Mon Mar 08 19:50:26 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.108260	86.477995	0.000000
-0.255479	85.435412	0.005005
-1.147992	70.285586	0.010010
-3.016130	28.062541	0.015014
-7.469921	27.424752	0.020019
-12.410074	16.242979	0.025024
-16.801665	18.835685	0.030029
-21.329380	17.973188	0.035034
-25.199384	22.540484	0.040038
-29.163429	13.864754	0.045043
-32.619935	15.857360	0.050048
-36.084607	24.223265	0.055053
-40.241651	27.382529	0.060058
-43.698683	19.568894	0.065062
-47.732032	24.696828	0.070067
-50.910838	12.933006	0.075072
-55.137399	23.949712	0.080077
-59.413454	27.938486	0.085082
-62.512959	15.495026	0.090086
-66.319220	22.280285	0.095091
-69.887673	17.436300	0.100096
-73.726353	22.126398	0.105101
-77.800169	22.483026	0.110106
-81.747434	20.257116	0.115110
-85.593713	23.491449	0.120115
-89.131398	12.093994	0.125120
-92.642403	18.086344	0.130125
-96.528839	15.169563	0.135130
-99.998202	13.580172	0.140134
-104.112491	20.067724	0.145139
-107.399820	16.558677	0.150144
-111.651091	18.714457	0.155149
-115.667299	23.134921	0.160154
-118.931594	25.650451	0.165158
-122.579068	32.319008	0.170163
-126.615984	15.879700	0.175168
-130.258853	23.257104	0.180173
-134.253120	23.515986	0.185178
-137.669375	15.349086	0.190182
-141.680664	28.252172	0.195187
-145.133921	17.574558	0.200192
-149.052231	15.044543	0.205197
-152.838677	12.802553	0.210202
-156.706480	6.454866	0.215206
-161.036742	14.233704	0.220211
-164.622874	13.136088	0.225216
-168.533506	14.578497	0.230221
-172.260354	19.769678	0.235226
-175.936238	4.307269	0.240230
-179.565010	14.489250	0.245235
-183.158880	14.856196	0.250240
-187.205055	25.114260	0.255245
-190.669699	16.362272	0.260250
-193.978968	7.728993	0.265254
-198.311705	27.269884	0.270259
-201.771162	9.883930	0.275264
-205.380227	9.687252	0.280269
-209.468325	21.994035	0.285274
-213.359912	19.918718	0.290278
-216.877446	22.493713	0.295283
-220.252613	11.756453	0.300288
-224.478551	24.022186	0.305293
-227.947303	15.654082	0.310298
-231.855883	4.621956	0.315302
-236.070219	31.747494	0.320307
-239.641359	3.724776	0.325312
-243.122524	2.523801	0.330317
-247.049792	13.150874	0.335322
-250.956415	17.186663	0.340326
-254.699478	26.023037	0.345331
-258.201667	22.978967	0.350336
-262.056472	20.082637	0.355341
-265.902612	26.289556	0.360346
-269.073888	8.766262	0.365350
-273.495778	16.474768	0.370355
-277.179830	16.526690	0.375360
-280.617355	16.895634	0.380365
-284.750564	27.636063	0.385370
-288.522916	19.847899	0.390374
-292.580692	23.259804	0.395379
-296.247112	20.697709	0.400384
-299.670133	9.659151	0.405389
-303.648733	6.336410	0.410394
-306.657499	8.584336	0.415398
-310.981681	17.185566	0.420403
-314.637770	18.135029	0.425408
-318.376885	25.004558	0.430413
-322.546436	22.822414	0.435418
-325.885505	20.367371	0.440422
-330.123936	34.737192	0.445427
-333.553555	13.015130	0.450432
-337.307723	15.355279	0.455437
-341.451309	26.195217	0.460442
-344.983373	19.324348	0.465446
-348.736728	23.386284	0.470451
-352.005523	18.343520	0.475456
-355.681606	20.735882	0.480461
-359.671117	21.871095	0.485466
-363.376616	7.944831	0.490470
-367.498310	26.061533	0.495475
-371.469567	20.907031	0.500480
-375.253623	16.336038	0.505485
-379.163876	19.502200	0.510490
-382.572921	13.892137	0.515494
-386.369368	24.917980	0.520499
-389.968703	22.685915	0.525504
-393.889268	23.791255	0.530509
-397.641727	20.085662	0.535514
-400.856383	14.460358	0.540518
-404.924686	23.265306	0.545523
-408.703777	20.007072	0.550528
-412.449871	17.104670	0.555533
-416.545559	30.015344	0.560538
-420.018090	18.070311	0.565542
-423.885154	27.617383	0.570547
-427.785132	19.903441	0.575552
-431.321811	17.502176	0.580557
-435.492681	22.863989	0.585562
-438.902471	16.976606	0.590566
-442.808848	30.661276	0.595571
-446.579856	21.740995	0.600576
-449.920834	22.162568	0.605581
-453.904150	20.786637	0.610586
-457.250423	24.626052	0.615590
-461.081990	16.346201	0.620595
-465.141640	14.925714	0.625600
-469.268244	24.615215	0.630605
-473.020731	21.844806	0.635610
-476.828419	19.691875	0.640614
-480.522687	24.462032	0.645619
-484.031921	18.156969	0.650624
-487.319772	15.400687	0.655629
-491.723338	18.918601	0.660634
-495.251325	9.689963	0.665638
-499.258373	21.944835	0.670643
-502.930017	12.985135	0.675648
-506.333904	8.213307	0.680653
-510.440501	18.948265	0.685658
-514.053911	9.074186	0.690662
-518.261696	30.416867	0.695667
-521.855511	19.314468	0.700672
-525.474675	12.531905	0.705677
-528.963770	13.045048	0.710682
-532.658595	13.600514	0.715686
-536.502934	14.645030	0.720691
-540.505150	19.086022	0.725696
-544.219136	19.835363	0.730701
-548.283801	21.451210	0.735706
-551.497679	11.817703	0.740710
-555.554907	15.964756	0.745715
-559.445074	23.916819	0.750720
-562.862009	19.191306	0.755725
-566.627523	17.091704	0.760730
-570.698864	11.567213	0.765734
-574.564060	21.498956	0.770739
-578.351977	19.641051	0.775744
-581.568377	17.423801	0.780749
-585.912968	28.171673	0.785754
-589.019720	21.446116	0.790758
-593.193385	27.819389	0.795763
-597.134586	23.168211	0.800768
-600.784026	14.165703	0.805773
-604.872966	19.850578	0.810778
-607.852285	15.056803	0.815782
-612.007707	20.384910	0.820787
-616.003932	23.000682	0.825792
-619.310408	16.953574	0.830797
-623.260444	26.913139	0.835802
-626.699519	21.669328	0.840806
-630.601306	18.743267	0.845811
-634.544468	18.818212	0.850816
-638.265962	13.097612	0.855821
-642.248474	25.506471	0.860826
-645.523410	19.131112	0.865830
-649.397729	19.441068	0.870835
-653.550476	21.547366	0.875840
-657.139343	13.620129	0.880845
-661.030244	22.490178	0.885850
-664.449646	12.195870	0.890854
-668.383632	25.609337	0.895859
-672.205735	19.925362	0.900864
-675.899719	7.174105	0.905869
-679.483635	26.902021	0.910874
-683.174029	11.474327	0.915878
-687.230097	22.655623	0.920883
-691.033718	16.695938	0.925888
-694.694979	16.257625	0.930893
-698.984766	25.524179	0.935898
-702.136843	20.833817	0.940902
-705.952547	17.985584	0.945907
-710.092746	18.533650	0.950912
-713.405363	10.850921	0.955917
-717.161300	19.305282	0.960922
-720.915123	14.957088	0.965926
-724.752110	25.677696	0.970931
-728.487194	25.021015	0.975936
-732.312712	11.385771	0.980941
-736.150050	17.055886	0.985946
-739.746447	14.313001	0.990950
-743.718943	12.694579	0.995955
-747.867012	22.153015	1.000960
-751.347816	19.333332	1.005965
-755.165246	22.565683	1.010970
-758.674341	17.752698	1.015974
-762.279183	16.570674	1.020979
-766.080158	14.899649	1.025984
-769.611783	12.949061	1.030989
-773.366911	20.257029	1.035994
-777.218848	18.198384	1.040998
-781.342064	16.067993	1.046003
-785.301535	14.999448	1.051008
-788.588699	21.769063	1.056013
-792.673860	15.015676	1.061018
-796.451351	15.755061	1.066022
-800.072452	26.195294	1.071027
-803.642195	28.528767	1.076032
-807.419790	20.162039	1.081037
-811.732736	31.248989	1.086042
-815.380321	23.916386	1.091046
-818.831908	18.685905	1.096051
-822.697249	20.735520	1.101056
-826.150976	21.492583	1.106061
-829.836687	16.441456	1.111066
-833.468168	14.779716	1.116070
-837.774879	25.085183	1.121075
-841.666227	19.846188	1.126080
-845.256454	20.842699	1.131085
-849.122338	21.280933	1.136090
-852.346568	19.371213	1.141094
-856.258515	15.531023	1.146099
-860.566575	18.081941	1.151104
-863.990445	14.198435	1.156109
-867.963275	21.443584	1.161114
-871.534813	17.209988	1.166118
-875.132954	25.388650	1.171123
-878.844377	23.662495	1.176128
-882.682379	22.439088	1.181133
-886.608720	30.862609	1.186138
-890.265602	23.829634	1.191142
-894.407595	20.387377	1.196147
-897.907150	21.618610	1.201152
-901.173165	17.853413	1.206157
-905.036521	20.719637	1.211162
-909.172536	12.613797	1.216166
-913.081986	23.516568	1.221171
-916.987443	28.552941	1.226176
-920.231976	10.055266	1.231181
-923.833315	16.654533	1.236186
-927.821234	14.267825	1.241190
-931.594269	16.827940	1.246195
-935.735700	21.911530	1.251200
-939.248120	15.125179	1.256205
-943.283118	12.900554	1.261210
-946.728083	18.796821	1.266214
-950.179766	21.609910	1.271219
-954.222164	18.943401	1.276224
-957.706892	3.886974	1.281229
-961.626058	23.265192	1.286234
-965.372241	19.580017	1.291238
-969.724119	11.318011	1.296243
-973.463409	20.709880	1.301248
-976.657436	25.389759	1.306253
-980.645323	14.532468	1.311258
-984.178147	11.324098	1.316262
-987.935820	21.196704	1.321267
-992.004079	23.007830	1.326272
-995.372257	8.396408	1.331277
-999.642200	18.891796	1.336282
-1003.197503	10.352676	1.341286
-1007.066240	16.379867	1.346291
-1010.810005	24.490556	1.351296
-1014.565070	13.346958	1.356301
-1018.328000	10.639025	1.361306
-1021.820367	14.737521	1.366310
-1025.691948	13.764128	1.371315
-1029.829864	23.098417	1.376320
-1033.271722	19.359954	1.381325
-1037.037732	20.952524	1.386330
-1040.581667	11.415097	1.391334
-1044.331591	10.889017	1.396339
-1048.441988	24.518915	1.401344
-1052.059119	19.211197	1.406349
-1056.331210	22.491514	1.411354
-1059.540286	27.599650	1.416358
-1063.170298	19.159296	1.421363
-1067.130163	24.821147	1.426368
-1070.620974	14.015393	1.431373
-1074.917677	31.196170	1.436378
-1078.328154	15.883648	1.441382
-1081.941361	19.334567	1.446387
-1085.865358	20.249223	1.451392
-1089.651790	22.315034	1.456397
-1093.528782	24.202965	1.461402
-1096.972135	27.823842	1.466406
-1100.642723	25.301526	1.471411
-1104.647398	27.619871	1.476416
-1108.329595	13.815727	1.481421
-1112.173138	17.024439	1.486426
-1116.293641	18.913516	1.491430
-1119.912867	28.281672	1.496435
-1123.510362	23.138068	1.501440
-1127.205450	15.107167	1.506445
-1130.893725	16.391009	1.511450
-1134.844998	13.505255	1.516454
-1138.453761	22.438137	1.521459
-1142.438449	20.652050	1.526464
-1145.876600	8.702691	1.531469
-1149.903704	28.954669	1.536474
-1153.678034	19.279252	1.541478
-1157.427992	22.737972	1.546483
-1161.405209	16.636557	1.551488
-1164.804343	18.150138	1.556493
-1168.987214	29.576404	1.561498
-1172.649499	21.338495	1.566502
-1175.962198	27.395261	1.571507
-1179.765019	28.025783	1.576512
-1183.304339	14.001809	1.581517
-1187.360413	16.721143	1.586522
-1191.303255	23.241414	1.591526
-1195.180357	17.925063	1.596531
-1198.815306	25.392632	1.601536
-1202.605761	22.941693	1.606541
-1205.847790	21.650273	1.611546
-1209.801763	19.165590	1.616550
-1213.739763	26.725822	1.621555
-1217.816697	34.584237	1.626560
-1221.271028	12.615347	1.631565
-1225.280874	21.352356	1.636570
-1228.781899	9.646559	1.641574
-1232.421954	19.043434	1.646579
-1236.510637	26.176845	1.651584
-1239.970061	16.366042	1.656589
-1244.176014	20.388254	1.661594
-1247.489668	13.758226	1.666598
-1251.447811	17.173142	1.671603
-1255.390796	22.129341	1.676608
-1258.893041	9.914478	1.681613
-1262.501776	18.177388	1.686618
-1266.249528	12.327998	1.691622
-1270.267275	18.217043	1.696627
-1274.051382	25.260778	1.701632
-1277.231477	15.619782	1.706637
-1281.737743	24.400060	1.711642
-1285.415384	10.444125	1.716646
-1289.099480	21.021281	1.721651
-1293.001570	27.815870	1.726656
-1296.382284	22.680426	1.731661
-1300.196381	31.403579	1.736666
-1303.900091	21.321340	1.741670
-1307.976506	17.084087	1.746675
-1311.704706	23.801993	1.751680
-1315.205456	15.388675	1.756685
-1319.258419	22.360402	1.761690
-1322.754759	30.677951	1.766694
-1326.275910	8.691562	1.771699
-1330.642248	14.723224	1.776704
-1334.245300	5.389691	1.781709
-1338.173124	24.173813	1.786714
-1341.714773	15.689820	1.791718
-1345.104865	12.206877	1.796723
-1349.290998	20.767319	1.801728
-1352.815485	12.275869	1.806733
-1356.769855	32.086051	1.811738
-1360.213289	9.224765	1.816742
-1364.027821	13.086771	1.821747
-1368.170858	19.271977	1.826752
-1371.768688	27.982697	1.831757
-1375.449094	21.072551	1.836762
-1379.192823	9.464194	1.841766
-1383.102531	24.822229	1.846771
-1386.630671	22.118314	1.851776
-1390.249292	10.923572	1.856781
-1394.361978	28.319823	1.861786
-1398.545153	22.784761	1.866790
-1401.778207	7.174743	1.871795
-1405.640856	30.030900	1.876800
-1409.102712	23.803271	1.881805
-1413.212816	1.810415	1.886810
-1416.746211	30.233626	1.891814
-1420.655222	0.198393	1.896819
-1424.832563	28.459797	1.901824
-1427.964439	19.645436	1.906829
-1431.793732	18.697491	1.911834
-1435.608924	12.348298	1.916838
-1439.312017	14.786071	1.921843
-1443.519337	16.590283	1.926848
-1446.796841	10.643835	1.931853
-1450.847204	20.223409	1.936858
-1454.675920	21.910259	1.941862
-1458.055442	26.544788	1.946867
-1462.245949	25.694147	1.951872
-1465.794163	18.007697	1.956877
-1469.419502	26.596819	1.961882
-1473.543277	30.811268	1.966886
-1476.863366	12.930499	1.971891
-1481.155458	24.983423	1.976896
-1484.718320	28.184067	1.981901
-1488.144703	21.340658	1.986906
-1491.806544	6.146340	1.991910
-1495.568189	33.128731	1.996915
-1500.082174	17.939229	2.006912
-1500.920793	26.992395	2.016909
-1498.383219	17.258419	2.026906
-1495.261737	18.332757	2.036902
-1493.281322	17.032110	2.046899
-1491.573182	20.072633	2.056896
-1489.375000	26.692838	2.066893
-1487.663862	11.907912	2.076890
-1485.900045	27.912758	2.086886
-1483.559204	23.889344	2.096883
-1481.755789	21.301884	2.106880
-1480.107223	20.068593	2.116877
-1477.911327	25.604520	2.126874
-1476.202520	21.882825	2.136870
-1474.477872	23.359257	2.146867
-1472.516530	23.515784	2.156864
-1470.639601	20.373444	2.166861
-1468.519019	15.108041	2.176858
-1466.716511	16.660426	2.186854
-1464.727834	18.123010	2.196851
-1463.007132	19.745334	2.206848
-1461.222999	18.877164	2.216845
-1459.310303	14.063444	2.226842
-1456.988256	22.267938	2.236838
-1455.482530	15.549001	2.246835
-1453.904681	19.903474	2.256832
-1451.531303	14.905483	2.266829
-1449.593338	17.004573	2.276826
-1447.673148	9.619330	2.286822
-1446.277834	11.135880	2.296819
-1444.140950	25.563779	2.306816
-1442.259621	12.764639	2.316813
-1440.287985	18.767526	2.326810
-1438.477048	11.822907	2.336806
-1436.270798	19.817031	2.346803
-1434.861477	11.248945	2.356800
-1433.092630	19.572028	2.366797
-1430.972457	15.906077	2.376794
-1429.035202	17.141679	2.386790
-1427.153281	23.244200	2.396787
-1425.240575	22.865435	2.406784
-1423.512675	25.361310	2.416781
-1421.723724	24.140320	2.426778
-1419.769351	23.974347	2.436774
-1417.733773	17.528999	2.446771
-1415.830051	22.472337	2.456768
-1413.809080	13.942120	2.466765
-1412.303583	27.820658	2.476762
-1410.122310	14.796690	2.486758
-1408.337276	21.020519	2.496755
-1406.520732	18.449960	2.506752
-1404.739421	24.314417	2.516749
-1402.775766	23.867519	2.526746
-1400.460109	20.272923	2.536742
-1398.950410	23.170036	2.546739
-1397.429320	18.562726	2.556736
-1395.348147	22.631422	2.566733
-1393.310914	20.368150	2.576730
-1391.268308	23.393102	2.586726
-1389.513027	27.686067	2.596723
-1387.786501	23.296909	2.606720
-1386.175860	20.629862	2.616717
-1384.167600	16.285602	2.626714
-1382.045803	17.513807	2.636710
-1379.936483	19.460800	2.646707
-1378.145750	23.795462	2.656704
-1376.523381	26.655610	2.666701
-1374.634861	17.898746	2.676698
-1372.568788	19.888982	2.686694
-1370.697372	16.461835	2.696691
-1368.843485	23.825645	2.706688
-1366.869820	16.376640	2.716685
-1365.209399	16.540376	2.726682
-1363.529627	12.960768	2.736678
-1361.528191	15.864450	2.746675
-1359.672933	22.575991	2.756672
-1357.741673	19.998158	2.766669
-1355.755301	15.458493	2.776666
-1353.856229	14.305185	2.786662
-1351.981773	15.216193	2.796659
-1350.210452	21.600149	2.806656
-1348.215536	18.895302	2.816653
-1346.560058	18.414101	2.826650
-1344.427319	13.776813	2.836646
-1342.607740	25.061637	2.846643
-1340.637023	19.064069	2.856640
-1339.084483	18.987742	2.866637
-1336.848327	14.787032	2.876634
-1335.129946	17.770778	2.886630
-1333.330282	13.208914	2.896627
-1331.460468	16.758907	2.906624
-1329.403400	17.673861	2.916621
-1327.527695	18.471012	2.926618
-1325.751807	22.118144	2.936614
-1323.925248	19.596568	2.946611
-1321.812028	22.007168	2.956608
-1320.239115	15.755941	2.966605
-1318.488664	24.034705	2.976602
-1315.926563	22.975822	2.986598
-1314.438849	23.033036	2.996595
-1312.965373	20.354835	3.006592
-1310.687041	18.673528	3.016589
-1308.580715	19.705345	3.026586
-1306.981708	19.193739	3.036582
-1305.126540	22.419282	3.046579
-1303.166001	20.578859	3.056576
-1301.542029	21.288435	3.066573
-1299.452601	27.471537	3.076570
-1297.566413	19.158753	3.086566
-1295.796100	22.170533	3.096563
-1293.581560	20.265785	3.106560
-1291.971987	22.294418	3.116557
-1290.231352	19.278234	3.126554
-1288.273361	19.220732	3.136550
-1286.417410	15.600350	3.146547
-1284.362137	16.719301	3.156544
-1282.604240	14.486619	3.166541
-1280.793497	16.203612	3.176538
-1278.772699	16.143961	3.186534
-1276.808963	10.090726	3.196531
-1275.131650	13.272128	3.206528
-1273.230249	14.115735	3.216525
-1271.370659	16.278043	3.226522
-1269.379674	19.020862	3.236518
-1267.214260	14.361044	3.246515
-1265.975945	21.922918	3.256512
-1264.001254	19.054022	3.266509
-1261.792655	17.273403	3.276506
-1260.311478	22.134506	3.286502
-1258.060757	15.064377	3.296499
-1256.197803	19.777553	3.306496
-1254.529339	22.180446	3.316493
-1252.649706	21.181898	3.326490
-1250.448040	15.603729	3.336486
-1248.767969	20.016200	3.346483
-1246.916181	19.947309	3.356480
-1245.019767	21.699566	3.366477
-1243.070755	13.196785	3.376474
-1241.583986	20.881537	3.386470
-1239.357035	18.684348	3.396467
-1237.675631	15.218240	3.406464
-1235.670249	15.232141	3.416461
-1233.715889	15.893635	3.426458
-1231.621735	12.999334	3.436454
-1229.855389	22.233980	3.446451
-1228.236023	15.549092	3.456448
-1226.481572	19.744431	3.466445
-1224.362332	26.514897	3.476442
-1222.281577	21.025566	3.486438
-1220.532770	13.199001	3.496435
-1218.737658	22.924807	3.506432
-1216.993754	27.472345	3.516429
-1215.171139	19.960788	3.526426
-1213.301200	18.722261	3.536422
-1211.213291	18.505099	3.546419
-1209.322894	16.803862	3.556416
-1207.687499	20.337788	3.566413
-1205.526604	27.808927	3.576410
-1203.805153	19.162595	3.586406
-1201.827086	19.982943	3.596403
-1199.833274	17.699944	3.606400
-1197.963560	20.806415	3.616397
-1196.320633	25.333812	3.626394
-1194.256733	29.040752	3.636390
-1192.555987	13.026166	3.646387
-1190.764077	17.256589	3.656384
-1188.958555	17.954565	3.666381
-1186.702421	10.728910	3.676378
-1184.846845	7.539689	3.686374
-1183.081685	14.709447	3.696371
-1181.365150	21.288612	3.706368
-1179.425144	13.324123	3.716365
-1177.408020	12.807286	3.726362
-1175.599003	13.375249	3.736358
-1173.565469	12.451608	3.746355
-1171.687997	16.584680	3.756352
-1170.179060	17.562209	3.766349
-1167.929204	15.490887	3.776346
-1166.320494	16.427195	3.786342
-1164.421703	16.442422	3.796339
-1162.489900	13.995703	3.806336
-1160.653407	20.775151	3.816333
-1158.693888	15.409474	3.826330
-1156.698284	16.331258	3.836326
-1155.130503	23.458416	3.846323
-1152.982329	30.877964	3.856320
-1151.335908	22.485228	3.866317
-1149.397014	26.659019	3.876314
-1147.362652	20.256711	3.886310
-1145.298534	18.774032	3.896307
-1143.640527	21.003429	3.906304
-1141.850746	12.470937	3.916301
-1140.225230	14.040844	3.926298
-1138.088670	21.171755	3.936294
-1136.249453	15.841128	3.946291
-1134.393251	22.590607	3.956288
-1132.502286	20.579888	3.966285
-1130.434704	14.221226	3.976282
-1128.650030	16.149338	3.986278
-1126.641032	26.753580	3.996275
-1124.821947	19.278965	4.006272
-1122.914544	29.140044	4.016269
-1121.207917	14.213952	4.026266
-1119.193221	26.116670	4.036262
-1117.224069	19.328531	4.046259
-1115.566124	19.781769	4.056256
-1114.036801	25.026824	4.066253
-1112.123281	22.215201	4.076250
-1109.879887	16.897303	4.086246
-1107.840192	19.233028	4.096243
-1106.230340	22.052747	4.106240
-1104.513050	21.784445	4.116237
-1102.194421	22.127276	4.126234
-1100.754018	25.836147	4.136230
-1098.561012	22.821946	4.146227
-1096.698372	21.887815	4.156224
-1095.109911	17.112027	4.166221
-1092.885783	24.382125	4.176218
-1090.847429	19.419123	4.186214
-1089.258486	18.901381	4.196211
-1087.549537	20.653757	4.206208
-1085.670989	26.340308	4.216205
-1083.428798	16.251384	4.226202
-1081.843337	17.494606	4.236198
-1079.746895	18.660836	4.246195
-1078.034943	18.497611	4.256192
-1076.523935	20.494798	4.266189
-1074.417635	22.709383	4.276186
-1072.151734	16.012753	4.286182
-1070.333204	14.236285	4.296179
-1068.753431	19.471722	4.306176
-1066.621180	21.579539	4.316173
-1064.930130	13.124464	4.326170
-1063.333545	18.595620	4.336166
-1061.118965	11.930893	4.346163
-1059.394034	18.095158	4.356160
-1057.158582	20.147006	4.366157
-1055.524991	18.471175	4.376154
-1053.640414	15.754221	4.386150
-1051.636655	9.306367	4.396147
-1049.884210	19.097560	4.406144
-1048.137763	22.162297	4.416141
-1045.872505	17.159886	4.426138
-1044.321922	19.536001	4.436134
-1042.353156	16.336678	4.446131
-1040.404959	17.521916	4.456128
-1038.703201	17.767689	4.466125
-1036.884296	10.062658	4.476122
-1034.889328	11.243578	4.486118
-1032.907662	21.650188	4.496115
-1031.279900	17.090772	4.506112
-1028.883144	16.977527	4.516109
-1027.080777	22.349491	4.526106
-1025.683806	15.124019	4.536102
-1023.752845	19.644951	4.546099
-1021.511118	24.131977	4.556096
-1019.715551	20.453562	4.566093
-1018.052556	18.875679	4.576090
-1016.091935	12.786830	4.586086
-1014.250705	19.319348	4.596083
-1012.848787	15.792306	4.606080
-1010.452268	19.013621	4.616077
-1008.298356	26.399239	4.626074
-1006.828246	16.015457	4.636070
-1004.717185	17.673593	4.646067
-1002.800680	18.971292	4.656064
-1001.116708	15.225481	4.666061
-999.104157	17.464599	4.676058
-997.507559	20.531234	4.686054
-995.603561	17.768591	4.696051
-993.538926	15.641795	4.706048
-991.588810	18.730845	4.716045
-989.750076	14.953978	4.726042
-988.015130	18.416888	4.736038
-986.204482	9.693284	4.746035
-984.410575	25.155404	4.756032
-982.518737	20.378539	4.766029
-980.304408	23.575341	4.776026
-978.360137	21.191507	4.786022
-976.470914	13.192660	4.796019
-974.728907	23.317146	4.806016
-973.056788	19.799022	4.816013
-971.293000	31.157842	4.826010
-969.176050	22.360002	4.836006
-967.158982	25.853604	4.846003
-965.503360	27.960365	4.856000
-963.841238	26.352660	4.865997
-961.717118	19.083576	4.875994
-959.666967	19.002141	4.885990
-957.852107	24.040610	4.895987
-956.060847	24.606847	4.905984
-954.321102	31.267747	4.915981
-952.375233	19.748518	4.925978
-950.154583	25.157869	4.935974
-948.725839	27.221977	4.945971
-946.527122	17.146435	4.955968
-944.861574	33.915878	4.965965
-942.742273	30.773084	4.975962
-941.000698	22.736289	4.985958
-939.166454	25.663925	4.995955
-937.584363	20.136148	5.005952
-935.436385	22.547867	5.015949
-933.490912	20.613846	5.025946
-931.834826	22.690559	5.035942
-929.758276	16.303785	5.045939
-927.732339	25.628233	5.055936
-925.945811	30.353913	5.065933
-924.299853	24.735410	5.075930
-922.262510	20.573178	5.085926
-920.405011	27.739452	5.095923
-918.410398	28.604763	5.105920
-916.643371	22.796395	5.115917
-914.465673	24.663419	5.125914
-912.811722	18.148447	5.135910
-911.117365	23.686186	5.145907
-909.437433	26.701670	5.155904
-907.379955	26.576481	5.165901
-905.322037	27.057497	5.175898
-903.578964	27.301502	5.185894
-901.500558	20.028724	5.195891
-899.707122	27.060003	5.205888
-897.823690	23.519198	5.215885
-896.157240	21.593501	5.225882
-894.248938	21.961087	5.235878
-892.248091	18.890956	5.245875
-890.448207	18.795911	5.255872
-888.251703	25.821180	5.265869
-886.565644	22.457189	5.275866
-884.636584	19.676417	5.285862
-882.862454	17.251969	5.295859
-881.323304	22.912432	5.305856
-879.286336	19.149742	5.315853
-876.889239	15.591571	5.325850
-875.407385	25.143564	5.335846
-873.569303	21.262682	5.345843
-871.627498	23.893723	5.355840
-869.550920	16.524955	5.365837
-868.168705	19.651215	5.375834
-865.932967	26.434988	5.385830
-863.688390	11.340949	5.395827
-862.502913	14.683385	5.405824
-860.610262	19.996845	5.415821
-858.361712	21.007918	5.425818
-856.624676	17.948410	5.435814
-854.858418	24.385691	5.445811
-852.787191	19.434995	5.455808
-851.022134	21.666441	5.465805
-849.224802	25.108437	5.475802
-847.128151	18.416958	5.485798
-845.319965	20.153652	5.495795
-843.638830	27.561327	5.505792
-841.502881	24.979607	5.515789
-839.717164	21.797074	5.525786
-837.654485	25.288237	5.535782
-835.866276	17.191958	5.545779
-834.105991	27.012087	5.555776
-832.092607	27.157678	5.565773
-830.475976	20.190857	5.575770
-828.671303	17.838931	5.585766
-826.660913	16.545102	5.595763
-824.711846	27.590242	5.605760
-822.459908	18.328871	5.615757
-820.912349	27.027302	5.625754
-819.080278	20.018159	5.635750
-817.520548	21.331987	5.645747
-815.272236	17.758187	5.655744
-813.387259	23.557620	5.665741
-811.565374	26.038945	5.675738
-809.447880	15.589682	5.685734
-807.898276	11.658650	5.695731
-806.130473	13.123953	5.705728
-804.429332	15.447750	5.715725
-802.160912	25.742442	5.725722
-800.047047	18.587228	5.735718
-798.256972	19.463228	5.745715
-796.650565	18.865529	5.755712
-794.767316	19.151942	5.765709
-792.989275	21.269260	5.775706
-790.880912	19.015656	5.785702
-788.891752	21.473421	5.795699
-786.954123	17.742472	5.805696
-785.441970	19.651255	5.815693
-783.511264	15.493550	5.825690
-781.411786	14.720749	5.835686
-779.598119	16.911325	5.845683
-777.968992	16.464733	5.855680
-776.158206	20.649849	5.865677
-774.118759	18.143607	5.875674
-772.060870	18.296346	5.885670
-770.202989	14.802352	5.895667
-768.341766	20.949807	5.905664
-766.562010	19.808142	5.915661
-764.982067	19.588879	5.925658
-762.751992	19.395183	5.935654
-760.828215	11.593059	5.945651
-758.911561	15.849684	5.955648
-757.141054	24.034143	5.965645
-755.209856	16.117159	5.975642
-753.542288	21.458789	5.985638
-751.731637	17.823944	5.995635
-749.743761	24.380621	6.005632
-747.513782	24.739549	6.015629
-745.967324	15.720449	6.025626
-744.289698	15.785569	6.035622
-741.755217	14.524894	6.045619
-740.390509	18.182942	6.055616
-738.507884	24.350687	6.065613
-736.534691	16.799612	6.075610
-734.380328	18.394238	6.085606
-732.598258	15.692334	6.095603
-731.082473	13.081928	6.105600
-728.867608	13.610645	6.115597
-727.280712	10.902042	6.125594
-725.381859	20.894314	6.135590
-723.256594	14.296253	6.145587
-721.314811	8.237482	6.155584
-719.763831	13.632499	6.165581
-717.977398	8.297981	6.175578
-715.869602	13.684547	6.185574
-713.836911	11.880442	6.195571
-712.299210	16.750255	6.205568
-710.162872	13.268649	6.215565
-708.179123	18.509267	6.225562
-706.205145	16.594557	6.235558
-704.613443	9.478653	6.245555
-702.676345	14.617789	6.255552
-701.040286	16.170535	6.265549
-699.326604	18.752916	6.275546
-697.070055	11.988647	6.285542
-695.363276	18.997627	6.295539
-693.217740	11.793235	6.305536
-691.460034	17.532586	6.315533
-689.754240	22.479762	6.325530
-687.674132	11.831321	6.335526
-685.660095	10.848060	6.345523
-684.222899	14.429827	6.355520
-682.190355	18.506960	6.365517
-680.005011	8.801649	6.375514
-678.121818	4.462158	6.385510
-676.375668	8.461903	6.395507
-674.489443	4.500852	6.405504
-672.909269	6.891438	6.415501
-671.066965	9.626960	6.425498
-668.920439	5.212247	6.435494
-667.143989	3.854884	6.445491
-665.180398	8.858774	6.455488
-663.302858	12.193370	6.465485
-661.565919	12.110133	6.475482
-659.730312	5.672084	6.485478
-657.558801	16.287124	6.495475
-655.794289	12.463945	6.505472
-653.927891	9.650738	6.515469
-652.201069	16.527084	6.525466
-650.298349	8.911552	6.535462
-648.182270	9.568226	6.545459
-646.523039	11.327294	6.555456
-644.575870	12.337777	6.565453
-642.673641	17.872511	6.575450
-640.758066	10.567542	6.585446
-638.938613	10.709546	6.595443
-636.988805	15.237275	6.605440
-635.158793	15.366542	6.615437
-633.457398	9.774107	6.625434
-631.457174	16.338389	6.635430
-629.744257	15.384335	6.645427
-627.599146	11.721410	6.655424
-625.726113	16.608761	6.665421
-623.810407	14.386080	6.675418
-622.024266	13.980823	6.685414
-620.531719	10.646350	6.695411
-618.556712	10.457223	6.705408
-616.148218	13.010768	6.715405
-614.754456	18.743589	6.725402
-612.796557	14.021182	6.735398
-610.878991	15.391662	6.745395
-608.710134	15.386299	6.755392
-606.933788	11.788617	6.765389
-605.235584	15.271902	6.775386
-603.464172	17.998280	6.785382
-601.157728	16.524724	6.795379
-599.458639	12.664670	6.805376
-597.792850	14.015384	6.815373
-595.553003	16.924291	6.825370
-593.986782	12.570762	6.835366
-592.304725	15.080910	6.845363
-590.203367	19.920767	6.855360
-588.155970	20.905815	6.865357
-586.452769	19.643889	6.875354
-584.485723	10.287715	6.885350
-582.646660	13.754831	6.895347
-580.754698	12.994829	6.905344
-578.924740	24.220268	6.915341
-577.158598	22.023092	6.925338
-575.063073	11.601206	6.935334
-573.117591	18.046399	6.945331
-571.399983	8.723764	6.955328
-569.674785	19.759112	6.965325
-567.870278	15.932763	6.975322
-565.604863	11.499146	6.985318
-563.773974	14.299733	6.995315
-562.072507	13.710690	7.005312
-560.264431	15.654453	7.015309
-558.291799	21.702193	7.025306
-556.233529	16.780651	7.035302
-554.466319	13.440238	7.045299
-552.912339	14.930414	7.055296
-550.654926	18.125487	7.065293
-548.911495	19.102280	7.075290
-547.109013	12.664861	7.085286
-544.999522	17.329787	7.095283
-543.289517	17.648808	7.105280
-541.531019	14.312954	7.115277
-539.574884	12.737523	7.125274
-537.594088	10.572404	7.135270
-535.727576	12.653686	7.145267
-533.925301	10.483927	7.155264
-532.219205	15.726418	7.165261
-530.000399	14.304819	7.175258
-528.251157	19.147291	7.185254
-526.244321	19.422074	7.195251
-524.482647	11.628645	7.205248
-522.663080	16.559356	7.215245
-520.805010	13.395496	7.225242
-518.734115	14.747878	7.235238
-516.728783	21.202511	7.245235
-515.226744	16.368258	7.255232
-513.542802	20.044932	7.265229
-511.479264	16.804055	7.275226
-509.400556	13.893895	7.285222
-507.464791	12.088074	7.295219
-505.753056	14.219360	7.305216
-503.812211	17.046642	7.315213
-501.872816	15.990198	7.325210
-500.146416	13.161571	7.335206
-498.143336	12.448621	7.345203
-496.168803	20.742809	7.355200
-494.564019	19.814013	7.365197
-492.588134	17.570772	7.375194
-490.634696	15.091132	7.385190
-489.009519	15.213753	7.395187
-487.086791	23.827257	7.405184
-485.082069	22.160431	7.415181
-483.180430	22.398370	7.425178
-481.257370	18.393686	7.435174
-479.357248	17.341952	7.445171
-477.669782	20.067624	7.455168
-475.594710	19.824744	7.465165
-473.961229	18.676656	7.475162
-472.145979	16.539604	7.485158
-469.786331	20.114722	7.495155
-468.418934	14.321534	7.505152
-466.384855	12.714769	7.515149
-464.252044	18.364405	7.525146
-462.343752	12.666414	7.535142
-460.799738	18.700584	7.545139
-459.123766	24.511594	7.555136
-456.964084	21.484342	7.565133
-454.974002	24.335382	7.575130
-453.490587	21.861356	7.585126
-451.058118	20.985148	7.595123
-449.235569	24.205554	7.605120
-447.607724	22.305273	7.615117
-445.499112	22.211790	7.625114
-443.806240	21.098447	7.635110
-441.904871	15.321054	7.645107
-440.143353	21.767323	7.655104
-438.205092	20.213774	7.665101
-436.195061	25.137829	7.675098
-434.538282	18.856372	7.685094
-432.632172	14.680759	7.695091
-430.821773	12.200324	7.705088
-428.746086	17.074428	7.715085
-426.942473	18.831126	7.725082
-425.235044	18.089658	7.735078
-423.232126	15.717427	7.745075
-421.245182	17.989559	7.755072
-419.365356	18.398388	7.765069
-417.254260	21.370655	7.775066
-415.776086	18.919593	7.785062
-413.736723	13.022301	7.795059
-411.790140	22.746729	7.805056
-409.937679	17.030849	7.815053
-408.200970	18.839294	7.825050
-406.530928	21.196771	7.835046
-404.379798	17.757272	7.845043
-402.540286	15.891117	7.855040
-400.613518	19.126498	7.865037
-398.792672	28.465254	7.875034
-396.810179	19.667234	7.885030
-394.915530	18.995364	7.895027
-393.132316	21.738967	7.905024
-391.519290	15.175595	7.915021
-389.395086	24.721696	7.925018
-387.137681	16.362921	7.935014
-385.724616	18.703024	7.945011
-383.907853	19.837168	7.955008
-381.720760	12.740073	7.965005
-380.170097	16.300763	7.975002
-378.138984	23.757134	7.984998
-376.207690	21.915816	7.994995
-374.456836	20.142778	8.004992
-372.524528	21.752664	8.014989
-370.570739	19.055182	8.024986
-368.527433	18.073827	8.034982
-366.851132	15.406439	8.044979
-364.877087	17.701203	8.054976
-363.159278	18.416978	8.064973
-361.396955	17.925722	8.074970
-359.558690	15.200905	8.084966
-357.396670	22.197476	8.094963
-355.416912	17.280735	8.104960
-354.117209	17.807489	8.114957
-352.216464	23.563751	8.124954
-349.962005	13.298231	8.134950
-347.716189	14.960713	8.144947
-346.228519	17.721534	8.154944
-344.388858	20.565104	8.164941
-342.566244	13.718845	8.174938
-340.556746	16.813183	8.184934
-338.697512	9.743202	8.194931
-336.969214	19.620957	8.204928
-334.921688	22.862378	8.214925
-333.139548	19.908133	8.224922
-331.154121	20.454902	8.234918
-329.156283	23.090088	8.244915
-327.653406	10.494190	8.254912
-325.622698	21.046794	8.264909
-323.596874	21.879208	8.274906
-321.976201	24.667759	8.284902
-320.048037	28.842403	8.294899
-318.240755	24.897373	8.304896
-315.986756	24.810794	8.314893
-314.240218	27.137182	8.324890
-312.648593	26.283234	8.334886
-310.717043	23.087273	8.344883
-308.767206	30.247230	8.354880
-306.782860	25.642404	8.364877
-304.769245	24.569532	8.374874
-302.778452	17.647510	8.384870
-301.209513	20.717474	8.394867
-299.692086	22.136290	8.404864
-297.764718	20.663533	8.414861
-295.622351	22.209955	8.424858
-293.803674	17.462648	8.434854
-291.618294	23.857171	8.444851
-289.909738	20.445783	8.454848
-287.987939	26.403991	8.464845
-286.144629	21.299094	8.474842
-284.345198	22.606597	8.484838
-282.327213	19.122143	8.494835
-280.517775	22.523186	8.504832
-278.819278	18.625546	8.514829
-276.545666	22.988231	8.524826
-274.931665	20.831342	8.534822
-273.273693	22.013020	8.544819
-271.460236	17.062890	8.554816
-269.455445	15.470436	8.564813
-267.177634	19.854563	8.574810
-265.714664	25.868655	8.584807
-263.799014	22.059516	8.594803
-261.511259	22.569142	8.604800
-259.633764	22.678489	8.614797
-258.269902	17.026488	8.624794
-256.273790	23.986483	8.634791
-254.244773	19.174056	8.644787
-252.408190	18.852596	8.654784
-250.592668	21.032240	8.664781
-248.711032	22.470326	8.674778
-246.584683	20.069064	8.684775
-244.682808	11.789258	8.694771
-242.803415	11.847791	8.704768
-241.418581	13.954080	8.714765
-239.247906	12.066772	8.724762
-237.310557	11.560305	8.734759
-235.520520	8.495929	8.744755
-233.590593	13.183487	8.754752
-231.842953	11.846826	8.764749
-229.850385	6.386595	8.774746
-227.988391	15.949435	8.784743
-226.240368	3.101324	8.794739
-223.877111	5.586708	8.804736
-222.731940	12.751997	8.814733
-220.835432	9.451180	8.824730
-218.713769	11.160439	8.834727
-216.769499	6.770491	8.844723
-215.073273	17.397102	8.854720
-212.906105	14.127304	8.864717
-211.089154	11.298635	8.874714
-209.467105	11.685613	8.884711
-207.361866	14.013254	8.894707
-205.372996	12.270245	8.904704
-203.767929	12.718353	8.914701
-201.645303	17.073628	8.924698
-200.044001	20.841085	8.934695
-198.051149	15.690285	8.944691
-196.157960	21.648399	8.954688
-194.342068	22.007612	8.964685
-192.217764	15.462239	8.974682
-190.661762	22.978810	8.984679
-188.586824	12.753120	8.994675
-186.690981	23.493160	9.004672
-184.983204	18.444697	9.014669
-183.182262	17.137458	9.024666
-181.101621	18.095448	9.034663
-178.686004	19.839938	9.044659
-177.472319	13.427253	9.054656
-175.739545	18.571031	9.064653
-173.720550	14.890726	9.074650
-171.672050	18.119505	9.084647
-169.841484	6.586067	9.094643
-167.917818	16.104384	9.104640
-166.115328	17.722523	9.114637
-164.413021	14.004341	9.124634
-162.390776	11.804489	9.134631
-160.499770	14.491600	9.144627
-158.320696	17.892176	9.154624
-156.897457	9.838793	9.164621
-155.155875	11.877159	9.174618
-153.072371	17.771786	9.184615
-151.030220	16.378718	9.194611
-149.178290	18.350538	9.204608
-147.418797	30.247568	9.214605
-145.280055	28.775938	9.224602
-143.496021	21.991226	9.234599
-141.764551	21.201913	9.244595
-139.922677	18.961388	9.254592
-138.250643	28.470945	9.264589
-136.136739	24.333445	9.274586
-134.096402	17.493639	9.284583
-132.453237	19.276162	9.294579
-130.226457	17.428942	9.304576
-128.853252	20.553936	9.314573
-126.813255	13.174224	9.324570
-124.829867	24.061395	9.334567
-122.970425	17.673590	9.344563
-121.484895	21.454838	9.354560
-119.206286	15.060157	9.364557
-116.828052	11.317847	9.374554
-115.629440	16.332169	9.384551
-113.679686	9.652088	9.394547
-111.599255	17.525545	9.404544
-109.814634	17.919809	9.414541
-108.192128	19.530393	9.424538
-105.963802	22.111631	9.434535
-104.341820	20.902469	9.444531
-102.264103	17.146540	9.454528
-100.464970	16.630655	9.464525
-98.518859	21.955183	9.474522
-96.781220	23.781078	9.484519
-94.691882	19.799103	9.494515
-93.145247	19.940837	9.504512
-91.197255	21.352673	9.514509
-88.959824	20.406895	9.524506
-87.160918	14.371386	9.534503
-85.477294	22.093449	9.544499
-83.618944	26.809925	9.554496
-81.659944	22.817175	9.564493
-79.939726	19.434065	9.574490
-78.007009	20.944659	9.584487
-76.218004	19.080488	9.594483
-74.316225	20.859689	9.604480
-72.142117	20.456102	9.614477
-70.302014	18.702197	9.624474
-68.462356	22.576979	9.634471
-66.654679	17.195307	9.644467
-64.819884	19.915146	9.654464
-62.813238	24.031700	9.664461
-61.477251	31.785560	9.674458
-59.349849	28.741694	9.684455
-56.909097	25.322602	9.694451
-55.325484	20.500859	9.704448
-53.718642	19.835693	9.714445
-51.796686	18.577136	9.724442
-49.748175	23.470134	9.734439
-48.040818	16.860341	9.744435
-46.042058	22.255459	9.754432
-44.094517	24.188429	9.764429
-42.108736	25.990571	9.774426
-40.373871	20.868410	9.784423
-38.729740	20.519392	9.794419
-36.752714	20.960383	9.804416
-34.767494	21.322705	9.814413
-32.873233	18.200796	9.824410
-30.972045	18.145497	9.834407
-29.044843	21.736362	9.844403
-27.561527	21.891396	9.854400
-25.342905	11.764481	9.864397
-23.552375	16.056056	9.874394
-21.619615	15.078415	9.884391
-19.656243	13.244890	9.894387
-18.141206	7.292600	9.904384
-15.753881	22.067313	9.914381
-14.171991	16.922206	9.924378
-12.608363	17.347053	9.934375
-10.133617	26.438169	9.944371
-8.321545	25.452947	9.954368
-6.743302	22.280414	9.964365
-4.762186	16.028013	9.974362
-3.398635	23.490158	9.984359
-2.078421	54.837859	9.994355
-1.055314	108.537621	10.004352
0.000000	153.725497	10.009357
0.776428	187.108235	10.014362
1.235327	221.514616	10.019367
1.659480	253.315338	10.024371
2.601641	279.948123	10.029376
2.606695	294.757273	10.034381
2.755031	301.211419	10.039386
3.068856	322.141630	10.044391
3.370678	345.298751	10.049395
3.280947	337.960152	10.054400
3.176286	350.787386	10.059405
3.487027	350.606983	10.064410
3.253223	340.544450	10.069415
3.406073	364.715637	10.074419
4.104716	371.099390	10.079424
4.010649	385.063468	10.084429
4.165051	392.150592	10.089434
3.668776	375.798739	10.094439
3.725001	391.661063	10.099443
3.744211	392.389708	10.104448
4.130952	388.797438	10.109453
4.079619	395.724998	10.114458
4.252017	402.558533	10.119463
4.380699	399.500982	10.124467
4.678039	399.985004	10.129472
4.672912	403.207421	10.134477
4.498223	406.713914	10.139482
4.785029	402.284489	10.144487
3.999328	398.379343	10.149491
4.344147	395.684692	10.154496
4.469740	413.270541	10.159501
4.437410	411.050760	10.164506
4.616585	414.984918	10.169511
4.657927	414.104772	10.174515
4.611881	420.388134	10.179520
4.562426	425.695954	10.184525
4.631783	424.117511	10.189530
4.596338	427.846217	10.194535
4.734659	424.918004	10.199539
4.571819	415.384971	10.204544
4.614544	432.055277	10.209549
4.837306	433.800086	10.214554
5.256596	444.746192	10.219559
5.127975	466.860459	10.224563
5.111385	448.158149	10.229568
5.044298	459.307991	10.234573
5.277820	476.674862	10.239578
5.210732	476.773906	10.244583
5.208881	475.033358	10.249587
5.607414	465.860168	10.254592
5.477191	476.893942	10.259597
5.458700	475.807302	10.264602
5.359420	480.479719	10.269607
5.575307	490.185754	10.274611
5.478791	472.249914	10.279616
5.183227	480.856428	10.284621
5.380955	486.151653	10.289626
5.458388	480.932462	10.294631
5.390505	494.515594	10.299635
5.722251	482.164579	10.304640
5.473393	478.941731	10.309645
5.594581	497.062949	10.314650
5.940387	510.070780	10.319655
5.626793	518.979802	10.324659
6.328087	522.592604	10.329664
6.047764	525.292836	10.334669
6.018849	520.353934	10.339674
6.000061	529.540782	10.344679
5.868759	532.385976	10.349683
6.571638	529.914880	10.354688
6.187689	533.681851	10.359693
6.030827	534.733465	10.364698
6.126057	530.791854	10.369703
5.971243	526.284599	10.374707
6.195153	523.836282	10.379712
6.415164	550.627323	10.384717
6.638054	552.181321	10.389722
6.923836	552.993610	10.394727
6.609427	552.083466	10.399731
6.806882	541.832165	10.404736
6.471025	536.581104	10.409741
6.629600	553.313495	10.414746
6.927339	559.340244	10.419751
6.801506	567.404094	10.424755
7.128234	558.978708	10.429760
7.357344	570.756306	10.434765
7.134667	554.874680	10.439770
6.998535	538.022095	10.444775
6.964198	538.842863	10.449779
6.800346	539.431985	10.454784
7.156688	554.899706	10.459789
7.121917	569.882640	10.464794
7.137757	573.262594	10.469799
7.176266	568.082695	10.474803
7.468533	577.489612	10.479808
7.586403	580.995216	10.484813
7.402805	575.893314	10.489818
7.634191	573.172571	10.494823
7.529125	580.468322	10.499827
7.378449	593.019267	10.504832
7.441974	583.088910	10.509837
7.255494	587.265931	10.514842
7.418767	587.058585	10.519847
7.547229	586.793716	10.524851
7.811252	592.337018	10.529856
7.411454	590.641003	10.534861
7.662568	591.182866	10.539866
8.033889	582.731432	10.544871
7.729102	597.934072	10.549875
7.760515	608.417060	10.554880
7.901052	619.328913	10.559885
8.292135	627.595772	10.564890
8.427708	631.294100	10.569895
8.014099	630.874420	10.574899
8.269808	617.089399	10.579904
7.909022	628.729323	10.584909
7.902892	628.560034	10.589914
8.406234	622.683101	10.594919
8.129964	633.972093	10.599923
8.535891	632.027721	10.604928
8.522700	626.594281	10.609933
8.476567	625.639767	10.614938
8.458672	621.192643	10.619943
8.231581	623.047068	10.624947
8.423730	640.485388	10.629952
8.428398	630.094468	10.634957
8.412608	655.612906	10.639962
9.019775	656.970013	10.644967
8.908863	659.614866	10.649971
8.944558	661.154579	10.654976
8.886961	655.466444	10.659981
9.206298	668.070221	10.664986
8.932991	657.676309	10.669991
8.609297	665.913692	10.674995
9.207445	661.291034	10.680000
9.346689	663.112267	10.685005
9.254398	662.102036	10.690010
9.511363	655.012323	10.695015
9.535515	658.078745	10.700019
9.087692	643.185381	10.705024
9.242051	646.663105	10.710029
9.710106	668.472787	10.715034
9.259574	651.544061	10.720039
9.241814	670.223804	10.725043
9.580494	662.116565	10.730048
9.505407	668.193361	10.735053
9.770625	659.651575	10.740058
9.807062	669.889385	10.745063
9.604091	670.804864	10.750067
9.606766	672.029733	10.755072
9.756872	667.218342	10.760077
9.733154	675.278581	10.765082
9.883565	665.093042	10.770087
9.855662	674.581048	10.775091
9.748056	668.531888	10.780096
9.725285	677.613813	10.785101
9.639629	670.233395	10.790106
9.861094	676.411126	10.795111
9.925682	678.378305	10.800115
10.203209	672.062720	10.805120
10.133945	688.964067	10.810125
10.338586	694.846453	10.815130
10.167762	693.714708	10.820135
9.821898	702.384567	10.825139
10.422168	700.694612	10.830144
10.358790	704.992378	10.835149
10.393730	703.993390	10.840154
10.492933	701.404089	10.845159
10.304587	702.260468	10.850163
10.610767	704.107120	10.855168
10.474435	712.109649	10.860173
10.710413	704.897106	10.865178
10.746688	696.962654	10.870183
10.310141	703.043499	10.875187
10.766722	709.089131	10.880192
11.311234	721.895156	10.885197
10.736393	709.112968	10.890202
11.010516	705.502314	10.895207
10.853176	708.496770	10.900211
11.130091	715.391053	10.905216
11.340110	726.635673	10.910221
11.111587	715.916039	10.915226
11.220003	705.508518	10.920231
11.099820	725.882503	10.925235
11.547708	732.823640	10.930240
11.883588	714.233501	10.935245
11.250043	705.664726	10.940250
11.502185	696.065321	10.945255
11.392577	699.186200	10.950259
11.687888	692.945038	10.955264
11.304196	698.754107	10.960269
11.172653	695.816843	10.965274
11.699678	713.017342	10.970279
11.614527	730.657689	10.975283
11.771415	736.448364	10.980288
11.680567	735.704396	10.985293
11.531050	730.529197	10.990298
11.809401	734.021858	10.995303
11.668659	738.880739	11.000307
12.174568	737.732519	11.005312
12.107569	720.501273	11.010317
11.869901	728.546781	11.015322
12.090706	729.591789	11.020327
12.038306	736.902872	11.025331
11.949488	740.449364	11.030336
12.109348	730.686463	11.035341
11.940917	743.117371	11.040346
12.364907	740.837376	11.045351
12.191529	742.344212	11.050355
12.246132	739.795133	11.055360
12.135711	741.690887	11.060365
12.534136	744.994094	11.065370
12.574648	757.655035	11.070375
12.462120	768.883324	11.075379
12.440676	766.130331	11.080384
12.886747	761.096667	11.085389
12.765881	762.855322	11.090394
12.850430	767.736627	11.095399
13.021867	764.992294	11.100403
12.896071	758.256885	11.105408
12.817819	737.198661	11.110413
12.915404	740.748539	11.115418
12.900319	738.183767	11.120423
13.010684	756.751727	11.125427
12.956596	760.480338	11.130432
13.253430	760.532380	11.135437
12.762742	768.815379	11.140442
12.945920	769.158355	11.145447
13.113720	769.469091	11.150451
13.215150	770.876909	11.155456
12.956553	771.336074	11.160461
12.954110	779.088633	11.165466
13.507610	768.466581	11.170471
13.059612	773.464362	11.175475
13.338053	764.545099	11.180480
13.115582	774.122549	11.185485
13.231154	786.030392	11.190490
13.990185	793.095396	11.195495
13.783388	798.568792	11.200499
14.080133	790.163825	11.205504
13.996773	784.211672	11.210509
13.252593	777.480264	11.215514
13.636041	777.691953	11.220519
13.453694	791.556964	11.225523
13.646416	808.139128	11.230528
14.035916	802.868473	11.235533
14.033188	806.139482	11.240538
14.156060	805.760386	11.245543
14.359271	801.539711	11.250547
14.594544	804.001646	11.255552
14.496977	795.014604	11.260557
14.543380	806.119805	11.265562
14.332737	771.984740	11.270567
14.328454	776.383486	11.275571
14.382000	760.702001	11.280576
14.345970	770.224481	11.285581
14.654299	771.283918	11.290586
14.695335	767.190041	11.295591
14.489985	765.557606	11.300595
14.301036	758.723461	11.305600
14.494529	777.823803	11.310605
14.327958	794.799139	11.315610
14.893509	791.714406	11.320615
14.396127	795.395458	11.325619
14.469266	802.830052	11.330624
14.961072	802.190269	11.335629
14.716794	799.368732	11.340634
14.945759	797.879909	11.345639
14.667802	805.564462	11.350643
14.664942	800.439963	11.355648
14.890884	796.163626	11.360653
14.847730	800.514964	11.365658
15.106432	795.722480	11.370663
15.337126	824.772054	11.375667
15.338615	816.742161	11.380672
15.162660	812.321764	11.385677
15.207575	810.945871	11.390682
15.611870	812.735889	11.395687
15.347453	824.463099	11.400691
15.329697	817.347738	11.405696
15.791622	822.692413	11.410701
15.530807	827.732897	11.415706
15.844984	806.427484	11.420711
15.515929	810.483808	11.425715
15.749692	806.639874	11.430720
15.621931	794.279882	11.435725
15.677541	812.312609	11.440730
15.884931	809.132034	11.445735
15.831015	831.017327	11.450739
15.812275	820.481773	11.455744
16.134294	826.591493	11.460749
15.738350	825.158180	11.465754
15.911556	822.195939	11.470759
15.962698	827.350669	11.475763
16.328881	834.085696	11.480768
16.065701	824.287701	11.485773
15.835986	836.238040	11.490778
16.138755	830.990670	11.495783
15.897289	833.728914	11.500787
15.973303	841.721301	11.505792
16.172421	835.112228	11.510797
15.977257	837.690127	11.515802
16.521685	845.745002	11.520807
16.763881	852.458811	11.525811
16.831504	844.921396	11.530816
16.619146	831.799016	11.535821
16.825475	821.632834	11.540826
16.721039	823.051414	11.545831
16.365240	829.556240	11.550835
16.397869	832.059961	11.555840
16.827326	844.851331	11.560845
16.801415	862.373583	11.565850
17.049062	854.687604	11.570855
17.117072	863.756744	11.575859
17.100512	858.514562	11.580864
17.230011	853.009394	11.585869
17.534472	852.572951	11.590874
17.130411	826.589780	11.595879
17.114770	819.955041	11.600883
16.938047	819.150650	11.605888
17.232410	827.873013	11.610893
17.415457	852.983203	11.615898
17.624398	836.406388	11.620903
17.192927	838.444821	11.625907
17.289115	852.711737	11.630912
17.514249	863.175052	11.635917
17.143471	855.532511	11.640922
17.674480	855.682822	11.645927
17.428681	851.473822	11.650931
17.587868	861.160766	11.655936
17.446671	860.560438	11.660941
17.508742	858.979957	11.665946
17.337626	857.047166	11.670951
17.166270	859.162385	11.675955
17.520862	860.134027	11.680960
17.666227	866.202554	11.685965
18.049976	875.803232	11.690970
18.153135	875.824664	11.695975
18.065432	889.956945	11.700979
18.171548	879.358857	11.705984
18.658402	865.368005	11.710989
18.530908	871.019589	11.715994
18.299203	860.189969	11.720999
18.256284	843.307968	11.726003
18.445990	859.559518	11.731008
18.269137	845.442730	11.736013
18.082955	856.510948	11.741018
18.481396	849.993079	11.746023
18.225552	854.860894	11.751027
18.517702	875.536751	11.756032
19.046823	871.186808	11.761037
18.555752	860.370169	11.766042
18.669131	855.960383	11.771047
18.496312	855.377713	11.776051
18.807139	876.000130	11.781056
18.981279	869.172678	11.786061
18.429589	890.030445	11.791066
18.814814	877.749413	11.796071
18.905460	877.082146	11.801075
18.607970	886.105516	11.806080
18.882895	877.620401	11.811085
18.809602	872.374647	11.816090
19.083271	874.388931	11.821095
18.746195	886.900475	11.826099
18.945268	879.137075	11.831104
19.017089	872.608210	11.836109
18.707764	886.053600	11.841114
19.099974	892.663080	11.846119
19.274260	900.352825	11.851123
19.633480	906.600148	11.856128
19.596694	907.441828	11.861133
19.597910	907.192517	11.866138
19.642233	905.488707	11.871143
19.443850	910.481416	11.876147
19.537624	912.443973	11.881152
19.693795	898.460097	11.886157
19.611143	912.306170	11.891162
19.979475	903.520718	11.896167
20.065187	907.875190	11.901171
19.680776	913.509419	11.906176
20.117436	904.351951	11.911181
20.485150	908.786025	11.916186
20.104460	895.272547	11.921191
19.827080	879.960673	11.926195
20.083560	879.777883	11.931200
20.234743	893.000026	11.936205
19.947173	898.040070	11.941210
20.396900	897.329726	11.946215
20.225631	904.219887	11.951219
20.022830	903.624651	11.956224
20.411431	900.971813	11.961229
20.157094	915.832430	11.966234
20.517259	910.828187	11.971239
20.295119	902.691989	11.976243
20.519647	906.713665	11.981248
20.451974	896.635285	11.986253
20.177418	908.972876	11.991258
20.220070	897.519160	11.996263
20.521531	900.410520	12.001267
20.125118	907.035397	12.006272
20.622345	906.811057	12.011277
20.797811	921.311399	12.016282
20.942093	929.026445	12.021287
20.715925	898.749162	12.026291
20.622392	900.834630	12.031296
20.741604	896.185784	12.036301
20.618399	906.389299	12.041306
20.972768	917.536931	12.046311
20.765490	911.442064	12.051315
20.640586	904.570827	12.056320
20.507860	907.096202	12.061325
20.726346	911.675501	12.066330
21.167398	906.921707	12.071335
20.716201	904.446959	12.076339
20.920338	903.750552	12.081344
21.430382	892.707993	12.086349
20.917483	901.440879	12.091354
21.063588	907.622845	12.096359
20.855769	892.523788	12.101363
21.020222	889.326391	12.106368
20.980854	892.850841	12.111373
20.924780	897.126999	12.116378
21.044600	889.100271	12.121383
20.684875	888.028598	12.126387
20.479421	881.627528	12.131392
20.639426	882.712207	12.136397
20.955224	893.355047	12.141402
20.984895	885.606046	12.146407
20.396389	882.410467	12.151411
20.653343	891.334375	12.156416
20.968453	899.335969	12.161421
20.704398	899.445929	12.166426
20.907117	886.162684	12.171431
20.662473	877.738357	12.176435
20.469659	882.886284	12.181440
20.541439	883.789494	12.186445
20.420954	907.063756	12.191450
20.911030	898.027082	12.196455
20.767210	905.080022	12.201459
20.608374	914.008756	12.206464
20.700765	905.787700	12.211469
20.686534	912.979246	12.216474
21.217806	901.699908	12.221479
20.992230	911.049287	12.226483
20.727086	909.125177	12.231488
20.959645	883.786258	12.236493
20.708634	887.464308	12.241498
20.620621	876.275873	12.246503
20.827922	878.154088	12.251507
20.678812	883.399123	12.256512
20.754733	874.343361	12.261517
20.624138	876.095696	12.266522
20.562790	868.714453	12.271527
20.715198	881.310349	12.276531
20.625088	896.630449	12.281536
20.958436	904.014134	12.286541
20.853796	906.965533	12.291546
20.719845	897.837574	12.296551
20.691435	882.303066	12.301555
20.680706	879.277111	12.306560
20.710780	873.373060	12.311565
20.499775	901.171768	12.316570
21.014056	899.670547	12.321575
20.615210	901.383667	12.326579
20.663213	911.294956	12.331584
20.962004	902.268286	12.336589
20.903696	900.106189	12.341594
20.901579	885.258181	12.346599
20.512604	887.980538	12.351603
20.553225	886.972747	12.356608
20.813441	897.096182	12.361613
20.827916	900.090082	12.366618
20.984376	886.897791	12.371623
20.543859	896.488020	12.376627
20.843017	891.816784	12.381632
20.681532	882.653802	12.386637
20.693282	888.549687	12.391642
20.924036	879.453459	12.396647
20.827721	883.299221	12.401651
20.798036	888.116786	12.406656
20.946267	887.393026	12.411661
20.442316	891.168187	12.416666
20.498387	888.856964	12.421671
20.719463	890.740869	12.426675
20.681809	889.212559	12.431680
20.814125	879.444489	12.436685
20.784578	898.790296	12.441690
20.783734	890.610926	12.446695
21.048042	892.077933	12.451699
20.493902	892.073311	12.456704
20.885699	884.580366	12.461709
20.610103	892.352896	12.466714
21.041689	888.431660	12.471719
20.807658	897.083798	12.476723
20.645506	895.070725	12.481728
20.914671	890.407427	12.486733
20.903028	905.957870	12.491738
20.808893	899.132189	12.496743
21.152496	889.751456	12.501747
20.899574	895.096628	12.506752
21.280382	895.658821	12.511757
21.109879	905.070375	12.516762
21.105766	892.020382	12.521767
20.997522	873.414139	12.526771
20.658533	867.941107	12.531776
20.789267	866.710791	12.536781
20.549618	883.876079	12.541786
20.628600	861.586245	12.546791
20.541645	872.127726	12.551795
20.595701	867.956051	12.556800
21.148469	869.544205	12.561805
20.799467	873.100687	12.566810
20.452045	866.897305	12.571815
20.584759	868.806338	12.576819
20.387571	871.986952	12.581824
20.770098	879.766475	12.586829
21.102274	898.751822	12.591834
20.989186	881.344810	12.596839
20.921454	873.811620	12.601843
20.713335	873.904774	12.606848
21.196371	860.799192	12.611853
20.676643	863.916129	12.616858
20.881876	873.840163	12.621863
20.776532	868.033404	12.626867
20.957568	871.639391	12.631872
20.733845	868.357252	12.636877
20.414806	868.270980	12.641882
20.374898	865.244951	12.646887
20.563050	874.033166	12.651891
20.408658	871.315549	12.656896
20.636832	874.724787	12.661901
20.515363	876.157126	12.666906
20.799159	883.709551	12.671911
21.019189	894.547435	12.676915
20.739205	902.826866	12.681920
20.805170	879.384766	12.686925
20.558193	868.355729	12.691930
20.767360	873.546773	12.696935
20.909733	879.242051	12.701939
20.693364	882.010994	12.706944
20.830922	867.985962	12.711949
20.607044	882.130492	12.716954
20.691581	871.073811	12.721959
20.540599	876.699182	12.726963
20.845792	903.407909	12.731968
21.125602	886.300924	12.736973
20.848161	880.903224	12.741978
20.791722	874.680239	12.746983
21.102365	868.572173	12.751987
20.934714	872.435617	12.756992
21.017887	878.181336	12.761997
20.948715	881.426690	12.767002
20.946696	883.623714	12.772007
20.950280	873.647524	12.777011
20.852868	876.698687	12.782016
21.060198	883.446458	12.787021
20.838997	880.026721	12.792026
20.721412	866.979079	12.797031
20.594927	863.731895	12.802035
20.643731	865.061385	12.807040
21.088104	867.554637	12.812045
20.858220	869.923616	12.817050
20.469103	844.616107	12.822055
20.559444	846.869357	12.827059
20.960581	869.434328	12.832064
20.758349	874.115406	12.837069
20.512323	864.101763	12.842074
21.070209	862.845899	12.847079
20.813220	852.248972	12.852083
20.674355	843.199101	12.857088
20.674233	832.696837	12.862093
20.579747	859.560689	12.867098
20.802671	864.784228	12.872103
20.812138	870.454968	12.877107
20.654204	869.420499	12.882112
20.681899	854.840577	12.887117
20.626053	872.280884	12.892122
20.891523	867.074142	12.897127
20.671222	867.203931	12.902131
20.772880	883.012242	12.907136
20.942977	873.717537	12.912141
20.630274	865.258340	12.917146
20.415506	861.918006	12.922151
20.507839	856.240572	12.927155
20.806058	876.325692	12.932160
21.087230	874.345995	12.937165
20.848783	884.776030	12.942170
20.780258	872.305599	12.947175
20.735616	854.348394	12.952179
20.654660	861.938480	12.957184
21.063284	853.512479	12.962189
20.818511	855.106406	12.967194
20.783770	860.218076	12.972199
21.149251	838.563817	12.977203
20.627898	869.933236	12.982208
20.626791	844.959653	12.987213
20.512924	863.118820	12.992218
20.765907	841.219152	12.997223
20.668070	842.458488	13.002227
20.480529	856.810084	13.007232
20.810576	847.090923	13.012237
20.563033	851.656220	13.017242
20.425978	857.055438	13.022247
21.132850	868.302929	13.027251
20.754067	860.492930	13.032256
20.782197	862.447027	13.037261
20.553628	857.912006	13.042266
20.653023	868.551494	13.047271
21.108981	879.280778	13.052275
20.625505	871.679856	13.057280
20.797631	859.312979	13.062285
20.705449	851.983970	13.067290
20.508503	859.709246	13.072295
20.807040	857.206396	13.077299
20.748822	864.731357	13.082304
20.755463	859.947514	13.087309
20.602051	861.886410	13.092314
20.641415	873.834866	13.097319
21.022133	868.392127	13.102323
20.626350	870.375986	13.107328
20.690346	870.793166	13.112333
20.829040	877.151340	13.117338
20.857085	876.777904	13.122343
20.873756	867.849866	13.127347
20.627946	855.051339	13.132352
20.865261	849.524247	13.137357
20.707928	853.718772	13.142362
20.669886	852.778722	13.147367
20.893284	857.284681	13.152371
20.703742	862.386348	13.157376
20.936192	856.861606	13.162381
21.036032	860.687117	13.167386
20.639432	852.857887	13.172391
20.874458	849.568819	13.177395
20.992928	862.009265	13.182400
20.976868	863.375907	13.187405
20.718475	865.959164	13.192410
20.669680	851.837714	13.197415
20.804564	854.143785	13.202419
20.570353	863.070317	13.207424
20.564956	861.789174	13.212429
20.893850	868.552242	13.217434
20.837696	849.617606	13.222439
20.676313	855.036472	13.227443
20.727225	874.049298	13.232448
20.922709	856.992065	13.237453
20.329641	863.165747	13.242458
20.644753	863.793608	13.247463
20.936621	864.027790	13.252467
20.714951	863.776182	13.257472
20.949027	861.926998	13.262477
20.733863	870.238649	13.267482
20.823394	872.492032	13.272487
20.646216	862.544679	13.277491
20.176430	875.957304	13.282496
20.653434	865.848846	13.287501
20.616302	865.985691	13.292506
20.350063	865.722268	13.297511
20.585068	861.236312	13.302515
20.453102	871.206238	13.307520
21.066486	877.964938	13.312525
21.213300	885.529749	13.317530
21.188407	875.718946	13.322535
21.214239	860.278312	13.327539
20.856162	873.900197	13.332544
21.203462	856.462366	13.337549
20.921136	865.833383	13.342554
20.702305	868.648447	13.347559
21.170612	868.036064	13.352563
20.723149	867.271695	13.357568
20.680532	854.842878	13.362573
20.401739	855.179112	13.367578
20.402880	863.640761	13.372583
20.676907	872.484665	13.377587
20.503077	875.887056	13.382592
21.024652	863.333558	13.387597
20.900609	863.753919	13.392602
20.867211	879.110687	13.397607
20.904256	861.416408	13.402611
20.835133	867.042911	13.407616
21.011782	868.698936	13.412621
20.875771	854.096239	13.417626
20.562331	850.437335	13.422631
20.851745	840.882352	13.427635
20.421651	851.871198	13.432640
20.763886	853.158619	13.437645
21.027518	859.332859	13.442650
20.521972	852.016160	13.447655
20.712206	851.508050	13.452659
20.716071	849.703468	13.457664
21.141279	846.849263	13.462669
20.858717	850.439297	13.467674
20.660975	848.316791	13.472679
20.831795	836.700759	13.477683
20.881435	845.359663	13.482688
20.843143	839.885992	13.487693
20.734228	843.175522	13.492698
20.531077	835.741218	13.497703
20.791643	835.508892	13.502707
20.993287	844.730170	13.507712
21.032219	842.598303	13.512717
20.807433	849.523782	13.517722
20.772844	843.350940	13.522727
21.071619	842.945366	13.527731
20.493581	850.906456	13.532736
20.805306	843.158225	13.537741
20.636478	848.805354	13.542746
20.425251	836.414482	13.547751
20.630722	843.522069	13.552755
20.840589	855.020700	13.557760
20.967564	843.522040	13.562765
20.645345	844.568508	13.567770
20.658891	851.427593	13.572775
20.869912	847.669276	13.577779
20.557700	848.289956	13.582784
20.725688	853.244713	13.587789
20.741243	848.462607	13.592794
20.770500	853.620837	13.597799
20.878714	854.582888	13.602803
20.941223	854.796881	13.607808
20.885639	844.822263	13.612813
20.758700	842.262696	13.617818
20.798011	855.521570	13.622823
21.021981	853.021151	13.627827
20.950919	855.445221	13.632832
20.918145	847.750354	13.637837
20.772077	854.526088	13.642842
21.137469	836.691164	13.647847
20.973092	833.137799	13.652851
20.567859	829.791579	13.657856
20.710452	816.734025	13.662861
20.497913	822.295077	13.667866
20.638481	838.093979	13.672871
20.962892	844.282173	13.677875
20.816551	841.646854	13.682880
20.582506	835.584672	13.687885
20.783183	830.306277	13.692890
20.784395	841.115943	13.697895
20.956714	828.455754	13.702899
20.534098	831.800043	13.707904
20.932481	824.151539	13.712909
20.670251	819.040014	13.717914
20.587811	816.599508	13.722919
20.863027	813.819693	13.727923
20.653862	816.726244	13.732928
20.656164	809.919917	13.737933
20.700664	828.823322	13.742938
20.934157	830.314161	13.747943
21.083813	822.519250	13.752947
21.022902	830.440431	13.757952
20.813113	817.098461	13.762957
20.552381	821.998583	13.767962
20.522363	824.865526	13.772967
20.637308	820.540654	13.777971
20.542010	811.792931	13.782976
21.091097	821.412934	13.787981
21.031623	824.700883	13.792986
20.956676	821.959565	13.797991
21.011628	815.203186	13.802995
20.834946	821.698365	13.808000
21.185887	815.933971	13.813005
20.824200	817.835116	13.818010
20.559996	830.451682	13.823015
21.034841	819.932022	13.828019
20.577040	828.692347	13.833024
20.775782	815.293108	13.838029
20.815234	827.109049	13.843034
20.698512	828.718820	13.848039
20.736486	818.213645	13.853043
20.744762	831.829101	13.858048
20.912224	817.931809	13.863053
20.751752	823.197557	13.868058
20.562708	830.002211	13.873063
20.870933	828.786168	13.878067
20.645393	827.029214	13.883072
20.702618	820.513739	13.888077
20.814220	820.026055	13.893082
20.425435	829.828758	13.898087
20.620958	816.395340	13.903091
20.633484	827.255230	13.908096
20.633088	824.536714	13.913101
20.585666	818.160930	13.918106
20.623049	831.883705	13.923111
20.771610	830.658434	13.928115
20.818236	823.009262	13.933120
20.588041	825.849784	13.938125
20.485491	831.774913	13.943130
20.139445	834.540875	13.948135
20.514492	821.722205	13.953139
20.735465	836.043320	13.958144
20.759121	825.127269	13.963149
20.975656	836.347282	13.968154
20.587888	839.695477	13.973159
20.817282	827.748417	13.978163
20.670626	842.782594	13.983168
20.593790	835.536300	13.988173
20.566718	835.166924	13.993178
20.688972	835.732504	13.998183
21.049590	847.235471	14.003187
20.601857	839.513749	14.008192
20.895674	834.785178	14.013210
20.669085	825.696952	14.018227
20.693244	834.779791	14.023245
20.451398	840.235476	14.028263
20.645066	855.840862	14.033280
21.018334	855.329945	14.038298
20.934047	869.488562	14.043315
21.129343	861.805269	14.048333
21.146630	850.677397	14.053351
20.393706	846.555396	14.058368
20.766280	844.646280	14.063386
21.339129	858.991069	14.068403
20.896856	859.445433	14.073421
20.881529	857.311912	14.078439
21.284471	862.062348	14.083456
21.146975	855.172972	14.088474
20.794597	848.039467	14.093491
20.741015	854.871308	14.098509
21.184066	857.646070	14.103527
20.958429	866.713716	14.108544
21.026058	856.480659	14.113562
21.140830	872.811171	14.118579
21.124380	866.254816	14.123597
21.468080	866.448558	14.128615
21.414157	867.673053	14.133632
21.025473	851.851888	14.138650
21.141338	845.702270	14.143667
20.975350	862.384264	14.148685
21.254666	860.913130	14.153703
20.858583	874.676347	14.158720
21.075618	880.601516	14.163738
21.051532	874.590600	14.168755
21.230210	867.587877	14.173773
21.441271	862.966089	14.178791
20.957646	870.954974	14.183808
21.172881	867.358054	14.188826
21.450450	856.284614	14.193843
21.336511	868.823149	14.198861
21.332292	860.883834	14.203879
21.131948	869.599836	14.208896
21.446793	877.991449	14.213914
21.364173	862.676696	14.218931
21.440969	880.200817	14.223949
21.599992	887.055390	14.228967
21.479729	900.601623	14.233984
21.412056	910.410109	14.239002
21.576355	900.696393	14.244019
21.183336	902.467293	14.249037
21.706967	899.519551	14.254055
21.600286	910.859981	14.259072
21.434093	904.579156	14.264090
21.649557	904.310468	14.269107
21.532044	905.115703	14.274125
21.269784	910.876670	14.279143
21.367812	895.006146	14.284160
21.610040	899.508541	14.289178
21.879828	898.999971	14.294195
21.413361	906.712453	14.299213
21.598046	900.407128	14.304231
21.332821	911.884521	14.309248
21.564659	928.454382	14.314266
22.218096	928.494915	14.319283
22.060611	945.765491	14.324301
22.252257	930.141102	14.329319
22.033080	922.067735	14.334336
21.740184	924.024001	14.339354
21.972913	903.721541	14.344371
21.951384	914.659885	14.349389
21.876356	906.214351	14.354407
21.902735	914.384597	14.359424
21.708517	924.842440	14.364442
21.928726	929.634626	14.369459
21.855171	937.331647	14.374477
22.340627	934.657383	14.379495
22.236969	942.642333	14.384512
21.970759	947.035508	14.389530
22.316498	942.919142	14.394547
22.237759	935.196150	14.399565
22.504176	938.574786	14.404583
22.239783	926.739927	14.409600
21.881950	908.266570	14.414618
22.417015	912.497339	14.419635
22.237842	920.981923	14.424653
22.028216	916.811002	14.429671
22.255582	923.009799	14.434688
22.276694	928.137310	14.439706
22.572079	931.720520	14.444723
22.188684	933.603138	14.449741
22.764386	922.810838	14.454759
22.315049	920.486996	14.459776
21.873868	919.281765	14.464794
22.164155	920.789544	14.469811
22.191793	929.502252	14.474829
22.261748	923.094101	14.479847
22.569590	931.077905	14.484864
22.671485	927.723973	14.489882
22.802734	926.440031	14.494899
22.573767	931.973915	14.499917
22.808744	931.541677	14.504935
22.607384	930.770071	14.509952
22.437146	937.965025	14.514970
22.783273	929.587579	14.519987
22.619864	936.235642	14.525005
22.576108	933.079531	14.530023
22.613660	936.570166	14.535040
22.973432	933.242740	14.540058
22.862579	925.180407	14.545075
22.602716	935.878373	14.550093
22.373345	933.450238	14.555111
22.734600	931.550781	14.560128
22.284766	936.103791	14.565146
22.619875	929.722556	14.570163
22.172111	934.814744	14.575181
22.103459	924.057574	14.580199
22.354660	949.264378	14.585216
23.082923	955.981012	14.590234
23.176038	945.105224	14.595251
22.840403	977.515243	14.600269
22.889194	967.653175	14.605287
22.985694	952.874436	14.610304
23.217167	960.201948	14.615322
23.802377	944.810483	14.620339
23.483783	920.775320	14.625357
23.457060	929.784542	14.630375
23.228332	923.930503	14.635392
23.230690	898.675516	14.640410
23.452667	913.041715	14.645427
23.476805	918.483321	14.650445
23.516845	904.731309	14.655463
23.450883	899.697547	14.660480
23.009057	904.362519	14.665498
22.844489	896.841986	14.670515
22.937937	901.386984	14.675533
23.333665	910.953264	14.680551
23.347196	912.866950	14.685568
22.921882	912.113760	14.690586
23.322638	904.262406	14.695603
23.204159	916.328261	14.700621
23.267150	918.023289	14.705639
23.629110	907.710223	14.710656
23.630046	912.782748	14.715674
23.650293	914.321010	14.720691
23.625820	911.345859	14.725709
23.598561	913.816569	14.730727
23.464153	915.719245	14.735744
23.466728	901.160017	14.740762
23.782113	900.167583	14.745779
23.433026	891.710714	14.750797
23.484236	892.882267	14.755815
23.645071	896.994977	14.760832
23.210562	906.498625	14.765850
23.446234	909.913614	14.770867
23.416288	916.457019	14.775885
23.417130	911.873461	14.780903
23.349280	893.775413	14.785920
23.490502	909.230357	14.790938
23.662200	916.484016	14.795955
23.551046	905.200421	14.800973
23.709010	903.865033	14.805991
23.921616	904.257422	14.811008
23.716051	911.078925	14.816026
23.700323	900.978672	14.821043
23.755870	923.751888	14.826061
23.589328	910.646253	14.831079
23.541120	905.659991	14.836096
23.617809	933.148580	14.841114
24.047953	923.645689	14.846131
23.897797	939.607999	14.851149
23.933214	952.459390	14.856167
24.498768	937.456433	14.861184
23.996263	928.711000	14.866202
23.887131	909.464999	14.871219
23.783798	926.753655	14.876237
23.918565	929.942515	14.881255
24.387217	933.141041	14.886272
24.189540	937.809554	14.891290
24.357533	928.628448	14.896307
23.933066	925.363182	14.901325
24.057126	937.423404	14.906343
24.514018	931.494620	14.911360
24.185650	934.513542	14.916378
24.020826	917.579157	14.921395
24.375169	928.608565	14.926413
24.178842	932.455800	14.931431
24.256015	944.512496	14.936448
24.071278	947.948929	14.941466
24.323329	937.574725	14.946483
24.485516	942.091472	14.951501
24.496637	940.307626	14.956519
24.592557	936.209083	14.961536
24.343288	933.301238	14.966554
24.185144	949.116979	14.971571
24.663720	940.955913	14.976589
24.751841	937.649790	14.981607
24.790979	927.715361	14.986624
24.582328	920.835729	14.991642
24.233951	903.949508	14.996659
24.689760	913.136574	15.001677
24.369010	935.236846	15.006695
24.529483	941.125446	15.011712
24.214709	946.822448	15.016730
24.505123	939.569078	15.021747
24.553508	931.547408	15.026765
24.384023	936.373434	15.031783
24.599703	937.010709	15.036800
24.512620	941.927407	15.041818
24.431451	940.334446	15.046835
24.718034	933.987689	15.051853
24.584939	930.224526	15.056871
25.032973	929.143300	15.061888
24.903265	937.396651	15.066906
24.833061	944.913830	15.071923
25.023690	934.510102	15.076941
25.011932	933.093248	15.081959
25.060494	934.603403	15.086976
24.963460	941.122913	15.091994
25.302193	939.058746	15.097011
25.069386	932.030388	15.102029
25.028978	939.723697	15.107047
25.334954	926.045648	15.112064
25.459947	928.120871	15.117082
25.127543	934.802177	15.122099
25.420428	932.383552	15.127117
25.072413	935.770524	15.132135
25.350383	922.877109	15.137152
25.372813	937.031355	15.142170
25.252662	936.929442	15.147187
25.335729	931.481819	15.152205
25.089845	939.366762	15.157223
24.892764	934.555233	15.162240
24.922336	941.564176	15.167258
24.945111	945.396919	15.172275
25.121034	934.001454	15.177293
24.956124	939.243574	15.182311
25.345603	935.013276	15.187328
25.162983	940.140252	15.192346
25.360671	936.190635	15.197363
25.507930	947.402511	15.202381
25.452178	966.096104	15.207399
25.464097	958.202922	15.212416
25.461089	964.351968	15.217434
25.480901	971.450566	15.222451
25.724092	965.930205	15.227469
25.506945	971.921510	15.232487
25.947610	973.436770	15.237504
25.465045	958.969013	15.242522
25.429062	969.757131	15.247539
26.080951	952.572909	15.252557
25.477536	961.968260	15.257575
25.742106	957.128710	15.262592
25.645176	951.241057	15.267610
25.523830	959.073119	15.272627
25.876688	967.458723	15.277645
25.753384	973.357990	15.282663
25.679417	969.424949	15.287680
25.978109	969.235789	15.292698
25.948529	965.423076	15.297715
26.120286	959.116642	15.302733
26.053927	966.930500	15.307751
25.984055	969.043099	15.312768
26.014795	969.382704	15.317786
25.850181	975.400237	15.322803
25.821648	971.225585	15.327821
25.732793	962.901764	15.332839
25.941327	960.896108	15.337856
25.730046	972.698404	15.342874
25.697351	982.180486	15.347891
25.956200	970.085975	15.352909
25.825286	976.489791	15.357927
25.798457	977.083952	15.362944
26.281142	976.181228	15.367962
26.207307	983.072985	15.372979
26.015202	982.969964	15.377997
26.103668	990.166152	15.383015
26.284890	986.669003	15.388032
26.391379	994.732143	15.393050
26.458299	986.801862	15.398067
26.936883	985.992594	15.403085
26.428279	980.348324	15.408103
26.430427	971.335203	15.413120
26.329064	963.589064	15.418138
26.449713	961.223070	15.423155
26.542061	952.738231	15.428173
26.358512	964.169608	15.433191
26.440306	956.977814	15.438208
26.745233	958.366867	15.443226
26.557766	967.159519	15.448243
26.383053	951.728806	15.453261
26.344449	964.038346	15.458279
26.299648	975.936781	15.463296
26.423275	980.083763	15.468314
26.740763	982.041783	15.473331
26.676723	981.441743	15.478349
26.532892	984.141827	15.483367
27.058823	981.417058	15.488384
26.992094	983.666002	15.493402
26.718654	989.200709	15.498419
27.053754	979.173429	15.503437
27.174466	986.512327	15.508455
27.000735	987.966710	15.513472
27.218777	970.332597	15.518490
26.829550	976.131140	15.523507
26.786785	956.770679	15.528525
27.116121	962.827398	15.533543
26.870953	956.148614	15.538560
27.126175	959.352874	15.543578
26.495687	960.762131	15.548595
27.283058	982.077028	15.553613
27.058995	986.293618	15.558631
26.928638	986.953052	15.563648
27.319679	981.589991	15.568666
27.273513	996.782352	15.573683
27.425874	1002.716312	15.578701
26.929670	1000.330721	15.583719
27.111043	983.131848	15.588736
27.384886	992.423486	15.593754
26.959151	1004.536843	15.598771
27.231863	989.816474	15.603789
27.304293	985.787727	15.608807
27.103084	1000.701245	15.613824
27.166137	988.829842	15.618842
27.531263	984.760706	15.623859
27.599652	992.979349	15.628877
27.435186	992.643846	15.633895
27.562835	985.798632	15.638912
27.400817	990.329349	15.643930
27.355275	984.976144	15.648947
27.549740	985.915659	15.653965
27.540910	984.962344	15.658983
27.560851	969.815151	15.664000
27.559246	986.087280	15.669018
27.379177	987.344486	15.674035
27.539886	984.306755	15.679053
27.389602	993.107649	15.684071
27.519610	982.686814	15.689088
27.526653	988.307340	15.694106
27.557893	995.238971	15.699123
28.005274	1003.738501	15.704141
28.039232	1006.551797	15.709159
27.696628	998.054508	15.714176
28.076913	989.393173	15.719194
27.919273	984.839587	15.724211
27.907409	986.032217	15.729229
27.866982	988.854227	15.734247
27.611618	996.396245	15.739264
27.944646	1004.212490	15.744282
27.826798	1015.315699	15.749299
28.269752	1008.473667	15.754317
28.495097	1022.650688	15.759335
27.870351	1006.775771	15.764352
28.299567	998.699619	15.769370
28.067222	1003.213244	15.774387
28.323501	1006.044563	15.779405
28.100277	996.737056	15.784423
27.798850	993.224077	15.789440
28.514858	997.729589	15.794458
28.081882	1014.683985	15.799475
28.161822	1012.752310	15.804493
28.454622	1005.574028	15.809511
28.426328	1020.636157	15.814528
28.679501	1009.799283	15.819546
28.391865	1017.237927	15.824563
28.543740	1004.311070	15.829581
28.443929	990.535666	15.834599
28.464266	990.713347	15.839616
28.817633	981.189632	15.844634
28.123888	987.782309	15.849651
28.235200	1003.240551	15.854669
28.802239	1001.940581	15.859687
28.364212	1005.722570	15.864704
28.504292	1003.317293	15.869722
28.740396	1007.318937	15.874739
28.917106	1013.113748	15.879757
28.803185	1015.816933	15.884775
28.515709	1013.210873	15.889792
28.652443	999.951403	15.894810
28.396952	1015.034031	15.899827
28.554660	1007.970095	15.904845
28.868256	1002.356700	15.909863
28.717078	1008.836115	15.914880
28.684935	1010.129503	15.919898
28.597783	1006.572910	15.924915
28.735151	1004.602192	15.929933
28.771405	1013.738266	15.934951
28.747291	1000.417938	15.939968
28.974538	1003.139063	15.944986
28.841759	1023.389622	15.950003
28.808978	1030.551689	15.955021
29.432542	1018.334482	15.960039
29.204183	1019.254923	15.965056
29.051376	1020.850681	15.970074
29.475646	1026.399962	15.975091
29.165900	1012.211308	15.980109
29.080301	1008.750415	15.985127
29.185071	1004.722797	15.990144
29.206801	1006.465312	15.995162
29.115957	1031.775573	16.000179
29.334526	1029.272837	16.005197
29.599545	1028.664357	16.010215
29.302316	1022.461003	16.015232
29.567438	1010.672178	16.020250
29.313375	1006.437536	16.025267
29.649147	1012.553022	16.030285
29.663195	994.084733	16.035303
29.371949	994.739941	16.040320
29.294535	983.776497	16.045338
29.549951	995.270016	16.050355
29.466515	1016.706542	16.055373
29.538674	1019.214894	16.060391
29.723212	1022.949505	16.065408
29.591950	1020.076301	16.070426
29.537938	1028.780070	16.075443
29.529782	1020.680857	16.080461
29.747068	1022.571500	16.085479
29.729276	1027.846813	16.090496
29.849328	1028.839095	16.095514
29.824271	1018.172422	16.100531
29.728278	1025.560058	16.105549
29.943135	1017.658073	16.110567
29.608905	1017.289872	16.115584
29.794336	1020.896934	16.120602
29.432798	1028.830256	16.125619
29.800803	1016.732455	16.130637
30.033893	1025.303924	16.135655
29.526042	1019.725581	16.140672
29.851280	1016.076476	16.145690
30.323870	1035.392139	16.150707
30.288444	1033.085629	16.155725
30.274830	1025.904298	16.160743
29.921830	1023.349582	16.165760
29.858206	1028.242121	16.170778
30.069294	1035.851330	16.175795
30.210017	1039.824154	16.180813
30.710752	1045.897615	16.185831
30.217246	1054.105239	16.190848
30.405915	1049.133056	16.195866
30.859214	1048.680153	16.200883
30.590459	1029.953346	16.205901
30.364611	1029.515954	16.210919
30.097717	1018.996381	16.215936
30.263668	1023.945107	16.220954
30.462475	1048.937089	16.225971
30.543795	1047.366962	16.230989
30.494796	1060.724238	16.236007
30.339403	1058.886714	16.241024
30.631763	1045.031411	16.246042
30.626466	1055.874471	16.251059
30.487177	1055.361929	16.256077
30.640631	1057.196693	16.261095
30.178196	1052.627204	16.266112
30.531128	1056.018810	16.271130
30.443579	1059.186529	16.276147
30.317504	1049.677888	16.281165
30.902783	1050.153984	16.286183
30.507362	1054.297255	16.291200
30.899321	1052.458949	16.296218
30.962816	1055.846382	16.301235
30.622628	1064.501438	16.306253
31.051823	1062.595848	16.311271
30.920409	1082.000037	16.316288
31.266805	1075.698731	16.321306
30.960014	1076.625392	16.326323
31.215591	1073.179281	16.331341
31.354520	1065.172982	16.336359
31.066988	1056.520592	16.341376
31.339466	1054.416642	16.346394
31.204705	1049.491321	16.351411
31.067805	1047.808141	16.356429
31.111764	1048.944686	16.361447
31.200838	1051.551013	16.366464
31.137087	1071.336055	16.371482
31.482327	1071.686849	16.376499
31.559848	1078.323292	16.381517
31.647913	1059.184059	16.386535
31.226401	1059.979587	16.391552
31.149710	1055.269931	16.396570
31.805984	1057.208537	16.401587
31.333235	1059.685829	16.406605
31.364725	1071.141194	16.411623
31.211124	1080.060639	16.416640
31.473321	1069.035104	16.421658
31.516847	1075.728874	16.426675
31.440164	1077.131611	16.431693
31.957028	1071.024904	16.436711
31.843003	1070.206330	16.441728
31.620386	1066.094062	16.446746
32.016392	1070.380089	16.451763
31.757216	1065.311021	16.456781
31.901730	1069.668615	16.461799
31.901336	1074.307281	16.466816
31.859556	1064.476893	16.471834
31.659240	1069.452589	16.476851
31.445766	1074.763847	16.481869
31.954269	1067.848416	16.486887
31.867273	1070.177679	16.491904
31.746604	1072.075038	16.496922
32.155558	1061.644264	16.501939
31.759360	1075.531950	16.506957
32.026099	1066.201309	16.511975
32.096948	1071.921797	16.516992
31.893262	1062.401932	16.522010
32.020118	1060.439174	16.527027
31.850754	1073.641064	16.532045
32.684943	1076.746724	16.537063
32.576037	1079.195878	16.542080
31.944851	1066.922355	16.547098
32.252554	1069.025085	16.552115
32.087387	1083.218831	16.557133
32.050603	1085.418972	16.562151
32.261579	1094.428138	16.567168
32.342071	1089.212087	16.572186
32.553501	1101.209752	16.577203
32.762153	1100.265787	16.582221
32.963886	1091.429960	16.587239
33.013401	1096.400427	16.592256
32.363196	1078.640399	16.597274
32.308548	1071.155723	16.602291
32.730240	1095.327348	16.607309
32.865311	1088.268556	16.612327
32.901823	1090.889564	16.617344
33.004197	1078.247373	16.622362
32.963048	1063.784610	16.627379
32.682511	1069.027914	16.632397
33.003654	1053.220729	16.637415
32.931701	1051.130813	16.642432
32.794577	1058.358295	16.647450
32.912264	1053.139471	16.652467
32.625411	1052.026011	16.657485
32.927383	1065.265974	16.662503
32.856918	1073.171775	16.667520
32.891147	1076.801392	16.672538
33.276605	1077.474514	16.677555
33.086093	1088.417919	16.682573
33.021555	1076.318269	16.687591
33.241540	1088.828907	16.692608
33.060287	1093.092179	16.697626
33.436995	1081.298085	16.702643
33.353814	1087.645576	16.707661
33.410728	1086.305839	16.712679
33.020257	1091.511632	16.717696
32.992433	1087.484688	16.722714
33.232455	1075.762731	16.727731
32.832311	1098.075675	16.732749
32.924421	1088.733547	16.737767
33.199108	1084.513650	16.742784
33.240598	1090.617903	16.747802
33.365306	1096.811128	16.752819
33.297211	1103.576192	16.757837
33.821397	1104.760416	16.762855
33.702932	1108.216203	16.767872
33.598824	1109.519503	16.772890
34.046108	1110.848118	16.777907
33.857876	1096.282946	16.782925
33.923933	1082.315843	16.787943
33.806204	1080.980365	16.792960
33.391288	1086.471608	16.797978
33.799132	1077.730326	16.802995
33.769353	1097.491111	16.808013
34.013277	1108.033357	16.813031
33.905091	1100.815165	16.818048
33.832959	1091.645511	16.823066
34.265622	1101.652742	16.828083
33.909380	1100.317550	16.833101
33.823725	1094.487812	16.838119
34.540286	1094.530865	16.843136
34.134411	1098.570429	16.848154
34.078300	1079.825373	16.853171
33.864755	1077.888589	16.858189
34.254600	1089.069753	16.863207
34.452595	1112.852392	16.868224
34.206741	1092.490721	16.873242
34.141795	1081.007720	16.878259
34.287991	1101.196595	16.883277
34.216444	1110.741583	16.888295
34.525013	1110.314907	16.893312
34.383792	1112.723606	16.898330
34.438799	1106.923336	16.903347
34.573430	1110.334041	16.908365
34.543110	1112.539447	16.913383
34.235584	1107.218540	16.918400
34.268377	1108.125650	16.923418
34.520987	1116.533621	16.928435
34.501400	1118.402282	16.933453
34.477332	1105.009495	16.938471
34.689122	1106.666659	16.943488
34.214522	1109.480861	16.948506
34.411498	1095.606117	16.953523
34.641588	1116.086782	16.958541
34.335281	1127.294060	16.963559
34.642941	1122.120415	16.968576
34.504271	1140.264346	16.973594
35.058671	1128.753316	16.978611
34.919561	1138.987032	16.983629
34.721096	1136.250356	16.988647
35.351258	1133.678816	16.993664
35.016864	1135.987772	16.998682
35.348812	1124.642776	17.003699
35.177528	1127.273337	17.008717
35.583144	1124.364823	17.013735
35.196738	1128.302195	17.018752
35.174935	1128.628162	17.023770
35.289148	1113.975414	17.028787
35.385812	1124.685868	17.033805
35.057661	1131.011101	17.038823
35.258569	1123.432162	17.043840
35.370976	1121.314407	17.048858
35.499878	1126.056731	17.053875
35.454356	1136.594826	17.058893
35.380097	1120.845907	17.063911
35.737985	1125.326783	17.068928
35.505383	1136.335135	17.073946
35.821267	1118.705685	17.078963
35.606109	1126.557517	17.083981
35.477285	1123.657162	17.088999
35.623480	1114.447956	17.094016
35.690805	1125.510708	17.099034
35.674603	1119.800436	17.104051
35.753594	1129.113801	17.109069
35.761543	1130.912008	17.114087
35.984511	1121.759763	17.119104
35.905105	1118.709964	17.124122
36.060331	1112.969210	17.129139
35.714006	1124.777437	17.134157
35.614306	1119.399787	17.139175
36.150470	1120.825906	17.144192
35.687044	1123.853822	17.149210
36.112593	1122.596855	17.154227
35.807055	1132.633753	17.159245
35.882034	1123.525556	17.164263
36.107457	1116.779511	17.169280
36.136467	1112.392732	17.174298
36.128256	1120.301214	17.179315
36.087052	1120.620837	17.184333
36.330051	1125.222276	17.189351
36.052822	1119.316120	17.194368
35.871069	1125.556659	17.199386
36.094642	1131.414827	17.204403
36.168569	1126.349238	17.209421
36.125291	1137.162238	17.214439
36.370528	1143.273344	17.219456
36.038742	1147.750965	17.224474
35.969453	1144.073519	17.229491
36.338520	1134.067456	17.234509
36.255587	1149.836817	17.239527
36.777845	1151.510535	17.244544
36.630248	1173.375928	17.249562
37.020240	1157.395636	17.254579
37.225598	1163.903199	17.259597
36.882953	1140.730326	17.264615
37.052318	1130.719936	17.269632
36.945606	1145.764816	17.274650
37.154018	1134.168969	17.279667
37.115317	1124.570843	17.284685
36.580593	1132.717447	17.289703
37.033336	1125.788862	17.294720
36.873224	1133.539116	17.299738
36.956703	1129.928540	17.304755
36.760421	1136.128931	17.309773
37.119502	1152.283953	17.314791
37.427825	1147.341415	17.319808
36.956781	1149.653291	17.324826
37.262908	1157.837261	17.329843
37.408563	1156.801099	17.334861
36.956170	1155.355401	17.339879
37.336954	1158.228240	17.344896
37.113547	1155.298920	17.349914
37.106668	1158.738497	17.354931
37.300385	1164.508636	17.359949
37.207498	1165.958008	17.364967
37.381265	1157.853299	17.369984
36.778583	1166.057947	17.375002
37.338102	1157.831947	17.380019
37.412411	1159.539355	17.385037
37.309257	1177.768900	17.390055
37.615143	1185.095671	17.395072
37.720148	1190.521338	17.400090
37.746418	1182.937187	17.405107
37.844481	1190.306542	17.410125
38.088100	1190.297614	17.415143
37.979616	1171.274517	17.420160
37.627424	1168.689759	17.425178
37.856063	1173.000937	17.430195
38.484474	1168.205535	17.435213
38.128606	1166.286716	17.440231
38.204853	1151.583359	17.445248
38.050346	1143.488542	17.450266
38.221410	1140.707089	17.455283
38.319562	1150.391771	17.460301
38.298820	1151.559090	17.465319
38.591846	1142.847092	17.470336
38.011383	1143.104860	17.475354
37.926540	1155.642150	17.480371
38.339002	1149.723511	17.485389
38.039601	1156.578969	17.490407
38.172197	1149.603907	17.495424
38.110878	1144.872895	17.500442
38.276357	1175.054810	17.505459
38.518282	1183.738217	17.510477
38.455300	1188.877659	17.515495
38.532322	1180.351088	17.520512
38.453420	1180.209562	17.525530
38.673576	1181.450145	17.530547
39.103529	1175.986432	17.535565
38.900309	1184.119519	17.540583
38.906311	1177.842571	17.545600
39.035373	1173.773281	17.550618
38.635084	1161.977201	17.555635
38.638848	1156.641236	17.560653
38.590815	1185.682239	17.565671
38.888497	1176.041443	17.570688
38.812750	1182.145557	17.575706
38.531542	1181.035905	17.580723
38.854039	1171.773379	17.585741
38.666532	1179.375451	17.590759
39.111366	1177.091422	17.595776
38.767278	1179.373618	17.600794
38.695976	1178.741695	17.605811
38.839536	1188.231981	17.610829
39.017959	1208.603046	17.615847
39.010770	1207.611705	17.620864
38.660127	1210.025505	17.625882
38.755482	1216.597823	17.630899
39.369582	1202.865656	17.635917
39.482395	1200.139097	17.640935
39.154130	1210.297642	17.645952
39.248612	1213.293226	17.650970
39.389239	1208.852441	17.655987
39.843066	1202.746296	17.661005
39.382563	1198.874836	17.666023
39.501392	1198.060016	17.671040
39.883025	1204.556787	17.676058
39.575193	1209.482041	17.681075
40.059052	1213.002235	17.686093
39.905101	1217.538028	17.691111
39.915604	1193.415318	17.696128
39.958126	1194.284704	17.701146
39.959241	1194.187042	17.706163
39.992486	1190.735465	17.711181
39.813894	1203.204380	17.716199
39.697439	1190.131398	17.721216
39.896901	1192.103554	17.726234
39.881402	1213.502797	17.731251
40.369383	1213.229968	17.736269
40.351058	1213.185741	17.741287
40.099845	1205.826719	17.746304
40.270262	1199.127159	17.751322
40.168353	1204.442692	17.756339
40.669278	1204.159934	17.761357
40.438870	1199.580133	17.766375
40.284651	1198.395174	17.771392
40.323022	1195.752843	17.776410
39.954391	1202.139615	17.781427
40.693860	1206.726395	17.786445
40.496302	1223.429569	17.791463
40.283408	1214.364079	17.796480
40.449316	1213.272776	17.801498
40.409933	1215.732887	17.806515
41.035129	1223.177060	17.811533
40.525443	1222.764478	17.816551
40.839356	1217.938996	17.821568
40.826712	1219.087727	17.826586
40.794017	1219.987985	17.831603
41.088550	1212.675625	17.836621
41.079265	1220.985433	17.841639
40.577703	1221.738681	17.846656
40.600213	1219.852315	17.851674
40.850338	1222.244236	17.856691
40.963579	1212.746082	17.861709
40.732592	1220.068834	17.866727
40.744203	1217.544019	17.871744
40.752157	1218.110622	17.876762
40.715925	1232.946161	17.881779
41.084447	1243.388417	17.886797
41.223953	1249.223861	17.891815
41.346122	1247.025885	17.896832
41.225281	1241.819866	17.901850
41.359296	1240.049416	17.906867
41.596709	1245.779587	17.911885
41.457693	1241.158457	17.916903
41.522121	1241.915819	17.921920
41.498501	1242.542511	17.926938
41.379064	1241.336272	17.931955
41.488766	1240.875245	17.936973
41.204226	1244.805840	17.941991
41.543329	1241.019196	17.947008
41.374968	1239.208884	17.952026
41.393482	1247.051827	17.957043
41.482217	1237.931927	17.962061
41.573127	1256.143205	17.967079
42.042289	1262.341341	17.972096
41.946464	1260.885954	17.977114
41.942003	1268.012163	17.982131
42.401938	1262.466563	17.987149
42.298415	1261.647875	17.992167
42.057111	1240.494075	17.997184
42.286193	1234.345111	18.002202
41.750035	1231.155783	18.007219
42.147883	1247.399107	18.012237
41.888333	1261.241583	18.017255
41.986725	1259.541302	18.022272
42.425391	1261.719127	18.027290
42.027143	1266.416584	18.032307
42.413274	1258.760847	18.037325
42.921100	1249.261087	18.042343
42.933935	1257.133255	18.047360
42.802305	1254.796437	18.052378
42.903261	1259.013179	18.057395
43.139581	1241.901185	18.062413
43.029437	1225.385558	18.067431
43.113755	1227.860548	18.072448
43.021359	1218.756962	18.077466
42.824073	1219.115636	18.082483
43.029413	1220.764405	18.087501
42.769761	1228.634398	18.092519
42.753165	1219.842750	18.097536
42.664789	1212.001602	18.102554
42.838207	1221.587817	18.107571
43.104887	1213.603532	18.112589
43.026842	1218.286087	18.117607
42.747737	1211.526082	18.122624
42.913203	1211.109643	18.127642
42.655185	1226.304572	18.132659
42.814104	1216.204559	18.137677
42.834352	1229.997665	18.142695
42.908995	1241.004285	18.147712
43.088371	1248.914380	18.152730
42.673949	1262.188554	18.157747
43.017385	1254.294248	18.162765
42.984997	1248.603808	18.167783
43.240595	1272.113270	18.172800
43.496304	1266.052851	18.177818
43.192263	1289.722374	18.182835
43.514550	1280.794851	18.187853
43.399170	1282.013452	18.192871
43.670592	1283.999312	18.197888
44.019126	1279.410523	18.202906
43.829887	1293.301588	18.207923
44.103116	1281.523835	18.212941
44.070053	1285.431638	18.217959
43.928545	1279.683087	18.222976
44.262143	1278.123037	18.227994
44.008671	1268.049431	18.233011
43.794311	1259.971958	18.238029
44.009783	1251.171594	18.243047
43.648731	1261.986605	18.248064
43.927071	1273.092892	18.253082
43.715951	1277.257166	18.258099
44.007478	1274.509958	18.263117
43.926218	1275.485601	18.268135
43.617613	1295.042596	18.273152
43.829668	1292.644670	18.278170
44.130220	1301.949553	18.283187
44.012178	1305.976301	18.288205
44.168838	1309.103555	18.293223
44.209695	1323.522645	18.298240
44.644864	1311.409170	18.303258
44.349065	1314.010859	18.308275
44.493623	1315.872243	18.313293
44.581800	1312.501535	18.318311
44.420256	1308.931563	18.323328
44.871496	1306.772330	18.328346
44.525093	1318.664093	18.333363
44.367579	1324.915008	18.338381
44.883679	1324.942847	18.343399
45.058826	1336.814367	18.348416
45.192566	1337.916169	18.353434
45.161377	1340.209834	18.358451
45.282864	1326.798347	18.363469
45.428785	1304.544548	18.368487
45.056229	1309.505324	18.373504
45.357570	1310.268950	18.378522
45.289000	1299.366773	18.383539
45.112683	1291.226589	18.388557
45.216417	1294.912814	18.393575
45.233245	1295.511036	18.398592
45.412531	1291.311014	18.403610
45.342196	1296.560200	18.408627
45.273593	1306.535837	18.413645
45.355920	1316.929410	18.418663
45.245341	1330.474500	18.423680
45.438002	1325.611694	18.428698
45.589211	1335.774082	18.433715
45.683968	1332.235586	18.438733
45.757378	1332.862538	18.443751
45.880310	1327.063931	18.448768
45.588417	1328.644152	18.453786
45.364734	1338.364556	18.458803
45.550338	1336.843832	18.463821
46.029984	1321.053548	18.468839
45.700546	1328.063306	18.473856
45.851381	1322.867412	18.478874
46.192738	1318.135044	18.483891
46.186078	1328.593152	18.488909
46.104337	1333.971580	18.493927
45.928890	1320.835532	18.498944
46.102833	1327.183019	18.503962
46.088658	1331.874300	18.508979
45.904116	1336.194794	18.513997
46.381430	1337.416402	18.519015
45.866559	1346.052292	18.524032
46.493614	1362.971744	18.529050
46.193664	1358.380960	18.534067
46.414924	1366.545552	18.539085
46.335302	1357.686796	18.544103
46.412495	1352.581284	18.549120
46.649198	1347.149900	18.554138
46.797450	1349.543932	18.559155
46.444177	1351.009680	18.564173
47.094290	1350.149448	18.569191
47.082488	1351.246148	18.574208
46.905803	1353.460776	18.579226
47.133253	1352.247969	18.584243
46.820190	1352.820156	18.589261
46.980155	1348.494216	18.594279
46.704500	1360.997621	18.599296
46.801390	1353.002587	18.604314
46.802100	1354.743778	18.609331
46.716229	1357.802759	18.614349
47.290698	1364.968819	18.619367
46.722092	1387.633102	18.624384
47.137674	1395.408084	18.629402
47.530399	1380.234043	18.634419
47.123694	1380.569491	18.639437
47.758889	1377.813072	18.644455
47.478681	1381.285281	18.649472
47.651864	1377.761007	18.654490
47.286207	1377.158716	18.659507
47.395924	1384.035548	18.664525
47.810181	1374.217161	18.669543
47.690634	1379.293335	18.674560
48.039549	1365.567129	18.679578
47.960457	1373.056061	18.684595
47.833828	1371.710964	18.689613
47.590955	1378.645596	18.694631
48.046003	1378.083875	18.699648
47.997364	1361.484354	18.704666
48.185755	1361.872756	18.709683
47.926554	1366.593686	18.714701
48.119630	1362.333245	18.719719
48.150473	1374.775200	18.724736
48.018013	1362.662547	18.729754
48.151159	1367.119569	18.734771
48.309246	1360.741212	18.739789
48.157935	1357.586430	18.744807
47.946304	1375.992393	18.749824
48.017458	1375.139550	18.754842
48.183629	1392.041304	18.759859
48.048591	1397.310283	18.764877
48.661378	1383.181770	18.769895
48.023373	1395.823213	18.774912
47.976922	1390.609995	18.779930
48.476649	1390.964477	18.784947
48.482369	1412.068060	18.789965
48.926724	1413.010224	18.794983
48.660578	1429.477618	18.800000
49.022390	1430.517887	18.805018
49.175450	1417.055665	18.810035
48.864666	1414.168540	18.815053
49.440878	1408.906351	18.820071
49.058644	1418.711866	18.825088
49.287930	1407.372012	18.830106
49.137903	1388.792537	18.835123
49.173933	1399.503427	18.840141
49.264678	1408.173329	18.845159
49.296445	1413.090109	18.850176
49.007013	1414.605454	18.855194
49.600308	1416.540002	18.860211
49.342062	1421.034291	18.865229
49.301155	1415.997925	18.870247
49.433656	1409.183197	18.875264
49.240559	1410.530601	18.880282
49.430110	1421.415218	18.885299
49.070953	1421.983747	18.890317
49.636185	1403.955551	18.895335
49.459839	1406.876394	18.900352
49.610555	1419.019283	18.905370
49.966067	1421.034222	18.910387
49.883608	1443.422869	18.915405
50.200449	1431.746575	18.920423
49.956993	1430.981652	18.925440
49.945142	1440.729688	18.930458
50.125279	1427.898618	18.935475
49.748522	1436.753199	18.940493
50.084919	1432.200904	18.945511
50.081215	1430.828333	18.950528
50.065978	1429.778487	18.955546
50.249440	1424.162090	18.960563
49.978235	1437.262579	18.965581
50.131311	1428.678117	18.970599
50.530252	1428.603524	18.975616
50.277230	1422.729559	18.980634
50.555327	1421.974268	18.985651
50.560146	1423.615715	18.990669
50.913886	1425.868456	18.995687
50.866089	1427.595369	19.000704
50.641776	1429.679183	19.005722
50.795063	1419.551613	19.010739
50.622193	1422.103830	19.015757
50.730739	1427.082300	19.020775
50.788768	1435.090498	19.025792
50.552747	1454.914548	19.030810
51.121146	1451.700024	19.035827
51.270641	1455.894926	19.040845
51.350542	1451.592734	19.045863
51.528036	1453.796511	19.050880
51.319390	1445.618925	19.055898
51.743633	1417.012965	19.060915
51.646034	1415.784352	19.065933
51.113597	1411.798467	19.070951
51.404221	1411.668791	19.075968
51.295528	1408.870556	19.080986
51.334333	1416.603395	19.086003
51.591079	1429.822595	19.091021
51.713679	1438.012399	19.096039
51.299441	1439.940892	19.101056
51.444314	1441.336644	19.106074
51.822358	1445.974851	19.111091
51.721602	1444.628767	19.116109
51.935233	1443.537702	19.121127
51.906830	1444.058204	19.126144
51.823373	1441.004264	19.131162
52.199045	1432.085438	19.136179
51.665555	1438.268950	19.141197
51.872513	1437.487251	19.146215
52.031999	1440.022648	19.151232
51.845028	1438.207412	19.156250
52.041647	1433.488651	19.161267
51.961123	1441.918482	19.166285
52.123542	1442.460461	19.171303
52.771301	1446.434334	19.176320
52.805366	1462.573900	19.181338
52.403075	1454.971437	19.186355
52.221191	1458.926615	19.191373
52.520335	1459.368141	19.196391
52.650393	1448.909213	19.201408
52.509271	1462.163578	19.206426
52.911519	1447.286814	19.211443
52.735010	1454.124385	19.216461
52.932117	1446.217133	19.221479
52.971510	1448.158225	19.226496
52.716801	1458.309931	19.231514
53.047519	1453.796287	19.236531
52.694984	1457.794408	19.241549
52.884389	1450.530154	19.246567
52.712822	1452.328716	19.251584
52.805460	1458.133969	19.256602
53.152194	1458.759809	19.261619
53.202756	1482.984983	19.266637
53.191286	1486.027407	19.271655
53.253390	1489.089558	19.276672
53.481447	1490.649796	19.281690
53.420014	1486.079133	19.286707
53.493924	1487.181050	19.291725
53.547621	1487.052980	19.296743
53.921987	1478.895653	19.301760
53.567806	1496.410604	19.306778
53.723419	1483.987649	19.311795
53.702278	1482.081471	19.316813
53.415950	1475.202947	19.321831
53.681612	1484.721146	19.326848
53.727368	1496.626017	19.331866
53.671762	1479.550860	19.336883
53.346931	1484.453748	19.341901
53.603960	1498.476755	19.346919
53.760084	1509.783608	19.351936
53.884173	1513.270021	19.356954
54.076146	1507.018326	19.361971
54.185884	1515.096971	19.366989
54.204035	1511.241897	19.372007
54.277330	1509.599071	19.377024
54.178867	1515.802899	19.382042
54.407150	1532.949736	19.387059
54.684860	1532.795379	19.392077
54.940962	1534.749113	19.397095
54.955817	1529.762015	19.402112
54.356559	1537.558920	19.407130
54.955587	1532.069687	19.412147
55.164026	1526.601847	19.417165
54.990607	1515.274222	19.422183
55.439808	1499.106368	19.427200
54.929046	1497.786339	19.432218
55.020688	1495.302193	19.437235
55.125191	1499.060705	19.442253
54.987587	1504.531472	19.447271
55.451026	1496.196342	19.452288
55.073695	1503.446622	19.457306
55.125963	1498.134254	19.462323
55.125137	1509.554223	19.467341
55.312073	1529.315644	19.472359
55.801470	1525.759784	19.477376
55.531265	1533.652072	19.482394
55.713140	1526.775934	19.487411
55.633766	1523.658405	19.492429
55.638372	1528.074630	19.497447
55.945262	1522.918271	19.502464
55.952004	1525.322316	19.507482
55.884318	1506.945055	19.512499
55.732507	1495.958480	19.517517
55.895640	1510.128602	19.522535
56.088174	1517.734736	19.527552
56.023933	1525.993711	19.532570
55.922141	1521.311500	19.537587
55.889028	1521.614111	19.542605
55.970164	1519.120627	19.547623
56.255234	1523.746946	19.552640
55.900836	1520.751926	19.557658
56.099298	1510.799554	19.562675
56.049235	1518.406624	19.567693
56.061715	1531.719925	19.572711
55.886702	1511.778931	19.577728
56.121408	1546.155148	19.582746
56.742289	1522.271168	19.587763
56.555521	1553.219460	19.592781
56.387927	1562.469399	19.597799
56.634086	1531.710675	19.602816
56.226780	1563.544354	19.607834
56.515452	1556.586678	19.612851
56.729570	1542.517657	19.617869
56.714294	1559.903922	19.622887
57.129347	1561.177951	19.627904
57.175577	1573.590883	19.632922
57.300033	1572.850648	19.637939
57.335151	1570.243373	19.642957
57.243787	1571.812088	19.647975
57.712410	1567.886735	19.652992
57.272638	1560.689729	19.658010
57.300536	1550.642624	19.663027
57.640384	1549.466932	19.668045
57.528525	1560.035576	19.673063
57.851531	1567.224538	19.678080
57.812739	1563.880312	19.683098
58.147155	1542.756162	19.688115
57.674163	1538.104827	19.693133
57.136690	1542.936255	19.698151
57.668692	1542.226982	19.703168
57.580243	1561.433844	19.708186
57.590581	1579.219517	19.713203
58.136865	1551.970977	19.718221
57.835170	1558.558794	19.723239
57.992241	1559.864526	19.728256
57.826380	1567.710306	19.733274
57.776549	1566.387549	19.738291
57.987905	1578.561799	19.743309
58.079257	1589.997019	19.748327
58.598731	1594.796760	19.753344
58.315796	1592.562664	19.758362
58.444048	1599.551472	19.763379
58.485807	1588.107678	19.768397
58.574301	1595.297874	19.773415
58.513646	1588.320388	19.778432
58.763954	1584.360633	19.783450
58.678783	1592.475123	19.788467
58.613733	1589.706072	19.793485
58.683908	1590.344562	19.798503
59.001166	1580.516339	19.803520
58.873260	1583.539601	19.808538
58.896954	1597.017910	19.813555
59.285551	1601.627745	19.818573
59.196788	1617.634493	19.823591
59.378985	1615.178357	19.828608
59.417557	1604.888059	19.833626
59.153837	1590.691491	19.838643
59.430899	1601.335779	19.843661
59.240505	1616.945038	19.848679
59.450175	1615.747630	19.853696
59.463537	1614.248054	19.858714
59.441141	1614.240653	19.863731
59.885799	1601.302754	19.868749
59.791814	1605.616751	19.873767
59.920564	1614.302738	19.878784
59.800239	1613.189414	19.883802
59.964260	1605.192974	19.888819
59.882879	1605.111611	19.893837
59.816083	1613.564520	19.898855
60.082931	1606.604010	19.903872
59.868898	1611.467249	19.908890
59.875650	1611.406437	19.913907
59.829667	1606.702714	19.918925
59.909550	1614.688651	19.923943
60.073096	1630.691356	19.928960
59.974382	1637.268074	19.933978
60.204947	1639.947898	19.938995
60.393916	1627.233217	19.944013
60.254426	1635.553016	19.949031
59.844781	1640.283869	19.954048
60.213043	1647.527001	19.959066
60.407001	1664.012520	19.964083
60.874135	1668.487159	19.969101
61.109891	1668.204215	19.974119
60.790314	1660.217225	19.979136
60.939609	1670.858345	19.984154
60.949874	1663.023243	19.989171
61.415081	1661.843281	19.994189
61.040439	1663.768633	19.999207
61.483534	1659.332958	20.004224
61.448310	1659.157720	20.009242
61.565827	1666.486465	20.014259
61.418803	1664.164618	20.019277
61.360354	1658.744008	20.024295
61.537839	1663.433147	20.029312
61.664366	1654.659308	20.034330
61.316165	1660.632469	20.039347
61.783348	1652.784281	20.044365
61.614568	1666.271327	20.049383
61.513563	1656.714243	20.054400
62.071284	1664.848945	20.059418
61.871706	1680.889164	20.064435
62.030809	1669.319630	20.069453
62.245129	1681.915057	20.074471
62.447445	1683.290663	20.079488
62.067370	1673.839417	20.084506
62.358517	1676.630707	20.089523
62.646575	1669.399375	20.094541
61.949098	1666.671388	20.099559
62.180956	1666.170419	20.104576
62.416550	1679.615014	20.109594
62.261153	1680.176225	20.114611
62.469207	1688.786691	20.119629
62.578393	1680.558286	20.124647
62.759584	1669.833073	20.129664
63.027207	1667.833631	20.134682
62.435241	1675.552368	20.139699
62.911046	1665.675210	20.144717
62.837970	1671.387428	20.149735
62.868385	1671.006671	20.154752
63.028888	1669.571713	20.159770
62.790659	1676.779446	20.164787
63.003697	1670.489716	20.169805
62.959221	1672.077706	20.174823
63.016262	1693.845184	20.179840
63.089054	1702.776097	20.184858
63.410558	1704.909758	20.189875
63.432559	1702.575107	20.194893
63.301934	1701.134663	20.199911
63.395265	1704.676364	20.204928
63.523896	1717.224140	20.209946
63.549975	1705.034007	20.214963
63.401952	1704.222390	20.219981
63.570463	1718.837018	20.224999
63.399436	1723.471643	20.230016
64.037890	1725.701052	20.235034
63.913052	1737.546811	20.240051
64.428441	1731.418049	20.245069
64.155137	1715.797748	20.250087
64.325585	1716.450140	20.255104
64.606561	1719.955629	20.260122
64.413759	1713.471055	20.265139
64.664391	1709.037744	20.270157
64.391609	1711.005058	20.275175
64.849950	1707.993647	20.280192
64.705802	1714.786854	20.285210
64.550858	1720.784276	20.290227
64.893710	1710.184262	20.295245
64.820068	1711.850837	20.300263
64.319529	1709.690748	20.305280
64.932901	1710.719239	20.310298
64.742285	1713.175237	20.315315
64.765917	1708.369146	20.320333
64.631379	1716.530902	20.325351
64.646371	1713.786815	20.330368
65.054434	1733.041352	20.335386
64.852405	1747.888129	20.340403
65.218852	1737.073550	20.345421
65.329701	1737.356355	20.350439
65.357366	1741.142913	20.355456
65.644650	1735.094570	20.360474
65.830299	1729.872530	20.365491
65.568901	1732.969019	20.370509
65.895980	1731.567265	20.375527
65.524871	1735.472469	20.380544
65.686479	1733.592169	20.385562
65.659347	1730.957041	20.390579
65.835640	1732.560167	20.395597
65.753824	1734.357035	20.400615
65.657866	1746.555266	20.405632
66.336553	1761.362283	20.410650
66.153096	1767.671006	20.415667
66.231645	1759.304299	20.420685
66.353470	1757.661571	20.425703
66.318425	1759.663339	20.430720
66.329688	1765.020803	20.435738
66.291533	1769.283474	20.440755
66.797154	1762.039424	20.445773
66.915719	1762.887281	20.450791
66.247522	1769.674421	20.455808
66.731494	1769.499756	20.460826
66.450219	1767.174132	20.465843
66.642201	1759.711115	20.470861
66.597402	1766.688275	20.475879
66.658987	1776.673361	20.480896
66.982097	1780.063608	20.485914
67.037541	1793.227156	20.490931
67.146378	1790.433482	20.495949
67.178481	1787.497891	20.500967
67.228706	1786.511511	20.505984
67.643359	1778.638601	20.511002
67.394777	1779.464782	20.516019
67.494069	1770.303539	20.521037
67.599266	1776.703087	20.526055
67.487271	1785.013868	20.531072
67.731010	1772.653691	20.536090
67.331878	1779.799045	20.541107
67.732867	1786.503781	20.546125
67.787978	1790.367772	20.551143
67.807972	1800.878599	20.556160
68.236927	1793.395079	20.561178
67.917884	1800.499357	20.566195
67.987175	1800.035320	20.571213
68.101452	1801.253519	20.576231
68.173117	1802.093126	20.581248
68.358001	1796.811411	20.586266
68.294651	1790.233801	20.591283
68.308417	1790.574559	20.596301
68.710850	1802.447972	20.601319
68.558791	1800.389597	20.606336
68.822612	1807.844520	20.611354
68.524974	1816.826710	20.616371
68.478117	1829.371108	20.621389
68.697800	1821.604771	20.626407
68.743019	1825.753490	20.631424
69.062372	1818.915066	20.636442
68.847620	1816.268943	20.641459
68.731003	1819.328205	20.646477
69.218985	1817.992019	20.651495
68.987843	1829.150096	20.656512
68.990709	1833.752307	20.661530
69.339843	1846.736936	20.666547
69.533012	1850.959596	20.671565
69.039334	1844.502494	20.676583
69.646770	1844.756448	20.681600
69.860150	1842.866306	20.686618
69.715652	1842.829613	20.691635
69.868476	1837.110979	20.696653
70.201534	1830.344296	20.701671
69.956876	1836.245960	20.706688
70.243434	1833.762135	20.711706
70.216827	1841.357769	20.716723
69.877919	1839.343342	20.721741
70.223131	1847.244625	20.726759
70.103311	1844.127185	20.731776
70.227193	1834.472773	20.736794
70.223724	1835.193804	20.741811
70.264909	1855.258910	20.746829
70.534558	1855.113703	20.751847
70.547303	1869.256250	20.756864
70.929046	1862.247409	20.761882
71.013608	1868.055689	20.766899
70.972798	1853.057257	20.771917
71.201319	1860.088403	20.776935
71.145178	1853.615006	20.781952
71.115350	1852.611500	20.786970
71.096625	1856.842784	20.791987
71.023498	1849.146721	20.797005
71.271092	1851.786117	20.802023
70.985371	1851.281164	20.807040
71.290793	1848.402648	20.812058
71.345531	1845.483885	20.817075
71.363410	1842.042469	20.822093
71.522342	1845.454194	20.827111
71.528945	1849.296049	20.832128
71.819522	1845.630249	20.837146
71.760310	1852.386381	20.842163
71.408457	1841.794808	20.847181
71.816828	1860.615316	20.852199
71.855296	1877.446770	20.857216
72.044473	1871.794685	20.862234
72.059748	1878.427266	20.867251
71.946956	1885.489258	20.872269
71.712931	1876.500649	20.877287
71.681722	1881.265610	20.882304
72.201097	1896.101318	20.887322
72.265627	1899.177327	20.892339
72.460308	1915.821894	20.897357
72.566990	1908.948129	20.902375
72.434790	1907.429263	20.907392
72.854951	1904.714910	20.912410
72.899134	1901.859167	20.917427
73.029758	1907.726184	20.922445
73.205829	1897.426336	20.927463
72.797595	1897.505631	20.932480
72.918118	1891.718195	20.937498
73.227180	1899.261905	20.942515
72.981433	1898.228333	20.947533
73.429280	1897.681904	20.952551
73.216791	1892.822170	20.957568
72.924846	1912.769019	20.962586
73.048117	1917.521942	20.967603
73.159587	1927.903444	20.972621
73.390323	1927.907587	20.977639
73.401431	1933.501091	20.982656
73.560815	1944.809339	20.987674
74.391652	1953.399303	20.992691
73.985837	1955.935275	20.997709
74.225997	1942.888113	21.002727
74.137636	1948.469171	21.007744
74.235991	1950.537781	21.012762
74.360594	1941.021610	21.017779
74.426893	1949.996184	21.022797
74.617768	1946.678166	21.027815
74.440764	1948.095410	21.032832
74.735879	1949.818039	21.037850
74.840865	1930.811810	21.042867
74.383156	1935.997157	21.047885
74.686411	1938.865220	21.052903
74.518205	1945.332036	21.057920
74.744655	1940.806557	21.062938
74.800125	1938.004063	21.067955
74.685051	1947.295420	21.072973
74.709570	1946.048861	21.077991
74.996606	1948.985579	21.083008
75.103258	1964.217507	21.088026
75.460904	1955.752698	21.093043
75.400598	1967.840037	21.098061
75.604753	1960.334079	21.103079
75.630938	1968.817985	21.108096
75.857800	1963.669515	21.113114
76.186431	1955.055177	21.118131
75.873180	1942.325926	21.123149
76.113483	1932.744119	21.128167
75.579976	1941.255912	21.133184
75.849270	1955.145276	21.138202
75.961494	1950.908569	21.143219
75.801740	1951.918795	21.148237
76.391591	1954.355769	21.153255
76.480642	1955.820250	21.158272
76.170035	1950.112552	21.163290
76.519856	1955.958792	21.168307
76.418985	1958.433553	21.173325
76.509957	1950.859131	21.178343
76.403463	1947.148087	21.183360
76.397383	1951.825693	21.188378
76.514824	1955.613722	21.193395
76.360007	1972.427345	21.198413
76.755047	1964.903529	21.203431
76.688172	1972.238238	21.208448
76.741107	1975.729819	21.213466
77.066910	1972.627806	21.218483
76.720288	1974.921534	21.223501
76.726420	1992.956925	21.228519
76.921766	2000.026464	21.233536
77.325411	1996.624168	21.238554
77.664758	1997.512338	21.243571
77.652820	1998.810456	21.248589
77.718837	1997.187613	21.253607
77.501297	2002.419628	21.258624
77.698965	1992.492223	21.263642
78.088290	1994.860507	21.268659
78.164433	2002.403661	21.273677
78.289791	1995.424630	21.278695
77.928516	1996.630590	21.283712
78.054668	2001.928922	21.288730
78.268379	1994.655804	21.293747
77.788176	1999.593075	21.298765
78.117396	2010.924630	21.303783
78.378685	2018.570403	21.308800
78.421728	2030.922887	21.313818
78.460007	2034.564684	21.318835
78.530802	2025.701981	21.323853
78.438083	2028.076353	21.328871
78.347512	2040.676668	21.333888
78.265170	2054.288717	21.338906
78.746662	2049.360737	21.343923
78.949966	2062.758928	21.348941
78.937327	2052.865018	21.353959
79.308532	2044.704737	21.358976
79.295034	2052.043560	21.363994
79.458279	2046.483632	21.369011
79.564242	2045.609470	21.374029
79.686941	2037.759382	21.379047
79.596131	2050.721543	21.384064
79.843914	2060.452189	21.389082
80.428622	2063.357195	21.394099
79.900308	2046.817647	21.399117
79.714821	2046.370634	21.404135
79.709441	2038.957824	21.409152
80.150578	2057.192916	21.414170
79.935455	2055.080066	21.419187
79.758350	2063.991277	21.424205
80.263685	2052.356790	21.429223
80.388148	2057.765524	21.434240
80.072721	2060.573393	21.439258
80.535041	2060.194540	21.444275
80.826086	2077.909322	21.449293
80.501972	2076.719918	21.454311
80.736509	2083.240551	21.459328
81.073676	2078.867262	21.464346
81.402093	2077.948187	21.469363
81.214618	2084.185328	21.474381
81.368866	2073.879397	21.479399
81.437715	2055.712475	21.484416
81.454101	2045.958660	21.489434
81.573983	2037.476662	21.494451
81.434745	2044.157554	21.499469
81.441041	2038.660410	21.504487
81.475611	2038.118532	21.509504
81.784288	2041.375864	21.514522
81.675102	2038.060056	21.519539
81.419208	2049.925395	21.524557
81.732008	2067.767258	21.529575
82.017881	2063.910244	21.534592
81.827872	2087.466925	21.539610
82.141980	2070.240879	21.544627
82.073080	2069.611679	21.549645
82.102616	2075.471289	21.554663
81.908072	2069.134697	21.559680
81.861508	2077.553189	21.564698
82.169711	2086.431071	21.569715
81.921155	2111.686571	21.574733
82.041869	2111.749158	21.579751
82.354720	2103.782196	21.584768
82.435683	2118.732090	21.589786
82.416894	2130.410245	21.594803
82.578338	2133.713099	21.599821
82.738272	2146.655810	21.604839
82.828421	2142.785941	21.609856
82.826823	2161.505475	21.614874
83.062121	2160.752257	21.619891
83.193836	2164.981664	21.624909
83.492647	2166.036759	21.629927
83.509774	2167.415202	21.634944
83.458051	2167.717648	21.639962
83.543449	2163.694373	21.644979
83.763438	2178.785756	21.649997
84.150027	2179.199210	21.655015
84.113796	2187.892974	21.660032
84.426496	2176.484165	21.665050
84.344443	2170.046219	21.670067
84.218528	2168.789022	21.675085
84.183402	2167.231053	21.680103
84.926565	2181.310916	21.685120
84.456196	2174.986800	21.690138
84.531820	2169.841925	21.695155
84.614455	2183.485990	21.700173
84.423672	2173.895688	21.705191
84.762880	2176.246826	21.710208
84.705837	2179.708802	21.715226
84.859515	2170.272789	21.720243
84.926385	2186.969511	21.725261
84.888349	2176.338660	21.730279
84.931820	2180.693829	21.735296
84.703376	2187.724071	21.740314
85.148094	2203.009310	21.745331
85.088652	2215.007053	21.750349
85.364673	2211.382811	21.755367
85.599865	2205.894722	21.760384
85.398156	2217.759422	21.765402
85.598906	2210.532308	21.770419
85.607087	2213.209949	21.775437
85.636851	2222.402880	21.780455
86.139905	2231.416524	21.785472
86.254079	2227.914042	21.790490
86.287523	2232.756900	21.795507
86.190394	2224.647604	21.800525
86.119387	2235.785176	21.805543
86.521867	2231.739635	21.810560
86.200931	2237.969807	21.815578
86.475052	2228.649834	21.820595
86.504672	2233.158241	21.825613
86.379090	2235.070689	21.830631
86.692933	2220.713760	21.835648
86.743189	2239.300854	21.840666
86.741087	2250.205648	21.845683
87.064422	2255.782524	21.850701
87.105267	2250.638447	21.855719
87.135411	2254.353957	21.860736
86.953555	2255.742115	21.865754
87.312851	2241.148252	21.870771
87.650779	2236.872325	21.875789
87.528406	2235.147360	21.880807
87.551069	2245.294708	21.885824
87.708474	2259.630078	21.890842
88.320299	2261.944052	21.895859
88.300502	2259.217994	21.900877
88.194693	2258.130618	21.905895
88.296406	2247.774739	21.910912
88.112313	2243.970596	21.915930
88.239244	2254.231888	21.920947
88.669187	2250.254323	21.925965
88.324463	2265.556972	21.930983
88.827774	2257.038874	21.936000
88.726344	2260.345922	21.941018
88.585451	2264.620401	21.946035
88.798561	2257.057806	21.951053
88.544225	2270.217700	21.956071
88.913494	2258.903628	21.961088
88.464926	2264.871014	21.966106
88.782242	2262.416822	21.971123
88.976783	2286.666000	21.976141
89.019220	2295.042111	21.981159
89.174905	2292.376155	21.986176
89.329732	2287.333442	21.991194
89.367696	2287.780469	21.996211
89.448818	2289.015008	22.001229
89.259961	2303.457547	22.006247
89.687395	2320.444574	22.011264
89.683520	2324.231595	22.016282
89.735401	2318.299203	22.021299
89.807819	2315.564721	22.026317
89.799653	2323.401491	22.031335
90.198149	2322.960451	22.036352
90.023913	2343.434972	22.041370
90.116425	2342.120906	22.046387
90.253704	2342.833677	22.051405
90.392165	2346.657783	22.056423
90.219754	2343.532889	22.061440
90.148726	2349.797193	22.066458
91.036993	2356.097301	22.071475
91.155330	2353.648080	22.076493
90.625381	2370.155455	22.081511
91.292510	2357.330857	22.086528
91.208130	2356.861419	22.091546
91.262530	2364.269798	22.096563
91.517594	2360.552905	22.101581
91.564904	2355.418772	22.106599
91.910151	2353.551585	22.111616
91.817246	2363.547553	22.116634
91.871147	2354.555206	22.121651
91.757844	2358.690029	22.126669
91.723149	2361.377681	22.131687
91.921756	2343.932197	22.136704
92.180980	2353.522788	22.141722
91.747440	2352.635533	22.146739
92.352356	2365.447708	22.151757
92.508269	2373.473852	22.156775
92.684914	2377.049626	22.161792
92.484016	2377.863515	22.166810
92.674133	2372.056926	22.171827
92.769211	2365.631548	22.176845
92.625998	2383.219318	22.181863
92.758588	2370.206231	22.186880
93.032030	2371.738882	22.191898
92.856165	2384.872209	22.196915
92.907613	2380.822826	22.201933
93.197452	2385.700359	22.206951
93.267814	2395.888972	22.211968
93.186329	2400.836731	22.216986
93.470765	2401.646379	22.222003
93.407808	2396.903419	22.227021
93.253441	2409.328603	22.232039
93.625830	2400.661408	22.237056
93.721733	2416.272276	22.242074
93.883968	2424.525536	22.247091
94.406280	2421.567495	22.252109
94.108379	2424.732083	22.257127
94.517788	2412.678440	22.262144
94.497948	2417.368616	22.267162
94.324092	2422.552128	22.272179
94.488140	2421.931386	22.277197
94.731087	2416.973682	22.282215
94.699157	2419.148081	22.287232
94.733445	2420.263468	22.292250
94.762031	2422.664966	22.297267
94.558146	2426.775712	22.302285
94.793903	2438.839830	22.307303
95.048894	2441.371975	22.312320
94.953402	2457.736237	22.317338
95.345707	2455.667258	22.322355
95.867921	2457.768246	22.327373
95.587752	2449.993974	22.332391
95.304412	2439.671829	22.337408
95.782987	2444.161411	22.342426
95.799424	2453.941012	22.347443
95.883301	2439.977626	22.352461
95.994584	2443.319225	22.357479
96.319955	2453.201366	22.362496
96.217501	2460.501881	22.367514
96.209459	2480.407382	22.372531
96.625330	2479.407484	22.377549
96.229487	2475.308270	22.382567
96.283422	2472.395016	22.387584
96.273148	2465.041759	22.392602
96.191247	2469.391051	22.397619
96.599734	2462.419349	22.402637
96.590150	2487.113558	22.407655
96.740544	2486.348694	22.412672
96.931646	2479.060064	22.417690
97.026442	2482.871506	22.422707
97.333199	2475.612415	22.427725
96.996345	2492.438360	22.432743
97.343140	2507.857519	22.437760
97.919649	2507.372359	22.442778
97.880509	2519.242842	22.447795
97.761745	2516.935225	22.452813
98.082283	2510.860025	22.457831
98.436356	2495.646946	22.462848
98.258438	2504.527093	22.467866
98.360842	2516.421410	22.472883
98.309294	2511.548387	22.477901
98.414940	2503.824255	22.482919
98.465535	2503.521273	22.487936
98.568449	2506.065882	22.492954
98.723577	2498.131721	22.497971
98.777429	2486.767092	22.502989
98.765192	2494.643931	22.508007
98.894650	2503.544280	22.513024
99.135452	2509.202058	22.518042
99.122950	2521.157175	22.523059
99.573178	2518.366345	22.528077
99.246631	2524.470113	22.533095
98.910345	2520.819157	22.538112
99.551797	2528.576836	22.543130
99.556835	2523.761642	22.548147
99.685710	2517.612391	22.553165
99.610469	2529.026151	22.558183
99.707522	2518.390026	22.563200
99.786264	2531.821101	22.568218
99.866991	2555.726281	22.573235
100.057265	2539.892735	22.578253
100.200429	2542.736111	22.583271
100.280610	2550.309582	22.588288
100.469730	2547.257562	22.593306
100.341031	2539.164922	22.598323
100.394552	2543.008131	22.603341
100.225173	2559.782280	22.608359
100.618306	2569.966741	22.613376
100.989913	2578.448624	22.618394
100.410533	2582.771090	22.623411
100.811941	2569.386186	22.628429
100.734440	2584.224182	22.633447
101.016793	2598.020057	22.638464
101.497473	2594.449608	22.643482
101.273960	2603.769687	22.648499
101.160146	2596.410063	22.653517
101.354958	2595.766318	22.658535
101.708898	2618.762836	22.663552
101.991471	2621.197803	22.668570
101.869999	2621.762289	22.673587
102.358406	2608.940015	22.678605
102.480276	2623.214555	22.683623
102.052879	2619.095948	22.688640
102.394311	2615.697143	22.693658
102.144806	2627.626427	22.698675
102.563308	2637.378222	22.703693
102.803998	2650.569641	22.708711
102.824045	2656.106940	22.713728
103.314523	2642.603942	22.718746
103.131376	2637.334989	22.723763
103.460851	2645.929027	22.728781
103.349670	2648.059466	22.733799
103.315706	2641.053619	22.738816
103.685310	2646.454949	22.743834
103.739999	2644.853505	22.748851
103.796552	2633.076179	22.753869
103.720681	2641.763950	22.758887
103.578276	2642.176038	22.763904
103.892812	2641.539157	22.768922
103.604152	2664.988227	22.773939
104.018676	2668.516705	22.778957
104.218088	2670.714818	22.783975
104.200929	2672.565200	22.788992
104.473958	2657.601628	22.794010
104.223258	2661.530345	22.799027
104.524697	2667.256386	22.804045
104.914275	2679.169543	22.809063
105.056412	2688.480137	22.814080
105.255858	2686.951566	22.819098
105.143655	2679.597149	22.824115
105.280134	2683.997417	22.829133
105.170832	2684.504119	22.834151
104.983222	2689.670255	22.839168
105.105304	2691.369443	22.844186
105.147174	2689.582052	22.849203
105.442268	2697.572026	22.854221
105.461304	2714.446877	22.859239
105.406901	2712.670115	22.864256
105.697326	2700.768135	22.869274
105.560422	2712.453007	22.874291
105.822412	2741.184196	22.879309
106.385881	2734.774424	22.884327
106.572790	2737.535354	22.889344
106.908097	2742.209120	22.894362
106.575524	2742.707378	22.899379
106.857311	2721.834533	22.904397
106.813326	2728.786068	22.909415
106.586774	2734.116526	22.914432
107.109644	2727.938185	22.919450
106.900767	2728.552006	22.924467
107.048963	2734.813768	22.929485
107.458620	2748.183625	22.934503
107.146321	2754.732766	22.939520
107.445309	2751.926681	22.944538
107.670300	2746.018425	22.949555
107.792836	2753.163655	22.954573
107.808056	2753.758262	22.959591
107.845919	2749.463965	22.964608
108.551192	2746.391741	22.969626
108.156899	2737.436014	22.974643
107.807159	2746.780243	22.979661
108.398576	2769.128768	22.984679
108.282186	2771.790980	22.989696
108.674608	2768.380864	22.994714
109.093012	2775.859622	22.999731
108.793165	2772.117056	23.004749
108.779896	2776.653708	23.009767
108.722945	2779.960073	23.014784
109.141769	2772.094622	23.019802
109.378661	2789.835430	23.024819
109.077526	2791.720096	23.029837
109.531023	2803.640469	23.034855
109.506267	2809.646680	23.039872
109.719380	2793.549653	23.044890
109.534354	2796.015949	23.049907
109.654350	2795.980337	23.054925
109.991552	2791.667400	23.059943
110.121740	2808.058208	23.064960
110.596209	2816.400341	23.069978
110.662448	2824.271138	23.074995
110.590840	2815.463696	23.080013
110.754817	2821.110251	23.085031
110.800209	2822.569197	23.090048
111.086055	2824.979295	23.095066
110.800484	2836.370988	23.100083
110.826798	2828.737203	23.105101
111.057316	2815.690014	23.110119
111.032639	2824.029152	23.115136
110.949192	2817.223817	23.120154
111.120387	2813.161513	23.125171
110.953555	2826.055469	23.130189
111.062946	2838.413006	23.135207
111.605349	2832.085207	23.140224
112.118165	2826.462167	23.145242
111.845849	2848.409744	23.150259
111.709806	2831.814609	23.155277
111.951213	2825.560763	23.160295
112.049238	2849.012184	23.165312
112.507705	2852.192334	23.170330
112.724243	2849.300272	23.175347
112.627831	2859.685700	23.180365
112.817288	2856.149041	23.185383
112.648093	2857.911998	23.190400
112.871269	2855.994211	23.195418
112.794668	2855.975788	23.200435
112.919651	2856.968202	23.205453
112.887685	2866.544213	23.210471
112.770318	2879.261218	23.215488
112.988352	2879.004680	23.220506
113.366660	2890.871830	23.225523
113.374604	2881.654450	23.230541
113.766377	2900.088829	23.235559
113.765491	2916.506951	23.240576
113.841635	2903.243610	23.245594
114.000097	2907.447734	23.250611
114.191728	2904.297707	23.255629
114.447952	2897.664704	23.260647
114.225749	2911.096134	23.265664
114.638688	2909.723062	23.270682
114.835133	2923.796445	23.275699
114.783800	2925.940977	23.280717
115.197331	2928.576929	23.285735
115.154396	2931.480731	23.290752
115.427762	2916.039396	23.295770
115.538715	2928.488003	23.300787
115.596684	2932.958285	23.305805
115.681765	2919.640018	23.310823
115.402462	2923.970580	23.315840
115.604642	2920.774819	23.320858
115.523873	2913.585169	23.325875
115.885567	2910.185426	23.330893
115.988290	2925.297861	23.335911
115.983089	2940.899458	23.340928
116.143549	2950.659575	23.345946
116.198744	2950.752280	23.350963
116.206506	2950.390834	23.355981
116.794897	2944.286906	23.360999
116.399599	2950.300344	23.366016
116.553139	2958.289437	23.371034
116.939243	2964.488981	23.376051
116.779614	2975.040311	23.381069
117.316488	2977.125672	23.386087
117.171228	2968.356625	23.391104
117.619989	2959.301733	23.396122
117.667444	2966.220710	23.401139
117.244134	2971.768256	23.406157
117.692946	2979.799162	23.411175
117.625088	2992.270828	23.416192
117.714037	3003.738224	23.421210
117.931486	2988.445738	23.426227
117.917377	3004.061408	23.431245
118.347939	2990.714734	23.436263
117.811401	3007.234098	23.441280
118.183073	3016.919680	23.446298
118.486415	3027.166764	23.451315
118.190207	3019.102137	23.456333
118.619472	3029.786928	23.461351
118.732144	3059.247322	23.466368
118.886670	3046.133387	23.471386
119.399907	3044.819035	23.476403
119.495938	3050.461568	23.481421
119.805830	3032.402084	23.486439
119.718712	3043.409124	23.491456
119.963092	3032.672050	23.496474
119.895005	3039.360929	23.501491
119.878943	3041.998540	23.506509
120.344444	3030.885626	23.511527
120.302137	3036.514029	23.516544
120.154716	3044.498456	23.521562
120.248789	3062.916011	23.526579
120.174724	3067.628414	23.531597
120.334738	3063.362529	23.536615
120.551895	3063.230408	23.541632
120.630505	3073.203447	23.546650
120.806669	3084.922076	23.551667
120.857794	3092.411580	23.556685
121.382438	3087.309628	23.561703
121.250353	3090.442411	23.566720
121.240572	3090.919100	23.571738
121.892486	3095.252256	23.576755
121.696230	3112.257071	23.581773
121.626258	3110.766695	23.586791
121.818326	3122.907569	23.591808
122.164623	3122.023342	23.596826
122.184245	3112.273016	23.601843
121.804615	3111.684660	23.606861
122.362184	3121.672608	23.611879
122.456875	3139.156497	23.616896
122.298271	3140.789585	23.621914
122.914943	3137.234297	23.626931
122.722929	3136.776488	23.631949
122.594425	3138.159365	23.636967
122.795107	3149.509165	23.641984
123.135411	3163.839079	23.647002
123.321168	3161.028162	23.652019
123.518391	3171.491272	23.657037
123.809725	3149.692065	23.662055
123.791955	3148.787228	23.667072
123.970838	3156.393259	23.672090
124.004089	3159.092248	23.677107
124.314024	3181.438312	23.682125
124.455392	3182.139462	23.687143
124.717785	3180.901278	23.692160
124.661553	3172.074650	23.697178
124.708975	3163.111155	23.702195
124.694030	3172.637459	23.707213
125.058330	3173.907942	23.712231
124.940885	3174.468659	23.717248
124.958005	3181.994308	23.722266
124.944720	3177.972330	23.727283
125.011164	3180.641647	23.732301
124.898632	3170.080153	23.737319
125.079262	3193.429288	23.742336
125.335859	3192.394178	23.747354
125.728181	3197.793668	23.752371
125.194230	3206.671228	23.757389
125.676992	3222.148129	23.762407
125.922234	3217.476893	23.767424
126.080899	3229.977930	23.772442
125.970004	3229.194124	23.777459
125.970911	3244.123332	23.782477
126.767244	3246.659767	23.787495
126.937753	3248.571543	23.792512
127.051959	3242.622546	23.797530
127.421765	3238.013247	23.802547
127.274472	3249.468163	23.807565
127.529162	3235.391830	23.812583
127.774110	3229.946641	23.817600
127.548330	3234.054022	23.822618
127.828045	3228.644980	23.827635
127.845502	3244.243289	23.832653
128.195075	3242.097644	23.837671
128.120475	3252.516842	23.842688
128.095821	3259.591401	23.847706
128.541407	3265.211320	23.852723
127.953591	3260.063294	23.857741
128.151869	3255.455382	23.862759
128.623842	3260.325412	23.867776
128.450914	3276.294702	23.872794
128.559864	3279.536185	23.877811
128.906657	3279.153711	23.882829
129.054066	3282.969562	23.887847
129.422786	3304.531657	23.892864
129.414430	3311.429021	23.897882
129.761413	3302.180915	23.902899
129.746887	3312.297182	23.907917
129.674584	3313.106346	23.912935
129.939669	3312.709369	23.917952
129.826952	3317.133045	23.922970
130.073087	3314.798583	23.927987
130.163507	3326.503548	23.933005
130.067219	3328.102337	23.938023
130.574631	3324.646232	23.943040
130.582577	3344.848481	23.948058
131.071932	3331.976661	23.953075
130.460752	3336.468020	23.958093
131.161375	3344.304812	23.963111
131.265871	3353.072011	23.968128
130.877563	3375.399915	23.973146
131.541323	3365.535705	23.978163
131.418942	3368.662280	23.983181
131.781580	3367.576428	23.988199
131.636160	3360.250559	23.993216
131.761584	3375.315006	23.998234
132.023715	3380.625202	24.003251
131.900154	3395.347085	24.008269
132.019398	3398.933053	24.013287
132.498427	3383.326289	24.018304
132.217441	3393.831196	24.023322
132.599424	3406.345547	24.028339
132.761259	3416.507707	24.033357
132.772535	3409.598107	24.038375
133.136172	3400.873513	24.043392
133.314678	3412.748565	24.048410
133.232884	3418.127769	24.053427
133.757077	3434.625580	24.058445
133.805829	3437.136514	24.063463
134.057412	3432.689951	24.068480
133.896277	3429.555155	24.073498
134.304047	3427.525273	24.078515
133.965361	3423.693550	24.083533
134.150350	3424.521478	24.088551
134.164411	3444.040129	24.093568
134.443423	3458.107945	24.098586
134.821552	3451.953171	24.103603
135.011104	3466.711729	24.108621
135.170821	3462.924026	24.113639
135.523362	3455.084514	24.118656
135.177584	3468.122409	24.123674
135.201857	3456.231576	24.128691
135.522495	3462.402446	24.133709
135.347723	3471.345604	24.138727
135.697257	3481.548675	24.143744
135.729164	3486.288366	24.148762
135.914867	3484.813035	24.153779
136.002164	3503.707331	24.158797
135.934662	3513.175376	24.163815
136.554960	3514.033016	24.168832
136.366132	3520.976558	24.173850
136.499122	3509.872249	24.178867
136.674542	3523.977884	24.183885
137.177423	3527.427205	24.188903
137.505544	3530.849327	24.193920
137.122549	3542.647252	24.198938
137.279326	3529.831432	24.203955
137.282446	3531.600817	24.208973
137.076086	3546.715981	24.213991
137.682061	3552.120085	24.219008
137.584474	3563.033220	24.224026
137.906641	3563.218659	24.229043
137.807280	3564.559959	24.234061
138.098039	3562.068103	24.239079
138.751969	3569.605691	24.244096
138.410069	3585.336387	24.249114
138.664800	3582.264255	24.254131
138.737954	3577.229404	24.259149
138.711531	3572.268639	24.264167
139.279135	3575.746195	24.269184
139.057217	3587.456332	24.274202
138.941975	3600.598389	24.279219
139.417550	3604.974765	24.284237
139.304458	3598.919488	24.289255
139.813147	3608.297301	24.294272
139.711797	3632.266317	24.299290
140.499564	3625.841643	24.304307
140.495179	3631.626269	24.309325
140.624366	3634.872471	24.314343
140.734000	3624.834500	24.319360
140.660602	3638.327037	24.324378
141.129278	3628.645572	24.329395
141.058240	3628.755262	24.334413
140.705829	3626.074112	24.339431
141.132423	3613.947527	24.344448
141.066381	3633.458750	24.349466
141.229830	3632.609156	24.354483
141.668805	3644.637160	24.359501
141.541226	3654.399625	24.364519
141.705819	3640.783273	24.369536
141.399423	3654.203635	24.374554
141.589222	3661.245770	24.379571
142.196042	3666.627758	24.384589
142.140681	3685.894288	24.389607
142.504384	3695.499791	24.394624
142.485146	3695.590997	24.399642
142.813896	3694.401975	24.404659
142.992760	3684.913776	24.409677
143.439884	3704.220566	24.414695
143.338148	3715.283144	24.419712
143.593810	3720.622815	24.424730
143.619322	3706.857096	24.429747
143.665168	3713.775898	24.434765
143.922083	3712.313577	24.439783
144.319222	3701.919005	24.444800
144.131713	3715.429019	24.449818
144.216848	3717.993196	24.454835
144.579161	3724.810418	24.459853
144.616835	3734.303528	24.464871
145.185066	3728.287452	24.469888
144.685473	3727.899112	24.474906
145.183954	3731.932848	24.479923
145.625553	3726.518266	24.484941
145.332255	3726.209520	24.489959
145.435813	3721.703878	24.494976
145.519726	3724.893604	24.499994
145.386357	3729.937397	24.505011
145.753634	3736.594152	24.510029
145.638877	3744.088414	24.515047
145.825887	3754.139817	24.520064
146.251582	3759.339121	24.525082
146.471183	3756.795651	24.530099
146.579741	3765.558518	24.535117
146.502080	3783.054926	24.540135
147.151343	3790.372337	24.545152
146.733060	3772.219588	24.550170
146.803974	3798.784757	24.555187
147.278116	3790.662952	24.560205
147.167243	3795.948604	24.565223
147.428949	3795.820391	24.570240
147.302114	3809.351496	24.575258
147.394429	3802.266748	24.580275
147.606594	3807.312900	24.585293
147.561441	3839.310113	24.590311
148.045829	3835.287269	24.595328
148.149494	3839.204635	24.600346
148.040669	3851.195078	24.605363
148.666729	3856.897370	24.610381
148.564178	3871.641555	24.615399
148.660276	3874.765655	24.620416
148.940524	3863.713116	24.625434
149.473128	3893.315125	24.630451
149.501776	3890.736786	24.635469
149.367655	3895.687148	24.640487
149.782656	3885.227457	24.645504
150.010114	3902.666709	24.650522
150.400531	3919.651294	24.655539
150.701430	3915.324944	24.660557
150.415117	3910.545517	24.665575
150.515013	3916.500058	24.670592
150.624170	3915.778670	24.675610
150.785172	3896.583960	24.680627
150.934665	3910.768832	24.685645
151.032765	3921.896460	24.690663
151.330580	3916.114572	24.695680
151.092844	3927.239897	24.700698
151.486284	3938.421925	24.705715
152.049368	3929.214490	24.710733
152.037184	3934.554466	24.715751
152.378145	3914.901547	24.720768
152.223513	3932.531544	24.725786
152.375288	3939.582236	24.730803
152.693767	3938.054228	24.735821
152.342890	3958.751109	24.740839
152.569980	3942.422472	24.745856
152.852297	3939.282940	24.750874
152.594090	3940.957954	24.755891
153.103359	3958.118716	24.760909
152.991300	3978.682369	24.765927
153.230689	3975.600803	24.770944
153.288551	3966.772023	24.775962
153.293708	3983.848784	24.780979
153.505256	4000.880861	24.785997
153.772828	3996.787921	24.791015
154.118778	3995.331830	24.796032
154.421450	4011.629632	24.801050
154.418744	4028.358438	24.806067
154.531601	4019.584574	24.811085
154.610286	4015.990572	24.816103
155.329984	4006.161860	24.821120
155.403231	4016.938756	24.826138
155.223577	4013.619568	24.831155
155.335618	4012.214141	24.836173
155.106074	4031.760616	24.841191
155.808803	4035.383509	24.846208
155.949523	4037.120005	24.851226
155.737077	4038.116742	24.856243
156.333341	4046.104287	24.861261
156.417446	4064.954195	24.866279
156.299897	4063.177894	24.871296
156.691563	4067.261795	24.876314
156.793192	4059.561869	24.881331
156.952449	4054.057670	24.886349
156.682474	4067.420685	24.891367
156.850201	4093.226019	24.896384
157.281922	4100.386336	24.901402
157.010056	4108.028546	24.906419
157.426275	4119.058409	24.911437
157.666930	4121.428737	24.916455
157.807474	4135.695491	24.921472
158.209059	4140.698975	24.926490
158.097877	4158.701472	24.931507
158.585117	4156.546338	24.936525
158.547488	4151.391291	24.941543
158.710195	4162.734566	24.946560
158.940929	4174.008793	24.951578
158.851408	4180.036905	24.956595
159.219742	4179.019316	24.961613
159.430609	4177.479336	24.966631
159.645296	4175.056932	24.971648
159.805123	4199.351021	24.976666
159.996191	4205.738739	24.981683
160.177650	4204.614067	24.986701
160.144094	4209.227555	24.991719
160.050112	4202.393359	24.996736
160.712905	4222.422409	25.001754
160.430295	4236.522308	25.006771
160.744072	4236.017646	25.011789
160.714821	4237.787558	25.016807
161.153505	4245.453430	25.021824
161.293553	4258.025969	25.026842
161.519474	4260.659047	25.031859
161.827505	4251.697388	25.036877
161.904216	4252.327092	25.041895
161.948978	4257.221524	25.046912
162.161640	4272.587644	25.051930
162.454704	4287.531124	25.056947
162.663709	4279.011595	25.061965
162.558452	4275.767802	25.066983
162.520066	4275.436493	25.072000
162.868822	4269.764342	25.077018
162.535300	4278.839495	25.082035
163.005591	4293.805858	25.087053
163.175186	4305.759363	25.092071
163.275955	4306.726635	25.097088
163.550364	4308.247550	25.102106
163.709141	4334.139694	25.107123
163.840443	4332.989970	25.112141
163.935783	4336.053720	25.117159
164.385325	4334.642440	25.122176
164.458389	4343.252412	25.127194
164.319552	4357.777890	25.132211
164.681899	4348.688730	25.137229
164.921791	4355.913583	25.142247
164.717396	4358.177910	25.147264
165.025166	4370.468935	25.152282
165.271350	4382.877559	25.157299
165.309706	4386.442843	25.162317
165.624931	4400.929799	25.167335
165.707206	4396.812013	25.172352
166.044009	4397.000643	25.177370
165.967847	4420.794657	25.182387
166.072047	4426.376637	25.187405
166.645313	4430.042301	25.192423
166.807348	4432.610077	25.197440
166.862674	4438.669481	25.202458
167.342404	4458.979770	25.207475
167.387876	4448.084581	25.212493
167.545183	4443.102882	25.217511
167.965258	4447.115498	25.222528
168.206270	4441.617001	25.227546
168.141662	4444.224845	25.232563
168.457847	4447.456364	25.237581
168.379250	4474.937868	25.242599
168.117615	4475.627816	25.247616
168.563987	4464.326509	25.252634
168.790368	4472.413379	25.257651
169.091562	4488.551474	25.262669
169.173690	4496.923310	25.267687
169.132281	4499.942030	25.272704
169.613456	4492.324539	25.277722
169.241994	4508.580121	25.282739
169.747244	4514.763704	25.287757
170.411523	4524.033925	25.292775
170.020530	4537.994060	25.297792
170.411735	4519.541407	25.302810
170.150373	4519.811242	25.307827
170.483251	4534.549606	25.312845
170.908909	4542.380550	25.317863
170.861842	4550.293156	25.322880
170.925256	4542.873612	25.327898
170.697580	4559.550785	25.332915
171.252871	4570.860109	25.337933
171.548400	4575.969544	25.342951
171.251134	4579.131336	25.347968
171.659820	4590.608792	25.352986
171.896666	4612.279595	25.358003
172.297080	4608.088218	25.363021
172.151758	4607.899814	25.368039
172.558448	4628.537433	25.373056
172.915592	4623.686652	25.378074
173.004220	4638.154904	25.383091
172.725487	4632.852475	25.388109
173.214131	4647.048499	25.393127
173.135741	4660.723703	25.398144
173.736137	4650.309436	25.403162
173.747958	4660.972308	25.408179
173.630227	4668.030919	25.413197
173.888825	4678.824380	25.418215
174.254033	4688.741820	25.423232
174.432105	4678.062892	25.428250
174.483268	4700.244076	25.433267
174.706887	4711.306669	25.438285
175.160506	4706.227296	25.443303
175.297289	4711.507620	25.448320
175.435204	4705.261614	25.453338
175.757687	4710.017524	25.458355
176.199522	4720.345206	25.463373
176.554577	4730.939250	25.468391
176.448873	4727.129818	25.473408
176.594775	4728.406161	25.478426
176.425085	4736.926053	25.483443
176.751761	4736.556987	25.488461
176.900727	4723.381868	25.493479
176.927591	4733.326533	25.498496
176.815657	4731.598027	25.503514
177.225689	4747.194354	25.508531
177.080822	4756.120150	25.513549
177.293353	4757.008276	25.518567
177.490808	4777.060357	25.523584
177.662129	4780.295380	25.528602
178.065355	4784.134565	25.533619
178.565691	4803.947238	25.538637
178.518319	4809.865048	25.543655
178.391084	4812.921115	25.548672
178.749051	4812.980513	25.553690
179.022304	4819.980798	25.558707
179.195623	4834.910103	25.563725
179.275792	4843.807157	25.568743
179.330843	4838.025852	25.573760
179.657850	4851.884405	25.578778
179.497085	4854.233891	25.583795
179.672885	4873.989837	25.588813
180.286086	4877.333011	25.593831
180.150127	4882.567197	25.598848
180.481921	4890.403068	25.603866
180.661547	4898.230161	25.608883
180.790020	4900.167742	25.613901
181.402539	4914.363946	25.618919
181.154082	4912.218221	25.623936
181.626745	4913.883811	25.628954
181.244458	4914.603238	25.633971
181.391002	4930.859304	25.638989
182.175318	4936.179654	25.644007
181.930787	4950.156948	25.649024
182.178228	4957.032400	25.654042
182.396571	4965.070479	25.659059
182.390235	4970.131417	25.664077
182.745471	4971.892042	25.669095
182.373813	4993.295400	25.674112
183.489120	5001.188932	25.679130
183.360064	5004.544265	25.684148
183.289474	5022.335239	25.689165
184.011563	5025.066361	25.694183
184.174035	5029.459266	25.699200
184.535434	5021.889708	25.704218
184.502047	5026.237528	25.709236
184.745885	5041.032293	25.714253
184.778873	5046.607769	25.719271
184.956758	5053.403887	25.724288
185.373119	5043.506427	25.729306
185.582874	5047.395406	25.734324
185.140752	5061.489266	25.739341
185.775649	5062.660938	25.744359
185.832141	5073.098290	25.749376
185.896990	5072.099134	25.754394
186.292848	5074.876767	25.759412
186.665846	5092.666338	25.764429
187.036755	5086.641846	25.769447
186.819611	5097.133065	25.774464
187.423120	5093.136528	25.779482
187.294390	5098.444373	25.784500
187.114115	5098.451911	25.789517
187.673287	5117.480749	25.794535
187.408490	5122.902336	25.799552
187.459275	5130.949125	25.804570
187.919536	5123.233165	25.809588
188.112213	5149.324309	25.814605
188.502112	5152.553677	25.819623
188.543426	5163.913935	25.824640
188.829474	5167.505217	25.829658
189.002610	5174.146385	25.834676
188.966128	5181.954587	25.839693
189.592108	5173.362563	25.844711
189.433104	5206.140844	25.849728
189.404772	5211.413057	25.854746
189.765226	5196.710668	25.859764
189.839130	5215.111337	25.864781
190.462928	5217.190269	25.869799
190.226070	5236.690733	25.874816
190.567510	5240.989877	25.879834
190.932396	5255.145650	25.884852
190.905721	5259.135311	25.889869
190.820506	5261.058231	25.894887
190.988107	5272.411027	25.899904
191.388832	5283.780950	25.904922
191.812516	5279.991611	25.909940
191.833485	5278.023939	25.914957
192.458020	5277.774159	25.919975
192.354560	5306.113951	25.924992
192.336627	5306.667533	25.930010
193.260100	5301.170061	25.935028
193.122125	5306.984511	25.940045
193.399723	5303.769926	25.945063
193.483857	5307.900848	25.950080
193.142131	5319.476480	25.955098
193.461916	5324.706612	25.960116
193.804714	5331.867557	25.965133
193.961607	5352.089737	25.970151
193.744100	5369.246088	25.975168
194.108658	5366.741387	25.980186
194.217228	5391.496399	25.985204
194.247376	5403.832552	25.990221
194.508463	5404.786142	25.995239
194.616876	5432.232541	26.000256
194.941154	5433.113910	26.005274
195.340988	5447.080996	26.010292
195.650012	5458.811822	26.015309
196.337919	5466.829604	26.020327
196.249191	5471.617490	26.025344
196.397126	5489.474103	26.030362
196.955870	5482.230015	26.035380
196.581926	5483.731690	26.040397
197.178760	5480.104294	26.045415
197.351320	5506.034857	26.050432
197.570714	5505.160509	26.055450
197.837185	5502.873605	26.060468
197.521192	5511.012899	26.065485
197.830266	5505.505520	26.070503
197.963845	5530.396025	26.075520
198.237716	5530.391741	26.080538
198.679409	5532.466710	26.085556
198.592434	5548.088840	26.090573
199.124595	5561.510209	26.095591
199.230187	5557.666877	26.100608
199.240600	5564.334950	26.105626
199.383285	5570.525650	26.110644
199.643152	5580.702797	26.115661
200.018170	5594.267253	26.120679
199.981092	5598.069855	26.125696
200.432365	5602.811035	26.130714
200.843352	5602.357710	26.135732
200.398927	5601.464878	26.140749
200.801783	5604.745780	26.145767
200.862923	5640.042014	26.150784
201.123072	5639.984847	26.155802
201.549834	5632.807356	26.160820
201.381842	5654.650442	26.165837
201.610483	5655.722509	26.170855
201.709774	5656.522539	26.175872
202.067787	5671.328060	26.180890
202.382330	5680.856178	26.185908
202.238694	5691.554019	26.190925
202.638137	5691.428231	26.195943
202.930510	5697.750105	26.200960
203.510423	5700.179902	26.205978
203.601031	5709.230799	26.210996
203.520287	5714.181127	26.216013
203.958850	5733.292146	26.221031
204.045479	5737.333106	26.226048
204.157707	5733.254230	26.231066
204.555773	5736.449387	26.236084
204.608639	5760.981820	26.241101
204.573553	5772.802368	26.246119
205.092016	5762.857472	26.251136
205.156866	5774.139711	26.256154
205.768931	5789.200659	26.261172
205.625329	5797.389727	26.266189
206.221950	5794.149357	26.271207
206.102416	5810.029491	26.276224
205.962774	5823.256880	26.281242
206.609930	5813.370108	26.286260
206.381188	5821.758427	26.291277
206.371099	5837.411089	26.296295
206.702598	5858.063216	26.301312
207.104459	5880.054959	26.306330
207.299846	5884.914909	26.311348
207.461560	5903.993971	26.316365
207.808856	5910.528251	26.321383
208.011691	5912.691705	26.326400
208.238711	5923.598114	26.331418
208.847335	5925.495481	26.336436
209.042557	5930.608799	26.341453
208.828511	5931.444632	26.346471
209.625939	5946.591843	26.351488
209.954808	5960.202544	26.356506
210.306185	5960.563536	26.361524
209.974194	5962.230075	26.366541
210.526183	5960.402667	26.371559
210.729882	5953.902550	26.376576
210.189463	5957.332326	26.381594
210.568434	5972.314972	26.386612
210.825202	5972.503018	26.391629
210.960230	5980.500652	26.396647
211.404245	5993.845211	26.401664
211.406228	6014.514682	26.406682
211.808529	6012.554571	26.411700
211.650625	6012.962919	26.416717
211.654495	6030.773135	26.421735
211.868028	6035.136963	26.426752
211.940194	6045.151605	26.431770
212.589023	6053.629102	26.436788
212.651440	6058.788810	26.441805
212.968121	6083.518105	26.446823
213.257026	6088.996537	26.451840
213.489476	6089.236451	26.456858
213.951162	6084.407086	26.461876
213.635187	6103.501188	26.466893
214.207663	6123.405640	26.471911
214.302229	6116.657719	26.476928
214.574654	6127.482302	26.481946
215.015721	6133.045851	26.486964
215.083822	6139.408388	26.491981
215.276201	6142.709591	26.496999
215.529937	6137.691498	26.502016
215.590070	6154.902843	26.507034
216.266818	6166.495372	26.512052
216.185731	6171.954140	26.517069
216.336301	6158.866388	26.522087
216.654676	6170.001520	26.527104
216.283995	6200.822156	26.532122
216.723470	6197.764887	26.537140
216.881270	6208.072819	26.542157
217.093089	6227.312674	26.547175
217.191250	6237.203719	26.552192
217.381750	6250.717949	26.557210
217.989053	6247.321581	26.562228
217.801650	6272.784544	26.567245
218.303925	6282.540394	26.572263
218.807962	6276.133089	26.577280
218.571086	6296.814281	26.582298
218.969999	6301.246981	26.587316
219.456727	6306.349366	26.592333
219.507966	6324.771556	26.597351
219.888330	6336.457883	26.602368
219.957965	6349.089857	26.607386
220.600810	6345.838858	26.612404
220.870555	6360.745689	26.617421
220.958834	6357.396629	26.622439
221.117463	6362.776344	26.627456
220.818841	6372.727582	26.632474
221.192174	6381.579622	26.637492
221.313553	6386.965284	26.642509
221.559676	6399.634469	26.647527
221.613715	6418.721920	26.652544
221.990508	6427.241427	26.657562
222.418657	6431.560148	26.662580
222.452668	6456.457074	26.667597
222.542410	6454.573481	26.672615
223.263121	6453.593207	26.677632
223.305085	6483.616185	26.682650
223.314160	6482.501519	26.687668
223.563023	6494.705377	26.692685
223.647144	6508.700200	26.697703
224.290961	6504.006102	26.702720
224.156592	6526.391911	26.707738
224.461099	6524.217591	26.712756
224.888661	6544.159876	26.717773
224.867459	6547.207263	26.722791
225.279031	6548.439848	26.727808
225.381232	6557.126722	26.732826
225.657127	6551.688763	26.737844
225.948735	6559.250279	26.742861
226.061023	6583.325366	26.747879
226.590283	6584.141094	26.752896
226.368609	6585.447086	26.757914
226.824426	6593.260170	26.762932
226.861155	6603.000753	26.767949
227.114493	6617.022992	26.772967
227.355200	6609.697671	26.777984
227.585436	6644.000847	26.783002
227.770055	6648.047681	26.788020
227.973556	6650.475492	26.793037
228.056145	6666.797171	26.798055
228.543908	6670.382637	26.803072
228.095228	6685.606514	26.808090
228.612472	6700.961246	26.813108
229.112920	6725.817319	26.818125
229.159990	6734.613006	26.823143
229.771994	6740.128298	26.828160
230.067976	6759.479743	26.833178
230.327238	6763.307789	26.838196
230.380299	6767.935020	26.843213
230.616851	6785.317244	26.848231
230.715538	6809.150181	26.853248
230.789887	6812.194980	26.858266
231.047247	6815.227917	26.863284
231.274402	6823.537835	26.868301
231.552395	6829.664226	26.873319
231.827748	6863.101561	26.878336
232.107205	6859.647957	26.883354
232.083878	6869.594196	26.888372
232.505637	6892.233371	26.893389
232.897637	6909.662559	26.898407
233.208756	6912.224322	26.903424
233.336533	6923.884503	26.908442
233.539330	6922.485582	26.913460
234.425385	6921.367992	26.918477
234.331409	6927.934516	26.923495
234.536037	6937.259888	26.928512
234.891090	6960.373214	26.933530
234.917128	6965.458786	26.938548
235.588456	6951.066244	26.943565
235.275171	6962.326266	26.948583
235.773393	6967.283073	26.953600
235.510018	6980.218077	26.958618
236.020695	6998.207525	26.963636
236.316457	6995.829184	26.968653
235.934354	7021.789455	26.973671
236.650635	7036.223746	26.978688
236.989981	7052.470305	26.983706
237.034672	7039.109904	26.988724
237.191434	7063.299062	26.993741
237.721317	7062.014003	26.998759
237.901996	7068.370798	27.003776
237.830458	7075.291011	27.008794
238.097436	7088.311519	27.013812
238.700048	7097.079451	27.018829
238.708375	7100.779213	27.023847
239.054679	7101.586372	27.028864
239.013122	7119.519223	27.033882
239.180989	7129.341533	27.038900
239.707516	7142.968245	27.043917
239.368334	7159.097268	27.048935
239.890466	7158.526270	27.053952
239.621397	7182.530151	27.058970
239.995504	7205.016896	27.063988
240.806847	7210.419556	27.069005
240.478958	7226.610582	27.074023
241.045043	7244.113128	27.079040
241.508152	7250.773534	27.084058
241.936959	7268.917199	27.089076
242.323007	7278.230392	27.094093
242.740154	7274.781497	27.099111
242.826740	7259.296162	27.104128
242.807363	7291.476150	27.109146
243.162876	7310.246825	27.114164
243.946641	7287.525083	27.119181
243.696991	7307.861953	27.124199
244.134300	7325.406366	27.129216
244.518237	7334.246277	27.134234
244.318741	7335.033443	27.139252
244.642781	7327.875452	27.144269
244.678987	7353.141758	27.149287
245.124353	7358.484002	27.154304
245.227854	7367.679420	27.159322
245.399119	7380.953843	27.164340
245.623163	7369.478061	27.169357
245.633066	7399.012320	27.174375
246.175558	7404.443745	27.179392
246.588029	7399.507722	27.184410
246.559210	7418.999137	27.189428
247.078097	7438.114520	27.194445
247.168710	7444.753347	27.199463
247.566490	7449.812092	27.204480
247.878681	7458.166252	27.209498
247.701103	7482.179637	27.214516
248.297818	7481.544813	27.219533
247.982215	7486.454485	27.224551
248.688533	7491.545106	27.229568
249.317717	7509.209435	27.234586
249.348968	7505.174454	27.239604
250.044815	7508.962222	27.244621
250.159982	7515.213204	27.249639
250.708083	7523.217436	27.254656
250.607761	7520.974532	27.259674
250.705629	7542.394846	27.264692
251.488753	7530.528480	27.269709
251.025969	7526.509293	27.274727
251.177091	7535.956872	27.279744
251.363297	7530.288158	27.284762
251.589132	7556.606450	27.289780
251.810038	7556.036246	27.294797
251.556505	7569.962363	27.299815
251.570245	7594.914002	27.304832
252.001801	7599.127885	27.309850
252.253803	7611.571359	27.314868
252.609254	7642.747399	27.319885
252.574511	7660.169960	27.324903
253.243421	7675.347321	27.329920
253.353672	7676.779893	27.334938
253.448341	7706.730855	27.339956
254.229798	7719.503898	27.344973
254.344460	7726.526135	27.349991
254.628209	7762.046878	27.355008
255.116777	7743.705319	27.360026
254.905402	7774.738297	27.365044
255.568775	7787.279223	27.370061
255.768191	7810.688566	27.375079
256.001725	7809.402690	27.380096
256.312211	7817.917052	27.385114
256.492871	7821.889306	27.390132
256.953618	7837.121257	27.395149
256.785103	7859.656932	27.400167
257.288528	7855.631574	27.405184
257.490101	7883.141636	27.410202
257.885572	7879.474963	27.415220
258.281527	7899.621613	27.420237
258.440660	7930.077338	27.425255
258.810024	7909.523121	27.430272
259.096968	7920.585119	27.435290
259.345435	7935.950935	27.440308
259.404868	7941.987521	27.445325
260.012822	7968.583190	27.450343
260.046119	7979.857977	27.455360
260.270334	7975.523015	27.460378
260.334515	8003.816855	27.465396
260.865678	8004.418353	27.470413
261.140069	8027.142557	27.475431
261.201937	8038.080789	27.480448
261.419894	8034.640655	27.485466
261.535894	8058.052668	27.490484
261.904096	8065.043310	27.495501
262.246121	8090.834945	27.500519
262.358574	8102.442632	27.505536
263.012664	8111.926865	27.510554
262.662317	8132.609415	27.515572
263.163386	8137.096425	27.520589
263.522216	8157.066796	27.525607
263.257482	8167.068116	27.530624
263.955261	8186.451021	27.535642
263.917324	8187.847463	27.540660
264.483822	8198.747085	27.545677
264.672925	8224.306814	27.550695
264.937455	8227.624529	27.555712
265.552781	8250.454464	27.560730
265.260762	8253.929347	27.565748
266.133629	8259.625537	27.570765
266.285083	8279.644075	27.575783
266.226506	8286.539179	27.580800
266.678438	8280.819960	27.585818
266.823309	8304.676264	27.590836
267.323025	8306.329303	27.595853
267.465040	8329.606980	27.600871
267.705406	8335.182905	27.605888
267.967229	8345.065010	27.610906
267.903276	8368.695826	27.615924
268.208978	8368.548783	27.620941
268.714828	8387.916120	27.625959
268.693203	8394.048428	27.630976
269.210805	8411.566384	27.635994
269.367561	8426.013325	27.641012
269.718725	8447.806099	27.646029
270.056160	8459.722850	27.651047
270.389244	8484.367779	27.656064
270.879957	8475.138413	27.661082
270.889244	8500.706819	27.666100
271.190630	8518.154709	27.671117
271.613539	8526.981257	27.676135
271.649548	8539.061784	27.681152
272.362607	8536.589942	27.686170
272.276288	8556.060535	27.691188
272.755806	8578.530205	27.696205
272.783011	8586.769120	27.701223
273.084582	8607.626579	27.706240
273.365215	8600.072813	27.711258
273.114995	8628.554077	27.716276
273.464492	8644.299532	27.721293
274.134146	8662.198788	27.726311
274.208591	8678.637286	27.731328
274.984136	8696.878520	27.736346
275.230651	8711.568740	27.741364
275.408753	8713.320300	27.746381
275.702937	8731.879867	27.751399
276.033093	8738.893417	27.756416
276.674555	8746.753605	27.761434
276.749296	8766.428570	27.766452
276.705734	8762.840315	27.771469
277.212366	8767.573714	27.776487
277.227326	8783.321489	27.781504
277.492531	8790.564167	27.786522
277.619403	8812.257093	27.791540
277.721567	8822.293224	27.796557
278.377763	8832.388207	27.801575
278.208600	8848.503754	27.806592
278.734461	8871.977624	27.811610
279.195834	8887.612654	27.816628
279.113418	8908.527014	27.821645
279.653572	8905.441363	27.826663
279.644666	8915.621161	27.831680
280.134424	8931.210009	27.836698
279.944273	8942.300809	27.841716
280.569568	8955.048670	27.846733
280.899022	8971.736422	27.851751
280.477114	9002.583995	27.856768
281.479258	9007.715352	27.861786
281.734099	9029.448395	27.866804
281.931694	9044.637760	27.871821
282.450342	9074.154060	27.876839
282.605968	9076.836598	27.881856
283.100394	9085.370769	27.886874
283.140165	9106.485867	27.891892
283.332359	9116.361092	27.896909
283.499839	9131.768987	27.901927
283.521868	9156.446112	27.906944
284.177675	9165.948853	27.911962
284.396012	9184.083557	27.916980
284.756799	9195.044245	27.921997
285.313779	9216.825802	27.927015
285.741109	9230.069329	27.932032
286.227106	9237.892000	27.937050
286.118357	9254.512594	27.942068
286.259629	9262.993773	27.947085
286.935792	9284.636039	27.952103
286.894295	9290.187213	27.957120
287.354997	9295.836977	27.962138
287.621193	9302.838562	27.967156
287.960781	9336.114239	27.972173
288.405268	9341.789033	27.977191
288.607686	9347.230926	27.982208
288.968141	9363.623021	27.987226
289.021024	9371.013137	27.992244
289.352230	9380.169968	27.997261
289.775175	9389.032832	28.002279
289.356750	9421.926674	28.007296
290.163432	9432.410033	28.012314
290.469928	9452.007258	28.017332
290.401387	9473.984888	28.022349
290.946141	9481.185712	28.027367
291.001644	9498.108935	28.032384
291.631808	9519.519652	28.037402
291.978567	9528.443530	28.042420
292.126001	9548.466773	28.047437
292.682187	9557.997054	28.052455
292.816784	9572.919609	28.057472
293.228473	9584.125466	28.062490
293.397193	9592.765744	28.067508
293.601470	9611.361196	28.072525
294.147645	9613.974900	28.077543
294.515702	9629.920680	28.082560
294.608219	9653.367662	28.087578
294.936549	9643.581930	28.092596
295.307842	9653.400638	28.097613
295.674882	9659.844917	28.102631
295.571158	9673.750291	28.107648
295.655713	9679.801283	28.112666
296.095298	9705.220149	28.117684
296.159128	9718.123860	28.122701
296.819260	9729.763174	28.127719
297.100890	9737.961388	28.132736
297.567888	9747.629161	28.137754
297.850838	9755.057166	28.142772
297.924119	9770.826982	28.147789
298.333729	9777.842921	28.152807
298.379940	9810.078087	28.157824
298.774616	9816.399597	28.162842
299.077129	9822.423386	28.167860
299.420220	9849.211005	28.172877
299.469581	9868.082498	28.177895
299.655403	9892.559245	28.182912
299.879339	9899.798419	28.187930
300.243256	9923.269853	28.192948
300.771693	9952.801678	28.197965
301.009924	9950.660263	28.202983
301.213252	9990.353381	28.208000
301.586232	9997.644789	28.213018
302.016118	10005.873429	28.218036
302.229502	10034.015522	28.223053
302.775570	10040.530590	28.228071
302.928891	10067.611289	28.233088
303.353726	10074.905882	28.238106
303.634035	10098.630147	28.243124
304.008287	10113.825892	28.248141
304.309681	10126.473716	28.253159
304.627027	10140.734220	28.258176
305.198867	10145.042953	28.263194
305.575688	10161.262943	28.268212
305.411955	10172.782081	28.273229
306.001458	10189.618622	28.278247
305.951451	10200.690375	28.283264
306.172623	10225.636958	28.288282
306.850970	10240.448339	28.293300
306.924619	10251.988335	28.298317
307.277319	10255.657212	28.303335
307.794238	10280.589806	28.308352
307.979851	10293.127163	28.313370
308.343521	10296.139161	28.318388
308.400867	10322.560013	28.323405
308.758117	10337.755941	28.328423
309.133852	10360.548213	28.333440
309.913860	10374.807608	28.338458
310.132017	10381.007969	28.343476
309.911124	10404.239685	28.348493
310.498089	10421.270091	28.353511
310.590990	10431.879328	28.358528
310.480649	10455.794297	28.363546
311.137522	10462.663735	28.368564
310.940563	10495.052841	28.373581
311.728178	10494.120326	28.378599
311.586791	10525.788436	28.383616
312.422672	10536.440276	28.388634
312.535765	10552.059372	28.393652
312.886650	10572.007490	28.398669
313.561311	10580.181700	28.403687
313.518172	10613.990640	28.408704
314.031014	10625.497132	28.413722
314.340507	10623.454837	28.418740
314.655411	10636.542433	28.423757
315.048697	10657.324002	28.428775
314.920715	10677.269483	28.433792
315.459043	10696.821164	28.438810
315.925803	10708.181602	28.443828
315.820760	10735.111870	28.448845
316.359619	10745.271328	28.453863
316.378379	10761.411703	28.458880
316.732100	10788.128479	28.463898
317.660397	10795.084276	28.468916
317.580709	10816.745344	28.473933
318.045814	10828.167916	28.478951
318.523172	10854.178856	28.483968
318.822432	10856.608241	28.488986
319.269724	10882.750333	28.494004
319.270484	10894.243414	28.499021
319.550318	10911.376053	28.504039
319.894014	10925.057817	28.509056
320.064792	10962.555909	28.514074
320.758209	10979.202462	28.519092
321.026190	10989.745236	28.524109
321.529045	10999.240087	28.529127
321.433096	11032.030962	28.534144
321.839400	11041.713185	28.539162
322.469210	11055.299499	28.544180
322.664563	11080.124123	28.549197
323.001558	11095.377170	28.554215
323.202154	11122.082347	28.559232
323.322451	11128.030247	28.564250
323.867537	11144.762796	28.569268
324.251826	11170.625814	28.574285
324.538647	11178.417900	28.579303
324.917196	11194.563577	28.584320
325.096551	11212.938331	28.589338
325.582218	11236.222426	28.594356
325.656910	11256.021077	28.599373
326.191555	11267.717014	28.604391
326.589767	11278.633921	28.609408
327.001082	11305.305056	28.614426
327.441637	11312.233761	28.619444
327.700288	11335.706082	28.624461
327.919012	11328.815616	28.629479
328.110896	11356.455204	28.634496
328.570529	11371.316732	28.639514
329.133805	11378.940520	28.644532
329.001391	11394.533506	28.649549
329.170160	11401.945506	28.654567
329.954583	11410.929247	28.659584
330.087761	11414.560598	28.664602
330.593815	11435.224537	28.669620
330.745425	11445.308851	28.674637
330.789703	11458.396611	28.679655
331.332776	11478.229523	28.684672
331.491088	11501.489856	28.689690
331.795142	11526.171184	28.694708
332.136308	11547.419944	28.699725
332.551344	11548.836592	28.704743
332.618242	11573.084756	28.709760
332.782696	11598.093026	28.714778
333.306494	11618.901956	28.719796
333.505509	11633.293709	28.724813
333.557764	11652.714749	28.729831
334.125224	11690.869995	28.734848
334.316668	11721.646240	28.739866
334.951188	11740.469725	28.744884
335.042216	11757.628694	28.749901
335.263868	11786.841148	28.754919
335.757648	11811.399837	28.759936
336.375160	11837.585331	28.764954
337.381012	11846.355984	28.769972
337.414829	11864.249053	28.774989
337.505820	11875.327506	28.780007
338.166554	11906.028164	28.785024
338.416432	11925.637253	28.790042
339.291191	11937.818245	28.795060
339.174256	11944.678283	28.800077
339.397865	11958.658740	28.805095
340.130249	11977.821490	28.810112
339.728622	12005.902360	28.815130
340.296767	12018.502977	28.820148
340.624986	12034.846862	28.825165
340.990715	12042.248255	28.830183
341.312182	12065.140305	28.835200
341.309860	12094.811690	28.840218
341.947388	12112.815057	28.845236
342.092300	12136.752614	28.850253
342.342333	12156.138848	28.855271
342.876012	12181.683865	28.860288
343.239008	12209.200153	28.865306
343.901552	12226.152885	28.870324
344.051563	12252.192435	28.875341
344.479154	12259.205108	28.880359
344.819136	12268.794410	28.885376
345.118215	12297.378458	28.890394
345.751195	12311.249539	28.895412
345.823873	12326.753150	28.900429
346.145498	12338.372697	28.905447
346.723404	12363.245120	28.910464
346.695177	12379.364804	28.915482
347.366045	12394.784574	28.920500
347.594990	12405.614561	28.925517
347.809421	12418.787409	28.930535
348.591319	12433.000072	28.935552
348.319793	12450.577684	28.940570
349.155152	12478.351335	28.945588
349.188933	12487.706815	28.950605
349.493480	12504.340492	28.955623
349.998428	12514.519350	28.960640
349.851190	12537.804586	28.965658
350.465990	12559.608558	28.970676
350.577140	12576.999799	28.975693
351.072507	12598.017681	28.980711
351.316014	12619.951153	28.985728
351.320743	12645.082039	28.990746
352.183707	12658.075996	28.995764
352.182551	12695.807872	29.000781
352.650605	12722.604900	29.005799
352.798835	12741.536842	29.010816
353.133227	12757.172938	29.015834
353.721884	12794.050157	29.020852
354.038140	12818.749166	29.025869
354.469543	12849.509147	29.030887
355.181379	12865.552151	29.035904
355.307125	12900.132284	29.040922
355.916742	12902.812436	29.045940
356.475488	12928.536148	29.050957
356.598531	12956.162673	29.055975
357.054338	12973.295788	29.060992
356.932419	12992.594981	29.066010
357.594348	13006.905228	29.071028
357.956626	13025.749697	29.076045
358.408500	13051.304697	29.081063
359.004462	13067.327222	29.086080
359.073558	13098.096641	29.091098
359.435669	13109.830955	29.096116
359.728423	13127.176573	29.101133
359.836365	13138.389025	29.106151
360.405528	13166.778980	29.111168
360.952314	13192.233692	29.116186
361.440895	13210.086189	29.121204
362.074940	13226.151419	29.126221
362.167460	13253.363623	29.131239
362.746434	13266.905539	29.136256
362.553056	13287.619518	29.141274
363.191561	13301.848771	29.146292
363.947681	13311.047154	29.151309
363.864064	13320.204414	29.156327
364.295318	13350.013618	29.161344
364.660162	13377.282811	29.166362
364.532221	13384.817251	29.171380
364.802729	13417.465162	29.176397
365.184617	13442.245838	29.181415
365.711303	13468.711142	29.186432
365.854181	13495.775648	29.191450
366.537130	13520.066116	29.196468
366.937136	13533.370347	29.201485
367.224993	13554.477920	29.206503
367.622068	13567.313718	29.211520
368.175664	13592.324670	29.216538
368.591724	13612.018482	29.221556
368.679961	13622.392597	29.226573
368.994825	13646.801743	29.231591
369.326273	13660.824838	29.236608
369.626714	13689.894398	29.241626
370.225936	13707.199127	29.246644
370.865739	13728.116853	29.251661
370.800287	13760.101165	29.256679
371.255212	13765.138019	29.261696
371.444776	13791.486796	29.266714
371.901655	13807.076517	29.271732
372.242671	13834.862559	29.276749
372.685921	13861.280840	29.281767
373.032014	13878.922065	29.286784
373.197425	13901.338184	29.291802
373.485880	13928.932347	29.296820
373.962949	13959.387991	29.301837
374.218078	13989.575221	29.306855
375.035119	14007.288751	29.311872
375.300241	14037.078940	29.316890
375.395801	14068.300683	29.321908
376.076519	14081.310648	29.326925
376.509241	14111.418952	29.331943
376.725313	14133.236875	29.336960
376.926808	14169.772270	29.341978
377.256587	14198.637500	29.346996
378.045718	14213.221252	29.352013
378.402153	14241.008826	29.357031
378.932882	14266.347269	29.362048
379.399026	14282.679675	29.367066
380.175235	14313.177436	29.372084
380.528605	14319.823783	29.377101
380.763117	14341.964560	29.382119
381.165197	14352.196083	29.387136
381.463228	14366.537858	29.392154
381.721649	14377.022338	29.397172
382.109152	14403.202190	29.402189
382.194583	14421.527811	29.407207
382.836697	14445.179215	29.412224
383.248200	14470.623486	29.417242
383.367918	14489.819751	29.422260
383.496700	14503.882215	29.427277
383.729022	14550.231552	29.432295
384.544018	14567.450932	29.437312
385.075532	14594.094740	29.442330
385.212894	14620.955194	29.447348
385.893751	14635.064323	29.452365
385.918463	14659.407380	29.457383
386.123651	14695.284178	29.462400
386.801483	14715.211652	29.467418
387.017966	14727.836525	29.472436
387.649773	14746.258895	29.477453
387.580509	14781.553418	29.482471
387.889505	14786.675270	29.487488
388.550856	14826.674529	29.492506
388.637848	14843.871280	29.497524
389.453299	14862.906189	29.502541
389.617210	14901.142181	29.507559
390.017429	14914.235245	29.512576
390.352882	14943.156774	29.517594
390.873289	14958.413822	29.522612
391.325314	14982.694916	29.527629
391.641740	15014.653774	29.532647
392.245444	15030.239268	29.537664
392.565365	15051.992758	29.542682
392.913365	15077.884961	29.547700
393.707691	15085.972819	29.552717
393.801636	15125.808879	29.557735
394.003183	15146.340923	29.562752
394.589159	15171.606438	29.567770
394.882115	15193.686494	29.572788
395.361745	15201.960841	29.577805
395.693711	15246.015861	29.582823
395.909613	15260.773633	29.587840
396.179537	15300.555761	29.592858
396.658733	15326.694839	29.597876
397.099407	15351.006373	29.602893
397.321075	15382.828575	29.607911
398.155127	15405.706280	29.612928
398.306891	15436.568596	29.617946
398.406007	15457.520043	29.622964
399.139617	15481.487048	29.627981
399.266054	15524.927632	29.632999
400.089196	15541.012132	29.638016
400.538789	15554.286126	29.643034
400.691119	15583.067508	29.648052
401.282209	15615.373637	29.653069
401.456148	15651.956915	29.658087
401.962750	15680.829248	29.663104
402.496836	15709.831677	29.668122
402.988082	15734.949669	29.673140
403.267511	15757.898656	29.678157
403.467834	15783.995467	29.683175
403.940418	15821.423608	29.688192
404.751122	15839.200419	29.693210
404.596614	15868.502488	29.698228
405.198434	15898.094559	29.703245
405.661599	15928.918484	29.708263
406.245990	15950.526215	29.713280
406.521684	15977.917393	29.718298
406.949730	15993.158605	29.723316
407.828741	16016.813381	29.728333
407.970281	16045.985368	29.733351
408.509292	16072.480493	29.738368
408.738262	16080.986068	29.743386
408.876176	16113.197371	29.748404
409.416914	16122.336932	29.753421
409.522954	16141.413059	29.758439
410.388405	16164.755223	29.763456
410.924201	16188.765092	29.768474
411.065770	16204.384087	29.773492
411.708803	16224.409618	29.778509
411.847443	16256.754350	29.783527
412.298681	16276.200573	29.788544
412.819712	16289.421510	29.793562
413.053462	16321.411618	29.798580
413.659845	16333.094548	29.803597
413.854075	16357.391640	29.808615
414.345889	16380.488203	29.813632
414.792852	16402.738937	29.818650
414.865064	16426.387775	29.823668
415.378052	16453.039944	29.828685
415.449874	16489.567384	29.833703
415.673451	16507.490577	29.838720
415.959843	16540.822443	29.843738
416.371718	16583.071802	29.848756
416.869367	16610.857815	29.853773
417.628915	16643.607706	29.858791
417.685177	16674.223982	29.863808
418.343427	16713.020970	29.868826
418.492024	16748.723327	29.873844
419.380206	16762.290747	29.878861
419.526802	16813.313467	29.883879
420.163332	16840.801035	29.888896
421.300957	16869.630282	29.893914
421.208252	16906.019588	29.898932
421.679071	16924.109558	29.903949
422.241477	16960.709540	29.908967
422.645578	16981.595087	29.913984
423.116806	17000.301538	29.919002
423.580416	17031.782839	29.924020
424.136699	17056.785070	29.929037
424.325385	17082.135832	29.934055
424.760884	17100.922696	29.939072
425.389257	17122.378733	29.944090
425.477697	17155.856447	29.949108
426.162996	17188.137692	29.954125
426.608300	17212.967525	29.959143
427.072027	17235.689970	29.964160
427.323014	17260.038689	29.969178
427.576744	17297.434436	29.974196
427.894556	17315.150663	29.979213
428.097754	17357.843027	29.984231
428.608811	17380.131811	29.989248
429.501412	17422.746604	29.994266
429.662258	17448.512993	29.999284
430.067706	17489.512636	30.004301
430.624574	17521.045821	30.009319
431.271304	17545.454175	30.014336
431.641364	17549.147871	30.019354
431.745294	17583.739888	30.024372
432.431152	17618.914214	30.029389
432.575105	17646.933235	30.034407
432.907680	17654.589488	30.039424
433.330717	17692.303677	30.044442
433.814541	17726.393989	30.049460
434.157728	17743.782086	30.054477
434.554096	17773.985952	30.059495
435.283569	17792.253043	30.064512
435.958188	17818.679481	30.069530
435.860966	17848.383825	30.074548
436.864051	17871.141351	30.079565
437.451888	17890.205872	30.084583
437.343203	17927.443966	30.089600
437.879405	17954.702282	30.094618
438.134377	17989.022535	30.099636
438.732179	18002.830028	30.104653
439.282521	18039.393748	30.109671
439.800849	18071.626679	30.114688
440.241616	18096.030729	30.119706
440.539841	18117.665942	30.124724
441.046065	18142.439144	30.129741
441.484893	18175.932925	30.134759
441.832587	18206.187121	30.139776
442.652649	18231.044713	30.144794
442.427753	18272.308263	30.149812
442.924827	18302.353423	30.154829
443.562221	18341.003508	30.159847
443.665614	18366.594365	30.164864
444.436891	18392.881985	30.169882
444.597555	18433.703450	30.174900
445.608822	18461.374560	30.179917
445.712108	18504.335994	30.184935
445.968396	18520.711673	30.189952
446.708475	18558.651474	30.194970
447.017713	18599.263883	30.199988
447.417772	18628.854672	30.205005
447.972026	18652.176974	30.210023
448.475203	18691.444580	30.215040
448.930287	18723.699181	30.220058
449.356468	18760.421784	30.225076
450.018829	18780.955832	30.230093
450.623197	18800.877499	30.235111
450.725322	18833.316115	30.240128
451.226610	18868.088834	30.245146
451.673635	18899.051389	30.250164
452.075308	18932.363748	30.255181
452.843447	18961.025667	30.260199
452.947111	18988.678925	30.265216
453.991606	19020.182763	30.270234
454.137207	19044.519582	30.275252
454.811548	19061.689082	30.280269
455.365928	19098.390095	30.285287
455.798815	19118.840282	30.290304
456.454484	19143.421593	30.295322
456.670138	19155.028766	30.300340
456.763900	19180.483126	30.305357
456.847089	19208.437285	30.310375
457.588753	19231.782576	30.315392
457.909776	19257.041799	30.320410
457.772481	19292.132950	30.325428
458.279058	19317.706420	30.330445
459.051041	19356.580517	30.335463
459.261563	19399.322216	30.340480
460.027660	19436.061560	30.345498
460.240581	19464.111263	30.350516
460.787659	19498.392650	30.355533
461.428245	19531.116245	30.360551
461.980891	19570.490796	30.365568
462.724938	19587.812383	30.370586
463.109672	19625.950386	30.375604
463.515119	19646.228466	30.380621
464.005752	19662.808582	30.385639
464.647745	19706.945843	30.390656
464.900383	19741.202620	30.395674
465.230580	19768.570375	30.400692
465.996540	19796.968427	30.405709
466.622628	19824.658062	30.410727
466.782300	19858.426728	30.415744
467.296298	19882.646325	30.420762
467.510905	19919.222288	30.425780
468.019887	19951.045234	30.430797
468.793851	19988.237811	30.435815
468.912440	20008.051002	30.440832
469.342734	20042.335262	30.445850
469.781977	20071.666632	30.450868
470.554088	20120.287812	30.455885
470.823626	20151.083876	30.460903
471.070138	20188.497972	30.465920
472.128431	20217.762502	30.470938
472.275640	20251.989159	30.475956
472.679098	20288.846954	30.480973
473.127461	20324.045568	30.485991
473.511480	20364.548298	30.491008
474.014167	20393.654793	30.496026
474.610134	20436.313913	30.501044
475.149623	20466.211214	30.506061
475.758375	20489.506730	30.511079
475.925459	20536.649054	30.516096
476.508983	20566.215483	30.521114
476.984303	20601.157252	30.526132
477.729549	20643.840408	30.531149
478.489376	20661.979670	30.536167
478.321872	20697.332355	30.541184
478.941933	20733.018771	30.546202
479.767894	20767.746377	30.551220
479.764458	20792.988506	30.556237
480.464501	20834.116600	30.561255
480.706779	20876.747033	30.566272
481.398312	20893.899683	30.571290
481.732670	20934.698450	30.576308
482.314909	20963.793337	30.581325
483.152859	20985.308370	30.586343
483.349921	21009.174246	30.591360
483.940650	21022.958792	30.596378
484.397597	21056.279093	30.601396
484.904059	21073.586637	30.606413
485.428956	21112.139072	30.611431
485.299479	21153.787994	30.616448
486.206473	21165.377891	30.621466
486.604186	21202.406101	30.626484
486.450434	21239.035163	30.631501
487.146735	21282.203126	30.636519
487.160519	21328.070480	30.641536
487.622623	21369.577306	30.646554
488.537462	21418.481806	30.651572
488.647600	21474.486631	30.656589
489.188993	21497.904243	30.661607
489.736183	21555.570729	30.666624
490.686473	21585.207062	30.671642
491.141645	21622.485028	30.676660
491.360892	21675.457713	30.681677
492.395555	21702.673324	30.686695
492.883234	21736.196116	30.691712
493.540599	21768.337376	30.696730
494.175323	21806.511754	30.701748
494.673249	21841.730299	30.706765
495.733562	21871.924561	30.711783
495.465377	21902.428153	30.716800
496.359165	21934.137531	30.721818
496.943078	21957.113540	30.726836
497.063197	21996.780859	30.731853
497.754179	22023.510725	30.736871
498.139022	22057.964937	30.741888
498.569865	22090.345342	30.746906
499.401596	22118.987197	30.751924
499.735182	22153.656912	30.756941
500.453043	22188.860893	30.761959
500.522473	22221.732297	30.766976
500.959483	22244.780957	30.771994
501.477873	22279.772768	30.777012
501.885933	22319.641544	30.782029
502.413639	22356.507249	30.787047
502.754114	22400.423305	30.792064
503.197590	22438.276061	30.797082
503.724946	22486.746288	30.802100
504.040494	22530.321717	30.807117
505.025933	22554.818471	30.812135
504.858164	22607.739375	30.817152
505.303994	22649.415990	30.822170
505.800967	22689.835451	30.827188
506.499613	22733.306314	30.832205
507.282339	22777.260875	30.837223
507.773767	22817.487799	30.842240
508.658083	22851.388481	30.847258
509.420582	22873.138663	30.852276
509.896768	22906.963494	30.857293
510.680989	22917.946149	30.862311
510.850886	22957.219666	30.867328
511.020289	22983.718416	30.872346
512.003175	23019.542842	30.877364
512.029774	23053.383678	30.882381
512.669502	23075.513633	30.887399
512.869997	23121.303296	30.892416
513.473761	23152.436756	30.897434
513.738685	23184.222836	30.902452
514.212825	23221.171556	30.907469
514.787820	23261.475302	30.912487
514.810588	23307.270183	30.917504
515.415626	23340.175169	30.922522
515.956422	23381.888211	30.927540
516.374063	23439.285291	30.932557
517.191482	23470.118342	30.937575
517.648212	23516.252697	30.942592
518.058886	23562.081832	30.947610
518.777950	23603.003059	30.952628
519.069813	23666.540133	30.957645
519.851342	23690.296103	30.962663
520.194342	23751.365575	30.967680
520.655318	23788.624897	30.972698
521.555913	23821.362511	30.977716
521.790805	23880.234051	30.982733
522.345109	23918.740628	30.987751
523.134729	23963.468504	30.992768
523.716818	24004.154236	30.997786
524.429192	24044.194709	31.002804
524.682754	24088.315182	31.007821
525.361461	24126.497625	31.012839
525.984969	24169.617358	31.017856
526.415177	24216.637008	31.022874
526.994051	24257.298696	31.027892
527.140392	24294.179254	31.032909
527.698738	24325.367943	31.037927
528.327677	24377.494392	31.042944
528.580690	24426.148162	31.047962
529.405811	24471.257779	31.052980
529.996076	24518.047243	31.057997
530.675306	24551.792050	31.063015
531.312087	24599.439221	31.068032
531.621330	24635.463617	31.073050
532.631278	24673.574139	31.078068
532.999712	24714.613949	31.083085
533.419495	24747.950726	31.088103
533.938819	24796.494683	31.093120
534.270149	24840.875824	31.098138
534.884338	24876.048745	31.103156
535.370952	24920.050910	31.108173
536.112088	24947.360643	31.113191
536.454894	24991.581261	31.118208
536.792287	25036.626803	31.123226
537.598267	25069.006333	31.128244
537.666379	25122.361997	31.133261
538.052048	25154.529008	31.138279
538.895788	25210.879983	31.143296
539.267830	25245.252584	31.148314
539.944427	25291.672951	31.153332
540.072373	25340.463651	31.158349
541.026047	25377.853036	31.163367
541.329954	25421.999119	31.168384
541.489491	25468.433032	31.173402
542.457776	25515.677245	31.178420
542.890037	25569.514423	31.183437
543.435111	25602.472251	31.188455
544.410811	25649.573889	31.193472
544.715204	25695.457608	31.198490
545.513309	25738.619169	31.203508
545.947893	25779.113943	31.208525
546.631595	25812.366012	31.213543
547.720637	25850.126456	31.218560
547.932398	25906.000761	31.223578
548.571013	25937.477596	31.228596
549.136423	25976.558505	31.233613
549.553696	26016.243678	31.238631
549.809447	26055.901895	31.243648
550.407249	26102.492358	31.248666
551.316641	26133.295460	31.253684
551.725667	26191.638118	31.258701
552.445701	26225.238967	31.263719
553.046683	26255.959869	31.268736
553.065962	26299.685773	31.273754
553.735066	26330.515709	31.278772
554.537381	26384.604713	31.283789
555.123995	26426.040358	31.288807
555.742753	26469.209613	31.293824
556.087154	26502.489586	31.298842
556.260586	26546.353893	31.303860
556.586384	26616.433523	31.308877
557.437420	26653.313645	31.313895
558.027535	26695.617569	31.318912
558.632483	26754.811031	31.323930
559.185136	26799.761870	31.328948
559.570915	26851.548321	31.333965
560.416495	26899.184859	31.338983
560.623927	26945.666631	31.344000
561.138869	26997.336870	31.349018
562.221942	27041.872246	31.354036
562.972707	27095.427486	31.359053
563.502508	27131.980936	31.364071
564.152294	27166.333914	31.369088
564.795920	27223.555782	31.374106
565.310815	27259.334325	31.379124
565.849300	27296.275160	31.384141
566.251098	27342.273341	31.389159
566.870387	27384.723333	31.394176
567.431001	27427.509730	31.399194
568.229024	27466.095562	31.404212
568.530117	27501.083053	31.409229
569.050222	27536.371355	31.414247
569.585226	27571.230357	31.419264
569.985402	27617.246127	31.424282
570.689941	27653.572039	31.429300
571.179378	27688.593756	31.434317
571.387208	27735.734013	31.439335
572.429941	27772.635817	31.444352
572.556811	27828.039499	31.449370
573.233838	27865.477190	31.454388
573.954323	27923.187224	31.459405
574.567237	27964.283089	31.464423
575.347871	27999.761757	31.469440
575.544087	28052.207814	31.474458
576.194974	28083.758608	31.479476
576.739254	28130.445418	31.484493
577.349603	28174.217791	31.489511
577.645492	28214.663587	31.494528
578.438691	28274.191136	31.499546
579.390336	28313.869367	31.504564
579.707378	28364.102199	31.509581
580.159553	28407.657732	31.514599
581.244853	28449.068812	31.519616
581.284777	28500.898311	31.524634
582.078476	28552.322722	31.529652
582.496178	28605.064633	31.534669
582.758291	28652.417162	31.539687
583.699488	28699.363863	31.544704
583.859871	28750.762125	31.549722
584.750586	28800.392826	31.554740
585.297763	28857.511367	31.559757
585.790876	28911.658898	31.564775
586.981222	28956.385775	31.569792
587.007986	29017.087597	31.574810
587.779611	29062.644137	31.579828
588.665978	29106.601997	31.584845
589.173114	29160.439268	31.589863
589.756762	29205.391093	31.594880
590.272877	29259.165805	31.599898
590.919533	29299.705005	31.604916
591.561793	29344.449327	31.609933
591.722074	29396.021416	31.614951
592.643691	29443.209771	31.619968
593.400603	29496.348104	31.624986
593.601471	29540.564436	31.630004
594.255465	29602.002183	31.635021
594.825943	29662.025729	31.640039
595.307564	29701.654576	31.645056
595.987066	29771.214075	31.650074
596.762371	29816.201683	31.655092
597.417699	29869.492939	31.660109
597.934500	29919.816970	31.665127
598.791238	29968.173888	31.670144
599.305780	30014.546232	31.675162
599.707216	30053.882983	31.680180
600.639404	30083.914692	31.685197
601.287212	30141.248656	31.690215
601.867763	30176.217126	31.695232
602.247029	30219.625241	31.700250
602.814618	30259.474995	31.705268
603.278313	30311.546936	31.710285
603.497003	30360.780408	31.715303
604.137553	30395.911572	31.720320
604.750156	30458.626197	31.725338
605.549133	30514.589975	31.730356
606.079547	30562.798907	31.735373
606.305883	30615.220077	31.740391
606.924340	30664.160715	31.745408
607.488231	30710.875471	31.750426
608.305726	30765.880552	31.755444
609.188685	30827.530740	31.760461
609.371687	30890.246092	31.765479
610.318876	30941.957800	31.770496
610.790085	30990.073407	31.775514
611.427781	31060.351111	31.780532
612.475682	31114.542135	31.785549
612.957694	31157.376903	31.790567
613.640313	31210.059860	31.795584
614.089983	31273.602601	31.800602
614.945997	31324.456926	31.805620
615.404321	31361.359119	31.810637
615.865942	31420.341080	31.815655
617.043198	31463.187294	31.820672
617.512832	31512.497750	31.825690
618.084673	31565.702251	31.830708
618.868329	31614.245907	31.835725
619.679594	31671.422103	31.840743
620.561084	31720.654994	31.845760
620.972264	31758.872147	31.850778
621.408664	31803.183186	31.855796
621.788757	31846.664840	31.860813
622.105989	31901.707700	31.865831
623.214448	31945.505480	31.870848
623.591331	32001.243685	31.875866
623.862090	32071.327255	31.880884
624.489844	32118.623747	31.885901
624.852185	32175.480738	31.890919
625.855279	32226.353849	31.895936
625.955087	32294.558499	31.900954
626.851277	32358.508753	31.905972
628.311216	32402.719898	31.910989
628.560040	32470.367242	31.916007
629.412566	32516.814229	31.921024
630.039577	32577.586573	31.926042
630.541625	32625.861262	31.931060
631.235523	32673.911678	31.936077
632.053753	32735.428049	31.941095
632.556919	32785.715785	31.946112
633.305545	32829.629969	31.951130
633.786050	32872.412715	31.956148
634.585652	32904.333772	31.961165
634.770337	32957.182016	31.966183
635.369202	33000.333988	31.971200
636.019475	33051.754456	31.976218
636.583303	33095.079332	31.981236
637.376402	33149.186839	31.986253
637.421162	33201.123458	31.991271
638.348641	33249.794064	31.996288
638.709459	33312.715745	32.001306
639.301294	33367.779678	32.006324
640.264137	33421.969812	32.011341
640.455408	33493.162834	32.016359
641.139752	33544.697631	32.021376
642.020391	33601.606267	32.026394
642.359191	33664.674655	32.031412
643.273314	33722.560379	32.036429
643.905460	33791.663729	32.041447
644.743260	33845.813692	32.046464
645.110985	33919.225051	32.051482
645.690721	33971.744093	32.056500
646.528263	34026.304520	32.061517
646.915558	34093.460426	32.066535
647.792648	34159.502990	32.071552
648.633024	34218.407869	32.076570
649.328561	34273.978488	32.081588
650.108197	34330.147512	32.086605
650.595670	34387.093081	32.091623
651.446174	34445.451750	32.096640
651.887655	34505.620746	32.101658
652.452214	34566.413506	32.106676
653.530287	34617.271034	32.111693
654.019104	34680.819102	32.116711
654.413107	34752.622096	32.121728
655.169545	34813.214963	32.126746
656.007678	34860.823162	32.131764
656.570095	34929.814676	32.136781
657.274710	34991.395369	32.141799
658.178377	35046.828247	32.146816
659.008265	35106.958072	32.151834
659.406926	35171.729883	32.156852
660.557303	35217.765022	32.161869
661.058605	35272.288505	32.166887
661.756001	35320.226252	32.171904
662.491177	35376.172590	32.176922
662.897546	35439.131343	32.181940
663.481146	35498.236139	32.186957
663.846886	35557.514559	32.191975
664.486638	35604.179091	32.196992
665.198121	35664.041295	32.202010
665.436037	35736.034178	32.207028
666.483345	35793.051494	32.212045
667.026989	35861.017281	32.217063
667.600514	35919.412617	32.222080
668.479508	35976.641807	32.227098
669.347188	36043.637666	32.232116
669.799389	36081.509878	32.237133
670.139647	36146.187573	32.242151
671.088881	36205.359626	32.247168
671.941912	36247.795392	32.252186
672.284776	36314.689872	32.257204
673.383761	36374.751476	32.262221
673.768941	36430.476459	32.267239
674.346154	36480.872388	32.272256
675.125132	36543.205281	32.277274
675.590415	36608.074532	32.282292
676.284857	36664.309145	32.287309
676.797355	36730.285960	32.292327
677.641717	36789.609210	32.297344
678.413905	36841.334162	32.302362
678.453429	36918.478041	32.307380
679.253922	36966.722570	32.312397
680.409286	37037.490308	32.317415
680.783710	37114.472984	32.322432
681.461811	37179.504482	32.327450
682.251982	37233.569004	32.332468
683.451245	37296.966624	32.337485
683.834838	37367.458176	32.342503
684.551406	37428.409011	32.347520
685.640830	37490.811096	32.352538
685.823862	37552.454320	32.357556
686.461736	37616.915299	32.362573
687.458228	37701.946452	32.367591
688.098689	37756.345513	32.372608
689.111464	37805.644961	32.377626
689.560175	37863.693283	32.382644
690.555735	37932.937249	32.387661
690.930961	37998.904640	32.392679
691.700498	38056.003853	32.397696
692.855627	38106.374147	32.402714
693.055524	38181.885353	32.407732
693.837060	38235.601301	32.412749
694.692408	38299.391718	32.417767
695.202529	38359.242004	32.422784
695.913893	38426.947098	32.427802
696.536673	38494.657107	32.432820
697.610493	38543.922199	32.437837
697.977031	38600.923441	32.442855
698.820733	38671.321970	32.447872
699.655836	38730.128501	32.452890
699.890175	38800.268240	32.457908
701.092876	38858.717118	32.462925
701.438584	38917.742545	32.467943
701.871591	38987.342143	32.472960
702.648639	39056.564020	32.477978
702.994399	39124.137750	32.482996
703.980339	39188.420030	32.488013
704.568230	39265.957216	32.493031
705.480185	39332.758896	32.498048
706.148849	39390.134122	32.503066
706.467253	39464.690844	32.508084
707.631788	39518.260023	32.513101
708.143292	39576.099249	32.518119
708.469731	39638.490422	32.523136
709.185132	39697.735653	32.528154
709.721353	39769.859127	32.533172
710.676425	39837.892163	32.538189
711.283594	39913.363595	32.543207
711.608735	39987.587251	32.548224
712.783168	40054.558133	32.553242
713.682023	40131.448991	32.558260
714.396670	40193.114966	32.563277
714.953003	40247.117570	32.568295
715.500638	40331.542744	32.573312
716.280434	40399.197522	32.578330
717.160774	40488.171842	32.583348
718.040004	40539.425915	32.588365
718.825785	40612.815750	32.593383
719.005201	40683.721036	32.598400
719.835768	40738.526764	32.603418
720.585566	40827.044255	32.608436
721.528498	40906.210245	32.613453
722.334360	40972.611073	32.618471
723.369050	41043.323352	32.623488
724.092571	41111.336845	32.628506
724.904036	41176.663676	32.633524
725.885193	41241.071186	32.638541
726.419205	41310.498632	32.643559
727.049388	41372.161822	32.648576
728.034240	41427.303177	32.653594
728.554288	41506.816822	32.658612
729.516218	41574.537159	32.663629
730.017422	41630.882134	32.668647
730.754624	41710.251765	32.673664
731.697281	41771.478710	32.678682
732.128111	41840.855347	32.683700
732.989158	41902.578319	32.688717
733.492150	41974.713254	32.693735
734.024401	42053.019490	32.698752
735.193435	42121.103281	32.703770
735.536063	42199.733702	32.708788
736.489524	42264.354492	32.713805
737.303940	42333.959084	32.718823
737.971100	42413.589144	32.723840
738.781074	42483.778564	32.728858
739.323855	42549.863092	32.733876
740.258326	42616.204092	32.738893
740.981400	42687.512137	32.743911
741.207810	42766.110028	32.748928
742.743340	42837.011794	32.753946
743.190790	42914.527979	32.758964
743.761898	42975.909844	32.763981
744.511246	43059.179259	32.768999
745.101893	43134.080845	32.774016
746.004030	43197.741806	32.779034
746.809838	43274.325677	32.784052
747.463648	43328.686809	32.789069
748.224818	43392.847231	32.794087
748.468620	43456.203883	32.799104
749.306568	43518.608212	32.804122
750.115907	43596.035157	32.809140
750.917158	43683.261183	32.814157
751.483003	43746.514012	32.819175
752.221557	43815.414321	32.824192
753.039887	43887.872986	32.829210
753.777574	43975.347185	32.834228
754.881644	44043.594036	32.839245
755.543640	44111.488833	32.844263
755.852480	44197.057737	32.849280
756.714771	44269.469996	32.854298
757.459667	44346.058852	32.859316
758.417614	44420.159936	32.864333
759.451240	44502.804324	32.869351
760.238910	44587.295800	32.874368
760.921688	44647.154811	32.879386
761.577835	44714.106540	32.884404
762.153373	44784.926233	32.889421
763.180350	44872.765854	32.894439
764.062428	44953.471212	32.899456
765.218482	45008.391754	32.904474
765.762683	45098.381938	32.909492
766.408642	45174.649504	32.914509
767.475998	45250.645276	32.919527
768.196078	45324.277034	32.924544
768.820980	45384.419101	32.929562
769.797096	45457.001172	32.934580
770.189989	45537.253965	32.939597
771.320432	45610.121271	32.944615
771.419014	45685.361434	32.949632
772.669840	45765.592289	32.954650
773.444266	45837.015557	32.959668
774.117728	45920.960685	32.964685
774.787769	45986.684742	32.969703
775.219282	46079.912654	32.974720
776.478402	46145.171278	32.979738
777.237357	46225.286944	32.984756
777.746709	46304.092436	32.989773
779.079641	46378.306234	32.994791
779.285051	46472.827861	32.999808
780.523565	46537.334065	33.004826
781.392906	46620.279673	33.009844
782.035570	46705.366079	33.014861
782.527642	46772.187778	33.019879
783.203431	46852.685526	33.024896
784.069856	46932.686369	33.029914
784.678033	47021.991661	33.034932
785.431891	47091.426236	33.039949
786.536247	47176.924157	33.044967
787.167486	47268.274623	33.049984
788.011692	47342.551375	33.055002
788.916087	47419.292410	33.060020
789.849481	47482.913622	33.065037
790.668332	47546.345062	33.070055
791.480010	47615.722029	33.075072
792.432420	47677.671887	33.080090
792.776601	47754.216441	33.085108
793.711377	47818.251966	33.090125
794.736638	47889.381812	33.095143
795.091328	47967.266546	33.100160
796.008207	48030.103585	33.105178
797.061881	48107.505380	33.110196
797.422329	48176.678726	33.115213
798.407846	48253.849064	33.120231
799.009862	48335.349766	33.125248
799.826088	48409.013903	33.130266
800.697997	48491.977410	33.135284
801.216663	48575.313054	33.140301
802.442423	48636.061652	33.145319
803.296301	48711.866635	33.150336
803.743765	48800.812124	33.155354
804.731492	48872.248510	33.160372
805.115445	48961.302728	33.165389
805.957150	49039.559578	33.170407
806.423245	49133.568074	33.175424
807.528926	49214.882233	33.180442
808.690200	49305.647729	33.185460
809.419804	49392.339367	33.190477
810.513408	49472.274571	33.195495
811.089426	49563.680422	33.200512
811.863395	49644.800073	33.205530
812.511368	49730.723809	33.210548
813.140858	49815.076326	33.215565
814.514690	49904.318525	33.220583
815.271115	49996.029214	33.225600
816.232822	50067.591320	33.230618
816.966277	50144.822650	33.235636
817.631042	50237.391697	33.240653
818.777314	50309.127356	33.245671
819.806069	50411.027149	33.250688
820.435635	50490.393902	33.255706
821.440059	50567.552386	33.260724
822.119373	50646.744671	33.265741
823.171923	50728.658014	33.270759
823.370608	50818.719802	33.275776
824.339676	50890.318759	33.280794
825.609847	50980.270792	33.285812
826.131796	51064.965069	33.290829
827.111518	51146.958194	33.295847
827.673359	51226.689284	33.300864
828.456162	51310.611085	33.305882
829.248671	51388.463240	33.310900
830.110002	51476.684068	33.315917
830.951812	51552.581989	33.320935
831.625041	51648.473726	33.325952
832.870992	51734.558106	33.330970
833.552489	51810.542595	33.335988
834.004374	51895.438146	33.341005
835.465859	51961.938948	33.346023
835.988853	52046.350521	33.351040
836.444673	52117.284981	33.356058
837.508819	52186.750101	33.361076
838.410774	52281.927155	33.366093
839.192011	52362.164886	33.371111
839.700226	52451.118918	33.376128
840.543332	52529.469771	33.381146
841.413906	52600.728316	33.386164
842.128547	52707.933230	33.391181
842.965962	52779.522826	33.396199
843.577494	52868.525599	33.401216
844.596821	52960.995499	33.406234
845.518696	53047.030449	33.411252
845.936182	53147.749124	33.416269
847.102773	53236.564387	33.421287
847.838736	53328.775132	33.426304
849.226074	53427.115984	33.431322
849.847232	53519.462749	33.436340
850.476168	53613.588806	33.441357
851.653517	53694.801493	33.446375
852.648606	53793.276199	33.451392
853.513602	53879.283139	33.456410
854.548233	53969.650603	33.461428
855.410412	54060.563581	33.466445
856.359504	54137.541073	33.471463
857.355377	54229.339460	33.476480
858.001433	54314.234437	33.481498
858.753255	54405.327677	33.486516
859.640004	54487.417113	33.491533
860.395006	54585.423016	33.496551
861.371051	54683.271177	33.501568
862.225511	54768.075143	33.506586
863.139445	54850.935199	33.511604
864.142209	54939.775432	33.516621
865.058104	55032.016717	33.521639
865.644221	55122.713813	33.526656
866.519833	55211.891249	33.531674
867.740236	55300.234617	33.536692
867.856184	55416.534031	33.541709
869.108916	55497.221986	33.546727
869.930371	55589.578976	33.551744
870.713806	55679.130050	33.556762
871.716503	55771.866309	33.561780
872.792868	55868.906285	33.566797
873.402383	55947.025014	33.571815
874.737824	56054.769609	33.576832
875.501778	56140.591841	33.581850
876.512529	56224.885295	33.586868
876.915352	56320.254535	33.591885
877.736181	56417.956785	33.596903
878.737386	56503.177930	33.601920
879.524425	56600.921257	33.606938
880.575727	56684.866302	33.611956
881.168052	56768.742718	33.616973
882.642817	56850.496695	33.621991
883.275660	56938.357500	33.627008
883.793537	57020.368672	33.632026
884.847158	57083.591305	33.637044
885.554108	57191.755120	33.642061
886.285817	57264.263102	33.647079
887.518183	57348.346526	33.652096
888.008952	57453.578910	33.657114
889.103661	57549.561033	33.662132
889.549530	57642.057588	33.667149
890.884277	57722.758098	33.672167
891.827093	57811.517648	33.677184
892.332563	57925.952634	33.682202
893.497825	58014.374705	33.687220
894.251212	58110.840246	33.692237
894.989597	58212.160874	33.697255
896.301483	58303.541140	33.702272
896.996048	58402.827246	33.707290
897.983310	58489.066888	33.712308
898.850923	58593.188221	33.717325
899.885811	58697.940181	33.722343
900.458628	58797.958107	33.727360
901.443786	58902.845421	33.732378
902.674106	58989.645405	33.737396
903.513918	59100.792160	33.742413
904.692266	59184.965170	33.747431
905.845000	59282.064680	33.752448
906.490014	59373.259576	33.757466
907.406380	59462.811075	33.762484
908.285916	59568.091502	33.767501
909.497216	59657.912729	33.772519
910.175046	59745.053577	33.777536
910.952880	59844.109992	33.782554
912.354748	59932.626715	33.787572
912.996920	60042.983364	33.792589
913.791559	60130.792554	33.797607
915.110798	60216.270712	33.802624
915.800898	60316.941179	33.807642
916.628692	60405.115789	33.812660
917.386409	60506.347990	33.817677
918.615061	60601.468990	33.822695
919.367910	60694.677051	33.827712
919.946032	60794.821690	33.832730
921.380563	60897.533321	33.837748
921.866061	60993.090297	33.842765
922.573900	61104.566804	33.847783
923.643640	61208.017028	33.852800
924.681173	61304.769679	33.857818
925.618251	61405.709827	33.862836
926.487993	61510.614404	33.867853
927.510926	61607.320421	33.872871
928.608954	61716.705056	33.877888
929.127303	61813.113514	33.882906
930.209811	61894.222783	33.887924
931.279119	61993.496815	33.892941
932.152565	62077.431427	33.897959
932.782120	62173.148316	33.902976
933.849425	62261.303030	33.907994
934.971528	62345.401364	33.913012
935.417091	62448.506195	33.918029
936.568071	62540.071787	33.923047
937.585499	62628.592974	33.928064
938.223418	62727.102729	33.933082
939.485664	62835.798316	33.938100
940.107321	62924.418595	33.943117
940.689704	63038.623222	33.948135
941.997966	63144.875492	33.953152
942.612492	63246.170503	33.958170
943.947290	63349.261926	33.963188
944.661306	63452.818984	33.968205
945.483179	63560.139367	33.973223
946.778380	63670.220798	33.978240
947.423471	63775.830555	33.983258
948.592013	63890.929161	33.988276
949.404188	64004.348317	33.993293
950.246298	64105.734872	33.998311
951.363250	64214.524655	34.003328
952.163342	64320.987532	34.008346
953.203617	64423.212692	34.013364
953.947094	64544.528298	34.018381
955.454487	64657.752322	34.023399
956.685615	64761.430043	34.028416
957.667107	64880.597204	34.033434
958.534696	64975.548243	34.038452
959.545459	65088.023268	34.043469
960.455247	65193.093487	34.048487
961.569791	65304.441626	34.053504
962.123359	65408.795966	34.058522
963.139694	65501.152076	34.063540
964.300028	65622.133456	34.068557
965.490439	65735.812243	34.073575
966.487396	65834.126230	34.078592
967.053803	65948.063461	34.083610
968.145312	66051.833567	34.088628
969.253092	66160.582218	34.093645
970.286857	66261.172804	34.098663
971.424763	66372.431851	34.103680
972.355514	66480.430381	34.108698
972.865525	66578.051864	34.113716
974.164566	66693.250836	34.118733
975.220404	66804.888654	34.123751
976.224895	66896.845945	34.128768
977.057289	67006.454900	34.133786
978.132603	67120.090713	34.138804
978.984965	67221.062606	34.143821
979.887356	67333.864938	34.148839
981.294411	67437.317541	34.153856
981.878807	67544.473818	34.158874
983.370833	67627.203750	34.163892
984.327413	67725.830735	34.168909
985.038685	67817.257897	34.173927
986.044074	67905.511744	34.178944
986.639326	68021.557082	34.183962
987.948901	68100.654137	34.188980
988.905323	68197.723218	34.193997
989.703297	68292.973365	34.199015
991.164382	68390.019982	34.204032
991.745959	68490.416176	34.209050
992.774515	68578.827340	34.214068
993.707836	68692.441288	34.219085
994.799596	68793.111659	34.224103
995.603845	68886.935997	34.229120
996.687151	68991.184391	34.234138
997.165983	69117.697531	34.239156
998.155644	69215.739307	34.244173
998.925163	69331.979546	34.249191
999.692918	69447.197310	34.254208
1000.681978	69583.209769	34.259226
1001.863275	69703.840651	34.264244
1002.999106	69824.252073	34.269261
1003.559460	69950.106916	34.274279
1005.336859	70060.650499	34.279296
1005.990115	70204.377859	34.284314
1006.884959	70299.919351	34.289332
1008.283451	70431.014144	34.294349
1009.021423	70564.912650	34.299367
1010.207337	70673.734221	34.304384
1011.272585	70796.285695	34.309402
1012.076644	70920.812810	34.314420
1013.234060	71061.749486	34.319437
1013.908923	71174.660808	34.324455
1015.373529	71285.330564	34.329472
1016.274652	71414.672455	34.334490
1017.302461	71529.222952	34.339508
1018.486665	71660.511679	34.344525
1019.189798	71789.274648	34.349543
1020.670693	71911.779591	34.354560
1021.612272	72041.611994	34.359578
1022.582294	72156.137413	34.364596
1023.788013	72279.598270	34.369613
1024.480388	72408.044738	34.374631
1026.102713	72524.383049	34.379648
1027.103206	72644.030813	34.384666
1027.863994	72766.383900	34.389684
1029.015575	72884.296727	34.394701
1030.181000	73005.942421	34.399719
1031.063084	73119.242610	34.404736
1032.045797	73248.608793	34.409754
1033.172988	73368.967438	34.414772
1034.577018	73485.346115	34.419789
1035.262263	73603.090951	34.424807
1036.583746	73718.024450	34.429824
1037.410775	73832.089412	34.434842
1038.190224	73950.965057	34.439860
1039.173096	74042.523345	34.444877
1040.431083	74160.508964	34.449895
1041.437911	74270.124467	34.454912
1042.678951	74373.693795	34.459930
1043.380641	74474.619556	34.464948
1044.458814	74594.709038	34.469965
1045.270030	74716.149791	34.474983
1046.431017	74814.508101	34.480000
1047.412328	74928.289371	34.485018
1047.964826	75046.013269	34.490036
1048.913072	75179.043724	34.495053
1050.033727	75294.113025	34.500071
1051.144431	75418.101369	34.505088
1051.997880	75562.676196	34.510106
1053.157439	75692.933764	34.515124
1054.256556	75806.739192	34.520141
1055.038986	75939.175409	34.525159
1056.433299	76062.636003	34.530176
1057.492610	76204.692737	34.535194
1058.336142	76327.319874	34.540212
1059.879274	76458.747422	34.545229
1061.038515	76601.334558	34.550247
1062.268847	76720.199121	34.555264
1063.305257	76857.517846	34.560282
1064.405881	76975.355429	34.565300
1065.519379	77103.341595	34.570317
1066.315549	77236.687890	34.575335
1067.531054	77362.662331	34.580352
1068.611050	77488.349421	34.585370
1069.254662	77619.466205	34.590388
1070.714474	77748.292504	34.595405
1071.985711	77870.785115	34.600423
1073.036667	78001.631007	34.605440
1074.195704	78136.695176	34.610458
1075.010284	78268.174486	34.615476
1076.370339	78387.078743	34.620493
1077.479579	78530.332060	34.625511
1078.457014	78645.436877	34.630528
1080.082314	78755.269109	34.635546
1080.600900	78896.830226	34.640564
1081.931328	79014.402889	34.645581
1083.145612	79142.468012	34.650599
1083.990427	79276.401411	34.655616
1085.258763	79407.209094	34.660634
1086.115802	79525.732242	34.665652
1087.390968	79650.548305	34.670669
1088.204300	79779.736751	34.675687
1089.490388	79932.503585	34.680704
1090.600886	80062.303917	34.685722
1091.416740	80169.794665	34.690740
1092.650307	80305.847359	34.695757
1093.389208	80443.490352	34.700775
1094.910628	80570.820219	34.705792
1096.002379	80705.014417	34.710810
1096.702149	80837.748425	34.715828
1097.799758	80943.946806	34.720845
1098.706906	81067.597350	34.725863
1099.900839	81198.346069	34.730880
1100.671107	81300.887751	34.735898
1101.544353	81463.586499	34.740916
1102.672058	81588.488313	34.745933
1103.378111	81720.411516	34.750951
1104.737950	81851.864937	34.755968
1105.542332	82003.446747	34.760986
1106.448673	82138.912414	34.766004
1108.017695	82278.989494	34.771021
1109.103467	82438.488627	34.776039
1110.207958	82570.259028	34.781056
1111.438931	82714.862240	34.786074
1112.265312	82874.570322	34.791092
1113.475671	83013.995019	34.796109
1114.266232	83156.344891	34.801127
1115.968669	83305.074935	34.806144
1117.348397	83463.441454	34.811162
1118.292576	83610.283866	34.816180
1119.449158	83733.063417	34.821197
1120.305204	83893.008462	34.826215
1121.561021	84041.517619	34.831232
1123.032767	84193.995431	34.836250
1124.006267	84342.197566	34.841268
1125.289379	84471.650231	34.846285
1126.072306	84652.254888	34.851303
1127.666650	84769.799219	34.856320
1128.620333	84929.553261	34.861338
1129.713856	85088.103975	34.866356
1131.111337	85224.756994	34.871373
1132.213214	85363.272472	34.876391
1133.198157	85526.996607	34.881408
1134.846666	85659.610322	34.886426
1135.619506	85803.087355	34.891444
1136.918394	85935.391678	34.896461
1138.219768	86095.459619	34.901479
1139.156495	86244.585081	34.906496
1140.733639	86371.151033	34.911514
1141.470026	86524.818498	34.916532
1142.652157	86660.509674	34.921549
1143.864901	86820.888018	34.926567
1145.265618	86965.246780	34.931584
1146.263850	87102.209318	34.936602
1147.349673	87251.052543	34.941620
1148.789859	87395.603953	34.946637
1149.916155	87538.151220	34.951655
1150.937750	87678.085625	34.956672
1152.527161	87819.663227	34.961690
1153.494393	87964.761607	34.966708
1154.568443	88098.177409	34.971725
1155.598932	88240.143858	34.976743
1156.447909	88388.969410	34.981760
1157.973020	88529.215026	34.986778
1159.037281	88652.189451	34.991796
1159.896217	88791.524619	34.996813
1160.882680	88931.061735	35.001831
1161.887169	89054.421050	35.006848
1163.130597	89200.742241	35.011866
1164.008623	89345.187470	35.016884
1165.455418	89470.761691	35.021901
1166.816126	89615.561990	35.026919
1167.786531	89748.618730	35.031936
1168.835535	89905.966418	35.036954
1170.425123	90047.634514	35.041972
1171.158561	90188.763005	35.046989
1172.193389	90334.264962	35.052007
1173.562524	90475.066568	35.057024
1174.352621	90630.493893	35.062042
1175.117692	90797.891558	35.067060
1176.590093	90946.053728	35.072077
1177.898577	91098.486518	35.077095
1178.607125	91277.400602	35.082112
1180.009771	91421.308206	35.087130
1180.912210	91599.416203	35.092148
1182.744163	91755.438472	35.097165
1183.332962	91908.174741	35.102183
1184.605411	92079.473292	35.107200
1186.101966	92256.113415	35.112218
1187.356556	92413.104950	35.117236
1188.733522	92562.703618	35.122253
1190.064510	92739.342323	35.127271
1191.413247	92879.840082	35.132288
1192.484547	93062.448939	35.137306
1193.722395	93215.242871	35.142324
1194.718243	93377.462446	35.147341
1195.868467	93540.670653	35.152359
1196.958881	93701.182487	35.157376
1197.918222	93877.345430	35.162394
1199.087511	94051.275269	35.167412
1200.868534	94213.799907	35.172429
1202.178424	94376.255163	35.177447
1203.294137	94552.303718	35.182464
1204.375959	94711.723633	35.187482
1205.569952	94884.175948	35.192500
1207.079675	95048.685361	35.197517
1208.247752	95206.665571	35.202535
1209.416808	95363.179241	35.207552
1210.714956	95547.897796	35.212570
1212.206865	95699.314747	35.217588
1212.976663	95863.036915	35.222605
1214.524759	96033.841423	35.227623
1215.769378	96173.636444	35.232640
1216.992004	96361.612447	35.237658
1218.024442	96526.809541	35.242676
1219.431841	96682.149554	35.247693
1220.588658	96842.540553	35.252711
1221.519440	97026.418742	35.257728
1222.885827	97148.753621	35.262746
1224.031864	97326.147571	35.267764
1225.654752	97457.419922	35.272781
1227.263838	97592.326390	35.277799
1228.024281	97731.429937	35.282816
1229.933390	97878.594684	35.287834
1231.413303	98013.309108	35.292852
1233.200165	98136.177143	35.297869
1234.012968	98248.559952	35.302887
1235.009365	98401.199892	35.307904
1236.829049	98507.186190	35.312922
1237.323651	98689.938885	35.317940
1238.513533	98804.206685	35.322957
1239.667855	98966.188376	35.327975
1240.658435	99106.073527	35.332992
1241.476704	99259.101809	35.338010
1242.755080	99379.710255	35.343028
1243.651167	99578.096091	35.348045
1244.831185	99717.916907	35.353063
1245.817905	99897.108695	35.358080
1247.289327	100044.983357	35.363098
1248.043148	100239.462292	35.368116
1249.441209	100390.318105	35.373133
1250.766235	100586.309854	35.378151
1251.461555	100740.841718	35.383168
1252.855437	100940.140839	35.388186
1253.923431	101115.026831	35.393204
1255.505573	101317.918347	35.398221
1256.515797	101477.099773	35.403239
1257.721211	101683.148345	35.408256
1259.201537	101859.809297	35.413274
1260.423616	102040.650692	35.418292
1261.719881	102243.924772	35.423309
1263.449463	102414.678547	35.428327
1264.473344	102597.181913	35.433344
1265.915732	102792.490290	35.438362
1267.018466	102965.638300	35.443380
1268.598260	103143.906704	35.448397
1270.127851	103335.807848	35.453415
1271.046312	103516.708946	35.458432
1272.410037	103697.736820	35.463450
1273.768171	103880.456496	35.468468
1275.038692	104051.219263	35.473485
1276.604806	104237.388961	35.478503
1278.235989	104407.261702	35.483520
1279.626125	104590.456400	35.488538
1280.598606	104776.838627	35.493556
1282.105816	104945.981920	35.498573
1283.237807	105120.805434	35.503591
1284.633341	105313.231273	35.508608
1286.127473	105460.206432	35.513626
1287.295659	105661.897767	35.518644
1287.853145	105820.876880	35.523661
1289.802639	105968.282740	35.528679
1291.068090	106193.384328	35.533696
1292.226095	106331.400335	35.538714
1293.784021	106534.650867	35.543732
1294.955957	106667.065888	35.548749
1295.865295	106843.538575	35.553767
1297.086437	106996.692675	35.558784
1298.357952	107181.799477	35.563802
1299.226935	107320.481018	35.568820
1300.343134	107517.013085	35.573837
1301.822583	107686.534664	35.578855
1302.959276	107851.434907	35.583872
1304.068792	108045.156019	35.588890
1305.261877	108244.662716	35.593908
1306.825785	108407.562205	35.598925
1308.013479	108610.332209	35.603943
1308.972650	108777.039127	35.608960
1310.245436	109004.343099	35.613978
1311.810618	109177.785596	35.618996
1313.135020	109346.729547	35.624013
1314.614255	109576.828905	35.629031
1315.636422	109757.678515	35.634048
1317.095624	109957.549433	35.639066
1318.204990	110143.046473	35.644084
1319.617719	110370.689089	35.649101
1321.227186	110520.531441	35.654119
1322.632919	110768.110582	35.659136
1323.941334	110926.814074	35.664154
1325.231377	111154.211301	35.669172
1326.472164	111363.452068	35.674189
1328.334787	111535.762670	35.679207
1329.439178	111763.612806	35.684224
1330.942600	111940.059756	35.689242
1332.242661	112136.929051	35.694260
1333.700202	112330.350356	35.699277
1335.736049	112545.431318	35.704295
1336.657020	112720.248307	35.709312
1337.925596	112936.454766	35.714330
1339.431788	113117.530687	35.719348
1340.659427	113286.282901	35.724365
1341.944768	113514.284967	35.729383
1343.335085	113676.696332	35.734400
1344.689710	113900.019122	35.739418
1346.158620	114069.023158	35.744436
1347.138056	114302.050432	35.749453
1349.036568	114461.315839	35.754471
1350.278959	114694.507548	35.759488
1351.779572	114855.807518	35.764506
1353.576306	115070.372179	35.769524
1354.273207	115255.048761	35.774541
1356.041111	115408.143141	35.779559
1357.211241	115636.442380	35.784576
1358.544983	115832.240219	35.789594
1360.038073	116010.667497	35.794612
1361.357178	116207.648122	35.799629
1362.748308	116408.784647	35.804647
1363.771785	116578.401793	35.809664
1365.163998	116796.508493	35.814682
1366.860962	116954.587108	35.819700
1367.722763	117161.258511	35.824717
1369.180574	117310.994818	35.829735
1370.560000	117503.392066	35.834752
1371.602533	117687.569231	35.839770
1373.284561	117836.228314	35.844788
1374.359390	118064.355553	35.849805
1375.719188	118235.209212	35.854823
1377.422870	118395.093816	35.859840
1378.418721	118621.003524	35.864858
1380.082941	118791.217334	35.869876
1381.153357	119008.178345	35.874893
1382.845406	119162.902927	35.879911
1383.905397	119367.224191	35.884928
1385.572819	119585.937722	35.889946
1386.472393	119759.742933	35.894964
1387.966071	119981.146789	35.899981
1389.474436	120172.897635	35.904999
1390.913655	120367.301330	35.910016
1392.374156	120584.580800	35.915034
1394.212329	120762.676000	35.920052
1394.848475	120979.133608	35.925069
1397.007652	121138.323223	35.930087
1398.385584	121382.388631	35.935104
1399.810623	121547.675043	35.940122
1401.177552	121781.842219	35.945140
1402.664928	121954.264172	35.950157
1404.130439	122185.227754	35.955175
1405.483526	122356.863132	35.960192
1406.599474	122567.115073	35.965210
1408.843513	122759.635513	35.970228
1410.306241	122949.735796	35.975245
1411.877912	123145.684186	35.980263
1413.392260	123348.026515	35.985280
1414.674361	123529.547162	35.990298
1416.202425	123719.211952	35.995316
1417.538054	123922.460981	36.000333
1419.107107	124106.422447	36.005351
1420.566936	124296.152851	36.010368
1421.548276	124480.856245	36.015386
1422.945417	124686.355860	36.020404
1424.447094	124884.582725	36.025421
1425.925620	125074.569001	36.030439
1427.299469	125265.282569	36.035456
1428.887000	125457.977501	36.040474
1430.325114	125647.974251	36.045492
1431.751964	125872.402013	36.050509
1433.257695	126046.696876	36.055527
1434.616801	126237.584334	36.060544
1435.862346	126438.928704	36.065562
1437.382687	126649.997157	36.070580
1438.822373	126835.910565	36.075597
1440.093968	127039.966010	36.080615
1441.702798	127224.183131	36.085632
1443.071345	127439.310019	36.090650
1444.717618	127626.310729	36.095668
1445.741893	127797.678474	36.100685
1447.256809	127985.576574	36.105703
1448.875849	128159.423609	36.110720
1449.989400	128344.841738	36.115738
1451.661445	128524.522514	36.120756
1452.866548	128714.337007	36.125773
1454.046049	128920.663334	36.130791
1455.511878	129105.055175	36.135808
1456.817885	129309.894810	36.140826
1458.332871	129507.190448	36.145844
1459.787973	129689.953685	36.150861
1461.203241	129902.748771	36.155879
1462.221761	130121.461414	36.160896
1463.561654	130299.230206	36.165914
1465.322856	130529.318547	36.170932
1466.877706	130743.187401	36.175949
1468.479356	130927.063016	36.180967
1470.001826	131159.702939	36.185984
1471.534859	131348.495155	36.191002
1472.989973	131567.415811	36.196020
1474.006640	131790.956128	36.201037
1475.909658	131979.237709	36.206055
1477.347150	132191.489233	36.211072
1478.737979	132437.298951	36.216090
1480.426826	132633.638813	36.221108
1482.007383	132849.749491	36.226125
1483.478277	133054.869083	36.231143
1485.004435	133289.654547	36.236160
1486.341423	133494.519848	36.241178
1487.749514	133721.776252	36.246196
1489.242129	133936.224027	36.251213
1490.740083	134146.947466	36.256231
1492.454266	134389.415720	36.261248
1494.187236	134594.783509	36.266266
1495.805154	134801.032654	36.271284
1497.834763	135019.217106	36.276301
1499.882319	135217.697152	36.281319
1501.455614	135406.788706	36.286336
1502.773516	135624.127818	36.291354
1504.351546	135807.962763	36.296372
1505.779293	136026.833328	36.301389
1507.351152	136221.936605	36.306407
1509.415531	136408.181676	36.311424
1510.151677	136634.047257	36.316442
1511.884195	136817.559943	36.321460
1513.208972	137020.323444	36.326477
1514.484876	137215.987269	36.331495
1516.039235	137446.455715	36.336512
1516.962368	137654.292795	36.341530
1518.684861	137870.494617	36.346548
1520.139481	138092.911908	36.351565
1521.438786	138277.402288	36.356583
1522.890924	138526.561603	36.361600
1524.305983	138717.283795	36.366618
1525.651179	138945.718940	36.371636
1527.214528	139138.004349	36.376653
1528.242526	139355.657998	36.381671
1530.290987	139549.212313	36.386688
1531.357924	139784.135868	36.391706
1533.097102	139977.856159	36.396724
1534.701857	140180.064634	36.401741
1535.941517	140413.026731	36.406759
1537.584899	140607.590077	36.411776
1538.667891	140853.000213	36.416794
1540.336014	141052.897975	36.421812
1541.720254	141284.437125	36.426829
1543.186626	141532.250555	36.431847
1544.825428	141745.680287	36.436864
1546.111625	141969.661412	36.441882
1547.871126	142219.068824	36.446900
1549.370610	142454.641592	36.451917
1550.862918	142687.479728	36.456935
1552.438702	142930.230253	36.461952
1554.026322	143173.056876	36.466970
1555.497637	143392.545055	36.471988
1557.020153	143659.074257	36.477005
1558.768085	143883.490406	36.482023
1560.855881	144124.850921	36.487040
1562.242357	144381.889335	36.492058
1564.238365	144603.102637	36.497076
1565.792667	144840.244044	36.502093
1567.326854	145097.974748	36.507111
1569.242582	145293.412010	36.512128
1570.600297	145561.327377	36.517146
1572.527256	145771.443799	36.522164
1574.018216	146017.933303	36.527181
1575.806756	146255.593344	36.532199
1577.712066	146478.799113	36.537216
1579.297499	146706.861373	36.542234
1581.312517	146909.619549	36.547252
1582.942236	147143.191912	36.552269
1584.379309	147370.471292	36.557287
1586.428295	147585.131166	36.562304
1587.436820	147813.267714	36.567322
1588.944120	148025.988432	36.572340
1590.578015	148252.773866	36.577357
1592.038998	148473.731878	36.582375
1593.856857	148681.641327	36.587392
1595.278979	148932.398476	36.592410
1596.962294	149161.324873	36.597428
1598.604917	149385.594315	36.602445
1599.861304	149626.508014	36.607463
1601.480710	149852.533814	36.612480
1602.841484	150082.291300	36.617498
1604.488491	150303.764821	36.622516
1606.101402	150542.828591	36.627533
1607.512888	150774.585947	36.632551
1609.603688	151023.846000	36.637568
1611.058014	151243.467612	36.642586
1612.706739	151460.651088	36.647604
1613.949414	151692.809447	36.652621
1615.194392	151895.455256	36.657639
1617.170570	152124.482879	36.662656
1618.607929	152342.048081	36.667674
1620.057799	152570.452441	36.672692
1621.657191	152791.253133	36.677709
1623.072927	153013.136760	36.682727
1624.684054	153257.152476	36.687744
1626.318201	153493.610025	36.692762
1627.803791	153709.591786	36.697780
1629.563322	153956.467089	36.702797
1631.004091	154189.562451	36.707815
1632.486070	154435.914847	36.712832
1634.204209	154683.588187	36.717850
1635.753018	154920.538530	36.722868
1637.557069	155168.366635	36.727885
1639.128040	155441.274813	36.732903
1640.833086	155666.135089	36.737920
1642.191188	155935.378745	36.742938
1643.941478	156178.594868	36.747956
1645.736171	156436.450483	36.752973
1647.260734	156697.964632	36.757991
1649.274054	156936.034537	36.763008
1650.718995	157204.120600	36.768026
1652.815575	157456.940166	36.773044
1654.392835	157704.505807	36.778061
1655.968986	157976.736100	36.783079
1658.261129	158206.959649	36.788096
1659.603024	158474.399941	36.793114
1661.403616	158734.224662	36.798132
1663.376571	158961.232400	36.803149
1664.650668	159216.097534	36.808167
1666.321051	159481.629391	36.813184
1668.232902	159731.857368	36.818202
1670.088957	159972.369840	36.823220
1671.462429	160250.495977	36.828237
1673.325181	160494.586975	36.833255
1675.118109	160747.110976	36.838272
1676.761212	161004.568182	36.843290
1678.212294	161241.539509	36.848308
1680.415769	161527.330195	36.853325
1681.839939	161756.751163	36.858343
1683.640555	161999.683042	36.863360
1684.991201	162271.690838	36.868378
1687.185683	162517.937010	36.873396
1688.726091	162763.096648	36.878413
1690.323059	163022.490712	36.883431
1692.026597	163255.719537	36.888448
1693.277963	163531.240173	36.893466
1695.325457	163777.657812	36.898484
1697.179253	164025.959489	36.903501
1699.069285	164305.037078	36.908519
1700.765717	164551.084513	36.913536
1702.386668	164790.525336	36.918554
1703.476261	165030.216970	36.923572
1705.334378	165276.509949	36.928589
1707.031995	165510.350254	36.933607
1708.982314	165729.972539	36.938624
1710.347560	165969.766041	36.943642
1711.871763	166225.668604	36.948660
1713.564630	166457.537120	36.953677
1714.774420	166705.185512	36.958695
1716.578445	166955.506143	36.963712
1718.150897	167212.904463	36.968730
1720.128795	167472.941744	36.973748
1721.846564	167724.359310	36.978765
1723.416465	167993.800030	36.983783
1725.250147	168242.830830	36.988800
1726.692269	168512.917046	36.993818
1728.548911	168797.995098	36.998836
1730.558392	169024.717623	37.003853
1732.214794	169324.037412	37.008871
1734.112780	169573.916574	37.013888
1735.343359	169863.642914	37.018906
1737.635528	170106.664242	37.023924
1739.284009	170392.687838	37.028941
1741.033864	170662.956040	37.033959
1743.058360	170915.665168	37.038976
1744.489641	171182.029999	37.043994
1746.153742	171469.987149	37.049012
1747.690985	171736.643391	37.054029
1749.870177	172021.453114	37.059047
1751.215071	172296.541123	37.064064
1753.442556	172597.672961	37.069082
1755.309484	172858.500096	37.074100
1756.928674	173124.721468	37.079117
1758.390914	173419.562330	37.084135
1760.711453	173689.177309	37.089152
1762.185802	173968.848541	37.094170
1764.101995	174252.713956	37.099188
1766.213063	174516.405546	37.104205
1767.655989	174807.783854	37.109223
1769.397950	175081.965483	37.114240
1771.123133	175344.975303	37.119258
1772.902676	175646.734097	37.124276
1774.769484	175913.797355	37.129293
1776.482424	176207.895778	37.134311
1778.942133	176476.429011	37.139328
1781.012783	176755.187582	37.144346
1782.339923	177031.034010	37.149364
1784.304286	177303.266948	37.154381
1786.112201	177595.254275	37.159399
1787.833610	177848.829243	37.164416
1789.793239	178149.486812	37.169434
1791.737332	178412.874859	37.174452
1793.964688	178679.340603	37.179469
1795.168187	178954.585101	37.184487
1797.189407	179225.451400	37.189504
1799.228323	179490.670813	37.194522
1800.685845	179776.093589	37.199540
1802.651019	180000.360567	37.204557
1804.354283	180248.256297	37.209575
1805.885808	180507.358457	37.214592
1807.078974	180751.252700	37.219610
1809.612699	180987.462492	37.224628
1811.332739	181279.654276	37.229645
1812.929305	181518.604062	37.234663
1814.180355	181774.903643	37.239680
1816.091939	182032.254502	37.244698
1817.412131	182314.899270	37.249716
1819.221564	182596.668863	37.254733
1820.994197	182869.640484	37.259751
1823.001452	183148.666958	37.264768
1825.065292	183430.211218	37.269786
1826.665867	183729.214033	37.274804
1828.597758	183989.022069	37.279821
1829.888502	184283.586065	37.284839
1831.518755	184580.585114	37.289856
1833.793557	184868.842758	37.294874
1835.164881	185165.645714	37.299892
1837.206538	185454.413626	37.304909
1839.252115	185778.915161	37.309927
1841.340721	186050.701482	37.314944
1843.453578	186355.997819	37.319962
1844.972148	186656.010268	37.324980
1846.898059	186932.789212	37.329997
1848.600759	187239.666608	37.335015
1850.888313	187542.024573	37.340032
1853.283727	187846.283542	37.345050
1854.885870	188134.186478	37.350068
1856.604437	188434.597554	37.355085
1858.881739	188714.821123	37.360103
1860.638234	189016.879618	37.365120
1862.444629	189306.749707	37.370138
1864.120668	189605.906058	37.375156
1866.603586	189899.149515	37.380173
1868.417124	190190.762464	37.385191
1870.084296	190474.900439	37.390208
1872.313426	190785.004367	37.395226
1874.236992	191066.008706	37.400244
1876.591240	191353.811943	37.405261
1878.018847	191648.769212	37.410279
1880.089231	191941.735348	37.415296
1882.155194	192220.325271	37.420314
1884.112387	192509.657849	37.425332
1886.372675	192786.621123	37.430349
1887.782033	193077.097356	37.435367
1889.496661	193361.841243	37.440384
1891.770112	193647.602220	37.445402
1893.213414	193938.331963	37.450420
1894.981583	194219.138001	37.455437
1896.751125	194521.520779	37.460455
1898.741397	194808.957873	37.465472
1900.348718	195104.262690	37.470490
1902.086183	195377.680926	37.475508
1904.699253	195643.968570	37.480525
1905.993839	195910.416087	37.485543
1907.494418	196189.219521	37.490560
1909.544339	196468.597278	37.495578
1911.212346	196749.255594	37.500596
1913.014234	197030.973019	37.505613
1914.817413	197315.750573	37.510631
1916.657725	197609.573314	37.515648
1918.544054	197898.986208	37.520666
1920.088328	198215.641918	37.525684
1922.357999	198497.445367	37.530701
1924.347063	198807.878262	37.535719
1926.092997	199093.867679	37.540736
1928.510273	199395.262457	37.545754
1930.361522	199707.651770	37.550772
1932.293322	199980.098766	37.555789
1934.216362	200298.813814	37.560807
1936.051469	200612.175612	37.565824
1938.107101	200920.325507	37.570842
1939.847949	201234.226272	37.575860
1942.088215	201530.685435	37.580877
1944.338629	201831.104864	37.585895
1945.976844	202150.815259	37.590912
1947.995071	202459.944447	37.595930
1949.706708	202766.102985	37.600948
1952.048281	203094.008686	37.605965
1954.192093	203404.519476	37.610983
1956.054486	203693.802174	37.616000
1958.000794	204015.784606	37.621018
1959.852213	204347.900834	37.626036
1961.933652	204651.776859	37.631053
1963.835351	204968.123019	37.636071
1965.775610	205293.249015	37.641088
1968.146175	205603.824694	37.646106
1970.118235	205923.782730	37.651124
1972.003587	206228.409053	37.656141
1974.282700	206555.849472	37.661159
1976.104567	206864.107028	37.666176
1979.049677	207172.619584	37.671194
1979.971078	207493.336823	37.676212
1982.035359	207797.003475	37.681229
1984.428276	208126.440254	37.686247
1986.253639	208429.640240	37.691264
1988.484662	208740.800428	37.696282
1990.643951	209050.627953	37.701300
1992.556205	209357.284462	37.706317
1994.818594	209663.391855	37.711335
1996.574873	209975.725427	37.716352
1998.519210	210279.321966	37.721370
2000.202941	210607.742115	37.726388
2002.397327	210907.011113	37.731405
2004.940751	211220.508260	37.736423
2006.340028	211528.475629	37.741440
2008.497529	211840.881821	37.746458
2010.445711	212135.841220	37.751476
2012.193346	212400.669446	37.756493
2014.284985	212712.874535	37.761511
2016.464707	212996.806866	37.766528
2018.529311	213272.950911	37.771546
2020.259295	213575.276884	37.776564
2022.246372	213853.276561	37.781581
2024.047633	214145.361114	37.786599
2025.716621	214446.291547	37.791616
2028.084653	214755.656779	37.796634
2030.058742	215069.085170	37.801652
2032.051501	215359.252987	37.806669
2034.044326	215656.836544	37.811687
2036.006636	215986.395078	37.816704
2038.168170	216283.548348	37.821722
2039.996480	216587.903754	37.826740
2042.007314	216905.689621	37.831757
2044.457984	217234.681536	37.836775
2045.956724	217560.055190	37.841792
2048.203930	217873.897501	37.846810
2050.244338	218203.708162	37.851828
2052.138598	218528.515701	37.856845
2054.113155	218856.156037	37.861863
2056.132717	219197.795200	37.866880
2058.119652	219510.517943	37.871898
2060.035800	219854.627103	37.876916
2062.170874	220200.620392	37.881933
2064.573848	220528.454293	37.886951
2066.741788	220873.937671	37.891968
2069.019381	221198.963014	37.896986
2071.123595	221539.063353	37.902004
2073.263666	221869.700160	37.907021
2075.373520	222208.215489	37.912039
2077.436069	222551.869533	37.917056
2079.477911	222887.122775	37.922074
2081.267716	223220.296995	37.927092
2083.254705	223580.258377	37.932109
2085.681284	223909.690386	37.937127
2087.728292	224260.363512	37.942144
2089.448624	224667.251579	37.947162
2091.792174	225017.487395	37.952180
2093.695330	225371.540431	37.957197
2096.113059	225719.685117	37.962215
2098.200660	226067.020209	37.967232
2100.875619	226397.172247	37.972250
2102.795052	226748.574832	37.977268
2105.292844	227107.036147	37.982285
2107.258755	227436.060390	37.987303
2109.415226	227780.191836	37.992320
2111.450919	228120.001069	37.997338
2113.485541	228463.976839	38.002356
2115.588627	228803.879687	38.007373
2117.924547	229152.762739	38.012391
2119.798001	229497.682464	38.017408
2121.805925	229833.769523	38.022426
2123.714548	230159.740245	38.027444
2125.936192	230479.668824	38.032461
2128.000589	230800.080633	38.037479
2129.626099	231128.055356	38.042496
2131.636321	231451.576518	38.047514
2133.863942	231776.994541	38.052532
2135.768621	232120.446325	38.057549
2138.151590	232452.191446	38.062567
2140.012745	232792.579503	38.067584
2141.807394	233126.680701	38.072602
2144.245892	233474.725946	38.077620
2146.275445	233826.621600	38.082637
2148.778153	234177.148196	38.087655
2150.412957	234538.811070	38.092672
2152.586338	234896.503935	38.097690
2154.396529	235247.829926	38.102708
2156.582421	235619.060677	38.107725
2158.865974	235971.914222	38.112743
2160.911891	236339.258445	38.117760
2163.497227	236709.540870	38.122778
2165.918399	237086.378124	38.127796
2167.733582	237449.140297	38.132813
2170.637363	237802.384279	38.137831
2172.337352	238180.355755	38.142848
2174.674344	238546.747153	38.147866
2177.038407	238916.411982	38.152884
2179.359739	239278.642852	38.157901
2181.682382	239640.823897	38.162919
2183.907798	240015.848228	38.167936
2186.016252	240382.535917	38.172954
2188.266811	240742.014166	38.177972
2190.469320	241109.578239	38.182989
2192.821402	241482.301292	38.188007
2195.032849	241852.025245	38.193024
2197.208351	242227.064618	38.198042
2199.542282	242604.442229	38.203060
2201.845962	242976.644194	38.208077
2204.719210	243344.997744	38.213095
2206.700788	243718.218212	38.218112
2209.036702	244075.432228	38.223130
2211.411015	244423.751038	38.228148
2213.018703	244802.317227	38.233165
2215.321410	245166.423032	38.238183
2217.408582	245533.815286	38.243200
2219.676223	245897.598445	38.248218
2221.791321	246267.655335	38.253236
2223.968146	246649.540185	38.258253
2226.295335	247022.359549	38.263271
2228.202742	247405.711627	38.268288
2230.735879	247776.290440	38.273306
2233.095861	248161.935063	38.278324
2235.123394	248537.295172	38.283341
2237.285414	248909.586767	38.288359
2239.869010	249286.257648	38.293376
2242.052398	249661.824456	38.298394
2244.463002	250008.500237	38.303412
2246.721479	250345.827794	38.308429
2249.125845	250681.532644	38.313447
2251.157530	251029.210584	38.318464
2253.485835	251367.494464	38.323482
2255.355045	251720.279933	38.328500
2257.263147	252064.042389	38.333517
2259.574457	252407.690806	38.338535
2261.419239	252785.172800	38.343552
2263.680688	253142.166489	38.348570
2265.910934	253512.222393	38.353588
2267.953799	253880.175000	38.358605
2270.345252	254248.555709	38.363623
2272.294490	254631.333985	38.368640
2274.576344	255003.848666	38.373658
2277.198365	255392.084836	38.378676
2279.212838	255772.187793	38.383693
2281.579195	256144.030765	38.388711
2283.954091	256536.042440	38.393728
2286.134950	256932.886645	38.398746
2288.750388	257321.508535	38.403764
2290.665360	257719.895074	38.408781
2293.141390	258109.810572	38.413799
2295.797608	258497.970802	38.418816
2297.982681	258900.609597	38.423834
2300.831148	259278.808251	38.428852
2302.816737	259678.355455	38.433869
2305.516129	260070.626591	38.438887
2308.013520	260467.299612	38.443904
2310.172422	260841.977339	38.448922
2312.488794	261233.752075	38.453940
2314.651908	261627.736300	38.458957
2317.348831	262016.047828	38.463975
2319.280312	262412.584725	38.468992
2321.672077	262811.360840	38.474010
2324.217726	263195.912845	38.479028
2326.674506	263611.064547	38.484045
2329.160793	263997.176493	38.489063
2331.415023	264396.992480	38.494080
2333.634769	264794.248680	38.499098
2335.887735	265195.488328	38.504116
2338.206063	265595.041436	38.509133
2340.634916	265984.975055	38.514151
2343.248051	266410.698255	38.519168
2345.386897	266792.422582	38.524186
2348.365138	267182.117795	38.529204
2350.263956	267602.112637	38.534221
2352.432159	268010.024011	38.539239
2354.747399	268396.040213	38.544256
2357.156697	268799.900273	38.549274
2359.266741	269204.443138	38.554292
2361.460333	269611.564166	38.559309
2364.236664	270017.754776	38.564327
2366.628345	270423.650951	38.569344
2368.873207	270828.148035	38.574362
2371.620282	271193.469969	38.579380
2373.421823	271581.169872	38.584397
2375.740236	271954.892367	38.589415
2378.013703	272328.164864	38.594432
2380.123667	272708.449332	38.599450
2382.644512	273100.659193	38.604468
2384.493714	273483.779587	38.609485
2387.029645	273871.363838	38.614503
2389.399422	274275.588333	38.619520
2391.610110	274678.872781	38.624538
2394.126129	275070.651947	38.629556
2396.084099	275482.029420	38.634573
2398.659926	275895.011016	38.639591
2401.043162	276307.896123	38.644608
2403.173542	276713.403495	38.649626
2406.068276	277139.442669	38.654644
2408.302378	277549.531541	38.659661
2411.131128	277979.645600	38.664679
2413.190121	278390.016109	38.669696
2415.497419	278820.441249	38.674714
2417.943836	279238.574376	38.679732
2420.650116	279682.374395	38.684749
2422.858488	280096.302580	38.689767
2425.347669	280539.730188	38.694784
2427.778404	280972.573647	38.699802
2430.554352	281401.018199	38.704820
2432.581379	281845.991734	38.709837
2435.813657	282259.680347	38.714855
2438.581963	282701.233412	38.719872
2440.729932	283132.926389	38.724890
2443.244514	283545.305286	38.729908
2445.921973	283989.335868	38.734925
2448.303206	284420.431976	38.739943
2450.892233	284851.952027	38.744960
2453.386257	285269.591208	38.749978
2456.125212	285699.435482	38.754996
2458.122668	286136.839929	38.760013
2461.080407	286562.431718	38.765031
2463.402456	287005.016793	38.770048
2465.795903	287432.500640	38.775066
2468.618102	287868.984894	38.780084
2471.127622	288296.169860	38.785101
2473.546209	288715.138142	38.790119
2476.094860	289145.618172	38.795136
2478.774609	289576.686498	38.800154
2481.273911	290000.949447	38.805172
2483.643713	290427.975796	38.810189
2486.368825	290853.624256	38.815207
2489.104308	291274.266085	38.820224
2491.072134	291704.986728	38.825242
2493.897183	292131.811239	38.830260
2496.442242	292557.155242	38.835277
2499.093773	292977.350332	38.840295
2501.738574	293404.709250	38.845312
2503.887875	293816.167778	38.850330
2506.712349	294198.737689	38.855348
2508.776544	294602.536755	38.860365
2511.326295	294976.918497	38.865383
2513.951538	295368.129315	38.870400
2516.075099	295768.970121	38.875418
2518.246644	296145.873724	38.880436
2520.799674	296561.174956	38.885453
2523.061249	296960.416603	38.890471
2525.526507	297367.728393	38.895488
2527.761570	297784.169679	38.900506
2530.282264	298194.442931	38.905524
2532.337109	298626.152005	38.910541
2534.598950	299050.308329	38.915559
2537.663343	299478.273743	38.920576
2540.028966	299921.462785	38.925594
2542.410412	300350.118473	38.930612
2544.730912	300798.113259	38.935629
2547.330837	301256.273927	38.940647
2549.765365	301702.165245	38.945664
2552.260244	302150.382666	38.950682
2555.132839	302594.169950	38.955700
2557.495543	303073.547511	38.960717
2560.102507	303523.343430	38.965735
2562.935448	303980.646272	38.970752
2565.404243	304454.439745	38.975770
2568.334707	304897.855350	38.980788
2570.814188	305371.872681	38.985805
2573.164063	305834.935852	38.990823
2576.190965	306299.947642	38.995840
2578.568419	306788.860943	39.000858
2581.450462	307237.407521	39.005876
2583.876024	307714.193783	39.010893
2586.581407	308195.683783	39.015911
2589.205611	308652.191128	39.020928
2591.717153	309135.156045	39.025946
2594.585622	309590.376641	39.030964
2597.246521	310075.904969	39.035981
2599.981817	310556.898398	39.040999
2602.950571	311012.935888	39.046016
2605.294541	311491.549112	39.051034
2608.259066	311940.446361	39.056052
2610.845095	312430.523226	39.061069
2613.593560	312891.413971	39.066087
2616.183691	313354.207406	39.071104
2618.924321	313825.280498	39.076122
2621.849005	314288.804319	39.081140
2624.564358	314753.375232	39.086157
2627.248408	315209.846892	39.091175
2630.064989	315668.098851	39.096192
2632.427249	316132.948118	39.101210
2635.531979	316587.924714	39.106228
2638.005104	317053.717319	39.111245
2640.366438	317505.835903	39.116263
2643.225399	317972.223411	39.121280
2645.667136	318410.813377	39.126298
2648.359988	318846.542425	39.131316
2651.018592	319272.369847	39.136333
2653.322848	319685.095586	39.141351
2655.755964	320120.809087	39.146368
2657.961091	320557.597932	39.151386
2660.956999	320976.532262	39.156404
2663.288577	321416.293819	39.161421
2665.802733	321861.433836	39.166439
2668.907889	322297.055831	39.171456
2671.193992	322747.814790	39.176474
2673.478348	323196.286014	39.181492
2676.181499	323656.116932	39.186509
2678.916565	324113.324516	39.191527
2681.561005	324573.515326	39.196544
2683.870246	325045.235656	39.201562
2686.992485	325501.942626	39.206580
2689.881890	325979.533753	39.211597
2692.113896	326452.223290	39.216615
2694.791208	326937.461016	39.221632
2697.694334	327404.553278	39.226650
2700.183408	327883.796396	39.231668
2702.809766	328378.353349	39.236685
2705.686086	328868.220342	39.241703
2708.867014	329353.795096	39.246720
2711.120758	329845.379701	39.251738
2713.881115	330338.023624	39.256756
2716.575432	330821.380550	39.261773
2719.268281	331317.685446	39.266791
2722.341995	331820.529047	39.271808
2724.860904	332324.777511	39.276826
2727.642043	332823.318217	39.281844
2730.564026	333323.712250	39.286861
2733.380993	333826.963408	39.291879
2736.475105	334321.965206	39.296896
2738.954124	334838.949350	39.301914
2741.934042	335331.422790	39.306932
2744.938473	335831.277965	39.311949
2747.357035	336341.302899	39.316967
2750.998574	336821.878875	39.321984
2753.660666	337325.306681	39.327002
2756.131364	337822.920935	39.332020
2758.691697	338324.935328	39.337037
2761.471355	338823.788031	39.342055
2764.218542	339315.634146	39.347072
2766.884600	339836.028522	39.352090
2769.966859	340337.157526	39.357108
2772.963007	340850.001135	39.362125
2775.225230	341352.521437	39.367143
2778.624496	341847.926207	39.372160
2781.220027	342355.539771	39.377178
2783.650080	342863.683131	39.382196
2786.867319	343371.189828	39.387213
2789.678018	343862.177581	39.392231
2792.527394	344374.761108	39.397248
2794.929830	344871.289212	39.402266
2797.972829	345341.003102	39.407284
2800.805780	345824.329196	39.412301
2803.050382	346287.408639	39.417319
2805.883419	346758.896136	39.422336
2808.545751	347211.264542	39.427354
2811.334155	347701.131995	39.432372
2814.028217	348190.096224	39.437389
2816.250562	348676.642981	39.442407
2819.206590	349153.143141	39.447424
2822.091428	349663.135309	39.452442
2824.636421	350163.022071	39.457460
2827.308621	350661.157893	39.462477
2829.798607	351175.082605	39.467495
2833.053613	351679.184041	39.472512
2835.639403	352194.607020	39.477530
2838.353544	352718.457942	39.482548
2841.307789	353242.925690	39.487565
2844.127197	353768.983414	39.492583
2846.698474	354298.628940	39.497600
2849.483893	354835.063485	39.502618
2852.235497	355375.254615	39.507636
2855.442057	355916.738746	39.512653
2858.565773	356462.418474	39.517671
2861.400244	357003.213814	39.522688
2864.146483	357555.084161	39.527706
2867.082922	358109.380395	39.532724
2870.212153	358652.801747	39.537741
2872.902783	359193.443770	39.542759
2876.120396	359752.829524	39.547776
2879.307168	360302.721130	39.552794
2881.967071	360858.299076	39.557812
2885.174209	361398.860120	39.562829
2888.118050	361950.243387	39.567847
2890.950487	362491.435069	39.572864
2894.225169	363057.143562	39.577882
2897.406044	363601.668178	39.582900
2900.423632	364147.608120	39.587917
2903.371958	364712.180687	39.592935
2906.474717	365211.346587	39.597952
2909.289964	365794.275609	39.602970
2912.297044	366324.025278	39.607988
2915.409388	366852.229397	39.613005
2917.903088	367427.244981	39.618023
2921.151734	367950.212182	39.623040
2924.076546	368496.697972	39.628058
2927.080533	369043.595845	39.633076
2930.116261	369595.760093	39.638093
2933.016846	370142.330668	39.643111
2936.263697	370671.761827	39.648128
2939.052966	371219.960393	39.653146
2941.958636	371763.540661	39.658164
2944.965213	372310.954932	39.663181
2947.848248	372853.966558	39.668199
2950.601692	373401.102243	39.673216
2953.729475	373929.344359	39.678234
2956.365316	374440.606816	39.683252
2959.120354	374949.915745	39.688269
2961.538809	375471.196755	39.693287
2964.920081	375966.667377	39.698304
2967.602006	376480.535836	39.703322
2970.083916	377003.055786	39.708340
2973.404361	377516.480181	39.713357
2976.297638	378047.522319	39.718375
2978.569081	378593.446871	39.723392
2981.597021	379130.567554	39.728410
2984.395843	379663.404296	39.733428
2987.205577	380216.781440	39.738445
2989.715084	380785.851056	39.743463
2992.839919	381355.195487	39.748480
2995.699314	381908.210872	39.753498
2998.338084	382494.789827	39.758516
3001.406782	383077.461218	39.763533
3004.706426	383663.816120	39.768551
3007.215886	384236.664936	39.773568
3009.987737	384843.251699	39.778586
3013.268777	385446.247519	39.783604
3016.480906	386031.564576	39.788621
3019.628337	386644.835142	39.793639
3022.997464	387255.802925	39.798656
3025.857032	387854.793026	39.803674
3028.956506	388458.985647	39.808692
3032.118518	389056.310110	39.813709
3035.315815	389679.286586	39.818727
3038.676598	390280.997752	39.823744
3041.679993	390875.171968	39.828762
3045.086568	391506.199278	39.833780
3048.033671	392083.090649	39.838797
3050.968998	392736.868879	39.843815
3054.388076	393307.350471	39.848832
3057.569277	393951.861058	39.853850
3060.956363	394544.136943	39.858868
3064.090418	395132.435881	39.863885
3067.020970	395765.844710	39.868903
3070.567278	396358.063909	39.873920
3073.404243	396959.818068	39.878938
3076.546933	397585.070067	39.883956
3079.529187	398178.867858	39.888973
3082.268200	398800.179911	39.893991
3085.800507	399424.955334	39.899008
3088.956092	400005.457124	39.904026
3091.615558	400661.711855	39.909044
3095.168876	401241.900562	39.914061
3098.210372	401865.185718	39.919079
3101.282895	402501.789901	39.924096
3104.464250	403100.943134	39.929114
3107.524757	403709.586125	39.934132
3110.770681	404320.926166	39.939149
3113.400936	404940.033341	39.944167
3116.869849	405552.480437	39.949184
3120.074468	406153.397500	39.954202
3122.896040	406740.142161	39.959220
3126.132208	407306.048768	39.964237
3129.000922	407888.708283	39.969255
3131.989941	408459.829419	39.974272
3135.010910	409058.564456	39.979290
3137.957107	409625.158623	39.984308
3140.485624	410217.409059	39.989325
3143.823203	410829.265048	39.994343
3146.454932	411424.060853	39.999360
3149.813810	412031.504090	40.004378
3152.489782	412650.448344	40.009396
3155.474606	413279.646135	40.014413
3158.983892	413899.902472	40.019431
3161.814146	414515.691302	40.024448
3165.173617	415148.616772	40.029466
3167.972743	415806.148695	40.034484
3171.493473	416443.506117	40.039501
3174.598195	417075.010744	40.044519
3177.693840	417739.217936	40.049536
3181.030338	418383.783635	40.054554
3184.156309	419029.913777	40.059572
3187.061862	419683.159010	40.064589
3190.331985	420369.068766	40.069607
3193.531657	421029.432383	40.074624
3196.744831	421692.692062	40.079642
3200.010083	422376.349038	40.084660
3203.493891	423040.952574	40.089677
3206.509571	423729.556094	40.094695
3209.555015	424411.474601	40.099712
3213.279041	425092.306071	40.104730
3215.943259	425787.145541	40.109748
3219.489264	426480.003755	40.114765
3222.748313	427152.674461	40.119783
3226.364792	427845.157035	40.124800
3229.375424	428546.076663	40.129818
3232.499948	429245.946591	40.134836
3236.302016	429923.882114	40.139853
3239.303259	430631.257692	40.144871
3242.719498	431333.432261	40.149888
3245.850391	432031.099442	40.154906
3249.321087	432709.445750	40.159924
3252.173443	433447.641791	40.164941
3255.796009	434126.610633	40.169959
3259.025739	434829.530203	40.174976
3262.555707	435545.500791	40.179994
3265.716769	436249.759508	40.185012
3269.366226	436947.008294	40.190029
3272.878875	437636.308311	40.195047
3276.092408	438351.920128	40.200064
3279.835973	439020.736555	40.205082
3282.890739	439722.205234	40.210100
3286.018732	440416.477138	40.215117
3289.632108	441116.577231	40.220135
3292.995301	441802.721542	40.225152
3295.818632	442482.906508	40.230170
3298.924194	443158.926592	40.235188
3302.134836	443793.950562	40.240205
3305.077296	444452.897532	40.245223
3308.134244	445119.402605	40.250240
3311.318752	445784.350142	40.255258
3314.307810	446449.056916	40.260276
3317.603025	447117.392245	40.265293
3320.493574	447814.121413	40.270311
3323.624435	448508.716512	40.275328
3326.867646	449177.710318	40.280346
3330.270249	449897.480505	40.285364
3333.288715	450576.795827	40.290381
3336.294308	451330.396332	40.295399
3339.668707	452022.317304	40.300416
3342.984016	452759.929412	40.305434
3345.527087	453498.399008	40.310452
3349.142009	454223.415743	40.315469
3352.399233	455003.576901	40.320487
3355.535110	455747.800602	40.325504
3358.929194	456517.564273	40.330522
3362.382940	457315.224243	40.335540
3365.783383	458041.720514	40.340557
3369.187785	458820.814701	40.345575
3372.426449	459633.098944	40.350592
3376.106379	460382.799073	40.355610
3379.652052	461187.135151	40.360628
3382.908537	461968.468402	40.365645
3386.874987	462740.858801	40.370663
3389.720805	463556.398082	40.375680
3393.884343	464317.774058	40.380698
3397.042151	465134.822900	40.385716
3400.680088	465919.139390	40.390733
3404.000440	466707.068347	40.395751
3407.555130	467517.893355	40.400768
3411.185683	468293.777741	40.405786
3414.617909	469116.344766	40.410804
3418.178102	469884.746995	40.415821
3421.590167	470705.484562	40.420839
3425.019548	471471.219174	40.425856
3428.740478	472304.638308	40.430874
3431.783775	473099.853602	40.435892
3435.768871	473865.967440	40.440909
3439.270276	474677.886236	40.445927
3442.701063	475500.754932	40.450944
3446.493318	476265.949261	40.455962
3450.149805	477055.301068	40.460980
3453.648902	477883.319353	40.465997
3457.138148	478659.136894	40.471015
3460.759562	479416.604754	40.476032
3463.929044	480195.496320	40.481050
3467.166693	481020.291352	40.486068
3470.570231	481822.180456	40.491085
3474.267019	482657.902910	40.496103
3477.490669	483458.439314	40.501120
3480.799166	484237.531257	40.506125
3484.430994	484962.876856	40.511130
3487.626092	485631.827165	40.516135
3490.869353	486273.339551	40.521140
3493.353133	486880.097560	40.526144
3496.253460	487372.944328	40.531149
3499.011746	487820.007922	40.536154
3501.533724	488198.866336	40.541159
3503.939817	488567.959303	40.546164
3505.619357	488878.098512	40.551168
3507.772856	489101.491530	40.556173
3509.470533	489308.542732	40.561178
3510.955969	489472.014323	40.566183
3512.494042	489570.895979	40.571188
3513.594779	489639.253031	40.576192
3515.034698	489656.044238	40.581197
3515.927073	489717.190844	40.586202
3516.563842	489663.552241	40.591207
3518.123677	489573.754622	40.596212
3518.556056	489503.078401	40.601216
3519.318314	489432.147174	40.606221
3519.840213	489307.208141	40.611226
3520.359920	489133.237177	40.616231
3520.390400	488975.145620	40.621236
3521.349746	488772.128427	40.626240
3521.690040	488581.110564	40.631245
3521.334532	488424.392421	40.636250
3520.998113	488181.354156	40.641255
3521.949850	487927.420869	40.646260
3521.578411	487697.704382	40.651264
3521.443780	487472.506813	40.656269
3521.347020	487294.006682	40.661274
3521.229382	487036.127299	40.666279
3521.470301	486759.140106	40.671284
3521.024506	486552.521953	40.676288
3521.278183	486283.327389	40.681293
3521.303006	486020.903088	40.686298
3520.615314	485792.885516	40.691303
3521.040120	485521.120166	40.696308
3520.183811	485302.597220	40.701312
3519.890873	485010.723742	40.706317
3519.872107	484793.531894	40.711322
3519.982214	484536.241615	40.716327
3519.206833	484289.727560	40.721332
3519.102198	484045.586985	40.726336
3519.127456	483827.921358	40.731341
3518.727668	483563.605461	40.736346
3518.352086	483364.795483	40.741351
3518.493407	483098.057031	40.746356
3518.055440	482896.009355	40.751360
3517.869693	482673.854647	40.756365
3517.842227	482418.128837	40.761370
3517.249433	482238.748340	40.766375
3517.179157	481977.247092	40.771380
3516.694025	481788.015232	40.776384
3516.960296	481555.236673	40.781389
3516.232368	481366.799209	40.786394
3516.114155	481130.630637	40.791399
3516.093472	480944.104281	40.796404
3515.590606	480735.710357	40.801408
3515.713353	480562.079689	40.806413
3515.237084	480348.711337	40.811418
3515.021005	480180.097050	40.816423
3514.901200	479963.374270	40.821428
3514.422009	479784.713593	40.826432
3514.568321	479623.942881	40.831437
3514.166880	479418.306291	40.836442
3513.664300	479274.460322	40.841447
3513.755545	479073.506039	40.846452
3513.579284	478936.650384	40.851456
3513.717887	478765.484744	40.856461
3513.206771	478581.598306	40.861466
3513.111903	478441.888312	40.866471
3513.071760	478243.227032	40.871476
3512.567751	478142.553087	40.876480
3512.604999	477953.404725	40.881485
3512.563228	477822.804679	40.886490
3512.236629	477662.092881	40.891495
3511.970432	477505.728955	40.896500
3511.357353	477390.573221	40.901504
3511.268757	477238.841972	40.906509
3511.048780	477125.345818	40.911514
3510.862445	476982.953865	40.916519
3510.886900	476864.906734	40.921524
3510.277570	476746.604287	40.926528
3510.406281	476613.131088	40.931533
3510.391341	476511.256584	40.936538
3510.319490	476397.226058	40.941543
3510.091161	476266.746750	40.946548
3509.849941	476165.261062	40.951552
3509.972467	476056.925411	40.956557
3509.920094	475939.239805	40.961562
3509.589337	475866.201922	40.966567
3509.795118	475726.324142	40.971572
3509.338605	475643.269277	40.976576
3509.159324	475545.065360	40.981581
3509.321848	475442.346416	40.986586
3508.908105	475363.237292	40.991591
3509.002507	475255.256610	40.996596
3508.786241	475158.222494	41.001600
3508.722337	475093.959454	41.006605
3508.324015	474988.336218	41.011610
3508.531604	474911.306754	41.016615
3508.328407	474799.518306	41.021620
3507.964859	474762.927304	41.026624
3507.927502	474648.982857	41.031629
3507.956398	474590.431505	41.036634
3507.626390	474493.564261	41.041639
3507.507533	474447.607017	41.046644
3507.469833	474348.056985	41.051648
3507.434372	474316.380999	41.056653
3507.327333	474234.228253	41.061658
3507.370571	474163.406217	41.066663
3507.337322	474084.231974	41.071668
3506.812605	474060.388674	41.076672
3506.800083	473977.560969	41.081677
3506.685760	473919.689315	41.086682
3506.430170	473882.876900	41.091687
3506.864113	473822.992032	41.096692
3506.746416	473763.295561	41.101696
3506.861932	473710.354805	41.106701
3506.757869	473652.075234	41.111706
3506.722948	473596.876808	41.116711
3506.601935	473549.143646	41.121716
3506.605940	473495.510262	41.126720
3506.792555	473443.317968	41.131725
3506.323895	473380.583588	41.136730
3506.113642	473334.993136	41.141735
3506.203112	473299.443152	41.146740
3506.191343	473247.636567	41.151744
3506.179595	473189.493168	41.156749
3506.094884	473162.436280	41.161754
3505.894060	473105.082928	41.166759
3506.594742	473054.126428	41.171764
3506.213056	473011.603977	41.176768
3506.155434	472964.315678	41.181773
3505.530864	472915.190500	41.186778
3505.726145	472902.840999	41.191783
3506.151230	472842.498420	41.196788
3505.432561	472805.402397	41.201792
3505.603305	472769.686567	41.206797
3505.364639	472748.229857	41.211802
3505.524293	472707.243440	41.216807
3505.651125	472667.428107	41.221812
3505.421122	472649.873419	41.226816
3505.193937	472609.759065	41.231821
3505.738046	472563.946279	41.236826
3505.545539	472520.480400	41.241831
3505.354058	472510.777242	41.246836
3505.452609	472473.450065	41.251840
3505.663670	472430.883420	41.256845
3505.238572	472396.122937	41.261850
3505.228978	472383.906897	41.266855
3505.808532	472329.165590	41.271860
3505.410339	472311.028848	41.276864
3505.174377	472266.555388	41.281869
3505.228712	472221.174121	41.286874
3505.147308	472217.486229	41.291879
3505.716151	472174.558332	41.296884
3504.977490	472158.300321	41.301888
3505.249656	472112.073249	41.306893
3504.950644	472096.911712	41.311898
3504.732009	472076.008792	41.316903
3504.667219	472047.781275	41.321908
3504.686261	472026.232383	41.326912
3504.782480	471994.329210	41.331917
3504.726993	471993.628269	41.336922
3504.597139	471963.078885	41.341927
3504.928980	471943.102755	41.346932
3504.950377	471914.202378	41.351936
3505.323058	471880.278167	41.356941
3504.942198	471878.766804	41.361946
3504.962717	471837.952738	41.366951
3505.219093	471808.710894	41.371956
3504.665464	471812.296517	41.376960
3504.652593	471767.837417	41.381965
3504.734528	471756.316296	41.386970
3504.540338	471709.097394	41.391975
3504.660772	471733.210197	41.396980
3504.495366	471677.063994	41.401984
3504.634933	471674.709903	41.406989
3504.349155	471645.807004	41.411994
3504.063180	471637.385800	41.416999
3504.392887	471612.441355	41.422004
3504.181096	471607.658621	41.427008
3504.265007	471597.556624	41.432013
3504.284891	471557.705354	41.437018
3504.220607	471569.071781	41.442023
3504.324378	471539.600189	41.447028
3504.391265	471562.859796	41.452032
3504.192847	471541.598257	41.457037
3504.718234	471512.161383	41.462042
3504.267155	471501.636920	41.467047
3504.401529	471514.087325	41.472052
3504.663282	471469.127899	41.477056
3504.255747	471479.027697	41.482061
3504.676138	471416.957969	41.487066
3504.303171	471441.960261	41.492071
3504.620579	471394.659780	41.497076
3504.560498	471409.118199	41.502080
3504.484596	471367.456581	41.507085
3504.286774	471367.994865	41.512090
3504.200291	471323.445048	41.517095
3504.725878	471335.326748	41.522100
3504.611283	471287.333832	41.527104
3504.076581	471308.914374	41.532109
3504.161775	471282.994218	41.537114
3504.294664	471275.622022	41.542119
3504.490682	471235.032518	41.547124
3504.236653	471249.471004	41.552128
3504.631195	471200.079262	41.557133
3504.593399	471176.358439	41.562138
3504.146808	471215.162599	41.567143
3504.326968	471171.482881	41.572148
3504.680647	471127.877042	41.577152
3504.660237	471144.661507	41.582157
3504.516014	471145.343420	41.587162
3504.233432	471096.464041	41.592167
3504.785170	471095.210807	41.597172
3504.252871	471068.374007	41.602176
3504.385767	471064.145051	41.607181
3504.294864	471037.644036	41.612186
3504.164847	471047.702971	41.617191
3504.678506	470983.690653	41.622196
3504.343574	471028.003691	41.627200
3504.200883	470987.264441	41.632205
3504.679313	470968.430276	41.637210
3504.307924	470958.247833	41.642215
3504.645164	470942.072304	41.647220
3504.066512	470914.837039	41.652224
3503.973685	470922.152408	41.657229
3504.278982	470881.849135	41.662234
3503.940744	470898.379839	41.667239
3504.498116	470879.127524	41.672244
3504.094921	470854.703598	41.677248
3504.478896	470854.744346	41.682253
3504.087740	470856.225785	41.687258
3503.891413	470832.428227	41.692263
3504.524479	470823.354440	41.697268
3503.988619	470806.961908	41.702272
3504.203013	470778.891330	41.707277
3504.468741	470756.288138	41.712282
3504.161193	470792.536141	41.717287
3504.308214	470765.642278	41.722292
3504.314640	470717.172619	41.727296
3504.452293	470698.797668	41.732301
3504.373561	470703.677307	41.737306
3504.177380	470711.820279	41.742311
3504.442916	470697.075479	41.747316
3503.915873	470652.188255	41.752320
3504.181864	470620.357532	41.757325
3503.970517	470648.326519	41.762330
3503.743857	470644.002209	41.767335
3504.220106	470613.963432	41.772340
3503.921724	470637.586010	41.777344
3503.878644	470600.429936	41.782349
3504.315925	470592.857288	41.787354
3503.646098	470626.830647	41.792359
3503.968432	470611.164214	41.797364
3503.688837	470586.771137	41.802368
3503.972581	470533.085834	41.807373
3503.629499	470580.291012	41.812378
3503.877289	470559.008638	41.817383
3504.148125	470578.485323	41.822388
3504.119361	470542.340879	41.827392
3504.168623	470562.663798	41.832397
3504.252936	470526.095855	41.837402
3503.912344	470534.211021	41.842407
3504.302490	470515.441100	41.847412
3504.050044	470509.194236	41.852416
3504.281443	470464.186731	41.857421
3504.194264	470491.325102	41.862426
3504.229328	470463.789443	41.867431
3504.192546	470456.190273	41.872436
3503.998697	470448.818726	41.877440
3504.273104	470425.047700	41.882445
3503.746208	470437.958170	41.887450
3503.855849	470405.898329	41.892455
3503.945166	470412.830187	41.897460
3504.029552	470415.250500	41.902464
3503.956001	470399.038076	41.907469
3504.213793	470363.862036	41.912474
3503.908226	470400.262510	41.917479
3504.110987	470370.266608	41.922484
3503.942044	470328.313406	41.927488
3504.094813	470357.036442	41.932493
3504.136368	470325.342141	41.937498
3504.100428	470335.386551	41.942503
3504.421420	470297.158383	41.947508
3503.749552	470308.368028	41.952512
3504.265303	470276.497303	41.957517
3504.044465	470279.117976	41.962522
3503.985548	470268.480201	41.967527
3504.138279	470272.664249	41.972532
3503.582317	470248.263755	41.977536
3503.870961	470249.587089	41.982541
3504.163998	470261.911769	41.987546
3503.985281	470204.496164	41.992551
3504.035487	470200.685709	41.997556
3504.041598	470234.045865	42.002560
3504.084717	470192.413777	42.007565
3504.432784	470159.200454	42.012570
3504.035434	470191.509028	42.017575
3504.251992	470127.997342	42.022580
3504.234092	470151.069130	42.027584
3503.925158	470152.841827	42.032589
3504.139450	470084.564482	42.037594
3503.880957	470125.318287	42.042599
3503.698103	470106.334357	42.047604
3504.157414	470077.362206	42.052608
3503.829040	470097.238256	42.057613
3503.768864	470094.814156	42.062618
3503.983191	470056.754509	42.067623
3504.204967	470083.084064	42.072628
3503.380799	470063.339539	42.077632
3504.074438	470023.023925	42.082637
3504.012825	470063.138319	42.087642
3503.730734	470074.692092	42.092647
3503.803920	470024.080820	42.097652
3504.319110	469990.536608	42.102656
3504.149431	470005.824546	42.107661
3503.955864	470014.423688	42.112666
3504.015156	469991.801595	42.117671
3504.077470	469992.349498	42.122676
3504.194527	469978.692385	42.127680
3503.848204	469977.834537	42.132685
3503.886871	469948.624484	42.137690
3504.091869	469932.266268	42.142695
3504.219169	469953.540775	42.147700
3504.024085	469952.456217	42.152704
3503.694976	469911.642920	42.157709
3504.377614	469911.332258	42.162714
3504.272607	469921.337082	42.167719
3503.681377	469877.218851	42.172724
3504.155717	469875.927080	42.177728
3503.852561	469872.730133	42.182733
3504.271831	469827.488752	42.187738
3503.766813	469861.488009	42.192743
3504.144728	469814.579984	42.197748
3503.905273	469807.570330	42.202752
3504.175188	469833.486978	42.207757
3504.015468	469797.108430	42.212762
3503.907324	469809.344681	42.217767
3503.916089	469804.628072	42.222772
3504.170359	469777.310368	42.227776
3503.583992	469789.520812	42.232781
3504.323316	469730.437748	42.237786
3503.945508	469744.491226	42.242791
3504.181796	469742.527246	42.247796
3503.942309	469729.889659	42.252800
3503.986178	469703.517748	42.257805
3503.987759	469731.758523	42.262810
3503.921291	469708.598278	42.267815
3504.004503	469698.292661	42.272820
3503.720737	469672.023196	42.277824
3503.844699	469659.885846	42.282829
3503.914862	469704.036269	42.287834
3503.754663	469672.170055	42.292839
3504.239962	469629.047295	42.297844
3503.536495	469670.480744	42.302848
3503.984350	469667.063660	42.307853
3504.292701	469619.608469	42.312858
3504.203843	469640.461141	42.317863
3504.374265	469581.264764	42.322868
3504.093360	469601.742210	42.327872
3503.909719	469558.725034	42.332877
3504.020981	469591.055553	42.337882
3503.761825	469549.571361	42.342887
3503.974049	469563.886619	42.347892
3503.632763	469540.262600	42.352896
3503.893722	469504.070563	42.357901
3504.239420	469548.228469	42.362906
3503.660069	469553.593121	42.367911
3503.853397	469500.679985	42.372916
3504.193980	469505.290821	42.377920
3503.534273	469535.917990	42.382925
3503.757293	469497.298223	42.387930
3504.104003	469461.092559	42.392935
3504.055918	469468.097151	42.397940
3504.025436	469504.557113	42.402944
3504.109518	469452.573768	42.407949
3504.466088	469441.160065	42.412954
3503.759796	469460.386615	42.417959
3504.161985	469388.680224	42.422964
3503.796818	469437.818181	42.427968
3503.116079	469408.873186	42.432973
3503.733278	469392.297289	42.437978
3503.536962	469442.270496	42.442983
3503.651735	469424.506469	42.447988
3503.605256	469408.897428	42.452992
3504.220991	469377.516557	42.457997
3503.516357	469389.188195	42.463002
3503.529371	469383.710279	42.468007
3503.875949	469372.298117	42.473012
3503.297654	469401.290127	42.478016
3503.218409	469430.913057	42.483021
3503.731501	469427.029300	42.488026
3503.928705	469411.128232	42.493031
3503.647217	469375.731547	42.498036
3503.817374	469341.530989	42.503040
3503.833683	469382.141404	42.508045
3504.059802	469378.556509	42.513050
3504.055179	469333.583869	42.518055
3504.038057	469332.775368	42.523060
3503.821240	469338.133477	42.528064
3503.615152	469326.605830	42.533069
3504.240745	469279.657459	42.538074
3503.638510	469286.901806	42.543079
3503.781153	469325.920570	42.548084
3503.476609	469309.693105	42.553088
3503.879796	469283.770902	42.558093
3504.349008	469256.824170	42.563098
3503.455354	469284.345093	42.568103
3503.539566	469253.605779	42.573108
3503.799904	469269.434727	42.578112
3503.405584	469307.879254	42.583117
3503.650915	469269.509055	42.588122
3503.780568	469253.162216	42.593127
3503.461760	469235.213043	42.598132
3503.761589	469227.154597	42.603136
3503.982141	469209.931404	42.608141
3503.919511	469235.191511	42.613146
3503.955074	469228.341006	42.618151
3504.209834	469234.334451	42.623156
3504.022869	469240.499116	42.628160
3503.933542	469231.792337	42.633165
3503.872023	469212.484197	42.638170
3503.841124	469188.405096	42.643175
3503.937891	469177.742158	42.648180
3503.841454	469189.267075	42.653184
3503.418333	469155.312093	42.658189
3503.810290	469136.946276	42.663194
3503.371312	469140.260711	42.668199
3503.933774	469130.943838	42.673204
3504.643852	469104.820799	42.678208
3504.137428	469090.501098	42.683213
3504.238329	469108.890541	42.688218
3503.931065	469129.575428	42.693223
3503.782210	469086.196858	42.698228
3503.682303	469064.511585	42.703232
3503.962017	469036.479043	42.708237
3504.273857	469031.663655	42.713242
3503.990982	469023.595823	42.718247
3503.907991	469027.361047	42.723252
3503.965832	469030.901196	42.728256
3503.836596	469031.580808	42.733261
3503.907254	469031.468271	42.738266
3503.981212	469030.138326	42.743271
3503.522102	468998.369032	42.748276
3504.068865	468988.243318	42.753280
3504.452764	468954.971717	42.758285
3503.973549	468965.644589	42.763290
3503.438422	468976.529107	42.768295
3503.464070	468967.043488	42.773300
3504.189495	468951.717733	42.778304
3504.087979	468917.965054	42.783309
3503.920581	468908.357809	42.788314
3504.017791	468904.590392	42.793319
3504.331478	468879.949435	42.798324
3503.156264	468897.678791	42.803329
3503.031290	468903.884461	42.808333
3504.058832	468880.448978	42.813338
3503.743308	468876.442567	42.818343
3503.852676	468902.182930	42.823348
3503.810356	468918.110684	42.828353
3503.888836	468898.577312	42.833357
3503.644105	468881.275278	42.838362
3504.013427	468854.952266	42.843367
3504.080267	468846.119235	42.848372
3503.856131	468874.548955	42.853377
3503.079294	468843.640908	42.858381
3504.089450	468815.644734	42.863386
3503.795257	468821.572950	42.868391
3503.769872	468842.112160	42.873396
3503.723383	468854.896968	42.878401
3503.755146	468824.165314	42.883405
3503.481184	468804.484743	42.888410
3503.776695	468792.877522	42.893415
3503.938184	468822.260446	42.898420
3504.023736	468773.723063	42.903425
3503.819535	468745.462393	42.908429
3503.738999	468787.762509	42.913434
3503.682428	468788.075713	42.918439
3503.635194	468774.240965	42.923444
3503.686343	468751.973747	42.928449
3504.216366	468723.698408	42.933453
3503.942772	468733.730445	42.938458
3503.774749	468777.413427	42.943463
3503.918292	468740.021728	42.948468
3503.277463	468717.458209	42.953473
3503.252092	468708.335467	42.958477
3503.263906	468703.415311	42.963482
3503.758447	468679.708918	42.968487
3503.585209	468683.995512	42.973492
3503.912297	468740.580652	42.978497
3503.709925	468713.333735	42.983501
3504.338494	468677.639917	42.988506
3503.998299	468661.823220	42.993511
3503.783159	468638.786698	42.998516
3504.130695	468639.796602	43.003521
3503.776390	468651.666799	43.008525
3503.842989	468640.044970	43.013530
3503.744161	468614.201286	43.018535
3503.869579	468614.992776	43.023540
3503.658273	468605.696559	43.028545
3503.167627	468619.819328	43.033549
3503.624290	468630.800791	43.038554
3503.385188	468638.393601	43.043559
3503.394717	468639.456929	43.048564
3503.484983	468641.166656	43.053569
3503.413422	468642.749846	43.058573
3503.416607	468623.785869	43.063578
3503.938615	468596.931355	43.068583
3503.524484	468639.538019	43.073588
3503.529501	468630.410441	43.078593
3503.945724	468599.871216	43.083597
3503.928635	468599.011976	43.088602
3503.676989	468618.674482	43.093607
3503.748951	468596.403810	43.098612
3504.030659	468584.900065	43.103617
3503.995988	468548.246058	43.108621
3503.595359	468540.754403	43.113626
3503.719779	468556.301144	43.118631
3503.620716	468576.852259	43.123636
3503.514766	468595.224141	43.128641
3503.707163	468572.731590	43.133645
3504.070767	468548.133058	43.138650
3503.561870	468537.565523	43.143655
3504.135385	468498.888520	43.148660
3503.946824	468549.724610	43.153665
3503.543769	468500.503250	43.158669
3504.233856	468481.329167	43.163674
3503.868747	468492.541997	43.168679
3504.028142	468485.367448	43.173684
3503.870615	468466.479435	43.178689
3503.873164	468458.569092	43.183693
3503.989111	468453.531008	43.188698
3503.485794	468467.300946	43.193703
3503.626478	468443.700921	43.198708
3503.847768	468419.682488	43.203713
3503.856985	468459.687350	43.208717
3503.767693	468430.748928	43.213722
3503.439756	468409.606070	43.218727
3503.937972	468417.538770	43.223732
3503.854015	468431.597385	43.228737
3503.302629	468405.317922	43.233741
3504.165835	468379.879653	43.238746
3504.350036	468368.543317	43.243751
3504.064139	468353.072741	43.248756
3504.036819	468349.426319	43.253761
3504.016183	468333.761687	43.258765
3503.995485	468371.793937	43.263770
3503.797690	468340.134458	43.268775
3503.819423	468296.220239	43.273780
3503.702671	468348.617334	43.278785
3503.844070	468330.239709	43.283789
3503.825969	468323.346686	43.288794
3503.333472	468328.292276	43.293799
3503.755353	468283.503500	43.298804
3503.675728	468321.900092	43.303809
3503.538877	468304.479120	43.308813
3503.701970	468286.655788	43.313818
3504.125021	468276.042232	43.318823
3503.844713	468292.464425	43.323828
3503.612650	468261.013065	43.328833
3504.080827	468234.369419	43.333837
3503.809622	468257.179098	43.338842
3503.805375	468265.241978	43.343847
3504.051131	468214.244119	43.348852
3503.578775	468256.150883	43.353857
3503.364617	468223.429000	43.358861
3503.684198	468253.548317	43.363866
3503.533473	468227.509538	43.368871
3504.017412	468237.523491	43.373876
3503.690144	468225.456630	43.378881
3503.717812	468174.442439	43.383885
3504.130119	468200.287898	43.388890
3503.782219	468198.669638	43.393895
3504.101742	468141.220328	43.398900
3503.996159	468164.713809	43.403905
3503.890508	468147.946950	43.408909
3503.942061	468149.662836	43.413914
3503.706947	468139.863118	43.418919
3503.653696	468118.118787	43.423924
3503.999104	468102.801775	43.428929
3503.778405	468114.042687	43.433933
3503.765048	468152.936172	43.438938
3503.655955	468099.763068	43.443943
3504.011363	468116.591979	43.448948
3503.723888	468090.270409	43.453953
3503.868930	468087.813640	43.458957
3503.494757	468091.320818	43.463962
3503.902870	468071.176812	43.468967
3503.710832	468050.975526	43.473972
3503.956340	468064.678077	43.478977
3503.986434	468035.213182	43.483981
3504.127414	468042.695428	43.488986
3503.580939	468031.677221	43.493991
3503.649446	468017.164503	43.498996
3503.603891	467999.526024	43.504001
3503.574510	468019.813138	43.509005
3503.623113	468027.259283	43.514010
3503.840002	468035.135182	43.519015
3503.878580	467987.769647	43.524020
3503.944066	467990.446760	43.529025
3503.204129	467995.076593	43.534029
3503.081745	467983.484271	43.539034
3503.662662	467961.335308	43.544039
3503.782282	468008.118208	43.549044
3503.502193	467988.894195	43.554049
3503.713415	467983.283173	43.559053
3503.484949	467967.194761	43.564058
3503.700834	467936.229883	43.569063
3503.507300	467960.548794	43.574068
3503.615876	467953.432802	43.579073
3503.828061	467928.705362	43.584077
3504.007724	467955.145663	43.589082
3503.585929	467969.004452	43.594087
3503.027128	467929.998312	43.599092
3503.474771	467913.650878	43.604097
3503.667174	467904.391955	43.609101
3503.531550	467923.580415	43.614106
3503.585812	467916.777233	43.619111
3503.508291	467953.247325	43.624116
3503.718376	467919.088847	43.629121
3503.401295	467938.255267	43.634125
3503.753404	467920.351044	43.639130
3503.568667	467897.917380	43.644135
3503.780188	467897.529042	43.649140
3503.875846	467899.897159	43.654145
3503.743760	467891.652938	43.659149
3503.703454	467907.682552	43.664154
3503.900756	467877.126175	43.669159
3503.415995	467879.180382	43.674164
3503.532927	467863.189418	43.679169
3503.095437	467850.379165	43.684173
3503.732730	467868.938447	43.689178
3503.506335	467861.064065	43.694183
3503.502548	467870.952455	43.699188
3503.485871	467881.451354	43.704193
3503.499816	467851.228158	43.709197
3503.765670	467890.230117	43.714202
3503.557996	467870.386073	43.719207
3503.610345	467833.057882	43.724212
3503.730277	467861.079644	43.729217
3503.666662	467826.660037	43.734221
3503.863688	467863.999607	43.739226
3503.711682	467842.422720	43.744231
3503.852734	467818.264164	43.749236
3503.181110	467839.210734	43.754241
3503.582200	467802.587966	43.759245
3503.902894	467808.317866	43.764250
3503.517215	467846.915817	43.769255
3503.544925	467813.495884	43.774260
3503.754185	467786.892597	43.779265
3503.262985	467787.984404	43.784269
3503.498669	467791.344534	43.789274
3503.770145	467831.917616	43.794279
3503.502127	467798.189454	43.799284
3503.851191	467764.718652	43.804289
3503.592006	467798.327445	43.809293
3503.582251	467785.094601	43.814298
3504.018042	467773.464647	43.819303
3503.983763	467764.596438	43.824308
3503.764486	467754.134850	43.829313
3503.853090	467744.486610	43.834317
3503.808178	467763.711584	43.839322
3503.773934	467724.520741	43.844327
3503.621618	467746.298045	43.849332
3503.738442	467702.722506	43.854337
3503.486808	467728.673484	43.859341
3504.034396	467695.221901	43.864346
3503.541031	467736.169589	43.869351
3503.318532	467708.518897	43.874356
3504.085510	467678.784916	43.879361
3503.626931	467703.602375	43.884365
3503.939138	467698.228852	43.889370
3503.900997	467654.221344	43.894375
3503.956397	467690.468054	43.899380
3503.581000	467641.595259	43.904385
3503.580502	467668.571465	43.909389
3503.634085	467650.815611	43.914394
3503.694938	467629.610518	43.919399
3503.694233	467673.928535	43.924404
3503.766602	467639.689957	43.929409
3504.107852	467647.698466	43.934413
3503.447894	467620.066093	43.939418
3503.616318	467616.236484	43.944423
3503.404557	467624.028166	43.949428
3503.679892	467595.690157	43.954433
3503.345891	467631.035081	43.959437
3504.174395	467590.693488	43.964442
3503.800466	467615.903328	43.969447
3503.313825	467593.060693	43.974452
3503.813841	467554.748526	43.979457
3503.453184	467599.579955	43.984461
3503.253085	467590.332225	43.989466
3503.853849	467558.291819	43.994471
3503.630364	467596.458935	43.999476
3503.619326	467568.774636	44.004481
3503.857112	467531.112359	44.009485
3503.869473	467541.758960	44.014490
3503.254688	467569.288748	44.019495
3503.039008	467564.100039	44.024500
3502.638837	467555.289573	44.029505
3502.828655	467556.882239	44.034509
3503.779346	467528.792347	44.039514
3503.430878	467523.624616	44.044519
3503.684248	467520.998538	44.049524
3503.807301	467531.678355	44.054529
3503.354941	467584.282516	44.059533
3503.753550	467552.679710	44.064538
3503.670185	467574.040636	44.069543
3503.349454	467559.639831	44.074548
3503.863020	467507.735913	44.079553
3503.395423	467545.586753	44.084557
3503.495501	467535.581653	44.089562
3503.563397	467514.426038	44.094567
3503.264127	467535.618299	44.099572
3503.662746	467505.891589	44.104577
3503.260646	467551.084623	44.109581
3503.479774	467541.060709	44.114586
3503.437005	467516.677326	44.119591
3503.115922	467548.217302	44.124596
3503.197857	467551.196114	44.129601
3503.636850	467512.639980	44.134605
3503.928050	467505.038607	44.139610
3503.567024	467525.834980	44.144615
3503.305015	467512.641835	44.149620
3504.019301	467495.896984	44.154625
3503.284999	467508.385663	44.159629
3503.720459	467485.904243	44.164634
3503.547545	467507.989292	44.169639
3503.633222	467512.235200	44.174644
3503.436223	467522.255706	44.179649
3502.920037	467496.882274	44.184653
3503.385202	467483.624885	44.189658
3503.456265	467526.410647	44.194663
3503.421172	467482.199470	44.199668
3503.680383	467510.453221	44.204673
3502.953565	467476.289986	44.209677
3503.543850	467500.485540	44.214682
3503.702755	467470.086765	44.219687
3503.247654	467500.988797	44.224692
3503.282670	467468.479894	44.229697
3503.503123	467500.593544	44.234701
3503.939053	467481.813678	44.239706
3503.673027	467484.796789	44.244711
3503.511181	467508.401309	44.249716
3503.504562	467488.525128	44.254721
3503.442806	467456.335745	44.259725
3503.463296	467480.519966	44.264730
3503.190855	467460.432236	44.269735
3503.662004	467430.541834	44.274740
3503.574568	467444.195997	44.279745
3503.380090	467476.882340	44.284749
3503.696442	467456.397301	44.289754
3503.284543	467479.230057	44.294759
3503.604790	467449.059287	44.299764
3503.406156	467474.799371	44.304769
3502.973661	467457.576548	44.309773
3503.476289	467454.403991	44.314778
3503.242482	467477.310016	44.319783
3503.467054	467452.732182	44.324788
3503.686642	467464.715169	44.329793
3503.459452	467465.613141	44.334797
3503.890479	467439.126487	44.339802
3503.475740	467434.729821	44.344807
3503.288424	467431.970554	44.349812
3503.792799	467439.395578	44.354817
3503.725537	467445.186896	44.359821
3503.680251	467441.644571	44.364826
3503.640518	467420.860826	44.369831
3503.507044	467444.359518	44.374836
3503.546596	467399.933540	44.379841
3503.541143	467419.913204	44.384845
3503.262081	467402.919623	44.389850
3503.625941	467386.128657	44.394855
3503.216339	467423.767718	44.399860
3503.386590	467406.449586	44.404865
3503.604507	467395.107399	44.409869
3503.370798	467433.631378	44.414874
3503.416068	467391.891975	44.419879
3503.624423	467417.111435	44.424884
3503.648291	467407.169027	44.429889
3503.423443	467424.698694	44.434893
3503.443567	467384.484476	44.439898
3503.743368	467394.122275	44.444903
3503.397780	467399.095568	44.449908
3503.991500	467387.186904	44.454913
3503.634632	467409.250423	44.459917
3504.133629	467381.941635	44.464922
3503.487555	467380.573268	44.469927
3503.846780	467355.669794	44.474932
3503.792569	467347.362344	44.479937
3503.913854	467353.783085	44.484941
3503.772116	467374.037871	44.489946
3503.455148	467340.063175	44.494951
3503.450866	467313.493044	44.499956
3503.669216	467341.854894	44.504961
3503.031712	467337.594831	44.509965
3503.659994	467301.695903	44.514970
3503.750052	467335.250232	44.519975
3503.772486	467350.813983	44.524980
3503.705123	467332.164239	44.529985
3503.422203	467313.447134	44.534989
3504.111443	467277.893485	44.539994
3503.906875	467325.236217	44.544999
3503.671747	467314.827624	44.550004
3503.865553	467299.026914	44.555009
3503.666525	467288.156232	44.560013
3503.176265	467267.646375	44.565018
3503.731634	467241.951148	44.570023
3503.889175	467221.186735	44.575028
3503.949865	467253.833091	44.580033
3503.266191	467278.534503	44.585037
3503.301511	467239.889551	44.590042
3503.580008	467256.579182	44.595047
3503.207135	467285.237385	44.600052
3503.690577	467293.477094	44.605057
3503.348037	467263.562940	44.610061
3503.986380	467211.790699	44.615066
3503.630478	467198.967154	44.620071
3503.458218	467239.611510	44.625076
3503.559653	467237.009411	44.630081
3503.191591	467226.216122	44.635085
3503.882718	467223.115154	44.640090
3503.919667	467255.156766	44.645095
3503.570897	467225.852038	44.650100
3503.661462	467192.421187	44.655105
3503.699827	467169.342989	44.660109
3503.716987	467179.025560	44.665114
3503.710576	467221.266396	44.670119
3503.292977	467195.978435	44.675124
3503.992717	467167.217817	44.680129
3503.564103	467198.978141	44.685133
3503.643148	467155.255320	44.690138
3503.517657	467126.929327	44.695143
3503.383576	467172.790722	44.700148
3503.549370	467163.484973	44.705153
3503.992510	467154.591757	44.710157
3503.734666	467145.809331	44.715162
3504.130169	467122.066136	44.720167
3503.515536	467124.140940	44.725172
3503.948319	467110.127813	44.730177
3503.566362	467156.332671	44.735181
3503.868106	467122.665500	44.740186
3503.847034	467083.065718	44.745191
3503.558844	467101.974788	44.750196
3503.832709	467094.781674	44.755201
3503.612124	467077.474339	44.760205
3503.845978	467075.409082	44.765210
3503.398069	467096.675984	44.770215
3503.392564	467062.499488	44.775220
3503.942433	467028.742242	44.780225
3503.615181	467047.556117	44.785229
3504.201188	467081.387421	44.790234
3503.997326	467067.119932	44.795239
3503.711749	467021.527548	44.800244
3504.074680	466979.027205	44.805249
3503.730931	467011.484316	44.810253
3503.705650	467040.696413	44.815258
3503.903722	467033.565967	44.820263
3503.971072	466996.842429	44.825268
3504.026307	466972.797888	44.830273
3503.526079	466995.138041	44.835277
3504.070296	466958.592608	44.840282
3503.707670	466964.785701	44.845287
3503.790659	466936.527919	44.850292
3503.624739	466953.693701	44.855297
3503.845238	466927.087557	44.860301
3503.985524	466957.693442	44.865306
3503.432342	466917.112572	44.870311
3503.636425	466890.154016	44.875316
3503.528193	466908.831979	44.880321
3503.644707	466902.931388	44.885325
3503.564438	466889.962673	44.890330
3503.451284	466911.683937	44.895335
3503.385160	466891.157387	44.900340
3503.733570	466898.404418	44.905345
3503.542102	466897.521961	44.910349
3503.904618	466859.433105	44.915354
3503.714177	466879.696061	44.920359
3503.485331	466878.058879	44.925364
3503.303688	466857.246301	44.930369
3503.677423	466854.499700	44.935373
3503.834912	466834.444840	44.940378
3503.762177	466853.573621	44.945383
3503.564615	466832.915662	44.950388
3503.510886	466854.779719	44.955393
3503.531402	466836.673446	44.960397
3503.698741	466848.360788	44.965402
3503.415117	466836.387649	44.970407
3503.349743	466850.038708	44.975412
3503.972639	466851.309434	44.980417
3503.562351	466825.664912	44.985421
3503.490507	466812.542691	44.990426
3503.339003	466795.883423	44.995431
3503.317841	466813.178565	45.000436
3503.531393	466812.232089	45.005441
3503.254344	466801.018526	45.010445
3503.621766	466814.144822	45.015450
3503.345091	466795.426270	45.020455
3503.111427	466825.685780	45.025460
3503.770952	466802.356877	45.030465
3503.516504	466813.654522	45.035469
3503.543820	466808.579348	45.040474
3503.778626	466795.611484	45.045479
3503.596001	466798.987180	45.050484
3503.676308	466776.054051	45.055489
3503.293028	466780.120683	45.060493
3503.652327	466797.355704	45.065498
3503.604528	466778.702381	45.070503
3503.258331	466777.033030	45.075508
3503.549252	466802.645845	45.080513
3503.106145	466782.584445	45.085517
3503.248632	466782.105581	45.090522
3503.517686	466804.273636	45.095527
3503.372935	466779.905522	45.100532
3503.509182	466788.251015	45.105537
3503.315615	466777.937006	45.110541
3503.534192	466802.800619	45.115546
3503.630750	466750.200122	45.120551
3503.241791	466779.267224	45.125556
3503.862773	466745.599706	45.130561
3503.432503	466774.825471	45.135565
3503.534749	466753.967921	45.140570
3503.197555	466773.341410	45.145575
3503.475355	466759.555385	45.150580
3503.634854	466765.463175	45.155585
3503.689694	466745.170909	45.160589
3503.837220	466756.607887	45.165594
3503.393826	466737.611380	45.170599
3502.989607	466749.439823	45.175604
3503.202590	466724.761559	45.180609
3503.234531	466740.425674	45.185613
3503.453706	466716.456350	45.190618
3503.320524	466762.217072	45.195623
3503.415413	466725.387293	45.200628
3503.658920	466719.415871	45.205633
3503.681222	466749.685741	45.210637
3503.884767	466704.623875	45.215642
3503.630431	466756.742409	45.220647
3503.254803	466728.404709	45.225652
3503.399253	466743.239694	45.230657
3503.254785	466743.668239	45.235661
3503.391438	466750.137444	45.240666
3503.335255	466739.142484	45.245671
3503.603993	466736.564590	45.250676
3503.403892	466708.401958	45.255681
3503.529101	466706.353838	45.260685
3503.804704	466702.202869	45.265690
3503.772221	466694.398821	45.270695
3503.364975	466724.685909	45.275700
3503.699064	466693.092020	45.280705
3503.449348	466728.120873	45.285709
3503.653481	466681.537591	45.290714
3503.647060	466711.812055	45.295719
3503.514159	466683.993732	45.300724
3503.679892	466653.339160	45.305729
3503.371908	466695.932965	45.310733
3503.789019	466653.321988	45.315738
3503.688586	466694.868804	45.320743
3503.270019	466675.462644	45.325748
3503.447275	466684.105951	45.330753
3503.456313	466677.715193	45.335757
3503.726759	466676.962556	45.340762
3503.703190	466657.544657	45.345767
3503.652402	466631.437405	45.350772
3503.732761	466652.570545	45.355777
3503.350650	466625.856432	45.360781
3503.426657	466653.582480	45.365786
3503.508189	466642.667122	45.370791
3503.603542	466626.577216	45.375796
3503.610454	466663.137607	45.380801
3503.484909	466641.200345	45.385805
3503.800736	466613.311006	45.390810
3503.636044	466592.039104	45.395815
3503.621476	466599.343608	45.400820
3503.700142	466623.671741	45.405825
3503.473535	466585.219123	45.410829
3503.725314	466624.732737	45.415834
3503.091723	466591.212557	45.420839
3503.502650	466545.356933	45.425844
3503.681983	466579.861831	45.430849
3503.715973	466550.799928	45.435853
3503.764230	466566.968689	45.440858
3503.334224	466572.462611	45.445863
3503.864457	466554.579792	45.450868
3503.757208	466578.075299	45.455873
3503.491572	466524.973685	45.460877
3503.534635	466545.859279	45.465882
3503.306401	466540.773721	45.470887
3503.648772	466511.764443	45.475892
3503.730234	466506.629928	45.480897
3503.447027	466504.747760	45.485901
3503.600754	466494.175883	45.490906
3503.585517	466531.500647	45.495911
3503.229621	466562.185528	45.500916
3503.762529	466521.330818	45.505921
3503.480181	466540.847979	45.510925
3503.291448	466509.336451	45.515930
3502.976588	466512.530254	45.520935
3503.652323	466491.125417	45.525940
3503.359946	466522.053865	45.530945
3503.470972	466489.784994	45.535949
3503.743626	466471.182170	45.540954
3503.526062	466526.236624	45.545959
3503.406027	466499.734477	45.550964
3503.687496	466484.172853	45.555969
3503.393068	466540.912839	45.560973
3503.410002	466503.638610	45.565978
3503.626218	466498.026407	45.570983
3503.332006	466510.293983	45.575988
3503.340102	466467.493731	45.580993
3503.525602	466480.040472	45.585997
3503.275649	466457.412747	45.591002
3503.181047	466483.188301	45.596007
3503.488544	466471.070816	45.601012
3503.392575	466487.566692	45.606017
3503.454027	466456.624059	45.611021
3503.476627	466492.117358	45.616026
3503.544959	466470.301406	45.621031
3503.857563	466469.998486	45.626036
3503.492893	466505.147296	45.631041
3503.580485	466464.869959	45.636045
3503.563060	466484.700268	45.641050
3503.670743	466446.143851	45.646055
3503.485719	466465.138601	45.651060
3503.580004	466434.900684	45.656065
3503.318700	466469.830375	45.661069
3503.525594	466424.108158	45.666074
3503.048336	466429.305326	45.671079
3503.503872	466461.535527	45.676084
3503.493367	466448.809064	45.681089
3503.313267	466434.486683	45.686093
3503.521343	466472.739742	45.691098
3503.317880	466459.131007	45.696103
3503.485549	466436.893641	45.701108
3503.854832	466475.577603	45.706113
3503.768926	466425.743468	45.711117
3503.553988	466442.765280	45.716122
3503.697310	466412.012482	45.721127
3503.545415	466447.026337	45.726132
3503.311390	466426.120195	45.731137
3503.651497	466416.938698	45.736141
3503.669050	466443.051544	45.741146
3503.489250	466413.769695	45.746151
3503.442684	466414.689871	45.751156
3503.565506	466375.268864	45.756161
3503.825083	466402.966226	45.761165
3503.638548	466376.322306	45.766170
3503.494574	466393.028682	45.771175
3503.438098	466390.045759	45.776180
3503.817125	466388.109621	45.781185
3503.330360	466393.206881	45.786189
3503.742577	466354.855715	45.791194
3503.587916	466361.269664	45.796199
3503.329863	466390.012347	45.801204
3503.575424	466352.549587	45.806209
3503.495613	466396.274260	45.811213
3503.625526	466382.054975	45.816218
3503.454976	466369.658020	45.821223
3503.745767	466369.612097	45.826228
3503.767051	466370.521551	45.831233
3503.595208	466327.293068	45.836237
3503.684411	466307.907735	45.841242
3503.448483	466362.407704	45.846247
3503.507537	466326.901358	45.851252
3503.694546	466316.983364	45.856257
3503.212493	466331.968369	45.861261
3503.500985	466341.709857	45.866266
3503.670515	466316.023784	45.871271
3503.391543	466341.777941	45.876276
3503.743954	466317.736398	45.881281
3503.204859	466307.527483	45.886285
3503.487389	466302.969661	45.891290
3503.503621	466291.354501	45.896295
3503.094064	466306.226645	45.901300
3503.335294	466303.703757	45.906305
3502.866336	466302.003061	45.911309
3503.387975	466274.435719	45.916314
3503.211832	466331.056149	45.921319
3503.287093	466313.245038	45.926324
3503.325999	466288.086680	45.931329
3503.424768	466310.332876	45.936333
3503.393730	466303.491948	45.941338
3503.756094	466305.361699	45.946343
3503.424897	466328.892878	45.951348
3503.296750	466293.872456	45.956353
3503.412455	466286.044835	45.961357
3503.208655	466303.217130	45.966362
3503.561978	466334.550896	45.971367
3503.176259	466341.052080	45.976372
3503.627539	466341.893573	45.981377
3503.412746	466340.406257	45.986381
3503.422553	466342.940249	45.991386
3503.356015	466326.824994	45.996391
3503.177178	466323.202170	46.001396
3503.540331	466313.154913	46.006401
3503.238783	466333.385242	46.011405
3503.668147	466291.126573	46.016410
3503.466692	466284.566125	46.021415
3503.409866	466316.167585	46.026420
3503.105252	466288.071623	46.031425
3503.631861	466268.110018	46.036429
3503.725063	466282.395612	46.041434
3503.763830	466268.799179	46.046439
3503.799780	466295.416401	46.051444
3503.784180	466272.751439	46.056449
3503.581473	466271.870731	46.061453
3503.751072	466264.998079	46.066458
3503.699488	466243.251557	46.071463
3504.047784	466215.356565	46.076468
3503.890888	466247.227496	46.081473
3503.813223	466212.655354	46.086477
3503.238226	466208.283759	46.091482
3503.494649	466233.192769	46.096487
3503.097923	466205.922622	46.101492
3503.567588	466190.888854	46.106497
3503.866848	466182.423658	46.111501
3503.716175	466220.632452	46.116506
3503.687990	466241.631026	46.121511
3503.577736	466193.372214	46.126516
3504.001314	466193.305303	46.131521
3503.255836	466183.636052	46.136525
3503.519751	466159.354766	46.141530
3503.608255	466199.047111	46.146535
3503.386453	466187.368095	46.151540
3503.664128	466161.157639	46.156545
3503.755523	466202.776519	46.161549
3503.817484	466174.216784	46.166554
3503.666232	466127.536327	46.171559
3503.383116	466162.723522	46.176564
3503.922785	466146.309474	46.181569
3503.511585	466120.157137	46.186573
3503.397631	466166.423209	46.191578
3503.568676	466150.422401	46.196583
3503.608249	466129.929118	46.201588
3503.646803	466149.446628	46.206593
3503.654318	466150.408979	46.211597
3503.871881	466140.232521	46.216602
3503.904788	466131.099455	46.221607
3503.514969	466138.767692	46.226612
3503.749362	466134.623127	46.231617
3503.184533	466117.369417	46.236621
3503.269491	466093.065629	46.241626
3503.310557	466064.001942	46.246631
3503.098758	466068.700844	46.251636
3503.962962	466046.150136	46.256641
3503.522829	466067.619679	46.261645
3503.848177	466089.627451	46.266650
3503.423589	466073.670017	46.271655
3503.299490	466087.381559	46.276660
3503.950970	466074.347399	46.281665
3503.697699	466058.007900	46.286669
3503.996780	466029.004806	46.291674
3503.779141	466056.423071	46.296679
3503.214169	466037.495863	46.301684
3503.720709	465999.382703	46.306689
3503.637462	466005.430494	46.311693
3503.365318	466055.525126	46.316698
3503.735060	466061.349172	46.321703
3503.158873	466030.405280	46.326708
3503.475965	465997.443852	46.331713
3503.910368	465981.604135	46.336717
3503.563715	465962.338087	46.341722
3503.672446	465973.274509	46.346727
3503.688129	466015.463543	46.351732
3503.669985	466006.744180	46.356737
3503.707318	465983.969122	46.361741
3504.174917	465955.040714	46.366746
3503.915322	465981.705041	46.371751
3503.476448	466005.050752	46.376756
3503.540926	465975.831112	46.381761
3503.588432	465982.416064	46.386765
3503.179284	465950.634279	46.391770
3503.690630	465929.204150	46.396775
3503.736126	465909.825363	46.401780
3503.814166	465887.804434	46.406785
3503.376430	465894.922509	46.411789
3503.945762	465890.319269	46.416794
3503.539300	465891.042796	46.421799
3503.134435	465936.645391	46.426804
3503.139715	465923.966830	46.431809
3502.844011	465920.210275	46.436813
3502.961417	465921.155267	46.441818
3503.559021	465906.506766	46.446823
3503.428646	465914.590476	46.451828
3503.469447	465914.939043	46.456833
3503.646391	465897.567913	46.461837
3503.525838	465940.590006	46.466842
3503.593361	465931.349961	46.471847
3503.637609	465887.376474	46.476852
3503.749201	465870.015651	46.481857
3503.667542	465864.196806	46.486861
3503.561235	465874.913711	46.491866
3503.619439	465879.164289	46.496871
3503.562908	465907.165816	46.501876
3503.756857	465917.632397	46.506881
3503.209018	465898.600935	46.511885
3503.436758	465877.418424	46.516890
3503.328612	465856.238269	46.521895
3503.535214	465837.442488	46.526900
3503.567631	465820.854807	46.531905
3503.540079	465821.974849	46.536909
3503.365142	465856.587627	46.541914
3503.454876	465886.848068	46.546919
3503.611560	465878.101020	46.551924
3503.218151	465864.724770	46.556929
3503.549062	465846.771440	46.561933
3503.589225	465858.175160	46.566938
3503.571972	465890.988066	46.571943
3503.104781	465839.945043	46.576948
3503.099661	465859.419011	46.581953
3503.230915	465862.085999	46.586957
3503.838004	465863.967821	46.591962
3503.136586	465873.308161	46.596967
3503.354773	465831.284803	46.601972
3503.608561	465812.887232	46.606977
3503.443771	465869.963496	46.611981
3503.416255	465850.849751	46.616986
3503.230926	465836.882772	46.621991
3502.775709	465844.003627	46.626996
3502.898504	465846.874798	46.632001
3503.276753	465857.464414	46.637005
3503.269932	465868.165597	46.642010
3503.240361	465880.543840	46.647015
3503.096484	465873.771320	46.652020
3502.961933	465842.148816	46.657025
3503.055005	465869.873190	46.662029
3503.004627	465885.398813	46.667034
3503.740061	465885.789724	46.672039
3503.681335	465917.747054	46.677044
3503.663259	465898.834705	46.682049
3503.121787	465873.311187	46.687053
3503.750708	465888.780153	46.692058
3503.645754	465883.573529	46.697063
3503.556701	465883.283376	46.702068
3503.554228	465868.476138	46.707073
3503.559982	465843.728183	46.712077
3503.647744	465846.706315	46.717082
3503.569275	465848.037248	46.722087
3503.384472	465806.787494	46.727092
3503.585886	465805.944316	46.732097
3503.273120	465829.929534	46.737101
3503.399499	465797.099363	46.742106
3503.584814	465775.872745	46.747111
3503.477647	465814.379659	46.752116
3503.730388	465810.181421	46.757121
3503.750302	465803.078722	46.762125
3503.419348	465848.314845	46.767130
3503.323702	465847.924310	46.772135
3503.293284	465849.602627	46.777140
3503.491888	465832.836556	46.782145
3503.546374	465774.611340	46.787149
3503.777283	465756.825874	46.792154
3503.904494	465758.682131	46.797159
3502.915546	465786.831189	46.802164
3503.039491	465784.174644	46.807169
3503.489509	465778.728144	46.812173
3503.272444	465764.918269	46.817178
3503.251636	465770.956258	46.822183
3503.385251	465818.603876	46.827188
3503.616561	465824.804847	46.832193
3503.437286	465813.017482	46.837197
3503.206787	465788.661784	46.842202
3503.673491	465777.482258	46.847207
3503.538064	465783.132669	46.852212
3503.840467	465761.076147	46.857217
3503.618792	465741.638012	46.862221
3503.261918	465766.238812	46.867226
3503.306919	465765.268220	46.872231
3503.167597	465731.415002	46.877236
3503.625462	465729.212788	46.882241
3503.495132	465753.625661	46.887245
3503.253671	465750.925443	46.892250
3503.572330	465776.129421	46.897255
3503.300753	465796.355521	46.902260
3503.282189	465803.407374	46.907265
3503.430583	465759.924276	46.912269
3503.438619	465734.871566	46.917274
3503.093232	465769.815695	46.922279
3503.553116	465791.041841	46.927284
3503.650753	465793.562016	46.932289
3503.135745	465795.418352	46.937293
3503.518538	465772.639178	46.942298
3503.977273	465740.111368	46.947303
3502.839530	465755.961083	46.952308
3502.872863	465758.795696	46.957313
3503.191857	465773.400924	46.962317
3503.086478	465770.729912	46.967322
3503.603156	465743.111957	46.972327
3503.536114	465787.038709	46.977332
3503.562908	465793.474860	46.982337
3503.162306	465750.636340	46.987341
3503.133986	465718.236190	46.992346
3503.290361	465766.083175	46.997351
3502.897749	465783.032174	47.002356
3503.380208	465799.690715	47.007361
3503.395832	465810.439092	47.012365
3503.317637	465814.508396	47.017370
3503.323841	465804.213050	47.022375
3503.177249	465792.724776	47.027380
3503.879780	465754.681625	47.032385
3503.469213	465767.931535	47.037389
3503.157164	465787.048390	47.042394
3503.603305	465780.537564	47.047399
3503.135376	465765.296708	47.052404
3502.658913	465762.988615	47.057409
3502.588570	465769.034434	47.062413
3503.302035	465780.636045	47.067418
3503.801095	465773.406894	47.072423
3503.453407	465799.223278	47.077428
3503.425404	465795.982214	47.082433
3503.304908	465773.333299	47.087437
3503.188454	465747.083205	47.092442
3503.509846	465761.840197	47.097447
3503.198049	465779.942788	47.102452
3502.901600	465765.334077	47.107457
3503.966735	465743.562676	47.112461
3503.949441	465729.771914	47.117466
3503.662438	465737.424044	47.122471
3503.360303	465734.581279	47.127476
3503.830973	465732.529176	47.132481
3503.579078	465737.437333	47.137485
3502.843931	465731.671029	47.142490
3503.181119	465742.672884	47.147495
3503.401091	465753.439702	47.152500
3503.407729	465777.171651	47.157505
3503.498188	465775.433203	47.162509
3503.634172	465723.635317	47.167514
3503.820301	465703.067749	47.172519
3503.536893	465701.489810	47.177524
3503.927391	465694.784907	47.182529
3504.005600	465701.517228	47.187533
3503.558349	465686.475893	47.192538
3503.914309	465671.561155	47.197543
3503.891321	465672.071943	47.202548
3503.051067	465698.169149	47.207553
3503.437191	465718.899908	47.212557
3503.536245	465721.166311	47.217562
3503.468433	465727.161030	47.222567
3503.321266	465698.887269	47.227572
3503.379482	465660.235824	47.232577
3503.710969	465659.067812	47.237581
3503.146580	465674.573407	47.242586
3503.480047	465688.060750	47.247591
3503.323402	465700.002778	47.252596
3503.543803	465653.363962	47.257601
3503.636210	465641.736409	47.262605
3503.023699	465658.263857	47.267610
3503.667013	465666.428222	47.272615
3503.380690	465674.942365	47.277620
3503.681222	465689.144877	47.282625
3503.668454	465690.566858	47.287629
3503.274582	465691.136266	47.292634
3503.421827	465686.599696	47.297639
3503.364394	465695.787617	47.302644
3503.494051	465688.261841	47.307649
3503.062210	465680.774099	47.312653
3503.398408	465664.898958	47.317658
3503.988442	465633.973008	47.322663
3503.510277	465666.402704	47.327668
3503.581659	465638.702860	47.332673
3503.919302	465619.379057	47.337677
3503.585745	465637.028803	47.342682
3503.595961	465621.915117	47.347687
3503.631820	465650.561632	47.352692
3503.869310	465587.489366	47.357697
3503.556213	465620.805855	47.362701
3503.282060	465610.250456	47.367706
3502.915515	465590.226539	47.372711
3503.590201	465572.928609	47.377716
3503.732986	465602.268254	47.382721
3503.525304	465625.324281	47.387725
3503.463150	465627.159767	47.392730
3503.716632	465635.081489	47.397735
3503.295378	465623.535112	47.402740
3503.566860	465631.301855	47.407745
3503.204290	465612.190141	47.412749
3503.353772	465601.111374	47.417754
3503.544978	465581.050004	47.422759
3502.878626	465571.317254	47.427764
3504.082020	465536.186552	47.432769
3503.698429	465548.925214	47.437773
3503.143888	465557.076102	47.442778
3503.639336	465539.552915	47.447783
3503.296371	465552.538714	47.452788
3503.532433	465590.636799	47.457793
3503.595104	465603.254183	47.462797
3503.468462	465586.133630	47.467802
3503.339033	465575.758187	47.472807
3502.951392	465580.130006	47.477812
3503.706518	465591.674424	47.482817
3503.438003	465573.207064	47.487821
3503.631590	465523.681624	47.492826
3503.166054	465534.455478	47.497831
3503.218517	465556.861917	47.502836
3503.590012	465541.741784	47.507841
3503.149807	465521.070188	47.512845
3503.063735	465506.174488	47.517850
3503.396521	465514.387993	47.522855
3502.803306	465541.409872	47.527860
3503.044394	465560.540927	47.532865
3502.773881	465581.679877	47.537869
3502.871627	465581.512330	47.542874
3503.343609	465574.946647	47.547879
3503.104321	465589.133122	47.552884
3503.302503	465598.229971	47.557889
3503.475211	465602.411795	47.562893
3503.277465	465621.764290	47.567898
3503.725413	465622.606340	47.572903
3503.327881	465626.827577	47.577908
3503.662634	465634.584318	47.582913
3503.674095	465620.738229	47.587917
3503.728611	465588.324789	47.592922
3502.840417	465562.196445	47.597927
3503.601285	465539.813673	47.602932
3503.602607	465525.563428	47.607937
3503.723518	465583.001000	47.612941
3503.535396	465572.634832	47.617946
3503.864263	465538.859444	47.622951
3503.663364	465545.331658	47.627956
3503.496132	465561.332394	47.632961
3503.400292	465554.298620	47.637965
3503.652906	465543.355658	47.642970
3503.179469	465522.587892	47.647975
3503.478215	465498.503196	47.652980
3503.910101	465536.925411	47.657985
3503.743864	465524.932978	47.662989
3503.133005	465520.668331	47.667994
3503.567684	465506.298868	47.672999
3503.912447	465488.799456	47.678004
3503.655159	465488.637311	47.683009
3503.387959	465519.258962	47.688013
3503.254850	465494.278990	47.693018
3503.627624	465484.787657	47.698023
3503.058325	465480.617858	47.703028
3503.366653	465493.095055	47.708033
3503.463117	465507.482078	47.713037
3503.100454	465491.666555	47.718042
3503.227814	465483.836798	47.723047
3502.968419	465491.281803	47.728052
3503.706586	465471.133880	47.733057
3503.321697	465478.902997	47.738061
3502.795901	465480.710353	47.743066
3503.201013	465484.652619	47.748071
3503.781141	465477.562691	47.753076
3504.056471	465460.581352	47.758081
3504.011697	465507.345042	47.763085
3503.591582	465498.486156	47.768090
3503.268446	465463.140202	47.773095
3503.561938	465436.926356	47.778100
3503.546106	465458.126600	47.783105
3503.612394	465484.182206	47.788109
3503.283308	465494.427392	47.793114
3503.460589	465485.372655	47.798119
3503.419267	465472.041933	47.803124
3503.193178	465453.618476	47.808129
3503.145489	465442.367942	47.813133
3503.085024	465481.375198	47.818138
3503.579528	465437.532467	47.823143
3503.411810	465483.909942	47.828148
3503.368135	465486.756762	47.833153
3502.784255	465461.797287	47.838157
3503.625629	465443.560087	47.843162
3503.522581	465455.645917	47.848167
3503.241259	465501.990597	47.853172
3503.072313	465473.922828	47.858177
3503.692305	465451.207245	47.863181
3503.609511	465505.127368	47.868186
3503.525302	465485.515136	47.873191
3503.298987	465450.407418	47.878196
3503.470197	465429.740520	47.883201
3503.914231	465401.829333	47.888205
3503.297062	465441.178214	47.893210
3503.160635	465432.578736	47.898215
3503.763550	465407.989453	47.903220
3503.564423	465431.957157	47.908225
3503.336502	465442.794925	47.913229
3503.442693	465417.219205	47.918234
3503.914512	465444.326434	47.923239
3503.482160	465415.539538	47.928244
3503.512468	465416.650456	47.933249
3503.364579	465414.696090	47.938253
3503.557519	465388.853064	47.943258
3503.824376	465429.482188	47.948263
3503.251500	465419.379607	47.953268
3503.141769	465394.294399	47.958273
3503.786105	465385.774347	47.963277
3503.723060	465434.366729	47.968282
3503.511228	465414.521042	47.973287
3503.846925	465374.810977	47.978292
3503.661810	465366.827717	47.983297
3503.894203	465406.701644	47.988301
3503.833006	465367.358571	47.993306
3503.898453	465356.850796	47.998311
3503.625035	465340.767493	48.003316
3503.531378	465348.084927	48.008321
3503.932265	465321.853966	48.013325
3503.738734	465330.404292	48.018330
3503.624549	465332.248027	48.023335
3503.760243	465321.881270	48.028340
3503.782535	465305.497639	48.033345
3503.602503	465315.668639	48.038349
3503.822109	465282.214390	48.043354
3503.957367	465297.102549	48.048359
3503.724195	465300.131482	48.053364
3503.885676	465286.007902	48.058369
3503.921072	465264.905898	48.063373
3503.978081	465272.858808	48.068378
3503.741694	465251.749035	48.073383
3503.994011	465254.498390	48.078388
3503.581354	465241.276928	48.083393
3503.992732	465195.367619	48.088397
3503.486656	465234.141481	48.093402
3503.689497	465185.729475	48.098407
3503.231992	465233.522543	48.103412
3503.251555	465236.410114	48.108417
3503.415382	465213.056399	48.113421
3503.398449	465191.151189	48.118426
3503.347971	465235.837149	48.123431
3503.353589	465245.978839	48.128436
3503.185502	465195.799827	48.133441
3503.295661	465188.175531	48.138445
3503.332207	465239.744672	48.143450
3503.218488	465207.458669	48.148455
3503.391077	465187.856288	48.153460
3503.490940	465196.461721	48.158465
3504.055438	465149.361717	48.163469
3503.656945	465167.022113	48.168474
3503.586598	465188.839794	48.173479
3503.532137	465200.461673	48.178484
3503.362787	465178.681966	48.183489
3503.271224	465182.195662	48.188493
3503.547048	465161.309118	48.193498
3503.825539	465183.680224	48.198503
3503.538095	465184.435673	48.203508
3503.227581	465134.380454	48.208513
3503.662367	465152.010584	48.213517
3503.106018	465143.984489	48.218522
3503.623359	465126.711070	48.223527
3503.160819	465152.495674	48.228532
3503.535156	465128.652180	48.233537
3503.693355	465154.186532	48.238541
3503.616140	465129.653715	48.243546
3503.527185	465149.395146	48.248551
3503.455220	465113.755350	48.253556
3503.591516	465156.079158	48.258561
3503.476449	465099.349575	48.263565
3503.758254	465106.607747	48.268570
3503.565141	465115.158093	48.273575
3503.819883	465090.268486	48.278580
3503.611578	465124.989149	48.283585
3503.886198	465091.424481	48.288589
3503.732148	465094.390224	48.293594
3503.952353	465075.794475	48.298599
3503.659599	465051.802767	48.303604
3503.833518	465018.203188	48.308609
3504.105278	465056.448724	48.313613
3503.999776	465070.360831	48.318618
3503.632166	465030.507724	48.323623
3504.063166	465001.533099	48.328628
3503.753007	465022.831007	48.333633
3503.874741	464975.597749	48.338637
3503.891768	464994.308305	48.343642
3503.576631	464981.527689	48.348647
3503.660353	464992.519280	48.353652
3503.472148	464972.821588	48.358657
3503.733230	464949.046507	48.363661
3503.585919	464929.190171	48.368666
3503.638320	464911.330790	48.373671
3503.400139	464942.760094	48.378676
3503.232292	464963.477720	48.383681
3503.482045	464941.732956	48.388685
3503.685421	464917.104834	48.393690
3503.801789	464958.722194	48.398695
3503.473464	464970.336770	48.403700
3503.362851	464950.373226	48.408705
3503.843524	464909.827971	48.413709
3503.328924	464938.816009	48.418714
3503.549641	464921.335741	48.423719
3503.650320	464906.004397	48.428724
3503.860590	464881.020149	48.433729
3503.719762	464917.556171	48.438733
3502.825829	464915.263254	48.443738
3503.725573	464898.132063	48.448743
3503.377694	464907.214088	48.453748
3503.523987	464888.984854	48.458753
3503.445354	464928.401698	48.463757
3503.228066	464897.906568	48.468762
3503.540697	464888.728760	48.473767
3503.356367	464909.195476	48.478772
3503.158168	464876.263051	48.483777
3503.804131	464844.464991	48.488781
3503.540196	464879.600554	48.493786
3503.981109	464848.849181	48.498791
3503.556392	464895.522120	48.503796
3503.150610	464888.283547	48.508801
3504.108449	464866.376077	48.513805
3503.667474	464885.970535	48.518810
3503.357935	464857.772037	48.523815
3503.254718	464822.187409	48.528820
3503.275097	464849.062465	48.533825
3503.465228	464821.799217	48.538829
3503.195985	464822.095379	48.543834
3503.304819	464856.208502	48.548839
3503.282930	464822.893132	48.553844
3503.527763	464852.116252	48.558849
3503.472115	464835.896721	48.563853
3503.083464	464834.233923	48.568858
3503.358036	464848.035389	48.573863
3503.186580	464833.862706	48.578868
3503.133138	464859.075866	48.583873
3503.526040	464825.390659	48.588877
3503.216620	464849.985011	48.593882
3503.265041	464832.481188	48.598887
3503.209718	464857.390366	48.603892
3503.337814	464848.444561	48.608897
3503.364056	464836.167750	48.613901
3503.336850	464867.665246	48.618906
3503.669130	464828.715413	48.623911
3503.119641	464855.071968	48.628916
3503.685607	464825.923633	48.633921
3503.549751	464864.386079	48.638925
3503.767563	464844.370527	48.643930
3503.339993	464854.378016	48.648935
3503.706356	464806.040734	48.653940
3503.662077	464834.396726	48.658945
3503.653295	464805.187063	48.663949
3503.541958	464797.039787	48.668954
3503.690793	464838.652249	48.673959
3503.316344	464817.361013	48.678964
3503.179965	464794.814998	48.683969
3503.399443	464832.815628	48.688973
3503.116706	464801.215005	48.693978
3503.215714	464840.756074	48.698983
3503.302937	464835.721675	48.703988
3503.534942	464823.209480	48.708993
3503.529201	464815.248375	48.713997
3503.458456	464836.407200	48.719002
3503.708861	464804.215178	48.724007
3503.370140	464798.791669	48.729012
3503.723433	464769.626158	48.734017
3503.996032	464771.915946	48.739021
3503.777510	464746.441462	48.744026
3503.533188	464801.048170	48.749031
3503.488506	464782.088323	48.754036
3503.556367	464766.660639	48.759041
3503.473223	464752.372517	48.764045
3503.254612	464743.430753	48.769050
3503.493877	464735.684464	48.774055
3503.544454	464754.643496	48.779060
3503.183432	464736.342174	48.784065
3503.441078	464753.087782	48.789069
3503.333629	464737.789214	48.794074
3503.264984	464768.380556	48.799079
3503.577706	464718.073715	48.804084
3503.584916	464754.180905	48.809089
3503.071802	464743.713560	48.814093
3503.241553	464725.886191	48.819098
3503.430458	464721.292118	48.824103
3503.332430	464764.870871	48.829108
3503.072537	464767.396964	48.834113
3503.748444	464728.696920	48.839117
3503.291047	464769.391056	48.844122
3503.638085	464733.937971	48.849127
3503.135087	464759.222304	48.854132
3503.326893	464748.339262	48.859137
3503.586502	464741.299753	48.864141
3503.522210	464755.205551	48.869146
3503.629533	464695.751914	48.874151
3503.285843	464726.234646	48.879156
3503.395973	464717.393054	48.884161
3503.547646	464703.625638	48.889165
3503.445936	464709.271002	48.894170
3503.262994	464718.174896	48.899175
3503.769732	464714.443438	48.904180
3503.678433	464708.727230	48.909185
3503.514249	464710.021067	48.914189
3503.198005	464729.190242	48.919194
3503.625938	464705.489948	48.924199
3503.519570	464690.444745	48.929204
3503.306574	464690.022022	48.934209
3503.504620	464680.405809	48.939213
3503.372000	464668.559724	48.944218
3503.465789	464695.829081	48.949223
3503.549101	464656.360432	48.954228
3503.760568	464690.102599	48.959233
3503.801956	464674.425463	48.964237
3503.527242	464696.884515	48.969242
3503.758048	464660.333972	48.974247
3503.641889	464669.582329	48.979252
3503.299426	464633.883059	48.984257
3503.235848	464653.012367	48.989261
3502.924135	464642.614568	48.994266
3503.601853	464614.411851	48.999271
3503.086052	464668.554664	49.004276
3503.024999	464640.975889	49.009281
3503.406766	464644.972716	49.014285
3503.016911	464649.547928	49.019290
3503.568591	464639.520804	49.024295
3503.595766	464641.595826	49.029300
3503.820240	464640.495389	49.034305
3503.486212	464664.535987	49.039309
3503.681037	464637.728190	49.044314
3503.846758	464639.882742	49.049319
3503.454901	464684.065955	49.054324
3503.311270	464620.797509	49.059329
3503.771030	464623.919872	49.064333
3503.043480	464622.412050	49.069338
3503.991137	464592.594500	49.074343
3503.549881	464626.490648	49.079348
3503.512687	464594.293054	49.084353
3503.634128	464627.593120	49.089357
3503.252884	464616.597728	49.094362
3503.946925	464592.043823	49.099367
3503.442521	464619.458540	49.104372
3503.314302	464576.980327	49.109377
3503.678179	464549.435701	49.114381
3503.276759	464595.497038	49.119386
3503.284800	464554.670814	49.124391
3503.657689	464564.551920	49.129396
3503.317018	464593.614363	49.134401
3503.274193	464562.381181	49.139405
3503.167025	464586.386010	49.144410
3503.793118	464556.314950	49.149415
3503.204210	464599.515196	49.154420
3503.374376	464562.771214	49.159425
3503.889250	464594.639861	49.164429
3503.685105	464566.931465	49.169434
3503.522972	464577.099985	49.174439
3503.657011	464539.600960	49.179444
3503.455252	464534.764308	49.184449
3503.434455	464547.091222	49.189453
3503.511481	464553.722663	49.194458
3503.649669	464534.530836	49.199463
3503.330565	464528.394157	49.204468
3503.052511	464548.977459	49.209473
3503.619252	464536.310761	49.214477
3503.328669	464534.886011	49.219482
3503.139997	464544.906599	49.224487
3503.637983	464543.712212	49.229492
3503.317861	464528.396394	49.234497
3503.283047	464544.934818	49.239501
3503.420699	464541.058808	49.244506
3503.418359	464531.727773	49.249511
3503.375284	464524.837463	49.254516
3503.022166	464517.894726	49.259521
3503.522415	464488.046318	49.264525
3503.015449	464534.479470	49.269530
3502.983896	464527.790197	49.274535
3503.275201	464532.004201	49.279540
3503.322841	464542.798869	49.284545
3503.051167	464538.581841	49.289549
3502.819104	464548.761428	49.294554
3503.671783	464520.328077	49.299559
3503.633640	464555.783482	49.304564
3503.369327	464575.096730	49.309569
3503.528855	464533.029379	49.314573
3503.242216	464532.567578	49.319578
3503.379820	464528.133716	49.324583
3503.922037	464500.915841	49.329588
3503.176494	464521.623773	49.334593
3503.387582	464496.030374	49.339597
3503.199851	464517.867291	49.344602
3503.360391	464510.843366	49.349607
3503.307001	464506.338258	49.354612
3503.349870	464524.994425	49.359617
3503.650335	464490.106157	49.364621
3503.179857	464529.179953	49.369626
3503.229173	464512.842159	49.374631
3503.549125	464519.688787	49.379636
3503.465418	464523.911351	49.384641
3503.392319	464513.323631	49.389645
3503.363731	464534.932520	49.394650
3504.030557	464493.596341	49.399655
3503.483426	464506.919328	49.404660
3503.323075	464492.947522	49.409665
3503.731331	464473.205810	49.414669
3503.128293	464495.564822	49.419674
3503.635524	464469.011724	49.424679
3503.340571	464474.839836	49.429684
3503.265978	464491.739590	49.434689
3503.441196	464482.025468	49.439693
3503.180257	464459.650931	49.444698
3503.414854	464487.354729	49.449703
3503.651509	464469.060141	49.454708
3503.375389	464493.649638	49.459713
3503.741824	464477.363123	49.464717
3503.414327	464471.329183	49.469722
3503.179630	464501.896435	49.474727
3503.409364	464466.968594	49.479732
3503.061037	464490.605931	49.484737
3503.623220	464457.096249	49.489741
3503.017665	464475.702802	49.494746
3503.260041	464458.827308	49.499751
3503.415355	464475.487878	49.504756
3502.762954	464477.416754	49.509761
3503.458650	464459.810322	49.514765
3502.990426	464511.866713	49.519770
3503.288314	464470.791660	49.524775
3503.204084	464496.618687	49.529780
3503.567996	464506.856239	49.534785
3503.418773	464476.654038	49.539789
3503.236749	464509.393679	49.544794
3503.431481	464490.294304	49.549799
3503.579858	464480.888711	49.554804
3503.546419	464460.658940	49.559809
3503.482235	464481.969221	49.564813
3503.418836	464434.611890	49.569818
3503.202763	464462.184093	49.574823
3503.278968	464431.591197	49.579828
3502.831635	464470.915013	49.584833
3503.182509	464452.348786	49.589837
3503.119269	464465.291030	49.594842
3503.104913	464464.076188	49.599847
3503.326580	464455.876149	49.604852
3503.105745	464464.177562	49.609857
3503.565613	464464.612061	49.614861
3503.361544	464458.862895	49.619866
3503.569607	464460.554343	49.624871
3503.451856	464458.341552	49.629876
3503.617112	464459.938336	49.634881
3503.651430	464447.406453	49.639885
3503.359694	464471.694156	49.644890
3503.796478	464474.313027	49.649895
3503.749895	464451.296027	49.654900
3503.377635	464476.509313	49.659905
3503.400542	464421.987566	49.664909
3503.151165	464450.832914	49.669914
3503.442623	464410.671625	49.674919
3503.384132	464446.688288	49.679924
3503.343328	464423.112484	49.684929
3503.494164	464439.621646	49.689933
3503.275397	464422.717580	49.694938
3503.196332	464442.610243	49.699943
3503.233050	464410.045687	49.704948
3503.316985	464445.938412	49.709953
3503.431343	464447.086810	49.714957
3503.479372	464432.067737	49.719962
3503.318862	464444.822509	49.724967
3503.737161	464409.864772	49.729972
3503.412648	464456.066396	49.734977
3503.673169	464416.112865	49.739981
3503.292969	464431.285956	49.744986
3503.228932	464453.001960	49.749991
3503.611184	464432.300744	49.754996
3503.440841	464442.927057	49.760001
3503.444080	464437.753695	49.765005
3503.006089	464442.742275	49.770010
3503.356533	464423.567516	49.775015
3503.245210	464440.625259	49.780020
3503.198001	464449.457096	49.785025
3503.726648	464421.987693	49.790029
3503.424786	464442.067714	49.795034
3503.385268	464398.256549	49.800039
3503.060183	464407.487326	49.805044
3503.211039	464398.740595	49.810049
3503.090293	464410.525523	49.815053
3503.192674	464393.874963	49.820058
3502.951125	464393.203174	49.825063
3502.944881	464444.020272	49.830068
3503.010088	464449.639322	49.835073
3503.408151	464440.295676	49.840077
3503.435798	464454.897142	49.845082
3503.331666	464428.897055	49.850087
3503.427654	464465.447131	49.855092
3503.446477	464460.626313	49.860097
3503.672470	464409.926742	49.865101
3503.363603	464443.142963	49.870106
3503.715669	464393.133430	49.875111
3503.658783	464422.303394	49.880116
3503.155694	464401.691367	49.885121
3503.368918	464413.220649	49.890125
3503.634640	464386.198474	49.895130
3503.326306	464424.283253	49.900135
3503.381997	464398.917158	49.905140
3503.599817	464419.878641	49.910145
3503.216741	464419.229221	49.915149
3503.746466	464397.693229	49.920154
3503.740763	464421.834349	49.925159
3503.544585	464377.642186	49.930164
3503.172609	464392.966148	49.935169
3503.571589	464378.449430	49.940173
3503.190307	464378.864735	49.945178
3503.143462	464373.902132	49.950183
3503.338163	464349.173299	49.955188
3503.178433	464391.646836	49.960193
3503.100801	464372.793265	49.965197
3503.015099	464361.751030	49.970202
3503.354896	464397.806253	49.975207
3503.396379	464393.336841	49.980212
3503.129704	464358.842288	49.985217
3503.682171	464371.585842	49.990221
3503.276803	464384.531495	49.995226
3503.440251	464374.362752	50.000231
3503.388455	464385.731078	50.005236
3503.432778	464373.806148	50.010241
3502.968063	464388.384050	50.015245
3503.248649	464386.767584	50.020250
3503.397739	464378.173268	50.025255
3503.035725	464392.278503	50.030260
3503.056997	464372.395005	50.035265
3503.067811	464396.736402	50.040269
3503.220077	464370.087142	50.045274
3503.378766	464407.489557	50.050279
3503.716302	464389.584675	50.055284
3503.876792	464387.682902	50.060289
3503.642961	464393.602805	50.065293
3503.384494	464412.255983	50.070298
3503.605144	464394.876726	50.075303
3503.801441	464390.433559	50.080308
3502.982744	464395.228750	50.085313
3503.501509	464365.072956	50.090317
3503.546340	464345.439284	50.095322
3503.542738	464383.425255	50.100327
3503.436302	464364.069082	50.105332
3503.411464	464321.979743	50.110337
3503.545907	464336.209406	50.115341
3503.363390	464386.090921	50.120346
3503.239986	464357.760916	50.125351
3503.472705	464335.967516	50.130356
3503.285802	464373.576759	50.135361
3503.458713	464342.765592	50.140365
3503.595855	464375.607134	50.145370
3503.422250	464357.123721	50.150375
3503.048856	464368.289313	50.155380
3503.193017	464369.686579	50.160385
3503.679527	464345.520197	50.165389
3503.557547	464372.418351	50.170394
3503.623364	464355.672111	50.175399
3503.561837	464340.163142	50.180404
3503.262403	464351.519911	50.185409
3503.228231	464326.725798	50.190413
3503.644049	464344.714596	50.195418
3503.621018	464343.399689	50.200423
3503.293852	464338.126381	50.205428
3503.440116	464333.183962	50.210433
3503.856809	464348.586162	50.215437
3503.685718	464339.535289	50.220442
3503.252997	464337.169409	50.225447
3503.711201	464342.016364	50.230452
3503.051648	464317.574659	50.235457
3503.554349	464295.992122	50.240461
3503.081590	464306.362011	50.245466
3503.552215	464296.803974	50.250471
3503.530139	464288.997401	50.255476
3503.347189	464300.437216	50.260481
3503.488642	464300.262752	50.265485
3503.521808	464307.763355	50.270490
3503.337436	464301.808175	50.275495
3503.683750	464292.675504	50.280500
3503.565599	464295.483538	50.285505
3503.058204	464316.711890	50.290509
3503.385506	464287.194828	50.295514
3503.131717	464296.870818	50.300519
3503.030411	464310.732040	50.305524
3503.039764	464300.080469	50.310529
3503.695782	464297.187499	50.315533
3503.236358	464293.659391	50.320538
3503.287363	464323.319586	50.325543
3503.381956	464310.270948	50.330548
3503.215878	464296.147774	50.335553
3503.487193	464298.488531	50.340557
3503.299497	464310.182666	50.345562
3503.462411	464290.733139	50.350567
3503.424477	464318.936665	50.355572
3503.235912	464307.352796	50.360577
3503.637347	464280.917617	50.365581
3503.395177	464286.230288	50.370586
3503.303657	464287.157661	50.375591
3503.901716	464255.417017	50.380596
3503.697365	464268.381683	50.385601
3503.176952	464279.063407	50.390605
3503.371160	464252.559517	50.395610
3503.231813	464284.329169	50.400615
3503.545738	464266.884351	50.405620
3503.123392	464287.896429	50.410625
3503.417274	464254.783843	50.415629
3503.253483	464287.013790	50.420634
3503.115076	464263.757527	50.425639
3503.486968	464287.129107	50.430644
3503.344528	464264.938497	50.435649
3503.380679	464285.573820	50.440653
3503.271260	464271.999539	50.445658
3503.248657	464276.973218	50.450663
3503.260261	464274.892108	50.455668
3503.183958	464285.554350	50.460673
3503.440883	464279.427984	50.465677
3503.364585	464288.822350	50.470682
3503.034784	464285.020178	50.475687
3503.774797	464274.050249	50.480692
3503.431696	464307.424236	50.485697
3503.288579	464264.187035	50.490701
3503.112961	464293.528086	50.495706
3503.001788	464286.394888	50.500711
3503.744544	464266.853692	50.505716
3503.255395	464298.272892	50.510721
3503.615713	464274.227805	50.515725
3503.331906	464258.753910	50.520730
3503.542983	464245.788252	50.525735
3503.642566	464215.089922	50.530740
3503.404781	464213.758235	50.535745
3503.574753	464151.453141	50.540749
3503.420512	464089.756980	50.545754
3503.036148	464023.583329	50.550759
3502.649690	463961.213484	50.555764
3502.686413	463879.453817	50.560769
3502.667371	463779.394131	50.565773
3502.400174	463699.659747	50.570778
3502.333248	463594.585853	50.575783
3502.309892	463461.965301	50.580788
3501.375060	463370.315315	50.585793
3501.873213	463209.310616	50.590797
3501.376074	463094.564525	50.595802
3501.258940	462921.786976	50.600807
3500.930976	462804.223105	50.605812
3500.849300	462624.387714	50.610817
3500.473677	462467.420956	50.615821
3500.218160	462279.190785	50.620826
3500.072137	462113.613553	50.625831
3499.727613	461912.054891	50.630836
3499.938261	461718.116203	50.635841
3499.077613	461533.018478	50.640845
3498.481371	461294.771559	50.645850
3498.263107	461117.582842	50.650855
3497.926534	460870.566004	50.655860
3497.608585	460649.564582	50.660865
3496.951766	460431.860827	50.665869
3496.878248	460188.599018	50.670874
3496.329113	459950.888001	50.675879
3495.947943	459721.010335	50.680884
3495.733339	459461.987123	50.685889
3495.268511	459201.224983	50.690893
3495.056710	458969.486549	50.695898
3494.414581	458672.171756	50.700903
3494.313587	458430.822573	50.705908
3493.126709	458133.485200	50.710913
3492.727893	457888.118850	50.715917
3492.170692	457587.630859	50.720922
3491.565119	457322.607520	50.725927
3491.293972	457042.714516	50.730932
3490.845094	456762.237312	50.735937
3490.693148	456466.946354	50.740941
3490.222923	456189.813740	50.745946
3489.745991	455873.664070	50.750951
3489.214266	455556.047303	50.755956
3488.201790	455282.084057	50.760961
3487.811745	454940.235283	50.765965
3487.464264	454666.311669	50.770970
3486.516882	454329.057360	50.775975
3486.149739	454023.773090	50.780980
3485.800573	453715.843441	50.785985
3485.113506	453372.597312	50.790989
3484.432226	453076.077268	50.795994
3483.957689	452751.308529	50.800999
3483.536222	452407.295547	50.806004
3482.346093	452086.080958	50.811009
3481.697159	451784.718531	50.816013
3481.385317	451453.055348	50.821018
3480.683061	451117.744731	50.826023
3480.402091	450799.210219	50.831028
3479.608789	450452.435835	50.836033
3478.938782	450121.875867	50.841037
3478.694514	449783.682475	50.846042
3477.834315	449462.633057	50.851047
3477.715186	449091.829257	50.856052
3476.684029	448779.526366	50.861057
3476.155998	448400.960756	50.866061
3475.604309	448090.399934	50.871066
3475.039215	447705.586550	50.876071
3474.035162	447393.869995	50.881076
3473.607954	447035.313944	50.886081
3473.021468	446673.478596	50.891085
3471.957369	446334.248591	50.896090
3471.266892	445994.447126	50.901095
3470.764078	445635.729635	50.906100
3469.833589	445300.879636	50.911105
3469.299405	444952.511379	50.916109
3468.802117	444599.310125	50.921114
3468.127036	444257.654240	50.926119
3467.562571	443915.468418	50.931124
3466.587115	443566.845283	50.936129
3466.237028	443206.239982	50.941133
3465.255146	442866.744921	50.946138
3464.322611	442519.318231	50.951143
3464.171117	442138.360337	50.956148
3463.413831	441821.709807	50.961153
3462.817248	441445.024932	50.966157
3462.062786	441129.786437	50.971162
3461.105501	440759.392291	50.976167
3460.530016	440413.173807	50.981172
3459.852980	440092.858394	50.986177
3459.344587	439726.946926	50.991181
3458.472676	439379.161581	50.996186
3457.463420	439023.269782	51.001191
3457.117438	438680.468570	51.006196
3456.238871	438350.363661	51.011201
3455.849556	437986.870199	51.016205
3454.975937	437641.091768	51.021210
3454.173019	437308.600194	51.026215
3454.004855	436960.517588	51.031220
3452.922901	436610.213567	51.036225
3452.388212	436261.519172	51.041229
3451.585569	435916.670593	51.046234
3450.739855	435570.275418	51.051239
3450.219257	435209.707774	51.056244
3448.990901	434890.301674	51.061249
3448.868215	434519.353249	51.066253
3447.808367	434217.583401	51.071258
3447.370364	433849.137955	51.076263
3446.793507	433527.834531	51.081268
3446.064775	433193.982504	51.086273
3445.735591	432851.658422	51.091277
3444.772557	432468.803109	51.096282
3443.704638	432169.245030	51.101287
3443.477350	431795.455418	51.106292
3442.909608	431473.617208	51.111297
3441.920317	431120.506541	51.116301
3441.239066	430780.953316	51.121306
3440.330735	430435.667194	51.126311
3440.193277	430099.117223	51.131316
3438.988596	429745.920526	51.136321
3438.211903	429418.655720	51.141325
3437.686627	429087.360085	51.146330
3436.611425	428756.096454	51.151335
3436.033254	428402.858976	51.156340
3435.193572	428091.028368	51.161345
3435.016785	427756.740514	51.166349
3433.758698	427412.079792	51.171354
3433.079784	427100.593166	51.176359
3432.753163	426743.763817	51.181364
3431.700626	426447.567088	51.186369
3431.509480	426090.936257	51.191373
3430.719658	425759.082491	51.196378
3429.646279	425450.382180	51.201383
3429.457657	425088.048475	51.206388
3428.521299	424790.443719	51.211393
3427.857502	424432.164083	51.216397
3426.847735	424114.726549	51.221402
3426.514116	423794.384433	51.226407
3426.200954	423470.149087	51.231412
3425.020919	423135.327875	51.236417
3424.081039	422801.531472	51.241421
3423.585590	422469.921494	51.246426
3422.944521	422152.885692	51.251431
3422.282681	421838.338939	51.256436
3421.229857	421506.195926	51.261441
3420.736326	421182.419565	51.266445
3420.447678	420882.206237	51.271450
3419.592461	420549.385545	51.276455
3419.151925	420195.740796	51.281460
3418.270270	419908.668148	51.286465
3417.957342	419535.611960	51.291469
3417.289949	419257.263186	51.296474
3415.905091	418920.391524	51.301479
3415.684188	418569.867286	51.306484
3414.624329	418268.655699	51.311489
3414.232907	417898.613635	51.316493
3413.208676	417619.060395	51.321498
3412.593625	417285.401272	51.326503
3412.196043	416980.158905	51.331508
3411.383724	416640.425990	51.336513
3410.707954	416341.445447	51.341517
3409.758569	416001.472623	51.346522
3408.884180	415692.176086	51.351527
3407.764814	415367.187649	51.356532
3407.606560	415050.326623	51.361537
3406.986965	414756.377074	51.366541
3406.171008	414436.716847	51.371546
3405.532222	414144.136248	51.376551
3405.194170	413804.828863	51.381556
3403.874375	413503.202313	51.386561
3403.533961	413193.947434	51.391565
3403.161492	412879.078826	51.396570
3402.062990	412550.930550	51.401575
3401.196035	412259.460009	51.406580
3400.724293	411934.356726	51.411585
3400.157388	411639.402257	51.416589
3399.452497	411311.584694	51.421594
3398.660620	411012.873369	51.426599
3398.332798	410705.369512	51.431604
3397.252527	410393.153221	51.436609
3396.573591	410085.266558	51.441613
3395.943671	409773.684213	51.446618
3395.304648	409455.111617	51.451623
3394.951492	409155.143605	51.456628
3393.715155	408855.159802	51.461633
3393.356767	408543.598189	51.466637
3392.633245	408238.419155	51.471642
3391.824753	407920.238570	51.476647
3391.374065	407623.168181	51.481652
3390.583194	407318.626036	51.486657
3389.668699	407021.851930	51.491661
3389.302450	406685.061370	51.496666
3388.333970	406416.551472	51.501671
3388.260212	406074.447111	51.506676
3386.889979	405801.064831	51.511681
3386.610682	405472.405876	51.516685
3385.806769	405177.604601	51.521690
3384.945907	404880.903333	51.526695
3384.259799	404572.683292	51.531700
3383.694613	404253.867672	51.536705
3382.699958	403967.142427	51.541709
3382.276974	403666.598794	51.546714
3381.586180	403356.690127	51.551719
3380.770163	403062.023584	51.556724
3380.090171	402767.892018	51.561729
3379.528586	402468.858703	51.566733
3378.790571	402161.233587	51.571738
3377.763222	401890.101919	51.576743
3377.473864	401566.665928	51.581748
3376.365046	401287.967199	51.586753
3375.933257	400985.696792	51.591757
3375.579634	400684.682205	51.596762
3374.586940	400390.070050	51.601767
3374.112447	400100.864075	51.606772
3373.087444	399816.801262	51.611777
3372.502842	399516.803849	51.616781
3372.338025	399218.872684	51.621786
3371.022854	398925.366052	51.626791
3370.858106	398625.446675	51.631796
3370.071113	398350.561559	51.636801
3369.309185	398037.079896	51.641805
3368.531572	397748.002936	51.646810
3367.830480	397448.183175	51.651815
3367.423146	397161.839050	51.656820
3366.482878	396869.170224	51.661825
3366.307856	396564.683300	51.666829
3365.404678	396273.783042	51.671834
3364.544079	395975.068568	51.676839
3364.262796	395685.463205	51.681844
3363.504868	395392.447678	51.686849
3362.575536	395092.083759	51.691853
3362.055339	394786.567650	51.696858
3361.436030	394490.141032	51.701863
3360.696541	394188.747612	51.706868
3359.733874	393901.141730	51.711873
3359.261344	393604.048644	51.716877
3358.717067	393311.744319	51.721882
3357.566605	393030.949463	51.726887
3357.097997	392731.712532	51.731892
3356.580200	392435.837042	51.736897
3355.825756	392148.971919	51.741901
3355.060704	391854.885018	51.746906
3354.228578	391577.409850	51.751911
3354.100897	391276.199574	51.756916
3353.110422	390986.107645	51.761921
3352.175522	390697.479329	51.766925
3351.927257	390405.154816	51.771930
3351.064490	390116.205238	51.776935
3350.692221	389820.945926	51.781940
3349.781666	389531.363471	51.786945
3349.035998	389237.582363	51.791949
3348.373079	388956.983157	51.796954
3347.651181	388661.210158	51.801959
3347.071135	388369.048639	51.806964
3346.246132	388088.442884	51.811969
3345.569183	387792.604821	51.816973
3345.161798	387505.876352	51.821978
3344.006556	387226.257059	51.826983
3343.669347	386934.605075	51.831988
3343.038252	386659.374233	51.836993
3342.620030	386364.526340	51.841997
3341.558328	386072.320892	51.847002
3340.792292	385794.383865	51.852007
3340.125942	385497.660989	51.857012
3339.618743	385223.035630	51.862017
3338.886603	384925.250486	51.867021
3338.596743	384645.017050	51.872026
3337.400264	384356.201818	51.877031
3336.598300	384065.999521	51.882036
3336.185290	383792.900123	51.887041
3335.425771	383507.671498	51.892045
3334.922500	383209.505951	51.897050
3334.071372	382931.484858	51.902055
3333.523712	382665.952123	51.907060
3332.782117	382376.897252	51.912065
3332.311808	382096.190251	51.917069
3331.630261	381801.806006	51.922074
3330.698861	381514.478685	51.927079
3329.972976	381235.026625	51.932084
3329.720413	380961.932483	51.937089
3328.976974	380663.123837	51.942093
3328.239349	380392.035386	51.947098
3327.139059	380105.004103	51.952103
3326.788646	379823.396890	51.957108
3326.302907	379542.190576	51.962113
3325.488625	379254.421093	51.967117
3324.796930	378968.563200	51.972122
3323.840625	378688.213699	51.977127
3323.396490	378408.849516	51.982132
3322.584069	378128.371563	51.987137
3322.107870	377844.709844	51.992141
3321.646602	377553.540090	51.997146
3320.802950	377275.070541	52.002151
3320.152208	376987.029869	52.007156
3319.273716	376710.367913	52.012161
3318.458962	376434.736893	52.017165
3318.086905	376141.278947	52.022170
3317.099039	375869.181772	52.027175
3316.454970	375589.956821	52.032180
3315.596616	375318.089862	52.037185
3314.993240	375030.740084	52.042189
3314.712051	374757.658879	52.047194
3313.611543	374496.992014	52.052199
3313.418943	374199.243627	52.057204
3312.421770	373929.984163	52.062209
3311.457844	373651.915952	52.067213
3311.297664	373369.902968	52.072218
3310.619343	373104.861456	52.077223
3309.951049	372830.302473	52.082228
3308.911654	372544.479923	52.087233
3308.166839	372273.185629	52.092237
3307.822308	372014.902227	52.097242
3306.812354	371739.906830	52.102247
3306.635290	371445.723457	52.107252
3305.586468	371183.679521	52.112257
3304.652156	370918.130561	52.117261
3304.479348	370635.134631	52.122266
3303.592501	370370.083583	52.127271
3302.673065	370097.760020	52.132276
3302.069486	369827.216533	52.137281
3301.589953	369547.518416	52.142285
3301.017606	369283.174210	52.147290
3299.915772	369012.144747	52.152295
3299.986297	368742.607336	52.157300
3298.764229	368478.132047	52.162305
3298.200312	368206.707239	52.167309
3297.799541	367931.718528	52.172314
3296.782778	367658.377499	52.177319
3296.266792	367384.853819	52.182324
3295.639664	367121.726546	52.187329
3294.992641	366842.164967	52.192333
3294.289915	366572.100593	52.197338
3293.330527	366321.411776	52.202343
3292.946844	366031.270155	52.207348
3292.488578	365779.226921	52.212353
3291.581806	365514.938651	52.217357
3290.962259	365230.299522	52.222362
3290.116996	364951.520910	52.227367
3289.522559	364683.616317	52.232372
3288.705464	364431.418838	52.237377
3288.492032	364157.802371	52.242381
3287.731919	363879.080121	52.247386
3286.984274	363615.468184	52.252391
3286.645550	363328.381113	52.257396
3285.776688	363060.866748	52.262401
3284.915422	362794.443779	52.267405
3284.487640	362518.307094	52.272410
3283.485056	362247.603172	52.277415
3283.357815	361976.861038	52.282420
3282.525133	361709.333267	52.287425
3281.752087	361434.542574	52.292429
3280.995604	361159.213318	52.297434
3279.925076	360895.204654	52.302439
3279.813270	360605.495133	52.307444
3278.955119	360341.984206	52.312449
3278.212053	360076.570613	52.317453
3277.851547	359810.586133	52.322458
3277.383597	359536.830544	52.327463
3276.741283	359250.326750	52.332468
3275.625019	358987.078317	52.337473
3274.874250	358703.794781	52.342477
3274.306434	358434.094896	52.347482
3273.213772	358174.146509	52.352487
3272.461579	357902.488000	52.357492
3272.214998	357630.086402	52.362497
3271.606089	357365.400375	52.367501
3271.192408	357095.694299	52.372506
3270.253031	356842.076677	52.377511
3269.819434	356555.982380	52.382516
3269.103493	356289.857080	52.387521
3268.289322	356013.973752	52.392525
3267.819345	355751.547638	52.397530
3266.932090	355482.569533	52.402535
3266.172084	355203.314039	52.407540
3265.590556	354938.738261	52.412545
3264.946354	354672.211464	52.417549
3264.262718	354399.988921	52.422554
3263.595793	354131.401556	52.427559
3262.940580	353873.397912	52.432564
3262.372295	353593.823482	52.437569
3261.480616	353337.916015	52.442573
3261.111494	353056.780248	52.447578
3260.008089	352780.594614	52.452583
3259.368541	352524.694229	52.457588
3259.166064	352260.426723	52.462593
3258.238505	351991.589735	52.467597
3257.802738	351727.127440	52.472602
3256.728088	351459.659926	52.477607
3256.008299	351180.631243	52.482612
3255.453066	350918.474445	52.487617
3254.425979	350653.235097	52.492621
3254.307310	350377.797602	52.497626
3253.333422	350128.250603	52.502631
3252.705766	349855.028889	52.507636
3252.106190	349584.575587	52.512641
3251.358691	349333.742063	52.517645
3250.888558	349064.767393	52.522650
3250.081891	348802.283961	52.527655
3249.620097	348541.450027	52.532660
3248.885442	348277.476535	52.537665
3248.007314	348011.284710	52.542669
3247.820312	347736.837586	52.547674
3247.016300	347481.066981	52.552679
3246.366737	347207.123156	52.557684
3245.581310	346942.718795	52.562689
3244.909096	346677.938970	52.567693
3244.530005	346401.326884	52.572698
3243.400639	346140.205758	52.577703
3242.931267	345867.626978	52.582708
3242.269495	345604.673221	52.587713
3241.751642	345338.233865	52.592717
3241.385241	345075.765536	52.597722
3240.507456	344800.344701	52.602727
3239.817804	344536.245170	52.607732
3239.124452	344263.287128	52.612737
3238.238670	343996.238130	52.617741
3237.731041	343716.859284	52.622746
3236.914680	343465.451171	52.627751
3236.612100	343173.641205	52.632756
3235.733547	342920.840682	52.637761
3235.032058	342656.480224	52.642765
3234.527388	342377.680190	52.647770
3233.533025	342099.669081	52.652775
3232.692444	341846.629024	52.657780
3232.179085	341576.608649	52.662785
3231.430136	341303.035206	52.667789
3231.133757	341047.793044	52.672794
3230.187857	340778.194004	52.677799
3229.675930	340512.318009	52.682804
3229.123142	340235.374230	52.687809
3228.099503	339986.072108	52.692813
3228.029523	339703.653059	52.697818
3227.014125	339442.510616	52.702823
3226.369454	339175.835452	52.707828
3225.300102	338903.982427	52.712833
3224.955512	338638.148536	52.717837
3224.307143	338381.500387	52.722842
3223.352880	338115.862630	52.727847
3222.799244	337855.989940	52.732852
3222.385888	337587.413366	52.737857
3221.168384	337333.116780	52.742861
3220.980663	337056.738097	52.747866
3220.305812	336791.814523	52.752871
3219.533687	336519.522783	52.757876
3218.870323	336259.228449	52.762881
3218.124080	336005.615986	52.767885
3217.718627	335730.131839	52.772890
3216.774262	335486.706208	52.777895
3216.126646	335224.597955	52.782900
3215.752422	334954.655461	52.787905
3215.063932	334693.468124	52.792909
3214.421020	334411.040875	52.797914
3213.429913	334152.928844	52.802919
3212.792674	333879.536065	52.807924
3212.363203	333623.497164	52.812929
3211.577964	333361.734630	52.817933
3211.135820	333091.566575	52.822938
3209.826781	332830.215901	52.827943
3209.575443	332562.841533	52.832948
3209.419295	332301.586603	52.837953
3208.639766	332039.385541	52.842957
3208.072318	331762.205761	52.847962
3206.860995	331500.682073	52.852967
3206.435625	331221.491988	52.857972
3205.633732	330972.452857	52.862977
3205.072387	330694.860746	52.867981
3204.381400	330426.249714	52.872986
3203.636309	330179.235672	52.877991
3202.718990	329899.431053	52.882996
3202.195122	329648.739599	52.888001
3201.247359	329381.743944	52.893005
3201.075015	329116.126802	52.898010
3200.313788	328852.715047	52.903015
3199.855439	328584.544429	52.908020
3199.021894	328323.790121	52.913025
3198.261100	328055.971040	52.918029
3197.567532	327786.943788	52.923034
3196.888670	327536.524597	52.928039
3195.848977	327256.678843	52.933044
3195.709630	326995.810312	52.938049
3194.554348	326748.341010	52.943053
3193.955866	326491.897183	52.948058
3193.474779	326231.182070	52.953063
3193.324693	325960.178609	52.958068
3192.432347	325706.834054	52.963073
3191.696635	325441.344633	52.968077
3190.909820	325158.319943	52.973082
3190.260872	324917.995852	52.978087
3189.745527	324641.291675	52.983092
3188.985292	324380.283870	52.988097
3188.209613	324113.752634	52.993101
3187.506321	323852.021276	52.998106
3187.195252	323590.990901	53.003111
3186.716426	323325.021304	53.008116
3185.751402	323062.386864	53.013121
3185.007084	322796.177561	53.018125
3184.441352	322512.217917	53.023130
3183.884468	322262.654682	53.028135
3183.165495	321991.397508	53.033140
3182.384120	321727.278688	53.038145
3181.484949	321466.182224	53.043149
3181.103730	321195.760359	53.048154
3180.392003	320941.227368	53.053159
3179.800373	320660.703292	53.058164
3179.218037	320412.641192	53.063169
3178.035398	320149.039557	53.068173
3177.576803	319874.501124	53.073178
3177.082749	319626.652105	53.078183
3176.226166	319357.700455	53.083188
3175.807567	319089.238919	53.088193
3175.048541	318837.253875	53.093197
3174.647345	318563.186317	53.098202
3173.703701	318304.175903	53.103207
3173.022965	318037.357031	53.108212
3172.578119	317772.842692	53.113217
3171.558597	317520.666245	53.118221
3171.167013	317234.574879	53.123226
3170.369160	316988.651373	53.128231
3169.645079	316722.141336	53.133236
3169.193079	316464.092268	53.138241
3168.418605	316190.942884	53.143245
3167.804519	315932.612540	53.148250
3167.032924	315666.438256	53.153255
3166.581945	315404.974234	53.158260
3165.955107	315146.491148	53.163265
3165.012354	314874.307032	53.168269
3164.688569	314603.755815	53.173274
3163.819568	314353.151903	53.178279
3163.226994	314066.676053	53.183284
3162.444062	313821.506534	53.188289
3161.588893	313544.314226	53.193293
3160.795720	313290.156342	53.198298
3160.110116	313032.110308	53.203303
3159.657047	312779.527131	53.208308
3158.893828	312514.591382	53.213313
3158.083083	312251.877913	53.218317
3157.462430	311993.539082	53.223322
3156.589350	311725.945099	53.228327
3156.265198	311474.866452	53.233332
3155.681398	311212.267456	53.238337
3154.984506	310956.917687	53.243341
3154.316613	310698.507018	53.248346
3153.581081	310447.644020	53.253351
3152.824370	310184.866353	53.258356
3152.642219	309909.799576	53.263361
3151.476674	309667.279017	53.268365
3151.133670	309400.156085	53.273370
3150.540320	309136.357152	53.278375
3149.962684	308873.904811	53.283380
3149.299297	308619.410573	53.288385
3148.528155	308361.571472	53.293389
3147.701326	308085.634931	53.298394
3147.120783	307833.901697	53.303399
3146.284659	307563.262255	53.308404
3145.923386	307304.363018	53.313409
3145.366530	307040.019157	53.318413
3144.596467	306776.192339	53.323418
3143.770298	306513.137834	53.328423
3143.304513	306249.771136	53.333428
3142.606993	305983.562978	53.338433
3141.746871	305715.393706	53.343437
3141.341567	305450.309689	53.348442
3140.324691	305202.765935	53.353447
3139.784731	304932.991078	53.358452
3139.303339	304654.955517	53.363457
3138.471361	304411.455641	53.368461
3137.863904	304144.007354	53.373466
3137.169158	303888.745103	53.378471
3136.629314	303617.567120	53.383476
3136.218845	303364.117991	53.388481
3135.304200	303100.689103	53.393485
3134.892620	302830.075107	53.398490
3133.973796	302571.739179	53.403495
3133.209030	302293.107336	53.408500
3132.695442	302031.217511	53.413505
3131.853788	301776.687980	53.418509
3131.143538	301499.090211	53.423514
3130.517685	301244.500214	53.428519
3129.917725	300976.459447	53.433524
3129.167183	300705.869951	53.438529
3128.319001	300455.617728	53.443533
3127.958767	300192.121721	53.448538
3126.990295	299932.414193	53.453543
3126.498734	299676.807333	53.458548
3126.285710	299405.264825	53.463553
3125.351294	299153.700060	53.468557
3124.580152	298887.975062	53.473562
3124.120986	298630.451538	53.478567
3123.665485	298351.662276	53.483572
3122.898741	298093.753717	53.488577
3121.972875	297819.851303	53.493581
3121.526662	297543.351365	53.498586
3120.628177	297295.241841	53.503591
3119.859819	297022.841361	53.508596
3119.373415	296756.966377	53.513601
3118.589691	296491.520081	53.518605
3118.065967	296243.859256	53.523610
3117.255278	295973.399519	53.528615
3116.619278	295717.351661	53.533620
3116.185261	295452.587211	53.538625
3115.293879	295192.529829	53.543629
3114.898645	294916.782192	53.548634
3113.655363	294661.313014	53.553639
3113.076364	294396.875798	53.558644
3112.732629	294127.969719	53.563649
3111.762314	293876.302007	53.568653
3110.787322	293611.620912	53.573658
3110.374911	293352.504264	53.578663
3109.944909	293077.931360	53.583668
3109.405639	292826.245237	53.588673
3108.527417	292571.479980	53.593677
3107.873141	292301.729572	53.598682
3106.773538	292051.812173	53.603687
3106.134896	291792.958863	53.608692
3105.742443	291529.405760	53.613697
3105.121022	291274.012801	53.618701
3104.597506	291003.527241	53.623706
3103.847128	290761.270050	53.628711
3103.183838	290493.913158	53.633716
3102.736983	290250.588782	53.638721
3101.956189	289984.676194	53.643725
3101.451707	289710.519009	53.648730
3100.681064	289461.922435	53.653735
3099.897434	289199.702419	53.658740
3099.294610	288931.901575	53.663745
3098.499680	288674.878344	53.668749
3097.828998	288413.123684	53.673754
3097.250936	288161.872408	53.678759
3096.708470	287889.375047	53.683764
3096.212438	287631.998088	53.688769
3095.139548	287379.500199	53.693773
3094.697218	287108.641797	53.698778
3093.831007	286857.868127	53.703783
3093.069447	286598.112981	53.708788
3092.571877	286340.582540	53.713793
3091.968559	286074.231243	53.718797
3091.523199	285814.272729	53.723802
3090.492405	285561.537758	53.728807
3090.172338	285286.456505	53.733812
3089.562009	285026.982036	53.738817
3088.881311	284758.502828	53.743821
3088.377291	284495.700372	53.748826
3087.454723	284241.164754	53.753831
3086.787813	283974.440222	53.758836
3086.091274	283708.000387	53.763841
3085.589614	283454.212746	53.768845
3084.958002	283182.414047	53.773850
3083.843186	282928.264762	53.778855
3083.310136	282664.243497	53.783860
3082.737265	282391.441868	53.788865
3081.618235	282139.941615	53.793869
3081.438519	281874.081322	53.798874
3080.590568	281624.091541	53.803879
3079.838088	281372.100036	53.808884
3079.414611	281100.445787	53.813889
3078.624756	280852.942445	53.818893
3078.092153	280588.920315	53.823898
3077.301697	280339.201173	53.828903
3076.538792	280065.970328	53.833908
3075.792844	279810.411753	53.838913
3075.517256	279556.001161	53.843917
3074.707925	279287.158012	53.848922
3073.936592	279039.294717	53.853927
3073.536702	278773.417397	53.858932
3072.660805	278505.552416	53.863937
3072.069312	278258.551915	53.868941
3071.386254	277997.609199	53.873946
3070.612189	277738.845660	53.878951
3069.857055	277470.885008	53.883956
3069.295194	277225.509668	53.888961
3068.625438	276961.406649	53.893965
3068.118120	276692.464379	53.898970
3067.455418	276440.304885	53.903975
3066.618743	276172.153294	53.908980
3066.138770	275915.202278	53.913985
3065.227778	275672.963796	53.918989
3064.891392	275400.148718	53.923994
3063.957445	275143.702516	53.928999
3063.328542	274878.701609	53.934004
3063.065877	274614.203064	53.939009
3062.034374	274373.027911	53.944013
3061.580484	274102.982096	53.949018
3060.957633	273847.683774	53.954023
3060.223686	273589.830760	53.959028
3059.693669	273315.773092	53.964033
3058.877016	273049.426811	53.969037
3058.394070	272788.248782	53.974042
3057.670084	272539.206420	53.979047
3056.782569	272265.281938	53.984052
3056.392428	272001.720831	53.989057
3055.629858	271747.081711	53.994061
3054.833176	271478.797028	53.999066
3054.364239	271211.504754	54.004071
3053.336985	270957.111484	54.009076
3053.085940	270703.334030	54.014081
3051.949275	270439.458557	54.019085
3051.733291	270173.400006	54.024090
3050.717102	269912.332635	54.029095
3050.165158	269661.532011	54.034100
3049.819849	269388.515922	54.039105
3048.824771	269120.620029	54.044109
3048.517516	268853.404914	54.049114
3047.965137	268591.347828	54.054119
3047.260213	268335.529251	54.059124
3046.644854	268057.717559	54.064129
3045.714548	267800.406815	54.069133
3045.060256	267526.319925	54.074138
3044.203855	267272.639706	54.079143
3043.536976	267008.844240	54.084148
3042.898707	266738.142531	54.089153
3041.977898	266487.223495	54.094157
3041.799823	266232.876200	54.099162
3041.057548	265961.478326	54.104167
3040.276235	265709.035054	54.109172
3039.751528	265438.418072	54.114177
3038.933397	265179.588481	54.119181
3038.557470	264915.977494	54.124186
3037.890798	264653.813449	54.129191
3037.267117	264393.731162	54.134196
3036.460101	264114.322426	54.139201
3035.565719	263846.693932	54.144205
3034.740905	263576.686121	54.149210
3034.318924	263307.506149	54.154215
3033.707648	263055.674520	54.159220
3032.929447	262786.042004	54.164225
3032.173449	262528.630769	54.169229
3031.645342	262268.891578	54.174234
3030.898773	262006.003713	54.179239
3030.350481	261751.107049	54.184244
3029.884748	261481.044229	54.189249
3028.795094	261219.815844	54.194253
3027.973213	260969.318162	54.199258
3027.333287	260696.889705	54.204263
3026.801448	260440.336232	54.209268
3026.449725	260187.243565	54.214273
3025.440434	259926.156519	54.219277
3024.838839	259667.908515	54.224282
3024.254598	259407.238611	54.229287
3023.507153	259152.044862	54.234292
3023.228640	258886.029874	54.239297
3022.267704	258634.002961	54.244301
3021.504516	258370.026252	54.249306
3020.930961	258112.666824	54.254311
3020.259496	257854.813831	54.259316
3019.787524	257581.725544	54.264321
3018.967429	257334.287351	54.269325
3018.502655	257071.028940	54.274330
3017.821931	256802.737041	54.279335
3017.165337	256547.506349	54.284340
3016.701751	256271.158571	54.289345
3016.002326	256020.544861	54.294349
3014.910223	255746.920378	54.299354
3014.499372	255484.266629	54.304359
3014.039634	255225.975829	54.309364
3013.246127	254945.862009	54.314369
3012.502919	254693.168588	54.319373
3012.014513	254417.413030	54.324378
3011.550590	254170.508027	54.329383
3010.793211	253892.834850	54.334388
3010.341039	253624.994919	54.339393
3009.227920	253364.467103	54.344397
3008.803215	253094.586255	54.349402
3007.935308	252817.365140	54.354407
3007.490990	252564.652784	54.359412
3007.094039	252290.413958	54.364417
3005.789930	252035.470054	54.369421
3005.634133	251746.270478	54.374426
3004.800491	251489.393864	54.379431
3004.065101	251220.558300	54.384436
3003.553392	250948.784589	54.389441
3003.130103	250679.314778	54.394445
3002.054855	250406.739842	54.399450
3001.306511	250144.376560	54.404455
3000.696683	249870.582885	54.409460
3000.363249	249608.791476	54.414465
2999.311381	249355.467138	54.419469
2998.720935	249077.444398	54.424474
2998.442957	248807.623728	54.429479
2997.282908	248543.673023	54.434484
2996.795441	248279.183402	54.439489
2996.037196	248010.535226	54.444493
2995.368954	247735.506810	54.449498
2994.661353	247486.842341	54.454503
2993.955684	247210.140098	54.459508
2993.790690	246947.486327	54.464513
2992.688251	246689.259673	54.469517
2992.027773	246410.667376	54.474522
2991.575650	246132.857559	54.479527
2990.580749	245881.261920	54.484532
2990.074017	245615.252369	54.489537
2989.407993	245343.207766	54.494541
2988.864579	245066.229476	54.499546
2988.158664	244817.595005	54.504551
2987.160971	244546.419425	54.509556
2986.576340	244286.078172	54.514561
2985.859114	244019.443049	54.519565
2985.185676	243761.816226	54.524570
2984.485721	243498.540861	54.529575
2983.628245	243235.978536	54.534580
2983.376284	242972.658822	54.539585
2982.723395	242712.178812	54.544589
2982.218811	242438.586905	54.549594
2981.773233	242177.311265	54.554599
2980.912552	241921.525899	54.559604
2980.302312	241646.679260	54.564609
2979.256681	241381.706081	54.569613
2978.682067	241111.285896	54.574618
2978.217722	240848.335465	54.579623
2977.723166	240584.702866	54.584628
2976.762475	240320.406182	54.589633
2975.894033	240047.564927	54.594637
2975.201993	239781.189809	54.599642
2974.490628	239524.010984	54.604647
2973.870985	239266.614514	54.609652
2973.764802	238994.673710	54.614657
2972.896512	238744.244061	54.619661
2972.351770	238477.594093	54.624666
2971.734367	238212.433188	54.629671
2970.865594	237947.694680	54.634676
2970.166061	237666.989655	54.639681
2969.580220	237399.228440	54.644685
2969.017835	237131.718824	54.649690
2968.500851	236875.152075	54.654695
2967.553006	236605.336692	54.659700
2967.157175	236327.184441	54.664705
2966.113903	236070.142788	54.669709
2965.324315	235804.149428	54.674714
2964.857980	235539.302368	54.679719
2964.339559	235275.533702	54.684724
2963.598578	235008.108793	54.689729
2962.807534	234733.053583	54.694733
2962.472250	234466.151557	54.699738
2961.825653	234204.519447	54.704743
2960.993831	233946.074760	54.709748
2960.493398	233667.640878	54.714753
2959.685162	233402.980963	54.719757
2958.835090	233133.923349	54.724762
2958.283029	232862.171201	54.729767
2957.630337	232602.912420	54.734772
2957.057174	232330.503109	54.739777
2956.119165	232065.409137	54.744781
2955.499650	231789.800471	54.749786
2954.797089	231527.038759	54.754791
2954.098140	231261.323608	54.759796
2953.585355	231001.665207	54.764801
2953.094142	230735.689540	54.769805
2952.215139	230475.403141	54.774810
2951.691200	230213.202567	54.779815
2950.945448	229944.366872	54.784820
2950.257339	229670.430513	54.789825
2949.422603	229405.251570	54.794829
2948.932452	229137.701870	54.799834
2948.597489	228875.424419	54.804839
2947.424535	228609.282970	54.809844
2947.164373	228341.011852	54.814849
2946.417966	228083.894208	54.819853
2945.681507	227812.339253	54.824858
2945.055685	227548.278685	54.829863
2944.386614	227276.943926	54.834868
2943.986198	227007.795347	54.839873
2942.894500	226751.678471	54.844877
2942.221034	226475.102065	54.849882
2941.834208	226204.833656	54.854887
2941.173995	225948.358160	54.859892
2940.682608	225666.434371	54.864897
2939.923172	225398.379028	54.869901
2938.743528	225129.970999	54.874906
2938.663639	224871.039218	54.879911
2937.849572	224599.799912	54.884916
2937.017953	224331.314003	54.889921
2936.715903	224071.337932	54.894925
2936.120593	223796.285925	54.899930
2935.398156	223524.946689	54.904935
2934.460248	223249.339804	54.909940
2934.217796	222981.923658	54.914945
2933.496484	222707.646504	54.919949
2932.735583	222436.877279	54.924954
2931.986139	222171.351841	54.929959
2931.251524	221892.153318	54.934964
2930.872302	221624.878134	54.939969
2929.850767	221348.018378	54.944973
2929.505016	221079.619631	54.949978
2929.246005	220803.430403	54.954983
2928.416125	220530.540397	54.959988
2927.771054	220251.893917	54.964993
2927.008712	219972.083231	54.969997
2926.105430	219691.201210	54.975002
2925.464924	219405.034226	54.980007
2924.649264	219142.025042	54.985012
2924.720496	218867.534740	54.990017
2923.445385	218598.452109	54.995021
2923.126260	218319.876022	55.000026
2922.671512	218035.938134	55.005031
2921.325274	217767.353616	55.010036
2920.585675	217490.183908	55.015041
2920.156453	217210.891357	55.020045
2919.104918	216936.980900	55.025050
2918.652816	216663.498501	55.030055
2917.693900	216402.393346	55.035060
2917.654338	216121.961559	55.040065
2916.585015	215858.101112	55.045069
2916.102919	215587.415316	55.050074
2915.328986	215316.522236	55.055079
2914.389712	215047.667514	55.060084
2914.100648	214773.174076	55.065089
2913.259267	214508.493660	55.070093
2912.642387	214234.983504	55.075098
2911.766483	213966.784976	55.080103
2911.031771	213707.424002	55.085108
2910.792370	213429.237089	55.090113
2910.008384	213161.090937	55.095117
2909.540079	212894.665105	55.100122
2909.052386	212615.579102	55.105127
2908.156269	212352.328860	55.110132
2907.676847	212070.761961	55.115137
2906.747217	211804.973698	55.120141
2906.548099	211530.403280	55.125146
2905.725323	211253.947269	55.130151
2904.829035	210983.473372	55.135156
2904.904174	210701.837467	55.140161
2903.790042	210432.036815	55.145165
2903.002726	210147.065339	55.150170
2902.346753	209856.347036	55.155175
2901.388663	209593.601764	55.160180
2900.818156	209323.987136	55.165185
2900.576023	209047.487168	55.170189
2899.649231	208768.716864	55.175194
2898.760674	208496.025355	55.180199
2898.141727	208232.697698	55.185204
2897.975889	207946.645347	55.190209
2896.962402	207677.553608	55.195213
2896.340730	207406.453825	55.200218
2895.803302	207123.785959	55.205223
2894.942734	206849.519372	55.210228
2894.472075	206574.237816	55.215233
2893.667129	206306.684656	55.220237
2893.116815	206025.373113	55.225242
2892.550766	205756.613791	55.230247
2891.805189	205483.200785	55.235252
2891.140428	205195.255418	55.240257
2890.236189	204919.464901	55.245261
2889.379647	204652.347494	55.250266
2888.899280	204373.629066	55.255271
2888.161947	204112.234843	55.260276
2887.859199	203827.267856	55.265281
2886.892236	203557.475125	55.270285
2886.198078	203282.130131	55.275290
2885.492760	203008.646239	55.280295
2884.866441	202736.551018	55.285300
2884.618150	202470.721999	55.290305
2883.703485	202195.137300	55.295309
2883.035199	201924.541609	55.300314
2882.597816	201646.618899	55.305319
2881.663225	201362.986188	55.310324
2880.973532	201103.520065	55.315329
2880.296310	200823.908833	55.320333
2879.575324	200551.648506	55.325338
2878.963378	200275.401986	55.330343
2878.156831	200011.098518	55.335348
2877.677171	199734.541142	55.340353
2876.943191	199471.335929	55.345357
2876.276469	199195.307237	55.350362
2875.639942	198916.819272	55.355367
2874.808291	198638.529089	55.360372
2874.575839	198367.576807	55.365377
2874.008013	198102.316100	55.370381
2872.978787	197831.721786	55.375386
2872.542649	197548.857467	55.380391
2871.448804	197273.949894	55.385396
2871.423970	196998.938130	55.390401
2870.253938	196730.967637	55.395405
2870.002231	196454.086027	55.400410
2869.561760	196177.184900	55.405415
2868.211229	195902.350731	55.410420
2867.572794	195623.702552	55.415425
2867.062841	195356.754460	55.420429
2866.336505	195080.209935	55.425434
2865.854481	194808.590588	55.430439
2865.108503	194539.241184	55.435444
2864.364083	194261.266219	55.440449
2863.857168	193983.471495	55.445453
2863.241467	193714.958394	55.450458
2862.565449	193420.550999	55.455463
2861.843627	193162.936385	55.460468
2861.330142	192883.202159	55.465473
2860.272265	192617.958626	55.470477
2859.790906	192341.619550	55.475482
2859.684765	192069.408576	55.480487
2858.869979	191785.847734	55.485492
2858.070974	191504.728889	55.490497
2857.756427	191232.186638	55.495501
2856.836962	190945.441090	55.500506
2856.006049	190670.044780	55.505511
2855.084598	190390.096895	55.510516
2854.665607	190117.144939	55.515521
2853.993810	189843.407604	55.520525
2853.587228	189562.327078	55.525530
2853.074726	189278.669597	55.530535
2852.133181	189015.412245	55.535540
2851.635372	188717.659339	55.540545
2851.093266	188439.991127	55.545549
2850.263636	188153.947984	55.550554
2849.598844	187872.155139	55.555559
2848.743078	187596.882502	55.560564
2848.454668	187313.646749	55.565569
2847.584697	187037.336496	55.570573
2846.749992	186756.518789	55.575578
2846.517934	186473.202962	55.580583
2845.477843	186196.301358	55.585588
2844.698181	185906.740370	55.590593
2844.419475	185635.166463	55.595597
2843.669761	185356.684699	55.600602
2843.035594	185061.801239	55.605607
2842.045642	184771.695650	55.610612
2841.546429	184507.516365	55.615617
2840.887471	184229.523353	55.620621
2839.821637	183945.935641	55.625626
2839.648428	183664.421838	55.630631
2838.814072	183391.333980	55.635636
2838.112366	183102.262197	55.640641
2837.533092	182823.972818	55.645645
2836.968300	182543.812977	55.650650
2836.109986	182261.284507	55.655655
2835.435818	181989.464790	55.660660
2834.889209	181714.382873	55.665665
2834.192728	181429.353707	55.670669
2833.234249	181150.015695	55.675674
2832.981109	180867.362321	55.680679
2832.181855	180600.748252	55.685684
2831.700698	180314.941890	55.690689
2831.101994	180041.074603	55.695693
2830.217056	179758.833885	55.700698
2829.718771	179475.796070	55.705703
2829.047630	179195.700320	55.710708
2828.610562	178912.720180	55.715713
2827.732451	178628.323608	55.720717
2826.740179	178345.104508	55.725722
2826.490511	178067.887712	55.730727
2825.365729	177794.220096	55.735732
2824.884495	177514.232708	55.740737
2824.352374	177234.229832	55.745741
2823.671367	176950.958217	55.750746
2823.147380	176669.927643	55.755751
2822.422567	176390.342578	55.760756
2821.669816	176107.953012	55.765761
2821.037646	175834.105929	55.770765
2820.597261	175542.424373	55.775770
2820.115092	175254.490746	55.780775
2819.075699	174976.326072	55.785780
2818.135096	174685.175044	55.790785
2817.674580	174415.240306	55.795789
2817.081569	174132.890075	55.800794
2816.670123	173849.432050	55.805799
2815.672297	173569.782526	55.810804
2815.227402	173286.232054	55.815809
2814.522547	173001.580179	55.820813
2813.664735	172717.971982	55.825818
2813.272799	172436.326847	55.830823
2812.397309	172158.829887	55.835828
2811.659277	171881.847247	55.840833
2811.399141	171596.753565	55.845837
2810.558027	171316.726386	55.850842
2810.097621	171036.030506	55.855847
2809.212314	170747.748313	55.860852
2808.809596	170454.890055	55.865857
2808.021014	170175.549499	55.870861
2807.213355	169895.031333	55.875866
2806.600536	169605.811624	55.880871
2805.580881	169326.793594	55.885876
2804.946693	168980.319535	55.890881
2804.351131	168708.232884	55.895885
2803.727109	168410.313324	55.900890
2802.724827	168131.975256	55.905895
2802.080015	167876.229878	55.910900
2802.070479	167581.360388	55.915905
2801.575952	167294.135940	55.920909
2799.893240	167035.000220	55.925914
2800.019280	166737.827045	55.930919
2799.279599	166452.834969	55.935924
2798.183527	166170.609910	55.940929
2797.579738	165917.325497	55.945933
2797.210843	165614.683057	55.950938
2796.925406	165335.413070	55.955943
2795.935729	165068.170759	55.960948
2795.268533	164774.953468	55.965953
2794.525209	164492.405646	55.970957
2793.762272	164207.612596	55.975962
2793.169265	163926.126102	55.980967
2792.418804	163658.805342	55.985972
2791.650693	163377.490690	55.990977
2791.313570	163097.584832	55.995981
2790.719816	162804.092066	56.000986
2790.051230	162521.814741	56.005991
2789.358827	162258.080552	56.010996
2789.152458	161958.722992	56.016001
2788.372400	161681.135974	56.021005
2787.249776	161398.583424	56.026010
2786.769424	161111.952010	56.031015
2786.011864	160823.497918	56.036020
2785.402163	160549.833965	56.041025
2784.813944	160248.644257	56.046029
2783.915276	159965.292160	56.051034
2783.702198	159679.888647	56.056039
2783.104182	159405.468952	56.061044
2782.400400	159102.019030	56.066049
2781.469106	158807.964441	56.071053
2780.557300	158549.581239	56.076058
2780.203502	158257.410320	56.081063
2779.529021	157976.034760	56.086068
2778.826369	157675.927812	56.091073
2777.969592	157408.162643	56.096077
2777.285026	157108.248465	56.101082
2776.817242	156820.836726	56.106087
2775.716582	156552.837197	56.111092
2775.360615	156262.107320	56.116097
2774.712138	155987.138050	56.121101
2773.823826	155702.026915	56.126106
2773.433610	155423.093394	56.131111
2772.532457	155144.293946	56.136116
2771.876364	154863.347897	56.141121
2771.104056	154576.740657	56.146125
2770.332260	154304.410433	56.151130
2770.122203	154025.154893	56.156135
2769.298862	153752.595814	56.161140
2768.410934	153469.486467	56.166145
2768.062459	153183.751936	56.171149
2767.104298	152904.293804	56.176154
2766.589672	152635.927634	56.181159
2765.631155	152351.390015	56.186164
2765.296799	152064.963836	56.191169
2764.594311	151790.469799	56.196173
2764.132493	151514.808738	56.201178
2763.566174	151214.496446	56.206183
2762.559708	150959.414847	56.211188
2762.081110	150670.341927	56.216193
2761.565512	150389.081172	56.221197
2760.277636	150120.489515	56.226202
2759.646132	149836.887933	56.231207
2759.191524	149561.623568	56.236212
2758.808112	149273.742718	56.241217
2758.223987	148996.076241	56.246221
2757.027147	148713.692501	56.251226
2756.978608	148429.159491	56.256231
2756.115039	148165.714900	56.261236
2755.533701	147869.439390	56.266241
2754.811726	147585.732262	56.271245
2753.956499	147309.051132	56.276250
2753.322596	147028.524862	56.281255
2753.049618	146746.939966	56.286260
2752.329325	146462.594528	56.291265
2751.838063	146183.400245	56.296269
2750.806407	145903.379074	56.301274
2750.307485	145617.633777	56.306279
2749.639419	145340.660749	56.311284
2748.695061	145061.243267	56.316289
2748.321826	144768.674602	56.321293
2747.328117	144491.366787	56.326298
2746.469906	144214.294138	56.331303
2745.800280	143930.954926	56.336308
2745.360399	143659.183381	56.341313
2744.912819	143370.883847	56.346317
2743.839926	143094.554151	56.351322
2743.560262	142809.371857	56.356327
2742.942652	142542.492281	56.361332
2742.315642	142267.306551	56.366337
2741.774876	141969.848268	56.371341
2740.768901	141696.188954	56.376346
2740.536177	141406.946389	56.381351
2739.512819	141133.955622	56.386356
2738.712571	140846.231382	56.391361
2738.044362	140555.820784	56.396365
2737.411507	140294.553924	56.401370
2737.193255	140005.957790	56.406375
2736.034543	139730.091669	56.411380
2735.370723	139448.724585	56.416385
2734.996404	139160.402736	56.421389
2734.096874	138880.945999	56.426394
2733.423927	138606.537936	56.431399
2732.817106	138327.802335	56.436404
2732.249408	138041.796134	56.441409
2731.775519	137755.879480	56.446413
2730.839496	137487.278614	56.451418
2730.800434	137194.107875	56.456423
2729.963915	136912.589010	56.461428
2729.137606	136629.394311	56.466433
2728.251375	136340.520521	56.471437
2727.298222	136060.336847	56.476442
2727.163734	135778.946382	56.481447
2725.988434	135496.440464	56.486452
2725.386219	135213.935445	56.491457
2724.968596	134931.785042	56.496461
2723.912639	134662.073246	56.501466
2723.779555	134377.317166	56.506471
2722.708712	134099.483088	56.511476
2722.072794	133839.887476	56.516481
2721.809491	133533.807065	56.521485
2720.910142	133264.286852	56.526490
2720.440470	132975.838088	56.531495
2719.631782	132711.173758	56.536500
2718.838501	132426.935466	56.541505
2718.181953	132142.259199	56.546509
2717.395514	131855.815409	56.551514
2716.761305	131574.265987	56.556519
2716.333166	131318.140791	56.561524
2715.506873	131029.463528	56.566529
2714.635774	130749.801606	56.571533
2713.970756	130476.752584	56.576538
2713.614789	130191.476893	56.581543
2712.855558	129927.135736	56.586548
2712.118434	129649.978402	56.591553
2711.844049	129364.507744	56.596557
2710.910021	129099.440105	56.601562
2710.470985	128811.638908	56.606567
2709.657709	128537.768786	56.611572
2709.146007	128257.351089	56.616577
2708.302227	127965.825465	56.621581
2707.795859	127704.272216	56.626586
2707.385613	127411.083606	56.631591
2706.154756	127137.318996	56.636596
2705.534130	126855.980404	56.641601
2705.183601	126573.801860	56.646605
2704.267704	126286.369392	56.651610
2703.667241	126008.325491	56.656615
2703.455416	125735.226303	56.661620
2702.244567	125457.526036	56.666625
2701.842135	125175.090892	56.671629
2701.059919	124882.458352	56.676634
2700.961368	124619.384451	56.681639
2699.946940	124327.226492	56.686644
2699.305815	124031.291990	56.691649
2698.355480	123756.666403	56.696653
2697.714400	123475.086939	56.701658
2696.996117	123195.871784	56.706663
2696.540918	122918.268585	56.711668
2695.657480	122639.402883	56.716673
2695.132999	122353.423461	56.721677
2694.412822	122083.997351	56.726682
2693.960999	121803.180183	56.731687
2693.283373	121523.785758	56.736692
2692.500610	121243.991957	56.741697
2692.231350	120954.635287	56.746701
2691.318219	120676.353716	56.751706
2690.894630	120399.756017	56.756711
2690.123229	120102.153063	56.761716
2689.228969	119812.844563	56.766721
2689.108989	119530.926349	56.771725
2688.212778	119257.742027	56.776730
2687.596877	118963.174505	56.781735
2686.589858	118680.669709	56.786740
2686.160390	118384.835064	56.791745
2685.722529	118106.105829	56.796749
2684.682483	117821.692327	56.801754
2683.820664	117539.672158	56.806759
2683.110092	117266.473178	56.811764
2682.397462	116980.119243	56.816769
2681.930017	116684.246739	56.821773
2681.384741	116407.984027	56.826778
2680.762623	116123.535898	56.831783
2679.825704	115857.039746	56.836788
2679.145920	115564.793689	56.841793
2678.871639	115271.852061	56.846797
2677.702713	115001.219010	56.851802
2677.229380	114724.328559	56.856807
2676.357186	114448.735619	56.861812
2675.620923	114158.818677	56.866817
2675.313860	113886.138021	56.871821
2674.645463	113611.131269	56.876826
2673.911112	113326.478615	56.881831
2672.920205	113054.841954	56.886836
2672.368147	112780.174976	56.891841
2672.016823	112492.545491	56.896845
2670.651255	112221.288260	56.901850
2670.299669	111954.106230	56.906855
2670.179338	111670.917364	56.911860
2669.218283	111384.165222	56.916865
2668.666395	111128.687804	56.921869
2667.714136	110852.423946	56.926874
2667.604085	110564.315423	56.931879
2666.626027	110277.064870	56.936884
2665.746467	109999.631482	56.941889
2665.466094	109720.386659	56.946893
2664.627603	109438.974456	56.951898
2663.911537	109163.682134	56.956903
2663.524340	108879.749211	56.961908
2662.617356	108586.307898	56.966913
2661.869016	108324.247418	56.971917
2661.475718	108045.192006	56.976922
2660.900213	107765.464381	56.981927
2660.254756	107485.916052	56.986932
2659.583405	107197.397017	56.991937
2659.015489	106914.956099	56.996941
2658.223468	106629.591006	57.001946
2657.905279	106340.696384	57.006951
2656.744244	106050.339950	57.011956
2656.080648	105771.398181	57.016961
2655.710053	105509.327590	57.021965
2654.848305	105209.442662	57.026970
2654.123249	104924.721787	57.031975
2653.700793	104647.956464	57.036980
2652.718625	104367.774736	57.041985
2652.249085	104081.596078	57.046989
2651.594080	103799.079046	57.051994
2650.853221	103528.949672	57.056999
2650.180596	103249.353894	57.062004
2649.225817	102949.639272	57.067009
2648.744827	102677.708601	57.072013
2647.767504	102410.293928	57.077018
2647.427803	102122.133013	57.082023
2646.992205	101849.056607	57.087028
2646.060225	101566.807026	57.092033
2645.305158	101281.335805	57.097037
2644.739326	101010.903325	57.102042
2644.090963	100724.039226	57.107047
2643.348267	100441.132691	57.112052
2642.767084	100165.181348	57.117057
2642.288795	99878.573547	57.122061
2641.190912	99614.882767	57.127066
2640.803572	99313.184265	57.132071
2640.188793	99045.592432	57.137076
2639.443394	98769.335011	57.142081
2638.673287	98481.693612	57.147085
2637.816471	98228.407751	57.152090
2637.657177	97937.403706	57.157095
2636.897005	97649.130649	57.162100
2636.190426	97396.724502	57.167105
2635.874030	97094.619141	57.172109
2634.794161	96810.003407	57.177114
2634.433683	96542.147012	57.182119
2633.684776	96258.754179	57.187124
2632.931773	95978.447696	57.192129
2632.179258	95689.272484	57.197133
2631.146318	95405.599281	57.202138
2630.497223	95141.902004	57.207143
2630.061218	94864.571458	57.212148
2629.075841	94588.986520	57.217153
2628.804419	94298.281804	57.222157
2627.814437	94040.961198	57.227162
2627.590531	93770.909469	57.232167
2626.717600	93491.490181	57.237172
2625.996130	93213.565925	57.242177
2625.333087	92939.136121	57.247181
2624.954104	92663.707230	57.252186
2624.267503	92386.802373	57.257191
2623.649861	92111.202599	57.262196
2622.629466	91838.700933	57.267201
2622.134372	91545.810484	57.272205
2621.424271	91275.124429	57.277210
2620.885198	91000.058735	57.282215
2620.125444	90727.009655	57.287220
2619.510779	90453.826869	57.292225
2618.831910	90164.642346	57.297229
2617.920033	89900.542016	57.302234
2617.489696	89622.236650	57.307239
2616.948117	89344.744966	57.312244
2616.317430	89076.470104	57.317249
2615.735714	88785.950814	57.322253
2615.000944	88516.418746	57.327258
2614.328174	88233.066166	57.332263
2613.982773	87955.028687	57.337268
2613.038583	87684.880880	57.342273
2612.230237	87404.191565	57.347277
2611.709250	87114.953046	57.352282
2611.052430	86837.511870	57.357287
2610.496177	86569.174027	57.362292
2609.640427	86291.498872	57.367297
2609.298417	85987.077889	57.372301
2608.565955	85730.397834	57.377306
2607.798780	85454.976184	57.382311
2607.027381	85173.448248	57.387316
2606.180671	84886.503770	57.392321
2605.700987	84601.704495	57.397325
2604.595502	84340.758457	57.402330
2604.073993	84059.890284	57.407335
2603.265258	83781.784159	57.412340
2602.699782	83504.340363	57.417345
2602.196366	83237.380009	57.422349
2601.502968	82962.898189	57.427354
2601.105252	82709.770114	57.432359
2600.430938	82421.405853	57.437364
2599.721754	82147.082999	57.442369
2599.183185	81860.821791	57.447373
2598.243102	81580.915074	57.452378
2597.443412	81300.444845	57.457383
2596.766364	81033.159912	57.462388
2596.043171	80764.459820	57.467393
2595.821558	80474.206607	57.472397
2595.210446	80199.025706	57.477402
2594.295158	79936.051292	57.482407
2593.600627	79654.617102	57.487412
2593.047627	79379.640702	57.492417
2591.986740	79105.775036	57.497421
2591.542675	78830.332462	57.502426
2590.787536	78555.658929	57.507431
2590.128148	78296.105768	57.512436
2589.122658	78034.088801	57.517441
2588.915595	77741.850472	57.522445
2588.082240	77491.858792	57.527450
2587.504520	77217.472939	57.532455
2587.201546	76933.530262	57.537460
2585.987389	76676.740498	57.542465
2585.439904	76402.240473	57.547469
2584.567096	76133.231971	57.552474
2583.885184	75853.438486	57.557479
2583.520827	75591.193019	57.562484
2582.662771	75314.875242	57.567489
2582.156081	75054.306593	57.572493
2581.410873	74779.093352	57.577498
2580.718496	74512.688112	57.582503
2580.519354	74252.290190	57.587508
2579.630305	73971.668737	57.592513
2579.242783	73696.375654	57.597517
2578.510068	73431.676344	57.602522
2577.541437	73150.280813	57.607527
2577.164001	72879.742319	57.612532
2576.351480	72618.360620	57.617537
2575.510631	72340.472127	57.622541
2575.127606	72070.908408	57.627546
2574.135404	71807.760477	57.632551
2573.963635	71529.694964	57.637556
2573.203045	71256.616840	57.642561
2572.820675	70966.056836	57.647565
2571.894688	70710.229170	57.652570
2571.207644	70425.844290	57.657575
2570.573282	70149.233391	57.662580
2569.931328	69880.380367	57.667585
2569.523588	69583.865540	57.672589
2568.718881	69332.641330	57.677594
2567.967220	69047.349280	57.682599
2567.354698	68763.958429	57.687604
2566.302773	68498.204178	57.692609
2565.565252	68220.294206	57.697613
2564.732873	67940.978238	57.702618
2563.912768	67674.356174	57.707623
2563.566966	67401.655601	57.712628
2562.729180	67134.312289	57.717633
2562.076805	66873.824080	57.722637
2561.737609	66616.149055	57.727642
2561.097025	66329.049141	57.732647
2560.399409	66060.805553	57.737652
2559.374939	65797.354318	57.742657
2558.996996	65525.214128	57.747661
2558.004325	65274.908227	57.752666
2557.512358	64994.754572	57.757671
2557.164255	64728.085804	57.762676
2556.312502	64462.599213	57.767681
2555.830995	64189.756716	57.772685
2554.884537	63921.402060	57.777690
2554.311774	63649.844993	57.782695
2553.420760	63390.084634	57.787700
2552.894097	63130.013647	57.792705
2552.663264	62853.338874	57.797709
2551.532436	62592.272473	57.802714
2550.851374	62320.324220	57.807719
2550.408946	62043.365586	57.812724
2549.506421	61789.216469	57.817729
2548.927713	61519.213577	57.822733
2547.980303	61251.150172	57.827738
2547.419004	60986.685566	57.832743
2546.830383	60719.212320	57.837748
2546.277771	60457.235529	57.842753
2545.657016	60195.928435	57.847757
2544.692141	59935.610142	57.852762
2544.079984	59673.802531	57.857767
2543.816372	59404.932321	57.862772
2542.779909	59149.279767	57.867777
2542.002348	58892.288811	57.872781
2541.362403	58613.816941	57.877786
2540.822214	58370.595484	57.882791
2540.124607	58106.323067	57.887796
2539.545484	57837.667966	57.892801
2538.934028	57570.471431	57.897805
2538.063995	57307.282188	57.902810
2537.423508	57047.810660	57.907815
2537.107973	56785.097996	57.912820
2535.754682	56534.253671	57.917825
2535.048908	56265.524449	57.922829
2534.651525	56010.507090	57.927834
2534.226076	55752.361581	57.932839
2533.452648	55492.341305	57.937844
2532.629491	55237.006624	57.942849
2532.331552	54970.177951	57.947853
2531.584985	54721.395162	57.952858
2530.648908	54462.057718	57.957863
2530.213112	54193.350965	57.962868
2529.482863	53946.136209	57.967873
2529.044118	53683.158540	57.972877
2528.009745	53419.567139	57.977882
2527.387463	53153.882859	57.982887
2526.848328	52891.055998	57.987892
2525.958650	52659.046573	57.992897
2525.727799	52368.160495	57.997901
2525.059256	52135.695605	58.002906
2524.133137	51870.119504	58.007911
2523.178730	51609.269186	58.012916
2522.672959	51357.843114	58.017921
2521.990865	51095.286583	58.022925
2521.193891	50841.075973	58.027930
2520.453119	50587.394733	58.032935
2520.177421	50331.969790	58.037940
2519.483784	50088.807380	58.042945
2518.692821	49823.645138	58.047949
2517.945951	49575.480719	58.052954
2517.041570	49333.975420	58.057959
2516.689582	49074.721113	58.062964
2515.885592	48815.573867	58.067969
2515.546089	48572.429826	58.072973
2514.375437	48313.550492	58.077978
2513.871221	48049.840222	58.082983
2513.019174	47807.262422	58.087988
2511.889441	47553.961335	58.092993
2511.583600	47317.993812	58.097997
2511.165374	47074.718368	58.103002
2510.444205	46828.973353	58.108007
2509.783296	46582.602271	58.113012
2508.850654	46339.007354	58.118017
2508.478543	46105.919590	58.123021
2507.559282	45851.448881	58.128026
2506.895910	45608.213639	58.133031
2506.293421	45361.531016	58.138036
2505.598192	45118.430988	58.143041
2505.347573	44871.364265	58.148045
2504.513500	44626.050756	58.153050
2503.365764	44390.790596	58.158055
2502.775675	44142.861373	58.163060
2502.119391	43902.694358	58.168065
2501.552095	43664.635421	58.173069
2500.878693	43427.282821	58.178074
2500.314986	43183.173867	58.183079
2499.528729	42943.632115	58.188084
2498.482230	42712.002748	58.193089
2497.790126	42460.502430	58.198093
2497.204411	42241.012667	58.203098
2496.616287	42004.545197	58.208103
2495.871181	41773.974776	58.213108
2495.059794	41545.675687	58.218113
2494.407636	41308.089595	58.223117
2493.580507	41091.157123	58.228122
2492.970794	40856.174477	58.233127
2492.395594	40633.301322	58.238132
2491.414593	40411.953024	58.243137
2491.435603	40172.290322	58.248141
2490.546916	39946.756635	58.253146
2489.585364	39717.848084	58.258151
2489.120121	39484.078688	58.263156
2488.001149	39270.513270	58.268161
2487.586800	39052.796698	58.273165
2486.814596	38820.872981	58.278170
2486.073075	38604.987663	58.283175
2485.492766	38380.540316	58.288180
2484.325449	38184.640595	58.293185
2483.328250	37963.567017	58.298189
2482.601144	37746.507991	58.303194
2481.945994	37544.213318	58.308199
2481.420523	37347.993939	58.313204
2480.635343	37144.553407	58.318209
2479.635684	36937.885358	58.323213
2478.880671	36737.517683	58.328218
2477.804461	36554.339961	58.333223
2476.982559	36363.443967	58.338228
2475.931681	36194.421685	58.343233
2475.112850	36017.022282	58.348237
2474.119611	35845.084631	58.353242
2473.400644	35677.676067	58.358247
2472.272737	35514.142969	58.363252
2471.118626	35364.074890	58.368257
2470.475811	35205.084468	58.373261
2469.519644	35073.927784	58.378266
2468.804441	34935.865392	58.383271
2468.156397	34782.318080	58.388276
2467.173569	34655.954405	58.393281
2466.316990	34508.964991	58.398285
2466.169780	34379.828535	58.403290
2465.083607	34261.305521	58.408295
2464.590998	34122.938018	58.413300
2463.812229	34001.850624	58.418305
2462.980363	33856.209513	58.423309
2462.222015	33737.951171	58.428314
2461.636490	33617.872630	58.433319
2460.924228	33497.306197	58.438324
2460.069494	33383.842883	58.443329
2459.640217	33275.188032	58.448333
2458.992057	33151.273265	58.453338
2457.992393	33038.657029	58.458343
2457.505710	32917.610268	58.463348
2456.948381	32803.601272	58.468353
2456.325960	32689.462742	58.473357
2455.568157	32577.318558	58.478362
2454.991481	32462.635496	58.483367
2454.765399	32339.901933	58.488372
2453.934415	32230.524384	58.493377
2453.107626	32112.298003	58.498381
2452.569939	32003.561253	58.503386
2451.665672	31873.361869	58.508391
2451.293771	31767.199721	58.513396
2450.218185	31660.336058	58.518401
2449.923702	31541.882437	58.523405
2449.190593	31433.009789	58.528410
2448.696532	31317.575802	58.533415
2448.030042	31202.776711	58.538420
2447.340231	31086.443141	58.543425
2446.638805	30972.090460	58.548429
2445.966975	30864.774538	58.553434
2445.538213	30756.046158	58.558439
2445.003111	30642.195560	58.563444
2444.047805	30526.293584	58.568449
2443.781909	30408.925916	58.573453
2442.946439	30300.835417	58.578458
2442.152153	30189.100424	58.583463
2442.038796	30068.108678	58.588468
2441.083375	29956.166990	58.593473
2440.137850	29837.365982	58.598477
2439.571541	29730.840224	58.603482
2439.225142	29615.473831	58.608487
2438.779039	29498.686344	58.613492
2437.430444	29384.426839	58.618497
2436.968565	29262.180270	58.623501
2436.567518	29140.259908	58.628506
2435.971261	29034.765628	58.633511
2435.568571	28914.090573	58.638516
2435.009047	28797.318202	58.643521
2434.568156	28682.659050	58.648525
2433.429487	28563.488790	58.653530
2432.703808	28441.639355	58.658535
2432.242514	28324.785299	58.663540
2431.060694	28209.785658	58.668545
2430.587171	28082.726739	58.673549
2430.032174	27975.379736	58.678554
2429.268116	27857.344841	58.683559
2428.712744	27749.326425	58.688564
2428.133480	27636.268453	58.693569
2427.281851	27519.707204	58.698573
2426.787993	27405.984880	58.703578
2426.126517	27299.401709	58.708583
2425.524287	27175.543926	58.713588
2424.563706	27059.119384	58.718593
2424.049946	26941.201571	58.723597
2423.541641	26826.270076	58.728602
2422.642389	26708.178929	58.733607
2422.444331	26585.592442	58.738612
2421.792207	26484.871208	58.743617
2421.064129	26366.766485	58.748621
2420.375881	26244.557279	58.753626
2419.572319	26135.857674	58.758631
2418.903772	26015.053705	58.763636
2417.935512	25901.597291	58.768641
2417.499139	25774.570412	58.773645
2416.964121	25657.669181	58.778650
2416.237608	25560.356798	58.783655
2415.723608	25440.361114	58.788660
2415.359589	25321.190740	58.793665
2414.548650	25204.350778	58.798669
2413.955276	25090.910956	58.803674
2412.928063	24971.237870	58.808679
2412.781443	24850.099323	58.813684
2411.901753	24729.359851	58.818689
2411.025022	24612.268514	58.823693
2410.511747	24497.458738	58.828698
2409.721136	24386.732303	58.833703
2409.128291	24256.907248	58.838708
2408.571732	24151.459208	58.843713
2408.077254	24036.926949	58.848717
2407.577149	23922.176085	58.853722
2406.397702	23807.067062	58.858727
2405.976696	23673.072940	58.863732
2405.365345	23566.944132	58.868737
2404.155674	23446.427799	58.873741
2403.703308	23323.725002	58.878746
2402.889919	23221.337948	58.883751
2402.524209	23093.549718	58.888756
2401.827740	22985.212303	58.893761
2401.175439	22874.935614	58.898765
2400.282517	22764.378048	58.903770
2399.681044	22648.949692	58.908775
2398.904536	22533.207240	58.913780
2398.164007	22419.812954	58.918785
2397.505487	22307.119488	58.923789
2396.940223	22201.200182	58.928794
2396.486136	22101.141663	58.933799
2395.699682	21989.880161	58.938804
2394.840132	21878.173078	58.943809
2394.010967	21762.919945	58.948813
2393.625425	21658.980506	58.953818
2392.732721	21559.420545	58.958823
2392.249879	21447.978132	58.963828
2391.454439	21348.499618	58.968833
2390.789187	21229.195316	58.973837
2390.166066	21111.658544	58.978842
2389.490750	21026.355802	58.983847
2388.815422	20921.085098	58.988852
2388.027287	20816.820287	58.993857
2387.514095	20723.905749	58.998861
2386.744589	20616.414518	59.003866
2385.774482	20517.390168	59.008871
2385.233237	20397.654075	59.013876
2384.916640	20316.734930	59.018881
2383.841477	20200.119843	59.023885
2383.241809	20108.948099	59.028890
2382.199062	20006.332109	59.033895
2381.518717	19909.974771	59.038900
2380.726037	19825.161782	59.043905
2380.104129	19727.729324	59.048909
2379.760704	19630.011740	59.053914
2378.890393	19544.775613	59.058919
2378.525572	19450.122103	59.063924
2377.628003	19353.101209	59.068929
2376.739567	19262.242683	59.073933
2376.617909	19162.720546	59.078938
2375.685367	19074.361982	59.083943
2375.002798	18988.299821	59.088948
2374.342862	18897.936106	59.093953
2373.807505	18795.593784	59.098957
2373.308999	18703.634646	59.103962
2372.205045	18615.803198	59.108967
2371.870653	18516.303524	59.113972
2371.015225	18429.838473	59.118977
2370.262507	18345.789760	59.123981
2369.897695	18248.666797	59.128986
2368.888730	18153.749520	59.133991
2368.521567	18047.702543	59.138996
2367.190600	17977.222731	59.144001
2366.781771	17881.847259	59.149005
2366.272898	17793.147383	59.154010
2365.793102	17714.734795	59.159015
2365.021983	17624.885716	59.164020
2364.260703	17542.623911	59.169025
2363.594210	17448.541518	59.174029
2363.125426	17357.831629	59.179034
2362.096677	17271.738360	59.184039
2361.600065	17189.473562	59.189044
2360.811103	17102.965707	59.194049
2360.330063	17013.979940	59.199053
2360.139113	16927.667133	59.204058
2359.158504	16841.121672	59.209063
2358.686232	16744.480806	59.214068
2357.886885	16655.624535	59.219073
2357.246200	16573.706321	59.224077
2356.498477	16489.087144	59.229082
2355.744676	16395.572189	59.234087
2354.968896	16303.512803	59.239092
2354.253315	16220.178532	59.244097
2353.477899	16133.828069	59.249101
2353.055941	16050.298980	59.254106
2351.830763	15972.162605	59.259111
2351.413004	15889.773934	59.264116
2351.093226	15811.944981	59.269121
2350.367920	15730.264383	59.274125
2349.749338	15645.516892	59.279130
2348.970843	15562.625517	59.284135
2348.010824	15473.116570	59.289140
2347.565100	15402.519007	59.294145
2346.925985	15312.057504	59.299149
2346.374913	15231.217239	59.304154
2345.841855	15156.809199	59.309159
2345.038711	15073.831242	59.314164
2344.374663	14986.193868	59.319169
2343.714625	14895.610480	59.324173
2342.867534	14818.662559	59.329178
2341.910904	14745.946839	59.334183
2341.966395	14657.240021	59.339188
2340.930587	14581.476850	59.344193
2340.191856	14497.744912	59.349197
2339.530753	14424.420733	59.354202
2338.657329	14363.683048	59.359207
2338.236714	14271.330138	59.364212
2337.508506	14193.535194	59.369217
2336.299145	14130.998793	59.374221
2335.998190	14046.568752	59.379226
2335.461581	13976.360399	59.384231
2334.842726	13885.272867	59.389236
2333.886256	13819.273816	59.394241
2333.281668	13743.423141	59.399245
2333.411979	13659.374106	59.404250
2332.244774	13589.223762	59.409255
2331.573233	13519.289196	59.414260
2330.999924	13438.526442	59.419265
2330.656227	13358.307726	59.424269
2329.830999	13291.451781	59.429274
2329.220731	13208.625794	59.434279
2328.814255	13116.758012	59.439284
2327.789886	13051.923907	59.444289
2327.012998	12974.296390	59.449293
2326.419702	12889.504131	59.454298
2325.609473	12813.078046	59.459303
2325.087458	12734.562639	59.464308
2324.483768	12661.162969	59.469313
2323.551742	12580.100049	59.474317
2322.853910	12502.616675	59.479322
2322.123067	12432.696313	59.484327
2321.748554	12354.875582	59.489332
2320.936873	12279.444305	59.494337
2320.105450	12210.832261	59.499341
2319.831087	12134.254187	59.504346
2318.677506	12074.866141	59.509351
2317.838587	12000.149167	59.514356
2317.536021	11925.728031	59.519361
2316.730747	11856.863901	59.524365
2316.031516	11794.044068	59.529370
2315.144514	11722.277131	59.534375
2314.743821	11651.690774	59.539380
2313.669651	11586.308441	59.544385
2313.451175	11511.238057	59.549389
2313.200746	11452.117364	59.554394
2311.881231	11380.129881	59.559399
2311.349580	11306.938784	59.564404
2310.617405	11247.251831	59.569409
2310.479540	11175.547401	59.574413
2309.642348	11116.402722	59.579418
2308.869445	11041.022759	59.584423
2308.436912	10973.756549	59.589428
2307.750239	10902.592955	59.594433
2306.906971	10836.447413	59.599437
2306.577902	10746.034689	59.604442
2305.976406	10691.298002	59.609447
2305.321096	10613.840837	59.614452
2304.520553	10539.798614	59.619457
2303.848277	10463.084601	59.624461
2303.551026	10386.283493	59.629466
2302.209803	10317.994248	59.634471
2301.655176	10244.715693	59.639476
2301.202777	10168.882345	59.644481
2300.136965	10112.857255	59.649485
2299.827098	10047.694521	59.654490
2298.821471	9983.527242	59.659495
2298.288488	9913.064281	59.664500
2297.860163	9835.732916	59.669505
2297.106313	9764.680822	59.674509
2296.651794	9692.707824	59.679514
2295.742428	9635.054186	59.684519
2295.235096	9550.091884	59.689524
2294.634259	9484.449144	59.694529
2293.620007	9412.811228	59.699533
2293.241067	9342.459056	59.704538
2292.483194	9266.930380	59.709543
2291.870148	9206.696950	59.714548
2290.908574	9139.551249	59.719553
2290.296253	9077.606257	59.724557
2289.882885	9006.996436	59.729562
2288.862397	8947.360401	59.734567
2288.227373	8871.138533	59.739572
2287.541566	8804.446036	59.744577
2286.965009	8749.513277	59.749581
2286.499496	8679.273407	59.754586
2285.467931	8613.989563	59.759591
2284.748436	8546.550558	59.764596
2284.521721	8483.427823	59.769601
2283.495777	8418.388105	59.774605
2283.394626	8342.300414	59.779610
2282.509740	8286.396261	59.784615
2282.305981	8207.225232	59.789620
2281.449162	8130.029403	59.794625
2280.602743	8086.398700	59.799629
2279.997400	8007.715254	59.804634
2279.171834	7933.751413	59.809639
2278.481972	7864.539007	59.814644
2277.820957	7797.814339	59.819649
2277.011535	7736.238279	59.824653
2276.553807	7669.865324	59.829658
2275.315405	7613.487296	59.834663
2274.950586	7547.418055	59.839668
2274.532121	7471.502667	59.844673
2273.770535	7416.748915	59.849677
2273.138380	7340.040603	59.854682
2272.526770	7285.263549	59.859687
2271.657155	7224.434738	59.864692
2271.153931	7160.238961	59.869697
2270.125356	7095.601433	59.874701
2269.676604	7030.646621	59.879706
2268.871681	6992.916035	59.884711
2268.473461	6915.068476	59.889716
2268.112190	6851.768111	59.894721
2267.095209	6792.694292	59.899725
2266.728678	6728.007788	59.904730
2266.043473	6661.203714	59.909735
2265.358094	6605.278976	59.914740
2264.289178	6538.795826	59.919745
2264.148812	6472.849574	59.924750
2263.306231	6402.977225	59.929754
2262.342101	6343.770611	59.934759
2261.849945	6279.089425	59.939764
2261.399747	6219.492594	59.944769
2260.674070	6155.384563	59.949774
2259.677022	6088.665662	59.954778
2259.110001	6031.956850	59.959783
2258.653732	5966.595369	59.964788
2258.079058	5900.270170	59.969793
2257.117332	5838.102641	59.974798
2257.056959	5773.917556	59.979802
2255.791331	5716.006711	59.984807
2255.293249	5638.499559	59.989812
2254.475378	5578.081818	59.994817
2253.670834	5532.428100	59.999822
2253.074183	5462.615048	60.004826
2252.358300	5406.207517	60.009831
2251.771462	5342.752987	60.014836
2251.214934	5282.681478	60.019841
2250.568687	5229.369562	60.024846
2250.230049	5153.075589	60.029850
2249.192852	5094.263372	60.034855
2248.525981	5041.011407	60.039860
2248.208740	4981.609065	60.044865
2247.705942	4917.534154	60.049870
2246.997794	4849.452383	60.054874
2246.341695	4797.370018	60.059879
2245.674622	4722.605227	60.064884
2244.590939	4648.163220	60.069889
2243.953575	4576.449045	60.074894
2243.480933	4525.369353	60.079898
2242.705805	4469.571050	60.084903
2241.952004	4400.810870	60.089908
2241.324874	4341.068294	60.094913
2240.597094	4284.688243	60.099918
2240.077579	4222.276002	60.104922
2239.308993	4157.844341	60.109927
2238.915694	4100.145353	60.114932
2238.085207	4042.775407	60.119937
2237.603901	3984.888147	60.124942
2236.978049	3906.393802	60.129946
2235.608425	3855.335692	60.134951
2235.048183	3802.870987	60.139956
2234.831848	3739.769175	60.144961
2233.789213	3678.148847	60.149966
2233.095477	3630.154627	60.154970
2232.329538	3574.254963	60.159975
2231.788924	3510.168529	60.164980
2231.671105	3453.804538	60.169985
2230.695852	3396.206151	60.174990
2229.946094	3333.282970	60.179994
2229.480196	3275.807725	60.184999
2228.719937	3210.710952	60.190004
2228.176359	3162.369540	60.195009
2227.519797	3109.261746	60.200014
2226.827609	3044.620980	60.205018
2226.271517	2992.790189	60.210023
2225.574075	2933.625987	60.215028
2224.749880	2867.474704	60.220033
2223.732020	2830.833468	60.225038
2223.395764	2758.534717	60.230042
2222.488889	2705.992505	60.235047
2221.551704	2651.340320	60.240052
2221.346785	2598.434013	60.245057
2220.737953	2546.060381	60.250062
2220.157211	2484.198337	60.255066
2219.245798	2424.215331	60.260071
2218.744525	2369.860948	60.265076
2218.183491	2311.844705	60.270081
2217.301647	2265.729255	60.275086
2216.982050	2191.926885	60.280090
2216.151425	2138.720912	60.285095
2215.209910	2089.451027	60.290100
2214.695398	2030.847362	60.295105
2213.979157	1974.680201	60.300110
2213.597125	1919.997107	60.305114
2212.361829	1861.680363	60.310119
2211.994413	1811.062635	60.315124
2211.439566	1758.066640	60.320129
2210.240868	1717.947145	60.325134
2209.544842	1652.400044	60.330138
2209.254252	1600.185926	60.335143
2208.645339	1554.884197	60.340148
2208.067947	1500.508075	60.345153
2207.117968	1443.560775	60.350158
2206.725806	1391.156929	60.355162
2205.847825	1339.927944	60.360167
2205.152794	1286.011274	60.365172
2204.973280	1243.941508	60.370177
2204.187299	1196.199394	60.375182
2203.543818	1132.190979	60.380186
2203.021717	1085.158020	60.385191
2202.048778	1030.613011	60.390196
2201.428303	969.193440	60.395201
2200.731604	922.830535	60.400206
2199.959114	873.401561	60.405210
2199.206811	823.961668	60.410215
2198.715350	772.328019	60.415220
2198.106803	713.444964	60.420225
2197.246531	669.783326	60.425230
2196.767520	608.030609	60.430234
2195.709613	552.540527	60.435239
2195.341830	519.396630	60.440244
2194.676605	472.804673	60.445249
2193.714560	426.799260	60.450254
2193.040056	373.070387	60.455258
2192.320301	338.626596	60.460263
2191.679105	288.710450	60.465268
2191.005246	250.861360	60.470273
2189.918994	207.199125	60.475278
2189.417636	163.753307	60.480282
2188.659682	130.451434	60.485287
2187.900964	89.580724	60.490292
2187.355327	55.223524	60.495297
2186.327959	28.429832	60.500302
2185.728615	-16.862188	60.505306
2184.285167	-27.004234	60.510311
2183.547248	-31.360710	60.515316
2178.888427	60.471273	60.520321
2177.259604	99.897862	60.525326
2178.264269	92.488010	60.530330
2178.991270	84.138236	60.535335
2179.117244	98.846370	60.540340
2179.488982	84.871448	60.545345
2178.737963	91.668726	60.550350
2178.089749	98.017631	60.555354
2177.002984	93.333280	60.560359
2175.862445	83.437983	60.565364
2174.859929	98.952744	60.570369
2173.993470	108.545235	60.575374
2174.086375	84.782680	60.580378
2173.544975	110.204386	60.585383
2172.677991	80.687113	60.590388
2172.407979	108.446852	60.595393
2172.006529	106.451168	60.600398
2171.216365	87.168290	60.605402
2170.495141	112.504993	60.610407
2169.783640	101.907713	60.615412
2169.038515	89.871352	60.620417
2167.849696	114.555298	60.625422
2167.262853	83.500270	60.630426
2166.478625	95.804560	60.635431
2166.290112	100.509963	60.640436
2165.927140	87.017436	60.645441
2164.948812	107.151789	60.650446
2164.293290	85.375002	60.655450
2163.676464	113.492532	60.660455
2163.557910	85.177947	60.665460
2163.083681	99.315856	60.670465
2161.666772	97.955919	60.675470
2161.334176	89.597634	60.680474
2160.758936	101.499783	60.685479
2160.099773	87.764102	60.690484
2159.490419	100.846441	60.695489
2158.686703	99.084883	60.700494
2157.739732	92.361529	60.705498
2157.264755	97.683211	60.710503
2156.272808	102.367854	60.715508
2155.447814	89.842721	60.720513
2154.751311	94.054732	60.725518
2154.737003	95.518810	60.730522
2154.604120	105.141570	60.735527
2153.586755	104.087239	60.740532
2153.030688	91.976735	60.745537
2151.543995	99.836869	60.750542
2151.171522	95.185853	60.755546
2150.795388	95.458446	60.760551
2150.376786	94.597690	60.765556
2149.914446	85.175100	60.770561
2148.965389	102.903215	60.775566
2148.210844	92.208705	60.780570
2147.491489	98.671401	60.785575
2146.748418	105.525775	60.790580
2146.415746	96.088913	60.795585
2145.511721	97.381928	60.800590
2144.803403	102.106727	60.805594
2144.052938	92.124323	60.810599
2143.209459	103.346822	60.815604
2142.487460	99.509742	60.820609
2141.509288	104.056593	60.825614
2141.337010	102.921802	60.830618
2141.274805	102.753522	60.835623
2139.951265	101.802964	60.840628
2140.028246	93.409659	60.845633
2138.798880	101.317278	60.850638
2138.262798	92.685365	60.855642
2137.744583	92.529514	60.860647
2137.216219	104.012664	60.865652
2136.574960	92.000835	60.870657
2135.261469	100.208794	60.875662
2134.844013	95.186467	60.880666
2134.696241	98.087760	60.885671
2133.643448	98.549712	60.890676
2132.786808	109.228704	60.895681
2132.817431	101.856686	60.900686
2132.007427	93.012781	60.905690
2130.814830	105.796597	60.910695
2129.756649	101.995515	60.915700
2130.094314	105.161973	60.920705
2128.976554	102.474161	60.925710
2128.727686	90.832144	60.930714
2127.625494	96.996055	60.935719
2126.743354	115.189790	60.940724
2126.878288	101.906831	60.945729
2126.008272	94.879556	60.950734
2125.292970	94.743940	60.955738
2123.993009	98.197034	60.960743
2123.344719	103.163038	60.965748
2123.782314	92.069664	60.970753
2122.783254	107.259059	60.975758
2122.069416	101.189401	60.980762
2121.509648	94.248515	60.985767
2120.432412	94.482548	60.990772
2119.997161	92.796577	60.995777
2119.298892	104.308263	61.000782
2118.799708	86.019988	61.005786
2118.110643	91.077610	61.010791
2117.736388	103.599127	61.015796
2116.987692	91.774655	61.020801
2115.569350	108.862915	61.025806
2114.890462	99.771138	61.030810
2114.841660	94.275602	61.035815
2113.726498	104.043177	61.040820
2113.386209	81.327042	61.045825
2112.500799	108.971535	61.050830
2112.013821	93.423516	61.055834
2111.495933	99.150963	61.060839
2110.443115	94.920128	61.065844
2110.044559	85.687691	61.070849
2109.079707	110.910089	61.075854
2108.798718	90.008988	61.080858
2108.114149	78.975411	61.085863
2107.522678	113.295512	61.090868
2107.287565	73.388877	61.095873
2106.323234	114.059890	61.100878
2106.059129	85.664346	61.105882
2105.421924	100.764784	61.110887
2103.578522	111.829002	61.115892
2103.315955	92.957578	61.120897
2102.547641	102.870384	61.125902
2101.634757	95.561352	61.130906
2101.700997	100.295717	61.135911
2100.876647	96.626272	61.140916
2100.331245	110.438033	61.145921
2099.653831	105.456959	61.150926
2098.967672	106.250239	61.155930
2098.719772	98.208092	61.160935
2097.631593	102.190542	61.165940
2097.519153	85.279026	61.170945
2096.262087	94.564515	61.175950
2094.868772	104.587534	61.180954
2094.662446	85.306670	61.185959
2093.958334	100.245845	61.190964
2093.941556	83.021123	61.195969
2092.660127	108.694279	61.200974
2091.931159	93.362853	61.205978
2091.800633	86.407483	61.210983
2090.573104	124.570472	61.215988
2090.618623	83.397204	61.220993
2090.013661	112.706541	61.225998
2089.405467	98.917060	61.231002
2089.033455	92.567683	61.236007
2087.431514	99.019057	61.241012
2086.940701	92.530843	61.246017
2085.934913	100.846108	61.251022
2085.243067	98.511761	61.256026
2085.327907	96.246550	61.261031
2084.478011	103.374918	61.266036
2083.999160	89.375699	61.271041
2083.373740	88.636078	61.276046
2082.625699	98.536207	61.281050
2082.276867	103.841037	61.286055
2080.803651	99.870879	61.291060
2080.163277	93.138329	61.296065
2079.558154	102.810788	61.301070
2079.119825	88.522880	61.306074
2078.284773	92.539281	61.311079
2077.516883	105.750862	61.316084
2077.168769	86.924566	61.321089
2076.567175	104.357872	61.326094
2076.164937	104.588888	61.331098
2075.733008	96.202227	61.336103
2074.857634	104.622953	61.341108
2073.836811	95.333151	61.346113
2073.030698	98.554947	61.351118
2072.284518	88.887270	61.356122
2071.944158	85.757597	61.361127
2071.058469	96.753425	61.366132
2071.005905	85.763063	61.371137
2070.263348	103.655533	61.376142
2069.351787	96.526069	61.381146
2068.619275	88.616024	61.386151
2067.817210	85.750420	61.391156
2067.378856	94.617433	61.396161
2066.944792	86.391961	61.401166
2066.348979	106.971806	61.406170
2065.819060	103.129499	61.411175
2064.027110	93.097940	61.416180
2063.303126	104.717789	61.421185
2063.228623	100.174039	61.426190
2062.796299	78.112748	61.431194
2061.807216	106.246752	61.436199
2061.151509	89.219608	61.441204
2060.605356	114.367690	61.446209
2060.159872	80.472407	61.451214
2059.738546	113.433038	61.456218
2059.616756	87.055413	61.461223
2057.657841	113.239774	61.466228
2057.584741	94.734093	61.471233
2056.462472	86.650948	61.476238
2055.765005	108.006982	61.481242
2055.466290	85.462454	61.486247
2054.970265	93.895516	61.491252
2054.589229	92.006997	61.496257
2053.293704	87.217067	61.501262
2051.971471	107.954765	61.506266
2052.334286	87.692655	61.511271
2051.046459	95.574889	61.516276
2050.520453	95.861818	61.521281
2050.157822	89.164048	61.526286
2049.871044	89.058215	61.531290
2049.392010	84.862506	61.536295
2048.460032	97.653865	61.541300
2047.758307	93.737910	61.546305
2046.990377	87.937052	61.551310
2046.144356	77.075771	61.556314
2045.949373	91.197744	61.561319
2044.924013	108.414466	61.566324
2044.072216	93.859457	61.571329
2043.013151	92.371838	61.576334
2042.446910	88.234121	61.581338
2042.234646	87.419484	61.586343
2041.302900	101.175861	61.591348
2040.953017	92.645310	61.596353
2040.281800	99.267537	61.601358
2039.805257	92.592576	61.606362
2039.602003	97.450124	61.611367
2038.226713	94.081012	61.616372
2037.647927	93.401807	61.621377
2036.631364	93.640438	61.626382
2036.166568	89.125518	61.631386
2035.837792	84.776662	61.636391
2035.246282	107.129813	61.641396
2034.671033	99.240547	61.646401
2033.410756	93.036878	61.651406
2032.586043	97.993050	61.656410
2032.298807	89.288565	61.661415
2031.443156	96.266476	61.666420
2031.234483	97.513828	61.671425
2030.707596	91.767758	61.676430
2030.200194	93.265935	61.681434
2029.582694	84.623328	61.686439
2028.090699	103.700707	61.691444
2027.590231	89.720706	61.696449
2027.164134	90.794415	61.701454
2026.438481	80.923240	61.706458
2026.278315	82.208623	61.711463
2024.868395	93.497378	61.716468
2024.120772	85.154531	61.721473
2023.140055	81.071561	61.726478
2022.496161	85.674198	61.731482
2022.321116	87.703076	61.736487
2022.017437	75.284508	61.741492
2021.498721	84.001853	61.746497
2021.234589	86.432781	61.751502
2019.693798	94.216408	61.756506
2019.231470	84.177293	61.761511
2018.420741	77.415038	61.766516
2017.892825	106.322639	61.771521
2017.557674	88.020983	61.776526
2016.651786	75.923483	61.781530
2015.587492	80.174967	61.786535
2014.656337	88.311251	61.791540
2014.048526	71.320701	61.796545
2013.794887	95.255433	61.801550
2013.104866	65.766978	61.806554
2012.683950	92.076222	61.811559
2012.269192	87.250605	61.816564
2011.897540	70.694064	61.821569
2010.749824	92.991970	61.826574
2009.859946	72.277445	61.831578
2009.479283	98.665463	61.836583
2009.079464	89.911045	61.841588
2007.751582	74.964873	61.846593
2006.867273	90.699009	61.851598
2006.018454	96.900017	61.856602
2006.062780	83.681927	61.861607
2004.974002	78.425572	61.866612
2004.785612	104.445633	61.871617
2004.340175	68.265503	61.876622
2003.822074	102.313732	61.881626
2002.888065	84.364162	61.886631
2001.805610	84.515497	61.891636
2000.967437	95.812865	61.896641
2000.910532	93.313119	61.901646
2000.025856	81.633282	61.906650
2000.082704	103.639110	61.911655
1998.803345	76.352465	61.916660
1997.771434	90.298195	61.921665
1997.244780	93.732688	61.926670
1997.083907	88.663362	61.931674
1996.595136	73.326992	61.936679
1995.377339	92.352965	61.941684
1994.780353	91.481126	61.946689
1994.325710	89.856600	61.951694
1993.627568	89.015008	61.956698
1992.638183	74.713681	61.961703
1991.431670	99.742623	61.966708
1990.885517	76.693380	61.971713
1990.415876	83.483879	61.976718
1990.611782	92.256538	61.981722
1989.925858	70.438955	61.986727
1988.968083	84.901169	61.991732
1988.577695	83.124528	61.996737
1987.836040	85.339526	62.001742
1986.706171	93.343364	62.006746
1986.155468	80.954546	62.011751
1985.170738	102.036059	62.016756
1985.042628	84.721799	62.021761
1983.845402	76.464523	62.026766
1983.090558	101.193135	62.031770
1982.439014	72.811854	62.036775
1982.143053	101.152794	62.041780
1981.338313	84.392185	62.046785
1980.873266	83.023192	62.051790
1980.370438	75.368454	62.056794
1980.277201	106.752139	62.061799
1979.440414	87.487798	62.066804
1978.839837	75.963147	62.071809
1977.841455	81.678563	62.076814
1976.716932	81.702551	62.081818
1976.115662	88.062959	62.086823
1974.948635	87.108144	62.091828
1974.349712	84.940424	62.096833
1974.165758	86.232739	62.101838
1973.714380	94.086316	62.106842
1973.821602	82.725273	62.111847
1972.865471	91.745432	62.116852
1971.864062	80.311208	62.121857
1971.034055	84.482946	62.126862
1970.216594	87.091586	62.131866
1969.959509	86.462256	62.136871
1968.521249	89.834873	62.141876
1968.122216	81.933436	62.146881
1967.594225	82.577070	62.151886
1966.746956	78.685822	62.156890
1966.482896	92.993787	62.161895
1966.064355	87.878636	62.166900
1965.529304	81.791699	62.171905
1964.653206	79.871393	62.176910
1963.458418	96.208306	62.181914
1963.397845	75.623933	62.186919
1962.790932	80.654352	62.191924
1961.875689	80.771278	62.196929
1960.539881	93.454871	62.201934
1959.510041	100.318530	62.206938
1959.500114	83.340317	62.211943
1958.783175	81.967157	62.216948
1958.312043	104.878332	62.221953
1958.352435	79.542560	62.226958
1957.968441	80.038767	62.231962
1956.581057	97.434376	62.236967
1955.640791	84.459302	62.241972
1955.108625	95.857911	62.246977
1954.716446	83.857081	62.251982
1953.884702	97.662251	62.256986
1953.516688	85.173483	62.261991
1952.321524	88.520137	62.266996
1951.969893	84.220653	62.272001
1951.564819	88.034804	62.277006
1950.471020	74.204214	62.282010
1949.898357	79.112509	62.287015
1949.188454	80.852567	62.292020
1948.662163	81.518011	62.297025
1948.049420	73.680466	62.302030
1946.861963	94.064059	62.307034
1946.303554	61.828338	62.312039
1945.148888	109.147681	62.317044
1945.405854	72.633740	62.322049
1944.598985	90.553758	62.327054
1943.614654	87.797548	62.332058
1943.542912	97.852112	62.337063
1943.266929	84.207079	62.342068
1942.217347	80.694865	62.347073
1941.536879	88.956949	62.352078
1940.878834	90.647779	62.357082
1940.087491	79.478257	62.362087
1939.155859	88.459843	62.367092
1938.446821	75.269895	62.372097
1938.077782	94.908599	62.377102
1937.369756	93.270690	62.382106
1937.053165	81.393480	62.387111
1935.773861	90.387680	62.392116
1934.467545	94.248703	62.397121
1934.413794	87.011520	62.402126
1933.602356	91.399509	62.407130
1932.980688	80.994648	62.412135
1932.424431	95.397879	62.417140
1931.932177	93.153314	62.422145
1931.366365	99.001928	62.427150
1931.223390	101.177101	62.432154
1930.803342	85.426152	62.437159
1929.388732	92.792420	62.442164
1928.528646	86.873776	62.447169
1928.289618	83.283363	62.452174
1927.424143	89.898597	62.457178
1927.109983	84.957687	62.462183
1925.833475	99.812706	62.467188
1925.630188	93.132243	62.472193
1924.658801	100.227897	62.477198
1924.288310	100.947459	62.482202
1923.868868	91.160166	62.487207
1922.738531	100.640062	62.492212
1922.203474	92.943141	62.497217
1921.631738	97.863914	62.502222
1920.936209	91.113365	62.507226
1920.395478	84.552701	62.512231
1919.426514	92.389100	62.517236
1918.793454	104.319373	62.522241
1918.780709	90.375523	62.527246
1917.494398	84.707461	62.532250
1916.548559	97.382783	62.537255
1915.671935	101.697553	62.542260
1914.957487	91.905056	62.547265
1914.880605	82.993750	62.552270
1914.275533	78.698238	62.557274
1914.021201	98.955795	62.562279
1913.398304	92.411326	62.567284
1912.558504	91.391980	62.572289
1911.483337	77.806021	62.577294
1910.841603	92.971836	62.582298
1910.616220	96.145639	62.587303
1909.633251	92.305910	62.592308
1908.697857	87.988721	62.597313
1908.603240	87.899705	62.602318
1907.717994	83.563519	62.607322
1907.266472	87.593195	62.612327
1906.137498	90.227651	62.617332
1905.235836	95.222878	62.622337
1904.980087	87.144173	62.627342
1904.371921	103.786936	62.632346
1904.029779	78.444100	62.637351
1903.300687	87.193279	62.642356
1901.802961	79.590847	62.647361
1901.813465	93.300162	62.652366
1901.123890	98.843590	62.657370
1900.724668	74.709828	62.662375
1899.483045	99.318604	62.667380
1898.613663	85.972776	62.672385
1898.352406	77.543309	62.677390
1897.400346	99.212550	62.682394
1897.143230	88.869666	62.687399
1896.819674	82.082155	62.692404
1895.906736	99.273165	62.697409
1895.404673	79.090035	62.702414
1894.457053	84.102018	62.707418
1894.210508	107.551523	62.712423
1892.877229	88.725572	62.717428
1891.714628	98.284711	62.722433
1891.579415	83.157156	62.727438
1890.841204	82.164266	62.732442
1890.680613	84.324889	62.737447
1890.272095	97.977731	62.742452
1889.534126	97.874161	62.747457
1888.774707	88.569763	62.752462
1887.552756	86.641313	62.757466
1887.444767	89.405414	62.762471
1886.811829	94.518826	62.767476
1885.289197	100.017899	62.772481
1884.963425	90.404972	62.777486
1884.262149	80.186223	62.782490
1883.694941	74.741475	62.787495
1883.666184	100.627356	62.792500
1883.004429	82.825435	62.797505
1881.728333	75.244601	62.802510
1880.844413	104.632879	62.807514
1880.614026	78.114884	62.812519
1880.339539	81.067834	62.817524
1879.431720	90.037771	62.822529
1879.012338	83.475200	62.827534
1878.273830	89.879488	62.832538
1877.569980	78.633028	62.837543
1876.306071	101.832470	62.842548
1875.735088	94.686864	62.847553
1875.077442	86.899040	62.852558
1874.437455	76.632722	62.857562
1874.108010	75.735784	62.862567
1873.930852	98.046788	62.867572
1872.691028	93.516181	62.872577
1872.195088	76.011208	62.877582
1871.547573	96.466788	62.882586
1870.418998	87.722451	62.887591
1869.608039	84.467261	62.892596
1868.835166	82.640982	62.897601
1868.405929	83.590640	62.902606
1867.664981	90.662336	62.907610
1867.556595	82.225948	62.912615
1867.212981	86.639024	62.917620
1866.309763	101.833750	62.922625
1865.793466	95.914160	62.927630
1864.957037	94.569458	62.932634
1864.467919	82.951456	62.937639
1863.313250	85.200520	62.942644
1862.509165	99.598952	62.947649
1862.259657	82.807021	62.952654
1861.477715	86.069186	62.957658
1860.840034	83.606464	62.962663
1859.833178	79.141378	62.967668
1858.970361	89.827701	62.972673
1858.612387	88.646724	62.977678
1858.037026	84.508928	62.982682
1857.934522	96.422773	62.987687
1857.141629	90.797825	62.992692
1855.659457	97.708100	62.997697
1855.660140	83.970282	63.002702
1855.074445	85.551879	63.007706
1854.449275	94.048040	63.012711
1853.566704	94.263890	63.017716
1852.461630	84.356830	63.022721
1851.994136	93.561204	63.027726
1851.679847	78.492055	63.032730
1851.173308	89.604337	63.037735
1850.042732	94.719497	63.042740
1849.287605	85.458588	63.047745
1848.556909	82.126010	63.052750
1848.100280	106.001501	63.057754
1847.809666	83.078892	63.062759
1847.532015	89.676509	63.067764
1846.227732	93.551441	63.072769
1845.728034	82.505955	63.077774
1844.977145	92.996325	63.082778
1844.690439	92.163563	63.087783
1843.378226	88.803470	63.092788
1842.641252	95.029337	63.097793
1842.137271	80.535905	63.102798
1841.579438	89.768813	63.107802
1841.111968	82.810206	63.112807
1840.189252	86.105765	63.117812
1839.304547	90.932745	63.122817
1839.013759	82.613626	63.127822
1838.661258	81.307211	63.132826
1837.759333	89.837851	63.137831
1836.804849	94.008893	63.142836
1835.811704	93.297756	63.147841
1835.783050	84.188001	63.152846
1835.080920	84.346825	63.157850
1835.152875	80.227679	63.162855
1834.029596	89.413177	63.167860
1833.004458	88.670853	63.172865
1832.879165	90.337043	63.177870
1831.626004	84.160742	63.182874
1830.958986	87.773657	63.187879
1829.949009	86.494367	63.192884
1829.119853	91.252608	63.197889
1829.201405	81.920364	63.202894
1828.492177	92.262202	63.207898
1828.152738	88.003379	63.212903
1827.343512	94.313257	63.217908
1826.350093	92.873651	63.222913
1826.255793	89.900482	63.227918
1824.848388	82.946046	63.232922
1823.934447	83.061237	63.237927
1823.528510	81.889459	63.242932
1823.124088	86.512456	63.247937
1822.846135	84.308003	63.252942
1822.262868	92.370181	63.257946
1821.325698	81.665387	63.262951
1820.741586	86.039386	63.267956
1819.918013	91.131041	63.272961
1819.368087	87.268322	63.277966
1818.321466	94.973586	63.282970
1817.400069	87.784296	63.287975
1816.968384	83.346168	63.292980
1816.268020	88.438759	63.297985
1816.093160	89.325959	63.302990
1815.321174	89.087469	63.307994
1814.914591	88.310013	63.312999
1814.089999	84.418372	63.318004
1813.233062	107.146383	63.323009
1813.133588	64.742695	63.328014
1811.446526	74.208511	63.333018
1810.906354	95.435483	63.338023
1810.716668	90.176798	63.343028
1809.797859	99.673603	63.348033
1809.932156	83.199195	63.353038
1808.548687	88.751897	63.358042
1807.912873	90.043432	63.363047
1807.668379	83.226039	63.368052
1806.299203	89.552295	63.373057
1805.513373	92.329415	63.378062
1804.829546	88.625149	63.383066
1804.455509	80.885355	63.388071
1804.086803	73.778622	63.393076
1803.713379	79.420089	63.398081
1803.379780	80.712521	63.403086
1801.979972	81.256511	63.408090
1801.495730	76.271673	63.413095
1800.774493	85.111080	63.418100
1799.550660	80.964311	63.423105
1798.916391	72.512098	63.428110
1798.086004	84.386973	63.433114
1797.870150	80.857549	63.438119
1797.714995	78.673023	63.443124
1797.140632	80.864660	63.448129
1796.711811	75.292311	63.453134
1795.646514	82.309870	63.458138
1794.736848	77.477737	63.463143
1794.309142	69.604555	63.468148
1792.933903	95.887125	63.473153
1792.501731	61.198330	63.478158
1791.778885	88.094770	63.483162
1791.139288	88.391902	63.488167
1791.079411	77.464247	63.493172
1790.250668	81.318881	63.498177
1790.121320	96.028050	63.503182
1788.952787	67.949744	63.508186
1788.175151	95.780523	63.513191
1787.672970	70.150941	63.518196
1786.105904	99.800645	63.523201
1785.939178	80.333826	63.528206
1785.292211	66.333042	63.533210
1785.002334	83.552840	63.538215
1784.759457	79.322847	63.543220
1783.551342	77.696589	63.548225
1783.135936	75.498201	63.553230
1782.263458	90.328521	63.558234
1781.666914	88.903179	63.563239
1780.477554	72.583784	63.568244
1779.657638	83.063043	63.573249
1779.433023	72.323971	63.578254
1778.701268	99.757984	63.583258
1778.387530	80.376011	63.588263
1778.284396	68.446033	63.593268
1777.072385	88.978628	63.598273
1776.659536	77.335933	63.603278
1776.028328	87.416241	63.608282
1774.859756	82.590537	63.613287
1774.153567	81.272490	63.618292
1773.292983	88.117210	63.623297
1773.375995	85.858597	63.628302
1772.569802	81.825285	63.633306
1771.421758	83.258090	63.638311
1770.944455	79.114208	63.643316
1770.260057	80.883375	63.648321
1769.832706	82.537611	63.653326
1768.456612	83.729102	63.658330
1767.805839	74.374394	63.663335
1767.695941	76.437088	63.668340
1766.929829	81.382441	63.673345
1766.794387	84.209246	63.678350
1766.235081	93.010335	63.683354
1764.980744	77.073406	63.688359
1764.474123	94.373364	63.693364
1764.018335	91.873898	63.698369
1763.159938	80.571603	63.703374
1762.157048	90.433408	63.708378
1761.368627	80.717376	63.713383
1761.047481	78.218608	63.718388
1760.536390	77.434105	63.723393
1760.284134	81.881564	63.728398
1758.653692	95.446187	63.733402
1758.045058	75.797258	63.738407
1757.864690	98.198633	63.743412
1757.318239	88.196603	63.748417
1756.633609	82.333740	63.753422
1755.932008	81.043354	63.758426
1755.276310	82.349097	63.763431
1754.738000	79.306103	63.768436
1753.590688	82.957461	63.773441
1752.775420	70.459367	63.778446
1752.172911	83.236301	63.783450
1751.810628	75.313315	63.788455
1751.351180	71.579745	63.793460
1750.722243	87.096753	63.798465
1749.800063	84.253485	63.803470
1748.964981	81.910447	63.808474
1748.492841	85.605966	63.813479
1748.322416	76.791539	63.818484
1746.992072	78.007312	63.823489
1746.223545	76.833208	63.828494
1745.670181	77.994975	63.833498
1745.268797	72.754156	63.838503
1745.028917	79.013053	63.843508
1744.128820	74.480604	63.848513
1743.256105	70.133034	63.853518
1742.505037	78.603467	63.858522
1741.694145	90.041620	63.863527
1741.781924	65.608262	63.868532
1740.525809	93.117650	63.873537
1740.291027	72.387548	63.878542
1739.320572	80.610563	63.883546
1738.292639	77.683175	63.888551
1737.549878	77.335994	63.893556
1737.022787	81.026049	63.898561
1736.665682	85.215785	63.903566
1735.982899	82.925831	63.908570
1735.623854	84.461997	63.913575
1734.966650	78.243145	63.918580
1733.932829	94.234449	63.923585
1733.149846	87.089443	63.928590
1732.898230	84.423525	63.933594
1731.981498	68.529202	63.938599
1731.387664	87.569677	63.943604
1730.800810	74.898126	63.948609
1730.222776	62.545290	63.953614
1729.644437	86.099462	63.958618
1728.643092	82.166541	63.963623
1728.076982	71.658323	63.968628
1727.821809	93.048175	63.973633
1727.014558	81.066025	63.978638
1726.106648	83.572408	63.983642
1725.295353	74.624811	63.988647
1724.910960	70.463033	63.993652
1723.496482	100.632542	63.998657
1723.081869	78.849261	64.003662
1722.397442	66.092297	64.008666
1721.823073	76.217191	64.013671
1721.598391	77.538063	64.018676
1720.744981	86.431591	64.023681
1720.598743	83.922395	64.028686
1719.588807	81.913051	64.033690
1718.916612	75.518399	64.038695
1718.440206	79.611970	64.043700
1717.624475	86.156281	64.048705
1716.712890	83.754445	64.053710
1715.997260	85.993764	64.058714
1715.433530	83.768482	64.063719
1715.316698	77.124788	64.068724
1713.680929	88.353347	64.073729
1713.113847	80.030830	64.078734
1712.851389	85.763487	64.083738
1712.359452	81.714977	64.088743
1711.635430	79.294393	64.093748
1711.021902	77.944303	64.098753
1710.153746	86.895365	64.103758
1709.332279	73.605105	64.108762
1708.928856	80.315733	64.113767
1708.758585	88.127837	64.118772
1707.559974	84.279868	64.123777
1706.948285	72.709775	64.128782
1706.224515	91.086529	64.133786
1705.841533	86.732147	64.138791
1704.942829	75.497783	64.143796
1704.350061	80.658457	64.148801
1703.801553	78.443377	64.153806
1703.238191	73.870079	64.158810
1702.066717	75.601510	64.163815
1701.447871	82.994448	64.168820
1700.865364	89.414995	64.173825
1700.563597	63.359418	64.178830
1699.886182	94.851540	64.183834
1698.674759	68.880509	64.188839
1698.140847	74.421322	64.193844
1697.488617	79.583557	64.198849
1697.442108	73.333954	64.203854
1696.299856	76.241822	64.208858
1695.310706	91.489638	64.213863
1694.741048	66.670299	64.218868
1694.311640	82.975589	64.223873
1694.006949	82.508383	64.228878
1693.591580	84.384643	64.233882
1692.193633	86.867950	64.238887
1691.680523	90.144229	64.243892
1691.191456	84.966227	64.248897
1690.913275	87.855127	64.253902
1689.909901	83.686013	64.258906
1688.653992	83.601688	64.263911
1688.358100	72.929145	64.268916
1687.395944	84.034956	64.273921
1687.486917	84.556682	64.278926
1686.454895	80.940872	64.283930
1685.589226	82.000875	64.288935
1685.397754	74.736714	64.293940
1684.860449	77.414470	64.298945
1683.777760	74.142584	64.303950
1682.789283	66.126700	64.308954
1682.345174	83.628017	64.313959
1682.533820	79.116621	64.318964
1681.377326	74.571308	64.323969
1680.431458	79.717110	64.328974
1680.295060	81.009772	64.333978
1679.205450	77.089315	64.338983
1678.348332	77.692246	64.343988
1677.618633	87.247343	64.348993
1677.238290	73.420279	64.353998
1676.806085	79.747570	64.359002
1675.725332	82.336613	64.364007
1674.912904	79.278834	64.369012
1674.267273	88.276558	64.374017
1673.835201	74.527093	64.379022
1673.756893	80.422878	64.384026
1672.794785	78.554182	64.389031
1671.865755	78.164070	64.394036
1671.067993	77.778338	64.399041
1670.726151	92.033987	64.404046
1670.284138	72.853776	64.409050
1669.100650	75.180032	64.414055
1668.869782	77.921076	64.419060
1668.177687	85.888598	64.424065
1667.508955	82.079482	64.429070
1666.459294	73.094081	64.434074
1665.753215	76.785770	64.439079
1665.401754	85.126519	64.444084
1664.716397	87.881410	64.449089
1663.377392	67.993750	64.454094
1662.865298	90.397326	64.459098
1662.176637	68.346970	64.464103
1662.159506	84.104253	64.469108
1661.729644	85.708444	64.474113
1661.454193	69.631876	64.479118
1660.155130	70.686613	64.484122
1659.362428	85.106906	64.489127
1659.119547	84.322396	64.494132
1657.997802	75.895623	64.499137
1657.341258	63.015993	64.504142
1656.891765	89.414875	64.509146
1656.154640	69.371693	64.514151
1655.454966	71.515455	64.519156
1654.220216	72.156301	64.524161
1653.655769	74.500923	64.529166
1653.344988	65.372939	64.534170
1652.525876	68.287840	64.539175
1652.631824	65.349109	64.544180
1651.396597	82.906705	64.549185
1650.778502	85.146316	64.554190
1650.257327	77.256475	64.559194
1649.986059	76.627855	64.564199
1649.098188	70.032534	64.569204
1648.047473	83.982905	64.574209
1647.697787	79.135994	64.579214
1647.101891	83.806769	64.584218
1645.816455	81.814410	64.589223
1645.506116	74.528138	64.594228
1644.898844	85.265368	64.599233
1644.446518	78.108876	64.604238
1643.237093	70.350443	64.609242
1642.217314	82.234930	64.614247
1641.959848	73.767069	64.619252
1641.266302	81.646519	64.624257
1641.279891	80.064374	64.629262
1640.772324	67.766601	64.634266
1639.375827	75.683598	64.639271
1639.230063	76.936750	64.644276
1638.361854	77.935673	64.649281
1637.371017	67.146468	64.654286
1636.510113	78.843299	64.659290
1635.900064	70.855625	64.664295
1635.687712	71.721983	64.669300
1635.384626	74.608534	64.674305
1634.679537	74.550273	64.679310
1633.938823	65.096371	64.684314
1633.176709	84.344914	64.689319
1632.362175	73.045178	64.694324
1631.349474	81.779533	64.699329
1630.362279	77.975287	64.704334
1630.194202	67.690868	64.709338
1629.593002	74.920169	64.714343
1629.820801	71.249335	64.719348
1628.710718	82.788644	64.724353
1627.930571	75.968069	64.729358
1627.493327	75.867263	64.734362
1626.222778	68.367695	64.739367
1625.539189	66.248207	64.744372
1624.561463	72.390936	64.749377
1624.646288	69.118108	64.754382
1623.759035	71.771044	64.759386
1622.584067	72.344064	64.764391
1622.266790	70.057581	64.769396
1621.485190	77.298197	64.774401
1621.211239	69.014301	64.779406
1620.835392	75.327912	64.784410
1619.601373	74.077990	64.789415
1619.054299	69.571511	64.794420
1618.134359	71.479050	64.799425
1617.909389	72.244917	64.804430
1617.308430	63.655023	64.809434
1616.282036	72.177097	64.814439
1615.800343	75.486240	64.819444
1615.095586	75.074713	64.824449
1614.430600	73.430062	64.829454
1613.590755	73.932504	64.834458
1612.634547	83.630820	64.839463
1612.401388	71.965939	64.844468
1612.020932	66.039041	64.849473
1611.745509	72.440772	64.854478
1610.803549	64.297690	64.859482
1609.822221	78.536648	64.864487
1609.449195	73.788066	64.869492
1608.493178	75.163628	64.874497
1607.364279	73.222113	64.879502
1607.164674	80.310356	64.884506
1606.411966	75.584246	64.889511
1606.543661	60.918975	64.894516
1605.177347	78.287679	64.899521
1604.407525	80.871507	64.904526
1603.799274	63.540605	64.909530
1603.435909	72.753673	64.914535
1602.814338	63.807531	64.919540
1601.552012	74.007036	64.924545
1601.008053	71.720299	64.929550
1600.825258	70.746487	64.934554
1600.207343	76.157165	64.939559
1599.238166	72.719059	64.944564
1598.486892	72.097318	64.949569
1597.808216	74.542094	64.954574
1597.871028	72.917439	64.959578
1596.560646	78.969531	64.964583
1595.724737	73.670047	64.969588
1594.936115	75.621385	64.974593
1594.338777	63.560232	64.979598
1594.478618	74.427915	64.984602
1593.466552	86.960864	64.989607
1592.805475	67.746108	64.994612
1592.141155	88.237466	64.999617
1591.596084	82.721473	65.004622
1590.653409	62.824524	65.009626
1589.871981	82.492430	65.014631
1589.501249	77.454919	65.019636
1588.724949	62.653216	65.024641
1588.250101	93.004603	65.029646
1587.589753	71.481188	65.034650
1586.571240	70.875100	65.039655
1586.419642	87.260831	65.044660
1585.532114	70.819499	65.049665
1584.267081	74.174251	65.054670
1584.352995	89.092029	65.059674
1583.506048	72.056077	65.064679
1582.938147	80.686666	65.069684
1581.689940	80.322063	65.074689
1581.379267	65.064784	65.079694
1581.113067	71.867152	65.084698
1580.304779	70.201125	65.089703
1579.585126	56.604622	65.094708
1578.641752	66.461737	65.099713
1577.936912	67.701215	65.104718
1577.880599	67.055800	65.109722
1576.515195	69.802060	65.114727
1575.980961	72.182895	65.119732
1575.241412	81.935103	65.124737
1574.860339	73.370204	65.129742
1574.616594	81.570846	65.134746
1573.252658	80.276935	65.139751
1572.883711	67.633903	65.144756
1572.186329	70.660368	65.149761
1571.757856	74.924529	65.154766
1571.147128	64.669450	65.159770
1569.863166	70.195409	65.164775
1569.749148	70.036952	65.169780
1569.177825	80.210265	65.174785
1568.304306	62.585650	65.179790
1567.581448	62.635881	65.184794
1566.445737	80.830511	65.189799
1565.938449	55.485710	65.194804
1565.502103	81.023084	65.199809
1565.100879	82.537588	65.204814
1564.128380	66.491375	65.209818
1563.461843	73.152355	65.214823
1563.148142	70.620898	65.219828
1562.606714	79.010752	65.224833
1561.819342	78.730630	65.229838
1560.872493	62.979953	65.234842
1560.242004	77.771852	65.239847
1559.848057	71.388237	65.244852
1558.504909	86.012687	65.249857
1557.779490	76.357691	65.254862
1557.535850	75.127059	65.259866
1557.135718	75.021945	65.264871
1557.081227	70.386760	65.269876
1555.956522	69.549987	65.274881
1554.963222	70.835302	65.279886
1554.265147	75.667398	65.284890
1553.993529	65.916657	65.289895
1553.224231	78.067280	65.294900
1552.058880	68.691912	65.299905
1551.797464	68.328229	65.304910
1551.426542	66.837138	65.309914
1550.308047	77.154153	65.314919
1549.528949	73.135540	65.319924
1548.856440	76.531777	65.324929
1548.325218	78.234086	65.329934
1548.344448	66.231095	65.334938
1546.879833	73.804160	65.339943
1546.295554	71.457614	65.344948
1545.800586	66.058253	65.349953
1545.473000	76.552365	65.354958
1544.694802	61.276347	65.359962
1543.529953	72.980486	65.364967
1543.060352	60.831252	65.369972
1542.645251	72.912981	65.374977
1541.735059	76.334369	65.379982
1540.722609	68.910531	65.384986
1540.236097	69.979720	65.389991
1539.537414	70.254763	65.394996
1539.188327	73.607499	65.400001
1539.134931	64.221039	65.405006
1538.183245	62.864801	65.410010
1537.273084	65.663321	65.415015
1536.770904	71.241689	65.420020
1535.858159	64.929475	65.425025
1534.820628	70.113536	65.430030
1534.918176	69.216606	65.435034
1533.935274	69.254550	65.440039
1533.276368	70.780039	65.445044
1532.335480	71.752699	65.450049
1531.613682	72.340484	65.455054
1531.316320	67.513669	65.460058
1530.830256	79.750174	65.465063
1530.353033	71.143797	65.470068
1529.146377	77.453812	65.475073
1528.669595	73.775081	65.480078
1528.293670	74.370985	65.485082
1526.894734	76.501313	65.490087
1526.544797	66.909671	65.495092
1526.173623	71.489567	65.500097
1525.052327	74.558170	65.505102
1525.172907	67.313837	65.510106
1523.706720	77.635646	65.515111
1523.034581	71.966411	65.520116
1522.573461	77.495685	65.525121
1522.029311	77.208466	65.530126
1521.588674	69.091416	65.535130
1520.633162	75.577560	65.540135
1520.156417	73.128783	65.545140
1519.823765	70.899949	65.550145
1518.460514	71.862458	65.555150
1517.803892	65.071185	65.560154
1517.205693	73.444832	65.565159
1517.005471	76.070634	65.570164
1516.641082	67.927279	65.575169
1515.369662	70.106732	65.580174
1514.693209	66.068670	65.585178
1513.750665	74.705179	65.590183
1513.443311	60.243716	65.595188
1512.308142	62.136606	65.600193
1511.532308	75.844640	65.605198
1511.069300	67.529309	65.610202
1510.625841	74.916481	65.615207
1510.459065	74.061550	65.620212
1510.270839	72.185063	65.625217
1509.063083	74.215639	65.630222
1508.396095	65.816033	65.635226
1507.166100	74.252228	65.640231
1506.361043	70.201488	65.645236
1505.682180	71.121484	65.650241
1505.275608	77.274416	65.655246
1505.106705	74.686844	65.660250
1504.562668	82.400645	65.665255
1503.829503	67.527470	65.670260
1502.986203	63.717763	65.675265
1501.983631	73.414007	65.680270
1501.690153	64.040470	65.685274
1500.863995	66.557586	65.690279
1500.352467	75.944006	65.695284
1499.309733	65.820671	65.700289
1498.846890	69.112643	65.705294
1498.550289	64.481246	65.710298
1497.087543	66.908717	65.715303
1496.661659	66.355143	65.720308
1496.284422	77.137829	65.725313
1496.053538	61.088926	65.730318
1495.328612	66.079831	65.735322
1494.346424	65.458546	65.740327
1493.681292	74.218127	65.745332
1493.101590	62.169978	65.750337
1491.673536	71.709920	65.755342
1491.372739	56.078966	65.760346
1490.658035	82.862138	65.765351
1490.917418	75.070649	65.770356
1490.423643	70.647192	65.775361
1489.270158	73.263632	65.780366
1488.860834	69.381814	65.785370
1487.382025	82.644931	65.790375
1486.401472	69.700162	65.795380
1485.752094	76.990755	65.800385
1485.309949	70.092873	65.805390
1485.322803	66.500342	65.810394
1484.927517	66.813916	65.815399
1483.777857	76.118824	65.820404
1483.225066	68.669276	65.825409
1482.413557	62.812482	65.830414
1482.049105	74.763169	65.835418
1481.087354	78.697368	65.840423
1480.108072	69.480119	65.845428
1479.678708	69.313434	65.850433
1479.208874	73.364993	65.855438
1478.348865	54.133039	65.860442
1477.361816	72.231520	65.865447
1476.871124	81.209378	65.870452
1476.627492	78.319887	65.875457
1475.879840	80.657389	65.880462
1475.080107	70.055503	65.885466
1474.496542	68.945126	65.890471
1473.745442	59.765738	65.895476
1473.429547	55.279332	65.900481
1472.609968	82.837643	65.905486
1471.887743	79.576375	65.910490
1471.000941	70.598309	65.915495
1470.515504	66.063153	65.920500
1469.470915	70.262816	65.925505
1468.627624	64.272312	65.930510
1468.593413	63.099868	65.935514
1467.934761	59.122067	65.940519
1467.665225	70.680797	65.945524
1466.763778	70.280069	65.950529
1465.783229	62.516904	65.955534
1465.541208	65.904668	65.960538
1464.569499	68.962137	65.965543
1463.531239	65.501953	65.970548
1462.933734	77.518063	65.975553
1462.407297	61.916661	65.980558
1461.731857	87.143542	65.985562
1461.558997	63.325654	65.990567
1460.604940	60.159581	65.995572
1459.998812	75.952078	66.000577
1459.247792	74.218646	66.005582
1459.012395	63.864538	66.010586
1457.576012	60.486549	66.015591
1456.805343	83.579288	66.020596
1456.877405	61.639955	66.025601
1456.228678	78.702295	66.030606
1455.652314	73.006823	66.035610
1454.051475	68.152214	66.040615
1453.680775	66.099739	66.045620
1453.467220	72.310304	66.050625
1452.904185	72.499162	66.055630
1452.860584	66.942942	66.060634
1451.363097	74.951762	66.065639
1450.798057	71.987204	66.070644
1450.061753	58.581048	66.075649
1449.089517	71.910315	66.080654
1449.116717	62.711321	66.085658
1448.442872	74.446264	66.090663
1447.377287	68.513170	66.095668
1446.787169	56.409931	66.100673
1445.911888	68.072808	66.105678
1445.737050	55.971378	66.110682
1444.441131	57.158177	66.115687
1443.862476	81.068751	66.120692
1443.423168	63.871909	66.125697
1442.594844	67.089515	66.130702
1442.069445	53.137368	66.135706
1441.066353	73.587936	66.140711
1440.516864	71.324192	66.145716
1440.263656	69.390234	66.150721
1439.706051	70.120674	66.155726
1439.583141	73.047989	66.160730
1438.284249	62.071315	66.165735
1437.363088	72.595108	66.170740
1436.740715	69.095647	66.175745
1436.043164	69.684335	66.180750
1435.205489	60.457223	66.185754
1434.377980	74.302782	66.190759
1434.122975	70.765436	66.195764
1434.098049	64.225440	66.200769
1432.724177	56.490112	66.205774
1432.082865	66.829086	66.210778
1431.457842	79.790963	66.215783
1430.959117	73.881319	66.220788
1430.502053	58.212142	66.225793
1429.215594	72.580047	66.230798
1428.943982	66.298440	66.235802
1428.088406	69.369002	66.240807
1427.673968	66.063567	66.245812
1426.880032	66.956142	66.250817
1426.167548	64.806612	66.255822
1425.840998	64.219918	66.260826
1425.145176	77.161507	66.265831
1424.135683	67.786670	66.270836
1423.614360	53.348207	66.275841
1422.541377	74.424865	66.280846
1422.739055	73.698087	66.285850
1421.281522	68.811264	66.290855
1420.720395	72.511508	66.295860
1420.144696	62.930545	66.300865
1419.483410	60.810725	66.305870
1419.685604	63.784135	66.310874
1418.198909	77.693467	66.315879
1417.584630	57.719204	66.320884
1417.224473	61.554653	66.325889
1416.617405	71.607507	66.330894
1415.828871	53.242543	66.335898
1414.800592	78.019311	66.340903
1414.228754	66.348385	66.345908
1414.041311	55.419000	66.350913
1412.413790	71.865811	66.355918
1411.970540	57.694045	66.360922
1411.569544	69.456582	66.365927
1411.286018	59.567428	66.370932
1410.828626	62.486405	66.375937
1409.819208	71.767469	66.380942
1409.081664	67.396968	66.385946
1408.507886	68.006989	66.390951
1407.692979	66.099235	66.395956
1406.844971	69.066105	66.400961
1406.178858	66.292656	66.405966
1405.573902	58.329485	66.410970
1405.060302	61.452927	66.415975
1404.623941	77.201100	66.420980
1404.177648	76.363796	66.425985
1403.226034	70.713790	66.430990
1403.145776	63.034632	66.435994
1401.906400	69.717305	66.440999
1400.998119	62.327440	66.446004
1400.617645	73.438627	66.451009
1399.640265	85.155600	66.456014
1399.257388	58.971128	66.461018
1398.359317	64.054225	66.466023
1398.025537	62.735442	66.471028
1397.824220	49.909723	66.476033
1396.335802	67.403541	66.481038
1395.515034	73.245443	66.486042
1395.392373	62.206417	66.491047
1394.704633	66.852408	66.496052
1394.002156	60.336534	66.501057
1392.782488	75.119592	66.506062
1392.358767	69.292651	66.511066
1392.166945	63.182863	66.516071
1391.406855	70.166232	66.521076
1390.464087	75.437779	66.526081
1389.508252	69.503037	66.531086
1389.259895	57.880054	66.536090
1388.863454	63.458978	66.541095
1387.963985	81.305459	66.546100
1387.223919	72.248917	66.551105
1386.268696	56.737779	66.556110
1386.126849	74.162650	66.561114
1385.627469	71.356398	66.566119
1384.858893	70.161914	66.571124
1384.079784	69.427974	66.576129
1383.500363	77.503783	66.581134
1382.777839	60.512823	66.586138
1381.508202	63.701248	66.591143
1380.949673	59.986665	66.596148
1380.807267	72.682606	66.601153
1380.418356	66.268273	66.606158
1379.359852	57.842644	66.611162
1378.353715	79.862695	66.616167
1378.194187	70.128864	66.621172
1377.888547	46.095608	66.626177
1376.347121	71.040660	66.631182
1375.642658	73.257788	66.636186
1375.010561	60.726029	66.641191
1374.868884	54.961494	66.646196
1374.474317	53.420578	66.651201
1373.219773	69.207335	66.656206
1372.399820	62.855211	66.661210
1371.579395	68.391151	66.666215
1371.435356	67.450619	66.671220
1371.437076	62.729250	66.676225
1370.139306	75.831177	66.681230
1369.569952	63.160142	66.686234
1368.927512	60.140105	66.691239
1368.098114	70.617790	66.696244
1367.471910	64.094530	66.701249
1366.259314	75.954542	66.706254
1366.157127	69.906197	66.711258
1365.909651	67.556621	66.716263
1365.086103	61.135691	66.721268
1364.299038	62.702090	66.726273
1363.325305	71.138604	66.731278
1363.194907	69.388549	66.736282
1362.089505	60.282868	66.741287
1361.226404	62.974621	66.746292
1360.890244	64.778414	66.751297
1360.228044	81.835020	66.756302
1360.024806	55.883776	66.761306
1359.153786	87.337243	66.766311
1357.858886	47.894415	66.771316
1358.134898	59.188229	66.776321
1356.990016	74.615385	66.781326
1356.018827	55.088950	66.786330
1355.496069	64.923413	66.791335
1355.106284	69.864232	66.796340
1354.031808	58.646948	66.801345
1353.184073	67.277887	66.806350
1352.933284	70.602401	66.811354
1352.476592	66.549954	66.816359
1351.682479	69.601308	66.821364
1350.780173	59.241280	66.826369
1349.873256	57.737658	66.831374
1349.677985	59.424444	66.836378
1349.234425	68.976677	66.841383
1348.284242	58.010861	66.846388
1347.538624	66.371693	66.851393
1346.779444	71.724449	66.856398
1346.504050	49.720549	66.861402
1346.362969	84.643765	66.866407
1345.136688	64.189677	66.871412
1343.824441	78.514411	66.876417
1343.564554	53.486765	66.881422
1343.158932	53.948651	66.886426
1342.302446	67.879246	66.891431
1341.348627	59.395996	66.896436
1341.061264	77.244520	66.901441
1340.387745	60.129103	66.906446
1340.134987	49.110777	66.911450
1338.984140	80.000041	66.916455
1338.367390	59.352882	66.921460
1337.979960	81.878530	66.926465
1337.108571	55.812745	66.931470
1336.173371	81.175517	66.936474
1335.899740	75.133927	66.941479
1334.645430	73.109976	66.946484
1335.023901	44.417157	66.951489
1333.448710	82.794599	66.956494
1333.169492	61.046746	66.961498
1332.660289	64.732442	66.966503
1331.925511	83.456297	66.971508
1330.950425	45.304575	66.976513
1330.073432	91.657203	66.981518
1329.610447	51.993838	66.986522
1329.450891	72.151065	66.991527
1328.622559	64.010548	66.996532
1327.673430	52.904237	67.001537
1326.916818	84.289051	67.006542
1326.940740	37.250589	67.011546
1326.241430	71.098784	67.016551
1325.156585	52.374140	67.021556
1324.461348	70.765283	67.026561
1324.038115	71.337199	67.031566
1323.117379	79.255976	67.036570
1322.411612	53.479249	67.041575
1321.493919	68.584881	67.046580
1321.393491	67.982753	67.051585
1320.738238	66.117454	67.056590
1320.139161	49.195217	67.061594
1319.186829	66.589650	67.066599
1318.463531	71.745909	67.071604
1318.259719	53.584491	67.076609
1316.837846	66.389208	67.081614
1316.503472	58.209596	67.086618
1315.933531	64.125174	67.091623
1315.187362	68.003077	67.096628
1315.149226	41.839559	67.101633
1313.905513	78.598474	67.106638
1313.765282	53.383093	67.111642
1312.870560	51.126960	67.116647
1312.002951	74.131028	67.121652
1311.404299	62.204222	67.126657
1310.700568	62.571587	67.131662
1310.201184	63.903044	67.136666
1308.957629	42.217075	67.141671
1308.053829	70.501494	67.146676
1307.590761	71.374619	67.151681
1307.308437	62.473990	67.156686
1307.014030	60.723207	67.161690
1306.597658	52.220764	67.166695
1305.590682	70.103258	67.171700
1305.160853	72.697766	67.176705
1303.939130	78.751660	67.181710
1303.156426	73.615708	67.186714
1302.574404	58.247123	67.191719
1301.889906	76.031052	67.196724
1301.660308	72.183773	67.201729
1301.030035	74.143134	67.206734
1300.152955	63.876881	67.211738
1299.457131	58.548939	67.216743
1298.676407	75.867222	67.221748
1298.301940	72.095011	67.226753
1297.038396	67.842862	67.231758
1296.531535	67.562379	67.236762
1296.185565	67.111246	67.241767
1295.629462	63.962392	67.246772
1295.274219	63.927449	67.251777
1294.395310	69.505821	67.256782
1293.786192	63.635844	67.261786
1292.795915	53.876425	67.266791
1291.544853	85.953248	67.271796
1291.427938	47.143177	67.276801
1290.798191	86.185565	67.281806
1290.141087	61.310958	67.286810
1289.825928	52.010304	67.291815
1288.352851	85.193112	67.296820
1288.296146	49.372663	67.301825
1287.382044	70.531306	67.306830
1287.125469	67.308027	67.311834
1286.403933	57.650955	67.316839
1285.444894	70.060425	67.321844
1285.281849	55.287522	67.326849
1284.330343	62.492143	67.331854
1283.374439	71.413096	67.336858
1282.673874	67.818883	67.341863
1282.025810	65.875184	67.346868
1281.744866	56.204835	67.351873
1281.229569	66.930625	67.356878
1280.242659	67.700968	67.361882
1279.646332	70.435484	67.366887
1278.857642	70.240810	67.371892
1278.569588	70.732898	67.376897
1277.269430	71.409550	67.381902
1276.687965	75.196627	67.386906
1276.342167	64.024372	67.391911
1276.024094	64.764069	67.396916
1275.261339	62.490121	67.401921
1274.315635	68.446526	67.406926
1273.494568	64.674368	67.411930
1273.243702	62.136119	67.416935
1271.894341	72.365352	67.421940
1271.534086	64.524157	67.426945
1270.765277	65.262981	67.431950
1270.461195	65.276675	67.436954
1270.538205	64.851331	67.441959
1269.236208	64.709887	67.446964
1268.940407	67.674153	67.451969
1267.750589	67.391879	67.456974
1266.441278	54.824343	67.461978
1265.970298	58.600159	67.466983
1265.488891	66.404943	67.471988
1265.501262	71.575128	67.476993
1264.993401	74.224623	67.481998
1263.756526	62.870789	67.487002
1263.094048	60.593517	67.492007
1262.429639	81.075426	67.497012
1262.553638	65.840588	67.502017
1261.117864	64.627651	67.507022
1260.323586	59.425755	67.512026
1259.957767	75.553772	67.517031
1258.578065	63.784280	67.522036
1258.138446	64.082861	67.527041
1257.331076	72.548144	67.532046
1256.895087	69.831185	67.537050
1256.689415	66.407439	67.542055
1256.216508	79.349878	67.547060
1255.506737	58.930426	67.552065
1254.555512	73.456390	67.557070
1254.203890	69.953354	67.562074
1253.349445	69.843255	67.567079
1252.531452	74.615639	67.572084
1251.705944	65.996914	67.577089
1251.271771	67.991335	67.582094
1249.977433	65.816106	67.587098
1249.712850	72.973021	67.592103
1248.824744	79.910551	67.597108
1248.465024	77.547298	67.602113
1248.224138	71.730740	67.607118
1247.584638	75.645315	67.612122
1246.737212	52.568672	67.617127
1245.901560	77.341639	67.622132
1245.734024	65.111355	67.627137
1244.719090	59.157694	67.632142
1243.674070	65.960905	67.637146
1243.036436	67.080981	67.642151
1242.489353	66.081548	67.647156
1242.362880	54.841321	67.652161
1241.351191	60.119136	67.657166
1240.560139	69.411257	67.662170
1240.289455	62.913507	67.667175
1239.178751	62.718010	67.672180
1238.657248	52.724820	67.677185
1237.908933	57.386781	67.682190
1237.284691	69.235278	67.687194
1237.282145	56.729624	67.692199
1235.892089	69.669660	67.697204
1235.433231	68.247792	67.702209
1234.867645	73.024198	67.707214
1234.058318	63.593979	67.712218
1232.930567	65.760181	67.717223
1232.067687	79.248725	67.722228
1231.812573	58.477888	67.727233
1231.523366	57.768595	67.732238
1230.847669	64.601390	67.737242
1230.610565	69.828585	67.742247
1229.715980	69.422119	67.747252
1229.102574	51.898258	67.752257
1227.734888	69.478596	67.757262
1226.901115	64.935812	67.762266
1226.272009	63.164147	67.767271
1225.735152	72.792723	67.772276
1225.707315	61.435892	67.777281
1225.493019	67.433699	67.782286
1224.726329	67.208737	67.787290
1223.916781	63.160391	67.792295
1222.694518	69.260130	67.797300
1221.936133	66.387872	67.802305
1221.467705	65.907339	67.807310
1220.586626	73.004596	67.812314
1220.736814	57.686764	67.817319
1219.462163	65.146203	67.822324
1218.680136	53.518240	67.827329
1218.337596	72.946076	67.832334
1217.788103	61.498738	67.837338
1216.911720	53.463680	67.842343
1215.830843	60.398749	67.847348
1215.165571	78.189090	67.852353
1214.743259	63.006439	67.857358
1214.218425	56.962247	67.862362
1213.955497	68.527803	67.867367
1213.023673	77.008157	67.872372
1212.141626	65.829729	67.877377
1211.989369	69.542260	67.882382
1210.974163	78.625622	67.887386
1210.256101	72.367736	67.892391
1209.502773	65.035311	67.897396
1209.014431	62.580562	67.902401
1208.011724	70.723699	67.907406
1207.380160	67.851779	67.912410
1207.102932	54.643954	67.917415
1206.201497	64.847711	67.922420
1205.876760	67.876504	67.927425
1205.193576	62.084560	67.932430
1204.119536	62.515570	67.937434
1203.943666	61.755143	67.942439
1202.885090	67.264344	67.947444
1202.149614	62.057849	67.952449
1201.563592	60.839125	67.957454
1201.339994	58.066329	67.962458
1200.557255	58.205028	67.967463
1199.784379	61.369733	67.972468
1198.725659	67.765155	67.977473
1198.228437	60.240632	67.982478
1197.830810	65.960104	67.987482
1197.162261	67.167103	67.992487
1196.027758	62.058754	67.997492
1195.568482	67.046904	68.002497
1195.149898	59.934053	68.007502
1194.778147	69.200505	68.012506
1193.766611	63.623195	68.017511
1192.807932	58.493197	68.022516
1192.125200	69.458497	68.027521
1191.927479	47.322462	68.032526
1191.230286	72.771955	68.037530
1190.446805	62.353682	68.042535
1189.545193	74.227374	68.047540
1189.148057	67.473789	68.052545
1188.663506	60.623728	68.057550
1187.516709	64.956432	68.062554
1187.278978	72.484370	68.067559
1186.748825	78.996009	68.072564
1186.317705	60.571163	68.077569
1185.380205	59.971276	68.082574
1184.304894	63.180926	68.087578
1184.586534	48.067695	68.092583
1182.950348	73.035766	68.097588
1182.071941	66.546363	68.102593
1181.748347	64.213646	68.107598
1181.545016	73.517968	68.112602
1180.669373	61.616337	68.117607
1179.818280	58.974868	68.122612
1179.245308	54.849497	68.127617
1178.645754	60.036564	68.132622
1177.799563	72.902751	68.137626
1177.263526	69.184642	68.142631
1176.246868	62.275707	68.147636
1176.050613	67.682477	68.152641
1175.866442	62.211710	68.157646
1174.513726	77.724007	68.162650
1174.020183	59.184522	68.167655
1173.023852	64.245466	68.172660
1172.827810	64.382331	68.177665
1171.723978	69.461950	68.182670
1170.547949	73.711007	68.187674
1170.444787	59.460006	68.192679
1169.665391	67.805747	68.197684
1169.550968	62.566725	68.202689
1169.096925	60.997457	68.207694
1167.950691	65.963978	68.212698
1167.466256	67.721991	68.217703
1166.582145	71.263921	68.222708
1166.352518	70.901531	68.227713
1165.134583	64.403057	68.232718
1164.228649	75.025415	68.237722
1164.284018	65.809350	68.242727
1163.697897	61.887911	68.247732
1162.522720	72.382785	68.252737
1161.872836	63.526447	68.257742
1161.415785	66.554210	68.262746
1161.413342	60.713942	68.267751
1160.062537	56.204528	68.272756
1159.219577	77.970013	68.277761
1158.757699	66.030969	68.282766
1158.174364	60.402925	68.287770
1157.463037	66.031949	68.292775
1156.141711	61.500501	68.297780
1155.907804	78.176786	68.302785
1155.706633	66.926368	68.307790
1155.220380	51.069561	68.312794
1153.964961	72.411806	68.317799
1153.351121	70.926298	68.322804
1152.805964	50.832370	68.327809
1152.434707	70.045580	68.332814
1151.831110	71.627016	68.337818
1150.888952	51.197280	68.342823
1150.047518	62.064826	68.347828
1149.388925	72.069141	68.352833
1148.592905	69.248621	68.357838
1147.915389	76.974231	68.362842
1147.641405	57.800633	68.367847
1147.001419	64.395966	68.372852
1146.160732	55.592059	68.377857
1145.534026	63.128242	68.382862
1144.701540	76.586736	68.387866
1144.406858	69.589798	68.392871
1144.123801	65.412019	68.397876
1142.826263	64.041556	68.402881
1142.313635	52.924259	68.407886
1141.627175	67.438094	68.412890
1140.856224	63.233838	68.417895
1139.857215	67.140958	68.422900
1139.572770	60.128205	68.427905
1139.316767	60.791818	68.432910
1138.464570	58.355532	68.437914
1137.596623	53.168553	68.442919
1136.673711	72.450579	68.447924
1136.474210	63.047985	68.452929
1136.040571	65.401862	68.457934
1134.786706	67.935073	68.462938
1134.425167	59.494908	68.467943
1134.034886	67.982185	68.472948
1132.929995	65.851001	68.477953
1132.199418	57.505800	68.482958
1131.129139	69.199758	68.487962
1131.312234	60.841697	68.492967
1130.754277	65.228997	68.497972
1129.339122	66.431762	68.502977
1128.479752	62.575867	68.507982
1128.067378	71.131312	68.512986
1128.149707	60.050269	68.517991
1127.332201	65.208937	68.522996
1126.611730	63.885466	68.528001
1125.960549	60.349678	68.533006
1124.928592	70.389725	68.538010
1124.246796	72.393589	68.543015
1123.404142	56.877306	68.548020
1122.872953	80.805546	68.553025
1122.394322	65.343315	68.558030
1121.611517	60.071840	68.563034
1121.584322	54.593462	68.568039
1120.471617	70.025022	68.573044
1119.699380	69.187575	68.578049
1119.476940	64.246419	68.583054
1118.441358	60.659815	68.588058
1117.647814	56.217903	68.593063
1116.994834	70.330626	68.598068
1116.719314	57.915710	68.603073
1115.846428	49.277782	68.608078
1114.758587	61.772422	68.613082
1114.298486	46.753519	68.618087
1114.036278	75.461003	68.623092
1113.359341	68.327761	68.628097
1112.617647	64.606111	68.633102
1111.725030	65.475054	68.638106
1111.485340	57.595801	68.643111
1111.045928	60.149283	68.648116
1109.840856	54.714755	68.653121
1108.996700	53.991247	68.658126
1108.402266	74.786856	68.663130
1108.323301	57.376721	68.668135
1107.023985	61.069857	68.673140
1106.253412	67.110415	68.678145
1106.202539	46.756557	68.683150
1105.417198	59.086397	68.688154
1104.062237	53.664676	68.693159
1103.433493	66.434788	68.698164
1103.121977	49.798046	68.703169
1102.835568	53.304844	68.708174
1102.398999	65.829937	68.713178
1101.752200	65.114462	68.718183
1100.860330	70.529379	68.723188
1099.949150	73.025446	68.728193
1099.145002	61.911951	68.733198
1098.242048	68.672116	68.738202
1098.123930	51.794889	68.743207
1097.294156	64.051382	68.748212
1096.808517	62.439848	68.753217
1095.899874	64.845630	68.758222
1094.815191	59.795636	68.763226
1094.925157	68.088237	68.768231
1094.354832	67.300679	68.773236
1093.273698	64.317383	68.778241
1092.859524	63.380417	68.783246
1092.111280	57.373371	68.788250
1091.500458	59.780665	68.793255
1090.996688	71.436564	68.798260
1090.021674	59.962344	68.803265
1089.854764	49.561162	68.808270
1088.230711	59.077263	68.813274
1087.520633	52.220530	68.818279
1087.015366	63.690592	68.823284
1086.266811	66.867228	68.828289
1086.106334	49.820136	68.833294
1085.744453	56.330242	68.838298
1085.352895	55.200457	68.843303
1084.256708	68.325606	68.848308
1083.729415	64.913618	68.853313
1083.258145	60.169735	68.858318
1081.857563	73.455264	68.863322
1081.371700	58.650180	68.868327
1080.667229	59.443477	68.873332
1080.157931	71.488164	68.878337
1078.989374	66.839424	68.883342
1078.386993	72.638784	68.888346
1077.965659	57.862859	68.893351
1077.638183	63.024012	68.898356
1077.389392	70.881697	68.903361
1076.517152	71.548727	68.908366
1075.471115	67.586933	68.913370
1075.001970	65.237963	68.918375
1074.382025	64.876171	68.923380
1073.247443	57.095120	68.928385
1072.902294	58.107213	68.933390
1071.999476	66.160388	68.938394
1071.859871	60.837079	68.943399
1071.063120	64.759355	68.948404
1070.356655	63.083611	68.953409
1069.578330	68.185602	68.958414
1069.297320	67.331530	68.963418
1068.321696	58.254247	68.968423
1067.658146	68.312974	68.973428
1066.835265	66.069156	68.978433
1066.210363	62.754696	68.983438
1065.072955	66.784776	68.988442
1064.715472	72.283424	68.993447
1064.112292	71.961542	68.998452
1063.569779	66.355413	69.003457
1063.366612	63.910523	69.008462
1062.474969	69.978235	69.013466
1061.679690	67.420964	69.018471
1061.343833	69.869678	69.023476
1060.557283	69.565928	69.028481
1059.395951	61.650374	69.033486
1058.677097	64.606263	69.038490
1058.480066	65.869171	69.043495
1058.045316	70.279462	69.048500
1056.835650	73.133665	69.053505
1056.054502	67.158669	69.058510
1055.478940	73.931420	69.063514
1055.393708	64.214214	69.068519
1054.852423	65.464079	69.073524
1053.534900	72.140404	69.078529
1053.170264	66.247377	69.083534
1052.557771	72.688556	69.088538
1051.689122	73.104302	69.093543
1050.792552	66.952137	69.098548
1050.372887	69.578178	69.103553
1050.163513	68.525066	69.108558
1049.050846	80.438676	69.113562
1048.347464	65.601970	69.118567
1047.745110	65.374572	69.123572
1047.097380	65.225352	69.128577
1047.036230	55.532705	69.133582
1045.836073	62.070518	69.138586
1045.365685	66.089110	69.143591
1044.825330	65.990614	69.148596
1043.733103	66.798300	69.153601
1043.173260	57.255942	69.158606
1042.468101	66.195413	69.163610
1041.822522	58.492697	69.168615
1040.661731	57.423791	69.173620
1039.449697	69.047291	69.178625
1039.861553	62.847828	69.183630
1039.323673	70.786193	69.188634
1038.804790	69.742897	69.193639
1038.376418	59.632455	69.198644
1037.303602	78.747550	69.203649
1036.899242	57.010255	69.208654
1036.106852	68.861871	69.213658
1035.065670	59.869144	69.218663
1034.198916	62.531619	69.223668
1033.728528	70.323637	69.228673
1033.797152	65.082316	69.233678
1032.795885	72.353275	69.238682
1031.637960	69.533601	69.243687
1031.059147	67.776063	69.248692
1030.600986	68.194320	69.253697
1030.500260	53.518789	69.258702
1029.125973	61.183380	69.263706
1028.604391	67.999582	69.268711
1028.183252	71.726508	69.273716
1027.292210	63.000041	69.278721
1026.144911	65.803337	69.283726
1025.566720	65.613099	69.288730
1025.471645	57.229913	69.293735
1025.300409	72.067053	69.298740
1024.228391	69.709928	69.303745
1023.419834	56.678133	69.308750
1022.714559	62.851815	69.313754
1022.245975	65.495102	69.318759
1021.195136	70.058599	69.323764
1020.214945	72.754894	69.328769
1019.957449	63.028831	69.333774
1019.343960	75.531621	69.338778
1019.344461	73.901106	69.343783
1018.163648	60.155871	69.348788
1017.230079	64.003740	69.353793
1017.039224	63.423897	69.358798
1015.253954	82.830531	69.363802
1014.579250	72.440749	69.368807
1015.100019	64.413722	69.373812
1014.329471	71.198576	69.378817
1014.175679	73.233578	69.383822
1012.456707	68.328681	69.388826
1011.752066	76.720911	69.393831
1011.082289	72.500602	69.398836
1010.748866	67.118251	69.403841
1010.663555	60.040729	69.408846
1009.510412	66.342434	69.413850
1008.744009	70.603656	69.418855
1008.469999	77.271675	69.423860
1007.514944	79.752678	69.428865
1006.691923	62.189714	69.433870
1005.775843	65.635859	69.438874
1005.008033	69.586665	69.443879
1005.082643	63.913910	69.448884
1004.257154	69.906463	69.453889
1003.868678	63.842209	69.458894
1003.171489	66.577059	69.463898
1002.565220	64.543215	69.468903
1001.649548	56.897676	69.473908
1000.432115	74.130937	69.478913
1000.506348	54.181366	69.483918
999.864140	67.652180	69.488922
998.751516	58.467424	69.493927
998.022714	68.318936	69.498932
997.382870	66.473351	69.503937
997.396511	57.304942	69.508942
996.508074	61.019488	69.513946
995.631495	57.290956	69.518951
994.844051	63.862470	69.523956
994.258577	62.538060	69.528961
993.918050	53.139014	69.533966
992.773657	59.384140	69.538970
992.302994	59.766548	69.543975
991.753485	60.248227	69.548980
990.993925	63.570132	69.553985
990.190968	55.342151	69.558990
989.434498	59.560796	69.563994
989.059629	64.486660	69.568999
988.330957	59.375346	69.574004
987.646934	61.453708	69.579009
986.989043	67.853236	69.584014
986.097348	65.475324	69.589018
985.827222	64.471306	69.594023
985.617978	62.752746	69.599028
984.361976	71.846098	69.604033
983.926061	62.295078	69.609038
983.118419	69.268756	69.614042
982.495332	65.640235	69.619047
981.585044	60.556241	69.624052
980.691646	69.468908	69.629057
980.509417	71.358633	69.634062
980.156534	68.981723	69.639066
979.202268	59.435911	69.644071
978.442961	64.334637	69.649076
977.744296	67.646859	69.654081
977.251802	65.317392	69.659086
975.862930	65.587290	69.664090
975.395492	70.445888	69.669095
975.063411	66.257013	69.674100
974.533560	71.070353	69.679105
974.381079	51.398122	69.684110
972.983267	65.257223	69.689114
972.419420	67.792680	69.694119
972.056993	60.120626	69.699124
971.044614	61.412347	69.704129
970.287700	44.203160	69.709134
969.280719	71.966304	69.714138
968.807299	64.898499	69.719143
968.982943	58.236751	69.724148
968.043665	68.768268	69.729153
967.586277	59.677959	69.734158
966.576945	68.771491	69.739162
965.970158	61.586144	69.744167
965.059743	58.716086	69.749172
964.018161	60.431901	69.754177
963.704700	60.224787	69.759182
963.267901	63.864330	69.764186
962.932940	51.097815	69.769191
962.633754	49.672674	69.774196
961.456242	65.685405	69.779201
961.022940	59.708714	69.784206
959.465560	58.934745	69.789210
958.907864	58.418006	69.794215
958.560892	59.539208	69.799220
957.897094	61.497672	69.804225
957.589861	52.493859	69.809230
956.746388	65.763325	69.814234
956.072767	54.794699	69.819239
955.442885	72.161551	69.824244
954.830252	69.579985	69.829249
954.067572	66.192867	69.834254
953.190718	55.256579	69.839258
952.686849	46.181563	69.844263
952.383402	64.231280	69.849268
951.045154	44.446558	69.854273
950.722021	45.956603	69.859278
950.007929	59.255938	69.864282
949.648562	66.205601	69.869287
948.481205	50.923994	69.874292
947.772505	56.689828	69.879297
947.481167	66.917991	69.884302
946.788481	63.883993	69.889306
945.981094	63.383334	69.894311
945.080439	56.440286	69.899316
944.549858	78.610220	69.904321
944.143695	47.052589	69.909326
944.138716	71.037414	69.914330
942.782497	69.332638	69.919335
942.344160	63.038226	69.924340
941.411215	70.432374	69.929345
940.685783	59.563453	69.934350
939.666233	60.946208	69.939354
939.083899	62.024443	69.944359
938.772082	55.705173	69.949364
938.320153	49.622653	69.954369
937.871032	59.689848	69.959374
936.735177	65.455852	69.964378
936.014942	59.734546	69.969383
936.117443	58.734316	69.974388
934.763354	66.905063	69.979393
934.134350	65.776817	69.984398
933.747007	58.302690	69.989402
933.004351	61.847411	69.994407
931.854187	60.299077	69.999412
930.770228	64.785879	70.004417
930.416143	58.864396	70.009422
930.013029	72.210449	70.014426
929.628478	58.050002	70.019431
929.590448	59.781173	70.024436
928.366633	82.086652	70.029441
928.175797	63.120647	70.034446
927.203064	61.709651	70.039450
926.145302	62.415714	70.044455
925.416400	55.073207	70.049460
924.859933	60.324421	70.054465
924.392000	60.633871	70.059470
923.321109	61.483941	70.064474
922.544296	56.905404	70.069479
922.352960	53.545648	70.074484
921.745369	57.152452	70.079489
921.528958	57.787710	70.084494
920.260527	55.078713	70.089498
919.290355	67.182552	70.094503
919.228567	49.899038	70.099508
918.328803	59.183288	70.104513
917.565479	57.699553	70.109518
916.961726	64.175627	70.114522
916.591649	62.758617	70.119527
916.070103	50.387639	70.124532
914.808183	65.087678	70.129537
914.344090	55.922765	70.134542
913.763630	77.197095	70.139546
913.146373	70.163228	70.144551
912.095055	70.541862	70.149556
911.494448	65.489036	70.154561
911.534041	63.349286	70.159566
910.779503	56.647914	70.164570
909.985505	70.798867	70.169575
909.077340	57.052890	70.174580
908.472373	62.953607	70.179585
907.903711	67.006779	70.184590
906.706822	64.259596	70.189594
906.363149	70.471951	70.194599
906.041292	60.937494	70.199604
905.442233	72.741026	70.204609
904.461671	53.771409	70.209614
903.506095	60.617266	70.214618
902.941916	63.471314	70.219623
902.768155	61.340287	70.224628
901.351644	69.407450	70.229633
900.879681	59.258254	70.234638
900.165500	64.430500	70.239642
899.850294	65.855717	70.244647
899.868502	64.591373	70.249652
898.399491	70.667438	70.254657
898.084326	60.293030	70.259662
897.291471	63.554031	70.264666
896.529263	67.357325	70.269671
895.709875	65.095666	70.274676
895.018484	71.625115	70.279681
894.941292	64.104792	70.284686
894.365856	66.146975	70.289690
893.289401	67.131976	70.294695
892.987967	54.513098	70.299700
891.995586	68.421249	70.304705
890.897895	58.347981	70.309710
890.335602	72.020546	70.314714
889.717578	68.165755	70.319719
889.433128	57.636661	70.324724
888.571411	71.371067	70.329729
887.660360	70.251450	70.334734
886.818648	69.761003	70.339738
886.446404	66.188779	70.344743
886.059533	55.735908	70.349748
885.490028	79.747496	70.354753
884.997840	56.450535	70.359758
884.253489	68.526331	70.364762
883.467888	69.569122	70.369767
882.877786	56.825883	70.374772
881.372163	67.978951	70.379777
880.816183	70.908966	70.384782
880.637238	72.966897	70.389786
880.372067	63.536957	70.394791
879.649251	65.888009	70.399796
878.292517	81.386864	70.404801
878.184306	69.588730	70.409806
877.572487	73.101608	70.414810
876.895445	62.354312	70.419815
875.703243	72.694309	70.424820
875.342875	50.557449	70.429825
874.810930	76.431627	70.434830
874.471752	64.212967	70.439834
873.167687	71.051223	70.444839
872.726033	60.239663	70.449844
872.216004	66.516338	70.454849
871.551619	53.936306	70.459854
870.371905	70.141795	70.464858
869.981784	60.976156	70.469863
869.725655	54.562887	70.474868
868.970755	66.064811	70.479873
868.222617	57.440247	70.484878
867.805629	62.421708	70.489882
867.020763	71.145254	70.494887
866.598638	59.816532	70.499892
865.339930	52.421180	70.504897
865.091444	57.303287	70.509902
864.114788	62.520466	70.514906
863.038446	65.552220	70.519911
862.430538	68.802720	70.524916
861.558200	61.812624	70.529921
861.226722	81.848924	70.534926
860.835419	66.481692	70.539930
860.638783	57.075543	70.544935
860.103589	58.299248	70.549940
859.067464	71.498479	70.554945
858.393454	71.746127	70.559950
857.529472	76.232641	70.564954
856.368022	64.949048	70.569959
856.126338	63.874291	70.574964
855.515585	62.831465	70.579969
855.164533	58.175730	70.584974
854.397608	77.514975	70.589978
853.571830	57.519445	70.594983
852.908416	76.353389	70.599988
852.661732	67.417220	70.604993
851.267724	72.453263	70.609998
851.139696	76.505701	70.615002
850.264291	53.268175	70.620007
850.050843	66.268666	70.625012
848.742046	75.689002	70.630017
848.121640	56.576945	70.635022
847.916462	49.021814	70.640026
847.001158	71.440610	70.645031
846.563014	56.060350	70.650036
845.293002	61.131847	70.655041
845.018230	60.179045	70.660046
844.676638	65.325117	70.665050
843.977990	70.267837	70.670055
843.037135	61.628224	70.675060
842.483870	68.714405	70.680065
841.897835	47.611630	70.685070
840.999527	58.549787	70.690074
839.773764	86.235834	70.695079
839.418929	52.159718	70.700084
838.927490	71.850901	70.705089
838.845180	59.780594	70.710094
837.849533	42.782925	70.715098
836.527137	74.838023	70.720103
836.296941	55.793168	70.725108
835.735184	64.667276	70.730113
835.453984	68.540676	70.735118
834.149810	63.136258	70.740122
833.596717	57.661183	70.745127
833.214749	68.428864	70.750132
832.913537	63.093458	70.755137
831.947581	67.894234	70.760142
831.348341	53.279167	70.765146
830.806863	74.700243	70.770151
829.936893	51.460290	70.775156
828.390451	64.806974	70.780161
828.360904	45.697086	70.785166
827.816400	82.839893	70.790170
827.284760	54.782401	70.795175
827.068307	54.474713	70.800180
826.109370	84.530877	70.805185
825.623001	58.312674	70.810190
824.246864	59.545662	70.815194
823.427938	64.043934	70.820199
823.197505	55.277069	70.825204
822.733263	75.851697	70.830209
822.343680	52.491134	70.835214
820.935796	54.932317	70.840218
820.199791	77.127056	70.845223
819.997551	66.420894	70.850228
819.613842	62.587174	70.855233
818.640360	60.403683	70.860238
817.716015	66.549204	70.865242
816.856963	42.955896	70.870247
816.715616	73.414880	70.875252
816.404806	49.324317	70.880257
815.331270	81.413934	70.885262
814.463266	52.877014	70.890266
813.986105	68.363604	70.895271
813.805084	55.168949	70.900276
812.314258	70.999801	70.905281
811.738610	70.186350	70.910286
811.527887	57.527823	70.915290
810.602558	66.473996	70.920295
809.739807	67.084416	70.925300
809.049421	64.721834	70.930305
808.699331	56.939052	70.935310
808.257452	63.468222	70.940314
807.795377	63.540232	70.945319
807.010774	56.947756	70.950324
805.750216	68.637405	70.955329
805.405672	68.523562	70.960334
804.840738	60.167887	70.965338
803.591802	65.396889	70.970343
803.268516	60.257379	70.975348
802.802391	57.844913	70.980353
802.392934	69.629312	70.985358
801.214042	71.288206	70.990362
800.336814	71.691211	70.995367
800.277182	57.416012	71.000372
799.887752	64.805681	71.005377
799.360355	66.313568	71.010382
798.312944	63.960514	71.015386
797.181714	57.688127	71.020391
796.464840	62.204852	71.025396
795.549259	70.122948	71.030401
794.970918	63.617483	71.035406
794.701987	67.555161	71.040410
794.253019	78.718268	71.045415
793.991623	71.241465	71.050420
793.203466	59.039108	71.055425
791.974289	67.841277	71.060430
791.912187	64.724297	71.065434
791.093437	64.310648	71.070439
790.032517	59.055182	71.075444
789.492187	57.983819	71.080449
789.149121	63.103322	71.085454
788.514607	57.762637	71.090458
787.312749	67.229045	71.095463
786.679905	59.371434	71.100468
786.546998	69.672145	71.105473
785.646882	59.200078	71.110478
784.599865	53.940827	71.115482
783.859318	63.551408	71.120487
783.757169	58.129136	71.125492
783.185136	70.549658	71.130497
782.323546	62.255402	71.135502
781.484506	49.444608	71.140506
780.853820	56.883716	71.145511
780.519275	56.536487	71.150516
779.816416	58.477559	71.155521
778.967733	75.122364	71.160526
778.815514	64.058187	71.165530
777.671679	61.077135	71.170535
776.652410	57.095452	71.175540
775.898863	82.762073	71.180545
775.610175	59.882167	71.185550
775.458866	52.386277	71.190554
774.588883	60.590409	71.195559
773.937956	51.816379	71.200564
773.129250	54.873368	71.205569
771.994744	77.349152	71.210574
771.507697	57.403819	71.215578
770.642758	58.001985	71.220583
770.508244	57.176666	71.225588
770.072132	67.503564	71.230593
769.360979	70.980240	71.235598
768.423293	66.974533	71.240602
767.605471	72.778282	71.245607
767.259888	58.332579	71.250612
766.260893	64.502613	71.255617
765.603265	68.413865	71.260622
765.160653	58.975931	71.265626
764.459189	58.923641	71.270631
763.828095	64.631436	71.275636
762.822690	64.498229	71.280641
761.875237	70.421957	71.285646
761.781640	64.416464	71.290650
760.983594	73.659340	71.295655
760.921538	58.148279	71.300660
759.420011	66.370958	71.305665
759.030213	73.260830	71.310670
758.886226	62.108622	71.315674
757.974784	64.139671	71.320679
757.100632	56.601166	71.325684
756.568914	57.499506	71.330689
755.862163	74.169024	71.335694
755.917871	54.339137	71.340698
754.312784	63.972241	71.345703
754.103591	83.711541	71.350708
753.252910	64.111082	71.355713
752.240395	68.696960	71.360718
751.599931	55.348392	71.365722
750.909970	76.252246	71.370727
750.667323	66.427685	71.375732
750.315337	67.923425	71.380737
749.171858	61.066423	71.385742
748.572639	66.740763	71.390746
747.793047	59.251858	71.395751
747.490229	66.520518	71.400756
746.414679	69.135903	71.405761
745.795695	55.386552	71.410766
745.247079	77.015333	71.415770
745.072499	78.903853	71.420775
744.375675	58.397451	71.425780
743.467429	60.672409	71.430785
742.505045	82.013853	71.435790
742.516517	42.773637	71.440794
740.799667	77.528048	71.445799
740.446560	41.252022	71.450804
739.789231	73.297443	71.455809
739.690180	54.592842	71.460814
738.899568	52.768178	71.465818
737.653341	72.097003	71.470823
737.429540	53.510028	71.475828
736.826598	52.557448	71.480833
735.939303	77.488464	71.485838
735.714486	62.913159	71.490842
734.580660	63.841132	71.495847
734.649343	58.910453	71.500852
733.115267	69.978242	71.505857
732.492154	73.690055	71.510862
732.184674	49.800832	71.515866
731.196944	77.567250	71.520871
730.513689	66.242291	71.525876
729.622099	61.940699	71.530881
729.179011	69.454028	71.535886
729.112987	62.449155	71.540890
728.430126	71.533360	71.545895
727.835797	67.466699	71.550900
726.660297	69.910359	71.555905
726.075805	70.705151	71.560910
725.730333	63.662770	71.565914
724.312426	72.936534	71.570919
723.826505	66.365916	71.575924
723.431136	71.974695	71.580929
722.941542	62.331375	71.585934
722.652097	55.593873	71.590938
721.151853	81.034040	71.595943
720.817478	53.493946	71.600948
720.151328	81.761074	71.605953
719.850791	56.038434	71.610958
719.129616	60.286220	71.615962
718.131150	71.129981	71.620967
717.528872	69.302145	71.625972
716.747332	68.742255	71.630977
715.787577	59.227406	71.635982
715.211923	57.813199	71.640986
714.928496	64.202041	71.645991
714.432858	64.998457	71.650996
713.927605	72.961629	71.656001
713.124786	68.876129	71.661006
712.260100	64.720061	71.666010
711.726738	67.141913	71.671015
710.781969	53.491751	71.676020
709.635648	68.730088	71.681025
709.338127	58.225193	71.686030
708.929736	83.627142	71.691034
708.678795	54.392841	71.696039
707.974522	66.449669	71.701044
707.290062	64.537155	71.706049
706.384104	63.722705	71.711054
706.019600	42.392355	71.716058
704.586676	88.309860	71.721063
704.030849	58.160636	71.726068
703.442379	61.428571	71.731073
702.950866	74.555329	71.736078
702.691778	37.933223	71.741082
701.144224	82.312608	71.746087
701.095980	57.030747	71.751092
700.503020	68.355540	71.756097
700.447697	42.691655	71.761102
699.247999	74.754047	71.766106
698.201609	72.031890	71.771111
697.910720	42.878089	71.776116
697.010523	72.926459	71.781121
695.887672	67.592592	71.786126
695.782970	58.737926	71.791130
694.543854	74.062006	71.796135
695.030504	57.883313	71.801140
694.055217	69.669501	71.806145
693.250155	67.927570	71.811150
692.819630	51.648925	71.816154
691.437354	88.917223	71.821159
691.296915	45.352242	71.826164
690.482638	82.282523	71.831169
690.336641	57.013075	71.836174
689.068130	49.070644	71.841178
688.409004	74.331159	71.846183
687.915588	42.289276	71.851188
687.126198	67.460140	71.856193
685.999598	38.311691	71.861198
685.792235	72.707504	71.866202
685.021275	55.161658	71.871207
684.846351	61.389731	71.876212
684.580345	40.245547	71.881217
683.234624	74.086223	71.886222
682.915360	53.421980	71.891226
681.526081	54.554641	71.896231
681.116906	60.287036	71.901236
680.791310	51.691460	71.906241
679.879064	75.484809	71.911246
679.526114	51.569730	71.916250
678.065549	57.100545	71.921255
677.423568	72.507735	71.926260
676.880757	52.432565	71.931265
676.328607	67.488001	71.936270
676.067550	66.022134	71.941274
675.921582	50.608032	71.946279
674.521521	69.420505	71.951284
674.483806	36.844066	71.956289
673.022215	81.033156	71.961294
672.375537	77.678120	71.966298
671.744172	72.105168	71.971303
671.027704	67.140242	71.976308
670.604022	49.241090	71.981313
670.334024	41.593818	71.986318
669.393834	74.513698	71.991322
668.378371	78.346341	71.996327
668.398372	33.600027	72.001332
667.622874	78.613361	72.006337
666.145979	75.764235	72.011342
665.811914	41.803192	72.016346
665.079641	39.855732	72.021351
664.748066	90.973364	72.026356
664.442205	48.834974	72.031361
663.304114	74.408281	72.036366
662.795964	51.262196	72.041370
662.226496	48.222862	72.046375
661.407456	60.545531	72.051380
660.640235	57.293270	72.056385
659.734814	62.309952	72.061390
659.663739	53.142453	72.066394
659.105222	58.207968	72.071399
658.250481	59.255528	72.076404
657.679286	56.393075	72.081409
657.019246	54.886670	72.086414
655.716957	61.582819	72.091418
654.921130	59.770051	72.096423
654.488715	55.182501	72.101428
654.390943	50.686737	72.106433
653.805268	80.894763	72.111438
653.307350	44.769560	72.116442
652.327903	54.675227	72.121447
651.470241	77.486973	72.126452
650.710008	42.758063	72.131457
649.566036	62.608324	72.136462
649.351259	67.597033	72.141466
648.854053	48.925901	72.146471
648.642453	50.337801	72.151476
647.618345	60.102360	72.156481
646.837659	60.098987	72.161486
646.998038	55.592075	72.166490
645.594257	60.751191	72.171495
644.859418	61.625131	72.176500
644.191343	64.986174	72.181505
643.458338	50.755162	72.186510
642.194791	38.431484	72.191514
641.698631	63.866289	72.196519
641.560403	67.630209	72.201524
641.395938	50.692667	72.206529
640.682595	53.576824	72.211534
640.023027	66.287243	72.216538
639.110365	51.641744	72.221543
638.543933	56.492494	72.226548
637.240808	59.790669	72.231553
636.013427	68.015486	72.236558
636.014479	39.646232	72.241562
635.661200	76.864183	72.246567
635.124407	44.230029	72.251572
634.929859	54.381274	72.256577
633.710273	70.564797	72.261582
633.253890	39.478934	72.266586
632.531131	55.461909	72.271591
631.887752	58.506804	72.276596
630.835460	64.289580	72.281601
629.970970	49.537076	72.286606
629.946723	53.331724	72.291610
628.829637	56.150875	72.296615
627.850916	55.357504	72.301620
627.687938	60.866207	72.306625
627.106672	61.124378	72.311630
626.982449	63.429056	72.316634
625.639977	64.833398	72.321639
624.882709	50.511647	72.326644
624.625723	57.831352	72.331649
623.843575	61.478629	72.336654
623.341482	51.592925	72.341658
622.176184	65.864543	72.346663
621.500483	56.277701	72.351668
621.573277	57.371520	72.356673
620.168309	54.864188	72.361678
619.654620	47.766630	72.366682
618.638366	50.899288	72.371687
618.550360	41.515317	72.376692
618.427789	58.597970	72.381697
616.943697	68.707014	72.386702
616.696057	52.020827	72.391706
615.924024	51.513070	72.396711
615.034055	64.411559	72.401716
614.063407	63.873933	72.406721
613.425564	51.262975	72.411726
613.158453	64.089081	72.416730
612.771521	67.269751	72.421735
611.971788	58.193064	72.426740
610.974076	56.756215	72.431745
610.557057	38.925418	72.436750
610.518487	70.593181	72.441754
609.339064	47.227620	72.446759
608.604700	64.950144	72.451764
608.069055	36.915516	72.456769
607.338729	65.798337	72.461774
606.604826	48.303404	72.466778
605.290582	44.248937	72.471783
605.112349	55.644871	72.476788
604.720204	55.658477	72.481793
604.630397	49.018509	72.486798
603.587085	64.951628	72.491802
602.966820	49.220441	72.496807
601.726968	53.377401	72.501812
601.354845	58.838991	72.506817
600.163430	50.065949	72.511822
599.638589	46.414014	72.516826
599.452949	61.644453	72.521831
598.691519	53.854693	72.526836
598.086094	48.973033	72.531841
597.097514	60.989999	72.536846
597.002342	48.920213	72.541850
596.239358	62.008202	72.546855
595.006696	50.431783	72.551860
594.911454	59.438190	72.556865
593.927393	53.542995	72.561870
593.259906	51.462244	72.566874
592.326876	57.063622	72.571879
591.929258	58.027365	72.576884
591.354338	67.405040	72.581889
590.982034	62.082577	72.586894
590.505611	62.823921	72.591898
589.248620	56.125424	72.596903
588.876343	55.705388	72.601908
588.524970	63.077973	72.606913
587.046728	66.055579	72.611918
586.377066	58.689571	72.616922
586.089247	59.806129	72.621927
585.593560	56.463344	72.626932
584.897059	51.542579	72.631937
583.689357	62.736642	72.636942
583.222945	50.814284	72.641946
582.814265	62.412492	72.646951
582.147491	65.502124	72.651956
581.872425	55.942949	72.656961
580.795663	56.229584	72.661966
580.313098	51.533352	72.666970
579.790812	57.695328	72.671975
578.672681	54.095310	72.676980
578.228084	42.443858	72.681985
577.115750	57.211638	72.686990
577.082839	47.017855	72.691994
576.419838	55.531247	72.696999
575.253903	55.349570	72.702004
574.936329	55.958392	72.707009
574.444952	56.013036	72.712014
573.905864	59.304669	72.717018
572.735948	60.255806	72.722023
572.096958	53.384782	72.727028
571.954829	47.134750	72.732033
570.574608	62.176999	72.737038
570.089282	55.554296	72.742042
569.433075	59.990454	72.747047
568.943222	55.301692	72.752052
568.400282	48.432719	72.757057
567.196119	52.021074	72.762062
566.861513	55.037305	72.767066
566.281608	49.933984	72.772071
566.023293	60.667783	72.777076
565.270502	57.342299	72.782081
563.793074	64.405407	72.787086
563.272031	51.518839	72.792090
563.009505	51.377775	72.797095
562.544436	58.494096	72.802100
561.887711	58.839989	72.807105
560.937387	57.684176	72.812110
560.614915	46.036929	72.817114
559.519267	62.869311	72.822119
559.121660	62.729263	72.827124
558.640595	66.976691	72.832129
558.170694	64.173818	72.837134
557.059789	53.599828	72.842138
555.998514	50.452783	72.847143
555.807251	55.794113	72.852148
555.490314	64.138863	72.857153
554.371979	62.390109	72.862158
553.412537	55.401407	72.867162
552.928125	65.983575	72.872167
552.576053	53.596765	72.877172
551.886657	54.200159	72.882177
550.603998	56.121681	72.887182
550.401915	61.840027	72.892186
549.714581	61.801316	72.897191
549.382894	50.597054	72.902196
548.566017	64.374835	72.907201
547.535502	65.272244	72.912206
547.263579	49.827775	72.917210
546.560352	49.236545	72.922215
545.217322	53.938208	72.927220
545.102273	54.785994	72.932225
544.410135	58.370074	72.937230
544.044916	52.374758	72.942234
543.639291	54.591802	72.947239
542.346778	61.698002	72.952244
541.862200	50.399831	72.957249
541.356083	58.178660	72.962254
540.696244	60.934481	72.967258
539.871191	63.756039	72.972263
539.175428	59.311377	72.977268
538.973973	46.845397	72.982273
537.790220	59.360212	72.987278
537.003266	58.725554	72.992282
536.672046	57.956810	72.997287
536.015992	58.711007	73.002292
535.149216	49.593001	73.007297
534.008080	56.760241	73.012302
533.791615	53.488105	73.017306
533.312402	56.298730	73.022311
532.863836	50.892242	73.027316
532.097556	57.194006	73.032321
530.945963	60.520134	73.037326
530.614763	48.650370	73.042330
530.477568	49.787093	73.047335
529.333973	42.250614	73.052340
528.614506	44.219624	73.057345
527.401076	58.692883	73.062350
527.432555	48.343778	73.067354
526.943872	48.279740	73.072359
525.778639	53.850319	73.077364
525.361197	53.098464	73.082369
524.486950	54.172828	73.087374
524.319542	53.021626	73.092378
523.188894	57.996957	73.097383
522.570646	54.574369	73.102388
522.253377	51.212643	73.107393
521.519582	52.761343	73.112398
520.830085	48.829746	73.117402
519.991896	55.713785	73.122407
519.754482	53.402135	73.127412
518.770958	49.998312	73.132417
517.628620	49.336696	73.137422
517.100382	38.999489	73.142426
516.778330	53.999345	73.147431
516.164871	49.528970	73.152436
515.779964	47.598760	73.157441
514.805071	52.117227	73.162446
514.566637	47.665958	73.167450
513.915575	39.787700	73.172455
512.416479	54.654947	73.177460
512.250451	46.505473	73.182465
511.599701	50.497676	73.187470
510.740158	49.149240	73.192474
510.126915	46.859614	73.197479
509.139079	45.167363	73.202484
509.227509	43.429820	73.207489
508.143110	59.872516	73.212494
507.182008	50.974537	73.217498
506.539173	47.942199	73.222503
506.299792	51.110413	73.227508
505.929976	43.613105	73.232513
504.718169	51.007639	73.237518
504.180960	53.108463	73.242522
503.477150	45.117191	73.247527
503.026881	51.072173	73.252532
502.240976	41.763121	73.257537
501.116203	51.676210	73.262542
500.920782	48.645138	73.267546
500.499541	48.836849	73.272551
499.199869	61.258187	73.277556
498.758633	56.012954	73.282561
497.682456	55.195738	73.287566
497.383903	50.679935	73.292570
497.220306	53.665778	73.297575
496.860845	51.469761	73.302580
495.937115	48.925266	73.307585
495.155598	58.911407	73.312590
494.305989	52.532823	73.317594
493.350714	50.978884	73.322599
492.405233	59.243997	73.327604
492.220851	50.597587	73.332609
491.687661	61.472936	73.337614
491.656345	43.971794	73.342618
490.605462	59.139792	73.347623
489.620060	61.373513	73.352628
489.413622	55.341876	73.357633
488.058692	53.061602	73.362638
487.542590	55.324637	73.367642
487.313728	50.001426	73.372647
486.512009	54.935411	73.377652
485.394398	49.268109	73.382657
484.461377	49.829912	73.387662
484.331954	42.959744	73.392666
484.067385	53.543155	73.397671
483.334642	46.420611	73.402676
482.804166	45.844456	73.407681
481.646839	57.270207	73.412686
481.101907	49.031296	73.417690
480.427612	49.493542	73.422695
479.311653	57.419987	73.427700
479.034428	53.924163	73.432705
478.178389	51.282165	73.437710
477.916324	47.000235	73.442714
477.488690	44.665282	73.447719
476.276576	62.771408	73.452724
475.787463	51.321026	73.457729
475.352684	53.660987	73.462734
474.471635	42.124825	73.467738
473.781170	49.887297	73.472743
473.054910	53.975112	73.477748
472.932698	50.982840	73.482753
471.300347	54.041826	73.487758
470.698646	59.182056	73.492762
470.581280	57.475720	73.497767
469.997945	63.134963	73.502772
469.756004	46.868935	73.507777
468.513184	58.622104	73.512782
467.941526	51.529091	73.517786
467.554724	44.056574	73.522791
466.132215	58.255675	73.527796
465.366383	45.972656	73.532801
464.499742	36.116704	73.537806
464.225079	49.732419	73.542810
464.013003	39.981907	73.547815
463.404520	46.823056	73.552820
463.309218	46.196500	73.557825
462.218682	54.013250	73.562830
461.457053	45.253819	73.567834
460.355630	46.179904	73.572839
459.202527	45.337117	73.577844
459.069018	48.392278	73.582849
458.569718	61.097682	73.587854
458.334780	58.896023	73.592858
457.855338	50.142094	73.597863
456.607634	49.748012	73.602868
456.563703	46.448400	73.607873
455.300882	52.961741	73.612878
454.186598	57.434632	73.617882
453.797151	47.871637	73.622887
452.987936	45.986960	73.627892
453.052612	44.456615	73.632897
452.067798	46.218777	73.637902
451.042201	46.951449	73.642906
451.001256	57.611192	73.647911
450.176274	58.698231	73.652916
449.470884	48.606868	73.657921
448.697287	54.395764	73.662926
447.970368	54.760753	73.667930
447.773040	48.577874	73.672935
446.594841	58.821174	73.677940
445.788546	58.739948	73.682945
445.383156	56.122353	73.687950
445.194901	48.517288	73.692954
444.575654	55.781177	73.697959
443.368695	54.205858	73.702964
442.921772	59.091215	73.707969
441.487772	54.139770	73.712974
440.707484	47.959887	73.717978
440.546452	48.395561	73.722983
439.754009	60.643077	73.727988
439.472766	48.577734	73.732993
439.124745	58.849613	73.737998
438.547637	44.193344	73.743002
437.653995	49.644999	73.748007
436.828003	62.241615	73.753012
436.548669	53.452655	73.758017
435.434310	64.436372	73.763022
434.691290	53.583081	73.768026
434.280005	47.629820	73.773031
433.413603	61.125369	73.778036
432.982453	54.481458	73.783041
432.105901	55.035861	73.788046
431.637056	57.471137	73.793050
431.576573	50.930588	73.798055
430.034207	50.219213	73.803060
429.587991	44.246291	73.808065
428.819462	44.993204	73.813070
428.343709	51.753294	73.818074
427.568590	50.178563	73.823079
426.805120	58.058328	73.828084
426.265001	49.030244	73.833089
426.030207	49.160725	73.838094
424.941994	52.686518	73.843098
424.434680	46.931474	73.848103
423.605571	58.215073	73.853108
422.874209	48.276081	73.858113
421.772087	56.902039	73.863118
421.165370	58.894114	73.868122
420.916210	53.706601	73.873127
420.360410	63.546418	73.878132
420.036966	45.278180	73.883137
419.007190	53.947799	73.888142
418.331823	66.364316	73.893146
417.924705	46.784855	73.898151
416.918439	60.504526	73.903156
416.243559	54.954363	73.908161
415.384809	53.337771	73.913166
414.985495	53.970673	73.918170
414.612037	54.845444	73.923175
413.394031	63.029432	73.928180
412.996779	56.853178	73.933185
412.487340	59.312271	73.938190
411.706981	55.964426	73.943194
411.441387	57.230415	73.948199
410.153079	56.202625	73.953204
409.678217	53.091516	73.958209
409.182993	54.969641	73.963214
408.255847	54.827262	73.968218
407.265762	50.298664	73.973223
406.711302	52.034850	73.978228
406.605956	53.139697	73.983233
406.209064	62.460644	73.988238
405.377316	55.744958	73.993242
404.407328	52.818388	73.998247
403.660978	58.360122	74.003252
403.617133	46.337383	74.008257
402.600013	45.875051	74.013262
401.687217	53.617774	74.018266
401.068944	53.552333	74.023271
400.423310	60.464068	74.028276
400.079775	45.619220	74.033281
399.126038	52.611580	74.038286
398.532155	52.554868	74.043290
398.181979	58.862899	74.048295
397.179868	52.964364	74.053300
396.605093	48.599817	74.058305
395.904963	58.066842	74.063310
395.290953	50.351439	74.068314
394.337853	55.199190	74.073319
393.468676	52.354326	74.078324
393.072618	41.996097	74.083329
392.501487	53.073024	74.088334
392.331805	61.777488	74.093338
391.823258	50.689751	74.098343
390.418368	57.881726	74.103348
389.937274	56.931894	74.108353
389.032252	49.332245	74.113358
388.348083	56.841438	74.118362
387.593466	50.416227	74.123367
386.896341	54.169860	74.128372
386.796033	53.821630	74.133377
386.380077	44.091003	74.138382
385.344304	51.156359	74.143386
384.873858	43.951061	74.148391
384.058237	49.946927	74.153396
383.787843	49.949053	74.158401
382.930344	59.067444	74.163406
381.886140	50.625862	74.168410
381.398978	42.909178	74.173415
379.954346	48.915392	74.178420
379.962094	42.468052	74.183425
379.102903	52.955411	74.188430
378.453946	52.749794	74.193434
378.276448	41.308141	74.198439
377.651779	49.867492	74.203444
377.241429	39.073183	74.208449
376.433911	36.555950	74.213454
375.259067	51.286436	74.218458
374.629922	46.947904	74.223463
373.765241	57.187001	74.228468
373.610548	43.215605	74.233473
372.988921	49.661500	74.238478
371.800490	62.861470	74.243482
371.293651	45.612731	74.248487
370.612562	53.518800	74.253492
370.214967	45.595470	74.258497
369.359574	61.505005	74.263502
368.360194	54.260997	74.268506
368.250262	47.584842	74.273511
367.587783	48.248648	74.278516
367.256281	52.240471	74.283521
366.084362	54.041943	74.288526
365.222593	51.334672	74.293530
364.959570	47.614269	74.298535
364.069658	50.621242	74.303540
363.383846	38.651931	74.308545
362.696514	42.534885	74.313550
361.912475	51.360892	74.318554
361.707404	54.645065	74.323559
361.018833	55.492791	74.328564
360.032407	42.261022	74.333569
359.468632	49.790453	74.338574
358.944832	52.158809	74.343578
358.712623	48.553337	74.348583
357.295704	47.415192	74.353588
356.976660	37.494105	74.358593
356.419823	50.536657	74.363598
355.289448	48.632233	74.368602
354.762597	49.492035	74.373607
353.976233	50.831554	74.378612
353.706833	46.959215	74.383617
353.344270	51.282396	74.388622
352.593067	52.299366	74.393626
351.957690	45.255968	74.398631
351.211202	45.294543	74.403636
350.103687	58.063758	74.408641
349.237903	57.903739	74.413646
348.618798	57.007445	74.418650
348.285599	52.561839	74.423655
347.976276	51.335502	74.428660
347.210141	50.401142	74.433665
346.399422	55.472207	74.438670
345.576525	49.458412	74.443674
345.380163	53.125948	74.448679
344.008086	50.736533	74.453684
343.426024	44.222347	74.458689
343.187001	49.751050	74.463694
342.632949	51.274310	74.468698
341.754888	50.092877	74.473703
340.805066	48.091884	74.478708
340.236387	53.327792	74.483713
339.782881	44.088831	74.488718
339.477425	55.498716	74.493722
338.768345	46.973794	74.498727
337.999987	50.718290	74.503732
337.090918	47.327911	74.508737
336.126866	48.473416	74.513742
335.625179	48.250649	74.518746
335.345619	53.672281	74.523751
334.605383	54.228647	74.528756
333.759128	40.633957	74.533761
333.219728	37.249322	74.538766
332.484803	42.084396	74.543770
332.013891	42.027025	74.548775
330.928955	42.983653	74.553780
330.338724	50.165669	74.558785
329.928139	38.721751	74.563790
329.345853	47.413117	74.568794
328.605321	34.927454	74.573799
327.841686	47.607174	74.578804
327.050342	51.811045	74.583809
326.525029	40.662935	74.588814
325.239594	48.840351	74.593818
324.944131	32.849396	74.598823
324.273927	45.544185	74.603828
323.963511	39.906016	74.608833
323.623902	42.806380	74.613838
322.793663	46.899763	74.618842
322.209447	43.791911	74.623847
321.435850	50.695667	74.628852
320.293094	49.540657	74.633857
319.587975	52.401509	74.638862
318.655158	50.722645	74.643866
318.331478	39.354760	74.648871
317.975653	52.076720	74.653876
317.900984	38.808475	74.658881
316.957849	51.549921	74.663886
315.863597	54.499595	74.668890
315.719853	42.508563	74.673895
314.546276	58.588652	74.678900
313.624094	47.003930	74.683905
313.155928	53.964661	74.688910
312.721060	51.088458	74.693914
312.367119	49.902350	74.698919
311.007220	56.655139	74.703924
310.451710	59.359696	74.708929
310.222359	52.784574	74.713934
309.280415	51.496648	74.718938
308.483538	47.020876	74.723943
307.653267	51.306645	74.728948
307.419987	54.384019	74.733953
307.053441	40.320256	74.738958
306.262648	45.107475	74.743962
305.834433	45.722924	74.748967
304.847437	57.364423	74.753972
304.246017	49.677005	74.758977
303.317547	47.729390	74.763982
302.251496	57.346207	74.768986
302.043452	51.735874	74.773991
301.700876	62.907270	74.778996
300.704209	43.715110	74.784001
299.923924	47.404751	74.789006
299.292678	44.332784	74.794010
299.282584	40.304019	74.799015
298.107440	50.362389	74.804020
297.554903	43.722095	74.809025
296.766957	46.742798	74.814030
296.010453	37.817054	74.819034
295.717756	36.197018	74.824039
294.558294	50.846235	74.829044
294.431156	48.185901	74.834049
293.909588	43.869671	74.839054
292.571053	44.379488	74.844058
291.914404	46.625536	74.849063
291.205446	45.686812	74.854068
290.938587	51.694584	74.859073
290.928771	50.936148	74.864078
289.284926	57.563903	74.869082
288.908711	41.000810	74.874087
288.094812	52.658873	74.879092
287.636007	56.644188	74.884097
286.713055	41.590548	74.889102
285.958953	51.261719	74.894106
286.143905	53.178106	74.899111
284.883770	56.835430	74.904116
283.844452	45.857556	74.909121
283.491661	59.042630	74.914126
282.791465	57.200556	74.919130
283.008073	45.598341	74.924135
281.484527	58.359773	74.929140
280.694686	42.248933	74.934145
280.347912	53.711131	74.939150
279.538833	49.532184	74.944154
278.905184	46.556793	74.949159
277.945834	54.754795	74.954164
277.796905	48.223628	74.959169
277.191086	56.002610	74.964174
276.209223	51.573678	74.969178
275.594947	50.030128	74.974183
275.194980	57.211791	74.979188
274.455624	42.177777	74.984193
273.614117	47.816701	74.989198
272.663363	55.351060	74.994202
272.170459	49.565377	74.999207
272.027021	48.258998	75.004212
271.352351	57.048674	75.009217
270.576312	42.263343	75.014222
269.549946	52.435198	75.019226
269.576362	47.225864	75.024231
268.026547	48.348071	75.029236
267.069270	51.063060	75.034241
266.411803	48.588174	75.039246
266.209801	52.365414	75.044250
266.108073	50.617178	75.049255
265.429784	53.861671	75.054260
264.706489	49.025704	75.059265
263.722281	50.751574	75.064270
263.174875	47.628410	75.069274
262.398958	57.337757	75.074279
261.409579	52.162605	75.079284
260.774471	56.450395	75.084289
260.694610	53.563346	75.089294
260.178176	60.123377	75.094298
259.167388	44.352094	75.099303
258.467181	48.874170	75.104308
257.960337	61.831507	75.109313
257.341101	55.629175	75.114318
256.429805	50.302818	75.119322
255.569719	51.047032	75.124327
255.043089	57.093060	75.129332
254.702187	42.536402	75.134337
254.510074	49.809503	75.139342
253.235373	52.619243	75.144346
252.596291	45.765690	75.149351
252.191083	56.071917	75.154356
250.988126	51.085344	75.159361
250.737225	50.256534	75.164366
249.938936	55.838119	75.169370
249.324876	41.850092	75.174375
248.213888	57.472400	75.179380
247.458670	56.862738	75.184385
247.030901	49.712170	75.189390
246.807492	55.214737	75.194394
246.517816	46.722340	75.199399
245.424391	52.991167	75.204404
244.850672	43.107543	75.209409
243.853126	50.505875	75.214414
242.892762	50.781987	75.219418
242.492719	44.696103	75.224423
241.856065	44.084890	75.229428
241.354129	47.239780	75.234433
241.233442	48.414882	75.239438
239.950693	53.772514	75.244442
239.559140	53.287801	75.249447
238.634573	54.725073	75.254452
237.473055	48.639150	75.259457
236.797344	56.810876	75.264462
236.270498	52.225859	75.269466
235.914207	48.761599	75.274471
235.141020	58.263951	75.279476
235.242797	42.182886	75.284481
234.793563	39.324759	75.289486
233.448978	54.828197	75.294490
232.758957	46.582533	75.299495
232.151422	48.659928	75.304500
231.173731	50.719063	75.309505
230.533077	52.560482	75.314510
229.975494	56.457479	75.319514
229.765168	52.020692	75.324519
228.714571	62.483414	75.329524
228.137469	61.526843	75.334529
227.928683	43.692948	75.339534
226.730329	51.746149	75.344538
226.107152	51.738299	75.349543
225.447567	61.391269	75.354548
225.013540	57.680797	75.359553
224.179290	54.027818	75.364558
223.309109	48.248675	75.369562
222.782454	48.376817	75.374567
222.146796	56.237830	75.379572
221.739309	54.148856	75.384577
220.773453	44.540623	75.389582
219.762909	54.689473	75.394586
219.476192	60.254170	75.399591
219.117718	55.244952	75.404596
218.098915	55.788992	75.409601
217.621042	52.137549	75.414606
216.814964	59.983156	75.419610
216.395195	48.241129	75.424615
215.626613	44.790560	75.429620
214.308083	53.085258	75.434625
214.317239	44.496351	75.439630
213.504324	52.893363	75.444634
213.302396	54.220179	75.449639
212.332385	62.071422	75.454644
211.478421	57.664704	75.459649
211.414317	48.166596	75.464654
210.068910	59.125718	75.469658
209.564163	56.883528	75.474663
208.413293	68.257892	75.479668
208.353900	51.623810	75.484673
208.073263	45.553589	75.489678
207.200320	57.648410	75.494682
206.663190	52.839551	75.499687
206.023700	50.637765	75.504692
204.622726	49.952876	75.509697
204.345605	50.864354	75.514702
203.283788	56.497423	75.519706
203.201088	48.128147	75.524711
202.589103	41.169376	75.529716
201.352267	42.702169	75.534721
200.789075	45.445814	75.539726
200.259860	50.817370	75.544730
199.987491	53.151981	75.549735
199.534488	47.579138	75.554740
198.410912	52.160837	75.559745
197.985080	41.088369	75.564750
196.807140	48.132300	75.569754
196.123927	53.227231	75.574759
195.059683	55.260756	75.579764
194.535021	48.850996	75.584769
194.284073	40.879105	75.589774
193.854659	47.549838	75.594778
193.521283	42.740041	75.599783
192.651263	38.253900	75.604788
191.701148	50.616469	75.609793
191.449633	37.365403	75.614798
190.334611	59.830288	75.619802
190.023847	56.431312	75.624807
189.267233	51.064556	75.629812
188.351521	53.143786	75.634817
187.577397	47.272080	75.639822
186.553921	54.034368	75.644826
186.619903	46.644264	75.649831
185.915026	53.904502	75.654836
185.485236	57.497303	75.659841
184.455216	59.446535	75.664846
184.015940	55.287510	75.669850
183.817677	49.899547	75.674855
182.752760	49.414967	75.679860
181.505681	60.601260	75.684865
181.152307	40.647504	75.689870
180.647445	44.895621	75.694874
179.726807	45.922308	75.699879
178.972995	45.006537	75.704884
178.047316	51.229724	75.709889
177.874270	42.073822	75.714894
177.293378	50.886406	75.719898
176.746896	51.826638	75.724903
176.033976	43.075328	75.729908
175.266196	47.371670	75.734913
174.742013	45.274504	75.739918
173.818113	45.160081	75.744922
173.196713	56.361734	75.749927
172.296001	56.782894	75.754932
171.965581	54.952859	75.759937
171.760148	62.915594	75.764942
170.764396	52.446460	75.769946
170.054545	44.011607	75.774951
169.502999	62.506061	75.779956
168.729897	46.648052	75.784961
167.893998	44.805574	75.789966
167.295363	51.061773	75.794970
167.153452	43.928728	75.799975
166.308427	53.469351	75.804980
165.340072	53.185411	75.809985
164.928553	41.489394	75.814990
163.792614	52.955992	75.819994
163.121633	53.299532	75.824999
162.461891	47.682393	75.830004
162.053552	49.622398	75.835009
161.923886	44.843203	75.840014
161.050026	45.263240	75.845018
159.872031	45.514161	75.850023
159.093205	51.937852	75.855028
158.584901	51.694101	75.860033
158.202017	47.045157	75.865038
157.306113	51.401353	75.870042
156.671482	39.742489	75.875047
156.001944	42.870501	75.880052
155.545953	54.348537	75.885057
155.209712	52.796958	75.890062
154.118379	50.892713	75.895066
153.615220	55.175257	75.900071
153.189214	47.046791	75.905076
151.817254	58.568372	75.910081
151.195513	47.087209	75.915086
150.421809	58.120774	75.920090
150.184020	53.696260	75.925095
149.990465	49.857588	75.930100
148.854121	54.756712	75.935105
148.308525	53.304740	75.940110
147.762437	52.600270	75.945114
146.728153	61.456768	75.950119
146.046638	47.162587	75.955124
145.366439	59.149427	75.960129
145.013913	56.499809	75.965134
144.321645	60.970192	75.970138
143.505345	55.478935	75.975143
142.977982	52.246957	75.980148
142.237932	61.526442	75.985153
141.854992	44.745286	75.990158
140.895221	63.684848	75.995162
140.312318	56.122252	76.000167
140.050603	52.333869	76.005172
138.514790	44.377624	76.010177
138.162489	45.103991	76.015182
137.306718	58.914847	76.020186
136.857462	59.055897	76.025191
136.830315	45.245552	76.030196
135.861971	60.022039	76.035201
134.777884	62.129712	76.040206
134.132798	64.020745	76.045210
133.662932	52.389221	76.050215
132.880117	51.571122	76.055220
132.040473	68.037971	76.060225
131.681800	47.717663	76.065230
130.948376	55.657353	76.070234
130.650058	58.194790	76.075239
129.827456	53.778375	76.080244
128.908916	46.020163	76.085249
128.988591	47.339928	76.090254
127.444294	52.434984	76.095258
126.730931	58.282162	76.100263
126.475543	54.779757	76.105268
125.966412	55.980532	76.110273
125.159713	47.176387	76.115278
124.095042	54.412010	76.120282
123.478866	55.592009	76.125287
123.474267	42.033522	76.130292
122.730237	51.364099	76.135297
121.738756	48.508882	76.140302
121.279178	53.309570	76.145306
120.488484	44.878165	76.150311
119.600877	41.966967	76.155316
118.547154	51.115129	76.160321
118.628124	40.630457	76.165326
117.968855	44.467996	76.170330
117.198007	53.925845	76.175335
116.327863	51.623677	76.180340
115.567174	46.930911	76.185345
115.302645	42.565858	76.190350
114.344927	53.769107	76.195354
113.997964	45.276413	76.200359
113.262892	47.259062	76.205364
112.424771	55.463013	76.210369
112.395600	45.957773	76.215374
111.164320	44.041174	76.220378
110.466184	42.924173	76.225383
109.918517	47.310006	76.230388
109.407034	49.712711	76.235393
108.599043	50.395057	76.240398
107.571469	52.006485	76.245402
107.156980	51.233735	76.250407
106.788620	45.697878	76.255412
105.510185	50.182891	76.260417
104.833462	47.387871	76.265422
104.278500	57.945050	76.270426
103.858161	50.079024	76.275431
103.674382	53.651529	76.280436
103.000830	55.895589	76.285441
102.001127	42.377517	76.290446
101.392235	54.796081	76.295450
100.945418	53.884995	76.300455
100.050881	49.385452	76.305460
98.828109	55.643423	76.310465
98.767033	49.021007	76.315470
98.361038	47.707625	76.320474
97.243354	48.354207	76.325479
96.492323	40.255512	76.330484
95.838039	56.367968	76.335489
95.635368	46.805246	76.340494
94.150841	52.855816	76.345498
93.642911	52.425952	76.350503
93.295895	44.097263	76.355508
92.611534	52.970510	76.360513
92.617321	48.254871	76.365518
91.726984	47.307285	76.370522
90.809613	46.783450	76.375527
90.141108	56.224987	76.380532
89.326464	54.880582	76.385537
88.428657	49.314044	76.390542
87.689255	55.616358	76.395546
87.272340	47.557417	76.400551
86.996293	47.216726	76.405556
86.328519	50.664573	76.410561
85.547699	44.795552	76.415566
84.956695	56.025483	76.420570
84.301361	55.384176	76.425575
83.334343	49.076524	76.430580
82.491274	55.234533	76.435585
82.204717	49.947391	76.440590
81.769513	52.426241	76.445594
81.229474	40.518949	76.450599
80.245355	44.184387	76.455604
79.679403	51.892391	76.460609
79.097716	40.445871	76.465614
77.705610	46.800232	76.470618
77.014703	37.458869	76.475623
76.781038	41.731559	76.480628
76.163940	58.159765	76.485633
75.968805	47.055271	76.490638
74.942464	45.955926	76.495642
74.245907	50.110061	76.500647
74.099130	51.735576	76.505652
72.643918	56.734462	76.510657
72.052863	41.102926	76.515662
71.464243	52.498043	76.520666
71.098945	42.475595	76.525671
70.165683	49.050082	76.530676
68.826362	49.277892	76.535681
69.020645	46.418097	76.540686
68.340611	51.383248	76.545690
67.782363	53.637312	76.550695
67.027741	29.125880	76.555700
65.596297	47.368000	76.560705
65.760632	41.969539	76.565710
65.160560	38.820136	76.570714
64.681875	54.442576	76.575719
63.579498	51.985087	76.580724
62.802328	46.932295	76.585729
62.710319	46.669483	76.590734
61.695175	47.187773	76.595738
60.556767	47.769873	76.600743
59.953574	51.841318	76.605748
59.267476	59.923278	76.610753
59.178929	45.819984	76.615758
58.843709	43.096666	76.620762
58.042751	50.791691	76.625767
57.348203	42.210950	76.630772
55.931404	56.847673	76.635777
55.532110	50.496801	76.640782
54.578299	47.839018	76.645786
54.492539	49.170972	76.650791
53.999808	43.140911	76.655796
53.381319	53.238325	76.660801
52.306915	42.934757	76.665806
51.908090	46.943651	76.670810
51.378204	35.810559	76.675815
50.195042	44.151541	76.680820
49.421032	49.172681	76.685825
48.925659	55.773531	76.690830
48.468422	53.725638	76.695834
47.887518	43.761232	76.700839
47.374643	47.411451	76.705844
46.067894	55.139837	76.710849
45.700777	44.297728	76.715854
45.190621	41.384708	76.720858
44.790648	48.394511	76.725863
43.937550	50.471690	76.730868
43.090929	45.199764	76.735873
42.822404	37.287473	76.740878
41.616699	45.512215	76.745882
40.725140	49.397857	76.750887
40.342608	50.881211	76.755892
39.859318	52.737001	76.760897
39.552714	47.260690	76.765902
38.575248	53.600981	76.770906
37.723013	51.975605	76.775911
37.336110	45.357854	76.780916
36.680410	50.544619	76.785921
35.852527	48.885400	76.790926
34.848414	47.743107	76.795930
34.261056	52.562608	76.800935
34.192646	53.418743	76.805940
33.532911	47.549352	76.810945
32.993541	34.933974	76.815950
31.963224	56.335203	76.820954
31.503122	47.665042	76.825959
30.709525	40.774713	76.830964
29.623588	49.456566	76.835969
29.567261	51.657395	76.840974
28.810432	46.793746	76.845978
27.649964	48.074766	76.850983
26.992045	43.189037	76.855988
26.451178	48.849463	76.860993
26.380145	43.859096	76.865998
25.882702	52.500708	76.871002
24.862184	49.312721	76.876007
24.226520	45.114098	76.881012
23.241003	52.772340	76.886017
22.353388	47.186860	76.891022
21.405962	45.045277	76.896026
21.118241	49.094799	76.901031
20.886068	43.888876	76.906036
20.557227	50.070535	76.911041
19.531033	58.003330	76.916046
18.694200	54.104854	76.921050
18.227718	47.805706	76.926055
17.350626	53.343153	76.931060
16.283123	60.049450	76.936065
15.895022	49.204385	76.941070
15.386970	50.647842	76.946074
14.997045	48.709061	76.951079
14.352799	40.394685	76.956084
13.266562	50.964068	76.961089
12.995110	46.352571	76.966094
12.234709	45.819499	76.971098
11.162464	52.406711	76.976103
10.836185	38.779711	76.981108
10.099302	50.521733	76.986113
10.079797	47.287631	76.991118
8.931706	47.256332	76.996122
7.725815	52.549777	77.001127
7.385971	44.756090	77.006132
7.202110	43.743163	77.011137
6.272374	43.205564	77.016142
5.141393	49.226599	77.021147
4.708747	48.215507	77.026151
4.421775	42.589427	77.031156
3.383509	51.814004	77.036161