225087	44.930356
3504.275252	511184.531056	44.935361
3503.877327	511204.981862	44.940365
3504.059553	511203.941338	44.945370
3503.836758	511192.340904	44.950375
3504.040074	511192.764159	44.955380
3504.123882	511207.169181	44.960385
3503.984489	511249.535163	44.965389
3503.976488	511252.976627	44.970394
3504.410720	511257.258810	44.975399
3504.240673	511267.251988	44.980404
3504.139094	511210.708489	44.985409
3504.363335	511203.388150	44.990413
3504.139004	511194.115105	44.995418
3504.352628	511193.423749	45.000423
3504.019087	511218.468065	45.005428
3504.252960	511188.987731	45.010433
3504.179423	511180.753237	45.015437
3504.129689	511225.988746	45.020442
3504.487119	511172.610332	45.025447
3504.229215	511220.509451	45.030452
3504.081347	511202.573420	45.035457
3504.070975	511175.559994	45.040461
3504.475721	511137.502816	45.045466
3504.428468	511122.232085	45.050471
3504.031336	511145.262945	45.055476
3504.146081	511182.782845	45.060481
3504.177030	511198.460983	45.065485
3503.983053	511194.899824	45.070490
3504.175759	511198.157805	45.075495
3504.070860	511205.914756	45.080500
3504.008179	511205.823564	45.085505
3503.894087	511189.045753	45.090509
3503.619032	511179.072456	45.095514
3503.434272	511179.202921	45.100519
3503.841401	511191.128521	45.105524
3504.240203	511187.928976	45.110529
3503.875246	511196.890610	45.115533
3503.893271	511206.297606	45.120538
3504.243946	511202.245639	45.125543
3503.711910	511186.292739	45.130548
3503.711601	511189.429459	45.135553
3503.437041	511190.687102	45.140557
3503.782692	511184.157007	45.145562
3504.591809	511174.670011	45.150567
3504.471501	511161.636831	45.155572
3504.238207	511164.051529	45.160577
3504.217659	511173.262278	45.165581
3504.027859	511179.767905	45.170586
3503.821220	511207.372279	45.175591
3503.892407	511205.590454	45.180596
3504.086094	511183.401437	45.185601
3504.390383	511173.336563	45.190605
3504.310053	511165.305496	45.195610
3504.231302	511167.493405	45.200615
3503.736379	511174.755525	45.205620
3503.947721	511182.563681	45.210625
3504.030015	511231.420800	45.215629
3504.056177	511243.001860	45.220634
3504.293781	511203.453547	45.225639
3504.241233	511206.294981	45.230644
3503.849718	511191.179906	45.235649
3504.051112	511178.753562	45.240653
3504.116288	511168.422938	45.245658
3503.926748	511178.318069	45.250663
3503.999725	511154.276257	45.255668
3504.073333	511165.849870	45.260673
3504.311048	511146.942210	45.265677
3504.029471	511151.894056	45.270682
3504.598208	511152.259553	45.275687
3504.164350	511167.252334	45.280692
3504.341456	511162.620710	45.285697
3503.472991	511186.029558	45.290701
3503.743099	511194.334321	45.295706
3504.077819	511210.672695	45.300711
3503.722839	511200.104962	45.305716
3504.206278	511153.789188	45.310721
3504.349572	511175.166289	45.315725
3504.057945	511211.738553	45.320730
3504.219222	511171.190428	45.325735
3504.335080	511166.669667	45.330740
3504.510395	511158.446418	45.335745
3504.492729	511132.395292	45.340749
3504.767374	511128.152964	45.345754
3504.553813	511127.782079	45.350759
3504.151013	511163.815524	45.355764
3504.555544	511177.158071	45.360769
3504.508602	511146.912607	45.365773
3503.995154	511125.492960	45.370778
3504.310990	511127.567914	45.375783
3504.271644	511129.951960	45.380788
3504.199807	511112.206179	45.385793
3504.310171	511098.984718	45.390797
3504.698117	511088.906572	45.395802
3504.886747	511073.750284	45.400807
3504.260097	511067.475011	45.405812
3504.393997	511099.933011	45.410817
3504.283346	511111.991099	45.415821
3504.201140	511101.127237	45.420826
3504.328617	511080.263902	45.425831
3504.329383	511043.939856	45.430836
3504.630591	511017.736972	45.435841
3504.298477	511028.008860	45.440845
3504.370475	511019.953648	45.445850
3504.837860	511011.835935	45.450855
3504.517515	511004.905135	45.455860
3504.381214	510988.990681	45.460865
3504.485549	511003.190266	45.465869
3504.580946	511008.234339	45.470874
3504.526552	511035.309019	45.475879
3503.958843	510991.435532	45.480884
3504.653246	510952.725070	45.485889
3504.235106	510948.946338	45.490893
3504.409217	511003.708725	45.495898
3504.127136	510976.636751	45.500903
3504.566929	510954.206173	45.505908
3504.376544	510970.425413	45.510913
3504.072458	510975.431458	45.515917
3504.043198	510919.027336	45.520922
3503.950022	510951.268556	45.525927
3503.969736	510948.027706	45.530932
3504.445077	510922.808970	45.535937
3504.026720	510971.695374	45.540941
3504.352732	510945.741413	45.545946
3504.560070	510906.652517	45.550951
3504.442758	510928.172301	45.555956
3504.110121	510968.242341	45.560961
3504.102287	510963.235169	45.565965
3503.608057	510956.837742	45.570970
3504.401139	510930.658159	45.575975
3504.048121	510938.555631	45.580980
3503.924142	510981.526931	45.585985
3503.663630	510966.542722	45.590989
3503.932776	510956.129140	45.595994
3504.275894	510942.718997	45.600999
3504.078269	510966.123291	45.606004
3504.210554	510937.973943	45.611009
3504.109859	510924.229209	45.616013
3504.173296	510909.598474	45.621018
3504.144938	510911.727859	45.626023
3504.121486	510907.684368	45.631028
3504.020718	510940.078582	45.636033
3503.833306	510908.286581	45.641037
3504.115501	510933.588126	45.646042
3504.538829	510919.709969	45.651047
3503.932189	510932.301899	45.656052
3504.405298	510916.139279	45.661057
3504.466810	510967.479394	45.666061
3503.968315	510944.842976	45.671066
3504.399025	510910.322552	45.676071
3504.231879	510952.491292	45.681076
3504.007172	510897.129808	45.686081
3504.499190	510882.583080	45.691085
3504.244664	510922.843244	45.696090
3504.429284	510889.171129	45.701095
3504.209425	510900.234807	45.706100
3504.489938	510926.194312	45.711105
3504.245689	510894.765407	45.716109
3504.678465	510859.637461	45.721114
3504.520778	510891.888990	45.726119
3504.404055	510867.117893	45.731124
3505.013626	510835.250375	45.736129
3504.481426	510876.920499	45.741133
3504.159965	510862.856472	45.746138
3504.321199	510835.613021	45.751143
3504.156726	510830.225839	45.756148
3504.026893	510827.210969	45.761153
3504.232098	510814.682576	45.766157
3504.691359	510798.066712	45.771162
3504.277633	510827.323353	45.776167
3504.375883	510854.525965	45.781172
3504.600674	510812.955130	45.786177
3504.706289	510776.664536	45.791181
3504.524786	510779.425240	45.796186
3504.735237	510809.392715	45.801191
3504.395483	510775.752670	45.806196
3504.402201	510744.283820	45.811201
3504.539374	510754.127554	45.816205
3504.590903	510767.627402	45.821210
3504.929126	510729.478650	45.826215
3504.189156	510756.813909	45.831220
3504.741803	510709.676534	45.836225
3504.293034	510722.041298	45.841229
3504.136337	510707.394594	45.846234
3504.326822	510731.041412	45.851239
3504.306874	510714.754170	45.856244
3504.746922	510664.194242	45.861249
3504.278331	510699.024861	45.866253
3504.032047	510687.073655	45.871258
3504.563583	510658.051274	45.876263
3504.063827	510701.639181	45.881268
3504.293450	510691.838786	45.886273
3504.289089	510681.569452	45.891277
3504.350152	510637.747447	45.896282
3504.522709	510669.643643	45.901287
3504.139247	510657.461140	45.906292
3504.753945	510633.585930	45.911297
3504.272102	510626.073400	45.916301
3504.426360	510668.040262	45.921306
3504.400667	510660.455648	45.926311
3503.859783	510657.910453	45.931316
3503.961563	510633.104480	45.936321
3504.170352	510618.298746	45.941325
3504.110805	510598.324448	45.946330
3504.606977	510571.179411	45.951335
3504.172349	510614.453693	45.956340
3504.274210	510633.662569	45.961345
3504.201441	510598.411630	45.966349
3504.284879	510614.638517	45.971354
3504.488869	510619.716132	45.976359
3503.694866	510593.989264	45.981364
3504.437086	510578.036749	45.986369
3504.630462	510544.969679	45.991373
3504.340667	510589.485932	45.996378
3504.258898	510594.355763	46.001383
3504.054799	510590.998446	46.006388
3503.755972	510572.276145	46.011393
3504.269208	510553.324282	46.016397
3504.191846	510585.563690	46.021402
3504.558964	510558.489624	46.026407
3504.309733	510572.441900	46.031412
3503.958181	510537.133716	46.036417
3504.604555	510506.878718	46.041421
3504.274458	510550.035456	46.046426
3504.458111	510526.025860	46.051431
3504.843444	510506.031727	46.056436
3504.582139	510538.907404	46.061441
3504.356283	510501.049673	46.066445
3504.646085	510466.904775	46.071450
3504.739327	510518.089443	46.076455
3504.465362	510520.965988	46.081460
3504.376810	510469.274826	46.086465
3504.460343	510445.635089	46.091469
3504.661146	510445.451654	46.096474
3504.490256	510469.965430	46.101479
3504.264522	510454.621130	46.106484
3504.782495	510396.965169	46.111489
3504.552918	510422.753102	46.116493
3504.359269	510396.627488	46.121498
3504.606765	510415.864181	46.126503
3503.774853	510409.115183	46.131508
3504.634799	510388.185823	46.136513
3504.284204	510408.174764	46.141517
3504.209497	510377.122851	46.146522
3504.514478	510353.397391	46.151527
3504.289311	510388.898459	46.156532
3504.279977	510359.050400	46.161537
3504.267165	510371.042952	46.166541
3504.134330	510413.561741	46.171546
3504.572555	510384.047723	46.176551
3504.506824	510359.571388	46.181556
3503.799307	510342.785361	46.186561
3503.685770	510332.735446	46.191565
3504.307382	510313.513225	46.196570
3504.490178	510344.396553	46.201575
3504.052605	510344.212835	46.206580
3503.653429	510341.341637	46.211585
3504.283730	510322.826351	46.216589
3504.242410	510355.313458	46.221594
3504.041081	510349.021283	46.226599
3503.733894	510349.272290	46.231604
3504.332720	510327.372276	46.236609
3504.424043	510320.932648	46.241613
3504.691190	510362.730635	46.246618
3504.631815	510305.924516	46.251623
3504.190768	510336.855871	46.256628
3504.423285	510303.124444	46.261633
3504.629690	510281.842920	46.266637
3504.352170	510331.720742	46.271642
3504.486037	510278.476068	46.276647
3504.534498	510251.856630	46.281652
3504.556139	510284.789255	46.286657
3504.382643	510262.808864	46.291661
3504.475756	510243.568916	46.296666
3504.373162	510272.423172	46.301671
3504.054025	510228.356660	46.306676
3504.431269	510198.548405	46.311681
3504.175006	510233.245220	46.316685
3503.899044	510253.020172	46.321690
3504.093268	510228.755526	46.326695
3504.466576	510220.045196	46.331700
3504.047075	510224.007247	46.336705
3504.214339	510237.438625	46.341709
3504.407626	510249.904614	46.346714
3504.810887	510197.072444	46.351719
3504.401236	510220.157116	46.356724
3504.436188	510180.587884	46.361729
3504.559679	510214.314035	46.366733
3504.057138	510201.593506	46.371738
3504.566382	510163.467059	46.376743
3503.971654	510180.712227	46.381748
3504.109741	510165.208975	46.386753
3504.471630	510130.293116	46.391757
3504.272688	510171.456935	46.396762
3504.384279	510135.568786	46.401767
3504.227496	510165.190686	46.406772
3504.361035	510134.510163	46.411777
3504.521886	510167.117451	46.416781
3504.230716	510157.601442	46.421786
3504.536417	510114.498331	46.426791
3504.762168	510092.909956	46.431796
3504.154842	510133.025362	46.436801
3504.231077	510103.416300	46.441805
3504.353287	510119.536341	46.446810
3504.330474	510095.609372	46.451815
3503.983855	510075.528060	46.456820
3504.047217	510098.841690	46.461825
3504.118333	510073.837383	46.466829
3504.251833	510071.590250	46.471834
3504.098396	510084.161757	46.476839
3504.087383	510053.706312	46.481844
3504.163664	510094.017318	46.486849
3504.166164	510073.982008	46.491853
3503.879674	510088.901841	46.496858
3503.664277	510066.725448	46.501863
3503.858710	510088.804130	46.506868
3504.243827	510084.898239	46.511873
3504.057786	510067.422394	46.516877
3503.854534	510108.182298	46.521882
3504.297580	510065.057354	46.526887
3504.491548	510086.579584	46.531892
3504.479847	510083.647097	46.536897
3504.182643	510086.426200	46.541901
3503.949014	510082.415735	46.546906
3504.460744	510032.955675	46.551911
3503.543463	510069.173924	46.556916
3504.013730	510040.919089	46.561921
3504.008217	510057.615905	46.566925
3504.222831	510044.073593	46.571930
3504.221870	510057.025768	46.576935
3504.507462	510038.716443	46.581940
3503.978972	510074.772040	46.586945
3504.540161	510034.866327	46.591949
3504.449488	510071.510443	46.596954
3504.780506	510022.837819	46.601959
3504.466556	510058.555977	46.606964
3504.285609	510032.731363	46.611969
3504.703954	510004.332895	46.616973
3504.341368	510043.752107	46.621978
3504.370838	509998.618032	46.626983
3504.531259	509978.911807	46.631988
3504.205315	510001.275229	46.636993
3504.013148	509984.255610	46.641997
3504.256896	509953.051407	46.647002
3504.619828	509929.164422	46.652007
3504.680939	509963.457458	46.657012
3504.313488	509987.547647	46.662017
3504.421668	509951.153716	46.667021
3504.595849	509926.992999	46.672026
3504.699781	509925.408242	46.677031
3504.657647	509957.238510	46.682036
3504.668489	509894.298081	46.687041
3504.852245	509868.870920	46.692045
3504.468206	509888.460998	46.697050
3504.487229	509881.223129	46.702055
3504.222689	509891.889765	46.707060
3503.946236	509856.922468	46.712065
3504.900862	509816.751686	46.717069
3504.247112	509861.630916	46.722074
3504.055285	509857.967950	46.727079
3504.404657	509830.035444	46.732084
3504.277380	509856.566967	46.737089
3504.322101	509877.860079	46.742093
3504.114739	509858.009472	46.747098
3504.339994	509800.600158	46.752103
3504.288964	509801.771973	46.757108
3504.314903	509833.237550	46.762113
3504.313771	509814.922714	46.767117
3504.012289	509817.247188	46.772122
3504.841515	509781.700218	46.777127
3504.492479	509779.782290	46.782132
3504.315196	509753.450734	46.787137
3504.406864	509749.641746	46.792141
3504.260984	509745.718521	46.797146
3504.409530	509770.486369	46.802151
3504.293910	509769.897593	46.807156
3504.278648	509741.466041	46.812161
3504.585103	509755.229957	46.817165
3503.874977	509778.969846	46.822170
3503.777411	509749.134674	46.827175
3504.181029	509725.392759	46.832180
3504.016675	509761.442049	46.837185
3503.736992	509735.784378	46.842189
3503.755565	509762.647153	46.847194
3504.424108	509734.107504	46.852199
3504.623639	509737.111714	46.857204
3504.090907	509763.201524	46.862209
3504.153763	509731.165406	46.867213
3503.928970	509754.120294	46.872218
3503.980317	509725.020459	46.877223
3503.985191	509758.766253	46.882228
3504.110557	509744.883653	46.887233
3504.659117	509726.633621	46.892237
3504.126062	509780.955148	46.897242
3504.070280	509752.125264	46.902247
3504.483106	509735.869877	46.907252
3504.246390	509760.496257	46.912257
3504.375976	509725.717486	46.917261
3504.050803	509729.259983	46.922266
3504.371055	509735.989101	46.927271
3504.021837	509709.128115	46.932276
3503.564957	509699.739233	46.937281
3503.914021	509700.645437	46.942285
3504.061348	509710.235192	46.947290
3504.039789	509691.974049	46.952295
3504.059469	509714.637375	46.957300
3503.757353	509701.530632	46.962305
3504.314552	509691.627295	46.967309
3504.072257	509734.165066	46.972314
3503.827817	509716.900473	46.977319
3504.272890	509692.140070	46.982324
3504.265637	509688.144325	46.987329
3504.267938	509743.443837	46.992333
3504.112301	509724.040249	46.997338
3504.712375	509685.746605	47.002343
3504.691687	509715.347767	47.007348
3504.279026	509686.877750	47.012353
3504.771986	509650.725932	47.017357
3504.294580	509707.113278	47.022362
3504.584444	509675.395337	47.027367
3504.873583	509631.534716	47.032372
3504.608161	509625.252405	47.037377
3504.194426	509634.981481	47.042381
3504.101705	509663.379845	47.047386
3504.630551	509605.011189	47.052391
3505.024393	509584.103936	47.057396
3504.361173	509627.568615	47.062401
3504.540318	509634.977809	47.067405
3504.195955	509610.848017	47.072410
3504.025008	509571.765283	47.077415
3504.552609	509544.917232	47.082420
3504.083593	509584.809672	47.087425
3504.493399	509580.697386	47.092429
3503.796606	509564.060684	47.097434
3504.519606	509534.348413	47.102439
3504.219023	509570.622015	47.107444
3504.292512	509583.006234	47.112449
3504.224664	509593.894938	47.117453
3504.391799	509596.803103	47.122458
3504.560014	509567.178580	47.127463
3504.301266	509553.305945	47.132468
3503.824979	509533.598661	47.137473
3504.300142	509487.836254	47.142477
3503.797126	509531.326448	47.147482
3504.043751	509551.879719	47.152487
3504.539717	509552.155571	47.157492
3504.041525	509554.915932	47.162497
3503.924353	509531.458448	47.167501
3504.483920	509502.834452	47.172506
3504.608650	509532.159969	47.177511
3504.193730	509518.463776	47.182516
3504.099280	509478.862789	47.187521
3504.335113	509493.700577	47.192525
3504.207940	509492.961832	47.197530
3504.523323	509470.498392	47.202535
3504.598766	509471.093691	47.207540
3504.225097	509508.390880	47.212545
3504.223395	509484.004368	47.217549
3504.375715	509452.611329	47.222554
3504.387270	509442.186953	47.227559
3504.039259	509477.810507	47.232564
3503.758467	509449.420443	47.237569
3504.925591	509421.459209	47.242573
3504.389372	509434.547052	47.247578
3504.380427	509469.054528	47.252583
3504.201470	509439.585852	47.257588
3503.755115	509419.924300	47.262593
3504.361396	509391.140950	47.267597
3504.293584	509384.321361	47.272602
3504.130288	509423.811681	47.277607
3504.154774	509448.650197	47.282612
3504.048998	509412.339542	47.287617
3504.390982	509407.580195	47.292621
3504.025642	509442.346439	47.297626
3504.230519	509385.546107	47.302631
3504.020821	509427.877099	47.307636
3503.864727	509412.318478	47.312641
3504.239289	509408.009341	47.317645
3504.044885	509444.822974	47.322650
3504.394978	509413.904556	47.327655
3504.107680	509383.390405	47.332660
3504.365431	509359.974617	47.337665
3504.613859	509369.599178	47.342669
3504.393069	509389.012232	47.347674
3504.115789	509385.565053	47.352679
3504.600128	509347.339548	47.357684
3504.453723	509381.413567	47.362689
3504.378041	509331.032432	47.367693
3504.279845	509350.071982	47.372698
3504.253470	509351.088144	47.377703
3504.316771	509329.726873	47.382708
3504.064507	509353.951526	47.387713
3504.209688	509321.395679	47.392717
3504.557080	509326.096842	47.397722
3504.504151	509344.016139	47.402727
3504.121201	509302.689503	47.407732
3504.499193	509281.834985	47.412737
3504.347039	509327.142279	47.417741
3504.148743	509311.843216	47.422746
3504.182816	509304.501534	47.427751
3504.133710	509300.866486	47.432756
3503.701592	509296.836615	47.437761
3504.765840	509264.590751	47.442765
3504.331384	509313.282027	47.447770
3504.302191	509300.283626	47.452775
3504.467758	509287.912176	47.457780
3504.288499	509284.753058	47.462785
3504.566158	509279.093120	47.467789
3504.163596	509295.853433	47.472794
3504.233683	509278.083323	47.477799
3503.766828	509262.371303	47.482804
3503.942455	509263.760307	47.487809
3504.193020	509286.539489	47.492813
3504.355186	509293.192577	47.497818
3504.344571	509255.196889	47.502823
3504.188136	509227.545741	47.507828
3504.510162	509204.473754	47.512833
3504.777486	509181.056210	47.517837
3504.585939	509187.056904	47.522842
3504.738347	509161.836040	47.527847
3504.588111	509163.883713	47.532852
3504.157663	509214.699671	47.537857
3504.525178	509212.870802	47.542861
3504.214790	509190.860082	47.547866
3504.259026	509187.665620	47.552871
3503.873198	509187.271322	47.557876
3504.304803	509162.107520	47.562881
3504.511432	509145.529998	47.567885
3504.468391	509130.813388	47.572890
3504.287268	509160.744439	47.577895
3504.519790	509157.267229	47.582900
3504.310945	509139.035103	47.587905
3504.172635	509129.949728	47.592909
3503.992110	509135.645120	47.597914
3504.454141	509088.973000	47.602919
3504.767318	509079.310272	47.607924
3503.555914	509112.237654	47.612929
3503.687761	509111.862721	47.617933
3504.307821	509084.898148	47.622938
3504.326413	509093.446073	47.627943
3504.383869	509131.384279	47.632948
3503.887693	509126.048991	47.637953
3504.276865	509116.627252	47.642957
3504.374932	509125.820350	47.647962
3504.049720	509107.353603	47.652967
3504.249964	509094.774148	47.657972
3504.748023	509064.135295	47.662977
3504.785214	509029.369724	47.667981
3504.878351	509031.530734	47.672986
3504.644366	509064.000134	47.677991
3504.639625	509044.217754	47.682996
3504.397937	509032.871826	47.688001
3503.787951	509030.995060	47.693005
3503.973433	509024.388275	47.698010
3504.343499	509028.782356	47.703015
3504.571803	509020.347326	47.708020
3504.711845	508993.053712	47.713025
3504.679693	509002.824022	47.718029
3504.321074	509031.822017	47.723034
3504.522502	509026.275238	47.728039
3504.866539	509002.642942	47.733044
3504.608113	508978.195100	47.738049
3504.356775	508955.618182	47.743053
3504.536898	508940.107185	47.748058
3504.794051	508916.336713	47.753063
3504.201508	508948.559423	47.758068
3504.153090	508917.399528	47.763073
3504.386296	508905.320694	47.768077
3504.319388	508895.869731	47.773082
3504.581384	508913.942085	47.778087
3504.502794	508902.013725	47.783092
3504.499518	508882.534510	47.788097
3504.189347	508885.417047	47.793101
3504.379699	508857.558700	47.798106
3504.067679	508877.745703	47.803111
3504.306479	508848.361775	47.808116
3503.995859	508859.491704	47.813121
3504.498883	508867.356005	47.818125
3504.359424	508841.725435	47.823130
3504.614722	508862.379352	47.828135
3504.004337	508835.254700	47.833140
3504.687063	508798.463940	47.838145
3504.382263	508820.319576	47.843149
3504.355945	508842.687735	47.848154
3504.028204	508816.074945	47.853159
3504.409054	508797.192680	47.858164
3503.960574	508824.889698	47.863169
3504.258122	508821.250352	47.868173
3504.339721	508782.884869	47.873178
3504.089358	508789.097386	47.878183
3504.369670	508796.440353	47.883188
3504.459942	508782.764916	47.888193
3504.510200	508781.795705	47.893197
3504.615705	508768.370835	47.898202
3504.391657	508785.154023	47.903207
3504.266945	508744.746579	47.908212
3504.460491	508718.354826	47.913217
3504.562301	508753.402798	47.918221
3504.553560	508727.700800	47.923226
3504.336799	508755.513094	47.928231
3504.470850	508702.617705	47.933236
3504.324807	508722.272680	47.938241
3504.035184	508698.436542	47.943245
3503.859685	508705.345620	47.948250
3503.789499	508703.383494	47.953255
3504.508998	508691.581828	47.958260
3503.699532	508702.537720	47.963265
3504.119835	508708.998439	47.968269
3504.481484	508693.357333	47.973274
3504.200947	508695.476254	47.978279
3504.733511	508708.395708	47.983284
3504.663890	508682.247888	47.988289
3504.771987	508671.200617	47.993293
3504.544642	508687.933822	47.998298
3504.377764	508646.470265	48.003303
3504.576102	508662.630234	48.008308
3504.109466	508645.956261	48.013313
3504.714991	508612.010776	48.018317
3504.217384	508639.108683	48.023322
3504.288141	508602.667225	48.028327
3504.413702	508640.190963	48.033332
3504.358574	508609.739940	48.038337
3504.365390	508621.629411	48.043341
3504.528459	508584.667347	48.048346
3504.474857	508606.129363	48.053351
3504.518505	508572.930384	48.058356
3504.411718	508608.770589	48.063361
3504.356870	508579.786804	48.068365
3504.467518	508533.978294	48.073370
3504.314099	508554.090007	48.078375
3503.962345	508547.466762	48.083380
3504.229498	508517.369420	48.088385
3504.022792	508545.079267	48.093389
3503.470880	508549.163822	48.098394
3503.660053	508511.742095	48.103399
3504.130152	508541.115902	48.108404
3503.729361	508564.656765	48.113409
3503.965895	508527.986555	48.118413
3504.158521	508560.996643	48.123418
3504.198734	508538.676684	48.128423
3504.179180	508566.559307	48.133428
3504.136572	508527.858706	48.138433
3504.284188	508558.447210	48.143437
3504.285423	508530.871219	48.148442
3504.454604	508542.026709	48.153447
3504.579777	508557.439371	48.158452
3504.197705	508511.000311	48.163457
3504.252657	508526.879482	48.168461
3504.249959	508501.479780	48.173466
3504.265790	508525.562021	48.178471
3504.375090	508536.018607	48.183476
3503.917149	508525.718486	48.188481
3504.055627	508490.075655	48.193485
3503.885764	508533.212111	48.198490
3504.115714	508500.843711	48.203495
3504.555949	508480.889156	48.208500
3504.203542	508525.066448	48.213505
3504.365664	508463.058248	48.218509
3504.485097	508492.841752	48.223514
3504.443125	508476.505276	48.228519
3504.403415	508453.590663	48.233524
3504.654121	508472.373638	48.238529
3504.625655	508437.465461	48.243533
3504.493233	508447.201334	48.248538
3503.978253	508430.635992	48.253543
3504.735921	508420.902639	48.258548
3504.284224	508433.927277	48.263553
3504.413209	508432.844407	48.268557
3504.675559	508407.503869	48.273562
3504.278360	508382.722930	48.278567
3504.542641	508397.961952	48.283572
3504.346799	508395.969054	48.288577
3504.834498	508391.742980	48.293581
3504.516969	508386.227428	48.298586
3504.782083	508335.890721	48.303591
3505.051958	508318.695228	48.308596
3504.584879	508355.655476	48.313601
3504.643520	508350.181650	48.318605
3504.664185	508337.933622	48.323610
3504.208047	508316.703803	48.328615
3504.716646	508284.594547	48.333620
3503.974962	508282.384321	48.338625
3504.302056	508288.202149	48.343629
3504.498994	508256.040906	48.348634
3504.426625	508271.889837	48.353639
3504.278663	508277.428567	48.358644
3504.557832	508241.105202	48.363649
3504.383162	508265.673305	48.368653
3504.536839	508263.119157	48.373658
3504.539318	508254.466456	48.378663
3504.589597	508243.377453	48.383668
3504.427832	508242.087534	48.388673
3504.266290	508204.518183	48.393677
3504.572375	508186.051862	48.398682
3503.912818	508223.346410	48.403687
3504.004187	508202.333502	48.408692
3504.087137	508178.943747	48.413697
3504.069723	508202.323306	48.418701
3504.522993	508165.769868	48.423706
3504.501730	508206.960884	48.428711
3504.213523	508182.870816	48.433716
3504.244431	508192.935209	48.438721
3504.412926	508164.775609	48.443725
3504.118453	508152.071271	48.448730
3503.931555	508164.902458	48.453735
3504.703090	508122.176137	48.458740
3504.180618	508162.991088	48.463745
3504.454777	508126.061085	48.468749
3504.376483	508157.191998	48.473754
3504.300937	508131.196079	48.478759
3504.559005	508131.256567	48.483764
3504.180113	508102.070206	48.488769
3504.262785	508116.933387	48.493773
3504.127156	508083.610010	48.498778
3504.101453	508113.872500	48.503783
3504.206862	508089.871884	48.508788
3504.287461	508100.940461	48.513793
3504.208181	508109.605540	48.518797
3504.227667	508104.188425	48.523802
3504.229638	508100.089657	48.528807
3504.584307	508054.038911	48.533812
3503.941261	508084.601429	48.538817
3504.415982	508051.485111	48.543821
3504.319187	508053.271470	48.548826
3504.240330	508074.535739	48.553831
3504.177131	508059.467209	48.558836
3504.485653	508053.700796	48.563841
3504.281131	508079.994258	48.568845
3504.018782	508045.729451	48.573850
3504.277852	508052.468900	48.578855
3504.095980	508025.528241	48.583860
3504.427297	508017.380038	48.588865
3504.208113	508049.494804	48.593869
3504.150039	508043.685134	48.598874
3504.036108	508015.316936	48.603879
3503.969660	508049.937533	48.608884
3504.120138	508032.052237	48.613889
3504.614300	508017.401566	48.618893
3504.135718	508046.571969	48.623898
3504.348769	508007.020204	48.628903
3504.383223	508009.190618	48.633908
3504.631617	507977.880916	48.638913
3504.824521	507956.244467	48.643917
3504.497147	508002.847915	48.648922
3504.338651	507958.143015	48.653927
3504.351901	507973.523289	48.658932
3504.570625	507944.292800	48.663937
3504.410298	507955.956148	48.668941
3504.444760	507929.740140	48.673946
3504.306524	507974.137981	48.678951
3504.047290	507947.766024	48.683956
3504.134232	507925.893287	48.688961
3504.129900	507934.496007	48.693965
3504.342419	507886.291497	48.698970
3504.135014	507913.800063	48.703975
3504.518232	507908.983192	48.708980
3504.266280	507903.102920	48.713985
3504.754173	507884.708742	48.718989
3504.461791	507899.732592	48.723994
3503.979281	507888.828776	48.728999
3504.336009	507852.897138	48.734004
3504.148132	507864.058903	48.739009
3504.121307	507881.520189	48.744013
3503.609328	507872.392016	48.749018
3503.697644	507895.097479	48.754023
3504.049752	507871.209366	48.759028
3503.506458	507895.026661	48.764033
3503.915698	507856.455539	48.769037
3503.628901	507916.613585	48.774042
3503.182814	507915.469782	48.779047
3503.776223	507893.567550	48.784052
3503.620372	507939.435659	48.789057
3503.463674	507919.119415	48.794061
3504.356017	507885.025974	48.799066
3504.105682	507926.506862	48.804071
3503.905495	507917.228231	48.809076
3503.903629	507924.616172	48.814081
3504.041819	507907.694086	48.819085
3504.036924	507922.824274	48.824090
3504.148152	507910.814628	48.829095
3504.041915	507921.862252	48.834100
3504.015153	507908.963620	48.839105
3503.992367	507905.172318	48.844109
3503.863283	507935.704458	48.849114
3503.752056	507912.699234	48.854119
3503.706587	507929.404423	48.859124
3503.817540	507897.003106	48.864129
3503.897711	507945.920481	48.869133
3503.757142	507927.018488	48.874138
3504.279675	507901.534886	48.879143
3504.277376	507893.186359	48.884148
3504.372356	507929.755073	48.889153
3504.282293	507944.038509	48.894157
3504.244078	507914.443786	48.899162
3504.347598	507926.723246	48.904167
3504.125134	507934.803847	48.909172
3504.217002	507897.902173	48.914177
3504.435487	507927.670992	48.919181
3503.823240	507893.916589	48.924186
3503.836457	507901.150356	48.929191
3504.105101	507898.426184	48.934196
3504.050246	507897.827737	48.939201
3504.055510	507895.043996	48.944205
3504.181545	507895.277155	48.949210
3503.840488	507885.059375	48.954215
3504.697384	507861.799859	48.959220
3504.095769	507910.926298	48.964225
3503.915790	507902.555260	48.969229
3504.644087	507869.853914	48.974234
3504.338768	507917.719102	48.979239
3504.579137	507870.825741	48.984244
3504.450482	507886.835720	48.989249
3504.457956	507845.393286	48.994253
3504.184449	507862.083984	48.999258
3504.442607	507834.263875	49.004263
3504.561145	507869.816992	49.009268
3503.960630	507854.226014	49.014273
3504.348059	507825.373459	49.019277
3504.323459	507837.572033	49.024282
3504.192894	507802.881116	49.029287
3504.348181	507818.694477	49.034292
3504.041986	507823.752362	49.039297
3504.224942	507798.271684	49.044301
3504.431776	507778.859217	49.049306
3504.438682	507827.181304	49.054311
3504.221258	507812.491136	49.059316
3504.165566	507806.225610	49.064321
3504.524906	507755.619326	49.069325
3504.449552	507749.508687	49.074330
3504.361557	507786.511427	49.079335
3504.294400	507793.201342	49.084340
3504.349453	507784.337696	49.089345
3504.104245	507777.697313	49.094349
3504.059122	507772.442108	49.099354
3504.396759	507750.934326	49.104359
3504.618304	507718.059792	49.109364
3504.120576	507732.104237	49.114369
3504.108083	507766.312069	49.119373
3503.977167	507740.982119	49.124378
3504.144128	507722.081894	49.129383
3504.309855	507728.380821	49.134388
3504.088582	507756.094230	49.139393
3504.159410	507718.284696	49.144397
3504.232252	507728.494531	49.149402
3503.871058	507763.921291	49.154407
3504.136615	507732.456634	49.159412
3504.361768	507725.640684	49.164417
3504.685948	507747.853655	49.169421
3504.334150	507698.422214	49.174426
3504.419683	507666.075085	49.179431
3504.109425	507695.573674	49.184436
3504.204189	507715.444728	49.189441
3504.141486	507685.752285	49.194445
3504.133351	507713.988677	49.199450
3504.327694	507688.910842	49.204455
3504.369204	507691.737986	49.209460
3504.293639	507643.072332	49.214465
3504.490341	507676.842469	49.219469
3504.498588	507639.902864	49.224474
3504.334544	507662.243715	49.229479
3504.157391	507664.093416	49.234484
3504.552786	507647.130422	49.239489
3504.060110	507641.541114	49.244493
3504.300738	507598.037214	49.249498
3503.785240	507640.269108	49.254503
3504.034884	507607.693528	49.259508
3503.913646	507619.401524	49.264513
3504.088016	507616.388605	49.269517
3504.221739	507602.452366	49.274522
3503.742455	507633.951203	49.279527
3504.157428	507616.327277	49.284532
3504.005144	507619.589870	49.289537
3504.351063	507610.123552	49.294541
3503.751863	507635.417458	49.299546
3503.926943	507602.954856	49.304551
3504.469752	507626.196039	49.309556
3503.848695	507634.795189	49.314561
3503.539922	507622.952932	49.319565
3504.512888	507604.785390	49.324570
3503.751535	507600.857758	49.329575
3503.920970	507649.458255	49.334580
3503.575614	507625.578848	49.339585
3504.323710	507596.921908	49.344589
3504.366423	507597.927252	49.349594
3504.258518	507618.437661	49.354599
3504.069765	507634.710375	49.359604
3504.270042	507613.881943	49.364609
3504.328873	507621.361621	49.369613
3504.186050	507629.834580	49.374618
3504.124000	507606.719976	49.379623
3504.236492	507587.119804	49.384628
3504.447512	507587.845542	49.389633
3504.418065	507577.122919	49.394637
3504.329403	507590.546211	49.399642
3504.158942	507592.344261	49.404647
3504.151248	507584.603647	49.409652
3504.394594	507586.791697	49.414657
3504.047842	507577.637251	49.419661
3504.278863	507558.777323	49.424666
3503.732522	507566.403281	49.429671
3504.115513	507549.948160	49.434676
3504.084141	507568.624900	49.439681
3504.018756	507556.238120	49.444685
3503.951339	507528.013575	49.449690
3503.745213	507564.934257	49.454695
3503.843866	507539.820732	49.459700
3504.379897	507555.675352	49.464705
3503.986817	507561.860264	49.469709
3504.154397	507549.588457	49.474714
3503.908085	507537.685669	49.479719
3503.845807	507560.314171	49.484724
3504.298908	507540.407104	49.489729
3504.011842	507569.446833	49.494733
3503.852290	507544.627131	49.499738
3503.915532	507552.359145	49.504743
3504.037885	507578.348696	49.509748
3503.998622	507556.647244	49.514753
3503.959318	507546.988779	49.519757
3504.697884	507530.882244	49.524762
3504.290473	507519.055507	49.529767
3504.429923	507553.189141	49.534772
3503.891946	507573.362774	49.539777
3503.984073	507556.245224	49.544781
3504.484666	507529.954934	49.549786
3504.209783	507536.121172	49.554791
3504.320442	507549.563591	49.559796
3504.070450	507506.035808	49.564801
3503.871575	507530.709978	49.569805
3503.977715	507531.452296	49.574810
3503.747509	507515.954283	49.579815
3504.182159	507498.782536	49.584820
3504.503793	507495.847521	49.589825
3503.951908	507495.479427	49.594829
3504.159434	507486.996336	49.599834
3504.129264	507512.048675	49.604839
3503.950799	507552.456476	49.609844
3503.898468	507522.812716	49.614849
3504.132421	507495.097093	49.619853
3504.083019	507497.584431	49.624858
3504.051867	507546.824132	49.629863
3503.894052	507527.570224	49.634868
3504.061126	507510.390181	49.639873
3503.914294	507549.527966	49.644877
3504.037302	507508.319470	49.649882
3503.896033	507530.201482	49.654887
3503.777048	507547.323466	49.659892
3504.114228	507513.266448	49.664897
3504.222966	507513.856553	49.669901
3504.058653	507521.472746	49.674906
3503.903019	507518.461372	49.679911
3504.077484	507509.629312	49.684916
3504.365150	507549.963440	49.689921
3504.415094	507507.855677	49.694925
3504.462253	507532.389754	49.699930
3504.177827	507491.852830	49.704935
3504.424629	507497.633016	49.709940
3504.043675	507500.577569	49.714945
3503.985653	507477.664560	49.719949
3504.434099	507462.919447	49.724954
3504.459998	507503.902272	49.729959
3504.310083	507480.244777	49.734964
3504.260736	507464.363924	49.739969
3504.239108	507488.453525	49.744973
3504.488459	507493.524895	49.749978
3504.133219	507475.162352	49.754983
3504.475271	507428.049319	49.759988
3504.498411	507466.907417	49.764993
3503.925610	507454.094757	49.769997
3504.258342	507445.693058	49.775002
3503.984509	507467.292496	49.780007
3504.256635	507430.917950	49.785012
3504.296801	507447.761869	49.790017
3504.133399	507433.821859	49.795021
3504.621061	507389.924183	49.800026
3504.095265	507428.211317	49.805031
3503.860236	507402.998534	49.810036
3504.271915	507384.059260	49.815041
3504.246574	507432.691150	49.820045
3504.426614	507408.475392	49.825050
3503.929659	507420.091105	49.830055
3504.136459	507392.531414	49.835060
3503.997100	507424.128704	49.840065
3504.008430	507410.262258	49.845069
3504.273280	507406.981996	49.850074
3504.078366	507415.564496	49.855079
3503.993973	507401.713174	49.860084
3504.104761	507384.693708	49.865089
3504.003321	507402.976891	49.870093
3504.435634	507364.755241	49.875098
3504.051903	507397.757442	49.880103
3504.103126	507373.258389	49.885108
3504.299719	507354.859094	49.890113
3503.942933	507383.606545	49.895117
3504.374736	507366.333915	49.900122
3503.829583	507379.728321	49.905127
3504.027600	507380.607927	49.910132
3503.976028	507386.384711	49.915137
3504.209264	507359.124397	49.920141
3504.210964	507396.417397	49.925146
3504.171764	507368.947154	49.930151
3504.140975	507387.370990	49.935156
3504.163233	507377.753300	49.940161
3504.070131	507404.839794	49.945165
3504.294979	507368.219584	49.950170
3504.016265	507351.818267	49.955175
3504.217718	507325.423147	49.960180
3504.059201	507340.021508	49.965185
3504.460841	507369.711732	49.970189
3504.329500	507356.373808	49.975194
3503.740651	507343.917813	49.980199
3504.692754	507319.529294	49.985204
3504.658277	507310.122942	49.990209
3504.198039	507317.178781	49.995213
3504.230828	507342.676825	50.000218
3503.880502	507307.412437	50.005223
3504.291022	507301.579052	50.010228
3503.935468	507314.589329	50.015233
3504.207802	507290.510623	50.020237
3504.222156	507327.548763	50.025242
3503.805095	507313.952360	50.030247
3504.469725	507283.132233	50.035252
3504.258291	507326.834874	50.040257
3503.935440	507304.165903	50.045261
3504.291652	507268.384945	50.050266
3503.958398	507316.964625	50.055271
3503.655156	507319.441511	50.060276
3504.323156	507292.972598	50.065281
3503.944859	507322.786182	50.070285
3503.920042	507311.354243	50.075290
3503.917236	507282.967284	50.080295
3503.919632	507329.925223	50.085300
3504.102184	507330.908479	50.090305
3503.946083	507312.210677	50.095309
3504.192114	507304.025021	50.100314
3503.883619	507334.637177	50.105319
3504.100855	507291.895231	50.110324
3504.093690	507325.597071	50.115329
3503.888094	507308.121524	50.120333
3504.333410	507293.073154	50.125338
3503.983925	507341.655330	50.130343
3504.148888	507306.866109	50.135348
3504.368920	507312.852994	50.140353
3503.712557	507288.566868	50.145357
3504.163260	507260.310595	50.150362
3504.021348	507247.227266	50.155367
3504.095237	507290.530687	50.160372
3503.778379	507284.002644	50.165377
3503.816365	507268.209010	50.170381
3503.908808	507299.162667	50.175386
3503.700971	507302.737709	50.180391
3504.004792	507299.046455	50.185396
3504.219443	507282.921301	50.190401
3503.952533	507321.774967	50.195405
3503.911160	507313.988955	50.200410
3503.712988	507313.008329	50.205415
3504.114572	507321.344786	50.210420
3504.088043	507332.683794	50.215425
3503.956167	507336.550432	50.220429
3503.815581	507318.305597	50.225434
3503.914178	507319.757538	50.230439
3503.849684	507358.983939	50.235444
3504.059881	507362.847102	50.240449
3504.104564	507369.064090	50.245453
3504.156475	507349.827436	50.250458
3503.897121	507341.924087	50.255463
3503.673805	507343.730516	50.260468
3503.711529	507334.009155	50.265473
3504.273924	507336.399814	50.270477
3504.111947	507373.263323	50.275482
3504.156616	507354.280825	50.280487
3503.918358	507344.046477	50.285492
3503.606601	507343.033206	50.290497
3503.673614	507346.311788	50.295501
3504.230352	507322.592983	50.300506
3503.987352	507319.544782	50.305511
3503.895365	507307.111427	50.310516
3503.990181	507333.206900	50.315521
3504.032039	507368.924966	50.320525
3504.196358	507323.762597	50.325530
3504.036504	507348.582661	50.330535
3503.862051	507365.258179	50.335540
3503.773113	507351.356933	50.340545
3503.659550	507347.023242	50.345549
3504.045590	507320.902548	50.350554
3503.847569	507335.456555	50.355559
3503.855081	507372.141472	50.360564
3504.117346	507354.490817	50.365569
3503.951017	507355.073804	50.370573
3504.038815	507330.012293	50.375578
3504.216617	507333.779381	50.380583
3503.855360	507335.253405	50.385588
3503.799212	507347.963324	50.390593
3503.725826	507348.329215	50.395597
3504.456342	507328.023847	50.400602
3504.190622	507338.591034	50.405607
3504.074967	507363.910105	50.410612
3504.420235	507371.192811	50.415617
3504.370945	507312.351202	50.420621
3504.221206	507324.367510	50.425626
3504.148036	507316.839532	50.430631
3503.944815	507317.833164	50.435636
3504.233330	507317.787641	50.440641
3504.170942	507289.511313	50.445645
3504.074393	507301.013214	50.450650
3504.015768	507319.998138	50.455655
3504.408204	507332.738367	50.460660
3504.401127	507348.021204	50.465665
3504.221448	507307.669700	50.470669
3504.350695	507300.514532	50.475674
3504.193818	507286.775779	50.480679
3504.356783	507252.492780	50.485684
3504.057198	507273.388105	50.490689
3503.732319	507281.535799	50.495693
3504.043786	507275.718063	50.500698
3504.261994	507269.965667	50.505703
3504.599197	507249.115156	50.510708
3503.837437	507281.114695	50.515713
3503.660955	507288.884718	50.520717
3504.149562	507278.231831	50.525722
3504.003586	507297.787204	50.530727
3504.234580	507291.577380	50.535732
3504.361317	507242.828028	50.540737
3504.476688	507191.752649	50.545741
3504.144829	507154.359752	50.550746
3503.227808	507111.391832	50.555751
3503.704403	507048.316833	50.560756
3503.731709	507005.199386	50.565761
3503.559896	506898.708196	50.570765
3503.630234	506785.346668	50.575770
3503.210362	506724.942352	50.580775
3502.965205	506609.149988	50.585780
3503.017226	506451.662816	50.590785
3503.106400	506335.613376	50.595789
3502.637116	506208.214771	50.600794
3502.655108	506068.238752	50.605799
3502.419649	505935.234632	50.610804
3502.001633	505735.205400	50.615809
3501.768495	505600.578976	50.620813
3502.034394	505394.567399	50.625818
3501.472761	505236.862653	50.630823
3501.157121	505004.673089	50.635828
3501.011588	504846.392983	50.640833
3500.287209	504650.296678	50.645837
3500.243997	504437.237448	50.650842
3500.072225	504185.681367	50.655847
3499.417553	503969.727115	50.660852
3499.073438	503750.431365	50.665857
3499.172249	503522.053866	50.670861
3498.834705	503285.239388	50.675866
3498.442392	503021.706285	50.680871
3498.316872	502731.605001	50.685876
3497.635345	502485.116182	50.690881
3497.170750	502215.103756	50.695885
3496.945045	501926.118721	50.700890
3495.662352	501675.056939	50.705895
3495.635073	501396.256727	50.710900
3495.209257	501131.182370	50.715905
3494.786112	500857.650117	50.720909
3494.697498	500524.884981	50.725914
3494.256390	500201.028224	50.730919
3493.058744	499935.906325	50.735924
3492.993911	499639.619912	50.740929
3492.599077	499351.581924	50.745933
3492.577740	499017.765785	50.750938
3491.969638	498668.291487	50.755943
3491.305936	498370.914512	50.760948
3491.328247	498061.121641	50.765953
3490.181487	497739.762403	50.770957
3489.807314	497378.834787	50.775962
3489.328993	497026.928755	50.780967
3489.003752	496718.585614	50.785972
3488.324753	496387.052860	50.790977
3487.829040	496011.079520	50.795981
3487.469779	495626.317100	50.800986
3486.687118	495279.134562	50.805991
3486.102861	494929.534182	50.810996
3485.850644	494553.441865	50.816001
3484.685364	494258.355930	50.821005
3484.377215	493890.107887	50.826010
3483.919306	493497.872608	50.831015
3482.913923	493131.390823	50.836020
3482.295984	492787.477736	50.841025
3481.571142	492440.384654	50.846029
3481.391257	492066.306804	50.851034
3480.779241	491684.439726	50.856039
3480.091922	491302.576749	50.861044
3480.131524	490916.184742	50.866049
3479.566814	490530.741333	50.871053
3478.677604	490142.758185	50.876058
3477.923189	489811.525004	50.881063
3477.207876	489429.881646	50.886068
3476.328742	489029.818945	50.891073
3475.374740	488631.633808	50.896077
3475.531888	488233.568587	50.901082
3474.697942	487894.918849	50.906087
3474.106468	487503.440606	50.911092
3473.709318	487081.022397	50.916097
3472.643408	486708.092914	50.921101
3472.024427	486320.495502	50.926106
3471.641239	485913.500549	50.931111
3470.733439	485534.899901	50.936116
3470.087980	485167.902784	50.941121
3469.489955	484776.319240	50.946125
3469.139878	484377.798142	50.951130
3468.033066	483968.596624	50.956135
3467.211736	483567.448064	50.961140
3466.907628	483166.108125	50.966145
3466.241799	482745.562838	50.971149
3465.487825	482384.205158	50.976154
3464.810121	482015.076076	50.981159
3464.150364	481600.484381	50.986164
3462.938583	481184.653693	50.991169
3463.094694	480781.874614	50.996173
3462.368970	480408.010231	51.001178
3461.728385	480036.253705	51.006183
3460.769808	479613.103170	51.011188
3460.169781	479186.846223	51.016193
3459.366687	478794.111272	51.021197
3458.862653	478430.411761	51.026202
3457.678662	478019.223463	51.031207
3457.192253	477611.818960	51.036212
3457.162195	477209.402358	51.041217
3456.068155	476801.874723	51.046221
3455.652296	476418.053719	51.051226
3454.939903	476044.257477	51.056231
3454.079860	475613.099685	51.061236
3453.436802	475199.183138	51.066241
3452.546041	474846.732752	51.071245
3451.716385	474430.701080	51.076250
3450.721954	474035.571763	51.081255
3450.309519	473629.596024	51.086260
3450.412160	473213.949763	51.091265
3449.112378	472852.962413	51.096269
3448.361025	472476.521393	51.101274
3447.670664	472063.765437	51.106279
3447.055184	471652.256805	51.111284
3446.853866	471241.536365	51.116289
3445.771147	470905.271949	51.121293
3444.772845	470471.999793	51.126298
3444.641615	470070.421783	51.131303
3443.796507	469708.800613	51.136308
3442.816670	469299.888737	51.141313
3442.297527	468876.698939	51.146317
3441.575409	468515.291199	51.151322
3440.838678	468096.632786	51.156327
3439.700915	467736.747835	51.161332
3438.489030	467325.349550	51.166337
3438.808192	466931.398503	51.171341
3438.140383	466539.421711	51.176346
3437.185181	466196.621495	51.181351
3436.449509	465784.610901	51.186356
3436.175959	465368.715854	51.191361
3434.962588	465025.176914	51.196365
3434.229361	464630.284682	51.201370
3434.125124	464225.041300	51.206375
3433.012174	463869.904934	51.211380
3432.483847	463456.954598	51.216385
3431.647321	463056.673812	51.221389
3430.757405	462722.176125	51.226394
3430.093070	462355.278642	51.231399
3429.170351	461964.019341	51.236404
3428.622574	461584.359603	51.241409
3428.032511	461198.207508	51.246413
3427.485888	460809.251952	51.251418
3426.478988	460422.086867	51.256423
3425.661801	460050.558911	51.261428
3425.470586	459651.128045	51.266433
3424.304840	459263.358952	51.271437
3423.957701	458903.607349	51.276442
3423.168379	458557.312054	51.281447
3422.676628	458153.944841	51.286452
3422.083389	457799.134945	51.291457
3420.956844	457408.739973	51.296461
3420.568869	457025.831148	51.301466
3419.775787	456672.049552	51.306471
3419.040562	456265.896399	51.311476
3418.504300	455928.753754	51.316481
3417.552616	455518.562581	51.321485
3416.819167	455174.641317	51.326490
3415.970377	454775.531518	51.331495
3415.553628	454439.413195	51.336500
3414.571508	454050.814375	51.341505
3414.172664	453671.199013	51.346509
3413.931446	453284.601014	51.351514
3413.244112	452959.057544	51.356519
3412.001727	452587.473097	51.361524
3411.468267	452181.265639	51.366529
3410.723639	451849.321907	51.371533
3409.875821	451451.980597	51.376538
3409.301730	451095.388121	51.381543
3408.187276	450715.887766	51.386548
3408.084093	450368.394614	51.391553
3406.986811	449988.727406	51.396557
3406.506329	449650.975927	51.401562
3406.168962	449265.848236	51.406567
3404.750361	448899.967054	51.411572
3404.138347	448535.373636	51.416577
3403.804620	448191.995334	51.421581
3403.136808	447815.574526	51.426586
3402.560909	447454.866556	51.431591
3401.882273	447081.633179	51.436596
3401.389505	446723.489344	51.441601
3400.087255	446368.513403	51.446605
3399.498431	445977.027338	51.451610
3398.644510	445648.312109	51.456615
3398.113796	445285.330745	51.461620
3397.582639	444919.247693	51.466625
3396.496075	444579.590783	51.471629
3395.928104	444211.979997	51.476634
3395.047066	443857.001702	51.481639
3394.834220	443489.272985	51.486644
3394.310484	443161.740560	51.491649
3392.596301	442789.822318	51.496653
3392.542455	442427.483963	51.501658
3392.088824	442093.276031	51.506663
3391.354684	441723.014031	51.511668
3390.634308	441369.699987	51.516673
3389.700792	441022.506517	51.521677
3389.102486	440665.660148	51.526682
3388.192439	440308.756362	51.531687
3387.745423	439970.863178	51.536692
3387.034703	439611.150903	51.541697
3385.953913	439278.044629	51.546701
3385.298820	438929.178434	51.551706
3384.656441	438579.949936	51.556711
3383.928188	438232.354832	51.561716
3383.339879	437884.986627	51.566721
3382.314419	437552.508587	51.571725
3382.063942	437219.827437	51.576730
3381.626370	436868.308614	51.581735
3380.469283	436533.121451	51.586740
3379.920395	436175.187464	51.591745
3379.230233	435834.179482	51.596749
3378.541847	435495.527793	51.601754
3378.026943	435149.735198	51.606759
3377.426932	434811.974446	51.611764
3376.768780	434457.765808	51.616769
3375.594435	434137.478993	51.621773
3374.813537	433767.106675	51.626778
3374.278199	433466.794344	51.631783
3373.571147	433102.951616	51.636788
3373.359262	432788.056474	51.641793
3372.235741	432428.612049	51.646797
3371.593593	432122.638601	51.651802
3371.142795	431748.427107	51.656807
3370.206271	431467.808820	51.661812
3369.548264	431095.829892	51.666817
3369.113493	430764.109831	51.671821
3368.097898	430417.545866	51.676826
3367.724024	430089.921445	51.681831
3367.009551	429749.370249	51.686836
3366.418273	429415.499393	51.691841
3366.062452	429079.428506	51.696845
3365.190020	428734.521260	51.701850
3364.576745	428392.438272	51.706855
3363.498552	428086.639175	51.711860
3363.156081	427721.546726	51.716865
3362.283237	427395.567904	51.721869
3361.941395	427048.421629	51.726874
3361.114880	426727.201997	51.731879
3360.102225	426391.429725	51.736884
3359.705199	426039.123439	51.741889
3358.999373	425704.462412	51.746893
3358.416335	425367.009388	51.751898
3357.786408	425022.524085	51.756903
3357.027087	424694.005606	51.761908
3356.719394	424346.793888	51.766913
3355.534982	424023.236676	51.771917
3354.851629	423677.244267	51.776922
3354.520480	423332.842836	51.781927
3353.209281	423013.154650	51.786932
3352.727215	422676.414520	51.791937
3352.148190	422349.947789	51.796941
3351.500100	422019.830293	51.801946
3350.678499	421681.861694	51.806951
3350.005353	421346.278737	51.811956
3349.209987	421011.396945	51.816961
3348.672764	420687.114143	51.821965
3347.710281	420359.897265	51.826970
3347.493905	420038.096551	51.831975
3346.277769	419690.995663	51.836980
3346.030059	419379.531739	51.841985
3345.122723	419051.909906	51.846989
3344.352283	418717.733638	51.851994
3344.043523	418389.857082	51.856999
3343.414969	418060.452202	51.862004
3342.630362	417733.913625	51.867009
3341.746267	417413.941764	51.872013
3341.172625	417070.619820	51.877018
3340.484915	416748.399158	51.882023
3339.365942	416429.241089	51.887028
3339.052825	416099.814666	51.892033
3338.335361	415778.629588	51.897037
3337.631727	415450.350062	51.902042
3337.132322	415134.357339	51.907047
3336.133446	414818.389368	51.912052
3335.616808	414486.969642	51.917057
3334.770846	414156.538371	51.922061
3333.940126	413859.056391	51.927066
3333.662398	413520.117749	51.932071
3332.574629	413206.052189	51.937076
3331.846542	412902.928842	51.942081
3331.376253	412580.018032	51.947085
3330.696696	412260.668845	51.952090
3330.178728	411938.241411	51.957095
3329.606755	411636.579704	51.962100
3329.184647	411309.937547	51.967105
3327.933416	410996.840174	51.972109
3327.293231	410673.274951	51.977114
3326.946237	410354.970981	51.982119
3326.208768	410033.396416	51.987124
3325.428063	409703.057974	51.992129
3325.068757	409397.757081	51.997133
3323.986249	409067.052856	52.002138
3323.571140	408753.774655	52.007143
3322.507716	408436.987058	52.012148
3322.325416	408114.059183	52.017153
3321.171237	407801.345586	52.022157
3320.575344	407484.397989	52.027162
3319.812794	407180.129952	52.032167
3319.199789	406869.608645	52.037172
3318.644204	406547.002990	52.042177
3317.770568	406229.781513	52.047181
3317.176466	405918.968161	52.052186
3316.679281	405607.983897	52.057191
3315.826466	405292.604974	52.062196
3315.321749	404984.233579	52.067201
3314.339151	404679.823483	52.072205
3313.599297	404358.241106	52.077210
3313.545947	404036.368968	52.082215
3312.172281	403733.460394	52.087220
3311.894586	403426.715465	52.092225
3310.948963	403119.209017	52.097229
3310.453188	402782.855176	52.102234
3309.664570	402493.034296	52.107239
3308.753820	402188.741530	52.112244
3308.590540	401881.124899	52.117249
3307.641192	401578.052577	52.122253
3306.977840	401264.637365	52.127258
3306.845109	400952.914572	52.132263
3306.252260	400637.168977	52.137268
3305.290375	400319.140047	52.142273
3304.395271	400017.010558	52.147277
3303.911546	399687.638680	52.152282
3303.327679	399382.861232	52.157287
3302.375933	399072.800737	52.162292
3302.265496	398743.055324	52.167297
3301.468412	398440.362023	52.172301
3300.623601	398128.801326	52.177306
3300.172758	397810.692799	52.182311
3299.365487	397501.433699	52.187316
3298.636730	397180.846331	52.192321
3297.864649	396872.414798	52.197325
3297.059194	396556.028339	52.202330
3296.778505	396248.250634	52.207335
3295.690632	395943.775717	52.212340
3295.002961	395620.141627	52.217345
3294.209510	395305.114452	52.222349
3293.693725	395006.159322	52.227354
3293.261642	394691.781202	52.232359
3292.676707	394388.102684	52.237364
3291.301173	394074.605438	52.242369
3290.896551	393761.434847	52.247373
3290.205511	393452.400180	52.252378
3289.703696	393146.790688	52.257383
3288.733477	392854.855328	52.262388
3288.575498	392532.379676	52.267393
3287.769308	392240.514927	52.272397
3287.022379	391915.507843	52.277402
3286.157446	391606.941985	52.282407
3285.320819	391310.878927	52.287412
3285.023316	391012.287118	52.292417
3284.286503	390714.779361	52.297421
3283.838991	390403.721378	52.302426
3283.281471	390085.660037	52.307431
3282.108606	389784.958724	52.312436
3281.912122	389459.816603	52.317441
3281.173107	389156.244292	52.322445
3280.066072	388857.152192	52.327450
3279.688085	388547.135074	52.332455
3279.176178	388248.732090	52.337460
3278.342805	387935.247130	52.342465
3277.782062	387629.675747	52.347469
3276.900973	387316.142140	52.352474
3276.509442	387002.757276	52.357479
3275.642434	386707.551135	52.362484
3275.422277	386388.106994	52.367489
3274.442694	386070.306033	52.372493
3273.347013	385783.698730	52.377498
3273.161085	385458.341217	52.382503
3272.257313	385163.510016	52.387508
3271.800971	384853.346922	52.392513
3270.866662	384556.354090	52.397517
3270.438949	384237.432918	52.402522
3270.061787	383929.385917	52.407527
3269.260391	383634.272169	52.412532
3268.399631	383314.597856	52.417537
3267.869075	383004.914480	52.422541
3267.296323	382703.170280	52.427546
3266.416632	382388.297963	52.432551
3265.896781	382082.547513	52.437556
3265.304153	381770.040856	52.442561
3264.497464	381464.763225	52.447565
3263.715468	381140.327625	52.452570
3263.164357	380839.811616	52.457575
3262.116567	380539.346410	52.462580
3261.695017	380225.630243	52.467585
3261.128691	379917.987890	52.472589
3260.395314	379613.676067	52.477594
3259.900839	379299.735103	52.482599
3259.110137	379004.279010	52.487604
3258.693267	378685.386452	52.492609
3257.936077	378393.277967	52.497613
3257.392959	378071.271867	52.502618
3256.658506	377748.504915	52.507623
3255.712564	377461.811890	52.512628
3255.012057	377142.366821	52.517633
3254.300888	376835.308514	52.522637
3253.886402	376529.828893	52.527642
3253.415838	376215.580087	52.532647
3252.013880	375902.035796	52.537652
3251.607011	375604.535275	52.542657
3251.225336	375303.467348	52.547661
3250.551739	374990.487658	52.552666
3250.058116	374673.457924	52.557671
3248.933766	374376.596193	52.562676
3248.604180	374059.535798	52.567681
3247.868797	373759.046750	52.572685
3247.154116	373444.815376	52.577690
3246.374426	373142.904330	52.582695
3246.037928	372828.786576	52.587700
3245.342253	372516.605796	52.592705
3244.413614	372218.960024	52.597709
3243.448956	371907.962066	52.602714
3243.139902	371598.206429	52.607719
3242.301569	371308.451757	52.612724
3241.814078	370993.530201	52.617729
3241.168647	370684.533471	52.622733
3240.766061	370368.678046	52.627738
3239.914791	370066.476618	52.632743
3239.175202	369764.916875	52.637748
3238.571101	369460.636853	52.642753
3238.083625	369138.807245	52.647757
3237.449110	368822.748289	52.652762
3237.061578	368509.904510	52.657767
3235.950668	368197.936191	52.662772
3235.067137	367888.066822	52.667777
3234.611081	367579.679633	52.672781
3233.981010	367264.473848	52.677786
3233.053542	366954.528593	52.682791
3232.133836	366658.624314	52.687796
3231.612220	366347.694723	52.692801
3230.992942	366043.215518	52.697805
3229.888137	365747.258204	52.702810
3229.579263	365442.980290	52.707815
3228.972543	365131.445168	52.712820
3228.412596	364828.933033	52.717825
3227.547127	364538.349512	52.722829
3227.088410	364224.622085	52.727834
3226.443461	363920.717999	52.732839
3225.679877	363626.117876	52.737844
3225.268986	363303.471116	52.742849
3224.366750	363001.968062	52.747853
3223.150171	362708.171694	52.752858
3223.253570	362389.381224	52.757863
3222.462555	362089.839429	52.762868
3222.015924	361784.261599	52.767873
3221.219857	361484.844004	52.772877
3220.681781	361173.169789	52.777882
3220.061290	360864.356513	52.782887
3219.110021	360563.634515	52.787892
3218.842450	360241.504037	52.792897
3217.889439	359935.892734	52.797901
3216.947245	359623.967064	52.802906
3216.811892	359314.100165	52.807911
3215.911028	359026.363896	52.812916
3215.260951	358702.680598	52.817921
3214.689468	358395.141669	52.822925
3213.944749	358076.507765	52.827930
3213.522497	357763.622819	52.832935
3212.338714	357472.537746	52.837940
3211.706314	357149.783076	52.842945
3211.010744	356854.825456	52.847949
3210.566231	356550.537846	52.852954
3209.946467	356247.650333	52.857959
3208.943934	355943.625493	52.862964
3208.406403	355632.501478	52.867969
3207.788952	355320.472061	52.872973
3207.075891	355026.906278	52.877978
3206.931094	354707.494551	52.882983
3205.595004	354417.128642	52.887988
3205.058631	354103.653890	52.892993
3204.659247	353800.844343	52.897997
3203.928318	353498.543589	52.903002
3203.559226	353185.062319	52.908007
3202.528269	352884.586985	52.913012
3202.267083	352563.577244	52.918017
3201.309120	352264.461151	52.923021
3200.653347	351960.892669	52.928026
3199.839812	351638.539533	52.933031
3199.092595	351344.627761	52.938036
3198.619206	351032.626487	52.943041
3198.096157	350723.558128	52.948045
3197.135783	350422.497930	52.953050
3196.408411	350109.869826	52.958055
3195.533673	349811.134229	52.963060
3195.065042	349501.388636	52.968065
3194.356429	349204.379628	52.973069
3193.727671	348897.684739	52.978074
3193.414314	348584.091710	52.983079
3192.422510	348286.079095	52.988084
3191.869774	347979.290800	52.993089
3191.384141	347673.330151	52.998093
3190.522224	347379.135502	53.003098
3190.113176	347072.217765	53.008103
3189.140997	346764.013032	53.013108
3188.709891	346436.453243	53.018113
3188.092095	346144.020794	53.023117
3187.036151	345838.267860	53.028122
3186.858463	345520.996771	53.033127
3185.532685	345223.581068	53.038132
3184.951258	344913.802957	53.043137
3184.790364	344611.338244	53.048141
3183.970449	344315.212427	53.053146
3183.539085	343995.631536	53.058151
3182.597604	343686.285805	53.063156
3181.921698	343382.623652	53.068161
3181.326989	343085.463423	53.073165
3180.567599	342770.611522	53.078170
3180.044581	342450.349688	53.083175
3178.921839	342152.886639	53.088180
3178.563688	341849.421121	53.093185
3178.102835	341548.159487	53.098189
3177.239540	341248.691008	53.103194
3176.387481	340929.695199	53.108199
3175.465082	340635.553266	53.113204
3174.992838	340341.516924	53.118209
3174.580304	340037.491200	53.123213
3173.868523	339734.835062	53.128218
3173.418773	339419.306321	53.133223
3172.404271	339124.561030	53.138228
3171.869171	338805.708061	53.143233
3171.307818	338497.091047	53.148237
3170.586418	338209.677502	53.153242
3169.861068	337896.195994	53.158247
3169.039083	337591.459860	53.163252
3168.782453	337280.726935	53.168257
3167.786990	336982.354143	53.173261
3167.289315	336687.312473	53.178266
3166.949678	336365.311040	53.183271
3165.925625	336070.680890	53.188276
3165.071906	335770.701956	53.193281
3164.925492	335462.107051	53.198285
3163.852022	335152.486396	53.203290
3163.203086	334855.322280	53.208295
3162.605258	334546.107338	53.213300
3161.852930	334236.508143	53.218305
3161.460379	333941.285257	53.223309
3160.213927	333631.048749	53.228314
3159.950585	333322.997469	53.233319
3159.610349	333018.928496	53.238324
3158.730147	332726.476273	53.243329
3157.857787	332403.293325	53.248333
3157.081834	332106.290489	53.253338
3156.535093	331807.111646	53.258343
3156.056799	331504.178313	53.263348
3155.235561	331208.553758	53.268353
3154.671903	330903.594752	53.273357
3153.837650	330585.591361	53.278362
3153.480061	330277.058373	53.283367
3152.403097	329983.607977	53.288372
3151.843832	329683.964281	53.293377
3151.241945	329379.132419	53.298381
3150.976040	329075.646450	53.303386
3150.234153	328757.289780	53.308391
3149.119224	328459.816901	53.313396
3148.547621	328149.985263	53.318401
3147.865612	327832.073599	53.323405
3147.303548	327556.201673	53.328410
3146.661410	327242.634987	53.333415
3145.702278	326950.529285	53.338420
3145.044557	326638.592142	53.343425
3144.348908	326338.244287	53.348429
3143.921855	326038.234723	53.353434
3143.039232	325728.926629	53.358439
3142.376119	325441.529770	53.363444
3141.562112	325124.443022	53.368449
3141.069635	324837.475354	53.373453
3140.085150	324544.270226	53.378458
3139.612984	324238.481615	53.383463
3139.195885	323950.455079	53.388468
3138.587788	323648.250407	53.393473
3137.821569	323334.230158	53.398477
3137.166922	323035.951740	53.403482
3136.591735	322737.328720	53.408487
3135.970913	322439.348437	53.413492
3135.141660	322145.448531	53.418497
3134.847568	321843.289731	53.423501
3133.621317	321538.145594	53.428506
3133.503940	321229.693128	53.433511
3132.598260	320926.558601	53.438516
3132.096734	320623.842887	53.443521
3131.198336	320312.837361	53.448525
3130.610760	320024.875903	53.453530
3130.069272	319718.624267	53.458535
3128.988680	319420.375757	53.463540
3128.670418	319115.283554	53.468545
3128.121438	318821.659592	53.473549
3126.955439	318508.933480	53.478554
3126.650874	318212.009738	53.483559
3126.359897	317907.698699	53.488564
3125.361950	317597.412933	53.493569
3124.828696	317291.304975	53.498573
3124.294394	317003.758833	53.503578
3123.459858	316679.057662	53.508583
3122.677906	316376.500155	53.513588
3121.757415	316080.253105	53.518593
3121.226867	315776.991973	53.523597
3120.228891	315480.653587	53.528602
3120.118474	315184.963267	53.533607
3119.380268	314880.892060	53.538612
3118.597686	314576.826990	53.543617
3117.863751	314263.790094	53.548621
3117.101524	313977.290088	53.553626
3116.927052	313664.926817	53.558631
3116.074372	313375.358385	53.563636
3115.577174	313063.095378	53.568641
3114.992762	312760.445261	53.573645
3113.869135	312459.789460	53.578650
3113.429164	312152.582201	53.583655
3112.641448	311851.973468	53.588660
3111.786587	311548.802658	53.593665
3111.143690	311255.630504	53.598669
3110.608126	310963.841168	53.603674
3110.181131	310643.284381	53.608679
3109.100150	310356.010679	53.613684
3108.251554	310047.792958	53.618689
3107.802959	309744.273059	53.623693
3107.068935	309456.636708	53.628698
3106.728722	309161.705318	53.633703
3106.144566	308858.128262	53.638708
3105.534928	308563.008888	53.643713
3105.047001	308255.646304	53.648717
3104.065065	307953.479646	53.653722
3103.601985	307639.898133	53.658727
3102.609470	307350.642594	53.663732
3101.876136	307034.377590	53.668737
3101.342361	306731.169462	53.673741
3100.357373	306441.223156	53.678746
3099.866150	306129.475988	53.683751
3099.171188	305833.014226	53.688756
3098.600277	305537.092429	53.693761
3097.954121	305232.039721	53.698765
3097.238692	304937.081740	53.703770
3097.277030	304620.918170	53.708775
3096.178302	304339.389143	53.713780
3095.683050	304024.989440	53.718785
3094.995223	303717.138816	53.723789
3094.259621	303406.290116	53.728794
3093.535207	303104.886904	53.733799
3092.958822	302798.468299	53.738804
3092.224959	302493.805695	53.743809
3091.750138	302186.809530	53.748813
3091.006339	301887.164144	53.753818
3090.391340	301582.735600	53.758823
3089.706119	301274.141100	53.763828
3088.774627	300968.029756	53.768833
3087.981265	300665.614079	53.773837
3087.609295	300362.392628	53.778842
3086.775671	300058.174090	53.783847
3085.876996	299752.641034	53.788852
3085.567607	299462.039492	53.793857
3085.199999	299154.740527	53.798861
3084.163033	298840.772803	53.803866
3083.831065	298530.996836	53.808871
3083.027517	298220.836565	53.813876
3082.053351	297911.008371	53.818881
3082.134145	297615.987241	53.823885
3080.886061	297307.220068	53.828890
3080.352903	297012.702630	53.833895
3079.487387	296693.457923	53.838900
3079.132424	296383.376440	53.843905
3078.447228	296089.951292	53.848909
3077.359875	295788.363475	53.853914
3077.124261	295473.983223	53.858919
3076.464817	295171.715569	53.863924
3075.879065	294865.844935	53.868929
3075.632117	294560.480525	53.873933
3074.433656	294240.724432	53.878938
3073.945121	293929.539893	53.883943
3073.187812	293624.204030	53.888948
3072.456389	293321.741484	53.893953
3071.904951	293006.006977	53.898957
3070.845275	292704.054002	53.903962
3070.225963	292392.557034	53.908967
3069.511877	292094.012193	53.913972
3068.985284	291795.309986	53.918977
3068.154425	291481.502348	53.923981
3067.613946	291184.380624	53.928986
3067.079384	290869.506656	53.933991
3066.143284	290572.599674	53.938996
3065.572386	290262.544157	53.944001
3065.210935	289964.908887	53.949005
3064.476744	289667.994467	53.954010
3063.476422	289349.092205	53.959015
3062.979316	289050.993595	53.964020
3062.201199	288740.892871	53.969025
3061.948162	288438.552848	53.974029
3060.975786	288115.035214	53.979034
3060.365543	287821.308377	53.984039
3059.429340	287500.789644	53.989044
3058.902292	287208.526259	53.994049
3058.302861	286911.002215	53.999053
3057.365662	286609.609313	54.004058
3057.017856	286302.036023	54.009063
3056.216132	285997.004735	54.014068
3055.472118	285692.473443	54.019073
3054.944850	285392.415475	54.024077
3054.489508	285082.617090	54.029082
3053.783740	284793.640124	54.034087
3052.898083	284482.050256	54.039092
3052.138880	284180.474627	54.044097
3052.042760	283871.560897	54.049101
3050.781059	283567.670419	54.054106
3050.307922	283257.236965	54.059111
3049.678828	282957.015312	54.064116
3048.988157	282665.946346	54.069121
3048.677788	282348.813955	54.074125
3047.543610	282044.571396	54.079130
3047.055656	281744.683362	54.084135
3046.345833	281441.213817	54.089140
3045.362210	281140.003223	54.094145
3045.084810	280833.230513	54.099149
3044.262243	280545.492405	54.104154
3043.753511	280244.460996	54.109159
3043.122734	279924.882388	54.114164
3042.290083	279624.818913	54.119169
3041.885995	279320.994611	54.124173
3041.214016	279024.929543	54.129178
3040.634433	278704.425619	54.134183
3040.206456	278406.666349	54.139188
3039.284867	278100.733398	54.144193
3038.284855	277781.136288	54.149197
3037.522571	277483.786336	54.154202
3037.100234	277189.438745	54.159207
3036.611793	276875.312651	54.164212
3035.940175	276574.993923	54.169217
3035.026034	276260.349393	54.174221
3034.203170	275953.101705	54.179226
3033.731390	275650.179007	54.184231
3032.832224	275341.135141	54.189236
3032.408100	275036.345721	54.194241
3031.962911	274722.034474	54.199245
3031.170026	274424.663828	54.204250
3030.350018	274122.560386	54.209255
3029.947673	273803.632678	54.214260
3029.071842	273513.915786	54.219265
3028.319432	273214.908919	54.224269
3027.711565	272905.997502	54.229274
3027.023753	272608.967063	54.234279
3026.775603	272291.899911	54.239284
3025.577309	271992.887488	54.244289
3025.305212	271686.368193	54.249293
3024.330382	271380.953491	54.254298
3023.747052	271085.766122	54.259303
3022.956610	270791.706775	54.264308
3022.488439	270476.508766	54.269313
3022.034155	270176.691537	54.274317
3020.969145	269871.087929	54.279322
3020.360697	269562.508805	54.284327
3019.826637	269257.381735	54.289332
3019.029271	268968.214146	54.294337
3018.835480	268650.452203	54.299341
3018.290761	268346.422418	54.304346
3017.399573	268049.374996	54.309351
3016.837023	267724.031499	54.314356
3016.101580	267427.723827	54.319361
3015.272730	267117.245357	54.324365
3014.536445	266814.698499	54.329370
3014.201178	266505.390247	54.334375
3013.452337	266197.395615	54.339380
3012.429715	265898.027289	54.344385
3011.933779	265580.417077	54.349389
3011.202730	265273.744658	54.354394
3010.372919	264967.928559	54.359399
3009.790094	264663.958244	54.364404
3008.918736	264363.981392	54.369409
3008.576566	264056.382506	54.374413
3007.765143	263756.014663	54.379418
3007.472133	263463.714758	54.384423
3006.762891	263143.517249	54.389428
3006.044260	262858.900158	54.394433
3005.452272	262536.214313	54.399437
3004.621362	262234.653981	54.404442
3004.074916	261918.939762	54.409447
3003.313665	261621.087322	54.414452
3002.496497	261306.893751	54.419457
3002.001108	261009.891234	54.424461
3001.410842	260702.844320	54.429466
3000.729353	260408.469618	54.434471
3000.461842	260080.718057	54.439476
2999.303362	259781.504313	54.444481
2998.779724	259474.601092	54.449485
2998.148909	259161.857680	54.454490
2997.350484	258856.373968	54.459495
2996.573754	258535.606730	54.464500
2995.891308	258240.852715	54.469505
2995.704415	257918.413966	54.474509
2995.085805	257630.526824	54.479514
2994.315163	257309.352847	54.484519
2993.534317	257006.160861	54.489524
2992.527419	256700.865833	54.494529
2992.334662	256389.839570	54.499533
2991.715653	256083.134264	54.504538
2990.787391	255764.177735	54.509543
2990.131450	255466.367227	54.514548
2989.302107	255151.343406	54.519553
2989.272882	254840.497351	54.524557
2987.921320	254538.392564	54.529562
2987.504031	254224.247288	54.534567
2987.224452	253912.983959	54.539572
2986.676541	253607.824739	54.544577
2985.633833	253288.482936	54.549581
2985.038661	252975.233806	54.554586
2984.311497	252672.422011	54.559591
2983.714016	252358.919664	54.564596
2982.970253	252053.030096	54.569601
2982.560678	251724.728500	54.574605
2981.742554	251425.447673	54.579610
2980.879326	251114.179800	54.584615
2980.683975	250798.986814	54.589620
2979.628400	250494.219042	54.594625
2978.994442	250178.918429	54.599629
2978.290300	249866.405376	54.604634
2977.584026	249560.896499	54.609639
2976.999211	249249.613631	54.614644
2976.481494	248931.444911	54.619649
2976.039753	248615.531310	54.624653
2975.018448	248301.594611	54.629658
2974.343847	247992.696885	54.634663
2974.050417	247679.282926	54.639668
2972.540564	247369.423713	54.644673
2971.951997	247065.760307	54.649677
2971.586217	246748.387162	54.654682
2970.973514	246449.923914	54.659687
2970.153553	246136.010999	54.664692
2969.331356	245836.792803	54.669697
2969.189306	245525.626110	54.674701
2968.661083	245214.037425	54.679706
2967.549725	244902.363528	54.684711
2967.097320	244586.995427	54.689716
2966.401796	244283.533405	54.694721
2965.934915	243959.358120	54.699725
2965.109456	243660.119898	54.704730
2964.761865	243342.853820	54.709735
2964.069140	243022.001678	54.714740
2963.364288	242712.000366	54.719745
2962.659122	242393.698316	54.724749
2961.881929	242077.853124	54.729754
2961.221626	241761.251770	54.734759
2960.656819	241438.651923	54.739764
2959.893806	241128.332827	54.744769
2959.431376	240820.691671	54.749773
2958.706266	240503.161750	54.754778
2957.918401	240180.320566	54.759783
2957.355693	239872.774197	54.764788
2956.451353	239558.254597	54.769793
2956.100722	239234.990372	54.774797
2954.946809	238924.637266	54.779802
2954.451164	238612.143685	54.784807
2954.069353	238300.371426	54.789812
2953.152144	237988.455647	54.794817
2952.364317	237675.043381	54.799821
2951.954386	237359.458707	54.804826
2951.482663	237054.044776	54.809831
2950.502331	236744.943633	54.814836
2949.611277	236421.060400	54.819841
2949.379179	236115.280244	54.824845
2948.680336	235797.607087	54.829850
2947.732913	235487.002155	54.834855
2947.237403	235164.333432	54.839860
2946.630970	234860.398739	54.844865
2945.966391	234530.374504	54.849869
2945.021724	234235.712911	54.854874
2944.409415	233909.960263	54.859879
2943.983100	233599.813442	54.864884
2943.106181	233299.160182	54.869889
2942.729013	232984.831662	54.874893
2942.235423	232675.615130	54.879898
2941.737837	232361.791524	54.884903
2940.880916	232029.616517	54.889908
2940.315839	231720.185282	54.894913
2939.371059	231397.549361	54.899917
2938.356884	231084.703030	54.904922
2937.918140	230763.949805	54.909927
2937.237363	230448.532128	54.914932
2936.679832	230150.919375	54.919937
2936.424580	229827.594238	54.924941
2935.561169	229515.366031	54.929946
2934.781645	229200.273944	54.934951
2934.295903	228881.750088	54.939956
2933.547683	228564.414721	54.944961
2932.729371	228248.517452	54.949965
2932.301413	227939.077622	54.954970
2931.587593	227609.799002	54.959975
2931.044464	227288.540332	54.964980
2929.881109	226976.636152	54.969985
2929.469559	226660.553090	54.974989
2928.738998	226337.227225	54.979994
2928.256168	226025.638967	54.984999
2927.580156	225699.353531	54.990004
2926.725296	225383.078226	54.995009
2926.292665	225068.850513	55.000013
2925.397015	224759.191078	55.005018
2924.718343	224441.987732	55.010023
2924.463630	224117.920682	55.015028
2923.519496	223803.333390	55.020033
2922.973578	223479.480562	55.025037
2921.954907	223164.933096	55.030042
2921.263668	222866.183704	55.035047
2920.826169	222548.084209	55.040052
2920.192595	222229.100538	55.045057
2919.535341	221906.481263	55.050061
2918.869936	221594.964883	55.055066
2917.917392	221280.032812	55.060071
2917.589183	220958.842122	55.065076
2916.660943	220654.779845	55.070081
2916.075062	220340.735668	55.075085
2915.530053	220016.210099	55.080090
2914.901245	219706.999853	55.085095
2914.653115	219386.821681	55.090100
2913.556490	219070.712593	55.095105
2913.036433	218744.788544	55.100109
2912.294053	218432.050313	55.105114
2911.699976	218109.144946	55.110119
2911.489060	217794.072336	55.115124
2910.346464	217472.402340	55.120129
2909.881437	217148.437175	55.125133
2909.126653	216831.953005	55.130138
2908.540756	216511.115774	55.135143
2907.843553	216191.455969	55.140148
2907.154476	215863.255474	55.145153
2906.785644	215541.599237	55.150157
2906.043062	215217.330724	55.155162
2905.229659	214898.764591	55.160167
2904.719468	214576.791671	55.165172
2904.027055	214259.329520	55.170177
2903.229348	213931.435676	55.175181
2902.676363	213607.208609	55.180186
2901.793681	213282.640777	55.185191
2901.299258	212956.880282	55.190196
2900.360667	212639.897695	55.195201
2900.070017	212310.849814	55.200205
2899.123561	211995.768098	55.205210
2898.490834	211665.084890	55.210215
2898.028402	211342.942194	55.215220
2897.204459	211022.894806	55.220225
2896.536845	210704.326145	55.225229
2895.698279	210383.877042	55.230234
2894.853553	210061.483256	55.235239
2894.355745	209739.036209	55.240244
2893.739228	209425.238776	55.245249
2893.315588	209094.536040	55.250253
2892.492540	208785.114582	55.255258
2891.698667	208465.991996	55.260263
2891.053884	208134.845854	55.265268
2890.501791	207824.444590	55.270273
2889.764296	207504.592720	55.275277
2889.304270	207190.171177	55.280282
2888.600804	206865.812033	55.285287
2887.450020	206538.776525	55.290292
2886.878262	206237.511716	55.295297
2886.528298	205902.475130	55.300301
2885.895716	205586.765895	55.305306
2885.130006	205274.604683	55.310311
2884.831788	204954.620757	55.315316
2883.622282	204636.984565	55.320321
2883.297495	204315.875758	55.325325
2882.625762	203993.678341	55.330330
2882.004163	203672.034759	55.335335
2881.142060	203348.573089	55.340340
2880.684080	203029.248846	55.345345
2879.776437	202705.199970	55.350349
2879.048379	202382.473471	55.355354
2878.122381	202075.598276	55.360359
2877.757076	201746.315183	55.365364
2877.319122	201434.301453	55.370369
2876.722605	201105.440576	55.375373
2876.000898	200795.078834	55.380378
2875.281719	200472.743896	55.385383
2874.633481	200150.157859	55.390388
2874.038694	199823.722274	55.395393
2873.464681	199506.574728	55.400397
2872.757356	199187.630490	55.405402
2872.046335	198866.143750	55.410407
2871.830623	198529.717835	55.415412
2870.746048	198216.170912	55.420417
2870.339117	197880.415662	55.425421
2869.436742	197556.065973	55.430426
2868.657152	197231.291669	55.435431
2868.061607	196908.577069	55.440436
2867.236542	196583.750401	55.445441
2866.532763	196249.477835	55.450445
2866.079690	195941.659661	55.455450
2865.440389	195627.587082	55.460455
2864.936120	195295.146893	55.465460
2863.797352	194981.691817	55.470465
2863.440586	194654.003991	55.475469
2862.686962	194343.889183	55.480474
2862.055750	194013.207998	55.485479
2861.440019	193687.921400	55.490484
2860.396845	193372.641768	55.495489
2859.899534	193045.381193	55.500493
2859.382562	192726.599720	55.505498
2858.731199	192402.663188	55.510503
2858.050488	192075.552627	55.515508
2857.314203	191760.552824	55.520513
2856.790464	191440.762959	55.525517
2856.170050	191118.242343	55.530522
2855.448964	190792.775382	55.535527
2854.938743	190476.348632	55.540532
2854.045476	190152.223746	55.545537
2853.457591	189829.973828	55.550541
2852.773211	189514.128125	55.555546
2851.669841	189187.384079	55.560551
2851.428629	188865.263947	55.565556
2850.790993	188550.714988	55.570561
2850.163595	188224.423882	55.575565
2849.685120	187902.576956	55.580570
2848.603454	187590.649234	55.585575
2848.253691	187260.618808	55.590580
2847.408345	186944.230776	55.595585
2846.829015	186617.867060	55.600589
2846.452083	186288.267744	55.605594
2845.383342	185960.574124	55.610599
2844.951503	185645.847020	55.615604
2844.325450	185321.344626	55.620609
2843.478108	184996.752400	55.625613
2842.970410	184670.976536	55.630618
2842.396366	184352.324685	55.635623
2841.910556	184016.589448	55.640628
2840.396790	183695.012630	55.645633
2840.165696	183370.169270	55.650637
2839.763255	183056.079071	55.655642
2838.747866	182726.021937	55.660647
2837.939519	182406.365401	55.665652
2837.566779	182091.170719	55.670657
2836.913988	181766.520514	55.675661
2836.114371	181441.183654	55.680666
2835.574073	181128.515688	55.685671
2835.216552	180796.550028	55.690676
2834.232969	180477.927652	55.695681
2833.757790	180153.744833	55.700685
2832.823724	179825.935678	55.705690
2832.312759	179504.587276	55.710695
2831.610901	179186.018992	55.715700
2830.659298	178862.875465	55.720705
2830.218495	178549.320315	55.725709
2829.402749	178234.097057	55.730714
2828.816738	177904.886750	55.735719
2828.543431	177574.497512	55.740724
2827.724719	177260.032526	55.745729
2827.117796	176931.812615	55.750733
2826.824189	176604.614077	55.755738
2825.478544	176268.719785	55.760743
2825.066297	175946.416572	55.765748
2824.178489	175624.496469	55.770753
2823.560318	175288.914732	55.775757
2823.300321	174972.865315	55.780762
2822.335475	174651.117758	55.785767
2821.861614	174322.541665	55.790772
2820.834588	174005.400375	55.795777
2820.415533	173674.022940	55.800781
2819.494344	173348.221896	55.805786
2818.872924	173038.298657	55.810791
2818.272643	172707.008848	55.815796
2817.427407	172388.999568	55.820801
2816.913276	172065.077673	55.825805
2816.358616	171757.443052	55.830810
2815.531057	171426.467083	55.835815
2815.299466	171099.392700	55.840820
2814.007494	170772.667053	55.845825
2813.512456	170455.571803	55.850829
2812.969214	170131.924914	55.855834
2812.443344	169782.590271	55.860839
2811.691275	169429.416075	55.865844
2811.009649	169106.143087	55.870849
2810.553964	168785.227723	55.875853
2809.694430	168460.793046	55.880858
2808.798135	168146.946793	55.885863
2808.336602	167813.604181	55.890868
2807.330273	167501.052324	55.895873
2806.966406	167168.895241	55.900877
2806.633912	166844.352834	55.905882
2805.611617	166538.474556	55.910887
2804.961873	166210.834435	55.915892
2804.485602	165889.832581	55.920897
2804.163079	165553.334676	55.925901
2803.080475	165237.355325	55.930906
2802.389932	164921.431019	55.935911
2802.139750	164587.511627	55.940916
2801.253505	164262.939694	55.945921
2800.579246	163949.309858	55.950925
2800.117003	163608.973927	55.955930
2799.356320	163277.792016	55.960935
2798.659306	162962.317994	55.965940
2797.678493	162640.089560	55.970945
2797.274318	162306.418954	55.975949
2796.837154	161987.644784	55.980954
2795.432119	161665.924567	55.985959
2795.440239	161337.957079	55.990964
2794.502627	161013.613244	55.995969
2793.975718	160692.360280	56.000973
2793.268417	160359.328024	56.005978
2792.555704	160031.372381	56.010983
2792.127686	159695.022130	56.015988
2791.268221	159378.270727	56.020993
2790.478232	159060.278030	56.025997
2790.115105	158739.665335	56.031002
2788.711324	158416.817726	56.036007
2788.481020	158074.171695	56.041012
2787.721093	157763.928078	56.046017
2787.065665	157443.856746	56.051021
2786.537160	157126.348874	56.056026
2785.836672	156803.138009	56.061031
2785.237093	156471.778526	56.066036
2784.274598	156149.581458	56.071041
2783.785757	155828.392913	56.076045
2783.322120	155513.508393	56.081050
2782.405520	155189.469980	56.086055
2781.833583	154872.028149	56.091060
2781.368419	154538.797690	56.096065
2780.672081	154216.881955	56.101069
2779.979970	153896.087215	56.106074
2779.154275	153572.202543	56.111079
2778.935516	153242.822792	56.116084
2777.860870	152927.131454	56.121089
2777.180614	152595.301811	56.126093
2777.007183	152271.809511	56.131098
2775.952133	151949.642097	56.136103
2775.155314	151627.170022	56.141108
2774.140877	151301.761441	56.146113
2773.750415	150983.222293	56.151117
2773.170428	150661.780314	56.156122
2772.735373	150345.033840	56.161127
2771.891985	150026.130970	56.166132
2770.932607	149707.567353	56.171137
2770.424968	149383.038209	56.176141
2770.053640	149052.453891	56.181146
2769.116958	148742.131768	56.186151
2768.673188	148404.168947	56.191156
2767.867111	148100.834964	56.196161
2767.461498	147765.211280	56.201165
2766.831902	147440.695739	56.206170
2765.993309	147132.152950	56.211175
2765.364991	146806.970155	56.216180
2764.848946	146480.197118	56.221185
2764.038605	146151.428106	56.226189
2763.560328	145833.221005	56.231194
2762.702404	145509.536704	56.236199
2762.088166	145181.852381	56.241204
2761.625097	144865.050571	56.246209
2760.890295	144539.641333	56.251213
2759.986276	144201.898206	56.256218
2759.318615	143884.401810	56.261223
2758.892888	143559.906952	56.266228
2757.780323	143232.487395	56.271233
2757.443275	142907.693119	56.276237
2756.862481	142580.132757	56.281242
2755.676252	142265.390925	56.286247
2755.096174	141952.424145	56.291252
2754.450760	141632.596915	56.296257
2753.937942	141304.175502	56.301261
2753.193056	140989.758165	56.306266
2752.674946	140664.355836	56.311271
2752.066054	140334.321158	56.316276
2751.256186	140018.793460	56.321281
2750.771261	139710.777278	56.326285
2750.171932	139377.549883	56.331290
2749.492066	139058.619444	56.336295
2748.860306	138731.324971	56.341300
2747.959160	138408.828369	56.346305
2747.326111	138086.635834	56.351309
2746.916206	137762.073837	56.356314
2745.923394	137448.215896	56.361319
2745.390261	137109.947205	56.366324
2744.664937	136800.449473	56.371329
2743.927906	136480.514230	56.376333
2743.631633	136158.556283	56.381338
2742.848942	135835.789699	56.386343
2742.191564	135507.302969	56.391348
2741.654292	135192.253807	56.396353
2740.618586	134858.295707	56.401357
2739.898050	134535.965679	56.406362
2739.004207	134223.206630	56.411367
2738.529352	133899.422087	56.416372
2738.089201	133572.536255	56.421377
2737.142996	133268.370223	56.426381
2736.882075	132947.382529	56.431386
2736.211688	132619.261156	56.436391
2735.707109	132291.688901	56.441396
2735.088280	131973.144211	56.446401
2734.342874	131646.608329	56.451405
2733.833091	131324.433671	56.456410
2732.906994	131006.151811	56.461415
2732.834260	130666.222260	56.466420
2731.972997	130338.653017	56.471425
2731.193152	130024.258418	56.476429
2730.738265	129690.332676	56.481434
2729.888720	129353.806307	56.486439
2729.418797	129032.655115	56.491444
2728.492151	128703.375508	56.496449
2727.944257	128365.733819	56.501453
2727.280823	128037.207880	56.506458
2726.337681	127719.804583	56.511463
2725.644518	127379.353218	56.516468
2725.235484	127053.656216	56.521473
2724.123873	126724.772524	56.526477
2723.902570	126393.313467	56.531482
2722.767432	126070.041846	56.536487
2722.446644	125743.419490	56.541492
2721.661077	125424.671856	56.546497
2720.811812	125098.496586	56.551501
2720.330166	124776.406774	56.556506
2719.556339	124458.684593	56.561511
2719.077446	124126.798905	56.566516
2718.341803	123815.110005	56.571521
2717.771079	123485.240438	56.576525
2717.243282	123157.336318	56.581530
2716.291544	122836.207795	56.586535
2715.435961	122504.655928	56.591540
2715.159415	122176.800295	56.596545
2714.224300	121849.929175	56.601549
2713.868587	121520.557864	56.606554
2712.917768	121208.108381	56.611559
2712.199971	120883.233647	56.616564
2711.385832	120557.197418	56.621569
2710.803040	120244.434486	56.626573
2710.308707	119917.866751	56.631578
2709.271705	119590.163911	56.636583
2708.661007	119274.623894	56.641588
2708.149909	118962.207805	56.646593
2707.697276	118641.984728	56.651597
2707.117888	118322.852125	56.656602
2706.160847	118005.535268	56.661607
2705.789760	117675.726272	56.666612
2705.124196	117347.561396	56.671617
2704.177812	117036.043772	56.676621
2703.679728	116710.215433	56.681626
2702.856244	116398.457609	56.686631
2702.667152	116067.155257	56.691636
2701.574589	115746.758737	56.696641
2701.166231	115413.354330	56.701645
2700.483555	115094.894081	56.706650
2699.579658	114774.168983	56.711655
2698.839635	114448.706333	56.716660
2698.172725	114132.680221	56.721665
2697.532683	113820.404691	56.726669
2696.677966	113496.578257	56.731674
2696.246501	113187.584130	56.736679
2695.519754	112854.568741	56.741684
2695.202221	112544.498337	56.746689
2694.372143	112215.931249	56.751693
2693.870895	111890.610060	56.756698
2692.928076	111582.630748	56.761703
2692.413682	111254.077175	56.766708
2691.825217	110933.211906	56.771713
2690.979176	110612.601044	56.776717
2690.480151	110293.335445	56.781722
2689.693822	109972.418892	56.786727
2689.243036	109651.440691	56.791732
2688.339952	109334.662940	56.796737
2687.612911	109013.464051	56.801741
2687.101755	108687.571390	56.806746
2686.149344	108367.311442	56.811751
2685.604076	108059.313498	56.816756
2685.133631	107721.834788	56.821761
2684.520371	107419.211010	56.826765
2683.939837	107087.665799	56.831770
2683.189761	106768.873366	56.836775
2682.871837	106446.964882	56.841780
2682.119243	106117.604853	56.846785
2681.134197	105793.666377	56.851789
2680.557402	105472.141955	56.856794
2679.721805	105145.885565	56.861799
2679.140506	104823.063688	56.866804
2678.561911	104502.409152	56.871809
2677.528042	104174.884286	56.876813
2676.862293	103862.360026	56.881818
2676.129909	103550.656149	56.886823
2675.660437	103218.677808	56.891828
2675.065871	102906.611717	56.896833
2674.137138	102588.849000	56.901837
2673.673903	102269.348469	56.906842
2672.843188	101959.578061	56.911847
2672.282096	101640.012841	56.916852
2671.861330	101326.284683	56.921857
2671.017056	101012.672271	56.926861
2670.533962	100677.598655	56.931866
2669.570603	100376.693726	56.936871
2669.088675	100055.513965	56.941876
2668.072819	99733.402072	56.946881
2667.436212	99426.907715	56.951885
2667.368934	99103.385770	56.956890
2666.291540	98801.314388	56.961895
2665.385021	98480.071702	56.966900
2665.168709	98164.559243	56.971905
2664.491363	97843.466789	56.976909
2663.798880	97520.281960	56.981914
2662.906427	97206.557939	56.986919
2662.234535	96891.623672	56.991924
2661.642939	96578.957851	56.996929
2660.944115	96258.531778	57.001933
2660.570109	95938.515397	57.006938
2659.851481	95631.209996	57.011943
2659.068815	95315.173765	57.016948
2658.234208	95005.872303	57.021953
2657.594759	94678.762613	57.026957
2657.192337	94356.141571	57.031962
2656.438518	94052.757023	57.036967
2655.927203	93744.309578	57.041972
2655.224182	93427.184055	57.046977
2654.234673	93114.198437	57.051981
2653.930925	92792.922388	57.056986
2652.899457	92479.698749	57.061991
2652.268920	92167.310069	57.066996
2651.786338	91852.290004	57.072001
2651.086802	91528.057889	57.077005
2650.565566	91209.660932	57.082010
2649.657294	90905.082292	57.087015
2649.542510	90579.763402	57.092020
2648.608341	90265.002537	57.097025
2647.608810	89949.787401	57.102029
2647.289855	89625.941613	57.107034
2646.714891	89315.772118	57.112039
2645.752327	89012.788148	57.117044
2644.971534	88687.843983	57.122049
2644.414627	88375.371069	57.127053
2643.936698	88058.382712	57.132058
2643.145721	87745.765819	57.137063
2642.638128	87422.420326	57.142068
2641.811987	87115.542649	57.147073
2641.021908	86796.587437	57.152077
2640.695435	86472.916932	57.157082
2640.161889	86162.012906	57.162087
2639.339607	85836.807819	57.167092
2638.822304	85520.078763	57.172097
2637.816744	85206.651880	57.177101
2637.261810	84891.890484	57.182106
2636.323544	84581.022997	57.187111
2635.643743	84264.623672	57.192116
2635.043966	83949.623521	57.197121
2634.210873	83652.133337	57.202125
2633.748355	83330.034502	57.207130
2633.279601	83031.779137	57.212135
2632.304458	82716.780874	57.217140
2631.632771	82407.532100	57.222145
2631.047856	82086.327381	57.227149
2630.768052	81769.604373	57.232154
2629.666244	81462.611591	57.237159
2628.946621	81149.066813	57.242164
2628.948525	80840.374624	57.247169
2627.899395	80524.926888	57.252173
2627.357991	80214.169095	57.257178
2626.352573	79898.210671	57.262183
2625.572093	79594.952556	57.267188
2624.813875	79285.504174	57.272193
2624.275176	78970.677354	57.277197
2623.928961	78660.773859	57.282202
2622.803135	78355.256833	57.287207
2621.988778	78044.562388	57.292212
2621.573638	77736.502396	57.297217
2620.666391	77435.811873	57.302221
2620.267664	77131.047002	57.307226
2619.540944	76813.983114	57.312231
2619.136645	76507.036159	57.317236
2618.453823	76211.688504	57.322241
2617.806841	75904.586380	57.327245
2617.176651	75585.188468	57.332250
2616.305315	75279.575962	57.337255
2615.782133	74974.483119	57.342260
2615.133571	74659.170251	57.347265
2614.484250	74362.532909	57.352269
2613.586993	74044.310474	57.357274
2612.921284	73745.619546	57.362279
2612.441254	73430.229611	57.367284
2611.676424	73136.599915	57.372289
2610.837483	72810.760512	57.377293
2610.395127	72513.376631	57.382298
2609.822018	72207.668743	57.387303
2608.715880	71906.978387	57.392308
2608.396311	71596.229048	57.397313
2607.785076	71295.760929	57.402317
2607.228148	70978.699136	57.407322
2606.558186	70675.893385	57.412327
2605.822706	70361.017135	57.417332
2605.152683	70062.071996	57.422337
2604.139951	69756.934121	57.427341
2603.654753	69441.323552	57.432346
2603.319235	69148.521159	57.437351
2602.255317	68847.155160	57.442356
2602.006448	68530.666795	57.447361
2600.992416	68228.802098	57.452365
2600.534839	67921.413545	57.457370
2599.525552	67618.012245	57.462375
2598.819279	67314.016683	57.467380
2598.318196	67005.009261	57.472385
2597.426311	66717.043448	57.477389
2597.693441	66390.641466	57.482394
2596.583377	66103.621819	57.487399
2595.428948	65784.386610	57.492404
2595.298863	65491.249095	57.497409
2594.220179	65195.505450	57.502413
2593.494522	64889.043567	57.507418
2592.942950	64586.532487	57.512423
2592.332288	64276.607947	57.517428
2591.434063	63972.065602	57.522433
2590.146252	63691.144732	57.527437
2590.007779	63380.716686	57.532442
2589.293366	63091.045500	57.537447
2588.722202	62798.870855	57.542452
2588.189479	62500.372562	57.547457
2587.472952	62212.051108	57.552461
2587.160940	61899.382839	57.557466
2586.353282	61609.052672	57.562471
2585.614649	61302.337332	57.567476
2584.911982	61001.803566	57.572481
2584.254256	60721.371440	57.577485
2583.623584	60411.839416	57.582490
2582.739947	60121.598095	57.587495
2581.670746	59818.577440	57.592500
2581.057465	59525.251154	57.597505
2580.563584	59240.523144	57.602509
2580.187891	58948.089363	57.607514
2579.113055	58644.895609	57.612519
2578.753664	58360.919374	57.617524
2578.240878	58074.211892	57.622529
2577.212565	57791.869614	57.627533
2576.824275	57479.774791	57.632538
2575.983535	57191.550504	57.637543
2575.412992	56902.949258	57.642548
2575.026277	56605.367068	57.647553
2574.470157	56314.310564	57.652557
2573.593369	56019.451753	57.657562
2573.119472	55720.774246	57.662567
2572.569385	55413.091481	57.667572
2571.665022	55120.017351	57.672577
2570.446740	54831.696922	57.677581
2570.326351	54537.109189	57.682586
2569.596877	54246.109896	57.687591
2568.633604	53946.032745	57.692596
2568.012112	53667.790460	57.697601
2567.005566	53368.267645	57.702605
2566.812633	53083.555689	57.707610
2565.798812	52794.450472	57.712615
2565.218551	52513.798831	57.717620
2564.854367	52210.921718	57.722625
2563.813547	51940.869184	57.727629
2563.007094	51646.522625	57.732634
2562.540563	51354.911206	57.737639
2562.097833	51073.516708	57.742644
2561.510747	50790.738467	57.747649
2560.478263	50499.354056	57.752653
2559.857785	50206.532894	57.757658
2559.255334	49923.296254	57.762663
2558.779749	49644.811491	57.767668
2558.370237	49348.759951	57.772673
2557.184338	49076.027727	57.777677
2556.525084	48780.714867	57.782682
2555.997731	48502.531416	57.787687
2555.013697	48215.361838	57.792692
2554.387244	47926.024022	57.797697
2553.766469	47657.478637	57.802701
2553.368517	47365.209959	57.807706
2552.203224	47088.231685	57.812711
2551.738815	46811.007496	57.817716
2551.210855	46520.658623	57.822721
2550.283745	46251.730924	57.827725
2549.879172	45969.522548	57.832730
2549.129013	45691.355530	57.837735
2548.350415	45413.146837	57.842740
2547.771722	45136.549192	57.847745
2546.567948	44867.332400	57.852749
2546.200148	44584.454248	57.857754
2545.437126	44320.195179	57.862759
2544.587675	44048.101196	57.867764
2544.203474	43772.582305	57.872769
2543.274472	43510.999389	57.877773
2542.328743	43233.509828	57.882778
2541.510063	42961.722121	57.887783
2540.471428	42696.234929	57.892788
2540.226996	42445.921790	57.897793
2539.427469	42193.907298	57.902797
2538.662933	41924.521144	57.907802
2537.730538	41681.911043	57.912807
2537.078241	41436.290774	57.917812
2536.521974	41173.963265	57.922817
2535.769507	40931.338412	57.927821
2534.994498	40684.741265	57.932826
2534.010732	40434.369102	57.937831
2533.348331	40195.344967	57.942836
2532.553593	39953.662364	57.947841
2531.263391	39734.396419	57.952845
2530.588619	39493.512316	57.957850
2529.513873	39274.777762	57.962855
2528.225160	39066.435892	57.967860
2527.627944	38869.356084	57.972865
2526.053902	38673.280715	57.977869
2525.291485	38472.101125	57.982874
2524.438921	38286.244585	57.987879
2523.515734	38096.759281	57.992884
2522.758582	37918.259442	57.997889
2521.545346	37760.697417	58.002893
2520.663333	37587.623696	58.007898
2519.891680	37442.377710	58.012903
2518.723489	37277.867600	58.017908
2518.783622	37111.273930	58.022913
2517.423073	36973.824629	58.027917
2516.536052	36814.637534	58.032922
2516.151149	36684.140776	58.037927
2515.365793	36532.199924	58.042932
2514.663295	36399.738899	58.047937
2513.891882	36254.188602	58.052941
2513.123744	36123.063094	58.057946
2512.856873	35993.765268	58.062951
2511.694775	35857.633945	58.067956
2511.200439	35721.083348	58.072961
2510.224004	35596.813290	58.077965
2509.739282	35463.833607	58.082970
2509.458842	35333.232813	58.087975
2508.642906	35205.818791	58.092980
2508.185147	35076.373402	58.097985
2507.536534	34954.215045	58.102989
2506.963436	34814.525054	58.107994
2506.262889	34688.561740	58.112999
2505.277069	34564.198136	58.118004
2505.141820	34429.262173	58.123009
2504.234986	34308.364805	58.128013
2504.027486	34184.776718	58.133018
2503.010856	34045.871493	58.138023
2502.498070	33913.586595	58.143028
2501.998819	33788.922504	58.148033
2500.851739	33666.446485	58.153037
2500.229964	33524.311343	58.158042
2499.569925	33406.409271	58.163047
2498.812577	33297.828134	58.168052
2498.470588	33167.407381	58.173057
2497.268024	33045.300314	58.178061
2497.130257	32927.950952	58.183066
2496.447893	32807.027367	58.188071
2495.769857	32682.052302	58.193076
2495.028316	32552.682636	58.198081
2494.434879	32436.407694	58.203085
2493.987782	32305.898207	58.208090
2493.554388	32194.627737	58.213095
2492.676244	32071.642112	58.218100
2492.481839	31945.124826	58.223105
2491.529054	31812.752673	58.228109
2490.635046	31689.453232	58.233114
2490.091075	31552.010956	58.238119
2489.588148	31440.500629	58.243124
2489.029384	31309.855570	58.248129
2488.329976	31185.456181	58.253133
2488.002983	31051.116983	58.258138
2487.121498	30920.132755	58.263143
2486.297840	30792.156696	58.268148
2485.898178	30661.068129	58.273153
2485.104942	30545.128967	58.278157
2484.668312	30411.317998	58.283162
2483.892869	30289.054670	58.288167
2483.231903	30167.074302	58.293172
2482.707830	30023.909529	58.298177
2481.450057	29906.327968	58.303181
2480.929332	29771.225792	58.308186
2480.505364	29653.250012	58.313191
2480.033092	29534.102547	58.318196
2479.285781	29406.129980	58.323201
2478.814255	29288.358709	58.328205
2478.376308	29145.958973	58.333210
2477.568073	29024.702486	58.338215
2477.029191	28889.021214	58.343220
2476.357470	28743.404409	58.348225
2475.363339	28618.886461	58.353229
2474.661652	28494.942391	58.358234
2474.650793	28367.828082	58.363239
2473.184909	28226.392441	58.368244
2472.738058	28108.140816	58.373249
2472.044507	27975.643357	58.378253
2471.696333	27842.858421	58.383258
2471.108617	27723.723579	58.388263
2470.401510	27586.786067	58.393268
2469.792840	27448.797026	58.398273
2468.729789	27340.060642	58.403277
2468.109819	27196.087693	58.408282
2467.867468	27067.942154	58.413287
2466.582926	26937.417243	58.418292
2466.238710	26804.911910	58.423297
2465.701965	26672.947623	58.428301
2464.573521	26553.376396	58.433306
2464.203868	26429.430275	58.438311
2463.572314	26299.299058	58.443316
2463.068896	26174.966989	58.448321
2461.975297	26055.746188	58.453325
2461.735489	25922.520755	58.458330
2461.001697	25791.114623	58.463335
2460.357650	25667.442180	58.468340
2459.898532	25540.991415	58.473345
2459.052691	25420.675402	58.478349
2458.347019	25275.429347	58.483354
2457.755746	25155.540916	58.488359
2456.875848	25023.746469	58.493364
2456.602832	24890.249783	58.498369
2455.335056	24774.490411	58.503373
2454.656542	24641.861664	58.508378
2454.510328	24519.924450	58.513383
2453.475796	24390.047953	58.518388
2452.956711	24265.157499	58.523393
2452.267158	24155.523509	58.528397
2451.945477	24020.184451	58.533402
2451.130514	23899.402771	58.538407
2450.289105	23774.341422	58.543412
2450.045535	23644.987594	58.548417
2449.004755	23511.517575	58.553421
2448.247375	23385.985584	58.558426
2447.872027	23251.387267	58.563431
2447.121967	23139.764953	58.568436
2446.599852	23008.266842	58.573441
2445.698276	22881.332462	58.578445
2445.230757	22750.210804	58.583450
2444.897682	22621.548314	58.588455
2443.695461	22500.983179	58.593460
2443.612175	22361.820045	58.598465
2442.405080	22239.287613	58.603469
2441.850868	22112.724386	58.608474
2440.934312	21986.676797	58.613479
2440.473303	21865.088594	58.618484
2439.927682	21736.768622	58.623489
2438.796137	21622.885888	58.628493
2438.212673	21491.320102	58.633498
2437.828580	21363.779747	58.638503
2437.218153	21242.464797	58.643508
2436.812636	21109.285412	58.648513
2435.863271	20991.778832	58.653517
2434.872281	20873.011351	58.658522
2434.196744	20739.179179	58.663527
2433.524178	20635.207643	58.668532
2433.238376	20506.815046	58.673537
2432.314384	20377.767951	58.678541
2431.818720	20251.274348	58.683546
2431.077945	20130.111026	58.688551
2430.086616	20018.788279	58.693556
2429.595767	19892.508390	58.698561
2428.918639	19780.498826	58.703565
2428.358891	19668.670396	58.708570
2427.742785	19539.170471	58.713575
2426.977288	19409.906091	58.718580
2426.272364	19293.186629	58.723585
2425.654413	19183.989506	58.728589
2425.312075	19055.716841	58.733594
2424.911528	18926.944486	58.738599
2423.747097	18821.253220	58.743604
2423.301752	18684.161122	58.748609
2422.520230	18562.981677	58.753613
2422.001593	18441.379416	58.758618
2421.168673	18321.885516	58.763623
2420.486655	18201.119782	58.768628
2419.995063	18074.782485	58.773633
2419.219962	17952.026817	58.778637
2418.105492	17831.928905	58.783642
2417.682055	17712.894561	58.788647
2416.953822	17603.470452	58.793652
2416.911354	17477.468976	58.798657
2415.685844	17358.882250	58.803661
2415.052748	17237.740915	58.808666
2414.865549	17114.301313	58.813671
2414.064078	17000.948342	58.818676
2413.266285	16884.529667	58.823681
2412.397965	16769.425238	58.828685
2411.714937	16634.653687	58.833690
2411.264730	16511.872710	58.838695
2410.499980	16407.872776	58.843700
2409.818911	16283.890814	58.848705
2409.138413	16165.918639	58.853709
2408.560322	16053.301037	58.858714
2408.095061	15941.483075	58.863719
2407.132771	15804.560568	58.868724
2406.616063	15677.645096	58.873729
2405.853940	15577.829418	58.878733
2405.330532	15449.832341	58.883738
2404.888485	15324.721649	58.888743
2403.958471	15225.119569	58.893748
2403.301289	15094.980677	58.898753
2402.385509	14975.704155	58.903757
2401.551488	14859.961782	58.908762
2400.947117	14742.878718	58.913767
2400.547559	14630.855951	58.918772
2399.900167	14514.016124	58.923777
2399.003238	14405.560595	58.928781
2398.252671	14288.309427	58.933786
2397.890374	14179.798339	58.938791
2396.805231	14072.392384	58.943796
2395.713413	13955.755439	58.948801
2395.485974	13850.255725	58.953805
2394.949891	13730.297058	58.958810
2394.051511	13633.462009	58.963815
2393.186851	13520.517410	58.968820
2392.859367	13416.111710	58.973825
2391.785380	13319.347637	58.978829
2391.204062	13222.366571	58.983834
2390.813184	13105.363964	58.988839
2389.963620	13017.664356	58.993844
2389.504164	12899.041892	58.998849
2388.781085	12798.307679	59.003853
2387.894337	12698.903705	59.008858
2387.458225	12599.251961	59.013863
2386.202887	12498.204067	59.018868
2385.858966	12383.767104	59.023873
2385.057445	12292.015206	59.028877
2384.181181	12197.998210	59.033882
2383.456143	12094.035494	59.038887
2382.745484	12010.754514	59.043892
2382.120088	11911.313660	59.048897
2381.379530	11825.265836	59.053901
2380.928772	11719.742246	59.058906
2380.422143	11640.802944	59.063911
2379.569818	11544.908442	59.068916
2379.107328	11443.434118	59.073921
2378.208541	11357.381695	59.078925
2377.288251	11267.703590	59.083930
2376.676334	11175.357913	59.088935
2376.030314	11082.237068	59.093940
2375.593684	10992.178739	59.098945
2374.453536	10917.209513	59.103949
2374.120069	10830.071147	59.108954
2373.574010	10743.486169	59.113959
2372.516902	10645.748451	59.118964
2371.998995	10560.225220	59.123969
2371.208977	10473.034290	59.128973
2370.460662	10390.720727	59.133978
2370.184673	10307.047050	59.138983
2369.600859	10223.372554	59.143988
2368.774482	10138.847022	59.148993
2367.884407	10053.443285	59.153997
2366.954760	9967.444323	59.159002
2366.560550	9885.589014	59.164007
2365.500498	9809.883994	59.169012
2365.293336	9725.584480	59.174017
2364.645103	9650.894641	59.179021
2363.845236	9575.574786	59.184026
2363.048867	9496.212979	59.189031
2362.292871	9416.870436	59.194036
2361.471675	9330.187720	59.199041
2360.839131	9264.220609	59.204045
2360.355930	9184.249855	59.209050
2360.143986	9109.084854	59.214055
2359.098397	9026.530460	59.219060
2358.596685	8947.148103	59.224065
2357.645338	8873.529491	59.229069
2356.844004	8807.367110	59.234074
2356.422497	8731.961907	59.239079
2355.585786	8660.103966	59.244084
2354.805410	8577.190881	59.249089
2354.272999	8522.498329	59.254093
2353.654713	8440.600453	59.259098
2353.244102	8361.189007	59.264103
2352.399173	8301.191075	59.269108
2351.946073	8220.611676	59.274113
2351.283052	8140.963745	59.279117
2350.550058	8072.449638	59.284122
2349.986833	7993.929740	59.289127
2349.197456	7927.828921	59.294132
2348.507799	7841.115437	59.299137
2347.449097	7766.711124	59.304141
2346.920761	7702.770416	59.309146
2346.615876	7628.631409	59.314151
2345.528107	7558.964260	59.319156
2344.941279	7483.780507	59.324161
2344.380828	7426.066486	59.329165
2343.708589	7358.571516	59.334170
2343.181541	7287.709184	59.339175
2342.572748	7218.355770	59.344180
2342.115185	7143.971245	59.349185
2340.875469	7084.854896	59.354189
2340.432892	7002.755624	59.359194
2339.710224	6933.047703	59.364199
2338.997477	6867.042779	59.369204
2338.368036	6800.290559	59.374209
2337.501458	6732.042032	59.379213
2337.018820	6661.972329	59.384218
2336.507254	6593.912658	59.389223
2335.635841	6531.136897	59.394228
2335.271938	6466.565297	59.399233
2334.431299	6395.252135	59.404237
2333.909693	6324.318602	59.409242
2333.180731	6264.829517	59.414247
2332.217293	6206.694323	59.419252
2331.847952	6139.142661	59.424257
2331.315354	6070.523970	59.429261
2330.448169	6005.764443	59.434266
2329.977531	5933.783530	59.439271
2329.187860	5863.320651	59.444276
2328.758989	5791.728971	59.449281
2327.826108	5731.037615	59.454285
2327.268148	5657.804377	59.459290
2326.773179	5583.383133	59.464295
2325.856882	5535.036104	59.469300
2325.191779	5452.510624	59.474305
2324.696636	5393.969931	59.479309
2323.640629	5327.637473	59.484314
2323.411954	5262.327993	59.489319
2322.209287	5198.523573	59.494324
2321.829646	5147.872452	59.499329
2320.908386	5083.380304	59.504333
2320.220432	5011.174924	59.509338
2319.785087	4944.446828	59.514343
2319.288462	4897.546489	59.519348
2318.633075	4840.920776	59.524353
2317.922754	4761.431000	59.529357
2317.409023	4692.401655	59.534362
2316.413086	4634.379557	59.539367
2315.722710	4571.498239	59.544372
2314.876474	4501.994106	59.549377
2314.239781	4443.914992	59.554381
2313.593871	4384.203433	59.559386
2313.373113	4339.381078	59.564391
2312.371783	4265.861500	59.569396
2311.587403	4206.892680	59.574401
2311.423312	4133.635300	59.579405
2310.552281	4093.629095	59.584410
2310.033664	4032.673196	59.589415
2309.228589	3973.254331	59.594420
2308.839937	3903.240384	59.599425
2308.027133	3843.686044	59.604429
2307.504100	3781.323366	59.609434
2306.689028	3704.624849	59.614439
2305.625592	3639.160023	59.619444
2305.286152	3597.570082	59.624449
2305.000697	3524.112596	59.629453
2303.844151	3461.202722	59.634458
2303.166266	3390.108576	59.639463
2302.501262	3345.057679	59.644468
2301.940420	3281.980746	59.649473
2301.527290	3225.374888	59.654477
2300.265625	3166.395271	59.659482
2300.061708	3104.207245	59.664487
2298.949625	3048.880075	59.669492
2298.495211	2996.805873	59.674497
2297.854243	2943.454739	59.679501
2297.343306	2880.303015	59.684506
2296.672749	2820.621450	59.689511
2295.681036	2760.183557	59.694516
2295.324672	2701.842135	59.699521
2294.861741	2644.596629	59.704525
2293.757965	2591.101756	59.709530
2293.345029	2519.266406	59.714535
2292.356064	2477.790562	59.719540
2291.783791	2413.379405	59.724545
2291.184209	2356.029747	59.729549
2290.693877	2296.643474	59.734554
2290.255528	2247.105418	59.739559
2289.244255	2191.415393	59.744564
2288.658512	2124.347843	59.749569
2287.930928	2066.277599	59.754573
2287.005183	2022.672613	59.759578
2286.883383	1965.265265	59.764583
2286.229491	1905.378205	59.769588
2285.425962	1850.705293	59.774593
2284.642767	1801.419799	59.779597
2283.926833	1731.349095	59.784602
2283.813317	1670.131403	59.789607
2282.971875	1623.631377	59.794612
2282.046063	1563.334666	59.799617
2281.487496	1501.314596	59.804621
2280.267970	1453.652882	59.809626
2280.058724	1384.618439	59.814631
2279.449480	1345.111292	59.819636
2278.511247	1294.935860	59.824641
2277.782705	1245.266677	59.829645
2277.163926	1190.896540	59.834650
2276.738649	1124.743310	59.839655
2275.986981	1082.676344	59.844660
2275.170580	1024.515540	59.849665
2274.764121	964.799692	59.854669
2273.505589	918.931073	59.859674
2272.793670	864.083341	59.864679
2272.062175	812.074308	59.869684
2271.632489	765.729341	59.874689
2270.946483	724.044088	59.879693
2270.358176	685.320744	59.884698
2269.694584	628.402008	59.889703
2268.517431	588.450851	59.894708
2268.218161	540.428550	59.899713
2267.470481	502.374369	59.904718
2266.659107	458.514678	59.909722
2266.232715	406.581705	59.914727
2265.479737	374.699200	59.919732
2264.813936	339.882489	59.924737
2264.213957	285.820266	59.929742
2263.758427	241.239331	59.934746
2262.960151	200.652001	59.939751
2261.841008	170.843312	59.944756
2260.970945	127.367663	59.949761
2260.614679	99.601600	59.954766
2259.550898	52.068036	59.959770
2258.676762	24.769029	59.964775
2257.693865	8.799855	59.969780
2256.759764	-11.844599	59.974785
2255.670555	-11.447815	59.979790
2251.580499	57.208808	59.984794
2251.453989	65.638486	59.989799
2251.799663	66.682820	59.994804
2251.820039	69.026075	59.999809
2252.083805	61.923021	60.004814
2251.621791	70.896336	60.009818
2251.189840	58.652620	60.014823
2249.820179	76.064340	60.019828
2248.936794	79.088685	60.024833
2248.761283	64.451570	60.029838
2248.029357	75.050898	60.034842
2247.183436	77.471660	60.039847
2246.225720	77.740362	60.044852
2246.043900	83.272622	60.049857
2245.375850	81.946868	60.054862
2244.428953	83.931084	60.059866
2244.717174	57.844751	60.064871
2244.003734	84.755609	60.069876
2242.928778	81.792946	60.074881
2242.480420	85.716491	60.079886
2241.354410	77.786850	60.084890
2240.565009	89.443937	60.089895
2240.480053	87.949992	60.094900
2239.772619	77.098206	60.099905
2239.330614	82.014180	60.104910
2238.301712	87.297641	60.109914
2237.408130	81.552961	60.114919
2236.797518	84.330619	60.119924
2236.598006	89.241241	60.124929
2236.693372	79.632412	60.129934
2235.408695	84.507037	60.134938
2234.534229	76.646300	60.139943
2233.755037	80.377910	60.144948
2232.966846	84.651822	60.149953
2232.299822	82.488583	60.154958
2231.391238	83.936891	60.159962
2230.998540	65.953388	60.164967
2230.728197	72.160402	60.169972
2230.073588	78.647569	60.174977
2229.565423	72.201536	60.179982
2228.496506	80.214628	60.184986
2227.658764	76.030098	60.189991
2226.720920	86.928600	60.194996
2226.218760	87.620180	60.200001
2226.583405	69.806672	60.205006
2225.454921	81.408745	60.210010
2224.615017	76.160161	60.215015
2223.946342	84.666400	60.220020
2223.457262	76.780795	60.225025
2223.197451	77.654691	60.230030
2222.288244	80.758831	60.235034
2221.681955	81.449585	60.240039
2220.793531	79.272590	60.245044
2220.046271	77.770183	60.250049
2219.410046	67.700289	60.255054
2218.269182	73.198624	60.260058
2218.193599	75.609140	60.265063
2216.957036	76.437732	60.270068
2216.264820	71.394371	60.275073
2216.615012	71.077132	60.280078
2215.805554	78.402540	60.285082
2215.084784	79.835248	60.290087
2214.048929	85.313776	60.295092
2213.671424	91.160925	60.300097
2213.401258	73.449703	60.305102
2211.978851	85.878973	60.310106
2211.574948	79.966734	60.315111
2211.069955	84.408601	60.320116
2210.431458	80.337540	60.325121
2209.423638	77.689080	60.330126
2209.166023	82.134276	60.335130
2208.633272	76.884274	60.340135
2207.769709	80.192479	60.345140
2206.771303	82.019306	60.350145
2206.496701	82.275834	60.355150
2205.747787	74.037238	60.360154
2205.292591	76.022300	60.365159
2204.072041	73.959503	60.370164
2203.633368	82.099684	60.375169
2203.545024	74.546306	60.380174
2202.346737	85.546055	60.385178
2201.671609	75.922285	60.390183
2201.069639	73.319821	60.395188
2200.579901	81.516987	60.400193
2199.853223	73.309557	60.405198
2198.832113	79.063280	60.410202
2198.645538	84.405492	60.415207
2197.859192	84.927708	60.420212
2197.126659	81.246868	60.425217
2196.867145	78.624763	60.430222
2195.091267	80.608060	60.435226
2195.097799	75.852795	60.440231
2194.681871	81.997761	60.445236
2193.910159	84.077196	60.450241
2193.584712	69.118539	60.455246
2192.470247	84.190701	60.460250
2191.908261	76.561089	60.465255
2191.230496	71.009263	60.470260
2190.374229	75.893201	60.475265
2190.211964	76.844659	60.480270
2189.019551	82.229766	60.485274
2188.666553	73.489987	60.490279
2187.806857	84.216832	60.495284
2187.188505	69.110692	60.500289
2186.579470	69.199519	60.505294
2186.055888	78.244110	60.510298
2185.610305	72.617602	60.515303
2184.493533	78.805958	60.520308
2183.380906	74.363874	60.525313
2183.599700	68.494768	60.530318
2182.873308	84.926133	60.535322
2182.261426	74.390357	60.540327
2181.386559	73.244085	60.545332
2180.099781	82.674688	60.550337
2180.117862	75.385112	60.555342
2179.286922	75.042391	60.560346
2178.554275	70.431216	60.565351
2178.194055	68.933643	60.570356
2177.735575	70.416204	60.575361
2177.097860	72.868603	60.580366
2176.215141	71.819769	60.585370
2175.901345	66.705342	60.590375
2174.966962	74.116808	60.595380
2174.279730	80.536624	60.600385
2173.804074	76.887572	60.605390
2172.700799	78.975467	60.610394
2171.677197	71.340264	60.615399
2171.167564	69.306605	60.620404
2170.908345	65.686291	60.625409
2170.750980	71.091669	60.630414
2169.187522	75.296224	60.635418
2168.758328	74.221163	60.640423
2168.020495	68.197926	60.645428
2167.819196	77.830021	60.650433
2167.145464	70.080962	60.655438
2165.828586	70.444525	60.660442
2165.614105	72.621624	60.665447
2165.452845	72.093806	60.670452
2164.562722	78.630967	60.675457
2164.223426	72.292193	60.680462
2163.195177	70.542665	60.685466
2162.206351	72.039995	60.690471
2161.363533	68.031332	60.695476
2160.691615	70.049210	60.700481
2160.499448	65.858464	60.705486
2159.209536	72.216219	60.710490
2158.942353	66.979286	60.715495
2158.278931	76.714667	60.720500
2157.400616	73.533193	60.725505
2157.022630	62.253878	60.730510
2156.490182	70.554008	60.735514
2155.728232	74.361745	60.740519
2155.318933	65.648257	60.745524
2154.544652	76.926075	60.750529
2154.382609	68.252197	60.755534
2153.169364	74.481101	60.760538
2152.720937	80.801531	60.765543
2151.357238	76.878672	60.770548
2150.695145	79.041645	60.775553
2150.678561	63.803772	60.780558
2149.879926	73.994250	60.785562
2149.037408	70.264651	60.790567
2148.724543	73.181152	60.795572
2147.968761	76.432850	60.800577
2147.628480	73.517652	60.805582
2146.800597	70.698748	60.810586
2146.090381	64.146036	60.815591
2144.809209	70.546562	60.820596
2143.775630	72.721175	60.825601
2144.037863	63.905865	60.830606
2143.445274	74.885206	60.835610
2142.365398	74.288696	60.840615
2142.007079	71.295941	60.845620
2141.084930	65.491188	60.850625
2140.971470	61.147614	60.855630
2140.020535	74.035077	60.860634
2139.677242	75.087799	60.865639
2138.883326	59.520713	60.870644
2137.416288	62.773313	60.875649
2137.000314	65.499603	60.880654
2136.209304	73.601079	60.885658
2136.235609	61.948548	60.890663
2135.526162	68.647846	60.895668
2134.574417	64.117183	60.900673
2134.513823	59.465614	60.905678
2133.821222	66.209544	60.910682
2133.157043	51.709932	60.915687
2131.943144	72.293309	60.920692
2130.735530	59.059432	60.925697
2130.631212	67.679540	60.930702
2129.531156	69.757479	60.935706
2128.732528	61.416426	60.940711
2128.892994	67.134053	60.945716
2128.211414	70.932196	60.950721
2128.224963	51.804117	60.955726
2127.436200	64.678456	60.960730
2126.259436	67.711544	60.965735
2125.328076	71.653399	60.970740
2124.287718	64.367795	60.975745
2124.007045	57.234445	60.980750
2123.205874	76.476638	60.985754
2122.717256	70.912165	60.990759
2122.668391	60.340692	60.995764
2121.680601	70.040817	61.000769
2121.363006	62.763520	61.005774
2120.072880	63.745729	61.010778
2119.451830	60.657482	61.015783
2118.464685	69.414530	61.020788
2117.412404	78.401105	61.025793
2117.753724	64.360066	61.030798
2116.791826	82.248000	61.035802
2116.220153	73.547669	61.040807
2116.208995	71.911139	61.045812
2115.319537	72.918075	61.050817
2114.210888	64.512687	61.055822
2113.152855	76.652365	61.060826
2112.682969	70.179790	61.065831
2112.386510	55.837863	61.070836
2111.501467	83.222203	61.075841
2111.426066	67.992090	61.080846
2110.849999	70.344837	61.085850
2109.440619	66.441869	61.090855
2108.519721	77.134285	61.095860
2107.684334	71.072935	61.100865
2107.693548	73.469994	61.105870
2106.773561	62.855418	61.110874
2106.123825	69.043798	61.115879
2106.025581	67.239747	61.120884
2105.328273	69.482431	61.125889
2105.211105	69.556297	61.130894
2103.639486	67.266999	61.135898
2102.657937	64.593917	61.140903
2102.580537	63.617576	61.145908
2101.686918	78.536441	61.150913
2101.270766	63.617441	61.155918
2100.837546	77.053510	61.160922
2099.728524	70.630328	61.165927
2098.725911	60.032025	61.170932
2097.772035	75.927079	61.175937
2097.701446	68.996922	61.180942
2096.982057	67.368711	61.185946
2096.509499	66.895029	61.190951
2096.332819	73.024110	61.195956
2095.457074	78.989753	61.200961
2094.707560	66.939969	61.205966
2093.480297	71.494893	61.210970
2092.767129	71.065704	61.215975
2092.442872	62.766073	61.220980
2091.913842	70.609949	61.225985
2091.290551	76.089270	61.230990
2090.720647	56.763638	61.235994
2089.903785	72.018809	61.240999
2089.353696	73.153238	61.246004
2088.403035	66.200330	61.251009
2088.071204	64.406542	61.256014
2087.250562	73.572397	61.261018
2086.643423	66.448283	61.266023
2086.304134	65.991299	61.271028
2084.875655	69.586300	61.276033
2084.174037	67.299289	61.281038
2083.346275	65.480132	61.286042
2082.933220	70.251183	61.291047
2082.590174	74.877090	61.296052
2081.902173	76.276248	61.301057
2081.503332	60.141887	61.306062
2081.067379	71.577322	61.311066
2080.449192	72.509681	61.316071
2079.163621	66.526096	61.321076
2078.068127	72.886145	61.326081
2077.938437	53.957417	61.331086
2077.084215	67.360948	61.336090
2076.776294	72.370770	61.341095
2076.472679	70.235053	61.346100
2075.798557	61.241931	61.351105
2074.698676	62.449424	61.356110
2073.843789	60.066899	61.361114
2073.368084	61.362983	61.366119
2073.294650	59.386271	61.371124
2072.002161	77.066486	61.376129
2071.069990	72.181096	61.381134
2070.192463	77.967263	61.386138
2069.604856	71.888680	61.391143
2069.310375	64.658185	61.396148
2068.459175	61.723167	61.401153
2068.206642	54.487596	61.406158
2067.670730	67.911572	61.411162
2067.146860	68.075215	61.416167
2066.872713	53.720300	61.421172
2065.663282	72.738717	61.426177
2065.032617	69.002333	61.431182
2064.691092	58.928305	61.436186
2063.126754	62.483378	61.441191
2062.542795	66.496266	61.446196
2061.483552	75.438232	61.451201
2061.489366	61.177645	61.456206
2060.657852	72.093990	61.461210
2060.245224	63.235983	61.466215
2059.979847	58.664227	61.471220
2059.231578	73.670408	61.476225
2058.327910	65.596776	61.481230
2057.292429	67.240313	61.486234
2056.632963	67.327712	61.491239
2056.129825	70.406876	61.496244
2055.552937	69.979721	61.501249
2055.510790	72.941570	61.506254
2054.011287	78.088474	61.511258
2053.170919	66.977181	61.516263
2052.791585	68.134977	61.521268
2052.097082	72.750437	61.526273
2051.550331	65.932127	61.531278
2051.410165	66.656167	61.536282
2050.833302	64.973811	61.541287
2049.930223	58.581048	61.546292
2048.670821	66.316929	61.551297
2048.255649	61.366843	61.556302
2047.801134	65.570492	61.561306
2047.160803	69.125573	61.566311
2046.087132	54.626334	61.571316
2045.192090	78.461120	61.576321
2044.700302	53.813749	61.581326
2044.152632	67.119748	61.586330
2043.454755	68.190914	61.591335
2043.186235	64.067492	61.596340
2042.759658	71.437817	61.601345
2042.369917	63.487620	61.606350
2041.166965	62.412392	61.611354
2040.359384	73.996696	61.616359
2039.801948	59.144298	61.621364
2038.984480	61.428144	61.626369
2038.357743	60.018623	61.631374
2037.209522	68.257234	61.636378
2036.585514	69.576863	61.641383
2036.448638	58.484809	61.646388
2035.656877	72.302619	61.651393
2035.665502	64.371192	61.656398
2034.976963	58.832169	61.661402
2033.832302	64.208175	61.666407
2033.000610	58.198310	61.671412
2032.477439	61.233349	61.676417
2032.010178	60.533345	61.681422
2031.759672	60.294079	61.686426
2030.500706	59.514739	61.691431
2029.643033	63.001822	61.696436
2028.794721	66.638801	61.701441
2028.323752	65.969347	61.706446
2027.826792	66.065652	61.711450
2027.192237	61.005318	61.716455
2027.039281	69.309881	61.721460
2025.800048	72.329273	61.726465
2025.054637	72.062908	61.731470
2024.364920	68.384792	61.736474
2023.916129	67.768586	61.741479
2023.583242	56.592535	61.746484
2022.591205	75.630076	61.751489
2021.812444	65.505609	61.756494
2021.181137	66.775939	61.761498
2020.834433	65.955881	61.766503
2020.408943	64.929142	61.771508
2019.110808	76.938229	61.776513
2018.393567	63.937228	61.781518
2018.066398	68.407660	61.786522
2017.416207	65.306720	61.791527
2017.040277	60.203763	61.796532
2015.485420	65.132398	61.801537
2014.650151	70.932369	61.806542
2013.975324	71.552050	61.811546
2013.477987	71.673647	61.816551
2013.715781	67.146603	61.821556
2013.104962	68.568218	61.826561
2012.715387	66.096086	61.831566
2011.269291	64.493366	61.836570
2010.348142	60.328466	61.841575
2010.211906	63.254786	61.846580
2009.648957	69.391562	61.851585
2009.092261	54.225263	61.856590
2008.010426	63.123518	61.861594
2006.822538	63.327919	61.866599
2006.471717	60.081698	61.871604
2005.923073	71.968666	61.876609
2005.607357	60.996462	61.881614
2005.294120	58.100650	61.886618
2004.240694	63.230384	61.891623
2003.499885	59.899416	61.896628
2002.722137	69.572540	61.901633
2002.088184	60.658221	61.906638
2001.641999	66.785924	61.911642
2000.784341	68.022805	61.916647
2000.019787	57.104504	61.921652
1998.944175	62.281913	61.926657
1998.752294	61.107716	61.931662
1997.933598	63.740259	61.936666
1997.951068	67.317087	61.941671
1997.697464	63.765289	61.946676
1995.927370	73.189098	61.951681
1995.233336	59.455908	61.956686
1994.784791	61.096184	61.961690
1994.264899	73.076357	61.966695
1993.978746	60.319164	61.971700
1992.491467	69.718580	61.976705
1992.192640	64.961340	61.981710
1991.752817	63.987341	61.986714
1990.963002	63.396889	61.991719
1990.632163	65.426895	61.996724
1989.295779	64.189953	62.001729
1988.540534	46.735596	62.006734
1987.854278	69.217382	62.011738
1987.531978	62.678839	62.016743
1987.272906	55.611470	62.021748
1986.480783	57.933883	62.026753
1985.292215	55.705277	62.031758
1984.807382	66.298533	62.036762
1984.122896	74.296404	62.041767
1983.825463	65.585701	62.046772
1983.131503	71.754316	62.051777
1982.709660	61.014997	62.056782
1981.239260	57.471859	62.061786
1980.592896	65.017417	62.066791
1980.243810	62.977238	62.071796
1979.604222	72.715165	62.076801
1979.580829	60.370408	62.081806
1978.852871	55.197190	62.086810
1977.621713	61.559881	62.091815
1976.922958	68.192860	62.096820
1976.463494	59.690801	62.101825
1975.523833	67.106309	62.106830
1974.714551	66.886366	62.111834
1973.663395	74.522994	62.116839
1973.767670	73.584047	62.121844
1973.297500	70.735226	62.126849
1972.739734	65.505029	62.131854
1972.573770	60.605282	62.136858
1971.220290	75.567205	62.141863
1970.197501	62.053360	62.146868
1969.631009	62.591202	62.151873
1969.191638	74.113914	62.156878
1968.636710	62.739741	62.161882
1967.283145	57.963867	62.166887
1966.660953	60.109507	62.171892
1966.354343	67.850282	62.176897
1965.693202	70.494094	62.181902
1965.450098	53.612845	62.186906
1964.581592	82.200875	62.191911
1964.630715	56.486850	62.196916
1962.997140	62.020915	62.201921
1962.388053	67.373427	62.206926
1962.109739	68.363818	62.211930
1961.134274	71.650435	62.216935
1960.316200	54.992919	62.221940
1959.582667	73.981546	62.226945
1959.457740	66.071327	62.231950
1959.045453	63.995454	62.236954
1958.074656	68.955977	62.241959
1957.195376	60.395994	62.246964
1956.308114	68.296753	62.251969
1956.161849	70.310077	62.256974
1955.571138	69.030469	62.261978
1954.312837	59.551414	62.266983
1953.740681	70.634755	62.271988
1953.105875	78.287295	62.276993
1952.489039	55.604110	62.281998
1952.045220	80.169906	62.287002
1951.575718	62.723799	62.292007
1950.528658	71.883049	62.297012
1949.535017	67.969365	62.302017
1948.972789	70.886047	62.307022
1948.510661	59.090316	62.312026
1947.831738	63.902008	62.317031
1947.914614	66.101296	62.322036
1946.892868	66.203659	62.327041
1946.016270	65.511886	62.332046
1945.665690	68.353969	62.337050
1944.292791	70.796979	62.342055
1944.310729	64.937680	62.347060
1943.255600	62.749407	62.352065
1942.416634	61.097649	62.357070
1941.952425	57.467336	62.362074
1941.643843	55.204701	62.367079
1941.106960	54.003282	62.372084
1939.926000	58.254461	62.377089
1938.888666	59.031053	62.382094
1938.670515	54.835001	62.387098
1938.112465	59.578621	62.392103
1937.679962	58.349593	62.397108
1936.999639	65.361257	62.402113
1936.163806	50.926823	62.407118
1935.628322	64.443770	62.412122
1934.724771	74.196803	62.417127
1934.468608	64.738426	62.422132
1932.887783	66.186324	62.427137
1932.272005	66.933839	62.432142
1931.983001	68.028427	62.437146
1931.237152	63.569235	62.442151
1931.143376	63.896427	62.447156
1930.638893	66.570565	62.452161
1929.453721	63.642888	62.457166
1928.922820	63.407147	62.462170
1928.003154	60.295400	62.467175
1927.835623	57.229819	62.472180
1927.016466	63.047752	62.477185
1925.997708	55.739894	62.482190
1925.301879	57.698547	62.487194
1924.684873	65.958510	62.492199
1924.404295	53.686135	62.497204
1923.877858	57.918561	62.502209
1922.701415	57.410011	62.507214
1922.040999	56.772230	62.512218
1921.418944	65.234836	62.517223
1920.866581	57.731515	62.522228
1920.373190	62.948976	62.527233
1919.851924	61.858616	62.532238
1919.228048	61.268649	62.537242
1917.964042	68.393484	62.542247
1917.743857	57.371446	62.547252
1917.296063	69.447401	62.552257
1916.407441	67.959646	62.557262
1915.620904	66.149769	62.562266
1914.637473	60.831058	62.567271
1914.899936	52.908232	62.572276
1913.519118	58.465270	62.577281
1912.900255	63.392007	62.582286
1912.161775	58.502743	62.587290
1911.392979	55.986764	62.592295
1911.080576	50.902129	62.597300
1910.708362	61.759768	62.602305
1909.917131	59.643147	62.607310
1909.245734	52.086195	62.612314
1908.656923	70.629242	62.617319
1908.076272	55.652855	62.622324
1906.879747	52.786914	62.627329
1905.847786	66.325920	62.632334
1905.555628	52.989418	62.637338
1904.758726	57.641662	62.642343
1904.731961	52.298799	62.647348
1904.114454	58.963041	62.652353
1902.857256	57.842877	62.657358
1902.411603	58.033557	62.662362
1901.639777	67.658452	62.667367
1901.281075	57.457887	62.672372
1900.749188	60.120612	62.677377
1899.766670	56.063267	62.682382
1899.341845	59.558931	62.687386
1898.139569	49.962216	62.692391
1898.296166	48.694855	62.697396
1897.154972	58.572345	62.702401
1896.092516	51.217828	62.707406
1895.710415	54.090149	62.712410
1894.717897	63.371631	62.717415
1894.745213	54.495858	62.722420
1894.187616	64.416307	62.727425
1893.076715	54.579590	62.732430
1892.197043	59.673889	62.737434
1891.769538	57.931590	62.742439
1891.328691	50.270234	62.747444
1890.891957	59.403551	62.752449
1890.107004	59.143503	62.757454
1889.171660	45.946977	62.762458
1888.614702	55.553520	62.767463
1888.361874	57.348808	62.772468
1887.087685	67.252154	62.777473
1886.426367	62.011617	62.782478
1886.175191	51.354039	62.787482
1885.141711	54.355013	62.792487
1884.982702	58.365111	62.797492
1883.295511	56.925317	62.802497
1883.045013	57.070822	62.807502
1882.667759	52.031180	62.812506
1882.075120	62.849705	62.817511
1881.874608	51.349915	62.822516
1880.376273	57.499610	62.827521
1879.822052	51.811586	62.832526
1879.273091	52.466506	62.837530
1878.515473	62.530671	62.842535
1878.557712	42.863539	62.847540
1877.459240	55.448055	62.852545
1876.395275	61.803162	62.857550
1876.068532	53.054568	62.862554
1875.327370	56.253549	62.867559
1874.747682	54.339884	62.872564
1873.497776	50.656152	62.877569
1873.093613	52.205824	62.882574
1872.838333	48.425666	62.887578
1872.038463	61.587220	62.892583
1872.004450	46.084113	62.897588
1870.978652	48.178744	62.902593
1869.821880	59.594595	62.907598
1869.505596	53.685876	62.912602
1868.778365	68.803846	62.917607
1868.250516	46.868219	62.922612
1867.275933	53.529240	62.927617
1866.460260	47.132141	62.932622
1866.196361	52.075058	62.937626
1865.827159	56.055456	62.942631
1865.142560	60.111164	62.947636
1864.010535	59.611357	62.952641
1863.268943	47.382242	62.957646
1862.907573	49.462836	62.962650
1862.192192	55.385723	62.967655
1861.301121	40.092824	62.972660
1860.587105	52.047044	62.977665
1859.949242	53.140263	62.982670
1859.472780	43.603360	62.987674
1859.175299	58.388168	62.992679
1858.534134	47.696333	62.997684
1857.507209	60.979093	63.002689
1857.011371	48.463387	63.007694
1856.608562	53.010490	63.012698
1855.417964	53.023011	63.017703
1854.774995	56.909692	63.022708
1854.212377	46.057161	63.027713
1853.516061	50.532602	63.032718
1853.290029	48.526519	63.037722
1852.057107	57.343159	63.042727
1851.083782	44.849664	63.047732
1850.525956	59.727849	63.052737
1850.179144	52.863662	63.057742
1850.245576	52.517320	63.062746
1849.270918	47.660852	63.067751
1848.414230	51.311823	63.072756
1847.339967	45.608621	63.077761
1847.162295	49.345728	63.082766
1846.569490	51.929828	63.087770
1845.540398	63.027386	63.092775
1844.818315	57.466944	63.097780
1844.243142	63.208310	63.102785
1843.424918	58.390075	63.107790
1843.488377	52.592941	63.112794
1842.151044	43.702072	63.117799
1841.429756	54.380182	63.122804
1840.807689	56.551059	63.127809
1840.180396	47.361369	63.132814
1840.114447	51.025545	63.137818
1839.374295	48.624885	63.142823
1838.709884	55.254008	63.147828
1838.024181	46.253359	63.152833
1837.178779	54.677323	63.157838
1836.301883	46.139098	63.162842
1835.282160	58.704816	63.167847
1834.698801	49.539688	63.172852
1834.132830	41.403081	63.177857
1833.835291	50.134265	63.182862
1833.811324	52.393086	63.187866
1832.076284	58.446358	63.192871
1831.533289	42.257724	63.197876
1831.289681	52.629758	63.202881
1830.500984	57.299639	63.207886
1830.208661	52.541397	63.212890
1828.900683	51.612252	63.217895
1828.190493	46.198158	63.222900
1827.775240	47.331725	63.227905
1827.268174	51.989998	63.232910
1827.096087	47.302547	63.237914
1825.669731	48.517830	63.242919
1825.000290	54.778765	63.247924
1824.561445	48.758638	63.252929
1823.891141	44.517716	63.257934
1823.303452	31.414256	63.262938
1822.039997	60.145382	63.267943
1821.552289	41.100134	63.272948
1821.212606	49.043265	63.277953
1820.655255	54.671420	63.282958
1820.302926	42.596545	63.287962
1819.027509	45.334777	63.292967
1818.725651	50.706326	63.297972
1818.303584	44.171053	63.302977
1817.291557	52.112150	63.307982
1816.092792	38.260520	63.312986
1815.151457	54.170957	63.317991
1815.080063	44.334786	63.322996
1814.652997	42.903078	63.328001
1814.331357	43.433607	63.333006
1814.152152	48.312615	63.338010
1812.938585	46.356132	63.343015
1812.090958	47.805932	63.348020
1811.547618	41.587950	63.353025
1810.342239	39.696397	63.358030
1809.925507	39.420475	63.363034
1808.955835	50.442368	63.368039
1808.620151	51.128085	63.373044
1808.557298	56.341839	63.378049
1806.995038	52.316679	63.383054
1806.659416	36.746379	63.388058
1805.760451	49.497913	63.393063
1805.929350	43.739231	63.398068
1805.457349	42.027669	63.403073
1803.884887	57.864882	63.408078
1803.298963	42.835773	63.413082
1802.951657	51.822431	63.418087
1802.010896	45.852057	63.423092
1801.106919	45.721319	63.428097
1800.201242	48.796639	63.433102
1800.009988	45.217625	63.438106
1799.204899	53.225208	63.443111
1799.020156	46.002577	63.448116
1798.369163	48.132326	63.453121
1797.255007	54.328279	63.458126
1796.854013	41.456932	63.463130
1796.034498	44.610029	63.468135
1795.617714	48.829788	63.473140
1794.723450	48.968733	63.478145
1794.196583	52.715568	63.483150
1793.704263	47.027201	63.488154
1793.125346	56.269830	63.493159
1792.055948	50.053394	63.498164
1791.534548	43.666360	63.503169
1790.816771	51.901340	63.508174
1790.539924	48.071005	63.513178
1789.359078	43.479109	63.518183
1788.286779	38.594024	63.523188
1787.829405	45.898288	63.528193
1787.371155	55.777734	63.533198
1787.423450	45.716929	63.538202
1786.560430	40.254586	63.543207
1785.560831	46.498576	63.548212
1784.846831	39.728992	63.553217
1784.398052	44.598774	63.558222
1783.976261	32.828247	63.563226
1782.763080	56.174250	63.568231
1781.950973	47.605260	63.573236
1781.962140	42.032469	63.578241
1781.080149	52.930065	63.583246
1780.303138	44.670878	63.588250
1779.062596	47.343669	63.593255
1778.448982	37.123712	63.598260
1778.394350	41.714867	63.603265
1777.557632	52.442855	63.608270
1777.338272	36.783140	63.613274
1776.391813	40.949832	63.618279
1775.459696	47.020690	63.623284
1774.902833	44.098956	63.628289
1774.314050	50.375473	63.633294
1774.263713	39.756990	63.638298
1772.717897	52.428347	63.643303
1772.155131	47.897561	63.648308
1771.887488	37.638429	63.653313
1771.190613	51.657220	63.658318
1770.204421	39.616801	63.663322
1769.282222	46.264798	63.668327
1768.787793	43.284267	63.673332
1768.802714	50.053079	63.678337
1768.023892	45.263310	63.683342
1767.289915	37.812542	63.688346
1766.164784	43.600258	63.693351
1765.630315	45.971691	63.698356
1765.459421	47.053844	63.703361
1764.271432	52.362715	63.708366
1763.669639	46.089376	63.713370
1762.990460	39.572876	63.718375
1762.563463	45.115681	63.723380
1762.253998	35.462407	63.728385
1760.757024	50.172791	63.733390
1760.226125	44.058497	63.738394
1759.758242	41.934726	63.743399
1759.055815	46.426926	63.748404
1759.091633	44.532223	63.753409
1758.041946	54.847785	63.758414
1757.412953	48.797952	63.763418
1756.786260	54.187983	63.768423
1755.614405	55.676682	63.773428
1755.329670	48.362710	63.778433
1754.651696	59.975352	63.783438
1754.025217	51.383196	63.788442
1752.990400	56.008612	63.793447
1751.908913	50.546286	63.798452
1751.420222	54.504674	63.803457
1750.755634	53.944867	63.808462
1750.507970	50.154055	63.813466
1750.142134	47.627743	63.818471
1749.695368	48.991820	63.823476
1749.109955	45.968976	63.828481
1747.713539	53.367202	63.833486
1747.474674	48.064347	63.838490
1746.773907	53.242228	63.843495
1745.914170	53.131290	63.848500
1745.404323	41.311678	63.853505
1744.692135	56.971281	63.858510
1744.205247	49.533308	63.863514
1743.038007	52.268587	63.868519
1742.215459	48.059753	63.873524
1741.814382	51.097523	63.878529
1741.023570	53.514408	63.883534
1740.840594	39.381644	63.888538
1740.475041	56.354918	63.893543
1739.443172	44.854749	63.898548
1738.685254	47.178103	63.903553
1738.034884	53.759284	63.908558
1737.508732	49.284190	63.913562
1736.407290	48.131486	63.918567
1735.745101	47.774720	63.923572
1735.439458	51.689844	63.928577
1734.926759	53.573726	63.933582
1734.213533	46.023480	63.938586
1733.423477	48.602664	63.943591
1732.891449	52.435480	63.948596
1732.406510	49.565407	63.953601
1730.952347	50.856117	63.958606
1730.426759	44.945980	63.963610
1730.087007	52.078615	63.968615
1729.403900	50.518863	63.973620
1729.243472	37.052694	63.978625
1727.821550	54.805580	63.983630
1727.033766	47.779663	63.988634
1726.338449	48.582432	63.993639
1726.244722	52.771388	63.998644
1725.939708	45.820171	64.003649
1724.989585	52.332277	64.008654
1724.184088	50.416670	64.013658
1723.709305	44.635654	64.018663
1722.859222	56.835426	64.023668
1722.117034	54.105558	64.028673
1721.274511	59.837369	64.033678
1720.554061	45.315335	64.038682
1720.229917	51.830510	64.043687
1719.638159	53.015782	64.048692
1719.178705	49.512491	64.053697
1717.895358	55.710117	64.058702
1717.432509	46.172667	64.063706
1716.809344	47.107474	64.068711
1716.418365	49.870844	64.073716
1715.512658	47.602170	64.078721
1714.455261	54.552344	64.083726
1714.450008	46.509624	64.088730
1713.897628	52.699948	64.093735
1713.135088	44.211420	64.098740
1712.566942	50.060489	64.103745
1711.480505	53.192933	64.108750
1711.260645	49.640549	64.113754
1709.940468	46.496318	64.118759
1709.480102	46.910129	64.123764
1708.520460	47.504166	64.128769
1707.918614	55.969895	64.133774
1707.840090	43.356419	64.138778
1707.377800	48.559501	64.143783
1706.309327	51.876742	64.148788
1705.567084	51.228363	64.153793
1705.028607	58.156036	64.158798
1704.814196	43.255601	64.163802
1703.643653	54.597998	64.168807
1702.988070	52.545051	64.173812
1702.653828	50.185608	64.178817
1701.910015	58.158251	64.183822
1700.808081	47.610624	64.188826
1699.982726	61.080589	64.193831
1699.205998	58.048723	64.198836
1698.888522	43.970443	64.203841
1698.639023	56.150509	64.208846
1698.269585	51.828717	64.213850
1697.054432	53.171362	64.218855
1696.438574	54.977025	64.223860
1696.102522	54.763996	64.228865
1695.031787	54.803279	64.233870
1693.928691	50.448225	64.238874
1693.546258	60.243101	64.243879
1692.655010	57.417077	64.248884
1692.747761	41.316736	64.253889
1692.010957	59.875397	64.258894
1691.387397	47.909866	64.263898
1690.428055	55.692830	64.268903
1689.756979	57.945637	64.273908
1689.431419	49.936453	64.278913
1687.983355	54.466694	64.283918
1687.660191	46.561205	64.288922
1687.366714	52.084387	64.293927
1686.902027	60.399030	64.298932
1686.056997	59.686563	64.303937
1684.885829	62.269535	64.308942
1684.361759	56.808574	64.313946
1683.671445	50.352209	64.318951
1683.384224	53.863885	64.323956
1682.959931	56.916389	64.328961
1681.800583	56.540845	64.333966
1681.238568	66.961888	64.338970
1680.819072	63.376564	64.343975
1679.707045	52.218721	64.348980
1679.062862	44.867252	64.353985
1678.311756	55.381400	64.358990
1677.966178	55.376456	64.363994
1677.737025	51.073383	64.368999
1676.494625	52.961233	64.374004
1676.006637	45.067738	64.379009
1675.222597	55.801573	64.384014
1674.652104	46.798450	64.389018
1674.050638	43.722986	64.394023
1673.170210	53.891842	64.399028
1672.735454	44.264793	64.404033
1671.864357	54.597739	64.409038
1671.551857	55.443785	64.414042
1670.345038	45.750157	64.419047
1669.700226	61.162538	64.424052
1669.487892	47.550084	64.429057
1668.813643	49.790784	64.434062
1668.337055	56.349103	64.439066
1667.215561	52.233515	64.444071
1666.345329	53.229659	64.449076
1666.211803	56.896684	64.454081
1665.385621	57.635108	64.459086
1664.870780	42.028664	64.464090
1664.115428	44.179752	64.469095
1663.151301	50.176885	64.474100
1663.229013	45.033476	64.479105
1661.862159	45.583415	64.484110
1661.433259	52.608796	64.489114
1660.717673	45.476824	64.494119
1660.376744	57.130546	64.499124
1659.802060	47.737028	64.504129
1658.599996	53.358821	64.509134
1657.944886	52.770727	64.514138
1657.556061	42.579750	64.519143
1656.865551	51.529476	64.524148
1655.727913	42.195434	64.529153
1654.928817	50.441779	64.534158
1654.398983	56.369925	64.539162
1654.243118	50.415263	64.544167
1654.013201	49.814813	64.549172
1653.285640	47.218256	64.554177
1651.933014	48.721525	64.559182
1651.153368	54.864389	64.564186
1650.981086	43.973571	64.569191
1650.215473	66.132090	64.574196
1649.279537	46.331829	64.579201
1648.444803	59.558876	64.584206
1648.418201	49.084860	64.589210
1648.071191	51.361883	64.594215
1646.918915	51.269068	64.599220
1645.948183	34.530334	64.604225
1645.258585	42.806587	64.609230
1645.199916	46.756594	64.614234
1644.355296	53.256693	64.619239
1643.157824	47.773424	64.624244
1643.000971	47.683312	64.629249
1642.558845	48.124198	64.634254
1641.714791	46.337741	64.639258
1641.168992	44.231103	64.644263
1640.060428	47.562621	64.649268
1639.878144	47.500203	64.654273
1639.080955	51.752032	64.659278
1637.931065	43.187883	64.664282
1637.331424	40.071141	64.669287
1636.382523	62.408576	64.674292
1636.312208	50.467127	64.679297
1635.668073	56.391358	64.684302
1635.613644	46.468941	64.689306
1634.687115	44.243027	64.694311
1633.650549	47.260350	64.699316
1633.199999	44.359606	64.704321
1632.259961	42.129533	64.709326
1631.344228	42.213600	64.714330
1630.389546	40.451031	64.719335
1630.135753	51.240971	64.724340
1630.100786	37.299174	64.729345
1629.462347	48.301602	64.734350
1628.375632	47.238064	64.739354
1627.792484	49.628295	64.744359
1627.128965	47.716972	64.749364
1626.867486	44.076599	64.754369
1625.447774	58.175561	64.759374
1624.964578	45.158058	64.764378
1624.761624	48.493931	64.769383
1623.751207	42.433781	64.774388
1622.940719	43.374718	64.779393
1621.965509	53.549182	64.784398
1621.738159	44.792743	64.789402
1621.378033	45.925467	64.794407
1620.899542	51.263592	64.799412
1619.859653	43.943474	64.804417
1619.169789	50.951974	64.809422
1618.441006	47.999248	64.814426
1618.103357	41.173082	64.819431
1616.599683	47.856738	64.824436
1616.531287	36.131031	64.829441
1615.591107	46.706760	64.834446
1615.325882	47.532685	64.839450
1614.994416	43.770976	64.844455
1613.798056	51.888069	64.849460
1613.371263	47.247418	64.854465
1612.646531	39.443594	64.859470
1611.861957	48.414578	64.864474
1611.013111	41.750052	64.869479
1610.350470	52.291152	64.874484
1610.187312	44.421757	64.879489
1609.475366	39.627729	64.884494
1608.507013	43.902027	64.889498
1607.806751	54.330841	64.894503
1607.254967	57.145004	64.899508
1607.057959	46.543535	64.904513
1605.565876	55.716816	64.909518
1604.835870	45.409756	64.914522
1604.682949	48.742411	64.919527
1604.027159	63.852208	64.924532
1603.667863	46.409241	64.929537
1602.576774	47.309615	64.934542
1601.946479	58.580405	64.939546
1601.462019	56.295303	64.944551
1600.662280	51.080005	64.949556
1599.792678	48.025086	64.954561
1599.104311	51.051751	64.959566
1598.614997	48.685425	64.964570
1598.110866	51.384789	64.969575
1597.467847	56.504645	64.974580
1596.553894	55.476746	64.979585
1595.482096	50.829775	64.984590
1595.200238	56.423654	64.989594
1595.053685	51.366337	64.994599
1594.208156	54.113639	64.999604
1593.673098	45.327251	65.004609
1592.893465	56.285894	65.009614
1592.074623	52.768772	65.014618
1591.382753	45.639363	65.019623
1590.238081	58.950357	65.024628
1589.776375	48.950736	65.029633
1589.316730	48.249606	65.034638
1588.921279	53.979798	65.039642
1588.499589	50.415344	65.044647
1587.320141	48.773654	65.049652
1586.996631	42.372580	65.054657
1586.273402	52.369829	65.059662
1585.262034	51.899857	65.064666
1584.352645	40.353505	65.069671
1583.749547	58.346907	65.074676
1583.269393	45.287936	65.079681
1582.777799	59.499632	65.084686
1582.546953	58.621806	65.089690
1582.029106	53.629793	65.094695
1580.795696	54.360412	65.099700
1580.426373	46.615236	65.104705
1579.674452	54.191818	65.109710
1578.289991	49.130935	65.114714
1577.901552	49.870791	65.119719
1577.525688	52.048333	65.124724
1577.205023	48.822626	65.129729
1576.473939	49.066598	65.134734
1575.254143	44.764836	65.139738
1574.843026	45.732211	65.144743
1574.319787	48.953406	65.149748
1574.123638	49.539713	65.154753
1573.078283	51.032044	65.159758
1572.208468	50.422897	65.164762
1571.741830	47.988322	65.169767
1570.650659	48.770456	65.174772
1570.214695	45.809064	65.179777
1569.109844	46.229116	65.184782
1568.877262	48.637768	65.189786
1568.364628	49.482510	65.194791
1567.843859	49.618953	65.199796
1567.439678	50.664072	65.204801
1566.027925	51.752601	65.209806
1566.018536	36.956818	65.214810
1565.115613	44.363437	65.219815
1563.857227	53.363991	65.224820
1563.783478	48.550564	65.229825
1563.098396	49.351750	65.234830
1562.473833	54.066577	65.239834
1561.398335	51.077502	65.244839
1560.344749	52.768254	65.249844
1560.424847	46.410278	65.254849
1559.931446	51.684551	65.259854
1559.392745	45.516360	65.264858
1558.507737	41.361673	65.269863
1557.226888	44.758444	65.274868
1556.756719	44.024301	65.279873
1556.678084	43.516510	65.284878
1555.776045	40.362690	65.289882
1555.109696	43.879425	65.294887
1554.289687	45.570909	65.299892
1553.743810	42.860362	65.304897
1553.345022	48.211060	65.309902
1552.202197	52.984587	65.314906
1551.536193	41.727566	65.319911
1550.743000	47.514653	65.324916
1550.822920	41.418468	65.329921
1550.187766	47.364937	65.334926
1549.311885	40.023524	65.339930
1548.784656	43.228011	65.344935
1548.197174	47.720914	65.349940
1547.229781	40.009288	65.354945
1546.208523	36.953260	65.359950
1545.283686	39.891361	65.364954
1545.254465	47.080308	65.369959
1544.320654	45.003812	65.374964
1544.076156	46.286896	65.379969
1543.247235	57.234458	65.384974
1542.383728	45.486877	65.389978
1542.440166	48.893492	65.394983
1541.388902	43.558924	65.399988
1540.398311	50.586842	65.404993
1539.918688	48.745664	65.409998
1539.377255	50.560033	65.415002
1538.129989	45.545179	65.420007
1537.327267	51.608161	65.425012
1537.256969	34.761093	65.430017
1536.616725	46.651595	65.435022
1536.184016	48.231079	65.440026
1536.001345	45.857038	65.445031
1534.677558	45.728453	65.450036
1533.870429	44.844443	65.455041
1533.532929	37.486868	65.460046
1532.558751	43.313756	65.465050
1531.684306	45.758180	65.470055
1530.888895	50.112250	65.475060
1530.631779	48.204178	65.480065
1530.178983	44.248886	65.485070
1529.036758	55.228891	65.490074
1528.488942	37.607771	65.495079
1527.648345	44.042604	65.500084
1527.521671	41.869390	65.505089
1527.312763	45.751809	65.510094
1526.089317	43.908994	65.515098
1525.468869	43.258659	65.520103
1524.740191	52.061516	65.525108
1523.951297	35.429564	65.530113
1523.219017	34.806463	65.535118
1522.264758	41.593655	65.540122
1521.902362	41.589829	65.545127
1521.338736	37.415622	65.550132
1521.263772	43.168999	65.555137
1520.092348	44.506352	65.560142
1519.723149	40.544086	65.565146
1519.425183	46.571010	65.570151
1518.068864	46.944317	65.575156
1517.130189	38.860731	65.580161
1516.941340	42.782538	65.585166
1516.054488	48.660208	65.590170
1515.381653	40.569066	65.595175
1514.601832	47.506729	65.600180
1514.027643	35.178633	65.605185
1513.502261	38.269296	65.610190
1512.908950	41.889544	65.615194
1511.928912	40.058515	65.620199
1511.186433	40.091439	65.625204
1511.050200	44.356526	65.630209
1510.362105	40.809198	65.635214
1509.786665	45.297040	65.640218
1508.831854	47.475137	65.645223
1508.291135	52.113574	65.650228
1507.632773	40.768627	65.655233
1506.399936	44.730195	65.660238
1505.488723	44.179687	65.665242
1505.218291	38.320523	65.670247
1504.582700	48.964564	65.675252
1504.349963	35.636085	65.680257
1503.905008	50.337076	65.685262
1503.114183	57.910397	65.690266
1502.467328	49.025114	65.695271
1501.416224	43.908146	65.700276
1501.205659	37.948011	65.705281
1500.367105	39.675571	65.710286
1499.493001	48.734919	65.715290
1499.046839	44.190407	65.720295
1498.199651	51.572421	65.725300
1497.816268	46.231074	65.730305
1496.905219	42.416422	65.735310
1496.136772	39.101053	65.740314
1495.903318	43.014180	65.745319
1495.211938	53.244491	65.750324
1493.690012	51.734540	65.755329
1493.301553	39.832646	65.760334
1492.608232	46.818064	65.765338
1492.488094	40.375227	65.770343
1491.915083	43.156514	65.775348
1491.173622	39.947238	65.780353
1490.673423	40.378455	65.785358
1489.486473	55.703549	65.790362
1489.367642	40.458414	65.795367
1488.323943	46.608587	65.800372
1487.706643	35.861067	65.805377
1487.144527	43.260849	65.810382
1486.359568	43.328914	65.815386
1485.817802	39.758338	65.820391
1484.594858	45.154871	65.825396
1483.955299	45.201405	65.830401
1483.675044	40.018706	65.835406
1483.239575	50.992049	65.840410
1483.150756	47.984963	65.845415
1481.975945	35.708182	65.850420
1481.483104	36.207614	65.855425
1480.411792	47.059670	65.860430
1479.578913	51.545859	65.865434
1479.288003	38.324395	65.870439
1478.684626	45.008530	65.875444
1477.760863	39.552810	65.880449
1476.674565	37.169433	65.885454
1476.151901	45.040738	65.890458
1475.597735	42.325220	65.895463
1475.465614	44.136047	65.900468
1474.968444	40.063248	65.905473
1473.786200	44.116132	65.910478
1473.299295	44.352862	65.915482
1473.089861	34.884018	65.920487
1471.524015	46.934251	65.925492
1470.923922	46.212888	65.930497
1470.740509	41.990881	65.935502
1469.800580	45.601576	65.940506
1469.569422	40.518303	65.945511
1468.227064	47.152742	65.950516
1467.876731	38.390652	65.955521
1467.449465	43.834186	65.960526
1466.636112	51.111488	65.965530
1465.610475	40.698516	65.970535
1464.815273	49.027857	65.975540
1464.348538	43.565731	65.980545
1464.224656	52.759729	65.985550
1463.640208	43.889774	65.990554
1462.809954	42.689358	65.995559
1461.988913	50.489826	66.000564
1461.739983	42.577319	66.005569
1460.779466	43.974212	66.010574
1459.561369	42.980512	66.015578
1458.943541	33.228093	66.020583
1458.569112	42.401985	66.025588
1458.221967	46.837783	66.030593
1457.247787	39.196659	66.035598
1456.443090	55.780847	66.040602
1455.920204	41.769976	66.045607
1455.100325	49.732677	66.050612
1454.921951	47.835752	66.055617
1454.327548	48.524787	66.060622
1452.972885	52.934652	66.065626
1452.835944	39.748643	66.070631
1452.061877	47.800251	66.075636
1451.736608	49.509321	66.080641
1450.763835	45.389124	66.085646
1449.722812	43.582004	66.090650
1449.486962	46.279749	66.095655
1448.841329	42.747766	66.100660
1447.827808	42.711830	66.105665
1447.572542	53.123553	66.110670
1446.806753	43.093467	66.115674
1446.593076	42.597683	66.120679
1445.176831	54.830726	66.125684
1444.639450	47.340939	66.130689
1444.485172	43.068575	66.135694
1443.646655	45.877879	66.140698
1442.638181	37.012257	66.145703
1441.423558	35.958093	66.150708
1441.096785	46.805355	66.155713
1440.914762	41.780504	66.160718
1440.465780	39.314767	66.165722
1440.078452	39.575098	66.170727
1438.728751	47.841200	66.175732
1438.402356	43.861107	66.180737
1437.950478	34.011358	66.185742
1436.640315	49.387582	66.190746
1435.824070	38.370519	66.195751
1435.209804	46.332079	66.200756
1435.202440	34.699198	66.205761
1434.413462	36.340055	66.210766
1433.161446	37.472647	66.215770
1432.936744	41.308696	66.220775
1432.133219	48.885624	66.225780
1431.944639	49.470738	66.230785
1430.955763	46.392265	66.235790
1430.027954	40.729060	66.240794
1429.800998	38.064041	66.245799
1429.147500	45.968763	66.250804
1428.424600	41.193880	66.255809
1427.906884	40.599776	66.260814
1426.975398	41.779189	66.265818
1426.646603	34.655207	66.270823
1425.080280	45.117631	66.275828
1424.543399	45.671380	66.280833
1424.406323	46.379188	66.285838
1423.929810	42.916519	66.290842
1423.337903	48.709488	66.295847
1422.177201	48.075670	66.300852
1421.543214	50.658517	66.305857
1421.187001	42.304202	66.310862
1419.868181	55.532543	66.315866
1419.437102	39.067678	66.320871
1418.563496	43.178753	66.325876
1417.998185	46.537540	66.330881
1417.943664	41.861413	66.335886
1417.668360	61.009024	66.340890
1416.560129	37.998983	66.345895
1415.965940	48.535535	66.350900
1415.047135	52.327385	66.355905
1414.256710	40.831588	66.360910
1412.873311	50.924341	66.365914
1412.771986	36.550030	66.370919
1412.514146	45.375828	66.375924
1411.607937	44.379881	66.380929
1411.774945	47.606495	66.385934
1410.547124	48.974937	66.390938
1409.786149	42.507825	66.395943
1409.237626	42.188266	66.400948
1408.483547	43.885081	66.405953
1407.635808	43.013876	66.410958
1406.895010	50.025781	66.415962
1406.925203	35.441343	66.420967
1406.114249	42.719849	66.425972
1405.170931	42.204441	66.430977
1404.471095	38.640089	66.435982
1403.683919	38.437311	66.440986
1403.630399	32.253543	66.445991
1402.622835	50.355387	66.450996
1401.746450	42.714511	66.456001
1401.246794	37.230829	66.461006
1400.505269	48.497239	66.466010
1399.416734	24.998425	66.471015
1398.849560	45.559552	66.476020
1398.157341	45.384257	66.481025
1397.994727	38.322167	66.486030
1397.699845	38.826415	66.491034
1396.959888	32.863722	66.496039
1395.621076	40.765428	66.501044
1395.355231	37.586229	66.506049
1395.042596	38.954269	66.511054
1394.032015	41.880821	66.516058
1393.143366	40.503641	66.521063
1392.635365	36.550850	66.526068
1391.960700	43.307828	66.531073
1390.724215	38.849554	66.536078
1389.948315	47.101729	66.541082
1389.874214	45.448417	66.546087
1389.440304	40.238122	66.551092
1389.109646	34.834807	66.556097
1388.430940	30.379327	66.561102
1387.259211	35.736218	66.566106
1386.879144	37.621152	66.571111
1386.231155	23.223380	66.576116
1385.057911	44.543134	66.581121
1384.687126	33.612971	66.586126
1383.697887	30.357970	66.591130
1383.692001	35.092740	66.596135
1382.582557	42.858648	66.601140
1381.917393	37.773422	66.606145
1381.661860	30.169476	66.611150
1381.089363	37.823218	66.616154
1380.289121	37.158925	66.621159
1379.186395	39.746912	66.626164
1378.614430	42.271025	66.631169
1378.313238	31.318764	66.636174
1377.139270	43.297280	66.641178
1376.482082	34.847331	66.646183
1376.125020	41.597975	66.651188
1375.314648	45.787315	66.656193
1375.325522	31.948660	66.661198
1374.207014	49.828462	66.666202
1373.360911	39.976747	66.671207
1372.825572	35.399137	66.676212
1372.142315	44.781392	66.681217
1371.172452	47.020273	66.686222
1370.378429	42.600473	66.691226
1370.322379	28.491779	66.696231
1369.238538	42.881190	66.701236
1369.145918	43.268136	66.706241
1368.437770	31.497527	66.711246
1367.305686	43.992908	66.716250
1366.976987	36.941458	66.721255
1366.367412	38.254210	66.726260
1365.522750	41.170164	66.731265
1364.938509	36.343301	66.736270
1364.229339	41.032189	66.741274
1363.738657	30.836992	66.746279
1362.545601	38.449049	66.751284
1361.946418	32.724172	66.756289
1361.442721	45.360919	66.761294
1360.903566	37.956595	66.766298
1360.664277	35.555305	66.771303
1359.522549	49.121342	66.776308
1358.650968	45.156975	66.781313
1358.514552	35.665506	66.786318
1357.307850	41.704447	66.791322
1357.224313	32.059502	66.796327
1356.133763	43.132258	66.801332
1355.248544	36.308049	66.806337
1355.116318	23.572309	66.811342
1354.361355	32.634817	66.816346
1353.627110	35.727174	66.821351
1352.585938	35.252572	66.826356
1351.985025	44.610701	66.831361
1351.985770	36.202811	66.836366
1350.999423	37.597541	66.841370
1350.468816	39.618371	66.846375
1349.737647	40.560972	66.851380
1348.966635	28.116007	66.856385
1348.906446	30.831558	66.861390
1347.554025	43.940685	66.866394
1346.800536	33.475052	66.871399
1346.311848	41.429273	66.876404
1345.979804	38.282681	66.881409
1345.054120	35.843869	66.886414
1344.244645	34.610231	66.891418
1343.737163	36.961680	66.896423
1343.417584	32.294586	66.901428
1342.499939	40.014245	66.906433
1341.469765	32.300084	66.911438
1340.884100	45.281006	66.916442
1340.773830	29.671874	66.921447
1339.632654	40.790527	66.926452
1338.922833	39.843804	66.931457
1338.475050	32.346119	66.936462
1337.927635	43.171690	66.941466
1337.233362	39.754700	66.946471
1336.194844	46.601075	66.951476
1335.549144	41.495422	66.956481
1335.260127	43.231855	66.961486
1334.963760	43.089830	66.966490
1333.743555	37.050555	66.971495
1333.176402	46.203058	66.976500
1332.345519	30.408891	66.981505
1332.165973	33.627517	66.986510
1330.458306	46.662251	66.991514
1330.314410	47.309650	66.996519
1329.280425	36.830274	67.001524
1329.261918	38.999912	67.006529
1329.135569	34.753082	67.011534
1328.126603	32.242367	67.016538
1327.440746	30.402487	67.021543
1326.399504	37.769659	67.026548
1325.707682	46.839489	67.031553
1325.580906	33.328637	67.036558
1324.454587	44.435474	67.041562
1323.651219	46.526482	67.046567
1323.313059	44.673896	67.051572
1322.743314	48.520658	67.056577
1321.992823	39.298703	67.061582
1321.052545	44.344451	67.066586
1320.809868	37.265142	67.071591
1320.395071	41.850471	67.076596
1319.292999	39.212644	67.081601
1318.372638	40.134873	67.086606
1317.704928	45.575655	67.091610
1317.569525	40.191766	67.096615
1316.803422	36.076614	67.101620
1315.812633	43.962445	67.106625
1315.372831	41.839031	67.111630
1315.006894	54.217355	67.116634
1313.990912	37.085475	67.121639
1313.413791	39.774414	67.126644
1312.631825	41.757949	67.131649
1312.494053	35.013604	67.136654
1311.055547	34.706267	67.141658
1310.103073	40.372086	67.146663
1309.606457	40.083718	67.151668
1309.108140	47.333041	67.156673
1308.994379	40.152815	67.161678
1308.503409	36.273026	67.166682
1307.591307	34.085945	67.171687
1306.885988	42.060422	67.176692
1306.074383	40.674178	67.181697
1305.453857	35.439962	67.186702
1304.487387	35.724590	67.191706
1303.813917	36.982863	67.196711
1303.449144	25.955583	67.201716
1303.203051	31.535895	67.206721
1302.142037	28.241881	67.211726
1301.063117	37.218724	67.216730
1300.594372	38.742475	67.221735
1300.554264	36.468786	67.226740
1299.441995	40.846488	67.231745
1298.778457	35.767338	67.236750
1298.227256	44.510477	67.241754
1297.518058	36.746876	67.246759
1297.223489	34.624028	67.251764
1296.091564	44.039788	67.256769
1295.844014	35.119480	67.261774
1294.878945	57.547823	67.266778
1294.405922	27.791966	67.271783
1293.520689	27.787730	67.276788
1292.595446	48.760589	67.281793
1292.404982	45.053781	67.286798
1291.379044	50.698178	67.291802
1290.701557	46.365525	67.296807
1290.393063	39.340838	67.301812
1289.995491	37.792579	67.306817
1289.298599	31.894036	67.311822
1288.043217	32.680322	67.316826
1287.371828	34.622628	67.321831
1286.956643	36.230900	67.326836
1286.199929	38.593605	67.331841
1285.654281	34.661018	67.336846
1284.613755	43.898255	67.341850
1284.061992	47.382639	67.346855
1283.839966	36.375234	67.351860
1283.059189	37.431391	67.356865
1282.026761	48.676271	67.361870
1281.540949	47.660832	67.366874
1281.012332	35.298767	67.371879
1280.685416	39.491678	67.376884
1279.632723	41.819451	67.381889
1278.887551	38.525684	67.386894
1278.272556	44.303424	67.391898
1277.842108	37.481048	67.396903
1277.018633	41.330318	67.401908
1275.963179	42.307157	67.406913
1275.503798	31.012665	67.411918
1274.932814	47.567588	67.416922
1274.651237	36.984370	67.421927
1273.956158	29.696327	67.426932
1272.623767	42.059592	67.431937
1272.324541	29.107580	67.436942
1271.887590	38.982086	67.441946
1271.626384	29.138338	67.446951
1270.491371	41.071271	67.451956
1269.481019	52.462449	67.456961
1269.163876	35.694111	67.461966
1268.403677	41.627398	67.466970
1267.002746	42.698598	67.471975
1267.074822	39.580794	67.476980
1266.611788	38.821919	67.481985
1266.382509	32.035365	67.486990
1265.098958	35.552540	67.491994
1264.279738	39.883656	67.496999
1263.725523	35.436802	67.502004
1263.374089	40.910875	67.507009
1262.832820	39.155247	67.512014
1261.746695	35.972469	67.517018
1260.898547	30.273021	67.522023
1260.817610	47.757636	67.527028
1259.771522	40.925932	67.532033
1258.973548	35.414035	67.537038
1258.240143	28.709225	67.542042
1257.943138	43.411915	67.547047
1257.666384	40.441038	67.552052
1256.209192	43.299895	67.557057
1255.810342	22.156154	67.562062
1255.374550	35.308772	67.567066
1254.641805	33.828009	67.572071
1254.008577	37.041515	67.577076
1252.862493	48.004871	67.582081
1252.733885	37.999695	67.587086
1252.097942	42.243327	67.592090
1251.152957	47.088007	67.597095
1250.274543	42.747898	67.602100
1249.402110	38.644946	67.607105
1249.406179	30.780559	67.612110
1248.939057	37.545557	67.617114
1248.388070	33.875588	67.622119
1247.325207	25.971143	67.627124
1246.473173	39.301914	67.632129
1246.389450	35.004161	67.637134
1245.130771	50.668715	67.642138
1244.532363	39.593442	67.647143
1244.165233	30.521861	67.652148
1243.787588	43.578513	67.657153
1242.625355	35.782902	67.662158
1241.886306	50.149061	67.667162
1241.249567	46.385501	67.672167
1241.026554	40.698603	67.677172
1239.814555	40.831499	67.682177
1239.299015	38.013710	67.687182
1238.419460	51.620090	67.692186
1238.109744	33.620627	67.697191
1237.858598	32.168934	67.702196
1236.437839	48.269247	67.707201
1236.170912	36.050075	67.712206
1235.666849	32.583948	67.717210
1234.720898	37.204869	67.722215
1233.721135	36.663810	67.727220
1233.189342	40.545550	67.732225
1232.355281	44.115834	67.737230
1232.277843	42.075152	67.742234
1231.795740	38.182932	67.747239
1231.131449	34.122578	67.752244
1229.987706	41.826188	67.757249
1229.543923	37.480046	67.762254
1228.898140	40.693978	67.767258
1227.424966	45.313595	67.772263
1227.314517	31.984662	67.777268
1226.631060	48.945383	67.782273
1226.589432	43.434634	67.787278
1226.183441	40.678268	67.792282
1224.833487	40.096715	67.797287
1224.556237	36.121460	67.802292
1223.407679	50.582706	67.807297
1222.616565	40.572510	67.812302
1221.787807	33.108635	67.817306
1221.440884	37.482918	67.822311
1220.941747	29.113542	67.827316
1220.439927	32.243082	67.832321
1220.084616	27.657383	67.837326
1218.829037	40.226059	67.842330
1218.035619	39.319473	67.847335
1217.788537	36.099471	67.852340
1216.641157	32.762462	67.857345
1215.939953	27.151621	67.862350
1215.237597	50.537915	67.867354
1214.588956	33.413907	67.872359
1214.877215	23.471754	67.877364
1213.786106	37.086540	67.882369
1213.376429	34.398569	67.887374
1212.527008	31.700114	67.892378
1211.299146	40.150348	67.897383
1210.657130	39.643863	67.902388
1209.858769	42.582461	67.907393
1209.468575	32.065417	67.912398
1209.261483	39.489193	67.917402
1208.642529	38.110189	67.922407
1207.618978	27.458922	67.927412
1206.673723	48.034451	67.932417
1206.513179	42.522116	67.937422
1206.196072	38.311942	67.942426
1205.249107	36.724921	67.947431
1204.528240	44.897423	67.952436
1203.980220	43.194919	67.957441
1203.118556	43.035586	67.962446
1201.999114	34.086813	67.967450
1201.376495	33.356485	67.972455
1201.221207	44.657417	67.977460
1200.565706	20.072801	67.982465
1199.680325	21.208692	67.987470
1199.239782	33.155766	67.992474
1199.086055	37.141377	67.997479
1197.637178	35.769794	68.002484
1196.727827	33.626469	68.007489
1196.323398	19.969014	68.012494
1195.689876	30.226421	68.017498
1195.383918	44.452743	68.022503
1194.583174	38.753662	68.027508
1193.627080	39.976492	68.032513
1193.549193	25.648968	68.037518
1192.589726	39.422588	68.042522
1191.634829	39.472041	68.047527
1191.108749	29.370832	68.052532
1190.200899	44.211668	68.057537
1190.309570	39.452836	68.062542
1188.836386	50.285321	68.067546
1188.260920	38.257148	68.072551
1187.791932	41.351513	68.077556
1187.209881	46.737699	68.082561
1186.781795	36.154150	68.087566
1185.647481	36.320445	68.092570
1184.508392	43.734766	68.097575
1184.348979	35.931073	68.102580
1183.590788	41.384694	68.107585
1183.380640	29.970171	68.112590
1183.206163	33.228995	68.117594
1181.908982	43.096829	68.122599
1181.574626	43.438655	68.127604
1180.740346	41.005868	68.132609
1180.034292	43.641226	68.137614
1178.983439	50.536923	68.142618
1178.210200	41.074228	68.147623
1178.334483	27.502982	68.152628
1177.322568	41.043688	68.157633
1176.533394	32.212703	68.162638
1175.948031	43.927368	68.167642
1175.153212	46.756609	68.172647
1174.898450	36.101344	68.177652
1173.526395	35.722018	68.182657
1172.826705	31.247867	68.187662
1172.207745	31.366893	68.192666
1171.987826	36.022161	68.197671
1171.956202	30.858316	68.202676
1171.013655	39.651096	68.207681
1170.155911	36.961862	68.212686
1169.750459	45.404307	68.217690
1168.588193	35.517821	68.222695
1167.705692	30.125054	68.227700
1167.078554	37.098427	68.232705
1166.770704	30.762756	68.237710
1166.419264	34.142761	68.242714
1165.447602	44.394042	68.247719
1164.610274	41.155968	68.252724
1164.022276	45.795670	68.257729
1163.799165	36.117760	68.262734
1162.789076	31.577871	68.267738
1161.819246	37.235458	68.272743
1161.313327	35.141514	68.277748
1160.700360	47.303672	68.282753
1160.184026	35.617747	68.287758
1159.223754	39.819948	68.292762
1158.404018	41.552506	68.297767
1158.220961	34.337595	68.302772
1157.919877	36.970043	68.307777
1157.172828	28.239595	68.312782
1156.489562	43.574541	68.317786
1155.770652	36.787039	68.322791
1154.980966	25.825806	68.327796
1153.916473	41.918359	68.332801
1153.515521	38.662918	68.337806
1152.966608	31.815266	68.342810
1152.095005	35.442002	68.347815
1151.364717	44.691433	68.352820
1150.522807	39.241753	68.357825
1149.880103	32.781160	68.362830
1149.665698	45.228410	68.367834
1149.104717	26.360677	68.372839
1148.290999	31.446265	68.377844
1147.314464	35.039233	68.382849
1146.900877	28.056525	68.387854
1146.534037	30.708894	68.392858
1145.361092	45.967199	68.397863
1144.869886	34.669922	68.402868
1144.004112	30.162278	68.407873
1143.846939	33.891408	68.412878
1143.352744	38.889908	68.417882
1141.969922	37.354894	68.422887
1141.618133	37.645885	68.427892
1141.185548	42.145759	68.432897
1140.806696	34.550432	68.437902
1139.449239	36.087844	68.442906
1138.397173	42.815019	68.447911
1138.542287	41.574681	68.452916
1137.812928	36.528127	68.457921
1136.740485	35.777907	68.462926
1136.163661	37.902316	68.467930
1135.536421	40.296504	68.472935
1135.468337	40.260109	68.477940
1134.359004	39.113658	68.482945
1133.624224	31.794134	68.487950
1133.058270	23.657753	68.492954
1132.490403	40.082874	68.497959
1131.993600	31.768342	68.502964
1130.803811	42.410699	68.507969
1130.758296	34.793890	68.512974
1130.091938	42.653399	68.517978
1128.616820	35.114190	68.522983
1128.192116	26.498050	68.527988
1127.594879	32.995190	68.532993
1127.400561	25.578664	68.537998
1126.840865	27.183139	68.543002
1125.494156	38.637309	68.548007
1125.123346	26.969253	68.553012
1124.552520	34.313698	68.558017
1123.784644	34.519498	68.563022
1122.853156	35.719517	68.568026
1122.421248	36.806955	68.573031
1121.824865	37.097433	68.578036
1121.037334	44.211442	68.583041
1120.580003	41.130546	68.588046
1119.931547	41.743104	68.593050
1119.108525	43.860950	68.598055
1118.872550	36.462085	68.603060
1117.606188	42.628878	68.608065
1116.664146	41.938343	68.613070
1116.230562	43.738791	68.618074
1115.779541	32.357866	68.623079
1115.790376	32.807207	68.628084
1114.679888	41.079546	68.633089
1113.790209	45.853974	68.638094
1113.507797	37.667756	68.643098
1112.487741	46.318352	68.648103
1111.641498	39.134828	68.653108
1110.757683	45.573491	68.658113
1110.496567	32.974981	68.663118
1110.209830	38.159667	68.668122
1109.349253	47.767282	68.673127
1108.784162	39.714335	68.678132
1108.189530	49.817356	68.683137
1107.695915	33.712619	68.688142
1106.490365	28.954706	68.693146
1105.803791	37.304683	68.698151
1105.272265	24.205180	68.703156
1104.628228	51.026062	68.708161
1104.060284	37.426168	68.713166
1103.077022	39.312481	68.718170
1102.186417	42.511773	68.723175
1101.973992	33.505496	68.728180
1101.334354	38.834627	68.733185
1101.100056	40.697986	68.738190
1100.201619	37.220513	68.743194
1099.369697	37.534274	68.748199
1098.789624	33.682902	68.753204
1098.012565	46.785749	68.758209
1097.013748	34.566353	68.763214
1096.577271	38.369877	68.768218
1096.037056	45.296325	68.773223
1096.041467	33.202749	68.778228
1094.765324	38.424990	68.783233
1094.029335	41.922945	68.788238
1093.448650	39.651685	68.793242
1092.660992	39.162092	68.798247
1091.775038	36.652407	68.803252
1091.201471	39.697194	68.808257
1091.086610	38.802545	68.813262
1090.653142	34.361759	68.818266
1089.111628	42.693215	68.823271
1088.749485	47.741677	68.828276
1088.184636	42.545973	68.833281
1087.754960	35.468070	68.838286
1086.912994	31.937468	68.843290
1086.115216	31.372221	68.848295
1085.444451	23.965269	68.853300
1084.772744	36.549908	68.858305
1083.798762	26.442723	68.863310
1083.191060	29.910808	68.868314
1082.411647	34.957843	68.873319
1082.315390	35.580329	68.878324
1081.660741	40.284261	68.883329
1081.068311	36.710809	68.888334
1080.056910	33.230817	68.893338
1079.583184	37.876005	68.898343
1079.421556	29.288984	68.903348
1078.039186	36.708929	68.908353
1076.917950	33.271641	68.913358
1076.854353	31.430606	68.918362
1076.307539	34.862200	68.923367
1076.249666	33.009216	68.928372
1074.892539	43.058508	68.933377
1074.225643	31.730862	68.938382
1073.787263	33.577807	68.943386
1072.784321	34.683561	68.948391
1072.006516	28.105724	68.953396
1071.219677	43.263201	68.958401
1070.640751	28.577040	68.963406
1070.522166	29.020163	68.968410
1069.881013	43.052237	68.973415
1069.241742	33.825308	68.978420
1068.225069	28.567461	68.983425
1067.810998	39.387610	68.988430
1067.106556	39.225387	68.993434
1066.004637	23.356217	68.998439
1066.011522	24.837451	69.003444
1065.365167	36.885081	69.008449
1064.409701	26.770229	69.013454
1063.578702	33.440180	69.018458
1062.758305	34.567356	69.023463
1062.769552	25.727345	69.028468
1061.490672	40.513696	69.033473
1060.595745	43.866645	69.038478
1060.480462	28.185838	69.043482
1059.761748	41.046029	69.048487
1059.475503	29.561643	69.053492
1058.354082	40.863313	69.058497
1057.500566	32.222375	69.063502
1057.167352	24.492087	69.068506
1056.671988	31.734654	69.073511
1055.843919	30.324308	69.078516
1054.887597	27.174590	69.083521
1054.139385	41.475995	69.088526
1053.994277	28.316606	69.093530
1053.159113	36.444242	69.098535
1052.413073	44.376364	69.103540
1051.473137	40.557025	69.108545
1050.901667	34.496691	69.113550
1051.009424	28.485983	69.118554
1049.484499	34.622980	69.123559
1049.062944	43.260370	69.128564
1048.624561	40.904985	69.133569
1048.083832	32.196942	69.138574
1047.066832	39.426316	69.143578
1045.966352	38.324225	69.148583
1045.684304	29.185545	69.153588
1045.113843	38.948849	69.158593
1044.610856	42.345095	69.163598
1044.382875	27.363427	69.168602
1043.151183	35.850602	69.173607
1042.505346	26.867568	69.178612
1042.141434	33.545206	69.183617
1041.102676	31.135542	69.188622
1040.506413	35.492743	69.193626
1039.476646	42.361475	69.198631
1039.424297	41.439538	69.203636
1039.061098	47.667664	69.208641
1037.816273	39.019607	69.213646
1037.612651	30.437696	69.218650
1036.847561	30.256748	69.223655
1035.542160	27.459028	69.228660
1034.469794	38.942122	69.233665
1034.256275	28.046956	69.238670
1034.085935	31.506964	69.243674
1033.413259	50.886468	69.248679
1033.037363	39.272850	69.253684
1031.952955	31.305711	69.258689
1031.153574	34.892609	69.263694
1030.856485	38.696041	69.268698
1029.908082	39.274348	69.273703
1029.251131	31.765872	69.278708
1028.609717	30.404680	69.283713
1028.172953	38.683388	69.288718
1028.057928	37.498626	69.293722
1026.946764	42.923294	69.298727
1026.126366	24.598334	69.303732
1025.629744	37.626605	69.308737
1024.226572	45.232805	69.313742
1023.651846	39.332258	69.318746
1022.834372	32.685060	69.323751
1022.485164	27.057701	69.328756
1022.372863	41.540189	69.333761
1021.674515	41.157826	69.338766
1020.971416	31.901649	69.343770
1020.131640	37.428209	69.348775
1019.534583	39.417097	69.353780
1018.960054	30.156234	69.358785
1018.262652	47.535480	69.363790
1017.844837	40.755308	69.368794
1016.549291	28.868584	69.373799
1015.736092	32.504990	69.378804
1015.089313	35.659205	69.383809
1014.680415	37.025257	69.388814
1014.215401	26.958542	69.393818
1013.782918	42.422322	69.398823
1012.974807	35.901362	69.403828
1012.210809	38.602749	69.408833
1011.321238	32.474776	69.413838
1010.961304	37.578080	69.418842
1009.983879	42.767022	69.423847
1009.514157	23.164208	69.428852
1008.746478	28.381270	69.433857
1008.550992	35.363253	69.438862
1007.830667	32.524490	69.443866
1006.704338	37.062227	69.448871
1006.193199	38.185943	69.453876
1005.857848	39.450413	69.458881
1005.012369	37.683329	69.463886
1004.159449	32.976586	69.468890
1003.314980	46.388201	69.473895
1003.076506	20.827486	69.478900
1002.284918	30.793121	69.483905
1001.612914	31.456761	69.488910
1001.213389	32.285191	69.493914
1000.246224	38.727682	69.498919
999.840508	29.775835	69.503924
998.755276	27.789876	69.508929
997.944744	25.072697	69.513934
997.850485	36.359168	69.518938
996.850833	33.944877	69.523943
996.225512	26.360423	69.528948
995.273241	30.692282	69.533953
994.921021	35.300803	69.538958
994.907428	38.743756	69.543962
993.528722	42.525344	69.548967
993.075492	33.260954	69.553972
992.423848	39.621706	69.558977
991.785299	36.656400	69.563982
991.224512	25.918998	69.568986
990.048736	40.670045	69.573991
989.358830	35.166283	69.578996
988.820587	32.325360	69.584001
988.417197	37.829795	69.589006
988.102877	36.353492	69.594010
986.882927	33.999489	69.599015
986.668701	34.185037	69.604020
986.128817	37.555625	69.609025
984.900091	36.160173	69.614030
984.277663	30.459609	69.619034
983.561498	27.077753	69.624039
983.305452	33.761885	69.629044
982.650037	35.397389	69.634049
981.433967	32.801512	69.639054
981.111287	24.233829	69.644058
980.283908	34.839065	69.649063
979.945743	30.573939	69.654068
978.983172	32.755031	69.659073
978.229389	37.577254	69.664078
977.897492	20.114401	69.669082
977.416684	39.116452	69.674087
976.987021	29.463566	69.679092
975.971860	37.179919	69.684097
975.282654	37.524624	69.689102
974.618201	33.131658	69.694106
973.410167	30.214404	69.699111
972.854895	38.434708	69.704116
972.633225	41.896581	69.709121
971.954257	37.881216	69.714126
971.480710	30.460264	69.719130
970.291944	45.369497	69.724135
969.945865	34.588468	69.729140
969.845574	33.407673	69.734145
968.337928	29.574639	69.739150
967.908242	39.779147	69.744154
967.124057	34.509580	69.749159
966.786962	31.762801	69.754164
965.791860	28.363841	69.759169
964.203582	33.654730	69.764174
964.174525	32.718051	69.769178
963.955466	37.190273	69.774183
963.488395	35.451292	69.779188
963.121041	24.791923	69.784193
962.473084	36.907625	69.789198
961.624737	33.713956	69.794202
960.803007	39.027938	69.799207
959.938446	35.693355	69.804212
959.062041	47.839113	69.809217
958.291968	32.390249	69.814222
957.965026	39.017861	69.819226
957.665871	36.921020	69.824231
956.629009	32.615706	69.829236
956.140826	39.417202	69.834241
955.120641	43.236368	69.839246
954.946463	26.084288	69.844250
953.960144	35.467527	69.849255
952.829909	34.854309	69.854260
952.511858	23.703001	69.859265
952.172003	38.792513	69.864270
951.964542	28.192850	69.869274
951.141427	34.457899	69.874279
950.438843	23.123373	69.879284
949.812439	26.160824	69.884289
948.333909	27.990398	69.889294
948.030814	33.750095	69.894298
947.330957	31.288117	69.899303
946.940666	30.727450	69.904308
945.993356	35.481135	69.909313
945.015880	26.618717	69.914318
944.317610	19.922626	69.919322
943.738509	35.997900	69.924327
943.869997	25.426297	69.929332
943.198647	25.537947	69.934337
942.100809	28.503777	69.939342
941.521969	28.130802	69.944346
941.050966	34.939025	69.949351
939.999463	26.436876	69.954356
939.351123	34.971596	69.959361
938.310178	27.178931	69.964366
938.209496	31.570817	69.969370
938.048736	38.616657	69.974375
937.135907	23.354525	69.979380
936.255266	36.577946	69.984385
935.215038	37.003754	69.989390
935.093933	28.467074	69.994394
934.235502	37.721165	69.999399
933.111681	35.053865	70.004404
932.806531	29.764843	70.009409
932.006639	35.624103	70.014414
932.014906	33.145624	70.019418
930.895501	38.029199	70.024423
930.023912	33.889971	70.029428
929.646614	30.403743	70.034433
928.648521	28.241531	70.039438
928.740021	25.713540	70.044442
927.826014	30.868759	70.049447
927.177945	30.431116	70.054452
926.532119	30.923462	70.059457
925.431011	38.431173	70.064462
924.752535	26.613452	70.069466
924.256365	33.329493	70.074471
924.033637	39.131594	70.079476
922.984931	35.244470	70.084481
922.059364	40.671177	70.089486
921.631837	35.466282	70.094490
921.276519	41.965958	70.099495
920.690515	27.247869	70.104500
919.588038	33.193132	70.109505
918.821260	39.047126	70.114510
918.421751	24.154291	70.119514
917.912589	38.233174	70.124519
916.727216	31.404887	70.129524
916.533881	29.146140	70.134529
915.643927	39.997880	70.139534
915.294402	28.476295	70.144538
913.719269	36.986643	70.149543
913.311577	35.752278	70.154548
913.010762	22.108379	70.159553
912.417558	35.036915	70.164558
912.304267	20.871193	70.169562
911.325393	28.091384	70.174567
910.381977	29.171959	70.179572
909.867032	21.782846	70.184577
909.320177	30.615211	70.189582
908.689580	14.959700	70.194586
907.537765	23.519358	70.199591
907.190677	36.757211	70.204596
906.827087	32.986547	70.209601
905.605170	34.103564	70.214606
904.927396	21.992448	70.219610
904.019815	31.246480	70.224615
903.754340	33.904820	70.229620
903.571212	29.184552	70.234625
902.594865	37.612222	70.239630
902.019007	32.358405	70.244634
901.343013	37.966156	70.249639
900.614654	33.337395	70.254644
899.848037	32.313113	70.259649
898.939581	41.707632	70.264654
898.660369	24.420907	70.269658
898.161349	30.038334	70.274663
896.859850	38.175578	70.279668
896.758249	28.560382	70.284673
895.837688	25.438153	70.289678
895.539586	21.955098	70.294682
894.623550	34.230161	70.299687
893.520004	34.084202	70.304692
893.050358	32.290456	70.309697
892.307066	43.558804	70.314702
892.404593	23.831064	70.319706
891.616290	32.876893	70.324711
890.794215	32.558412	70.329716
890.232885	22.666329	70.334721
888.859038	44.166345	70.339726
888.340588	26.151345	70.344730
887.497271	30.866421	70.349735
887.325810	30.740837	70.354740
887.428431	32.941647	70.359745
886.197337	34.637264	70.364750
885.261269	26.703361	70.369754
884.818478	28.741836	70.374759
884.062136	36.376025	70.379764
883.344499	31.086437	70.384769
882.382883	32.240877	70.389774
882.346932	31.893464	70.394778
881.727497	40.907692	70.399783
880.845035	34.573651	70.404788
880.196241	28.779550	70.409793
879.267091	36.371864	70.414798
878.852960	30.843170	70.419802
877.762962	35.072419	70.424807
877.065557	36.241575	70.429812
876.725729	31.801701	70.434817
875.976764	32.032949	70.439822
875.981540	20.633173	70.444826
874.740032	35.793657	70.449831
873.896592	33.411321	70.454836
873.635707	24.263005	70.459841
872.839557	33.008907	70.464846
871.794810	30.518274	70.469850
871.029802	32.861912	70.474855
870.856300	35.861986	70.479860
870.660140	27.482334	70.484865
869.665250	29.774258	70.489870
868.701098	23.800137	70.494874
868.260067	22.017611	70.499879
867.512866	24.590213	70.504884
867.266228	22.286343	70.509889
865.602189	24.285831	70.514894
865.042378	14.723084	70.519898
864.656823	22.787077	70.524903
864.530477	29.702863	70.529908
864.045341	19.413910	70.534913
862.794575	25.297644	70.539918
862.269802	20.721644	70.544922
861.847756	21.088506	70.549927
860.552066	29.600128	70.554932
860.089417	21.084714	70.559937
859.086486	25.795241	70.564942
859.202783	19.595536	70.569946
858.888177	25.182036	70.574951
857.561755	27.184557	70.579956
856.965065	27.845707	70.584961
856.341617	28.290357	70.589966
855.798082	26.241891	70.594970
854.842409	22.393607	70.599975
853.926468	21.350534	70.604980
853.978665	15.919501	70.609985
853.117908	26.383422	70.614990
852.049907	14.891079	70.619994
851.520378	23.761688	70.624999
850.844408	19.831039	70.630004
850.631534	26.940358	70.635009
849.502513	27.646823	70.640014
848.590707	21.629690	70.645018
847.987513	22.323414	70.650023
847.585816	27.745594	70.655028
847.669384	22.949769	70.660033
846.603730	28.964885	70.665038
846.044367	23.782574	70.670042
845.098196	32.815697	70.675047
844.504754	31.109472	70.680052
843.760793	16.619983	70.685057
842.820933	13.642767	70.690062
842.334407	20.401429	70.695066
842.225754	19.067441	70.700071
840.915206	42.963676	70.705076
840.608938	31.041008	70.710081
839.542966	24.034499	70.715086
839.476506	25.469061	70.720090
838.582503	18.515600	70.725095
837.499480	36.134415	70.730100
837.020301	18.204653	70.735105
836.465429	24.805473	70.740110
836.078415	16.676973	70.745114
834.979133	28.083983	70.750119
834.060308	27.910224	70.755124
834.329595	15.884914	70.760129
833.368738	27.533225	70.765134
832.254237	34.861760	70.770138
831.614414	30.650988	70.775143
830.995178	19.951333	70.780148
830.832584	17.615168	70.785153
829.987002	26.302717	70.790158
828.954213	33.367526	70.795162
828.667550	32.536508	70.800167
827.968592	35.207091	70.805172
827.817815	18.675764	70.810177
826.514269	22.292512	70.815182
826.207165	31.446246	70.820186
825.369651	40.302821	70.825191
824.308810	24.471411	70.830196
823.726976	21.369403	70.835201
823.156743	31.567904	70.840206
822.940279	29.363309	70.845210
821.954970	15.199238	70.850215
820.875802	24.707669	70.855220
821.055498	19.956464	70.860225
820.055543	28.006311	70.865230
819.333450	18.869931	70.870234
818.554707	28.891901	70.875239
817.885808	21.907344	70.880244
817.602960	28.915847	70.885249
816.408310	28.219911	70.890254
815.574609	23.981665	70.895258
815.106317	27.957435	70.900263
814.541689	19.839868	70.905268
814.250403	24.825030	70.910273
813.534811	19.470494	70.915278
812.600299	21.059010	70.920282
811.844632	23.339678	70.925287
811.356633	21.384879	70.930292
811.104682	17.408820	70.935297
809.791246	32.550811	70.940302
809.167773	23.485459	70.945306
808.953904	16.146214	70.950311
808.204326	31.460201	70.955316
807.243525	21.075109	70.960321
806.435194	17.996549	70.965326
805.869497	26.369906	70.970330
805.583003	27.828459	70.975335
805.232456	30.024138	70.980340
804.277444	28.187837	70.985345
803.472502	29.878725	70.990350
803.106651	24.403863	70.995354
801.911668	29.345245	71.000359
800.930590	22.588576	71.005364
800.659142	28.428392	71.010369
799.534383	30.717363	71.015374
799.611207	21.280351	71.020378
799.535716	24.080330	71.025383
798.442422	39.209362	71.030388
797.754403	19.368596	71.035393
796.888774	25.407075	71.040398
795.909023	21.633607	71.045402
795.083053	31.801866	71.050407
794.677952	27.801305	71.055412
794.227691	20.617957	71.060417
793.873804	26.685349	71.065422
793.146260	19.850478	71.070426
792.700730	22.791363	71.075431
791.384005	27.134004	71.080436
790.490959	27.858117	71.085441
789.714380	29.911902	71.090446
789.034350	22.727289	71.095450
788.837412	26.823856	71.100455
788.861528	25.631149	71.105460
787.930361	19.941957	71.110465
786.697980	22.489325	71.115470
786.272791	21.803361	71.120474
786.222641	19.551794	71.125479
785.219341	20.712906	71.130484
784.284301	18.460299	71.135489
783.597017	29.715008	71.140494
783.142854	27.266002	71.145498
781.978209	18.605343	71.150503
781.272452	29.473511	71.155508
781.113343	29.355429	71.160513
780.528460	32.392616	71.165518
780.172538	19.375657	71.170522
778.958918	17.060177	71.175527
778.264093	18.796615	71.180532
778.122455	13.199339	71.185537
776.502762	27.442405	71.190542
775.787197	22.352788	71.195546
775.373835	14.909700	71.200551
774.885935	29.053000	71.205556
774.790988	20.614679	71.210561
774.072651	18.502607	71.215566
773.353403	20.247665	71.220570
772.687090	19.563824	71.225575
771.662335	18.818786	71.230580
770.489625	15.123358	71.235585
769.726744	28.692310	71.240590
769.774318	28.984420	71.245594
769.153774	19.467638	71.250599
768.523361	31.080703	71.255604
768.375998	24.298540	71.260609
767.298936	28.792259	71.265614
766.651945	26.034933	71.270618
766.062348	23.965440	71.275623
764.931878	24.233807	71.280628
764.490831	21.757488	71.285633
763.799424	34.474604	71.290638
763.391929	28.072880	71.295642
762.339023	26.886077	71.300647
761.434481	21.867550	71.305652
761.137821	19.120678	71.310657
760.669056	22.864733	71.315662
760.009920	18.806862	71.320666
759.089454	21.894326	71.325671
758.103668	30.150082	71.330676
758.388526	22.699901	71.335681
757.530961	25.540824	71.340686
756.507931	24.827054	71.345690
755.879175	31.548456	71.350695
755.497629	27.834294	71.355700
754.369282	28.723609	71.360705
753.473024	23.579195	71.365710
752.711064	28.489499	71.370714
752.756376	29.732812	71.375719
752.065475	33.132215	71.380724
751.436436	19.332477	71.385729
750.470250	35.004217	71.390734
749.970702	27.434511	71.395738
749.811689	16.119176	71.400743
748.728887	34.471211	71.405748
748.059291	29.071526	71.410753
747.431347	21.047633	71.415758
746.594252	22.600164	71.420762
745.751692	27.504380	71.425767
745.154166	26.478455	71.430772
744.746861	21.109547	71.435777
744.193760	24.364016	71.440782
743.776644	22.757468	71.445786
742.979500	25.522547	71.450791
741.975383	27.174207	71.455796
741.180551	21.515363	71.460801
740.212311	25.599128	71.465806
739.410511	30.514203	71.470810
739.183833	19.307406	71.475815
738.732985	21.935352	71.480820
738.717469	21.538960	71.485825
737.992842	23.079893	71.490830
737.266590	29.556640	71.495834
736.047102	20.676094	71.500839
735.080570	27.164291	71.505844
734.747567	27.739333	71.510849
733.908549	28.623588	71.515854
733.325467	29.240025	71.520858
733.122285	18.237634	71.525863
731.616479	28.575647	71.530868
731.256766	37.546964	71.535873
730.233517	26.359771	71.540878
729.740474	28.794177	71.545882
729.767293	25.959535	71.550887
729.193702	34.436659	71.555892
728.655411	16.581004	71.560897
727.679179	20.569857	71.565902
726.968712	19.257587	71.570906
725.945879	19.830512	71.575911
725.136144	20.853600	71.580916
724.925077	24.285408	71.585921
724.454219	28.922302	71.590926
723.330858	30.056826	71.595930
722.985930	32.701025	71.600935
722.199549	27.982223	71.605940
721.837221	19.975967	71.610945
720.593497	29.518519	71.615950
719.923365	22.677686	71.620954
719.482627	17.489140	71.625959
718.986565	33.194830	71.630964
718.680502	25.094463	71.635969
717.629011	22.294334	71.640974
716.939290	21.712000	71.645978
716.593800	22.763666	71.650983
715.236284	33.276761	71.655988
714.607472	21.864357	71.660993
714.305800	24.400749	71.665998
713.192677	28.660549	71.671002
713.331700	22.394153	71.676007
712.293388	36.705525	71.681012
711.688243	22.771116	71.686017
710.852474	26.352857	71.691022
710.572088	29.967583	71.696026
709.781575	16.813279	71.701031
708.660960	28.778778	71.706036
708.405202	27.163888	71.711041
707.884463	38.368443	71.716046
707.130968	34.546369	71.721050
706.237936	22.523222	71.726055
705.437272	30.957662	71.731060
705.415276	23.111668	71.736065
704.515097	26.870814	71.741070
703.429608	22.696358	71.746074
703.146168	26.024582	71.751079
702.426353	34.137087	71.756084
702.091658	21.358028	71.761089
700.962514	21.667211	71.766094
700.087027	28.774817	71.771098
700.110294	30.078406	71.776103
699.312794	27.605246	71.781108
698.187413	22.248197	71.786113
697.639018	30.998837	71.791118
696.964322	18.909394	71.796122
696.786204	23.069194	71.801127
695.377219	21.801936	71.806132
694.884668	18.748820	71.811137
694.408201	22.172432	71.816142
693.709128	22.368983	71.821146
693.782585	20.417839	71.826151
692.094383	22.787116	71.831156
691.837383	19.401621	71.836161
691.549549	28.191188	71.841166
690.602630	23.952096	71.846170
689.728420	24.291648	71.851175
688.744810	34.951783	71.856180
688.555933	28.288196	71.861185
688.123859	34.803261	71.866190
687.335134	29.012583	71.871194
686.644419	16.600865	71.876199
685.612485	28.960655	71.881204
685.418285	29.135155	71.886209
684.357144	27.780974	71.891214
683.509608	24.776505	71.896218
683.139236	27.883623	71.901223
682.442891	30.203764	71.906228
682.296620	20.680869	71.911233
681.443605	27.231426	71.916238
680.434381	20.045662	71.921242
680.308026	19.826183	71.926247
679.451169	30.983341	71.931252
678.678836	26.339584	71.936257
678.168342	30.828265	71.941262
677.236608	28.395411	71.946266
676.610423	24.378046	71.951271
675.072550	31.215851	71.956276
674.975218	24.036251	71.961281
674.280622	22.536977	71.966286
674.016631	33.497231	71.971290
674.153027	21.281786	71.976295
672.953195	19.263766	71.981300
672.184550	25.124419	71.986305
671.862035	13.745258	71.991310
670.611061	22.636163	71.996314
669.860520	24.523419	72.001319
669.108111	30.480831	72.006324
668.804550	23.699903	72.011329
668.060564	30.472784	72.016334
666.740901	25.075731	72.021338
666.550351	20.995302	72.026343
665.667342	25.035559	72.031348
665.651246	34.166609	72.036353
665.078732	24.153387	72.041358
664.156237	36.230849	72.046362
663.446029	22.701097	72.051367
662.916230	28.157887	72.056372
662.331606	24.176482	72.061377
661.360387	24.999818	72.066382
660.499180	31.827636	72.071386
660.255354	22.142095	72.076391
659.673824	31.992352	72.081396
658.875271	35.180279	72.086401
658.365816	34.507756	72.091406
657.818588	28.167731	72.096410
657.086711	21.619010	72.101415
655.852270	29.102317	72.106420
655.514169	22.897713	72.111425
654.944042	27.835835	72.116430
653.893765	30.119315	72.121434
653.550258	21.014164	72.126439
652.677172	31.115845	72.131444
652.643979	34.085697	72.136449
651.349166	18.400462	72.141454
650.477038	28.306459	72.146458
650.077418	20.366079	72.151463
649.637622	28.900745	72.156468
649.297724	31.610379	72.161473
647.780212	30.268973	72.166478
647.368615	28.155394	72.171482
647.023153	29.437284	72.176487
646.547335	21.034407	72.181492
646.043660	22.775128	72.186497
645.040116	29.589350	72.191502
644.307576	27.851716	72.196506
643.904384	19.184978	72.201511
642.317887	17.632228	72.206516
641.548663	32.034791	72.211521
641.270769	24.689998	72.216526
640.828122	28.955003	72.221530
640.663525	17.673691	72.226535
640.239575	31.843082	72.231540
638.881041	25.329516	72.236545
638.458289	29.059954	72.241550
637.716963	23.424165	72.246554
637.181354	24.271168	72.251559
635.959231	35.565354	72.256564
635.753000	25.714566	72.261569
635.506039	20.848392	72.266574
633.986530	31.403089	72.271578
633.367681	26.443187	72.276583
632.736507	21.665010	72.281588
632.342980	29.238314	72.286593
632.098922	23.682592	72.291598
631.381136	25.594603	72.296602
630.443753	26.049885	72.301607
629.793036	28.706526	72.306612
629.036142	25.768060	72.311617
627.924909	19.599870	72.316622
627.236008	28.338204	72.321626
626.844605	12.986897	72.326631
626.339373	19.666567	72.331636
626.005035	27.604157	72.336641
625.669857	25.718093	72.341646
624.824263	21.568542	72.346650
624.390670	23.294951	72.351655
622.857077	30.717115	72.356660
622.214651	22.099521	72.361665
621.821836	12.611177	72.366670
621.198394	22.094394	72.371674
620.812984	22.352966	72.376679
619.503067	36.188835	72.381684
618.938900	15.063802	72.386689
618.550867	30.403802	72.391694
618.109200	32.063695	72.396698
617.443985	24.719097	72.401703
616.172166	21.569354	72.406708
615.892593	41.510690	72.411713
615.721764	36.020569	72.416718
614.215544	28.012030	72.421722
613.632024	30.079268	72.426727
612.758161	24.488250	72.431732
612.724330	33.371399	72.436737
612.389292	26.392080	72.441742
611.054214	32.853868	72.446746
610.553474	35.281637	72.451751
610.132911	39.528940	72.456756
609.495592	33.132318	72.461761
608.590841	32.461268	72.466766
607.643115	36.499239	72.471770
607.393644	36.750353	72.476775
606.632612	26.710409	72.481780
605.977503	14.004492	72.486785
605.365227	31.340234	72.491790
604.575520	36.407952	72.496794
604.177760	20.928355	72.501799
602.755593	33.713001	72.506804
602.069511	33.442337	72.511809
601.798743	35.153855	72.516814
601.326901	39.466094	72.521818
601.194687	29.745438	72.526823
600.197116	39.111652	72.531828
599.227981	36.224344	72.536833
598.682115	31.888297	72.541838
597.961450	43.364390	72.546842
597.796568	19.036249	72.551847
596.298310	28.859073	72.556852
595.702513	26.222944	72.561857
594.931726	34.764609	72.566862
594.503697	31.906228	72.571866
594.254847	37.416048	72.576871
593.494889	35.726948	72.581876
592.839166	26.515429	72.586881
592.150436	31.567065	72.591886
591.852649	29.865849	72.596890
590.643955	15.272316	72.601895
589.586236	35.760181	72.606900
589.480982	34.518699	72.611905
588.702913	34.423529	72.616910
588.257353	28.570346	72.621914
587.481446	30.141565	72.626919
586.666033	32.405008	72.631924
586.303012	29.708151	72.636929
585.828498	24.591242	72.641934
584.415069	29.360944	72.646938
583.856221	38.622590	72.651943
583.354742	28.763648	72.656948
582.948220	25.425636	72.661953
582.495852	18.822962	72.666958
581.434466	28.937305	72.671962
580.930131	30.816907	72.676967
580.274435	45.079992	72.681972
579.900117	36.105905	72.686977
578.881451	29.598159	72.691982
578.126073	17.404931	72.696986
578.248667	25.963554	72.701991
576.738363	40.809010	72.706996
576.175721	34.911402	72.712001
575.621684	25.841379	72.717006
575.000287	26.386689	72.722010
573.942643	17.362198	72.727015
573.194393	36.320110	72.732020
572.766487	25.984283	72.737025
572.662135	19.699890	72.742030
571.967074	24.640580	72.747034
571.100991	32.328583	72.752039
570.463201	25.695524	72.757044
569.718751	29.064078	72.762049
568.870202	23.765494	72.767054
567.891454	27.161908	72.772058
567.647075	27.205648	72.777063
566.993280	34.987563	72.782068
566.899905	25.636019	72.787073
565.795990	22.722892	72.792078
564.958528	26.547781	72.797082
564.251620	37.173337	72.802087
563.482900	42.855851	72.807092
562.530150	26.641549	72.812097
562.185616	19.454036	72.817102
561.682123	34.957502	72.822106
561.645083	37.625211	72.827111
560.655567	29.067653	72.832116
559.830555	25.170298	72.837121
559.466011	29.823393	72.842126
558.182743	30.068888	72.847130
557.383987	23.385786	72.852135
556.713241	26.115016	72.857140
556.412098	44.408823	72.862145
556.005187	29.460513	72.867150
555.130921	37.378469	72.872154
554.132371	16.701103	72.877159
553.966312	21.360424	72.882164
553.102162	39.852711	72.887169
552.695273	16.260110	72.892174
551.694420	31.144254	72.897178
551.217877	21.894750	72.902183
550.617236	39.227074	72.907188
549.900559	31.493328	72.912193
549.169081	12.916368	72.917198
548.319966	23.462075	72.922202
547.838129	21.020682	72.927207
547.177291	39.619346	72.932212
546.241759	28.304743	72.937217
545.682681	28.294543	72.942222
545.362122	34.142195	72.947226
545.048172	22.583510	72.952231
543.870796	14.175736	72.957236
542.830505	51.943138	72.962241
542.349872	16.898566	72.967246
541.772370	33.738374	72.972250
541.476476	20.713498	72.977255
540.233779	37.386481	72.982260
539.401669	27.181280	72.987265
539.493988	27.333801	72.992270
538.801530	21.196710	72.997274
538.069375	24.689461	73.002279
537.334781	31.881895	73.007284
536.665648	16.298908	73.012289
536.142648	28.230757	73.017294
535.027187	21.016258	73.022298
534.497905	10.436422	73.027303
533.927686	32.311526	73.032308
533.611823	31.086253	73.037313
533.162413	14.096407	73.042318
532.052436	31.881999	73.047322
531.220122	26.993977	73.052327
530.666983	15.616899	73.057332
529.937050	37.988932	73.062337
529.218974	25.151151	73.067342
528.426790	26.026435	73.072346
527.969113	30.215008	73.077351
527.534375	11.972386	73.082356
526.793619	29.820575	73.087361
526.037111	24.718643	73.092366
525.133225	23.594932	73.097370
524.883393	16.001283	73.102375
524.158768	26.681697	73.107380
523.351674	29.246589	73.112385
523.157359	26.256380	73.117390
522.134730	30.109204	73.122394
521.432748	22.521356	73.127399
520.521993	23.227887	73.132404
519.945888	24.537075	73.137409
519.841838	17.860005	73.142414
518.533536	33.203120	73.147418
517.925344	28.929061	73.152423
517.383540	38.657902	73.157428
516.925092	26.821062	73.162433
516.201280	17.853799	73.167438
515.258547	33.797799	73.172442
514.503587	21.522532	73.177447
513.998151	29.148364	73.182452
513.902803	31.472145	73.187457
512.912646	25.658436	73.192462
511.898684	31.282263	73.197466
511.325322	28.492782	73.202471
511.246049	36.031802	73.207476
509.850529	19.787158	73.212481
509.252583	22.225698	73.217486
508.597121	30.499864	73.222490
508.165883	25.532187	73.227495
507.960618	26.846950	73.232500
506.908436	32.532058	73.237505
506.505832	24.846060	73.242510
505.234419	30.075694	73.247514
505.130560	29.288128	73.252519
504.169261	25.433005	73.257524
503.378664	25.361934	73.262529
503.192402	20.069822	73.267534
502.324048	30.639109	73.272538
501.645253	18.879960	73.277543
500.858113	25.912047	73.282548
500.229761	28.899448	73.287553
500.072788	26.051517	73.292558
498.874617	28.814330	73.297562
498.284207	21.140911	73.302567
497.737203	30.244568	73.307572
497.130824	36.918301	73.312577
496.410666	31.201922	73.317582
495.243531	27.642929	73.322586
494.853976	32.266902	73.327591
494.587511	25.323990	73.332596
493.840569	24.485926	73.337601
492.988229	21.969540	73.342606
491.864310	26.888694	73.347610
491.884613	14.150906	73.352615
491.192904	29.430482	73.357620
490.361035	21.792381	73.362625
489.803706	15.793042	73.367630
489.084810	19.310498	73.372634
488.490423	18.962184	73.377639
487.506221	19.194758	73.382644
486.354922	26.251753	73.387649
486.422478	15.825982	73.392654
485.725757	23.960075	73.397658
485.343567	19.932278	73.402663
484.426260	30.938271	73.407668
483.328034	17.979745	73.412673
483.263472	24.193437	73.417678
482.661996	35.857121	73.422682
482.024325	21.067027	73.427687
481.017319	28.824810	73.432692
480.528092	42.876889	73.437697
480.024751	19.190878	73.442702
479.184428	29.396181	73.447706
478.597662	36.043139	73.452711
478.288987	9.345883	73.457716
477.195542	28.636317	73.462721
476.552315	17.377682	73.467726
475.663404	32.256625	73.472730
475.140081	24.094738	73.477735
474.467240	20.770797	73.482740
473.492414	30.357332	73.487745
473.019517	25.866201	73.492750
472.059628	28.849665	73.497754
471.915858	25.755221	73.502759
471.905240	17.987859	73.507764
470.629634	26.375027	73.512769
470.142828	26.961993	73.517774
469.126247	24.730387	73.522778
468.295892	34.714927	73.527783
467.910101	28.830174	73.532788
466.990959	26.786458	73.537793
466.779314	20.620090	73.542798
466.068145	31.093383	73.547802
465.580843	18.909526	73.552807
464.585816	23.484899	73.557812
464.011685	27.095985	73.562817
463.342387	27.109673	73.567822
462.326289	25.456697	73.572826
461.930618	17.324938	73.577831
461.497447	22.906700	73.582836
460.671509	26.270921	73.587841
459.673489	20.657175	73.592846
458.955038	17.589649	73.597850
458.585922	20.963078	73.602855
458.287409	17.122215	73.607860
457.391643	20.402950	73.612865
456.681254	10.064871	73.617870
456.188897	22.835453	73.622874
455.404948	16.817043	73.627879
454.929015	13.329280	73.632884
453.760261	27.554268	73.637889
453.367220	17.939853	73.642894
452.510195	22.915838	73.647898
452.114484	9.963665	73.652903
451.449898	30.021504	73.657908
450.500391	22.435277	73.662913
450.147770	4.547016	73.667918
449.489106	43.972353	73.672922
448.892818	7.364705	73.677927
448.018575	31.082700	73.682932
447.476949	23.727931	73.687937
446.848094	11.848897	73.692942
445.705364	23.693428	73.697946
444.966387	13.665815	73.702951
444.602271	30.457432	73.707956
443.994625	13.555907	73.712961
443.711035	27.791235	73.717966
443.286250	29.375931	73.722970
442.522744	31.905518	73.727975
442.139791	9.520182	73.732980
440.691178	20.645526	73.737985
439.978671	24.735951	73.742990
439.212059	31.999735	73.747994
438.964534	19.927481	73.752999
438.534759	22.940020	73.758004
437.171233	22.184452	73.763009
436.818261	23.354032	73.768014
436.355553	23.325347	73.773018
436.031887	14.573459	73.778023
435.108373	17.026047	73.783028
434.081049	33.940690	73.788033
433.828407	22.249271	73.793038
432.538534	18.328273	73.798042
431.927652	21.191486	73.803047
431.391298	18.260522	73.808052
430.703535	28.031546	73.813057
430.354465	22.084187	73.818062
429.934759	18.500742	73.823066
428.969077	23.344247	73.828071
428.389628	22.932069	73.833076
427.545632	23.186478	73.838081
427.515159	11.033919	73.843086
426.042005	20.181084	73.848090
425.452650	31.104874	73.853095
424.871898	16.684183	73.858100
424.201964	26.578513	73.863105
423.435151	15.815801	73.868110
422.489940	26.651223	73.873114
422.109758	16.164348	73.878119
422.153269	26.121600	73.883124
421.658529	26.686187	73.888129
420.766189	7.912596	73.893134
419.677252	24.773976	73.898138
418.856233	29.696929	73.903143
417.737469	20.365312	73.908148
416.726922	25.605452	73.913153
416.908637	21.916712	73.918158
416.481297	29.965321	73.923162
416.216077	18.916114	73.928167
415.819737	15.702663	73.933172
414.448239	24.917211	73.938177
413.920397	19.047226	73.943182
413.195066	16.930074	73.948186
412.226705	23.554272	73.953191
411.603637	31.479540	73.958196
410.782592	26.667036	73.963201
410.760544	14.068463	73.968206
410.105864	30.505862	73.973210
409.076792	24.504451	73.978215
408.738428	19.659185	73.983220
407.720578	32.373178	73.988225
407.053946	17.698114	73.993230
405.984029	21.914882	73.998234
405.429698	25.453442	74.003239
405.287009	29.451497	74.008244
404.917789	20.897671	74.013249
404.307685	14.156188	74.018254
403.253484	24.138561	74.023258
402.528099	22.193296	74.028263
401.833035	19.860026	74.033268
400.476013	29.518524	74.038273
400.166364	25.513873	74.043278
399.531529	16.885691	74.048282
399.482455	19.386589	74.053287
399.158318	22.566790	74.058292
397.809085	21.695433	74.063297
397.138777	29.899449	74.068302
396.654636	21.933179	74.073306
396.054406	33.525714	74.078311
395.151910	27.942502	74.083316
394.323531	29.474834	74.088321
393.980060	20.114291	74.093326
393.482039	28.271929	74.098330
392.864740	25.126806	74.103335
392.409786	25.891626	74.108340
391.330262	32.533549	74.113345
390.846738	27.358203	74.118350
389.686192	29.993652	74.123354
389.193115	24.529689	74.128359
388.926600	33.990759	74.133364
388.009610	34.439728	74.138369
387.053413	25.372358	74.143374
386.490990	27.751652	74.148378
386.140043	28.518820	74.153383
385.748555	31.630915	74.158388
384.440032	22.212868	74.163393
383.915541	18.832200	74.168398
383.684813	25.783528	74.173402
382.871035	21.302594	74.178407
382.030343	15.758424	74.183412
381.128134	29.579862	74.188417
380.616173	17.081441	74.193422
380.444635	24.210980	74.198426
379.288943	27.015960	74.203431
378.470473	27.222165	74.208436
377.818314	22.846354	74.213441
377.494023	33.723179	74.218446
376.999803	34.984659	74.223450
375.952254	27.830377	74.228455
375.183203	33.194463	74.233460
374.561787	31.492817	74.238465
374.133301	13.173567	74.243470
373.778832	31.635103	74.248474
372.677677	19.586949	74.253479
372.244349	29.538193	74.258484
371.592490	33.368253	74.263489
370.849771	21.026448	74.268494
369.621435	25.717880	74.273498
369.297913	21.922013	74.278503
368.755766	25.693589	74.283508
368.278614	35.602939	74.288513
367.865762	17.011555	74.293518
367.043978	21.116258	74.298522
365.988408	16.391610	74.303527
365.758202	17.675666	74.308532
364.684336	16.071360	74.313537
363.941127	16.837972	74.318542
363.540417	16.791536	74.323546
362.817876	28.096078	74.328551
362.465915	30.493872	74.333556
361.195771	30.962866	74.338561
360.606774	23.314495	74.343566
360.501935	20.492961	74.348570
359.670219	29.869075	74.353575
359.163663	21.616249	74.358580
358.180345	23.193784	74.363585
357.694685	16.516055	74.368590
356.988329	31.649759	74.373594
356.382082	26.785697	74.378599
355.381884	28.126244	74.383604
354.559089	31.417461	74.388609
354.816730	23.318790	74.393614
353.933807	25.424340	74.398618
352.666667	22.695013	74.403623
352.218352	23.455628	74.408628
351.954526	35.106510	74.413633
351.476429	24.387689	74.418638
350.542601	31.052135	74.423642
349.431591	26.848803	74.428647
349.070853	24.140587	74.433652
347.970978	24.003748	74.438657
347.202765	18.498500	74.443662
346.871087	18.529368	74.448666
346.392791	26.600294	74.453671
346.223201	14.846782	74.458676
345.004286	21.605544	74.463681
344.617824	19.746621	74.468686
343.755753	23.584958	74.473690
343.526187	30.110355	74.478695
342.413942	19.254506	74.483700
341.419693	27.737226	74.488705
341.059757	21.386368	74.493710
340.579416	31.356147	74.498714
339.673933	25.951619	74.503719
338.740768	32.967600	74.508724
338.249760	28.350087	74.513729
337.907159	22.818004	74.518734
337.439852	16.747595	74.523738
336.524039	30.717857	74.528743
336.176854	16.143289	74.533748
335.272790	24.628981	74.538753
334.544810	24.719861	74.543758
333.618773	27.142927	74.548762
333.163262	22.909241	74.553767
332.917982	22.510053	74.558772
331.728782	29.956324	74.563777
330.984174	28.201790	74.568782
330.226966	28.319405	74.573786
329.563538	32.764711	74.578791
329.485340	17.913897	74.583796
328.549284	19.576945	74.588801
327.715757	22.157144	74.593806
326.826836	13.938470	74.598810
326.530813	20.312039	74.603815
326.385530	18.523481	74.608820
325.135079	30.279578	74.613825
324.815489	15.771573	74.618830
324.218473	18.060204	74.623834
323.044937	21.577632	74.628839
322.581244	19.953357	74.633844
321.715021	25.378671	74.638849
321.255473	19.940920	74.643854
320.691223	18.130838	74.648858
320.097562	27.667699	74.653863
319.080697	15.308121	74.658868
318.516194	17.585264	74.663873
318.073630	27.030237	74.668878
317.549057	25.406205	74.673882
316.522823	22.351515	74.678887
315.972902	13.623103	74.683892
315.330365	29.582365	74.688897
315.198984	19.051131	74.693902
314.039809	30.455238	74.698906
313.372575	24.798296	74.703911
312.561705	20.260158	74.708916
311.322124	28.045605	74.713921
310.798489	25.040107	74.718926
310.390974	26.937440	74.723930
310.020635	35.248192	74.728935
309.819965	21.452889	74.733940
309.234253	32.551143	74.738945
308.435806	25.220005	74.743950
307.600052	27.675996	74.748954
306.570017	21.886087	74.753959
305.607737	20.472166	74.758964
304.740550	41.057449	74.763969
304.469454	18.346840	74.768974
304.122107	20.139971	74.773978
303.801781	25.278018	74.778983
303.199637	25.640565	74.783988
302.319847	21.059804	74.788993
301.575431	19.265829	74.793998
301.126357	21.437850	74.799002
300.020413	32.332042	74.804007
299.695615	9.817653	74.809012
298.995077	22.749152	74.814017
298.557541	17.293708	74.819022
297.583396	17.955234	74.824026
296.805164	20.695351	74.829031
296.324417	21.680326	74.834036
295.057842	31.232998	74.839041
294.559881	9.107312	74.844046
294.064324	19.013284	74.849050
293.519465	21.208459	74.854055
293.398417	22.117177	74.859060
292.103592	29.004751	74.864065
291.169071	18.902719	74.869070
291.085512	23.283983	74.874074
290.449208	15.220586	74.879079
289.506388	12.789658	74.884084
288.598494	12.800428	74.889089
288.132571	19.659944	74.894094
287.566271	22.399395	74.899098
287.327558	24.479544	74.904103
286.386115	12.615708	74.909108
285.490591	16.057299	74.914113
285.185297	16.937043	74.919118
284.559808	3.598960	74.924122
283.061927	37.853523	74.929127
282.916416	9.424192	74.934132
282.382214	21.372033	74.939137
281.947663	10.248938	74.944142
280.976347	19.108036	74.949146
280.036905	14.122084	74.954151
279.821246	8.350602	74.959156
279.126265	15.480002	74.964161
278.243842	24.973018	74.969166
277.547752	22.726676	74.974170
276.830078	16.292520	74.979175
276.819331	21.054811	74.984180
275.636737	14.335247	74.989185
274.874216	19.293064	74.994190
274.355030	9.768193	74.999194
273.993874	19.075617	75.004199
273.295332	13.198194	75.009204
272.200301	18.976939	75.014209
271.633324	21.615584	75.019214
271.337802	13.887352	75.024218
270.547224	15.889904	75.029223
269.370899	12.054971	75.034228
268.986071	25.273594	75.039233
268.506111	14.151431	75.044238
267.973198	19.313905	75.049242
266.709779	30.644767	75.054247
266.390352	14.880007	75.059252
265.281255	26.069579	75.064257
265.190471	11.906718	75.069262
264.758453	22.857475	75.074266
263.880577	31.755303	75.079271
263.295117	14.492375	75.084276
262.629017	18.575444	75.089281
262.061256	15.086596	75.094286
261.236734	20.644040	75.099290
260.325871	29.137146	75.104295
260.216686	8.428583	75.109300
259.100606	19.209284	75.114305
258.308387	16.431108	75.119310
257.749272	18.316347	75.124314
256.932822	27.671128	75.129319
257.175050	9.440536	75.134324
255.926705	26.369945	75.139329
255.386375	25.631474	75.144334
254.678257	34.413940	75.149338
253.329940	19.633161	75.154343
252.860281	15.124226	75.159348
251.889632	25.755604	75.164353
251.375076	19.189735	75.169358
251.599838	23.720529	75.174362
250.825442	22.287716	75.179367
250.721897	16.410059	75.184372
249.641546	21.131564	75.189377
249.068027	10.467419	75.194382
247.707718	10.253880	75.199386
246.856842	20.219655	75.204391
246.353559	15.049076	75.209396
246.066081	18.581391	75.214401
245.685401	19.468427	75.219406
245.067270	14.945319	75.224410
243.929813	23.879799	75.229415
243.299022	18.877771	75.234420
242.680910	21.718525	75.239425
241.966246	18.391864	75.244430
241.356398	22.246789	75.249434
240.629515	28.835701	75.254439
239.959778	14.012986	75.259444
239.149899	22.184087	75.264449
238.505260	29.590886	75.269454
238.037380	21.237320	75.274458
237.203771	26.036182	75.279463
237.161098	20.158281	75.284468
236.221195	27.411892	75.289473
235.514281	28.377745	75.294478
234.812101	20.947720	75.299482
234.097856	28.114898	75.304487
233.179567	22.324555	75.309492
232.412154	30.146716	75.314497
231.914294	31.596448	75.319502
231.718614	28.871400	75.324506
231.129875	34.009671	75.329511
230.046439	17.830594	75.334516
229.141840	24.534566	75.339521
228.926689	24.269348	75.344526
228.491862	21.211869	75.349530
227.273309	27.835017	75.354535
226.620698	10.526049	75.359540
226.024348	27.231684	75.364545
225.407219	21.330258	75.369550
225.354104	28.820938	75.374554
224.360450	30.354444	75.379559
223.658846	22.142216	75.384564
223.146214	25.125420	75.389569
221.950903	29.800616	75.394574
221.437983	22.163815	75.399578
220.715474	27.209880	75.404583
220.409163	20.022656	75.409588
219.803280	30.315213	75.414593
218.644005	19.774418	75.419598
217.865560	24.771057	75.424602
217.373707	38.101366	75.429607
217.336193	17.042354	75.434612
216.049985	27.982655	75.439617
215.281515	26.493719	75.444622
215.228277	23.113649	75.449626
214.305131	35.945053	75.454631
213.302020	28.577202	75.459636
212.742143	28.218722	75.464641
212.036515	13.904754	75.469646
211.743229	22.663659	75.474650
211.173303	35.080805	75.479655
210.805558	15.293349	75.484660
209.796226	17.392293	75.489665
209.360423	26.973382	75.494670
208.539922	23.248894	75.499674
207.528792	24.409904	75.504679
207.368946	17.844261	75.509684
206.409134	17.477012	75.514689
205.178427	28.074178	75.519694
204.839111	24.239859	75.524698
203.926679	32.011038	75.529703
204.243571	-2.379903	75.534708
203.491520	26.672003	75.539713
202.246356	22.338757	75.544718
201.764801	18.924484	75.549722
201.044221	12.605931	75.554727
200.565688	13.223166	75.559732
199.313086	27.575135	75.564737
198.997637	20.789890	75.569742
198.616684	16.151716	75.574746
197.803435	24.894183	75.579751
197.080141	16.576624	75.584756
196.399830	31.635236	75.589761
195.972416	23.655248	75.594766
195.216591	25.310108	75.599770
194.026166	26.652664	75.604775
193.622454	23.333205	75.609780
193.029862	29.651576	75.614785
192.504651	19.916387	75.619790
192.401327	15.005307	75.624794
191.093774	30.386261	75.629799
190.336718	11.824600	75.634804
189.994648	22.054594	75.639809
189.691381	18.968263	75.644814
188.377471	8.379615	75.649818
187.472352	8.929260	75.654823
187.475036	10.556216	75.659828
186.585628	30.328237	75.664833
185.585667	13.593448	75.669838
184.992213	15.126234	75.674842
184.449303	21.197000	75.679847
184.472290	12.954410	75.684852
183.305564	21.552979	75.689857
182.303722	18.767255	75.694862
182.099638	17.826964	75.699866
181.216164	29.890430	75.704871
180.592136	17.558172	75.709876
179.690665	17.577418	75.714881
179.203581	21.436435	75.719886
178.758667	26.539166	75.724890
177.942781	24.715628	75.729895
177.138839	17.092131	75.734900
176.472652	20.736871	75.739905
175.744231	41.257470	75.744910
175.788372	26.770345	75.749914
174.694682	29.283273	75.754919
173.876559	18.598230	75.759924
173.300383	16.151464	75.764929
172.907543	21.034594	75.769934
172.269199	26.765792	75.774938
171.113858	19.507389	75.779943
171.009857	16.876533	75.784948
170.031537	26.522053	75.789953
169.041478	9.724204	75.794958
168.747987	12.790736	75.799962
168.055276	17.363737	75.804967
167.648250	13.043519	75.809972
166.797654	17.219100	75.814977
165.814108	13.938492	75.819982
165.641456	12.108583	75.824986
164.777717	17.785838	75.829991
164.074092	9.435200	75.834996
163.105663	15.230066	75.840001
162.415454	28.346009	75.845006
161.989900	22.633237	75.850010
161.527431	23.702049	75.855015
160.867606	19.056312	75.860020
159.996285	19.064452	75.865025
159.275867	22.679999	75.870030
159.319084	16.958710	75.875034
157.779421	17.114417	75.880039
156.935814	36.601624	75.885044
156.611951	12.002549	75.890049
155.996320	25.216977	75.895054
156.177190	17.359191	75.900058
155.187667	23.255190	75.905063
154.372976	21.071950	75.910068
153.956392	21.468019	75.915073
152.604167	15.412617	75.920078
152.085500	13.213713	75.925082
151.195456	20.790532	75.930087
150.921107	17.031016	75.935092
150.658245	11.841049	75.940097
149.304579	23.993685	75.945102
148.681178	20.772341	75.950106
147.995482	28.392269	75.955111
147.947692	13.114053	75.960116
147.110939	24.767978	75.965121
145.854956	26.579872	75.970126
145.446096	15.313955	75.975130
144.803646	18.868191	75.980135
144.561253	26.914135	75.985140
143.502702	18.353609	75.990145
142.719159	18.231071	75.995150
142.417277	11.986113	76.000154
141.928691	12.185522	76.005159
140.945577	17.134397	76.010164
140.063140	21.900074	76.015169
139.493145	13.999609	76.020174
139.461305	8.962027	76.025178
137.816939	15.768219	76.030183
137.670529	17.234458	76.035188
136.858220	26.348926	76.040193
136.289953	26.911102	76.045198
136.048734	19.686709	76.050202
135.011196	19.935813	76.055207
134.413398	18.567912	76.060212
133.622387	16.328868	76.065217
133.353466	19.143923	76.070222
132.679764	9.940183	76.075226
131.513199	20.218082	76.080231
131.094963	23.227247	76.085236
130.619660	19.335786	76.090241
129.521734	15.322856	76.095246
129.396319	20.619053	76.100250
128.344875	27.275515	76.105255
127.756045	11.137477	76.110260
126.732991	17.794138	76.115265
126.190000	25.577379	76.120270
125.918039	14.595546	76.125274
125.079278	17.217640	76.130279
124.396271	14.806846	76.135284
123.850901	16.382436	76.140289
122.977071	27.935055	76.145294
122.788454	14.756003	76.150298
122.042108	14.971292	76.155303
121.237737	12.204564	76.160308
120.500577	14.484051	76.165313
119.843958	24.948700	76.170318
119.368313	11.812270	76.175322
118.072254	14.556174	76.180327
117.781616	9.786929	76.185332
117.432048	16.918047	76.190337
116.719947	30.397009	76.195342
115.933456	12.872913	76.200346
115.047133	26.237740	76.205351
114.594851	19.493257	76.210356
113.701995	12.060575	76.215361
112.775711	14.750243	76.220366
112.221487	5.246782	76.225370
111.650584	9.962783	76.230375
111.505044	26.125055	76.235380
111.209030	14.782810	76.240385
110.065742	24.473576	76.245390
109.563369	16.265890	76.250394
108.594464	19.705049	76.255399
107.707459	9.611306	76.260404
106.959803	7.027915	76.265409
106.021055	11.477750	76.270414
105.874866	7.749840	76.275418
105.421430	32.280636	76.280423
105.010138	17.525563	76.285428
104.021222	9.573657	76.290433
103.384444	18.351073	76.295438
103.298786	5.207650	76.300442
101.786987	34.152090	76.305447
101.055993	23.568290	76.310452
100.846442	-2.058147	76.315457
99.953991	17.059965	76.320462
99.239813	19.089806	76.325466
98.313811	5.539544	76.330471
98.041387	16.228327	76.335476
97.696502	32.308863	76.340481
96.512308	-0.240590	76.345486
96.396161	21.763912	76.350490
94.897029	36.547877	76.355495
94.590182	14.659858	76.360500
94.642436	5.042337	76.365505
93.245256	25.045144	76.370510
92.939798	-0.171789	76.375514
92.019891	26.238871	76.380519
91.669742	22.072011	76.385524
90.586952	6.675045	76.390529
89.325100	25.568252	76.395534
89.517166	0.612571	76.400538
88.941520	32.315404	76.405543
88.579820	26.012186	76.410548
87.571291	2.526797	76.415553
86.265253	38.061164	76.420558
86.655158	22.823523	76.425562
85.393841	23.770611	76.430567
84.559794	18.414723	76.435572
84.162684	31.395632	76.440577
83.526795	26.690911	76.445582
83.254218	0.814348	76.450586
81.661895	18.252793	76.455591
81.088840	25.203532	76.460596
81.122260	13.414545	76.465601
80.393201	25.864959	76.470606
79.626481	14.334460	76.475610
78.659103	15.794451	76.480615
78.417203	28.189248	76.485620
78.074001	16.007771	76.490625
76.872985	16.587303	76.495630
76.345999	22.535707	76.500634
75.662917	20.624798	76.505639
74.797919	18.050669	76.510644
73.839055	17.718012	76.515649
72.814040	18.157519	76.520654
72.955783	9.244765	76.525658
72.418998	12.872042	76.530663
71.791848	18.344447	76.535668
71.082032	15.225212	76.540673
70.303931	23.478012	76.545678
69.991612	16.110443	76.550682
69.253038	29.563673	76.555687
67.647820	15.224524	76.560692
67.341947	9.152094	76.565697
66.951185	17.503952	76.570702
66.852492	19.238532	76.575706
65.879726	31.461336	76.580711
64.973076	17.193684	76.585716
64.599195	11.029606	76.590721
63.647829	24.007452	76.595726
62.633474	23.152253	76.600730
61.678640	18.075818	76.605735
61.206180	22.539605	76.610740
61.403105	20.862056	76.615745
60.682056	27.480037	76.620750
60.351277	17.422166	76.625754
59.228286	24.041181	76.630759
58.752255	27.789653	76.635764
57.496307	24.692875	76.640769
56.656134	26.435340	76.645774
56.245847	18.988787	76.650778
55.651987	18.339318	76.655783
55.453442	31.406820	76.660788
54.425081	18.718083	76.665793
53.315596	27.050550	76.670798
53.229611	27.963146	76.675802
52.780617	28.842185	76.680807
51.804743	20.148680	76.685812
50.955638	20.744630	76.690817
50.132991	23.006236	76.695822
49.808315	19.704161	76.700826
49.158368	21.819958	76.705831
48.573237	23.953801	76.710836
47.936056	15.330850	76.715841
46.901332	32.016541	76.720846
47.045853	23.765609	76.725850
45.971422	24.506303	76.730855
45.212981	20.382499	76.735860
44.743267	17.094099	76.740865
43.711381	20.923346	76.745870
42.906433	19.763539	76.750874
42.266023	20.986902	76.755879
41.600386	21.149920	76.760884
41.605566	21.445622	76.765889
40.866262	22.741525	76.770894
39.964240	23.825280	76.775898
39.160088	22.720536	76.780903
38.543338	24.952458	76.785908
38.073528	16.933550	76.790913
37.240259	18.225520	76.795918
36.663993	20.512481	76.800922
35.844068	16.330684	76.805927
35.295618	26.814361	76.810932
34.536621	15.035086	76.815937
33.593258	22.352381	76.820942
33.155785	18.153734	76.825946
32.933404	20.737462	76.830951
32.381368	19.486859	76.835956
31.527125	23.149014	76.840961
30.886074	34.021179	76.845966
30.076803	27.254814	76.850970
29.286391	21.382667	76.855975
28.483749	29.139536	76.860980
28.125882	16.058458	76.865985
27.757298	9.395262	76.870990
26.707596	20.782000	76.875994
25.988389	26.127184	76.880999
25.509870	16.643206	76.886004
24.601066	13.432734	76.891009
23.428136	22.530636	76.896014
23.030246	12.418833	76.901018
22.680704	19.888974	76.906023
22.269480	23.847871	76.911028
21.785320	14.339566	76.916033
20.705751	25.633309	76.921038
20.030579	15.862180	76.926042
19.441739	29.950654	76.931047
18.944695	21.568688	76.936052
18.047771	20.067195	76.941057
17.084481	25.843949	76.946062
16.631115	24.941860	76.951066
16.602872	23.096812	76.956071
15.643709	12.817515	76.961076
14.969833	18.305268	76.966081
14.329340	23.543288	76.971086
13.658352	24.667464	76.976090
12.371877	23.067273	76.981095
11.609764	16.214557	76.986100
11.374085	16.909775	76.991105
11.321683	20.984888	76.996110
10.753705	26.843655	77.001114
9.571581	25.512229	77.006119
8.964689	20.383468	77.011124
8.534627	14.900097	77.016129
6.992357	21.693237	77.021134
6.480038	18.116772	77.026139
6.079856	16.466664	77.031143
5.762332	23.359308	77.036148
5.117141	16.145768	77.041153
4.207550	19.253829	77.046158