Mon Mar 08 19:47:01 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.485489	110.222888	0.000000
-0.785219	80.028371	0.005005
-1.516684	52.108785	0.010010
-3.059111	-10.289864	0.015014
-7.271234	-22.227910	0.020019
-12.963774	-24.998604	0.025024
-17.880947	-27.505062	0.030029
-22.569808	-27.067709	0.035034
-26.080664	-26.606960	0.040038
-30.393261	-17.736775	0.045043
-34.076650	-32.919082	0.050048
-37.441341	-27.629712	0.055053
-41.212510	-23.642610	0.060058
-44.993864	-24.922085	0.065062
-48.794448	-17.760839	0.070067
-52.510910	-18.856704	0.075072
-56.065244	-20.017847	0.080077
-60.243628	-19.124155	0.085082
-63.893903	-20.618462	0.090086
-67.661767	-18.027346	0.095091
-71.181033	-17.708682	0.100096
-75.032878	-18.836526	0.105101
-78.711116	-17.822335	0.110106
-82.541879	-19.883863	0.115110
-86.423106	-20.150780	0.120115
-90.006892	-28.037103	0.125120
-93.929806	-16.327605	0.130125
-97.664702	-21.889208	0.135130
-101.069725	-22.929037	0.140134
-105.126586	-16.296057	0.145139
-108.563591	-29.912333	0.150144
-112.598178	-23.555689	0.155149
-116.734487	-11.298059	0.160154
-120.172077	-28.466834	0.165158
-123.845426	-9.624088	0.170163
-127.484333	-28.093157	0.175168
-131.283989	-21.147965	0.180173
-135.511999	-24.798545	0.185178
-138.940909	-31.063287	0.190182
-143.042582	-28.322608	0.195187
-146.713653	-32.801567	0.200192
-150.475973	-21.488169	0.205197
-154.735309	-19.644759	0.210202
-158.192715	-16.297281	0.215206
-161.908202	-22.718099	0.220211
-165.581088	-13.829923	0.225216
-168.946083	-23.778846	0.230221
-173.237318	-25.402500	0.235226
-176.479551	-31.025244	0.240230
-180.727135	-18.722956	0.245235
-184.357603	-27.940413	0.250240
-187.652981	-28.623906	0.255245
-191.942585	-17.070195	0.260250
-195.106632	-32.577940	0.265254
-199.165376	-12.516202	0.270259
-202.731136	-28.287814	0.275264
-206.852168	-20.125942	0.280269
-210.790782	-25.866146	0.285274
-214.181618	-21.843293	0.290278
-218.439173	-20.753782	0.295283
-221.847325	-26.958642	0.300288
-225.310745	-31.396507	0.305293
-229.410225	-22.938441	0.310298
-232.846422	-34.003332	0.315302
-236.945068	-28.899309	0.320307
-240.677794	-24.156432	0.325312
-244.388010	-23.947378	0.330317
-248.749722	-20.376602	0.335322
-251.665033	-21.011867	0.340326
-255.659937	-20.260656	0.345331
-259.462721	-23.718706	0.350336
-262.891503	-27.654305	0.355341
-266.934755	-18.055642	0.360346
-270.738267	-22.357163	0.365350
-274.961812	-19.751339	0.370355
-278.430217	-21.829392	0.375360
-282.153789	-23.016798	0.380365
-285.992948	-21.626551	0.385370
-289.279765	-16.658330	0.390374
-293.301432	-10.342876	0.395379
-296.960236	-15.925768	0.400384
-300.828637	-21.003722	0.405389
-304.778641	-16.167719	0.410394
-308.269500	-24.650385	0.415398
-312.323151	-19.189170	0.420403
-315.756890	-19.609146	0.425408
-319.558921	-15.400668	0.430413
-323.754787	-16.799598	0.435418
-326.839449	-25.227239	0.440422
-331.074410	-14.787378	0.445427
-334.819963	-20.775797	0.450432
-338.115582	-16.506220	0.455437
-342.256944	-21.207817	0.460442
-346.069629	-29.058770	0.465446
-349.725496	-20.903125	0.470451
-353.553788	-23.136484	0.475456
-357.137513	-23.576606	0.480461
-360.926975	-30.440992	0.485466
-364.805640	-20.728114	0.490470
-368.683833	-14.001818	0.495475
-372.652884	-22.449037	0.500480
-376.378284	-19.190921	0.505485
-380.262229	-21.580919	0.510490
-383.483974	-27.110457	0.515494
-387.254423	-17.542544	0.520499
-390.585445	-23.691666	0.525504
-394.720022	-29.993154	0.530509
-399.143412	-13.387653	0.535514
-402.383627	-26.930818	0.540518
-406.017841	-29.579825	0.545523
-409.770844	-24.641083	0.550528
-413.704096	-21.770736	0.555533
-417.741129	-21.775714	0.560538
-421.113847	-25.956557	0.565542
-424.875761	-19.083176	0.570547
-429.107416	-25.898917	0.575552
-432.401264	-26.771537	0.580557
-436.055800	-18.141353	0.585562
-439.797764	-24.929624	0.590566
-443.975587	-25.697336	0.595571
-447.885780	-17.027887	0.600576
-451.291525	-21.346904	0.605581
-455.422565	-23.924382	0.610586
-458.588591	-20.490561	0.615590
-462.606458	-18.037096	0.620595
-466.316224	-23.504353	0.625600
-470.104396	-17.651648	0.630605
-474.221492	-24.536060	0.635610
-477.810989	-30.697385	0.640614
-481.725889	-23.116722	0.645619
-485.119421	-6.661350	0.650624
-488.848643	-29.357041	0.655629
-492.888336	-21.746969	0.660634
-496.312872	-15.346797	0.665638
-500.099485	-23.964843	0.670643
-504.014748	-20.917464	0.675648
-507.787817	-16.692823	0.680653
-511.907883	-18.461466	0.685658
-515.278462	-29.459135	0.690662
-518.879256	-20.424289	0.695667
-522.936377	-20.430612	0.700672
-526.666943	-27.185869	0.705677
-530.613078	-14.030785	0.710682
-533.885661	-24.826479	0.715686
-537.572090	-16.061755	0.720691
-541.241589	-26.672624	0.725696
-545.055218	-27.788466	0.730701
-549.110750	-28.941350	0.735706
-552.835597	-34.644153	0.740710
-556.740700	-13.983588	0.745715
-560.644247	-26.059756	0.750720
-564.118968	-23.987749	0.755725
-568.243637	-16.028115	0.760730
-571.795337	-27.785180	0.765734
-575.586519	-22.417498	0.770739
-579.605293	-20.353170	0.775744
-582.835334	-25.259832	0.780749
-586.576949	-17.506428	0.785754
-590.185441	-26.759852	0.790758
-593.937302	-22.707188	0.795763
-598.003925	-23.028807	0.800768
-601.872948	-28.065156	0.805773
-606.085673	-11.912398	0.810778
-609.682652	-20.666203	0.815782
-613.155683	-20.350979	0.820787
-616.898605	-26.374043	0.825792
-620.314494	-21.931925	0.830797
-624.382325	-16.702880	0.835802
-627.758210	-27.365243	0.840806
-631.875857	-26.926506	0.845811
-635.815794	-25.568483	0.850816
-639.279748	-29.374912	0.855821
-643.407825	-27.225212	0.860826
-646.991860	-28.336573	0.865830
-650.785736	-10.610766	0.870835
-654.468539	-10.772857	0.875840
-658.259567	-27.561037	0.880845
-661.982305	-14.518713	0.885850
-665.740583	-30.512658	0.890854
-669.425786	-22.717688	0.895859
-673.548350	-22.550884	0.900864
-676.962628	-31.677513	0.905869
-680.856384	-20.019098	0.910874
-684.283313	-27.995769	0.915878
-688.544380	-24.831341	0.920883
-692.121210	-19.054642	0.925888
-695.655509	-28.726569	0.930893
-699.819400	-19.596758	0.935898
-703.202638	-29.505682	0.940902
-707.070716	-22.569186	0.945907
-711.102558	-22.490924	0.950912
-714.396138	-20.064478	0.955917
-718.634657	-20.232274	0.960922
-722.051090	-29.134582	0.965926
-726.006783	-14.314128	0.970931
-729.730707	-26.986354	0.975936
-733.362430	-25.388866	0.980941
-737.468437	-25.188329	0.985946
-740.908994	-21.178881	0.990950
-744.748023	-19.898300	0.995955
-748.491307	-23.149035	1.000960
-752.220186	-24.869395	1.005965
-755.868913	-22.159072	1.010970
-759.609619	-23.935871	1.015974
-763.580480	-19.748605	1.020979
-767.338145	-21.111132	1.025984
-771.290071	-30.604236	1.030989
-775.181156	-10.065435	1.035994
-778.430135	-21.441654	1.040998
-782.383145	-25.105055	1.046003
-786.258967	-14.975706	1.051008
-789.878878	-26.374612	1.056013
-793.703074	-22.133475	1.061018
-797.410136	-20.727257	1.066022
-801.187467	-22.488676	1.071027
-804.746721	-26.325352	1.076032
-808.615593	-18.368365	1.081037
-812.667628	-15.727520	1.086042
-816.170087	-33.155996	1.091046
-819.849903	-24.458149	1.096051
-823.662588	-31.403196	1.101056
-827.510504	-27.484617	1.106061
-831.303321	-23.931201	1.111066
-834.959296	-23.856044	1.116070
-839.137545	-18.963777	1.121075
-842.896952	-31.352612	1.126080
-846.008949	-23.229577	1.131085
-850.300560	-10.658968	1.136090
-853.598836	-22.454511	1.141094
-857.347846	-21.894555	1.146099
-861.166492	-18.087823	1.151104
-864.843932	-18.318246	1.156109
-869.187502	-23.599953	1.161114
-872.855458	-25.653106	1.166118
-876.714879	-17.878858	1.171123
-880.146361	-19.435263	1.176128
-883.936624	-33.201964	1.181133
-887.730473	-27.950060	1.186138
-891.418406	-20.859164	1.191142
-895.249459	-21.071287	1.196147
-898.847573	-31.486402	1.201152
-902.530340	-30.511224	1.206157
-906.351541	-24.412895	1.211162
-910.061303	-28.523362	1.216166
-913.807873	-24.234527	1.221171
-918.007668	-30.270770	1.226176
-921.464099	-25.225712	1.231181
-925.469374	-23.337989	1.236186
-929.109373	-20.166789	1.241190
-932.815836	-25.818301	1.246195
-936.700745	-25.387863	1.251200
-940.124469	-22.810999	1.256205
-944.307218	-19.217130	1.261210
-947.836874	-26.426403	1.266214
-951.517482	-19.234094	1.271219
-955.566086	-16.043245	1.276224
-959.106007	-21.839607	1.281229
-963.036186	-27.127317	1.286234
-966.428680	-23.263994	1.291238
-969.966946	-14.044553	1.296243
-974.500307	-23.524739	1.301248
-978.032331	-31.947732	1.306253
-981.805287	-23.591113	1.311258
-985.692600	-24.528889	1.316262
-989.283000	-35.386595	1.321267
-993.188637	-14.299583	1.326272
-996.809003	-29.370480	1.331277
-1000.731205	-23.025636	1.336282
-1004.245030	-23.794471	1.341286
-1007.852090	-26.874196	1.346291
-1012.221538	-28.072261	1.351296
-1015.636204	-30.004859	1.356301
-1019.495516	-18.189022	1.361306
-1022.825104	-29.376947	1.366310
-1026.753184	-20.199155	1.371315
-1030.414665	-28.735391	1.376320
-1034.081466	-25.395758	1.381325
-1038.356081	-26.419722	1.386330
-1042.062947	-25.339555	1.391334
-1045.834537	-28.309334	1.396339
-1049.573344	-28.419273	1.401344
-1052.887121	-40.431192	1.406349
-1057.031950	-17.971851	1.411354
-1060.768934	-32.511517	1.416358
-1064.202055	-28.821317	1.421363
-1068.340190	-25.675877	1.426368
-1072.037891	-27.395978	1.431373
-1075.719757	-16.422075	1.436378
-1079.370327	-35.660251	1.441382
-1083.598024	-18.996603	1.446387
-1087.019980	-21.533428	1.451392
-1090.473204	-42.282197	1.456397
-1094.618602	-20.726227	1.461402
-1098.711071	-21.954244	1.466406
-1102.267338	-26.047954	1.471411
-1106.230701	-33.868777	1.476416
-1109.073140	-42.140111	1.481421
-1112.936511	-28.322514	1.486426
-1117.183322	-32.089709	1.491430
-1121.202239	-30.464377	1.496435
-1125.221305	-16.249715	1.501440
-1128.312439	-43.737313	1.506445
-1132.068357	-21.475685	1.511450
-1135.752989	-27.964489	1.516454
-1139.793243	-28.387148	1.521459
-1143.720489	-11.251112	1.526464
-1147.277128	-23.782238	1.531469
-1150.889907	-24.093510	1.536474
-1154.861506	-26.819818	1.541478
-1158.539289	-24.411710	1.546483
-1161.883740	-26.908787	1.551488
-1165.663755	-23.781053	1.556493
-1170.055281	-8.696239	1.561498
-1173.722171	-24.544648	1.566502
-1177.467628	-30.660982	1.571507
-1181.191010	-22.614738	1.576512
-1184.651413	-26.078739	1.581517
-1188.609062	-19.114538	1.586522
-1192.233926	-19.970968	1.591526
-1195.797586	-19.755490	1.596531
-1199.727208	-24.315965	1.601536
-1203.637307	-26.648362	1.606541
-1208.065889	-23.918212	1.611546
-1211.505211	-29.001778	1.616550
-1214.783753	-24.624953	1.621555
-1218.556341	-16.935021	1.626560
-1221.929351	-34.504936	1.631565
-1226.032632	-22.727013	1.636570
-1230.024405	-30.148866	1.641574
-1233.961558	-20.437909	1.646579
-1237.992202	-18.422603	1.651584
-1241.211223	-22.929576	1.656589
-1244.998775	-19.311696	1.661594
-1248.615321	-30.272014	1.666598
-1252.216996	-33.213452	1.671603
-1256.566937	-15.725781	1.676608
-1259.935650	-21.214780	1.681613
-1264.032376	-18.681121	1.686618
-1267.544969	-20.999761	1.691622
-1271.020996	-31.167315	1.696627
-1274.730810	-32.136164	1.701632
-1278.783366	-24.078089	1.706637
-1283.044892	-15.179231	1.711642
-1286.667764	-23.374322	1.716646
-1290.517664	-14.323729	1.721651
-1293.851538	-21.374567	1.726656
-1297.158056	-39.357081	1.731661
-1301.389428	-9.570250	1.736666
-1304.922437	-18.229088	1.741670
-1309.119321	-5.059476	1.746675
-1313.013454	-11.768328	1.751680
-1316.423537	-16.637241	1.756685
-1320.254839	-17.354781	1.761690
-1324.108360	-26.747535	1.766694
-1327.666376	-28.117454	1.771699
-1331.827761	-18.971214	1.776704
-1335.448130	-22.713705	1.781709
-1339.353160	-22.583701	1.786714
-1342.897864	-25.236099	1.791718
-1346.540866	-25.774019	1.796723
-1350.465164	-22.640239	1.801728
-1353.477025	-21.997228	1.806733
-1357.836568	-21.010762	1.811738
-1361.326660	-29.086644	1.816742
-1365.053089	-23.846358	1.821747
-1369.214661	-21.008848	1.826752
-1372.871597	-23.543894	1.831757
-1376.939721	-18.597364	1.836762
-1380.512432	-25.750171	1.841766
-1384.116711	-27.415343	1.846771
-1387.931189	-27.364402	1.851776
-1391.282349	-23.656892	1.856781
-1395.838355	-20.450289	1.861786
-1399.050051	-18.889059	1.866790
-1403.153520	-14.928639	1.871795
-1407.148782	-15.667090	1.876800
-1410.425641	-25.405879	1.881805
-1414.334209	-13.885874	1.886810
-1417.953720	-24.962119	1.891814
-1421.965233	-11.273271	1.896819
-1425.591925	-19.625203	1.901824
-1428.995931	-30.190351	1.906829
-1433.184316	-6.514029	1.911834
-1436.695255	-17.388454	1.916838
-1440.422119	-14.101646	1.921843
-1444.488004	-11.591531	1.926848
-1447.888118	-21.190693	1.931853
-1452.228851	-21.790179	1.936858
-1456.068050	-13.847960	1.941862
-1459.380095	-28.972154	1.946867
-1463.679683	-6.350209	1.951872
-1466.836181	-35.982300	1.956877
-1470.482151	-10.686671	1.961882
-1473.974179	-17.044921	1.966886
-1477.963818	-19.171742	1.971891
-1481.961122	-8.272872	1.976896
-1485.510312	-20.951268	1.981901
-1489.604264	-8.838534	1.986906
-1493.236909	-26.976658	1.991910
-1496.973051	-21.587966	1.996915
-1501.228145	-5.124692	2.006912
-1501.910696	-14.434565	2.016909
-1499.432227	-19.908849	2.026906
-1496.538735	-16.383953	2.036902
-1494.231697	-9.765365	2.046899
-1492.496360	-22.455881	2.056896
-1490.926696	-16.120238	2.066893
-1488.819523	-13.868259	2.076890
-1486.550815	-14.555085	2.086886
-1484.905734	-19.108067	2.096883
-1483.176252	-17.869208	2.106880
-1481.398875	-13.837173	2.116877
-1479.203969	-21.558489	2.126874
-1477.461883	-18.640191	2.136870
-1475.246169	-20.118986	2.146867
-1473.419680	-16.210064	2.156864
-1471.722221	-12.376787	2.166861
-1469.989938	-16.313770	2.176858
-1467.864372	-23.160353	2.186854
-1465.582764	-23.366102	2.196851
-1464.062249	-19.802887	2.206848
-1462.310595	-21.335250	2.216845
-1460.698205	-19.607134	2.226842
-1458.400548	-22.054226	2.236838
-1456.513536	-18.331810	2.246835
-1454.572126	-15.568557	2.256832
-1452.809267	-24.152181	2.266829
-1451.119731	-15.172215	2.276826
-1449.081825	-15.089472	2.286822
-1446.907724	-24.441517	2.296819
-1445.190355	-21.051903	2.306816
-1443.360580	-21.444214	2.316813
-1441.795859	-17.600714	2.326810
-1439.792360	-22.272626	2.336806
-1437.717998	-22.451481	2.346803
-1435.879152	-15.757871	2.356800
-1434.065843	-20.160925	2.366797
-1432.043425	-21.706619	2.376794
-1430.060110	-15.001400	2.386790
-1428.459051	-29.497080	2.396787
-1426.197546	-24.873091	2.406784
-1424.468880	-29.654133	2.416781
-1422.609739	-24.237880	2.426778
-1420.748750	-25.225653	2.436774
-1419.145777	-21.773496	2.446771
-1417.259561	-26.870262	2.456768
-1415.320853	-23.934452	2.466765
-1413.336294	-22.352722	2.476762
-1411.189584	-29.363679	2.486758
-1409.458821	-18.767245	2.496755
-1407.638978	-21.540393	2.506752
-1405.725210	-14.625084	2.516749
-1403.762266	-20.176199	2.526746
-1402.185835	-21.153135	2.536742
-1400.157267	-19.066898	2.546739
-1398.008674	-21.287977	2.556736
-1396.141002	-23.328301	2.566733
-1394.652986	-16.635329	2.576730
-1392.690624	-16.174154	2.586726
-1390.600708	-18.047963	2.596723
-1388.775305	-19.096325	2.606720
-1387.247471	-16.669407	2.616717
-1385.426742	-17.855955	2.626714
-1382.957989	-20.860851	2.636710
-1381.180282	-13.912686	2.646707
-1379.382456	-20.387806	2.656704
-1377.691170	-18.605949	2.666701
-1375.796521	-19.711172	2.676698
-1373.788724	-15.892764	2.686694
-1371.831506	-20.509848	2.696691
-1369.976783	-26.648302	2.706688
-1368.169080	-17.440887	2.716685
-1366.703174	-16.863904	2.726682
-1364.202070	-24.537826	2.736678
-1362.442632	-16.254189	2.746675
-1360.710695	-19.771069	2.756672
-1358.810642	-12.859837	2.766669
-1356.951906	-17.486406	2.776666
-1355.105798	-18.748041	2.786662
-1353.247619	-27.310542	2.796659
-1351.223089	-16.667928	2.806656
-1349.413995	-17.663126	2.816653
-1347.736805	-18.223555	2.826650
-1345.665299	-11.724989	2.836646
-1343.772087	-18.422180	2.846643
-1341.932885	-18.651721	2.856640
-1340.219166	-7.509372	2.866637
-1337.942411	-12.586496	2.876634
-1335.967171	-24.188029	2.886630
-1334.455139	-23.586833	2.896627
-1332.622567	-17.209475	2.906624
-1330.790778	-22.984257	2.916621
-1328.815424	-18.772224	2.926618
-1326.833798	-20.364979	2.936614
-1324.960220	-23.639260	2.946611
-1323.435156	-20.682946	2.956608
-1321.227004	-8.936086	2.966605
-1319.131866	-20.536276	2.976602
-1317.375600	-18.635310	2.986598
-1315.719711	-20.325908	2.996595
-1313.595365	-18.862773	3.006592
-1312.035193	-17.790880	3.016589
-1309.793755	-19.669923	3.026586
-1308.211754	-11.450989	3.036582
-1305.836745	-24.592693	3.046579
-1304.514782	-16.496338	3.056576
-1302.728593	-17.034709	3.066573
-1300.543005	-21.637764	3.076570
-1298.776447	-25.194874	3.086566
-1296.847813	-24.856105	3.096563
-1294.801893	-23.314089	3.106560
-1293.170666	-26.118537	3.116557
-1291.117281	-16.326734	3.126554
-1288.959305	-25.022429	3.136550
-1287.463139	-27.497385	3.146547
-1285.882938	-19.767587	3.156544
-1283.784621	-15.812017	3.166541
-1281.998496	-18.232331	3.176538
-1279.594500	-16.122390	3.186534
-1278.098088	-18.799471	3.196531
-1276.282921	-20.071880	3.206528
-1274.411472	-18.959785	3.216525
-1272.559966	-14.361590	3.226522
-1270.659059	-16.421346	3.236518
-1268.787768	-18.591614	3.246515
-1266.596292	-23.907634	3.256512
-1264.957365	-21.992585	3.266509
-1263.071158	-18.640900	3.276506
-1261.283169	-19.782642	3.286502
-1259.262743	-16.452432	3.296499
-1257.197049	-15.936630	3.306496
-1255.724808	-16.877849	3.316493
-1253.907842	-20.379841	3.326490
-1251.494076	-15.205340	3.336486
-1250.143261	-23.163983	3.346483
-1248.151810	-15.823627	3.356480
-1246.290342	-19.639029	3.366477
-1244.109366	-19.397435	3.376474
-1242.535656	-11.947593	3.386470
-1240.306810	-12.318349	3.396467
-1238.358064	-15.506706	3.406464
-1236.854043	-14.349992	3.416461
-1235.189888	-17.195985	3.426458
-1233.138276	-17.865191	3.436454
-1230.884064	-13.803473	3.446451
-1229.093549	-18.068528	3.456448
-1227.434364	-18.095501	3.466445
-1225.609348	-17.340646	3.476442
-1223.809347	-17.601714	3.486438
-1221.864618	-17.964880	3.496435
-1219.927758	-17.316332	3.506432
-1218.083413	-15.243080	3.516429
-1215.916845	-10.682620	3.526426
-1214.279336	-17.779293	3.536422
-1212.415520	-17.076422	3.546419
-1210.477815	-17.484242	3.556416
-1208.533559	-11.944059	3.566413
-1206.492373	-13.194164	3.576410
-1204.929241	-14.563549	3.586406
-1203.177274	-17.085700	3.596403
-1201.221557	-21.429269	3.606400
-1199.488659	-18.116152	3.616397
-1197.150567	-14.795665	3.626394
-1195.703182	-15.963379	3.636390
-1193.629575	-20.960497	3.646387
-1191.683353	-21.652275	3.656384
-1189.799151	-17.225020	3.666381
-1187.905102	-22.802833	3.676378
-1186.147306	-24.050204	3.686374
-1184.379835	-16.781312	3.696371
-1182.247616	-21.396248	3.706368
-1180.557855	-18.087266	3.716365
-1178.874869	-16.657590	3.726362
-1176.599802	-12.251810	3.736358
-1174.897939	-17.419946	3.746355
-1172.923050	-22.126534	3.756352
-1171.278626	-14.485863	3.766349
-1169.158667	-18.453083	3.776346
-1167.385026	-12.857147	3.786342
-1165.328598	-19.125614	3.796339
-1163.351772	-22.883625	3.806336
-1161.745130	-23.579464	3.816333
-1159.866123	-10.592487	3.826330
-1158.035301	-19.565711	3.836326
-1156.111088	-25.045701	3.846323
-1154.293777	-14.682347	3.856320
-1152.233412	-15.626021	3.866317
-1150.286892	-14.568463	3.876314
-1148.823923	-19.030513	3.886310
-1146.913155	-12.450781	3.896307
-1144.776680	-18.886763	3.906304
-1143.047808	-26.553754	3.916301
-1141.174267	-23.130471	3.926298
-1139.166821	-25.188219	3.936294
-1137.054112	-28.307993	3.946291
-1135.671698	-22.567348	3.956288
-1133.523195	-23.788771	3.966285
-1131.758979	-23.853003	3.976282
-1129.721491	-18.810791	3.986278
-1127.805949	-21.455364	3.996275
-1126.004900	-26.031479	4.006272
-1124.393759	-24.285556	4.016269
-1122.269728	-21.030214	4.026266
-1120.268137	-21.067679	4.036262
-1118.627355	-27.564855	4.046259
-1116.649700	-24.145576	4.056256
-1114.931464	-24.854499	4.066253
-1112.848058	-18.292883	4.076250
-1111.262695	-24.752771	4.086246
-1109.125357	-20.605924	4.096243
-1107.180547	-22.028407	4.106240
-1105.068073	-22.753023	4.116237
-1103.687226	-22.629601	4.126234
-1101.722578	-21.079148	4.136230
-1099.828034	-20.505830	4.146227
-1098.195911	-20.788890	4.156224
-1096.247804	-18.417948	4.166221
-1094.132342	-19.733517	4.176218
-1092.100994	-20.298313	4.186214
-1090.445063	-18.718992	4.196211
-1088.668718	-24.048970	4.206208
-1086.681905	-24.035099	4.216205
-1084.932195	-24.273805	4.226202
-1082.688478	-19.736610	4.236198
-1080.672382	-15.191420	4.246195
-1079.285656	-17.471913	4.256192
-1077.290390	-17.850938	4.266189
-1075.336436	-21.406286	4.276186
-1073.366078	-29.050282	4.286182
-1071.718875	-24.840791	4.296179
-1069.777810	-22.145040	4.306176
-1067.712433	-27.345983	4.316173
-1066.271581	-23.651337	4.326170
-1064.062791	-26.634848	4.336166
-1062.191851	-23.564742	4.346163
-1060.311468	-29.882323	4.356160
-1058.626240	-29.387590	4.366157
-1056.767850	-24.245618	4.376154
-1054.709421	-22.250683	4.386150
-1053.087522	-21.998430	4.396147
-1050.862270	-22.752087	4.406144
-1049.072540	-21.909349	4.416141
-1047.206295	-27.233152	4.426138
-1045.410201	-24.979950	4.436134
-1043.608307	-22.942396	4.446131
-1041.734423	-26.306501	4.456128
-1039.651546	-25.621160	4.466125
-1038.006244	-26.392568	4.476122
-1035.718942	-24.429485	4.486118
-1034.238181	-25.774531	4.496115
-1032.374210	-24.880501	4.506112
-1030.402145	-24.330576	4.516109
-1028.323994	-35.709935	4.526106
-1026.578174	-27.597513	4.536102
-1024.631062	-35.439842	4.546099
-1023.103700	-20.615578	4.556096
-1020.979450	-21.174645	4.566093
-1019.308754	-27.123949	4.576090
-1017.396151	-42.262868	4.586086
-1015.125246	-23.422544	4.596083
-1013.227808	-33.779903	4.606080
-1011.731214	-28.223217	4.616077
-1009.797316	-25.450484	4.626074
-1007.563962	-22.678274	4.636070
-1005.953788	-22.027825	4.646067
-1004.174165	-24.410579	4.656064
-1002.299058	-32.392947	4.666061
-1000.146406	-26.666452	4.676058
-998.369211	-32.563303	4.686054
-996.823526	-26.717635	4.696051
-994.786321	-22.783598	4.706048
-992.926127	-25.032397	4.716045
-990.861226	-30.032687	4.726042
-989.172840	-19.487530	4.736038
-987.275677	-15.417411	4.746035
-985.250730	-21.949099	4.756032
-983.379044	-27.977886	4.766029
-981.803210	-17.520504	4.776026
-979.654021	-29.189066	4.786022
-977.932901	-28.974731	4.796019
-976.078646	-32.826665	4.806016
-973.994502	-18.986594	4.816013
-972.131533	-24.974509	4.826010
-970.380039	-27.929016	4.836006
-968.569546	-25.082834	4.846003
-966.619942	-25.577611	4.856000
-964.684683	-34.791590	4.865997
-963.006865	-28.438117	4.875994
-960.570865	-30.095328	4.885990
-958.690067	-28.633969	4.895987
-957.284714	-24.150472	4.905984
-955.468150	-21.674698	4.915981
-953.611903	-29.262465	4.925978
-951.461339	-25.204419	4.935974
-949.560280	-26.171387	4.945971
-947.746391	-19.473365	4.955968
-946.018381	-27.815832	4.965965
-944.247278	-26.984245	4.975962
-942.384848	-20.505544	4.985958
-940.241289	-20.183477	4.995955
-938.293014	-26.540245	5.005952
-936.645837	-29.356477	5.015949
-934.628601	-26.630161	5.025946
-932.892602	-18.737123	5.035942
-930.887089	-26.224013	5.045939
-928.884338	-31.918477	5.055936
-927.018286	-18.378199	5.065933
-925.279510	-20.635952	5.075930
-923.585579	-24.471687	5.085926
-921.504261	-28.211475	5.095923
-919.840221	-22.072063	5.105920
-917.849018	-24.649625	5.115917
-915.780794	-21.830397	5.125914
-914.068643	-23.787063	5.135910
-912.113128	-29.515012	5.145907
-910.398842	-26.088177	5.155904
-908.120716	-16.456656	5.165901
-906.557467	-31.872793	5.175898
-904.967530	-16.903707	5.185894
-902.773717	-25.846374	5.195891
-900.960167	-31.035335	5.205888
-898.836910	-14.751078	5.215885
-897.047169	-30.165532	5.225882
-895.287835	-17.779660	5.235878
-893.406159	-28.372824	5.245875
-891.517340	-27.774738	5.255872
-889.634726	-22.615972	5.265869
-887.874145	-24.168285	5.275866
-886.108865	-26.700228	5.285862
-884.044000	-16.780393	5.295859
-881.836525	-28.780281	5.305856
-880.422080	-24.558696	5.315853
-878.577461	-17.737641	5.325850
-876.497843	-17.774741	5.335846
-874.351416	-32.303634	5.345843
-872.684626	-23.280088	5.355840
-870.868689	-21.664613	5.365837
-869.016533	-18.723964	5.375834
-867.207612	-24.711057	5.385830
-865.381774	-20.883627	5.395827
-863.327061	-19.484726	5.405824
-861.308393	-17.143809	5.415821
-859.738110	-21.584956	5.425818
-857.534889	-27.718753	5.435814
-855.882304	-20.033354	5.445811
-854.052374	-28.261011	5.455808
-852.149997	-25.331535	5.465805
-850.228841	-25.169609	5.475802
-848.302914	-28.527677	5.485798
-846.199307	-28.742257	5.495795
-844.546445	-18.808626	5.505792
-842.680213	-25.617965	5.515789
-841.221098	-23.689655	5.525786
-839.177143	-24.931992	5.535782
-837.055224	-23.352772	5.545779
-834.920122	-30.700839	5.555776
-833.418448	-28.394091	5.565773
-831.792225	-26.694579	5.575770
-829.388583	-23.106315	5.585766
-827.580304	-34.587636	5.595763
-826.101075	-26.230340	5.605760
-823.865373	-24.506676	5.615757
-822.179016	-27.014905	5.625754
-820.146753	-24.732964	5.635750
-818.498663	-25.370464	5.645747
-816.209081	-25.685793	5.655744
-814.659684	-25.726501	5.665741
-813.052876	-21.115648	5.675738
-810.765430	-24.152552	5.685734
-808.735067	-27.263616	5.695731
-806.873270	-26.552202	5.705728
-805.358880	-24.683228	5.715725
-803.370910	-19.621747	5.725722
-801.420914	-25.383464	5.735718
-799.343821	-22.109264	5.745715
-797.787500	-20.111205	5.755712
-795.949386	-24.808264	5.765709
-793.846326	-22.870751	5.775706
-791.923689	-21.164906	5.785702
-790.192897	-25.604824	5.795699
-788.437589	-26.840453	5.805696
-786.771008	-25.546806	5.815693
-784.365269	-21.393604	5.825690
-782.604366	-27.317702	5.835686
-780.395293	-25.618158	5.845683
-779.176034	-23.270972	5.855680
-777.290883	-21.852789	5.865677
-775.160457	-23.033107	5.875674
-773.268948	-26.270361	5.885670
-771.383195	-19.522100	5.895667
-769.569935	-26.302396	5.905664
-767.684612	-15.152252	5.915661
-765.596202	-22.075989	5.925658
-763.867098	-27.080844	5.935654
-762.118588	-19.904879	5.945651
-760.188644	-23.650337	5.955648
-758.395121	-19.835023	5.965645
-756.349019	-21.079211	5.975642
-754.788440	-17.398758	5.985638
-752.642616	-23.005432	5.995635
-750.440201	-26.311302	6.005632
-749.027957	-22.630822	6.015629
-747.168723	-16.705615	6.025626
-745.142694	-16.591939	6.035622
-743.094952	-19.996234	6.045619
-741.349919	-20.560759	6.055616
-739.549609	-24.179702	6.065613
-737.821654	-17.128317	6.075610
-736.065799	-14.424783	6.085606
-734.136468	-21.528323	6.095603
-731.838215	-30.222290	6.105600
-729.988314	-13.439458	6.115597
-728.268120	-21.319518	6.125594
-726.605893	-31.785925	6.135590
-724.191871	-34.779819	6.145587
-722.658462	-24.778059	6.155584
-720.821865	-27.970184	6.165581
-718.739481	-23.373686	6.175578
-716.948222	-20.126359	6.185574
-715.321250	-23.401817	6.195571
-713.312305	-23.525368	6.205568
-711.543912	-16.077818	6.215565
-709.497613	-25.033066	6.225562
-707.497940	-21.970606	6.235558
-705.961836	-18.189898	6.245555
-704.117081	-26.040900	6.255552
-701.793256	-22.534476	6.265549
-700.279057	-20.914858	6.275546
-698.077525	-33.731485	6.285542
-696.305740	-28.655892	6.295539
-694.460174	-24.075210	6.305536
-692.587928	-20.755548	6.315533
-690.821680	-12.065087	6.325530
-688.831905	-19.233512	6.335526
-687.060954	-18.812203	6.345523
-684.965007	-24.142447	6.355520
-683.458030	-19.832894	6.365517
-681.589503	-16.746296	6.375514
-679.406681	-19.066933	6.385510
-677.262597	-20.105672	6.395507
-675.698345	-24.181028	6.405504
-673.897277	-18.979048	6.415501
-671.984238	-19.534052	6.425498
-670.394677	-22.727719	6.435494
-668.144320	-26.810072	6.445491
-666.249022	-21.141595	6.455488
-664.595260	-13.887255	6.465485
-662.392943	-15.953640	6.475482
-660.520147	-26.202620	6.485478
-658.999542	-24.980289	6.495475
-657.128574	-23.823409	6.505472
-655.317705	-22.064858	6.515469
-653.017748	-18.954018	6.525466
-651.246909	-23.720744	6.535462
-649.553690	-17.247910	6.545459
-647.547426	-20.293418	6.555456
-645.657228	-26.001255	6.565453
-643.642151	-23.961132	6.575450
-642.136872	-17.559311	6.585446
-640.188684	-22.944854	6.595443
-637.994811	-17.693504	6.605440
-636.298717	-28.763653	6.615437
-634.595257	-21.602490	6.625434
-632.592963	-21.945949	6.635430
-630.637455	-22.300877	6.645427
-628.879919	-22.341561	6.655424
-627.126236	-25.071979	6.665421
-624.955061	-24.231439	6.675418
-623.420410	-24.075468	6.685414
-621.172460	-33.039178	6.695411
-619.317928	-22.038710	6.705408
-617.601577	-24.278451	6.715405
-615.655612	-18.387513	6.725402
-613.788868	-18.428266	6.735398
-611.844408	-23.625308	6.745395
-610.036866	-19.520028	6.755392
-608.215128	-24.648517	6.765389
-606.368436	-16.163458	6.775386
-604.574765	-27.626522	6.785382
-602.686374	-17.397183	6.795379
-600.673803	-25.210192	6.805376
-598.826592	-28.358135	6.815373
-596.907577	-17.904752	6.825370
-595.017997	-22.763036	6.835366
-593.130633	-26.668920	6.845363
-591.245858	-22.937519	6.855360
-589.640951	-27.055630	6.865357
-587.525590	-22.664791	6.875354
-585.646321	-21.479181	6.885350
-583.734882	-26.165696	6.895347
-581.818772	-24.425479	6.905344
-579.881530	-26.515756	6.915341
-578.312702	-23.477509	6.925338
-576.753418	-21.857118	6.935334
-574.576753	-20.692165	6.945331
-572.497858	-23.081362	6.955328
-570.615097	-20.732689	6.965325
-568.723812	-28.808911	6.975322
-566.843846	-23.363675	6.985318
-564.992545	-28.294763	6.995315
-563.072319	-27.469339	7.005312
-561.179932	-23.584402	7.015309
-559.293984	-30.706141	7.025306
-557.395382	-17.794357	7.035302
-555.636938	-28.696009	7.045299
-553.764915	-29.283838	7.055296
-552.042280	-25.021275	7.065293
-550.290416	-20.946525	7.075290
-548.164459	-25.499921	7.085286
-546.029891	-25.910221	7.095283
-544.450996	-30.148877	7.105280
-542.708166	-26.917361	7.115277
-540.516418	-26.916817	7.125274
-538.978838	-24.762442	7.135270
-536.846792	-24.790251	7.145267
-534.780807	-25.052227	7.155264
-533.180931	-22.922008	7.165261
-531.457265	-23.473493	7.175258
-529.213982	-27.811943	7.185254
-527.590967	-22.684030	7.195251
-525.291461	-23.963760	7.205248
-524.049119	-24.719397	7.215245
-522.286766	-21.263629	7.225242
-519.916127	-22.439459	7.235238
-518.265433	-26.015400	7.245235
-516.008671	-24.716355	7.255232
-514.393305	-26.109422	7.265229
-512.522673	-20.001112	7.275226
-510.648548	-21.591811	7.285222
-508.616632	-25.913852	7.295219
-506.739307	-22.471698	7.305216
-505.084595	-20.858605	7.315213
-503.061698	-23.625617	7.325210
-501.179250	-21.699968	7.335206
-499.218205	-23.718198	7.345203
-497.580512	-16.986919	7.355200
-495.907616	-30.500492	7.365197
-493.839020	-28.817712	7.375194
-491.787529	-31.780320	7.385190
-489.735172	-24.985798	7.395187
-488.187655	-22.266170	7.405184
-486.224065	-20.492406	7.415181
-484.210307	-21.207021	7.425178
-482.565316	-22.792682	7.435174
-480.449897	-30.494135	7.445171
-478.711012	-23.636910	7.455168
-476.916080	-20.833636	7.465165
-474.693646	-20.304281	7.475162
-473.282524	-18.852778	7.485158
-471.428849	-22.882657	7.495155
-469.289064	-15.784726	7.505152
-467.419010	-20.047730	7.515149
-465.773284	-12.621436	7.525146
-463.752172	-16.643316	7.535142
-461.607201	-14.759558	7.545139
-459.832260	-26.622147	7.555136
-458.191241	-20.491332	7.565133
-456.132186	-24.252438	7.575130
-454.511975	-26.944052	7.585126
-452.356902	-14.407838	7.595123
-450.510243	-26.948148	7.605120
-448.974371	-20.565287	7.615117
-446.790723	-18.109834	7.625114
-444.833164	-25.834997	7.635110
-442.969412	-18.784535	7.645107
-441.460227	-25.732352	7.655104
-439.339475	-27.013453	7.665101
-437.467056	-15.823053	7.675098
-435.541104	-14.646356	7.685094
-433.608714	-20.731808	7.695091
-431.769846	-29.634772	7.705088
-429.877949	-15.935531	7.715085
-428.323687	-24.789892	7.725082
-425.782200	-22.456293	7.735078
-424.402272	-25.608435	7.745075
-422.484624	-20.129621	7.755072
-420.345078	-23.682512	7.765069
-418.679722	-23.027839	7.775066
-417.057342	-16.038280	7.785062
-415.117674	-22.926934	7.795059
-413.086749	-21.004397	7.805056
-410.951182	-19.516961	7.815053
-409.445412	-17.044807	7.825050
-407.289910	-18.711933	7.835046
-405.414757	-12.179539	7.845043
-403.655517	-21.137667	7.855040
-401.793277	-17.015690	7.865037
-399.943146	-16.564180	7.875034
-397.944677	-21.472861	7.885030
-396.195619	-20.976791	7.895027
-394.249606	-24.748216	7.905024
-392.211939	-15.385625	7.915021
-390.587421	-23.381238	7.925018
-388.944602	-19.858915	7.935014
-386.786129	-26.733538	7.945011
-384.742669	-19.839606	7.955008
-382.986435	-27.493108	7.965005
-381.419191	-24.522363	7.975002
-379.138299	-18.138409	7.984998
-377.380047	-27.508438	7.994995
-375.349247	-15.913822	8.004992
-373.678639	-18.656060	8.014989
-371.612935	-23.087591	8.024986
-370.008910	-19.251184	8.034982
-368.014148	-20.291070	8.044979
-366.075872	-17.824786	8.054976
-364.268482	-19.251570	8.064973
-362.699271	-17.689458	8.074970
-360.591919	-17.536336	8.084966
-358.830564	-25.097489	8.094963
-356.559580	-21.481232	8.104960
-354.491418	-23.091738	8.114957
-353.061089	-20.544349	8.124954
-351.354447	-13.700815	8.134950
-349.185665	-22.981642	8.144947
-347.395589	-17.430294	8.154944
-345.561806	-24.123582	8.164941
-343.638307	-24.500006	8.174938
-341.944193	-23.003608	8.184934
-339.776532	-26.669858	8.194931
-338.053723	-19.533652	8.204928
-336.097095	-24.572964	8.214925
-334.533602	-13.825753	8.224922
-332.468038	-13.416476	8.234918
-330.410029	-16.222110	8.244915
-328.540633	-20.109141	8.254912
-326.532920	-21.406834	8.264909
-325.225332	-17.564123	8.274906
-323.107305	-13.039257	8.284902
-320.912275	-24.586744	8.294899
-319.091889	-15.317283	8.304896
-317.392011	-23.291728	8.314893
-315.414389	-25.331404	8.324890
-313.220770	-18.601893	8.334886
-311.853509	-9.318506	8.344883
-309.944208	-19.304679	8.354880
-308.255331	-23.917569	8.364877
-306.068754	-12.466163	8.374874
-304.079767	-19.199989	8.384870
-302.297731	-21.364740	8.394867
-300.424961	-18.709534	8.404864
-298.609057	-10.793991	8.414861
-296.607180	-14.807931	8.424858
-294.883156	-17.222348	8.434854
-293.048609	-22.717375	8.444851
-291.022776	-19.972917	8.454848
-289.215475	-14.765302	8.464845
-287.089686	-23.557667	8.474842
-285.523244	-20.054655	8.484838
-283.714273	-19.714899	8.494835
-281.962620	-26.933421	8.504832
-280.047203	-25.893855	8.514829
-277.824830	-18.889442	8.524826
-275.932749	-19.196065	8.534822
-274.314357	-18.150134	8.544819
-272.179487	-24.384619	8.554816
-270.258551	-22.900690	8.564813
-268.623861	-19.454346	8.574810
-266.722369	-20.322956	8.584807
-264.893429	-20.400032	8.594803
-263.087151	-26.582061	8.604800
-260.969389	-22.562330	8.614797
-258.953532	-17.433766	8.624794
-257.328136	-18.090942	8.634791
-255.753669	-23.746524	8.644787
-253.643241	-19.474578	8.654784
-251.728847	-12.567813	8.664781
-249.806875	-19.554570	8.674778
-247.656350	-25.586283	8.684775
-246.200323	-12.330423	8.694771
-244.130262	-22.727448	8.704768
-242.200008	-23.687465	8.714765
-240.711486	-20.312504	8.724762
-238.651079	-18.403994	8.734759
-236.501666	-20.016316	8.744755
-234.722397	-16.578812	8.754752
-232.928240	-18.481780	8.764749
-231.260034	-17.247992	8.774746
-228.827108	-29.818574	8.784743
-227.006824	-24.557724	8.794739
-225.284568	-19.207020	8.804736
-223.753522	-25.973480	8.814733
-221.620245	-29.760448	8.824730
-219.738967	-23.498863	8.834727
-218.025767	-23.914252	8.844723
-215.935157	-20.587997	8.854720
-214.102349	-22.983406	8.864717
-212.244188	-25.708102	8.874714
-210.439682	-17.050188	8.884711
-208.757161	-28.476321	8.894707
-206.720055	-27.309283	8.904704
-204.271561	-25.953701	8.914701
-203.169728	-22.668574	8.924698
-201.113307	-24.861252	8.934695
-199.161481	-25.625743	8.944691
-197.554450	-24.320594	8.954688
-195.609565	-25.532369	8.964685
-193.391241	-22.466461	8.974682
-191.793095	-23.547114	8.984679
-189.585927	-24.344451	8.994675
-187.799378	-29.732275	9.004672
-186.159968	-18.356054	9.014669
-184.228357	-21.291386	9.024666
-182.230210	-26.796653	9.034663
-180.219136	-24.836013	9.044659
-178.238081	-32.583674	9.054656
-176.637516	-23.545844	9.064653
-174.927328	-18.534207	9.074650
-173.273927	-23.199766	9.084647
-170.811935	-22.924659	9.094643
-168.963052	-26.612521	9.104640
-167.489872	-23.266641	9.114637
-165.610692	-16.317870	9.124634
-163.555007	-15.265858	9.134631
-161.493145	-25.978859	9.144627
-159.744801	-28.141289	9.154624
-157.835245	-16.708683	9.164621
-155.941428	-24.357153	9.174618
-154.162250	-20.332241	9.184615
-151.974456	-15.360481	9.194611
-150.442809	-15.592126	9.204608
-148.421742	-18.203831	9.214605
-146.792357	-21.577197	9.224602
-144.750200	-20.450383	9.234599
-143.008634	-25.508915	9.244595
-140.951589	-22.292494	9.254592
-138.991569	-27.960581	9.264589
-137.120615	-27.567450	9.274586
-135.384560	-25.349744	9.284583
-133.618171	-27.306626	9.294579
-131.615731	-28.315967	9.304576
-129.582356	-23.344812	9.314573
-127.948843	-22.792218	9.324570
-126.193563	-21.272267	9.334567
-123.950247	-24.800413	9.344563
-122.137049	-20.078313	9.354560
-120.305585	-19.659922	9.364557
-118.414010	-16.944416	9.374554
-116.713581	-24.230444	9.384551
-115.082074	-17.936810	9.394547
-112.806805	-25.376127	9.404544
-110.854769	-24.446472	9.414541
-109.253871	-26.932689	9.424538
-107.160722	-24.795619	9.434535
-105.150354	-27.374004	9.444531
-103.325628	-32.351043	9.454528
-101.497423	-19.225510	9.464525
-99.732276	-23.517295	9.474522
-97.785575	-27.719629	9.484519
-96.084290	-30.981282	9.494515
-94.202287	-30.425680	9.504512
-92.242048	-32.906062	9.514509
-90.704075	-30.601461	9.524506
-88.520334	-27.697296	9.534503
-86.517384	-21.057137	9.544499
-84.738784	-28.227728	9.554496
-82.796063	-26.060322	9.564493
-81.200549	-24.780097	9.574490
-79.064025	-33.627688	9.584487
-76.932236	-25.421329	9.594483
-75.246212	-32.176114	9.604480
-73.569158	-15.478755	9.614477
-71.585508	-33.302999	9.624474
-69.681749	-27.090661	9.634471
-67.808806	-20.829194	9.644467
-65.785838	-28.065598	9.654464
-64.161411	-27.276261	9.664461
-62.377860	-24.286124	9.674458
-60.484638	-22.791289	9.684455
-58.465402	-21.742845	9.694451
-56.340414	-23.606888	9.704448
-54.673305	-25.874700	9.714445
-52.847665	-18.880979	9.724442
-50.791678	-15.586944	9.734439
-49.208264	-21.182258	9.744435
-47.327896	-19.581157	9.754432
-45.316849	-23.020079	9.764429
-43.111407	-22.351832	9.774426
-41.673418	-27.423444	9.784423
-39.745397	-22.901164	9.794419
-37.985270	-28.153627	9.804416
-35.952055	-23.180784	9.814413
-33.991251	-19.045811	9.824410
-32.429443	-26.006534	9.834407
-30.141425	-27.231863	9.844403
-28.547769	-24.617174	9.854400
-26.596335	-25.780915	9.864397
-24.571043	-23.282442	9.874394
-22.817602	-24.239345	9.884391
-21.019253	-19.462693	9.894387
-19.071645	-29.407407	9.904384
-17.278092	-24.659988	9.914381
-15.508347	-20.674513	9.924378
-13.130105	-24.184611	9.934375
-11.672736	-29.851368	9.944371
-9.462305	-30.964834	9.954368
-7.559831	-30.033505	9.964365
-5.952314	-23.420195	9.974362
-4.793104	-6.188612	9.984359
-3.682894	41.050734	9.994355
-2.229621	97.062965	10.004352
-0.822733	172.982959	10.014349
0.000000	242.321226	10.019354
0.702603	284.458226	10.024359
1.480181	330.858296	10.029363
1.896472	362.403599	10.034368
2.292910	381.064290	10.039373
2.926941	426.451554	10.044378
3.141438	442.104264	10.049383
3.331336	464.336541	10.054387
3.824350	483.997478	10.059392
3.887919	479.114807	10.064397
3.745273	493.264992	10.069402
4.110153	497.138048	10.074407
4.483230	518.056023	10.079411
4.274051	537.255044	10.084416
4.680475	545.707104	10.089421
4.389240	548.048005	10.094426
4.633624	541.747225	10.099431
4.408483	555.666210	10.104435
4.203838	545.895334	10.109440
4.859371	545.213693	10.114445
4.392430	564.557939	10.119450
4.832424	554.066092	10.124455
4.903006	548.379637	10.129459
4.481957	558.345051	10.134464
5.041323	590.426253	10.139469
4.678576	580.805147	10.144474
5.281976	601.416855	10.149479
5.237158	599.929160	10.154483
5.191769	588.259493	10.159488
5.371076	600.762605	10.164493
5.097394	618.248466	10.169498
5.436308	603.767365	10.174503
5.661291	603.540736	10.179507
5.397740	619.178427	10.184512
5.426962	609.863777	10.189517
5.518911	619.682756	10.194522
5.446408	612.262425	10.199527
5.510572	628.577962	10.204531
5.312616	627.084729	10.209536
5.552642	617.569299	10.214541
5.412054	623.688104	10.219546
5.582992	630.457370	10.224551
5.808330	629.691381	10.229555
5.688243	623.163280	10.234560
5.988213	617.355058	10.239565
5.556975	626.793880	10.244570
5.878945	623.256046	10.249575
5.822124	626.452099	10.254579
5.649225	634.873616	10.259584
6.157224	644.120064	10.264589
6.005440	654.924087	10.269594
6.132159	662.397415	10.274599
6.446318	659.647697	10.279603
6.015788	683.970908	10.284608
6.267161	669.541551	10.289613
6.307287	663.348990	10.294618
6.324751	685.353650	10.299623
6.374796	670.270447	10.304627
6.550027	679.131613	10.309632
6.756365	661.732236	10.314637
6.606256	699.461800	10.319642
6.659068	674.047786	10.324647
6.755506	685.660620	10.329651
6.466438	695.761191	10.334656
6.644662	687.810410	10.339661
6.501747	688.858260	10.344666
6.690841	682.853237	10.349671
6.460295	681.628540	10.354675
6.332846	696.074536	10.359680
6.818088	700.519792	10.364685
7.099709	711.469190	10.369690
7.228269	712.472165	10.374695
7.463499	709.000184	10.379699
7.410978	722.866565	10.384704
7.513169	711.031337	10.389709
7.036758	698.056835	10.394714
7.181278	714.164115	10.399719
7.039387	714.886959	10.404723
7.080050	715.246379	10.409728
7.167509	731.870546	10.414733
7.179382	727.972150	10.419738
7.049441	730.232161	10.424743
7.477714	719.098682	10.429747
7.132857	752.340003	10.434752
7.410326	729.067788	10.439757
7.387881	769.798547	10.444762
7.966431	733.547544	10.449767
7.916216	779.522862	10.454771
8.118810	748.155597	10.459776
8.068394	766.198946	10.464781
7.965127	750.141921	10.469786
7.637862	737.083673	10.474791
7.926032	765.122723	10.479795
7.964044	773.182680	10.484800
8.099274	778.812864	10.489805
7.988405	787.779653	10.494810
8.071148	773.490628	10.499815
7.974989	771.219489	10.504819
7.975204	789.893445	10.509824
8.247871	788.632631	10.514829
8.162491	789.671311	10.519834
8.240839	779.587063	10.524839
8.398798	776.561045	10.529843
8.201034	791.959774	10.534848
8.560599	768.300670	10.539853
8.667725	775.999528	10.544858
8.642806	784.876913	10.549863
8.517452	781.411967	10.554867
8.246168	786.660725	10.559872
8.821376	805.813837	10.564877
8.600384	793.791973	10.569882
8.739608	813.014634	10.574887
9.264049	810.873158	10.579891
9.262859	812.034028	10.584896
9.231293	795.377323	10.589901
8.864790	801.251543	10.594906
9.080067	780.133784	10.599911
9.159579	785.474820	10.604915
9.164966	781.582175	10.609920
9.412894	767.470231	10.614925
9.229948	776.374394	10.619930
9.200130	786.534600	10.624935
9.377997	786.496830	10.629939
9.263794	783.324990	10.634944
9.472168	789.856552	10.639949
9.265483	795.441932	10.644954
9.337607	789.876560	10.649959
9.564803	801.039707	10.654963
9.635342	811.381040	10.659968
9.258423	812.163452	10.664973
9.599952	826.886431	10.669978
9.392074	828.140192	10.674983
10.067145	827.362386	10.679987
9.960602	816.265251	10.684992
9.925536	817.188678	10.689997
9.875614	827.117157	10.695002
9.661919	824.905757	10.700007
10.218249	827.247131	10.705011
9.709804	827.187942	10.710016
10.280850	815.826618	10.715021
10.291163	833.934481	10.720026
10.237632	826.003243	10.725031
9.960748	833.591496	10.730035
10.010141	829.319663	10.735040
10.356108	818.905701	10.740045
9.981535	835.773989	10.745050
10.235010	836.586741	10.750055
10.256615	832.675725	10.755059
10.019507	837.699857	10.760064
10.134672	835.675695	10.765069
10.314268	840.385785	10.770074
10.525072	853.060709	10.775079
10.996728	863.382255	10.780083
10.714026	863.823218	10.785088
10.824562	846.713286	10.790093
10.471110	851.221399	10.795098
10.598075	860.784225	10.800103
11.076577	869.327480	10.805107
10.626409	870.589928	10.810112
10.673222	870.227713	10.815117
10.814207	869.599745	10.820122
11.091834	875.563643	10.825127
11.063413	876.240011	10.830131
10.897156	873.360302	10.835136
11.244653	869.225411	10.840141
10.784275	872.451192	10.845146
11.087568	876.360983	10.850151
11.223712	869.561669	10.855155
11.174778	868.169219	10.860160
11.488406	868.697992	10.865165
11.627181	866.507636	10.870170
11.796015	864.200524	10.875175
11.700166	865.136802	10.880179
11.407153	870.149361	10.885184
11.825464	859.397406	10.890189
11.494788	863.769428	10.895194
11.415564	866.527566	10.900199
11.620719	865.663862	10.905203
11.735538	867.850163	10.910208
11.908734	869.982998	10.915213
11.831978	870.228688	10.920218
11.853177	874.300165	10.925223
12.015510	874.476183	10.930227
11.742157	879.163914	10.935232
12.236376	867.584571	10.940237
12.026366	878.200931	10.945242
12.112014	871.791288	10.950247
12.076578	872.046157	10.955251
12.094688	869.747315	10.960256
12.375905	881.327680	10.965261
12.177794	888.647934	10.970266
12.364862	888.179770	10.975271
12.176372	882.151312	10.980275
12.565053	902.792970	10.985280
12.832427	894.831010	10.990285
12.352876	902.544663	10.995290
12.501615	909.812759	11.000295
12.800552	900.683559	11.005299
12.581853	897.454245	11.010304
12.515909	881.318582	11.015309
12.747615	897.932549	11.020314
13.451784	891.153011	11.025319
12.581617	884.192500	11.030323
12.554016	886.081401	11.035328
12.974051	888.685797	11.040333
12.824440	897.412830	11.045338
12.952745	904.949108	11.050343
12.926728	899.527080	11.055347
12.918142	906.982692	11.060352
13.077573	910.330394	11.065357
12.728633	916.588208	11.070362
13.066856	904.412403	11.075367
13.025073	909.372290	11.080371
12.951984	918.795176	11.085376
13.203532	913.942300	11.090381
13.175704	912.491286	11.095386
13.410965	927.406358	11.100391
13.715038	927.687501	11.105395
13.353534	938.244490	11.110400
13.885020	930.368118	11.115405
13.441200	923.226047	11.120410
13.476032	921.373957	11.125415
13.600825	929.320812	11.130419
13.757530	950.305464	11.135424
13.752649	938.643245	11.140429
14.014561	937.734215	11.145434
13.770635	935.890315	11.150439
13.766391	945.360585	11.155443
13.770242	951.161601	11.160448
14.128032	944.948215	11.165453
13.852188	941.127190	11.170458
13.864790	944.717514	11.175463
14.438657	942.615445	11.180467
14.297187	953.738165	11.185472
14.043459	949.557221	11.190477
13.843621	943.528969	11.195482
13.961753	937.014769	11.200487
14.282559	945.094371	11.205491
13.993045	946.023697	11.210496
14.200685	953.678233	11.215501
14.470006	964.872635	11.220506
14.597154	966.798366	11.225511
14.738584	976.551348	11.230515
14.555790	985.214341	11.235520
14.877905	972.895969	11.240525
15.101715	965.876048	11.245530
14.658319	954.400452	11.250535
14.892738	941.127852	11.255539
14.736707	947.302872	11.260544
14.740718	936.899212	11.265549
14.429183	949.091411	11.270554
15.099363	959.447595	11.275559
15.402360	965.047940	11.280563
15.115753	968.935150	11.285568
15.249887	963.959060	11.290573
15.141715	955.325265	11.295578
15.344084	967.285703	11.300583
15.013687	946.666319	11.305587
15.041299	960.665225	11.310592
15.331962	968.992498	11.315597
15.198148	973.426193	11.320602
15.422110	975.998800	11.325607
15.554650	972.211978	11.330611
14.985662	975.451950	11.335616
15.623699	969.441436	11.340621
15.657090	972.228940	11.345626
15.805253	964.415266	11.350631
15.677904	968.874737	11.355635
15.659067	955.029086	11.360640
15.923231	967.902180	11.365645
15.584685	974.360210	11.370650
15.578967	975.015616	11.375655
15.518726	976.018761	11.380659
15.679807	979.326793	11.385664
15.452332	968.513756	11.390669
15.587505	981.609285	11.395674
15.917474	994.229058	11.400679
15.793201	992.799726	11.405683
15.879171	1001.867715	11.410688
16.015578	1014.322836	11.415693
16.374723	1014.659852	11.420698
16.128063	1007.129902	11.425703
16.475870	1002.547072	11.430707
16.227754	1009.500048	11.435712
16.518673	1001.482236	11.440717
16.386929	1000.320599	11.445722
16.511320	1001.515071	11.450727
16.948119	1002.066782	11.455731
16.721919	1012.646398	11.460736
17.022548	993.601020	11.465741
16.750458	1007.409654	11.470746
16.920504	1008.188415	11.475751
17.109725	994.645431	11.480755
16.866256	995.785035	11.485760
17.156249	1001.448970	11.490765
17.188503	1004.733400	11.495770
16.838246	994.551783	11.500775
17.125556	990.776541	11.505779
16.911398	997.843944	11.510784
17.393624	997.096889	11.515789
17.110069	977.936549	11.520794
17.155423	983.470763	11.525799
17.269296	982.186375	11.530803
17.182207	996.856467	11.535808
17.306955	997.509988	11.540813
17.551335	999.847532	11.545818
17.274623	994.873882	11.550823
17.315611	992.290675	11.555827
17.064985	1006.728241	11.560832
17.310994	1004.140717	11.565837
17.433058	1005.179442	11.570842
17.186842	1015.390093	11.575847
17.561670	1010.386636	11.580851
17.406269	1008.235295	11.585856
17.189890	1001.477953	11.590861
17.895759	1009.347942	11.595866
17.577451	1009.692086	11.600871
17.904000	1010.311844	11.605875
17.796523	1028.859783	11.610880
17.855239	1019.060773	11.615885
17.977904	1026.555437	11.620890
17.932965	1024.017469	11.625895
18.291024	1022.325124	11.630899
18.218661	1023.276590	11.635904
18.293098	1017.898419	11.640909
18.357477	1017.937098	11.645914
18.316991	1014.791295	11.650919
18.169357	1021.742443	11.655923
18.227090	1024.483497	11.660928
18.289443	1017.770000	11.665933
18.419206	1013.283445	11.670938
18.186295	1018.065695	11.675943
18.556108	1009.615827	11.680947
18.926583	1022.265434	11.685952
18.658603	1013.879442	11.690957
18.558046	1014.575207	11.695962
18.537089	1035.862710	11.700967
18.670578	1004.859148	11.705971
18.474628	1046.952460	11.710976
18.836051	1019.293500	11.715981
18.789391	1026.728439	11.720986
18.271841	1045.326035	11.725991
18.836819	1018.658052	11.730995
18.618875	1035.140468	11.736000
18.920031	1050.910905	11.741005
18.955794	1043.966670	11.746010
19.201621	1049.027389	11.751015
19.292284	1052.215782	11.756019
19.138335	1050.316515	11.761024
19.607969	1055.153881	11.766029
19.710992	1044.527771	11.771034
19.447194	1034.713958	11.776039
19.617100	1023.430646	11.781043
19.497952	1031.421197	11.786048
19.608641	1011.634960	11.791053
19.513170	1023.040555	11.796058
19.535524	1022.907741	11.801063
19.873466	1008.727590	11.806067
19.350446	1017.189401	11.811072
19.604559	1015.835334	11.816077
19.575337	1023.862000	11.821082
19.517717	1050.359308	11.826087
19.792989	1048.870976	11.831091
19.739116	1050.044998	11.836096
19.993063	1039.122008	11.841101
19.873164	1044.565908	11.846106
19.933450	1048.350503	11.851111
20.026605	1052.675481	11.856115
19.931051	1060.523513	11.861120
19.984177	1039.551088	11.866125
19.705160	1040.518168	11.871130
19.459284	1056.345897	11.876135
19.785026	1058.195811	11.881139
19.952780	1078.414065	11.886144
20.342035	1082.259740	11.891149
20.092878	1083.412872	11.896154
20.245209	1086.481050	11.901159
20.515459	1076.641955	11.906163
20.519966	1078.992539	11.911168
20.521108	1090.125733	11.916173
20.636475	1080.442226	11.921178
20.640946	1076.710496	11.926183
20.775610	1075.851716	11.931187
20.568191	1086.206040	11.936192
20.586043	1075.703878	11.941197
20.885345	1079.556015	11.946202
20.641659	1077.328858	11.951207
20.790922	1071.541340	11.956211
20.824437	1086.420945	11.961216
21.090269	1107.834700	11.966221
21.009468	1109.288990	11.971226
21.469069	1104.782915	11.976231
21.634591	1094.006452	11.981235
21.677496	1094.660416	11.986240
21.587017	1072.715786	11.991245
21.523406	1077.594056	11.996250
21.456973	1075.696597	12.001255
21.665230	1065.246076	12.006259
21.196039	1068.263569	12.011264
21.353337	1072.401704	12.016269
21.562976	1077.047157	12.021274
21.524907	1077.603648	12.026279
21.541732	1069.886559	12.031283
21.408509	1082.011006	12.036288
21.457339	1074.914861	12.041293
21.431863	1071.124831	12.046298
21.431315	1077.453303	12.051303
21.424525	1071.135586	12.056307
21.562559	1077.451417	12.061312
21.749721	1074.406488	12.066317
21.357343	1070.317008	12.071322
21.367825	1077.121538	12.076327
21.520438	1078.537020	12.081331
21.484112	1081.365627	12.086336
21.727364	1080.511605	12.091341
21.545307	1075.765681	12.096346
21.295753	1081.200312	12.101351
21.463777	1080.139091	12.106355
21.290771	1081.324232	12.111360
21.563537	1077.499248	12.116365
21.387086	1080.220894	12.121370
21.377177	1081.085131	12.126375
21.380501	1077.862941	12.131379
21.493235	1077.081775	12.136384
21.671109	1078.285070	12.141389
21.596540	1078.893114	12.146394
21.364515	1084.780691	12.151399
21.739438	1082.107937	12.156403
21.521421	1085.187875	12.161408
21.893482	1089.307531	12.166413
21.889774	1085.689067	12.171418
21.733001	1077.012488	12.176423
21.807953	1056.123290	12.181427
21.384356	1057.589671	12.186432
21.711980	1051.683827	12.191437
21.694136	1055.976048	12.196442
21.325883	1054.625047	12.201447
21.452710	1057.047582	12.206451
21.322935	1056.579486	12.211456
21.438691	1058.585894	12.216461
21.403196	1060.154379	12.221466
21.409415	1061.140622	12.226471
21.826657	1054.512430	12.231475
21.439065	1060.361731	12.236480
21.153370	1055.479379	12.241485
21.561884	1057.163126	12.246490
21.406452	1059.961841	12.251495
21.784186	1062.853714	12.256499
21.785520	1051.594113	12.261504
21.779292	1055.477627	12.266509
21.679397	1051.483429	12.271514
21.770843	1065.765570	12.276519
22.020198	1059.350234	12.281523
21.527528	1067.244261	12.286528
21.746254	1054.437684	12.291533
21.596293	1036.667331	12.296538
21.560147	1040.451535	12.301543
21.311460	1029.837377	12.306547
21.611889	1019.704924	12.311552
21.595122	1022.366398	12.316557
21.542936	1027.122980	12.321562
21.757427	1030.556546	12.326567
21.777281	1020.705386	12.331571
21.455786	1027.091333	12.336576
21.557141	1020.221804	12.341581
21.566226	1019.319978	12.346586
21.182041	1026.148008	12.351591
21.422940	1030.086717	12.356595
21.295984	1024.119346	12.361600
21.491361	1024.588140	12.366605
21.503925	1039.289689	12.371610
21.192218	1033.301319	12.376615
21.637016	1031.577793	12.381619
21.327738	1031.731261	12.386624
21.290838	1035.428851	12.391629
21.484325	1032.622619	12.396634
21.292432	1036.641396	12.401639
21.351052	1039.268772	12.406643
21.557155	1043.131032	12.411648
21.693232	1035.221477	12.416653
21.769157	1041.097767	12.421658
21.550037	1038.483498	12.426663
21.490517	1037.162105	12.431667
21.590515	1034.804445	12.436672
21.618699	1031.977269	12.441677
21.589336	1027.938712	12.446682
21.256931	1033.665660	12.451687
21.448342	1034.004199	12.456691
21.320805	1036.284373	12.461696
21.416192	1042.140213	12.466701
21.221477	1033.245784	12.471706
21.328199	1040.344030	12.476711
21.707261	1035.082846	12.481715
21.707942	1032.181209	12.486720
21.758009	1039.173373	12.491725
21.834432	1030.789210	12.496730
21.843026	1041.681482	12.501735
21.744295	1029.785000	12.506739
21.614235	1034.659661	12.511744
21.545885	1035.667257	12.516749
21.676671	1038.229506	12.521754
21.571656	1041.993155	12.526759
21.366074	1036.055666	12.531763
21.745217	1040.495877	12.536768
21.794251	1040.458155	12.541773
21.597612	1020.970081	12.546778
21.253524	1027.208245	12.551783
21.610488	1021.050152	12.556787
21.352317	1011.300112	12.561792
21.332316	1013.949484	12.566797
21.321197	1022.786968	12.571802
21.472704	1028.334230	12.576807
21.514468	1025.804510	12.581811
21.599575	1034.957813	12.586816
21.309823	1027.628689	12.591821
21.580622	1029.238204	12.596826
21.574482	1034.216102	12.601831
21.419660	1025.039349	12.606835
21.723746	1015.507135	12.611840
21.346218	1018.386995	12.616845
21.453907	1011.741963	12.621850
21.332663	1011.854403	12.626855
21.539394	1022.133165	12.631859
21.035446	1025.017421	12.636864
21.320756	1031.651940	12.641869
21.934883	1032.446606	12.646874
21.737787	1051.713766	12.651879
21.868971	1029.117260	12.656883
21.655854	1023.545253	12.661888
21.458127	1021.668742	12.666893
21.536020	1017.195189	12.671898
21.317447	1029.713249	12.676903
21.950619	1013.929556	12.681907
21.571246	1022.059376	12.686912
21.467728	1021.099817	12.691917
21.832085	1023.385113	12.696922
21.557135	1025.551603	12.701927
21.596192	1025.895518	12.706931
21.367190	1033.342196	12.711936
21.434886	1027.129313	12.716941
21.194733	1025.686921	12.721946
21.240086	1017.720883	12.726951
21.820477	1021.742637	12.731955
21.674265	1022.849383	12.736960
21.727168	1028.000789	12.741965
21.357215	1020.630843	12.746970
21.475738	1031.950275	12.751975
21.719853	1026.106646	12.756979
21.552645	1023.417868	12.761984
21.519617	1028.616095	12.766989
21.871195	1031.846448	12.771994
21.519572	1042.133853	12.776999
21.836301	1033.090043	12.782003
21.159402	1010.704452	12.787008
20.968821	1005.368554	12.792013
21.364050	1024.724132	12.797018
21.437663	1025.508813	12.802023
21.502921	1030.357051	12.807027
21.405118	1031.787237	12.812032
21.494718	1032.905258	12.817037
21.820334	1025.131058	12.822042
21.598657	1033.757704	12.827047
21.749010	1023.863651	12.832051
21.585242	1027.013771	12.837056
21.640932	1010.751330	12.842061
21.561658	1000.070750	12.847066
21.491970	1005.560243	12.852071
21.515221	997.930477	12.857075
21.362602	998.923126	12.862080
21.123107	1011.217427	12.867085
21.648130	1010.725321	12.872090
21.421123	1006.554290	12.877095
21.648481	1000.314376	12.882099
21.413785	1005.338180	12.887104
21.464298	1009.198439	12.892109
21.581972	1004.614467	12.897114
21.380034	1006.662076	12.902119
21.762225	1013.850414	12.907123
21.408852	1012.055498	12.912128
21.588960	1004.963681	12.917133
21.652851	998.377680	12.922138
21.599743	1008.213752	12.927143
21.655144	998.528825	12.932147
21.780613	1001.781041	12.937152
21.957734	996.760237	12.942157
21.916370	1001.081424	12.947162
21.644719	1009.299712	12.952167
21.650649	998.444695	12.957171
21.335693	1005.974454	12.962176
21.572395	1000.310213	12.967181
21.896222	992.790203	12.972186
21.472002	989.060638	12.977191
21.711044	972.485146	12.982195
21.645254	974.525229	12.987200
21.508283	970.226308	12.992205
21.423171	961.022708	12.997210
21.457735	990.275894	13.002215
21.587299	968.905027	13.007219
21.611391	975.962804	13.012224
21.064786	968.580060	13.017229
21.243730	968.162075	13.022234
21.252793	978.344600	13.027239
21.337598	983.044626	13.032243
21.143714	982.712914	13.037248
21.491792	1003.522043	13.042253
21.502007	994.769994	13.047258
21.633709	1011.906243	13.052263
21.710845	1013.493029	13.057267
21.527436	1003.428295	13.062272
21.268838	991.869577	13.067277
21.748925	988.248092	13.072282
21.446961	985.915126	13.077287
21.429000	976.879000	13.082291
21.580532	978.704650	13.087296
21.154653	967.667793	13.092301
20.902588	984.275442	13.097306
21.130336	1003.227197	13.102311
21.576108	1000.027495	13.107315
21.461565	999.809284	13.112320
21.275836	1016.589315	13.117325
21.634067	1018.333117	13.122330
21.560616	1019.702648	13.127335
21.569956	1013.503809	13.132339
21.156799	1015.115177	13.137344
21.426477	1006.145119	13.142349
21.528020	1005.129200	13.147354
21.597846	1010.422979	13.152359
21.843428	1006.039379	13.157363
22.109296	1020.033459	13.162368
21.820785	1009.594402	13.167373
21.782761	981.843104	13.172378
21.368099	991.872448	13.177383
21.385509	990.636561	13.182387
21.373383	983.810379	13.187392
21.069911	983.762649	13.192397
21.137386	993.845983	13.197402
21.397163	1014.612441	13.202407
21.648720	1017.136500	13.207411
21.685859	1015.474842	13.212416
21.402920	1016.240696	13.217421
21.951809	1015.196005	13.222426
21.682702	1003.597953	13.227431
21.493992	992.969525	13.232435
21.241133	989.906485	13.237440
21.186523	989.741793	13.242445
21.551064	985.607306	13.247450
21.226176	989.768707	13.252455
21.861087	987.309969	13.257459
21.522822	987.181057	13.262464
20.914758	995.564956	13.267469
21.605718	1001.497676	13.272474
21.479288	1013.151051	13.277479
21.682555	1020.084078	13.282483
21.653294	1008.523462	13.287488
21.247202	988.379711	13.292493
21.444339	997.231272	13.297498
21.276336	1016.623055	13.302503
21.526746	1011.062279	13.307507
21.689016	1026.085290	13.312512
21.349802	1015.116575	13.317517
21.625903	1005.010090	13.322522
21.648712	1001.732770	13.327527
21.633071	991.636556	13.332531
21.505356	1001.553908	13.337536
21.471380	998.366070	13.342541
21.547342	984.539963	13.347546
21.367436	1003.547275	13.352551
21.524521	993.275278	13.357555
21.633333	989.840741	13.362560
21.651170	1002.691655	13.367565
21.552385	984.738162	13.372570
21.514174	987.966019	13.377575
21.416644	992.666744	13.382579
21.513642	1000.993386	13.387584
21.470442	987.224129	13.392589
21.444899	985.991939	13.397594
21.086004	991.338321	13.402599
21.241896	990.239618	13.407603
21.210289	992.056632	13.412608
21.275188	999.904271	13.417613
21.318677	1011.951589	13.422618
21.347077	1024.759836	13.427623
21.709666	1024.812453	13.432627
21.671869	1038.463901	13.437632
21.386134	1027.502416	13.442637
21.694168	1029.176955	13.447642
21.392080	1029.486972	13.452647
21.366536	1030.713245	13.457651
21.563595	1034.772488	13.462656
21.860609	1023.675483	13.467661
21.588792	1006.361418	13.472666
21.421811	1010.696335	13.477671
21.655084	1001.632739	13.482675
21.123259	1013.603085	13.487680
21.310517	1005.499302	13.492685
21.585557	995.773038	13.497690
21.411319	998.825475	13.502695
21.438955	995.601002	13.507699
21.568304	1002.796545	13.512704
21.646325	998.129013	13.517709
21.860072	999.006459	13.522714
21.580673	1018.963213	13.527719
21.478286	1002.784341	13.532723
21.289530	1014.327809	13.537728
21.403450	1001.925925	13.542733
21.512100	995.053667	13.547738
21.579564	1005.154356	13.552743
21.691296	1005.890379	13.557747
21.720055	1002.192641	13.562752
21.552153	1004.239552	13.567757
21.573054	1007.536833	13.572762
21.461806	1007.237672	13.577767
21.529710	1006.850012	13.582771
21.547561	1014.768241	13.587776
21.428859	1002.433420	13.592781
21.687940	997.241848	13.597786
21.389482	1005.559027	13.602791
21.310165	1001.082168	13.607795
21.713632	1009.184893	13.612800
21.744521	1008.399439	13.617805
21.589638	1001.771059	13.622810
21.390337	1014.557268	13.627815
21.938288	1006.339186	13.632819
22.017452	1007.309061	13.637824
21.817338	986.946380	13.642829
21.604195	972.819466	13.647834
21.483893	966.594016	13.652839
21.333429	979.055438	13.657843
21.479680	961.870288	13.662848
21.541632	974.182710	13.667853
21.515557	966.390517	13.672858
21.138177	971.503299	13.677863
21.105396	972.642412	13.682867
21.517759	982.000528	13.687872
21.221772	987.800497	13.692877
21.472963	984.740643	13.697882
21.389052	995.819522	13.702887
21.544774	1004.802272	13.707891
21.524554	1015.150342	13.712896
21.663924	1015.757377	13.717901
21.526177	981.938116	13.722906
21.131716	994.514161	13.727911
21.726267	993.042720	13.732915
21.448479	992.142496	13.737920
21.153156	1005.532213	13.742925
21.895672	1009.477644	13.747930
21.624840	1001.721316	13.752935
21.761671	987.757765	13.757939
21.238286	980.800240	13.762944
21.240393	983.103883	13.767949
21.459243	978.704054	13.772954
21.317750	982.484544	13.777959
21.474391	990.074695	13.782963
21.328913	1002.349263	13.787968
21.387922	1017.893358	13.792973
21.563166	1019.398264	13.797978
21.653601	1014.339240	13.802983
21.632521	1006.345957	13.807987
21.621016	983.844819	13.812992
21.337757	980.182659	13.817997
21.340240	973.322614	13.823002
21.220136	1001.176509	13.828007
21.326831	1004.633570	13.833011
21.291087	1009.035865	13.838016
21.157299	1012.192239	13.843021
21.303390	1016.122411	13.848026
21.371369	1021.758687	13.853031
21.605426	1016.418136	13.858035
21.353819	1023.735951	13.863040
21.120261	1029.491287	13.868045
21.588995	1017.286687	13.873050
21.242777	1016.930385	13.878055
21.707584	1014.358425	13.883059
21.884220	1016.210037	13.888064
21.343490	1023.253845	13.893069
21.666002	1026.320098	13.898074
21.588120	1028.264346	13.903079
21.567184	1020.051836	13.908083
21.590397	1017.389458	13.913088
21.433819	1024.381458	13.918093
21.762801	1018.872802	13.923098
21.519274	1032.364669	13.928103
21.493256	1018.346637	13.933107
21.595310	1021.468552	13.938112
21.698031	1021.124225	13.943117
21.891729	1015.542530	13.948122
21.693894	1010.146287	13.953127
21.414529	1000.584137	13.958131
21.505519	992.229212	13.963136
21.257430	990.532624	13.968141
21.390027	981.756333	13.973146
21.395964	992.992766	13.978151
21.680823	984.349883	13.983155
21.474412	983.351543	13.988160
21.615799	988.269626	13.993165
21.491608	986.709396	13.998170
21.404756	988.737070	14.003175
21.354890	985.067647	14.008179
21.368395	995.888139	14.013184
21.451830	986.700217	14.018189
21.495190	986.293209	14.023207
21.303701	995.333520	14.028224
21.467936	983.447543	14.033242
21.733907	993.773896	14.038259
21.523081	1000.269157	14.043277
21.452466	993.951033	14.048295
21.499536	1001.600584	14.053312
21.463370	998.199460	14.058330
21.521743	1004.645495	14.063347
21.413799	1024.267728	14.068365
21.627269	1024.738652	14.073383
21.567937	1023.368719	14.078400
21.967905	1016.826102	14.083418
21.846051	1023.233255	14.088435
21.764750	1034.330707	14.093453
21.811207	1022.089127	14.098471
21.820993	1027.445019	14.103488
21.571936	1029.405349	14.108506
21.773780	1040.143059	14.113523
21.846486	1028.545333	14.118541
22.173819	1029.182130	14.123559
21.587738	1027.405457	14.128576
21.693927	1032.436108	14.133594
22.034831	1027.205292	14.138611
21.812737	1029.952504	14.143629
21.713817	1033.453952	14.148647
21.668784	1032.463960	14.153664
21.675690	1031.160535	14.158682
21.943485	1022.803389	14.163699
21.823168	1031.780465	14.168717
21.790194	1034.563577	14.173735
21.664483	1045.589474	14.178752
21.873801	1035.206277	14.183770
21.879395	1023.642853	14.188787
21.936581	1047.808135	14.193805
21.798754	1056.371191	14.198823
22.278906	1055.709541	14.203840
21.915620	1062.957414	14.208858
22.419591	1056.824455	14.213875
22.330633	1067.275106	14.218893
22.146501	1068.841291	14.223911
22.070098	1070.066269	14.228928
22.179765	1064.928946	14.233946
22.267489	1058.745978	14.238963
21.759526	1067.202918	14.243981
22.084036	1058.644809	14.248999
22.229955	1065.938875	14.254016
22.090570	1063.390997	14.259034
22.465633	1063.968276	14.264051
22.096680	1068.779011	14.269069
22.264754	1066.998446	14.274087
22.570116	1066.633645	14.279104
22.356934	1070.573299	14.284122
22.353262	1059.577580	14.289139
22.323758	1058.328722	14.294157
22.343967	1066.262573	14.299175
22.371124	1067.342053	14.304192
22.240059	1061.985165	14.309210
22.596857	1085.338278	14.314227
22.485701	1098.804661	14.319245
22.855556	1098.701691	14.324263
22.545109	1076.101014	14.329280
22.467129	1072.368360	14.334298
22.611519	1088.103040	14.339315
22.568546	1099.913260	14.344333
22.510322	1094.415762	14.349351
22.679584	1106.758393	14.354368
22.569707	1103.589211	14.359386
22.710170	1100.781200	14.364403
22.312084	1103.193148	14.369421
22.644784	1104.271087	14.374439
22.999481	1102.641641	14.379456
22.731256	1103.022664	14.384474
22.780582	1099.906737	14.389491
22.670614	1100.550367	14.394509
22.571781	1100.243740	14.399527
22.823391	1105.389641	14.404544
22.528830	1104.035198	14.409562
22.862976	1098.025258	14.414579
22.529734	1118.536082	14.419597
22.693535	1099.961950	14.424615
22.755438	1107.182925	14.429632
22.733442	1127.625245	14.434650
23.478855	1123.092753	14.439667
23.187307	1128.193166	14.444685
23.348439	1119.788486	14.449703
23.015967	1102.388268	14.454720
22.872289	1105.118269	14.459738
22.985663	1100.488400	14.464755
23.123742	1114.764431	14.469773
23.212253	1125.760941	14.474791
23.545500	1110.093301	14.479808
22.924605	1112.067332	14.484826
23.023759	1098.365461	14.489843
22.916699	1114.198473	14.494861
23.046149	1114.604155	14.499879
23.089503	1119.312968	14.504896
23.210756	1121.115153	14.509914
23.431226	1122.006511	14.514931
23.575370	1127.094060	14.519949
23.533187	1116.886190	14.524967
23.552538	1121.221328	14.529984
23.408814	1119.120846	14.535002
23.830914	1113.346969	14.540019
23.606825	1110.538902	14.545037
23.847179	1103.348487	14.550055
23.341464	1098.592429	14.555072
22.994537	1099.421708	14.560090
23.314099	1097.138806	14.565107
23.290103	1105.914958	14.570125
23.617737	1118.347165	14.575143
23.589840	1120.786584	14.580160
23.195481	1123.671394	14.585178
23.675781	1114.220143	14.590195
23.585055	1131.022643	14.595213
23.534128	1121.816554	14.600231
23.557856	1121.968552	14.605248
23.874764	1122.485899	14.610266
23.722558	1117.314823	14.615283
23.420617	1125.913534	14.620301
23.691095	1124.519302	14.625319
23.933161	1118.409215	14.630336
24.052204	1127.236494	14.635354
23.891211	1119.458887	14.640371
23.786191	1124.850428	14.645389
23.866143	1127.996199	14.650407
23.910858	1126.968292	14.655424
23.619542	1119.467859	14.660442
23.752280	1116.118414	14.665459
23.488733	1117.981972	14.670477
23.464195	1123.904913	14.675495
23.819164	1124.315522	14.680512
23.442404	1123.803125	14.685530
23.438732	1117.707065	14.690547
23.478450	1137.722728	14.695565
23.756271	1153.371707	14.700583
23.965394	1160.433955	14.705600
23.855607	1155.902580	14.710618
23.841027	1161.433858	14.715635
23.969561	1165.679239	14.720653
24.144168	1154.003816	14.725671
24.324045	1150.266193	14.730688
24.001231	1157.421145	14.735706
24.120707	1158.245248	14.740723
24.238500	1156.718072	14.745741
24.237674	1156.107964	14.750759
24.608767	1155.361463	14.755776
24.080574	1157.713950	14.760794
24.322294	1159.478051	14.765811
24.645987	1160.739892	14.770829
24.350443	1163.317956	14.775847
24.733110	1153.608559	14.780864
24.339359	1158.015886	14.785882
24.598277	1153.318745	14.790899
24.813640	1149.704443	14.795917
24.444515	1154.765331	14.800935
24.766086	1144.546614	14.805952
24.371025	1133.792578	14.810970
24.407882	1133.648343	14.815987
24.482943	1147.879405	14.821005
24.461536	1142.934410	14.826023
24.973749	1143.923950	14.831040
24.396313	1147.401077	14.836058
24.266815	1147.015974	14.841075
24.601866	1146.989337	14.846093
24.627201	1155.729338	14.851111
24.784136	1145.112185	14.856128
24.302815	1148.706109	14.861146
24.885220	1138.873635	14.866163
24.780472	1145.076777	14.871181
24.597869	1156.567985	14.876199
24.980704	1145.380001	14.881216
24.655827	1143.410650	14.886234
24.571715	1147.741849	14.891251
24.826302	1150.831458	14.896269
24.378416	1155.204950	14.901287
25.072541	1152.462772	14.906304
24.491823	1148.663998	14.911322
24.766674	1149.221087	14.916339
24.789725	1154.073141	14.921357
24.734246	1160.336069	14.926375
25.018300	1143.274747	14.931392
24.759434	1146.616125	14.936410
24.878626	1147.871259	14.941427
25.016379	1139.374347	14.946445
25.031114	1156.826984	14.951463
25.246393	1148.441964	14.956480
25.089793	1146.252302	14.961498
25.246975	1153.632701	14.966515
25.349250	1130.305477	14.971533
24.940878	1144.615213	14.976551
25.113775	1142.882632	14.981568
25.108192	1145.804534	14.986586
24.982638	1152.913866	14.991603
25.392580	1159.443890	14.996621
25.171314	1163.376993	15.001639
25.218706	1171.765866	15.006656
25.570356	1166.190384	15.011674
25.135340	1169.429308	15.016691
25.428996	1158.642482	15.021709
25.289071	1175.278284	15.026727
25.486452	1178.089174	15.031744
25.332216	1174.768184	15.036762
25.622630	1183.590187	15.041779
25.755981	1173.190694	15.046797
25.477198	1158.941889	15.051815
25.528070	1142.461997	15.056832
25.611740	1148.548577	15.061850
25.309283	1146.899676	15.066867
25.607761	1150.852121	15.071885
25.397221	1176.501132	15.076903
25.587253	1169.627008	15.081920
25.450350	1170.661880	15.086938
25.638286	1175.536406	15.091955
25.487476	1169.471656	15.096973
25.364083	1168.407640	15.101991
25.572870	1168.635511	15.107008
25.818998	1167.399307	15.112026
25.868972	1163.303320	15.117043
26.133834	1164.300854	15.122061
25.889234	1168.069375	15.127079
25.894219	1164.778045	15.132096
25.752757	1173.944188	15.137114
25.987061	1155.105496	15.142131
26.340866	1164.637784	15.147149
26.085771	1172.060353	15.152167
25.968467	1160.544734	15.157184
26.041868	1163.818966	15.162202
25.647949	1163.576704	15.167219
25.988216	1150.753354	15.172237
25.640323	1162.832469	15.177255
25.893574	1166.726069	15.182272
26.092093	1161.690938	15.187290
26.114945	1160.721568	15.192307
26.461502	1160.416259	15.197325
26.067667	1160.045003	15.202343
26.003250	1163.927923	15.207360
26.367142	1164.300933	15.212378
26.156237	1169.679492	15.217395
26.221097	1166.299965	15.222413
26.152400	1172.992847	15.227431
26.202769	1170.748149	15.232448
26.158297	1168.907096	15.237466
25.974226	1171.594790	15.242483
26.156689	1159.045126	15.247501
26.273730	1174.582926	15.252519
26.167603	1162.054120	15.257536
26.340395	1170.279854	15.262554
26.185318	1170.679010	15.267571
26.129237	1164.382088	15.272589
26.284465	1180.848132	15.277607
26.896267	1192.624778	15.282624
26.552794	1179.632042	15.287642
26.595730	1167.828179	15.292659
26.553580	1163.693405	15.297677
26.202625	1168.161546	15.302695
26.662147	1180.410758	15.307712
26.816141	1187.725620	15.312730
26.473630	1208.793299	15.317747
26.595809	1189.602803	15.322765
26.459144	1206.195651	15.327783
26.579614	1201.841457	15.332800
26.421888	1194.006662	15.337818
26.411864	1197.534868	15.342835
26.749678	1189.655646	15.347853
26.644049	1189.844005	15.352871
27.025744	1186.516183	15.357888
26.824309	1195.916835	15.362906
26.443357	1202.967830	15.367923
27.137545	1190.347534	15.372941
27.189424	1189.489931	15.377959
26.992303	1202.152188	15.382976
26.990821	1185.388030	15.387994
27.054949	1203.938626	15.393011
27.114297	1185.640580	15.398029
26.817474	1196.270760	15.403047
27.126655	1197.484585	15.408064
27.051529	1190.648023	15.413082
26.914910	1192.474043	15.418099
27.178207	1194.621651	15.423117
27.156936	1191.919639	15.428135
27.097766	1207.447828	15.433152
27.244393	1185.508645	15.438170
26.701911	1197.249183	15.443187
27.160019	1194.495880	15.448205
27.323909	1216.211077	15.453223
27.373180	1214.406974	15.458240
27.360472	1204.853406	15.463258
27.257122	1201.588784	15.468275
27.444105	1209.135910	15.473293
27.317097	1206.197514	15.478311
27.375521	1211.345953	15.483328
27.816343	1215.190774	15.488346
27.342677	1201.045365	15.493363
27.827231	1197.418004	15.498381
27.555853	1197.662685	15.503399
27.810544	1196.930029	15.508416
27.777711	1190.925102	15.513434
27.712690	1204.296139	15.518451
27.816734	1188.087700	15.523469
27.454709	1184.829734	15.528487
27.437206	1189.889606	15.533504
27.890317	1181.240131	15.538522
27.573911	1190.920226	15.543539
27.586234	1189.982420	15.548557
27.467596	1182.935735	15.553575
27.486806	1187.484835	15.558592
27.918268	1198.164020	15.563610
27.545230	1201.792594	15.568627
27.672287	1210.730326	15.573645
27.987730	1218.381231	15.578663
27.872950	1215.286734	15.583680
28.182815	1210.567293	15.588698
28.079020	1222.672017	15.593715
28.575614	1197.133146	15.598733
27.964655	1188.916060	15.603751
27.982215	1183.717883	15.608768
28.388349	1182.559973	15.613786
28.236474	1180.553587	15.618803
27.945612	1173.575270	15.623821
28.033681	1185.248262	15.628839
27.835650	1180.914987	15.633856
27.785928	1179.677207	15.638874
28.288012	1173.988072	15.643891
28.483022	1203.669968	15.648909
28.154529	1191.244239	15.653927
27.890235	1191.777213	15.658944
28.493755	1200.192230	15.663962
28.427672	1204.147781	15.668979
28.269114	1206.144035	15.673997
28.253510	1202.203207	15.679015
28.126655	1202.706396	15.684032
28.576484	1211.279632	15.689050
28.247894	1207.574329	15.694067
28.764149	1213.484983	15.699085
28.312761	1210.895610	15.704103
28.326520	1210.232839	15.709120
28.398657	1198.278009	15.714138
28.076967	1211.063957	15.719155
28.448019	1211.619862	15.724173
28.520487	1216.309907	15.729191
28.375203	1211.666204	15.734208
28.474376	1212.638260	15.739226
28.491606	1212.840057	15.744243
28.419047	1207.011337	15.749261
28.408875	1213.212007	15.754279
28.144481	1231.042717	15.759296
28.763938	1239.807556	15.764314
28.426757	1247.892884	15.769331
28.838218	1238.666454	15.774349
28.683550	1243.340827	15.779367
28.702715	1254.082666	15.784384
29.408227	1242.695286	15.789402
28.993231	1226.605764	15.794419
29.192183	1246.641797	15.799437
29.405714	1236.015550	15.804455
29.564124	1230.521199	15.809472
29.518917	1215.093122	15.814490
29.323742	1217.452276	15.819507
29.439299	1200.949418	15.824525
28.911397	1202.833126	15.829543
28.810474	1200.787151	15.834560
29.176956	1196.022507	15.839578
29.256990	1206.397544	15.844595
29.578270	1196.636564	15.849613
29.568502	1197.325561	15.854631
29.072809	1204.297334	15.859648
29.445357	1202.591102	15.864666
28.960009	1197.562788	15.869683
29.061255	1211.316280	15.874701
29.130969	1196.909613	15.879719
29.160733	1205.065375	15.884736
29.192690	1196.424862	15.889754
29.466924	1223.651379	15.894771
29.488837	1227.780084	15.899789
29.563582	1224.123701	15.904807
29.200389	1221.402288	15.909824
29.787830	1232.141561	15.914842
29.693123	1232.924327	15.919859
29.572252	1207.210226	15.924877
29.610494	1224.566391	15.929895
29.683824	1221.828837	15.934912
29.435248	1208.341190	15.939930
29.827556	1222.013666	15.944947
29.815793	1217.152046	15.949965
29.945129	1218.967111	15.954983
29.526793	1205.486094	15.960000
29.794926	1212.562551	15.965018
29.644825	1221.338438	15.970035
29.570739	1228.845419	15.975053
29.790963	1231.350671	15.980071
29.550663	1233.492092	15.985088
29.586609	1235.955953	15.990106
29.475119	1238.896339	15.995123
29.618624	1242.513321	16.000141
30.102719	1237.144767	16.005159
29.815589	1236.753344	16.010176
30.065006	1231.771416	16.015194
30.006710	1245.973510	16.020211
29.785775	1233.470818	16.025229
30.100936	1239.106830	16.030247
30.116854	1254.769379	16.035264
30.262964	1254.439411	16.040282
30.175750	1264.690161	16.045299
30.246499	1245.040627	16.050317
30.419459	1253.021001	16.055335
30.251543	1252.045874	16.060352
30.478323	1255.641713	16.065370
30.579568	1238.779315	16.070387
30.255075	1239.881862	16.075405
30.301228	1225.655094	16.080423
30.306246	1240.685467	16.085440
30.712433	1246.805590	16.090458
30.625220	1232.559189	16.095475
30.186370	1230.559241	16.100493
30.566760	1235.348039	16.105511
30.521961	1248.697017	16.110528
30.606535	1249.745333	16.115546
30.745434	1255.442496	16.120563
30.604013	1252.290895	16.125581
30.704136	1240.801879	16.130599
30.772073	1256.034582	16.135616
30.731816	1253.927016	16.140634
30.979335	1248.149471	16.145651
30.533226	1233.875370	16.150669
30.868816	1245.304450	16.155687
30.650501	1249.652364	16.160704
30.830903	1241.458463	16.165722
31.108446	1250.203912	16.170739
30.932128	1255.833378	16.175757
30.847932	1250.487820	16.180775
31.007418	1248.263458	16.185792
31.161573	1247.993553	16.190810
31.095697	1249.183835	16.195827
30.782750	1248.713162	16.200845
31.183160	1234.193942	16.205863
30.966115	1248.864930	16.210880
30.955348	1246.169097	16.215898
31.064954	1247.257463	16.220915
31.181527	1256.163863	16.225933
30.883866	1238.655685	16.230951
30.752289	1258.557270	16.235968
30.688638	1247.803771	16.240986
31.122075	1242.032755	16.246003
31.031545	1252.408288	16.251021
31.081699	1244.367286	16.256039
30.887146	1266.602175	16.261056
31.328483	1281.934219	16.266074
31.442485	1286.161506	16.271091
31.414335	1290.206982	16.276109
31.798385	1285.780838	16.281127
31.826180	1289.572010	16.286144
31.607783	1278.119609	16.291162
31.769219	1268.042744	16.296179
31.470612	1272.787272	16.301197
31.751142	1257.412586	16.306215
31.578038	1254.497262	16.311232
31.577826	1238.258205	16.316250
31.547093	1253.564841	16.321267
31.484539	1274.218321	16.326285
31.891905	1271.208841	16.331303
31.768033	1268.411499	16.336320
31.599881	1273.915406	16.341338
31.660760	1272.895921	16.346355
31.845791	1282.186231	16.351373
32.162981	1271.283888	16.356391
31.526042	1277.908578	16.361408
31.931377	1277.977694	16.366426
32.218784	1281.579601	16.371443
31.817042	1279.688553	16.376461
31.998460	1274.857449	16.381479
31.756408	1284.546196	16.386496
31.749300	1281.206434	16.391514
31.762946	1279.489798	16.396531
31.899462	1280.224678	16.401549
32.176590	1273.681091	16.406567
31.958961	1291.683733	16.411584
32.153336	1289.266619	16.416602
32.341336	1290.384955	16.421619
32.532410	1290.521276	16.426637
32.782454	1293.169641	16.431655
32.551970	1274.305827	16.436672
32.621695	1263.559357	16.441690
32.593125	1258.442440	16.446707
32.258129	1264.427537	16.451725
32.432778	1264.953424	16.456743
32.415719	1271.790691	16.461760
32.415861	1269.712858	16.466778
32.401734	1257.409958	16.471795
32.051599	1275.309450	16.476813
32.770657	1281.393845	16.481831
33.010851	1300.191752	16.486848
32.789937	1279.077077	16.491866
32.806803	1262.682692	16.496883
32.425538	1266.507640	16.501901
32.627705	1259.634684	16.506919
32.594042	1259.784826	16.511936
32.896041	1285.372734	16.516954
33.255442	1288.904960	16.521971
32.793703	1276.255027	16.526989
33.077625	1256.969436	16.532007
32.888188	1262.874690	16.537024
32.539409	1264.022009	16.542042
32.757817	1271.735608	16.547059
32.680287	1282.008420	16.552077
32.999906	1289.474661	16.557095
32.891747	1286.138431	16.562112
32.778571	1296.530191	16.567130
32.995355	1295.680886	16.572147
32.939751	1296.004408	16.577165
33.071508	1289.255920	16.582183
32.775557	1294.869876	16.587200
33.146322	1298.331083	16.592218
33.341436	1300.922146	16.597235
33.262743	1297.033824	16.602253
33.214915	1286.799994	16.607271
33.311682	1285.298179	16.612288
33.110839	1291.337393	16.617306
33.443057	1304.212604	16.622323
33.268982	1323.586251	16.627341
33.653846	1331.408609	16.632359
33.577363	1321.721995	16.637376
33.449413	1326.326069	16.642394
33.535654	1315.051558	16.647411
33.567912	1318.204978	16.652429
33.714601	1318.228833	16.657447
33.610666	1315.841989	16.662464
33.685773	1322.663008	16.667482
34.132520	1317.563067	16.672499
34.122492	1321.096022	16.677517
33.763632	1297.091774	16.682535
33.540184	1290.837219	16.687552
33.567913	1288.605552	16.692570
33.750061	1301.042246	16.697587
33.564817	1316.516731	16.702605
34.011800	1313.508789	16.707623
34.077314	1312.817311	16.712640
33.788186	1319.114425	16.717658
34.023095	1316.528827	16.722675
33.905203	1321.813960	16.727693
33.979627	1322.321229	16.732711
34.235806	1316.904057	16.737728
34.061685	1313.073420	16.742746
34.059393	1314.684558	16.747763
34.105378	1320.311626	16.752781
34.452932	1311.177136	16.757799
34.456159	1311.774408	16.762816
34.390968	1322.948159	16.767834
34.540905	1315.602181	16.772851
34.506456	1315.716271	16.777869
34.352495	1321.760604	16.782887
34.188537	1320.904385	16.787904
34.346712	1325.572932	16.792922
34.667491	1316.588995	16.797939
34.414287	1317.447378	16.802957
34.076627	1321.337742	16.807975
34.256460	1317.686596	16.812992
34.121089	1322.510494	16.818010
34.317839	1315.275022	16.823027
34.384407	1327.684557	16.828045
34.596016	1324.882459	16.833063
34.874746	1339.191335	16.838080
34.740180	1342.792920	16.843098
35.090386	1345.566886	16.848115
34.908813	1327.305512	16.853133
34.843408	1315.531391	16.858151
35.048532	1306.631970	16.863168
34.907740	1312.318710	16.868186
34.790437	1305.688585	16.873203
35.014955	1311.499525	16.878221
35.013455	1308.234364	16.883239
34.846556	1313.058568	16.888256
34.985208	1332.610429	16.893274
35.413037	1332.908757	16.898291
35.214346	1314.860905	16.903309
34.910613	1310.212554	16.908327
35.264529	1309.814838	16.913344
35.215671	1331.762334	16.918362
35.378912	1332.430036	16.923379
35.055959	1326.282568	16.928397
35.290522	1325.447729	16.933415
35.205957	1328.006328	16.938432
35.159725	1334.950520	16.943450
35.431604	1325.345192	16.948467
35.269142	1336.918270	16.953485
35.086320	1335.245546	16.958503
35.549603	1325.921137	16.963520
35.584044	1330.667619	16.968538
35.342017	1332.960335	16.973555
35.353521	1329.590853	16.978573
35.592609	1335.374311	16.983591
35.536045	1333.475392	16.988608
35.142825	1335.804805	16.993626
35.803155	1318.211379	16.998643
35.768556	1332.025976	17.003661
35.601414	1328.642516	17.008679
35.805054	1330.568436	17.013696
35.516010	1358.780059	17.018714
35.928065	1357.259411	17.023731
35.850650	1360.007204	17.028749
35.971183	1361.694708	17.033767
36.019467	1350.366451	17.038784
36.157064	1355.595118	17.043802
36.335718	1346.386875	17.048819
36.465732	1344.733466	17.053837
36.467687	1330.109393	17.058855
36.458044	1306.112351	17.063872
36.457510	1316.081910	17.068890
36.522017	1309.569071	17.073907
36.340326	1306.181646	17.078925
36.568288	1292.079965	17.083943
36.759300	1303.341823	17.088960
36.451366	1314.853145	17.093978
36.726908	1302.151664	17.098995
36.367670	1297.081179	17.104013
36.327959	1283.121295	17.109031
36.378313	1277.230473	17.114048
36.269264	1302.187150	17.119066
36.496205	1298.206039	17.124083
36.472171	1296.012513	17.129101
36.561797	1305.333784	17.134119
36.653778	1303.739926	17.139136
36.547080	1317.783077	17.144154
36.507775	1313.006039	17.149171
36.212197	1313.146046	17.154189
36.238480	1316.780171	17.159207
36.396216	1308.643327	17.164224
36.249431	1313.609035	17.169242
36.393393	1330.017275	17.174259
36.851301	1344.766322	17.179277
36.969276	1346.657144	17.184295
37.029329	1346.893011	17.189312
36.879564	1349.024728	17.194330
36.609617	1350.747768	17.199347
36.894808	1341.799377	17.204365
36.993065	1349.068157	17.209383
36.912695	1355.067734	17.214400
36.723677	1362.778725	17.219418
36.787793	1350.735389	17.224435
36.782940	1361.125649	17.229453
36.857807	1373.211442	17.234471
37.454765	1369.583416	17.239488
37.034073	1384.132870	17.244506
37.448080	1380.886364	17.249523
37.840926	1370.509836	17.254541
37.436408	1377.698374	17.259559
37.528106	1372.857952	17.264576
37.298868	1381.490833	17.269594
37.346123	1379.070428	17.274611
37.896822	1374.493416	17.279629
37.524461	1378.279221	17.284647
37.955703	1374.644591	17.289664
37.343325	1374.635358	17.294682
37.943998	1372.730710	17.299699
38.176252	1374.177036	17.304717
37.584778	1379.238857	17.309735
37.996718	1376.678495	17.314752
37.911074	1377.193992	17.319770
37.995941	1368.005412	17.324787
37.906476	1369.411816	17.329805
37.688441	1375.766827	17.334823
37.768385	1382.612270	17.339840
37.594874	1380.299431	17.344858
37.493339	1365.698119	17.349875
37.792170	1365.482214	17.354893
37.633891	1369.488693	17.359911
37.804673	1369.760381	17.364928
37.907282	1396.158903	17.369946
38.075935	1388.632158	17.374963
38.521065	1397.028511	17.379981
38.255332	1394.812172	17.384999
38.572969	1390.602649	17.390016
38.529279	1402.268517	17.395034
38.527329	1367.838222	17.400051
38.355084	1364.831506	17.405069
38.466829	1371.264474	17.410087
38.565463	1363.264436	17.415104
38.718011	1350.744545	17.420122
38.628081	1367.551912	17.425139
38.514787	1351.167175	17.430157
38.627667	1362.004256	17.435175
38.546950	1361.178801	17.440192
38.684481	1359.162410	17.445210
38.336606	1373.615299	17.450227
38.904617	1384.458457	17.455245
38.690117	1392.805860	17.460263
38.659779	1397.713701	17.465280
38.875374	1401.130470	17.470298
38.874230	1397.327278	17.475315
39.062035	1393.855733	17.480333
38.928434	1402.114737	17.485351
38.794730	1399.504546	17.490368
38.837333	1396.786017	17.495386
38.908945	1395.432915	17.500403
39.077852	1385.074790	17.505421
39.140466	1403.479598	17.510439
38.789495	1385.874354	17.515456
39.001580	1399.509678	17.520474
39.223703	1401.611978	17.525491
39.211817	1383.461891	17.530509
38.935140	1407.622822	17.535527
39.239586	1382.982550	17.540544
39.071688	1396.659598	17.545562
38.819184	1430.740571	17.550579
39.545417	1418.660790	17.555597
39.392607	1410.702401	17.560615
39.597946	1427.212643	17.565632
39.858554	1422.449082	17.570650
39.654013	1432.852366	17.575667
40.155977	1423.738796	17.580685
39.587604	1413.383410	17.585703
40.029508	1418.101115	17.590720
39.846482	1427.752229	17.595738
39.682194	1417.585642	17.600755
40.082446	1414.371210	17.605773
39.862311	1410.428340	17.610791
39.615881	1389.984510	17.615808
39.365669	1415.692180	17.620826
39.979693	1409.495909	17.625843
39.993502	1413.657419	17.630861
39.638127	1417.420076	17.635879
40.347548	1409.997404	17.640896
40.388242	1415.070094	17.645914
40.088178	1418.317434	17.650931
40.326605	1406.743310	17.655949
39.950097	1409.452300	17.660967
40.039526	1406.828543	17.665984
40.289488	1408.397886	17.671002
40.352317	1421.578854	17.676019
40.486727	1405.922159	17.681037
39.987418	1414.634310	17.686055
40.521973	1408.812498	17.691072
40.380141	1408.717207	17.696090
39.882465	1405.156791	17.701107
40.102500	1410.424239	17.706125
40.064195	1417.604726	17.711143
40.503635	1443.207172	17.716160
40.492146	1444.052180	17.721178
40.672452	1445.822967	17.726195
41.197396	1443.543436	17.731213
40.833869	1441.278195	17.736231
40.766949	1441.594086	17.741248
40.858424	1445.669289	17.746266
40.632473	1450.537561	17.751283
40.670011	1456.718144	17.756301
40.735917	1444.414904	17.761319
40.773764	1440.328638	17.766336
40.801778	1440.115027	17.771354
40.650626	1457.814700	17.776371
40.924284	1438.182878	17.781389
40.565909	1447.710966	17.786407
40.922411	1464.242758	17.791424
41.128801	1473.039016	17.796442
40.805030	1458.307892	17.801459
41.251565	1462.140861	17.806477
41.061728	1472.309027	17.811495
41.148992	1455.818256	17.816512
41.578723	1459.389644	17.821530
41.146342	1464.682515	17.826547
41.569379	1456.347552	17.831565
41.365963	1455.242795	17.836583
41.196131	1465.723934	17.841600
41.644648	1465.330004	17.846618
41.316678	1487.581791	17.851635
41.724538	1494.895646	17.856653
41.760819	1496.856144	17.861671
41.937015	1492.607804	17.866688
41.912692	1493.300709	17.871706
42.168219	1492.569481	17.876723
41.778909	1461.996338	17.881741
41.706532	1468.129963	17.886759
41.811843	1467.166298	17.891776
42.140506	1474.436145	17.896794
41.852437	1468.078565	17.901811
41.771376	1464.096197	17.906829
42.037559	1471.715771	17.911847
42.105590	1478.242273	17.916864
42.401500	1482.468920	17.921882
42.124216	1491.616027	17.926899
42.415271	1484.826313	17.931917
42.160117	1486.166348	17.936935
42.338119	1491.431091	17.941952
42.480772	1476.760836	17.946970
42.485797	1507.705299	17.951987
42.541431	1485.243789	17.957005
42.405462	1468.912870	17.962023
42.409646	1480.308479	17.967040
42.212169	1480.001845	17.972058
42.760981	1479.540011	17.977075
42.579460	1469.756796	17.982093
42.482372	1482.706928	17.987111
42.611405	1491.123864	17.992128
43.043346	1453.382257	17.997146
42.752652	1501.218860	18.002163
42.788152	1467.617607	18.007181
42.840032	1472.891447	18.012199
42.772702	1482.401454	18.017216
42.705196	1478.703202	18.022234
42.392077	1476.000493	18.027251
42.638231	1473.548351	18.032269
42.762577	1484.166624	18.037287
42.383870	1492.645662	18.042304
43.000024	1485.693990	18.047322
42.912401	1496.552139	18.052339
43.180016	1503.232433	18.057357
43.339832	1515.230080	18.062375
43.105611	1498.324144	18.067392
43.396881	1513.259598	18.072410
43.236580	1500.721048	18.077427
43.315701	1500.244463	18.082445
43.462778	1507.044653	18.087463
43.319559	1512.721634	18.092480
43.732072	1500.744515	18.097498
43.547156	1498.553022	18.102515
43.321121	1507.215353	18.107533
43.358192	1516.555366	18.112551
43.330265	1505.559243	18.117568
43.266562	1508.347347	18.122586
43.152238	1536.389096	18.127603
43.861083	1539.665886	18.132621
43.751621	1534.616826	18.137639
43.582960	1534.744458	18.142656
43.901940	1532.194177	18.147674
44.278237	1540.795070	18.152691
44.167084	1528.508987	18.157709
43.876496	1532.085166	18.162727
43.916997	1537.452078	18.167744
44.070209	1533.734341	18.172762
44.287652	1541.714073	18.177779
44.380985	1530.729266	18.182797
44.323449	1522.949096	18.187815
44.133811	1534.034322	18.192832
44.641752	1535.488606	18.197850
44.394039	1536.572635	18.202867
44.163686	1529.727635	18.207885
44.563558	1525.884047	18.212903
44.337383	1528.632002	18.217920
44.684706	1524.788930	18.222938
44.399025	1522.154192	18.227955
44.666569	1522.819427	18.232973
44.287316	1539.468648	18.237991
44.647839	1527.874955	18.243008
44.606353	1511.699588	18.248026
44.753933	1520.189872	18.253043
44.456253	1518.585779	18.258061
44.862210	1521.448415	18.263079
44.714736	1527.444609	18.268096
44.985112	1531.170416	18.273114
44.888282	1552.301654	18.278131
44.967869	1553.571005	18.283149
45.287314	1523.372321	18.288167
45.153736	1553.635865	18.293184
45.247739	1541.636367	18.298202
45.296507	1536.928576	18.303219
45.136026	1520.983743	18.308237
45.198277	1530.145934	18.313255
45.405697	1538.616461	18.318272
45.606208	1531.831729	18.323290
45.623362	1522.351837	18.328307
45.469246	1510.236997	18.333325
45.651426	1505.503221	18.338343
45.399512	1506.823865	18.343360
45.246633	1508.759479	18.348378
45.309875	1523.769064	18.353395
45.685358	1531.160458	18.358413
45.459808	1529.283745	18.363431
45.824174	1541.270027	18.368448
45.665303	1537.583185	18.373466
45.689842	1542.638049	18.378483
45.596445	1537.743724	18.383501
45.818482	1542.443055	18.388519
45.635974	1542.722328	18.393536
46.000740	1535.728931	18.398554
46.001337	1540.310998	18.403571
45.895248	1536.272829	18.408589
46.117594	1531.929029	18.413607
45.866413	1534.588167	18.418624
45.994125	1532.762077	18.423642
45.668294	1541.959428	18.428659
46.004601	1558.486685	18.433677
46.465598	1558.808044	18.438695
45.979053	1557.946630	18.443712
46.124976	1566.500912	18.448730
46.117442	1568.704356	18.453747
46.430147	1559.746726	18.458765
46.451074	1554.351256	18.463783
46.520879	1572.891983	18.468800
46.635061	1562.168089	18.473818
46.647140	1561.601522	18.478835
46.392595	1563.232469	18.483853
46.722698	1549.965234	18.488871
46.558167	1558.528126	18.493888
46.873987	1563.226664	18.498906
47.135183	1545.345845	18.503923
46.517266	1557.337793	18.508941
46.856540	1569.373717	18.513959
46.840446	1589.446097	18.518976
47.214901	1593.501378	18.523994
47.084264	1586.231471	18.529011
47.269535	1587.842612	18.534029
47.283718	1575.516050	18.539047
47.273940	1577.443008	18.544064
47.567352	1581.797496	18.549082
47.187566	1567.392936	18.554099
47.119177	1558.905061	18.559117
47.446069	1563.979350	18.564135
47.384583	1575.656061	18.569152
47.533364	1582.331749	18.574170
47.725153	1578.968062	18.579187
47.098332	1589.748683	18.584205
47.694615	1588.437726	18.589223
47.714658	1585.606358	18.594240
47.600232	1586.848454	18.599258
47.842436	1579.369654	18.604275
47.666696	1580.415467	18.609293
47.860382	1583.977344	18.614311
47.902379	1576.055432	18.619328
48.282266	1571.884693	18.624346
48.349656	1573.262955	18.629363
47.810318	1577.657444	18.634381
48.209444	1572.511530	18.639399
47.808544	1576.619679	18.644416
47.895427	1581.535628	18.649434
48.174244	1574.931864	18.654451
47.879446	1584.874609	18.659469
48.268397	1566.970242	18.664487
47.948892	1572.698169	18.669504
47.969377	1574.096496	18.674522
48.119309	1558.205932	18.679539
47.560512	1588.411525	18.684557
48.390275	1605.734720	18.689575
48.764869	1604.685629	18.694592
48.327229	1606.885317	18.699610
49.011139	1608.788162	18.704627
48.710528	1603.034976	18.709645
48.699151	1601.260946	18.714663
49.034047	1612.588186	18.719680
49.048769	1609.243294	18.724698
49.014112	1608.443511	18.729715
48.787725	1601.701662	18.734733
49.177591	1603.239277	18.739751
48.913812	1606.603564	18.744768
48.911268	1612.269945	18.749786
48.870062	1595.667372	18.754803
48.744890	1605.839475	18.759821
49.227751	1603.672024	18.764839
48.953921	1600.215854	18.769856
48.910089	1601.066029	18.774874
49.168021	1596.711816	18.779891
49.042063	1600.724215	18.784909
48.973617	1589.870554	18.789927
49.014446	1603.317885	18.794944
49.049688	1617.881371	18.799962
49.417047	1629.022552	18.804979
49.544983	1625.637578	18.809997
49.620321	1616.198682	18.815015
49.164190	1636.610287	18.820032
49.317922	1622.314064	18.825050
49.535191	1626.897781	18.830067
49.005483	1638.743596	18.835085
49.210022	1643.014750	18.840103
49.528156	1654.017513	18.845120
49.608054	1662.168683	18.850138
49.874824	1662.799442	18.855155
49.631605	1663.182780	18.860173
49.897444	1650.525015	18.865191
50.044813	1675.269983	18.870208
50.288647	1676.354278	18.875226
50.899229	1671.777064	18.880243
50.647160	1658.616734	18.885261
50.596439	1646.630793	18.890279
50.554398	1654.567030	18.895296
50.656404	1647.596610	18.900314
50.825864	1642.547073	18.905331
50.940032	1655.125474	18.910349
50.852284	1642.890615	18.915367
50.864402	1645.941927	18.920384
50.609581	1654.102431	18.925402
50.905398	1636.450355	18.930419
50.880046	1641.149848	18.935437
50.728076	1635.572714	18.940455
50.851861	1626.228329	18.945472
50.704740	1639.029281	18.950490
51.029861	1640.676326	18.955507
50.904131	1639.441190	18.960525
51.207273	1640.091315	18.965543
50.939917	1640.292888	18.970560
50.870325	1636.074267	18.975578
51.195817	1631.034456	18.980595
50.918471	1642.698456	18.985613
51.013275	1636.841298	18.990631
51.026489	1638.231352	18.995648
51.131113	1638.320118	19.000666
51.233152	1623.951914	19.005683
51.085776	1644.487319	19.010701
51.238856	1644.658019	19.015719
50.980800	1643.019278	19.020736
51.341311	1660.870400	19.025754
51.609365	1669.359649	19.030771
51.430920	1672.046536	19.035789
51.535404	1669.896949	19.040807
51.950135	1663.173944	19.045824
51.725707	1671.831397	19.050842
51.869821	1679.461112	19.055859
51.698753	1674.645194	19.060877
51.679440	1664.068353	19.065895
52.131934	1673.629288	19.070912
51.632583	1679.889298	19.075930
51.832204	1674.466858	19.080947
51.971280	1670.131579	19.085965
51.908775	1679.673978	19.090983
52.217299	1691.773110	19.096000
52.196825	1703.780005	19.101018
52.135529	1700.466091	19.106035
52.129813	1701.138736	19.111053
52.304209	1693.513392	19.116071
52.421014	1700.872198	19.121088
52.265194	1692.550770	19.126106
52.746566	1695.110410	19.131123
52.531768	1695.298882	19.136141
52.448897	1698.947364	19.141159
52.732795	1694.461569	19.146176
52.540126	1690.520533	19.151194
52.874926	1706.909777	19.156211
52.611499	1726.878650	19.161229
52.863655	1723.936305	19.166247
52.898150	1717.582225	19.171264
52.783107	1735.677594	19.176282
53.124226	1724.118301	19.181299
52.740555	1727.824201	19.186317
52.907474	1725.403530	19.191335
53.179284	1722.083677	19.196352
52.961745	1720.298468	19.201370
53.274928	1715.542158	19.206387
53.383300	1719.754741	19.211405
53.277439	1725.162368	19.216423
53.284426	1735.988304	19.221440
53.541665	1746.170303	19.226458
53.705623	1742.112602	19.231475
53.827584	1741.662210	19.236493
53.777786	1740.525066	19.241511
54.260991	1726.840003	19.246528
54.055170	1715.872878	19.251546
53.927289	1700.742180	19.256563
53.930100	1710.544739	19.261581
53.952391	1703.083645	19.266599
54.571292	1689.601915	19.271616
54.067037	1691.027311	19.276634
54.548601	1688.405459	19.281651
54.288621	1689.672349	19.286669
54.415919	1697.060941	19.291687
54.420038	1698.756040	19.296704
54.347690	1692.585748	19.301722
54.339972	1682.815567	19.306739
54.565397	1683.629098	19.311757
54.528922	1688.031510	19.316775
54.488259	1680.402718	19.321792
54.177176	1699.071991	19.326810
54.490761	1691.260858	19.331827
54.712401	1699.033946	19.336845
54.306587	1694.632979	19.341863
54.651091	1685.300546	19.346880
54.675351	1688.331055	19.351898
54.914801	1687.495418	19.356915
54.561815	1692.476837	19.361933
54.492027	1683.650916	19.366951
54.584001	1683.310699	19.371968
54.383271	1695.255101	19.376986
54.672542	1714.484590	19.382003
55.091937	1714.183389	19.387021
55.006451	1716.893210	19.392039
55.073918	1721.834326	19.397056
54.791852	1723.486981	19.402074
54.860859	1717.519075	19.407091
55.195988	1741.993544	19.412109
55.442179	1750.546102	19.417127
55.767536	1751.854926	19.422144
55.461769	1747.765172	19.427162
55.255519	1761.945751	19.432179
55.323670	1759.724868	19.437197
55.474803	1750.602555	19.442215
55.562622	1754.107427	19.447232
55.516564	1744.852973	19.452250
55.476876	1761.473461	19.457267
55.669639	1782.376381	19.462285
55.762195	1781.155184	19.467303
56.062145	1771.957214	19.472320
55.947438	1784.639869	19.477338
55.749524	1789.864001	19.482355
55.910677	1783.934854	19.487373
56.157059	1783.625065	19.492391
56.253794	1774.848037	19.497408
56.397414	1780.785326	19.502426
56.511072	1772.092116	19.507443
56.605085	1771.114503	19.512461
56.481877	1774.624721	19.517479
56.918631	1768.857691	19.522496
56.757328	1771.285462	19.527514
56.801401	1762.672567	19.532531
56.608190	1760.770216	19.537549
56.673768	1771.023697	19.542567
56.855598	1760.719872	19.547584
56.470177	1751.135721	19.552602
56.614202	1758.908636	19.557619
56.794075	1765.044629	19.562637
56.905855	1772.673258	19.567655
57.425104	1765.645678	19.572672
57.244768	1778.533846	19.577690
57.088036	1770.360380	19.582707
57.035496	1772.151040	19.587725
56.824698	1791.995206	19.592743
57.256721	1783.597278	19.597760
57.410106	1794.341709	19.602778
57.228944	1782.757125	19.607795
57.412361	1790.872983	19.612813
57.319463	1788.885418	19.617831
57.704437	1768.474060	19.622848
57.830592	1782.499402	19.627866
57.692226	1782.024459	19.632883
58.178454	1778.480064	19.637901
57.768693	1782.493729	19.642919
58.102078	1778.995731	19.647936
57.952452	1785.780452	19.652954
58.161206	1788.586505	19.657971
57.875379	1776.326494	19.662989
57.671750	1785.306310	19.668007
57.920013	1783.376021	19.673024
57.713690	1781.736877	19.678042
57.815911	1798.949824	19.683059
58.120307	1813.649905	19.688077
58.171771	1817.113400	19.693095
58.445726	1810.560643	19.698112
58.239132	1814.230459	19.703130
58.506404	1809.226613	19.708147
58.448936	1812.358270	19.713165
58.371148	1810.750534	19.718183
58.920777	1796.902231	19.723200
58.449403	1812.185350	19.728218
58.475685	1804.803790	19.733235
58.421135	1815.763868	19.738253
58.807006	1827.073710	19.743271
59.074278	1828.196751	19.748288
58.973764	1856.122872	19.753306
59.032330	1830.451403	19.758323
59.162297	1828.903340	19.763341
59.317247	1840.954732	19.768359
59.443198	1841.815596	19.773376
59.356607	1821.693299	19.778394
59.231727	1826.509397	19.783411
59.471343	1821.758494	19.788429
59.410892	1833.084465	19.793447
59.630441	1825.662635	19.798464
59.429554	1830.484564	19.803482
59.661712	1830.910068	19.808499
59.635170	1825.158701	19.813517
59.118826	1831.396316	19.818535
59.622121	1833.853387	19.823552
59.360390	1837.756943	19.828570
59.321325	1853.432054	19.833587
59.607288	1855.639072	19.838605
59.560056	1860.411339	19.843623
59.801438	1859.111344	19.848640
59.916420	1859.443852	19.853658
59.964217	1868.465419	19.858675
60.246682	1875.974073	19.863693
60.013229	1890.933041	19.868711
60.508204	1882.726365	19.873728
60.734939	1880.344893	19.878746
60.649222	1887.073851	19.883763
60.868679	1888.371263	19.888781
60.905320	1876.319289	19.893799
60.882110	1865.519554	19.898816
60.697689	1850.289179	19.903834
60.620668	1853.642613	19.908851
60.600122	1851.058338	19.913869
60.438426	1866.325160	19.918887
60.836070	1883.083680	19.923904
61.240264	1877.669439	19.928922
61.131957	1886.772541	19.933939
61.218615	1884.693406	19.938957
61.273990	1868.757808	19.943975
61.191376	1869.559128	19.948992
61.357680	1874.212401	19.954010
61.303637	1875.827135	19.959027
61.566721	1878.404319	19.964045
61.463919	1882.840963	19.969063
61.440937	1877.822036	19.974080
61.631297	1872.978298	19.979098
61.363182	1869.398454	19.984115
61.375940	1860.455442	19.989133
61.393980	1870.461747	19.994151
61.694359	1875.334310	19.999168
61.662564	1875.092478	20.004186
61.390273	1880.289179	20.009203
61.917337	1885.948284	20.014221
61.847782	1895.141166	20.019239
61.747104	1917.185902	20.024256
62.100705	1906.351212	20.029274
61.975326	1907.017782	20.034291
62.170525	1900.968327	20.039309
62.321977	1908.524635	20.044327
62.244340	1909.134827	20.049344
62.404388	1896.317542	20.054362
62.134290	1907.990036	20.059379
62.558711	1914.812257	20.064397
62.197320	1934.948048	20.069415
62.388056	1929.536369	20.074432
62.975626	1923.156917	20.079450
62.683427	1941.362592	20.084467
62.390190	1942.765368	20.089485
62.421161	1936.853774	20.094503
62.566379	1934.255632	20.099520
62.913735	1930.434474	20.104538
62.632932	1954.650454	20.109555
63.201068	1956.892713	20.114573
63.238143	1961.335388	20.119591
63.398413	1960.432140	20.124608
63.627525	1954.459052	20.129626
63.232741	1962.704970	20.134643
63.501833	1970.885918	20.139661
63.441474	1966.141909	20.144679
63.388284	1964.014279	20.149696
63.526258	1961.365378	20.154714
63.564150	1957.220757	20.159731
63.607582	1965.506903	20.164749
63.650409	1956.334093	20.169767
63.502713	1965.084875	20.174784
63.770159	1957.384779	20.179802
63.541409	1961.533219	20.184819
64.012085	1964.435964	20.189837
63.816657	1973.225823	20.194855
64.150096	1978.245734	20.199872
64.347203	1987.688731	20.204890
63.951622	1994.688952	20.209907
64.167052	1980.042763	20.214925
64.491845	1978.562715	20.219943
64.072148	1989.024303	20.224960
64.425460	1979.861738	20.229978
64.175309	1983.357644	20.234995
64.379005	1987.715552	20.240013
64.486261	1991.184349	20.245031
64.692908	2010.674375	20.250048
64.659323	2010.693950	20.255066
64.841083	2017.661885	20.260083
65.089816	1999.113957	20.265101
65.061208	2012.418584	20.270119
65.068052	2007.536429	20.275136
65.229665	2007.054537	20.280154
65.375408	2006.114277	20.285171
65.445807	2001.720640	20.290189
65.356820	2010.949727	20.295207
65.479125	2002.643540	20.300224
65.738282	2001.381598	20.305242
65.186922	2012.856783	20.310259
65.752363	2004.497229	20.315277
65.825568	2000.754380	20.320295
65.412750	2008.136457	20.325312
65.521282	2004.771794	20.330330
65.656868	2011.871360	20.335347
65.606966	2012.110616	20.340365
65.749938	2014.143834	20.345383
65.540936	2015.319250	20.350400
65.868930	2034.722316	20.355418
65.797126	2035.067312	20.360435
66.097975	2028.217584	20.365453
65.953145	2035.072442	20.370471
65.667200	2032.766415	20.375488
66.025267	2038.457252	20.380506
66.285721	2042.582755	20.385523
66.481939	2060.727991	20.390541
66.799390	2064.254520	20.395559
66.837084	2066.535772	20.400576
66.801676	2046.038482	20.405594
66.362390	2049.415127	20.410611
66.751486	2052.200338	20.415629
66.784527	2054.180306	20.420647
66.739258	2055.974560	20.425664
67.107013	2064.144546	20.430682
66.820329	2067.853938	20.435699
66.770985	2059.894420	20.440717
67.089497	2055.690862	20.445735
67.146766	2067.517344	20.450752
67.134144	2060.275568	20.455770
67.074367	2063.223602	20.460787
67.144006	2066.108525	20.465805
67.017116	2072.732449	20.470823
66.978777	2089.754223	20.475840
67.398822	2090.980339	20.480858
67.274112	2096.751337	20.485875
67.609956	2082.214831	20.490893
67.598233	2104.239372	20.495911
67.830849	2116.244000	20.500928
68.292649	2101.989413	20.505946
68.150579	2114.461211	20.510963
68.490935	2104.117705	20.515981
68.631862	2081.076947	20.520999
68.273396	2078.378205	20.526016
68.222415	2069.223431	20.531034
68.093368	2061.962467	20.536051
68.886511	2070.037876	20.541069
68.878483	2066.861676	20.546087
68.761931	2074.972049	20.551104
68.761905	2057.220351	20.556122
68.476406	2070.155435	20.561139
68.587408	2064.278218	20.566157
68.785049	2056.995047	20.571175
68.229903	2066.836490	20.576192
68.777094	2070.220989	20.581210
69.085438	2086.330165	20.586227
69.263409	2090.473555	20.591245
69.261508	2097.617111	20.596263
69.209707	2103.181427	20.601280
69.281988	2087.362444	20.606298
69.189997	2093.788901	20.611315
68.896414	2087.115741	20.616333
69.403429	2085.219655	20.621351
69.429329	2089.445499	20.626368
69.586726	2095.358699	20.631386
69.527282	2091.674734	20.636403
69.689008	2082.452996	20.641421
70.109365	2080.768934	20.646439
69.736730	2087.281042	20.651456
69.884257	2077.520444	20.656474
69.944970	2082.904786	20.661491
69.729285	2074.594256	20.666509
70.038892	2091.242789	20.671527
69.898835	2110.461047	20.676544
69.904608	2110.878619	20.681562
70.508293	2115.663569	20.686579
70.401941	2096.064720	20.691597
70.368317	2105.942571	20.696615
69.983874	2110.741954	20.701632
70.566805	2096.741765	20.706650
70.242557	2109.572951	20.711667
70.196965	2106.954871	20.716685
70.281455	2120.420888	20.721703
70.366371	2130.789519	20.726720
70.568873	2134.523163	20.731738
70.765069	2145.360130	20.736755
70.760435	2141.942695	20.741773
70.788262	2143.248669	20.746791
70.849319	2156.688569	20.751808
71.238253	2152.388808	20.756826
71.260026	2162.868207	20.761843
71.197231	2165.486402	20.766861
71.316360	2159.549647	20.771879
71.083904	2157.041584	20.776896
71.187984	2164.105350	20.781914
71.496736	2162.451661	20.786931
71.580455	2181.988264	20.791949
71.769415	2191.539661	20.796967
71.724241	2191.962214	20.801984
71.880392	2183.840865	20.807002
72.145413	2183.515514	20.812019
72.180273	2182.740793	20.817037
72.529854	2182.939940	20.822055
72.425123	2189.061725	20.827072
72.198311	2176.774658	20.832090
72.633482	2177.161507	20.837107
72.564463	2181.857127	20.842125
72.696066	2177.850085	20.847143
72.473170	2185.359269	20.852160
72.817404	2170.380883	20.857178
72.705676	2180.979113	20.862195
72.561110	2182.521799	20.867213
73.125205	2178.700621	20.872231
72.530874	2184.175304	20.877248
72.481972	2189.021878	20.882266
72.607002	2177.820737	20.887283
72.650573	2171.200739	20.892301
72.958191	2185.973047	20.897319
72.895752	2211.329702	20.902336
72.960551	2205.624967	20.907354
73.383632	2209.631773	20.912371
73.139886	2216.873732	20.917389
73.306176	2211.769448	20.922407
73.211203	2205.555353	20.927424
73.183648	2207.461634	20.932442
73.308226	2228.802371	20.937459
73.126092	2243.158900	20.942477
73.716112	2239.267504	20.947495
73.700127	2242.019823	20.952512
73.842645	2241.080063	20.957530
73.801910	2240.902573	20.962547
73.762516	2242.367143	20.967565
74.152737	2253.283363	20.972583
74.647844	2267.011231	20.977600
74.510418	2265.084184	20.982618
74.572598	2257.223179	20.987635
74.731286	2257.514119	20.992653
75.020104	2244.419584	20.997671
74.461972	2239.142946	21.002688
74.794785	2230.450694	21.007706
74.665309	2231.180853	21.012723
74.690442	2237.794766	21.017741
75.027011	2239.339382	21.022759
74.845820	2244.913374	21.027776
75.344839	2242.914723	21.032794
75.289738	2246.124749	21.037811
75.165077	2253.034696	21.042829
75.674802	2256.871966	21.047847
75.040887	2250.017044	21.052864
75.252298	2253.739861	21.057882
75.424189	2240.154304	21.062899
75.157309	2251.812402	21.067917
75.336593	2241.727299	21.072935
75.323017	2234.702670	21.077952
75.498575	2254.767431	21.082970
75.496485	2271.999147	21.087987
75.693881	2274.904638	21.093005
76.103125	2274.159874	21.098023
75.816741	2270.033843	21.103040
75.884078	2266.612767	21.108058
76.476321	2264.272049	21.113075
75.882522	2272.593923	21.118093
76.005833	2261.551871	21.123111
75.969611	2282.715406	21.128128
76.126424	2291.976261	21.133146
76.290512	2302.466099	21.138163
76.236809	2303.556995	21.143181
76.453843	2306.114859	21.148199
76.275430	2308.701180	21.153216
76.369116	2329.068543	21.158234
76.741115	2332.073620	21.163251
76.756414	2333.985668	21.168269
77.017109	2335.328458	21.173287
77.004550	2330.439849	21.178304
77.427436	2324.959542	21.183322
77.219319	2323.540851	21.188339
77.272713	2333.894203	21.193357
77.372289	2324.510759	21.198375
77.444175	2331.351646	21.203392
77.592093	2351.641177	21.208410
77.712644	2349.685564	21.213427
77.875132	2355.251983	21.218445
77.921668	2353.942120	21.223463
78.280685	2357.020848	21.228480
78.219659	2343.476272	21.233498
78.371478	2326.000487	21.238515
77.994713	2330.156904	21.243533
77.879930	2309.844937	21.248551
78.352645	2317.089098	21.253568
78.060388	2327.978927	21.258586
78.498624	2333.553275	21.263603
78.566963	2333.517270	21.268621
78.857067	2340.542018	21.273639
78.639825	2337.016866	21.278656
78.639797	2344.997118	21.283674
78.588118	2340.569362	21.288691
78.310331	2343.012655	21.293709
78.703295	2339.992678	21.298727
78.732443	2335.622822	21.303744
78.429288	2340.970902	21.308762
78.888585	2339.142173	21.313779
78.837725	2355.527588	21.318797
79.442198	2365.307790	21.323815
79.425795	2367.467937	21.328832
79.551655	2368.498741	21.333850
80.051372	2354.442362	21.338867
79.664163	2357.262554	21.343885
79.713569	2361.409222	21.348903
79.834615	2356.253899	21.353920
79.558173	2364.008460	21.358938
79.808688	2363.630361	21.363955
79.551623	2370.205177	21.368973
79.673326	2360.379293	21.373991
79.893541	2375.278995	21.379008
79.879856	2381.899164	21.384026
80.217852	2376.400914	21.389043
80.233148	2393.020435	21.394061
80.431995	2386.386588	21.399079
80.333598	2385.353100	21.404096
79.969241	2382.954909	21.409114
80.478177	2417.420937	21.414131
80.322920	2414.320051	21.419149
80.548286	2406.715309	21.424167
80.830456	2415.965691	21.429184
80.999485	2420.204201	21.434202
81.079928	2423.885024	21.439219
81.034268	2428.714643	21.444237
80.816791	2409.612095	21.449255
81.004053	2429.108922	21.454272
81.368337	2437.698115	21.459290
81.500690	2448.496724	21.464307
81.346978	2447.953416	21.469325
81.632401	2449.827908	21.474343
81.682321	2445.844044	21.479360
81.521370	2447.692188	21.484378
82.048308	2435.289420	21.489395
81.790447	2457.765895	21.494413
81.853803	2444.453083	21.499431
82.165801	2440.371583	21.504448
81.953631	2431.602520	21.509466
82.547298	2432.048263	21.514483
82.113253	2433.530955	21.519501
82.189233	2443.974383	21.524519
81.993967	2445.127977	21.529536
81.855965	2469.791605	21.534554
82.267446	2459.560780	21.539571
82.390749	2464.468863	21.544589
82.497150	2471.705448	21.549607
82.879314	2477.715888	21.554624
82.687760	2487.946384	21.559642
83.132363	2492.473677	21.564659
83.315079	2489.457310	21.569677
83.691323	2498.315203	21.574695
83.823196	2477.988050	21.579712
83.789640	2470.602323	21.584730
83.838154	2454.046596	21.589747
83.379339	2466.095708	21.594765
83.370701	2450.363957	21.599783
83.928849	2437.244390	21.604800
83.690394	2445.017319	21.609818
83.483069	2447.284219	21.614835
83.634843	2466.645179	21.619853
83.904239	2467.078138	21.624871
83.932232	2484.065413	21.629888
83.573304	2493.030314	21.634906
84.151474	2487.560580	21.639923
84.016472	2484.395098	21.644941
83.881181	2484.119421	21.649959
84.128786	2493.065467	21.654976
84.390909	2515.547990	21.659994
84.253772	2514.392463	21.665011
84.609803	2515.894681	21.670029
84.282059	2507.015009	21.675047
84.839422	2502.442888	21.680064
84.568191	2526.791217	21.685082
84.683128	2533.350042	21.690099
84.744711	2539.878839	21.695117
84.969793	2521.687178	21.700135
85.255301	2519.768947	21.705152
85.386934	2525.537775	21.710170
85.179450	2518.238752	21.715187
85.491572	2529.910135	21.720205
85.615025	2543.172909	21.725223
85.500479	2555.573052	21.730240
85.651113	2557.059262	21.735258
86.423514	2550.165556	21.740275
85.872806	2538.465471	21.745293
85.663579	2547.285404	21.750311
86.139725	2533.443408	21.755328
86.278317	2544.599759	21.760346
86.159138	2534.612389	21.765363
86.366263	2537.503798	21.770381
86.247150	2542.119429	21.775399
86.267102	2533.307782	21.780416
86.349413	2532.936839	21.785434
86.626612	2546.063409	21.790451
86.636083	2551.905214	21.795469
86.593707	2566.460793	21.800487
87.000188	2558.926196	21.805504
87.075437	2569.257355	21.810522
87.127420	2560.925883	21.815539
87.018074	2566.671019	21.820557
87.167644	2563.645764	21.825575
87.316423	2554.466694	21.830592
87.101491	2551.096856	21.835610
87.466235	2543.085983	21.840627
87.481467	2558.579370	21.845645
87.626076	2566.746687	21.850663
87.776492	2552.638064	21.855680
87.557506	2573.787908	21.860698
87.981396	2587.669018	21.865715
87.827998	2581.738584	21.870733
87.976688	2598.427521	21.875751
87.818152	2592.929717	21.880768
88.044158	2588.049385	21.885786
88.375651	2594.887538	21.890803
88.364390	2594.157119	21.895821
88.537313	2579.031806	21.900839
88.525619	2574.054884	21.905856
88.781384	2591.481825	21.910874
89.020740	2601.911112	21.915891
89.166307	2608.631049	21.920909
89.158947	2594.636426	21.925927
89.124453	2581.319429	21.930944
88.677237	2588.019050	21.935962
89.081512	2589.964275	21.940979
89.434126	2601.566336	21.945997
88.814944	2613.948683	21.951015
89.424542	2613.584893	21.956032
88.942158	2609.850259	21.961050
89.112346	2606.223143	21.966067
89.835590	2627.276295	21.971085
89.595945	2633.160218	21.976103
89.968316	2638.110444	21.981120
89.923312	2633.363767	21.986138
89.630307	2624.519383	21.991155
89.920726	2633.555435	21.996173
89.766481	2631.354154	22.001191
90.156328	2636.783748	22.006208
90.018959	2660.477780	22.011226
89.822163	2666.382413	22.016243
90.573441	2653.542544	22.021261
90.232329	2658.768583	22.026279
90.450033	2664.022708	22.031296
90.656719	2685.971614	22.036314
90.530619	2693.814851	22.041331
91.117058	2691.793552	22.046349
90.855496	2695.345715	22.051367
91.307377	2685.212117	22.056384
91.444646	2689.804215	22.061402
91.336451	2681.546984	22.066419
91.537837	2680.893554	22.071437
91.355505	2688.161346	22.076455
91.601567	2682.311896	22.081472
91.650513	2687.161909	22.086490
91.751404	2679.476197	22.091507
91.778823	2682.633045	22.096525
91.555797	2686.613239	22.101543
91.863201	2700.555508	22.106560
91.938453	2718.238700	22.111578
91.999923	2710.239917	22.116595
91.989391	2714.529957	22.121613
92.066020	2709.295859	22.126631
92.189827	2708.552547	22.131648
92.344713	2726.890836	22.136666
92.469948	2736.238027	22.141683
92.888424	2728.938970	22.146701
92.683754	2747.992184	22.151719
93.186551	2734.247215	22.156736
92.955030	2736.389022	22.161754
93.082423	2740.016818	22.166771
93.244249	2734.363262	22.171789
93.097067	2730.031632	22.176807
92.913216	2740.823464	22.181824
93.262525	2742.744441	22.186842
92.874742	2769.657059	22.191859
93.530429	2761.985872	22.196877
93.483624	2767.318396	22.201895
93.517335	2765.843791	22.206912
93.767105	2787.466638	22.211930
93.774163	2799.417348	22.216947
93.990129	2792.608331	22.221965
94.232251	2797.638374	22.226983
94.474010	2779.934546	22.232000
94.807569	2789.795996	22.237018
94.873584	2776.137944	22.242035
95.095676	2768.628711	22.247053
95.141513	2769.612527	22.252071
95.102217	2783.173622	22.257088
94.869195	2786.360225	22.262106
94.837866	2773.145587	22.267123
94.787015	2766.227324	22.272141
94.883515	2766.424369	22.277159
95.147083	2767.146149	22.282176
95.202544	2769.479737	22.287194
95.012732	2773.367350	22.292211
95.505661	2764.784538	22.297229
95.742327	2789.112878	22.302247
95.831144	2789.922305	22.307264
95.705296	2785.123972	22.312282
95.843019	2790.260328	22.317299
95.969365	2785.675052	22.322317
95.806790	2792.408031	22.327335
96.019619	2790.358202	22.332352
96.366291	2784.034104	22.337370
96.346379	2793.958215	22.342387
96.416949	2789.330705	22.347405
96.359723	2790.843794	22.352423
96.267540	2779.151409	22.357440
96.395320	2796.902617	22.362458
96.554510	2795.249115	22.367475
96.652504	2799.311863	22.372493
96.944995	2807.683051	22.377511
97.007370	2817.922052	22.382528
97.429650	2811.007764	22.387546
96.865881	2822.701860	22.392563
97.376064	2806.367860	22.397581
97.303573	2815.080415	22.402599
97.312847	2818.771115	22.407616
97.465983	2810.361232	22.412634
97.517147	2810.628431	22.417651
97.542473	2815.732380	22.422669
97.701193	2836.849904	22.427687
97.567104	2835.955789	22.432704
97.835585	2836.594988	22.437722
97.762848	2848.129000	22.442739
98.079519	2840.701395	22.447757
98.136062	2849.974664	22.452775
97.885613	2867.303322	22.457792
98.213429	2863.821692	22.462810
98.380140	2875.282934	22.467827
98.493756	2866.707850	22.472845
98.586286	2882.726478	22.477863
98.625280	2887.954910	22.482880
99.067787	2894.516724	22.487898
99.144766	2894.885208	22.492915
99.171587	2885.470530	22.497933
99.484651	2885.963399	22.502951
99.263789	2889.095386	22.507968
99.481079	2892.549214	22.512986
99.295191	2896.610064	22.518003
99.387385	2899.660669	22.523021
99.426873	2917.619599	22.528039
99.262088	2920.341501	22.533056
99.812492	2911.706178	22.538074
99.641555	2922.522828	22.543091
100.066293	2937.631972	22.548109
100.322328	2941.204697	22.553127
100.219576	2941.844105	22.558144
100.474302	2949.852497	22.563162
100.600504	2947.943885	22.568179
100.611595	2939.079132	22.573197
100.732595	2942.601026	22.578215
100.973476	2944.628204	22.583232
101.090944	2935.120383	22.588250
100.765006	2947.949424	22.593267
100.966637	2954.299548	22.598285
101.182023	2967.996394	22.603303
101.331878	2979.269269	22.608320
101.179778	2972.570775	22.613338
101.624542	2980.629111	22.618355
101.624201	2978.056357	22.623373
101.462181	2975.359151	22.628391
101.170872	2968.806349	22.633408
102.031048	2981.015240	22.638426
101.943711	2969.327435	22.643443
102.065522	2985.103176	22.648461
102.506562	2986.552563	22.653479
102.036032	2996.644629	22.658496
102.352746	2992.843033	22.663514
101.991382	2994.394415	22.668531
102.341326	2994.164056	22.673549
102.189202	2993.629124	22.678567
102.242806	3006.133406	22.683584
102.651811	3000.975200	22.688602
102.804666	3021.185437	22.693619
102.850737	3019.369824	22.698637
103.122868	3019.395710	22.703655
102.979811	3022.277772	22.708672
103.350128	3026.723482	22.713690
103.632759	3043.929588	22.718707
103.547497	3047.478106	22.723725
103.472419	3047.848817	22.728743
103.621959	3053.476564	22.733760
103.789242	3035.896783	22.738778
103.651963	3041.051910	22.743795
103.716723	3068.516667	22.748813
104.266051	3079.921777	22.753831
104.281099	3076.091965	22.758848
104.227307	3065.044512	22.763866
104.285448	3073.127581	22.768883
104.485871	3067.836645	22.773901
104.501303	3072.002305	22.778919
104.297187	3093.866312	22.783936
105.096708	3087.714499	22.788954
105.128256	3085.845346	22.793971
105.353521	3084.584003	22.798989
105.344962	3083.433096	22.804007
105.160032	3092.156666	22.809024
105.717106	3078.354741	22.814042
105.726650	3095.118352	22.819059
105.627910	3092.123933	22.824077
105.743349	3086.922053	22.829095
105.746865	3084.632619	22.834112
106.023733	3083.618684	22.839130
105.931714	3096.176942	22.844147
106.081981	3120.315104	22.849165
106.305857	3119.934159	22.854183
106.119533	3130.768361	22.859200
106.409988	3117.748298	22.864218
106.275944	3120.449603	22.869235
106.596230	3112.476187	22.874253
106.793532	3110.694654	22.879271
106.703425	3111.775682	22.884288
106.891376	3113.131722	22.889306
106.706861	3115.096186	22.894323
106.911376	3133.024347	22.899341
107.017010	3134.100907	22.904359
107.363407	3141.717231	22.909376
107.175033	3137.272486	22.914394
106.960108	3147.321537	22.919411
107.075159	3150.061785	22.924429
107.262289	3168.596068	22.929447
107.120921	3175.039525	22.934464
107.132019	3184.546002	22.939482
107.634405	3199.694165	22.944499
107.881209	3208.698203	22.949517
107.951112	3195.285339	22.954535
108.208826	3214.720860	22.959552
108.570831	3225.655690	22.964570
108.578063	3242.246789	22.969587
108.724251	3221.098272	22.974605
108.948264	3222.969290	22.979623
108.854808	3222.994479	22.984640
109.422668	3221.061028	22.989658
109.429813	3229.204230	22.994675
108.893988	3229.119832	22.999693
109.233611	3223.722479	23.004711
109.197617	3223.696031	23.009728
109.171336	3232.239429	23.014746
109.370499	3254.604137	23.019763
109.636430	3246.888664	23.024781
109.830182	3244.365145	23.029799
109.791945	3258.766585	23.034816
110.401092	3245.756944	23.039834
110.186286	3255.616483	23.044851
110.068503	3255.732862	23.049869
110.735660	3268.806558	23.054887
110.711415	3268.136382	23.059904
111.104023	3276.832469	23.064922
110.901056	3273.655626	23.069939
111.150254	3271.688817	23.074957
111.328182	3271.083940	23.079975
111.071428	3273.417053	23.084992
110.821507	3280.105976	23.090010
111.158256	3270.491392	23.095027
111.039573	3273.196568	23.100045
111.549580	3269.467908	23.105063
111.401471	3276.313644	23.110080
111.631550	3269.000315	23.115098
111.653650	3278.995929	23.120115
111.835081	3289.017271	23.125133
112.268642	3288.368484	23.130151
111.863942	3299.162120	23.135168
111.963553	3282.408524	23.140186
112.300211	3272.937112	23.145203
112.304566	3284.082400	23.150221
112.445771	3268.039555	23.155239
112.298958	3298.656507	23.160256
112.390266	3307.965427	23.165274
112.332186	3314.439713	23.170291
112.266144	3304.789438	23.175309
112.624259	3320.410661	23.180327
112.628711	3344.890228	23.185344
113.038286	3351.175118	23.190362
113.022432	3340.241754	23.195379
113.297776	3369.748522	23.200397
113.675049	3367.375848	23.205415
113.307614	3378.077075	23.210432
113.741744	3363.091791	23.215450
113.732240	3373.176674	23.220467
113.662081	3370.988615	23.225485
114.321809	3378.187762	23.230503
114.195528	3386.272882	23.235520
114.444354	3391.007093	23.240538
114.803100	3387.297018	23.245555
114.246083	3399.677186	23.250573
114.941511	3379.753683	23.255591
115.112357	3394.788160	23.260608
115.019395	3397.736247	23.265626
115.217311	3380.336017	23.270643
115.083464	3392.528354	23.275661
115.449689	3395.873603	23.280679
115.416257	3411.572304	23.285696
115.321560	3415.922381	23.290714
115.442353	3409.975416	23.295731
115.539084	3415.974344	23.300749
115.827396	3400.103759	23.305767
115.749749	3403.131997	23.310784
115.866331	3426.850492	23.315802
116.049685	3435.193037	23.320819
116.117080	3432.940559	23.325837
116.311841	3425.224542	23.330855
116.231256	3431.479076	23.335872
116.450712	3450.078570	23.340890
116.956602	3468.552968	23.345907
116.972500	3473.240181	23.350925
116.759415	3466.995610	23.355943
117.318215	3471.486917	23.360960
117.184109	3464.461249	23.365978
117.118370	3470.280804	23.370995
117.098773	3479.723934	23.376013
117.500965	3478.832365	23.381031
117.510301	3482.432765	23.386048
117.778900	3485.406596	23.391066
118.109314	3480.514041	23.396083
118.159182	3487.661037	23.401101
118.336066	3478.846606	23.406119
118.300393	3485.685523	23.411136
118.446213	3492.071527	23.416154
118.174254	3486.781825	23.421171
118.213230	3489.594836	23.426189
118.807822	3501.148023	23.431207
118.620219	3513.893358	23.436224
118.790805	3519.526583	23.441242
118.766771	3512.406254	23.446259
118.739921	3514.454180	23.451277
118.932330	3515.211733	23.456295
119.243236	3532.528753	23.461312
119.574648	3537.161744	23.466330
119.745066	3534.470418	23.471347
119.463006	3539.578012	23.476365
119.806943	3535.040399	23.481383
119.920708	3549.551610	23.486400
119.430018	3550.875103	23.491418
119.776160	3557.703513	23.496435
119.906613	3570.217264	23.501453
120.049589	3576.014594	23.506471
120.510082	3577.498700	23.511488
120.427366	3590.654502	23.516506
120.988406	3601.582264	23.521523
120.931089	3599.540791	23.526541
121.357150	3594.367862	23.531559
121.085640	3593.290308	23.536576
121.255892	3589.629118	23.541594
121.322017	3591.755836	23.546611
121.523593	3582.306551	23.551629
121.784766	3570.805752	23.556647
121.707207	3600.659515	23.561664
121.944298	3614.616236	23.566682
122.426235	3614.260207	23.571699
121.839604	3619.984320	23.576717
122.143249	3606.641573	23.581735
122.503330	3613.197983	23.586752
122.088098	3617.837570	23.591770
122.408619	3613.245459	23.596787
122.164320	3612.607209	23.601805
122.280370	3627.337595	23.606823
122.342418	3636.867707	23.611840
122.584710	3646.623158	23.616858
123.003689	3663.220663	23.621875
123.028367	3677.894088	23.626893
123.445016	3671.060533	23.631911
123.799553	3670.086879	23.636928
123.526222	3677.890404	23.641946
123.609018	3657.209957	23.646963
123.956938	3685.875137	23.651981
123.795205	3687.603206	23.656999
124.024915	3689.460792	23.662016
124.128608	3689.823465	23.667034
124.487742	3684.341028	23.672051
124.184217	3690.088461	23.677069
124.464157	3702.864815	23.682087
124.860699	3708.115976	23.687104
124.453129	3718.296034	23.692122
124.782780	3731.746477	23.697139
124.759085	3715.530423	23.702157
124.847719	3716.649070	23.707175
125.080091	3710.799037	23.712192
125.212958	3731.921981	23.717210
125.450965	3738.372841	23.722227
125.269677	3742.760419	23.727245
125.409875	3745.422043	23.732263
125.979525	3755.594976	23.737280
125.557751	3771.355985	23.742298
126.026941	3771.950641	23.747315
126.281478	3766.839614	23.752333
126.176455	3767.212757	23.757351
126.351137	3764.202919	23.762368
126.363387	3791.580656	23.767386
127.027727	3783.311316	23.772403
126.807611	3796.272893	23.777421
127.039174	3796.557756	23.782439
127.393046	3786.801662	23.787456
127.260233	3798.637050	23.792474
127.299330	3786.562653	23.797491
127.436005	3793.339621	23.802509
127.177724	3816.323254	23.807527
127.639073	3809.195394	23.812544
127.813782	3824.534119	23.817562
127.949471	3815.644247	23.822579
127.979753	3821.829353	23.827597
127.895949	3841.529406	23.832615
128.193579	3842.225363	23.837632
128.294070	3846.217998	23.842650
128.202550	3849.417663	23.847667
128.055078	3861.399388	23.852685
128.287150	3875.624609	23.857703
128.662808	3883.118666	23.862720
128.650939	3902.915098	23.867738
129.137452	3898.116296	23.872755
129.241042	3902.318480	23.877773
129.582645	3902.581080	23.882791
129.753734	3902.571168	23.887808
129.599750	3915.836953	23.892826
129.965753	3924.482609	23.897843
130.003925	3928.520601	23.902861
130.217143	3925.965546	23.907879
130.342878	3932.162224	23.912896
130.497785	3935.834705	23.917914
130.539340	3929.842741	23.922931
130.515890	3934.091149	23.927949
130.588735	3950.558530	23.932967
131.146998	3949.826907	23.937984
130.998968	3965.100033	23.943002
130.884106	3955.858289	23.948019
130.916959	3953.247033	23.953037
131.060384	3968.188146	23.958055
131.407748	3981.792534	23.963072
131.370783	3989.357946	23.968090
131.890881	3982.717781	23.973107
132.088940	3988.427044	23.978125
131.929616	3990.168137	23.983143
132.012731	3991.074509	23.988160
132.174573	3991.597043	23.993178
132.201283	4000.744434	23.998195
132.409159	4016.095377	24.003213
132.136892	4019.806100	24.008231
132.700298	4013.743480	24.013248
132.592283	4039.479503	24.018266
132.980085	4031.044878	24.023283
133.182630	4031.185702	24.028301
132.765272	4034.093605	24.033319
133.059996	4036.757389	24.038336
133.125133	4057.549420	24.043354
133.482026	4066.531717	24.048371
133.893230	4065.546645	24.053389
133.787959	4060.156211	24.058407
134.299961	4080.506521	24.063424
134.446384	4087.234874	24.068442
134.995601	4083.072625	24.073459
135.166977	4089.994445	24.078477
135.009596	4097.364361	24.083495
135.193831	4084.802466	24.088512
135.332001	4079.520308	24.093530
135.472999	4066.276235	24.098547
135.591863	4052.247503	24.103565
135.442684	4054.544705	24.108583
135.838028	4059.210935	24.113600
135.887106	4071.242516	24.118618
135.767155	4069.704966	24.123635
136.085728	4070.566721	24.128653
135.901897	4070.205140	24.133671
136.346635	4058.872921	24.138688
136.295600	4063.238252	24.143706
136.282437	4064.156835	24.148723
136.198305	4065.960677	24.153741
136.339180	4076.193551	24.158759
136.620570	4090.492142	24.163776
136.290360	4093.725198	24.168794
136.383891	4091.113682	24.173811
136.692521	4107.040988	24.178829
136.461081	4126.104981	24.183847
136.848150	4135.959604	24.188864
136.873300	4151.149460	24.193882
137.115165	4159.143266	24.198899
137.463974	4177.939388	24.203917
137.476877	4187.168547	24.208935
138.031558	4182.103917	24.213952
137.791433	4193.483965	24.218970
137.811526	4210.207840	24.223987
138.542227	4213.028692	24.229005
138.550241	4219.860199	24.234023
138.842444	4217.782575	24.239040
138.833403	4233.294195	24.244058
138.820307	4245.142318	24.249075
139.232760	4241.063977	24.254093
139.357740	4232.483137	24.259111
139.666134	4247.554773	24.264128
139.367013	4244.124016	24.269146
139.560052	4230.489192	24.274163
139.814893	4237.216847	24.279181
139.862026	4257.101106	24.284199
140.122441	4250.480990	24.289216
140.330591	4260.534140	24.294234
139.966843	4256.953997	24.299251
140.289970	4263.189353	24.304269
140.254036	4282.671546	24.309287
140.631311	4290.222982	24.314304
140.761997	4292.610899	24.319322
140.797989	4287.698160	24.324339
141.029679	4303.764598	24.329357
141.242113	4325.716632	24.334375
141.674843	4314.217792	24.339392
141.714155	4315.307377	24.344410
141.468558	4315.355251	24.349427
141.787450	4318.204815	24.354445
141.982976	4336.356935	24.359463
142.161260	4331.599276	24.364480
142.374550	4338.773336	24.369498
142.341612	4342.683545	24.374515
142.792087	4331.273113	24.379533
142.604333	4342.970596	24.384551
142.733527	4354.978622	24.389568
142.920300	4356.973725	24.394586
143.194664	4364.778388	24.399603
143.024473	4368.252661	24.404621
142.886962	4384.730471	24.409639
143.395560	4391.907031	24.414656
143.322064	4397.201925	24.419674
143.304716	4411.815135	24.424691
143.695400	4411.321035	24.429709
143.488742	4428.366865	24.434727
144.080944	4442.495100	24.439744
144.460904	4453.349329	24.444762
144.733259	4458.073059	24.449779
144.810229	4452.367083	24.454797
145.176860	4463.805566	24.459815
145.432897	4456.480431	24.464832
145.155035	4451.465070	24.469850
145.109113	4459.110816	24.474867
145.547892	4458.080419	24.479885
145.437658	4462.647250	24.484903
145.226509	4480.364868	24.489920
145.591151	4483.787719	24.494938
145.663722	4472.487778	24.499955
145.941141	4501.415954	24.504973
146.011968	4520.956173	24.509991
146.321713	4508.261414	24.515008
146.211805	4516.010216	24.520026
146.413838	4515.732630	24.525043
146.556980	4525.001022	24.530061
146.716852	4527.310379	24.535079
146.911892	4537.627765	24.540096
147.268247	4531.546818	24.545114
147.676611	4528.800855	24.550131
147.747738	4550.339951	24.555149
147.400762	4556.866354	24.560167
147.562073	4555.770846	24.565184
148.002086	4557.787746	24.570202
147.787160	4564.059461	24.575219
148.090773	4565.565544	24.580237
148.231208	4578.939168	24.585255
148.186123	4582.863177	24.590272
148.574142	4583.977423	24.595290
148.530527	4586.901360	24.600307
149.366282	4592.462772	24.605325
149.044231	4617.610116	24.610343
149.260119	4612.283911	24.615360
149.287975	4601.312743	24.620378
149.053976	4610.735720	24.625395
149.895111	4624.088131	24.630413
150.097114	4633.671310	24.635431
149.923856	4633.197895	24.640448
150.477477	4635.948737	24.645466
150.278564	4630.211160	24.650483
150.398661	4631.496353	24.655501
150.256214	4646.860549	24.660519
150.546975	4651.911805	24.665536
150.991330	4664.527483	24.670554
150.742324	4662.358304	24.675571
151.074393	4667.345553	24.680589
151.292203	4695.888714	24.685607
151.184989	4683.612709	24.690624
151.859813	4686.622716	24.695642
151.840621	4678.283295	24.700659
151.780601	4683.993860	24.705677
152.411533	4711.829269	24.710695
152.338805	4707.371109	24.715712
152.640111	4713.614859	24.720730
152.246020	4710.597183	24.725747
152.630667	4710.708195	24.730765
152.627362	4713.850715	24.735783
152.974056	4724.883518	24.740800
153.214010	4735.818495	24.745818
153.312938	4733.629231	24.750835
153.398186	4743.585883	24.755853
153.242188	4750.053601	24.760871
153.461473	4761.658198	24.765888
153.597493	4763.339703	24.770906
153.423229	4779.094576	24.775923
154.013714	4778.729878	24.780941
154.273874	4788.476953	24.785959
154.176218	4798.492698	24.790976
154.292883	4801.306162	24.795994
154.322331	4806.313388	24.801011
154.547790	4820.824572	24.806029
154.556347	4842.773701	24.811047
154.878094	4838.896102	24.816064
155.494970	4843.916669	24.821082
155.597109	4854.027251	24.826099
155.626301	4861.875204	24.831117
155.580900	4862.597589	24.836135
155.663962	4861.156600	24.841152
156.323463	4857.993722	24.846170
156.111681	4880.323386	24.851187
156.395157	4880.494585	24.856205
156.688409	4889.148484	24.861223
156.404081	4888.988557	24.866240
157.102834	4883.981750	24.871258
156.794200	4910.840040	24.876275
156.847819	4912.326233	24.881293
157.237970	4901.669174	24.886311
157.319793	4919.270595	24.891328
157.475143	4935.806169	24.896346
157.429927	4943.603883	24.901363
157.934854	4933.136184	24.906381
157.895153	4952.192701	24.911399
157.979666	4966.945198	24.916416
158.460145	4964.098766	24.921434
158.442139	4958.866368	24.926451
158.311426	4963.794557	24.931469
159.021421	4987.131470	24.936487
158.990163	4981.134167	24.941504
159.235482	4990.088413	24.946522
159.464560	4990.548344	24.951539
159.735923	5004.180752	24.956557
159.792052	5026.386108	24.961575
159.942353	5022.379247	24.966592
160.452860	5014.506644	24.971610
160.080125	5015.875168	24.976627
159.982766	5014.402356	24.981645
160.281942	5022.674637	24.986663
160.334263	5035.938432	24.991680
160.593914	5037.893690	24.996698
160.658287	5035.349591	25.001715
161.191300	5044.873972	25.006733
160.954322	5062.457952	25.011751
161.208270	5066.925211	25.016768
161.679609	5065.685835	25.021786
161.609646	5088.906540	25.026803
161.638561	5095.951460	25.031821
161.988830	5088.116953	25.036839
161.821586	5098.124330	25.041856
162.167013	5119.696835	25.046874
162.216827	5119.595339	25.051891
162.836121	5114.875678	25.056909
163.207707	5120.112456	25.061927
162.753688	5117.118408	25.066944
163.287233	5134.432515	25.071962
163.450866	5145.785896	25.076979
164.051265	5143.956377	25.081997
164.190277	5141.122660	25.087015
164.111714	5145.495061	25.092032
164.373393	5146.841116	25.097050
164.310048	5155.129577	25.102067
164.395980	5140.765996	25.107085
164.433567	5134.671119	25.112103
164.343438	5138.176861	25.117120
164.658150	5136.412558	25.122138
164.676257	5157.381998	25.127155
164.610589	5166.736009	25.132173
164.872626	5173.672210	25.137191
164.951331	5181.294528	25.142208
165.121402	5189.027366	25.147226
165.159508	5202.989797	25.152243
165.183017	5212.095973	25.157261
165.792263	5223.847235	25.162279
165.616435	5244.400092	25.167296
165.994231	5262.309533	25.172314
166.350796	5273.154731	25.177331
165.982705	5284.625249	25.182349
166.506870	5292.876760	25.187367
166.861641	5294.181239	25.192384
167.324358	5302.358377	25.197402
167.563821	5326.340419	25.202419
167.267392	5327.314469	25.207437
167.803640	5334.431235	25.212455
167.482423	5338.631546	25.217472
168.001628	5344.598524	25.222490
168.078503	5351.318094	25.227507
168.537750	5358.628876	25.232525
168.600731	5359.426048	25.237543
168.630007	5362.247260	25.242560
169.022781	5358.702777	25.247578
169.015062	5384.472365	25.252595
169.078998	5381.370508	25.257613
169.370000	5379.990720	25.262631
169.256669	5394.123802	25.267648
169.657168	5396.043280	25.272666
169.701821	5398.862047	25.277683
169.703159	5407.230807	25.282701
170.043573	5405.780204	25.287719
169.893258	5428.130004	25.292736
170.316064	5426.906206	25.297754
170.039067	5443.793709	25.302771
170.391047	5457.925042	25.307789
170.583902	5465.479746	25.312807
170.774781	5487.064058	25.317824
171.174939	5485.828919	25.322842
171.488478	5491.998677	25.327859
171.396586	5494.489149	25.332877
172.183587	5511.614606	25.337895
171.965563	5518.842278	25.342912
172.306014	5511.213659	25.347930
172.266373	5514.233123	25.352947
172.419797	5516.551534	25.357965
172.424855	5508.249472	25.362983
172.807646	5534.562039	25.368000
173.116867	5531.339226	25.373018
173.278735	5534.352529	25.378035
173.063379	5538.761015	25.383053
173.245188	5547.118390	25.388071
173.557703	5552.394637	25.393088
173.826145	5559.462167	25.398106
173.948383	5563.666576	25.403123
174.037223	5562.072764	25.408141
174.544582	5563.957134	25.413159
174.558409	5590.188591	25.418176
174.108404	5590.860658	25.423194
174.556142	5602.154150	25.428211
174.757404	5614.146997	25.433229
175.406575	5609.617525	25.438247
175.432738	5622.062332	25.443264
175.822556	5615.671153	25.448282
175.701899	5628.635001	25.453299
175.834696	5642.592980	25.458317
176.347287	5636.562200	25.463335
176.086251	5656.222921	25.468352
176.372710	5651.941649	25.473370
176.773886	5651.642524	25.478387
176.804134	5682.421876	25.483405
177.222311	5666.176489	25.488423
177.220572	5675.529285	25.493440
177.380570	5672.799115	25.498458
177.515026	5686.700227	25.503475
177.759648	5707.801120	25.508493
178.164304	5704.688143	25.513511
177.931187	5704.114092	25.518528
177.895370	5702.563741	25.523546
178.288628	5711.817396	25.528563
178.209854	5723.853406	25.533581
178.438643	5729.707929	25.538599
178.535956	5749.612955	25.543616
178.742560	5762.104638	25.548634
179.097916	5766.253059	25.553651
178.943701	5774.878123	25.558669
179.387136	5786.587045	25.563687
179.603145	5800.772644	25.568704
179.752422	5797.125270	25.573722
179.927960	5808.867480	25.578739
180.175639	5822.891493	25.583757
180.610074	5818.813945	25.588775
180.987683	5821.135212	25.593792
181.272277	5827.053256	25.598810
181.743812	5832.983982	25.603827
181.392749	5850.471438	25.608845
182.159602	5835.680787	25.613863
181.870152	5841.970429	25.618880
181.998612	5844.115860	25.623898
182.092242	5826.689244	25.628915
182.031268	5833.824373	25.633933
182.088430	5837.317025	25.638951
182.200005	5835.618072	25.643968
182.251857	5850.834535	25.648986
182.366673	5861.392222	25.654003
182.058138	5865.943110	25.659021
182.733949	5871.381050	25.664039
182.952959	5894.516044	25.669056
182.928673	5902.469846	25.674074
183.454344	5922.033819	25.679092
183.494283	5929.550203	25.684109
183.643834	5935.304153	25.689127
183.656851	5952.956329	25.694144
183.999150	5957.288621	25.699162
184.285537	5962.951534	25.704180
184.279027	5995.475285	25.709197
184.747999	5997.949590	25.714215
185.498867	5998.823585	25.719232
185.267633	6021.127391	25.724250
185.413708	6012.531927	25.729268
185.855852	6028.683928	25.734285
185.774803	6022.088354	25.739303
185.824971	6030.048449	25.744320
186.125191	6040.511407	25.749338
186.439331	6044.599607	25.754356
186.228313	6055.891478	25.759373
186.809395	6057.738987	25.764391
186.659747	6074.146665	25.769408
186.996561	6078.216312	25.774426
187.273169	6096.255407	25.779444
187.157175	6107.043604	25.784461
187.612069	6098.980256	25.789479
187.761148	6123.851286	25.794496
187.852287	6131.051209	25.799514
188.160039	6139.918318	25.804532
188.028269	6145.178283	25.809549
188.756170	6155.127058	25.814567
188.995927	6167.691688	25.819584
188.801246	6172.617887	25.824602
189.191942	6178.445991	25.829620
189.195142	6188.900549	25.834637
189.646044	6197.933689	25.839655
189.435603	6203.438306	25.844672
189.791352	6209.488349	25.849690
190.233149	6216.379079	25.854708
190.275540	6217.731874	25.859725
190.422217	6222.947476	25.864743
190.488193	6231.486563	25.869760
190.808918	6239.102315	25.874778
191.167405	6252.046967	25.879796
190.882619	6256.144955	25.884813
191.051531	6270.592634	25.889831
191.217139	6274.105864	25.894848
191.336001	6285.903122	25.899866
191.944471	6297.794632	25.904884
191.783870	6306.263673	25.909901
191.818136	6305.210324	25.914919
192.018935	6310.590413	25.919936
192.324449	6327.769202	25.924954
192.371418	6341.807613	25.929972
192.524620	6345.725654	25.934989
192.753826	6359.571385	25.940007
193.280891	6368.500439	25.945024
193.618510	6389.773156	25.950042
194.069841	6378.559283	25.955060
194.068458	6387.373548	25.960077
194.471284	6389.563435	25.965095
194.547616	6399.583210	25.970112
194.535582	6403.688107	25.975130
194.933905	6406.571057	25.980148
195.042928	6403.848881	25.985165
195.278100	6402.531404	25.990183
195.532821	6426.779516	25.995200
195.774145	6428.405091	26.000218
195.767195	6434.616901	26.005236
195.790192	6438.376345	26.010253
196.210943	6435.489600	26.015271
196.592969	6452.036374	26.020288
196.409621	6461.849762	26.025306
196.433074	6453.880968	26.030324
196.716374	6472.849404	26.035341
196.689420	6486.069708	26.040359
196.769074	6502.095131	26.045376
197.138992	6518.594344	26.050394
197.564739	6526.540463	26.055412
197.589185	6539.142096	26.060429
197.786595	6544.765133	26.065447
198.184317	6547.346879	26.070464
198.057443	6574.606421	26.075482
198.519983	6585.676447	26.080500
199.035986	6594.234478	26.085517
198.909956	6610.401382	26.090535
199.295229	6611.004052	26.095552
199.362165	6615.641646	26.100570
199.565338	6619.894823	26.105588
199.578185	6636.581696	26.110605
199.802336	6650.747933	26.115623
200.305299	6654.542637	26.120640
200.262714	6668.144030	26.125658
200.708768	6680.904372	26.130676
200.666650	6679.079553	26.135693
200.848102	6706.435737	26.140711
201.238980	6699.780360	26.145728
200.585953	6717.260327	26.150746
201.125227	6726.138088	26.155764
201.709520	6739.165974	26.160781
201.914696	6757.558725	26.165799
202.212655	6760.467976	26.170816
201.852916	6775.075169	26.175834
202.421910	6768.363830	26.180852
202.667443	6794.292196	26.185869
203.063980	6792.561869	26.190887
203.339157	6800.557318	26.195904
202.996657	6803.757504	26.200922
203.319414	6809.569943	26.205940
203.475026	6830.704729	26.210957
203.507572	6839.621642	26.215975
203.969236	6834.880163	26.220992
204.366701	6856.277765	26.226010
204.656657	6844.339471	26.231028
204.896980	6869.582731	26.236045
205.026720	6869.826467	26.241063
205.726606	6880.670052	26.246080
205.488465	6885.178554	26.251098
205.678769	6864.793541	26.256116
205.992560	6889.105380	26.261133
206.046618	6903.450037	26.266151
206.401175	6905.244082	26.271168
206.311416	6906.920132	26.276186
206.714840	6910.714249	26.281204
206.671670	6933.784880	26.286221
206.899846	6924.701372	26.291239
207.159464	6937.887410	26.296256
207.549560	6958.201363	26.301274
208.146207	6946.424167	26.306292
207.898770	6949.066349	26.311309
207.766189	6959.203993	26.316327
208.141522	6974.907418	26.321344
208.457583	6983.524302	26.326362
208.703832	6981.404065	26.331380
208.716564	7001.948182	26.336397
209.105557	7011.675412	26.341415
209.571508	6999.241587	26.346432
209.263033	7013.414404	26.351450
209.527731	7031.175661	26.356468
209.895699	7034.741787	26.361485
209.902380	7050.962759	26.366503
210.094952	7057.811793	26.371520
210.280909	7063.646140	26.376538
210.563456	7087.482559	26.381556
210.651589	7104.167398	26.386573
210.655050	7113.001778	26.391591
211.050808	7121.073381	26.396608
211.258687	7131.716277	26.401626
211.639645	7151.176710	26.406644
211.992256	7154.716203	26.411661
211.846045	7165.875845	26.416679
212.274489	7175.942297	26.421696
212.821983	7190.837220	26.426714
212.745877	7182.857941	26.431732
213.203830	7198.505946	26.436749
213.142101	7198.180674	26.441767
213.813791	7200.298715	26.446784
213.630031	7200.888269	26.451802
213.883530	7212.328055	26.456820
214.330743	7211.139574	26.461837
214.130477	7231.829690	26.466855
214.445352	7230.002969	26.471872
214.502894	7231.715369	26.476890
214.848898	7245.276588	26.481908
214.822426	7252.856161	26.486925
215.318636	7257.159586	26.491943
215.374796	7269.553003	26.496960
215.498726	7290.879969	26.501978
215.598608	7294.675368	26.506996
216.051536	7306.914297	26.512013
215.895105	7327.418954	26.517031
216.232238	7328.669790	26.522048
216.197870	7356.799601	26.527066
216.474022	7353.549415	26.532084
216.863923	7374.202298	26.537101
216.944857	7393.216765	26.542119
217.542582	7400.722872	26.547136
217.963014	7419.278047	26.552154
217.988913	7426.007475	26.557172
218.284301	7432.867831	26.562189
218.272795	7450.889208	26.567207
218.762061	7441.202770	26.572224
218.872950	7457.763212	26.577242
219.575179	7459.038473	26.582260
219.656099	7464.584443	26.587277
219.320862	7475.112742	26.592295
219.865551	7483.265449	26.597312
219.712339	7503.792653	26.602330
220.220204	7511.317076	26.607348
220.513206	7534.066747	26.612365
220.512891	7533.905562	26.617383
220.757410	7550.385793	26.622400
220.793025	7549.754661	26.627418
221.141403	7557.293516	26.632436
221.739507	7585.106561	26.637453
221.527269	7595.708969	26.642471
221.982184	7581.663448	26.647488
222.198028	7612.157577	26.652506
222.544401	7630.099303	26.657524
222.789839	7624.342433	26.662541
222.814865	7637.302121	26.667559
223.427763	7639.032260	26.672576
223.665545	7655.918107	26.677594
223.894167	7647.429712	26.682612
224.003098	7653.470917	26.687629
224.155935	7667.812369	26.692647
224.500981	7673.053514	26.697664
224.433777	7663.840396	26.702682
224.657690	7680.888995	26.707700
224.937642	7692.760835	26.712717
224.699197	7703.811265	26.717735
224.957584	7711.558890	26.722752
225.397053	7731.974619	26.727770
225.484190	7731.786902	26.732788
225.796826	7737.073365	26.737805
225.759940	7764.108302	26.742823
226.260279	7763.447927	26.747840
226.717430	7774.252977	26.752858
226.476597	7791.369493	26.757876
226.899779	7792.310807	26.762893
227.166238	7812.367894	26.767911
227.281523	7829.639342	26.772928
227.804262	7830.621440	26.777946
227.833053	7831.744438	26.782964
228.242190	7851.519968	26.787981
228.181309	7864.617081	26.792999
228.468605	7873.961384	26.798016
228.779535	7890.430620	26.803034
228.773124	7893.371308	26.808052
229.191984	7903.327270	26.813069
229.343127	7917.791980	26.818087
229.616340	7925.170690	26.823104
230.075811	7933.705472	26.828122
230.128613	7951.197893	26.833140
230.653240	7945.655264	26.838157
230.423366	7970.690519	26.843175
230.853699	7986.578241	26.848192
231.049776	7984.483960	26.853210
231.095757	8002.498415	26.858228
231.702654	8013.382058	26.863245
231.546138	8026.627534	26.868263
231.814592	8031.411274	26.873280
232.118317	8044.089265	26.878298
232.518769	8059.871671	26.883316
232.964213	8059.007590	26.888333
232.953886	8081.375658	26.893351
233.255258	8085.356311	26.898368
233.534598	8092.051936	26.903386
233.560516	8109.797470	26.908404
233.709254	8116.873513	26.913421
233.862888	8138.613988	26.918439
234.110746	8141.488227	26.923456
234.630144	8147.573574	26.928474
234.770357	8156.528407	26.933492
235.305329	8168.462268	26.938509
235.451015	8180.167060	26.943527
235.627400	8179.705452	26.948544
235.880772	8196.312460	26.953562
235.949611	8207.912282	26.958580
236.364570	8202.959081	26.963597
236.366973	8217.078761	26.968615
236.607790	8235.536123	26.973632
236.557163	8236.772528	26.978650
236.591630	8269.783366	26.983668
236.957551	8267.981434	26.988685
237.204667	8292.844412	26.993703
237.304018	8303.604594	26.998720
237.703408	8312.433228	27.003738
238.046006	8333.707162	27.008756
238.389542	8335.159290	27.013773
238.741462	8354.578725	27.018791
238.682989	8370.155282	27.023808
239.377692	8375.638374	27.028826
239.155046	8388.472957	27.033844
239.548143	8399.485390	27.038861
239.440942	8403.016652	27.043879
240.072812	8425.193558	27.048896
240.484827	8421.041779	27.053914
240.560754	8432.945949	27.058932
240.701332	8446.265616	27.063949
240.776469	8453.233161	27.068967
241.342611	8470.730919	27.073984
241.802261	8482.739203	27.079002
241.505983	8496.719485	27.084020
241.981553	8495.649143	27.089037
242.343731	8501.994972	27.094055
242.230051	8523.928125	27.099072
242.605247	8541.221130	27.104090
242.672909	8554.610745	27.109108
242.851123	8572.249146	27.114125
243.331734	8580.722706	27.119143
243.625717	8593.482980	27.124160
243.953794	8602.432530	27.129178
243.946348	8636.384087	27.134196
244.358483	8618.572157	27.139213
244.890798	8632.140360	27.144231
244.947674	8661.873536	27.149248
245.293370	8645.359488	27.154266
245.333128	8675.265385	27.159284
245.578600	8684.243102	27.164301
245.954897	8682.707793	27.169319
246.221574	8707.405462	27.174336
246.576972	8715.455262	27.179354
246.605180	8726.057125	27.184372
246.963399	8742.102725	27.189389
247.089522	8746.662306	27.194407
247.275087	8759.307810	27.199424
247.884069	8776.963558	27.204442
247.843357	8775.438057	27.209460
248.322523	8789.811985	27.214477
248.792094	8792.961042	27.219495
248.634459	8799.284415	27.224512
249.378052	8810.520629	27.229530
249.193924	8817.724818	27.234548
249.524516	8819.205028	27.239565
250.037597	8832.502646	27.244583
250.043747	8854.442363	27.249600
250.281677	8861.366052	27.254618
250.681094	8861.627430	27.259636
250.695916	8864.295811	27.264653
251.009332	8889.350659	27.269671
251.131266	8894.130495	27.274688
251.547041	8884.332880	27.279706
251.434148	8905.063321	27.284724
251.861594	8911.937940	27.289741
252.317881	8915.603765	27.294759
251.862931	8918.446971	27.299776
252.620489	8924.501762	27.304794
252.739706	8945.668180	27.309812
252.887483	8956.689444	27.314829
252.986536	8969.148260	27.319847
253.099013	8982.124293	27.324864
253.221733	9004.118830	27.329882
253.535905	9016.996251	27.334900
254.145516	9034.972079	27.339917
253.924425	9045.414036	27.344935
254.507917	9089.470563	27.349952
254.997602	9070.766774	27.354970
255.197927	9099.100891	27.359988
255.362473	9104.348894	27.365005
255.590128	9115.813549	27.370023
256.043009	9108.710504	27.375040
256.543631	9128.656108	27.380058
256.608222	9154.071331	27.385076
257.159050	9149.483320	27.390093
257.255368	9155.048319	27.395111
257.006907	9189.772941	27.400128
257.537055	9191.982313	27.405146
257.595082	9205.259554	27.410164
257.659210	9209.292493	27.415181
258.323751	9218.915094	27.420199
258.345464	9251.632293	27.425216
259.017785	9256.833643	27.430234
259.164971	9272.442492	27.435252
259.325090	9272.137287	27.440269
259.939673	9293.665118	27.445287
259.936153	9317.989808	27.450304
260.642274	9311.255495	27.455322
260.353115	9302.115693	27.460340
260.435702	9338.305046	27.465357
260.836134	9329.715527	27.470375
261.041854	9356.023771	27.475392
261.515148	9362.192911	27.480410
261.923354	9383.546417	27.485428
261.771926	9393.938166	27.490445
262.631243	9402.957758	27.495463
262.332603	9426.581312	27.500480
262.547192	9429.640131	27.505498
262.473761	9448.234466	27.510516
262.889644	9457.962173	27.515533
263.490301	9478.529308	27.520551
263.731664	9488.878581	27.525568
264.027186	9498.152956	27.530586
264.251568	9528.096838	27.535604
264.514010	9532.276884	27.540621
264.974452	9540.759327	27.545639
264.822372	9549.681324	27.550656
265.292061	9561.332016	27.555674
265.705729	9576.883363	27.560692
265.841814	9578.648437	27.565709
266.265467	9586.434443	27.570727
266.429326	9602.562315	27.575744
266.804423	9591.894096	27.580762
266.867363	9611.231785	27.585780
267.182845	9634.447337	27.590797
267.500700	9625.847205	27.595815
267.724486	9646.888172	27.600832
267.710059	9661.971947	27.605850
268.058150	9665.232629	27.610868
268.192038	9692.416172	27.615885
268.637577	9687.914822	27.620903
268.746627	9714.693949	27.625920
269.355317	9718.224729	27.630938
269.648431	9731.167506	27.635956
269.596579	9745.283506	27.640973
270.038490	9752.421014	27.645991
270.261081	9787.549997	27.651008
270.520269	9801.588143	27.656026
270.630009	9810.146707	27.661044
271.209582	9820.996303	27.666061
271.416039	9824.128505	27.671079
271.156963	9855.266366	27.676096
271.304634	9861.573787	27.681114
272.262494	9868.633442	27.686132
272.336318	9904.615448	27.691149
272.790190	9905.916374	27.696167
273.094546	9927.606315	27.701184
273.532518	9937.049092	27.706202
273.795371	9947.998841	27.711220
274.282836	9954.854544	27.716237
274.420459	9960.439623	27.721255
274.330103	9970.310524	27.726272
274.672035	9987.837940	27.731290
275.057105	10001.362404	27.736308
275.048811	10016.970056	27.741325
275.544151	10020.492615	27.746343
275.614287	10043.660558	27.751360
275.677269	10059.260829	27.756378
276.311769	10072.819967	27.761396
276.343298	10078.402720	27.766413
276.712331	10103.962652	27.771431
276.555447	10115.232822	27.776448
277.393784	10129.194706	27.781466
277.666726	10144.504660	27.786484
277.913751	10162.268935	27.791501
278.362830	10164.724713	27.796519
278.761065	10175.499989	27.801536
279.123112	10194.474401	27.806554
279.564457	10197.611739	27.811572
279.399345	10211.527850	27.816589
279.977713	10229.170534	27.821607
280.439148	10241.142186	27.826624
280.553608	10240.107257	27.831642
280.620710	10239.653568	27.836660
280.372406	10259.352155	27.841677
280.964551	10264.719709	27.846695
281.175809	10274.100860	27.851712
281.124593	10297.064647	27.856730
281.610127	10306.889623	27.861748
281.836790	10324.837550	27.866765
282.325468	10324.994237	27.871783
282.531383	10342.475283	27.876800
282.937854	10357.971538	27.881818
283.378773	10354.409575	27.886836
283.370364	10394.735726	27.891853
283.653859	10394.077164	27.896871
283.868991	10404.957733	27.901888
284.001889	10425.079760	27.906906
284.462312	10433.697684	27.911924
284.781146	10446.994265	27.916941
285.308488	10463.446809	27.921959
285.629623	10473.260324	27.926976
285.601441	10489.548430	27.931994
286.058309	10501.106287	27.937012
286.512753	10522.475695	27.942029
286.811103	10516.499958	27.947047
287.353862	10532.922578	27.952064
287.769450	10539.537786	27.957082
288.408530	10532.750669	27.962100
288.017525	10541.602731	27.967117
288.480894	10544.551697	27.972135
288.487273	10562.472454	27.977152
288.344252	10566.217691	27.982170
288.752366	10578.026947	27.987188
288.712081	10605.287910	27.992205
289.252656	10612.760707	27.997223
289.691770	10647.556176	28.002240
289.867020	10646.473364	28.007258
290.173665	10673.349413	28.012276
290.357027	10698.021155	28.017293
290.753450	10710.371460	28.022311
291.008369	10726.033121	28.027328
291.381527	10750.318590	28.032346
291.565177	10748.784278	28.037364
291.812558	10768.506833	28.042381
292.261932	10785.316858	28.047399
292.740882	10812.545807	28.052416
292.930234	10817.101455	28.057434
293.231829	10824.641172	28.062452
293.446847	10838.175398	28.067469
294.013069	10853.454681	28.072487
294.129490	10872.787438	28.077504
294.353963	10885.497009	28.082522
295.304104	10889.785831	28.087540
295.147590	10910.282023	28.092557
295.281135	10914.715955	28.097575
295.696245	10925.775943	28.102592
295.961840	10935.096907	28.107610
296.414222	10932.643430	28.112628
296.033230	10954.518068	28.117645
296.527283	10961.338562	28.122663
296.995847	10977.327666	28.127680
297.095299	11003.965029	28.132698
297.559070	11001.445193	28.137716
297.568781	11013.092817	28.142733
298.008296	11031.370864	28.147751
298.203206	11044.700713	28.152768
298.415325	11062.641217	28.157786
298.629323	11067.915084	28.162804
298.788420	11102.369427	28.167821
299.064222	11108.507816	28.172839
299.436943	11134.720162	28.177856
299.750515	11165.865870	28.182874
300.342998	11170.856336	28.187892
300.497772	11184.863234	28.192909
300.667604	11216.557282	28.197927
300.973044	11229.345139	28.202944
301.561881	11243.551675	28.207962
301.973269	11259.055557	28.212980
301.923806	11283.036596	28.217997
302.691534	11292.541795	28.223015
302.752532	11314.854132	28.228032
302.996816	11339.303149	28.233050
303.598202	11348.010893	28.238068
303.780021	11371.369476	28.243085
304.068033	11377.435592	28.248103
304.473908	11385.348939	28.253120
304.658274	11408.532653	28.258138
305.445334	11425.594941	28.263156
305.525304	11438.801796	28.268173
306.005102	11457.459581	28.273191
306.346208	11462.869553	28.278208
306.193216	11481.692362	28.283226
306.899674	11490.787186	28.288244
306.873940	11486.178227	28.293261
307.005974	11508.875400	28.298279
307.387941	11518.659444	28.303296
307.706381	11526.504951	28.308314
307.968370	11546.237218	28.313332
307.831084	11576.855526	28.318349
308.063253	11598.810451	28.323367
308.932444	11610.524215	28.328384
308.961752	11636.669785	28.333402
309.590618	11649.198285	28.338420
309.271382	11675.640696	28.343437
309.622982	11701.986075	28.348455
309.996895	11722.758112	28.353472
310.210595	11740.788893	28.358490
311.056651	11758.120375	28.363508
311.165254	11783.185554	28.368525
311.282439	11796.476906	28.373543
312.004297	11808.056506	28.378560
312.270558	11829.922515	28.383578
312.776016	11823.242703	28.388596
313.236350	11844.427710	28.393613
313.538776	11859.374646	28.398631
313.795010	11862.068048	28.403648
313.888006	11877.641809	28.408666
314.123319	11880.119751	28.413684
314.473493	11890.236121	28.418701
315.080988	11918.001059	28.423719
315.488696	11924.419413	28.428736
315.585589	11945.137919	28.433754
315.722669	11943.020628	28.438772
316.423055	11965.078551	28.443789
316.242567	11982.582160	28.448807
316.630150	11983.899358	28.453824
316.847592	12006.097666	28.458842
316.935850	12012.897922	28.463860
317.451821	12045.553839	28.468877
317.845136	12054.149554	28.473895
318.429423	12063.092623	28.478912
318.293398	12095.468870	28.483930
318.740167	12100.413221	28.488948
318.967940	12125.376155	28.493965
318.764479	12156.815274	28.498983
319.223187	12178.042329	28.504000
319.310943	12204.017824	28.509018
319.929284	12226.434331	28.514036
320.214089	12249.690301	28.519053
320.670514	12282.978982	28.524071
321.185229	12299.148870	28.529088
321.280815	12320.628992	28.534106
321.749116	12343.293702	28.539124
322.419831	12358.800286	28.544141
322.400269	12382.888098	28.549159
323.546141	12384.322179	28.554176
323.981241	12392.242028	28.559194
324.586980	12422.738515	28.564212
324.961619	12416.699900	28.569229
325.243158	12427.735062	28.574247
325.731555	12418.747466	28.579264
325.624712	12435.133438	28.584282
326.196107	12444.021531	28.589300
326.302446	12443.078068	28.594317
325.735472	12458.126374	28.599335
326.553216	12465.723186	28.604352
326.604953	12488.584762	28.609370
327.083894	12492.703201	28.614388
327.287454	12505.273834	28.619405
327.500665	12521.635653	28.624423
327.779624	12535.360738	28.629440
327.903421	12557.071839	28.634458
327.960986	12574.786712	28.639476
328.677981	12598.789558	28.644493
328.649483	12622.914201	28.649511
329.108078	12646.822532	28.654528
329.548372	12661.634363	28.659546
329.867376	12685.896561	28.664564
330.050072	12704.303954	28.669581
329.774072	12726.545555	28.674599
330.803547	12735.020995	28.679616
330.657174	12769.555369	28.684634
331.301698	12792.897704	28.689652
332.109074	12813.803463	28.694669
332.172918	12839.196099	28.699687
332.638239	12856.617473	28.704704
332.974328	12863.598608	28.709722
333.432328	12876.156155	28.714740
333.810306	12901.927012	28.719757
333.908128	12918.807849	28.724775
334.577651	12932.533627	28.729792
334.621954	12958.071647	28.734810
334.797671	12967.422954	28.739828
335.565657	12996.481117	28.744845
335.624577	13002.327807	28.749863
336.109903	13016.465941	28.754880
336.505235	13035.598811	28.759898
337.063774	13045.624115	28.764916
337.209870	13056.890297	28.769933
337.428213	13079.008571	28.774951
338.248747	13086.175107	28.779968
338.236379	13109.184593	28.784986
338.073561	13112.150440	28.790004
338.776466	13136.717791	28.795021
338.978580	13157.645906	28.800039
339.162858	13183.499471	28.805056
339.221068	13205.157015	28.810074
339.560101	13233.487044	28.815092
339.724943	13250.730856	28.820109
339.945318	13284.508998	28.825127
340.715405	13305.520952	28.830144
341.165063	13330.762408	28.835162
341.374032	13356.043246	28.840180
341.860292	13371.256766	28.845197
342.097148	13402.168219	28.850215
342.588579	13423.056497	28.855232
343.025885	13452.289057	28.860250
343.295731	13470.053399	28.865268
343.876100	13481.427204	28.870285
344.206964	13516.015323	28.875303
344.578389	13516.159076	28.880320
344.909016	13542.513958	28.885338
344.817566	13560.110470	28.890356
345.552003	13582.389275	28.895373
345.773118	13604.012768	28.900391
346.239393	13622.520325	28.905408
346.364271	13659.812138	28.910426
346.687414	13672.957788	28.915444
347.633200	13674.611241	28.920461
347.390502	13707.732280	28.925479
348.058532	13715.234540	28.930496
348.580420	13737.895753	28.935514
348.768064	13740.255465	28.940532
349.278095	13741.596606	28.945549
349.327341	13774.388684	28.950567
349.581865	13778.553871	28.955584
349.869886	13801.953791	28.960602
350.244176	13814.971965	28.965620
350.452384	13840.202369	28.970637
350.330474	13863.427236	28.975655
350.886696	13869.689338	28.980672
351.360977	13894.513278	28.985690
351.422631	13931.836003	28.990708
351.848797	13948.527121	28.995725
352.188438	13983.356264	29.000743
352.556622	14009.319578	29.005760
353.123109	14040.562847	29.010778
353.369262	14066.017426	29.015796
353.929370	14070.096312	29.020813
354.216765	14095.687533	29.025831
354.614036	14120.564555	29.030848
355.293068	14145.836443	29.035866
355.327098	14164.851007	29.040884
355.844369	14192.098348	29.045901
355.861854	14216.536594	29.050919
356.507997	14236.394953	29.055936
356.688239	14261.038982	29.060954
357.241228	14282.064654	29.065972
357.912205	14295.004574	29.070989
357.785558	14329.080222	29.076007
358.350144	14337.454635	29.081024
358.951148	14355.731936	29.086042
359.242230	14376.983673	29.091060
359.496510	14404.880409	29.096077
359.544290	14430.078415	29.101095
360.084541	14439.724997	29.106112
360.334159	14459.953244	29.111130
360.838879	14486.601416	29.116148
360.950748	14503.108944	29.121165
361.389168	14540.575324	29.126183
361.837701	14571.318942	29.131200
362.573988	14581.120347	29.136218
362.676650	14614.036191	29.141236
362.647297	14623.486140	29.146253
362.799307	14645.486293	29.151271
363.335792	14674.367894	29.156288
364.163639	14703.863275	29.161306
364.465400	14720.005437	29.166324
364.980595	14736.948222	29.171341
365.355866	14769.423134	29.176359
365.807341	14776.083505	29.181376
366.423619	14794.604701	29.186394
366.270623	14812.105403	29.191412
366.942685	14834.526468	29.196429
367.225617	14850.962735	29.201447
367.777243	14866.755475	29.206464
367.936459	14886.442737	29.211482
367.957986	14891.254159	29.216500
368.657931	14902.140812	29.221517
368.643644	14932.970521	29.226535
368.939941	14954.951671	29.231552
369.566742	14964.920834	29.236570
369.744895	14991.532285	29.241588
370.202330	15005.148510	29.246605
370.773715	15040.145155	29.251623
371.035921	15052.385108	29.256640
371.535469	15075.884028	29.261658
371.811782	15103.593044	29.266676
372.260588	15119.243907	29.271693
372.153177	15133.981203	29.276711
372.646044	15149.188962	29.281728
373.220590	15163.449400	29.286746
373.109038	15200.424666	29.291764
373.309523	15231.276840	29.296781
373.576430	15263.420153	29.301799
374.056128	15288.764476	29.306816
374.365847	15314.989666	29.311834
374.429107	15364.641118	29.316852
374.970014	15380.757877	29.321869
375.509615	15419.735336	29.326887
376.115693	15459.925356	29.331904
376.662598	15478.019266	29.336922
377.207824	15510.940910	29.341940
377.545028	15528.694854	29.346957
378.042644	15557.616990	29.351975
378.534060	15581.198501	29.356992
379.072104	15601.680662	29.362010
379.416631	15635.364615	29.367028
379.625465	15651.128066	29.372045
379.882182	15665.571383	29.377063
380.204189	15698.992191	29.382080
380.892522	15704.241400	29.387098
381.123012	15724.040699	29.392116
381.468927	15754.400967	29.397133
381.379164	15781.689424	29.402151
381.676344	15808.519402	29.407168
382.443840	15830.160540	29.412186
382.619321	15875.588037	29.417204
383.293498	15887.567482	29.422221
383.690953	15912.307758	29.427239
384.099495	15939.903042	29.432256
384.457193	15964.706124	29.437274
384.458844	15999.635837	29.442292
385.105006	16017.231885	29.447309
385.771614	16043.156618	29.452327
386.039193	16064.498683	29.457344
386.736432	16101.744314	29.462362
386.825087	16121.528347	29.467380
387.023973	16136.417367	29.472397
387.789321	16172.415432	29.477415
387.811908	16190.364050	29.482432
388.241106	16200.193398	29.487450
388.496093	16219.742527	29.492468
388.750798	16244.632146	29.497485
388.851508	16265.805642	29.502503
389.190975	16298.601064	29.507520
389.989236	16322.826540	29.512538
389.989847	16345.823471	29.517556
390.743192	16376.700761	29.522573
391.188454	16401.508507	29.527591
391.184859	16434.563870	29.532608
391.709802	16451.642320	29.537626
392.067917	16480.760841	29.542644
392.571889	16505.054164	29.547661
392.850715	16551.137951	29.552679
392.872955	16581.897144	29.557696
393.679166	16602.710104	29.562714
393.990550	16635.087258	29.567732
394.471628	16660.918896	29.572749
395.190951	16694.254057	29.577767
395.557518	16738.831724	29.582784
395.949346	16743.908004	29.587802
396.468765	16769.387111	29.592820
397.179495	16791.195131	29.597837
397.582408	16816.331708	29.602855
397.631115	16838.927079	29.607872
397.965855	16860.498297	29.612890
398.144114	16885.786910	29.617908
398.510492	16911.010554	29.622925
399.276457	16941.269924	29.627943
399.454491	16971.815135	29.632960
400.018010	17001.739997	29.637978
400.205923	17036.972558	29.642996
400.600269	17070.191044	29.648013
401.162930	17091.597938	29.653031
401.276966	17123.304693	29.658048
401.944185	17147.207511	29.663066
402.179530	17174.450664	29.668084
402.792415	17197.156840	29.673101
403.451373	17223.759812	29.678119
403.364575	17257.591726	29.683136
404.028997	17284.519882	29.688154
404.515644	17304.428122	29.693172
404.787125	17323.606182	29.698189
405.262400	17353.379271	29.703207
405.416864	17380.342791	29.708224
406.096018	17403.392615	29.713242
406.037096	17444.120615	29.718260
406.579150	17468.533987	29.723277
406.959077	17494.151076	29.728295
407.437807	17529.758661	29.733312
407.816251	17568.681628	29.738330
408.301349	17600.786499	29.743348
408.625153	17614.404100	29.748365
409.133185	17641.246981	29.753383
409.232152	17672.458681	29.758400
409.487720	17686.281099	29.763418
409.956513	17725.903790	29.768436
410.209844	17751.716858	29.773453
410.895065	17782.811357	29.778471
411.089230	17814.739816	29.783488
411.853738	17847.322887	29.788506
412.486166	17872.430720	29.793524
412.947355	17901.479403	29.798541
413.252966	17921.796199	29.803559
413.220244	17951.078188	29.808576
413.953410	17975.890038	29.813594
414.291834	18006.687903	29.818612
414.817810	18044.461068	29.823629
415.252582	18060.725604	29.828647
415.400936	18096.967813	29.833664
415.710768	18126.867763	29.838682
416.198545	18157.419702	29.843700
416.587933	18197.001924	29.848717
417.035484	18219.712330	29.853735
417.473108	18262.379023	29.858752
417.890828	18298.352809	29.863770
418.397569	18321.067318	29.868788
418.552572	18368.126019	29.873805
419.186308	18385.160350	29.878823
419.315021	18435.198934	29.883840
419.605620	18463.543197	29.888858
420.296984	18487.865891	29.893876
420.779560	18533.696556	29.898893
421.483727	18558.287000	29.903911
421.975957	18594.411802	29.908928
422.531197	18611.238028	29.913946
422.807602	18642.671042	29.918964
423.501996	18678.400845	29.923981
424.199183	18697.618687	29.928999
424.304803	18722.458299	29.934016
424.621166	18748.640343	29.939034
424.676850	18777.884017	29.944052
425.319451	18808.562966	29.949069
425.881488	18834.769399	29.954087
426.182305	18869.769833	29.959104
426.452113	18896.469779	29.964122
426.849445	18937.580577	29.969140
427.184450	18966.243488	29.974157
427.950190	19000.796914	29.979175
428.270264	19026.285524	29.984192
428.999993	19060.123948	29.989210
429.299633	19080.948929	29.994228
429.685574	19104.932669	29.999245
430.312452	19141.042804	30.004263
430.670285	19176.904544	30.009280
431.049138	19191.976405	30.014298
431.467393	19203.865957	30.019316
431.737704	19260.537126	30.024333
432.358937	19280.643800	30.029351
432.869579	19311.053028	30.034368
433.224709	19332.591966	30.039386
433.158462	19348.776654	30.044404
434.027594	19377.854845	30.049421
434.547997	19399.627395	30.054439
434.463318	19432.682184	30.059456
435.037700	19452.533938	30.064474
435.477597	19473.427654	30.069492
435.652177	19506.834615	30.074509
435.967007	19530.469698	30.079527
436.474416	19576.858168	30.084544
436.654450	19608.146670	30.089562
437.189952	19635.320144	30.094580
437.478547	19672.909493	30.099597
438.149460	19705.023570	30.104615
438.553908	19755.070893	30.109632
439.197213	19781.104156	30.114650
439.887157	19802.829392	30.119668
439.985960	19852.763904	30.124685
440.633528	19879.722300	30.129703
440.929836	19911.781913	30.134720
441.313441	19943.045741	30.139738
442.018178	19980.464406	30.144756
442.647349	20011.968009	30.149773
442.941799	20040.705900	30.154791
443.074707	20073.376171	30.159808
443.767448	20105.639184	30.164826
444.524343	20124.260265	30.169844
444.749108	20162.746072	30.174861
445.466571	20191.970830	30.179879
445.891348	20219.856329	30.184896
446.157201	20263.674083	30.189914
446.526542	20280.942408	30.194932
447.082254	20307.048781	30.199949
447.577034	20332.093941	30.204967
447.872960	20365.986998	30.209984
448.236650	20411.484619	30.215002
448.992208	20434.629951	30.220020
449.096242	20468.050996	30.225037
449.660594	20504.430581	30.230055
450.496207	20527.944439	30.235072
450.681120	20564.161757	30.240090
451.157299	20597.750191	30.245108
451.248852	20630.425064	30.250125
452.188881	20659.181729	30.255143
452.355998	20696.561766	30.260160
452.612462	20725.136476	30.265178
453.010123	20752.363390	30.270196
453.318516	20795.650991	30.275213
453.732235	20837.873377	30.280231
454.357435	20868.111075	30.285248
454.740965	20909.385194	30.290266
455.359447	20936.290991	30.295284
455.722554	20988.852719	30.300301
456.286929	21011.726177	30.305319
456.884104	21047.580468	30.310336
457.121605	21076.637251	30.315354
458.089735	21082.545337	30.320372
458.387411	21121.200649	30.325389
458.844824	21137.799892	30.330407
459.420847	21166.395374	30.335424
460.219210	21196.062735	30.340442
460.181612	21206.917622	30.345460
460.419592	21248.777323	30.350477
460.659652	21278.883444	30.355495
461.091773	21305.553385	30.360512
461.455436	21335.177253	30.365530
462.000052	21369.595942	30.370548
462.448175	21417.496013	30.375565
462.605659	21455.976420	30.380583
463.342711	21488.858957	30.385600
463.686623	21531.214430	30.390618
464.145548	21565.215632	30.395636
465.155093	21605.540527	30.400653
465.407050	21638.528223	30.405671
465.809158	21673.827913	30.410688
465.988136	21710.472912	30.415706
467.046902	21735.233193	30.420724
467.313310	21784.429702	30.425741
467.635058	21809.997406	30.430759
468.440544	21848.615744	30.435776
468.867826	21878.970012	30.440794
469.320758	21901.188776	30.445812
469.559226	21942.337511	30.450829
470.015580	21979.039755	30.455847
470.427638	22011.576660	30.460864
470.819655	22060.962725	30.465882
471.233670	22091.768427	30.470900
472.020058	22128.631871	30.475917
472.587952	22169.638151	30.480935
472.989533	22204.543759	30.485952
473.275720	22242.229044	30.490970
473.692781	22278.263298	30.495988
474.270205	22317.132552	30.501005
474.847441	22350.144740	30.506023
475.254957	22398.192091	30.511040
475.517692	22437.004662	30.516058
476.485972	22461.334741	30.521076
476.954665	22508.876509	30.526093
477.158935	22549.015507	30.531111
477.737949	22578.125410	30.536128
478.358294	22618.361332	30.541146
478.681082	22641.169726	30.546164
479.103569	22676.386509	30.551181
479.813560	22706.171226	30.556199
480.139066	22744.531927	30.561216
480.434398	22792.967734	30.566234
481.149263	22817.838072	30.571252
481.513407	22855.429706	30.576269
482.226026	22886.170491	30.581287
482.795408	22915.160473	30.586304
483.309892	22949.900102	30.591322
483.491368	22984.032054	30.596340
483.400769	23010.040719	30.601357
484.035843	23037.836688	30.606375
484.365189	23071.624717	30.611392
484.703087	23113.352949	30.616410
485.235796	23153.677446	30.621428
486.058802	23194.194449	30.626445
486.073752	23237.274022	30.631463
486.668033	23280.191326	30.636480
487.521795	23323.289520	30.641498
488.015565	23359.943335	30.646516
488.489415	23389.907948	30.651533
488.792712	23436.142253	30.656551
489.598109	23464.041012	30.661568
489.533727	23521.614577	30.666586
490.318660	23560.859471	30.671604
491.056418	23594.151932	30.676621
491.569572	23628.500233	30.681639
492.208480	23675.134665	30.686656
492.405630	23699.060996	30.691674
493.357056	23746.665852	30.696692
493.592446	23781.491149	30.701709
493.839732	23820.419847	30.706727
494.598859	23855.784119	30.711744
494.691560	23906.445276	30.716762
495.433043	23932.903404	30.721780
496.219921	23979.092190	30.726797
496.575658	24004.906935	30.731815
497.066096	24046.665313	30.736832
497.826664	24083.565012	30.741850
498.016012	24124.242839	30.746868
498.624275	24159.585350	30.751885
498.923582	24202.070879	30.756903
499.738380	24239.181273	30.761920
499.930991	24281.068052	30.766938
500.337952	24312.877188	30.771956
501.179178	24338.233120	30.776973
501.444491	24392.898067	30.781991
502.231941	24428.444999	30.787008
502.397554	24464.530591	30.792026
503.679028	24497.756460	30.797044
504.369622	24520.264794	30.802061
504.936748	24554.057490	30.807079
505.859283	24564.446662	30.812096
506.228839	24607.475039	30.817114
506.932894	24620.671707	30.822132
507.188208	24638.873945	30.827149
507.672953	24654.901082	30.832167
508.217438	24681.223279	30.837184
508.624570	24709.127027	30.842202
509.026282	24726.805862	30.847220
509.292443	24755.625391	30.852237
509.727206	24795.760932	30.857255
510.326741	24803.844141	30.862272
510.342084	24836.506768	30.867290
510.811477	24859.831429	30.872308
511.159006	24895.686583	30.877325
511.201450	24930.315912	30.882343
511.987107	24966.214077	30.887360
512.079573	25020.944949	30.892378
512.749765	25047.387153	30.897396
513.005559	25094.386900	30.902413
513.016385	25133.894485	30.907431
514.084015	25174.100315	30.912448
514.192644	25244.916882	30.917466
514.756078	25290.519629	30.922484
515.713016	25332.492232	30.927501
515.889573	25381.531467	30.932519
516.393581	25428.665960	30.937536
516.910242	25491.056901	30.942554
517.662093	25531.513231	30.947572
518.095297	25582.663499	30.952589
518.781759	25627.536289	30.957607
519.621094	25669.470221	30.962624
519.962505	25715.864203	30.967642
520.575508	25763.859868	30.972660
521.206947	25788.845062	30.977677
522.042877	25848.257709	30.982695
522.595815	25880.310621	30.987712
522.862897	25920.077098	30.992730
523.372417	25960.133551	30.997748
523.993085	25992.854156	31.002765
524.440672	26038.230925	31.007783
525.115575	26067.473763	31.012800
525.637333	26117.281900	31.017818
526.064851	26159.878265	31.022836
526.526774	26192.152694	31.027853
526.598646	26239.994138	31.032871
527.139246	26299.379089	31.037888
527.996178	26338.098662	31.042906
528.697766	26378.580113	31.047924
529.292113	26419.252060	31.052941
529.595403	26475.496001	31.057959
530.709671	26505.504703	31.062976
531.008435	26551.396630	31.067994
531.237574	26578.595424	31.073012
532.225177	26619.793716	31.078029
532.846825	26653.554607	31.083047
533.389934	26696.885536	31.088064
533.667946	26731.194482	31.093082
533.980057	26771.631037	31.098100
534.527733	26811.738689	31.103117
534.829301	26864.463611	31.108135
535.328573	26900.449560	31.113152
536.021816	26949.950151	31.118170
536.397104	26990.584386	31.123188
537.438381	27031.676715	31.128205
537.821085	27085.673563	31.133223
538.380809	27107.554099	31.138240
538.721434	27153.991759	31.143258
539.497716	27167.468963	31.148276
540.092185	27210.495306	31.153293
540.210879	27252.583625	31.158311
540.918821	27293.381503	31.163328
541.734653	27321.966056	31.168346
541.868306	27365.984023	31.173364
542.603276	27394.127799	31.178381
543.240180	27434.366178	31.183399
543.467963	27474.721819	31.188416
544.049432	27510.421091	31.193434
544.654075	27560.200810	31.198452
545.095717	27595.026777	31.203469
545.410222	27650.327642	31.208487
546.086241	27679.282536	31.213504
546.721062	27730.083739	31.218522
547.090364	27772.458877	31.223540
547.709743	27819.610387	31.228557
547.970853	27862.363038	31.233575
548.582523	27906.445005	31.238592
548.858263	27962.696169	31.243610
549.538108	28017.857379	31.248628
550.497419	28064.019491	31.253645
550.998303	28121.027930	31.258663
551.160551	28166.009439	31.263680
551.928849	28215.067070	31.268698
552.472499	28271.235668	31.273716
553.239447	28327.269625	31.278733
553.511809	28370.210917	31.283751
554.118768	28415.323984	31.288768
554.655295	28465.082679	31.293786
555.245591	28518.233446	31.298804
556.485090	28556.845442	31.303821
556.679606	28610.751309	31.308839
557.175427	28658.252707	31.313856
557.913698	28702.439595	31.318874
558.372062	28740.289282	31.323892
559.205079	28787.283531	31.328909
559.961584	28828.459691	31.333927
560.619239	28871.829442	31.338944
561.069380	28918.464317	31.343962
561.869025	28961.936183	31.348980
562.400827	28984.470588	31.353997
562.642188	29027.678569	31.359015
563.174887	29073.456109	31.364032
563.897103	29114.964653	31.369050
563.994838	29160.562737	31.374068
564.897709	29194.018643	31.379085
565.031380	29246.663050	31.384103
565.589890	29292.706565	31.389120
566.155530	29340.249271	31.394138
566.508625	29390.054207	31.399156
567.267481	29432.654516	31.404173
567.580189	29485.851094	31.409191
567.933880	29528.610734	31.414208
569.030444	29567.512661	31.419226
568.916803	29618.517795	31.424244
569.508750	29658.204719	31.429261
570.339031	29715.609127	31.434279
571.059771	29756.958812	31.439296
571.377932	29808.058084	31.444314
571.650735	29856.545618	31.449332
572.607709	29891.749888	31.454349
572.929418	29948.550606	31.459367
573.672157	29998.411966	31.464384
574.643660	30050.986999	31.469402
575.637132	30108.415659	31.474420
576.112785	30141.082694	31.479437
576.853923	30187.247795	31.484455
577.354368	30226.638649	31.489472
577.907231	30260.414108	31.494490
578.336545	30303.032939	31.499508
578.808975	30339.368073	31.504525
579.150190	30397.391749	31.509543
579.444351	30440.607682	31.514560
580.204207	30491.654513	31.519578
580.735912	30547.665845	31.524596
581.298290	30603.948276	31.529613
582.086470	30652.690202	31.534631
582.463796	30703.987736	31.539648
583.174221	30751.232562	31.544666
583.638218	30811.446094	31.549684
584.613379	30841.376306	31.554701
585.241962	30897.014084	31.559719
585.652460	30959.570718	31.564736
586.522682	30999.679939	31.569754
587.338218	31048.847364	31.574772
587.775855	31088.748321	31.579789
588.115155	31132.491586	31.584807
588.904155	31171.446342	31.589824
589.530352	31211.051221	31.594842
590.147306	31265.896219	31.599860
590.861678	31309.688971	31.604877
591.579503	31358.097485	31.609895
591.860414	31402.983938	31.614912
592.719862	31438.569582	31.619930
592.867843	31488.041648	31.624948
593.631881	31523.037470	31.629965
594.372496	31571.386248	31.634983
595.102375	31602.792708	31.640000
595.630649	31646.879202	31.645018
596.209040	31712.222089	31.650036
597.252075	31726.804865	31.655053
597.619604	31777.027720	31.660071
597.817838	31829.102785	31.665088
598.564465	31863.459071	31.670106
598.756485	31905.268789	31.675124
599.366578	31965.658735	31.680141
600.006384	32011.789974	31.685159
600.286251	32058.289156	31.690176
601.077720	32104.692810	31.695194
601.277082	32155.069690	31.700212
602.071682	32193.047228	31.705229
602.713245	32230.387257	31.710247
602.835716	32287.774739	31.715264
603.785899	32331.171740	31.720282
604.337046	32388.641038	31.725300
604.925265	32433.005379	31.730317
605.738706	32484.302082	31.735335
606.426141	32529.676950	31.740352
607.430261	32577.513891	31.745370
607.666677	32632.050514	31.750388
608.388057	32673.992243	31.755405
609.109363	32709.900547	31.760423
609.324504	32758.536681	31.765440
610.333904	32810.712644	31.770458
610.805847	32863.968930	31.775476
611.178447	32902.882211	31.780493
611.756954	32952.168755	31.785511
612.437217	33004.769728	31.790528
613.367298	33060.278569	31.795546
614.275161	33092.865333	31.800564
615.217765	33129.421807	31.805581
615.785533	33169.169972	31.810599
616.362109	33217.723108	31.815616
617.087208	33250.416524	31.820634
617.556575	33289.159263	31.825652
617.860472	33332.535734	31.830669
618.787530	33377.922071	31.835687
619.333545	33427.275108	31.840704
619.938884	33467.957444	31.845722
620.519445	33515.424797	31.850740
620.847735	33558.766453	31.855757
621.808789	33595.743460	31.860775
621.896438	33641.945134	31.865792
622.691000	33687.563065	31.870810
623.643066	33750.483856	31.875828
623.908953	33781.337874	31.880845
624.781923	33831.223270	31.885863
624.974708	33884.246727	31.890880
625.900819	33928.687393	31.895898
626.288738	33986.297019	31.900916
626.697213	34045.985848	31.905933
627.820104	34092.539371	31.910951
628.065182	34140.169130	31.915968
628.721636	34194.527378	31.920986
629.380737	34249.802794	31.926004
629.786059	34300.750845	31.931021
630.585102	34355.654388	31.936039
631.305661	34419.962344	31.941056
631.826982	34466.209175	31.946074
632.025759	34524.938458	31.951092
632.316970	34581.440049	31.956109
633.623013	34631.137518	31.961127
633.754896	34689.089862	31.966144
634.409952	34746.844023	31.971162
634.996018	34799.612311	31.976180
635.756823	34850.975200	31.981197
636.627252	34899.916829	31.986215
636.582785	34953.110741	31.991232
637.629891	35014.946118	31.996250
638.299729	35073.717403	32.001268
638.824003	35131.534714	32.006285
639.983729	35175.361417	32.011303
640.411314	35220.936393	32.016320
641.038381	35284.234771	32.021338
641.500811	35332.399267	32.026356
642.086406	35395.778764	32.031373
642.884712	35446.998800	32.036391
643.614654	35507.046830	32.041408
644.538150	35565.506741	32.046426
645.258247	35618.335108	32.051444
645.542280	35672.226237	32.056461
646.836697	35710.211108	32.061479
646.993404	35766.268357	32.066496
647.575006	35823.432597	32.071514
648.204544	35874.427013	32.076532
648.983618	35935.156100	32.081549
649.559474	35986.271335	32.086567
650.274442	36055.530322	32.091584
651.192832	36095.958010	32.096602
651.973485	36159.244715	32.101620
652.354019	36219.560622	32.106637
653.113843	36270.111425	32.111655
653.848464	36323.163575	32.116672
654.662905	36369.744232	32.121690
655.364684	36423.341096	32.126708
656.018782	36471.647049	32.131725
656.586716	36516.355051	32.136743
656.659557	36575.193584	32.141760
657.495288	36620.316416	32.146778
658.239216	36681.460558	32.151796
658.387453	36749.146259	32.156813
659.159173	36805.115367	32.161831
659.935715	36871.017763	32.166848
661.072914	36923.425968	32.171866
661.453091	36990.481349	32.176884
661.848869	37052.364934	32.181901
662.496457	37104.433874	32.186919
662.859882	37177.185686	32.191936
663.744495	37239.391000	32.196954
664.452842	37299.116249	32.201972
664.798373	37362.063718	32.206989
666.008601	37422.054767	32.212007
666.681477	37498.618232	32.217024
667.307954	37549.477922	32.222042
668.216828	37608.207452	32.227060
668.829130	37654.708777	32.232077
669.375858	37698.403230	32.237095
669.965147	37768.703086	32.242112
670.535649	37821.928012	32.247130
671.416003	37877.131341	32.252148
672.062188	37930.172705	32.257165
672.432505	37987.605010	32.262183
673.219290	38052.887633	32.267200
674.168346	38106.195085	32.272218
674.743374	38143.976830	32.277236
675.229870	38219.885823	32.282253
675.957188	38257.123270	32.287271
676.344650	38325.526146	32.292288
676.955355	38383.126493	32.297306
678.005428	38443.450995	32.302324
678.105314	38498.271354	32.307341
679.278637	38566.367184	32.312359
679.583898	38627.616635	32.317376
680.374505	38685.947773	32.322394
681.090667	38761.062650	32.327412
681.744818	38815.653883	32.332429
682.234557	38869.461024	32.337447
682.824911	38944.399654	32.342464
683.402335	39006.925307	32.347482
684.394409	39071.499606	32.352500
684.721445	39144.095407	32.357517
685.738098	39210.839111	32.362535
686.317439	39277.868724	32.367552
687.044638	39349.857705	32.372570
688.169068	39402.294598	32.377588
688.852326	39481.784048	32.382605
690.159903	39537.443559	32.387623
690.459066	39599.358176	32.392640
691.230000	39662.982861	32.397658
691.952115	39716.866074	32.402676
692.810459	39778.564593	32.407693
693.592766	39831.136128	32.412711
693.931454	39897.197334	32.417728
694.615513	39954.594248	32.422746
695.458992	40022.839918	32.427764
695.839056	40084.085875	32.432781
696.687586	40131.147730	32.437799
697.429973	40197.456470	32.442816
698.330317	40260.830993	32.447834
698.921031	40311.953841	32.452852
699.246661	40378.126221	32.457869
700.473100	40439.923073	32.462887
701.351273	40509.836677	32.467904
701.894772	40568.495905	32.472922
702.668909	40621.220993	32.477940
703.116684	40693.182888	32.482957
704.001592	40733.221793	32.487975
704.871855	40794.228261	32.492992
704.953017	40851.605921	32.498010
705.949071	40911.645051	32.503028
706.448423	40978.124834	32.508045
706.834426	41046.433252	32.513063
707.709894	41104.508466	32.518080
708.418284	41163.329568	32.523098
709.042037	41206.331683	32.528116
709.368363	41277.649901	32.533133
710.352813	41336.856585	32.538151
710.981188	41404.884996	32.543168
711.348838	41464.083085	32.548186
712.335638	41527.141045	32.553204
713.008629	41591.614874	32.558221
713.263421	41655.590960	32.563239
713.952950	41733.186482	32.568256
714.328837	41797.159588	32.573274
715.326290	41877.359275	32.578292
715.939616	41966.997497	32.583309
716.884317	42042.181945	32.588327
717.415226	42111.405147	32.593344
718.339283	42195.718317	32.598362
719.012017	42271.716669	32.603380
719.700737	42338.275671	32.608397
720.355887	42422.456135	32.613415
721.571940	42506.465706	32.618432
722.213498	42566.923507	32.623450
723.065125	42639.125778	32.628468
723.352252	42723.104507	32.633485
724.194714	42789.501997	32.638503
725.392602	42867.841812	32.643520
725.593596	42930.866019	32.648538
726.989034	43005.462481	32.653556
727.586978	43086.482131	32.658573
728.315935	43142.641402	32.663591
728.806522	43222.546399	32.668608
729.684292	43295.848110	32.673626
730.633618	43364.186471	32.678644
731.154269	43440.425536	32.683661
731.905294	43509.978917	32.688679
733.073725	43573.952324	32.693696
733.426304	43648.704978	32.698714
734.570433	43701.491050	32.703732
735.558446	43782.701068	32.708749
735.973485	43846.574617	32.713767
737.030477	43926.739689	32.718784
737.647459	43996.234353	32.723802
738.567057	44041.972372	32.728820
738.775456	44111.056222	32.733837
739.768058	44180.438205	32.738855
740.359105	44233.828132	32.743872
740.814026	44312.428432	32.748890
741.796500	44386.096642	32.753908
742.466454	44459.117770	32.758925
743.072479	44524.319856	32.763943
744.141247	44597.820658	32.768960
744.956360	44667.693412	32.773978
745.492954	44727.263827	32.778996
746.096581	44812.132912	32.784013
746.865752	44869.114739	32.789031
747.547138	44922.394614	32.794048
748.245993	44998.479678	32.799066
748.775390	45065.282763	32.804084
749.914067	45129.007986	32.809101
750.348465	45201.811058	32.814119
750.867390	45256.165161	32.819136
751.317535	45338.370328	32.824154
752.354680	45398.308170	32.829172
753.051852	45481.913224	32.834189
753.965395	45565.329656	32.839207
754.711065	45627.201205	32.844224
755.144957	45713.114371	32.849242
756.331515	45769.666758	32.854260
757.173366	45843.496039	32.859277
757.718164	45925.209382	32.864295
758.314301	45991.961231	32.869312
758.838581	46083.830694	32.874330
759.971723	46151.157022	32.879348
760.543654	46226.270733	32.884365
761.375689	46305.163879	32.889383
762.364677	46385.228088	32.894400
763.295394	46473.526698	32.899418
763.996837	46533.512422	32.904436
765.163370	46613.142434	32.909453
765.649461	46682.851652	32.914471
766.021782	46757.412605	32.919488
766.540760	46830.268947	32.924506
767.856734	46910.173086	32.929524
768.438360	47003.915449	32.934541
769.195102	47079.943586	32.939559
770.140647	47153.247630	32.944576
770.429779	47236.844003	32.949594
771.603179	47316.018642	32.954612
772.408390	47398.713328	32.959629
772.975460	47487.444074	32.964647
773.806045	47550.186017	32.969664
774.404791	47645.137468	32.974682
775.204007	47725.856409	32.979700
775.885865	47811.926546	32.984717
776.656466	47901.523035	32.989735
777.948842	47980.388305	32.994752
778.545248	48066.599495	32.999770
779.544087	48141.808055	33.004788
780.375075	48227.414760	33.009805
780.701891	48313.092668	33.014823
781.816014	48375.047794	33.019840
782.391571	48464.542518	33.024858
783.459844	48538.085221	33.029876
784.474898	48628.211282	33.034893
785.349015	48701.501598	33.039911
786.263603	48763.994698	33.044928
786.917979	48846.215344	33.049946
787.542513	48923.143350	33.054964
788.422174	48997.923322	33.059981
789.152895	49070.446007	33.064999
789.940057	49132.616762	33.070016
790.593697	49201.198598	33.075034
791.568176	49261.718134	33.080052
791.994075	49335.315920	33.085069
792.641498	49404.710469	33.090087
793.881084	49476.336572	33.095104
794.268578	49544.065961	33.100122
794.842168	49615.688195	33.105140
795.858770	49685.132364	33.110157
796.487133	49777.275897	33.115175
797.419602	49851.000297	33.120192
797.626844	49936.802911	33.125210
798.285011	50022.000884	33.130228
799.063166	50108.997748	33.135245
799.518785	50200.448355	33.140263
800.708966	50287.891710	33.145280
801.555106	50387.731701	33.150298
802.202821	50470.317514	33.155316
803.307356	50569.274852	33.160333
803.874038	50655.127849	33.165351
804.924543	50744.788839	33.170368
805.697066	50832.992434	33.175386
806.686616	50918.918243	33.180404
807.283772	51009.145004	33.185421
808.077514	51100.956649	33.190439
809.229529	51195.832744	33.195456
809.953135	51285.491680	33.200474
810.491239	51377.724123	33.205492
811.628097	51454.934980	33.210509
812.659766	51541.197902	33.215527
813.419541	51624.146752	33.220544
814.197661	51733.529277	33.225562
814.827591	51806.199073	33.230580
815.955417	51900.852385	33.235597
816.321472	51995.018361	33.240615
817.298727	52082.453906	33.245632
817.728308	52175.266315	33.250650
818.832966	52271.790402	33.255668
820.162916	52357.255517	33.260685
820.693497	52443.706682	33.265703
822.015149	52535.612077	33.270720
822.445215	52625.251845	33.275738
823.163761	52715.306917	33.280756
824.364562	52794.406960	33.285773
824.712201	52885.708573	33.290791
825.688961	52973.997504	33.295808
826.829721	53070.160345	33.300826
827.353930	53160.150735	33.305844
828.085057	53229.957101	33.310861
828.955041	53344.498141	33.315879
830.090357	53423.074833	33.320896
830.927770	53509.343407	33.325914
831.890502	53591.849270	33.330932
832.709248	53673.141214	33.335949
833.378136	53758.418363	33.340967
834.304338	53837.140606	33.345984
835.079400	53903.300353	33.351002
835.613217	53989.884660	33.356020
836.525536	54063.784261	33.361037
837.334187	54151.793242	33.366055
838.226692	54226.154314	33.371072
838.771968	54315.118161	33.376090
839.574406	54397.773149	33.381108
840.854653	54478.771169	33.386125
841.416121	54570.337631	33.391143
843.026407	54633.248688	33.396160
844.225217	54678.682587	33.401178
845.288149	54764.839190	33.406196
846.093182	54836.230790	33.411213
846.667471	54908.410608	33.416231
847.452308	54967.275171	33.421248
848.123608	55040.393299	33.426266
848.942375	55106.414759	33.431284
849.748851	55182.437929	33.436301
850.341444	55273.750468	33.441319
851.299177	55353.585341	33.446336
851.938988	55439.316919	33.451354
852.584937	55535.476909	33.456372
853.487968	55608.235322	33.461389
854.052844	55704.592182	33.466407
854.514476	55793.434528	33.471424
855.549629	55893.464329	33.476442
856.289677	55986.994954	33.481460
857.655733	56081.240827	33.486477
857.649292	56188.357206	33.491495
858.814897	56296.026331	33.496512
860.027360	56379.562575	33.501530
860.731906	56483.780237	33.506548
861.330607	56584.416749	33.511565
862.015722	56685.418861	33.516583
862.785778	56784.706557	33.521600
863.877466	56892.880241	33.526618
865.293520	56994.714746	33.531636
866.430446	57082.461507	33.536653
867.371038	57187.845165	33.541671
867.909048	57281.247240	33.546688
868.697432	57373.782865	33.551706
869.608414	57479.059260	33.556724
870.566575	57577.588926	33.561741
871.555721	57676.032112	33.566759
872.512043	57773.672891	33.571776
873.112260	57847.448073	33.576794
873.847636	57944.528270	33.581812
875.257589	58047.152486	33.586829
876.086466	58156.082571	33.591847
876.784199	58257.208109	33.596864
878.351867	58336.071812	33.601882
879.173010	58429.627222	33.606900
880.180691	58505.026014	33.611917
881.036379	58599.277636	33.616935
881.280803	58672.159318	33.621952
882.379014	58758.992068	33.626970
882.803799	58850.203868	33.631988
883.945649	58922.107106	33.637005
884.891911	59010.480603	33.642023
885.232282	59098.909896	33.647040
886.267379	59174.152356	33.652058
886.883816	59262.914194	33.657076
887.902549	59349.408763	33.662093
888.643487	59459.162420	33.667111
889.499203	59550.997347	33.672128
890.354487	59653.361984	33.677146
890.858455	59744.253014	33.682164
891.897708	59839.782493	33.687181
892.810519	59949.956862	33.692199
893.672728	60059.745280	33.697216
894.737388	60165.523973	33.702234
895.612616	60264.238998	33.707252
896.554400	60376.801343	33.712269
897.457057	60478.986170	33.717287
898.324729	60573.151180	33.722304
899.339665	60676.026462	33.727322
900.109221	60785.691814	33.732340
901.040268	60901.012254	33.737357
902.211385	60992.339958	33.742375
902.813500	61096.148373	33.747392
903.910195	61202.224640	33.752410
904.748710	61310.423355	33.757428
905.619302	61413.808756	33.762445
906.491887	61522.817905	33.767463
907.337827	61629.043843	33.772480
908.201148	61737.926258	33.777498
909.047096	61850.326420	33.782516
910.269176	61949.648755	33.787533
911.299583	62063.770133	33.792551
912.059421	62177.180591	33.797568
913.365666	62287.154549	33.802586
913.914446	62399.100055	33.807604
914.724818	62498.250819	33.812621
915.533281	62620.652376	33.817639
916.576234	62726.935264	33.822656
917.645523	62830.944165	33.827674
918.288359	62945.328331	33.832692
919.693143	63066.437955	33.837709
920.422200	63167.986121	33.842727
921.381411	63274.796976	33.847744
922.147946	63375.077175	33.852762
923.325951	63488.346868	33.857780
924.187545	63587.690984	33.862797
925.021563	63710.326051	33.867815
926.025141	63809.790843	33.872832
927.119406	63913.088041	33.877850
927.557691	64031.591311	33.882868
928.960511	64141.039638	33.887885
929.602610	64246.153773	33.892903
930.408937	64362.699461	33.897920
931.299213	64456.902391	33.902938
932.480603	64560.246089	33.907956
933.191681	64666.955837	33.912973
934.062112	64767.820567	33.917991
934.922778	64873.007600	33.923008
936.061878	64957.838218	33.928026
937.061970	65067.659132	33.933044
937.770190	65168.254930	33.938061
938.783957	65270.947005	33.943079
939.096047	65387.062819	33.948096
940.635495	65492.622145	33.953114
941.332933	65605.270322	33.958132
942.479696	65718.671959	33.963149
943.594445	65819.534954	33.968167
944.444301	65935.653803	33.973184
945.381687	66032.652045	33.978202
946.223006	66156.792374	33.983220
947.110550	66270.734369	33.988237
948.111756	66372.224728	33.993255
949.144833	66488.352511	33.998272
950.313507	66592.726202	34.003290
951.401594	66706.338833	34.008308
952.246137	66815.790248	34.013325
953.290932	66926.555899	34.018343
954.322674	67042.924122	34.023360
955.430318	67139.297608	34.028378
955.882447	67252.420859	34.033396
956.826962	67371.448561	34.038413
957.994652	67474.958615	34.043431
958.737680	67603.201506	34.048448
960.017151	67708.245850	34.053466
960.614419	67835.900722	34.058484
961.673903	67943.028076	34.063501
963.125952	68058.065807	34.068519
963.670561	68176.085014	34.073536
964.842728	68278.464723	34.078554
966.046874	68399.033588	34.083572
966.818477	68505.034842	34.088589
968.081380	68619.272116	34.093607
968.533584	68723.107992	34.098624
969.624489	68839.490245	34.103642
970.732134	68958.902904	34.108660
971.827896	69071.040449	34.113677
972.962126	69181.049836	34.118695
973.376125	69305.786929	34.123712
974.533110	69414.656855	34.128730
975.704689	69531.043044	34.133748
976.218874	69654.534489	34.138765
977.261534	69762.685380	34.143783
978.005962	69887.146179	34.148800
978.982036	69995.643793	34.153818
980.116287	70126.703038	34.158836
980.957939	70248.869938	34.163853
982.063793	70370.540679	34.168871
982.506993	70497.978471	34.173888
984.094571	70593.146034	34.178906
985.049293	70688.414741	34.183924
985.660147	70803.709925	34.188941
986.972849	70923.007195	34.193959
988.002066	71038.711057	34.198976
988.956643	71139.800961	34.203994
989.657282	71260.385465	34.209012
990.783203	71372.752543	34.214029
991.700532	71478.481369	34.219047
992.403383	71605.613346	34.224064
993.918057	71715.178393	34.229082
994.717649	71833.968894	34.234100
995.355171	71970.641716	34.239117
996.496399	72081.493981	34.244135
997.457787	72196.431944	34.249152
998.835588	72309.231856	34.254170
999.831605	72434.054177	34.259188
1001.000940	72552.366832	34.264205
1002.472126	72660.724558	34.269223
1003.340445	72776.672723	34.274240
1004.383369	72888.486631	34.279258
1005.768755	73009.042377	34.284276
1006.457350	73112.857523	34.289293
1007.338308	73212.168893	34.294311
1007.968563	73332.808820	34.299328
1009.269154	73457.247911	34.304346
1010.207471	73581.998169	34.309364
1011.471172	73695.721409	34.314381
1012.550575	73799.888702	34.319399
1012.873516	73927.677349	34.324416
1014.337489	74048.416468	34.329434
1015.212333	74164.485427	34.334452
1015.947212	74295.149280	34.339469
1017.137047	74418.436630	34.344487
1018.233795	74543.306717	34.349504
1018.830049	74680.377558	34.354522
1019.939857	74802.763713	34.359540
1020.841410	74930.270820	34.364557
1021.966568	75059.670581	34.369575
1022.911631	75204.595077	34.374592
1023.884685	75326.254168	34.379610
1025.126841	75456.794342	34.384628
1025.854727	75593.831522	34.389645
1027.312044	75719.340405	34.394663
1028.082518	75848.036993	34.399680
1029.051232	75972.632996	34.404698
1029.986358	76118.507287	34.409716
1031.359337	76244.115013	34.414733
1032.793584	76365.795500	34.419751
1033.373469	76501.863865	34.424768
1034.762352	76633.677572	34.429786
1035.815863	76753.942109	34.434804
1036.837689	76871.614899	34.439821
1038.787802	76968.524900	34.444839
1039.637699	77070.205031	34.449856
1040.639692	77185.879356	34.454874
1041.499372	77292.507650	34.459892
1042.311701	77391.262845	34.464909
1043.622925	77489.048023	34.469927
1044.380088	77623.262872	34.474944
1045.520429	77710.243492	34.479962
1046.368561	77827.633447	34.484980
1046.908851	77941.084942	34.489997
1047.985198	78075.062392	34.495015
1048.769325	78183.281137	34.500032
1049.649644	78289.595357	34.505050
1050.797449	78427.071575	34.510068
1051.599805	78569.432517	34.515085
1052.742637	78698.422944	34.520103
1053.852480	78826.793697	34.525120
1054.728232	78974.037897	34.530138
1055.915969	79098.005139	34.535156
1056.541532	79236.043912	34.540173
1057.748184	79369.655164	34.545191
1058.479122	79533.252869	34.550208
1059.997135	79637.159254	34.555226
1060.952737	79811.039005	34.560244
1061.879085	79926.772498	34.565261
1063.405834	80090.974964	34.570279
1064.445880	80222.766224	34.575296
1065.737320	80349.657468	34.580314
1066.712541	80515.493375	34.585332
1067.908670	80619.519134	34.590349
1068.935818	80783.262964	34.595367
1070.298629	80895.316767	34.600384
1071.069863	81049.849180	34.605402
1072.639780	81167.345717	34.610420
1073.663319	81303.280617	34.615437
1074.954477	81444.332078	34.620455
1075.552910	81569.305556	34.625472
1076.550806	81723.756370	34.630490
1077.928566	81836.754788	34.635508
1078.840959	81981.245814	34.640525
1079.930513	82135.173062	34.645543
1080.927082	82250.939996	34.650560
1082.072796	82393.285355	34.655578
1083.075513	82544.839857	34.660596
1084.278420	82677.126557	34.665613
1085.107683	82810.567191	34.670631
1086.693265	82960.179724	34.675648
1087.569874	83107.124466	34.680666
1088.796924	83217.720427	34.685684
1089.374932	83399.687510	34.690701
1090.924463	83516.941361	34.695719
1091.760618	83653.597846	34.700736
1092.653017	83799.527084	34.705754
1093.815210	83931.897734	34.710772
1095.005244	84098.056750	34.715789
1096.196571	84205.464586	34.720807
1097.134224	84352.041648	34.725824
1098.480632	84470.907373	34.730842
1099.677265	84595.645733	34.735860
1100.813013	84736.693551	34.740877
1101.892892	84851.247707	34.745895
1102.485094	84996.379459	34.750912
1104.027431	85112.435769	34.755930
1104.791509	85232.460577	34.760948
1105.706179	85384.941043	34.765965
1106.819226	85509.830869	34.770983
1108.068255	85652.270393	34.776000
1109.216316	85782.195395	34.781018
1110.132714	85916.052826	34.786036
1111.074067	86051.019935	34.791053
1111.934149	86209.085348	34.796071
1113.465415	86339.009718	34.801088
1114.669904	86487.278936	34.806106
1115.623258	86634.381447	34.811124
1116.481462	86798.433019	34.816141
1117.996734	86924.885873	34.821159
1118.997048	87075.613365	34.826176
1119.786047	87243.264530	34.831194
1121.321913	87372.549511	34.836212
1122.338219	87520.090728	34.841229
1123.520194	87661.226478	34.846247
1124.637377	87838.782873	34.851264
1125.576229	87978.953976	34.856282
1126.861543	88126.013948	34.861300
1128.116498	88275.855731	34.866317
1129.265761	88448.113043	34.871335
1130.385996	88572.950086	34.876352
1131.432024	88734.261167	34.881370
1133.085520	88891.240046	34.886388
1134.223891	89049.807011	34.891405
1135.185416	89177.980057	34.896423
1136.235813	89330.884419	34.901440
1137.434458	89491.449656	34.906458
1138.518075	89640.999331	34.911476
1139.510953	89793.998319	34.916493
1140.831230	89938.352148	34.921511
1142.127912	90102.416081	34.926528
1143.002545	90254.235567	34.931546
1144.276183	90394.565143	34.936564
1145.758366	90558.710530	34.941581
1147.073067	90681.347000	34.946599
1148.001044	90833.946235	34.951616
1149.247259	90959.687673	34.956634
1150.560735	91139.839174	34.961652
1151.493073	91293.288373	34.966669
1152.517358	91424.816558	34.971687
1153.938315	91585.507351	34.976704
1154.981414	91726.248965	34.981722
1156.270738	91883.781699	34.986740
1157.619440	92016.242138	34.991757
1158.634996	92159.223456	34.996775
1159.640865	92282.297487	35.001792
1160.589043	92427.922288	35.006810
1162.153828	92545.071297	35.011828
1162.822938	92684.765384	35.016845
1164.128793	92830.974768	35.021863
1165.580992	92964.309922	35.026880
1166.311651	93101.606100	35.031898
1167.266516	93248.304148	35.036916
1168.724261	93401.716138	35.041933
1169.492479	93526.624847	35.046951
1170.575986	93695.328810	35.051968
1172.125850	93810.564119	35.056986
1173.281730	93969.132323	35.062004
1174.650654	94089.780477	35.067021
1175.603456	94256.390586	35.072039
1177.108209	94393.109939	35.077056
1177.921897	94532.628235	35.082074
1178.877738	94705.180595	35.087092
1180.173525	94845.901897	35.092109
1181.063225	94983.367854	35.097127
1182.204571	95173.978498	35.102144
1183.323554	95316.919469	35.107162
1184.459448	95481.219805	35.112180
1185.658631	95653.462473	35.117197
1186.901123	95808.924150	35.122215
1188.339877	95974.173059	35.127232
1189.466042	96137.220951	35.132250
1190.975443	96297.444754	35.137268
1192.131314	96456.928867	35.142285
1193.258907	96616.013754	35.147303
1194.550974	96764.465174	35.152320
1195.746369	96935.187411	35.157338
1197.051618	97084.100628	35.162356
1198.286533	97234.537919	35.167373
1199.231540	97400.280660	35.172391
1200.534940	97559.470761	35.177408
1201.711218	97733.295509	35.182426
1203.056672	97896.175739	35.187444
1204.217933	98049.527534	35.192461
1205.387906	98229.253102	35.197479
1206.526355	98372.703798	35.202496
1208.062248	98528.966292	35.207514
1209.074223	98689.165924	35.212532
1210.213475	98859.886266	35.217549
1211.423405	99030.463792	35.222567
1213.205945	99180.263840	35.227584
1214.191975	99343.376057	35.232602
1215.478301	99499.634265	35.237620
1216.841021	99655.754861	35.242637
1217.750284	99828.910474	35.247655
1218.911047	99981.383260	35.252672
1220.103231	100145.607218	35.257690
1221.580840	100308.230569	35.262708
1222.817457	100468.223447	35.267725
1223.840976	100623.493480	35.272743
1225.513643	100774.378003	35.277760
1226.184472	100921.316577	35.282778
1227.195697	101068.676493	35.287796
1228.495189	101219.420791	35.292813
1229.473947	101375.822889	35.297831
1230.957484	101521.604745	35.302848
1231.804309	101668.988292	35.307866
1233.211241	101836.916855	35.312884
1234.153815	101993.183342	35.317901
1235.135730	102159.093801	35.322919
1236.794425	102320.259880	35.327936
1238.295567	102480.306861	35.332954
1239.254483	102648.970565	35.337972
1240.867843	102800.396557	35.342989
1242.038310	102947.787368	35.348007
1243.026279	103128.738010	35.353024
1244.368547	103296.541838	35.358042
1246.056334	103454.009456	35.363060
1246.942165	103624.691361	35.368077
1247.832473	103790.457117	35.373095
1249.422941	103955.720407	35.378112
1250.896735	104123.439634	35.383130
1251.823174	104296.954846	35.388148
1253.403600	104453.402129	35.393165
1254.599717	104617.764585	35.398183
1256.210267	104773.759918	35.403200
1257.329721	104938.079839	35.408218
1258.710163	105105.795582	35.413236
1259.555323	105290.639372	35.418253
1261.098469	105451.168205	35.423271
1262.522184	105613.982629	35.428288
1263.711549	105787.479630	35.433306
1264.931477	105949.316220	35.438324
1265.936879	106131.362933	35.443341
1267.272929	106300.328209	35.448359
1268.520390	106468.119011	35.453376
1269.496472	106661.863148	35.458394
1270.838192	106837.140875	35.463412
1272.253027	106990.707404	35.468429
1273.479044	107181.175759	35.473447
1275.091356	107342.307560	35.478464
1276.431243	107527.260909	35.483482
1277.642038	107709.938844	35.488500
1278.975740	107869.675506	35.493517
1280.127647	108043.289758	35.498535
1281.758955	108213.500027	35.503552
1282.954444	108389.768003	35.508570
1284.207835	108564.907822	35.513588
1285.694530	108727.341003	35.518605
1286.820023	108899.022580	35.523623
1288.323167	109067.506073	35.528640
1289.680193	109240.944422	35.533658
1290.756450	109406.263900	35.538676
1292.147986	109567.040584	35.543693
1293.478647	109734.106714	35.548711
1294.787588	109882.151320	35.553728
1295.849918	110035.862882	35.558746
1297.100369	110202.058853	35.563764
1298.506462	110350.787103	35.568781
1299.717533	110514.839432	35.573799
1300.882429	110661.044447	35.578816
1302.065012	110808.918542	35.583834
1303.180718	110980.204916	35.588852
1304.325548	111155.007175	35.593869
1305.499853	111316.095749	35.598887
1307.184498	111478.389206	35.603904
1308.166094	111648.821718	35.608922
1309.452314	111822.257989	35.613940
1311.149780	111983.147503	35.618957
1311.761366	112194.647863	35.623975
1313.058197	112348.975960	35.628992
1315.005158	112525.344221	35.634010
1315.904132	112729.511241	35.639028
1317.650010	112880.903737	35.644045
1318.660323	113093.949921	35.649063
1320.334666	113249.242781	35.654080
1321.547169	113425.696205	35.659098
1322.272550	113622.004276	35.664116
1323.850747	113798.085692	35.669133
1325.019709	113980.557496	35.674151
1326.225618	114172.026698	35.679168
1327.793120	114376.765651	35.684186
1329.182974	114553.122882	35.689204
1330.785844	114740.215880	35.694221
1332.244581	114935.993538	35.699239
1333.842862	115113.397791	35.704256
1335.268148	115297.427444	35.709274
1336.473779	115467.825145	35.714292
1338.117425	115651.442828	35.719309
1339.233623	115843.546780	35.724327
1340.322436	116030.135959	35.729344
1341.795493	116206.871400	35.734362
1343.027598	116405.937946	35.739380
1344.399760	116575.962103	35.744397
1345.785664	116775.925111	35.749415
1347.023279	116959.901711	35.754432
1348.362240	117146.269396	35.759450
1349.236151	117338.701737	35.764468
1351.348648	117524.411084	35.769485
1352.431377	117728.437470	35.774503
1353.621872	117925.749715	35.779520
1355.573855	118106.024788	35.784538
1356.711197	118292.958384	35.789556
1358.065792	118481.796267	35.794573
1359.194965	118671.861703	35.799591
1360.662432	118862.374975	35.804608
1362.155880	119056.868162	35.809626
1363.166233	119243.233658	35.814644
1364.907402	119443.642221	35.819661
1366.045705	119635.448209	35.824679
1367.152232	119813.533152	35.829696
1368.729820	119981.540019	35.834714
1369.986632	120159.698431	35.839732
1371.001466	120344.950376	35.844749
1372.383888	120528.391240	35.849767
1373.467073	120721.512072	35.854784
1374.823109	120908.461454	35.859802
1375.632484	121119.156119	35.864820
1377.240025	121303.839424	35.869837
1378.516673	121506.547647	35.874855
1379.521931	121697.142482	35.879872
1381.427382	121913.900356	35.884890
1382.796601	122111.963232	35.889908
1384.385940	122341.085117	35.894925
1385.571689	122530.618774	35.899943
1386.848677	122759.565959	35.904960
1388.505722	122954.271138	35.909978
1389.321976	123159.648953	35.914996
1390.827913	123378.483471	35.920013
1392.364712	123601.342540	35.925031
1393.432071	123823.682793	35.930048
1395.325291	124033.937153	35.935066
1396.188564	124256.047461	35.940084
1397.408219	124481.054155	35.945101
1399.033710	124710.178061	35.950119
1400.720832	124927.045907	35.955136
1402.411657	125147.626148	35.960154
1403.171555	125384.695815	35.965172
1405.073270	125599.647691	35.970189
1406.618705	125830.757184	35.975207
1407.684289	126057.232882	35.980224
1409.074839	126279.782781	35.985242
1410.580309	126522.621366	35.990260
1412.060872	126735.749159	35.995277
1413.641174	126955.031680	36.000295
1415.273147	127190.775196	36.005312
1416.709419	127422.194274	36.010330
1418.263963	127639.738301	36.015348
1419.842924	127859.940370	36.020365
1421.272051	128096.699343	36.025383
1422.552022	128311.214090	36.030400
1424.144553	128519.612931	36.035418
1425.755067	128748.469280	36.040436
1427.371284	128966.862786	36.045453
1429.111542	129166.375391	36.050471
1430.219345	129381.217198	36.055488
1431.949922	129602.891314	36.060506
1433.100455	129827.953177	36.065524
1434.889991	130035.280669	36.070541
1436.269094	130244.714582	36.075559
1437.684033	130455.601285	36.080576
1439.220102	130671.221158	36.085594
1440.648445	130883.527880	36.090612
1441.785833	131092.107068	36.095629
1443.201903	131308.194339	36.100647
1444.416523	131517.448555	36.105664
1445.921354	131707.464177	36.110682
1447.275078	131912.822420	36.115700
1448.640391	132125.414612	36.120717
1449.957738	132312.866860	36.125735
1451.052077	132531.700605	36.130752
1453.057994	132740.420070	36.135770
1454.506581	132949.559049	36.140788
1455.663920	133152.892317	36.145805
1457.304857	133364.183024	36.150823
1458.451927	133572.588954	36.155840
1460.196104	133784.816642	36.160858
1461.115072	134005.691505	36.165876
1462.683058	134232.255349	36.170893
1464.104322	134439.623073	36.175911
1465.617342	134671.495413	36.180928
1466.910464	134891.608099	36.185946
1468.184576	135128.159576	36.190964
1469.837078	135348.205981	36.195981
1471.540081	135582.817744	36.200999
1472.984742	135815.597129	36.206016
1474.249880	136047.887386	36.211034
1475.385690	136286.003532	36.216052
1477.096618	136521.736718	36.221069
1479.049106	136756.331010	36.226087
1480.442241	136994.234664	36.231104
1481.783859	137222.885381	36.236122
1483.062808	137464.131003	36.241140
1484.647973	137694.850240	36.246157
1486.051936	137948.042319	36.251175
1487.334868	138200.051948	36.256192
1489.173912	138432.726173	36.261210
1490.448461	138677.049135	36.266228
1492.172020	138926.194361	36.271245
1493.756702	139167.126558	36.276263
1494.848448	139432.660712	36.281280
1496.700248	139669.727389	36.286298
1498.239510	139915.146367	36.291316
1499.821466	140156.619273	36.296333
1501.361422	140404.145881	36.301351
1502.624924	140654.265775	36.306368
1504.130312	140899.089891	36.311386
1505.689327	141151.283422	36.316404
1507.423110	141408.203878	36.321421
1509.104503	141651.612061	36.326439
1510.425053	141902.164158	36.331456
1512.235274	142144.985526	36.336474
1513.522440	142384.837511	36.341492
1515.120426	142636.416208	36.346509
1516.764481	142876.468852	36.351527
1517.840045	143141.467929	36.356544
1520.029012	143376.913228	36.361562
1521.337160	143632.817440	36.366580
1522.788536	143871.248144	36.371597
1524.446017	144104.134476	36.376615
1526.308524	144338.080029	36.381632
1527.364640	144555.234532	36.386650
1528.996006	144783.174275	36.391668
1530.717496	145008.439622	36.396685
1532.243035	145227.007244	36.401703
1533.580657	145455.201395	36.406720
1535.050026	145675.897858	36.411738
1536.550124	145917.606817	36.416756
1537.477764	146154.198955	36.421773
1539.312209	146378.923903	36.426791
1540.764188	146624.220483	36.431808
1542.059229	146868.745334	36.436826
1543.684883	147110.608332	36.441844
1545.174204	147350.846967	36.446861
1546.699158	147600.956435	36.451879
1548.139750	147860.550392	36.456896
1549.667625	148097.619525	36.461914
1551.332446	148354.050858	36.466932
1552.901609	148609.193774	36.471949
1554.559646	148853.042454	36.476967
1556.292195	149113.563672	36.481984
1558.012246	149361.450241	36.487002
1559.222755	149616.594780	36.492020
1561.148983	149873.212275	36.497037
1562.791686	150116.920875	36.502055
1564.283266	150375.804548	36.507072
1565.922364	150630.622807	36.512090
1567.254770	150880.953285	36.517108
1568.539634	151135.159873	36.522125
1570.426171	151408.758314	36.527143
1571.818378	151664.638100	36.532160
1573.743745	151925.354180	36.537178
1575.339823	152181.091521	36.542196
1577.019594	152440.227938	36.547213
1578.965524	152690.373396	36.552231
1580.094730	152961.189131	36.557248
1581.860985	153214.612718	36.562266
1583.777442	153479.779923	36.567284
1584.914966	153728.768449	36.572301
1586.619051	153994.670815	36.577319
1588.214155	154249.055018	36.582336
1589.761755	154514.694776	36.587354
1591.586810	154766.662786	36.592372
1593.247406	155036.612231	36.597389
1595.046047	155282.185428	36.602407
1596.270006	155549.178041	36.607424
1598.072123	155801.334955	36.612442
1600.001810	156061.740427	36.617460
1601.134449	156324.582156	36.622477
1602.974287	156577.360147	36.627495
1604.367280	156843.194942	36.632512
1605.794403	157093.303508	36.637530
1607.392951	157352.173800	36.642548
1609.311224	157618.945583	36.647565
1610.981249	157870.656954	36.652583
1612.334562	158116.156491	36.657600
1614.057567	158355.246275	36.662618
1615.751546	158587.507648	36.667636
1617.114763	158849.089427	36.672653
1618.911208	159081.185669	36.677671
1620.747210	159316.016179	36.682688
1621.900144	159558.349572	36.687706
1623.733197	159802.060274	36.692724
1625.128604	160059.042917	36.697741
1627.018753	160293.833355	36.702759
1628.138460	160541.961322	36.707776
1629.663891	160798.599014	36.712794
1631.642052	161051.463766	36.717812
1633.166990	161309.538220	36.722829
1634.840059	161564.598225	36.727847
1636.228576	161840.908651	36.732864
1637.725974	162096.152543	36.737882
1639.701968	162360.567170	36.742900
1641.468716	162625.777887	36.747917
1642.921819	162891.801287	36.752935
1644.492682	163143.781743	36.757952
1645.977830	163414.648411	36.762970
1647.760723	163682.210521	36.767988
1648.734736	163952.312685	36.773005
1650.897311	164227.681491	36.778023
1652.862280	164504.795887	36.783040
1654.361516	164776.811895	36.788058
1655.913492	165049.582504	36.793076
1657.414646	165328.057737	36.798093
1659.367598	165616.723699	36.803111
1660.804048	165887.857430	36.808128
1662.339500	166183.316049	36.813146
1664.389233	166452.631642	36.818164
1666.300908	166736.404551	36.823181
1667.949290	167016.568656	36.828199
1669.749393	167290.204210	36.833216
1671.432974	167579.143822	36.838234
1673.420548	167859.755030	36.843252
1674.799081	168141.987083	36.848269
1676.730531	168412.185369	36.853287
1677.982263	168681.263193	36.858304
1679.426405	168973.359042	36.863322
1681.717937	169246.512183	36.868340
1683.089973	169528.197485	36.873357
1684.786797	169814.120546	36.878375
1686.676762	170104.619468	36.883392
1688.562479	170378.644245	36.888410
1690.560578	170658.018658	36.893428
1691.815422	170941.229694	36.898445
1693.532099	171207.815987	36.903463
1695.219703	171498.636589	36.908480
1696.698504	171783.226206	36.913498
1698.741091	172064.899633	36.918516
1700.277661	172332.143773	36.923533
1701.951156	172602.919820	36.928551
1704.074636	172873.854611	36.933568
1705.701088	173132.844542	36.938586
1707.747010	173376.813529	36.943604
1709.254096	173628.721859	36.948621
1710.701238	173877.165473	36.953639
1712.461612	174138.779288	36.958656
1713.953880	174387.789767	36.963674
1715.709411	174656.194571	36.968692
1717.627979	174920.871016	36.973709
1718.881304	175178.918603	36.978727
1720.574487	175446.336387	36.983744
1722.119995	175719.716475	36.988762
1724.006624	175989.504798	36.993780
1725.512354	176274.198317	36.998797
1726.812901	176542.751301	37.003815
1728.491143	176843.533058	37.008832
1730.290342	177125.547119	37.013850
1732.060055	177408.214811	37.018868
1733.614763	177707.614279	37.023885
1735.220537	178001.666661	37.028903
1736.932417	178299.459594	37.033920
1738.931808	178595.508952	37.038938
1740.634851	178894.982218	37.043956
1742.260712	179195.992337	37.048973
1744.024187	179494.597557	37.053991
1745.537897	179800.501703	37.059008
1746.922541	180110.818402	37.064026
1749.061137	180424.633608	37.069044
1751.333880	180732.644275	37.074061
1752.699529	181047.639854	37.079079
1754.832958	181378.756239	37.084096
1756.191865	181687.895813	37.089114
1758.166140	181995.810669	37.094132
1759.831852	182311.313422	37.099149
1761.891247	182612.024996	37.104167
1764.222821	182923.772281	37.109184
1765.780958	183229.820629	37.114202
1767.778594	183547.906104	37.119220
1769.553391	183852.300265	37.124237
1771.129852	184152.426570	37.129255
1772.817870	184461.114756	37.134272
1774.578547	184768.397781	37.139290
1776.513635	185080.908426	37.144308
1778.077532	185390.904321	37.149325
1779.890745	185711.838802	37.154343
1781.736440	186020.855305	37.159360
1783.333806	186344.201412	37.164378
1785.417406	186641.776759	37.169396
1787.231715	186955.639232	37.174413
1789.083533	187267.975164	37.179431
1790.721261	187592.414994	37.184448
1792.412765	187903.714768	37.189466
1794.427196	188220.028582	37.194484
1796.097238	188540.954874	37.199501
1798.046391	188832.703013	37.204519
1799.990769	189111.865259	37.209536
1801.507683	189425.855131	37.214554
1803.188132	189706.953632	37.219572
1805.078249	189990.215932	37.224589
1807.085964	190287.852065	37.229607
1808.709229	190578.710974	37.234624
1810.361798	190866.813173	37.239642
1812.249428	191155.882346	37.244660
1813.962589	191470.869811	37.249677
1815.680831	191772.609436	37.254695
1817.687405	192064.799782	37.259712
1819.324057	192375.350819	37.264730
1820.678974	192678.689342	37.269748
1822.772636	192994.324290	37.274765
1824.330091	193320.021589	37.279783
1826.106487	193630.774145	37.284800
1827.480947	193940.031429	37.289818
1829.880464	194266.337384	37.294836
1831.591634	194594.061956	37.299853
1833.218664	194923.845361	37.304871
1835.506100	195239.400361	37.309888
1837.175240	195576.275951	37.314906
1839.089809	195902.212604	37.319924
1841.282580	196224.718466	37.324941
1842.880775	196553.679391	37.329959
1844.960792	196875.686883	37.334976
1846.534209	197216.180310	37.339994
1848.055381	197543.928648	37.345012
1850.297145	197875.080426	37.350029
1851.991242	198216.716246	37.355047
1854.291711	198553.460317	37.360064
1855.940469	198891.820391	37.365082
1857.743509	199228.800037	37.370100
1859.858964	199553.433063	37.375117
1861.562908	199903.353819	37.380135
1863.500645	200232.702793	37.385152
1865.215697	200583.273549	37.390170
1867.383545	200925.029256	37.395188
1869.297293	201249.247580	37.400205
1871.016299	201607.008577	37.405223
1873.043885	201937.775261	37.410240
1875.157964	202279.827222	37.415258
1877.073756	202624.134107	37.420276
1879.082831	202951.419119	37.425293
1880.691734	203288.581644	37.430311
1883.002357	203616.393894	37.435328
1884.710251	203953.405065	37.440346
1886.640447	204290.421042	37.445364
1888.804659	204624.621931	37.450381
1890.636187	204965.211823	37.455399
1892.770232	205291.170368	37.460416
1894.411702	205626.513653	37.465434
1896.233843	205960.954311	37.470452
1898.528654	206278.387849	37.475469
1900.205996	206604.870545	37.480487
1901.815478	206918.620738	37.485504
1903.340504	207247.885834	37.490522
1905.515231	207552.955590	37.495540
1907.196692	207864.033527	37.500557
1908.481044	208178.959084	37.505575
1910.928998	208505.241056	37.510592
1912.504573	208838.277184	37.515610
1914.374442	209164.857567	37.520628
1916.062885	209492.280960	37.525645
1917.945566	209825.641887	37.530663
1919.794972	210156.013880	37.535680
1921.851329	210504.775319	37.540698
1923.417180	210852.778673	37.545716
1925.538636	211197.483903	37.550733
1926.704023	211550.023380	37.555751
1929.543260	211894.428081	37.560768
1930.998556	212249.731105	37.565786
1932.776208	212604.604081	37.570804
1935.379398	212965.606914	37.575821
1936.561798	213325.478795	37.580839
1938.816588	213676.155852	37.585856
1940.596697	214042.411634	37.590874
1942.560320	214408.538763	37.595892
1944.668425	214769.655501	37.600909
1946.564101	215146.830215	37.605927
1948.631801	215513.327777	37.610944
1950.748462	215879.057794	37.615962
1952.988672	216244.160761	37.620980
1955.069817	216608.491058	37.625997
1956.479982	216986.679861	37.631015
1959.028034	217343.119025	37.636032
1960.712657	217721.484121	37.641050
1962.644116	218090.238922	37.646068
1965.336272	218454.862828	37.651085
1967.317313	218828.819211	37.656103
1969.143055	219185.687033	37.661120
1971.237234	219544.393154	37.666138
1973.406443	219921.296410	37.671156
1975.405598	220287.296571	37.676173
1977.315380	220645.123201	37.681191
1979.275200	221005.533820	37.686208
1981.697738	221367.586875	37.691226
1983.258902	221730.184669	37.696244
1985.958302	222095.739818	37.701261
1987.434330	222452.475783	37.706279
1989.533987	222826.395528	37.711296
1991.796875	223162.630748	37.716314
1993.771114	223537.018252	37.721332
1995.774426	223900.368814	37.726349
1998.005127	224262.542201	37.731367
1999.789147	224615.582349	37.736384
2001.530391	225032.233529	37.741402
2003.533267	225391.476949	37.746420
2005.844472	225746.343100	37.751437
2007.390354	226107.109751	37.756455
2009.426909	226436.626782	37.761472
2011.602371	226778.402016	37.766490
2013.457260	227115.823311	37.771508
2015.497443	227455.553015	37.776525
2017.330533	227789.399628	37.781543
2019.337760	228132.514983	37.786560
2021.217614	228471.486913	37.791578
2022.968453	228823.102721	37.796596
2025.246275	229167.550691	37.801613
2026.749680	229529.011709	37.806631
2028.619141	229888.892327	37.811648
2030.540680	230248.918527	37.816666
2032.603361	230611.006344	37.821684
2034.707752	230979.006535	37.826701
2036.584695	231357.609557	37.831719
2038.812341	231727.472614	37.836736
2040.572073	232103.354391	37.841754
2042.742394	232478.689994	37.846772
2044.509268	232851.932302	37.851789
2046.353549	233247.920191	37.856807
2048.472282	233626.925807	37.861824
2050.575663	234023.028176	37.866842
2052.582396	234422.525433	37.871860
2055.000442	234809.869536	37.876877
2056.910846	235197.397277	37.881895
2058.892458	235602.770272	37.886912
2061.345627	236001.187100	37.891930
2063.186086	236407.119062	37.896948
2065.749814	236801.813270	37.901965
2067.652506	237203.166717	37.906983
2069.447901	237609.085109	37.912000
2071.818864	237997.363069	37.917018
2074.156259	238394.258032	37.922036
2076.442238	238795.074069	37.927053
2078.550423	239195.259393	37.932071
2080.317569	239590.725186	37.937088
2082.886570	239974.889437	37.942106
2084.476775	240367.211093	37.947124
2086.913783	240762.930307	37.952141
2088.671502	241174.125421	37.957159
2091.281263	241571.496354	37.962176
2093.489980	241967.281243	37.967194
2095.322746	242377.579627	37.972212
2097.524815	242766.129211	37.977229
2099.753967	243174.081392	37.982247
2102.106673	243568.553223	37.987264
2104.523719	243956.488221	37.992282
2106.148262	244360.120502	37.997300
2108.783770	244745.838808	38.002317
2110.871475	245139.366887	38.007335
2112.970966	245541.860659	38.012352
2115.449146	245929.639413	38.017370
2117.584708	246318.692852	38.022388
2119.616861	246698.898924	38.027405
2121.558515	247075.589671	38.032423
2123.376750	247440.743589	38.037440
2125.699453	247803.583139	38.042458
2127.484427	248171.919306	38.047476
2130.025168	248518.291590	38.052493
2131.864770	248886.138251	38.057511
2133.960630	249253.005321	38.062528
2136.098959	249604.143151	38.067546
2137.902213	249988.610659	38.072564
2139.855257	250355.985616	38.077581
2141.716573	250732.266474	38.082599
2143.844806	251117.599612	38.087616
2146.265689	251503.522278	38.092634
2148.023469	251899.229025	38.097652
2150.322917	252282.480166	38.102669
2152.589088	252679.479777	38.107687
2154.644981	253070.112385	38.112704
2156.859578	253455.716514	38.117722
2158.966744	253857.824336	38.122740
2160.899569	254258.868399	38.127757
2163.220801	254660.562974	38.132775
2165.139112	255065.649963	38.137792
2167.374731	255476.377542	38.142810
2169.302837	255887.281748	38.147828
2171.455410	256300.030949	38.152845
2173.759482	256711.232808	38.157863
2176.156297	257132.073638	38.162880
2178.866086	257538.411704	38.167898
2180.828089	257956.173179	38.172916
2182.693880	258375.271609	38.177933
2185.062609	258787.254541	38.182951
2187.372458	259208.798884	38.187968
2189.603241	259630.000859	38.192986
2191.085977	260061.661042	38.198004
2193.796346	260486.954419	38.203021
2195.842660	260911.286874	38.208039
2198.318188	261340.632479	38.213056
2200.370779	261770.528466	38.218074
2202.458210	262209.361367	38.223092
2204.719712	262643.645602	38.228109
2206.798965	263066.959894	38.233127
2208.983405	263507.252637	38.238144
2211.237392	263943.775302	38.243162
2213.347116	264392.743473	38.248180
2215.551676	264827.039625	38.253197
2218.053548	265269.443528	38.258215
2219.989919	265711.505764	38.263232
2222.678219	266146.336382	38.268250
2224.974083	266591.467152	38.273268
2227.206982	267026.777333	38.278285
2229.646279	267473.410428	38.283303
2231.874396	267901.152026	38.288320
2234.473168	268344.940866	38.293338
2236.376809	268786.554002	38.298356
2238.521933	269223.099341	38.303373
2240.972884	269634.371029	38.308391
2243.344412	270054.521328	38.313408
2245.227851	270457.805257	38.318426
2247.538158	270859.929376	38.323444
2249.472051	271274.738846	38.328461
2252.030544	271685.435747	38.333479
2253.838078	272094.270431	38.338496
2256.489153	272496.950923	38.343514
2258.669447	272919.419228	38.348532
2260.433420	273340.200841	38.353549
2262.834685	273748.306837	38.358567
2264.624865	274186.816077	38.363584
2266.884951	274607.036649	38.368602
2269.152312	275046.842159	38.373620
2271.253391	275486.242218	38.378637
2273.235646	275928.734951	38.383655
2275.359053	276378.673909	38.388672
2278.051615	276826.439529	38.393690
2280.274404	277292.976497	38.398708
2282.169081	277738.760024	38.403725
2284.911231	278195.154740	38.408743
2287.079441	278650.471781	38.413760
2289.443104	279107.662950	38.418778
2291.760012	279572.812627	38.423796
2293.942592	280033.359996	38.428813
2296.433940	280502.393728	38.433831
2298.944086	280964.844769	38.438848
2301.358960	281429.596951	38.443866
2303.295805	281895.567777	38.448884
2305.727514	282364.254194	38.453901
2308.434163	282829.772077	38.458919
2310.747999	283302.032924	38.463936
2313.066141	283775.943895	38.468954
2315.115006	284246.442289	38.473972
2317.517441	284717.468455	38.478989
2320.044501	285191.776797	38.484007
2322.684984	285663.907384	38.489024
2324.990283	286128.342634	38.494042
2327.063098	286607.776603	38.499060
2329.274534	287087.365819	38.504077
2332.078496	287548.443306	38.509095
2334.454208	288024.956868	38.514112
2336.773371	288501.173888	38.519130
2339.192590	288981.133977	38.524148
2341.700765	289446.116953	38.529165
2344.472354	289916.163423	38.534183
2346.501813	290386.377583	38.539200
2348.673313	290855.958780	38.544218
2351.582240	291326.463788	38.549236
2353.955195	291790.930888	38.554253
2356.615346	292257.510846	38.559271
2358.889578	292720.162910	38.564288
2361.459364	293177.889968	38.569306
2363.708216	293643.592574	38.574324
2366.148981	294100.499996	38.579341
2368.643541	294548.329330	38.584359
2370.729293	294996.908411	38.589376
2373.266804	295415.364106	38.594394
2375.254335	295841.984036	38.599412
2377.647623	296272.018855	38.604429
2379.872509	296705.280108	38.609447
2381.966734	297128.857546	38.614464
2384.084911	297566.731560	38.619482
2386.170810	298016.142137	38.624500
2388.668510	298466.731041	38.629517
2391.051941	298921.477426	38.634535
2392.944379	299375.995648	38.639552
2395.418315	299834.738796	38.644570
2397.807966	300305.229597	38.649588
2400.154486	300775.014671	38.654605
2402.602384	301234.139139	38.659623
2404.720379	301717.166455	38.664640
2407.315468	302204.231687	38.669658
2409.484725	302669.619467	38.674676
2411.983798	303166.933554	38.679693
2414.696513	303639.496935	38.684711
2417.038186	304144.605411	38.689728
2419.484623	304630.822689	38.694746
2421.917819	305114.093915	38.699764
2423.887859	305623.421766	38.704781
2426.340262	306108.312129	38.709799
2428.847801	306625.806241	38.714816
2431.189820	307131.462592	38.719834
2434.042084	307627.282415	38.724852
2436.396880	308141.822908	38.729869
2438.714162	308640.263604	38.734887
2441.123596	309152.048097	38.739904
2443.504501	309669.067354	38.744922
2446.269892	310180.892719	38.749940
2448.663327	310702.807696	38.754957
2451.446252	311203.856405	38.759975
2453.966177	311724.019596	38.764992
2456.354766	312244.785414	38.770010
2458.731328	312753.892495	38.775028
2461.509123	313277.436528	38.780045
2464.080895	313788.666811	38.785063
2466.687639	314305.045092	38.790080
2469.052698	314816.303228	38.795098
2472.034767	315335.334661	38.800116
2474.295215	315845.461394	38.805133
2477.000249	316346.854301	38.810151
2479.751340	316860.961922	38.815168
2482.195948	317365.718172	38.820186
2484.470170	317875.883200	38.825204
2487.099120	318383.043198	38.830221
2489.505030	318884.242013	38.835239
2492.045355	319398.496618	38.840256
2494.441714	319908.707636	38.845274
2497.418468	320399.318788	38.850292
2499.596074	320930.841722	38.855309
2502.040810	321416.071329	38.860327
2504.582088	321893.714756	38.865344
2507.094371	322356.680913	38.870362
2510.065333	322829.705187	38.875380
2512.093690	323306.126989	38.880397
2514.967193	323769.028398	38.885415
2516.848581	324237.849422	38.890432
2519.306323	324717.039679	38.895450
2521.781373	325186.320063	38.900468
2523.658810	325679.412078	38.905485
2526.233450	326169.673337	38.910503
2528.908364	326662.963200	38.915520
2531.258944	327151.908047	38.920538
2533.670787	327661.765744	38.925556
2536.214855	328181.198476	38.930573
2538.882403	328681.003440	38.935591
2540.993223	329191.279770	38.940608
2543.446353	329716.963666	38.945626
2545.688774	330222.844403	38.950644
2548.331078	330766.851055	38.955661
2551.022969	331287.661265	38.960679
2553.494797	331830.315846	38.965696
2555.759240	332353.725577	38.970714
2558.711423	332883.929547	38.975732
2561.026435	333440.817145	38.980749
2563.613395	333971.147071	38.985767
2566.364733	334526.738120	38.990784
2568.620106	335077.400982	38.995802
2571.755511	335620.353116	39.000820
2574.299933	336178.020427	39.005837
2576.777461	336723.429448	39.010855
2579.486752	337291.979947	39.015872
2582.112875	337838.575125	39.020890
2584.764960	338394.657994	39.025908
2587.364680	338957.701573	39.030925
2590.182930	339516.490758	39.035943
2592.689067	340066.564757	39.040960
2595.502418	340638.598802	39.045978
2598.190232	341183.505461	39.050996
2600.722335	341746.992083	39.056013
2603.672910	342288.242075	39.061031
2606.573130	342853.412173	39.066048
2609.119096	343390.552637	39.071066
2611.957241	343941.250564	39.076084
2614.563361	344508.660622	39.081101
2617.443753	345053.045187	39.086119
2620.197129	345595.007571	39.091136
2622.579070	346148.651514	39.096154
2625.488143	346682.378782	39.101172
2628.232643	347239.331441	39.106189
2630.510499	347780.942472	39.111207
2633.636707	348324.724184	39.116224
2636.219714	348869.779871	39.121242
2639.048826	349402.047181	39.126260
2641.638040	349959.759140	39.131277
2644.455004	350468.129539	39.136295
2646.765566	350978.809383	39.141312
2649.278878	351482.395102	39.146330
2651.588292	351991.212427	39.151348
2654.322828	352499.196033	39.156365
2656.647223	353011.098264	39.161383
2659.690232	353520.089406	39.166400
2661.689768	354034.267008	39.171418
2664.520764	354558.994594	39.176436
2666.950011	355084.262796	39.181453
2669.586808	355611.472693	39.186471
2671.996214	356145.084405	39.191488
2674.478581	356692.639677	39.196506
2677.059940	357225.958936	39.201524
2679.713906	357775.023603	39.206541
2682.099914	358331.282461	39.211559
2685.201306	358880.365568	39.216576
2687.354029	359443.248148	39.221594
2690.399727	360001.896404	39.226612
2692.554649	360574.105913	39.231629
2695.326833	361139.687995	39.236647
2698.390117	361717.653741	39.241664
2700.828845	362305.939588	39.246682
2703.405867	362879.247446	39.251700
2706.133482	363464.605120	39.256717
2709.187632	364052.467027	39.261735
2711.616777	364645.623120	39.266752
2714.172042	365242.888291	39.271770
2716.955289	365836.277423	39.276788
2719.395898	366439.838839	39.281805
2722.386608	367027.418680	39.286823
2725.423021	367636.554227	39.291840
2728.146611	368232.560350	39.296858
2731.089168	368845.906690	39.301876
2733.987935	369449.405420	39.306893
2736.835906	370048.666067	39.311911
2739.929103	370654.908597	39.316928
2742.512129	371250.489684	39.321946
2745.568089	371857.710731	39.326964
2748.231244	372458.438696	39.331981
2751.075521	373048.193208	39.336999
2754.183493	373645.763520	39.342016
2756.712476	374261.787236	39.347034
2759.580879	374860.976525	39.352052
2762.565091	375451.841918	39.357069
2765.020774	376047.831541	39.362087
2767.853707	376654.155154	39.367104
2770.590594	377258.455165	39.372122
2773.428997	377855.448515	39.377140
2776.252891	378465.145962	39.382157
2778.875654	379063.094071	39.387175
2782.269022	379666.746193	39.392192
2784.684890	380278.662052	39.397210
2787.836870	380867.239004	39.402228
2790.719767	381475.053775	39.407245
2793.275646	382058.455655	39.412263
2796.102456	382618.797006	39.417280
2798.586677	383187.048331	39.422298
2801.348770	383744.263141	39.427316
2803.823170	384314.427006	39.432333
2806.656412	384881.684357	39.437351
2809.637729	385447.489150	39.442368
2812.145560	386022.973890	39.447386
2814.867073	386610.870199	39.452404
2817.497415	387180.534190	39.457421
2820.353149	387763.038787	39.462439
2823.292098	388353.510569	39.467456
2825.907730	388952.013458	39.472474
2828.879684	389523.362044	39.477492
2831.598083	390118.455911	39.482509
2834.189463	390713.306325	39.487527
2836.878474	391315.562359	39.492544
2839.484833	391931.719313	39.497562
2842.454006	392551.003500	39.502580
2845.423881	393167.461553	39.507597
2848.300642	393783.010428	39.512615
2850.979821	394411.310184	39.517632
2853.754249	395047.520810	39.522650
2856.706398	395675.627358	39.527668
2859.598598	396323.308389	39.532685
2862.229280	396963.512492	39.537703
2865.468573	397584.513980	39.542720
2868.276312	398236.532972	39.547738
2871.105237	398868.453590	39.552756
2874.075730	399509.518553	39.557773
2876.879499	400172.884786	39.562791
2880.126294	400806.933297	39.567808
2882.698200	401466.785614	39.572826
2885.686393	402107.162905	39.577844
2888.946241	402766.271290	39.582861
2891.297441	403422.670437	39.587879
2894.610220	404080.729230	39.592896
2897.789164	404751.953115	39.597914
2900.491559	405403.844473	39.602932
2903.330636	406052.912085	39.607949
2906.688668	406707.435752	39.612967
2909.562068	407351.705042	39.617984
2912.589452	408024.581016	39.623002
2915.489909	408683.824852	39.628020
2918.546160	409337.630708	39.633037
2921.390197	410007.425009	39.638055
2924.663432	410655.921231	39.643072
2927.789900	411311.447674	39.648090
2930.636493	411959.552432	39.653108
2933.663606	412617.397817	39.658125
2936.406161	413288.047393	39.663143
2939.457896	413943.274305	39.668160
2942.220301	414595.339138	39.673178
2945.211191	415241.499066	39.678196
2948.511958	415900.672312	39.683213
2951.108714	416552.820950	39.688231
2954.165442	417166.616736	39.693248
2956.942125	417794.457172	39.698266
2959.642050	418400.858183	39.703284
2962.662149	419015.354990	39.708301
2965.227275	419629.454391	39.713319
2968.030504	420250.065447	39.718336
2970.821794	420880.723880	39.723354
2973.806058	421508.601133	39.728372
2976.978701	422148.824147	39.733389
2979.632388	422799.679733	39.738407
2982.684886	423440.449302	39.743424
2985.452792	424098.932847	39.748442
2988.150662	424751.458056	39.753460
2991.260961	425409.653163	39.758477
2994.223331	426074.011689	39.763495
2997.365931	426737.413391	39.768512
2999.875982	427408.574414	39.773530
3003.021049	428097.932662	39.778548
3006.141208	428772.509265	39.783565
3009.055553	429453.180492	39.788583
3012.265621	430134.066014	39.793600
3015.322783	430820.479760	39.798618
3017.888854	431515.818030	39.803636
3021.271694	432201.713379	39.808653
3024.304747	432909.350895	39.813671
3027.341185	433586.906570	39.818688
3030.567132	434300.300355	39.823706
3033.687527	434998.850762	39.828724
3037.246177	435695.540007	39.833741
3040.040139	436404.334314	39.838759
3043.118299	437111.468452	39.843776
3046.672435	437806.656811	39.848794
3049.562847	438513.249402	39.853812
3052.861292	439213.047517	39.858829
3055.397492	439907.300230	39.863847
3059.149345	440607.594875	39.868864
3061.956051	441328.628133	39.873882
3065.192736	442039.141361	39.878900
3068.400173	442738.296637	39.883917
3071.163326	443456.691590	39.888935
3074.475703	444155.131177	39.893952
3077.721025	444859.990997	39.898970
3080.958670	445578.500729	39.903988
3084.103346	446266.172338	39.909005
3087.048615	446982.660948	39.914023
3089.938048	447689.163992	39.919040
3093.003562	448407.463424	39.924058
3096.058079	449119.971958	39.929076
3099.300777	449836.630328	39.934093
3102.246209	450566.018470	39.939111
3104.888257	451279.740968	39.944128
3108.649314	451996.098735	39.949146
3111.588382	452730.480867	39.954164
3114.753319	453438.283873	39.959181
3117.939057	454161.750352	39.964199
3121.130382	454824.818444	39.969216
3123.895120	455505.140562	39.974234
3127.273985	456184.181092	39.979252
3130.261370	456843.578537	39.984269
3133.136844	457535.257841	39.989287
3136.196820	458212.263185	39.994304
3139.168265	458889.261881	39.999322
3142.173380	459588.142829	40.004340
3145.149484	460270.866406	40.009357
3147.900879	460977.939687	40.014375
3151.169638	461688.702633	40.019392
3154.136418	462395.948840	40.024410
3157.203883	463150.304373	40.029428
3160.702745	463846.036663	40.034445
3163.255218	464568.301506	40.039463
3166.443370	465295.803283	40.044480
3169.823550	466039.992360	40.049498
3172.870927	466780.869772	40.054516
3175.895012	467520.763973	40.059533
3178.929979	468275.044697	40.064551
3182.202083	469017.224152	40.069568
3185.429955	469769.448211	40.074586
3188.301625	470565.040484	40.079604
3191.677997	471309.700915	40.084621
3194.627334	472089.546050	40.089639
3197.808301	472860.021075	40.094656
3200.954463	473662.023975	40.099674
3204.548935	474427.065500	40.104692
3207.846988	475215.786811	40.109709
3210.896978	476002.595485	40.114727
3214.214512	476784.680098	40.119744
3217.800027	477572.707729	40.124762
3220.827008	478371.560080	40.129780
3224.698312	479155.688738	40.134797
3227.641556	479967.430857	40.139815
3231.024244	480750.107846	40.144832
3234.657046	481539.486962	40.149850
3237.739435	482327.910553	40.154868
3240.765830	483103.979684	40.159885
3244.276851	483910.061286	40.164903
3247.538229	484714.026405	40.169920
3250.916635	485489.641211	40.174938
3253.997255	486295.236577	40.179956
3257.770126	487092.654576	40.184973
3260.829418	487903.844790	40.189991
3264.074735	488685.767941	40.195008
3267.520603	489476.721121	40.200026
3270.684361	490279.507479	40.205044
3273.853979	491060.990581	40.210061
3277.173691	491882.122794	40.215079
3280.462215	492650.790674	40.220096
3283.936449	493475.515715	40.225114
3286.612447	494263.660548	40.230132
3290.362959	495065.794313	40.235149
3293.719545	495876.389681	40.240167
3296.805748	496645.781737	40.245184
3300.102323	497386.777226	40.250202
3302.972040	498137.051266	40.255220
3306.167558	498913.955364	40.260237
3309.449076	499680.057161	40.265255
3312.196451	500440.151741	40.270272
3315.560597	501221.423357	40.275290
3318.211915	502017.970326	40.280308
3321.365706	502790.270159	40.285325
3324.992398	503605.170424	40.290343
3327.764845	504391.949365	40.295360
3331.060308	505213.895030	40.300378
3334.156072	506003.024205	40.305396
3337.450051	506860.175752	40.310413
3340.415785	507662.474591	40.315431
3344.007558	508529.944339	40.320448
3347.634299	509331.405278	40.325466
3350.449861	510224.650531	40.330484
3353.628788	511056.380244	40.335501
3357.904439	511890.065849	40.340519
3360.882637	512797.481371	40.345536
3364.346324	513630.604519	40.350554
3367.786338	514482.155570	40.355572
3370.954102	515347.882732	40.360589
3374.766219	516232.431122	40.365607
3377.667840	517086.861000	40.370624
3381.410754	517987.973632	40.375642
3384.506148	518847.023858	40.380660
3388.019376	519727.499370	40.385677
3391.630371	520642.307495	40.390695
3395.310413	521492.906765	40.395712
3398.880353	522374.088616	40.400730
3401.923270	523309.613340	40.405748
3405.703116	524199.991554	40.410765
3409.053193	525058.322202	40.415783
3412.403615	525948.974298	40.420800
3416.230154	526871.615009	40.425818
3419.772347	527773.831193	40.430836
3423.117131	528676.027474	40.435853
3426.997926	529535.243652	40.440871
3430.654250	530422.875391	40.445888
3433.914491	531346.756704	40.450906
3437.442560	532224.680783	40.455924
3440.668968	533089.450575	40.460941
3444.739221	533961.849554	40.465959
3448.098213	534834.211169	40.470976
3452.081428	535709.951891	40.475994
3455.361194	536603.941987	40.481012
3458.436664	537510.759033	40.486029
3461.969446	538409.742560	40.491047
3465.588367	539302.916966	40.496064
3469.247218	540185.454847	40.501082
3472.600653	541077.408265	40.506100
3476.180428	541961.214933	40.511117
3479.808791	542827.198355	40.516122
3482.935667	543656.891315	40.521127
3486.222265	544405.535487	40.526132
3489.413780	545111.701384	40.531136
3492.247257	545770.136096	40.536141
3495.527469	546359.820744	40.541146
3498.063389	546874.541206	40.546151
3500.292562	547334.375625	40.551156
3503.121096	547736.409864	40.556160
3505.997608	548055.751956	40.561165
3507.729554	548353.918609	40.566170
3509.384223	548596.372035	40.571175
3511.379876	548783.957349	40.576180
3512.096385	548957.358669	40.581184
3513.738616	549086.905669	40.586189
3515.117518	549167.589164	40.591194
3515.818635	549201.595141	40.596199
3516.601185	549175.934465	40.601204
3517.708702	549163.192822	40.606208
3518.827803	549125.972029	40.611213
3519.457071	549060.061282	40.616218
3520.198570	548938.919124	40.621223
3521.003516	548771.485078	40.626228
3521.361391	548625.367849	40.631232
3521.512752	548492.505185	40.636237
3522.005127	548323.651778	40.641242
3522.083923	548144.918794	40.646247
3522.453302	547922.074978	40.651252
3522.424041	547725.385627	40.656256
3522.549900	547494.901854	40.661261
3522.952882	547255.840386	40.666266
3522.795147	547026.706468	40.671271
3522.989996	546717.557957	40.676276
3523.244269	546457.155292	40.681280
3523.040809	546210.247727	40.686285
3523.042598	545987.331854	40.691290
3522.922124	545738.333653	40.696295
3523.014485	545459.564205	40.701300
3522.585413	545167.797034	40.706304
3522.169903	544889.551497	40.711309
3522.358991	544623.826239	40.716314
3521.878697	544357.949608	40.721319
3522.260661	544093.951402	40.726324
3522.024891	543839.234750	40.731328
3521.740831	543559.277561	40.736333
3521.720756	543249.636554	40.741338
3521.539318	542971.267793	40.746343
3521.375569	542703.948510	40.751348
3520.768528	542484.408893	40.756352
3520.766214	542203.372036	40.761357
3520.260376	541944.676991	40.766362
3520.036773	541665.230344	40.771367
3520.188021	541408.896463	40.776372
3520.087546	541196.478778	40.781376
3519.477802	540929.955920	40.786381
3519.353284	540676.380002	40.791386
3519.257040	540407.090415	40.796391
3519.390408	540166.493751	40.801396
3518.822780	539949.082478	40.806400
3518.629516	539677.926782	40.811405
3518.392991	539466.011338	40.816410
3517.924962	539201.152732	40.821415
3517.801462	539022.999239	40.826420
3517.683857	538786.713141	40.831424
3517.058608	538546.867289	40.836429
3517.275092	538325.420049	40.841434
3516.902902	538139.921787	40.846439
3515.930017	537908.302781	40.851444
3516.084797	537693.927061	40.856448
3515.797970	537539.318437	40.861453
3515.579740	537308.530733	40.866458
3515.732252	537107.683453	40.871463
3515.326848	536959.906466	40.876468
3515.311457	536757.363811	40.881472
3515.425459	536546.110141	40.886477
3515.253966	536351.112950	40.891482
3514.803607	536173.685125	40.896487
3514.957590	535979.439984	40.901492
3514.559653	535791.341247	40.906496
3514.237004	535614.695020	40.911501
3514.132486	535471.503486	40.916506
3513.450507	535330.270945	40.921511
3513.037668	535154.037823	40.926516
3512.989802	535000.073142	40.931520
3513.102549	534843.707266	40.936525
3512.959196	534684.298742	40.941530
3512.435298	534579.204582	40.946535
3513.019901	534421.294864	40.951540
3512.745831	534267.560728	40.956544
3512.127241	534123.023453	40.961549
3512.009866	533974.717699	40.966554
3512.003582	533835.334995	40.971559
3511.982041	533679.332252	40.976564
3511.955251	533591.834971	40.981568
3511.538159	533450.442397	40.986573
3511.890135	533306.906129	40.991578
3511.442584	533169.405981	40.996583
3511.428350	533085.591982	41.001588
3511.298531	532972.543190	41.006592
3510.908564	532825.381070	41.011597
3510.891709	532691.294737	41.016602
3510.999488	532557.591747	41.021607
3510.862565	532440.801449	41.026612
3510.660339	532370.604384	41.031616
3510.061704	532252.622536	41.036621
3510.162280	532132.356699	41.041626
3510.318391	532018.144255	41.046631
3510.062539	531952.248479	41.051636
3509.844897	531822.784299	41.056640
3510.203500	531705.152303	41.061645
3510.095142	531646.002516	41.066650
3509.467440	531526.655564	41.071655
3509.545753	531389.662985	41.076660
3509.698466	531315.918680	41.081664
3509.537406	531252.733496	41.086669
3509.423602	531179.131728	41.091674
3508.861487	531095.393665	41.096679
3508.936171	530977.144216	41.101684
3508.830294	530868.826196	41.106688
3508.600811	530839.302757	41.111693
3508.680046	530753.895096	41.116698
3508.593640	530661.489463	41.121703
3508.235348	530577.362717	41.126708
3508.435515	530495.421139	41.131712
3508.379909	530411.852039	41.136717
3508.117032	530372.378404	41.141722
3507.830817	530288.794568	41.146727
3508.322446	530205.491605	41.151732
3507.995226	530179.620651	41.156736
3507.489891	530115.828404	41.161741
3507.725108	530038.174122	41.166746
3507.819471	529948.767671	41.171751
3507.908332	529916.261308	41.176756
3507.652790	529871.984671	41.181760
3507.487623	529793.583944	41.186765
3507.287766	529717.917102	41.191770
3507.748485	529653.060706	41.196775
3507.624390	529603.254404	41.201780
3507.692534	529573.125686	41.206784
3507.144851	529512.319176	41.211789
3507.588761	529420.580473	41.216794
3507.013234	529361.597012	41.221799
3507.553603	529297.787794	41.226804
3507.323563	529248.300325	41.231808
3507.153463	529242.970595	41.236813
3507.094502	529189.716339	41.241818
3506.685690	529129.796037	41.246823
3506.971629	529040.253107	41.251828
3507.035395	529041.354867	41.256832
3506.406374	528991.525370	41.261837
3506.647068	528950.351460	41.266842
3506.537254	528910.445696	41.271847
3506.501298	528867.748687	41.276852
3506.883716	528801.688325	41.281856
3506.675146	528719.044107	41.286861
3507.150319	528670.757323	41.291866
3506.494952	528640.033670	41.296871
3506.433570	528643.429384	41.301876
3506.319299	528581.893826	41.306880
3505.496935	528543.716934	41.311885
3506.027535	528501.636914	41.316890
3506.101537	528475.244925	41.321895
3506.010905	528470.609894	41.326900
3505.993992	528419.873265	41.331904
3506.339700	528360.235105	41.336909
3506.407790	528366.137289	41.341914
3506.053428	528331.575154	41.346919
3506.846231	528253.621858	41.351924
3506.292036	528250.626700	41.356928
3506.005656	528241.726824	41.361933
3506.080481	528178.138303	41.366938
3506.143312	528117.583718	41.371943
3506.018731	528075.454508	41.376948
3505.995555	528090.973510	41.381952
3506.128168	528054.615504	41.386957
3505.901228	527993.499784	41.391962
3506.294118	527945.628116	41.396967
3506.282332	527960.286285	41.401972
3506.003880	527904.687089	41.406976
3506.149841	527844.320483	41.411981
3506.317381	527833.883003	41.416986
3505.568849	527819.446084	41.421991
3505.779680	527768.014373	41.426996
3505.803341	527741.578584	41.432000
3505.574345	527751.065712	41.437005
3505.608307	527700.824144	41.442010
3505.605891	527659.028302	41.447015
3506.174241	527618.405638	41.452020
3506.047731	527591.184697	41.457024
3505.636449	527591.148680	41.462029
3505.844534	527568.473952	41.467034
3505.626624	527536.567143	41.472039
3505.317440	527490.321273	41.477044
3505.180052	527467.599921	41.482048
3505.575252	527421.899551	41.487053
3505.647226	527393.535013	41.492058
3505.250815	527379.800150	41.497063
3505.509395	527367.023108	41.502068
3505.692559	527367.600708	41.507072
3505.748933	527366.025099	41.512077
3505.363404	527314.989426	41.517082
3505.711058	527272.581295	41.522087
3505.381058	527227.601476	41.527092
3505.658493	527241.759726	41.532096
3505.260031	527230.501568	41.537101
3505.710514	527203.845808	41.542106
3505.321753	527199.965101	41.547111
3505.542186	527139.028106	41.552116
3505.370681	527157.907187	41.557120
3505.024678	527099.333922	41.562125
3505.410357	527125.453494	41.567130
3505.573014	527071.954957	41.572135
3505.492147	527062.617607	41.577140
3505.463839	527019.055225	41.582144
3505.352586	527034.942966	41.587149
3505.091757	526994.904645	41.592154
3505.278274	526959.495920	41.597159
3504.991739	526989.310432	41.602164
3505.279157	526965.004971	41.607168
3505.037517	526919.858695	41.612173
3505.492153	526871.771883	41.617178
3505.516270	526886.273738	41.622183
3505.373243	526887.863210	41.627188
3504.958234	526843.653878	41.632192
3505.200946	526814.553736	41.637197
3505.285154	526790.987722	41.642202
3505.030585	526826.609866	41.647207
3504.824637	526791.717679	41.652212
3504.905239	526761.632213	41.657216
3504.848275	526731.214634	41.662221
3505.172333	526717.618044	41.667226
3504.735825	526734.366172	41.672231
3504.989842	526691.920760	41.677236
3505.446371	526677.545058	41.682240
3505.254009	526644.773201	41.687245
3505.650304	526618.226118	41.692250
3505.292354	526626.319088	41.697255
3505.143604	526623.967138	41.702260
3505.170797	526568.213894	41.707264
3505.085003	526557.512362	41.712269
3505.183626	526583.374929	41.717274
3504.930955	526589.631726	41.722279
3504.585867	526549.858322	41.727284
3504.741800	526522.944724	41.732288
3505.285766	526497.182795	41.737293
3505.018645	526514.611988	41.742298
3504.856837	526485.373009	41.747303
3504.819992	526467.991947	41.752308
3505.031871	526476.146562	41.757312
3504.955913	526426.575427	41.762317
3504.975905	526450.479436	41.767322
3505.045103	526418.120669	41.772327
3505.291741	526377.394074	41.777332
3504.951534	526408.431199	41.782336
3504.293722	526377.653018	41.787341
3505.048297	526344.983606	41.792346
3505.028344	526380.215854	41.797351
3504.897380	526362.900097	41.802356
3504.875375	526342.585013	41.807360
3504.618254	526310.176514	41.812365
3505.016206	526274.176875	41.817370
3505.033390	526336.393869	41.822375
3505.078476	526303.988138	41.827380
3505.307954	526270.340141	41.832384
3504.491105	526244.641249	41.837389
3505.265129	526199.534594	41.842394
3504.695614	526234.904563	41.847399
3504.473657	526236.253853	41.852404
3504.451100	526218.668086	41.857408
3504.371410	526214.485568	41.862413
3504.860943	526199.295514	41.867418
3504.424117	526189.407380	41.872423
3505.338083	526147.968201	41.877428
3505.264343	526124.678893	41.882432
3504.842541	526168.972045	41.887437
3504.585115	526140.808982	41.892442
3504.488600	526127.429998	41.897447
3505.253121	526091.675281	41.902452
3504.944880	526099.507935	41.907456
3504.957528	526109.311654	41.912461
3504.606177	526056.952404	41.917466
3504.910581	526046.643763	41.922471
3504.805052	526066.474053	41.927476
3505.011137	526058.809285	41.932480
3504.881540	526026.177878	41.937485
3504.470437	526006.328223	41.942490
3505.182794	525977.708332	41.947495
3505.042157	525987.030901	41.952500
3504.714128	525999.617959	41.957504
3504.828770	525996.162844	41.962509
3505.161090	525980.138167	41.967514
3504.918164	525941.358006	41.972519
3505.038909	525916.672939	41.977524
3505.218804	525934.183747	41.982528
3504.796312	525941.680719	41.987533
3504.757434	525897.106055	41.992538
3505.326799	525853.041681	41.997543
3504.727702	525880.885836	42.002548
3505.353895	525827.663704	42.007552
3505.259237	525836.069275	42.012557
3505.420399	525781.050305	42.017562
3505.167554	525780.635417	42.022567
3504.787587	525778.572614	42.027572
3504.795959	525741.875171	42.032576
3504.995340	525728.600726	42.037581
3505.144119	525725.140157	42.042586
3505.343391	525734.105876	42.047591
3505.043638	525703.219262	42.052596
3505.276287	525650.260927	42.057600
3504.991192	525687.356258	42.062605
3504.708994	525626.088587	42.067610
3505.004988	525600.768784	42.072615
3504.840714	525603.018841	42.077620
3505.070285	525604.549551	42.082624
3504.746620	525630.076028	42.087629
3505.050929	525587.114287	42.092634
3504.899221	525565.908887	42.097639
3505.104885	525519.778138	42.102644
3504.761623	525515.081083	42.107648
3504.909325	525535.326924	42.112653
3504.913175	525492.867335	42.117658
3505.110723	525466.602497	42.122663
3504.961799	525443.071350	42.127668
3505.538664	525450.713882	42.132672
3504.665308	525460.809667	42.137677
3504.861606	525420.038057	42.142682
3504.839683	525388.247631	42.147687
3504.752678	525430.468027	42.152692
3504.790372	525411.153264	42.157696
3504.669743	525385.747330	42.162701
3505.300679	525349.304424	42.167706
3504.783582	525388.509538	42.172711
3504.569865	525378.636187	42.177716
3505.024006	525324.984665	42.182720
3504.942527	525313.422321	42.187725
3504.932101	525345.571958	42.192730
3504.722043	525297.989868	42.197735
3505.160022	525266.935271	42.202740
3504.881121	525304.738165	42.207744
3504.627332	525300.077453	42.212749
3504.756300	525250.318659	42.217754
3505.060306	525223.581674	42.222759
3504.982566	525205.093666	42.227764
3505.047949	525188.604918	42.232768
3504.953427	525166.530646	42.237773
3504.508927	525156.289252	42.242778
3504.583813	525200.456020	42.247783
3504.384932	525178.196067	42.252788
3504.803367	525169.183080	42.257792
3504.344860	525134.125015	42.262797
3504.352110	525159.043912	42.267802
3504.536084	525133.791628	42.272807
3504.577408	525143.035380	42.277812
3505.028595	525164.497412	42.282816
3504.634207	525149.597717	42.287821
3504.498332	525132.786886	42.292826
3504.375826	525132.300832	42.297831
3504.632709	525130.288934	42.302836
3504.626632	525118.006864	42.307840
3504.273592	525089.654878	42.312845
3504.439896	525066.578838	42.317850
3504.858121	525107.709270	42.322855
3504.447354	525074.109414	42.327860
3504.915493	525026.368786	42.332864
3504.799698	525052.924830	42.337869
3505.092818	525050.250072	42.342874
3504.919847	524986.839691	42.347879
3504.473590	525025.933392	42.352884
3505.103387	525006.979496	42.357888
3504.513240	524975.227515	42.362893
3504.875159	524937.057011	42.367898
3504.867141	524988.263674	42.372903
3504.195998	524970.121924	42.377908
3504.770968	524916.298302	42.382912
3505.055591	524903.161351	42.387917
3504.717060	524953.106103	42.392922
3504.599856	524947.109447	42.397927
3504.405518	524899.675340	42.402932
3504.697382	524902.055596	42.407936
3504.044283	524918.384906	42.412941
3504.643288	524886.798644	42.417946
3505.140421	524865.135934	42.422951
3504.553616	524892.019428	42.427956
3504.902470	524890.043513	42.432960
3504.771035	524863.981334	42.437965
3504.994782	524819.463276	42.442970
3504.715578	524832.498464	42.447975
3504.561106	524840.711813	42.452980
3505.233135	524793.089917	42.457984
3504.989914	524794.493234	42.462989
3504.814116	524824.294257	42.467994
3504.663101	524796.364763	42.472999
3504.514826	524788.249911	42.478004
3504.549317	524788.295070	42.483008
3504.423208	524792.005121	42.488013
3504.512144	524756.859712	42.493018
3503.947121	524730.562552	42.498023
3504.227354	524724.705194	42.503028
3505.120432	524697.874236	42.508032
3504.638815	524728.734750	42.513037
3504.495118	524749.634221	42.518042
3504.555900	524709.842662	42.523047
3504.579468	524681.026043	42.528052
3504.722701	524677.768324	42.533056
3504.932855	524678.442858	42.538061
3504.942050	524651.852619	42.543066
3504.667069	524684.348682	42.548071
3504.435773	524670.838140	42.553076
3504.500191	524640.043575	42.558080
3504.640039	524626.777633	42.563085
3504.597350	524651.048067	42.568090
3504.774157	524631.609286	42.573095
3504.501853	524612.746956	42.578100
3504.750637	524615.437359	42.583104
3504.705643	524617.971996	42.588109
3504.695082	524569.597987	42.593114
3504.811847	524586.260899	42.598119
3504.460144	524582.373694	42.603124
3504.850916	524534.542742	42.608128
3504.999321	524551.200690	42.613133
3504.528023	524545.613694	42.618138
3505.197475	524494.958357	42.623143
3504.989808	524535.835323	42.628148
3504.935877	524507.131741	42.633152
3504.334652	524480.182748	42.638157
3504.727487	524447.516121	42.643162
3504.853609	524479.645903	42.648167
3504.415226	524439.325973	42.653172
3504.971800	524422.202761	42.658176
3504.463080	524461.964847	42.663181
3504.009670	524441.260598	42.668186
3504.734986	524405.609447	42.673191
3504.307815	524415.787009	42.678196
3504.417354	524417.539005	42.683200
3504.263565	524398.859893	42.688205
3504.957379	524373.728042	42.693210
3505.037067	524357.640585	42.698215
3504.701825	524346.471504	42.703220
3505.074326	524342.722531	42.708224
3504.618975	524382.981877	42.713229
3504.362960	524348.901100	42.718234
3504.806434	524303.841394	42.723239
3504.549757	524319.957000	42.728244
3504.773423	524341.152789	42.733248
3504.250239	524308.226255	42.738253
3504.445063	524289.239168	42.743258
3504.488942	524304.700683	42.748263
3504.239097	524304.790782	42.753268
3504.711859	524287.882876	42.758272
3504.438831	524303.546130	42.763277
3504.846979	524250.201611	42.768282
3504.752143	524280.951297	42.773287
3504.701731	524275.297687	42.778292
3504.960786	524226.475635	42.783296
3504.527255	524249.443580	42.788301
3504.618890	524212.729498	42.793306
3504.546721	524241.302003	42.798311
3504.447867	524223.271162	42.803316
3504.627538	524203.275358	42.808321
3504.821021	524164.876901	42.813325
3504.624570	524184.976628	42.818330
3504.620954	524189.779570	42.823335
3505.005894	524145.739688	42.828340
3504.498026	524170.337119	42.833345
3504.036779	524158.985620	42.838349
3504.924485	524137.765715	42.843354
3504.852159	524159.008525	42.848359
3504.260673	524135.595967	42.853364
3504.606936	524112.945080	42.858369
3504.465688	524118.780814	42.863373
3503.963681	524118.101954	42.868378
3504.652560	524109.905000	42.873383
3504.716171	524099.885931	42.878388
3504.645913	524117.994311	42.883393
3504.471926	524110.995301	42.888397
3504.317568	524094.439063	42.893402
3504.985616	524060.413835	42.898407
3504.214087	524077.066013	42.903412
3504.448612	524069.193605	42.908417
3504.783734	524034.412124	42.913421
3504.442122	524071.368446	42.918426
3504.528532	524019.236689	42.923431
3504.375366	524034.931810	42.928436
3504.369001	523987.768623	42.933441
3504.380693	524028.662751	42.938445
3504.908506	524012.857983	42.943450
3504.773392	523987.957649	42.948455
3504.802613	523993.463178	42.953460
3504.794320	523969.402142	42.958465
3504.766784	523980.173981	42.963469
3504.478333	523971.272052	42.968474
3504.731808	523950.455451	42.973479
3504.593442	523943.096879	42.978484
3504.478126	523945.592184	42.983489
3504.090975	523939.283957	42.988493
3504.555883	523891.388838	42.993498
3504.779786	523895.195429	42.998503
3504.464011	523925.171885	43.003508
3504.428796	523883.876923	43.008513
3504.527685	523920.056246	43.013517
3504.344345	523869.837047	43.018522
3504.589417	523856.705498	43.023527
3504.655888	523902.899210	43.028532
3504.672520	523855.580350	43.033537
3504.325086	523887.482842	43.038541
3504.335739	523841.024261	43.043546
3504.634202	523811.960440	43.048551
3504.332336	523851.135260	43.053556
3504.468723	523822.299281	43.058561
3504.250719	523860.550892	43.063565
3504.686441	523834.801828	43.068570
3504.623759	523813.681157	43.073575
3504.507223	523819.917507	43.078580
3504.689610	523812.204869	43.083585
3504.383219	523808.411417	43.088589
3504.515950	523800.251656	43.093594
3504.380368	523777.322593	43.098599
3504.355520	523768.884410	43.103604
3504.498195	523758.903186	43.108609
3504.253584	523781.336415	43.113613
3504.703638	523759.730222	43.118618
3504.586376	523747.515235	43.123623
3504.311201	523762.016655	43.128628
3504.776629	523724.686317	43.133633
3504.590196	523736.545025	43.138637
3504.354896	523743.609007	43.143642
3504.419842	523731.567419	43.148647
3504.792899	523708.052348	43.153652
3504.575085	523687.360448	43.158657
3504.779616	523709.166716	43.163661
3504.763103	523681.163486	43.168666
3504.646937	523671.071461	43.173671
3504.727001	523686.578400	43.178676
3504.910758	523662.284346	43.183681
3504.732598	523650.887747	43.188685
3504.905924	523632.307707	43.193690
3504.888570	523623.868264	43.198695
3504.884151	523591.414355	43.203700
3504.835533	523615.838936	43.208705
3504.726754	523624.197336	43.213709
3504.263434	523593.281979	43.218714
3504.634436	523549.545996	43.223719
3504.811888	523560.032954	43.228724
3504.936507	523579.931027	43.233729
3504.765912	523551.395847	43.238733
3504.756863	523546.139865	43.243738
3504.825940	523546.129009	43.248743
3504.546436	523521.149672	43.253748
3505.022354	523471.077806	43.258753
3504.865238	523489.605038	43.263757
3504.813149	523492.798158	43.268762
3504.751883	523444.934330	43.273767
3504.178045	523466.055099	43.278772
3504.805740	523421.267143	43.283777
3504.586407	523443.241866	43.288781
3504.605902	523423.118758	43.293786
3504.481436	523406.051562	43.298791
3504.823447	523387.950113	43.303796
3504.607174	523426.101368	43.308801
3504.903837	523385.258213	43.313805
3504.553548	523410.135207	43.318810
3504.636252	523379.385909	43.323815
3504.517263	523350.235581	43.328820
3504.806295	523378.348093	43.333825
3504.870835	523318.988440	43.338829
3504.406234	523339.839340	43.343834
3504.831046	523316.113310	43.348839
3504.534037	523307.566241	43.353844
3504.430491	523299.797445	43.358849
3504.644412	523282.777745	43.363853
3504.693522	523270.131676	43.368858
3504.580544	523281.069144	43.373863
3504.094083	523247.376344	43.378868
3504.313660	523260.890050	43.383873
3504.607424	523247.143672	43.388877
3504.040618	523251.934797	43.393882
3504.838294	523222.689915	43.398887
3504.219593	523258.175271	43.403892
3504.634023	523240.719409	43.408897
3504.760832	523227.656597	43.413901
3504.297532	523221.309571	43.418906
3504.734563	523213.758618	43.423911
3504.544059	523206.559612	43.428916
3504.890047	523190.631124	43.433921
3504.708687	523181.560172	43.438925
3504.434372	523162.595361	43.443930
3504.552387	523189.976921	43.448935
3504.431306	523156.428399	43.453940
3504.553772	523166.974855	43.458945
3504.264282	523151.450087	43.463949
3504.751151	523144.700088	43.468954
3504.780545	523158.142831	43.473959
3504.531097	523108.437261	43.478964
3504.567897	523111.919731	43.483969
3504.588143	523129.762139	43.488973
3504.410787	523102.642748	43.493978
3504.825905	523067.745447	43.498983
3504.420606	523099.658631	43.503988
3504.456791	523063.709023	43.508993
3504.440839	523091.617464	43.513997
3504.544693	523059.094825	43.519002
3504.433702	523091.618714	43.524007
3504.267093	523033.710065	43.529012
3504.482685	523038.124823	43.534017
3504.563123	523046.756939	43.539021
3504.381872	523044.460154	43.544026
3504.541558	523026.993770	43.549031
3504.333910	523052.708188	43.554036
3504.480238	523024.576980	43.559041
3504.372054	523010.590604	43.564045
3504.472650	523012.647492	43.569050
3504.455921	522997.585011	43.574055
3504.313311	523014.947741	43.579060
3504.485254	522996.569410	43.584065
3504.254888	523013.187696	43.589069
3504.193008	522977.607277	43.594074
3504.262434	522977.697474	43.599079
3504.017413	522969.849771	43.604084
3503.989721	522972.028049	43.609089
3504.311967	522964.950114	43.614093
3504.442781	522984.291840	43.619098
3504.352354	522952.861336	43.624103
3504.009249	522999.021246	43.629108
3504.142143	522967.909356	43.634113
3504.218780	522993.022839	43.639117
3504.098028	522976.005158	43.644122
3504.320071	522988.305396	43.649127
3504.455048	522994.401202	43.654132
3504.655855	522958.779224	43.659137
3504.403616	522981.416979	43.664141
3504.289561	522949.838541	43.669146
3504.543295	522960.162167	43.674151
3504.703173	522948.711648	43.679156
3504.630858	522934.618429	43.684161
3504.414504	522932.529394	43.689165
3504.038718	522921.618508	43.694170
3504.191651	522911.230707	43.699175
3504.157187	522922.408780	43.704180
3504.260318	522895.396375	43.709185
3504.435890	522916.298303	43.714189
3504.248832	522897.572163	43.719194
3504.431708	522923.174509	43.724199
3504.230501	522887.413694	43.729204
3504.214884	522888.326208	43.734209
3504.481783	522891.317366	43.739213
3504.046955	522888.504535	43.744218
3504.360751	522874.046911	43.749223
3504.027793	522890.327654	43.754228
3504.608836	522877.748873	43.759233
3504.914324	522875.880682	43.764237
3504.353398	522866.717880	43.769242
3504.381495	522865.095749	43.774247
3504.371958	522851.750857	43.779252
3504.108438	522855.533621	43.784257
3504.182266	522863.459113	43.789261
3503.919809	522844.188726	43.794266
3504.181435	522855.168384	43.799271
3504.127000	522844.257211	43.804276
3504.127149	522860.384228	43.809281
3504.373603	522860.294782	43.814285
3504.062862	522847.958033	43.819290
3504.631079	522876.886721	43.824295
3504.624434	522841.499492	43.829300
3504.478147	522817.761888	43.834305
3504.601946	522814.304650	43.839309
3504.715062	522844.063648	43.844314
3504.642133	522827.746021	43.849319
3504.333318	522806.814606	43.854324
3504.142751	522771.961844	43.859329
3504.411743	522766.105560	43.864333
3504.026469	522803.627770	43.869338
3504.767394	522761.347851	43.874343
3504.491461	522795.920602	43.879348
3504.186485	522767.910833	43.884353
3504.574260	522732.814916	43.889357
3504.382813	522773.087096	43.894362
3504.697238	522736.233352	43.899367
3504.536964	522750.717512	43.904372
3504.395482	522744.926096	43.909377
3504.622859	522714.456006	43.914381
3504.361314	522710.200209	43.919386
3504.581206	522698.638919	43.924391
3504.057219	522724.959960	43.929396
3503.960090	522687.918377	43.934401
3504.443397	522729.449013	43.939405
3504.435066	522710.492190	43.944410
3504.708622	522665.555907	43.949415
3504.327171	522656.920729	43.954420
3504.286550	522703.286446	43.959425
3504.212804	522675.593859	43.964429
3504.218671	522674.227998	43.969434
3504.224743	522707.239707	43.974439
3503.765066	522696.038597	43.979444
3504.193049	522678.226103	43.984449
3504.831219	522657.296491	43.989453
3504.325743	522661.875872	43.994458
3504.442773	522678.136262	43.999463
3503.884903	522650.469592	44.004468
3504.529456	522625.545052	44.009473
3504.827754	522620.695195	44.014477
3504.503054	522623.830460	44.019482
3504.702801	522609.997294	44.024487
3504.315480	522620.978564	44.029492
3504.038264	522643.620737	44.034497
3504.147192	522590.166393	44.039501
3503.967773	522626.089253	44.044506
3503.909585	522620.234072	44.049511
3504.255489	522603.799469	44.054516
3504.081633	522613.634784	44.059521
3504.401004	522639.923781	44.064525
3503.992421	522611.222340	44.069530
3504.318968	522638.622427	44.074535
3504.093066	522629.558207	44.079540
3504.315665	522610.109769	44.084545
3504.615265	522615.269698	44.089549
3504.119633	522631.424744	44.094554
3504.627613	522601.516759	44.099559
3504.057547	522591.698024	44.104564
3504.130879	522571.363130	44.109569
3504.480110	522557.455737	44.114573
3503.866238	522620.949555	44.119578
3503.939644	522607.439687	44.124583
3504.430770	522577.837656	44.129588
3504.372363	522612.679751	44.134593
3504.039045	522585.988592	44.139597
3504.490352	522572.570635	44.144602
3504.507908	522584.397942	44.149607
3504.629206	522544.995953	44.154612
3504.245927	522585.804472	44.159617
3504.341637	522566.881593	44.164621
3504.543562	522567.405852	44.169626
3504.563557	522561.032737	44.174631
3504.683950	522538.769248	44.179636
3504.399656	522524.203618	44.184641
3504.588060	522550.260680	44.189645
3504.124283	522553.468496	44.194650
3504.639763	522505.257968	44.199655
3503.988255	522531.801698	44.204660
3503.819952	522497.905391	44.209665
3504.251228	522507.897908	44.214669
3504.307426	522487.666730	44.219674
3504.467564	522506.094384	44.224679
3504.232724	522493.543145	44.229684
3504.571702	522501.477462	44.234689
3504.512714	522496.835705	44.239693
3504.398282	522523.850678	44.244698
3504.717031	522491.798500	44.249703
3504.348276	522465.820527	44.254708
3504.118866	522477.838612	44.259713
3504.551750	522456.385073	44.264717
3504.220254	522474.233237	44.269722
3504.048591	522475.069324	44.274727
3504.580925	522475.743590	44.279732
3504.442365	522439.668554	44.284737
3504.580729	522453.246325	44.289741
3504.323416	522472.852226	44.294746
3504.243953	522437.425073	44.299751
3504.477090	522420.300322	44.304756
3504.103625	522443.716326	44.309761
3504.432402	522471.520790	44.314765
3503.847349	522437.740780	44.319770
3504.459844	522414.084887	44.324775
3504.832077	522396.230341	44.329780
3504.555671	522423.321637	44.334785
3504.240864	522401.379524	44.339789
3504.775731	522375.511371	44.344794
3504.743695	522401.300174	44.349799
3504.743277	522379.813905	44.354804
3504.848141	522377.926811	44.359809
3504.734590	522368.288569	44.364813
3505.017118	522313.541974	44.369818
3504.281375	522308.147663	44.374823
3504.242195	522347.284587	44.379828
3504.591008	522309.413317	44.384833
3504.397609	522338.766675	44.389837
3504.152466	522310.291654	44.394842
3504.894997	522261.791740	44.399847
3504.931494	522255.011444	44.404852
3504.588467	522266.997084	44.409857
3504.834751	522281.670187	44.414861
3504.325365	522271.993336	44.419866
3504.534329	522276.358794	44.424871
3504.533053	522273.831227	44.429876
3504.430544	522238.002830	44.434881
3505.014248	522190.488385	44.439885
3504.372749	522215.109886	44.444890
3504.206652	522212.557803	44.449895
3504.566860	522221.752821	44.454900
3504.122142	522244.017567	44.459905
3504.052242	522205.453883	44.464909
3504.389821	522162.528368	44.469914
3504.433158	522183.856591	44.474919
3504.194595	522178.838669	44.479924
3504.562640	522154.715468	44.484929
3504.532970	522191.424527	44.489933
3503.943253	522184.894845	44.494938
3504.464735	522143.355805	44.499943
3504.685693	522131.440047	44.504948
3504.557095	522167.305327	44.509953
3504.097165	522146.396945	44.514957
3504.408168	522128.602342	44.519962
3504.304477	522155.110657	44.524967
3504.403662	522128.400948	44.529972
3503.882048	522149.869063	44.534977
3504.114412	522137.698721	44.539981
3504.507254	522149.163688	44.544986
3504.566269	522113.309488	44.549991
3504.413193	522099.228310	44.554996
3504.244892	522126.505240	44.560001
3504.762630	522095.684761	44.565005
3504.339754	522097.470600	44.570010
3504.345268	522098.531490	44.575015
3504.516544	522067.917388	44.580020
3504.136044	522059.736757	44.585025
3504.149329	522064.790442	44.590029
3504.732435	522039.621936	44.595034
3504.531131	522078.431226	44.600039
3504.423743	522068.286261	44.605044
3504.302759	522038.375539	44.610049
3504.509407	522056.341335	44.615053
3504.116756	522031.883164	44.620058
3503.734550	522030.073010	44.625063
3504.717515	522007.672468	44.630068
3504.332188	521997.975847	44.635073
3504.471453	522034.152986	44.640077
3504.301679	522067.446569	44.645082
3504.307310	522055.716459	44.650087
3504.251297	522017.554594	44.655092
3504.548905	521979.690653	44.660097
3504.532133	521972.261411	44.665101
3504.508407	521972.214664	44.670106
3504.551107	521971.803517	44.675111
3504.310684	522000.507667	44.680116
3504.160485	522002.250420	44.685121
3504.578861	521983.225310	44.690125
3503.836710	521966.102555	44.695130
3504.428496	521949.223972	44.700135
3504.439069	521989.921174	44.705140
3504.166156	521958.113133	44.710145
3504.572552	521932.011797	44.715149
3504.596953	521980.138810	44.720154
3504.168714	521945.271285	44.725159
3504.164086	521909.982831	44.730164
3504.126505	521910.747198	44.735169
3504.444955	521952.305872	44.740173
3504.042868	521923.854981	44.745178
3504.456138	521937.794194	44.750183
3504.437640	521913.428384	44.755188
3503.858063	521945.775830	44.760193
3504.341429	521915.314347	44.765197
3504.139167	521961.252701	44.770202
3504.200410	521916.347911	44.775207
3504.045254	521926.231242	44.780212
3503.725248	521920.366632	44.785217
3504.126839	521913.528491	44.790221
3504.450211	521935.015011	44.795226
3504.775335	521905.286326	44.800231
3504.274938	521923.616805	44.805236
3503.984669	521895.400979	44.810241
3504.383549	521910.960338	44.815245
3504.287569	521887.314542	44.820250
3504.548672	521902.238434	44.825255
3504.510100	521871.707688	44.830260
3504.183966	521903.509583	44.835265
3504.300507	521847.978738	44.840269
3504.320182	521881.192200	44.845274
3504.548592	521850.416988	44.850279
3504.567373	521879.939867	44.855284
3503.981054	521860.062249	44.860289
3504.373397	521883.004115	44.865293
3504.164369	521845.219936	44.870298
3504.264532	521846.670346	44.875303
3503.922923	521845.157102	44.880308
3504.034906	521823.652336	44.885313
3504.156037	521834.958237	44.890317
3503.902679	521811.994459	44.895322
3504.147645	521851.997705	44.900327
3504.102390	521825.917024	44.905332
3504.536532	521822.107179	44.910337
3504.413253	521853.068182	44.915341
3504.445307	521831.576060	44.920346
3504.332573	521821.330670	44.925351
3504.394671	521859.643827	44.930356
3504.182320	521803.558117	44.935361
3504.282522	521801.166113	44.940365
3504.113479	521822.629491	44.945370
3504.360274	521778.503924	44.950375
3504.028823	521788.718550	44.955380
3504.163238	521815.847039	44.960385
3504.647162	521780.127183	44.965389
3504.131305	521829.452306	44.970394
3504.470179	521789.609642	44.975399
3503.914700	521806.887237	44.980404
3503.963493	521795.352350	44.985409
3504.671939	521794.077606	44.990413
3504.251974	521810.373176	44.995418
3504.386176	521760.248949	45.000423
3503.985549	521786.349770	45.005428
3503.897454	521756.433333	45.010433
3504.475372	521774.441877	45.015437
3503.803489	521772.576361	45.020442
3504.582183	521751.269476	45.025447
3504.133645	521766.710115	45.030452
3504.046235	521784.318221	45.035457
3504.151907	521762.915489	45.040461
3504.011975	521795.143188	45.045466
3504.108400	521765.045930	45.050471
3504.390743	521760.400574	45.055476
3503.921656	521801.932426	45.060481
3504.700206	521751.200753	45.065485
3504.126208	521782.030894	45.070490
3504.312609	521760.665958	45.075495
3504.764276	521714.536069	45.080500
3504.409998	521747.353882	45.085505
3504.525374	521741.521512	45.090509
3504.493967	521732.931634	45.095514
3504.255352	521704.656757	45.100519
3504.318011	521708.691582	45.105524
3503.963602	521691.254463	45.110529
3504.338979	521711.519657	45.115533
3504.128496	521716.305467	45.120538
3504.463837	521703.259036	45.125543
3504.279972	521713.753733	45.130548
3504.216369	521698.444667	45.135553
3504.477476	521722.823135	45.140557
3504.284696	521688.170638	45.145562
3504.185316	521667.154098	45.150567
3504.702534	521650.994813	45.155572
3504.394234	521694.877775	45.160577
3504.552851	521655.063273	45.165581
3504.578125	521672.855923	45.170586
3504.509553	521625.341812	45.175591
3505.009231	521638.913714	45.180596
3504.538993	521631.100960	45.185601
3504.645579	521611.467436	45.190605
3504.387551	521630.265522	45.195610
3504.611835	521596.911997	45.200615
3504.266340	521587.411069	45.205620
3504.092494	521589.663190	45.210625
3504.780513	521596.632727	45.215629
3504.620280	521592.765094	45.220634
3504.600408	521550.298936	45.225639
3504.452573	521552.243598	45.230644
3504.210544	521549.956205	45.235649
3504.537182	521545.050993	45.240653
3504.779279	521564.174581	45.245658
3504.605213	521519.457569	45.250663
3504.544332	521535.342746	45.255668
3504.257467	521527.197606	45.260673
3504.705548	521497.853220	45.265677
3504.313063	521535.581716	45.270682
3504.111614	521497.037151	45.275687
3504.269412	521484.321961	45.280692
3504.028113	521483.450096	45.285697
3504.192036	521472.806849	45.290701
3504.390890	521477.983064	45.295706
3504.191033	521480.542665	45.300711
3504.675442	521480.668402	45.305716
3504.156764	521485.705225	45.310721
3504.920211	521459.748941	45.315725
3504.811157	521474.832844	45.320730
3504.711581	521438.344961	45.325735
3504.622714	521474.559395	45.330740
3504.290824	521440.029477	45.335745
3504.649067	521435.169797	45.340749
3504.309810	521418.741175	45.345754
3504.339902	521395.175861	45.350759
3504.218583	521429.474270	45.355764
3504.230142	521405.608544	45.360769
3504.582113	521408.991007	45.365773
3504.692546	521401.187485	45.370778
3504.195635	521366.936291	45.375783
3504.484789	521386.659362	45.380788
3504.096210	521357.295280	45.385793
3504.352869	521394.719266	45.390797
3504.004048	521382.690779	45.395802
3504.276529	521356.407454	45.400807
3504.404577	521374.892016	45.405812
3504.346894	521389.715082	45.410817
3504.323322	521350.333109	45.415821
3504.276030	521353.829246	45.420826
3504.414621	521321.651571	45.425831
3503.996706	521361.963022	45.430836
3503.915238	521333.359309	45.435841
3504.561069	521333.611213	45.440845
3504.068495	521331.262269	45.445850
3504.418637	521344.352456	45.450855
3504.383822	521331.465352	45.455860
3504.132589	521350.060447	45.460865
3504.612567	521338.608769	45.465869
3504.240265	521302.871520	45.470874
3504.393430	521317.357970	45.475879
3504.655920	521291.076119	45.480884
3504.068113	521313.819780	45.485889
3504.448723	521293.990887	45.490893
3504.227015	521324.614530	45.495898
3504.282470	521274.602381	45.500903
3504.705430	521288.995655	45.505908
3504.100723	521310.225203	45.510913
3504.246588	521280.270918	45.515917
3504.093378	521255.672620	45.520922
3504.380319	521261.087781	45.525927
3504.229148	521280.071619	45.530932
3504.276141	521256.756232	45.535937
3504.171655	521280.687544	45.540941
3504.754540	521245.759838	45.545946
3504.304075	521245.831094	45.550951
3503.932949	521252.462580	45.555956
3504.133554	521218.404191	45.560961
3504.453043	521241.358473	45.565965
3504.781442	521214.863844	45.570970
3504.158932	521262.437935	45.575975
3504.348139	521222.314188	45.580980
3504.406867	521239.242505	45.585985
3504.544343	521206.862542	45.590989
3503.938307	521226.322812	45.595994
3504.462216	521187.410076	45.600999
3504.692612	521214.170473	45.606004
3504.040846	521212.099471	45.611009
3504.539920	521178.651105	45.616013
3504.018623	521224.237470	45.621018
3503.866654	521192.712183	45.626023
3504.404940	521222.204702	45.631028
3504.098949	521172.401046	45.636033
3504.372341	521198.345714	45.641037
3504.133353	521164.963410	45.646042
3504.647284	521165.135045	45.651047
3503.951032	521169.289949	45.656052
3504.149549	521152.270464	45.661057
3504.307812	521189.305991	45.666061
3504.490726	521160.609631	45.671066
3504.126069	521197.171627	45.676071
3503.703408	521177.823469	45.681076
3504.112084	521151.417170	45.686081
3504.152524	521184.072605	45.691085
3503.951684	521187.491925	45.696090
3504.411473	521156.173240	45.701095
3504.724249	521131.905588	45.706100
3504.298681	521118.220552	45.711105
3504.314763	521124.083049	45.716109
3504.503144	521164.046360	45.721114
3504.033355	521146.728016	45.726119
3504.413005	521122.045299	45.731124
3503.979490	521112.204085	45.736129
3504.416908	521122.348165	45.741133
3503.878642	521157.066964	45.746138
3503.981671	521132.731343	45.751143
3504.192487	521120.411972	45.756148
3504.256363	521111.250547	45.761153
3504.034470	521130.801897	45.766157
3504.279710	521090.921773	45.771162
3503.868292	521118.238808	45.776167
3504.072228	521108.145162	45.781172
3504.428571	521091.656833	45.786177
3504.413001	521106.372379	45.791181
3504.149597	521087.909028	45.796186
3504.119297	521109.806454	45.801191
3504.354061	521096.522636	45.806196
3504.400822	521121.492040	45.811201
3504.165494	521102.114185	45.816205
3504.186411	521115.155470	45.821210
3504.211610	521102.157579	45.826215
3504.350663	521073.063516	45.831220
3503.901512	521087.544244	45.836225
3504.112510	521088.825524	45.841229
3504.088066	521078.515154	45.846234
3503.877021	521092.351522	45.851239
3504.292508	521078.331283	45.856244
3504.037359	521087.725320	45.861249
3504.242561	521064.991379	45.866253
3504.360676	521077.713969	45.871258
3504.334909	521084.543740	45.876263
3504.296880	521072.111981	45.881268
3504.369264	521100.515468	45.886273
3504.450353	521070.318236	45.891277
3503.901972	521073.691388	45.896282
3504.385612	521037.767720	45.901287
3504.348011	521065.683046	45.906292
3503.773879	521050.049580	45.911297
3504.320617	521023.216771	45.916301
3504.126720	521064.049713	45.921306
3503.969693	521054.063644	45.926311
3504.550477	521021.057086	45.931316
3504.071268	521060.266635	45.936321
3504.027669	521053.751302	45.941325
3504.163310	521036.134911	45.946330
3504.179786	521057.165486	45.951335
3504.453009	521048.678784	45.956340
3503.825344	521067.485376	45.961345
3504.101650	521056.217372	45.966349
3504.418533	521060.414419	45.971354
3504.532868	521049.222571	45.976359
3504.441814	521016.221066	45.981364
3504.330367	521027.362042	45.986369
3504.684008	521002.986620	45.991373
3504.477807	521029.664641	45.996378
3504.283369	520991.218898	46.001383
3504.255478	521005.683679	46.006388
3503.825420	520988.712810	46.011393
3504.218453	520955.735795	46.016397
3504.099917	520975.726039	46.021402
3504.237048	521012.613624	46.026407
3504.319057	520992.376516	46.031412
3504.280933	520976.304340	46.036417
3504.538921	520954.320312	46.041421
3504.241725	520975.703932	46.046426
3504.025835	521013.911324	46.051431
3504.259953	520985.206564	46.056436
3504.166490	520972.884612	46.061441
3504.326133	520961.786665	46.066445
3504.065960	520967.440077	46.071450
3504.025326	520924.267728	46.076455
3504.239906	520972.468769	46.081460
3504.199555	520989.413003	46.086465
3504.283638	520974.231600	46.091469
3504.429011	520962.680863	46.096474
3503.929318	520955.984773	46.101479
3504.490365	520937.744873	46.106484
3504.462902	520931.378623	46.111489
3504.614752	520932.719825	46.116493
3504.564250	520920.896652	46.121498
3504.760581	520895.838083	46.126503
3504.482563	520944.926032	46.131508
3504.158889	520943.359307	46.136513
3504.536328	520904.367929	46.141517
3504.374414	520899.893667	46.146522
3504.159226	520887.843695	46.151527
3504.283372	520897.734062	46.156532
3504.391468	520881.487001	46.161537
3503.954448	520890.202043	46.166541
3504.696193	520866.220126	46.171546
3504.093720	520898.573254	46.176551
3504.283287	520874.931426	46.181556
3503.983803	520901.674960	46.186561
3504.260830	520875.440707	46.191565
3504.283456	520856.881327	46.196570
3503.954984	520869.522979	46.201575
3504.206975	520825.090658	46.206580
3504.179527	520867.262931	46.211585
3504.235750	520829.333362	46.216589
3504.024697	520861.473016	46.221594
3504.183896	520846.633550	46.226599
3504.184201	520856.846881	46.231604
3504.414385	520831.580620	46.236609
3504.099333	520857.315465	46.241613
3504.499942	520812.859623	46.246618
3504.155517	520873.637891	46.251623
3504.178842	520855.280643	46.256628
3504.219945	520865.487521	46.261633
3504.680094	520814.702155	46.266637
3504.124553	520841.536817	46.271642
3504.127495	520823.789487	46.276647
3504.204060	520826.305501	46.281652
3504.486707	520806.693747	46.286657
3504.104042	520824.501232	46.291661
3504.779967	520797.445393	46.296666
3504.119087	520835.672969	46.301671
3504.040456	520802.770192	46.306676
3504.395430	520776.371778	46.311681
3504.256779	520808.550654	46.316685
3504.067974	520767.878807	46.321690
3503.975305	520795.348245	46.326695
3504.386639	520761.761214	46.331700
3503.981823	520806.824716	46.336705
3503.884445	520772.054079	46.341709
3504.195878	520802.796678	46.346714
3503.671664	520792.261749	46.351719
3504.461674	520748.755412	46.356724
3504.416382	520798.413752	46.361729
3504.259921	520800.814916	46.366733
3504.343527	520781.942447	46.371738
3503.785423	520796.895702	46.376743
3504.561521	520771.947556	46.381748
3504.238780	520794.194991	46.386753
3503.749400	520759.890773	46.391757
3504.519996	520739.493962	46.396762
3503.936324	520771.743245	46.401767
3504.244764	520727.554545	46.406772
3504.461358	520763.873955	46.411777
3504.326067	520738.614753	46.416781
3504.065166	520728.341534	46.421786
3504.131614	520785.920384	46.426791
3504.315533	520789.127293	46.431796
3504.105988	520766.003438	46.436801
3504.227396	520733.372274	46.441805
3504.441472	520759.630380	46.446810
3503.940690	520733.771639	46.451815
3504.487265	520692.680011	46.456820
3504.395112	520684.048623	46.461825
3504.007143	520696.649249	46.466829
3504.298257	520742.411919	46.471834
3504.063375	520738.758127	46.476839
3504.030298	520721.977045	46.481844
3504.318533	520706.510322	46.486849
3504.208049	520743.943260	46.491853
3504.708542	520695.729777	46.496858
3504.329508	520725.064805	46.501863
3504.542455	520689.334842	46.506868
3504.172970	520701.679736	46.511873
3504.524674	520668.253622	46.516877
3504.449723	520707.349559	46.521882
3504.425045	520673.426768	46.526887
3504.350647	520697.809228	46.531892
3504.913107	520657.877916	46.536897
3504.346876	520660.546110	46.541901
3504.439825	520640.761894	46.546906
3504.519165	520647.271865	46.551911
3504.407362	520639.401983	46.556916
3504.584945	520636.441402	46.561921
3504.322970	520608.876186	46.566925
3504.541289	520614.201285	46.571930
3504.247058	520586.944501	46.576935
3504.296262	520615.150244	46.581940
3504.469053	520585.392683	46.586945
3503.928219	520622.742229	46.591949
3504.436252	520588.330573	46.596954
3504.275254	520596.344842	46.601959
3504.080132	520583.533047	46.606964
3504.145005	520552.680123	46.611969
3504.458481	520575.282356	46.616973
3504.360728	520558.106835	46.621978
3504.204301	520572.440627	46.626983
3504.451119	520571.794936	46.631988
3504.731865	520565.784327	46.636993
3504.300383	520543.403101	46.641997
3504.431798	520547.326222	46.647002
3504.205227	520517.833905	46.652007
3504.065497	520535.249373	46.657012
3504.651896	520523.375814	46.662017
3504.293552	520546.589887	46.667021
3504.578455	520520.404385	46.672026
3504.148274	520533.264618	46.677031
3504.774050	520488.216128	46.682036
3504.720095	520504.960764	46.687041
3504.489540	520478.351042	46.692045
3504.634166	520490.008094	46.697050
3504.609782	520460.685967	46.702055
3504.517501	520472.431036	46.707060
3504.505955	520443.207973	46.712065
3504.569113	520459.731896	46.717069
3504.495274	520429.659097	46.722074
3503.939166	520446.634844	46.727079
3504.208394	520400.681785	46.732084
3503.925385	520423.277378	46.737089
3504.292839	520391.213395	46.742093
3503.952056	520419.986735	46.747098
3504.020866	520395.149807	46.752103
3504.137312	520433.103773	46.757108
3504.209103	520408.165269	46.762113
3503.994869	520428.727490	46.767117
3504.840731	520421.060081	46.772122
3504.289250	520414.624764	46.777127
3504.235934	520426.616519	46.782132
3504.175664	520410.041666	46.787137
3504.337006	520434.842318	46.792141
3503.875420	520411.403862	46.797146
3503.873291	520436.028100	46.802151
3504.331621	520411.331882	46.807156
3504.007208	520438.636294	46.812161
3504.012454	520393.432809	46.817165
3504.143573	520406.002178	46.822170
3504.186393	520390.270571	46.827175
3504.185914	520378.337976	46.832180
3504.532123	520392.339672	46.837185
3504.128056	520378.246118	46.842189
3504.472487	520389.264913	46.847194
3504.487332	520374.296149	46.852199
3504.404485	520403.281563	46.857204
3504.471138	520384.866379	46.862209
3504.475711	520368.432923	46.867213
3504.430375	520377.794204	46.872218
3504.235048	520357.094522	46.877223
3503.991530	520372.200691	46.882228
3504.536907	520342.383803	46.887233
3504.112734	520392.811127	46.892237
3503.974369	520374.731709	46.897242
3504.336058	520345.095545	46.902247
3504.358582	520375.884605	46.907252
3504.406759	520328.702221	46.912257
3504.073808	520341.193298	46.917261
3504.544777	520292.932738	46.922266
3504.067883	520343.773046	46.927271
3504.079133	520315.961906	46.932276
3504.543684	520295.714042	46.937281
3504.460231	520341.385342	46.942285
3504.739851	520306.806949	46.947290
3504.347518	520319.711929	46.952295
3504.622953	520289.583671	46.957300
3504.367259	520295.388293	46.962305
3504.342362	520275.672826	46.967309
3504.443211	520286.173997	46.972314
3504.285498	520291.103568	46.977319
3504.069912	520266.412520	46.982324
3504.513799	520257.291684	46.987329
3503.920000	520256.323776	46.992333
3504.216420	520234.130460	46.997338
3503.956775	520256.014709	47.002343
3504.394066	520236.074457	47.007348
3504.065679	520235.974731	47.012353
3503.973177	520263.192218	47.017357
3504.356319	520218.080212	47.022362
3504.246510	520272.149315	47.027367
3504.206970	520257.593542	47.032372
3504.433669	520235.714625	47.037377
3504.165419	520265.589153	47.042381
3504.387902	520233.699465	47.047386
3504.440458	520210.786217	47.052391
3504.276370	520225.374336	47.057396
3504.074053	520226.619884	47.062401
3504.201850	520220.886137	47.067405
3504.155468	520216.696806	47.072410
3504.434630	520199.208523	47.077415
3504.786561	520194.450602	47.082420
3504.412698	520193.245677	47.087425
3504.335105	520216.163029	47.092429
3504.455519	520191.974956	47.097434
3504.115111	520167.202361	47.102439
3504.443758	520164.925703	47.107444
3504.289644	520180.169607	47.112449
3504.181168	520186.810571	47.117453
3504.213774	520175.833297	47.122458
3504.348252	520156.193624	47.127463
3504.050521	520191.634889	47.132468
3504.046609	520146.432172	47.137473
3504.005592	520175.107999	47.142477
3504.248042	520130.624747	47.147482
3504.092619	520152.897166	47.152487
3504.015090	520130.307745	47.157492
3504.062959	520124.586597	47.162497
3504.274487	520174.256796	47.167501
3504.076180	520141.674989	47.172506
3504.346915	520113.620242	47.177511
3504.395564	520156.540760	47.182516
3504.102187	520151.328624	47.187521
3504.400372	520128.983198	47.192525
3504.249485	520158.889935	47.197530
3504.168141	520149.649800	47.202535
3503.972972	520147.000860	47.207540
3504.336746	520138.802758	47.212545
3503.883018	520129.318087	47.217549
3504.370687	520128.280372	47.222554
3504.246245	520109.288323	47.227559
3504.223465	520100.241158	47.232564
3504.312716	520104.980062	47.237569
3503.978096	520085.313318	47.242573
3504.381854	520097.890396	47.247578
3504.222455	520106.005776	47.252583
3504.381388	520114.273093	47.257588
3504.601583	520087.743187	47.262593
3503.774597	520119.071500	47.267597
3504.616523	520078.892363	47.272602
3504.572588	520098.113433	47.277607
3504.296984	520065.341439	47.282612
3503.908687	520074.655970	47.287617
3504.216294	520066.416145	47.292621
3504.094009	520064.969195	47.297626
3504.079628	520074.730262	47.302631
3504.309657	520064.834107	47.307636
3504.502684	520079.467040	47.312641
3503.666216	520069.031560	47.317645
3504.281237	520033.337751	47.322650
3503.899943	520095.742753	47.327655
3503.979911	520070.397939	47.332660
3504.381846	520076.907713	47.337665
3504.180724	520080.125053	47.342669
3504.803362	520041.092876	47.347674
3504.095532	520062.795399	47.352679
3503.925235	520041.383476	47.357684
3504.558856	520017.872488	47.362689
3504.028986	520061.946522	47.367693
3504.529827	520049.782765	47.372698
3504.020665	520028.424383	47.377703
3504.277283	520032.479530	47.382708
3504.120842	520032.959388	47.387713
3504.325437	520016.190585	47.392717
3504.142941	520048.580132	47.397722
3503.832514	520018.746228	47.402727
3503.878086	520035.425048	47.407732
3504.352009	520040.709935	47.412737
3503.907891	520029.909037	47.417741
3504.268250	519998.502737	47.422746
3503.822653	520021.478523	47.427751
3503.927595	520010.641398	47.432756
3504.187628	520001.953988	47.437761
3504.353517	520001.573885	47.442765
3504.547851	520022.425984	47.447770
3504.084880	520013.701160	47.452775
3504.174084	519980.669085	47.457780
3504.161578	520018.492698	47.462785
3503.968248	519987.831214	47.467789
3504.305066	520035.611175	47.472794
3504.176357	520019.299562	47.477799
3504.392303	519994.792720	47.482804
3504.208096	520036.081756	47.487809
3504.009541	520013.966374	47.492813
3504.449063	520006.413560	47.497818
3504.170731	519983.451166	47.502823
3504.306833	519980.901533	47.507828
3504.566427	519953.960676	47.512833
3504.388848	519982.051657	47.517837
3504.559112	519949.815726	47.522842
3504.490530	519971.063391	47.527847
3504.749723	519956.712956	47.532852
3504.350017	519932.859526	47.537857
3504.117868	519951.554313	47.542861
3504.588530	519931.507292	47.547866
3503.962963	519928.218448	47.552871
3504.021358	519932.406077	47.557876
3504.191847	519940.823346	47.562881
3504.306681	519940.855822	47.567885
3504.263587	519931.053317	47.572890
3504.376238	519944.485542	47.577895
3504.208667	519902.544103	47.582900
3504.614887	519905.716051	47.587905
3504.022485	519906.416507	47.592909
3504.319518	519898.431090	47.597914
3503.867357	519899.817277	47.602919
3504.449002	519868.021807	47.607924
3504.737743	519906.657653	47.612929
3504.451381	519909.736806	47.617933
3504.545445	519855.466869	47.622938
3504.377864	519855.796800	47.627943
3504.338728	519872.792557	47.632948
3504.153791	519842.028347	47.637953
3503.782412	519886.886825	47.642957
3503.925372	519862.593577	47.647962
3504.381410	519856.504442	47.652967
3503.874479	519871.501009	47.657972
3504.099898	519859.127823	47.662977
3504.151620	519872.165225	47.667981
3504.550769	519835.594956	47.672986
3504.377330	519845.431863	47.677991
3504.035731	519862.829383	47.682996
3504.054299	519817.622210	47.688001
3504.066164	519825.457839	47.693005
3504.091312	519813.166835	47.698010
3504.109516	519801.938769	47.703015
3504.112133	519849.013629	47.708020
3504.058657	519809.531559	47.713025
3504.194352	519835.348453	47.718029
3504.349281	519813.733139	47.723034
3504.129860	519840.263485	47.728039
3504.511566	519809.308528	47.733044
3504.233365	519823.358833	47.738049
3503.791238	519853.059334	47.743053
3504.264977	519823.303395	47.748058
3504.369647	519851.349989	47.753063
3504.410191	519809.425984	47.758068
3504.695272	519810.088887	47.763073
3504.024780	519829.459862	47.768077
3504.361654	519779.398684	47.773082
3504.293029	519819.001375	47.778087
3503.976935	519816.674879	47.783092
3504.477026	519781.049254	47.788097
3504.127280	519824.033605	47.793101
3503.877041	519835.450145	47.798106
3504.139101	519829.998427	47.803111
3503.826383	519808.052504	47.808116
3504.405539	519781.920451	47.813121
3504.037171	519829.155130	47.818125
3504.176353	519826.352166	47.823130
3504.047122	519803.264826	47.828135
3504.180150	519807.895769	47.833140
3504.517734	519762.435768	47.838145
3504.218496	519779.978373	47.843149
3504.091756	519737.979497	47.848154
3504.246773	519771.732046	47.853159
3504.226027	519748.880305	47.858164
3504.292565	519764.696491	47.863169
3503.979890	519759.082765	47.868173
3504.329059	519762.921094	47.873178
3504.003143	519759.079212	47.878183
3504.251692	519781.035464	47.883188
3504.545705	519742.307341	47.888193
3504.257816	519777.343426	47.893197
3504.066910	519717.151486	47.898202
3504.193269	519738.823719	47.903207
3504.046700	519706.687953	47.908212
3504.058941	519742.334015	47.913217
3504.153823	519720.879764	47.918221
3504.169365	519719.360435	47.923226
3504.178864	519740.242105	47.928231
3504.186574	519719.054450	47.933236
3504.374763	519727.772418	47.938241
3504.456129	519714.815118	47.943245
3504.141908	519753.799443	47.948250
3504.104024	519721.595964	47.953255
3504.136972	519739.743448	47.958260
3504.584791	519705.743983	47.963265
3503.969523	519720.909503	47.968269
3504.559201	519684.511044	47.973274
3504.401693	519709.312620	47.978279
3504.144777	519685.436264	47.983284
3504.006750	519700.273552	47.988289
3504.379557	519673.971683	47.993293
3504.234271	519699.175859	47.998298
3504.287619	519681.368766	48.003303
3504.119223	519705.009084	48.008308
3504.484615	519671.022575	48.013313
3504.280933	519694.516791	48.018317
3504.061191	519666.033158	48.023322
3504.405643	519637.915386	48.028327
3504.236858	519665.297611	48.033332
3504.251037	519662.059294	48.038337
3504.302283	519670.141596	48.043341
3504.329935	519676.761250	48.048346
3504.354679	519644.901675	48.053351
3504.035689	519676.605619	48.058356
3504.177430	519666.773744	48.063361
3504.371462	519630.690522	48.068365
3504.195140	519641.741559	48.073370
3504.230443	519643.708064	48.078375
3504.051799	519613.498644	48.083380
3504.377666	519621.739825	48.088385
3504.085373	519615.516051	48.093389
3504.335644	519632.971962	48.098394
3504.555522	519630.257341	48.103399
3503.952509	519611.087532	48.108404
3504.268055	519640.011323	48.113409
3504.275243	519622.767674	48.118413
3504.478469	519620.055683	48.123418
3504.260391	519615.539382	48.128423
3504.194339	519602.049080	48.133428
3504.308352	519594.496961	48.138433
3504.225477	519595.774241	48.143437
3504.312665	519598.592153	48.148442
3504.411621	519593.671785	48.153447
3504.542382	519588.493564	48.158452
3504.712627	519580.881986	48.163457
3504.495646	519554.521449	48.168461
3504.262138	519556.985534	48.173466
3504.370275	519547.613984	48.178471
3504.147059	519537.637453	48.183476
3504.780582	519547.700952	48.188481
3504.283332	519545.504178	48.193485
3504.282355	519533.065400	48.198490
3504.549576	519516.640147	48.203495
3504.359778	519508.377530	48.208500
3504.323290	519501.809892	48.213505
3504.222933	519513.809747	48.218509
3504.199973	519513.864001	48.223514
3504.443059	519513.825643	48.228519
3504.168152	519495.766840	48.233524
3504.580257	519493.173510	48.238529
3504.426188	519454.111009	48.243533
3504.420845	519477.928143	48.248538
3504.375912	519461.451041	48.253543
3504.221463	519478.465429	48.258548
3504.446055	519474.283646	48.263553
3504.065700	519462.107036	48.268557
3504.435403	519475.195626	48.273562
3504.505709	519441.154152	48.278567
3504.452887	519445.460613	48.283572
3504.314319	519419.491989	48.288577
3504.462673	519442.526401	48.293581
3504.543207	519417.585016	48.298586
3504.092900	519438.236348	48.303591
3503.832254	519404.247106	48.308596
3504.365939	519397.184787	48.313601
3504.406658	519407.342065	48.318605
3504.335655	519398.201005	48.323610
3504.424615	519373.106524	48.328615
3503.695793	519427.883017	48.333620
3503.956678	519405.289681	48.338625
3504.097346	519376.900281	48.343629
3504.276235	519425.566586	48.348634
3503.978422	519403.112114	48.353639
3504.056386	519382.064619	48.358644
3504.288666	519392.090499	48.363649
3504.069701	519425.498342	48.368653
3504.062318	519397.536900	48.373658
3504.351037	519392.687611	48.378663
3503.993599	519412.009595	48.383668
3504.166768	519386.092779	48.388673
3504.028940	519412.610917	48.393677
3504.284347	519402.103569	48.398682
3504.290197	519377.426754	48.403687
3504.086357	519384.133678	48.408692
3504.028924	519352.539355	48.413697
3503.926893	519348.156335	48.418701
3504.391542	519385.147502	48.423706
3504.447827	519352.169937	48.428711
3504.347214	519367.709528	48.433716
3503.908037	519361.407742	48.438721
3504.413773	519348.130255	48.443725
3504.327861	519388.697456	48.448730
3504.106828	519366.584758	48.453735
3503.800823	519378.617213	48.458740
3503.894940	519379.765406	48.463745
3503.950696	519366.508487	48.468749
3504.012539	519369.886665	48.473754
3503.911007	519376.729119	48.478759
3503.983576	519355.025091	48.483764
3504.176467	519393.828985	48.488769
3504.140050	519361.927965	48.493773
3504.434690	519372.702484	48.498778
3503.832688	519369.662629	48.503783
3504.420849	519345.652216	48.508788
3504.423884	519367.496126	48.513793
3504.432056	519361.376463	48.518797
3503.919601	519315.999017	48.523802
3504.148869	519336.897028	48.528807
3504.085152	519321.130674	48.533812
3504.363462	519340.251131	48.538817
3504.107823	519332.099963	48.543821
3504.210561	519313.880142	48.548826
3503.868227	519367.078780	48.553831
3504.000964	519353.860250	48.558836
3504.630977	519314.370101	48.563841
3504.199802	519347.659944	48.568845
3503.892711	519337.999942	48.573850
3504.521661	519308.319676	48.578855
3504.307616	519324.180631	48.583860
3504.169513	519310.752044	48.588865
3504.374883	519275.778700	48.593869
3504.334735	519301.877050	48.598874
3504.501951	519281.826637	48.603879
3504.235477	519303.966055	48.608884
3504.397031	519272.943758	48.613889
3504.076465	519312.081825	48.618893
3504.031001	519283.165460	48.623898
3504.292882	519309.519457	48.628903
3503.945778	519264.621392	48.633908
3504.226651	519272.920426	48.638913
3504.203844	519248.146815	48.643917
3504.163737	519269.138054	48.648922
3504.296555	519245.705121	48.653927
3504.068934	519265.107891	48.658932
3504.249410	519253.348146	48.663937
3504.282948	519266.186637	48.668941
3504.286825	519259.005733	48.673946
3504.265330	519271.347260	48.678951
3504.165614	519265.345746	48.683956
3504.131077	519257.715820	48.688961
3504.303093	519246.159669	48.693965
3504.334453	519279.325980	48.698970
3503.892167	519258.815646	48.703975
3504.026464	519225.572668	48.708980
3504.093127	519258.227782	48.713985
3503.798368	519242.497868	48.718989
3503.839734	519220.141238	48.723994
3504.031375	519258.945647	48.728999
3504.082559	519240.632762	48.734004
3504.318799	519253.489793	48.739009
3503.994068	519248.484588	48.744013
3504.350620	519224.106077	48.749018
3504.239344	519244.451237	48.754023
3504.050976	519260.510458	48.759028
3504.428806	519227.228993	48.764033
3504.333079	519261.224482	48.769037
3503.823733	519254.023558	48.774042
3504.497409	519235.410019	48.779047
3504.419334	519257.165762	48.784052
3504.273030	519249.856893	48.789057
3504.088563	519217.119372	48.794061
3504.250072	519228.420687	48.799066
3504.459965	519185.962673	48.804071
3504.145990	519215.745196	48.809076
3504.449539	519180.857266	48.814081
3504.128135	519223.788134	48.819085
3504.252041	519191.153521	48.824090
3504.479103	519205.933550	48.829095
3504.302250	519216.529861	48.834100
3504.272278	519160.355733	48.839105
3503.758320	519210.598596	48.844109
3503.690797	519179.157233	48.849114
3504.339423	519164.441164	48.854119
3503.508290	519221.611119	48.859124
3503.995679	519181.890366	48.864129
3504.035667	519225.320338	48.869133
3503.984963	519227.047656	48.874138
3504.136170	519188.998165	48.879143
3504.164305	519218.220952	48.884148
3504.236264	519215.731906	48.889153
3504.112687	519187.232246	48.894157
3503.966099	519169.001105	48.899162
3504.231505	519174.875457	48.904167
3504.067816	519179.401775	48.909172
3504.057599	519165.194365	48.914177
3504.101035	519173.126447	48.919181
3503.954497	519188.875729	48.924186
3504.434112	519171.658074	48.929191
3504.274098	519190.797416	48.934196
3504.387914	519169.036058	48.939201
3504.255142	519188.525060	48.944205
3504.041075	519174.147613	48.949210
3504.491688	519187.628173	48.954215
3504.039674	519169.243041	48.959220
3504.320756	519193.622108	48.964225
3504.017585	519179.916108	48.969229
3504.168196	519138.984326	48.974234
3503.929967	519170.676476	48.979239
3504.293626	519126.070228	48.984244
3504.490081	519152.535949	48.989249
3504.364976	519121.305842	48.994253
3504.132787	519155.828778	48.999258
3504.402620	519118.417735	49.004263
3504.145543	519148.393652	49.009268
3504.393256	519138.190751	49.014273
3504.459179	519153.046861	49.019277
3504.017533	519115.798828	49.024282
3504.423291	519114.622300	49.029287
3504.227464	519118.648050	49.034292
3504.254340	519098.063365	49.039297
3503.865852	519102.625233	49.044301
3503.770102	519118.366556	49.049306
3504.152006	519111.075274	49.054311
3503.631224	519102.915331	49.059316
3503.955865	519116.163028	49.064321
3504.284506	519105.694484	49.069325
3504.101232	519100.161213	49.074330
3504.052939	519115.895037	49.079335
3504.254838	519108.885035	49.084340
3504.176891	519111.526865	49.089345
3504.175507	519080.782790	49.094349
3504.146095	519120.886622	49.099354
3503.872840	519123.660451	49.104359
3503.986389	519102.303578	49.109364
3504.059272	519128.687735	49.114369
3504.010763	519121.413918	49.119373
3504.087228	519112.097693	49.124378
3503.960937	519128.703460	49.129383
3503.954590	519121.878076	49.134388
3504.208637	519107.123187	49.139393
3504.276259	519120.664334	49.144397
3504.297864	519129.510080	49.149402
3504.188681	519107.581622	49.154407
3504.356107	519114.331109	49.159412
3504.326757	519100.733464	49.164417
3504.435378	519079.276208	49.169421
3504.102015	519078.519894	49.174426
3504.467016	519061.522505	49.179431
3503.874493	519101.513118	49.184436
3504.236549	519059.334128	49.189441
3503.956278	519088.504755	49.194445
3503.932215	519058.067621	49.199450
3504.177958	519096.257064	49.204455
3504.134172	519070.475175	49.209460
3504.415824	519080.746274	49.214465
3504.197355	519093.220199	49.219469
3504.426130	519052.427548	49.224474
3504.671672	519034.791648	49.229479
3504.116788	519036.042439	49.234484
3504.421105	519045.399780	49.239489
3504.295591	519031.817277	49.244493
3504.056692	519055.065135	49.249498
3503.986847	519017.050185	49.254503
3504.066531	519015.470087	49.259508
3503.876604	519050.289963	49.264513
3503.865688	519025.160174	49.269517
3504.096850	519036.248345	49.274522
3503.964010	519022.414160	49.279527
3504.023972	519048.193689	49.284532
3504.011629	519064.326412	49.289537
3503.925857	519043.506631	49.294541
3504.203716	519017.269292	49.299546
3504.337213	519053.352776	49.304551
3504.158283	519049.436929	49.309556
3504.509312	519022.075570	49.314561
3504.190525	519062.933210	49.319565
3504.555995	519009.274959	49.324570
3504.491574	519031.787340	49.329575
3503.895115	519019.088325	49.334580
3504.603530	518986.310360	49.339585
3504.240811	519030.664126	49.344589
3504.326587	519019.222580	49.349594
3504.019312	519022.456902	49.354599
3503.866620	518988.247474	49.359604
3504.135704	519018.191034	49.364609
3504.110834	518992.760001	49.369613
3503.963303	519038.394469	49.374618
3503.946750	519007.298690	49.379623
3504.268581	518984.442313	49.384628
3504.395818	518997.215638	49.389633
3504.378441	519017.192270	49.394637
3503.644104	518983.833261	49.399642
3504.327158	518951.008668	49.404647
3504.291449	519003.806044	49.409652
3504.244601	518988.340106	49.414657
3504.383310	518956.612892	49.419661
3504.093670	519004.393720	49.424666
3504.196032	518958.361884	49.429671
3504.312230	519016.242458	49.434676
3503.864708	518978.438810	49.439681
3504.169278	518996.240781	49.444685
3504.038176	518989.232793	49.449690
3504.268801	518980.954030	49.454695
3503.845831	518994.876218	49.459700
3504.248282	518965.281703	49.464705
3503.993102	519008.152096	49.469709
3504.062598	518970.924083	49.474714
3504.191244	518976.516721	49.479719
3503.982133	519012.654443	49.484724
3504.405240	518955.548378	49.489729
3504.340863	518981.145396	49.494733
3503.999807	518935.284712	49.499738
3504.267536	518913.043590	49.504743
3503.824967	518949.724018	49.509748
3504.213889	518960.180505	49.514753
3504.049657	518937.148051	49.519757
3504.424424	518914.182078	49.524762
3504.282518	518927.958766	49.529767
3503.939106	518978.377645	49.534772
3503.790615	518975.013204	49.539777
3504.264622	518977.011585	49.544781
3503.966564	518974.479850	49.549786
3503.800281	518953.925514	49.554791
3504.126689	518932.332513	49.559796
3504.109025	518921.210650	49.564801
3504.217527	518957.955663	49.569805
3503.760670	518972.136060	49.574810
3504.260672	518927.811129	49.579815
3504.396815	518942.858598	49.584820
3503.868074	518990.272722	49.589825
3504.243183	518972.464577	49.594829
3503.799826	518956.100509	49.599834
3504.658365	518917.230663	49.604839
3504.246762	518934.741356	49.609844
3504.097199	518935.523558	49.614849
3504.232899	518900.155897	49.619853
3503.938889	518941.313323	49.624858
3503.993141	518898.171233	49.629863
3503.891661	518937.730663	49.634868
3503.953196	518923.916241	49.639873
3504.654495	518894.982304	49.644877
3503.792837	518930.919938	49.649882
3504.361336	518903.271176	49.654887
3504.119618	518940.880651	49.659892
3503.695189	518917.282492	49.664897
3503.933546	518915.576172	49.669901
3503.982927	518901.257983	49.674906
3504.054981	518935.834426	49.679911
3504.000859	518918.144630	49.684916
3503.858946	518914.273467	49.689921
3504.170547	518928.989816	49.694925
3504.059107	518913.635151	49.699930
3504.234255	518934.542225	49.704935
3504.204764	518903.498862	49.709940
3504.495262	518933.793159	49.714945
3504.530684	518910.981948	49.719949
3504.044693	518932.094653	49.724954
3504.324310	518888.057282	49.729959
3504.068586	518904.633164	49.734964
3504.535197	518863.600190	49.739969
3504.297056	518892.005999	49.744973
3504.216115	518880.894110	49.749978
3503.808231	518906.646668	49.754983
3504.043980	518889.972934	49.759988
3504.275250	518895.852781	49.764993
3504.199755	518861.984860	49.769997
3503.952833	518916.939713	49.775002
3504.102029	518886.980550	49.780007
3504.271093	518867.283311	49.785012
3504.128668	518917.164941	49.790017
3504.115229	518875.044828	49.795021
3504.146557	518884.293705	49.800026
3504.284383	518886.699199	49.805031
3504.226714	518857.986287	49.810036
3504.439762	518867.509855	49.815041
3504.416248	518836.869959	49.820045
3503.809565	518859.215444	49.825050
3504.249653	518849.538198	49.830055
3504.208192	518850.505587	49.835060
3504.066398	518867.265768	49.840065
3504.383971	518830.048797	49.845069
3504.133224	518869.985950	49.850074
3504.491091	518846.769719	49.855079
3504.062102	518865.395710	49.860084
3504.230283	518857.126754	49.865089
3504.140197	518814.462363	49.870093
3504.163220	518832.511278	49.875098
3504.471837	518804.448322	49.880103
3504.360271	518806.943811	49.885108
3504.150193	518797.874967	49.890113
3504.309246	518825.510171	49.895117
3504.128152	518798.384245	49.900122
3504.136761	518834.487946	49.905127
3503.969551	518810.292741	49.910132
3504.236951	518830.174023	49.915137
3504.254391	518794.875395	49.920141
3504.129149	518834.489393	49.925146
3504.394514	518800.061801	49.930151
3503.731875	518815.741306	49.935156
3503.886042	518768.790545	49.940161
3504.002945	518799.112526	49.945165
3504.126191	518807.841245	49.950170
3504.414667	518797.682259	49.955175
3504.193043	518792.862887	49.960180
3504.415592	518784.838139	49.965185
3504.566781	518770.149775	49.970189
3504.041628	518790.055233	49.975194
3504.450667	518776.337467	49.980199
3504.553143	518777.433813	49.985204
3504.354347	518773.976146	49.990209
3503.892194	518755.187616	49.995213
3503.846810	518752.009103	50.000218
3503.959371	518746.024416	50.005223
3503.662551	518751.077566	50.010228
3503.970589	518776.868877	50.015233
3504.058646	518787.828131	50.020237
3504.100109	518790.552274	50.025242
3504.297581	518781.419007	50.030247
3504.222537	518768.940792	50.035252
3503.952160	518774.293160	50.040257
3504.102656	518743.625589	50.045261
3503.985050	518754.010561	50.050266
3504.131341	518752.419911	50.055271
3504.145227	518755.300120	50.060276
3504.069919	518752.682578	50.065281
3504.197872	518754.280574	50.070285
3503.621121	518748.303699	50.075290
3503.693272	518750.567891	50.080295
3503.919998	518755.133753	50.085300
3503.954842	518751.487453	50.090305
3504.163261	518760.455573	50.095309
3504.014668	518758.506990	50.100314
3504.330336	518748.141406	50.105319
3504.572080	518731.213728	50.110324
3504.244816	518772.933070	50.115329
3504.573849	518733.489107	50.120333
3504.003039	518762.655660	50.125338
3504.413337	518753.337039	50.130343
3504.292238	518738.742249	50.135348
3504.351327	518757.645192	50.140353
3504.391145	518723.758762	50.145357
3504.018519	518744.651518	50.150362
3504.042264	518725.027645	50.155367
3503.923489	518726.462369	50.160372
3503.993349	518735.351266	50.165377
3504.347411	518728.620460	50.170381
3503.885094	518719.540871	50.175386
3504.153970	518732.140312	50.180391
3504.336097	518729.229241	50.185396
3504.183858	518715.145027	50.190401
3504.296118	518721.599989	50.195405
3504.198979	518730.616418	50.200410
3504.189426	518717.925545	50.205415
3504.095902	518725.879487	50.210420
3503.977318	518733.331712	50.215425
3504.482220	518720.053855	50.220429
3503.879064	518699.214278	50.225434
3504.166718	518714.895387	50.230439
3504.340108	518674.767938	50.235444
3504.205427	518712.917257	50.240449
3504.468698	518664.634201	50.245453
3504.023676	518693.679860	50.250458
3504.328270	518683.063147	50.255463
3504.264748	518682.769842	50.260468
3504.038355	518694.638507	50.265473
3504.488941	518691.128756	50.270477
3503.674466	518688.375191	50.275482
3504.148204	518702.762710	50.280487
3504.223396	518687.176067	50.285492
3503.846023	518709.586646	50.290497
3504.236399	518670.537378	50.295501
3503.867624	518711.454353	50.300506
3504.178658	518681.620943	50.305511
3504.032612	518702.933049	50.310516
3503.985437	518682.915794	50.315521
3504.103576	518688.661893	50.320525
3504.231587	518661.790295	50.325530
3504.023812	518694.641600	50.330535
3503.766354	518668.437747	50.335540
3504.299290	518659.352528	50.340545
3504.190122	518672.719713	50.345549
3504.021488	518643.113747	50.350554
3503.929823	518666.541151	50.355559
3504.261498	518652.734375	50.360564
3503.933806	518657.893567	50.365569
3504.443606	518664.943100	50.370573
3504.413253	518654.126469	50.375578
3504.272916	518642.821537	50.380583
3504.432246	518674.451802	50.385588
3504.251931	518638.577283	50.390593
3504.070770	518679.666956	50.395597
3503.766379	518658.982378	50.400602
3504.100791	518663.733517	50.405607
3504.313999	518666.076562	50.410612
3503.760486	518665.253888	50.415617
3504.254370	518669.929252	50.420621
3504.276404	518669.925831	50.425626
3504.330546	518655.960651	50.430631
3504.317931	518630.881099	50.435636
3504.166484	518621.904026	50.440641
3504.315578	518628.049796	50.445645
3504.142974	518636.623094	50.450650
3504.370758	518635.171256	50.455655
3504.294333	518621.631225	50.460660
3503.895171	518638.584018	50.465665
3504.304196	518622.995120	50.470669
3504.130543	518620.544803	50.475674
3504.137489	518632.680040	50.480679
3503.976428	518604.842682	50.485684
3504.087101	518637.036955	50.490689
3504.541116	518601.213804	50.495693
3503.592139	518591.604246	50.500698
3504.068627	518603.715861	50.505703
3504.111243	518569.373563	50.510708
3503.834962	518603.854050	50.515713
3504.580130	518579.716578	50.520717
3504.144457	518592.073505	50.525722
3504.135512	518585.400014	50.530727
3503.993158	518575.258416	50.535732
3503.848725	518575.837553	50.540737
3503.991680	518532.629924	50.545741
3503.925741	518511.401793	50.550746
3503.372187	518427.394282	50.555751
3503.864466	518402.335722	50.560756
3503.676034	518306.234584	50.565761
3503.599872	518239.950873	50.570765
3503.549694	518146.911669	50.575770
3503.540199	518041.425398	50.580775
3503.212326	517936.494475	50.585780
3502.865391	517829.543093	50.590785
3503.222914	517668.723087	50.595789
3502.929848	517561.508612	50.600794
3502.664930	517407.864408	50.605799
3502.245068	517236.087922	50.610804
3501.979881	517086.638274	50.615809
3501.866784	516929.375013	50.620813
3501.583444	516741.843653	50.625818
3501.367647	516562.340793	50.630823
3500.957723	516367.947164	50.635828
3500.455556	516184.034929	50.640833
3500.719054	515971.424316	50.645837
3500.192847	515767.179789	50.650842
3499.715519	515550.685384	50.655847
3499.825283	515318.112804	50.660852
3499.294048	515100.053194	50.665857
3499.045939	514857.263361	50.670861
3498.357167	514616.815773	50.675866
3498.298491	514380.261034	50.680871
3497.663833	514127.203318	50.685876
3497.663096	513877.278872	50.690881
3497.395734	513599.976912	50.695885
3496.926068	513325.231575	50.700890
3496.516932	513050.219290	50.705895
3496.461244	512763.107340	50.710900
3496.062052	512472.402612	50.715905
3495.585616	512168.198330	50.720909
3494.472731	511874.813894	50.725914
3494.352891	511587.793428	50.730919
3494.126618	511260.869537	50.735924
3493.646571	510951.433361	50.740929
3493.222806	510634.292743	50.745933
3492.574919	510319.357169	50.750938
3491.844312	509985.355070	50.755943
3491.475113	509659.333912	50.760948
3491.099572	509335.989150	50.765953
3490.763757	508989.661186	50.770957
3490.029781	508684.120269	50.775962
3489.687684	508322.094676	50.780967
3489.250908	507969.842208	50.785972
3488.576323	507650.004556	50.790977
3488.484284	507255.937608	50.795981
3487.703709	506937.166228	50.800986
3486.935030	506553.715678	50.805991
3486.710979	506212.121987	50.810996
3485.732681	505843.617365	50.816001
3485.364097	505447.984532	50.821005
3484.664006	505094.956512	50.826010
3484.264243	504728.918026	50.831015
3484.007257	504350.854772	50.836020
3483.043725	503963.177739	50.841025
3482.723976	503585.006771	50.846029
3482.157595	503197.148933	50.851034
3481.358824	502813.975870	50.856039
3481.053599	502451.013359	50.861044
3480.412541	502036.973728	50.866049
3479.489966	501658.553299	50.871053
3479.214455	501263.824528	50.876058
3478.329657	500865.386846	50.881063
3477.784015	500481.465572	50.886068
3477.099328	500083.130731	50.891073
3476.377254	499695.423870	50.896077
3475.823775	499295.025903	50.901082
3475.077734	498900.775177	50.906087
3474.716143	498496.532254	50.911092
3473.860242	498107.344264	50.916097
3473.314233	497698.809334	50.921101
3472.654134	497291.650264	50.926106
3471.828333	496896.609124	50.931111
3471.088806	496502.001479	50.936116
3470.289579	496114.635311	50.941121
3470.172790	495690.696287	50.946125
3469.433740	495298.543712	50.951130
3469.035425	494889.466900	50.956135
3467.955865	494485.552462	50.961140
3467.197492	494080.464351	50.966145
3466.654400	493680.194769	50.971149
3465.826099	493277.682768	50.976154
3465.617735	492860.124585	50.981159
3464.608768	492445.772820	50.986164
3463.560465	492075.276127	50.991169
3463.579171	491645.297583	50.996173
3462.865375	491245.863581	51.001178
3462.050395	490837.725648	51.006183
3461.398998	490418.156992	51.011188
3460.774367	490026.128311	51.016193
3460.301074	489607.171872	51.021197
3459.531571	489197.623604	51.026202
3458.785156	488774.538402	51.031207
3458.063479	488360.000433	51.036212
3457.115039	487961.243105	51.041217
3456.989958	487539.855772	51.046221
3455.775060	487143.909560	51.051226
3455.256796	486738.929092	51.056231
3454.501316	486322.072511	51.061236
3453.814606	485905.044015	51.066241
3453.308682	485485.799426	51.071245
3452.634936	485098.945920	51.076250
3452.180287	484671.366780	51.081255
3451.495763	484272.491026	51.086260
3450.297052	483862.845768	51.091265
3449.936867	483447.232570	51.096269
3448.960948	483029.731760	51.101274
3448.652112	482613.231282	51.106279
3447.644998	482216.543144	51.111284
3447.010292	481817.254517	51.116289
3446.726738	481398.393299	51.121293
3445.680493	480989.170374	51.126298
3444.755063	480582.858976	51.131303
3444.321369	480165.211453	51.136308
3443.339163	479769.939625	51.141313
3442.793440	479361.313315	51.146317
3442.168211	478957.809731	51.151322
3441.233939	478552.978457	51.156327
3440.628513	478151.634640	51.161332
3439.870981	477758.263867	51.166337
3439.316050	477342.198056	51.171341
3438.315053	476950.269026	51.176346
3437.528299	476552.672451	51.181351
3437.212908	476149.975598	51.186356
3436.302702	475756.032214	51.191361
3435.921430	475357.993186	51.196365
3434.991865	474958.106836	51.201370
3434.320242	474550.619024	51.206375
3433.442822	474155.574872	51.211380
3432.445735	473770.426907	51.216385
3432.078688	473372.296083	51.221389
3431.042213	472980.042446	51.226394
3430.551949	472580.800455	51.231399
3429.932064	472195.816728	51.236404
3429.098244	471811.670771	51.241409
3428.348032	471423.752815	51.246413
3427.834947	471037.057558	51.251418
3426.983052	470649.445353	51.256423
3426.388882	470263.356884	51.261428
3425.665691	469874.239555	51.266433
3425.078319	469477.234611	51.271437
3424.256012	469101.554687	51.276442
3423.368478	468711.275494	51.281447
3423.098556	468329.916931	51.286452
3421.970718	467950.208261	51.291457
3421.441104	467557.112914	51.296461
3420.773457	467191.667928	51.301466
3419.965246	466802.253550	51.306471
3419.422033	466422.222145	51.311476
3418.561436	466044.769649	51.316481
3418.095316	465650.665388	51.321485
3417.107405	465269.517325	51.326490
3416.362422	464894.003962	51.331495
3416.043566	464520.039500	51.336500
3415.142889	464135.307443	51.341505
3414.445212	463762.505412	51.346509
3413.636071	463389.714548	51.351514
3413.098163	463010.534628	51.356519
3412.772811	462626.901921	51.361524
3411.696838	462252.612074	51.366529
3411.341017	461862.224946	51.371533
3410.501133	461488.797590	51.376538
3410.057848	461114.996802	51.381543
3409.217350	460726.136908	51.386548
3408.476540	460348.819439	51.391553
3407.514626	459969.399990	51.396557
3407.046075	459598.620833	51.401562
3406.328292	459220.468747	51.406567
3405.856398	458845.314961	51.411572
3404.639591	458474.077215	51.416577
3404.497164	458091.858060	51.421581
3403.710422	457727.489740	51.426586
3402.680435	457342.912263	51.431591
3402.052007	456971.201286	51.436596
3401.363478	456600.457553	51.441601
3400.851388	456224.504971	51.446605
3400.205690	455855.670028	51.451610
3399.352084	455491.225132	51.456615
3398.752566	455119.225247	51.461620
3398.144447	454757.114277	51.466625
3397.437174	454367.564123	51.471629
3396.474939	454005.192699	51.476634
3395.626329	453637.013254	51.481639
3395.203386	453258.358830	51.486644
3394.205994	452898.258664	51.491649
3393.791843	452528.977842	51.496653
3392.987429	452166.958222	51.501658
3392.349444	451792.829661	51.506663
3391.736983	451441.779592	51.511668
3390.556097	451082.542628	51.516673
3390.565100	450705.959885	51.521677
3389.769510	450345.737144	51.526682
3388.841094	449988.320919	51.531687
3388.313351	449621.092212	51.536692
3387.555759	449266.327552	51.541697
3386.799298	448902.929878	51.546701
3386.148999	448544.381827	51.551706
3385.513253	448180.801622	51.556711
3384.807681	447826.006940	51.561716
3384.023492	447463.707932	51.566721
3383.417634	447092.036507	51.571725
3383.165131	446741.264939	51.576730
3382.024940	446384.791698	51.581735
3381.613315	446002.972229	51.586740
3380.785969	445653.189102	51.591745
3380.071701	445286.429985	51.596749
3379.457054	444934.420138	51.601754
3378.506221	444574.590639	51.606759
3378.053975	444198.281521	51.611764
3377.261334	443860.852137	51.616769
3376.575137	443501.370842	51.621773
3375.976338	443131.058080	51.626778
3374.958256	442790.654451	51.631783
3374.268774	442428.619628	51.636788
3373.378472	442086.764562	51.641793
3372.968658	441731.883682	51.646797
3372.368791	441378.347608	51.651802
3371.494287	441042.821151	51.656807
3371.139568	440676.290775	51.661812
3370.409318	440332.609076	51.666817
3369.623103	439987.433764	51.671821
3369.107558	439635.306216	51.676826
3368.058558	439282.648771	51.681831
3367.636028	438934.482005	51.686836
3366.724335	438586.083082	51.691841
3366.321003	438222.697295	51.696845
3365.185029	437887.854853	51.701850
3364.442081	437550.889461	51.706855
3364.133694	437198.618576	51.711860
3363.307114	436844.139822	51.716865
3362.423498	436500.505694	51.721869
3361.970046	436171.523994	51.726874
3360.826505	435830.587611	51.731879
3360.291639	435480.105760	51.736884
3359.644546	435155.432210	51.741889
3359.423794	434812.762135	51.746893
3358.762808	434462.540121	51.751898
3357.605210	434123.436566	51.756903
3357.682101	433770.066980	51.761908
3356.352119	433435.196415	51.766913
3355.772140	433078.163345	51.771917
3355.293359	432746.678620	51.776922
3354.417129	432402.048725	51.781927
3353.687283	432053.556878	51.786932
3352.827863	431735.755028	51.791937
3352.261930	431400.305655	51.796941
3351.457123	431056.459206	51.801946
3350.794453	430725.257122	51.806951
3350.484093	430373.553108	51.811956
3349.811289	430049.530555	51.816961
3349.197208	429715.895617	51.821965
3348.287062	429370.469297	51.826970
3347.766023	429023.097697	51.831975
3347.217556	428697.134257	51.836980
3346.404083	428357.672777	51.841985
3346.191360	428004.804412	51.846989
3345.404380	427664.263274	51.851994
3344.169206	427333.363249	51.856999
3343.589558	426984.145778	51.862004
3342.810971	426646.663431	51.867009
3341.917484	426311.988772	51.872013
3341.488061	425977.007997	51.877018
3340.617921	425642.245156	51.882023
3340.232765	425305.699780	51.887028
3339.513329	424983.807502	51.892033
3338.806228	424639.456514	51.897037
3338.528615	424309.384037	51.902042
3337.309625	423988.727398	51.907047
3336.980458	423635.388648	51.912052
3336.400978	423294.810606	51.917057
3335.438955	422961.426479	51.922061
3334.892118	422631.859047	51.927066
3334.011043	422291.087704	51.932071
3333.723511	421957.813442	51.937076
3332.397007	421632.015272	51.942081
3332.222450	421297.597551	51.947085
3331.391666	420963.787651	51.952090
3330.287183	420632.862183	51.957095
3330.018379	420303.350260	51.962100
3329.258764	419981.380735	51.967105
3328.776457	419635.331643	51.972109
3327.981124	419311.454834	51.977114
3327.018704	418980.690736	51.982119
3326.618815	418652.094849	51.987124
3325.852182	418337.652951	51.992129
3325.222788	417992.851943	51.997133
3324.844176	417664.774829	52.002138
3323.705567	417335.924937	52.007143
3323.530245	416995.155875	52.012148
3322.571359	416685.553427	52.017153
3321.780732	416345.814032	52.022157
3321.082380	416026.203859	52.027162
3320.387223	415698.611752	52.032167
3319.470122	415368.561102	52.037172
3318.561120	415062.769985	52.042177
3318.491349	414721.398537	52.047181
3317.756106	414397.279074	52.052186
3316.768126	414083.994719	52.057191
3316.502234	413752.044243	52.062196
3315.667489	413436.416541	52.067201
3315.162991	413104.598154	52.072205
3314.243494	412775.738404	52.077210
3313.467838	412465.681183	52.082215
3313.233779	412132.741941	52.087220
3312.457719	411820.162433	52.092225
3311.938046	411488.074315	52.097229
3311.506849	411155.409479	52.102234
3310.345235	410830.174991	52.107239
3309.600635	410496.408912	52.112244
3309.004414	410182.742045	52.117249
3308.116000	409850.948311	52.122253
3307.530116	409537.374779	52.127258
3306.933109	409214.219119	52.132263
3306.275180	408889.570292	52.137268
3305.483861	408579.424759	52.142273
3304.995071	408244.678631	52.147277
3304.604956	407920.968322	52.152282
3303.586022	407605.054563	52.157287
3303.419283	407275.939757	52.162292
3302.560266	406957.605127	52.167297
3301.881404	406625.692539	52.172301
3301.153356	406295.283688	52.177306
3300.010834	405972.154900	52.182311
3299.758968	405645.501613	52.187316
3298.733815	405332.793560	52.192321
3298.017223	405012.764525	52.197325
3297.361212	404680.903943	52.202330
3296.473318	404367.376680	52.207335
3296.077664	404050.235486	52.212340
3295.740108	403743.274292	52.217345
3294.835691	403430.884168	52.222349
3294.255038	403110.153561	52.227354
3293.277389	402792.913965	52.232359
3292.595087	402458.136686	52.237364
3292.109667	402143.583426	52.242369
3291.424265	401828.626601	52.247373
3290.903107	401503.396826	52.252378
3290.098130	401181.411511	52.257383
3289.483764	400872.153505	52.262388
3288.897914	400553.686062	52.267393
3288.341380	400241.794682	52.272397
3287.560435	399914.276883	52.277402
3286.690159	399593.709767	52.282407
3286.352200	399272.318132	52.287412
3285.492486	398950.243249	52.292417
3284.748066	398644.213284	52.297421
3284.150130	398310.117318	52.302426
3283.348017	397989.549285	52.307431
3282.771795	397682.365298	52.312436
3282.001517	397362.675978	52.317441
3281.496942	397041.365385	52.322445
3280.786143	396729.134849	52.327450
3280.338039	396404.097508	52.332455
3279.807706	396087.841074	52.337460
3278.910155	395777.868525	52.342465
3278.043919	395439.972911	52.347469
3277.601912	395118.939236	52.352474
3276.678461	394806.699200	52.357479
3276.101390	394481.358777	52.362484
3275.640691	394175.446767	52.367489
3274.448526	393860.011676	52.372493
3274.330154	393537.691623	52.377498
3273.437708	393219.431934	52.382503
3272.887853	392894.428196	52.387508
3272.050038	392595.375928	52.392513
3271.350438	392265.660795	52.397517
3270.842317	391942.268853	52.402522
3269.994056	391635.785539	52.407527
3269.344816	391320.419555	52.412532
3268.876138	391008.403984	52.417537
3268.168618	390685.693141	52.422541
3267.760840	390362.601396	52.427546
3266.515365	390048.157487	52.432551
3266.418648	389709.423434	52.437556
3265.488575	389409.901072	52.442561
3264.451629	389093.584958	52.447565
3263.962042	388773.644912	52.452570
3263.344069	388468.242191	52.457575
3262.962858	388141.439050	52.462580
3261.955390	387827.700945	52.467585
3261.503693	387512.677042	52.472589
3260.921303	387192.407141	52.477594
3259.948649	386889.513941	52.482599
3259.409393	386568.723164	52.487604
3258.396237	386245.410648	52.492609
3257.694192	385940.330678	52.497613
3257.692410	385622.040577	52.502618
3256.968868	385315.560169	52.507623
3256.107659	384994.272611	52.512628
3255.383650	384687.888838	52.517633
3254.741148	384358.702909	52.522637
3254.355917	384044.351047	52.527642
3253.400915	383738.097784	52.532647
3253.372919	383414.859239	52.537652
3252.200901	383085.669651	52.542657
3251.243761	382775.136275	52.547661
3250.987596	382454.036559	52.552666
3250.181591	382141.693816	52.557671
3249.919233	381821.174733	52.562676
3248.715586	381505.990310	52.567681
3248.228491	381181.788150	52.572685
3247.836996	380855.584301	52.577690
3247.045282	380545.540860	52.582695
3246.649307	380222.359072	52.587700
3245.625290	379908.786492	52.592705
3245.119638	379586.303528	52.597709
3244.459965	379259.340279	52.602714
3243.500162	378939.747136	52.607719
3242.947321	378611.388118	52.612724
3241.965676	378303.519030	52.617729
3241.481263	377986.640929	52.622733
3240.872096	377666.880335	52.627738
3239.915174	377357.448435	52.632743
3239.459811	377036.844527	52.637748
3238.938330	376711.975167	52.642753
3238.165224	376401.540253	52.647757
3237.626999	376087.580934	52.652762
3236.867075	375768.515935	52.657767
3236.333108	375453.152001	52.662772
3235.541517	375143.702481	52.667777
3234.874692	374815.101645	52.672781
3234.405005	374491.707239	52.677786
3233.507694	374183.284743	52.682791
3232.876886	373854.874077	52.687796
3232.030324	373539.417765	52.692801
3231.373519	373227.134341	52.697805
3230.675015	372913.863061	52.702810
3229.849313	372597.658618	52.707815
3229.332510	372280.894153	52.712820
3228.595976	371985.633061	52.717825
3228.158995	371671.878719	52.722829
3227.605448	371357.326423	52.727834
3226.636915	371049.960685	52.732839
3226.047076	370727.497619	52.737844
3225.542882	370410.539172	52.742849
3224.638351	370101.859060	52.747853
3224.623082	369782.707089	52.752858
3223.466956	369468.338066	52.757863
3222.609745	369140.206664	52.762868
3222.214118	368833.675873	52.767873
3221.308466	368515.418717	52.772877
3220.658743	368198.187328	52.777882
3219.995339	367897.289563	52.782887
3219.479550	367582.856631	52.787892
3218.826421	367261.370234	52.792897
3217.651259	366955.814774	52.797901
3217.349318	366636.965235	52.802906
3216.573117	366331.495065	52.807911
3216.072121	366017.328662	52.812916
3215.668422	365699.175546	52.817921
3214.550231	365397.315210	52.822925
3214.309747	365062.746286	52.827930
3213.523829	364766.375909	52.832935
3212.776229	364452.848370	52.837940
3212.373624	364129.290044	52.842945
3211.468525	363828.581542	52.847949
3210.881342	363507.287157	52.852954
3209.959062	363191.743150	52.857959
3209.279514	362886.489184	52.862964
3208.721744	362567.829934	52.867969
3208.101889	362245.743257	52.872973
3207.544813	361933.593553	52.877978
3206.644774	361625.287415	52.882983
3206.052749	361313.266386	52.887988
3205.873424	361004.969451	52.892993
3204.748569	360678.778937	52.897997
3204.205483	360356.158419	52.903002
3203.306873	360055.170425	52.908007
3202.752592	359734.430552	52.913012
3201.748449	359419.128961	52.918017
3200.987314	359119.334861	52.923021
3200.947876	358804.792781	52.928026
3200.216632	358499.977125	52.933031
3199.342478	358185.893951	52.938036
3198.848307	357872.868360	52.943041
3198.226788	357559.072070	52.948045
3197.717851	357252.075985	52.953050
3196.528243	356936.711556	52.958055
3196.114357	356612.137484	52.963060
3195.511118	356306.524740	52.968065
3194.722607	355996.715038	52.973069
3194.252294	355675.884804	52.978074
3193.634007	355368.563758	52.983079
3192.979699	355053.561027	52.988084
3192.337500	354736.569433	52.993089
3191.419771	354421.324575	52.998093
3191.143935	354100.835501	53.003098
3190.283633	353780.360570	53.008103
3189.662003	353467.455348	53.013108
3188.778487	353153.240856	53.018113
3187.865237	352848.242059	53.023117
3187.499766	352528.368372	53.028122
3186.593502	352221.608815	53.033127
3185.781576	351915.316129	53.038132
3185.099463	351604.165564	53.043137
3184.572491	351295.686424	53.048141
3184.307771	350975.380326	53.053146
3183.377175	350678.490729	53.058151
3182.864143	350366.517329	53.063156
3182.205009	350041.966914	53.068161
3181.314395	349731.067683	53.073165
3180.790345	349413.796737	53.078170
3180.135086	349106.038198	53.083175
3179.460377	348795.684953	53.088180
3178.951384	348480.773325	53.093185
3178.092178	348183.960854	53.098189
3177.254707	347866.807071	53.103194
3176.639844	347563.284205	53.108199
3175.827807	347244.086732	53.113204
3175.194972	346945.170319	53.118209
3174.668884	346633.559988	53.123213
3174.161615	346317.338022	53.128218
3173.225566	346006.221865	53.133223
3172.524552	345706.877128	53.138228
3172.240529	345392.625614	53.143233
3171.496469	345087.455714	53.148237
3171.098834	344778.080495	53.153242
3170.338351	344472.655480	53.158247
3169.675745	344154.766489	53.163252
3168.902205	343830.784404	53.168257
3168.219232	343520.506003	53.173261
3167.664733	343206.107549	53.178266
3166.831955	342893.304205	53.183271
3166.168869	342579.326954	53.188276
3165.501764	342272.705113	53.193281
3164.562335	341964.953908	53.198285
3164.209312	341648.402823	53.203290
3163.324045	341341.607232	53.208295
3162.784894	341035.442660	53.213300
3162.431346	340719.701505	53.218305
3161.312634	340412.632831	53.223309
3160.707207	340089.953597	53.228314
3159.977352	339778.492891	53.233319
3159.105086	339477.210044	53.238324
3158.660326	339167.024954	53.243329
3157.938624	338862.100668	53.248333
3157.536698	338544.243555	53.253338
3156.613102	338242.173930	53.258343
3155.862446	337931.471296	53.263348
3155.598891	337619.010000	53.268353
3154.678382	337328.009253	53.273357
3154.226573	337012.825569	53.278362
3153.600867	336705.228589	53.283367
3152.907318	336389.774734	53.288372
3152.371569	336075.414548	53.293377
3151.598572	335769.694968	53.298381
3150.819266	335454.683100	53.303386
3150.205553	335141.527431	53.308391
3149.489425	334828.259253	53.313396
3148.824443	334513.581394	53.318401
3148.095409	334209.197182	53.323405
3147.628517	333894.917973	53.328410
3146.940829	333588.258773	53.333415
3146.082309	333283.305505	53.338420
3145.326780	332970.060716	53.343425
3144.458887	332662.356787	53.348429
3144.105202	332346.958112	53.353434
3143.360930	332050.000922	53.358439
3142.671266	331750.157051	53.363444
3141.949768	331436.314676	53.368449
3141.436960	331138.222429	53.373453
3140.544707	330826.619391	53.378458
3140.094496	330512.908380	53.383463
3139.387356	330199.975018	53.388468
3138.964310	329894.149459	53.393473
3138.084077	329595.803676	53.398477
3137.696833	329282.892277	53.403482
3136.927762	328973.298837	53.408487
3135.952388	328659.459563	53.413492
3136.059938	328342.443416	53.418497
3135.136205	328041.527041	53.423501
3134.334059	327722.360919	53.428506
3133.576531	327411.664653	53.433511
3132.950645	327100.793577	53.438516
3132.085970	326789.017039	53.443521
3131.236874	326475.021769	53.448525
3131.114025	326175.193698	53.453530
3130.541801	325868.535804	53.458535
3129.929980	325555.874304	53.463540
3128.909303	325241.010296	53.468545
3128.071959	324926.854445	53.473549
3127.716754	324612.621119	53.478554
3126.974218	324306.951895	53.483559
3126.630121	323989.099008	53.488564
3126.076726	323679.731181	53.493569
3124.852385	323361.735155	53.498573
3124.406515	323035.925421	53.503578
3123.419804	322737.571181	53.508583
3122.923819	322420.449446	53.513588
3122.370042	322112.323690	53.518593
3121.536958	321808.773253	53.523597
3121.044414	321494.626675	53.528602
3120.258209	321179.150513	53.533607
3119.942822	320870.015186	53.538612
3119.344199	320559.472281	53.543617
3118.061660	320246.184765	53.548621
3117.617375	319924.946610	53.553626
3117.035492	319623.004157	53.558631
3116.289443	319314.619230	53.563636
3115.837112	319002.443816	53.568641
3115.220919	318683.367456	53.573645
3114.320349	318375.946037	53.578650
3113.739578	318071.095702	53.583655
3113.182399	317745.590254	53.588660
3112.637056	317436.098069	53.593665
3111.635313	317123.621556	53.598669
3110.967419	316801.848106	53.603674
3110.358267	316496.666349	53.608679
3109.568695	316181.403280	53.613684
3108.888968	315873.811791	53.618689
3108.214203	315570.649231	53.623693
3107.766679	315253.775898	53.628698
3106.883178	314944.482351	53.633703
3106.337701	314634.625125	53.638708
3105.608438	314322.937214	53.643713
3104.763885	314009.967974	53.648717
3104.475474	313699.659918	53.653722
3103.624314	313390.433113	53.658727
3102.536611	313087.048664	53.663732
3102.625561	312787.576908	53.668737
3101.754448	312467.757579	53.673741
3101.488452	312151.788542	53.678746
3100.391197	311849.089756	53.683751
3099.714363	311528.422153	53.688756
3099.178577	311220.921933	53.693761
3098.440479	310915.795647	53.698765
3097.554039	310598.519947	53.703770
3097.234276	310293.656879	53.708775
3096.404563	309985.970740	53.713780
3095.733188	309661.477440	53.718785
3095.080921	309350.145588	53.723789
3094.571920	309034.155650	53.728794
3093.764990	308727.175730	53.733799
3093.150641	308411.200868	53.738804
3092.416782	308097.841566	53.743809
3091.582946	307794.581529	53.748813
3091.250660	307471.658617	53.753818
3091.031307	307161.118640	53.758823
3089.535012	306848.640901	53.763828
3089.182959	306533.689458	53.768833
3088.582965	306229.319225	53.773837
3087.865500	305905.001888	53.778842
3086.921577	305607.738640	53.783847
3086.277867	305295.478887	53.788852
3086.062600	304985.060561	53.793857
3085.331383	304672.813259	53.798861
3084.417351	304354.176805	53.803866
3084.033678	304044.445178	53.808871
3082.680485	303733.338355	53.813876
3082.569413	303413.987047	53.818881
3081.997178	303103.442889	53.823885
3081.260864	302797.711683	53.828890
3080.621326	302484.222829	53.833895
3079.818418	302174.477255	53.838900
3079.285009	301861.683393	53.843905
3078.322888	301561.333384	53.848909
3077.643254	301238.884225	53.853914
3077.331038	300930.892135	53.858919
3076.518493	300620.712124	53.863924
3075.983122	300301.497985	53.868929
3075.052628	299996.632507	53.873933
3074.544998	299674.356797	53.878938
3074.063959	299356.405604	53.883943
3073.641900	299049.624379	53.888948
3073.002994	298729.608758	53.893953
3072.103838	298422.545414	53.898957
3071.301586	298105.636013	53.903962
3070.755857	297787.717726	53.908967
3070.153289	297469.222150	53.913972
3069.347922	297148.262368	53.918977
3068.819328	296837.699722	53.923981
3068.415855	296520.393477	53.928986
3067.419504	296213.647522	53.933991
3066.462110	295895.638461	53.938996
3066.002166	295570.928712	53.944001
3065.228395	295266.234412	53.949005
3064.699168	294953.529721	53.954010
3063.728651	294640.996279	53.959015
3063.052877	294329.205227	53.964020
3062.587329	294018.042616	53.969025
3061.828422	293712.859902	53.974029
3061.218092	293394.282868	53.979034
3060.193827	293086.594577	53.984039
3059.280380	292772.470539	53.989044
3059.261930	292458.000709	53.994049
3058.457774	292154.198391	53.999053
3058.048846	291850.893441	54.004058
3057.176272	291542.720789	54.009063
3056.276774	291237.659086	54.014068
3055.870049	290924.751402	54.019073
3054.774333	290619.872853	54.024077
3054.601553	290302.419648	54.029082
3053.951544	290001.952207	54.034087
3053.232619	289690.951693	54.039092
3052.652416	289377.076502	54.044097
3051.654099	289069.786922	54.049101
3050.769337	288764.465558	54.054106
3050.519443	288449.543898	54.059111
3049.776525	288150.439131	54.064116
3048.908462	287838.059636	54.069121
3048.357722	287538.007062	54.074125
3047.859778	287230.203607	54.079130
3047.070776	286918.039985	54.084135
3046.290319	286613.667963	54.089140
3045.877212	286302.972417	54.094145
3044.945486	285996.026104	54.099149
3044.260830	285691.001496	54.104154
3043.706698	285384.198706	54.109159
3043.248597	285080.767757	54.114164
3042.755236	284770.465781	54.119169
3041.979423	284468.536384	54.124173
3041.434373	284153.021203	54.129178
3040.729603	283850.876429	54.134183
3040.021147	283540.505828	54.139188
3039.738895	283218.148463	54.144193
3038.777746	282903.742574	54.149197
3038.051732	282585.453593	54.154202
3037.284806	282280.796438	54.159207
3036.976288	281970.616373	54.164212
3036.421295	281654.515594	54.169217
3035.475228	281346.830168	54.174221
3035.021414	281027.555030	54.179226
3034.957182	280696.477209	54.184231
3033.523611	280388.206387	54.189236
3033.046890	280065.343472	54.194241
3032.251933	279740.416943	54.199245
3031.845365	279426.838661	54.204250
3031.149470	279112.618439	54.209255
3030.225651	278787.635626	54.214260
3029.924585	278465.584905	54.219265
3028.837630	278147.249543	54.224269
3028.406598	277812.357735	54.229274
3027.481561	277493.028835	54.234279
3026.645861	277182.803436	54.239284
3026.429547	276864.253682	54.244289
3025.646988	276550.148619	54.249293
3024.727882	276236.319833	54.254298
3024.025982	275919.349514	54.259303
3023.391795	275590.856762	54.264308
3022.866581	275285.039103	54.269313
3022.144874	274985.543249	54.274317
3021.394500	274667.943926	54.279322
3020.736197	274353.411732	54.284327
3019.683833	274046.251370	54.289332
3019.667099	273733.069405	54.294337
3018.846786	273419.734525	54.299341
3018.118803	273099.024730	54.304346
3017.716831	272788.017785	54.309351
3016.606336	272471.647359	54.314356
3016.076140	272165.907340	54.319361
3015.491876	271862.340772	54.324365
3014.694832	271539.553909	54.329370
3014.273995	271228.270229	54.334375
3013.461387	270917.150539	54.339380
3013.310740	270604.678243	54.344385
3012.288545	270290.866858	54.349389
3011.735579	269966.921363	54.354394
3010.919532	269655.395239	54.359399
3010.281049	269330.419382	54.364404
3009.954808	269015.250482	54.369409
3008.985120	268703.570868	54.374413
3008.222155	268378.844441	54.379418
3008.139949	268060.657654	54.384423
3007.148076	267753.107938	54.389428
3006.486767	267432.619188	54.394433
3005.929968	267113.285642	54.399437
3005.352290	266796.706176	54.404442
3004.564800	266475.906965	54.409447
3003.629013	266163.179381	54.414452
3002.968298	265836.808532	54.419457
3002.300251	265529.718427	54.424461
3001.560677	265214.846658	54.429466
3001.227022	264895.275715	54.434471
3000.310338	264581.909649	54.439476
2999.736415	264270.374229	54.444481
2998.912478	263950.245019	54.449485
2998.411628	263627.212557	54.454490
2997.607668	263311.996096	54.459495
2996.972351	263001.210124	54.464500
2996.494528	262674.074627	54.469505
2995.867018	262371.565092	54.474509
2994.917549	262061.491947	54.479514
2994.581812	261726.287151	54.484519
2993.826364	261421.124718	54.489524
2993.304634	261095.245827	54.494529
2992.752282	260777.470891	54.499533
2992.084486	260449.400196	54.504538
2991.594799	260128.356246	54.509543
2990.462301	259812.507961	54.514548
2990.022292	259490.922119	54.519553
2988.999709	259177.451179	54.524557
2988.281314	258863.932489	54.529562
2988.108442	258533.774000	54.534567
2986.983162	258219.607471	54.539572
2986.834643	257902.154264	54.544577
2985.800599	257582.243998	54.549581
2985.218712	257270.997908	54.554586
2984.866401	256942.143487	54.559591
2983.429801	256629.505568	54.564596
2983.416837	256300.674813	54.569601
2982.489019	255994.400500	54.574605
2981.883030	255682.039987	54.579610
2980.898226	255361.055639	54.584615
2980.326659	255044.896067	54.589620
2979.829194	254722.562256	54.594625
2979.313142	254424.629279	54.599629
2978.870029	254100.938154	54.604634
2978.300176	253776.554574	54.609639
2977.457563	253451.119664	54.614644
2976.933052	253115.804797	54.619649
2976.091072	252805.752886	54.624653
2975.189000	252479.412339	54.629658
2975.045297	252155.346216	54.634663
2974.102897	251830.490336	54.639668
2972.967015	251509.409285	54.644673
2972.578877	251196.639895	54.649677
2971.921345	250869.576121	54.654682
2971.528261	250545.476173	54.659687
2970.594894	250242.141084	54.664692
2969.987316	249912.855760	54.669697
2969.305599	249593.591098	54.674701
2968.524039	249280.607580	54.679706
2968.431483	248947.499232	54.684711
2967.357214	248634.232311	54.689716
2966.543076	248311.629758	54.694721
2966.066203	247993.380130	54.699725
2965.420633	247675.259760	54.704730
2965.115199	247349.599274	54.709735
2964.017969	247039.166099	54.714740
2963.294557	246715.355833	54.719745
2962.839325	246393.846702	54.724749
2962.012167	246074.714567	54.729754
2961.529463	245740.860467	54.734759
2960.689598	245429.702575	54.739764
2960.168723	245107.875806	54.744769
2959.112339	244794.640033	54.749773
2958.698076	244475.115275	54.754778
2958.079835	244153.331715	54.759783
2957.298082	243835.139972	54.764788
2956.796105	243512.957631	54.769793
2956.284230	243196.991158	54.774797
2955.516384	242872.815336	54.779802
2955.041791	242545.563607	54.784807
2954.579385	242224.957154	54.789812
2953.648940	241902.388455	54.794817
2952.992446	241575.855678	54.799821
2952.232905	241245.418547	54.804826
2951.842977	240926.739403	54.809831
2950.712169	240607.159833	54.814836
2950.266950	240274.358405	54.819841
2949.592025	239954.453824	54.824845
2948.569494	239635.292706	54.829850
2948.052944	239318.955312	54.834855
2947.058052	239005.011779	54.839860
2946.960409	238694.135565	54.844865
2945.902835	238370.374611	54.849869
2945.308062	238044.555161	54.854874
2944.888352	237720.847943	54.859879
2944.126778	237401.753843	54.864884
2943.534770	237075.529475	54.869889
2942.893651	236758.455340	54.874893
2942.318147	236432.968799	54.879898
2941.726510	236114.360975	54.884903
2940.922008	235795.711445	54.889908
2940.589274	235463.263486	54.894913
2939.746150	235138.510931	54.899917
2939.029321	234824.484886	54.904922
2938.484550	234489.501935	54.909927
2937.384928	234167.466773	54.914932
2936.876317	233837.954857	54.919937
2936.219073	233524.050837	54.924941
2935.763300	233202.349802	54.929946
2935.131426	232869.474155	54.934951
2934.237473	232559.684791	54.939956
2933.844249	232229.829115	54.944961
2933.040929	231901.338106	54.949965
2932.207714	231583.012450	54.954970
2932.039519	231252.335278	54.959975
2931.111030	230934.052412	54.964980
2930.654643	230611.443754	54.969985
2930.069228	230283.535127	54.974989
2929.355261	229961.529738	54.979994
2928.683589	229635.063008	54.984999
2927.642464	229306.771811	54.990004
2926.972756	228971.701184	54.995009
2926.038759	228651.797799	55.000013
2925.786767	228340.189875	55.005018
2925.269938	228005.047857	55.010023
2924.196879	227691.942757	55.015028
2923.630011	227363.609321	55.020033
2923.214254	227042.255011	55.025037
2922.204099	226717.329671	55.030042
2921.764079	226393.219191	55.035047
2921.087111	226072.355544	55.040052
2920.383447	225738.614315	55.045057
2919.652021	225426.240198	55.050061
2919.049701	225103.357161	55.055066
2918.642941	224773.430145	55.060071
2918.025092	224461.538261	55.065076
2917.392981	224127.970594	55.070081
2916.833811	223798.084481	55.075085
2915.856738	223466.432808	55.080090
2915.248069	223135.017003	55.085095
2914.386400	222811.115079	55.090100
2913.996974	222480.685751	55.095105
2913.058910	222156.480436	55.100109
2912.336121	221843.660927	55.105114
2911.756991	221507.053781	55.110119
2911.192848	221189.781959	55.115124
2910.690747	220860.701413	55.120129
2910.015990	220539.758315	55.125133
2909.261038	220204.814252	55.130138
2908.803521	219874.076218	55.135143
2907.644911	219557.872951	55.140148
2907.440552	219228.790757	55.145153
2906.851601	218908.999594	55.150157
2906.098581	218576.188503	55.155162
2905.143942	218242.087067	55.160167
2904.791968	217920.862615	55.165172
2904.145102	217606.038048	55.170177
2903.499776	217268.811845	55.175181
2902.684682	216944.775734	55.180186
2901.862718	216614.848815	55.185191
2900.976509	216293.818267	55.190196
2901.016982	215950.774720	55.195201
2900.262139	215625.195119	55.200205
2899.252992	215301.630262	55.205210
2898.658337	214969.867856	55.210215
2898.016231	214641.627633	55.215220
2897.544862	214312.534649	55.220225
2896.485809	213991.860621	55.225229
2896.175029	213662.236310	55.230234
2895.345078	213331.957623	55.235239
2894.316052	213019.773242	55.240244
2893.781593	212677.779450	55.245249
2893.115584	212355.702047	55.250253
2892.407118	212038.367745	55.255258
2891.862314	211710.814130	55.260263
2891.271195	211391.338918	55.265268
2890.322979	211060.912419	55.270273
2889.691449	210738.697725	55.275277
2889.044185	210419.630879	55.280282
2889.108429	210094.547453	55.285287
2888.154013	209768.532463	55.290292
2887.451509	209439.717471	55.295297
2887.179480	209111.663347	55.300301
2886.389235	208790.349362	55.305306
2885.784394	208452.207894	55.310311
2885.139535	208123.899942	55.315316
2884.252032	207782.497937	55.320321
2883.680597	207451.471177	55.325325
2882.736383	207125.137852	55.330330
2882.151774	206787.117098	55.335335
2881.336802	206475.109970	55.340340
2880.700399	206139.684646	55.345345
2880.518724	205815.274082	55.350349
2879.916587	205481.883356	55.355354
2879.439946	205143.384103	55.360359
2878.484340	204819.954315	55.365364
2877.393687	204482.256118	55.370369
2877.061362	204149.033995	55.375373
2876.464627	203818.159118	55.380378
2875.464678	203476.660132	55.385383
2874.777890	203151.161083	55.390388
2874.155394	202823.592141	55.395393
2874.060096	202488.764269	55.400397
2872.855090	202153.185148	55.405402
2872.191436	201828.415517	55.410407
2871.625536	201492.268356	55.415412
2870.882846	201165.593583	55.420417
2870.187294	200836.495462	55.425421
2869.348532	200513.033896	55.430426
2868.860169	200183.614236	55.435431
2867.888374	199851.639019	55.440436
2867.319611	199528.026073	55.445441
2866.770756	199195.580739	55.450445
2866.016630	198881.277633	55.455450
2865.778746	198549.919616	55.460455
2865.120442	198221.518784	55.465460
2864.290814	197881.783934	55.470465
2863.884705	197554.467116	55.475469
2863.111889	197232.147559	55.480474
2862.534795	196892.989939	55.485479
2861.536410	196574.438470	55.490484
2860.563336	196245.145618	55.495489
2860.441633	195903.975571	55.500493
2859.638469	195576.886856	55.505498
2858.985713	195252.066764	55.510503
2858.015735	194922.514758	55.515508
2857.374963	194587.708688	55.520513
2856.720931	194270.491300	55.525517
2856.193689	193939.272429	55.530522
2855.829492	193605.586991	55.535527
2855.034803	193288.296337	55.540532
2854.603512	192954.689524	55.545537
2853.794186	192618.205723	55.550541
2852.937917	192303.946613	55.555546
2852.267604	191968.183219	55.560551
2851.618344	191638.780391	55.565556
2851.034098	191298.669395	55.570561
2850.404965	190980.171541	55.575565
2849.710243	190652.576579	55.580570
2849.444189	190313.210980	55.585575
2848.437147	189987.298555	55.590580
2847.970383	189652.944030	55.595585
2847.634087	189309.029292	55.600589
2846.562440	188984.469866	55.605594
2846.005254	188650.442102	55.610599
2845.304562	188314.391160	55.615604
2844.622139	187978.886801	55.620609
2843.841874	187649.926793	55.625613
2842.782015	187315.721047	55.630618
2842.581749	186978.926268	55.635623
2841.857592	186657.152338	55.640628
2841.004509	186320.682046	55.645633
2840.778456	185994.126866	55.650637
2840.048414	185661.229466	55.655642
2839.342862	185317.568290	55.660647
2838.305798	184989.660382	55.665652
2837.914368	184648.473398	55.670657
2837.233765	184325.347976	55.675661
2836.278470	183995.844255	55.680666
2835.824142	183665.958339	55.685671
2835.020287	183337.122463	55.690676
2834.032321	183011.383904	55.695681
2833.741963	182680.105547	55.700685
2833.112614	182352.101689	55.705690
2832.492550	182015.677855	55.710695
2831.588164	181691.246107	55.715700
2831.271358	181351.154081	55.720705
2830.665961	181020.116340	55.725709
2829.536886	180703.868527	55.730714
2829.260811	180362.264170	55.735719
2828.350751	180036.446596	55.740724
2827.666865	179724.053264	55.745729
2827.263831	179389.879746	55.750733
2826.385036	179062.487453	55.755738
2825.878951	178724.595950	55.760743
2825.081052	178403.174150	55.765748
2824.250561	178069.078815	55.770753
2823.839818	177737.209138	55.775757
2823.246353	177411.997708	55.780762
2822.672760	177079.879255	55.785767
2822.117173	176751.830674	55.790772
2821.097021	176423.667498	55.795777
2820.788777	176092.621522	55.800781
2819.841240	175757.266114	55.805786
2818.924190	175424.630397	55.810791
2818.329994	175107.475443	55.815796
2817.800327	174769.035034	55.820801
2817.389392	174436.886883	55.825805
2816.477789	174123.618104	55.830810
2815.898786	173782.217777	55.835815
2815.177731	173459.843376	55.840820
2814.503659	173127.099153	55.845825
2814.334025	172789.813926	55.850829
2813.441591	172457.580460	55.855834
2812.811671	172120.017756	55.860839
2811.958328	171792.514602	55.865844
2811.840622	171447.398759	55.870849
2810.799267	171054.374274	55.875853
2809.903518	170735.992146	55.880858
2809.591714	170380.959083	55.885863
2808.733283	170057.451718	55.890868
2807.734245	169740.772758	55.895873
2807.329429	169390.036355	55.900877
2806.739698	169071.886553	55.905882
2806.442710	168738.306260	55.910887
2805.665746	168403.609582	55.915892
2804.915044	168061.727092	55.920897
2804.421082	167743.916572	55.925901
2803.518976	167395.146587	55.930906
2802.595628	167042.848218	55.935911
2802.463888	166733.457574	55.940916
2801.407460	166384.746865	55.945921
2801.184907	166055.005929	55.950925
2800.368519	165724.332032	55.955930
2799.600556	165380.467751	55.960935
2799.044533	165042.040594	55.965940
2798.299945	164718.561076	55.970945
2797.783115	164374.666420	55.975949
2796.965416	164051.039085	55.980954
2796.555624	163694.775152	55.985959
2795.726271	163361.874120	55.990964
2794.658172	163023.445060	55.995969
2794.413490	162677.133056	56.000973
2793.305956	162365.886797	56.005978
2793.073641	162016.515083	56.010983
2792.234712	161681.876560	56.015988
2791.271473	161347.578709	56.020993
2791.089963	161003.345232	56.025997
2790.389332	160676.665724	56.031002
2789.637836	160340.576638	56.036007
2788.912050	160023.200673	56.041012
2787.856374	159673.588315	56.046017
2787.099641	159354.240039	56.051021
2786.476187	159015.333765	56.056026
2785.820079	158686.428235	56.061031
2785.299178	158356.347545	56.066036
2784.509963	158027.965129	56.071041
2784.200717	157699.954747	56.076045
2783.349762	157377.397893	56.081050
2782.525197	157030.534117	56.086055
2781.908820	156722.946677	56.091060
2781.439585	156394.211377	56.096065
2780.867346	156057.359972	56.101069
2780.020508	155739.267067	56.106074
2779.921914	155394.796440	56.111079
2778.856062	155065.774437	56.116084
2777.672097	154739.011552	56.121089
2777.529562	154404.104232	56.126093
2776.660435	154079.725740	56.131098
2775.971829	153748.165515	56.136103
2775.430001	153417.932688	56.141108
2774.744507	153096.712383	56.146113
2774.010059	152765.703060	56.151117
2773.407115	152443.497295	56.156122
2772.632591	152109.310564	56.161127
2772.273072	151775.468219	56.166132
2771.592973	151453.004744	56.171137
2770.936514	151112.276471	56.176141
2770.100411	150778.062225	56.181146
2769.954270	150461.815333	56.186151
2768.934349	150130.420288	56.191156
2768.142536	149787.401481	56.196161
2767.747588	149463.412852	56.201165
2766.856395	149131.257818	56.206170
2766.484013	148793.139745	56.211175
2765.525932	148468.360713	56.216180
2764.548980	148144.617385	56.221185
2764.318747	147801.670646	56.226189
2763.462598	147480.380417	56.231194
2762.667162	147141.673315	56.236199
2762.138499	146814.187106	56.241204
2761.699324	146487.084074	56.246209
2761.051810	146166.129991	56.251213
2760.221936	145833.898069	56.256218
2759.510387	145490.938308	56.261223
2759.071009	145162.286078	56.266228
2758.017471	144838.779462	56.271233
2757.657637	144504.276148	56.276237
2757.221196	144180.589694	56.281242
2756.259045	143849.594392	56.286247
2755.977458	143502.433292	56.291252
2755.042717	143176.917561	56.296257
2754.391731	142848.145555	56.301261
2753.644825	142508.083484	56.306266
2752.983726	142175.228825	56.311271
2752.634309	141845.657464	56.316276
2751.532366	141509.144297	56.321281
2750.891006	141175.852751	56.326285
2750.201774	140847.438790	56.331290
2749.705080	140520.509882	56.336295
2749.273448	140185.849258	56.341300
2748.167196	139857.804391	56.346305
2747.663476	139520.240382	56.351309
2746.831463	139198.956616	56.356314
2746.222820	138868.772864	56.361319
2745.699399	138531.007205	56.366324
2744.999608	138208.633297	56.371329
2744.197258	137871.262379	56.376333
2743.718916	137556.051289	56.381338
2743.001342	137226.817849	56.386343
2742.374582	136891.551965	56.391348
2741.717138	136563.942573	56.396353
2741.040955	136230.280096	56.401357
2740.346842	135904.373530	56.406362
2739.946873	135561.286943	56.411367
2739.141865	135233.652386	56.416372
2738.159579	134914.662427	56.421377
2737.909106	134572.478519	56.426381
2737.006489	134251.819171	56.431386
2736.324753	133927.254052	56.436391
2735.643582	133599.961445	56.441396
2735.018199	133264.572239	56.446401
2734.539142	132926.102524	56.451405
2733.992975	132605.379773	56.456410
2733.151880	132278.635769	56.461415
2732.443194	131948.597460	56.466420
2731.506907	131613.264311	56.471425
2731.239170	131278.489728	56.476429
2730.550836	130960.234182	56.481434
2729.828598	130633.223689	56.486439
2728.930535	130293.886611	56.491444
2728.178052	129972.007221	56.496449
2727.628124	129637.004841	56.501453
2726.952594	129311.920269	56.506458
2726.451681	128982.214231	56.511463
2726.060195	128646.436675	56.516468
2724.989180	128335.574510	56.521473
2724.262945	127995.273106	56.526477
2723.559468	127662.465296	56.531482
2723.057106	127331.229842	56.536487
2722.252412	127006.485027	56.541492
2721.340412	126692.136588	56.546497
2721.318794	126353.433007	56.551501
2720.542576	126028.784229	56.556506
2719.675027	125693.461192	56.561511
2719.019287	125371.683889	56.566516
2718.452582	125049.045498	56.571521
2718.044019	124710.398372	56.576525
2717.184268	124378.328591	56.581530
2716.656393	124051.365850	56.586535
2715.939191	123717.529311	56.591540
2715.487263	123378.220187	56.596545
2714.767482	123047.681212	56.601549
2713.957595	122719.649361	56.606554
2713.033917	122383.665566	56.611559
2712.573401	122046.749242	56.616564
2711.779831	121724.085417	56.621569
2711.383694	121386.710221	56.626573
2710.652889	121058.521408	56.631578
2709.644700	120730.393341	56.636583
2709.060326	120397.675929	56.641588
2708.580567	120075.547652	56.646593
2708.523956	119746.068686	56.651597
2707.435550	119410.510893	56.656602
2706.859358	119082.957226	56.661607
2706.019882	118751.018600	56.666612
2705.269264	118412.214553	56.671617
2704.743569	118074.553645	56.676621
2703.814232	117742.280418	56.681626
2703.386202	117417.599892	56.686631
2702.835498	117085.287881	56.691636
2701.851761	116759.694492	56.696641
2701.363084	116420.462664	56.701645
2700.609071	116094.378024	56.706650
2699.624779	115768.410217	56.711655
2699.243907	115436.188020	56.716660
2698.445935	115106.600436	56.721665
2697.703312	114784.586557	56.726669
2696.904577	114465.568678	56.731674
2696.416224	114126.519860	56.736679
2696.009517	113797.147641	56.741684
2695.191101	113479.795531	56.746689
2694.835596	113140.485146	56.751693
2694.167495	112814.562642	56.756698
2693.257795	112487.768815	56.761703
2692.587617	112148.731226	56.766708
2692.014340	111831.323212	56.771713
2691.071855	111496.627675	56.776717
2690.352233	111177.429930	56.781722
2689.978806	110858.422612	56.786727
2689.434276	110518.150053	56.791732
2688.577624	110194.328965	56.796737
2688.362141	109860.815992	56.801741
2687.285244	109541.366153	56.806746
2686.406141	109203.379475	56.811751
2686.267752	108871.409752	56.816756
2685.457768	108552.063859	56.821761
2684.680185	108216.194149	56.826765
2683.684612	107885.039981	56.831770
2683.428579	107559.147414	56.836775
2682.905697	107222.458040	56.841780
2681.903276	106906.717550	56.846785
2681.604955	106576.663733	56.851789
2680.774957	106243.253540	56.856794
2679.958936	105909.338214	56.861799
2679.306644	105583.433751	56.866804
2678.631815	105266.641547	56.871809
2677.722650	104934.264617	56.876813
2676.974432	104614.111220	56.881818
2676.535808	104285.056661	56.886823
2676.195586	103963.432677	56.891828
2675.192469	103642.596911	56.896833
2674.658515	103313.374343	56.901837
2674.386833	102982.452754	56.906842
2673.712402	102644.456627	56.911847
2672.766667	102314.977096	56.916852
2672.005296	101994.785303	56.921857
2671.673970	101653.456855	56.926861
2670.570764	101331.590236	56.931866
2669.824260	101000.169354	56.936871
2669.613876	100670.311145	56.941876
2668.631315	100352.244909	56.946881
2668.177507	100017.474289	56.951885
2667.494703	99704.761026	56.956890
2666.662947	99370.459296	56.961895
2665.924462	99040.086483	56.966900
2665.345477	98716.587599	56.971905
2664.866231	98380.950546	56.976909
2663.888674	98063.517755	56.981914
2663.284590	97730.491426	56.986919
2663.020848	97402.014187	56.991924
2661.827304	97083.214971	56.996929
2661.592731	96746.859267	57.001933
2661.073082	96431.158862	57.006938
2659.617912	96100.029044	57.011943
2659.414272	95775.034914	57.016948
2658.722172	95451.473658	57.021953
2658.283247	95121.161164	57.026957
2657.437320	94795.319050	57.031962
2656.882505	94475.352118	57.036967
2656.122942	94133.227491	57.041972
2655.105230	93822.944059	57.046977
2654.368175	93498.067506	57.051981
2653.940778	93186.006335	57.056986
2653.362751	92856.802038	57.061991
2652.760696	92533.966353	57.066996
2652.100110	92209.058537	57.072001
2651.401507	91881.669635	57.077005
2650.704495	91563.770899	57.082010
2649.751909	91236.273332	57.087015
2649.632385	90904.692230	57.092020
2648.651612	90600.516022	57.097025
2648.026740	90267.236680	57.102029
2647.466414	89937.566078	57.107034
2646.726184	89613.844232	57.112039
2646.195794	89292.033980	57.117044
2645.323059	88968.177913	57.122049
2644.824741	88649.110936	57.127053
2644.035229	88324.985035	57.132058
2643.205054	88005.523689	57.137063
2642.703911	87679.491617	57.142068
2642.007066	87364.576738	57.147073
2641.536268	87035.139039	57.152077
2640.636160	86707.137356	57.157082
2640.444027	86388.600547	57.162087
2639.484534	86058.589711	57.167092
2638.472437	85748.838775	57.172097
2638.053337	85412.451443	57.177101
2637.345135	85099.156452	57.182106
2636.363832	84778.455149	57.187111
2636.337216	84458.875126	57.192116
2635.260937	84143.782728	57.197121
2634.706874	83806.009805	57.202125
2634.229301	83498.171962	57.207130
2633.553086	83170.880330	57.212135
2633.225638	82848.374452	57.217140
2632.322297	82522.269774	57.222145
2631.636257	82192.364729	57.227149
2630.822478	81863.258339	57.232154
2630.032990	81541.790148	57.237159
2629.699743	81219.963096	57.242164
2628.883046	80898.433107	57.247169
2628.087509	80581.150770	57.252173
2627.339074	80251.964476	57.257178
2626.615554	79938.856819	57.262183
2626.442214	79615.077509	57.267188
2625.366970	79297.339570	57.272193
2624.702601	78978.489510	57.277197
2624.153905	78653.973682	57.282202
2623.359868	78330.103849	57.287207
2622.937844	78001.408761	57.292212
2621.898724	77697.833072	57.297217
2621.333355	77369.823518	57.302221
2620.764531	77050.183650	57.307226
2619.786162	76734.694191	57.312231
2619.606371	76408.210406	57.317236
2618.699514	76098.276233	57.322241
2618.279758	75762.431981	57.327245
2617.717555	75454.068706	57.332250
2616.636940	75138.987798	57.337255
2616.370829	74811.276352	57.342260
2615.468462	74501.473704	57.347265
2614.929793	74173.125291	57.352269
2614.028618	73852.150584	57.357274
2613.491603	73521.310170	57.362279
2612.896779	73209.236133	57.367284
2611.967502	72900.210077	57.372289
2611.331739	72574.468976	57.377293
2610.687916	72263.450105	57.382298
2609.940600	71950.317731	57.387303
2609.602288	71621.295456	57.392308
2609.043723	71310.639094	57.397313
2608.017860	70994.094718	57.402317
2607.641551	70679.485778	57.407322
2606.933032	70340.769777	57.412327
2606.278779	70023.707049	57.417332
2605.159456	69720.550116	57.422337
2604.754405	69388.820446	57.427341
2604.190766	69065.881064	57.432346
2603.172314	68771.349383	57.437351
2602.569721	68439.249119	57.442356
2602.003008	68133.502165	57.447361
2601.215512	67812.538050	57.452365
2600.581082	67498.040189	57.457370
2599.751869	67200.259713	57.462375
2599.361029	66875.825195	57.467380
2598.443793	66579.420325	57.472385
2597.852476	66259.692117	57.477389
2597.520408	65942.572030	57.482394
2596.667837	65647.694259	57.487399
2596.188679	65313.829626	57.492404
2595.534199	64997.862250	57.497409
2595.045795	64680.521824	57.502413
2594.017584	64360.888148	57.507418
2593.626778	64053.965429	57.512423
2592.828394	63728.967978	57.517428
2591.780675	63430.169361	57.522433
2591.195027	63116.938599	57.527437
2590.757578	62805.012836	57.532442
2589.769847	62492.932487	57.537447
2589.308157	62178.959958	57.542452
2588.806906	61874.261676	57.547457
2588.326854	61549.960260	57.552461
2587.477403	61254.865190	57.557466
2586.626202	60928.651654	57.562471
2586.084917	60607.063722	57.567476
2585.049021	60309.233790	57.572481
2584.548367	60001.792869	57.577485
2584.169238	59697.271983	57.582490
2583.023732	59378.507267	57.587495
2582.814318	59057.694196	57.592500
2581.801686	58767.206289	57.597505
2581.024445	58452.871420	57.602509
2580.419622	58143.787511	57.607514
2579.479279	57843.269428	57.612519
2579.252320	57538.424299	57.617524
2578.555837	57247.511329	57.622529
2577.649121	56930.475715	57.627533
2577.463251	56620.309655	57.632538
2576.491554	56320.428983	57.637543
2575.879105	56014.818837	57.642548
2574.963687	55716.011947	57.647553
2574.452109	55403.952818	57.652557
2573.930228	55100.628388	57.657562
2573.001796	54810.309776	57.662567
2572.479939	54498.831010	57.667572
2571.838268	54189.376435	57.672577
2571.173770	53895.752289	57.677581
2570.556657	53577.251150	57.682586
2569.943056	53281.581597	57.687591
2569.212166	52975.987368	57.692596
2568.266200	52685.411231	57.697601
2567.626549	52371.067199	57.702605
2566.965860	52069.843556	57.707610
2566.214316	51776.188508	57.712615
2565.830539	51474.475329	57.717620
2564.699676	51180.766737	57.722625
2564.153916	50885.571827	57.727629
2563.595976	50579.440368	57.732634
2562.792285	50287.909172	57.737639
2562.213236	50000.013770	57.742644
2561.525617	49696.499511	57.747649
2561.153571	49401.440781	57.752653
2560.281982	49097.114909	57.757658
2559.335986	48814.225519	57.762663
2558.841004	48510.318198	57.767668
2558.404172	48226.506536	57.772673
2557.453582	47933.721279	57.777677
2556.925605	47629.790017	57.782682
2556.064785	47340.476728	57.787687
2555.375086	47047.066991	57.792692
2554.394761	46752.474620	57.797697
2553.990338	46472.127436	57.802701
2553.632812	46168.883906	57.807706
2553.034340	45893.627936	57.812711
2552.286545	45592.594348	57.817716
2551.366802	45298.816993	57.822721
2550.675505	45014.136016	57.827725
2550.187564	44718.402348	57.832730
2549.071201	44433.643253	57.837735
2548.497523	44149.008370	57.842740
2547.529388	43872.324846	57.847745
2547.100533	43579.646688	57.852749
2546.456405	43294.837742	57.857754
2545.444714	43014.765722	57.862759
2545.134446	42728.781047	57.867764
2544.321458	42454.707662	57.872769
2543.587820	42179.857637	57.877773
2543.142241	41886.287435	57.882778
2542.310715	41616.565648	57.887783
2541.690719	41330.890425	57.892788
2540.921563	41062.362717	57.897793
2540.258578	40774.302030	57.902797
2540.057405	40496.270533	57.907802
2539.276080	40220.563039	57.912807
2538.501628	39938.204891	57.917812
2538.140854	39657.505838	57.922817
2537.121749	39384.423215	57.927821
2536.647597	39096.057392	57.932826
2535.555505	38814.776788	57.937831
2535.306684	38535.178745	57.942836
2534.091467	38268.520402	57.947841
2533.369442	37986.202181	57.952845
2533.080126	37707.945693	57.957850
2532.288748	37450.685616	57.962855
2531.525834	37168.441283	57.967860
2530.774680	36899.650868	57.972865
2530.155573	36635.885906	57.977869
2529.819705	36355.025858	57.982874
2528.991988	36082.212815	57.987879
2528.284767	35801.286549	57.992884
2527.538392	35528.422209	57.997889
2526.683226	35259.086611	58.002893
2526.173587	34980.187929	58.007898
2525.190346	34739.235664	58.012903
2524.559451	34460.876936	58.017908
2523.773150	34189.153406	58.022913
2522.806694	33935.309620	58.027917
2522.505517	33676.964662	58.032922
2521.873988	33420.226352	58.037927
2521.083596	33169.116077	58.042932
2520.289198	32897.824254	58.047937
2519.703482	32653.599742	58.052941
2519.151180	32376.883232	58.057946
2518.091644	32134.721477	58.062951
2517.419870	31880.238326	58.067956
2517.013073	31611.277994	58.072961
2515.964970	31365.579955	58.077965
2515.382116	31113.308278	58.082970
2514.462566	30871.665926	58.087975
2513.872446	30621.665581	58.092980
2512.997488	30379.999707	58.097985
2512.347613	30140.529487	58.102989
2511.584175	29893.081482	58.107994
2510.556092	29654.643684	58.112999
2509.884423	29419.461193	58.118004
2509.095920	29194.389745	58.123009
2508.110509	28958.849708	58.128013
2507.404728	28734.743116	58.133018
2506.744995	28524.642135	58.138023
2505.689025	28291.644343	58.143028
2505.046293	28076.432672	58.148033
2503.630446	27867.995598	58.153037
2503.273258	27670.249321	58.158042
2501.914696	27471.319074	58.163047
2501.247457	27276.394424	58.168052
2499.992975	27098.583092	58.173057
2498.787587	26912.667805	58.178061
2497.971029	26744.606970	58.183066
2496.853608	26577.337218	58.188071
2496.144879	26422.820599	58.193076
2495.226452	26273.491356	58.198081
2494.068144	26117.579915	58.203085
2493.456547	25975.314504	58.208090
2492.612697	25830.534613	58.213095
2492.138234	25696.777948	58.218100
2491.335334	25551.848762	58.223105
2490.439190	25436.947230	58.228109
2489.484044	25290.189406	58.233114
2488.854667	25163.650061	58.238119
2488.125654	25046.817603	58.243124
2487.194863	24920.065775	58.248129
2486.371853	24823.784485	58.253133
2485.979525	24694.379311	58.258138
2484.590247	24596.665790	58.263143
2484.212852	24487.146580	58.268148
2483.676314	24386.243771	58.273153
2482.914661	24270.162125	58.278157
2482.417356	24167.327613	58.283162
2481.581782	24075.754677	58.288167
2480.814644	23963.003107	58.293172
2480.270051	23862.453932	58.298177
2479.356941	23766.505238	58.303181
2479.018196	23667.203938	58.308186
2477.910611	23572.176417	58.313191
2477.394316	23475.646180	58.318196
2476.969184	23388.494251	58.323201
2476.193164	23277.993941	58.328205
2475.548589	23202.715485	58.333210
2474.488662	23113.648153	58.338215
2473.884182	23025.755957	58.343220
2473.222343	22939.154129	58.348225
2472.661695	22863.607347	58.353229
2472.449920	22761.328100	58.358234
2471.755656	22691.367024	58.363239
2470.827831	22603.434469	58.368244
2469.995536	22508.886882	58.373249
2469.667261	22416.264771	58.378253
2469.167548	22323.413759	58.383258
2468.402543	22250.046869	58.388263
2468.104786	22149.314661	58.393268
2467.346619	22056.221940	58.398273
2466.582430	21970.385437	58.403277
2466.194738	21888.436040	58.408282
2465.163113	21788.477834	58.413287
2464.670094	21705.510162	58.418292
2464.272972	21616.609907	58.423297
2463.434793	21528.545956	58.428301
2463.350603	21444.213641	58.433306
2462.310969	21355.801237	58.438311
2461.682107	21254.324258	58.443316
2461.234570	21167.460516	58.448321
2460.123446	21073.657383	58.453325
2459.629142	20975.170602	58.458330
2458.694718	20898.621877	58.463335
2458.212650	20813.475297	58.468340
2457.598850	20716.081264	58.473345
2456.838611	20636.849849	58.478349
2456.361182	20537.812445	58.483354
2455.497057	20459.771219	58.488359
2455.010838	20367.809899	58.493364
2454.222011	20288.175420	58.498369
2453.058976	20228.125753	58.503373
2452.658421	20129.489673	58.508378
2452.069900	20045.702724	58.513383
2451.204739	19976.772412	58.518388
2450.842955	19890.637152	58.523393
2450.018462	19815.716832	58.528397
2449.252099	19729.586208	58.533402
2449.258156	19646.635154	58.538407
2448.363301	19583.983222	58.543412
2447.933596	19482.048375	58.548417
2447.298121	19391.330647	58.553421
2446.776549	19308.622141	58.558426
2446.096392	19214.378147	58.563431
2445.223192	19127.073744	58.568436
2444.562654	19045.608749	58.573441
2443.726341	18974.286291	58.578445
2443.466163	18881.078198	58.583450
2442.321321	18800.483069	58.588455
2441.696541	18716.723603	58.593460
2441.249362	18628.804615	58.598465
2440.612871	18555.299258	58.603469
2439.920372	18462.938598	58.608474
2439.266817	18379.683231	58.613479
2438.752671	18303.894071	58.618484
2438.138874	18213.518416	58.623489
2437.434381	18128.104394	58.628493
2436.859309	18050.292656	58.633498
2436.144485	17968.670609	58.638503
2435.329300	17872.919215	58.643508
2434.690800	17788.133630	58.648513
2433.482839	17707.699033	58.653517
2433.321937	17634.053165	58.658522
2432.760958	17554.911395	58.663527
2431.876513	17463.541455	58.668532
2430.951385	17388.837041	58.673537
2430.563174	17310.975902	58.678541
2430.221776	17229.039438	58.683546
2429.151058	17149.399207	58.688551
2428.599850	17078.598126	58.693556
2427.931209	16980.180191	58.698561
2427.287032	16912.799994	58.703565
2426.543539	16836.589061	58.708570
2425.795752	16753.145437	58.713575
2425.227132	16682.507979	58.718580
2425.094556	16609.697787	58.723585
2424.106346	16521.314734	58.728589
2423.429895	16441.014782	58.733594
2422.524265	16368.723150	58.738599
2421.890971	16286.769292	58.743604
2421.685822	16207.097319	58.748609
2420.338393	16136.997463	58.753613
2419.876264	16066.854637	58.758618
2419.200308	15992.085709	58.763623
2418.534536	15903.766462	58.768628
2417.753072	15838.935855	58.773633
2417.292561	15760.109771	58.778637
2416.945697	15682.764890	58.783642
2416.226884	15604.861479	58.788647
2415.214526	15533.180177	58.793652
2415.003850	15448.782769	58.798657
2414.207986	15381.438649	58.803661
2413.395081	15297.443102	58.808666
2412.475636	15227.449227	58.813671
2411.969881	15152.860723	58.818676
2411.436569	15075.676120	58.823681
2410.762169	15006.114786	58.828685
2410.396652	14917.082062	58.833690
2409.325421	14848.464355	58.838695
2408.495090	14763.433706	58.843700
2408.168209	14691.457965	58.848705
2407.321029	14625.095056	58.853709
2406.756653	14553.153948	58.858714
2406.070985	14475.716453	58.863719
2405.520492	14403.988312	58.868724
2404.820097	14336.381301	58.873729
2403.797954	14261.545876	58.878733
2403.386474	14183.469852	58.883738
2402.616115	14110.073695	58.888743
2401.980255	14040.282171	58.893748
2401.491584	13966.733721	58.898753
2400.728497	13894.206212	58.903757
2400.234621	13824.804221	58.908762
2399.297732	13758.897390	58.913767
2398.829656	13678.520556	58.918772
2398.023724	13609.095142	58.923777
2396.958664	13543.150282	58.928781
2396.801649	13464.951168	58.933786
2396.191840	13399.457755	58.938791
2395.773215	13320.378742	58.943796
2395.095791	13250.529358	58.948801
2394.296642	13178.356840	58.953805
2393.887876	13097.466742	58.958810
2392.744202	13031.385842	58.963815
2392.302668	12957.054436	58.968820
2392.105076	12877.260473	58.973825
2390.647639	12805.661270	58.978829
2390.268033	12732.449188	58.983834
2389.533664	12652.737772	58.988839
2388.736925	12591.956712	58.993844
2388.205556	12520.724336	58.998849
2387.587638	12448.841990	59.003853
2386.582414	12373.562787	59.008858
2385.940049	12313.749469	59.013863
2385.126727	12241.902837	59.018868
2385.049013	12176.612417	59.023873
2384.038887	12117.534043	59.028877
2383.893064	12043.642345	59.033882
2382.850458	11966.338028	59.038887
2382.127206	11900.450659	59.043892
2381.697872	11834.548137	59.048897
2380.846755	11763.798091	59.053901
2380.517262	11685.279410	59.058906
2379.548323	11614.438672	59.063911
2378.985300	11551.878146	59.068916
2378.573224	11471.711131	59.073921
2377.906563	11413.174412	59.078925
2377.181406	11325.858157	59.083930
2376.417534	11257.238897	59.088935
2375.640568	11195.350133	59.093940
2375.381076	11131.326108	59.098945
2374.399218	11055.137246	59.103949
2373.631645	10980.283945	59.108954
2373.214396	10927.342406	59.113959
2372.514071	10847.408254	59.118964
2371.869956	10763.501609	59.123969
2371.011903	10695.241089	59.128973
2370.451857	10627.603883	59.133978
2369.636847	10554.093838	59.138983
2368.906034	10492.906402	59.143988
2368.540366	10405.551091	59.148993
2367.581761	10340.421499	59.153997
2367.197898	10276.892243	59.159002
2366.129618	10208.715791	59.164007
2365.675115	10144.189975	59.169012
2365.096034	10078.577256	59.174017
2364.266142	10014.552565	59.179021
2363.695682	9948.378086	59.184026
2363.553272	9873.105503	59.189031
2362.426131	9797.366964	59.194036
2361.798948	9735.342896	59.199041
2361.177446	9664.092921	59.204045
2360.612434	9590.308102	59.209050
2359.986094	9531.393214	59.214055
2359.045217	9454.485260	59.219060
2358.591988	9382.448211	59.224065
2357.777679	9317.980241	59.229069
2357.310771	9245.444650	59.234074
2356.771131	9173.209297	59.239079
2355.714951	9111.182866	59.244084
2355.005041	9039.675332	59.249089
2353.970289	8985.168015	59.254093
2353.833304	8916.059257	59.259098
2352.998760	8854.197158	59.264103
2352.484825	8783.006499	59.269108
2352.091143	8712.573391	59.274113
2351.489357	8653.983486	59.279117
2350.518172	8575.010438	59.284122
2349.910076	8507.261027	59.289127
2348.949520	8439.051095	59.294132
2348.814583	8373.718572	59.299137
2347.679504	8313.323217	59.304141
2347.256080	8234.277332	59.309146
2346.554761	8181.046183	59.314151
2345.795916	8101.340262	59.319156
2345.524029	8040.586659	59.324161
2344.361026	7979.459492	59.329165
2343.929155	7910.110266	59.334170
2343.406713	7854.987041	59.339175
2342.491794	7780.141726	59.344180
2341.954574	7712.453709	59.349185
2341.014205	7654.956792	59.354189
2340.470621	7576.317619	59.359194
2339.610632	7520.672517	59.364199
2339.248975	7458.595277	59.369204
2338.893530	7386.484895	59.374209
2337.803192	7325.860059	59.379213
2337.379224	7261.427815	59.384218
2336.552669	7183.251308	59.389223
2336.004265	7121.934752	59.394228
2335.347578	7062.979991	59.399233
2334.467726	7004.392158	59.404237
2334.072416	6932.142792	59.409242
2333.412090	6871.850753	59.414247
2332.550828	6799.474782	59.419252
2332.305328	6744.987756	59.424257
2331.247238	6668.049661	59.429261
2330.805562	6598.017906	59.434266
2330.407360	6532.666580	59.439271
2329.601876	6470.080940	59.444276
2328.735474	6396.791968	59.449281
2327.962244	6329.679713	59.454285
2327.403001	6272.979592	59.459290
2326.672535	6204.140013	59.464295
2325.898708	6151.684859	59.469300
2325.263671	6078.735434	59.474305
2324.579535	6015.880854	59.479309
2324.178689	5957.063445	59.484314
2323.565613	5884.564242	59.489319
2322.636526	5827.029247	59.494324
2321.855639	5755.342891	59.499329
2320.921632	5707.778934	59.504333
2320.620829	5630.369619	59.509338
2320.096473	5577.667133	59.514343
2319.017815	5513.941024	59.519348
2318.589335	5447.702496	59.524353
2318.050087	5393.855421	59.529357
2317.591609	5320.013347	59.534362
2317.040031	5266.126891	59.539367
2316.186058	5189.115221	59.544372
2315.819581	5132.575829	59.549377
2314.688141	5065.849501	59.554381
2314.455775	4992.767436	59.559386
2313.362664	4930.409821	59.564391
2312.813348	4866.881760	59.569396
2312.426135	4809.938346	59.574401
2311.260501	4741.382823	59.579405
2310.849089	4681.160407	59.584410
2310.238220	4628.512892	59.589415
2309.600410	4544.902895	59.594420
2309.122551	4490.484687	59.599425
2308.027903	4427.403863	59.604429
2307.489311	4361.393524	59.609434
2306.822648	4290.935972	59.614439
2306.090585	4240.922722	59.619444
2305.449882	4172.964063	59.624449
2304.706577	4105.041707	59.629453
2304.097988	4041.493488	59.634458
2303.400158	3978.960500	59.639463
2302.761230	3926.434305	59.644468
2302.366674	3873.173953	59.649473
2301.498049	3814.767361	59.654477
2300.817829	3747.420253	59.659482
2300.108636	3688.398185	59.664487
2299.416562	3628.412293	59.669492
2298.507368	3566.589660	59.674497
2297.739509	3507.218800	59.679501
2297.593570	3443.677866	59.684506
2296.892623	3394.659392	59.689511
2296.206842	3332.029463	59.694516
2295.938892	3262.363745	59.699521
2294.787067	3197.450349	59.704525
2294.103333	3142.971216	59.709530
2293.352508	3079.676846	59.714535
2292.627707	3025.017766	59.719540
2292.169699	2963.088269	59.724545
2291.146603	2916.636550	59.729549
2290.642328	2874.261739	59.734554
2290.289867	2797.224871	59.739559
2289.279704	2745.554331	59.744564
2288.970518	2684.715894	59.749569
2288.118703	2625.315406	59.754573
2287.570742	2562.395644	59.759578
2287.209062	2506.206271	59.764583
2286.337005	2453.152205	59.769588
2285.567798	2388.443529	59.774593
2284.594891	2323.443349	59.779597
2284.125467	2274.488119	59.784602
2283.591656	2210.751467	59.789607
2282.376668	2166.186482	59.794612
2282.388206	2095.617733	59.799617
2281.406328	2042.998148	59.804621
2280.880809	1988.558160	59.809626
2280.388781	1931.433591	59.814631
2279.635154	1879.993539	59.819636
2279.307986	1821.474345	59.824641
2278.304889	1754.234162	59.829645
2277.321018	1705.304093	59.834650
2276.797396	1637.406463	59.839655
2275.820376	1597.458586	59.844660
2275.420542	1520.497477	59.849665
2274.395029	1486.015748	59.854669
2274.023584	1432.198413	59.859674
2273.632833	1375.807476	59.864679
2272.634097	1328.858628	59.869684
2272.266225	1269.010796	59.874689
2271.514988	1220.886011	59.879693
2270.814545	1163.202985	59.884698
2270.004014	1105.707177	59.889703
2268.999372	1065.252625	59.894708
2268.750104	991.713013	59.899713
2267.436464	960.162549	59.904718
2267.092532	903.379659	59.909722
2266.714666	852.459243	59.914727
2265.637670	807.472059	59.919732
2265.242153	754.597772	59.924737
2264.097209	707.745094	59.929742
2263.800872	664.351833	59.934746
2263.345807	612.476258	59.939751
2262.187653	573.807304	59.944756
2261.802129	521.408519	59.949761
2260.814582	470.120959	59.954766
2260.150490	437.945069	59.959770
2259.386088	400.511933	59.964775
2258.407952	368.062744	59.969780
2258.269665	321.089491	59.974785
2257.425653	288.232863	59.979790
2256.725725	233.003980	59.984794
2255.884763	202.403614	59.989799
2255.091705	165.994311	59.994804
2254.773673	126.177776	59.999809
2253.944500	103.941165	60.004814
2253.027399	80.781865	60.009818
2252.862988	47.817985	60.014823
2251.869833	5.126989	60.019828
2250.936911	-20.246730	60.024833
2246.685374	59.027341	60.029838
2245.001259	61.896407	60.034842
2245.429756	56.520704	60.039847
2246.039794	64.343113	60.044852
2246.217426	45.364001	60.049857
2245.468297	54.788086	60.054862
2245.155383	57.166842	60.059866
2244.738866	67.402306	60.064871
2243.388054	75.672953	60.069876
2242.400151	62.561806	60.074881
2241.483530	74.975440	60.079886
2241.459652	76.177723	60.084890
2241.152731	68.865566	60.089895
2239.743761	69.847612	60.094900
2239.606780	64.602605	60.099905
2238.983585	84.791055	60.104910
2237.946667	76.738443	60.109914
2237.365417	68.946278	60.114919
2236.898088	83.206142	60.119924
2236.781079	69.542120	60.124929
2236.009870	69.445331	60.129934
2234.915285	83.290632	60.134938
2234.270359	77.790320	60.139943
2233.488824	79.010293	60.144948
2233.192324	69.660723	60.149953
2232.531131	71.350441	60.154958
2232.105764	80.075084	60.159962
2231.334500	72.614246	60.164967
2230.440325	80.446627	60.169972
2229.697537	83.505413	60.174977
2228.921976	80.078931	60.179982
2228.510345	76.742946	60.184986
2228.418263	81.467775	60.189991
2227.903985	72.080215	60.194996
2226.613638	80.059018	60.200001
2225.613842	73.290419	60.205006
2225.158794	85.219277	60.210010
2224.851884	68.587721	60.215015
2223.783424	81.031758	60.220020
2223.040235	87.868831	60.225025
2222.565028	80.447756	60.230030
2222.144354	80.235442	60.235034
2221.826705	86.123529	60.240039
2220.863779	82.181169	60.245044
2220.586269	66.557314	60.250049
2219.238388	85.701716	60.255054
2218.690742	79.511068	60.260058
2218.455663	66.975911	60.265063
2217.629723	85.701638	60.270068
2216.840147	73.666007	60.275073
2215.991765	78.999647	60.280078
2215.002057	81.386430	60.285082
2214.425470	70.414528	60.290087
2213.641274	80.820289	60.295092
2213.674144	79.635625	60.300097
2213.640456	79.488073	60.305102
2212.080305	81.632629	60.310106
2211.649818	78.868894	60.315111
2211.149036	80.313983	60.320116
2210.430946	78.538852	60.325121
2209.230376	71.740613	60.330126
2208.702564	79.846025	60.335130
2208.823126	79.904228	60.340135
2208.146732	74.853599	60.345140
2207.189721	79.554797	60.350145
2205.977780	62.581148	60.355150
2205.302426	77.807524	60.360154
2205.246705	64.887542	60.365159
2204.448283	73.220376	60.370164
2203.898071	72.252788	60.375169
2203.324718	70.795306	60.380174
2202.552661	75.998574	60.385178
2201.857978	68.139262	60.390183
2201.277399	75.147648	60.395188
2200.710958	73.837297	60.400193
2199.774665	70.300714	60.405198
2198.409922	79.109733	60.410202
2198.447218	68.095640	60.415207
2197.792859	85.244070	60.420212
2197.078183	70.913235	60.425217
2196.641415	70.250913	60.430222
2195.479217	80.335039	60.435226
2195.326136	67.116702	60.440231
2194.418178	70.599072	60.445236
2193.744641	80.657713	60.450241
2193.283572	75.041516	60.455246
2192.440259	79.141234	60.460250
2192.022368	71.726847	60.465255
2191.282621	73.597763	60.470260
2190.712448	71.764481	60.475265
2190.111911	79.141873	60.480270
2189.403725	74.372248	60.485274
2189.184390	70.490123	60.490279
2188.110802	79.252956	60.495284
2187.481528	69.691274	60.500289
2186.044713	71.873044	60.505294
2185.701941	82.889995	60.510298
2185.427274	67.431271	60.515303
2184.652491	80.651860	60.520308
2184.307453	75.149716	60.525313
2183.809764	77.665024	60.530318
2182.400878	79.372455	60.535322
2181.967758	77.615197	60.540327
2181.239596	74.483974	60.545332
2181.167345	76.647947	60.550337
2179.647695	70.348182	60.555342
2179.042955	76.680767	60.560346
2179.253919	70.070171	60.565351
2178.033324	79.043978	60.570356
2176.884418	66.097171	60.575361
2177.072046	71.766326	60.580366
2176.186718	81.046474	60.585370
2175.113009	68.936100	60.590375
2174.830201	78.940636	60.595380
2174.175187	73.544442	60.600385
2173.297566	80.530577	60.605390
2172.748799	75.682050	60.610394
2172.522927	71.766273	60.615399
2171.804851	74.628771	60.620404
2171.018245	70.951761	60.625409
2170.273626	71.013192	60.630414
2169.305552	77.892257	60.635418
2169.083960	66.252220	60.640423
2168.563174	72.662945	60.645428
2168.097911	69.158871	60.650433
2167.531266	72.098264	60.655438
2165.978839	78.264254	60.660442
2165.262872	76.734794	60.665447
2164.318489	74.582435	60.670452
2164.520426	69.146474	60.675457
2163.951940	69.284036	60.680462
2162.623465	84.767004	60.685466
2161.984113	66.325911	60.690471
2161.481262	79.274711	60.695476
2161.353165	65.051096	60.700481
2160.366652	68.779318	60.705486
2159.415046	76.373256	60.710490
2159.210484	66.390979	60.715495
2158.375732	75.281498	60.720500
2157.887921	78.555301	60.725505
2157.814706	72.221593	60.730510
2156.822166	82.001284	60.735514
2155.711946	63.701135	60.740519
2154.633174	76.954187	60.745524
2153.778362	77.619707	60.750529
2154.249814	65.987981	60.755534
2153.316729	64.286401	60.760538
2152.611172	61.421251	60.765543
2151.793541	78.100439	60.770548
2151.034085	65.252699	60.775553
2150.717522	74.718563	60.780558
2149.840336	70.661711	60.785562
2149.549684	67.683424	60.790567
2148.586075	72.995939	60.795572
2147.598560	79.622642	60.800577
2147.093370	68.756125	60.805582
2145.988440	79.342090	60.810586
2146.178856	68.254825	60.815591
2145.218210	70.982358	60.820596
2144.224868	77.744020	60.825601
2143.829865	76.393865	60.830606
2143.161990	73.243628	60.835610
2142.558777	69.387726	60.840615
2142.032977	66.706936	60.845620
2141.659490	75.163165	60.850625
2141.278405	75.805562	60.855630
2140.498307	78.731523	60.860634
2139.322646	63.139818	60.865639
2138.506716	76.106753	60.870644
2137.865421	71.376993	60.875649
2137.283486	65.242273	60.880654
2136.191116	74.993652	60.885658
2136.114986	69.975532	60.890663
2135.558354	70.404519	60.895668
2134.886465	61.548182	60.900673
2134.252237	68.577701	60.905678
2132.915148	65.107893	60.910682
2132.357229	67.503459	60.915687
2132.124838	77.927330	60.920692
2131.355438	80.305993	60.925697
2130.627847	69.219314	60.930702
2129.927263	75.198123	60.935706
2129.508869	70.073468	60.940711
2128.791153	68.976363	60.945716
2128.393155	69.734980	60.950721
2127.620681	71.191654	60.955726
2127.066891	72.350290	60.960730
2126.018701	78.868359	60.965735
2125.209290	70.850666	60.970740
2124.345139	78.451237	60.975745
2124.036143	69.059522	60.980750
2123.088065	63.566351	60.985754
2123.081715	71.279957	60.990759
2122.475980	68.258633	60.995764
2121.837593	76.685937	61.000769
2121.627126	70.747733	61.005774
2120.183491	72.418133	61.010778
2119.362989	76.891125	61.015783
2118.761081	79.938621	61.020788
2117.972197	75.169209	61.025793
2117.746842	71.849419	61.030798
2116.917290	75.095455	61.035802
2116.415412	82.441436	61.040807
2116.062691	72.624592	61.045812
2114.767933	73.219589	61.050817
2114.158587	67.619058	61.055822
2113.172448	70.650255	61.060826
2112.926574	78.483868	61.065831
2112.205525	73.211707	61.070836
2111.473940	78.299769	61.075841
2111.196201	72.704963	61.080846
2110.517037	75.670106	61.085850
2110.065456	71.670309	61.090855
2108.785454	76.172063	61.095860
2107.998138	73.472855	61.100865
2107.506534	75.272880	61.105870
2106.587383	89.074614	61.110874
2106.226083	78.581068	61.115879
2105.942609	84.186206	61.120884
2105.453192	82.682312	61.125889
2105.067538	63.590738	61.130894
2103.380937	85.209437	61.135898
2102.812726	74.701421	61.140903
2102.241731	79.634699	61.145908
2101.785652	72.518117	61.150913
2101.228272	76.774327	61.155918
2100.625710	70.955112	61.160922
2100.216357	67.222996	61.165927
2098.995189	78.702590	61.170932
2098.205390	70.497300	61.175937
2097.709833	72.728443	61.180942
2096.880633	70.007502	61.185946
2096.564118	73.345590	61.190951
2095.746330	66.433060	61.195956
2095.540232	76.371807	61.200961
2095.209596	61.842896	61.205966
2093.576965	76.033791	61.210970
2092.805099	59.401952	61.215975
2092.273357	75.351412	61.220980
2091.606416	73.021021	61.225985
2091.208539	68.766713	61.230990
2090.631319	67.620517	61.235994
2090.258268	75.617806	61.240999
2089.623297	62.256777	61.246004
2088.325321	73.701253	61.251009
2088.212890	70.125438	61.256014
2087.291599	78.632332	61.261018
2087.050248	64.097137	61.266023
2085.886198	73.341110	61.271028
2084.813420	75.187634	61.276033
2084.411456	72.170251	61.281038
2083.255451	73.619993	61.286042
2082.977190	74.510997	61.291047
2082.637580	76.116604	61.296052
2082.002096	74.804621	61.301057
2081.567361	75.955411	61.306062
2080.963382	76.773530	61.311066
2080.566061	70.475494	61.316071
2079.696534	66.062655	61.321076
2078.744921	63.257072	61.326081
2078.233626	63.261003	61.331086
2077.361175	73.895245	61.336090
2076.581996	64.116130	61.341095
2075.197012	76.697160	61.346100
2075.396554	66.601888	61.351105
2074.358529	69.505720	61.356110
2073.780080	76.557938	61.361114
2073.197066	62.485380	61.366119
2072.839031	68.362531	61.371124
2072.539797	74.887914	61.376129
2072.054876	66.746214	61.381134
2070.675616	75.707392	61.386138
2069.888231	72.185074	61.391143
2069.412768	73.408559	61.396148
2068.399606	76.097145	61.401153
2068.199781	70.359102	61.406158
2067.538530	83.881802	61.411162
2067.022353	59.561513	61.416167
2066.145316	73.506360	61.421172
2065.005760	78.299646	61.426177
2064.624274	66.771733	61.431182
2063.592842	77.877468	61.436186
2063.441840	68.589998	61.441191
2062.722785	66.286809	61.446196
2062.371642	77.339777	61.451201
2062.390118	67.378890	61.456206
2061.130220	67.613583	61.461210
2060.131524	69.036793	61.466215
2059.421385	76.303868	61.471220
2058.809351	75.136397	61.476225
2058.942350	73.607852	61.481230
2057.327767	85.378546	61.486234
2056.712306	76.954800	61.491239
2056.059116	78.966549	61.496244
2055.390605	73.041124	61.501249
2055.157028	70.490588	61.506254
2054.255783	76.360914	61.511258
2054.048995	70.609786	61.516263
2052.937346	68.159178	61.521268
2052.018946	78.234620	61.526273
2051.372571	68.707237	61.531278
2050.784737	71.424519	61.536282
2050.298549	69.678862	61.541287
2049.873650	65.419390	61.546292
2049.426349	77.034796	61.551297
2048.332880	68.276927	61.556302
2047.423483	69.118292	61.561306
2046.721954	64.059091	61.566311
2046.425394	74.091035	61.571316
2046.039664	69.694465	61.576321
2045.386092	61.142745	61.581326
2043.971870	67.390934	61.586330
2043.282366	69.682826	61.591335
2042.797611	65.803422	61.596340
2042.073566	79.941609	61.601345
2041.882006	67.967263	61.606350
2041.283987	68.730829	61.611354
2040.890168	67.888261	61.616359
2040.055741	69.227063	61.621364
2039.173910	70.748423	61.626369
2038.767330	70.559133	61.631374
2038.124791	67.770742	61.636378
2036.655923	63.470385	61.641383
2036.020982	77.220707	61.646388
2035.153317	77.875689	61.651393
2034.934768	64.443860	61.656398
2033.942939	86.890569	61.661402
2033.712365	73.613598	61.666407
2033.320150	88.440266	61.671412
2032.629500	76.970882	61.676417
2032.636645	73.584242	61.681422
2031.259751	77.043319	61.686426
2030.502170	68.566451	61.691431
2030.162405	78.072269	61.696436
2029.457011	80.245268	61.701441
2028.693764	79.120725	61.706446
2027.408228	78.780786	61.711450
2026.639727	80.028710	61.716455
2026.615953	68.041930	61.721460
2025.818134	75.715570	61.726465
2025.246432	80.316251	61.731470
2024.775004	78.142497	61.736474
2024.196364	76.439902	61.741479
2023.459291	68.719839	61.746484
2022.447982	87.784077	61.751489
2022.157364	71.444871	61.756494
2021.443382	74.852356	61.761498
2020.598203	72.097708	61.766503
2019.923054	78.974479	61.771508
2019.121793	70.739502	61.776513
2018.935422	71.508700	61.781518
2018.484849	83.242897	61.786522
2017.206326	74.285763	61.791527
2016.566506	66.903490	61.796532
2015.583354	77.640469	61.801537
2014.826256	67.313848	61.806542
2014.463693	74.041663	61.811546
2014.369635	81.341851	61.816551
2013.945745	75.093773	61.821556
2012.658459	75.738095	61.826561
2011.964265	71.661712	61.831566
2011.185268	75.234053	61.836570
2011.176813	70.564731	61.841575
2010.460003	71.489078	61.846580
2008.814524	73.593677	61.851585
2008.285181	65.194130	61.856590
2007.604836	69.443063	61.861594
2007.098584	80.878604	61.866599
2006.929892	70.458594	61.871604
2006.247129	78.380472	61.876609
2006.004215	68.298659	61.881614
2004.970120	76.602713	61.886618
2004.246913	77.301006	61.891623
2003.571304	68.796945	61.896628
2002.968178	83.147749	61.901633
2002.248427	64.921332	61.906638
2000.641468	85.418884	61.911642
2000.577359	68.531249	61.916647
1999.813097	70.426605	61.921652
1999.094075	74.166040	61.926657
1998.770951	62.307202	61.931662
1998.300137	73.661423	61.936666
1998.200041	67.702567	61.941671
1997.488267	72.929428	61.946676
1996.196146	63.684324	61.951681
1995.891086	61.214526	61.956686
1995.204463	72.573039	61.961690
1993.965652	71.654870	61.966695
1993.208378	66.752759	61.971700
1992.546960	69.213662	61.976705
1992.111853	70.096455	61.981710
1992.025001	70.859321	61.986714
1991.286560	69.823888	61.991719
1990.361987	68.053212	61.996724
1989.388433	76.975261	62.001729
1989.181545	59.687696	62.006734
1988.553214	76.196514	62.011738
1987.462051	69.016769	62.016743
1986.596679	74.742654	62.021748
1986.057058	73.945312	62.026753
1985.451493	76.532964	62.031758
1984.538679	71.948843	62.036762
1984.246917	77.394457	62.041767
1984.275515	70.771807	62.046772
1983.251698	82.423536	62.051777
1982.002127	56.862003	62.056782
1981.434733	78.866041	62.061786
1980.845865	62.411778	62.066791
1980.634850	73.817799	62.071796
1980.041813	70.537464	62.076801
1979.392594	66.441339	62.081806
1978.263662	77.982023	62.086810
1977.725817	77.033020	62.091815
1977.107811	71.123257	62.096820
1976.673940	77.055032	62.101825
1975.485049	58.660261	62.106830
1974.558932	76.820034	62.111834
1974.244906	71.191589	62.116839
1973.769990	73.936694	62.121844
1973.272427	68.651182	62.126849
1973.064148	72.191287	62.131854
1971.437893	65.750892	62.136858
1970.758866	74.495313	62.141863
1970.350216	63.414845	62.146868
1969.644252	79.976989	62.151873
1969.481900	65.003525	62.156878
1968.947754	73.445841	62.161882
1967.547400	73.527839	62.166887
1967.113954	72.631650	62.171892
1966.430592	83.617514	62.176897
1966.350463	78.574809	62.181902
1965.138872	70.420755	62.186906
1964.326044	63.991591	62.191911
1963.763999	73.636765	62.196916
1962.918225	82.265741	62.201921
1962.729289	68.975874	62.206926
1962.261367	66.162941	62.211930
1961.518011	67.829495	62.216935
1960.971368	61.003283	62.221940
1960.029555	65.725794	62.226945
1959.582357	60.170533	62.231950
1958.224775	78.403529	62.236954
1957.372572	65.065993	62.241959
1957.387273	68.285287	62.246964
1956.470673	72.202744	62.251969
1956.004430	65.008972	62.256974
1955.481780	71.677050	62.261978
1954.424174	61.361890	62.266983
1953.627095	62.297416	62.271988
1952.910782	66.020660	62.276993
1952.812657	70.200839	62.281998
1952.295060	70.475442	62.287002
1951.654987	63.922671	62.292007
1950.409885	66.883070	62.297012
1949.780665	68.183018	62.302017
1949.454176	73.427574	62.307022
1949.027017	66.202369	62.312026
1947.942115	71.791230	62.317031
1947.168954	60.200956	62.322036
1946.205415	80.545925	62.327041
1945.999107	63.726610	62.332046
1945.767933	73.997322	62.337050
1945.016069	61.911679	62.342055
1944.335523	73.147815	62.347060
1943.064352	74.612744	62.352065
1942.667142	74.339983	62.357070
1942.244663	68.150046	62.362074
1941.382710	64.751569	62.367079
1940.518034	61.750899	62.372084
1939.592713	67.216663	62.377089
1939.154701	70.255520	62.382094
1939.017738	70.412935	62.387098
1938.226412	70.234275	62.392103
1938.235440	57.140070	62.397108
1937.107045	61.512178	62.402113
1936.282570	65.503320	62.407118
1935.362633	63.474898	62.412122
1934.811720	63.273844	62.417127
1933.797714	61.842223	62.422132
1933.037383	69.530429	62.427137
1932.852409	65.242357	62.432142
1932.258813	61.243068	62.437146
1931.763369	74.137083	62.442151
1931.422849	57.744343	62.447156
1929.797207	71.644053	62.452161
1929.325389	71.165529	62.457166
1928.660731	59.064475	62.462170
1928.475010	71.480410	62.467175
1927.948515	66.071776	62.472180
1926.761226	73.889262	62.477185
1926.058871	63.516143	62.482190
1925.416462	75.001683	62.487194
1924.722636	67.902390	62.492199
1924.615861	69.653970	62.497204
1923.376100	67.371984	62.502209
1922.509480	64.994496	62.507214
1921.788994	73.409631	62.512218
1921.379871	71.979757	62.517223
1921.325212	58.890932	62.522228
1920.677733	79.958402	62.527233
1920.037747	57.305681	62.532238
1919.140280	68.702403	62.537242
1918.242427	74.469730	62.542247
1918.012604	66.574568	62.547252
1916.720343	65.491465	62.552257
1915.877565	61.287322	62.557262
1915.437383	75.817252	62.562266
1914.872205	66.221837	62.567271
1914.459401	74.133987	62.572276
1913.924025	70.432950	62.577281
1913.202053	63.737082	62.582286
1912.436350	69.149131	62.587290
1911.215711	68.557685	62.592295
1910.947199	59.542778	62.597300
1910.797669	66.332967	62.602305
1909.963869	62.274051	62.607310
1908.813591	66.528225	62.612314
1908.061371	69.599622	62.617319
1907.975209	60.055896	62.622324
1907.374736	67.258279	62.627329
1906.705693	59.469120	62.632334
1906.033001	60.949435	62.637338
1905.173267	73.196418	62.642343
1904.750368	70.925104	62.647348
1903.369202	71.526037	62.652353
1902.847368	64.799976	62.657358
1902.385725	68.959020	62.662362
1901.788431	57.063317	62.667367
1901.563080	59.863422	62.672372
1900.778700	79.974960	62.677377
1899.706929	67.470209	62.682382
1898.907779	68.273622	62.687386
1898.294899	71.925270	62.692391
1898.337900	62.130813	62.697396
1897.131942	67.486609	62.702401
1896.348966	65.590991	62.707406
1895.651663	63.978226	62.712410
1895.178995	63.714298	62.717415
1895.034273	65.733664	62.722420
1893.839332	69.378376	62.727425
1892.822458	59.042591	62.732430
1892.423244	61.397236	62.737434
1891.985048	77.383888	62.742439
1891.676561	63.020244	62.747444
1890.138057	66.943417	62.752449
1889.644776	73.666763	62.757454
1889.160739	68.252975	62.762458
1888.498681	66.815957	62.767463
1888.394572	58.345785	62.772468
1887.431695	72.682742	62.777473
1886.387110	68.930097	62.782478
1885.884956	68.579393	62.787482
1885.338138	64.331427	62.792487
1885.321682	56.864427	62.797492
1884.131375	70.415936	62.802497
1883.042376	64.290834	62.807502
1882.403901	64.505797	62.812506
1881.717071	74.511397	62.817511
1881.643701	58.681779	62.822516
1880.517738	61.293726	62.827521
1879.650144	76.348809	62.832526
1879.274587	68.431061	62.837530
1878.573003	71.563809	62.842535
1878.242940	65.666708	62.847540
1878.001413	70.628132	62.852545
1876.706660	72.628244	62.857550
1876.096529	75.371177	62.862554
1875.308721	77.861636	62.867559
1875.203447	63.703841	62.872564
1873.546582	69.251078	62.877569
1873.195548	65.274792	62.882574
1872.567192	75.118153	62.887578
1871.816152	72.335996	62.892583
1871.427705	64.067078	62.897588
1871.214019	71.045641	62.902593
1870.288381	65.851774	62.907598
1869.524818	59.036376	62.912602
1868.767031	65.256116	62.917607
1868.184298	57.030664	62.922612
1866.943769	69.107885	62.927617
1866.249965	54.322908	62.932622
1865.982690	60.989869	62.937626
1865.437149	64.879976	62.942631
1865.379218	56.787235	62.947636
1864.815851	68.400569	62.952641
1863.746087	69.448799	62.957646
1862.701131	63.412904	62.962650
1862.034500	64.736157	62.967655
1861.947646	58.155503	62.972660
1860.681986	67.943936	62.977665
1859.545375	76.363653	62.982670
1859.241372	67.761222	62.987674
1858.948566	79.530295	62.992679
1858.765051	63.845891	62.997684
1857.756408	62.582176	63.002689
1857.119690	65.285180	63.007694
1856.656781	61.630998	63.012698
1855.596133	67.627605	63.017703
1855.004512	65.485586	63.022708
1853.985187	71.734242	63.027713
1853.614783	62.957862	63.032718
1853.100486	57.537853	63.037722
1852.332946	60.001444	63.042727
1851.663014	65.155460	63.047732
1850.798510	64.592649	63.052737
1850.255868	66.668890	63.057742
1849.960439	56.929753	63.062746
1848.804326	62.050581	63.067751
1847.855781	57.565228	63.072756
1847.156494	73.008308	63.077761
1846.491428	65.850862	63.082766
1846.400831	60.600112	63.087770
1846.067123	57.851047	63.092775
1845.699495	57.967824	63.097780
1844.154142	68.046664	63.102785
1843.646604	64.259228	63.107790
1843.412774	62.002059	63.112794
1842.789645	67.233798	63.117799
1841.752309	62.332057	63.122804
1841.016903	72.816861	63.127809
1840.492785	71.148229	63.132814
1839.682112	68.763463	63.137818
1838.405798	78.197228	63.142823
1837.895620	64.130538	63.147828
1837.059884	63.036486	63.152833
1836.882052	72.384136	63.157838
1836.476320	60.588918	63.162842
1835.909437	78.945552	63.167847
1836.080887	60.528831	63.172852
1835.005518	75.998516	63.177857
1833.851728	69.696074	63.182862
1833.444069	55.857532	63.187866
1832.267891	68.564759	63.192871
1831.376926	55.394288	63.197876
1830.738182	68.191213	63.202881
1830.388152	58.501748	63.207886
1830.178597	61.800796	63.212890
1829.612752	65.558522	63.217895
1828.899343	68.316286	63.222900
1827.625803	58.763998	63.227905
1827.416486	63.575235	63.232910
1826.766860	58.671860	63.237914
1825.433092	69.483477	63.242919
1825.166270	63.137972	63.247924
1824.535904	69.503063	63.252929
1823.816635	61.272495	63.257934
1823.452962	59.838576	63.262938
1822.242332	74.482957	63.267943
1821.477912	62.519202	63.272948
1821.041682	68.385134	63.277953
1820.760053	60.848286	63.282958
1820.111315	62.731653	63.287962
1819.573623	61.218139	63.292967
1818.747109	66.843282	63.297972
1817.982346	64.137436	63.302977
1817.514111	79.323075	63.307982
1816.521144	67.193768	63.312986
1815.446325	66.501946	63.317991
1814.879576	55.544398	63.322996
1814.583784	66.375692	63.328001
1814.172293	69.003521	63.333006
1813.882907	59.555153	63.338010
1812.513281	67.031064	63.343015
1812.163560	61.296362	63.348020
1811.446097	65.354120	63.353025
1810.674013	57.628663	63.358030
1810.129833	61.023423	63.363034
1808.858183	71.257507	63.368039
1808.499695	63.269262	63.373044
1808.160002	62.262025	63.378049
1807.757424	67.586476	63.383054
1806.879230	62.049228	63.388058
1805.953757	59.110299	63.393063
1805.831669	56.830660	63.398068
1805.039203	67.592597	63.403073
1804.092375	67.172177	63.408078
1803.612304	61.172762	63.413082
1802.453748	66.836443	63.418087
1802.299188	57.158522	63.423092
1801.350781	64.135485	63.428097
1800.513055	72.603949	63.433102
1800.249259	54.281586	63.438106
1799.338332	57.360865	63.443111
1798.989074	60.926515	63.448116
1798.031709	57.251521	63.453121
1797.065962	65.043331	63.458126
1796.682879	59.537848	63.463130
1796.100252	62.801527	63.468135
1796.058380	59.034771	63.473140
1795.144540	66.567617	63.478145
1794.171717	56.499265	63.483150
1793.760697	56.638708	63.488154
1792.854968	61.855409	63.493159
1792.158427	53.641748	63.498164
1791.385743	64.400543	63.503169
1790.595380	75.207883	63.508174
1790.408737	60.052251	63.513178
1789.585700	62.532556	63.518183
1789.037028	55.441803	63.523188
1787.947635	67.819886	63.528193
1787.204586	60.454084	63.533198
1787.078635	59.077034	63.538202
1786.556132	66.459432	63.543207
1785.622741	52.709124	63.548212
1784.767970	62.268337	63.553217
1784.097682	68.445818	63.558222
1783.882001	59.985492	63.563226
1782.833618	63.149681	63.568231
1782.103200	49.124307	63.573236
1781.190653	64.785745	63.578241
1780.637887	65.192116	63.583246
1780.512010	54.382178	63.588250
1779.603842	55.338550	63.593255
1779.498241	58.584823	63.598260
1778.581084	62.598610	63.603265
1777.778458	66.597364	63.608270
1777.563538	62.596327	63.613274
1775.941717	58.443415	63.618279
1775.521255	58.043491	63.623284
1774.646335	64.020091	63.628289
1774.261830	56.408132	63.633294
1774.115249	62.674325	63.638298
1773.209021	67.593083	63.643303
1772.135871	61.142260	63.648308
1771.736066	65.528031	63.653313
1770.993653	66.035481	63.658318
1770.712582	64.025507	63.663322
1769.179962	59.782743	63.668327
1768.808783	63.716136	63.673332
1768.472015	51.582002	63.678337
1767.874515	50.817554	63.683342
1767.361094	60.713626	63.688346
1766.616315	64.219094	63.693351
1766.036894	63.434428	63.698356
1765.076957	62.754344	63.703361
1764.469073	68.417318	63.708366
1763.607012	63.096710	63.713370
1762.692981	73.102141	63.718375
1762.023625	59.371406	63.723380
1761.530779	56.157219	63.728385
1761.478620	59.287778	63.733390
1761.004179	54.929010	63.738394
1759.744036	55.857710	63.743399
1759.069645	58.483143	63.748404
1758.083483	63.409867	63.753409
1757.652061	66.638504	63.758414
1757.423811	56.144434	63.763418
1756.922421	62.170521	63.768423
1756.209534	65.937420	63.773428
1755.444051	65.459835	63.778433
1754.824359	57.986151	63.783438
1754.512973	58.433037	63.788442
1753.633279	67.486887	63.793447
1752.931464	55.746602	63.798452
1751.527409	64.674002	63.803457
1750.684704	58.747960	63.808462
1750.588962	50.199216	63.813466
1749.680893	65.598188	63.818471
1749.463467	56.754966	63.823476
1748.311148	67.318608	63.828481
1747.616929	62.141655	63.833486
1747.671083	49.689990	63.838490
1746.940632	72.680224	63.843495
1746.117631	53.729209	63.848500
1745.109993	60.866973	63.853505
1744.710912	59.919637	63.858510
1744.355731	60.851273	63.863514
1743.314026	61.180769	63.868519
1742.434396	64.647739	63.873524
1741.600711	62.545769	63.878529
1741.258285	54.733180	63.883534
1741.020461	63.137915	63.888538
1740.235917	65.553777	63.893543
1739.099875	64.004428	63.898548
1738.315429	67.530396	63.903553
1737.607343	57.948280	63.908558
1737.701317	42.978335	63.913562
1737.090992	62.464583	63.918567
1736.046312	55.572463	63.923572
1735.186088	60.789838	63.928577
1734.536993	59.458031	63.933582
1734.120151	61.842303	63.938586
1733.577120	55.239502	63.943591
1732.912323	62.166710	63.948596
1732.149436	54.217484	63.953601
1731.443773	62.149345	63.958606
1731.213490	56.666915	63.963610
1729.848145	54.516932	63.968615
1729.284794	55.103181	63.973620
1728.730244	58.520101	63.978625
1728.186746	53.278220	63.983630
1728.085799	45.801006	63.988634
1726.564268	61.516595	63.993639
1725.810541	57.147000	63.998644
1725.763422	53.904605	64.003649
1725.053404	47.968542	64.008654
1724.073621	46.698722	64.013658
1722.942359	46.807495	64.018663
1722.311794	51.676173	64.023668
1721.723547	60.190176	64.028673
1721.460843	49.151260	64.033678
1721.396154	45.179989	64.038682
1720.734406	55.034967	64.043687
1719.586300	56.461531	64.048692
1719.159932	41.022328	64.053697
1718.337761	52.766649	64.058702
1717.475169	45.572823	64.063706
1716.759897	47.039446	64.068711
1716.271132	55.290077	64.073716
1715.946940	52.268300	64.078721
1714.762020	60.426085	64.083726
1713.872048	48.130686	64.088730
1713.296340	54.482377	64.093735
1713.053929	53.123829	64.098740
1712.598604	56.103966	64.103745
1711.389329	60.179937	64.108750
1710.684039	54.649960	64.113754
1709.998947	52.710473	64.118759
1709.651300	53.547881	64.123764
1709.478980	58.507776	64.128769
1708.413639	50.286494	64.133774
1707.829167	51.926301	64.138778
1707.006906	67.013624	64.143783
1706.553032	56.014531	64.148788
1705.614915	53.345719	64.153793
1704.772859	59.287155	64.158798
1704.209818	59.554831	64.163802
1704.087159	55.788297	64.168807
1703.336023	58.243014	64.173812
1702.155358	58.250839	64.178817
1701.547954	57.380751	64.183822
1701.096365	55.998661	64.188826
1700.564102	66.217840	64.193831
1699.960836	59.088476	64.198836
1699.075431	51.825742	64.203841
1698.279247	61.664236	64.208846
1697.972244	60.631323	64.213850
1697.266367	55.472009	64.218855
1696.187004	54.342588	64.223860
1695.437793	56.429589	64.228865
1694.857616	53.506818	64.233870
1694.890724	53.030136	64.238874
1694.143643	59.358592	64.243879
1693.105750	60.691972	64.248884
1692.193689	59.699974	64.253889
1691.898447	60.133264	64.258894
1691.555932	61.964868	64.263898
1690.589020	68.892767	64.268903
1689.237045	54.541975	64.273908
1688.845886	60.478025	64.278913
1688.094165	70.777797	64.283918
1688.227826	63.373695	64.288922
1687.353928	63.648175	64.293927
1686.704537	64.965579	64.298932
1685.974540	65.363852	64.303937
1685.475223	58.687891	64.308942
1684.823767	60.660025	64.313946
1683.489642	60.987109	64.318951
1682.894019	57.305163	64.323956
1682.702677	60.062033	64.328961
1682.087523	66.711722	64.333966
1681.408567	58.793334	64.338970
1680.468727	53.396812	64.343975
1680.024059	58.411006	64.348980
1679.674165	63.386494	64.353985
1678.137344	64.527907	64.358990
1677.620289	61.776453	64.363994
1676.725464	64.651375	64.368999
1676.553330	58.825418	64.374004
1676.165353	60.615361	64.379009
1675.744631	66.653877	64.384014
1674.709763	62.366800	64.389018
1674.159865	60.303351	64.394023
1673.649425	68.060721	64.399028
1672.725109	55.378149	64.404033
1671.509318	60.524293	64.409038
1671.138771	50.218419	64.414042
1670.701788	70.353623	64.419047
1670.143112	59.245036	64.424052
1669.805973	62.952269	64.429057
1668.653379	71.809805	64.434062
1668.103929	57.919722	64.439066
1667.397906	61.909467	64.444071
1666.403214	59.602875	64.449076
1665.535225	63.558426	64.454081
1664.860810	65.660363	64.459086
1664.505117	65.187095	64.464090
1663.901626	67.334533	64.469095
1663.829779	68.036678	64.474100
1663.438740	64.576116	64.479105
1661.936185	70.614601	64.484110
1661.747583	75.476169	64.489114
1661.203934	67.750745	64.494119
1660.014197	62.155815	64.499124
1659.286734	60.167882	64.504129
1658.757182	65.894120	64.509134
1658.339331	60.204963	64.514138
1657.924538	64.176833	64.519143
1656.721643	57.434455	64.524148
1656.271682	60.019530	64.529153
1655.438206	65.833468	64.534158
1654.810753	54.639626	64.539162
1653.978806	64.985257	64.544167
1653.040528	63.092312	64.549172
1653.020065	51.188647	64.554177
1652.415927	62.469444	64.559182
1651.782585	62.704147	64.564186
1650.795610	53.844424	64.569191
1649.712341	55.446789	64.574196
1649.568241	59.388273	64.579201
1648.967189	52.968169	64.584206
1648.335570	56.206544	64.589210
1647.081058	63.180139	64.594215
1646.812388	55.806840	64.599220
1646.403226	58.752847	64.604225
1646.017386	64.263878	64.609230
1645.052317	45.885824	64.614234
1644.311689	70.796728	64.619239
1643.785305	66.837299	64.624244
1643.154616	46.956979	64.629249
1641.790100	63.488136	64.634254
1641.442935	57.637952	64.639258
1640.970198	56.907327	64.644263
1640.409140	66.984438	64.649268
1640.020579	52.414409	64.654273
1638.556432	58.415263	64.659278
1638.104656	55.760677	64.664282
1637.704637	61.045313	64.669287
1637.401918	60.557326	64.674292
1636.604078	52.930642	64.679297
1635.375009	65.622676	64.684302
1635.138328	57.651392	64.689306
1634.447687	64.057625	64.694311
1633.822215	53.111046	64.699316
1632.844789	60.417501	64.704321
1632.243596	60.531990	64.709326
1631.952664	44.066829	64.714330
1631.329689	60.415533	64.719335
1630.035721	65.279240	64.724340
1629.505029	51.777262	64.729345
1628.762396	66.801487	64.734350
1628.318408	60.471547	64.739354
1627.833135	66.998115	64.744359
1627.428562	59.968089	64.749364
1626.363890	54.788530	64.754369
1625.498081	65.134816	64.759374
1625.142489	55.342213	64.764378
1624.784978	54.670553	64.769383
1623.598690	60.471164	64.774388
1623.015004	47.165259	64.779393
1622.203820	63.608518	64.784398
1621.996744	54.300076	64.789402
1621.756167	60.341514	64.794407
1620.261747	66.531683	64.799412
1620.070380	50.820216	64.804417
1619.529132	67.657391	64.809422
1618.497000	62.961494	64.814426
1617.326557	59.743026	64.819431
1617.001440	62.199470	64.824436
1616.583760	53.957339	64.829441
1616.006234	65.527212	64.834446
1615.164359	62.067322	64.839450
1614.442447	53.884562	64.844455
1613.704344	57.817915	64.849460
1613.442037	51.460697	64.854465
1612.684881	69.361873	64.859470
1611.802126	58.301638	64.864474
1611.195303	60.872218	64.869479
1610.778584	54.306152	64.874484
1610.625926	61.956226	64.879489
1608.940245	71.768907	64.884494
1608.591900	57.892626	64.889498
1608.171918	63.115786	64.894503
1607.264121	66.439045	64.899508
1606.443577	53.721099	64.904513
1605.569623	67.274468	64.909518
1605.104399	65.904022	64.914522
1604.648250	58.237255	64.919527
1604.389821	57.832118	64.924532
1603.648212	56.598618	64.929537
1602.478028	60.629003	64.934542
1602.416106	57.521423	64.939546
1601.513968	54.189379	64.944551
1600.362050	46.721462	64.949556
1600.243003	51.909424	64.954561
1599.071414	59.975251	64.959566
1598.892288	48.743321	64.964570
1597.792561	60.363041	64.969575
1596.780862	64.700971	64.974580
1596.338915	58.539442	64.979585
1596.009217	63.040243	64.984590
1595.860694	65.069684	64.989594
1595.171476	56.569514	64.994599
1594.059537	50.091830	64.999604
1593.649712	55.518368	65.004609
1592.695157	66.479550	65.009614
1592.322736	59.955332	65.014618
1590.857941	60.240148	65.019623
1590.227942	58.315595	65.024628
1589.917732	58.153640	65.029633
1589.335263	55.019959	65.034638
1589.390460	56.438321	65.039642
1588.158826	53.146016	65.044647
1587.468637	53.626297	65.049652
1587.199317	53.623417	65.054657
1585.930725	63.505451	65.059662
1585.394707	50.879501	65.064666
1584.844056	62.290572	65.069671
1584.147324	52.836017	65.074676
1583.970436	55.011882	65.079681
1582.636353	65.423114	65.084686
1581.851127	58.411002	65.089690
1581.432160	60.354107	65.094695
1580.785823	63.996938	65.099700
1580.465183	48.618242	65.104705
1579.463398	57.376151	65.109710
1578.621417	53.790143	65.114714
1578.304370	60.920735	65.119719
1577.915130	53.235463	65.124724
1577.172880	55.669878	65.129729
1575.786254	61.956477	65.134734
1575.316625	44.433258	65.139738
1574.951138	54.797823	65.144743
1574.393594	59.325364	65.149748
1574.056381	49.209752	65.154753
1572.977534	51.842719	65.159758
1572.458209	55.605711	65.164762
1571.816811	54.931857	65.169767
1570.690612	56.061706	65.174772
1570.262878	53.330778	65.179777
1569.768212	58.245701	65.184782
1569.224663	49.673517	65.189786
1567.971171	61.762355	65.194791
1567.159287	54.904288	65.199796
1567.055777	45.286109	65.204801
1566.337912	58.051471	65.209806
1566.168211	62.411742	65.214810
1564.840784	62.994853	65.219815
1564.010451	58.659560	65.224820
1563.805607	52.313720	65.229825
1563.022086	67.095303	65.234830
1562.535760	50.721122	65.239834
1561.901418	53.086359	65.244839
1561.288368	54.863194	65.249844
1561.057129	49.396713	65.254849
1559.304318	50.058452	65.259854
1558.697173	55.943677	65.264858
1558.186653	53.897653	65.269863
1557.927296	59.995690	65.274868
1557.705672	51.768154	65.279873
1556.589069	58.399767	65.284878
1555.698181	52.752681	65.289882
1555.321150	54.607129	65.294887
1554.069926	54.132671	65.299892
1553.563336	48.019272	65.304897
1552.803495	56.812858	65.309902
1552.571621	49.225586	65.314906
1552.185827	58.781292	65.319911
1551.274464	57.502244	65.324916
1550.332557	51.598353	65.329921
1549.376473	61.596317	65.334926
1549.080309	52.707301	65.339930
1548.754687	57.409296	65.344935
1547.843575	54.542299	65.349940
1547.408917	57.441909	65.354945
1546.315039	53.979511	65.359950
1546.008244	55.620960	65.364954
1545.012864	50.078788	65.369959
1544.157370	49.278119	65.374964
1543.809844	48.691613	65.379969
1542.936605	59.887451	65.384974
1542.792190	53.295481	65.389978
1542.365391	43.067966	65.394983
1541.247205	46.074605	65.399988
1540.765982	53.128785	65.404993
1539.946570	57.297415	65.409998
1539.697335	48.110803	65.415002
1538.550559	56.596886	65.420007
1537.537425	56.306943	65.425012
1537.249862	48.704870	65.430017
1536.638619	57.219396	65.435022
1535.729656	48.733669	65.440026
1535.070971	55.883854	65.445031
1534.414569	46.542756	65.450036
1534.113455	43.342310	65.455041
1533.614668	58.419249	65.460046
1532.815102	45.619167	65.465050
1531.882074	51.904666	65.470055
1531.375259	45.013912	65.475060
1531.031325	50.828933	65.480065
1529.686657	45.760141	65.485070
1528.855790	41.311418	65.490074
1528.410734	45.775358	65.495079
1527.858787	51.415286	65.500084
1528.072983	45.302475	65.505089
1526.608001	54.340568	65.510094
1525.911369	50.766175	65.515098
1525.457904	59.295054	65.520103
1524.986390	57.927201	65.525108
1524.097476	48.354983	65.530113
1523.114436	60.358285	65.535118
1522.541676	56.595484	65.540122
1522.465293	50.002168	65.545127
1521.497958	58.092334	65.550132
1520.545138	61.578884	65.555137
1519.969241	50.791619	65.560142
1519.662003	51.329331	65.565146
1519.250096	55.892082	65.570151
1517.981566	49.231172	65.575156
1517.277041	50.232540	65.580161
1516.593779	58.749052	65.585166
1516.185623	48.332507	65.590170
1515.872692	53.163367	65.595175
1514.919751	44.478070	65.600180
1514.528501	50.663291	65.605185
1513.817957	51.500044	65.610190
1512.666670	48.521424	65.615194
1511.870175	40.561862	65.620199
1511.200360	54.814466	65.625204
1511.068114	43.491534	65.630209
1510.436662	50.520705	65.635214
1509.184635	44.426430	65.640218
1508.717026	47.156247	65.645223
1508.048098	46.431595	65.650228
1507.953297	46.654867	65.655233
1506.665386	49.030937	65.660238
1506.028023	52.634510	65.665242
1505.387564	43.552651	65.670247
1504.893543	49.079303	65.675252
1504.751623	38.768687	65.680257
1503.217290	54.566814	65.685262
1502.525347	41.584076	65.690266
1502.198931	42.686203	65.695271
1501.078476	54.583616	65.700276
1501.442497	33.668572	65.705281
1500.627484	53.245683	65.710286
1499.582283	51.686739	65.715290
1499.009330	45.259066	65.720295
1498.248423	50.528525	65.725300
1497.954889	40.926364	65.730305
1496.871185	49.946455	65.735310
1496.159992	59.971744	65.740314
1495.673712	45.130306	65.745319
1495.248906	40.795253	65.750324
1494.500200	47.469341	65.755329
1493.477194	47.726582	65.760334
1493.115644	46.860052	65.765338
1492.886278	44.936513	65.770343
1491.334853	48.349470	65.775348
1490.792115	53.290964	65.780353
1490.275684	50.648260	65.785358
1489.940861	49.017432	65.790362
1489.235063	55.886545	65.795367
1488.181016	53.586306	65.800372
1487.682923	49.239245	65.805377
1487.032906	44.217776	65.810382
1486.845636	49.897523	65.815386
1485.902881	47.182229	65.820391
1484.597602	60.668547	65.825396
1484.455707	47.248335	65.830401
1484.042881	54.602296	65.835406
1482.861004	49.939722	65.840410
1482.085345	46.664893	65.845415
1481.435560	64.914846	65.850420
1481.420623	54.000601	65.855425
1481.001243	51.438666	65.860430
1480.020652	62.672079	65.865434
1479.374834	43.276767	65.870439
1478.491436	56.197749	65.875444
1477.684236	44.898510	65.880449
1476.706746	48.985049	65.885454
1476.079465	54.895564	65.890458
1475.583837	49.360731	65.895463
1474.970940	58.306014	65.900468
1474.862196	53.625859	65.905473
1474.405167	57.254395	65.910478
1473.305780	53.080161	65.915482
1472.918235	43.276912	65.920487
1472.000853	56.247448	65.925492
1471.095934	45.378458	65.930497
1470.318708	55.746962	65.935502
1469.374241	58.278194	65.940506
1469.538964	45.082058	65.945511
1469.090548	53.681095	65.950516
1468.073878	52.068748	65.955521
1467.143080	57.491365	65.960526
1466.494654	49.585551	65.965530
1466.283206	39.196110	65.970535
1464.982320	50.026280	65.975540
1464.706581	39.631287	65.980545
1464.240045	44.063958	65.985550
1463.323277	54.948199	65.990554
1462.753862	44.010126	65.995559
1461.887223	60.239877	66.000564
1461.442897	47.788625	66.005569
1460.714105	51.864030	66.010574
1459.583427	46.248788	66.015578
1459.258828	45.371660	66.020583
1458.337198	52.503724	66.025588
1458.283229	49.235627	66.030593
1457.586981	46.219408	66.035598
1456.930550	60.438358	66.040602
1456.413137	42.722518	66.045607
1455.478547	61.452947	66.050612
1454.663860	36.264264	66.055617
1453.880020	51.208315	66.060622
1453.168550	45.230001	66.065626
1452.780816	41.384203	66.070631
1452.160471	46.874170	66.075636
1451.547843	44.398144	66.080641
1450.429102	46.867196	66.085646
1450.075256	44.424156	66.090650
1449.755715	43.983018	66.095655
1448.686467	45.936453	66.100660
1447.757225	49.196939	66.105665
1447.645700	58.690137	66.110670
1446.632769	49.788911	66.115674
1446.406881	48.916596	66.120679
1445.218687	48.107339	66.125684
1444.960571	37.129263	66.130689
1444.376273	44.512051	66.135694
1443.494839	38.041966	66.140698
1442.886484	45.901639	66.145703
1441.684077	48.680443	66.150708
1441.361346	40.694496	66.155713
1440.859399	39.339382	66.160718
1440.162133	42.961948	66.165722
1439.701375	39.384788	66.170727
1438.289799	56.382354	66.175732
1438.056150	48.678696	66.180737
1437.652538	50.341851	66.185742
1437.181892	46.870334	66.190746
1435.981434	38.085653	66.195751
1435.437530	45.119842	66.200756
1434.767935	42.217659	66.205761
1434.406027	39.643447	66.210766
1433.966831	47.471506	66.215770
1433.151635	39.377760	66.220775
1432.145506	48.246777	66.225780
1431.822651	33.658505	66.230785
1430.982593	37.819403	66.235790
1429.974066	44.143734	66.240794
1429.438817	43.060406	66.245799
1428.816517	51.050026	66.250804
1428.705334	42.677239	66.255809
1427.398021	39.583119	66.260814
1426.657372	45.765533	66.265818
1426.445418	44.301257	66.270823
1426.223498	46.771275	66.275828
1425.171083	47.066332	66.280833
1424.354256	38.420945	66.285838
1423.469876	32.884845	66.290842
1423.477104	35.545510	66.295847
1422.154395	48.408593	66.300852
1421.763619	39.378540	66.305857
1421.206179	43.433025	66.310862
1420.562389	51.782435	66.315866
1419.704262	40.002490	66.320871
1418.695329	41.482750	66.325876
1418.191364	45.170787	66.330881
1417.738253	39.422646	66.335886
1417.119680	45.565160	66.340890
1416.484595	40.752641	66.345895
1415.381372	48.049189	66.350900
1415.303791	44.606662	66.355905
1414.842132	35.696683	66.360910
1413.794589	38.665337	66.365914
1413.106711	37.573159	66.370919
1412.191672	37.042183	66.375924
1411.560986	31.801638	66.380929
1411.474040	39.450711	66.385934
1410.217302	49.911206	66.390938
1409.913515	42.485196	66.395943
1409.368146	40.727005	66.400948
1408.796118	35.327334	66.405953
1407.564969	31.241885	66.410958
1406.660791	37.259492	66.415962
1406.614180	38.999939	66.420967
1406.074816	46.150100	66.425972
1405.469500	43.449009	66.430977
1404.656513	42.807203	66.435982
1403.704522	45.008508	66.440986
1403.339661	34.627699	66.445991
1401.946731	44.397096	66.450996
1401.222577	36.336200	66.456001
1400.777711	33.064014	66.461006
1400.206825	40.252296	66.466010
1400.178261	40.081865	66.471015
1399.736886	43.310549	66.476020
1399.416657	39.126043	66.481025
1398.440122	46.938594	66.486030
1397.465799	47.689579	66.491034
1396.214898	42.054058	66.496039
1395.462662	46.819141	66.501044
1394.818677	46.959408	66.506049
1394.500181	43.887896	66.511054
1393.785881	47.003852	66.516058
1393.752577	35.411345	66.521063
1393.134169	55.108597	66.526068
1392.316571	46.679373	66.531073
1391.414643	44.474840	66.536078
1390.281116	48.994619	66.541082
1389.742115	46.387064	66.546087
1389.363292	51.015528	66.551092
1388.943293	44.855296	66.556097
1388.142906	53.175990	66.561102
1386.934596	45.772339	66.566106
1386.740607	44.467629	66.571111
1386.148736	51.911554	66.576116
1385.831647	43.016443	66.581121
1384.858865	42.806876	66.586126
1383.511214	46.886055	66.591130
1383.740092	51.684414	66.596135
1382.877576	51.864152	66.601140
1382.027136	47.396515	66.606145
1381.198678	45.599755	66.611150
1380.248718	51.168937	66.616154
1380.056165	44.601989	66.621159
1379.772417	49.084461	66.626164
1378.788497	42.250666	66.631169
1377.849982	44.147080	66.636174
1377.492852	52.542389	66.641178
1377.066512	42.401576	66.646183
1375.940912	56.170010	66.651188
1375.193817	42.768759	66.656193
1374.974800	42.825711	66.661198
1374.303933	51.595725	66.666202
1373.837049	41.511818	66.671207
1372.643794	51.791935	66.676212
1372.247684	48.578229	66.681217
1371.946407	44.299256	66.686222
1370.392388	52.446452	66.691226
1369.831014	36.111095	66.696231
1369.167119	46.136762	66.701236
1368.710889	45.359414	66.706241
1368.632291	55.899142	66.711246
1367.775655	40.492186	66.716250
1366.962942	30.469569	66.721255
1366.095297	38.578613	66.726260
1365.945898	33.624255	66.731265
1365.013209	39.845091	66.736270
1363.863122	40.018511	66.741274
1363.621755	34.282455	66.746279
1363.091739	46.122313	66.751284
1362.220313	35.194445	66.756289
1361.435954	33.103693	66.761294
1360.555016	45.906033	66.766298
1360.305015	32.178210	66.771303
1359.662073	42.768216	66.776308
1359.161521	44.088842	66.781313
1358.119197	36.065925	66.786318
1357.218999	39.019062	66.791322
1357.268652	32.574461	66.796327
1356.697497	49.119924	66.801332
1355.475058	36.880712	66.806337
1355.094301	34.039866	66.811342
1354.354588	43.727521	66.816346
1354.228605	32.454090	66.821351
1352.885725	38.434224	66.826356
1352.398747	33.486225	66.831361
1351.965561	35.696533	66.836366
1350.750335	48.550441	66.841370
1350.374091	32.072133	66.846375
1349.508865	47.833334	66.851380
1349.085326	36.060030	66.856385
1348.552304	38.898033	66.861390
1347.380922	43.024898	66.866394
1347.025926	39.005191	66.871399
1346.083125	48.340380	66.876404
1345.996848	37.055904	66.881409
1345.309932	44.316255	66.886414
1344.126524	37.567805	66.891418
1343.594562	33.248244	66.896423
1343.193349	31.694222	66.901428
1342.375796	43.483601	66.906433
1341.984909	37.448058	66.911438
1340.893302	43.538057	66.916442
1340.723830	44.861244	66.921447
1339.881189	35.791090	66.926452
1339.314555	36.914077	66.931457
1338.287580	33.759672	66.936462
1337.453483	26.645058	66.941466
1337.266688	29.424868	66.946471
1336.753871	35.813916	66.951476
1335.369493	31.774941	66.956481
1335.020565	30.386063	66.961486
1334.407893	23.803922	66.966490
1334.133974	35.852207	66.971495
1333.589890	29.501997	66.976500
1332.653467	33.030148	66.981505
1332.150850	35.149000	66.986510
1331.221848	42.946128	66.991514
1330.202507	45.052516	66.996519
1329.575957	41.553773	67.001524
1329.191395	40.867536	67.006529
1328.830766	46.693107	67.011534
1328.370340	46.275960	67.016538
1327.173508	37.151737	67.021543
1326.112297	46.955162	67.026548
1325.799332	43.802360	67.031553
1325.709004	49.214398	67.036558
1324.474009	47.737739	67.041562
1324.022347	43.362839	67.046567
1323.325718	35.750158	67.051572
1322.944539	47.940076	67.056577
1321.927982	37.243444	67.061582
1320.863765	45.462596	67.066586
1320.337938	43.141531	67.071591
1319.913110	41.517153	67.076596
1319.558311	52.182782	67.081601
1318.876070	48.218257	67.086606
1317.959387	43.064203	67.091610
1317.464668	45.692708	67.096615
1316.638150	59.517688	67.101620
1315.442235	46.679796	67.106625
1314.803996	49.837293	67.111630
1314.230351	54.299630	67.116634
1314.170586	43.167050	67.121639
1313.452369	56.563248	67.126644
1312.913475	49.909451	67.131649
1312.901055	49.479425	67.136654
1311.561747	62.430352	67.141658
1311.053462	48.459752	67.146663
1309.829743	48.692208	67.151668
1308.760597	48.404954	67.156673
1308.438595	45.368704	67.161678
1307.986547	61.491568	67.166682
1307.633195	45.837475	67.171687
1307.381156	54.562991	67.176692
1306.081080	50.296171	67.181697
1305.560571	51.779243	67.186702
1305.016882	50.579019	67.191706
1304.229086	52.949788	67.196711
1303.318921	46.744508	67.201716
1302.483052	47.593358	67.206721
1302.480216	48.757598	67.211726
1301.293408	50.818087	67.216730
1300.848855	43.223677	67.221735
1299.932120	62.500042	67.226740
1299.448718	56.137028	67.231745
1298.994447	44.682415	67.236750
1297.565201	53.421636	67.241754
1296.875883	49.190175	67.246759
1296.559364	47.804034	67.251764
1296.098940	55.603946	67.256769
1296.005851	49.733939	67.261774
1295.571858	54.054234	67.266778
1294.459315	51.515812	67.271783
1293.750368	52.259335	67.276788
1292.970505	45.184989	67.281793
1292.044469	52.604791	67.286798
1291.108309	45.004969	67.291802
1290.930978	49.032158	67.296807
1290.253160	46.017790	67.301812
1289.882708	48.289093	67.306817
1289.434705	38.541238	67.311822
1288.488999	50.390429	67.316826
1287.744340	46.416915	67.321831
1286.647619	48.507239	67.326836
1285.729777	39.237762	67.331841
1285.773313	44.505518	67.336846
1284.899929	43.485445	67.341850
1284.823110	42.102193	67.346855
1283.699457	39.177636	67.351860
1283.113341	41.041706	67.356865
1282.871563	41.102284	67.361870
1281.885552	44.064360	67.366874
1280.722264	31.205547	67.371879
1280.003735	43.474328	67.376884
1279.968857	47.951928	67.381889
1279.431921	36.672887	67.386894
1278.185697	44.162518	67.391898
1277.331760	41.016894	67.396903
1276.916332	39.603906	67.401908
1276.140252	46.772798	67.406913
1276.024260	32.249448	67.411918
1274.790816	43.969355	67.416922
1274.167678	37.541846	67.421927
1273.894944	46.111384	67.426932
1272.940912	40.993248	67.431937
1272.929820	34.838991	67.436942
1271.662931	44.605751	67.441946
1270.949582	45.379940	67.446951
1270.171203	36.873577	67.451956
1270.080875	47.296891	67.456961
1269.021828	41.468518	67.461966
1268.229795	49.950325	67.466970
1267.857625	49.955948	67.471975
1267.028022	48.452705	67.476980
1266.289145	47.046995	67.481985
1265.743733	47.453881	67.486990
1265.293779	50.076855	67.491994
1264.705725	50.659245	67.496999
1264.167347	49.710485	67.502004
1263.090583	48.490957	67.507009
1262.733153	42.913708	67.512014
1261.835780	54.917641	67.517018
1261.369186	47.456047	67.522023
1260.530515	50.457778	67.527028
1259.798411	53.094078	67.532033
1259.625747	51.968904	67.537038
1258.413387	48.692628	67.542042
1257.565084	50.205753	67.547047
1256.946566	46.811403	67.552052
1256.462524	50.321266	67.557057
1256.294589	53.809252	67.562062
1254.938619	55.658552	67.567066
1254.498768	44.266311	67.572071
1254.146626	40.003330	67.577076
1253.259511	52.038746	67.582081
1253.178908	37.208587	67.587086
1251.854954	48.214385	67.592090
1251.379317	39.636237	67.597095
1250.809779	50.665576	67.602100
1249.740005	47.686736	67.607105
1249.316714	46.541493	67.612110
1248.626968	48.281708	67.617114
1248.067554	42.129486	67.622119
1247.450209	43.837690	67.627124
1246.076275	45.158446	67.632129
1246.017034	46.911940	67.637134
1245.105622	46.276375	67.642138
1245.108435	33.927559	67.647143
1244.202154	42.254078	67.652148
1242.823334	47.311207	67.657153
1242.520303	40.545818	67.662158
1241.961945	43.364217	67.667162
1241.694275	33.204526	67.672167
1241.172290	44.104880	67.677172
1240.234056	45.130867	67.682177
1239.836564	47.687158	67.687182
1238.799757	49.402142	67.692186
1238.162619	39.655991	67.697191
1237.726330	41.534091	67.702196
1236.437066	50.998514	67.707201
1235.838979	36.614902	67.712206
1234.737807	51.650441	67.717210
1234.115648	40.917944	67.722215
1234.403759	38.599930	67.727220
1233.843428	56.226991	67.732225
1233.576236	35.456492	67.737230
1232.312748	46.809053	67.742234
1231.542310	50.145277	67.747239
1230.967931	48.809608	67.752244
1229.789599	37.099594	67.757249
1229.273917	44.712763	67.762254
1228.407052	54.800691	67.767258
1228.177418	40.323797	67.772263
1228.058463	48.320135	67.777268
1226.717848	53.341239	67.782273
1226.087120	42.641644	67.787278
1225.609322	56.056389	67.792282
1225.006230	41.895910	67.797287
1224.213556	40.579188	67.802292
1223.042900	45.820832	67.807297
1223.005880	41.175028	67.812302
1222.343574	38.703811	67.817306
1221.887820	35.461776	67.822311
1220.808004	45.561487	67.827316
1220.339571	46.673615	67.832321
1219.597468	48.677615	67.837326
1219.092877	51.932146	67.842330
1218.099282	46.014544	67.847335
1217.285996	50.593848	67.852340
1216.681685	48.865573	67.857345
1216.683321	41.397341	67.862350
1215.555306	39.731847	67.867354
1214.776813	45.502457	67.872359
1214.342045	39.614260	67.877364
1213.582039	53.928542	67.882369
1213.532595	42.097361	67.887374
1211.815470	44.267449	67.892378
1211.236151	54.877327	67.897383
1211.357526	40.647378	67.902388
1210.258867	41.640542	67.907393
1210.112991	36.564222	67.912398
1209.113210	46.312184	67.917402
1208.283202	38.526798	67.922407
1208.013302	46.093000	67.927412
1206.903870	45.487362	67.932417
1206.466226	45.233761	67.937422
1205.375164	43.445707	67.942426
1205.168271	47.835547	67.947431
1204.770127	44.719963	67.952436
1203.574318	47.447363	67.957441
1203.266803	45.132606	67.962446
1202.755001	47.014836	67.967450
1201.804442	44.196824	67.972455
1201.094180	44.557402	67.977460
1200.207657	45.680830	67.982465
1199.976659	42.634856	67.987470
1198.951658	49.211028	67.992474
1198.320512	36.242406	67.997479
1197.500825	49.457641	68.002484
1196.889196	55.233260	68.007489
1196.715590	42.031031	68.012494
1195.775029	47.661849	68.017498
1194.811518	54.631924	68.022503
1194.259835	48.246686	68.027508
1193.874478	56.769490	68.032513
1193.510849	39.803545	68.037518
1192.491579	45.200889	68.042522
1191.816907	47.446471	68.047527
1191.538331	41.577592	68.052532
1190.591642	43.540022	68.057537
1189.754617	37.267973	68.062542
1188.730202	47.407767	68.067546
1188.285822	46.300580	68.072551
1188.167076	40.406285	68.077556
1187.656658	43.992887	68.082561
1186.667512	36.015212	68.087566
1185.453077	49.862474	68.092570
1185.078513	35.876973	68.097575
1185.300165	33.161117	68.102580
1184.047122	35.549139	68.107585
1183.675816	42.021354	68.112590
1182.661141	43.663457	68.117594
1181.682653	51.791759	68.122599
1181.045541	41.791747	68.127604
1180.386184	35.778437	68.132609
1180.070750	40.586060	68.137614
1179.543625	46.621038	68.142618
1178.676303	39.915443	68.147623
1178.099171	42.467195	68.152628
1177.278596	45.443996	68.157633
1176.722954	34.021319	68.162638
1175.561740	49.097957	68.167642
1174.825979	41.858958	68.172647
1174.557630	40.980808	68.177652
1173.869965	41.372492	68.182657
1173.803878	46.113656	68.187662
1172.828682	49.350002	68.192666
1171.825622	48.374244	68.197671
1171.442292	47.109126	68.202676
1170.909605	43.664882	68.207681
1170.367782	39.205015	68.212686
1169.184749	49.032593	68.217690
1168.820672	35.944242	68.222695
1168.314499	33.826657	68.227700
1166.678556	48.827419	68.232705
1166.239742	33.822451	68.237710
1165.347876	44.001090	68.242714
1165.215380	34.204672	68.247719
1164.967277	41.067279	68.252724
1164.285749	43.378609	68.257729
1164.157280	30.579204	68.262734
1162.956305	49.096576	68.267738
1162.261731	40.851300	68.272743
1161.759359	40.442431	68.277748
1160.830795	43.734439	68.282753
1159.906925	38.685668	68.287758
1159.655259	31.767058	68.292762
1158.880160	36.589444	68.297767
1158.040457	45.193964	68.302772
1157.302853	51.416955	68.307777
1156.812360	41.084569	68.312782
1156.307323	44.123149	68.317786
1155.674597	30.754276	68.322791
1154.724271	33.649221	68.327796
1154.247235	46.278561	68.332801
1153.915514	42.423912	68.337806
1152.749690	52.392256	68.342810
1151.825505	44.189808	68.347815
1151.611858	31.074387	68.352820
1150.904751	35.715660	68.357825
1150.770044	39.198360	68.362830
1149.318897	46.916168	68.367834
1148.837625	44.324720	68.372839
1148.592116	40.491052	68.377844
1147.600999	47.071312	68.382849
1147.103646	44.091360	68.387854
1146.011868	42.864810	68.392858
1145.494908	53.505775	68.397863
1145.414113	39.692743	68.402868
1143.987555	44.289183	68.407873
1143.354352	48.444071	68.412878
1142.728819	45.935489	68.417882
1142.497942	52.759095	68.422887
1142.179844	37.591437	68.427892
1140.426590	55.614801	68.432897
1140.239937	38.770528	68.437902
1139.565054	47.295226	68.442906
1139.412993	49.848763	68.447911
1138.653806	43.733076	68.452916
1137.644440	48.977486	68.457921
1136.988076	33.794253	68.462926
1136.586313	45.749339	68.467930
1135.275437	42.963433	68.472935
1134.480115	37.159409	68.477940
1133.867194	47.172273	68.482945
1134.053919	41.541616	68.487950
1133.723159	48.065733	68.492954
1132.394723	42.833752	68.497959
1131.571090	41.572444	68.502964
1130.972273	38.901931	68.507969
1130.620082	40.768248	68.512974
1129.549462	50.393469	68.517978
1128.804987	48.687510	68.522983
1128.604055	34.934593	68.527988
1128.410934	48.343477	68.532993
1127.659498	42.956650	68.537998
1126.666895	42.111704	68.543002
1125.835622	41.955417	68.548007
1124.599325	46.408072	68.553012
1123.834449	47.181036	68.558017
1123.298175	38.931096	68.563022
1123.060181	52.252509	68.568026
1122.624236	46.115374	68.573031
1122.484112	46.705394	68.578036
1121.007302	49.813397	68.583041
1120.635630	41.002719	68.588046
1119.652235	47.329462	68.593050
1118.911437	43.847374	68.598055
1118.790904	42.611424	68.603060
1117.777057	49.914360	68.608065
1116.963614	45.724776	68.613070
1116.379360	43.987030	68.618074
1116.101819	39.261226	68.623079
1115.917233	32.336685	68.628084
1114.080601	45.363622	68.633089
1113.726677	37.543548	68.638094
1113.545199	32.722047	68.643098
1112.634229	35.225993	68.648103
1111.917737	33.966573	68.653108
1111.466420	45.603131	68.658113
1111.056746	38.091530	68.663118
1110.303701	48.902502	68.668122
1109.083028	44.129605	68.673127
1108.559111	35.811478	68.678132
1108.107562	44.723255	68.683137
1107.170198	38.998602	68.688142
1106.178135	43.131734	68.693146
1105.815059	39.307311	68.698151
1105.794956	38.168922	68.703156
1104.606223	49.426067	68.708161
1103.945848	38.707583	68.713166
1103.331552	46.057348	68.718170
1102.862634	49.749322	68.723175
1102.456762	42.085737	68.728180
1100.988168	44.829764	68.733185
1100.929691	43.043080	68.738190
1100.494294	40.515305	68.743194
1099.358143	47.673707	68.748199
1098.507491	36.285365	68.753204
1097.989804	40.250007	68.758209
1097.484825	39.816337	68.763214
1096.647914	37.331931	68.768218
1095.679290	41.959626	68.773223
1095.138359	38.458370	68.778228
1094.355949	45.625155	68.783233
1094.145182	41.902655	68.788238
1094.052866	42.503994	68.793242
1092.778127	48.703635	68.798247
1092.409884	44.097911	68.803252
1091.187417	46.616724	68.808257
1091.105945	32.028001	68.813262
1090.030641	40.553323	68.818266
1088.861300	45.531476	68.823271
1088.966886	34.033608	68.828276
1088.311112	48.637232	68.833281
1087.695700	42.932332	68.838286
1086.793411	41.825468	68.843290
1085.887338	50.792207	68.848295
1085.778520	40.514241	68.853300
1084.838031	47.182656	68.858305
1084.011485	46.437461	68.863310
1083.317759	42.468531	68.868314
1082.691877	42.142400	68.873319
1082.761862	33.220482	68.878324
1081.419158	48.502625	68.883329
1080.413637	41.751248	68.888334
1080.110510	36.920718	68.893338
1079.605558	38.401356	68.898343
1079.131492	44.446829	68.903348
1078.168113	42.551794	68.908353
1077.872375	37.053076	68.913358
1077.344104	39.846220	68.918362
1075.970852	48.898314	68.923367
1075.432237	29.631229	68.928372
1074.739317	41.832890	68.933377
1074.512405	46.531830	68.938382
1074.328780	32.668948	68.943386
1072.790993	49.134813	68.948391
1072.568291	42.509633	68.953396
1071.523616	41.352890	68.958401
1071.060900	33.335681	68.963406
1069.999250	29.453670	68.968410
1069.144050	40.085363	68.973415
1069.083021	45.899563	68.978420
1068.094054	49.470854	68.983425
1068.230529	44.978800	68.988430
1067.162755	41.127721	68.993434
1066.215380	41.718434	68.998439
1065.691348	34.444221	69.003444
1065.032108	39.617186	69.008449
1063.925958	41.978743	69.013454
1063.296311	44.398532	69.018458
1062.618150	41.135144	69.023463
1062.406230	42.947618	69.028468
1061.793133	45.667532	69.033473
1061.359027	33.949610	69.038478
1060.680880	39.341614	69.043482
1059.883401	42.414116	69.048487
1059.502009	34.357166	69.053492
1058.535230	45.249452	69.058497
1057.629587	30.955841	69.063502
1057.444356	45.546108	69.068506
1056.511776	60.323084	69.073511
1055.632704	36.723324	69.078516
1054.817224	43.606813	69.083521
1054.743981	37.621721	69.088526
1054.023828	36.799690	69.093530
1052.729715	41.985352	69.098535
1052.295000	36.802044	69.103540
1051.338146	42.629450	69.108545
1051.288742	35.172509	69.113550
1050.938558	45.443188	69.118554
1050.107394	52.624050	69.123559
1049.304156	42.245261	69.128564
1048.617140	40.750948	69.133569
1047.925427	34.622987	69.138574
1047.333889	33.853034	69.143578
1046.091390	34.545893	69.148583
1046.116109	39.744087	69.153588
1045.042472	55.555847	69.158593
1044.344725	53.031972	69.163598
1043.763428	42.953748	69.168602
1043.181456	48.748327	69.173607
1043.147054	40.834861	69.178612
1042.046642	39.720111	69.183617
1041.084151	46.773640	69.188622
1040.682651	49.469359	69.193626
1039.921492	39.752470	69.198631
1039.146296	32.135046	69.203636
1038.193296	43.397283	69.208641
1037.516611	42.416963	69.213646
1037.241476	35.528914	69.218650
1036.703116	40.856109	69.223655
1036.412217	34.349015	69.228660
1035.414102	39.148568	69.233665
1034.724439	39.296193	69.238670
1034.041273	41.358671	69.243674
1033.245854	41.545197	69.248679
1032.490941	35.417835	69.253684
1031.751140	39.802578	69.258689
1031.429160	37.105395	69.263694
1031.211710	40.564993	69.268698
1029.902306	46.976744	69.273703
1029.357567	35.415195	69.278708
1028.780430	42.017934	69.283713
1028.240352	48.143298	69.288718
1027.137335	41.878939	69.293722
1026.192316	39.318722	69.298727
1025.936580	42.040134	69.303732
1025.387094	45.117344	69.308737
1024.975998	41.392034	69.313742
1023.962678	42.761185	69.318746
1023.346394	36.345281	69.323751
1023.032625	42.265915	69.328756
1022.340942	51.135487	69.333761
1021.666186	34.982304	69.338766
1020.872585	36.854209	69.343770
1020.105927	35.637488	69.348775
1019.759860	35.460809	69.353780
1018.672593	51.205357	69.358785
1017.905585	37.550408	69.363790
1017.422208	36.996629	69.368794
1016.813979	41.305254	69.373799
1016.218709	39.589785	69.378804
1015.035084	41.187872	69.383809
1014.582012	36.789616	69.388814
1014.379015	36.944969	69.393818
1013.768882	37.355897	69.398823
1012.697998	40.719478	69.403828
1012.034699	38.202751	69.408833
1011.421761	30.510640	69.413838
1011.300937	29.243208	69.418842
1010.176558	40.710900	69.423847
1009.733964	52.002325	69.428852
1008.931524	39.540393	69.433857
1008.811842	31.597928	69.438862
1007.400277	40.987284	69.443866
1006.380021	46.258699	69.448871
1005.956358	37.543051	69.453876
1005.729176	40.348225	69.458881
1005.083259	46.179789	69.463886
1004.314485	35.317752	69.468890
1003.365726	48.559863	69.473895
1003.246825	38.822802	69.478900
1002.662265	53.128120	69.483905
1001.626255	50.784227	69.488910
1000.716176	41.934668	69.493914
1000.471766	54.158025	69.498919
999.911445	45.360043	69.503924
998.752824	56.905736	69.508929
997.806680	48.309479	69.513934
997.677827	40.056252	69.518938
997.266508	46.689382	69.523943
996.628309	35.322477	69.528948
995.536563	45.145051	69.533953
995.059734	36.026305	69.538958
994.724957	33.061521	69.543962
993.526991	48.014756	69.548967
992.730394	32.410800	69.553972
991.922105	48.752747	69.558977
991.720122	43.095630	69.563982
991.361255	38.922073	69.568986
990.410134	37.327881	69.573991
989.892910	36.262282	69.578996
989.032786	52.634557	69.584001
988.864387	36.910148	69.589006
987.616130	37.241274	69.594010
986.815357	50.898212	69.599015
986.718833	42.526307	69.604020
985.889127	39.430549	69.609025
984.926378	46.854698	69.614030
984.520101	42.814833	69.619034
983.562780	33.991726	69.624039
983.227269	36.511380	69.629044
982.667048	35.708076	69.634049
981.733739	44.318070	69.639054
981.413118	29.847842	69.644058
980.280285	43.984938	69.649063
980.100657	28.596621	69.654068
978.817908	39.264824	69.659073
978.321135	30.775272	69.664078
977.930452	39.000899	69.669082
977.525930	37.280320	69.674087
976.450454	39.994979	69.679092
975.710485	45.092505	69.684097
975.245564	42.151584	69.689102
974.852979	34.104320	69.694106
973.580808	48.604195	69.699111
972.981319	38.729154	69.704116
972.099916	47.933255	69.709121
972.055842	47.285932	69.714126
971.543436	36.553416	69.719130
970.716280	37.771547	69.724135
969.943406	35.891973	69.729140
969.488836	43.265226	69.734145
968.773530	40.110273	69.739150
967.723709	35.589374	69.744154
966.999607	41.447576	69.749159
966.665217	45.420920	69.754164
965.970769	40.362532	69.759169
965.405057	38.713331	69.764174
964.694173	49.911837	69.769178
963.493695	48.666396	69.774183
963.494210	39.197328	69.779188
962.942316	48.776329	69.784193
962.137459	43.491096	69.789198
961.401647	44.880766	69.794202
960.668623	37.105281	69.799207
960.154293	33.681824	69.804212
958.854839	47.068050	69.809217
958.042149	48.123044	69.814222
957.789950	40.113364	69.819226
957.486915	51.634882	69.824231
957.097660	40.475942	69.829236
956.567616	37.389280	69.834241
955.631356	45.175053	69.839246
955.116207	39.310746	69.844250
953.866380	48.671241	69.849255
953.194300	38.259011	69.854260
952.781324	42.659574	69.859265
952.079220	46.834925	69.864270
951.680873	38.348638	69.869274
950.271642	52.512386	69.874279
950.048182	52.290977	69.879284
949.429771	47.753472	69.884289
948.898743	44.966570	69.889294
947.914274	46.130898	69.894298
947.013815	47.362279	69.899303
947.047560	45.653961	69.904308
946.447136	49.739022	69.909313
945.875980	45.952469	69.914318
944.606360	43.395054	69.919322
943.990082	51.735431	69.924327
943.800287	47.501863	69.929332
942.959152	49.756648	69.934337
942.047690	41.128098	69.939342
941.711096	36.170461	69.944346
940.920377	46.743043	69.949351
940.203893	30.766843	69.954356
939.255557	48.364185	69.959361
938.501771	41.323673	69.964366
938.122251	41.459816	69.969370
937.690932	39.726163	69.974375
937.428140	42.879186	69.979380
936.101437	37.921418	69.984385
935.350568	41.940539	69.989390
935.387029	30.549876	69.994394
934.069647	46.733157	69.999399
933.200924	37.104390	70.004404
932.950538	46.816753	70.009409
932.388987	44.633918	70.014414
932.008221	38.032340	70.019418
930.678131	44.467925	70.024423
930.231677	32.941231	70.029428
929.669612	50.098663	70.034433
928.710981	50.028936	70.039438
928.543074	34.296582	70.044442
927.716389	42.615249	70.049447
927.310794	45.838304	70.054452
926.759247	45.839407	70.059457
925.473092	38.938809	70.064462
924.791107	32.005146	70.069466
924.165679	43.836566	70.074471
924.005287	42.069262	70.079476
922.842095	36.790609	70.084481
921.803787	40.704096	70.089486
921.742120	34.598911	70.094490
921.229359	47.563512	70.099495
921.026417	41.666876	70.104500
919.734400	39.403182	70.109505
919.245952	39.026837	70.114510
918.557189	33.139712	70.119514
917.204814	44.490764	70.124519
916.600235	37.763966	70.129524
916.108025	31.361468	70.134529
915.813543	44.895267	70.139534
915.667280	39.038496	70.144538
914.893607	38.226600	70.149543
914.105794	28.561319	70.154548
912.922723	45.497469	70.159553
912.269905	40.199099	70.164558
911.805436	42.466486	70.169562
910.953038	47.872063	70.174567
910.507608	37.983565	70.179572
910.037714	31.793547	70.184577
909.087821	50.830817	70.189582
908.120700	39.125225	70.194586
907.562761	49.547237	70.199591
907.443472	35.589002	70.204596
906.852885	44.190204	70.209601
905.789749	45.119500	70.214606
904.963593	42.956707	70.219610
904.182163	44.102931	70.224615
904.009558	44.806934	70.229620
903.398859	44.971988	70.234625
902.329954	44.795249	70.239630
901.656838	42.522951	70.244634
900.947054	44.520316	70.249639
900.983354	42.015279	70.254644
900.025428	39.947571	70.259649
899.009745	45.686623	70.264654
898.958254	40.246830	70.269658
898.387960	49.672658	70.274663
897.253825	30.361658	70.279668
896.269555	48.477206	70.284673
895.842503	41.714276	70.289678
895.574045	38.745261	70.294682
894.390800	45.681010	70.299687
893.759355	36.561669	70.304692
893.103092	33.534532	70.309697
892.721826	40.834628	70.314702
892.508736	38.638924	70.319706
891.327672	40.457419	70.324711
890.911754	32.297203	70.329716
890.353584	33.907764	70.334721
888.721936	36.908078	70.339726
888.088648	31.239202	70.344730
887.606261	41.005829	70.349735
887.284447	33.015129	70.354740
886.850233	40.856630	70.359745
886.445347	42.570522	70.364750
885.687939	38.375262	70.369754
884.805236	41.749942	70.374759
884.372132	39.887280	70.379764
883.088579	33.979717	70.384769
882.162607	38.062985	70.389774
881.474145	43.746811	70.394778
881.177808	34.867439	70.399783
880.850679	38.043319	70.404788
880.942032	41.089524	70.409793
879.746244	34.475753	70.414798
878.942445	35.751693	70.419802
878.159255	35.464841	70.424807
877.621852	42.143276	70.429812
876.691193	34.230555	70.434817
876.147861	37.543341	70.439822
875.633317	36.783251	70.444826
874.659767	41.361344	70.449831
874.229234	37.506703	70.454836
873.827631	36.157816	70.459841
873.088389	37.909156	70.464846
872.528950	38.463427	70.469850
871.409015	43.689256	70.474855
870.876009	38.184184	70.479860
870.062331	43.386501	70.484865
869.100913	41.382435	70.489870
868.450135	40.111051	70.494874
867.562118	41.204868	70.499879
867.558509	38.608418	70.504884
867.272090	32.048608	70.509889
866.466769	36.976796	70.514894
865.765463	27.643099	70.519898
864.953439	34.092444	70.524903
864.614926	34.807086	70.529908
863.705961	39.877920	70.534913
862.352011	34.670660	70.539918
862.354920	37.026084	70.544922
861.953669	36.432458	70.549927
860.919764	30.672821	70.554932
859.978194	36.996139	70.559937
859.151297	35.144122	70.564942
859.154426	37.166794	70.569946
858.657392	42.097955	70.574951
857.927862	39.760538	70.579956
857.305874	37.574727	70.584961
855.991221	38.406889	70.589966
855.288528	30.022684	70.594970
854.260927	41.968580	70.599975
854.100321	33.856040	70.604980
853.642040	36.931379	70.609985
853.113110	33.388854	70.614990
852.855115	29.520950	70.619994
851.576910	35.732280	70.624999
851.012383	25.599429	70.630004
850.543471	29.972635	70.635009
850.055010	31.846482	70.640014
849.285815	24.198221	70.645018
848.150585	32.502936	70.650023
848.066018	35.206576	70.655028
847.142942	33.409293	70.660033
845.888124	35.151243	70.665038
845.371870	26.038822	70.670042
844.638679	45.416896	70.675047
844.656576	31.239734	70.680052
844.310054	33.046839	70.685057
843.162745	36.244464	70.690062
842.512213	27.993879	70.695066
841.898605	25.573367	70.700071
841.091583	41.954546	70.705076
840.052472	33.207601	70.710081
839.416059	41.883910	70.715086
839.328835	31.325025	70.720090
838.708748	39.978235	70.725095
837.971764	31.802908	70.730100
837.172699	32.458403	70.735105
836.419126	39.546542	70.740110
835.947882	25.294289	70.745114
835.091850	40.631505	70.750119
834.053616	26.918903	70.755124
833.882762	38.077192	70.760129
833.189192	34.575069	70.765134
832.954733	37.105460	70.770138
831.843088	37.058549	70.775143
831.376840	23.907727	70.780148
830.815915	30.681365	70.785153
829.874470	35.894565	70.790158
829.060548	30.721209	70.795162
828.507585	34.092303	70.800167
828.344854	30.482035	70.805172
827.739886	37.302108	70.810177
826.503524	33.588359	70.815182
826.106860	34.853123	70.820186
825.742577	32.761913	70.825191
824.481911	35.018860	70.830196
823.810030	35.783416	70.835201
822.928150	38.520934	70.840206
822.807513	30.433576	70.845210
821.613168	33.531470	70.850215
821.062416	39.773671	70.855220
820.814538	26.846695	70.860225
819.575421	43.460651	70.865230
819.457864	29.475357	70.870234
818.879254	38.413686	70.875239
818.024352	39.849157	70.880244
817.670349	33.331650	70.885249
816.911549	33.682716	70.890254
816.092058	35.830021	70.895258
815.077930	46.338847	70.900263
814.750375	35.578536	70.905268
814.440185	41.738295	70.910273
812.817514	33.139443	70.915278
812.428782	39.739031	70.920282
812.042728	36.105968	70.925287
811.502830	39.547521	70.930292
811.304265	30.979013	70.935297
810.010547	32.880128	70.940302
809.331318	31.301072	70.945306
809.032207	35.514801	70.950311
807.960516	29.573558	70.955316
806.965413	39.752944	70.960321
806.217311	36.336776	70.965326
806.135634	28.523900	70.970330
805.674286	29.081494	70.975335
805.202515	25.673378	70.980340
804.223024	39.399782	70.985345
803.271362	41.848812	70.990350
803.100737	32.955754	70.995354
802.171661	43.184554	71.000359
801.176190	34.227267	71.005364
800.836800	25.395770	71.010369
800.136293	41.307441	71.015374
799.810458	27.997088	71.020378
798.879474	33.743186	71.025383
798.071728	28.139955	71.030388
797.614873	30.576448	71.035393
796.867617	28.426365	71.040398
796.210639	30.284471	71.045402
794.897180	27.735694	71.050407
794.541394	35.126349	71.055412
794.492570	29.416503	71.060417
793.838815	37.523178	71.065422
793.386015	35.070771	71.070426
792.511879	30.080470	71.075431
791.474113	38.387039	71.080436
790.948944	29.515733	71.085441
789.790113	39.741687	71.090446
789.709378	32.986732	71.095450
788.980317	32.973548	71.100455
788.348632	43.492459	71.105460
787.828563	34.320736	71.110465
786.622578	39.470413	71.115470
786.393870	27.234211	71.120474
785.816902	36.367811	71.125479
784.828697	32.636657	71.130484
784.048659	38.279889	71.135489
783.413302	40.812606	71.140494
783.368293	33.033315	71.145498
782.726266	29.625500	71.150503
781.454557	47.987086	71.155508
781.148985	32.446985	71.160513
780.497137	50.109117	71.165518
779.873405	42.462947	71.170522
778.834444	41.612906	71.175527
778.195918	36.637137	71.180532
777.709161	32.619591	71.185537
777.027792	39.469182	71.190542
776.913540	40.293205	71.195546
775.586119	36.958232	71.200551
774.666689	32.858186	71.205556
774.635635	37.278389	71.210561
773.625468	47.190545	71.215566
772.736787	39.737936	71.220570
771.905266	38.291937	71.225575
771.739720	43.991883	71.230580
771.604724	25.628870	71.235585
770.765397	43.429643	71.240590
770.116869	37.615004	71.245594
769.113005	34.324714	71.250599
768.221696	34.602278	71.255604
767.601081	29.729313	71.260609
766.686692	42.767317	71.265614
766.358417	34.514336	71.270618
765.438037	47.999549	71.275623
765.147439	25.880006	71.280628
764.988473	38.906549	71.285633
764.049395	41.225864	71.290638
763.111364	28.388272	71.295642
762.926672	35.950376	71.300647
762.179239	36.829472	71.305652
761.303824	30.379218	71.310657
760.410047	39.413457	71.315662
760.002301	36.774123	71.320666
759.030374	34.593591	71.325671
758.243734	30.710518	71.330676
757.756566	31.128738	71.335681
757.214970	41.176020	71.340686
756.970380	23.450166	71.345690
755.962541	32.505715	71.350695
755.069947	31.157750	71.355700
754.621981	31.457772	71.360705
754.286815	27.518595	71.365710
753.244123	32.620212	71.370714
752.159045	32.819826	71.375719
751.602234	35.089325	71.380724
751.725814	28.677140	71.385729
750.689489	35.272603	71.390734
749.926518	41.278959	71.395738
749.300853	35.544261	71.400743
749.000885	42.490824	71.405748
748.399304	34.836411	71.410753
747.299582	40.000725	71.415758
746.664006	35.719890	71.420762
746.287431	46.406338	71.425767
745.428966	35.418351	71.430772
744.553874	37.285965	71.435777
743.755470	41.479848	71.440782
743.800146	24.988351	71.445786
742.705677	30.889795	71.450791
741.579236	32.166684	71.455796
741.037723	28.605692	71.460801
740.743634	39.015668	71.465806
740.471385	31.151143	71.470810
739.488435	39.713914	71.475815
738.595761	30.011787	71.480820
738.709326	26.412731	71.485825
737.614124	32.254373	71.490830
736.591823	37.515167	71.495834
735.556760	33.733150	71.500839
735.086826	35.321810	71.505844
735.085107	34.808090	71.510849
734.145599	41.798131	71.515854
733.716040	32.829622	71.520858
733.007658	36.504581	71.525863
732.265605	31.952139	71.530868
731.592079	29.733572	71.535873
730.426986	37.871209	71.540878
729.867343	29.754418	71.545882
729.801272	34.167578	71.550887
729.024479	44.012629	71.555892
728.088842	32.857176	71.560897
727.375884	38.573316	71.565902
727.364170	24.815607	71.570906
725.901882	36.479103	71.575911
725.098788	36.835671	71.580916
724.957527	32.979159	71.585921
724.630938	37.140503	71.590926
723.977303	39.401770	71.595930
722.681291	32.468173	71.600935
721.998732	31.665486	71.605940
721.596536	38.074848	71.610945
721.177147	43.379997	71.615950
720.380299	36.784792	71.620954
719.461593	28.457107	71.625959
719.100601	31.690429	71.630964
718.567329	28.123401	71.635969
717.179114	40.014792	71.640974
716.891749	32.909568	71.645978
716.137591	35.724549	71.650983
715.509306	34.197329	71.655988
715.376039	23.182205	71.660993
714.325040	37.621714	71.665998
713.634626	33.975633	71.671002
712.921118	27.062833	71.676007
712.180968	28.435916	71.681012
711.517246	32.496405	71.686017
710.623208	43.656302	71.691022
710.317469	34.791079	71.696026
709.895322	33.221579	71.701031
709.242937	29.995196	71.706036
708.636896	30.605805	71.711041
707.861704	38.208315	71.716046
707.415400	36.227949	71.721050
706.638693	35.030273	71.726055
705.216219	33.604277	71.731060
705.099314	28.668476	71.736065
704.661797	30.665115	71.741070
703.973665	32.274331	71.746074
702.952786	35.767255	71.751079
702.155816	36.925475	71.756084
701.916919	29.244871	71.761089
700.590203	45.707243	71.766094
699.898956	36.025095	71.771098
699.352721	46.043165	71.776103
698.861138	46.069462	71.781108
698.693967	48.193360	71.786113
698.155946	47.008141	71.791118
697.562012	35.520767	71.796122
696.479828	33.249014	71.801127
696.098010	34.811036	71.806132
695.242676	29.440912	71.811137
694.735992	42.497588	71.816142
694.247718	36.301088	71.821146
693.110119	35.353257	71.826151
691.871373	42.059816	71.831156
691.623808	33.967455	71.836161
690.932009	37.530981	71.841166
690.643286	30.101148	71.846170
690.545672	36.678044	71.851175
689.256701	41.776325	71.856180
688.565520	35.785590	71.861185
687.858915	43.296766	71.866190
687.088374	39.097359	71.871194
686.137353	36.889875	71.876199
685.620072	40.140204	71.881204
685.274554	29.937843	71.886209
684.495099	35.565238	71.891214
684.559623	40.804375	71.896218
683.579813	34.118478	71.901223
682.379669	39.231001	71.906228
682.086063	34.291799	71.911233
681.116576	40.373629	71.916238
680.519712	37.141566	71.921242
680.028744	26.470390	71.926247
679.034242	44.563950	71.931252
679.212566	32.844815	71.936257
677.921492	37.593374	71.941262
677.275854	26.847486	71.946266
676.740404	30.532765	71.951271
676.210130	41.186918	71.956276
675.363129	34.487762	71.961281
674.193888	26.199992	71.966286
673.947670	25.988540	71.971290
673.901678	24.695021	71.976295
672.457553	41.794222	71.981300
671.789383	31.914459	71.986305
671.335264	34.553950	71.991310
671.040543	41.212693	71.996314
669.806612	31.058766	72.001319
668.799558	32.504322	72.006324
668.640200	26.548753	72.011329
667.826136	39.108783	72.016334
667.297989	33.021136	72.021338
667.391641	29.893576	72.026343
666.167890	29.043049	72.031348
665.812532	35.060204	72.036353
664.947546	29.802009	72.041358
664.122541	34.298173	72.046362
663.080243	41.091726	72.051367
662.456313	28.407585	72.056372
662.284600	33.780524	72.061377
661.476295	29.036820	72.066382
660.203836	31.746703	72.071386
659.815029	30.482544	72.076391
659.201293	39.387066	72.081396
658.946965	26.830141	72.086401
658.572037	35.385993	72.091406
657.936488	29.236611	72.096410
656.888898	36.718515	72.101415
656.307138	47.775088	72.106420
656.025614	25.852823	72.111425
654.706827	32.215771	72.116430
654.079526	33.334372	72.121434
653.750110	29.701784	72.126439
652.624125	32.648527	72.131444
651.692773	20.746587	72.136449
651.023879	40.496029	72.141454
650.439080	29.056106	72.146458
650.289050	29.972557	72.151463
650.143652	34.972322	72.156468
649.771465	19.674680	72.161473
648.571929	34.189892	72.166478
647.888542	21.642956	72.171482
646.867949	22.877800	72.176487
645.810313	34.609348	72.181492
645.594849	23.653054	72.186497
645.266907	30.154668	72.191502
644.494318	24.495440	72.196506
643.551725	22.310286	72.201511
642.798208	19.842727	72.206516
642.620891	26.342428	72.211521
641.611487	23.021543	72.216526
640.900284	25.536407	72.221530
640.367721	22.600028	72.226535
639.684873	26.568966	72.231540
639.112484	12.438550	72.236545
637.923217	27.573403	72.241550
637.703079	24.953101	72.246554
637.267729	27.698411	72.251559
636.603203	29.835283	72.256564
635.830277	19.828731	72.261569
634.702789	26.512859	72.266574
634.222351	26.046993	72.271578
633.941736	27.490411	72.276583
632.768094	26.420622	72.281588
632.320634	30.270081	72.286593
631.360988	28.150721	72.291598
631.144114	28.000828	72.296602
631.005253	23.128453	72.301607
629.595159	36.228078	72.306612
629.103918	29.956381	72.311617
628.644612	29.570724	72.316622
628.053288	33.100917	72.321626
627.382584	32.332636	72.326631
626.219080	29.556658	72.331636
626.141568	16.843866	72.336641
624.817152	26.012941	72.341646
624.109410	25.884454	72.346650
623.615537	17.463934	72.351655
623.011894	31.059560	72.356660
623.049293	23.081099	72.361665
622.112520	25.874726	72.366670
620.869000	28.468063	72.371674
620.683975	24.489231	72.376679
620.188016	27.882820	72.381684
619.175021	27.791910	72.386689
618.354925	22.808844	72.391694
617.378354	26.752029	72.396698
617.237353	21.443209	72.401703
617.040983	26.028492	72.406708
615.920349	21.332972	72.411713
615.154317	34.363144	72.416718
614.832035	34.867088	72.421722
613.934415	31.454298	72.426727
612.905807	37.826244	72.431732
612.188850	28.323260	72.436737
611.533728	34.897482	72.441742
611.323661	23.249674	72.446746
611.176719	35.586780	72.451751
609.759898	24.662557	72.456756
609.258709	31.106614	72.461761
608.707161	36.161601	72.466766
608.199517	32.661476	72.471770
607.139779	27.071646	72.476775
606.329487	29.543957	72.481780
605.940796	32.040582	72.486785
605.174454	35.759494	72.491790
604.732999	31.882999	72.496794
604.098109	38.688953	72.501799
602.885516	39.071356	72.506804
602.597985	30.127571	72.511809
601.906466	38.893111	72.516814
601.591245	36.146038	72.521818
600.709069	27.967122	72.526823
599.759958	33.657824	72.531828
599.664486	24.752837	72.536833
599.012129	28.463056	72.541838
597.818188	27.784423	72.546842
597.428005	27.647943	72.551847
596.370424	22.617558	72.556852
596.424251	26.734092	72.561857
595.502912	34.784074	72.566862
594.326014	32.992624	72.571866
594.080848	25.243658	72.576871
593.406706	36.106798	72.581876
593.382449	26.588110	72.586881
591.898862	38.193564	72.591886
591.134569	31.530153	72.596890
591.179550	28.083936	72.601895
590.174910	37.861227	72.606900
589.368600	35.689079	72.611905
588.747949	43.224430	72.616910
588.034925	34.126077	72.621914
587.859615	35.226319	72.626919
586.355527	40.994381	72.631924
585.977367	32.555434	72.636929
585.371663	37.194877	72.641934
585.135459	40.553412	72.646938
584.746373	35.110648	72.651943
583.388888	35.815740	72.656948
582.968487	32.207115	72.661953
582.423120	31.759484	72.666958
581.609661	41.722360	72.671962
580.703844	31.341198	72.676967
579.805144	39.777065	72.681972
579.457649	34.223607	72.686977
578.998314	39.071537	72.691982
578.284689	38.360565	72.696986
577.617245	35.496140	72.701991
576.942244	34.223964	72.706996
576.392301	38.280555	72.712001
575.226218	30.220980	72.717006
574.658820	33.610187	72.722010
574.121662	31.871385	72.727015
573.716261	35.170140	72.732020
573.513578	30.921330	72.737025
572.109605	36.892634	72.742030
571.616771	38.287864	72.747034
571.289652	29.017676	72.752039
570.614412	35.552535	72.757044
569.603116	28.524802	72.762049
569.136754	44.071221	72.767054
568.520301	33.058963	72.772058
567.880149	27.135834	72.777063
566.627035	37.632331	72.782068
566.161113	21.706287	72.787073
565.799727	32.322507	72.792078
565.185307	39.211935	72.797082
564.347615	30.570237	72.802087
563.256989	32.856993	72.807092
562.858466	38.113105	72.812097
562.473601	36.236515	72.817102
562.074142	40.447324	72.822106
561.050032	38.139576	72.827111
560.243504	41.494341	72.832116
559.992353	31.814687	72.837121
559.364547	44.231540	72.842126
558.435224	33.944012	72.847130
557.724010	35.910157	72.852135
557.378721	43.128858	72.857140
556.555607	34.664601	72.862145
555.236435	40.623986	72.867150
554.886059	28.438752	72.872154
554.474131	30.618984	72.877159
554.047091	35.975826	72.882164
553.055513	35.011109	72.887169
552.353873	39.773067	72.892174
551.702583	28.654411	72.897178
551.576610	33.968029	72.902183
550.523367	34.009705	72.907188
549.828743	26.928388	72.912193
549.198495	41.884361	72.917198
548.663401	38.407544	72.922202
548.379748	37.328491	72.927207
546.795125	44.987434	72.932212
546.173182	31.356907	72.937217
545.767031	32.221126	72.942222
545.345880	41.022455	72.947226
544.454377	31.515761	72.952231
543.492695	30.970459	72.957236
543.439301	40.962076	72.962241
542.956159	41.392310	72.967246
541.696099	33.180575	72.972250
541.086917	35.997740	72.977255
540.260982	33.193264	72.982260
540.374255	32.254401	72.987265
539.660411	28.489114	72.992270
538.296193	36.390476	72.997274
537.762886	32.738348	73.002279
537.254679	23.104381	73.007284
537.009616	25.221767	73.012289
536.197627	34.605710	73.017294
535.215291	28.467455	73.022298
534.864120	28.660640	73.027303
533.821283	40.252682	73.032308
533.298579	32.886956	73.037313
532.347173	30.450953	73.042318
531.565509	39.535198	73.047322
531.553119	34.242164	73.052327
530.927615	22.417715	73.057332
530.269694	33.833329	73.062337
529.572751	36.588788	73.067342
528.839775	33.551903	73.072346
528.167915	27.892440	73.077351
527.035534	31.034207	73.082356
526.691863	24.827338	73.087361
526.098794	29.215635	73.092366
525.335974	40.614852	73.097370
524.588876	25.733333	73.102375
523.486717	26.265329	73.107380
523.525198	32.634469	73.112385
523.023789	31.271583	73.117390
522.366343	32.164797	73.122394
521.451100	20.656148	73.127399
520.371750	42.128251	73.132404
520.370532	28.537622	73.137409
519.785826	32.621834	73.142414
518.551705	34.737513	73.147418
518.271537	28.474800	73.152423
517.449892	36.639803	73.157428
516.973902	38.699368	73.162433
515.854482	39.598370	73.167438
515.343818	38.746282	73.172442
514.811078	24.513399	73.177447
514.474318	32.531779	73.182452
513.804252	40.286310	73.187457
512.901837	42.703945	73.192462
512.372991	29.981062	73.197466
511.857983	29.568032	73.202471
510.496432	32.626472	73.207476
510.217317	30.955382	73.212481
509.514465	36.660499	73.217486
509.121845	29.515317	73.222490
508.069454	27.541661	73.227495
507.264363	32.900388	73.232500
506.821025	32.368716	73.237505
506.396255	33.283212	73.242510
505.689374	29.102115	73.247514
505.131497	23.441851	73.252519
504.005394	38.314398	73.257524
503.929150	23.799078	73.262529
503.214249	28.094831	73.267534
501.899779	35.117863	73.272538
501.652226	23.854495	73.277543
501.182639	28.620492	73.282548
500.386121	28.444686	73.287553
499.349187	35.194863	73.292558
498.545056	36.712232	73.297562
498.335557	25.715596	73.302567
498.159931	39.794954	73.307572
497.084860	34.117737	73.312577
496.709974	21.107006	73.317582
495.511405	31.288928	73.322586
495.101407	27.125191	73.327591
493.987427	36.079467	73.332596
493.713321	29.338005	73.337601
492.868814	31.706999	73.342606
492.145285	35.609919	73.347610
492.074147	28.154925	73.352615
490.727319	38.783068	73.357620
490.270838	26.212660	73.362625
489.812845	20.864474	73.367630
489.199075	27.294942	73.372634
488.759806	24.386313	73.377639
487.946243	27.970859	73.382644
487.323118	23.945150	73.387649
486.447405	29.300940	73.392654
485.277930	26.343069	73.397658
484.875735	31.352207	73.402663
483.978298	30.219566	73.407668
483.572485	29.626731	73.412673
483.352112	31.445318	73.417678
482.591906	42.946623	73.422682
481.797838	30.603448	73.427687
481.179280	35.718015	73.432692
481.026775	30.814713	73.437697
480.150520	19.806043	73.442702
479.003099	27.869996	73.447706
478.379275	27.431734	73.452711
477.880039	29.193829	73.457716
477.259237	31.576071	73.462721
476.338946	23.261369	73.467726
475.619932	26.617981	73.472730
475.579060	20.137395	73.477735
474.475034	30.272725	73.482740
473.687322	25.620424	73.487745
473.164781	29.456637	73.492750
472.404189	28.076710	73.497754
472.144921	30.953253	73.502759
470.970193	33.680772	73.507764
470.490903	21.279578	73.512769
470.143855	31.499303	73.517774
469.560566	31.305304	73.522778
468.640709	26.109545	73.527783
467.798441	37.645998	73.532788
467.485556	23.217269	73.537793
467.243375	32.248689	73.542798
465.727384	27.305589	73.547802
465.395543	19.431697	73.552807
464.810997	26.100348	73.557812
464.153966	30.495694	73.562817
463.032860	24.767488	73.567822
462.190596	27.727452	73.572826
462.276774	23.393216	73.577831
461.507024	24.897233	73.582836
460.367912	26.773889	73.587841
459.883124	21.529320	73.592846
459.062110	23.120347	73.597850
458.917683	24.494779	73.602855
458.356426	29.180776	73.607860
457.362404	26.838321	73.612865
456.893114	31.388250	73.617870
455.941108	26.993928	73.622874
455.000645	21.134452	73.627879
453.847141	36.279441	73.632884
453.683886	25.538781	73.637889
453.383153	28.473968	73.642894
452.858875	33.828968	73.647898
452.901709	28.640676	73.652903
451.657114	24.158939	73.657908
450.620432	23.709197	73.662913
450.310364	21.089054	73.667918
449.616245	32.513599	73.672922
448.573447	24.109625	73.677927
448.067836	22.149800	73.682932
447.783359	18.948454	73.687937
447.115771	17.295115	73.692942
445.672266	28.509492	73.697946
445.349483	25.464049	73.702951
444.837352	29.707012	73.707956
444.406334	25.606555	73.712961
443.693058	20.529273	73.717966
442.416458	35.110443	73.722970
442.298048	21.726150	73.727975
441.826367	34.906558	73.732980
440.692210	19.676772	73.737985
440.045170	37.442216	73.742990
439.096948	33.655960	73.747994
438.962424	18.826689	73.752999
438.533308	34.042334	73.758004
437.254041	28.105966	73.763009
436.933941	19.794998	73.768014
436.331536	35.236938	73.773018
436.155302	24.488888	73.778023
434.839755	31.680843	73.783028
433.908800	23.957601	73.788033
433.586704	34.695291	73.793038
432.968563	37.053467	73.798042
432.146719	24.140774	73.803047
430.930893	36.712822	73.808052
430.767906	39.159318	73.813057
430.549375	22.309293	73.818062
429.995525	39.353463	73.823066
429.103227	22.374263	73.828071
428.349172	27.483619	73.833076
427.656238	31.127807	73.838081
427.422598	22.397814	73.843086
426.123194	28.661589	73.848090
425.677094	15.482471	73.853095
424.683182	21.965633	73.858100
424.642504	32.459799	73.863105
423.792458	29.104157	73.868110
423.028780	37.755078	73.873114
422.400538	32.093431	73.878119
422.209231	34.359947	73.883124
420.919463	27.330928	73.888129
420.297487	29.431113	73.893134
419.359063	38.106725	73.898138
419.272833	22.795127	73.903143
418.016438	29.282274	73.908148
417.441698	27.563689	73.913153
417.078156	22.342387	73.918158
416.586687	37.314098	73.923162
416.124427	19.113711	73.928167
414.811651	28.563279	73.933172
414.005184	35.625247	73.938177
413.710713	19.354997	73.943182
413.180049	29.695436	73.948186
412.858199	31.514428	73.953191
411.719874	31.598104	73.958196
410.936704	29.248878	73.963201
410.936597	34.922461	73.968206
409.585339	30.102951	73.973210
408.999517	25.528884	73.978215
408.410950	39.894791	73.983220
407.841809	32.219555	73.988225
407.638187	31.012658	73.993230
406.042249	37.408846	73.998234
405.753541	16.128032	74.003239
405.112145	29.289751	74.008244
404.719171	30.541374	74.013249
404.188343	25.176429	74.018254
403.047322	33.151089	74.023258
402.858897	27.400447	74.028263
402.037770	37.082324	74.033268
400.620555	36.291140	74.038273
400.238771	29.227831	74.043278
399.653845	27.052012	74.048282
399.437580	30.244962	74.053287
399.156663	34.123106	74.058292
397.976872	38.108213	74.063297
397.501721	33.385634	74.068302
396.716010	37.476671	74.073306
395.884968	31.456288	74.078311
395.013932	30.634844	74.083316
394.446826	35.969872	74.088321
394.127529	26.600716	74.093326
393.456857	27.565452	74.098330
392.344914	16.247476	74.103335
391.668197	27.615640	74.108340
391.254038	30.245653	74.113345
390.830415	25.054427	74.118350
390.103612	38.448948	74.123354
389.269739	29.393585	74.128359
388.682645	33.039839	74.133364
387.910968	34.414884	74.138369
387.877976	23.427991	74.143374
386.691232	34.405956	74.148378
386.004879	22.252236	74.153383
385.459115	39.630988	74.158388
384.817507	32.329982	74.163393
384.039841	24.345809	74.168398
383.148152	36.465704	74.173402
383.075325	18.122856	74.178407
382.183366	22.044755	74.183412
381.205382	33.200752	74.188417
380.546719	22.225259	74.193422
379.933109	26.708314	74.198426
379.628145	25.224276	74.203431
378.677207	22.515469	74.208436
378.006828	35.465787	74.213441
377.904021	25.619043	74.218446
377.094070	28.447736	74.223450
376.093999	25.112866	74.228455
375.467997	27.475460	74.233460
374.483109	28.237976	74.238465
374.506774	20.052003	74.243470
373.279192	26.608688	74.248474
372.855649	22.614283	74.253479
372.220665	31.222627	74.258484
371.806437	25.430707	74.263489
370.786289	20.569497	74.268494
369.671832	25.659033	74.273498
369.168485	36.729940	74.278503
368.984599	27.869033	74.283508
368.552624	21.898605	74.288513
367.857686	30.281553	74.293518
366.777036	34.657701	74.298522
366.713964	21.247260	74.303527
365.499923	34.478167	74.308532
364.233072	21.876104	74.313537
364.105424	27.527430	74.318542
363.402136	36.287003	74.323546
363.368998	27.994969	74.328551
362.284767	24.310841	74.333556
361.219983	33.028679	74.338561
360.984194	26.506627	74.343566
360.473044	27.291419	74.348570
359.812437	20.649424	74.353575
358.591234	27.594580	74.358580
357.932383	23.229273	74.363585
357.758878	25.745250	74.368590
357.411353	24.816740	74.373594
356.804727	26.264832	74.378599
355.895009	24.126592	74.383604
355.103411	21.507512	74.388609
353.882766	30.133502	74.393614
352.835897	29.042070	74.398618
352.524987	24.353251	74.403623
352.302980	25.282765	74.408628
351.710119	24.374431	74.413633
351.644311	24.968414	74.418638
350.666204	36.649532	74.423642
349.806379	38.984746	74.428647
349.570058	27.145646	74.433652
348.192469	28.705566	74.438657
347.610219	30.209696	74.443662
346.471730	27.697937	74.448666
346.461399	25.473136	74.453671
346.084839	27.966284	74.458676
345.214310	37.947764	74.463681
344.708609	28.106887	74.468686
343.606566	28.258924	74.473690
343.444565	28.141310	74.478695
342.098906	24.495701	74.483700
341.098902	25.153414	74.488705
340.749482	23.469899	74.493710
340.211533	31.747415	74.498714
340.152266	22.439330	74.503719
339.346405	28.036326	74.508724
338.169149	28.985622	74.513729
337.769621	30.621473	74.518734
337.379327	28.113473	74.523738
336.954385	20.260753	74.528743
335.837326	34.646235	74.533748
335.094894	30.328944	74.538753
334.958413	26.020733	74.543758
333.932514	38.917340	74.548762
333.470197	28.637496	74.553767
332.839368	34.925644	74.558772
331.560614	37.141560	74.563777
330.744551	25.046377	74.568782
329.798905	34.541546	74.573786
329.661448	29.258998	74.578791
329.623439	28.363161	74.583796
329.038095	29.755832	74.588801
328.017325	27.567496	74.593806
326.850166	35.522700	74.598810
326.754548	32.076819	74.603815
326.209040	29.740204	74.608820
324.936513	28.771475	74.613825
324.513703	26.364848	74.618830
323.871975	35.693320	74.623834
323.320631	27.450765	74.628839
322.557836	36.863183	74.633844
321.534538	37.351163	74.638849
321.348263	32.213581	74.643854
320.869997	42.473153	74.648858
320.416371	24.015972	74.653863
319.489182	36.422217	74.658868
318.582582	28.717221	74.663873
318.307660	26.230259	74.668878
317.196363	35.813331	74.673882
316.440583	33.418773	74.678887
315.656591	35.631532	74.683892
315.242786	29.468996	74.688897
315.380459	28.188792	74.693902
314.280645	40.099041	74.698906
313.645180	22.785677	74.703911
313.123031	29.438102	74.708916
311.939675	33.830641	74.713921
311.255189	32.974764	74.718926
310.608361	39.054170	74.723930
310.175533	28.515761	74.728935
309.457441	34.295885	74.733940
308.237536	37.513192	74.738945
307.699263	32.944189	74.743950
307.301606	36.806256	74.748954
307.041541	33.992095	74.753959
306.548052	34.171727	74.758964
305.397808	36.471246	74.763969
304.747724	22.916268	74.768974
304.254134	29.415919	74.773978
303.755530	23.826685	74.778983
302.938296	33.454349	74.783988
301.968264	38.364790	74.788993
301.647233	28.275311	74.793998
300.111831	37.158061	74.799002
299.451256	26.004717	74.804007
299.288461	27.172363	74.809012
298.616489	32.063680	74.814017
298.728124	30.836507	74.819022
298.092857	28.102649	74.824026
297.097276	37.326686	74.829031
296.360277	42.332444	74.834036
295.474797	36.087403	74.839041
294.997389	23.041035	74.844046
294.030027	36.295726	74.849050
293.474966	38.796834	74.854055
292.985798	22.664874	74.859060
292.421348	19.711588	74.864065
291.644760	14.612915	74.869070
291.115098	31.547576	74.874074
290.538473	23.679622	74.879079
290.036320	21.086967	74.884084
288.810741	34.401735	74.889089
288.578282	20.573635	74.894094
287.408187	19.968620	74.899098
286.624906	27.515743	74.904103
286.244873	24.454221	74.909108
285.523158	22.386961	74.914113
285.350975	16.890777	74.919118
284.149835	20.308514	74.924122
283.300919	26.451668	74.929127
282.847835	29.518378	74.934132
282.468477	34.061882	74.939137
282.190055	16.078238	74.944142
281.010808	20.815460	74.949146
280.563079	25.622155	74.954151
279.918227	17.861270	74.959156
278.626904	26.362944	74.964161
278.075375	21.149558	74.969166
277.304995	28.915386	74.974170
277.192553	21.492233	74.979175
277.002403	22.322064	74.984180
275.642068	29.637916	74.989185
275.030224	30.948096	74.994190
274.521796	26.882092	74.999194
273.899675	15.478226	75.004199
272.797417	18.079169	75.009204
271.878563	36.808826	75.014209
272.167594	17.712937	75.019214
271.230361	21.241568	75.024218
270.965855	22.805447	75.029223
269.943139	29.165531	75.034228
269.022854	32.872802	75.039233
268.719130	22.517243	75.044238
267.333898	23.400381	75.049242
266.647080	22.738842	75.054247
265.728994	21.918637	75.059252
265.216574	30.105367	75.064257
265.093152	20.883207	75.069262
264.623901	30.089581	75.074266
264.451894	23.137939	75.079271
263.522332	21.277270	75.084276
262.539453	35.018532	75.089281
262.326105	11.988078	75.094286
261.174970	33.438547	75.099290
260.254720	26.114197	75.104295
260.095545	23.101049	75.109300
259.286493	24.426899	75.114305
258.397082	13.447244	75.119310
257.389295	23.165206	75.124314
257.018344	21.231264	75.129319
256.628219	29.901514	75.134324
255.962348	27.106319	75.139329
255.653324	24.828215	75.144334
254.732165	30.008404	75.149338
254.214565	17.818382	75.154343
253.090009	23.704304	75.159348
252.023517	24.033628	75.164353
251.455318	19.649175	75.169358
251.146029	25.167038	75.174362
251.251123	32.561525	75.179367
250.340756	15.287288	75.184372
249.065246	37.165994	75.189377
248.743434	13.700277	75.194382
248.002229	32.865206	75.199386
247.484931	21.487212	75.204391
246.721554	18.910977	75.209396
245.766543	26.282071	75.214401
245.463034	27.983048	75.219406
245.021708	34.338769	75.224410
243.645895	22.558345	75.229415
243.290733	34.886038	75.234420
242.630888	23.062443	75.239425
242.576550	28.497092	75.244430
241.199937	33.956456	75.249434
240.268069	33.378138	75.254439
240.018866	30.295769	75.259444
239.439404	25.837424	75.264449
238.883495	22.589497	75.269454
238.096723	19.871925	75.274458
237.570387	21.018683	75.279463
237.170095	27.960754	75.284468
236.240865	27.118684	75.289473
235.534260	16.100436	75.294478
234.620633	37.136189	75.299482
234.263898	23.599129	75.304487
233.414333	22.600868	75.309492
232.260800	29.617287	75.314497
232.287703	34.941223	75.319502
231.431374	40.521068	75.324506
231.202048	23.335373	75.329511
230.170211	29.223871	75.334516
228.979395	18.987662	75.339521
228.603836	29.076328	75.344526
228.342920	31.476945	75.349530
227.680079	27.996924	75.354535
226.761622	10.933716	75.359540
225.679603	32.652276	75.364545
225.254530	37.846427	75.369550
224.779801	3.917509	75.374554
224.536901	46.665147	75.379559
223.787537	14.451443	75.384564
222.910730	32.696616	75.389569
222.772463	22.666329	75.394574
221.418711	20.852800	75.399578
220.596461	29.008506	75.404583
220.254257	31.633379	75.409588
219.853341	22.384504	75.414593
219.192190	12.719836	75.419598
218.154316	29.126853	75.424602
217.300083	37.817483	75.429607
216.995522	23.997739	75.434612
216.354630	30.383698	75.439617
215.585253	29.795255	75.444622
215.015646	33.930732	75.449626
214.197771	33.059880	75.454631
213.981622	34.072044	75.459636
212.674301	29.671397	75.464641
212.143252	23.357280	75.469646
211.533146	32.316475	75.474650
210.991752	34.306098	75.479655
210.624144	32.425244	75.484660
208.852055	30.199050	75.489665
208.715597	14.991700	75.494670
208.079866	25.914994	75.499674
207.952965	20.820001	75.504679
207.746531	19.424352	75.509684
206.467520	21.403842	75.514689
205.667463	26.812303	75.519694
205.356626	31.149361	75.524698
204.480314	30.387171	75.529703
203.529807	27.706750	75.534708
202.554399	27.110159	75.539713
202.311362	34.465530	75.544718
202.296993	38.380037	75.549722
201.519680	31.498094	75.554727
200.721147	28.495422	75.559732
199.976107	26.824542	75.564737
198.993938	26.676854	75.569742
198.229221	21.639395	75.574746
197.829425	20.634093	75.579751
197.639243	27.832811	75.584756
196.023119	30.526749	75.589761
195.668512	22.533551	75.594766
194.850430	27.076048	75.599770
194.363497	26.563999	75.604775
194.311903	25.411728	75.609780
193.303964	22.573324	75.614785
192.656181	34.657529	75.619790
192.011423	34.787189	75.624794
191.143830	18.488538	75.629799
190.503764	13.978376	75.634804
189.673299	26.266728	75.639809
189.311928	23.631152	75.644814
188.850071	24.496423	75.649818
187.763039	26.000645	75.654823
186.988943	22.979892	75.659828
186.316166	26.266133	75.664833
185.992944	16.244845	75.669838
185.499313	28.389619	75.674842
184.432703	14.975217	75.679847
183.989481	13.447023	75.684852
183.067158	40.816779	75.689857
182.905324	19.848527	75.694862
181.836303	21.182734	75.699866
181.131219	15.681645	75.704871
180.394305	19.075875	75.709876
180.058366	29.576090	75.714881
179.400073	13.426996	75.719886
177.987100	20.886891	75.724890
177.651488	21.065030	75.729895
177.632896	16.630818	75.734900
176.902825	30.584086	75.739905
176.182179	22.888931	75.744910
175.315077	19.528221	75.749914
174.794649	20.707163	75.754919
174.593285	16.626921	75.759924
172.998824	28.720141	75.764929
172.620748	24.422083	75.769934
171.873314	10.639859	75.774938
171.484850	22.086665	75.779943
170.625565	19.221417	75.784948
169.555994	26.456268	75.789953
169.340631	17.784911	75.794958
168.866550	15.153119	75.799962
168.557852	16.378723	75.804967
167.789870	12.871337	75.809972
166.774830	22.328725	75.814977
166.092236	12.375781	75.819982
164.750503	16.587063	75.824986
164.276961	18.078631	75.829991
164.000004	19.165143	75.834996
163.554359	25.100541	75.840001
162.975695	13.798592	75.845006
162.655800	17.261946	75.850010
161.287974	19.272964	75.855015
160.835359	14.887455	75.860020
160.363881	19.418848	75.865025
159.506991	15.493584	75.870030
158.485291	19.161869	75.875034
158.154222	21.135312	75.880039
157.860122	18.717659	75.885044
156.792874	20.132013	75.890049
156.111799	16.558738	75.895054
155.699327	12.830681	75.900058
155.111008	21.127283	75.905063
154.516640	17.699444	75.910068
153.191558	23.899632	75.915073
153.135797	10.650488	75.920078
152.309739	19.073298	75.925082
151.100224	19.808644	75.930087
150.210899	12.271278	75.935092
149.876260	17.228677	75.940097
149.701629	12.027772	75.945102
149.123352	19.898603	75.950106
148.559325	22.158332	75.955111
147.729271	19.472923	75.960116
146.758355	23.759123	75.965121
146.580753	24.296823	75.970126
145.860978	14.305661	75.975130
144.823276	21.486555	75.980135
144.262731	19.727934	75.985140
143.914466	24.460443	75.990145
143.228734	24.358545	75.995150
142.240950	12.469025	76.000154
141.394566	33.358456	76.005159
140.860052	11.842565	76.010164
140.548014	34.204717	76.015169
139.601515	2.804644	76.020174
138.933401	17.825009	76.025178
138.378584	22.171012	76.030183
138.177590	17.614508	76.035188
136.511471	25.890596	76.040193
135.912501	12.360663	76.045198
135.796852	18.588771	76.050202
135.402644	13.090165	76.055207
134.453437	7.970195	76.060212
133.411368	28.048788	76.065217
133.032914	9.750011	76.070222
132.547300	13.731766	76.075226
131.794897	29.948216	76.080231
131.081853	18.484789	76.085236
130.142169	13.727551	76.090241
129.792041	27.483054	76.095246
129.516923	20.978353	76.100250
128.056465	21.323245	76.105255
127.705750	13.857689	76.110260
126.962221	22.812936	76.115265
126.547179	28.033880	76.120270
126.143745	27.954778	76.125274
124.913032	13.251492	76.130279
124.671073	19.187527	76.135284
123.715091	19.533976	76.140289
123.471435	35.417016	76.145294
122.423933	2.421526	76.150298
121.881852	33.038853	76.155303
121.495734	5.516772	76.160308
120.017728	36.270730	76.165313
119.699426	19.047225	76.170318
118.962888	16.250727	76.175322
118.244645	33.658559	76.180327
118.143891	18.570103	76.185332
117.645350	12.733348	76.190337
116.716082	29.200336	76.195342
116.052993	7.293410	76.200346
115.254835	29.084985	76.205351
114.343496	7.354830	76.210356
113.461982	46.109201	76.215361
113.112543	14.656490	76.220366
112.787971	19.244883	76.225370
112.601022	3.298194	76.230375
111.691790	30.006728	76.235380
110.903422	5.060708	76.240385
109.742809	21.968251	76.245390
109.351740	3.233141	76.250394
108.333834	37.371749	76.255399
108.507811	15.162613	76.260404
107.148259	14.089614	76.265409
106.298345	27.150584	76.270414
106.021774	8.179606	76.275418
105.372818	28.827832	76.280423
105.405774	23.708936	76.285428
103.751736	11.851568	76.290433
103.263742	22.060658	76.295438
102.977271	24.241447	76.300442
101.766368	10.567853	76.305447
101.153871	9.177048	76.310452
100.387212	34.976671	76.315457
99.529714	7.996510	76.320462
99.408013	24.670585	76.325466
99.003141	14.611881	76.330471
98.448196	8.350497	76.335476
97.536283	18.382775	76.340481
96.912478	10.814130	76.345486
95.903881	19.934645	76.350490
94.614468	13.523896	76.355495
94.722867	29.226215	76.360500
94.115178	20.600088	76.365505
93.684060	23.306956	76.370510
93.322882	17.095088	76.375514
92.115929	13.542621	76.380519
92.058833	3.589305	76.385524
90.370105	-0.901815	76.390529
89.680056	18.243913	76.395534
89.385651	5.466472	76.400538
88.743609	21.903422	76.405543
88.674374	4.548768	76.410548
87.584520	16.498479	76.415553
86.660318	14.553454	76.420558
86.232361	18.650593	76.425562
85.650152	13.245053	76.430567
84.921499	9.846534	76.435572
84.205692	11.558086	76.440577
83.750964	31.661293	76.445582
83.371886	4.707349	76.450586
81.960847	31.677249	76.455591
81.434135	6.087164	76.460596
80.888596	13.940167	76.465601
80.017536	18.760782	76.470606
79.181037	17.902409	76.475610
78.207555	9.645266	76.480615
77.948010	20.245249	76.485620
77.584371	21.514317	76.490625
77.265603	2.703039	76.495630
77.079913	19.321082	76.500634
75.841993	19.925385	76.505639
75.304377	10.895462	76.510644
74.448293	-11.832130	76.515649
73.233017	38.022778	76.520654
72.788586	14.330696	76.525658
72.351546	11.377650	76.530663
71.694319	19.011942	76.535668
70.700331	25.943059	76.540673
69.933653	13.958396	76.545678
69.428954	16.503548	76.550682
68.789360	28.148096	76.555687
69.133874	16.459273	76.560692
68.030488	24.592045	76.565697
67.010976	6.370302	76.570702
66.657244	18.465958	76.575706
65.593578	22.945161	76.580711
64.889492	21.796036	76.585716
64.088979	25.512656	76.590721
63.922147	18.498724	76.595726
63.200879	18.831417	76.600730
62.303838	17.754064	76.605735
61.614680	3.838033	76.610740
60.958293	23.790475	76.615745
60.520906	20.194134	76.620750
59.514324	32.825974	76.625754
58.744510	26.922113	76.630759
58.685384	9.015531	76.635764
58.030637	27.733051	76.640769
57.115226	28.751098	76.645774
56.250316	18.352639	76.650778
55.368071	10.893029	76.655783
55.493932	36.927181	76.660788
54.748349	21.364449	76.665793
53.574457	25.977923	76.670798
53.262368	15.559105	76.675802
52.644985	13.319175	76.680807
51.808903	5.953125	76.685812
50.785413	23.425402	76.690817
50.190749	23.622798	76.695822
49.786684	18.715520	76.700826
49.167281	19.560213	76.705831
48.823152	15.950579	76.710836
47.369541	10.967859	76.715841
46.501904	34.271681	76.720846
46.530767	19.369133	76.725850
45.805802	21.766507	76.730855
46.093513	29.738925	76.735860
44.579703	20.227651	76.740865
43.869617	20.973276	76.745870
43.738023	25.691737	76.750874
42.505482	25.990869	76.755879
41.959581	21.128289	76.760884
41.223385	22.160334	76.765889
40.471747	17.124002	76.770894
40.036479	9.194171	76.775898
38.614342	16.841661	76.780903
38.483784	15.087023	76.785908
37.969866	17.047067	76.790913
37.581948	22.115469	76.795918
36.699055	12.147216	76.800922
35.928846	23.008406	76.805927
35.420682	12.583023	76.810932
34.789241	15.807516	76.815937
34.083332	13.988534	76.820942
33.249849	27.423763	76.825946
32.502733	20.516577	76.830951
32.264162	10.522828	76.835956
31.255982	25.901780	76.840961
30.239324	36.947359	76.845966
29.826919	7.936239	76.850970
28.948048	27.559922	76.855975
28.768139	13.417606	76.860980
28.600363	17.727126	76.865985
27.076079	31.759783	76.870990
27.248212	22.017467	76.875994
26.359613	1.155743	76.880999
25.189122	28.013174	76.886004
24.556299	21.128760	76.891009
24.012471	25.517183	76.896014
23.768801	26.956345	76.901018
22.962203	20.627890	76.906023
22.118148	24.403502	76.911028
21.486514	13.283507	76.916033
20.939425	27.543476	76.921038
20.121730	27.005376	76.926042
19.321685	25.515204	76.931047
19.382024	18.167022	76.936052
18.207318	20.811165	76.941057
17.251275	26.110525	76.946062
16.466971	14.302149	76.951066
15.543899	31.052002	76.956071
15.777754	22.304290	76.961076
15.306665	27.032749	76.966081
14.273443	21.618744	76.971086
13.332419	15.254970	76.976090
12.876648	31.163945	76.981095
12.428475	23.285054	76.986100
11.383680	23.164776	76.991105
10.725740	23.744409	76.996110
10.691006	20.484373	77.001114
9.426534	37.716012	77.006119
8.602103	19.256607	77.011124
7.786964	22.329071	77.016129
7.508507	32.326572	77.021134
7.450113	18.264214	77.026139
6.068842	30.820223	77.031143
5.387996	12.131360	77.036148
4.795912	24.690787	77.041153
4.310591	20.351527	77.046158