Mon Mar 08 19:53:37 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.132186	91.725664	0.000000
-1.677298	92.563182	0.005005
-1.772149	50.877162	0.010010
-4.088251	24.066611	0.015014
-8.595356	10.683824	0.020019
-13.524405	21.768292	0.025024
-18.632256	30.279517	0.030029
-22.750849	20.709069	0.035034
-26.897898	22.534230	0.040038
-30.733026	20.868991	0.045043
-34.087481	18.989904	0.050048
-37.711015	26.009249	0.055053
-41.382689	12.835443	0.060058
-45.221927	22.951416	0.065062
-48.987280	21.935770	0.070067
-52.531347	22.091111	0.075072
-56.514579	17.690077	0.080077
-60.057146	17.108808	0.085082
-63.902320	18.641469	0.090086
-68.033563	18.133617	0.095091
-71.620600	20.366224	0.100096
-75.699530	30.545712	0.105101
-78.838504	18.064365	0.110106
-82.708114	19.422771	0.115110
-86.832782	19.670783	0.120115
-90.186507	17.645013	0.125120
-94.272954	31.502906	0.130125
-98.040033	15.618063	0.135130
-101.437606	12.987494	0.140134
-105.308983	27.853377	0.145139
-109.041662	20.444857	0.150144
-112.929801	20.566875	0.155149
-116.893363	23.509273	0.160154
-120.584840	14.285573	0.165158
-124.427648	16.164854	0.170163
-127.859487	23.565295	0.175168
-131.680893	25.234609	0.180173
-135.525057	25.986688	0.185178
-139.205771	19.654788	0.190182
-143.351253	18.583253	0.195187
-147.022752	21.926922	0.200192
-150.486282	21.831454	0.205197
-153.769831	9.169880	0.210202
-157.583887	26.609542	0.215206
-161.751926	16.455925	0.220211
-165.622862	17.425196	0.225216
-169.728685	16.400991	0.230221
-173.504840	4.098727	0.235226
-177.532169	15.719239	0.240230
-181.270432	29.726695	0.245235
-184.647747	16.862519	0.250240
-188.327022	9.235893	0.255245
-192.050216	21.722464	0.260250
-195.696662	17.390918	0.265254
-199.654904	20.999600	0.270259
-203.329015	18.452724	0.275264
-207.041491	21.481347	0.280269
-210.808627	19.226849	0.285274
-214.409165	23.363478	0.290278
-218.246249	23.225225	0.295283
-221.964366	15.835066	0.300288
-226.040671	29.169610	0.305293
-229.468895	26.575649	0.310298
-233.524542	16.322233	0.315302
-237.171577	13.425763	0.320307
-240.599076	18.758435	0.325312
-244.678752	27.058723	0.330317
-248.616103	9.857861	0.335322
-252.438925	22.734126	0.340326
-256.201143	21.156952	0.345331
-259.562017	12.082552	0.350336
-263.518894	22.704861	0.355341
-267.340207	21.706373	0.360346
-270.948375	18.953550	0.365350
-274.710666	20.753990	0.370355
-278.203999	10.947034	0.375360
-282.358661	23.166732	0.380365
-285.886929	20.051123	0.385370
-289.884180	28.133339	0.390374
-293.417158	14.089479	0.395379
-297.343664	14.563244	0.400384
-301.584902	16.791804	0.405389
-304.762883	26.384756	0.410394
-308.270019	19.126626	0.415398
-312.419476	21.247523	0.420403
-316.425502	20.597117	0.425408
-320.104925	17.652332	0.430413
-323.762924	13.024811	0.435418
-327.518549	20.527661	0.440422
-331.107887	27.308594	0.445427
-335.058006	15.084823	0.450432
-338.872749	29.383806	0.455437
-342.251528	23.760909	0.460442
-346.115201	14.554027	0.465446
-350.248777	25.070647	0.470451
-353.552928	15.805995	0.475456
-357.163112	17.311065	0.480461
-360.449705	23.345173	0.485466
-364.457328	9.009805	0.490470
-368.751615	20.274295	0.495475
-372.474292	17.792201	0.500480
-376.214778	22.869121	0.505485
-380.214604	15.830098	0.510490
-383.894007	15.614901	0.515494
-387.593941	27.080983	0.520499
-391.306718	14.098811	0.525504
-395.397289	28.974879	0.530509
-399.286383	15.413789	0.535514
-402.816021	20.447625	0.540518
-406.596941	23.252529	0.545523
-410.056388	28.724567	0.550528
-414.078297	17.575181	0.555533
-417.473814	24.397823	0.560538
-421.575085	22.476108	0.565542
-425.245497	22.671091	0.570547
-428.805726	16.392953	0.575552
-432.739825	26.054752	0.580557
-436.609841	29.358016	0.585562
-440.427246	28.989912	0.590566
-443.969955	27.396908	0.595571
-447.761199	15.865427	0.600576
-451.861873	21.846730	0.605581
-455.382833	24.484054	0.610586
-459.251426	19.324291	0.615590
-462.982710	15.504988	0.620595
-466.389102	22.411427	0.625600
-470.523612	15.723626	0.630605
-473.956730	19.386078	0.635610
-477.700563	26.668092	0.640614
-482.050228	15.020856	0.645619
-484.983990	22.178249	0.650624
-489.290273	24.684008	0.655629
-493.264797	14.004979	0.660634
-497.104992	16.477317	0.665638
-500.747310	16.518131	0.670643
-504.325092	18.000902	0.675648
-508.191713	24.323359	0.680653
-511.776398	12.120389	0.685658
-515.434145	28.833901	0.690662
-519.546966	29.594806	0.695667
-522.692424	11.506369	0.700672
-526.784123	22.194764	0.705677
-530.469045	22.035863	0.710682
-534.389550	15.821737	0.715686
-538.242851	19.232868	0.720691
-541.704984	30.481433	0.725696
-545.592833	24.217956	0.730701
-549.352921	18.951134	0.735706
-552.821551	8.713346	0.740710
-557.028231	25.139300	0.745715
-560.479075	15.163585	0.750720
-564.580900	24.686809	0.755725
-568.496532	16.344824	0.760730
-571.881017	18.757107	0.765734
-575.441990	23.455600	0.770739
-579.301312	15.864670	0.775744
-583.499979	27.580990	0.780749
-587.144566	16.455220	0.785754
-590.952222	21.562115	0.790758
-594.691581	28.469881	0.795763
-598.260290	17.745135	0.800768
-602.264245	21.360191	0.805773
-605.795853	25.625141	0.810778
-609.572053	27.907678	0.815782
-613.359580	25.527780	0.820787
-616.795432	12.257349	0.825792
-620.668202	28.161750	0.830797
-624.655666	29.852060	0.835802
-628.509635	21.296915	0.840806
-632.430276	23.522144	0.845811
-635.959535	12.053208	0.850816
-639.593884	29.234620	0.855821
-643.122612	11.153985	0.860826
-647.152485	20.746263	0.865830
-651.062949	35.299092	0.870835
-654.788031	23.244923	0.875840
-658.771632	30.472481	0.880845
-662.579365	18.172935	0.885850
-666.189619	19.538142	0.890854
-669.633031	27.217109	0.895859
-672.928075	15.438019	0.900864
-676.923137	29.900328	0.905869
-680.884850	18.450094	0.910874
-684.977142	20.614531	0.915878
-689.156124	21.209695	0.920883
-692.762030	8.583097	0.925888
-696.282101	24.814419	0.930893
-699.562510	17.555362	0.935898
-703.356611	18.207316	0.940902
-707.527579	23.451284	0.945907
-711.213077	13.767168	0.950912
-714.881817	20.368961	0.955917
-718.464676	10.562812	0.960922
-722.253283	9.851544	0.965926
-726.418637	27.064308	0.970931
-729.808744	19.936353	0.975936
-733.515373	20.055604	0.980941
-737.304056	22.581589	0.985946
-740.856007	7.191741	0.990950
-745.545418	19.773575	0.995955
-748.684696	13.015544	1.000960
-752.276107	17.616662	1.005965
-756.391000	14.792614	1.010970
-760.013704	13.432050	1.015974
-764.190960	6.614434	1.020979
-767.467707	7.458180	1.025984
-771.074330	16.386976	1.030989
-774.959485	15.449969	1.035994
-778.441471	25.021127	1.040998
-782.342751	20.789572	1.046003
-786.247025	15.175632	1.051008
-790.160444	11.397005	1.056013
-793.813924	20.304942	1.061018
-797.870129	13.583146	1.066022
-801.803983	18.128689	1.071027
-805.741627	13.959754	1.076032
-809.321294	21.520350	1.081037
-812.823057	16.125951	1.086042
-816.430966	10.658646	1.091046
-820.406804	10.152489	1.096051
-824.004268	9.928032	1.101056
-827.777251	25.709559	1.106061
-831.305761	15.259444	1.111066
-834.782766	12.313080	1.116070
-839.053002	15.941128	1.121075
-842.802655	14.131092	1.126080
-846.747669	20.627441	1.131085
-850.504564	27.697653	1.136090
-853.869987	24.806012	1.141094
-857.956958	15.181584	1.146099
-861.618625	11.408565	1.151104
-865.496795	23.622847	1.156109
-869.143283	9.378905	1.161114
-872.877178	11.879000	1.166118
-877.155832	22.897440	1.171123
-880.605743	17.398670	1.176128
-884.351535	20.148246	1.181133
-887.735888	19.263821	1.186138
-891.444160	19.136021	1.191142
-895.520936	26.396198	1.196147
-899.288559	11.686009	1.201152
-903.197498	29.599166	1.206157
-906.643470	16.777053	1.211162
-910.120520	21.926200	1.216166
-914.271861	22.389620	1.221171
-918.045221	17.224869	1.226176
-921.968354	20.953678	1.231181
-925.790229	17.726723	1.236186
-929.143823	19.467575	1.241190
-933.136834	25.989084	1.246195
-936.696775	14.011497	1.251200
-940.713363	21.274738	1.256205
-944.120156	22.562108	1.261210
-947.870981	19.956134	1.266214
-952.087872	20.471098	1.271219
-955.509669	20.584577	1.276224
-959.485983	20.138650	1.281229
-963.354737	18.991193	1.286234
-966.891473	21.899844	1.291238
-970.743033	20.636119	1.296243
-974.144185	19.484869	1.301248
-978.056949	27.215655	1.306253
-982.092554	18.992916	1.311258
-985.871903	21.120444	1.316262
-989.616239	38.597445	1.321267
-993.294045	18.794117	1.326272
-996.969001	14.329638	1.331277
-1000.704587	17.833060	1.336282
-1004.394503	13.218035	1.341286
-1008.215713	18.879632	1.346291
-1011.882262	14.522633	1.351296
-1015.883966	8.967247	1.356301
-1019.816504	19.397614	1.361306
-1023.344906	19.400517	1.366310
-1027.380870	23.678930	1.371315
-1030.943916	19.250220	1.376320
-1034.707281	17.660287	1.381325
-1038.254559	18.886689	1.386330
-1042.135795	14.761175	1.391334
-1045.920982	21.170789	1.396339
-1049.137667	24.927163	1.401344
-1053.389129	26.967891	1.406349
-1057.284481	12.063962	1.411354
-1060.964381	17.939564	1.416358
-1064.788088	30.000376	1.421363
-1068.450136	21.336458	1.426368
-1072.496182	16.310187	1.431373
-1076.096210	23.598481	1.436378
-1079.673787	7.984664	1.441382
-1084.015548	21.801358	1.446387
-1087.723731	5.981385	1.451392
-1091.685386	23.773945	1.456397
-1095.044386	8.777994	1.461402
-1098.415432	19.476612	1.466406
-1102.646573	20.047738	1.471411
-1105.943243	30.351310	1.476416
-1109.795386	21.850320	1.481421
-1113.493866	16.836330	1.486426
-1116.913531	19.188783	1.491430
-1121.001374	19.017992	1.496435
-1125.017408	7.613530	1.501440
-1129.139894	17.740167	1.506445
-1132.437282	27.756906	1.511450
-1135.873120	17.675627	1.516454
-1140.160902	26.893678	1.521459
-1143.609121	9.124267	1.526464
-1147.511315	17.383436	1.531469
-1151.591018	25.869691	1.536474
-1155.259998	23.060167	1.541478
-1159.262560	24.555110	1.546483
-1162.011881	21.770348	1.551488
-1165.907890	17.880777	1.556493
-1169.749914	18.761903	1.561498
-1173.840596	21.871434	1.566502
-1177.793188	15.468033	1.571507
-1181.541920	15.451237	1.576512
-1185.416977	25.752834	1.581517
-1188.532165	19.846202	1.586522
-1192.262622	9.659203	1.591526
-1196.452394	18.065375	1.596531
-1200.033021	15.973432	1.601536
-1203.811629	17.237094	1.606541
-1207.685460	24.299753	1.611546
-1211.333220	14.955761	1.616550
-1215.215364	17.943696	1.621555
-1218.604813	16.447189	1.626560
-1222.853760	22.218560	1.631565
-1226.513206	21.530019	1.636570
-1230.207565	14.317484	1.641574
-1234.086954	20.105431	1.646579
-1237.724226	10.639970	1.651584
-1241.338701	22.729060	1.656589
-1245.215801	23.142878	1.661594
-1248.996869	11.980141	1.666598
-1252.633355	15.362452	1.671603
-1256.425300	10.081406	1.676608
-1260.545453	12.323825	1.681613
-1264.630873	21.716270	1.686618
-1267.800583	21.203293	1.691622
-1271.349571	28.997750	1.696627
-1275.007077	22.676596	1.701632
-1278.877131	16.441499	1.706637
-1282.964058	13.230753	1.711642
-1286.514893	26.913343	1.716646
-1290.674952	29.148011	1.721651
-1294.384620	17.649100	1.726656
-1297.953252	19.899508	1.731661
-1301.625757	11.975609	1.736666
-1305.374848	9.666386	1.741670
-1309.631336	20.429726	1.746675
-1312.691336	12.198103	1.751680
-1316.857968	24.511275	1.756685
-1320.755489	22.995315	1.761690
-1324.173051	5.287533	1.766694
-1327.739047	25.502180	1.771699
-1331.358169	18.228890	1.776704
-1335.296393	12.253941	1.781709
-1339.370786	17.179214	1.786714
-1342.884618	19.766242	1.791718
-1347.197551	11.098174	1.796723
-1350.470200	16.689855	1.801728
-1354.000958	10.171948	1.806733
-1358.424036	20.779126	1.811738
-1362.216773	17.973979	1.816742
-1366.503260	23.707463	1.821747
-1369.464963	7.150394	1.826752
-1373.069550	18.578978	1.831757
-1376.713542	23.069604	1.836762
-1380.255149	17.125854	1.841766
-1384.259235	24.649575	1.846771
-1388.060078	24.398625	1.851776
-1392.014142	23.309692	1.856781
-1395.964333	21.401782	1.861786
-1399.291527	15.661839	1.866790
-1403.475164	16.875554	1.871795
-1406.970443	20.833109	1.876800
-1410.844822	17.709983	1.881805
-1414.302079	16.585709	1.886810
-1417.990532	12.581355	1.891814
-1421.910725	16.264787	1.896819
-1425.924230	12.186338	1.901824
-1429.969653	16.602549	1.906829
-1433.732065	13.679137	1.911834
-1436.773049	11.658854	1.916838
-1440.424468	18.117046	1.921843
-1444.262411	7.514069	1.926848
-1448.264760	4.632251	1.931853
-1452.489747	13.971662	1.936858
-1456.075718	5.725117	1.941862
-1459.516869	18.538902	1.946867
-1462.868202	10.713650	1.951872
-1466.394228	17.694227	1.956877
-1470.801322	22.327673	1.961882
-1474.586162	18.873381	1.966886
-1478.547978	19.181316	1.971891
-1482.219622	15.689992	1.976896
-1486.073449	19.001815	1.981901
-1490.015351	15.181650	1.986906
-1493.560273	15.567925	1.991910
-1497.222463	25.127937	1.996915
-1501.020607	21.328032	2.006912
-1502.101496	12.844395	2.016909
-1499.921078	17.370679	2.026906
-1496.888658	26.173369	2.036902
-1494.831029	18.843376	2.046899
-1492.438575	18.196633	2.056896
-1491.188940	20.205323	2.066893
-1488.965862	21.140849	2.076890
-1487.090029	17.291291	2.086886
-1485.436306	23.163408	2.096883
-1483.292651	17.010087	2.106880
-1481.439722	4.250143	2.116877
-1479.355445	16.477571	2.126874
-1477.654777	13.352330	2.136870
-1475.602499	13.402654	2.146867
-1473.489003	17.964941	2.156864
-1471.819860	14.118491	2.166861
-1470.302197	16.223215	2.176858
-1468.613658	19.511544	2.186854
-1466.122979	14.212082	2.196851
-1464.024657	14.062428	2.206848
-1462.338345	15.994903	2.216845
-1460.839284	14.862857	2.226842
-1458.994380	24.496732	2.236838
-1457.076860	16.513463	2.246835
-1454.887603	17.369181	2.256832
-1452.629037	15.362440	2.266829
-1451.310878	18.686398	2.276826
-1449.247946	15.416342	2.286822
-1447.411204	19.448270	2.296819
-1445.556809	15.008536	2.306816
-1443.509897	17.925322	2.316813
-1441.762736	27.759586	2.326810
-1439.955026	17.605652	2.336806
-1438.425641	23.210365	2.346803
-1435.882422	21.890645	2.356800
-1434.114034	16.744742	2.366797
-1432.396438	24.169716	2.376794
-1430.350106	21.004957	2.386790
-1428.447695	22.001352	2.396787
-1426.715333	19.330511	2.406784
-1424.812143	26.528427	2.416781
-1423.040400	21.402519	2.426778
-1421.051130	21.047746	2.436774
-1419.082611	20.573149	2.446771
-1417.509420	16.123194	2.456768
-1415.519969	19.274977	2.466765
-1413.635010	17.883830	2.476762
-1411.505853	18.572382	2.486758
-1409.866153	16.841581	2.496755
-1407.884650	20.065691	2.506752
-1406.143002	17.137608	2.516749
-1404.077951	16.668095	2.526746
-1402.228648	19.714440	2.536742
-1400.346768	13.569941	2.546739
-1398.487148	14.446904	2.556736
-1396.500250	14.637228	2.566733
-1394.765308	22.114715	2.576730
-1393.033579	18.687740	2.586726
-1391.288382	16.780603	2.596723
-1388.940685	22.552759	2.606720
-1386.907708	15.179436	2.616717
-1385.380641	18.001081	2.626714
-1383.459732	19.995531	2.636710
-1381.753417	11.536166	2.646707
-1379.755685	16.394948	2.656704
-1377.746165	22.901725	2.666701
-1375.956438	17.090918	2.676698
-1374.108486	22.826251	2.686694
-1372.355829	25.832833	2.696691
-1370.367594	11.259325	2.706688
-1368.397503	13.277491	2.716685
-1366.523609	21.231669	2.726682
-1364.489566	23.747987	2.736678
-1362.801046	17.105557	2.746675
-1361.000569	22.093819	2.756672
-1359.067056	18.947178	2.766669
-1357.389794	19.744425	2.776666
-1355.497422	16.983292	2.786662
-1353.188528	16.899500	2.796659
-1351.185095	8.957822	2.806656
-1349.529927	16.631256	2.816653
-1347.838208	13.966978	2.826650
-1345.976195	11.202819	2.836646
-1344.247419	9.637794	2.846643
-1342.062588	5.642584	2.856640
-1340.185984	5.231709	2.866637
-1338.529943	9.374746	2.876634
-1336.745862	5.680507	2.886630
-1334.622172	9.366623	2.896627
-1332.592451	5.846214	2.906624
-1331.046273	8.713779	2.916621
-1329.080552	7.357140	2.926618
-1327.030754	3.970881	2.936614
-1325.205832	9.212605	2.946611
-1323.555695	1.922715	2.956608
-1321.560814	6.448870	2.966605
-1319.872658	7.329656	2.976602
-1317.583619	6.702802	2.986598
-1315.949726	10.795722	2.996595
-1313.800064	4.873678	3.006592
-1312.034054	7.197691	3.016589
-1310.187373	7.794186	3.026586
-1308.515901	7.419323	3.036582
-1306.538544	4.794619	3.046579
-1304.582247	1.271776	3.056576
-1302.465921	4.783849	3.066573
-1300.701261	5.748715	3.076570
-1298.972299	10.947402	3.086566
-1297.316624	6.747990	3.096563
-1295.169090	3.324014	3.106560
-1293.457907	5.153168	3.116557
-1291.492537	4.016074	3.126554
-1289.746596	10.457748	3.136550
-1287.706727	-0.020572	3.146547
-1285.750692	2.172006	3.156544
-1283.680782	3.478006	3.166541
-1282.135965	10.553407	3.176538
-1280.178169	7.777129	3.186534
-1278.479151	6.444265	3.196531
-1276.753526	3.782507	3.206528
-1274.520164	9.609391	3.216525
-1272.765775	8.483971	3.226522
-1271.007759	15.288441	3.236518
-1269.016091	2.842728	3.246515
-1267.029843	7.177697	3.256512
-1264.869732	11.053827	3.266509
-1263.614747	14.545891	3.276506
-1261.478140	16.390673	3.286502
-1259.708388	6.874473	3.296499
-1257.580221	11.870377	3.306496
-1255.686975	11.316390	3.316493
-1253.728841	13.530766	3.326490
-1252.297298	18.718669	3.336486
-1250.311821	20.976038	3.346483
-1248.200419	16.313762	3.356480
-1246.401427	10.260005	3.366477
-1244.691932	10.799563	3.376474
-1243.084265	15.913503	3.386470
-1240.639571	9.266993	3.396467
-1238.723119	9.250846	3.406464
-1236.783150	11.390780	3.416461
-1235.477475	15.215776	3.426458
-1233.328564	12.546314	3.436454
-1231.405159	7.037885	3.446451
-1229.570133	7.634730	3.456448
-1227.419172	3.231390	3.466445
-1225.715517	13.015954	3.476442
-1223.974940	13.163740	3.486438
-1222.243092	14.399161	3.496435
-1220.164365	14.912814	3.506432
-1218.180212	6.562250	3.516429
-1216.418501	11.380002	3.526426
-1214.599120	10.446317	3.536422
-1212.730569	14.204949	3.546419
-1210.848483	19.420261	3.556416
-1208.662766	10.341186	3.566413
-1206.970476	15.817376	3.576410
-1205.106224	18.957802	3.586406
-1203.469400	14.772519	3.596403
-1201.089821	11.753571	3.606400
-1199.519459	6.045880	3.616397
-1197.809829	11.014074	3.626394
-1195.874319	12.354289	3.636390
-1193.903708	9.276052	3.646387
-1191.992210	12.988360	3.656384
-1190.193827	10.307128	3.666381
-1188.237360	5.653906	3.676378
-1186.450998	10.306697	3.686374
-1184.682100	9.791608	3.696371
-1182.527034	17.397831	3.706368
-1180.567871	7.622448	3.716365
-1178.876639	5.537799	3.726362
-1177.064116	10.955304	3.736358
-1175.426815	12.696903	3.746355
-1173.156843	6.023154	3.756352
-1171.139889	3.924293	3.766349
-1169.631058	5.528565	3.776346
-1167.574732	8.426728	3.786342
-1165.708562	8.339744	3.796339
-1163.883762	1.538290	3.806336
-1161.932780	4.601721	3.816333
-1160.105677	13.886628	3.826330
-1158.332061	12.881365	3.836326
-1156.297327	7.356762	3.846323
-1154.361078	2.465241	3.856320
-1152.536582	8.559748	3.866317
-1150.485227	12.107624	3.876314
-1148.897539	7.920765	3.886310
-1147.036092	11.757952	3.896307
-1145.307912	10.428413	3.906304
-1143.101402	4.484792	3.916301
-1141.373412	5.962451	3.926298
-1139.533823	2.879958	3.936294
-1137.559428	12.477614	3.946291
-1135.795192	10.330793	3.956288
-1133.782342	12.931229	3.966285
-1131.899701	11.807501	3.976282
-1130.219559	8.030571	3.986278
-1128.392165	7.832986	3.996275
-1126.060407	9.986127	4.006272
-1124.189258	5.734996	4.016269
-1122.871874	-0.292153	4.026266
-1121.020997	6.745460	4.036262
-1118.778391	6.476729	4.046259
-1116.779611	4.000322	4.056256
-1115.207857	1.450128	4.066253
-1113.018536	1.638314	4.076250
-1111.200127	6.904942	4.086246
-1109.385626	7.164138	4.096243
-1107.670841	0.108763	4.106240
-1105.557609	3.653095	4.116237
-1103.761216	5.879261	4.126234
-1101.957003	9.701957	4.136230
-1099.918410	5.817192	4.146227
-1098.244703	3.910653	4.156224
-1096.362622	5.666836	4.166221
-1094.460684	2.978585	4.176218
-1092.508137	5.320299	4.186214
-1090.535030	15.563951	4.196211
-1088.898429	9.121046	4.206208
-1086.728481	12.544230	4.216205
-1085.009849	11.101007	4.226202
-1083.502796	18.198388	4.236198
-1081.297699	13.612842	4.246195
-1079.336499	12.909192	4.256192
-1077.395038	16.559969	4.266189
-1075.684725	15.724356	4.276186
-1073.759893	11.740972	4.286182
-1072.057250	14.068994	4.296179
-1070.282063	7.704982	4.306176
-1068.218911	16.158065	4.316173
-1066.279824	16.353162	4.326170
-1064.285258	15.440518	4.336166
-1062.375652	11.626934	4.346163
-1060.703719	10.731159	4.356160
-1058.845428	11.594400	4.366157
-1056.783357	12.219804	4.376154
-1055.023809	16.466496	4.386150
-1053.145056	10.842193	4.396147
-1051.423063	3.787279	4.406144
-1049.287969	17.110632	4.416141
-1047.584001	10.619087	4.426138
-1046.002115	9.887713	4.436134
-1043.658688	21.082643	4.446131
-1041.715242	10.372045	4.456128
-1040.133132	4.536266	4.466125
-1037.866782	11.954320	4.476122
-1036.301345	15.600536	4.486118
-1034.461637	7.366362	4.496115
-1032.451724	13.237125	4.506112
-1030.689668	16.643495	4.516109
-1028.575467	10.940508	4.526106
-1026.980368	13.724679	4.536102
-1024.967912	15.925829	4.546099
-1022.994898	13.297314	4.556096
-1021.327755	16.797812	4.566093
-1019.677794	13.434701	4.576090
-1017.262634	21.583669	4.586086
-1015.420683	12.813920	4.596083
-1013.989233	14.988000	4.606080
-1011.838672	11.947445	4.616077
-1009.851964	14.496912	4.626074
-1008.311700	14.124299	4.636070
-1006.316568	8.876130	4.646067
-1004.452374	14.217629	4.656064
-1002.267035	13.623454	4.666061
-1000.379596	10.673929	4.676058
-998.767750	17.904603	4.686054
-996.856545	18.061587	4.696051
-995.256445	12.661872	4.706048
-993.354324	14.463881	4.716045
-991.042215	11.173317	4.726042
-989.157259	11.021896	4.736038
-987.548891	15.202822	4.746035
-985.411321	13.013782	4.756032
-983.872505	14.070264	4.766029
-981.892790	16.908222	4.776026
-980.030525	24.504633	4.786022
-978.221591	15.345479	4.796019
-975.854391	15.630080	4.806016
-974.259097	19.137366	4.816013
-972.710461	18.945004	4.826010
-970.556661	14.509854	4.836006
-968.644425	17.415452	4.846003
-966.957719	19.217192	4.856000
-965.122705	14.752498	4.865997
-962.913046	21.053990	4.875994
-961.326748	14.038193	4.885990
-959.280871	11.128099	4.895987
-957.428417	20.677540	4.905984
-955.749235	18.242891	4.915981
-953.738005	17.933949	4.925978
-951.809704	15.194228	4.935974
-949.662784	22.945665	4.945971
-948.027786	7.072708	4.955968
-946.133104	15.129718	4.965965
-944.395321	25.425351	4.975962
-942.532410	15.804464	4.985958
-940.675607	17.920057	4.995955
-938.668863	18.671245	5.005952
-936.762422	12.788408	5.015949
-935.095638	21.014490	5.025946
-933.044233	14.038026	5.035942
-931.283266	22.435356	5.045939
-929.206261	25.584628	5.055936
-927.341180	21.558806	5.065933
-925.475561	14.318387	5.075930
-923.661391	17.942284	5.085926
-921.888432	18.134063	5.095923
-919.663894	16.474297	5.105920
-918.064509	17.307996	5.115917
-916.311852	20.305462	5.125914
-914.577235	20.157611	5.135910
-912.517801	21.051967	5.145907
-910.369338	17.719751	5.155904
-908.580559	25.965825	5.165901
-906.769556	14.005527	5.175898
-904.950286	24.959173	5.185894
-903.033866	18.159037	5.195891
-901.209164	19.744568	5.205888
-899.412039	11.880425	5.215885
-897.288253	14.535963	5.225882
-895.644391	15.556764	5.235878
-893.508624	13.585973	5.245875
-891.913032	21.891361	5.255872
-889.746032	16.644226	5.265869
-888.031546	19.470986	5.275866
-886.337641	26.657057	5.285862
-884.435521	15.091127	5.295859
-882.367821	26.186646	5.305856
-880.361998	18.756487	5.315853
-878.567309	12.589999	5.325850
-876.863405	24.354689	5.335846
-874.790322	25.041647	5.345843
-873.164736	17.568074	5.355840
-871.138412	23.256379	5.365837
-869.195900	26.544039	5.375834
-867.294436	20.025774	5.385830
-865.615382	22.049850	5.395827
-863.780046	16.895225	5.405824
-861.821700	24.451120	5.415821
-859.850511	18.700083	5.425818
-857.871098	23.739102	5.435814
-856.042037	22.155241	5.445811
-854.247279	21.293658	5.455808
-852.502170	21.199435	5.465805
-850.584833	21.543440	5.475802
-848.539526	16.118438	5.485798
-846.583625	15.524767	5.495795
-844.864773	13.849592	5.505792
-842.992957	22.273486	5.515789
-840.996461	15.264821	5.525786
-839.616898	14.796434	5.535782
-837.354895	19.641890	5.545779
-835.381597	23.489883	5.555776
-833.609128	16.535977	5.565773
-831.702791	16.881756	5.575770
-829.900059	22.785825	5.585766
-828.111214	25.338660	5.595763
-825.867747	15.829119	5.605760
-824.253299	26.184040	5.615757
-822.180240	12.339405	5.625754
-820.632721	24.004410	5.635750
-818.686358	27.525167	5.645747
-816.643780	17.244111	5.655744
-814.829652	24.531015	5.665741
-812.935206	16.447703	5.675738
-811.022656	29.843203	5.685734
-809.373090	22.706862	5.695731
-807.312302	13.160225	5.705728
-805.641311	20.061091	5.715725
-803.430407	17.732604	5.725722
-801.894893	19.836507	5.735718
-799.908347	23.999760	5.745715
-797.881284	21.801706	5.755712
-795.737710	23.948948	5.765709
-794.172538	16.691906	5.775706
-792.488349	24.631132	5.785702
-790.464306	13.748365	5.795699
-788.620181	12.812630	5.805696
-786.776368	19.722205	5.815693
-784.809687	11.576848	5.825690
-782.701240	8.630062	5.835686
-781.222319	45.542272	5.845683
-779.390758	17.412996	5.855680
-777.270753	15.419565	5.865677
-775.520270	8.796036	5.875674
-773.547675	17.617540	5.885670
-771.756183	22.257222	5.895667
-769.839564	14.549320	5.905664
-767.855709	8.889486	5.915661
-765.974603	26.969734	5.925658
-764.255343	14.116354	5.935654
-762.497153	2.196174	5.945651
-760.691250	24.349217	5.955648
-758.424348	26.361531	5.965645
-756.219798	-1.756255	5.975642
-754.863516	23.451071	5.985638
-753.072053	17.537798	5.995635
-751.148625	14.607974	6.005632
-749.088623	6.463522	6.015629
-747.293133	15.351242	6.025626
-745.461421	9.729947	6.035622
-743.360336	20.152417	6.045619
-741.698068	14.660824	6.055616
-739.656419	17.444889	6.065613
-737.887127	17.334255	6.075610
-736.119141	9.460670	6.085606
-734.391202	18.296045	6.095603
-732.181234	14.381037	6.105600
-730.361753	14.175552	6.115597
-728.695182	13.424541	6.125594
-726.570525	14.226539	6.135590
-724.527775	13.265431	6.145587
-722.998671	10.641780	6.155584
-720.974200	10.569326	6.165581
-719.207620	19.853245	6.175578
-717.369360	12.260528	6.185574
-715.340120	11.210013	6.195571
-713.472928	19.773698	6.205568
-711.550749	22.092175	6.215565
-709.796041	15.329074	6.225562
-707.988433	18.927354	6.235558
-706.104644	22.071389	6.245555
-704.218065	23.476675	6.255552
-702.186155	15.032026	6.265549
-700.172156	19.100986	6.275546
-698.563261	20.746421	6.285542
-696.798296	29.283831	6.295539
-694.999357	14.507360	6.305536
-692.641205	12.106504	6.315533
-691.016797	23.407243	6.325530
-689.027699	10.447642	6.335526
-687.334410	12.837444	6.345523
-685.260356	21.655452	6.355520
-683.401424	7.943022	6.365517
-681.669928	14.925889	6.375514
-680.063155	14.028161	6.385510
-677.806208	14.965372	6.395507
-676.130284	19.432556	6.405504
-674.114611	6.917114	6.415501
-672.129701	15.376768	6.425498
-670.190818	10.456776	6.435494
-668.336376	16.111152	6.445491
-666.685578	16.030554	6.455488
-664.719083	8.538958	6.465485
-662.889172	13.565720	6.475482
-660.816524	21.450881	6.485478
-659.068684	13.923172	6.495475
-657.421709	17.371904	6.505472
-655.603349	24.159352	6.515469
-653.612240	16.327535	6.525466
-651.588917	14.777526	6.535462
-649.716967	27.341299	6.545459
-647.686813	14.312011	6.555456
-645.748097	22.441201	6.565453
-643.966325	12.745066	6.575450
-642.551229	17.962845	6.585446
-640.378331	24.925756	6.595443
-638.537724	30.181347	6.605440
-636.587579	12.641461	6.615437
-634.668201	19.744343	6.625434
-632.674539	14.656165	6.635430
-630.732194	11.516584	6.645427
-629.368096	19.598646	6.655424
-627.382292	22.871703	6.665421
-625.453135	21.485169	6.675418
-623.561192	14.131819	6.685414
-621.461736	16.630458	6.695411
-619.716835	16.819052	6.705408
-617.721006	17.367009	6.715405
-615.783670	11.151076	6.725402
-614.222468	15.710837	6.735398
-612.198821	14.618674	6.745395
-610.244583	11.063554	6.755392
-608.555274	3.944680	6.765389
-606.393099	15.797429	6.775386
-604.483737	16.741291	6.785382
-603.146985	14.066340	6.795379
-601.032550	9.064678	6.805376
-599.079753	25.084301	6.815373
-596.909044	5.895636	6.825370
-595.590654	22.597612	6.835366
-593.635187	10.222885	6.845363
-591.405989	22.484923	6.855360
-589.624352	12.916730	6.865357
-587.789491	16.978091	6.875354
-585.989498	21.285009	6.885350
-584.306294	15.335465	6.895347
-582.375590	28.502508	6.905344
-580.146551	16.827724	6.915341
-578.273056	27.425656	6.925338
-576.562468	25.423590	6.935334
-574.780351	26.457270	6.945331
-572.842033	19.740714	6.955328
-571.008145	19.521998	6.965325
-569.004195	26.057259	6.975322
-566.986171	17.434942	6.985318
-565.133018	23.651682	6.995315
-563.468276	19.160794	7.005312
-561.549966	27.105440	7.015309
-559.845863	25.477028	7.025306
-557.837506	19.478723	7.035302
-555.835588	28.182076	7.045299
-554.011058	25.375561	7.055296
-551.810628	28.415470	7.065293
-550.564151	18.904355	7.075290
-548.705415	31.715058	7.085286
-546.429914	22.759543	7.095283
-544.605707	26.765805	7.105280
-542.760702	32.355489	7.115277
-541.063012	16.336937	7.125274
-538.806742	22.033030	7.135270
-537.327950	25.560815	7.145267
-535.329299	18.889911	7.155264
-533.438935	26.966932	7.165261
-531.157248	16.395286	7.175258
-529.670758	24.311037	7.185254
-527.751254	23.871851	7.195251
-525.762641	19.166642	7.205248
-524.208757	18.121158	7.215245
-522.344236	19.076984	7.225242
-520.223214	28.159218	7.235238
-518.202167	22.244173	7.245235
-516.408362	25.170647	7.255232
-514.747851	20.704148	7.265229
-512.748745	21.223252	7.275226
-510.963808	24.231667	7.285222
-508.914178	15.640660	7.295219
-507.082779	18.134847	7.305216
-505.147021	14.399613	7.315213
-503.523924	19.080613	7.325210
-501.666965	23.378502	7.335206
-499.561956	20.505132	7.345203
-497.460029	19.904216	7.355200
-496.262573	16.882116	7.365197
-494.201324	21.660511	7.375194
-492.104616	26.651128	7.385190
-490.069041	16.541951	7.395187
-488.302832	15.336275	7.405184
-486.421128	15.545750	7.415181
-484.491969	24.731282	7.425178
-482.879189	17.271040	7.435174
-480.974651	24.647993	7.445171
-479.093068	19.078914	7.455168
-476.965429	16.775072	7.465165
-475.261025	21.296277	7.475162
-473.227661	13.716779	7.485158
-471.355949	15.925101	7.495155
-469.644533	14.833972	7.505152
-467.800074	26.567094	7.515149
-465.938181	13.149567	7.525146
-464.041077	22.371812	7.535142
-462.033495	13.699141	7.545139
-460.197775	16.787900	7.555136
-458.410295	24.404602	7.565133
-456.281057	11.621718	7.575130
-454.581637	21.661803	7.585126
-452.873370	31.806265	7.595123
-450.908035	20.026857	7.605120
-448.449195	22.597735	7.615117
-447.092019	33.102982	7.625114
-445.142960	22.838710	7.635110
-443.624870	23.598879	7.645107
-441.782637	13.544293	7.655104
-439.555259	26.465166	7.665101
-437.141481	21.674771	7.675098
-435.886182	26.210879	7.685094
-434.130782	21.685073	7.695091
-432.230465	20.628541	7.705088
-430.024582	23.482970	7.715085
-428.361116	18.682919	7.725082
-426.601689	16.786836	7.735078
-424.352495	28.913242	7.745075
-422.631411	19.026421	7.755072
-420.919802	17.401644	7.765069
-418.916657	21.373122	7.775066
-417.407024	23.162487	7.785062
-415.052090	19.927200	7.795059
-413.286223	23.256084	7.805056
-411.166291	19.576773	7.815053
-409.782734	17.672823	7.825050
-407.862873	10.834610	7.835046
-405.749760	16.395806	7.845043
-403.870690	18.754577	7.855040
-401.768003	12.024539	7.865037
-400.333307	13.679045	7.875034
-398.431968	15.508509	7.885030
-396.360121	11.516383	7.895027
-394.342615	16.371321	7.905024
-392.718619	16.917258	7.915021
-390.906425	21.609202	7.925018
-389.252649	15.096095	7.935014
-387.035600	16.860956	7.945011
-384.948967	10.356112	7.955008
-383.223399	7.953920	7.965005
-381.300722	10.932549	7.975002
-379.669101	16.109615	7.984998
-377.570703	9.121350	7.994995
-375.886868	11.260275	8.004992
-373.799284	15.846691	8.014989
-371.871016	14.245778	8.024986
-370.407902	-0.907900	8.034982
-368.565631	8.953135	8.044979
-366.202591	8.274335	8.054976
-364.441597	6.518565	8.064973
-362.966826	9.383988	8.074970
-361.070613	14.911960	8.084966
-358.694387	12.854308	8.094963
-356.824620	16.862919	8.104960
-355.041486	14.858899	8.114957
-353.253305	17.506940	8.124954
-351.369504	22.441680	8.134950
-349.686466	14.046675	8.144947
-347.553854	19.715334	8.154944
-345.594852	23.640242	8.164941
-343.881755	15.183604	8.174938
-342.029013	17.112445	8.184934
-340.108533	14.543387	8.194931
-338.324554	12.836068	8.204928
-336.509345	6.764567	8.214925
-334.670913	19.499755	8.224922
-332.669229	20.364367	8.234918
-330.709610	24.922308	8.244915
-328.918721	17.847384	8.254912
-326.812809	14.214591	8.264909
-325.172964	14.110716	8.274906
-323.311954	21.088989	8.284902
-321.424746	15.394399	8.294899
-319.271358	17.273689	8.304896
-317.573564	11.683544	8.314893
-315.782601	19.487689	8.324890
-313.861542	15.407601	8.334886
-311.792844	20.698099	8.344883
-310.126604	11.554269	8.354880
-308.486159	12.089744	8.364877
-306.423706	22.067267	8.374874
-304.404981	21.080350	8.384870
-302.578617	17.226950	8.394867
-300.466583	22.141092	8.404864
-298.847767	15.156808	8.414861
-296.750249	26.210259	8.424858
-294.793862	13.188257	8.434854
-293.680584	17.904997	8.444851
-291.465616	15.502118	8.454848
-289.440713	9.187192	8.464845
-287.684196	12.122950	8.474842
-285.668166	19.343337	8.484838
-283.687970	14.661764	8.494835
-282.050162	18.473790	8.504832
-280.327404	12.601807	8.514829
-278.044814	28.310185	8.524826
-276.272497	14.902335	8.534822
-274.639961	20.712452	8.544819
-272.572012	17.051028	8.554816
-270.481191	15.590030	8.564813
-268.678254	18.513659	8.574810
-267.092141	16.286952	8.584807
-265.233918	17.717641	8.594803
-263.179744	21.660586	8.604800
-261.613532	12.880096	8.614797
-259.320351	11.819416	8.624794
-257.653057	18.048708	8.634791
-255.184867	7.141237	8.644787
-253.637863	12.887654	8.654784
-251.917981	14.398849	8.664781
-250.002909	13.463255	8.674778
-248.302205	14.655428	8.684775
-246.409604	15.944864	8.694771
-244.495589	10.598137	8.704768
-242.399749	10.809943	8.714765
-240.709328	11.782723	8.724762
-238.841439	2.823062	8.734759
-237.080815	16.530693	8.744755
-235.428839	21.862504	8.754752
-232.710048	14.783240	8.764749
-231.195810	9.220865	8.774746
-229.386100	7.621617	8.784743
-227.819648	4.005529	8.794739
-225.749341	7.721732	8.804736
-223.867706	10.170233	8.814733
-221.881025	6.913376	8.824730
-219.975135	4.607251	8.834727
-218.135832	1.364444	8.844723
-216.354623	1.495436	8.854720
-214.446624	3.481869	8.864717
-212.667583	11.883225	8.874714
-210.653535	11.606036	8.884711
-208.838533	11.016422	8.894707
-206.848008	4.737046	8.904704
-204.902955	2.347319	8.914701
-202.932149	10.080226	8.924698
-201.202786	14.204521	8.934695
-199.744660	14.429711	8.944691
-197.781712	9.637280	8.954688
-195.663185	8.536639	8.964685
-193.740819	3.946467	8.974682
-191.932262	13.479903	8.984679
-190.009092	12.666213	8.994675
-188.275600	12.023310	9.004672
-186.269875	5.289972	9.014669
-184.366944	10.715975	9.024666
-182.691204	1.930688	9.034663
-180.699693	9.497689	9.044659
-178.546930	8.511593	9.054656
-176.929103	9.012874	9.064653
-174.943647	5.015769	9.074650
-173.374269	10.239230	9.084647
-171.554811	8.597419	9.094643
-169.375920	9.997541	9.104640
-167.360170	8.161791	9.114637
-165.659825	9.085676	9.124634
-163.630471	8.826609	9.134631
-161.798242	11.371458	9.144627
-160.002524	5.424760	9.154624
-158.305939	13.420923	9.164621
-156.309989	8.691149	9.174618
-154.260291	22.033808	9.184615
-152.207054	5.504034	9.194611
-150.732286	9.591624	9.204608
-149.062601	15.549054	9.214605
-146.826314	15.290140	9.224602
-144.977386	11.313262	9.234599
-143.152025	3.787731	9.244595
-141.209972	7.387113	9.254592
-139.434289	8.894223	9.264589
-137.441353	11.625018	9.274586
-135.534049	12.738522	9.284583
-133.749957	0.394615	9.294579
-131.932836	22.784904	9.304576
-130.007346	13.661392	9.314573
-128.174603	17.374537	9.324570
-126.301152	15.946763	9.334567
-124.061050	12.955847	9.344563
-122.478771	9.390978	9.354560
-120.646931	14.634180	9.364557
-119.081369	9.437868	9.374554
-117.153567	19.208121	9.384551
-115.146637	7.395476	9.394547
-112.867643	13.326773	9.404544
-111.085809	8.556987	9.414541
-109.494124	18.003524	9.424538
-107.540308	16.826611	9.434535
-105.732690	8.724495	9.444531
-103.816881	12.397566	9.454528
-101.786991	16.472414	9.464525
-99.794899	2.930149	9.474522
-97.917960	12.806418	9.484519
-96.082849	8.703893	9.494515
-94.724985	7.836786	9.504512
-92.584831	17.053741	9.514509
-90.590191	4.777314	9.524506
-88.783116	12.594862	9.534503
-86.905197	13.855190	9.544499
-84.840939	14.173218	9.554496
-82.800958	-0.278198	9.564493
-81.296657	6.945061	9.574490
-79.526267	12.794904	9.584487
-77.520865	7.858433	9.594483
-75.695907	19.574487	9.604480
-73.447530	5.364549	9.614477
-71.600599	14.591985	9.624474
-70.231705	15.830901	9.634471
-68.050681	14.114121	9.644467
-66.245901	19.740610	9.654464
-64.546108	8.758525	9.664461
-62.526879	17.626927	9.674458
-60.327193	17.321830	9.684455
-58.516039	12.223737	9.694451
-57.067068	16.456023	9.704448
-55.070850	16.126548	9.714445
-52.798760	15.680441	9.724442
-50.979429	8.182773	9.734439
-49.723929	15.652574	9.744435
-47.711577	16.855177	9.754432
-45.431039	12.406915	9.764429
-43.431329	5.826214	9.774426
-41.637654	11.588693	9.784423
-40.048369	12.441967	9.794419
-38.093807	9.253531	9.804416
-36.303620	15.496544	9.814413
-34.106268	9.564809	9.824410
-32.298109	13.242480	9.834407
-30.722644	9.396139	9.844403
-28.596122	10.135310	9.854400
-26.837320	8.817471	9.864397
-24.839275	8.877705	9.874394
-23.302140	3.013394	9.884391
-21.099748	10.671635	9.894387
-19.145399	13.151331	9.904384
-17.489510	13.071946	9.914381
-15.553670	14.176259	9.924378
-13.713522	12.799668	9.934375
-11.958519	12.623957	9.944371
-10.275831	11.416158	9.954368
-8.209154	12.363828	9.964365
-6.032438	7.679545	9.974362
-4.286038	10.860275	9.984359
-3.016893	38.908313	9.994355
-2.125987	83.155848	10.004352
-1.070890	142.957594	10.014349
0.000000	202.372162	10.019354
0.567979	243.022851	10.024359
1.235843	298.093925	10.029363
1.884902	326.410291	10.034368
2.254681	366.553649	10.039373
2.236683	386.455100	10.044378
2.721447	418.142404	10.049383
2.602125	429.488161	10.054387
3.583345	450.595915	10.059392
3.306546	475.844975	10.064397
3.571246	477.521564	10.069402
3.859566	491.296989	10.074407
3.844759	503.908145	10.079411
3.697887	512.792108	10.084416
3.908305	514.447397	10.089421
3.652293	535.213303	10.094426
4.317177	532.204204	10.099431
4.440405	539.498175	10.104435
4.789098	567.399314	10.109440
4.552951	565.431165	10.114445
4.570787	558.051607	10.119450
4.796170	568.959312	10.124455
4.388484	583.780929	10.129459
4.928601	564.764149	10.134464
4.730847	569.701409	10.139469
4.527314	578.482490	10.144474
4.878579	576.702919	10.149479
4.701572	579.673639	10.154483
4.859871	569.437989	10.159488
4.553062	597.175658	10.164493
4.798631	586.095052	10.169498
5.155314	589.612992	10.174503
4.974699	591.910954	10.179507
4.935196	590.368741	10.184512
4.545367	592.867221	10.189517
4.973425	598.750166	10.194522
5.081431	615.601036	10.199527
5.287467	630.039399	10.204531
5.459172	614.227232	10.209536
5.066280	647.149383	10.214541
5.520999	616.320957	10.219546
5.171085	647.974734	10.224551
5.319571	631.734179	10.229555
5.289074	623.914456	10.234560
5.267199	652.146086	10.239565
5.743057	613.847652	10.244570
5.655645	657.882412	10.249575
5.406066	633.286248	10.254579
5.445177	672.256362	10.259584
5.831747	658.735816	10.264589
5.518584	693.643295	10.269594
5.659141	668.541737	10.274599
5.625043	695.647914	10.279603
5.892141	676.507379	10.284608
5.519314	690.076210	10.289613
5.747621	686.734598	10.294618
6.328176	707.144983	10.299623
6.240008	735.133465	10.304627
6.728497	709.627847	10.309632
6.254965	689.138890	10.314637
6.072533	701.554608	10.319642
6.259535	694.491767	10.324647
6.198965	712.590163	10.329651
6.542930	725.560597	10.334656
6.403176	737.162160	10.339661
6.627239	732.886104	10.344666
6.700583	738.406219	10.349671
6.588214	739.212598	10.354675
6.987771	737.945688	10.359680
6.755764	735.836510	10.364685
6.521583	738.250268	10.369690
6.708870	745.491550	10.374695
6.717994	757.452575	10.379699
6.762470	750.229515	10.384704
6.408388	757.495645	10.389709
6.673651	757.101687	10.394714
6.779110	759.395049	10.399719
6.658926	762.219551	10.404723
7.021608	740.693582	10.409728
7.122514	784.268194	10.414733
7.281774	784.859369	10.419738
7.389772	774.712021	10.424743
7.397081	789.421929	10.429747
7.539274	766.757859	10.434752
7.307922	748.920412	10.439757
7.301697	769.402393	10.444762
7.455126	773.917869	10.449767
7.209819	773.540686	10.454771
7.453402	797.401623	10.459776
7.307926	785.746157	10.464781
7.351504	786.024629	10.469786
7.643196	792.247939	10.474791
7.493322	792.167765	10.479795
7.759271	798.105031	10.484800
7.568781	793.256421	10.489805
7.715950	792.521758	10.494810
7.782662	797.041610	10.499815
7.715205	799.788325	10.504819
7.791153	798.908906	10.509824
7.846718	825.229910	10.514829
7.717320	837.101132	10.519834
7.970980	835.871675	10.524839
8.075320	839.863577	10.529843
8.332834	813.150422	10.534848
7.931705	840.121443	10.539853
8.148979	848.591150	10.544858
8.295744	837.418881	10.549863
8.068166	843.330799	10.554867
8.487909	837.271540	10.559872
8.494362	837.316242	10.564877
8.310726	841.727803	10.569882
8.523749	841.905137	10.574887
8.356768	851.779670	10.579891
8.432222	855.333066	10.584896
8.300940	857.779317	10.589901
8.735566	875.832056	10.594906
9.328749	870.989319	10.599911
8.727539	873.256634	10.604915
8.924968	879.870326	10.609920
8.701943	886.249883	10.614925
8.893485	884.593520	10.619930
9.027109	877.368795	10.624935
8.849636	874.897667	10.629939
9.104600	875.380544	10.634944
8.852526	875.428631	10.639949
9.057758	878.816258	10.644954
9.391938	880.838200	10.649959
9.107374	888.364539	10.654963
9.328984	879.216118	10.659968
9.194099	869.929020	10.664973
9.391841	901.855546	10.669978
9.562882	878.461311	10.674983
9.494820	906.681880	10.679987
9.711426	884.242298	10.684992
9.119259	892.451624	10.689997
9.484677	890.120987	10.695002
9.401527	905.592906	10.700007
9.518006	903.472279	10.705011
9.777447	916.820637	10.710016
9.740423	934.850901	10.715021
9.758770	918.102508	10.720026
9.946032	932.755478	10.725031
9.508333	915.666664	10.730035
9.838316	942.469234	10.735040
9.805033	917.994206	10.740045
9.785802	943.447425	10.745050
10.019360	918.653874	10.750055
9.972183	928.736430	10.755059
10.392799	929.959280	10.760064
10.154426	941.171462	10.765069
10.574238	935.017536	10.770074
10.177018	929.041225	10.775079
10.270336	944.824083	10.780083
10.470048	932.019052	10.785088
10.409774	938.615524	10.790093
10.450106	932.761815	10.795098
10.784511	931.994130	10.800103
10.225968	946.963177	10.805107
10.582378	943.550613	10.810112
10.439920	953.102762	10.815117
10.645817	940.750895	10.820122
10.442592	941.685314	10.825127
10.653577	976.880460	10.830131
10.699159	943.426333	10.835136
10.760218	970.021111	10.840141
10.297387	970.131196	10.845146
10.927237	973.596203	10.850151
10.732478	964.157746	10.855155
10.941340	981.696272	10.860160
10.798715	968.171529	10.865165
11.006989	975.549927	10.870170
11.107468	1005.041629	10.875175
11.376780	1000.982204	10.880179
11.586466	989.031813	10.885184
11.132758	1004.786862	10.890189
11.240072	1022.694868	10.895194
11.767002	1005.283370	10.900199
11.456612	996.673881	10.905203
11.334475	1029.465407	10.910208
11.648743	1007.637683	10.915213
11.571839	1012.415471	10.920218
11.883494	1006.825964	10.925223
11.642449	1001.206336	10.930227
11.996681	1028.115584	10.935232
11.626206	991.433463	10.940237
11.590753	1014.449866	10.945242
11.687227	1004.577006	10.950247
11.551960	1025.335393	10.955251
11.875167	987.509751	10.960256
11.752697	1034.310892	10.965261
11.269584	1018.486025	10.970266
11.327269	1010.898032	10.975271
11.805511	1002.176957	10.980275
11.924593	1048.917544	10.985280
12.146954	1037.409791	10.990285
12.111746	1053.916583	10.995290
12.159314	1028.504382	11.000295
12.074209	1062.898562	11.005299
12.499288	1030.355111	11.010304
12.201428	1059.243404	11.015309
12.601557	1041.173999	11.020314
12.850832	1020.816873	11.025319
12.476634	1057.307174	11.030323
12.722761	1049.088290	11.035328
12.543992	1046.115870	11.040333
12.649256	1041.346163	11.045338
12.808077	1048.752986	11.050343
12.775796	1051.000554	11.055347
12.729461	1059.805739	11.060352
13.119142	1055.112093	11.065357
12.914917	1056.327375	11.070362
13.169471	1045.162986	11.075367
12.690826	1066.766247	11.080371
13.167317	1050.881342	11.085376
12.785400	1035.213781	11.090381
12.633107	1068.259362	11.095386
13.104079	1033.721627	11.100391
13.018217	1087.681171	11.105395
13.427785	1079.871442	11.110400
13.169935	1084.974579	11.115405
13.156295	1076.169482	11.120410
13.321085	1089.268167	11.125415
13.245583	1091.920026	11.130419
13.229902	1072.699489	11.135424
13.678431	1088.132540	11.140429
13.234988	1082.182460	11.145434
13.257453	1084.982697	11.150439
13.571184	1086.079106	11.155443
13.588949	1066.528391	11.160448
13.610814	1092.341170	11.165453
13.702868	1075.659688	11.170458
13.775558	1072.355422	11.175463
13.689393	1082.567305	11.180467
13.624967	1094.223371	11.185472
14.518257	1108.703994	11.190477
13.807984	1095.670210	11.195482
13.757647	1094.575948	11.200487
13.967564	1110.523317	11.205491
14.283487	1110.756784	11.210496
14.326627	1114.157702	11.215501
14.468098	1113.472819	11.220506
14.713522	1101.412556	11.225511
14.227972	1090.489170	11.230515
14.156145	1087.572225	11.235520
14.651283	1102.384424	11.240525
14.356833	1092.944434	11.245530
14.694793	1085.576631	11.250535
14.323439	1090.737295	11.255539
14.541803	1086.520393	11.260544
14.603424	1112.266943	11.265549
14.554646	1114.949237	11.270554
14.976483	1113.117348	11.275559
14.635255	1110.697527	11.280563
14.807524	1106.328698	11.285568
14.506347	1102.167841	11.290573
14.581528	1115.965239	11.295578
14.359147	1111.530039	11.300583
14.599113	1117.561467	11.305587
14.666127	1105.666850	11.310592
14.403757	1115.157804	11.315597
14.736970	1130.946760	11.320602
15.423613	1134.353865	11.325607
15.167238	1149.495702	11.330611
15.201331	1145.729218	11.335616
15.327619	1137.351201	11.340621
15.427874	1134.033063	11.345626
15.579023	1148.157422	11.350631
15.475294	1145.685525	11.355635
15.275303	1151.530090	11.360640
15.213982	1132.695222	11.365645
15.307331	1139.841298	11.370650
15.720485	1146.256704	11.375655
15.396227	1152.504288	11.380659
15.693013	1138.759496	11.385664
15.753264	1137.111428	11.390669
15.753597	1142.745844	11.395674
15.863627	1151.633381	11.400679
15.691675	1150.605818	11.405683
15.630006	1137.208356	11.410688
15.699652	1145.886286	11.415693
15.645788	1147.678416	11.420698
15.859204	1152.189175	11.425703
15.996865	1174.471745	11.430707
15.907869	1163.183861	11.435712
16.059709	1184.857056	11.440717
16.107395	1176.460012	11.445722
16.480852	1168.119829	11.450727
16.087136	1173.998452	11.455731
16.328997	1159.972239	11.460736
16.132261	1169.479570	11.465741
16.357277	1173.608437	11.470746
16.505503	1160.235826	11.475751
16.307502	1165.520258	11.480755
16.417574	1162.064930	11.485760
16.566299	1176.180242	11.490765
16.780933	1167.797579	11.495770
16.956646	1168.037639	11.500775
16.743466	1168.076368	11.505779
17.091368	1157.934646	11.510784
17.060402	1161.870945	11.515789
16.663642	1168.675728	11.520794
16.933631	1167.292252	11.525799
16.848549	1167.264820	11.530803
16.572068	1182.165468	11.535808
16.789336	1177.160233	11.540813
16.624693	1181.020085	11.545818
16.965637	1178.964546	11.550823
16.947490	1183.127466	11.555827
17.115671	1203.375663	11.560832
17.129490	1206.997324	11.565837
17.496010	1204.259607	11.570842
17.807673	1209.732433	11.575847
17.585129	1209.220718	11.580851
17.516566	1181.707328	11.585856
17.838517	1177.732501	11.590861
17.684685	1172.578292	11.595866
17.759708	1168.198146	11.600871
17.338346	1174.205758	11.605875
17.228857	1169.407180	11.610880
17.243245	1178.305255	11.615885
17.162144	1206.629413	11.620890
17.509963	1207.666779	11.625895
17.657631	1192.685722	11.630899
17.695437	1210.310154	11.635904
17.467323	1217.009214	11.640909
17.790097	1219.156028	11.645914
18.104912	1206.346592	11.650919
17.884001	1216.867067	11.655923
17.867353	1222.442721	11.660928
18.390550	1223.007413	11.665933
18.353495	1226.345454	11.670938
18.287013	1211.642961	11.675943
18.019029	1213.666369	11.680947
18.104038	1212.575743	11.685952
18.329809	1230.301111	11.690957
18.054805	1236.819999	11.695962
18.544425	1245.281199	11.700967
18.440517	1238.163563	11.705971
18.701142	1232.553724	11.710976
19.085717	1239.308047	11.715981
18.912799	1231.141698	11.720986
18.893661	1204.877225	11.725991
18.667352	1202.697681	11.730995
18.638110	1208.934510	11.736000
18.537423	1201.849495	11.741005
18.616729	1217.996011	11.746010
19.380558	1212.550356	11.751015
18.987212	1216.628043	11.756019
18.894133	1202.926443	11.761024
19.086362	1207.618796	11.766029
18.914087	1208.302288	11.771034
18.979955	1226.390623	11.776039
19.058605	1223.883318	11.781043
19.403329	1224.706711	11.786048
19.208114	1228.218211	11.791053
19.248858	1231.569076	11.796058
19.736909	1222.765881	11.801063
19.248093	1217.989936	11.806067
19.311252	1231.585934	11.811072
19.447765	1227.369429	11.816077
19.178839	1225.904737	11.821082
19.401231	1229.105206	11.826087
19.164206	1229.652368	11.831091
19.571588	1221.500711	11.836096
19.746661	1227.629268	11.841101
19.289376	1232.795802	11.846106
19.744050	1230.354684	11.851111
19.505723	1240.242435	11.856115
19.318169	1235.831604	11.861120
19.480740	1240.025644	11.866125
19.587609	1251.252391	11.871130
20.243126	1255.194352	11.876135
19.920130	1271.793022	11.881139
20.248610	1267.758782	11.886144
20.185604	1261.295363	11.891149
20.319814	1255.658367	11.896154
20.315286	1242.868288	11.901159
20.080878	1279.973950	11.906163
20.073244	1263.295535	11.911168
20.515392	1251.593286	11.916173
20.332088	1267.756507	11.921178
20.319778	1263.073288	11.926183
20.406766	1257.759216	11.931187
20.610091	1243.187128	11.936192
20.669372	1263.889599	11.941197
20.557055	1265.826685	11.946202
20.816151	1247.803170	11.951207
20.657299	1269.898208	11.956211
20.520276	1257.690649	11.961216
20.734476	1256.115788	11.966221
20.723811	1252.624500	11.971226
20.929792	1254.906642	11.976231
20.797298	1256.712902	11.981235
20.951821	1255.912389	11.986240
20.947416	1258.901451	11.991245
20.982095	1262.844655	11.996250
21.085329	1259.932872	12.001255
20.835635	1267.390766	12.006259
20.658082	1268.699584	12.011264
20.725555	1265.937007	12.016269
20.947133	1272.830884	12.021274
21.199347	1284.886042	12.026279
21.027971	1286.659083	12.031283
21.034005	1278.743291	12.036288
21.395466	1288.600076	12.041293
21.220953	1297.581968	12.046298
21.292530	1268.953219	12.051303
21.610647	1291.677128	12.056307
21.580225	1283.737186	12.061312
21.562322	1265.425084	12.066317
21.399168	1263.336386	12.071322
21.649276	1246.653154	12.076327
21.406860	1254.135112	12.081331
21.304163	1262.372238	12.086336
21.371103	1251.821092	12.091341
21.167278	1254.865610	12.096346
21.269481	1253.515194	12.101351
21.087590	1266.308204	12.106355
21.410451	1260.967552	12.111360
21.465307	1253.990171	12.116365
21.286847	1250.531951	12.121370
21.228564	1252.876738	12.126375
21.344658	1258.722976	12.131379
21.483036	1260.281032	12.136384
21.627301	1243.094284	12.141389
21.086251	1240.083405	12.146394
21.430604	1231.653209	12.151399
21.378498	1217.270118	12.156403
21.112830	1240.334634	12.161408
21.239004	1219.856512	12.166413
20.917967	1229.800025	12.171418
21.660658	1222.017519	12.176423
21.227558	1224.915669	12.181427
21.069471	1211.465704	12.186432
20.925400	1233.269745	12.191437
20.995491	1208.120143	12.196442
21.038129	1227.022745	12.201447
21.277938	1238.223549	12.206451
21.363227	1237.940286	12.211456
21.299147	1241.698959	12.216461
21.574009	1216.983468	12.221466
21.541342	1224.723698	12.226471
21.327192	1227.448157	12.231475
21.570936	1233.915853	12.236480
21.616280	1206.964572	12.241485
21.128478	1241.167930	12.246490
21.473894	1234.809700	12.251495
21.532169	1223.879906	12.256499
21.380584	1221.455052	12.261504
21.509548	1234.819783	12.266509
21.315383	1233.051428	12.271514
21.269219	1187.561762	12.276519
21.171196	1214.505639	12.281523
21.259807	1206.731260	12.286528
21.300073	1198.527776	12.291533
20.737633	1202.140413	12.296538
21.071300	1222.179318	12.301543
21.214255	1224.168729	12.306547
21.315798	1234.871182	12.311552
21.285848	1226.215253	12.316557
21.225112	1245.784075	12.321562
21.624808	1218.587024	12.326567
21.114003	1222.555710	12.331571
21.058415	1219.588839	12.336576
21.396028	1200.493139	12.341581
21.513082	1230.674946	12.346586
21.390585	1187.862528	12.351591
21.277715	1202.916878	12.356595
21.210955	1210.736656	12.361600
21.532371	1205.129748	12.366605
21.135866	1206.613828	12.371610
21.122270	1198.969295	12.376615
21.409128	1201.512922	12.381619
21.211415	1213.718624	12.386624
21.564119	1198.774248	12.391629
21.204625	1209.267933	12.396634
21.292199	1204.294412	12.401639
21.366982	1210.104640	12.406643
21.190525	1206.067365	12.411648
21.367916	1203.774553	12.416653
21.086355	1212.850736	12.421658
20.957035	1204.936071	12.426663
21.288763	1211.949548	12.431667
21.308857	1217.115637	12.436672
21.438539	1204.830894	12.441677
21.206586	1216.110073	12.446682
21.441772	1204.842994	12.451687
21.380668	1212.690257	12.456691
21.466008	1200.048311	12.461696
21.493734	1212.071400	12.466701
21.163911	1219.362275	12.471706
21.226786	1192.865544	12.476711
21.477205	1202.727364	12.481715
21.086796	1199.888012	12.486720
21.345768	1180.826958	12.491725
21.330026	1175.204445	12.496730
21.479862	1177.820383	12.501735
21.380107	1181.600500	12.506739
21.330430	1188.097624	12.511744
21.235555	1184.482586	12.516749
21.171088	1186.372607	12.521754
21.289962	1184.324098	12.526759
21.229347	1186.517858	12.531763
20.931508	1196.924430	12.536768
21.074781	1189.836784	12.541773
20.924276	1180.864214	12.546778
21.381441	1183.252943	12.551783
21.648166	1178.233512	12.556787
21.390234	1172.384696	12.561792
21.302008	1169.747895	12.566797
20.937273	1185.727070	12.571802
21.247640	1177.210862	12.576807
21.201531	1184.442279	12.581811
20.922884	1178.052712	12.586816
21.207460	1185.281854	12.591821
20.980123	1190.794903	12.596826
20.933270	1197.925520	12.601831
21.014504	1202.558301	12.606835
20.926233	1212.269137	12.611840
21.124513	1222.535104	12.616845
21.343128	1227.779924	12.621850
21.746760	1205.671143	12.626855
21.343810	1210.780118	12.631859
21.290283	1208.374320	12.636864
21.589681	1194.375167	12.641869
21.448112	1190.283447	12.646874
21.483659	1180.631497	12.651879
21.271817	1173.718765	12.656883
21.406548	1193.082878	12.661888
21.406972	1183.841806	12.666893
20.490585	1200.599686	12.671898
21.145074	1159.440675	12.676903
21.054270	1209.831227	12.681907
21.200402	1188.586715	12.686912
21.145654	1184.347108	12.691917
20.997658	1199.818645	12.696922
21.240028	1176.437785	12.701927
21.076444	1204.473894	12.706931
21.126830	1189.532010	12.711936
21.214650	1180.500932	12.716941
21.218910	1207.202977	12.721946
21.462944	1191.126332	12.726951
21.303408	1192.151570	12.731955
21.302325	1198.704027	12.736960
21.249364	1199.124061	12.741965
21.307480	1195.803168	12.746970
21.244043	1178.939782	12.751975
21.192300	1213.128725	12.756979
21.323312	1190.232384	12.761984
21.182520	1193.560153	12.766989
21.205260	1202.084748	12.771994
21.129773	1192.426844	12.776999
21.087030	1199.470073	12.782003
21.489611	1188.777134	12.787008
21.387478	1193.704086	12.792013
21.398693	1202.498603	12.797018
21.475793	1198.659014	12.802023
21.317675	1201.219989	12.807027
21.422840	1192.925734	12.812032
21.245967	1209.168289	12.817037
21.527455	1198.972475	12.822042
21.594456	1187.101447	12.827047
21.413885	1197.893020	12.832051
21.094072	1199.841112	12.837056
21.400649	1186.017443	12.842061
21.097540	1173.708708	12.847066
21.559660	1163.679654	12.852071
20.942821	1190.767729	12.857075
20.669837	1185.621480	12.862080
21.561469	1176.899030	12.867085
20.869526	1212.172518	12.872090
21.145766	1203.786317	12.877095
21.542592	1205.497116	12.882099
21.613989	1199.245681	12.887104
21.776452	1179.047259	12.892109
21.137482	1177.037610	12.897114
21.109595	1167.711178	12.902119
21.107591	1170.747147	12.907123
21.048977	1162.540530	12.912128
21.461743	1162.203464	12.917133
20.822000	1185.928374	12.922138
21.004226	1178.765134	12.927143
21.234795	1186.774025	12.932147
21.381678	1201.231857	12.937152
21.210184	1189.676408	12.942157
21.181644	1172.744385	12.947162
21.610269	1171.710926	12.952167
21.166609	1183.241464	12.957171
20.855466	1176.965890	12.962176
21.319915	1172.003238	12.967181
21.090089	1181.287195	12.972186
21.217747	1172.068418	12.977191
20.965384	1181.114693	12.982195
21.115969	1204.700975	12.987200
21.427839	1193.908957	12.992205
21.096299	1209.941213	12.997210
21.385664	1206.231775	13.002215
21.316101	1199.878239	13.007219
21.205129	1199.776088	13.012224
21.148080	1190.425906	13.017229
21.178274	1202.394977	13.022234
21.213025	1189.037283	13.027239
20.911879	1181.123225	13.032243
21.145374	1208.029988	13.037248
21.351550	1203.876498	13.042253
21.431309	1216.884781	13.047258
21.645943	1203.600887	13.052263
21.284580	1191.137424	13.057267
21.077574	1183.038040	13.062272
21.297976	1175.750441	13.067277
20.894783	1187.369146	13.072282
21.254593	1178.849782	13.077287
21.180216	1192.070283	13.082291
21.009087	1187.330415	13.087296
21.386690	1194.833311	13.092301
21.116426	1196.617381	13.097306
21.282317	1192.099731	13.102311
21.031037	1193.365106	13.107315
21.199202	1219.787144	13.112320
21.598034	1201.266734	13.117325
21.326174	1196.870937	13.122330
21.169022	1177.092500	13.127335
21.334417	1184.380073	13.132339
21.446332	1190.419339	13.137344
21.463079	1165.043351	13.142349
20.903055	1180.960626	13.147354
21.250213	1186.699021	13.152359
21.388722	1184.372989	13.157363
21.228564	1194.937375	13.162368
21.141912	1192.371282	13.167373
21.270000	1193.554078	13.172378
21.275980	1184.493471	13.177383
21.364370	1189.334843	13.182387
21.210103	1192.202710	13.187392
21.240728	1187.552092	13.192397
20.756228	1193.421547	13.197402
21.061796	1189.720567	13.202407
21.011356	1185.093918	13.207411
21.030883	1187.435747	13.212416
21.166853	1179.131855	13.217421
21.086236	1212.860199	13.222426
21.654956	1207.100308	13.227431
21.321999	1201.946271	13.232435
21.317250	1195.631287	13.237440
21.624049	1193.751503	13.242445
21.148728	1197.992069	13.247450
21.033611	1191.890232	13.252455
21.223555	1197.593779	13.257459
20.957787	1188.882440	13.262464
21.437620	1191.311710	13.267469
21.122801	1207.797038	13.272474
21.518877	1182.399949	13.277479
21.331551	1188.690366	13.282483
21.122455	1198.493002	13.287488
21.492183	1189.685043	13.292493
21.193440	1192.864536	13.297498
21.171318	1191.997580	13.302503
21.539993	1201.976159	13.307507
20.949054	1184.911462	13.312512
21.223298	1215.162786	13.317517
21.195977	1196.383914	13.322522
21.212430	1188.646284	13.327527
21.109466	1198.515573	13.332531
21.114190	1212.234414	13.337536
21.375773	1175.708066	13.342541
20.829845	1221.844061	13.347546
21.050659	1195.511373	13.352551
21.143734	1199.394784	13.357555
20.925229	1201.350374	13.362560
20.923412	1206.557801	13.367565
20.977674	1212.759237	13.372570
21.413883	1224.796040	13.377575
21.302401	1220.554432	13.382579
21.377137	1220.296506	13.387584
21.470885	1213.336596	13.392589
21.016791	1198.923016	13.397594
20.932719	1193.677249	13.402599
21.088463	1215.586414	13.407603
21.051132	1229.166896	13.412608
21.313818	1236.405863	13.417613
21.276295	1233.084445	13.422618
21.820223	1232.959851	13.427623
21.769407	1212.938900	13.432627
21.172991	1205.398351	13.437632
21.163610	1201.189352	13.442637
20.999939	1213.394355	13.447642
21.042738	1208.719712	13.452647
21.112346	1200.265541	13.457651
21.250194	1198.940984	13.462656
20.981793	1220.006314	13.467661
21.095803	1214.274783	13.472666
21.316337	1209.243785	13.477671
20.969045	1208.617922	13.482675
21.247126	1220.776135	13.487680
21.504429	1221.436850	13.492685
21.200088	1219.589873	13.497690
21.404377	1218.295720	13.502695
21.301258	1207.524143	13.507699
21.547849	1210.905254	13.512704
21.712269	1195.109386	13.517709
21.573948	1209.428206	13.522714
21.364250	1217.687102	13.527719
21.408843	1205.382813	13.532723
21.179965	1204.633986	13.537728
21.407400	1206.338683	13.542733
20.990878	1202.539970	13.547738
21.053150	1222.395075	13.552743
21.518045	1205.704444	13.557747
21.584363	1204.692495	13.562752
21.673396	1202.420082	13.567757
21.279187	1197.969679	13.572762
21.111497	1179.421375	13.577767
20.964840	1178.126423	13.582771
20.805602	1194.667350	13.587776
21.251023	1206.253234	13.592781
21.298791	1207.557651	13.597786
21.702799	1209.440771	13.602791
21.141402	1194.277903	13.607795
20.845526	1190.660226	13.612800
21.315516	1190.809200	13.617805
21.263542	1213.066881	13.622810
21.392347	1205.795452	13.627815
21.352908	1185.728569	13.632819
20.950610	1184.939592	13.637824
21.109941	1192.817920	13.642829
21.335796	1205.512732	13.647834
21.385007	1203.402790	13.652839
21.360138	1184.593580	13.657843
20.901926	1185.016742	13.662848
21.407763	1187.342515	13.667853
21.191137	1204.870323	13.672858
21.349695	1186.903918	13.677863
21.114381	1181.169763	13.682867
21.019047	1185.619386	13.687872
21.039915	1179.787604	13.692877
20.864152	1205.401868	13.697882
21.004257	1221.532383	13.702887
21.170039	1197.532918	13.707891
21.049852	1219.989146	13.712896
21.240100	1216.636137	13.717901
21.027583	1214.430738	13.722906
20.851779	1215.545305	13.727911
21.133047	1214.278299	13.732915
21.322098	1216.424362	13.737920
21.232646	1216.872293	13.742925
21.152530	1219.140132	13.747930
21.136460	1216.471314	13.752935
21.409566	1216.519222	13.757939
21.242724	1208.966934	13.762944
21.136004	1201.195324	13.767949
21.302195	1234.291418	13.772954
21.412956	1215.063142	13.777959
21.677815	1212.871497	13.782963
21.055996	1216.804270	13.787968
21.553162	1218.760844	13.792973
21.662366	1220.310933	13.797978
21.533163	1222.042547	13.802983
21.257179	1205.476381	13.807987
21.168870	1195.596590	13.812992
21.207551	1186.109718	13.817997
21.056458	1191.536490	13.823002
21.179502	1189.309118	13.828007
21.326812	1193.297419	13.833011
20.877477	1190.093727	13.838016
21.006499	1204.598565	13.843021
20.824294	1219.094705	13.848026
21.140956	1221.917436	13.853031
21.357408	1230.439540	13.858035
21.196853	1223.185865	13.863040
21.462576	1217.228286	13.868045
21.611378	1232.463287	13.873050
21.454941	1226.338062	13.878055
21.397990	1205.788239	13.883059
21.082828	1197.004346	13.888064
21.412811	1190.697482	13.893069
21.196002	1190.082350	13.898074
21.245343	1186.548392	13.903079
21.267146	1195.265522	13.908083
21.037253	1185.003039	13.913088
21.217495	1196.810980	13.918093
20.940047	1195.970551	13.923098
20.695115	1208.496018	13.928103
21.385933	1212.992161	13.933107
21.232234	1226.051877	13.938112
21.473504	1220.303202	13.943117
21.411563	1220.820864	13.948122
21.084973	1204.792630	13.953127
21.336690	1196.724160	13.958131
20.807032	1215.752711	13.963136
21.329026	1205.878084	13.968141
21.187189	1216.928424	13.973146
21.189434	1228.261725	13.978151
21.519198	1223.514503	13.983155
21.219459	1212.239688	13.988160
21.409933	1199.948409	13.993165
21.108376	1192.657311	13.998170
21.132722	1187.697033	14.003175
21.136521	1200.359445	14.008179
21.133571	1203.600577	14.013184
21.603141	1210.528992	14.018189
21.409235	1204.220548	14.023207
21.346548	1198.758282	14.028224
21.363969	1182.160982	14.033242
21.030275	1201.471711	14.038259
21.210447	1216.334022	14.043277
21.205990	1187.564058	14.048295
20.823317	1205.142931	14.053312
21.672558	1199.656345	14.058330
21.172941	1236.410772	14.063347
21.592357	1212.155150	14.068365
21.071728	1209.701024	14.073383
21.016140	1227.779863	14.078400
21.363261	1232.218406	14.083418
21.413123	1242.412578	14.088435
21.230034	1235.641934	14.093453
21.287997	1244.585897	14.098471
21.669677	1228.510869	14.103488
21.719415	1224.193069	14.108506
21.417591	1250.336369	14.113523
21.579163	1232.135212	14.118541
21.391842	1234.227217	14.123559
21.193265	1242.348545	14.128576
21.633214	1240.878459	14.133594
21.216213	1244.323651	14.138611
21.761646	1233.693210	14.143629
21.429548	1250.584560	14.148647
21.415914	1244.293375	14.153664
21.481448	1234.415836	14.158682
21.413814	1258.497421	14.163699
21.644808	1288.225502	14.168717
22.028340	1280.370366	14.173735
21.840559	1280.707039	14.178752
21.884787	1263.915044	14.183770
21.379722	1285.648815	14.188787
21.967506	1263.521198	14.193805
21.988507	1259.873328	14.198823
22.051312	1276.179509	14.203840
22.245233	1267.761617	14.208858
21.627071	1257.519641	14.213875
21.801470	1265.205565	14.218893
21.518363	1275.237368	14.223911
21.638075	1284.939107	14.228928
21.785106	1255.698131	14.233946
21.863625	1284.942460	14.238963
21.812654	1270.303280	14.243981
21.997953	1259.024001	14.248999
21.833089	1296.909624	14.254016
22.412079	1279.535274	14.259034
21.929184	1287.272555	14.264051
22.045262	1279.208401	14.269069
22.021201	1275.240540	14.274087
21.705832	1276.583800	14.279104
22.137280	1290.446614	14.284122
22.264304	1282.946975	14.289139
21.902266	1283.954775	14.294157
21.882859	1299.884003	14.299175
22.020997	1301.266618	14.304192
22.202680	1316.290805	14.309210
22.229285	1311.501637	14.314227
22.254579	1330.747420	14.319245
22.843022	1316.201266	14.324263
22.502659	1301.515403	14.329280
22.668752	1314.439037	14.334298
22.379272	1288.803610	14.339315
22.101317	1278.777909	14.344333
22.352941	1298.074066	14.349351
22.532301	1300.694313	14.354368
22.396919	1287.784668	14.359386
22.330485	1297.797662	14.364403
22.546525	1301.189097	14.369421
22.808586	1304.670717	14.374439
22.468307	1297.207846	14.379456
22.671168	1283.819564	14.384474
22.856923	1277.976316	14.389491
22.389564	1273.196728	14.394509
22.193071	1286.734987	14.399527
22.373015	1282.346071	14.404544
22.553044	1269.254013	14.409562
22.385388	1318.717046	14.414579
22.734437	1304.316043	14.419597
22.439692	1305.031554	14.424615
22.525553	1301.104355	14.429632
22.572964	1301.537220	14.434650
22.644274	1307.407118	14.439667
22.423127	1303.178111	14.444685
22.798882	1291.185772	14.449703
22.495088	1311.734510	14.454720
23.045161	1296.532282	14.459738
22.762363	1314.666340	14.464755
22.524272	1306.710562	14.469773
23.043526	1307.579387	14.474791
22.727993	1299.368561	14.479808
22.636663	1321.379306	14.484826
22.842028	1325.022550	14.489843
23.006113	1316.489843	14.494861
22.900678	1319.449655	14.499879
22.883734	1347.572089	14.504896
23.632777	1315.082777	14.509914
22.734327	1326.512011	14.514931
22.806639	1302.690677	14.519949
23.240041	1317.273618	14.524967
23.149434	1335.738831	14.529984
23.323740	1325.195825	14.535002
23.196158	1313.939662	14.540019
22.854726	1310.670462	14.545037
22.973729	1331.247750	14.550055
22.949365	1331.413650	14.555072
23.272571	1321.874039	14.560090
23.351143	1322.866627	14.565107
23.028035	1339.605642	14.570125
23.916137	1315.682497	14.575143
23.375155	1347.728086	14.580160
23.653998	1322.110497	14.585178
23.347306	1299.276082	14.590195
23.382565	1310.773463	14.595213
23.742309	1294.871739	14.600231
23.418347	1319.027337	14.605248
23.659964	1293.467642	14.610266
23.683104	1290.253558	14.615283
23.424174	1294.271273	14.620301
23.510442	1315.451481	14.625319
23.206805	1305.137288	14.630336
23.296212	1306.862715	14.635354
23.442801	1311.366296	14.640371
23.288381	1304.026357	14.645389
23.408312	1288.900600	14.650407
23.081619	1304.946477	14.655424
23.517823	1314.059812	14.660442
23.685657	1325.572239	14.665459
23.645386	1331.466233	14.670477
24.104727	1326.350082	14.675495
23.692042	1320.794156	14.680512
23.825365	1311.102373	14.685530
23.812604	1294.912434	14.690547
23.945502	1316.486309	14.695565
23.760231	1309.343188	14.700583
23.488672	1309.221336	14.705600
23.827310	1293.450389	14.710618
23.688453	1304.176473	14.715635
23.643621	1315.755841	14.720653
23.885235	1329.398868	14.725671
23.886512	1327.463929	14.730688
23.975896	1326.773303	14.735706
23.868616	1334.977646	14.740723
24.091267	1336.930354	14.745741
24.218133	1328.447619	14.750759
24.033699	1333.507344	14.755776
23.950328	1304.260544	14.760794
23.988210	1303.210062	14.765811
23.869390	1331.348713	14.770829
24.302259	1327.145952	14.775847
24.078046	1325.106981	14.780864
24.080187	1339.009995	14.785882
24.407441	1329.466589	14.790899
23.958346	1308.029633	14.795917
24.240942	1334.300094	14.800935
24.434159	1323.279041	14.805952
24.396751	1315.034861	14.810970
24.115704	1298.664344	14.815987
23.893138	1308.829654	14.821005
24.187218	1323.824914	14.826023
24.278837	1318.523602	14.831040
24.470670	1319.399030	14.836058
24.332401	1341.483356	14.841075
24.311558	1327.740617	14.846093
24.820828	1324.148563	14.851111
24.130846	1318.586527	14.856128
24.668951	1306.826248	14.861146
24.497870	1319.828827	14.866163
24.305302	1286.991119	14.871181
24.282289	1318.183292	14.876199
24.240572	1315.243802	14.881216
24.535071	1316.131170	14.886234
24.631892	1358.071192	14.891251
24.547400	1312.148058	14.896269
24.547727	1323.901119	14.901287
24.578572	1328.611919	14.906304
24.420231	1327.210501	14.911322
24.591350	1333.747154	14.916339
24.333575	1339.686850	14.921357
24.260179	1324.724016	14.926375
24.346266	1343.730471	14.931392
24.508105	1320.229869	14.936410
24.399238	1324.712850	14.941427
24.200382	1349.175720	14.946445
24.606645	1328.939335	14.951463
24.786395	1356.698525	14.956480
24.751139	1370.917406	14.961498
24.988859	1361.065801	14.966515
24.706549	1371.105408	14.971533
24.859783	1344.719758	14.976551
24.756564	1360.244011	14.981568
24.596615	1367.402890	14.986586
25.080256	1360.997744	14.991603
24.729270	1378.321672	14.996621
25.078888	1342.243585	15.001639
24.807320	1392.354197	15.006656
24.479981	1368.950407	15.011674
24.927831	1357.976804	15.016691
24.944456	1341.360574	15.021709
25.278495	1375.435784	15.026727
25.340977	1355.486986	15.031744
25.227089	1387.175125	15.036762
25.386038	1354.581640	15.041779
25.042242	1372.034970	15.046797
25.452472	1367.840527	15.051815
25.051946	1363.454500	15.056832
25.031146	1363.119631	15.061850
25.489188	1357.530216	15.066867
25.284506	1379.793498	15.071885
25.542543	1363.657819	15.076903
25.338450	1358.079624	15.081920
25.605120	1365.612465	15.086938
25.500625	1349.995495	15.091955
25.353550	1374.395096	15.096973
25.946554	1338.260902	15.101991
25.684324	1381.570099	15.107008
25.561623	1345.765522	15.112026
25.629671	1355.356004	15.117043
25.456717	1362.619196	15.122061
25.699559	1365.831774	15.127079
25.632173	1363.811830	15.132096
25.347461	1362.789197	15.137114
25.371147	1353.847869	15.142131
25.023152	1362.965181	15.147149
25.578081	1353.893514	15.152167
25.718264	1357.084712	15.157184
25.535398	1357.316787	15.162202
25.627305	1352.805042	15.167219
25.565274	1362.269988	15.172237
26.045664	1370.594552	15.177255
25.890247	1373.335840	15.182272
25.933028	1363.636439	15.187290
25.927310	1349.026141	15.192307
25.752347	1356.882656	15.197325
26.095847	1347.228112	15.202343
26.079179	1352.882407	15.207360
25.630125	1349.748334	15.212378
26.119667	1362.581104	15.217395
26.181954	1340.477404	15.222413
25.944531	1348.649030	15.227431
25.941836	1355.181953	15.232448
26.058222	1365.028990	15.237466
26.338034	1334.278659	15.242483
25.639951	1371.601456	15.247501
26.313475	1335.962492	15.252519
25.975309	1368.156672	15.257536
25.640924	1356.648750	15.262554
25.835112	1361.309917	15.267571
25.978792	1372.675230	15.272589
26.086081	1379.157592	15.277607
26.268477	1372.286126	15.282624
26.002253	1395.923004	15.287642
26.705266	1379.304227	15.292659
26.290874	1377.547252	15.297677
26.471855	1388.744614	15.302695
26.378625	1392.806713	15.307712
26.199599	1385.994453	15.312730
26.253703	1376.290092	15.317747
26.559938	1387.576012	15.322765
26.601486	1382.196149	15.327783
26.501226	1390.784780	15.332800
26.692262	1390.423991	15.337818
26.782378	1364.128593	15.342835
26.477681	1388.482572	15.347853
26.212622	1387.079291	15.352871
26.970016	1355.439530	15.357888
26.801102	1406.801626	15.362906
26.622365	1362.801366	15.367923
26.336111	1393.511887	15.372941
26.544836	1376.147710	15.377959
26.745216	1372.652095	15.382976
26.634659	1390.717883	15.387994
26.534777	1371.785922	15.393011
26.092493	1387.790552	15.398029
26.363316	1387.808706	15.403047
26.627079	1371.574582	15.408064
26.419869	1376.842439	15.413082
27.276020	1402.588991	15.418099
26.765688	1373.474634	15.423117
26.483482	1388.250420	15.428135
26.748878	1387.917096	15.433152
26.908121	1401.428616	15.438170
27.106306	1407.385282	15.443187
27.278513	1420.855428	15.448205
27.388749	1399.599685	15.453223
26.905787	1396.386068	15.458240
26.837549	1378.506084	15.463258
27.047400	1410.885083	15.468275
26.940756	1393.623088	15.473293
26.944910	1417.951455	15.478311
27.334912	1390.518119	15.483328
27.297630	1431.079803	15.488346
27.021101	1395.604791	15.493363
27.200238	1420.622527	15.498381
27.338609	1399.610826	15.503399
27.377946	1417.180852	15.508416
27.349890	1404.565434	15.513434
27.441701	1397.752445	15.518451
27.492840	1399.889810	15.523469
27.626843	1400.197189	15.528487
27.661240	1405.653032	15.533504
26.999038	1378.799639	15.538522
27.500301	1378.781043	15.543539
27.278465	1414.782215	15.548557
27.414179	1383.096826	15.553575
27.699538	1397.843453	15.558592
27.358660	1413.316006	15.563610
28.007488	1394.285062	15.568627
27.706936	1396.431325	15.573645
27.390925	1393.826561	15.578663
27.771293	1403.040090	15.583680
27.662989	1394.415504	15.588698
27.796627	1391.602183	15.593715
27.729987	1405.598024	15.598733
27.369624	1399.144999	15.603751
28.057162	1390.061600	15.608768
27.823933	1393.098434	15.613786
27.691984	1416.625845	15.618803
27.962703	1387.407347	15.623821
27.933734	1412.923856	15.628839
27.903167	1420.038533	15.633856
27.948145	1407.011931	15.638874
28.007592	1394.112017	15.643891
27.825075	1402.385024	15.648909
27.766512	1393.118601	15.653927
27.873109	1405.551603	15.658944
27.933460	1402.306393	15.663962
27.791066	1381.636783	15.668979
27.696089	1399.369775	15.673997
27.845265	1403.637028	15.679015
28.238649	1398.031169	15.684032
27.810789	1410.547837	15.689050
28.150833	1404.912731	15.694067
28.115766	1394.344866	15.699085
28.210096	1415.564832	15.704103
28.375491	1387.909354	15.709120
27.708047	1424.116888	15.714138
28.065923	1386.563506	15.719155
28.261391	1419.913764	15.724173
28.090399	1397.249454	15.729191
28.303857	1444.991090	15.734208
28.713032	1438.736208	15.739226
28.601756	1427.265005	15.744243
28.773770	1432.455102	15.749261
28.328190	1410.569137	15.754279
28.472407	1408.875650	15.759296
28.323415	1416.577050	15.764314
28.579797	1417.657687	15.769331
27.987569	1406.047706	15.774349
28.531990	1401.891626	15.779367
28.771141	1451.129792	15.784384
28.544250	1428.637937	15.789402
28.978843	1454.920556	15.794419
28.508124	1442.948260	15.799437
28.931318	1428.928552	15.804455
28.833117	1428.270983	15.809472
28.963193	1444.329108	15.814490
28.788552	1440.666777	15.819507
28.984756	1422.680073	15.824525
28.518538	1421.038319	15.829543
28.673416	1438.717356	15.834560
28.738214	1428.734413	15.839578
28.768592	1434.154730	15.844595
28.751549	1426.902926	15.849613
28.701185	1435.837543	15.854631
29.059529	1435.552315	15.859648
28.577081	1451.151301	15.864666
28.796405	1425.083715	15.869683
28.876015	1447.783091	15.874701
28.761295	1459.903809	15.879719
28.489541	1439.237445	15.884736
28.873596	1429.395489	15.889754
29.032425	1480.287167	15.894771
29.600274	1444.317165	15.899789
29.100476	1483.749437	15.904807
29.644479	1448.385675	15.909824
29.340419	1479.114947	15.914842
28.959428	1469.610469	15.919859
29.601014	1455.439507	15.924877
29.252790	1469.785472	15.929895
29.733887	1448.885777	15.934912
29.381674	1482.751370	15.939930
29.802630	1445.176765	15.944947
29.840727	1420.527020	15.949965
29.632550	1433.376747	15.954983
29.363987	1450.745816	15.960000
29.162626	1436.119441	15.965018
29.088801	1431.602643	15.970035
29.858969	1419.832006	15.975053
29.731792	1458.176065	15.980071
29.664042	1472.628309	15.985088
29.765290	1435.593909	15.990106
29.646071	1441.055389	15.995123
29.637280	1471.523632	16.000141
29.329859	1452.221984	16.005159
29.668043	1454.310434	16.010176
29.602271	1460.866049	16.015194
29.923367	1431.272926	16.020211
29.931564	1467.851002	16.025229
29.846887	1451.601573	16.030247
29.817298	1458.458145	16.035264
29.276948	1456.433394	16.040282
29.812929	1461.400295	16.045299
29.677170	1445.372943	16.050317
29.878072	1466.819799	16.055335
29.624779	1429.203331	16.060352
29.788642	1482.269627	16.065370
30.184142	1459.991486	16.070387
30.303074	1486.813698	16.075405
29.885005	1497.958820	16.080423
30.453981	1472.536934	16.085440
29.777953	1488.659172	16.090458
30.066007	1465.031245	16.095475
30.551367	1489.127267	16.100493
29.910973	1478.207579	16.105511
30.360066	1482.527696	16.110528
30.075185	1475.620593	16.115546
29.942494	1499.044441	16.120563
30.314209	1463.805643	16.125581
30.005932	1476.422842	16.130599
29.849179	1497.105689	16.135616
30.062070	1494.262407	16.140634
30.224427	1505.511592	16.145651
30.605030	1526.632585	16.150669
30.748267	1515.403859	16.155687
31.155083	1499.260033	16.160704
30.836333	1505.692422	16.165722
30.941929	1459.620532	16.170739
30.881441	1488.793064	16.175757
30.853315	1465.258031	16.180775
30.853387	1487.197825	16.185792
31.042786	1472.177199	16.190810
30.756077	1483.962009	16.195827
31.182811	1468.263338	16.200845
30.523655	1477.192826	16.205863
30.822757	1468.677822	16.210880
30.883769	1475.458608	16.215898
30.717984	1473.073682	16.220915
31.010259	1471.227592	16.225933
31.111194	1473.868243	16.230951
30.997290	1462.701014	16.235968
31.018586	1474.532649	16.240986
30.714656	1483.010674	16.246003
31.288978	1466.643549	16.251021
31.309074	1469.268777	16.256039
31.267101	1477.738056	16.261056
31.060086	1474.123349	16.266074
31.141789	1467.928544	16.271091
31.532394	1460.424529	16.276109
31.390272	1473.634978	16.281127
31.430092	1484.350003	16.286144
31.350088	1463.468986	16.291162
31.280431	1466.108528	16.296179
31.504576	1473.166879	16.301197
31.152051	1465.847439	16.306215
30.921991	1473.874820	16.311232
31.265545	1480.083603	16.316250
31.058851	1488.233103	16.321267
31.284076	1474.054594	16.326285
31.245142	1474.244841	16.331303
31.258327	1479.990376	16.336320
31.289686	1463.101105	16.341338
31.036509	1481.653776	16.346355
31.677391	1496.740196	16.351373
31.413632	1495.799151	16.356391
31.669303	1499.192178	16.361408
31.431673	1515.013304	16.366426
31.284562	1514.958116	16.371443
31.753331	1509.072787	16.376461
31.531813	1515.181371	16.381479
31.836094	1498.822670	16.386496
31.812832	1515.691815	16.391514
31.879430	1517.685166	16.396531
31.934852	1507.211322	16.401549
31.976854	1504.819994	16.406567
31.573085	1507.766075	16.411584
31.903300	1514.588888	16.416602
31.970077	1519.986130	16.421619
32.383743	1514.293625	16.426637
32.052401	1510.399871	16.431655
31.949697	1520.236337	16.436672
32.195981	1526.827156	16.441690
31.768145	1517.237311	16.446707
31.966116	1516.180159	16.451725
31.779833	1508.101179	16.456743
31.957173	1548.103590	16.461760
32.305893	1542.814676	16.466778
32.040290	1538.540780	16.471795
32.155048	1537.389935	16.476813
32.312725	1542.259898	16.481831
32.416447	1535.779989	16.486848
32.718167	1524.529127	16.491866
32.512074	1537.888258	16.496883
32.587405	1531.549728	16.501901
32.417122	1538.427203	16.506919
32.502033	1537.174154	16.511936
32.684082	1530.842200	16.516954
32.717818	1534.851059	16.521971
33.041039	1530.225294	16.526989
32.752666	1532.275256	16.532007
32.702922	1510.867115	16.537024
32.628296	1507.560039	16.542042
32.145473	1506.557978	16.547059
32.623657	1524.386900	16.552077
32.753323	1534.949212	16.557095
32.726484	1540.087693	16.562112
32.816624	1538.261246	16.567130
32.875843	1529.384927	16.572147
33.375614	1525.537945	16.577165
32.565637	1528.989245	16.582183
32.594758	1525.291251	16.587200
32.754805	1529.020423	16.592218
32.330806	1541.789837	16.597235
32.827880	1528.549460	16.602253
32.958757	1517.676623	16.607271
32.791293	1550.907316	16.612288
33.154216	1533.902167	16.617306
33.206769	1549.826485	16.622323
33.372203	1552.744720	16.627341
33.109678	1546.255576	16.632359
33.093618	1541.186854	16.637376
33.421585	1548.971131	16.642394
33.346212	1561.495421	16.647411
33.494227	1549.156169	16.652429
33.311932	1547.281936	16.657447
33.346744	1559.460685	16.662464
33.569377	1546.765839	16.667482
33.303072	1547.228294	16.672499
33.540658	1560.877689	16.677517
33.402426	1564.516016	16.682535
33.612999	1561.518939	16.687552
33.797992	1544.604286	16.692570
33.358213	1565.352028	16.697587
33.483615	1568.899551	16.702605
33.772046	1555.737253	16.707623
33.803040	1561.450880	16.712640
33.857079	1549.398740	16.717658
33.733416	1556.688774	16.722675
33.612231	1561.448276	16.727693
33.815750	1556.889569	16.732711
33.682883	1554.850154	16.737728
33.982550	1546.714103	16.742746
33.559219	1563.364756	16.747763
33.974417	1555.358923	16.752781
34.072404	1550.220101	16.757799
33.787522	1549.427135	16.762816
33.640453	1551.755004	16.767834
33.690360	1556.988213	16.772851
33.844750	1543.566526	16.777869
33.900714	1554.323071	16.782887
33.575178	1562.451454	16.787904
34.177301	1565.230839	16.792922
33.925878	1572.542828	16.797939
34.095963	1596.591783	16.802957
34.023401	1588.931912	16.807975
33.940541	1582.173433	16.812992
33.833889	1584.513737	16.818010
34.326285	1588.171047	16.823027
34.275240	1582.209716	16.828045
34.413782	1580.550147	16.833063
34.363671	1584.198021	16.838080
34.661617	1581.122513	16.843098
34.585799	1583.294310	16.848115
34.290719	1590.600686	16.853133
34.806114	1581.464401	16.858151
34.696799	1576.813222	16.863168
34.599836	1586.522978	16.868186
34.560515	1587.298438	16.873203
34.531518	1573.655864	16.878221
34.834888	1574.612619	16.883239
34.418626	1596.474259	16.888256
34.617715	1580.253362	16.893274
34.819165	1611.907434	16.898291
34.879564	1614.719739	16.903309
35.373706	1609.612098	16.908327
35.161700	1602.523430	16.913344
35.327646	1581.395385	16.918362
34.911737	1580.668929	16.923379
35.041321	1576.657607	16.928397
35.218952	1569.675126	16.933415
34.754128	1575.687260	16.938432
35.392824	1569.612791	16.943450
35.168917	1565.856041	16.948467
34.849876	1575.163917	16.953485
35.154899	1573.617794	16.958503
35.215489	1582.265827	16.963520
35.314911	1588.430223	16.968538
35.230396	1598.878878	16.973555
35.310255	1602.831637	16.978573
35.553755	1606.302135	16.983591
34.990734	1623.891398	16.988608
35.379336	1614.539364	16.993626
35.598745	1607.959179	16.998643
35.512903	1620.418337	17.003661
35.382116	1611.548674	17.008679
35.282167	1620.881412	17.013696
35.342493	1616.454845	17.018714
35.018424	1632.156178	17.023731
35.454638	1614.365337	17.028749
35.407120	1606.734495	17.033767
35.077053	1620.497281	17.038784
35.790587	1621.088188	17.043802
35.674399	1632.974910	17.048819
35.822659	1631.293336	17.053837
35.887394	1642.237306	17.058855
35.946878	1634.186700	17.063872
36.203242	1632.868550	17.068890
36.117579	1626.679919	17.073907
35.947715	1616.990666	17.078925
36.123299	1600.860009	17.083943
35.772915	1609.878757	17.088960
35.846281	1616.319447	17.093978
36.245609	1613.995382	17.098995
36.293929	1609.385119	17.104013
36.335472	1628.517025	17.109031
36.206469	1624.293677	17.114048
36.090467	1604.047393	17.119066
36.318707	1603.688532	17.124083
36.395418	1619.763228	17.129101
36.518913	1618.854795	17.134119
36.286859	1616.414348	17.139136
36.557244	1611.002626	17.144154
36.381560	1599.104267	17.149171
36.308011	1605.187719	17.154189
36.604041	1597.671977	17.159207
36.484328	1602.647543	17.164224
36.653018	1601.865608	17.169242
36.643100	1609.541786	17.174259
36.344203	1601.798456	17.179277
36.769709	1602.688546	17.184295
36.722524	1610.477630	17.189312
36.968612	1612.480121	17.194330
36.745408	1602.753767	17.199347
36.753429	1611.425931	17.204365
36.847569	1610.893405	17.209383
36.721548	1622.976737	17.214400
37.079255	1632.266386	17.219418
37.097755	1617.710154	17.224435
36.811579	1605.392121	17.229453
37.096295	1601.544811	17.234471
36.809928	1616.466206	17.239488
36.982639	1612.042166	17.244506
36.892190	1615.554912	17.249523
36.749878	1619.245812	17.254541
37.117026	1616.679920	17.259559
37.160902	1613.902893	17.264576
37.134016	1620.337551	17.269594
36.906060	1611.684726	17.274611
36.949171	1619.866819	17.279629
37.034011	1621.176171	17.284647
37.039361	1620.418711	17.289664
37.293694	1630.755150	17.294682
37.029824	1647.116993	17.299699
37.458309	1655.748870	17.304717
37.888178	1646.358776	17.309735
37.584495	1659.338761	17.314752
37.581525	1650.362176	17.319770
38.150905	1650.103064	17.324787
37.516113	1635.539316	17.329805
37.351981	1624.512103	17.334823
37.649495	1633.127102	17.339840
37.561370	1639.242779	17.344858
37.740067	1656.375603	17.349875
37.630798	1640.626949	17.354893
38.101538	1637.915548	17.359911
37.859555	1644.387664	17.364928
37.884999	1636.462032	17.369946
38.295928	1631.270130	17.374963
37.830857	1638.864756	17.379981
38.465298	1629.459351	17.384999
38.025407	1638.103863	17.390016
37.872031	1627.929065	17.395034
38.017191	1638.298650	17.400051
38.022871	1643.167719	17.405069
38.336953	1635.257404	17.410087
38.263999	1635.536447	17.415104
38.098897	1629.653059	17.420122
38.421298	1636.090221	17.425139
37.896804	1635.712979	17.430157
38.506058	1630.170132	17.435175
38.606420	1636.137775	17.440192
38.443111	1634.886552	17.445210
38.444677	1632.512662	17.450227
38.528768	1625.158117	17.455245
38.623424	1622.619949	17.460263
38.437509	1633.570853	17.465280
38.569551	1630.740439	17.470298
38.637352	1626.015381	17.475315
38.406155	1625.945288	17.480333
38.606929	1639.031993	17.485351
38.324266	1609.135253	17.490368
38.533490	1631.469763	17.495386
38.440730	1625.006992	17.500403
38.557071	1622.690303	17.505421
38.900387	1637.866798	17.510439
38.809777	1650.196184	17.515456
38.709031	1646.032815	17.520474
38.987338	1672.729285	17.525491
38.744025	1645.687469	17.530509
38.975291	1670.153071	17.535527
38.978873	1651.249861	17.540544
38.902717	1660.055025	17.545562
39.055747	1663.403115	17.550579
39.118089	1643.674161	17.555597
38.778611	1653.306236	17.560615
38.957382	1653.178628	17.565632
38.994961	1652.593775	17.570650
39.183528	1657.226048	17.575667
39.391964	1677.081721	17.580685
39.573031	1679.602667	17.585703
39.902948	1684.457795	17.590720
39.906011	1662.665063	17.595738
39.581046	1649.079055	17.600755
39.490008	1649.806137	17.605773
39.685458	1640.335456	17.610791
39.824499	1642.830066	17.615808
39.395580	1637.292333	17.620826
40.068565	1639.327421	17.625843
39.500779	1654.307891	17.630861
39.746702	1643.092577	17.635879
39.846721	1642.231931	17.640896
39.707913	1645.508583	17.645914
40.180681	1642.186538	17.650931
39.596224	1639.545888	17.655949
39.619514	1639.784414	17.660967
39.720616	1653.207917	17.665984
39.753329	1671.021549	17.671002
40.048494	1661.152716	17.676019
39.878881	1682.926389	17.681037
39.855035	1683.527929	17.686055
40.202401	1682.772551	17.691072
39.613072	1677.714979	17.696090
39.836645	1683.211544	17.701107
39.818496	1688.658571	17.706125
40.208015	1686.513808	17.711143
40.280773	1706.131614	17.716160
40.289118	1711.862283	17.721178
40.811318	1704.700521	17.726195
40.648286	1698.126229	17.731213
40.522823	1693.431970	17.736231
40.885715	1680.181395	17.741248
40.468088	1689.380799	17.746266
40.908887	1673.247092	17.751283
40.531410	1676.742706	17.756301
40.344699	1680.318008	17.761319
40.720238	1693.232177	17.766336
40.558282	1688.702611	17.771354
40.778351	1698.286381	17.776371
40.903911	1712.632533	17.781389
40.746293	1699.079564	17.786407
41.167320	1704.327574	17.791424
40.855150	1713.003671	17.796442
41.155130	1683.592724	17.801459
41.031611	1716.381069	17.806477
41.168817	1700.830565	17.811495
41.209147	1691.176953	17.816512
41.062287	1706.651909	17.821530
41.389454	1693.627239	17.826547
41.142852	1697.289173	17.831565
41.125998	1699.547536	17.836583
41.091039	1701.061614	17.841600
41.241480	1705.885597	17.846618
41.160063	1699.384804	17.851635
40.594519	1707.284919	17.856653
41.071061	1704.374383	17.861671
41.181323	1699.021197	17.866688
41.074210	1714.302636	17.871706
41.670105	1711.870133	17.876723
41.449414	1727.726540	17.881741
41.358276	1722.477821	17.886759
41.631882	1725.677711	17.891776
41.592265	1731.798275	17.896794
41.749338	1724.125306	17.901811
41.697646	1727.713694	17.906829
41.846883	1728.238871	17.911847
41.847763	1722.003365	17.916864
41.972330	1743.981895	17.921882
41.935555	1715.168846	17.926899
41.666379	1726.079615	17.931917
41.779645	1727.201976	17.936935
42.007871	1719.528674	17.941952
41.555935	1717.002153	17.946970
41.842525	1725.032221	17.951987
41.799940	1744.226460	17.957005
42.217950	1741.800298	17.962023
42.289316	1750.053463	17.967040
42.321988	1745.878227	17.972058
42.503032	1749.665456	17.977075
42.952156	1747.879261	17.982093
42.197389	1733.745098	17.987111
42.687351	1720.310631	17.992128
42.615317	1716.743548	17.997146
42.403171	1711.073692	18.002163
42.386794	1711.384611	18.007181
42.191963	1724.809756	18.012199
42.627913	1720.930432	18.017216
42.667678	1740.311304	18.022234
43.031788	1748.500481	18.027251
42.771116	1755.099893	18.032269
42.857254	1740.970046	18.037287
42.775176	1744.045767	18.042304
42.563046	1753.051993	18.047322
43.118922	1726.733570	18.052339
42.816318	1747.861597	18.057357
43.176464	1741.230594	18.062375
42.919498	1740.988433	18.067392
42.828117	1749.582151	18.072410
43.056930	1728.772624	18.077427
43.019255	1740.525792	18.082445
42.981156	1750.471659	18.087463
43.186025	1732.862283	18.092480
43.235574	1738.644593	18.097498
43.277586	1752.170418	18.102515
43.137645	1743.682799	18.107533
42.721920	1752.439926	18.112551
43.130838	1724.590817	18.117568
42.819891	1771.836726	18.122586
43.201071	1770.088105	18.127603
43.471260	1756.419669	18.132621
43.544656	1776.300159	18.137639
43.916142	1767.191428	18.142656
43.914322	1767.498454	18.147674
44.240420	1759.779636	18.152691
44.087086	1749.529241	18.157709
44.057314	1754.208949	18.162727
44.190053	1751.556149	18.167744
43.843749	1737.208981	18.172762
44.346917	1729.502839	18.177779
44.204795	1720.641208	18.182797
43.576228	1737.028277	18.187815
43.833956	1743.466364	18.192832
43.945783	1733.294816	18.197850
43.917820	1725.432708	18.202867
43.869393	1744.900008	18.207885
43.982652	1737.460531	18.212903
44.144556	1732.272127	18.217920
43.879771	1763.477075	18.222938
44.428960	1766.898864	18.227955
44.254866	1769.726572	18.232973
43.984680	1769.911230	18.237991
44.075090	1760.336101	18.243008
44.107959	1768.114076	18.248026
43.875790	1774.402216	18.253043
44.210120	1770.137970	18.258061
44.479019	1775.578578	18.263079
44.788352	1800.613964	18.268096
44.613368	1790.088571	18.273114
44.688863	1792.086833	18.278131
45.017685	1788.820744	18.283149
44.760201	1796.707959	18.288167
44.817741	1785.483253	18.293184
44.878029	1781.119561	18.298202
44.590080	1797.188114	18.303219
44.696746	1785.036938	18.308237
44.537377	1779.029880	18.313255
44.917244	1780.504554	18.318272
44.917747	1785.866847	18.323290
44.518087	1789.877252	18.328307
45.227943	1777.743147	18.333325
45.419917	1789.478608	18.338343
45.377684	1783.635337	18.343360
44.763894	1787.425062	18.348378
45.277692	1802.821505	18.353395
45.336274	1810.845511	18.358413
45.239780	1816.157217	18.363431
45.404412	1815.415244	18.368448
45.518864	1809.844274	18.373466
45.316950	1815.616380	18.378483
45.698057	1821.342703	18.383501
45.362298	1824.089238	18.388519
45.777642	1824.494905	18.393536
45.489561	1813.808207	18.398554
45.617560	1818.340081	18.403571
45.652438	1820.624820	18.408589
45.655020	1799.558689	18.413607
45.763421	1821.533623	18.418624
45.730151	1815.586664	18.423642
45.688514	1825.990892	18.428659
45.911721	1834.509325	18.433677
45.819458	1845.662528	18.438695
45.967924	1830.209190	18.443712
46.149906	1852.186594	18.448730
46.022914	1842.449454	18.453747
46.086297	1845.649862	18.458765
45.975207	1844.898375	18.463783
46.417076	1843.097597	18.468800
46.456663	1841.922537	18.473818
46.008318	1857.208206	18.478835
46.408656	1839.924603	18.483853
46.261624	1859.327558	18.488871
46.541172	1843.738471	18.493888
46.286468	1847.411173	18.498906
46.529456	1844.336511	18.503923
46.512364	1840.829849	18.508941
45.875718	1848.612390	18.513959
46.937960	1864.910863	18.518976
46.895173	1872.156697	18.523994
46.659766	1874.767689	18.529011
47.193432	1879.675334	18.534029
47.225650	1882.316008	18.539047
47.392077	1882.533285	18.544064
47.452273	1863.609759	18.549082
47.500688	1838.032726	18.554099
47.497554	1832.979144	18.559117
47.110990	1837.962739	18.564135
47.232251	1826.977947	18.569152
47.147114	1838.358096	18.574170
46.933523	1840.992344	18.579187
47.311533	1824.464219	18.584205
47.307029	1842.313884	18.589223
47.505265	1831.088728	18.594240
47.510037	1831.209089	18.599258
47.201543	1844.094051	18.604275
47.361047	1830.296907	18.609293
47.275209	1831.713720	18.614311
47.388308	1818.394317	18.619328
47.719691	1840.660908	18.624346
47.461033	1866.246304	18.629363
47.726095	1866.484031	18.634381
47.837262	1859.768412	18.639399
47.925050	1856.620970	18.644416
47.877187	1861.756626	18.649434
47.926582	1854.297386	18.654451
48.050430	1861.447429	18.659469
47.556834	1859.526843	18.664487
47.821647	1852.793017	18.669504
48.044588	1859.269737	18.674522
47.730675	1853.409988	18.679539
47.958410	1847.721838	18.684557
47.785997	1863.923049	18.689575
47.848463	1872.188714	18.694592
47.967857	1876.286253	18.699610
48.092673	1881.968529	18.704627
48.425562	1887.254258	18.709645
48.402122	1893.364446	18.714663
48.644769	1882.237560	18.719680
48.649981	1876.789377	18.724698
48.246091	1887.191643	18.729715
48.488127	1876.989793	18.734733
48.355428	1872.221124	18.739751
48.555764	1885.997104	18.744768
48.669767	1882.335819	18.749786
48.499823	1886.218382	18.754803
48.963927	1883.819453	18.759821
48.756388	1893.207277	18.764839
48.808751	1888.602572	18.769856
48.947148	1893.312136	18.774874
49.120895	1905.719131	18.779891
49.318315	1915.338117	18.784909
48.970486	1897.152867	18.789927
49.011524	1888.880120	18.794944
49.144459	1905.542340	18.799962
49.092483	1914.458633	18.804979
49.228357	1913.189561	18.809997
49.251184	1901.880638	18.815015
49.329328	1897.419683	18.820032
49.480795	1906.830489	18.825050
49.216918	1897.437609	18.830067
49.669802	1904.692503	18.835085
49.906411	1908.842146	18.840103
50.082395	1890.908424	18.845120
49.882868	1902.855847	18.850138
49.533709	1907.511032	18.855155
50.217279	1889.914790	18.860173
49.871809	1888.978881	18.865191
49.714865	1905.017223	18.870208
50.236122	1885.864414	18.875226
50.057815	1893.839727	18.880243
50.242054	1885.451338	18.885261
49.839732	1865.291244	18.890279
49.848507	1880.173708	18.895296
50.282410	1883.110546	18.900314
50.326657	1893.254164	18.905331
50.335517	1890.855473	18.910349
50.097741	1895.821653	18.915367
49.802508	1895.955249	18.920384
50.209531	1891.838250	18.925402
50.224623	1891.024167	18.930419
50.198648	1887.498460	18.935437
50.030012	1900.422517	18.940455
50.356665	1899.236280	18.945472
50.171530	1904.079237	18.950490
50.051515	1920.520692	18.955507
50.418029	1926.324890	18.960525
50.731662	1936.291872	18.965543
50.444036	1933.474840	18.970560
50.535345	1927.445048	18.975578
50.463497	1927.264597	18.980595
50.856485	1945.640884	18.985613
50.699243	1956.002293	18.990631
50.973780	1963.947901	18.995648
51.287882	1960.954683	19.000666
50.776582	1962.562053	19.005683
51.401896	1952.379253	19.010701
51.475171	1952.847340	19.015719
51.120266	1955.175382	19.020736
51.291178	1943.704386	19.025754
51.643543	1948.897370	19.030771
51.622713	1944.927237	19.035789
51.449674	1951.042429	19.040807
51.623667	1948.379869	19.045824
51.566338	1936.001463	19.050842
51.516368	1954.127502	19.055859
51.486219	1954.475229	19.060877
51.701321	1949.561409	19.065895
51.871461	1946.611601	19.070912
51.588277	1943.185100	19.075930
51.414559	1939.303843	19.080947
51.498772	1961.179027	19.085965
51.572603	1933.851716	19.090983
51.442512	1960.656316	19.096000
51.695382	1947.525291	19.101018
51.397023	1985.470180	19.106035
51.846022	1964.318463	19.111053
52.262079	1982.054043	19.116071
52.305937	1959.708519	19.121088
52.040832	1975.446436	19.126106
52.254139	1953.649627	19.131123
52.175655	1975.774148	19.136141
52.386855	1955.943953	19.141159
51.955442	1988.428082	19.146176
52.813388	1963.934536	19.151194
52.691113	2008.300806	19.156211
52.908692	1973.908046	19.161229
52.587300	1992.838762	19.166247
52.396300	1956.329410	19.171264
52.738892	1999.614787	19.176282
52.640593	1980.699080	19.181299
52.699457	1990.750772	19.186317
52.909267	2001.209410	19.191335
52.901386	1981.294567	19.196352
52.980439	1998.737844	19.201370
53.262158	1992.133392	19.206387
53.106804	1983.703146	19.211405
53.278911	1991.252971	19.216423
53.349414	1968.967678	19.221440
53.325501	2007.649080	19.226458
53.541357	1984.443957	19.231475
53.307996	1988.836882	19.236493
53.485991	1980.114379	19.241511
53.284040	2007.978162	19.246528
53.569888	1971.841042	19.251546
52.993556	2015.608060	19.256563
53.515460	1977.117784	19.261581
53.030200	2000.516867	19.266599
53.142342	2003.355603	19.271616
53.358413	2009.229444	19.276634
53.610796	2016.445582	19.281651
53.781623	2017.359013	19.286669
54.040591	2014.597947	19.291687
54.074844	2016.607536	19.296704
54.355892	2022.051021	19.301722
54.359003	1998.958452	19.306739
53.795872	2032.520759	19.311757
54.260174	2015.148097	19.316775
53.634384	2028.480224	19.321792
54.086324	2006.558765	19.326810
54.063063	2011.171450	19.331827
54.088895	2027.165049	19.336845
54.190418	2017.916742	19.341863
54.235498	2028.025714	19.346880
54.856943	2049.459855	19.351898
54.699741	2045.050543	19.356915
54.778580	2024.838665	19.361933
54.723879	2036.656137	19.366951
54.586284	2030.719433	19.371968
54.949304	2030.809408	19.376986
54.663706	2018.780366	19.382003
54.771611	2045.194811	19.387021
54.740092	2043.941411	19.392039
54.777812	2039.472702	19.397056
54.810837	2027.414864	19.402074
54.993017	2049.112537	19.407091
54.872136	2037.453616	19.412109
55.241620	2025.301228	19.417127
55.207397	2030.595216	19.422144
55.198663	2036.476603	19.427162
55.354701	2032.846330	19.432179
55.280652	2028.643986	19.437197
55.164942	2027.529856	19.442215
55.110478	2043.888637	19.447232
55.389729	2044.706128	19.452250
55.511054	2058.139366	19.457267
55.374199	2057.206358	19.462285
55.923282	2060.865766	19.467303
55.761823	2065.354214	19.472320
55.623468	2058.116720	19.477338
55.688033	2060.758561	19.482355
55.456052	2074.082986	19.487373
55.865279	2058.076586	19.492391
55.892694	2061.871093	19.497408
56.175547	2054.783511	19.502426
55.993176	2055.424503	19.507443
56.193734	2076.233667	19.512461
56.635140	2065.384835	19.517479
56.417406	2053.444043	19.522496
56.468946	2045.189981	19.527514
56.325603	2060.213292	19.532531
56.363390	2045.842319	19.537549
56.378777	2040.905261	19.542567
56.264693	2070.406836	19.547584
56.331757	2060.685794	19.552602
56.901963	2064.201834	19.557619
56.848976	2077.096595	19.562637
56.657968	2073.669520	19.567655
56.585148	2078.631478	19.572672
56.761168	2071.683621	19.577690
56.996445	2076.646785	19.582707
57.001236	2081.638840	19.587725
56.946690	2063.814027	19.592743
56.496213	2082.276229	19.597760
57.266617	2070.394927	19.602778
57.115503	2061.657217	19.607795
56.759009	2087.200401	19.612813
57.120492	2043.069451	19.617831
57.278432	2079.444294	19.622848
57.199031	2063.745471	19.627866
57.297477	2078.766424	19.632883
57.407434	2108.202461	19.637901
57.441672	2091.857843	19.642919
57.275822	2094.420029	19.647936
57.300181	2107.746079	19.652954
57.418446	2109.891722	19.657971
57.169646	2110.711625	19.662989
57.454281	2115.630752	19.668007
57.913717	2130.156886	19.673024
57.983187	2132.719305	19.678042
58.242164	2132.409017	19.683059
58.152682	2138.109836	19.688077
58.199018	2136.516820	19.693095
58.453743	2136.521818	19.698112
58.284747	2115.669781	19.703130
58.715751	2108.339896	19.708147
57.919607	2105.295605	19.713165
58.319093	2117.537795	19.718183
58.237423	2129.781218	19.723200
58.393347	2117.752472	19.728218
58.433231	2122.259167	19.733235
58.369749	2138.801967	19.738253
58.677801	2122.948485	19.743271
58.522254	2136.853815	19.748288
58.637694	2122.451507	19.753306
58.336715	2122.685122	19.758323
58.276279	2134.613700	19.763341
58.386917	2125.035105	19.768359
58.765914	2160.972202	19.773376
58.787705	2130.406054	19.778394
58.893118	2175.305967	19.783411
58.988025	2136.877068	19.788429
59.150822	2153.644926	19.793447
59.144400	2130.292543	19.798464
58.917301	2159.489847	19.803482
59.235894	2147.269967	19.808499
59.253382	2186.936262	19.813517
59.642262	2153.991280	19.818535
59.393946	2174.900480	19.823552
59.736495	2179.072634	19.828570
59.813784	2179.593572	19.833587
59.966964	2171.724358	19.838605
60.206625	2152.900826	19.843623
60.030908	2152.029065	19.848640
60.246039	2145.866178	19.853658
60.201906	2133.092238	19.858675
59.738218	2133.570452	19.863693
60.044289	2120.723373	19.868711
60.036824	2127.131563	19.873728
59.978429	2122.487817	19.878746
60.484928	2128.208426	19.883763
60.393423	2130.845279	19.888781
60.630829	2119.115001	19.893799
60.242219	2132.041308	19.898816
60.288053	2129.984324	19.903834
60.496723	2121.359093	19.908851
60.295208	2136.294231	19.913869
60.407608	2132.626847	19.918887
60.577532	2149.626374	19.923904
60.602418	2162.154857	19.928922
60.760216	2144.840356	19.933939
60.740718	2151.101036	19.938957
61.015020	2152.084492	19.943975
60.765966	2163.080469	19.948992
61.072626	2146.893697	19.954010
61.503328	2146.162764	19.959027
61.160259	2148.894793	19.964045
61.118280	2154.910518	19.969063
61.365061	2153.483739	19.974080
61.065611	2147.715945	19.979098
61.201372	2146.637210	19.984115
61.129493	2163.646997	19.989133
61.460235	2150.182471	19.994151
61.531686	2150.973330	19.999168
61.189160	2143.080931	20.004186
61.615930	2171.587245	20.009203
61.501179	2187.389505	20.014221
61.824608	2177.655819	20.019239
61.919332	2177.491274	20.024256
61.926008	2182.078790	20.029274
62.199916	2182.436238	20.034291
61.939262	2174.247618	20.039309
61.797778	2171.740720	20.044327
61.773774	2181.152944	20.049344
61.816456	2193.675470	20.054362
62.324366	2161.735544	20.059379
61.798037	2168.893463	20.064397
61.602873	2182.779986	20.069415
61.885656	2205.224779	20.074432
62.152939	2200.917617	20.079450
62.374397	2198.651717	20.084467
62.221864	2223.912501	20.089485
62.696605	2196.895150	20.094503
62.161187	2195.767709	20.099520
62.465906	2242.566180	20.104538
63.109764	2222.750001	20.109555
62.904741	2224.615301	20.114573
63.218098	2225.246464	20.119591
63.214175	2242.217192	20.124608
63.206110	2215.224887	20.129626
63.279888	2235.771348	20.134643
63.349576	2206.150672	20.139661
63.416618	2179.314773	20.144679
63.456481	2202.235606	20.149696
63.150432	2192.979820	20.154714
63.278068	2189.511343	20.159731
63.355560	2217.909849	20.164749
63.480461	2221.036036	20.169767
63.872207	2222.976062	20.174784
63.582935	2223.833886	20.179802
63.752495	2213.209196	20.184819
63.616724	2216.746616	20.189837
63.689089	2229.632534	20.194855
64.043552	2221.896366	20.199872
63.473988	2234.511839	20.204890
64.023473	2203.304528	20.209907
64.024031	2235.540995	20.214925
64.123532	2201.185404	20.219943
64.306357	2215.799781	20.224960
63.567160	2228.119823	20.229978
64.465140	2199.447766	20.234995
63.770183	2239.084666	20.240013
63.801850	2222.962111	20.245031
64.239467	2264.454006	20.250048
63.943880	2256.499003	20.255066
64.369775	2253.262953	20.260083
64.447231	2231.477953	20.265101
64.355016	2290.326547	20.270119
64.452688	2262.417503	20.275136
64.536437	2281.335898	20.280154
64.810697	2278.718640	20.285171
65.011023	2263.141739	20.290189
64.860454	2284.197534	20.295207
65.404410	2262.602372	20.300224
65.311296	2261.545968	20.305242
65.283197	2285.739361	20.310259
65.211148	2258.894034	20.315277
65.105296	2289.390486	20.320295
65.407814	2262.340701	20.325312
65.208452	2280.129167	20.330330
65.762581	2304.388626	20.335347
65.307684	2304.996006	20.340365
65.767361	2289.791436	20.345383
66.123582	2294.104592	20.350400
65.877251	2310.763263	20.355418
66.533423	2288.245658	20.360435
66.189847	2273.346949	20.365453
66.283944	2268.010290	20.370471
66.255894	2254.143549	20.375488
65.848813	2250.919204	20.380506
66.020108	2262.176993	20.385523
66.071155	2266.927350	20.390541
66.081359	2273.521554	20.395559
66.185814	2290.476629	20.400576
66.447122	2289.110444	20.405594
66.184806	2274.848449	20.410611
66.240833	2319.841630	20.415629
66.116189	2288.137580	20.420647
66.251373	2296.517737	20.425664
66.289954	2291.974879	20.430682
66.485655	2293.211558	20.435699
66.401641	2320.028351	20.440717
66.349769	2321.425637	20.445735
67.196547	2315.221731	20.450752
67.048220	2318.172853	20.455770
66.957468	2312.310363	20.460787
67.170629	2310.376113	20.465805
67.196852	2315.979898	20.470823
67.359379	2318.469308	20.475840
67.120814	2320.906271	20.480858
67.364905	2318.671352	20.485875
67.233322	2339.139019	20.490893
67.258712	2343.555284	20.495911
67.720411	2343.678294	20.500928
67.258496	2337.753854	20.505946
67.369155	2322.029163	20.510963
67.506090	2337.561784	20.515981
67.627021	2355.288256	20.520999
67.812352	2348.958572	20.526016
67.748976	2370.234974	20.531034
68.109644	2365.368592	20.536051
68.089862	2369.608018	20.541069
67.951197	2383.650895	20.546087
68.039830	2358.412608	20.551104
68.145728	2367.057031	20.556122
68.148047	2377.022051	20.561139
68.159502	2362.115402	20.566157
68.289114	2376.491455	20.571175
68.480918	2381.186369	20.576192
68.617344	2393.816819	20.581210
68.720710	2381.791517	20.586227
68.953202	2408.163161	20.591245
68.955884	2383.267309	20.596263
69.264252	2387.802062	20.601280
69.290691	2375.925889	20.606298
69.058780	2396.459974	20.611315
69.328519	2377.425284	20.616333
69.111692	2382.455928	20.621351
69.350568	2377.099288	20.626368
69.087093	2384.190227	20.631386
69.413007	2387.874298	20.636403
69.550418	2378.181153	20.641421
69.172884	2375.510507	20.646439
69.526090	2373.377733	20.651456
69.580595	2382.695769	20.656474
69.853608	2390.561631	20.661491
69.856351	2386.405141	20.666509
69.632693	2371.150572	20.671527
69.745542	2360.687405	20.676544
69.537677	2375.420874	20.681562
69.740449	2375.755065	20.686579
70.065826	2386.381176	20.691597
69.880279	2402.833625	20.696615
70.234403	2395.636984	20.701632
69.942186	2410.737880	20.706650
70.251186	2410.642988	20.711667
70.289688	2411.122928	20.716685
70.189632	2409.552439	20.721703
70.239239	2406.684682	20.726720
70.032487	2412.378353	20.731738
70.444483	2420.428928	20.736755
70.512824	2435.740564	20.741773
70.619080	2447.523264	20.746791
70.858654	2437.437037	20.751808
71.005297	2427.239003	20.756826
71.089064	2455.939004	20.761843
71.232063	2425.529878	20.766861
70.695675	2438.071806	20.771879
71.377786	2425.302927	20.776896
71.372759	2434.142837	20.781914
71.515052	2435.437597	20.786931
71.438549	2434.940120	20.791949
71.458285	2454.051425	20.796967
71.859165	2450.767411	20.801984
71.790585	2463.996919	20.807002
71.694556	2453.871385	20.812019
71.735327	2457.041714	20.817037
71.755146	2446.617703	20.822055
71.806946	2474.739227	20.827072
72.271280	2456.188588	20.832090
72.195631	2445.819128	20.837107
72.215468	2466.002484	20.842125
72.026047	2460.136791	20.847143
72.424931	2448.851636	20.852160
72.277275	2444.649897	20.857178
72.557015	2449.683968	20.862195
72.291043	2450.744947	20.867213
72.383642	2456.262695	20.872231
72.580880	2446.607157	20.877248
71.800424	2471.129262	20.882266
72.176281	2451.843951	20.887283
72.348005	2477.169089	20.892301
72.776058	2485.409056	20.897319
72.896124	2484.847197	20.902336
73.262648	2477.256056	20.907354
72.782297	2485.756498	20.912371
73.191479	2485.828895	20.917389
72.858174	2494.552868	20.922407
73.373522	2486.943496	20.927424
73.557059	2499.273932	20.932442
73.263514	2500.446281	20.937459
73.931063	2498.732144	20.942477
73.805126	2487.354462	20.947495
73.840842	2481.028128	20.952512
73.547020	2489.971540	20.957530
73.703203	2483.703862	20.962547
73.843781	2488.826207	20.967565
73.838842	2495.083140	20.972583
73.955101	2501.515812	20.977600
73.658532	2499.916872	20.982618
73.384258	2503.748590	20.987635
73.815719	2498.253441	20.992653
73.838523	2499.237700	20.997671
73.957605	2514.873249	21.002688
74.315710	2523.718231	21.007706
74.225879	2538.509337	21.012723
74.503568	2527.052318	21.017741
74.102006	2537.482987	21.022759
74.362428	2526.453455	21.027776
74.506624	2545.701556	21.032794
74.625433	2550.722784	21.037811
75.158739	2550.226381	21.042829
74.687423	2575.661308	21.047847
75.144657	2562.981655	21.052864
75.611509	2555.340654	21.057882
75.368090	2558.981842	21.062899
75.428629	2549.358259	21.067917
75.351070	2561.484981	21.072935
75.572617	2545.639329	21.077952
75.768644	2564.785592	21.082970
75.212524	2566.756472	21.087987
75.722046	2534.901207	21.093005
75.185671	2559.649604	21.098023
75.604714	2550.921359	21.103040
75.918244	2537.855639	21.108058
75.777243	2554.200478	21.113075
76.102098	2572.994288	21.118093
75.889840	2585.791408	21.123111
75.985319	2582.047169	21.128128
76.107532	2574.560219	21.133146
75.872276	2589.116578	21.138163
76.452355	2580.255667	21.143181
76.391613	2593.860799	21.148199
76.619389	2582.059323	21.153216
76.852197	2584.693310	21.158234
76.864207	2581.199918	21.163251
76.498547	2585.013981	21.168269
76.706980	2581.687478	21.173287
77.077050	2571.191010	21.178304
76.947942	2562.162399	21.183322
76.606950	2583.743728	21.188339
77.023722	2602.970463	21.193357
77.078944	2601.403508	21.198375
77.333058	2613.419967	21.203392
77.378529	2605.795007	21.208410
77.175441	2601.019231	21.213427
77.203351	2595.493223	21.218445
77.235887	2601.339155	21.223463
77.226137	2611.208728	21.228480
77.660434	2602.660499	21.233498
77.256136	2596.390121	21.238515
78.004862	2608.960876	21.243533
78.021290	2631.860167	21.248551
78.184027	2630.375957	21.253568
78.157145	2622.088453	21.258586
78.055310	2629.329135	21.263603
78.158087	2634.138221	21.268621
77.965696	2630.307733	21.273639
78.012351	2630.692781	21.278656
78.368008	2624.884042	21.283674
77.763747	2625.027589	21.288691
78.089101	2628.367304	21.293709
78.219116	2654.404149	21.298727
78.788432	2650.837605	21.303744
78.881096	2652.588633	21.308762
78.938960	2653.145721	21.313779
79.144817	2645.151444	21.318797
79.143258	2648.737570	21.323815
79.062459	2643.712607	21.328832
79.287259	2640.104255	21.333850
78.806346	2656.774770	21.338867
79.488870	2648.346603	21.343885
79.125415	2650.033502	21.348903
79.212645	2652.663971	21.353920
79.322263	2676.519861	21.358938
79.504744	2674.533038	21.363955
79.541183	2675.692896	21.368973
79.835471	2683.218882	21.373991
79.455766	2678.888901	21.379008
79.752728	2679.911257	21.384026
79.633526	2685.280385	21.389043
79.973376	2693.624204	21.394061
79.815515	2698.743872	21.399079
80.174250	2707.886184	21.404096
80.429975	2699.088720	21.409114
79.990654	2699.301926	21.414131
80.501573	2698.446489	21.419149
80.523538	2701.928985	21.424167
80.409835	2706.315627	21.429184
80.687128	2702.831817	21.434202
80.777792	2718.642799	21.439219
80.961869	2721.593696	21.444237
81.385010	2725.065713	21.449255
81.105570	2728.123558	21.454272
81.443151	2721.529537	21.459290
81.440581	2718.069900	21.464307
81.165747	2709.246128	21.469325
81.172517	2705.114075	21.474343
81.374537	2715.192995	21.479360
81.541913	2712.813726	21.484378
81.423800	2726.332957	21.489395
81.570953	2716.604213	21.494413
81.751686	2706.242451	21.499431
81.695267	2708.391656	21.504448
81.790543	2703.738165	21.509466
81.638832	2715.467045	21.514483
81.513003	2701.462878	21.519501
81.867277	2697.763077	21.524519
81.672565	2720.726065	21.529536
82.236888	2727.198294	21.534554
82.104613	2737.664821	21.539571
82.228850	2706.287492	21.544589
82.059049	2742.973461	21.549607
82.177281	2726.822387	21.554624
82.392468	2741.462810	21.559642
82.256798	2763.200437	21.564659
82.518181	2736.033632	21.569677
82.404439	2774.791964	21.574695
82.342411	2752.351988	21.579712
82.912978	2759.173253	21.584730
82.897825	2790.709490	21.589747
83.258871	2776.754251	21.594765
83.105962	2793.973548	21.599783
83.210479	2782.672151	21.604800
82.905589	2789.969674	21.609818
83.100962	2779.486756	21.614835
83.286188	2819.918521	21.619853
83.531365	2801.378009	21.624871
83.393638	2829.907202	21.629888
84.327710	2812.932197	21.634906
84.101165	2803.238600	21.639923
84.047527	2802.398457	21.644941
84.036640	2815.217154	21.649959
84.028015	2802.548654	21.654976
84.216347	2811.315486	21.659994
84.339542	2812.156337	21.665011
84.603185	2823.237806	21.670029
84.795825	2826.704129	21.675047
84.762569	2818.266511	21.680064
84.862685	2819.762312	21.685082
84.787411	2836.998384	21.690099
84.818658	2828.869031	21.695117
84.888816	2826.734921	21.700135
84.838960	2833.644927	21.705152
85.026819	2822.296388	21.710170
85.130388	2824.689103	21.715187
85.100708	2829.214976	21.720205
85.404208	2820.351617	21.725223
85.091416	2822.458344	21.730240
85.511300	2819.856313	21.735258
85.554370	2810.971561	21.740275
85.486106	2822.487435	21.745293
85.751719	2825.686491	21.750311
85.396423	2856.651793	21.755328
86.238825	2851.138968	21.760346
86.245149	2851.359770	21.765363
86.275234	2842.541568	21.770381
86.165956	2847.570166	21.775399
86.083953	2857.843134	21.780416
86.459960	2855.547773	21.785434
86.419692	2846.704604	21.790451
86.053015	2847.116238	21.795469
86.169309	2854.739127	21.800487
86.092575	2849.675689	21.805504
86.532855	2850.490364	21.810522
86.207574	2840.877770	21.815539
86.790290	2894.269434	21.820557
86.957697	2864.891403	21.825575
86.529530	2867.778710	21.830592
86.710105	2880.951564	21.835610
86.523074	2859.176337	21.840627
86.555113	2913.574582	21.845645
87.214103	2882.040030	21.850663
86.957975	2912.259708	21.855680
87.451056	2901.705635	21.860698
87.721284	2924.880329	21.865715
87.645804	2935.072082	21.870733
88.159593	2923.786333	21.875751
87.906724	2918.426105	21.880768
88.211157	2903.255880	21.885786
88.207071	2929.054248	21.890803
88.662721	2893.111154	21.895821
88.604247	2929.009794	21.900839
88.398329	2908.884570	21.905856
88.574243	2915.642203	21.910874
88.419849	2916.719244	21.915891
88.468188	2915.784177	21.920909
89.083761	2904.701664	21.925927
88.750703	2914.215555	21.930944
88.781242	2913.288833	21.935962
88.833153	2913.068970	21.940979
88.691881	2889.360893	21.945997
88.975187	2929.491015	21.951015
88.690995	2898.055696	21.956032
89.009980	2918.439747	21.961050
89.058365	2921.111855	21.966067
88.983698	2948.454525	21.971085
89.599288	2921.418885	21.976103
89.532448	2934.451902	21.981120
89.368548	2949.930108	21.986138
89.714031	2931.394674	21.991155
89.951982	2956.909877	21.996173
90.079022	2962.962697	22.001191
89.933735	2963.720516	22.006208
90.503404	2959.697636	22.011226
90.081167	2957.258964	22.016243
90.053132	2975.223891	22.021261
90.208517	2975.097648	22.026279
90.253166	2957.694038	22.031296
90.125307	2957.781284	22.036314
90.401007	2980.027046	22.041331
90.282241	2967.561595	22.046349
90.529263	2974.432194	22.051367
90.291686	3002.271309	22.056384
90.662973	2986.311635	22.061402
90.872601	2981.210356	22.066419
90.725176	2992.558863	22.071437
91.234238	3020.316713	22.076455
91.379125	3012.812551	22.081472
91.497333	3007.738425	22.086490
91.647992	3023.354542	22.091507
91.819037	3010.532934	22.096525
91.969941	3008.620321	22.101543
91.679668	3009.672627	22.106560
91.939072	3014.944537	22.111578
92.197668	3020.217365	22.116595
91.872549	3010.336411	22.121613
92.181865	3014.744576	22.126631
92.109889	3014.723017	22.131648
92.084297	3008.150595	22.136666
92.205714	3017.825697	22.141683
92.412414	3000.004486	22.146701
92.313527	3007.666486	22.151719
92.374068	3048.298892	22.156736
92.727825	3012.337142	22.161754
92.785787	3045.846000	22.166771
92.901183	3024.200067	22.171789
93.167967	3019.520701	22.176807
93.644892	3016.322761	22.181824
93.511127	3008.194450	22.186842
93.515649	3022.177354	22.191859
93.524238	3021.418518	22.196877
93.517601	3016.767018	22.201895
93.529455	3025.768202	22.206912
93.479412	3020.700448	22.211930
93.747465	3020.228239	22.216947
93.705963	3026.731135	22.221965
93.973746	3019.313560	22.226983
93.761612	3015.947047	22.232000
94.030048	3046.759810	22.237018
94.203797	3034.748705	22.242035
93.989148	3038.869163	22.247053
94.490833	3039.831374	22.252071
94.291689	3047.421285	22.257088
94.296893	3048.114997	22.262106
94.135904	3039.564687	22.267123
93.957295	3072.418359	22.272141
94.637826	3073.259240	22.277159
94.168434	3077.289757	22.282176
94.570668	3087.993014	22.287194
95.158782	3097.724325	22.292211
94.846258	3100.615261	22.297229
95.058081	3102.002825	22.302247
95.278087	3113.052146	22.307264
95.353509	3104.177003	22.312282
95.689046	3089.705609	22.317299
95.531789	3104.912339	22.322317
95.696416	3099.371420	22.327335
95.964285	3117.568575	22.332352
96.041680	3131.442429	22.337370
96.347167	3125.733524	22.342387
95.986216	3124.781115	22.347405
96.222799	3125.424566	22.352423
96.554619	3131.294568	22.357440
96.572247	3132.773665	22.362458
96.526631	3128.350946	22.367475
96.000469	3132.594253	22.372493
96.279534	3121.573100	22.377511
96.433567	3128.407473	22.382528
96.546635	3134.805540	22.387546
96.641690	3141.532910	22.392563
96.608026	3147.189040	22.397581
96.833859	3146.964252	22.402599
96.614173	3142.776941	22.407616
96.825636	3161.872763	22.412634
97.490020	3172.492594	22.417651
97.436486	3189.871919	22.422669
97.727575	3176.568517	22.427687
97.653218	3181.375352	22.432704
97.811207	3180.993054	22.437722
98.361246	3163.867294	22.442739
98.326727	3164.691625	22.447757
98.472105	3157.681281	22.452775
98.387147	3181.000329	22.457792
98.577205	3163.896572	22.462810
98.768981	3157.672486	22.467827
98.643824	3141.396941	22.472845
98.565742	3182.487588	22.477863
98.618314	3151.856965	22.482880
98.603501	3171.847821	22.487898
98.636651	3137.552515	22.492915
98.570230	3176.908461	22.497933
98.919343	3160.263879	22.502951
98.759187	3183.533568	22.507968
99.127959	3184.902407	22.512986
99.379490	3180.065747	22.518003
99.165575	3169.579379	22.523021
99.191566	3206.186526	22.528039
99.345238	3187.835521	22.533056
99.432359	3209.038024	22.538074
99.620803	3206.639586	22.543091
99.427564	3232.235037	22.548109
99.875061	3211.152554	22.553127
100.094973	3222.358503	22.558144
99.984362	3206.101803	22.563162
100.174284	3235.783013	22.568179
100.075669	3229.541487	22.573197
100.634356	3229.969188	22.578215
100.591047	3225.725412	22.583232
100.513791	3242.275594	22.588250
100.871982	3231.494235	22.593267
100.927639	3241.539439	22.598285
100.914295	3238.469180	22.603303
100.915771	3242.359375	22.608320
100.348520	3232.843308	22.613338
100.965066	3251.013351	22.618355
100.983478	3252.530092	22.623373
101.343500	3263.489556	22.628391
101.374684	3255.460659	22.633408
101.375265	3258.256865	22.638426
101.549967	3257.072733	22.643443
101.387878	3289.395676	22.648461
101.682492	3289.150481	22.653479
102.065636	3283.465316	22.658496
101.899750	3298.252800	22.663514
102.151808	3273.013616	22.668531
102.196458	3270.321889	22.673549
102.475248	3316.116409	22.678567
103.233454	3304.743417	22.683584
102.655991	3302.104470	22.688602
102.634457	3305.313236	22.693619
102.848915	3307.630929	22.698637
103.060238	3307.344741	22.703655
102.932900	3318.880651	22.708672
102.793828	3322.455045	22.713690
103.107577	3310.381276	22.718707
102.977770	3312.174936	22.723725
102.871080	3315.714276	22.728743
103.561009	3333.027929	22.733760
103.626845	3338.684000	22.738778
103.728274	3350.468989	22.743795
103.713807	3350.325777	22.748813
103.768917	3347.718893	22.753831
103.763900	3343.062312	22.758848
103.640253	3345.328519	22.763866
104.231294	3370.298891	22.768883
104.049309	3369.026891	22.773901
104.189441	3377.329012	22.778919
104.416024	3375.987147	22.783936
104.399185	3376.985653	22.788954
104.743434	3378.763515	22.793971
104.705973	3392.623681	22.798989
105.011185	3389.814087	22.804007
105.005605	3384.785525	22.809024
104.806886	3406.414600	22.814042
105.215261	3391.930509	22.819059
105.075473	3390.459851	22.824077
105.341672	3390.379650	22.829095
105.502342	3406.788251	22.834112
105.411736	3412.919225	22.839130
105.513016	3429.835233	22.844147
105.625347	3415.299998	22.849165
105.445899	3431.017955	22.854183
105.991671	3436.340325	22.859200
105.902105	3438.443793	22.864218
106.333745	3437.742550	22.869235
106.390457	3430.259314	22.874253
106.345446	3423.689801	22.879271
106.568020	3433.330172	22.884288
106.623162	3444.160617	22.889306
106.971991	3434.105840	22.894323
106.773970	3433.836936	22.899341
106.921573	3427.146252	22.904359
107.236425	3423.221302	22.909376
107.288154	3440.448847	22.914394
107.217627	3423.510618	22.919411
107.527767	3440.208488	22.924429
107.619095	3452.596127	22.929447
107.451447	3462.688887	22.934464
107.815896	3454.711359	22.939482
107.758545	3439.870426	22.944499
107.675230	3464.370339	22.949517
107.863546	3459.731663	22.954535
107.916052	3447.590099	22.959552
107.687133	3456.137531	22.964570
108.291784	3485.030243	22.969587
108.074568	3484.425376	22.974605
107.806581	3477.396624	22.979623
108.095394	3498.219713	22.984640
108.314846	3499.112118	22.989658
108.401715	3502.321735	22.994675
108.433126	3527.046518	22.999693
109.070524	3496.522507	23.004711
109.304250	3543.205913	23.009728
109.097851	3520.079049	23.014746
109.419562	3544.993554	23.019763
109.728466	3513.319178	23.024781
109.465804	3544.795825	23.029799
109.808909	3518.910849	23.034816
109.475583	3527.524525	23.039834
109.798983	3542.527642	23.044851
110.136582	3544.599200	23.049869
109.951363	3550.666657	23.054887
110.104484	3565.036991	23.059904
110.102021	3569.993743	23.064922
110.544780	3561.047954	23.069939
110.597742	3556.798171	23.074957
110.336036	3564.759372	23.079975
110.656847	3561.624754	23.084992
110.567210	3600.604042	23.090010
110.830451	3590.314240	23.095027
110.860546	3581.487725	23.100045
110.768966	3603.798509	23.105063
111.436107	3593.191020	23.110080
110.998699	3616.085558	23.115098
111.595353	3619.121886	23.120115
111.795722	3623.195999	23.125133
111.743022	3613.563026	23.130151
112.108967	3607.013646	23.135168
112.097633	3615.605138	23.140186
112.242094	3607.554839	23.145203
112.437364	3594.842129	23.150221
112.579403	3611.300341	23.155239
112.502595	3614.904209	23.160256
112.552674	3603.991573	23.165274
112.752897	3592.354931	23.170291
112.923616	3594.776398	23.175309
112.922994	3599.396201	23.180327
112.711597	3605.895765	23.185344
113.005818	3609.962776	23.190362
113.016761	3604.413921	23.195379
113.175903	3620.699511	23.200397
112.908851	3637.979691	23.205415
113.423374	3615.925498	23.210432
113.226263	3630.197566	23.215450
113.476519	3632.236654	23.220467
113.562998	3640.944715	23.225485
113.584222	3646.784217	23.230503
113.685496	3657.592519	23.235520
113.870148	3653.615114	23.240538
113.890297	3645.148837	23.245555
114.385376	3667.271001	23.250573
114.086408	3681.421702	23.255591
114.682138	3669.942975	23.260608
114.282185	3685.104049	23.265626
114.301992	3691.864911	23.270643
114.784111	3696.852207	23.275661
114.843071	3705.579640	23.280679
115.175000	3705.229379	23.285696
115.438372	3698.434373	23.290714
115.632065	3706.503960	23.295731
115.540371	3700.788940	23.300749
115.491087	3710.494080	23.305767
115.880657	3712.294651	23.310784
115.646742	3708.777271	23.315802
115.709820	3710.040730	23.320819
116.022879	3730.930295	23.325837
116.055187	3729.783776	23.330855
116.161179	3724.865526	23.335872
116.285274	3728.066110	23.340890
116.341705	3728.369396	23.345907
116.574828	3741.666802	23.350925
116.498140	3763.473600	23.355943
116.924390	3761.186612	23.360960
117.143911	3768.126477	23.365978
116.748529	3765.317606	23.370995
117.200153	3747.877271	23.376013
116.999315	3781.272546	23.381031
117.258039	3759.460297	23.386048
117.294485	3802.301936	23.391066
117.621668	3768.700829	23.396083
117.834317	3798.312699	23.401101
117.996603	3797.586739	23.406119
118.092109	3774.236708	23.411136
118.020252	3798.527689	23.416154
118.143063	3792.644708	23.421171
118.190059	3787.631224	23.426189
117.913803	3809.034912	23.431207
118.616802	3820.154073	23.436224
118.475222	3820.149902	23.441242
118.215748	3811.221534	23.446259
118.765822	3806.430677	23.451277
118.968200	3824.639946	23.456295
119.098030	3825.284720	23.461312
119.211915	3828.023640	23.466330
119.302312	3838.157323	23.471347
119.451198	3820.963397	23.476365
119.394577	3818.490663	23.481383
119.557362	3841.528987	23.486400
119.957314	3825.166594	23.491418
119.995198	3822.928147	23.496435
120.162813	3852.133548	23.501453
120.189946	3867.409996	23.506471
120.476462	3845.176282	23.511488
120.763637	3856.267377	23.516506
120.380262	3867.121642	23.521523
120.347728	3847.767461	23.526541
120.795491	3852.131000	23.531559
120.635852	3856.194144	23.536576
121.043669	3842.628465	23.541594
120.909589	3859.451133	23.546611
121.523666	3860.674737	23.551629
121.155842	3873.706237	23.556647
121.543170	3869.122230	23.561664
121.496635	3873.432435	23.566682
121.356648	3877.139261	23.571699
121.755178	3865.389764	23.576717
121.730249	3890.901321	23.581735
121.885247	3900.000573	23.586752
121.927458	3897.336652	23.591770
122.190451	3898.488804	23.596787
122.198712	3893.327282	23.601805
122.086190	3910.582357	23.606823
122.078869	3922.899597	23.611840
122.654814	3932.872548	23.616858
122.103646	3938.067154	23.621875
122.715235	3950.424183	23.626893
122.773091	3957.154715	23.631911
122.799537	3940.375841	23.636928
123.216873	3974.916640	23.641946
123.836955	3990.351183	23.646963
124.363277	3960.289936	23.651981
123.854327	3972.609321	23.656999
123.799314	3982.407589	23.662016
124.084495	3986.725508	23.667034
124.080094	3979.907777	23.672051
124.185871	3980.228372	23.677069
124.113343	3977.338091	23.682087
123.912467	3980.129585	23.687104
124.274328	3988.400636	23.692122
124.338356	4006.620391	23.697139
124.628255	4006.243002	23.702157
124.598641	4009.432758	23.707175
124.761302	3992.214410	23.712192
125.109981	4032.721807	23.717210
125.086242	4023.330946	23.722227
124.938345	4025.531900	23.727245
125.236390	4048.364128	23.732263
125.529227	4047.216950	23.737280
125.864373	4050.615225	23.742298
126.045101	4056.287081	23.747315
126.198194	4071.957425	23.752333
126.361892	4070.334474	23.757351
125.940835	4046.315929	23.762368
126.398232	4076.565838	23.767386
126.448816	4056.314748	23.772403
126.351096	4065.847709	23.777421
126.699014	4070.737753	23.782439
126.677692	4079.750382	23.787456
126.856574	4101.707299	23.792474
126.770638	4082.351095	23.797491
127.279123	4092.818689	23.802509
127.197053	4098.253209	23.807527
127.397673	4099.534104	23.812544
127.778999	4111.427688	23.817562
128.047668	4132.195900	23.822579
127.972514	4121.021232	23.827597
127.907051	4103.745516	23.832615
127.999890	4133.480216	23.837632
128.353119	4092.327296	23.842650
128.385381	4115.773097	23.847667
128.804488	4104.754054	23.852685
128.812060	4131.283464	23.857703
129.042445	4125.472089	23.862720
129.438439	4134.765119	23.867738
129.347982	4138.194300	23.872755
129.502245	4115.319707	23.877773
129.366956	4133.961568	23.882791
129.495998	4118.653648	23.887808
129.550233	4103.904377	23.892826
129.871908	4130.180756	23.897843
129.872467	4103.588694	23.902861
130.171060	4125.608370	23.907879
129.547176	4131.824667	23.912896
130.042813	4112.737549	23.917914
129.708276	4136.594274	23.922931
130.172540	4150.332686	23.927949
130.285333	4154.741858	23.932967
130.345130	4159.761253	23.937984
130.446039	4167.465947	23.943002
130.397298	4175.113481	23.948019
130.453181	4194.646871	23.953037
131.009141	4194.500807	23.958055
130.905297	4209.630942	23.963072
131.253779	4201.425862	23.968090
131.204012	4220.435714	23.973107
131.528936	4214.825555	23.978125
131.445148	4213.052468	23.983143
131.650896	4229.865432	23.988160
131.943539	4235.163169	23.993178
131.454143	4237.424108	23.998195
131.939928	4230.823882	24.003213
132.105484	4263.175398	24.008231
131.800419	4273.018447	24.013248
132.313773	4265.104846	24.018266
132.460246	4289.592315	24.023283
132.929309	4289.944674	24.028301
132.720361	4291.460013	24.033319
132.803136	4287.412938	24.038336
133.316813	4288.823291	24.043354
133.320658	4317.324160	24.048371
133.662225	4324.510717	24.053389
133.909166	4318.146765	24.058407
134.056195	4316.048170	24.063424
133.921156	4315.914731	24.068442
134.049684	4318.556226	24.073459
134.334572	4325.804526	24.078477
134.534619	4346.358217	24.083495
134.446467	4356.097514	24.088512
134.473978	4352.417940	24.093530
134.665253	4350.711112	24.098547
135.022343	4341.738394	24.103565
135.099498	4332.722209	24.108583
134.960990	4359.910928	24.113600
135.411579	4369.878997	24.118618
135.362364	4362.305190	24.123635
135.277185	4379.797956	24.128653
135.263566	4382.042058	24.133671
135.435549	4383.821556	24.138688
136.316577	4386.482326	24.143706
136.088979	4411.342722	24.148723
136.058971	4385.701355	24.153741
136.088160	4408.903469	24.158759
136.160492	4408.420736	24.163776
136.391100	4426.811117	24.168794
136.622858	4441.007729	24.173811
136.319606	4424.794545	24.178829
136.936561	4445.062432	24.183847
137.091967	4453.572766	24.188864
137.449768	4453.341085	24.193882
137.348583	4473.016312	24.198899
137.336069	4466.229540	24.203917
137.761056	4457.378871	24.208935
137.890481	4480.734246	24.213952
138.185630	4467.543883	24.218970
138.487087	4479.127190	24.223987
138.147256	4470.514087	24.229005
138.272871	4473.897097	24.234023
138.154789	4467.680956	24.239040
138.511174	4476.955348	24.244058
138.471559	4500.196109	24.249075
138.656542	4494.544438	24.254093
139.350272	4512.525191	24.259111
139.079927	4513.873344	24.264128
139.158247	4495.739607	24.269146
138.826458	4499.459861	24.274163
139.319414	4516.365028	24.279181
139.601917	4545.635308	24.284199
139.483075	4523.403838	24.289216
139.738303	4529.020736	24.294234
140.094779	4547.972536	24.299251
140.305329	4568.565771	24.304269
140.404942	4572.116573	24.309287
140.135694	4564.443224	24.314304
140.262195	4575.068040	24.319322
140.384186	4566.780084	24.324339
140.580697	4589.029916	24.329357
140.600767	4594.174579	24.334375
140.595165	4606.340294	24.339392
141.365252	4620.213683	24.344410
141.345934	4626.186691	24.349427
141.192273	4628.509798	24.354445
141.928432	4637.398069	24.359463
142.071739	4645.856165	24.364480
142.449906	4654.022732	24.369498
142.472913	4653.491217	24.374515
142.846732	4637.596219	24.379533
143.027382	4629.936853	24.384551
142.612963	4658.302111	24.389568
142.886089	4633.133536	24.394586
142.852183	4646.497941	24.399603
143.096881	4636.202501	24.404621
143.203421	4636.616603	24.409639
143.479868	4648.101767	24.414656
143.368695	4647.349354	24.419674
143.571647	4661.073272	24.424691
143.501855	4678.541127	24.429709
143.708988	4657.730107	24.434727
143.926391	4669.175929	24.439744
144.216524	4667.284960	24.444762
144.694655	4687.067137	24.449779
144.785298	4677.239118	24.454797
145.026712	4678.056514	24.459815
144.876578	4682.385045	24.464832
144.865005	4683.980661	24.469850
145.015895	4682.181902	24.474867
144.851556	4682.285982	24.479885
145.085012	4689.029762	24.484903
145.193390	4711.182125	24.489920
145.307452	4707.558677	24.494938
145.480371	4704.261749	24.499955
145.249648	4753.451485	24.504973
145.577499	4733.651640	24.509991
145.467369	4748.480467	24.515008
146.062681	4729.269676	24.520026
146.141881	4784.598770	24.525043
146.240096	4755.943844	24.530061
146.688658	4762.913749	24.535079
146.920483	4773.359077	24.540096
146.928763	4790.238781	24.545114
147.280046	4801.151243	24.550131
146.898591	4786.907347	24.555149
147.041547	4805.717311	24.560167
147.590319	4799.405726	24.565184
147.522429	4807.859827	24.570202
147.845728	4817.034299	24.575219
148.011097	4819.050906	24.580237
148.254467	4812.007633	24.585255
147.795286	4841.961578	24.590272
148.228779	4834.987103	24.595290
148.400654	4838.183462	24.600307
148.577970	4857.655895	24.605325
149.065815	4849.259106	24.610343
148.982392	4859.174981	24.615360
148.704635	4852.105425	24.620378
149.065056	4878.605105	24.625395
149.317814	4879.411265	24.630413
149.316244	4874.432686	24.635431
149.305329	4870.125054	24.640448
149.769233	4906.588757	24.645466
149.808694	4895.842841	24.650483
149.649345	4916.578138	24.655501
150.026000	4902.547601	24.660519
150.098683	4951.816281	24.665536
150.051120	4928.241783	24.670554
150.560607	4971.664361	24.675571
150.640167	4968.825943	24.680589
151.019792	4949.073410	24.685607
150.924192	4983.568568	24.690624
151.091532	4977.701616	24.695642
151.608888	4985.910687	24.700659
151.393687	5005.437241	24.705677
152.130007	5003.133679	24.710695
152.328437	5005.339350	24.715712
152.371004	5021.768594	24.720730
152.832007	5018.503550	24.725747
152.806196	5007.338433	24.730765
152.781572	5006.634350	24.735783
153.033143	5011.703705	24.740800
152.771413	5017.120792	24.745818
153.476338	5012.125507	24.750835
153.096573	5003.877178	24.755853
153.341773	5011.241496	24.760871
153.555520	5017.217627	24.765888
153.588490	5023.665480	24.770906
154.042168	5038.861773	24.775923
154.004105	5035.223163	24.780941
154.004044	5025.506135	24.785959
154.596641	5030.086882	24.790976
154.156117	5015.799472	24.795994
154.534669	5032.018614	24.801011
154.870456	5023.525608	24.806029
154.580822	5040.563229	24.811047
154.646417	5042.946632	24.816064
154.932471	5057.082479	24.821082
155.146822	5057.241829	24.826099
155.103011	5059.859800	24.831117
155.390080	5066.327737	24.836135
155.411821	5073.849646	24.841152
155.288232	5072.274750	24.846170
155.469283	5079.973441	24.851187
155.736961	5112.144560	24.856205
156.081815	5107.083927	24.861223
156.191380	5121.324281	24.866240
156.520247	5127.000471	24.871258
156.675254	5122.663953	24.876275
156.537194	5143.012274	24.881293
157.083853	5152.224509	24.886311
156.925663	5156.478155	24.891328
157.013405	5165.772216	24.896346
157.679247	5169.754464	24.901363
157.573219	5184.483954	24.906381
157.847693	5194.103844	24.911399
157.800663	5193.013915	24.916416
157.796681	5194.142657	24.921434
158.100729	5220.263320	24.926451
158.119317	5223.979029	24.931469
158.335100	5214.620022	24.936487
158.631613	5231.315036	24.941504
158.713414	5255.743627	24.946522
159.000064	5249.369800	24.951539
158.950495	5245.996513	24.956557
159.094561	5288.895352	24.961575
159.645757	5272.858897	24.966592
159.534471	5282.064397	24.971610
159.692010	5287.385633	24.976627
159.315302	5303.905636	24.981645
159.864585	5314.067093	24.986663
160.318831	5317.401054	24.991680
160.582516	5336.019378	24.996698
160.755475	5335.144535	25.001715
160.835230	5345.509099	25.006733
161.126928	5347.435625	25.011751
161.375392	5348.652365	25.016768
161.215578	5334.511845	25.021786
161.549596	5364.285325	25.026803
161.856017	5348.811750	25.031821
162.026662	5371.066106	25.036839
162.094067	5362.130302	25.041856
161.846582	5363.104350	25.046874
162.316783	5377.835785	25.051891
162.491366	5395.350495	25.056909
162.367665	5381.672257	25.061927
162.561208	5407.246809	25.066944
162.728245	5398.181815	25.071962
163.049181	5386.470232	25.076979
162.961818	5426.870059	25.081997
163.229795	5405.883864	25.087015
163.546169	5410.897399	25.092032
163.388373	5423.125028	25.097050
163.349496	5435.431259	25.102067
163.986461	5443.976323	25.107085
164.511845	5436.422856	25.112103
164.288449	5457.298929	25.117120
164.152999	5450.382616	25.122138
164.606394	5451.351138	25.127155
164.625945	5472.003627	25.132173
164.899664	5477.885422	25.137191
165.168739	5484.673454	25.142208
165.034012	5474.206630	25.147226
165.386910	5482.748229	25.152243
165.310515	5512.659029	25.157261
165.359899	5501.599555	25.162279
165.751276	5514.380085	25.167296
165.751183	5526.782480	25.172314
166.127831	5514.058082	25.177331
165.876373	5541.886912	25.182349
166.156179	5548.360154	25.187367
166.638092	5538.013683	25.192384
166.238508	5581.805630	25.197402
166.686825	5569.633040	25.202419
166.938607	5581.780557	25.207437
167.029634	5582.430026	25.212455
167.460679	5620.956408	25.217472
167.688212	5609.759100	25.222490
168.064061	5606.837924	25.227507
168.036104	5632.027290	25.232525
168.291512	5643.590541	25.237543
168.666725	5634.278231	25.242560
168.656127	5645.429172	25.247578
168.736442	5632.879360	25.252595
168.510450	5649.094865	25.257613
168.959133	5665.810171	25.262631
169.280217	5664.934510	25.267648
169.498355	5671.655225	25.272666
169.759858	5666.631293	25.277683
169.814085	5686.251108	25.282701
169.967371	5696.808743	25.287719
170.604398	5689.367945	25.292736
170.516474	5692.595683	25.297754
170.620465	5693.226569	25.302771
170.482777	5694.596945	25.307789
170.697655	5707.486026	25.312807
170.980527	5724.046889	25.317824
171.075199	5720.404256	25.322842
171.256090	5734.511893	25.327859
171.354512	5738.676806	25.332877
171.344759	5741.189556	25.337895
171.598296	5758.050151	25.342912
171.445198	5745.976441	25.347930
171.610362	5756.935024	25.352947
172.030914	5770.915590	25.357965
172.419245	5758.912112	25.362983
172.226489	5805.698247	25.368000
172.535964	5775.823647	25.373018
172.917229	5824.808468	25.378035
172.958018	5807.153492	25.383053
172.728290	5826.566225	25.388071
173.232848	5821.188018	25.393088
173.378113	5827.963692	25.398106
173.324324	5846.917281	25.403123
173.534821	5834.566826	25.408141
173.375365	5870.140245	25.413159
174.073627	5855.789265	25.418176
173.907137	5875.038569	25.423194
174.075040	5902.699737	25.428211
174.617083	5898.174630	25.433229
174.966385	5908.525729	25.438247
175.693664	5896.824492	25.443264
175.103858	5930.787006	25.448282
175.432449	5928.372087	25.453299
175.894401	5927.472382	25.458317
176.037648	5909.102339	25.463335
176.480063	5927.998170	25.468352
176.255475	5956.782515	25.473370
176.693356	5929.813759	25.478387
176.617216	5956.878259	25.483405
176.784589	5953.461572	25.488423
177.198892	5941.371200	25.493440
177.134682	5954.038289	25.498458
177.290379	5957.277597	25.503475
177.608255	5950.255738	25.508493
177.265380	5976.757018	25.513511
177.791180	5933.088538	25.518528
177.772282	5978.890061	25.523546
178.194066	5955.471181	25.528563
178.343607	5996.245472	25.533581
178.496579	5997.483786	25.538599
178.695821	5991.162126	25.543616
178.726276	5994.072888	25.548634
178.992071	6021.817015	25.553651
179.291751	6026.429046	25.558669
179.298045	6021.798134	25.563687
179.384467	6012.267284	25.568704
179.162749	6046.508891	25.573722
179.477200	6052.042198	25.578739
179.749692	6048.793613	25.583757
179.886299	6066.245157	25.588775
180.235959	6076.076287	25.593792
180.278024	6082.246225	25.598810
180.543072	6097.637330	25.603827
180.962405	6107.377915	25.608845
180.954247	6098.888776	25.613863
181.213519	6104.636236	25.618880
181.299114	6129.474773	25.623898
181.758413	6128.948394	25.628915
181.975226	6136.483806	25.633933
181.795072	6144.534878	25.638951
182.060233	6125.420547	25.643968
182.279211	6151.751538	25.648986
182.282280	6169.176500	25.654003
182.464986	6165.842288	25.659021
182.588894	6168.198483	25.664039
182.742561	6181.882117	25.669056
182.772039	6205.897358	25.674074
182.823556	6208.785136	25.679092
183.502420	6217.769275	25.684109
183.161055	6224.789497	25.689127
183.336133	6241.600215	25.694144
183.619729	6259.559606	25.699162
183.807095	6249.167550	25.704180
184.030160	6272.989971	25.709197
184.533152	6284.770739	25.714215
184.867722	6286.823518	25.719232
184.647123	6304.637544	25.724250
185.108975	6312.525783	25.729268
185.395125	6304.545838	25.734285
185.238148	6325.303976	25.739303
185.683999	6336.590377	25.744320
185.785700	6344.389711	25.749338
186.071937	6343.638368	25.754356
186.443175	6362.501261	25.759373
186.660358	6369.488370	25.764391
187.036053	6371.789513	25.769408
186.799327	6355.163131	25.774426
187.424332	6361.156862	25.779444
187.515203	6365.744068	25.784461
187.734041	6402.114443	25.789479
187.960327	6374.461880	25.794496
188.080022	6389.343046	25.799514
188.269781	6397.411601	25.804532
188.569544	6390.892796	25.809549
188.321011	6388.472248	25.814567
188.853278	6382.902967	25.819584
188.677551	6409.988892	25.824602
188.887853	6412.689327	25.829620
189.216512	6408.998212	25.834637
189.220760	6413.600028	25.839655
189.337240	6419.861308	25.844672
189.569961	6435.202848	25.849690
189.674597	6434.880121	25.854708
190.132830	6447.052090	25.859725
189.852195	6461.377972	25.864743
190.208902	6456.893260	25.869760
190.179367	6479.565138	25.874778
190.173133	6490.236888	25.879796
190.751569	6485.863945	25.884813
190.775459	6515.897684	25.889831
191.141656	6532.608246	25.894848
191.373763	6530.486339	25.899866
191.774141	6529.753771	25.904884
192.023081	6538.924657	25.909901
191.903406	6554.669457	25.914919
192.122433	6549.063505	25.919936
191.886444	6548.476438	25.924954
192.364660	6572.085582	25.929972
192.422077	6575.852089	25.934989
192.619249	6599.683099	25.940007
193.333564	6594.281410	25.945024
193.365220	6615.003590	25.950042
193.751266	6611.463776	25.955060
193.967943	6613.102678	25.960077
193.870624	6621.955888	25.965095
194.302433	6633.711307	25.970112
194.634987	6638.858011	25.975130
194.359280	6656.740252	25.980148
194.874571	6626.642305	25.985165
194.751225	6662.664260	25.990183
194.825670	6670.068435	25.995200
195.100681	6670.412471	26.000218
195.194837	6678.616009	26.005236
195.429579	6699.498690	26.010253
195.873071	6686.200884	26.015271
196.103471	6708.756934	26.020288
196.546370	6695.135854	26.025306
196.029701	6756.746597	26.030324
196.250736	6726.032110	26.035341
196.956677	6743.160815	26.040359
196.990926	6759.956022	26.045376
197.428330	6764.477097	26.050394
197.246128	6757.200199	26.055412
197.590346	6786.388787	26.060429
198.054988	6798.707153	26.065447
197.810043	6781.009231	26.070464
198.169578	6816.430596	26.075482
198.278344	6818.448638	26.080500
198.586916	6807.203679	26.085517
198.841836	6840.452978	26.090535
199.277188	6844.411862	26.095552
199.364004	6839.210823	26.100570
199.479625	6851.695805	26.105588
199.657132	6851.368535	26.110605
199.791871	6844.699601	26.115623
199.993086	6879.594826	26.120640
200.325359	6858.205300	26.125658
199.994130	6870.651381	26.130676
200.312395	6875.392110	26.135693
200.356113	6903.599729	26.140711
200.699007	6916.408881	26.145728
200.841453	6906.649802	26.150746
200.833732	6942.879811	26.155764
201.528811	6932.347337	26.160781
201.341719	6977.856971	26.165799
201.407987	6951.046308	26.170816
201.622972	6995.747609	26.175834
201.916260	6989.272849	26.180852
202.398141	6991.442296	26.185869
202.648190	7017.363899	26.190887
202.563899	7010.148373	26.195904
203.006566	7011.630132	26.200922
203.339798	7021.916917	26.205940
203.430178	7034.626376	26.210957
203.471284	7053.300450	26.215975
203.601745	7053.119150	26.220992
204.179881	7064.013662	26.226010
203.752392	7075.098383	26.231028
204.368726	7086.995484	26.236045
204.512150	7081.893913	26.241063
204.491047	7122.454607	26.246080
204.707917	7105.430131	26.251098
205.166041	7146.063202	26.256116
205.786358	7133.536190	26.261133
205.815388	7159.470456	26.266151
206.041465	7156.712123	26.271168
206.573230	7140.975741	26.276186
206.320769	7144.452682	26.281204
206.833233	7172.681295	26.286221
207.006599	7171.284642	26.291239
207.057641	7196.986509	26.296256
207.296768	7169.553081	26.301274
207.284326	7206.803382	26.306292
207.528928	7191.927052	26.311309
207.415153	7207.298664	26.316327
207.588235	7217.373503	26.321344
208.331399	7240.761309	26.326362
208.317941	7248.884755	26.331380
208.182491	7246.802455	26.336397
208.682648	7251.982456	26.341415
208.223696	7291.088596	26.346432
209.043794	7292.370958	26.351450
209.181534	7303.249302	26.356468
209.526390	7320.482660	26.361485
209.829257	7333.868199	26.366503
209.864429	7335.778450	26.371520
210.114186	7335.179223	26.376538
209.845798	7371.365282	26.381556
210.404600	7377.248035	26.386573
210.913231	7380.643050	26.391591
210.825494	7401.946351	26.396608
211.015677	7403.291368	26.401626
211.378700	7411.407606	26.406644
211.814967	7418.952756	26.411661
212.308891	7423.785257	26.416679
211.831289	7428.568841	26.421696
212.581787	7445.789615	26.426714
212.575036	7460.924123	26.431732
212.987976	7451.070428	26.436749
213.067344	7479.249068	26.441767
213.419289	7485.756518	26.446784
213.878979	7468.864444	26.451802
213.197387	7487.074387	26.456820
213.606324	7486.969074	26.461837
213.730268	7501.583954	26.466855
213.856216	7504.576569	26.471872
214.211457	7522.042190	26.476890
214.481051	7539.242166	26.481908
214.767752	7531.751663	26.486925
215.029011	7561.582880	26.491943
215.014534	7550.394364	26.496960
215.500005	7575.413925	26.501978
215.577123	7570.200800	26.506996
216.022516	7578.662001	26.512013
216.289483	7594.941890	26.517031
216.316801	7611.208066	26.522048
216.492459	7596.542960	26.527066
216.651002	7613.945626	26.532084
217.096692	7629.322913	26.537101
217.038978	7623.533282	26.542119
216.947899	7651.120981	26.547136
217.273608	7659.367621	26.552154
217.339746	7667.113525	26.557172
217.853197	7674.288501	26.562189
218.185683	7685.763964	26.567207
218.187215	7698.163986	26.572224
218.753183	7714.098927	26.577242
219.124343	7722.187289	26.582260
219.071020	7728.145726	26.587277
219.413692	7746.276119	26.592295
219.318562	7753.010742	26.597312
219.625247	7743.472784	26.602330
219.888538	7787.416571	26.607348
219.842550	7762.631886	26.612365
220.510572	7787.116779	26.617383
220.334854	7794.500020	26.622400
220.808899	7813.553744	26.627418
220.930896	7809.049394	26.632436
221.209656	7844.281519	26.637453
221.416467	7825.363144	26.642471
221.559869	7875.528852	26.647488
221.948278	7836.639359	26.652506
221.959525	7883.391661	26.657524
222.355012	7879.171017	26.662541
222.344616	7888.787725	26.667559
222.467762	7902.172526	26.672576
222.749931	7919.976799	26.677594
223.129570	7915.236216	26.682612
222.819410	7955.787034	26.687629
223.720258	7958.772676	26.692647
223.766727	7959.519054	26.697664
224.254457	7987.301523	26.702682
224.267154	7998.734569	26.707700
224.997102	8001.809621	26.712717
225.040635	7994.738477	26.717735
224.900708	8011.680888	26.722752
225.372015	8016.505391	26.727770
225.601016	8036.359331	26.732788
225.758937	8026.504993	26.737805
225.818591	8042.853826	26.742823
225.426593	8054.039048	26.747840
226.147205	8046.733274	26.752858
226.496724	8079.055180	26.757876
226.608704	8076.240117	26.762893
227.121961	8091.126356	26.767911
226.996906	8108.841545	26.772928
227.031653	8132.259099	26.777946
227.841870	8137.652800	26.782964
227.464697	8139.861000	26.787981
227.971635	8149.604716	26.792999
227.689881	8172.865450	26.798016
228.122384	8188.652220	26.803034
228.660470	8197.826835	26.808052
228.765108	8208.591519	26.813069
229.188985	8225.186219	26.818087
229.042388	8248.546702	26.823104
229.626250	8258.303408	26.828122
229.915616	8266.453891	26.833140
230.473729	8278.422614	26.838157
230.703100	8280.553825	26.843175
230.552775	8299.746251	26.848192
230.885380	8293.916964	26.853210
231.345438	8301.097612	26.858228
231.077711	8305.547439	26.863245
231.607025	8318.217149	26.868263
231.496423	8343.473864	26.873280
231.592613	8327.782061	26.878298
231.911160	8377.609950	26.883316
232.310378	8382.505866	26.888333
232.873654	8370.718696	26.893351
232.612674	8434.874932	26.898368
232.962616	8407.693031	26.903386
233.479782	8424.057486	26.908404
233.463047	8421.193631	26.913421
233.925894	8433.977113	26.918439
233.768226	8469.197662	26.923456
234.138803	8465.966762	26.928474
234.652563	8476.457911	26.933492
234.736171	8482.286237	26.938509
235.049680	8513.994783	26.943527
235.101758	8498.888175	26.948544
235.441639	8536.038434	26.953562
235.430129	8522.802869	26.958580
235.559922	8565.398731	26.963597
235.883615	8559.595154	26.968615
236.327546	8581.422857	26.973632
236.637552	8584.090492	26.978650
236.819382	8593.242666	26.983668
236.956463	8622.344347	26.988685
237.522742	8621.987339	26.993703
237.805657	8620.309493	26.998720
238.331010	8625.526100	27.003738
238.475341	8641.193255	27.008756
238.547232	8642.693372	27.013773
239.103054	8621.380573	27.018791
239.094622	8637.836910	27.023808
238.926116	8631.802518	27.028826
239.303040	8654.559285	27.033844
239.620448	8659.521054	27.038861
239.418344	8672.490203	27.043879
239.656376	8678.700017	27.048896
239.939793	8682.403497	27.053914
240.180884	8710.974947	27.058932
240.376839	8713.456986	27.063949
240.436889	8743.942703	27.068967
240.830049	8728.609172	27.073984
240.695610	8754.390505	27.079002
241.249134	8786.881300	27.084020
241.347937	8781.963310	27.089037
241.523573	8796.830107	27.094055
241.617465	8823.893973	27.099072
242.198858	8817.845421	27.104090
242.599190	8865.274517	27.109108
242.552283	8850.454805	27.114125
243.226762	8882.516566	27.119143
243.343142	8881.645823	27.124160
243.418665	8907.094938	27.129178
243.749926	8922.984398	27.134196
244.029598	8945.873569	27.139213
243.881873	8952.516394	27.144231
244.390719	8961.921196	27.149248
244.704673	8975.816748	27.154266
245.266692	8996.690237	27.159284
245.155388	9026.677021	27.164301
245.720156	9001.668993	27.169319
245.958767	9041.377122	27.174336
246.266148	9049.285557	27.179354
246.376669	9052.387963	27.184372
246.793978	9063.071166	27.189389
246.889083	9061.309896	27.194407
247.146388	9086.194863	27.199424
247.278333	9102.238645	27.204442
247.849056	9111.169413	27.209460
247.732305	9116.276078	27.214477
248.194658	9126.205778	27.219495
248.509515	9158.379748	27.224512
248.869664	9146.472873	27.229530
248.773796	9166.565808	27.234548
249.036596	9172.087676	27.239565
249.383387	9166.922687	27.244583
249.175429	9204.691906	27.249600
250.188500	9208.487356	27.254618
250.356149	9221.976024	27.259636
250.469498	9234.296942	27.264653
250.469641	9242.668753	27.269671
250.917318	9256.444891	27.274688
250.893693	9240.701587	27.279706
250.831450	9278.562261	27.284724
251.235708	9257.504462	27.289741
251.336548	9304.732061	27.294759
251.381650	9295.295406	27.299776
252.125282	9329.411156	27.304794
252.036905	9351.647462	27.309812
252.390431	9339.973233	27.314829
253.023379	9394.547453	27.319847
253.086984	9377.937879	27.324864
253.519229	9385.658982	27.329882
253.414414	9418.077062	27.334900
254.039857	9404.268231	27.339917
254.354025	9442.417926	27.344935
254.939110	9430.862135	27.349952
254.770323	9442.400756	27.354970
255.558590	9451.868750	27.359988
255.107930	9467.126801	27.365005
255.631518	9466.536184	27.370023
255.802343	9488.723513	27.375040
255.980533	9497.297261	27.380058
256.407866	9508.795219	27.385076
256.473102	9535.119338	27.390093
256.861919	9521.530679	27.395111
256.789367	9556.601330	27.400128
257.579916	9539.315036	27.405146
257.704077	9581.894234	27.410164
257.473604	9602.219314	27.415181
258.197899	9578.560439	27.420199
258.530673	9629.031972	27.425216
258.480998	9611.031212	27.430234
258.613296	9636.376122	27.435252
258.812816	9653.134086	27.440269
259.400353	9635.440544	27.445287
259.457980	9692.931024	27.450304
259.486631	9678.971935	27.455322
260.508778	9678.956571	27.460340
260.322737	9744.853055	27.465357
260.484752	9731.310979	27.470375
260.890054	9735.714550	27.475392
260.708444	9760.535244	27.480410
261.314716	9758.645600	27.485428
261.002069	9793.021261	27.490445
261.972322	9794.338179	27.495463
261.931796	9802.970963	27.500480
262.280858	9841.051979	27.505498
262.916127	9835.736518	27.510516
262.969269	9871.801834	27.515533
263.156897	9877.136064	27.520551
263.587786	9904.144632	27.525568
263.343676	9881.300654	27.530586
263.773168	9934.972036	27.535604
263.824625	9920.821009	27.540621
264.503196	9968.948589	27.545639
264.576312	9969.843096	27.550656
264.770310	9976.573557	27.555674
265.526986	9970.184201	27.560692
265.898658	9989.976691	27.565709
265.614318	10002.310082	27.570727
266.269827	9984.761898	27.575744
266.654957	10032.028716	27.580762
267.038706	9993.029708	27.585780
267.064305	10024.195177	27.590797
267.280806	10050.834872	27.595815
267.620931	10031.299899	27.600832
267.506425	10069.796913	27.605850
268.137843	10042.129257	27.610868
268.097462	10093.493234	27.615885
268.303905	10109.603343	27.620903
268.885095	10101.589315	27.625920
268.510395	10119.505632	27.630938
269.074685	10139.554070	27.635956
269.095924	10145.418562	27.640973
269.355131	10173.629106	27.645991
270.018808	10179.325904	27.651008
270.018707	10216.295296	27.656026
270.256789	10222.518341	27.661044
270.570359	10229.728787	27.666061
270.868992	10276.755189	27.671079
271.192148	10269.445995	27.676096
271.495661	10294.353153	27.681114
271.733146	10290.438365	27.686132
272.177385	10334.084589	27.691149
272.203271	10337.817333	27.696167
272.468819	10340.477819	27.701184
272.665528	10386.074379	27.706202
273.350097	10373.642263	27.711220
273.318977	10407.292949	27.716237
273.757701	10427.394051	27.721255
274.333871	10423.342227	27.726272
274.581529	10439.614927	27.731290
274.868736	10469.604431	27.736308
274.816082	10470.833799	27.741325
275.202061	10460.399693	27.746343
275.380825	10500.056697	27.751360
275.503949	10506.193909	27.756378
275.708611	10518.884191	27.761396
276.034484	10554.114810	27.766413
276.726209	10549.275667	27.771431
276.711117	10593.006080	27.776448
277.242833	10576.553520	27.781466
278.028257	10610.176830	27.786484
278.005694	10623.496792	27.791501
278.050280	10622.218331	27.796519
278.836471	10615.410846	27.801536
278.501186	10644.751105	27.806554
279.043709	10653.663300	27.811572
279.217111	10671.996188	27.816589
279.270511	10684.365629	27.821607
279.690693	10672.451920	27.826624
279.789200	10699.938684	27.831642
279.970249	10704.232302	27.836660
280.082239	10716.198549	27.841677
280.706050	10735.742900	27.846695
281.032474	10741.927686	27.851712
280.941111	10766.209166	27.856730
281.213672	10775.454855	27.861748
281.538464	10786.569964	27.866765
281.432014	10804.252709	27.871783
282.133689	10808.931638	27.876800
282.165294	10846.961134	27.881818
283.087360	10854.024538	27.886836
283.097213	10871.006511	27.891853
283.011505	10875.672832	27.896871
283.442841	10905.791339	27.901888
283.804198	10910.609927	27.906906
284.402787	10935.255881	27.911924
284.408802	10961.737138	27.916941
284.674564	10955.518481	27.921959
284.888561	10995.820838	27.926976
285.458246	10986.941703	27.931994
285.484614	11016.951835	27.937012
285.552694	11035.313757	27.942029
286.310809	11042.886203	27.947047
286.546777	11046.220871	27.952064
286.894796	11103.175052	27.957082
287.038001	11088.723806	27.962100
287.550995	11092.107593	27.967117
287.554949	11140.122942	27.972135
288.397691	11131.188008	27.977152
288.370750	11114.316284	27.982170
288.622841	11179.149342	27.987188
288.658045	11173.680363	27.992205
288.969585	11188.946564	27.997223
289.290996	11208.896239	28.002240
289.941179	11210.645226	28.007258
289.682632	11252.556663	28.012276
290.369963	11238.530504	28.017293
290.342981	11272.046704	28.022311
290.539121	11291.550151	28.027328
290.974462	11287.409973	28.032346
291.143687	11344.012648	28.037364
291.428545	11321.156548	28.042381
291.911441	11376.308085	28.047399
292.676037	11370.435533	28.052416
292.531178	11404.567762	28.057434
292.665738	11400.767077	28.062452
292.829869	11441.770950	28.067469
293.253553	11441.801018	28.072487
293.812716	11463.650381	28.077504
294.008412	11492.427189	28.082522
294.434613	11483.740630	28.087540
294.880190	11525.486698	28.092557
294.634521	11522.095230	28.097575
294.936403	11550.789117	28.102592
295.509821	11547.369419	28.107610
295.463492	11586.875093	28.112628
296.092173	11553.738058	28.117645
296.586425	11585.573446	28.122663
296.856325	11612.405335	28.127680
297.175468	11601.453005	28.132698
297.224111	11635.772137	28.137716
297.945319	11609.758954	28.142733
298.290650	11652.425642	28.147751
298.543022	11670.221035	28.152768
298.521666	11654.703866	28.157786
299.038661	11644.730517	28.162804
299.404071	11688.893393	28.167821
299.630442	11700.669049	28.172839
299.744285	11685.305810	28.177856
299.858585	11735.538268	28.182874
299.656597	11729.780271	28.187892
300.266648	11737.174405	28.192909
300.380589	11747.442355	28.197927
300.925924	11765.740127	28.202944
300.999353	11798.107378	28.207962
301.189800	11818.898036	28.212980
301.701811	11826.312167	28.217997
301.800039	11868.983037	28.223015
302.252920	11881.290191	28.228032
302.802254	11884.946590	28.233050
303.065404	11931.847662	28.238068
303.593673	11933.054222	28.243085
303.426291	11958.329993	28.248103
303.989407	11974.258942	28.253120
304.248543	11994.100346	28.258138
304.260586	12000.403835	28.263156
305.183564	12029.653689	28.268173
305.292436	12026.738434	28.273191
305.418427	12062.950075	28.278208
305.906856	12085.252362	28.283226
306.201675	12081.724260	28.288244
306.705270	12116.653172	28.293261
306.844054	12112.612767	28.298279
306.990903	12146.686802	28.303296
307.079174	12150.435634	28.308314
307.475906	12154.545757	28.313332
307.950058	12225.499526	28.318349
308.107761	12213.667763	28.323367
308.844834	12249.641978	28.328384
309.283437	12243.108370	28.333402
309.240806	12262.276485	28.338420
309.563019	12271.271393	28.343437
310.399280	12292.015076	28.348455
310.612584	12296.611752	28.353472
310.832671	12332.669733	28.358490
310.753134	12324.276193	28.363508
311.298858	12365.377010	28.368525
311.475356	12360.676479	28.373543
311.587243	12374.071793	28.378560
312.170062	12387.211046	28.383578
311.947004	12397.388912	28.388596
312.731634	12415.359308	28.393613
312.848536	12430.978910	28.398631
313.170136	12434.778190	28.403648
313.692351	12451.359166	28.408666
313.702170	12495.409487	28.413684
314.010068	12492.963397	28.418701
314.373762	12494.372932	28.423719
314.570461	12538.870956	28.428736
314.985074	12528.200654	28.433754
315.261151	12593.614851	28.438772
315.576999	12593.861049	28.443789
315.864860	12593.543831	28.448807
316.260774	12592.795392	28.453824
316.580804	12644.413048	28.458842
316.451898	12675.209566	28.463860
316.906586	12666.442238	28.468877
317.326700	12701.468450	28.473895
317.857357	12742.116775	28.478912
318.004266	12729.468748	28.483930
318.106105	12758.097243	28.488948
318.821002	12779.880805	28.493965
318.800160	12779.536235	28.498983
319.618811	12787.768364	28.504000
320.080720	12844.197192	28.509018
320.368020	12843.516622	28.514036
320.751818	12852.553225	28.519053
320.886265	12856.336589	28.524071
321.029383	12896.091363	28.529088
321.627071	12894.135040	28.534106
321.790236	12939.122267	28.539124
322.348061	12927.585888	28.544141
322.276340	12953.992505	28.549159
322.819454	12968.433759	28.554176
323.242437	12993.004027	28.559194
323.639024	12980.221355	28.564212
323.638066	13034.466277	28.569229
323.936715	13041.159203	28.574247
324.102722	13038.872594	28.579264
325.119090	13043.484189	28.584282
325.155634	13099.841846	28.589300
325.144129	13097.627988	28.594317
325.922453	13109.316394	28.599335
325.986013	13159.121668	28.604352
326.349336	13135.359727	28.609370
326.579258	13177.436349	28.614388
326.810738	13181.545936	28.619405
326.825334	13183.985410	28.624423
327.468737	13246.638014	28.629440
327.930017	13289.332559	28.634458
327.820763	13294.022068	28.639476
328.442651	13299.649406	28.644493
328.633860	13309.528683	28.649511
328.992174	13320.379595	28.654528
329.938965	13308.913773	28.659546
329.927400	13371.865682	28.664564
329.770577	13358.994765	28.669581
330.543006	13385.797343	28.674599
330.514962	13398.817974	28.679616
330.944785	13405.698942	28.684634
331.161862	13430.414502	28.689652
331.719600	13469.414796	28.694669
331.954688	13469.300196	28.699687
332.429985	13488.326323	28.704704
332.549698	13514.451922	28.709722
332.839207	13530.112844	28.714740
333.288009	13549.997300	28.719757
333.902235	13557.450316	28.724775
334.289884	13586.500611	28.729792
334.559567	13595.369886	28.734810
334.503782	13596.395941	28.739828
335.165585	13638.597078	28.744845
335.497505	13634.212415	28.749863
335.336372	13691.712239	28.754880
335.923830	13689.394978	28.759898
336.405595	13706.011329	28.764916
336.557042	13730.722487	28.769933
336.810016	13761.232474	28.774951
336.806686	13787.151059	28.779968
337.592430	13774.199057	28.784986
337.272284	13843.003481	28.790004
338.024935	13845.813874	28.795021
338.371525	13860.962665	28.800039
338.872008	13905.719336	28.805056
339.385513	13917.241093	28.810074
339.843386	13933.240739	28.815092
340.266263	13937.186122	28.820109
340.425827	13985.215694	28.825127
340.704655	13980.249130	28.830144
340.993560	14023.870261	28.835162
341.306671	14018.535543	28.840180
341.644368	14068.047432	28.845197
342.112520	14061.118708	28.850215
342.298048	14098.055995	28.855232
342.825578	14133.784118	28.860250
343.514927	14131.862240	28.865268
343.635672	14153.986088	28.870285
343.898777	14191.272347	28.875303
344.016109	14179.272318	28.880320
344.751260	14217.255230	28.885338
344.711365	14239.632780	28.890356
345.131229	14242.028312	28.895373
345.713403	14294.448521	28.900391
345.923717	14275.419678	28.905408
346.428377	14301.614997	28.910426
346.601064	14358.019965	28.915444
346.973940	14357.938016	28.920461
347.192120	14354.010907	28.925479
347.767516	14376.191627	28.930496
348.096790	14402.880948	28.935514
347.900924	14429.483670	28.940532
348.620321	14421.372075	28.945549
348.816640	14457.940315	28.950567
348.845693	14476.548676	28.955584
349.360912	14485.534717	28.960602
349.799293	14534.807537	28.965620
350.205735	14541.600160	28.970637
349.838115	14555.806863	28.975655
350.506884	14593.720115	28.980672
351.088695	14600.063089	28.985690
351.389923	14633.647564	28.990708
351.681888	14656.707580	28.995725
352.201237	14691.382210	29.000743
352.467006	14693.961086	29.005760
352.950573	14743.558195	29.010778
353.429062	14752.959191	29.015796
353.669849	14801.989434	29.020813
354.438612	14801.411548	29.025831
354.391729	14839.287321	29.030848
354.948141	14831.333732	29.035866
355.196165	14868.175250	29.040884
355.649600	14861.511930	29.045901
355.928248	14893.712066	29.050919
356.167455	14921.810374	29.055936
356.722555	14925.679453	29.060954
356.960392	14955.856536	29.065972
357.244015	14989.119780	29.070989
357.820523	15005.999849	29.076007
357.929141	15024.415339	29.081024
358.516343	15034.923410	29.086042
358.777500	15085.036374	29.091060
358.910901	15084.324542	29.096077
359.304209	15104.920981	29.101095
359.718714	15151.125139	29.106112
360.158690	15152.598255	29.111130
360.208277	15195.366204	29.116148
360.885945	15222.337190	29.121165
361.217884	15240.131277	29.126183
361.739722	15244.077474	29.131200
362.029396	15293.980328	29.136218
362.176432	15300.862154	29.141236
362.778880	15315.320108	29.146253
363.582457	15330.854036	29.151271
363.491303	15367.027151	29.156288
363.862497	15368.339734	29.161306
364.370885	15388.997729	29.166324
364.804370	15416.295400	29.171341
364.883047	15426.045592	29.176359
365.139802	15473.026203	29.181376
365.875953	15469.152076	29.186394
365.755798	15498.909524	29.191412
366.488126	15529.081961	29.196429
366.886057	15534.113196	29.201447
367.331592	15571.414986	29.206464
367.721528	15577.509678	29.211482
367.819642	15605.713005	29.216500
368.393286	15596.301379	29.221517
368.795694	15635.089993	29.226535
368.755560	15655.366066	29.231552
369.228630	15664.469933	29.236570
369.538953	15673.289371	29.241588
369.855046	15716.355606	29.246605
370.127266	15712.901037	29.251623
370.255636	15750.534154	29.256640
370.763597	15774.335592	29.261658
371.152532	15788.102673	29.266676
371.560475	15813.606082	29.271693
371.654798	15848.785423	29.276711
371.986728	15854.354340	29.281728
372.448195	15899.480678	29.286746
372.824299	15910.589121	29.291764
373.263115	15954.421454	29.296781
373.980463	15956.998563	29.301799
374.422318	15992.547679	29.306816
374.587699	16015.872683	29.311834
375.091076	16055.244288	29.316852
375.143283	16059.664078	29.321869
375.699653	16091.214425	29.326887
375.728234	16122.833974	29.331904
376.468956	16133.007774	29.336922
376.717451	16191.314544	29.341940
377.337200	16191.947557	29.346957
378.242656	16220.309645	29.351975
378.503695	16243.648193	29.356992
378.896747	16253.671206	29.362010
379.070836	16268.726867	29.367028
379.484755	16296.269046	29.372045
380.130140	16320.723240	29.377063
380.265454	16340.485139	29.382080
380.674623	16337.151698	29.387098
381.055733	16397.216756	29.392116
381.242981	16415.676990	29.397133
381.855024	16399.766128	29.402151
381.882535	16450.207049	29.407168
382.325852	16455.332229	29.412186
382.861513	16494.970642	29.417204
382.732116	16511.685270	29.422221
383.611675	16532.666813	29.427239
383.576293	16581.361569	29.432256
384.236048	16569.335643	29.437274
384.257723	16634.762609	29.442292
384.265597	16637.570777	29.447309
384.805618	16685.355997	29.452327
385.342076	16690.636865	29.457344
385.918928	16764.927574	29.462362
385.938136	16760.390116	29.467380
386.840306	16814.709428	29.472397
387.368530	16798.083071	29.477415
387.552974	16833.090581	29.482432
388.274366	16870.200908	29.487450
389.016819	16848.381216	29.492468
388.886804	16907.790828	29.497485
389.792483	16902.774140	29.502503
390.091815	16917.267247	29.507520
390.224769	16936.936599	29.512538
390.553764	16945.797788	29.517556
390.555599	16973.727957	29.522573
391.441153	16982.023191	29.527591
391.499980	17004.677684	29.532608
391.681537	17025.643376	29.537626
392.362928	17049.690487	29.542644
393.001577	17080.766629	29.547661
393.011438	17080.565869	29.552679
393.361303	17121.695559	29.557696
393.639681	17156.895508	29.562714
394.064736	17157.811136	29.567732
394.059471	17211.241312	29.572749
394.738122	17200.147415	29.577767
394.970988	17271.141421	29.582784
395.368500	17278.170626	29.587802
395.943636	17301.080855	29.592820
395.961538	17350.122067	29.597837
396.849330	17378.425343	29.602855
397.202491	17394.921931	29.607872
397.561014	17420.496900	29.612890
398.240908	17456.687787	29.617908
398.077972	17500.857581	29.622925
398.908732	17508.716207	29.627943
399.333187	17521.624347	29.632960
399.865818	17579.480703	29.637978
400.285026	17581.916842	29.642996
400.241264	17621.193227	29.648013
401.017599	17648.880955	29.653031
401.418541	17663.026911	29.658048
402.074093	17674.705546	29.663066
402.324073	17732.078613	29.668084
402.608916	17739.086024	29.673101
403.236696	17758.454375	29.678119
403.523035	17793.911771	29.683136
403.388960	17815.228405	29.688154
404.314722	17808.195394	29.693172
404.874176	17884.415188	29.698189
405.049945	17877.323696	29.703207
405.869542	17919.364660	29.708224
406.169460	17921.971424	29.713242
406.361346	17966.636569	29.718260
406.840757	17963.889296	29.723277
407.153067	18012.838264	29.728295
407.929545	18004.743780	29.733312
408.122318	18062.811989	29.738330
408.671356	18044.267318	29.743348
408.565468	18081.843058	29.748365
408.922094	18115.255657	29.753383
409.441810	18128.856769	29.758400
409.628976	18130.307973	29.763418
409.990246	18176.346466	29.768436
410.447460	18194.966006	29.773453
410.835913	18220.709572	29.778471
411.420482	18215.920598	29.783488
410.983343	18287.283477	29.788506
411.881561	18299.950853	29.793524
412.479804	18310.081887	29.798541
412.589876	18385.345666	29.803559
413.003989	18378.363803	29.808576
413.536407	18416.977200	29.813594
413.811982	18482.295742	29.818612
414.253415	18517.475959	29.823629
414.449185	18521.873779	29.828647
415.394180	18525.137697	29.833664
415.456726	18563.064921	29.838682
416.031944	18621.623489	29.843700
416.156906	18616.587547	29.848717
416.861939	18670.135175	29.853735
417.158786	18714.296586	29.858752
417.935110	18708.984010	29.863770
418.493541	18779.479916	29.868788
418.576222	18804.104676	29.873805
419.225123	18810.023286	29.878823
419.729122	18883.135398	29.883840
419.797315	18890.394580	29.888858
420.689435	18903.795316	29.893876
420.996129	18925.679076	29.898893
421.306504	18965.331181	29.903911
421.908038	18975.458981	29.908928
422.175926	19022.968802	29.913946
422.942414	19032.604609	29.918964
422.426602	19087.955271	29.923981
423.540506	19103.252361	29.928999
423.687915	19123.194434	29.934016
423.678942	19169.965732	29.939034
424.560010	19208.754693	29.944052
425.041062	19209.767443	29.949069
425.204797	19266.415619	29.954087
425.753834	19278.700056	29.959104
425.874144	19323.732286	29.964122
426.857343	19354.026795	29.969140
426.913104	19403.475951	29.974157
427.683335	19414.857910	29.979175
427.971468	19462.432778	29.984192
428.596195	19474.330497	29.989210
429.041172	19514.052324	29.994228
429.582842	19551.041421	29.999245
429.776862	19564.270867	30.004263
430.235885	19591.318903	30.009280
430.466204	19635.567547	30.014298
431.473499	19626.949620	30.019316
431.672625	19675.456287	30.024333
432.309797	19707.848441	30.029351
432.865058	19734.097498	30.034368
433.288395	19729.213281	30.039386
434.004247	19762.832447	30.044404
434.251765	19765.059669	30.049421
434.459210	19773.935354	30.054439
434.719822	19821.452707	30.059456
434.939941	19808.668905	30.064474
435.399665	19856.801926	30.069492
435.195503	19877.356911	30.074509
435.880793	19920.433818	30.079527
436.702335	19942.631897	30.084544
436.841069	19979.430676	30.089562
437.294774	19996.142579	30.094580
437.534540	20051.907027	30.099597
437.746838	20075.556780	30.104615
438.517059	20094.427974	30.109632
438.450923	20131.959012	30.114650
439.057108	20165.885519	30.119668
439.826463	20218.032454	30.124685
440.275136	20233.781951	30.129703
440.872130	20274.274083	30.134720
441.122962	20321.887044	30.139738
441.479065	20323.057194	30.144756
441.722429	20373.383944	30.149773
442.469212	20411.827190	30.154791
442.951058	20428.946138	30.159808
443.543877	20483.156526	30.164826
444.023212	20512.687422	30.169844
444.230178	20560.410469	30.174861
444.780397	20579.633081	30.179879
445.314454	20614.744224	30.184896
445.992895	20651.078643	30.189914
446.325787	20671.462097	30.194932
446.619651	20710.425130	30.199949
447.107914	20739.964483	30.204967
447.864295	20793.410437	30.209984
447.913281	20818.735556	30.215002
448.793767	20839.004038	30.220020
448.778882	20865.242272	30.225037
449.213512	20910.921606	30.230055
450.179231	20933.566698	30.235072
450.030558	20968.333007	30.240090
450.595730	21005.493879	30.245108
451.145147	21034.576351	30.250125
451.570989	21077.606825	30.255143
452.043166	21111.887096	30.260160
452.179758	21143.357113	30.265178
452.887261	21173.816432	30.270196
453.292481	21227.207587	30.275213
453.584106	21263.443609	30.280231
454.729036	21291.142525	30.285248
454.556306	21321.792361	30.290266
455.038537	21350.688455	30.295284
455.323160	21390.166540	30.300301
456.039725	21426.586466	30.305319
456.421659	21472.259686	30.310336
456.814420	21485.552029	30.315354
457.472355	21507.577586	30.320372
457.845709	21550.279474	30.325389
457.880271	21559.365242	30.330407
458.878098	21618.268984	30.335424
458.935413	21624.837352	30.340442
459.583257	21687.978923	30.345460
460.119015	21700.945468	30.350477
460.625408	21739.970133	30.355495
460.998434	21763.518864	30.360512
461.135198	21795.974590	30.365530
461.681419	21816.451953	30.370548
462.380335	21868.606159	30.375565
462.698164	21898.360315	30.380583
463.587309	21906.895113	30.385600
463.699301	21959.681801	30.390618
464.546111	21991.809034	30.395636
464.780872	22015.913344	30.400653
465.450840	22068.935988	30.405671
466.209948	22061.881405	30.410688
465.860608	22137.627047	30.415706
466.778896	22138.913342	30.420724
467.161469	22171.379515	30.425741
467.429084	22235.441510	30.430759
468.505933	22241.108204	30.435776
468.597971	22273.741367	30.440794
469.117861	22313.265411	30.445812
469.425931	22340.624595	30.450829
470.161904	22361.282725	30.455847
470.284990	22420.626521	30.460864
470.691339	22430.606535	30.465882
471.347274	22491.419606	30.470900
471.974136	22511.471552	30.475917
471.786068	22553.039330	30.480935
472.494690	22584.428985	30.485952
472.909055	22648.652001	30.490970
473.591900	22667.481558	30.495988
474.093053	22702.239144	30.501005
474.411239	22731.499424	30.506023
474.845538	22781.510092	30.511040
475.329353	22816.730647	30.516058
475.997961	22859.610370	30.521076
476.781594	22888.017077	30.526093
476.961538	22925.147375	30.531111
477.389183	22970.501044	30.536128
477.993449	23010.085855	30.541146
478.590462	23039.765404	30.546164
479.007017	23077.346685	30.551181
479.423502	23099.056154	30.556199
479.979139	23155.789042	30.561216
480.274585	23158.061499	30.566234
480.744384	23226.844612	30.571252
481.263989	23238.607591	30.576269
481.508081	23284.273365	30.581287
481.893804	23307.119828	30.586304
483.073324	23345.496217	30.591322
483.441936	23359.854135	30.596340
483.831202	23408.075031	30.601357
484.249128	23442.376505	30.606375
485.112776	23443.057280	30.611392
485.215304	23504.074245	30.616410
485.587744	23515.102385	30.621428
485.939922	23546.995747	30.626445
486.314149	23600.803935	30.631463
486.948938	23624.941500	30.636480
486.692237	23665.974934	30.641498
487.382464	23706.926165	30.646516
488.354269	23745.381511	30.651533
488.176275	23781.488611	30.656551
489.150843	23829.289899	30.661568
489.440349	23876.247398	30.666586
490.042409	23906.970620	30.671604
490.494248	23942.785577	30.676621
491.046674	23989.708621	30.681639
491.424126	24030.048880	30.686656
491.948885	24075.869143	30.691674
492.366873	24107.661782	30.696692
492.769349	24175.253041	30.701709
493.409390	24208.695324	30.706727
494.013456	24246.243211	30.711744
494.709263	24292.325926	30.716762
495.021892	24335.007210	30.721780
496.028966	24369.293253	30.726797
496.211072	24415.487294	30.731815
496.874076	24442.441489	30.736832
497.400128	24483.880095	30.741850
497.751601	24523.041864	30.746868
498.392035	24553.468786	30.751885
498.754860	24595.106971	30.756903
499.129732	24638.164331	30.761920
499.526125	24674.436388	30.766938
499.910048	24718.537785	30.771956
500.563577	24756.190065	30.776973
501.260886	24800.054301	30.781991
501.581462	24855.310461	30.787008
502.017198	24894.688156	30.792026
502.452249	24948.630642	30.797044
503.275791	24978.298226	30.802061
503.558510	25017.150780	30.807079
504.242091	25059.709542	30.812096
504.878353	25113.722153	30.817114
504.808447	25132.342140	30.822132
505.790394	25197.442925	30.827149
505.949776	25216.615699	30.832167
506.393149	25282.562760	30.837184
507.148008	25311.823629	30.842202
507.155421	25374.364305	30.847220
508.563898	25400.639744	30.852237
508.622804	25441.721214	30.857255
509.834709	25490.432612	30.862272
510.198340	25507.540867	30.867290
510.507046	25541.471981	30.872308
511.195051	25566.320076	30.877325
511.647037	25602.033191	30.882343
511.802566	25629.515300	30.887360
512.129755	25679.714431	30.892378
512.685609	25693.312834	30.897396
513.139977	25747.556649	30.902413
513.348829	25798.767555	30.907431
514.230733	25823.730900	30.912448
514.472502	25859.499343	30.917466
514.931662	25929.856364	30.922484
515.755851	25934.077407	30.927501
516.032252	26007.141437	30.932519
516.394016	26032.023314	30.937536
516.884823	26101.169208	30.942554
518.184973	26109.752719	30.947572
518.671477	26170.673829	30.952589
519.649326	26185.586387	30.957607
519.712430	26239.994236	30.962624
520.518257	26241.340585	30.967642
520.524617	26312.861674	30.972660
521.295350	26314.512184	30.977677
521.951665	26383.775524	30.982695
522.504462	26399.612291	30.987712
522.760717	26456.497590	30.992730
523.503956	26486.299732	30.997748
523.619448	26520.360594	31.002765
523.753468	26576.767912	31.007783
524.297811	26605.425797	31.012800
525.128998	26679.067053	31.017818
525.141752	26715.080281	31.022836
525.958257	26747.029779	31.027853
526.431312	26812.389937	31.032871
526.944096	26872.895939	31.037888
527.107133	26903.790192	31.042906
528.241446	26925.228274	31.047924
528.876822	26989.384754	31.052941
528.987885	27060.909827	31.057959
529.769032	27087.441601	31.062976
530.668627	27164.483027	31.067994
530.988195	27169.739605	31.073012
531.555514	27248.489544	31.078029
531.984456	27260.202202	31.083047
532.622298	27329.260641	31.088064
532.890731	27372.649563	31.093082
533.581434	27392.367424	31.098100
534.000609	27448.405437	31.103117
534.403042	27523.662198	31.108135
534.818882	27550.323036	31.113152
535.466001	27588.131124	31.118170
536.337097	27640.776336	31.123188
537.058708	27653.048513	31.128205
537.386598	27731.809011	31.133223
538.108798	27792.392264	31.138240
538.437538	27788.700084	31.143258
538.555570	27863.213522	31.148276
539.536798	27900.298676	31.153293
539.404303	27939.935866	31.158311
540.648582	27957.270470	31.163328
541.163900	28026.328564	31.168346
541.453743	28054.526920	31.173364
542.270990	28118.721964	31.178381
543.158840	28115.309382	31.183399
543.562391	28190.151511	31.188416
544.454527	28208.544631	31.193434
544.690622	28243.166642	31.198452
545.036372	28287.521873	31.203469
545.570039	28317.739760	31.208487
545.825075	28372.862474	31.213504
546.963818	28378.005535	31.218522
546.835013	28471.078384	31.223540
547.340394	28502.347418	31.228557
547.788450	28517.160604	31.233575
548.614896	28569.942813	31.238592
548.854868	28631.910746	31.243610
549.807397	28653.564467	31.248628
550.476501	28711.069552	31.253645
551.335948	28745.858094	31.258663
551.325150	28816.336458	31.263680
552.271484	28833.873894	31.268698
552.507230	28886.269022	31.273716
553.259152	28921.634472	31.278733
553.461111	28980.943555	31.283751
554.267351	29011.508554	31.288768
554.389603	29080.889030	31.293786
555.284616	29097.500475	31.298804
556.165223	29163.008530	31.303821
556.344534	29202.520358	31.308839
556.883452	29239.617583	31.313856
557.551890	29304.342147	31.318874
557.906416	29339.147771	31.323892
558.130871	29401.288153	31.328909
559.312029	29443.197025	31.333927
559.302706	29507.752990	31.338944
560.292504	29551.783769	31.343962
560.561589	29636.104378	31.348980
561.144537	29637.269077	31.353997
561.957157	29730.818531	31.359015
562.301231	29748.268502	31.364032
563.270398	29817.443181	31.369050
563.690552	29835.256189	31.374068
563.690566	29905.349886	31.379085
564.943519	29927.126097	31.384103
565.127745	30009.646733	31.389120
565.948188	30033.568999	31.394138
566.164878	30109.959456	31.399156
567.028466	30149.709735	31.404173
567.238125	30198.622607	31.409191
567.696385	30264.511246	31.414208
568.593091	30299.613956	31.419226
569.205419	30341.199696	31.424244
569.722616	30408.833541	31.429261
570.190171	30432.360302	31.434279
570.560311	30470.629771	31.439296
571.404101	30514.588707	31.444314
572.005734	30563.790112	31.449332
572.496068	30600.792594	31.454349
573.154187	30671.443526	31.459367
573.834136	30705.331895	31.464384
574.229470	30750.964066	31.469402
574.694336	30784.741863	31.474420
575.094086	30858.132811	31.479437
575.463279	30906.470806	31.484455
576.370138	30961.952378	31.489472
576.752042	30995.959734	31.494490
577.430389	31070.443559	31.499508
577.922827	31119.055692	31.504525
578.536884	31174.085020	31.509543
578.841293	31206.185577	31.514560
579.966960	31277.109818	31.519578
580.814279	31326.892198	31.524596
580.557546	31388.631363	31.529613
581.522913	31414.575121	31.534631
581.807399	31503.939922	31.539648
582.861066	31530.210228	31.544666
583.316243	31605.784826	31.549684
584.166845	31650.628328	31.554701
585.078903	31692.179238	31.559719
585.263024	31742.929024	31.564736
585.967156	31804.255111	31.569754
587.284522	31841.962444	31.574772
587.414571	31874.988864	31.579789
588.655646	31937.267002	31.584807
589.017432	31971.055786	31.589824
589.882107	31997.098465	31.594842
590.201744	32063.996756	31.599860
590.808265	32081.325478	31.604877
591.426649	32126.207265	31.609895
591.725336	32165.797091	31.614912
592.144302	32200.321163	31.619930
592.976060	32257.812869	31.624948
593.381265	32304.581023	31.629965
594.007250	32347.808859	31.634983
594.354836	32374.839176	31.640000
595.314422	32435.540628	31.645018
595.928115	32465.417765	31.650036
596.221837	32529.773473	31.655053
597.312148	32581.913556	31.660071
597.403150	32618.749347	31.665088
598.361699	32661.371823	31.670106
598.893403	32715.831539	31.675124
599.272044	32761.043251	31.680141
599.683950	32787.846495	31.685159
600.164986	32863.715929	31.690176
601.214274	32875.935971	31.695194
601.839298	32918.221335	31.700212
602.083802	32969.810123	31.705229
602.764647	33001.351447	31.710247
602.769236	33057.152447	31.715264
603.706195	33087.020221	31.720282
604.279751	33170.391619	31.725300
604.379633	33196.245904	31.730317
605.021931	33261.601866	31.735335
605.982894	33319.112962	31.740352
606.369114	33361.489506	31.745370
607.051932	33415.919591	31.750388
607.505798	33472.706522	31.755405
608.297357	33529.737783	31.760423
608.606453	33575.771412	31.765440
609.047139	33632.849443	31.770458
609.773210	33717.748766	31.775476
610.268414	33756.218778	31.780493
610.926294	33831.240116	31.785511
611.802646	33861.968555	31.790528
612.258735	33958.485052	31.795546
612.734160	33998.635934	31.800564
613.538735	34067.993486	31.805581
613.958867	34114.401851	31.810599
614.695787	34196.447241	31.815616
615.215466	34236.013152	31.820634
616.120859	34323.695997	31.825652
617.152350	34366.774710	31.830669
617.597714	34414.352675	31.835687
618.374914	34490.779841	31.840704
619.537448	34517.471101	31.845722
619.811307	34592.326891	31.850740
619.977423	34648.295112	31.855757
621.080404	34701.246971	31.860775
621.791198	34749.105206	31.865792
622.336092	34803.429405	31.870810
623.251777	34855.910301	31.875828
623.297889	34891.880265	31.880845
624.153653	34961.320106	31.885863
624.347132	35013.990587	31.890880
625.336455	35054.606050	31.895898
625.830261	35111.289772	31.900916
626.120294	35194.891481	31.905933
626.842227	35238.225108	31.910951
627.101812	35299.045394	31.915968
627.924453	35370.713369	31.920986
628.751232	35404.123008	31.926004
629.310398	35491.023766	31.931021
629.882453	35543.632490	31.936039
630.577769	35605.174303	31.941056
631.459163	35665.397189	31.946074
632.144773	35725.657773	31.951092
632.125180	35802.112215	31.956109
633.226547	35847.828935	31.961127
633.649203	35902.827262	31.966144
634.002400	35969.527892	31.971162
634.861787	36020.055576	31.976180
635.541152	36040.577105	31.981197
636.162897	36131.175943	31.986215
636.336155	36207.133315	31.991232
637.112937	36253.609098	31.996250
637.683598	36291.153873	32.001268
638.438749	36354.416762	32.006285
639.213296	36439.993857	32.011303
640.163744	36469.534533	32.016320
640.684418	36563.147178	32.021338
641.826488	36584.232620	32.026356
641.824383	36652.657355	32.031373
642.711727	36700.296022	32.036391
642.801978	36786.336987	32.041408
644.174854	36812.238567	32.046426
644.230750	36918.333032	32.051444
644.796582	36952.168852	32.056461
645.350591	37022.384230	32.061479
646.134139	37069.774036	32.066496
646.541146	37163.322995	32.071514
647.570673	37214.688014	32.076532
648.098141	37294.363522	32.081549
649.001103	37329.486528	32.086567
649.361664	37430.648281	32.091584
650.702400	37453.656607	32.096602
651.592918	37547.053465	32.101620
651.876013	37573.571197	32.106637
652.630387	37666.459075	32.111655
652.800295	37726.608741	32.116672
653.800776	37762.975282	32.121690
654.399994	37868.158345	32.126708
654.997362	37901.060840	32.131725
655.919370	37932.021308	32.136743
656.387274	38055.225487	32.141760
657.349334	38106.764800	32.146778
657.698646	38131.454973	32.151796
658.465296	38187.334680	32.156813
659.353459	38288.080172	32.161831
659.804329	38306.627444	32.166848
660.500314	38400.655998	32.171866
661.215601	38439.593699	32.176884
661.597043	38503.023519	32.181901
662.647418	38573.464338	32.186919
662.833597	38610.217790	32.191936
663.766854	38695.625011	32.196954
664.562054	38726.769537	32.201972
665.299028	38804.287101	32.206989
666.094550	38846.038469	32.212007
666.761643	38919.882860	32.217024
666.907204	38975.100920	32.222042
667.433388	39040.851182	32.227060
668.282757	39111.838696	32.232077
669.097847	39151.055428	32.237095
669.644704	39237.206490	32.242112
669.959303	39268.994596	32.247130
671.231181	39296.943849	32.252148
670.926660	39411.157658	32.257165
672.109440	39455.929922	32.262183
673.029755	39477.336577	32.267200
673.425200	39573.781538	32.272218
673.666173	39623.570203	32.277236
674.728415	39684.806793	32.282253
675.291581	39741.362648	32.287271
675.905548	39803.440523	32.292288
676.726127	39878.740565	32.297306
677.521336	39923.541083	32.302324
677.990056	40011.178125	32.307341
678.479708	40056.021331	32.312359
679.521543	40121.152830	32.317376
680.032020	40210.788434	32.322394
680.419706	40242.691300	32.327412
680.845355	40343.893222	32.332429
682.137239	40378.635837	32.337447
682.802030	40491.811642	32.342464
683.415083	40525.782729	32.347482
684.271636	40613.143515	32.352500
684.723971	40667.778934	32.357517
685.197887	40726.656132	32.362535
686.141155	40814.396795	32.367552
687.021562	40880.421054	32.372570
687.655286	40938.513465	32.377588
688.170804	41018.102748	32.382605
688.929406	41091.393238	32.387623
689.779624	41135.465954	32.392640
690.046593	41245.658701	32.397658
691.062924	41276.935143	32.402676
691.742915	41378.241480	32.407693
692.672859	41432.070020	32.412711
693.352941	41487.692109	32.417728
694.050948	41576.497619	32.422746
694.476631	41630.936932	32.427764
695.198446	41721.852575	32.432781
696.232420	41774.486037	32.437799
696.781824	41845.890697	32.442816
697.164550	41933.414097	32.447834
698.226461	41986.841738	32.452852
699.137330	42059.795157	32.457869
699.428557	42144.353610	32.462887
700.464116	42206.951890	32.467904
700.659615	42262.928049	32.472922
701.366808	42347.733538	32.477940
702.015488	42430.075922	32.482957
702.918733	42496.153251	32.487975
703.848138	42558.315517	32.492992
704.185844	42653.747761	32.498010
705.144098	42701.768958	32.503028
705.950636	42762.935880	32.508045
706.556952	42868.864716	32.513063
707.310975	42896.315669	32.518080
708.188489	42975.577264	32.523098
708.759482	43016.819466	32.528116
709.215912	43096.180192	32.533133
709.614583	43159.611969	32.538151
710.754401	43202.303344	32.543168
711.256381	43306.257979	32.548186
711.818052	43346.868443	32.553204
712.539175	43445.152296	32.558221
713.196448	43494.863870	32.563239
713.903284	43571.704467	32.568256
714.401447	43640.822068	32.573274
715.164546	43718.635366	32.578292
715.936664	43802.497683	32.583309
716.758611	43847.815240	32.588327
717.843655	43939.113778	32.593344
717.809365	44026.783594	32.598362
719.174423	44073.166651	32.603380
719.911411	44152.408707	32.608397
720.388908	44252.877806	32.613415
721.388900	44290.811974	32.618432
722.024013	44379.099386	32.623450
723.021611	44449.008197	32.628468
723.765508	44519.049158	32.633485
724.582399	44580.728755	32.638503
725.102877	44683.846464	32.643520
725.364054	44735.217703	32.648538
726.587189	44818.167725	32.653556
727.137293	44864.095889	32.658573
727.608443	44953.289295	32.663591
728.379950	45032.040917	32.668608
729.353680	45104.937277	32.673626
730.048674	45181.389419	32.678644
730.447937	45272.362500	32.683661
731.092962	45325.999359	32.688679
732.414293	45412.990331	32.693696
732.720704	45514.096500	32.698714
733.537820	45580.454870	32.703732
734.523109	45627.277962	32.708749
735.010402	45735.170803	32.713767
735.715732	45825.577520	32.718784
736.623235	45860.949267	32.723802
737.409081	45971.029610	32.728820
738.271333	46057.737238	32.733837
738.968602	46109.882289	32.738855
740.144384	46205.661276	32.743872
740.503370	46282.575553	32.748890
741.318155	46359.935009	32.753908
741.992953	46412.895338	32.758925
742.564678	46519.788960	32.763943
743.238479	46581.662482	32.768960
744.038004	46642.752725	32.773978
744.820476	46746.935680	32.778996
745.579303	46809.345429	32.784013
746.125912	46906.278997	32.789031
746.925239	46964.004068	32.794048
747.667955	47038.525918	32.799066
748.327679	47120.538602	32.804084
749.373527	47190.352938	32.809101
749.574536	47238.116029	32.814119
750.412013	47325.537450	32.819136
751.237247	47403.183804	32.824154
751.851649	47482.444740	32.829172
752.921918	47537.478334	32.834189
753.078224	47641.895631	32.839207
754.492803	47701.304661	32.844224
754.981194	47783.029048	32.849242
755.482586	47882.016548	32.854260
756.858280	47947.408398	32.859277
757.062590	48002.511876	32.864295
757.892889	48109.512842	32.869312
758.993615	48160.366111	32.874330
759.879168	48257.590782	32.879348
760.678519	48325.271787	32.884365
761.044117	48402.124878	32.889383
762.181919	48488.015013	32.894400
762.879895	48545.458514	32.899418
763.502950	48656.054892	32.904436
764.385183	48697.989875	32.909453
765.146991	48785.638840	32.914471
765.782525	48895.827701	32.919488
766.388734	48953.119903	32.924506
767.385118	49048.832519	32.929524
768.284596	49118.892369	32.934541
768.843255	49228.537042	32.939559
770.029373	49272.135226	32.944576
770.615672	49352.235744	32.949594
771.225825	49443.016999	32.954612
772.411856	49508.959166	32.959629
772.751567	49595.521290	32.964647
773.829595	49682.199823	32.969664
774.736317	49770.928693	32.974682
775.578812	49853.480352	32.979700
776.204719	49927.824742	32.984717
776.670232	49995.066707	32.989735
777.710642	50085.811167	32.994752
778.485850	50138.501658	32.999770
778.669306	50244.977918	33.004788
779.926790	50317.361645	33.009805
780.691532	50397.021940	33.014823
781.482987	50491.664200	33.019840
782.383397	50577.722168	33.024858
782.837562	50633.854338	33.029876
783.918812	50744.128884	33.034893
784.622025	50803.686830	33.039911
785.235421	50899.524026	33.044928
786.057766	50984.378300	33.049946
786.351152	51090.671703	33.054964
787.690448	51150.123255	33.059981
788.426868	51264.144911	33.064999
789.322721	51305.430665	33.070016
790.013898	51414.079965	33.075034
790.961012	51455.351595	33.080052
791.570382	51526.533754	33.085069
792.123240	51611.869395	33.090087
793.099863	51679.929450	33.095104
794.061820	51765.292230	33.100122
794.619235	51824.024715	33.105140
795.420881	51907.065756	33.110157
795.915348	52005.727030	33.115175
797.239833	52055.735346	33.120192
797.632814	52181.241714	33.125210
798.478399	52229.780354	33.130228
800.199128	52294.423258	33.135245
800.274080	52391.597561	33.140263
801.075423	52478.851293	33.145280
801.854245	52554.637163	33.150298
802.054945	52637.521596	33.155316
803.369594	52725.947749	33.160333
803.796110	52808.074308	33.165351
804.941471	52878.191856	33.170368
805.682389	53002.818550	33.175386
806.716357	53065.500027	33.180404
807.708189	53139.038921	33.185421
808.103103	53244.423125	33.190439
809.131662	53316.561917	33.195456
810.077651	53391.803954	33.200474
810.781123	53489.408054	33.205492
811.710625	53552.675953	33.210509
812.373499	53680.993477	33.215527
813.109380	53728.281697	33.220544
813.941452	53844.292870	33.225562
814.960230	53904.211720	33.230580
815.891338	53992.209609	33.235597
816.335999	54092.518828	33.240615
817.641093	54154.981040	33.245632
818.251611	54259.143788	33.250650
818.980599	54346.512755	33.255668
819.828458	54431.271924	33.260685
820.724666	54526.600521	33.265703
821.229339	54592.710893	33.270720
822.314041	54705.679420	33.275738
823.128750	54780.304237	33.280756
823.851172	54875.201497	33.285773
824.650386	54931.408946	33.290791
825.187452	55033.517253	33.295808
826.237937	55165.104098	33.300826
827.314899	55217.142813	33.305844
828.011474	55329.053301	33.310861
828.883010	55391.595088	33.315879
829.693786	55506.761721	33.320896
830.765661	55588.741361	33.325914
831.196515	55672.464758	33.330932
832.310545	55767.638936	33.335949
832.994541	55859.823377	33.340967
833.449098	55946.476666	33.345984
834.303652	56015.083847	33.351002
835.172698	56120.298797	33.356020
836.005249	56168.023068	33.361037
836.537373	56283.248412	33.366055
837.205948	56355.074627	33.371072
838.031554	56447.242651	33.376090
838.885771	56539.832732	33.381108
839.868960	56631.799836	33.386125
840.566993	56745.316030	33.391143
841.265412	56815.721955	33.396160
842.356039	56940.332611	33.401178
843.330129	57014.076263	33.406196
844.313885	57104.621968	33.411213
845.217889	57219.857151	33.416231
846.395407	57299.785231	33.421248
846.953488	57367.743857	33.426266
848.010204	57497.581850	33.431284
849.063377	57546.502603	33.436301
849.726500	57657.517167	33.441319
850.749198	57714.414216	33.446336
851.818087	57844.969325	33.451354
852.245836	57914.409180	33.456372
853.398783	58008.859567	33.461389
853.936374	58088.188922	33.466407
854.688288	58204.650938	33.471424
855.537921	58259.982967	33.476442
856.095079	58376.874834	33.481460
856.964721	58482.046387	33.486477
858.141899	58539.852711	33.491495
858.999796	58688.735761	33.496512
859.816542	58766.817630	33.501530
860.442918	58884.901358	33.506548
861.182326	58954.412336	33.511565
862.350697	59074.942983	33.516583
863.191472	59157.341551	33.521600
864.312914	59264.545373	33.526618
864.910621	59358.289105	33.531636
866.310530	59478.242506	33.536653
866.942576	59542.784493	33.541671
867.326743	59669.095090	33.546688
868.743098	59743.211807	33.551706
869.369563	59842.124874	33.556724
870.195390	59951.561329	33.561741
871.513062	60044.540412	33.566759
872.178480	60133.162554	33.571776
873.054110	60241.156236	33.576794
873.826045	60329.323500	33.581812
874.655573	60407.306043	33.586829
875.449853	60530.687236	33.591847
876.246397	60612.420465	33.596864
877.369270	60720.724888	33.601882
878.030552	60823.063343	33.606900
879.124686	60912.047209	33.611917
879.816758	61031.258123	33.616935
880.906617	61088.514795	33.621952
881.658929	61202.791652	33.626970
882.532431	61261.090501	33.631988
883.455134	61392.217935	33.637005
884.309789	61468.609547	33.642023
884.808941	61545.970553	33.647040
885.989716	61628.944814	33.652058
886.600814	61767.314089	33.657076
887.331171	61827.352014	33.662093
888.459182	61919.398089	33.667111
888.783053	62037.909859	33.672128
889.902190	62104.574548	33.677146
890.646667	62241.293616	33.682164
891.292511	62344.940605	33.687181
892.504197	62424.342191	33.692199
893.092853	62586.286514	33.697216
894.034290	62650.310030	33.702234
894.547316	62789.343425	33.707252
895.754003	62922.618309	33.712269
896.590130	63014.883543	33.717287
897.973348	63108.271597	33.722304
899.163962	63207.984189	33.727322
899.611978	63359.836875	33.732340
900.798845	63430.101681	33.737357
901.556476	63567.968227	33.742375
902.799647	63650.388849	33.747392
903.723950	63768.853832	33.752410
904.396570	63874.595452	33.757428
905.789937	63971.241927	33.762445
905.942189	64100.098138	33.767463
907.154816	64217.765307	33.772480
908.510787	64308.214107	33.777498
909.067894	64421.884661	33.782516
910.135722	64517.849910	33.787533
911.332185	64642.804598	33.792551
911.845890	64739.613894	33.797568
912.894017	64834.630152	33.802586
913.964122	64978.388007	33.807604
915.092615	65051.579842	33.812621
915.706838	65179.292942	33.817639
917.130829	65248.238252	33.822656
918.271303	65375.483647	33.827674
918.464182	65469.956990	33.832692
920.134461	65546.339518	33.837709
920.883621	65681.816204	33.842727
921.716108	65746.559148	33.847744
922.618175	65879.205272	33.852762
923.425406	65953.860244	33.857780
924.300715	66074.640224	33.862797
925.546826	66171.463414	33.867815
926.404310	66279.181808	33.872832
927.386405	66364.646607	33.877850
928.006467	66474.977880	33.882868
928.686294	66579.883749	33.887885
930.050657	66664.148907	33.892903
930.526711	66770.638982	33.897920
931.317628	66860.223316	33.902938
932.327472	66932.695851	33.907956
933.219772	67068.544868	33.912973
933.862528	67132.204599	33.917991
934.458203	67260.417736	33.923008
935.879017	67353.627947	33.928026
936.802609	67463.079600	33.933044
937.617192	67561.901957	33.938061
938.486092	67672.197336	33.943079
939.204993	67779.680857	33.948096
940.538749	67884.590860	33.953114
941.169929	67999.777444	33.958132
942.073391	68093.525211	33.963149
943.028229	68206.911686	33.968167
943.776062	68332.290256	33.973184
945.044536	68437.485284	33.978202
945.982018	68551.293472	33.983220
946.960529	68660.938998	33.988237
948.453295	68752.694684	33.993255
949.339093	68871.440514	33.998272
950.064501	69000.630041	34.003290
951.123528	69086.423155	34.008308
952.174438	69193.166766	34.013325
952.816129	69299.312723	34.018343
953.261995	69424.544216	34.023360
954.968937	69531.229535	34.028378
956.153806	69637.417272	34.033396
956.772575	69756.116212	34.038413
958.055290	69865.852800	34.043431
958.885940	69970.784618	34.048448
959.632409	70095.302907	34.053466
961.051544	70193.969818	34.058484
961.570092	70291.188400	34.063501
962.894915	70420.494136	34.068519
963.780694	70511.053184	34.073536
965.145593	70638.907182	34.078554
965.924857	70726.754810	34.083572
966.867057	70863.282630	34.088589
968.283907	70937.774527	34.093607
969.145493	71052.708719	34.098624
970.151069	71171.613739	34.103642
970.918806	71254.145688	34.108660
971.676464	71390.213708	34.113677
972.818850	71470.930504	34.118695
973.327129	71618.343098	34.123712
974.319033	71690.144363	34.128730
975.639475	71840.493797	34.133748
976.313655	71935.869748	34.138765
977.624122	72045.216055	34.143783
978.533496	72146.469651	34.148800
979.438175	72280.763895	34.153818
980.573063	72380.358961	34.158836
980.840254	72483.991112	34.163853
982.215684	72604.823646	34.168871
982.894291	72726.254301	34.173888
984.137181	72814.062753	34.178906
985.040596	72910.228362	34.183924
985.579192	73021.667969	34.188941
986.377712	73138.551543	34.193959
987.610166	73221.245258	34.198976
988.478829	73379.361902	34.203994
989.731287	73451.526204	34.209012
990.296637	73596.517989	34.214029
991.643879	73665.186269	34.219047
992.267870	73821.316966	34.224064
993.535367	73900.993781	34.229082
994.621985	74043.068660	34.234100
995.636068	74140.157832	34.239117
996.936634	74272.228796	34.244135
997.514755	74385.584440	34.249152
998.284083	74482.638381	34.254170
999.613623	74620.842978	34.259188
1000.726958	74721.906629	34.264205
1001.708028	74864.155797	34.269223
1002.398988	74982.476491	34.274240
1003.507867	75094.032854	34.279258
1004.293528	75218.861485	34.284276
1005.486221	75343.556632	34.289293
1006.817950	75460.053002	34.294311
1007.755202	75585.447511	34.299328
1008.895445	75702.639299	34.304346
1009.768879	75822.913944	34.309364
1010.595523	75940.643611	34.314381
1012.151671	76061.607362	34.319399
1012.831102	76191.318766	34.324416
1013.983143	76307.374645	34.329434
1015.286967	76421.233036	34.334452
1015.980559	76549.269739	34.339469
1017.228932	76659.529666	34.344487
1018.273545	76787.189728	34.349504
1019.445075	76909.597484	34.354522
1020.562824	77013.509606	34.359540
1021.092325	77129.113068	34.364557
1022.143840	77259.947664	34.369575
1023.365646	77382.780047	34.374592
1024.301993	77494.933306	34.379610
1025.596140	77613.129238	34.384628
1026.409025	77746.937490	34.389645
1027.669990	77861.739872	34.394663
1028.516627	77979.617261	34.399680
1029.767590	78097.260372	34.404698
1030.707085	78223.239698	34.409716
1031.367573	78335.523633	34.414733
1032.911408	78444.065038	34.419751
1033.327236	78590.001365	34.424768
1034.582115	78715.371043	34.429786
1035.601796	78841.531046	34.434804
1036.497201	78964.007728	34.439821
1037.365858	79081.338085	34.444839
1038.417501	79207.261397	34.449856
1039.704522	79314.261787	34.454874
1040.784252	79412.478288	34.459892
1041.989825	79528.708380	34.464909
1042.896522	79642.793349	34.469927
1043.601471	79748.321027	34.474944
1044.586791	79859.367016	34.479962
1045.791403	79975.258461	34.484980
1046.904085	80113.768868	34.489997
1047.433757	80218.189064	34.495015
1048.591603	80348.798970	34.500032
1049.329763	80457.156816	34.505050
1050.453751	80608.841823	34.510068
1051.412720	80732.734862	34.515085
1052.672529	80855.860183	34.520103
1053.810573	81017.786258	34.525120
1054.516516	81117.587440	34.530138
1055.637560	81271.338505	34.535156
1056.351116	81401.608524	34.540173
1058.196286	81510.358423	34.545191
1059.182787	81672.282111	34.550208
1060.095099	81778.678503	34.555226
1061.829696	81897.593956	34.560244
1062.537150	82061.866084	34.565261
1063.854783	82159.305559	34.570279
1064.488029	82318.711265	34.575296
1066.042358	82421.253798	34.580314
1066.869407	82580.346208	34.585332
1067.641422	82675.870901	34.590349
1068.218216	82846.744587	34.595367
1069.890166	82966.276682	34.600384
1070.826824	83125.450638	34.605402
1072.180411	83239.566521	34.610420
1072.881344	83386.648241	34.615437
1074.511864	83532.615887	34.620455
1075.045324	83656.195724	34.625472
1075.960287	83811.869623	34.630490
1077.183077	83950.103591	34.635508
1078.652918	84058.629349	34.640525
1079.647619	84236.187298	34.645543
1080.708499	84370.302420	34.650560
1081.738090	84489.464876	34.655578
1083.138483	84634.130135	34.660596
1084.068482	84779.471820	34.665613
1085.538476	84879.245325	34.670631
1086.595213	85062.332455	34.675648
1087.572969	85189.087716	34.680666
1088.941346	85293.431527	34.685684
1089.623049	85469.810418	34.690701
1090.659078	85563.896319	34.695719
1091.992325	85734.489786	34.700736
1093.034359	85831.244075	34.705754
1094.188344	85994.938500	34.710772
1095.019012	86116.127091	34.715789
1096.339345	86270.540671	34.720807
1097.303896	86371.103424	34.725824
1098.432855	86500.517034	34.730842
1099.440011	86633.523244	34.735860
1100.712157	86731.313609	34.740877
1102.204637	86867.734364	34.745895
1102.815645	86973.465152	34.750912
1103.561256	87137.764436	34.755930
1104.580050	87229.116240	34.760948
1105.654318	87388.995938	34.765965
1106.317496	87499.096636	34.770983
1108.127188	87628.769253	34.776000
1108.548756	87789.324822	34.781018
1110.016467	87917.713043	34.786036
1110.936746	88062.667683	34.791053
1112.227736	88205.597779	34.796071
1113.114487	88347.638274	34.801088
1114.329428	88460.046408	34.806106
1115.464001	88646.060703	34.811124
1116.621337	88775.983109	34.816141
1117.766427	88909.032093	34.821159
1118.715528	89067.243137	34.826176
1119.732161	89218.279882	34.831194
1120.806006	89366.658948	34.836212
1121.810726	89512.299190	34.841229
1123.312105	89668.377912	34.846247
1124.260193	89830.047489	34.851264
1125.518302	89963.711050	34.856282
1127.021942	90126.938708	34.861300
1127.980314	90275.544724	34.866317
1129.383691	90407.246455	34.871335
1130.497090	90556.373603	34.876352
1131.383603	90710.110177	34.881370
1132.759674	90852.354904	34.886388
1134.076414	91001.731028	34.891405
1135.313481	91132.217726	34.896423
1136.599850	91291.200838	34.901440
1138.189784	91402.356669	34.906458
1139.037802	91579.290393	34.911476
1140.007557	91691.646748	34.916493
1141.089763	91864.093164	34.921511
1142.278858	91972.842778	34.926528
1143.008811	92140.262504	34.931546
1144.322108	92272.166891	34.936564
1145.423328	92439.346448	34.941581
1146.868582	92567.841641	34.946599
1148.193596	92718.512055	34.951616
1149.238633	92857.799243	34.956634
1150.463317	93002.959749	34.961652
1151.476176	93160.753907	34.966669
1152.556578	93294.080256	34.971687
1154.003852	93435.710574	34.976704
1154.554644	93561.419034	34.981722
1155.962058	93735.055415	34.986740
1156.998940	93860.232881	34.991757
1158.182715	94039.074736	34.996775
1159.519112	94144.883138	35.001792
1160.460997	94294.777648	35.006810
1161.678177	94431.093526	35.011828
1162.396205	94561.777943	35.016845
1163.604666	94696.502882	35.021863
1165.072659	94848.347872	35.026880
1166.048687	94962.029196	35.031898
1166.655918	95135.797421	35.036916
1168.146416	95256.691598	35.041933
1168.937263	95427.276515	35.046951
1170.287414	95550.123859	35.051968
1171.159969	95736.600421	35.056986
1172.981948	95847.267296	35.062004
1173.631116	96022.446334	35.067021
1174.361413	96190.276061	35.072039
1176.442105	96309.506994	35.077056
1177.246437	96514.136651	35.082074
1178.518707	96630.284338	35.087092
1179.739893	96812.109216	35.092109
1181.207278	96965.176881	35.097127
1182.219623	97100.054988	35.102144
1182.998054	97287.748638	35.107162
1184.533624	97412.354276	35.112180
1185.575765	97599.167222	35.117197
1186.477354	97733.181064	35.122215
1187.788975	97934.484981	35.127232
1188.979127	98065.823230	35.132250
1190.364527	98254.896058	35.137268
1191.806508	98402.151007	35.142285
1192.786485	98561.487733	35.147303
1194.145310	98743.299894	35.152320
1195.266851	98897.099856	35.157338
1196.513718	99068.715241	35.162356
1198.366258	99221.426893	35.167373
1199.052514	99378.348680	35.172391
1200.387753	99553.357340	35.177408
1201.635584	99703.814858	35.182426
1202.941154	99869.422930	35.187444
1203.931351	100033.816989	35.192461
1205.188758	100192.077053	35.197479
1206.664423	100341.730664	35.202496
1207.838613	100522.884029	35.207514
1209.159403	100659.353827	35.212532
1210.623153	100825.899003	35.217549
1211.625520	100977.517423	35.222567
1212.992398	101141.277417	35.227584
1214.424059	101278.619038	35.232602
1215.412632	101466.642561	35.237620
1216.514738	101589.612573	35.242637
1217.492422	101773.761768	35.247655
1219.169802	101928.986853	35.252672
1220.335810	102076.979920	35.257690
1221.397413	102251.495748	35.262708
1222.861329	102388.959038	35.267725
1223.754434	102549.868391	35.272743
1224.938429	102697.881530	35.277760
1226.046680	102845.679859	35.282778
1227.163891	102992.901893	35.287796
1228.694683	103098.392012	35.292813
1229.738109	103278.923280	35.297831
1231.142395	103399.924891	35.302848
1232.351851	103565.119058	35.307866
1234.036194	103705.162068	35.312884
1235.210997	103852.418319	35.317901
1235.776006	103999.861021	35.322919
1237.171973	104148.412809	35.327936
1238.345515	104295.773283	35.332954
1239.632692	104469.459814	35.337972
1240.713068	104609.616883	35.342989
1241.709494	104761.355744	35.348007
1242.862603	104913.773088	35.353024
1244.074320	105095.512857	35.358042
1245.134674	105254.319544	35.363060
1247.023574	105394.498287	35.368077
1247.790846	105588.665116	35.373095
1249.474227	105736.674946	35.378112
1250.506177	105914.475411	35.383130
1251.797404	106081.610653	35.388148
1252.814913	106228.140973	35.393165
1254.066818	106420.263085	35.398183
1255.569625	106574.850464	35.403200
1256.819195	106750.148126	35.408218
1257.842196	106926.147592	35.413236
1259.645718	107072.918882	35.418253
1260.281653	107277.594223	35.423271
1261.917590	107419.831297	35.428288
1262.843782	107621.982575	35.433306
1264.361850	107764.746732	35.438324
1265.765085	107973.299512	35.443341
1267.081278	108115.230785	35.448359
1268.498203	108310.512596	35.453376
1270.069727	108455.265975	35.458394
1271.100471	108654.966307	35.463412
1272.958596	108791.669903	35.468429
1273.927567	108949.553611	35.473447
1275.153241	109150.840976	35.478464
1276.611026	109289.927503	35.483482
1277.998791	109454.722725	35.488500
1279.429586	109632.898698	35.493517
1280.513940	109784.902236	35.498535
1282.178878	109949.175723	35.503552
1282.892943	110109.284793	35.508570
1283.970702	110286.173492	35.513588
1285.429227	110443.476395	35.518605
1286.804373	110602.806363	35.523623
1287.982497	110807.684845	35.528640
1289.308350	110969.373318	35.533658
1290.818225	111110.829246	35.538676
1291.480331	111295.931283	35.543693
1292.919540	111451.091619	35.548711
1294.147839	111623.345308	35.553728
1295.690215	111761.426024	35.558746
1296.528845	111950.062298	35.563764
1297.994048	112071.496727	35.568781
1299.170654	112260.910877	35.573799
1300.386157	112409.966398	35.578816
1301.238168	112579.001287	35.583834
1302.831987	112751.249058	35.588852
1303.922554	112934.997606	35.593869
1304.925350	113069.246699	35.598887
1306.427353	113227.877157	35.603904
1307.855823	113444.125809	35.608922
1309.121427	113634.333913	35.613940
1310.873912	113750.704630	35.618957
1311.747624	113960.601631	35.623975
1312.730477	114146.205724	35.628992
1314.241598	114296.118160	35.634010
1315.462880	114511.516386	35.639028
1316.817842	114671.021351	35.644045
1317.943902	114879.771761	35.649063
1319.471571	115053.590620	35.654080
1320.758853	115248.270672	35.659098
1322.072143	115413.465644	35.664116
1323.728876	115602.803518	35.669133
1324.503672	115841.454921	35.674151
1326.148469	116009.950147	35.679168
1327.879500	116186.422476	35.684186
1329.079377	116372.597268	35.689204
1330.825032	116574.621978	35.694221
1332.153219	116742.165754	35.699239
1333.567349	116934.831661	35.704256
1334.991417	117109.991668	35.709274
1335.925025	117290.688362	35.714292
1337.495732	117488.138983	35.719309
1338.983409	117656.720752	35.724327
1339.965132	117864.195421	35.729344
1341.780571	118023.850916	35.734362
1343.083358	118220.165790	35.739380
1344.795535	118397.726450	35.744397
1345.283852	118608.394326	35.749415
1347.357394	118791.117490	35.754432
1348.582358	118952.582138	35.759450
1349.553197	119181.007955	35.764468
1351.222193	119334.401144	35.769485
1352.368463	119526.660538	35.774503
1353.626328	119710.146687	35.779520
1355.279438	119923.590810	35.784538
1356.443316	120091.708100	35.789556
1358.158288	120304.936574	35.794573
1358.961070	120473.715258	35.799591
1360.797587	120632.813660	35.804608
1361.992776	120853.221140	35.809626
1363.465277	121042.166191	35.814644
1365.232550	121215.298567	35.819661
1366.338695	121386.865439	35.824679
1367.200695	121572.466596	35.829696
1368.732022	121718.803555	35.834714
1370.266237	121917.737531	35.839732
1371.485620	122071.927519	35.844749
1373.131157	122232.851741	35.849767
1374.072864	122450.653294	35.854784
1375.278220	122598.300784	35.859802
1376.758346	122775.326592	35.864820
1378.251364	122942.130684	35.869837
1379.563888	123152.786560	35.874855
1380.667033	123315.488062	35.879872
1381.931418	123521.126341	35.884890
1383.105376	123700.993399	35.889908
1384.574905	123892.365815	35.894925
1385.919921	124111.472145	35.899943
1387.425953	124271.113674	35.904960
1388.499037	124484.427309	35.909978
1389.417552	124679.376071	35.914996
1391.190654	124887.591251	35.920013
1392.728394	125079.771966	35.925031
1393.660753	125303.323481	35.930048
1395.375497	125486.143870	35.935066
1396.444657	125709.233691	35.940084
1398.434337	125905.819785	35.945101
1399.819505	126113.244765	35.950119
1401.187760	126345.083031	35.955136
1403.200630	126509.128715	35.960154
1404.312086	126741.302515	35.965172
1405.858359	126940.626663	35.970189
1407.189400	127136.705662	35.975207
1408.495276	127332.549394	35.980224
1410.116324	127562.305771	35.985242
1411.215135	127756.779366	35.990260
1412.996757	127953.818710	35.995277
1413.939158	128180.989922	36.000295
1415.629770	128387.813647	36.005312
1417.359195	128581.686182	36.010330
1418.930107	128799.667103	36.015348
1420.307008	129010.700462	36.020365
1421.823449	129206.625466	36.025383
1423.101098	129415.144053	36.030400
1424.826602	129621.933496	36.035418
1425.906440	129823.075595	36.040436
1427.691141	130005.256367	36.045453
1429.152743	130231.158440	36.050471
1430.503224	130420.480031	36.055488
1432.543931	130618.016650	36.060506
1433.692928	130807.993659	36.065524
1435.122090	131008.848115	36.070541
1436.794281	131224.222181	36.075559
1438.713949	131407.138151	36.080576
1439.281236	131599.797471	36.085594
1440.568824	131810.891595	36.090612
1442.228931	131990.811965	36.095629
1443.939762	132210.963839	36.100647
1444.739634	132390.656023	36.105664
1446.234368	132563.587360	36.110682
1447.508226	132755.344122	36.115700
1448.827228	132928.888423	36.120717
1450.244066	133156.746966	36.125735
1451.674591	133313.108113	36.130752
1452.988714	133518.889362	36.135770
1454.394381	133739.595736	36.140788
1456.105238	133895.560779	36.145805
1457.198397	134132.094350	36.150823
1458.480269	134302.599363	36.155840
1460.278050	134512.150083	36.160858
1461.465038	134744.707921	36.165876
1462.800124	134908.986793	36.170893
1464.716603	135124.617751	36.175911
1465.912049	135370.445664	36.180928
1467.402538	135550.212736	36.185946
1468.450055	135769.965274	36.190964
1470.234458	135993.201033	36.195981
1472.058432	136205.458877	36.200999
1473.195703	136408.222458	36.206016
1474.766659	136652.050197	36.211034
1476.271216	136858.369940	36.216052
1477.833470	137071.461324	36.221069
1479.095221	137290.139568	36.226087
1480.644211	137518.429777	36.231104
1482.304295	137730.205216	36.236122
1483.823005	137965.409936	36.241140
1485.470935	138168.408729	36.246157
1486.971197	138382.064391	36.251175
1488.084934	138626.906276	36.256192
1490.213980	138807.935234	36.261210
1491.668027	139067.540773	36.266228
1493.290962	139262.111151	36.271245
1494.675098	139482.104173	36.276263
1496.443260	139677.883458	36.281280
1497.735749	139931.464617	36.286298
1499.148503	140124.287146	36.291316
1500.358745	140369.318153	36.296333
1501.998775	140554.896368	36.301351
1503.141954	140817.937601	36.306368
1505.519416	140997.229523	36.311386
1506.717255	141245.666117	36.316404
1508.777492	141434.161279	36.321421
1510.076862	141677.528562	36.326439
1511.500796	141874.086600	36.331456
1513.225227	142101.801101	36.336474
1514.432617	142332.172252	36.341492
1516.133341	142536.383682	36.346509
1518.031756	142754.658665	36.351527
1519.270768	142982.431529	36.356544
1520.921621	143199.101378	36.361562
1522.833267	143386.288805	36.366580
1523.877178	143637.076145	36.371597
1525.655371	143821.410331	36.376615
1526.755700	144041.291522	36.381632
1528.749935	144203.882069	36.386650
1529.376134	144433.829033	36.391668
1531.199949	144616.094745	36.396685
1532.624108	144825.093086	36.401703
1533.545763	145046.201261	36.406720
1535.372068	145229.129294	36.411738
1536.379674	145453.294092	36.416756
1537.735223	145668.418458	36.421773
1539.524369	145887.911816	36.426791
1540.888322	146118.869502	36.431808
1542.343459	146334.413606	36.436826
1544.049193	146579.364920	36.441844
1545.413133	146801.746226	36.446861
1546.960070	147040.058918	36.451879
1548.446227	147258.304391	36.456896
1550.078490	147500.042184	36.461914
1551.714887	147731.830417	36.466932
1552.979916	147966.607538	36.471949
1554.712701	148206.141773	36.476967
1556.087947	148435.758277	36.481984
1557.731024	148677.389239	36.487002
1559.253171	148936.775794	36.492020
1560.778533	149166.525833	36.497037
1562.779876	149401.640257	36.502055
1563.980591	149658.421588	36.507072
1565.724463	149915.499006	36.512090
1567.576914	150133.325680	36.517108
1569.049730	150398.221044	36.522125
1570.862463	150628.569739	36.527143
1572.524055	150867.260423	36.532160
1574.412755	151133.857900	36.537178
1576.017571	151348.296488	36.542196
1577.454082	151589.627121	36.547213
1579.361011	151832.444182	36.552231
1580.863649	152053.622831	36.557248
1582.460261	152315.344678	36.562266
1584.387605	152563.311149	36.567284
1585.694298	152773.331084	36.572301
1587.292307	153023.736809	36.577319
1588.786008	153262.332161	36.582336
1590.593017	153485.690787	36.587354
1592.031179	153752.076798	36.592372
1593.536716	153962.909479	36.597389
1595.274650	154214.151433	36.602407
1596.970201	154445.318896	36.607424
1598.753470	154684.372932	36.612442
1600.529085	154919.562823	36.617460
1601.586648	155147.058140	36.622477
1603.166680	155410.150972	36.627495
1604.818068	155620.970930	36.632512
1606.500078	155897.047520	36.637530
1608.210218	156108.837498	36.642548
1609.781518	156382.196885	36.647565
1611.568119	156583.009951	36.652583
1612.900998	156833.815913	36.657600
1614.422494	157025.835995	36.662618
1616.249620	157288.143369	36.667636
1617.330179	157486.601323	36.672653
1618.761801	157723.095237	36.677671
1620.281058	157940.328563	36.682688
1621.990849	158183.337045	36.687706
1624.031162	158402.519358	36.692724
1625.084699	158653.814103	36.697741
1626.956463	158889.675505	36.702759
1628.188592	159106.099491	36.707776
1629.833334	159369.072998	36.712794
1631.411761	159589.287203	36.717812
1632.776735	159858.801317	36.722829
1634.847552	160072.980432	36.727847
1636.328043	160371.595303	36.732864
1638.191570	160622.065458	36.737882
1639.438351	160860.512205	36.742900
1641.715678	161084.517903	36.747917
1643.000093	161340.436577	36.752935
1644.437947	161634.960172	36.757952
1645.663515	161876.498698	36.762970
1648.016458	162110.796217	36.767988
1649.028550	162414.068036	36.773005
1650.939481	162651.952112	36.778023
1652.928040	162903.154032	36.783040
1654.089382	163188.793651	36.788058
1656.238988	163434.279524	36.793076
1657.478840	163741.838251	36.798093
1659.414750	163984.267356	36.803111
1660.891178	164254.786223	36.808128
1662.768814	164514.869199	36.813146
1664.727155	164793.546413	36.818164
1666.413207	165077.849323	36.823181
1668.390463	165308.726842	36.828199
1669.757532	165610.485143	36.833216
1671.728655	165835.228485	36.838234
1673.255560	166146.148167	36.843252
1674.722767	166396.163279	36.848269
1676.434458	166680.309591	36.853287
1678.475737	166920.534486	36.858304
1679.947754	167202.452545	36.863322
1681.870831	167471.706491	36.868340
1683.450259	167723.729346	36.873357
1685.790929	168012.491489	36.878375
1686.870103	168264.305676	36.883392
1688.587202	168566.590395	36.888410
1690.949762	168799.381665	36.893428
1691.899853	169058.831939	36.898445
1693.724536	169347.153473	36.903463
1695.464494	169585.794280	36.908480
1697.036747	169889.926340	36.913498
1698.675304	170151.342246	36.918516
1700.603040	170402.832887	36.923533
1702.035376	170660.289417	36.928551
1703.849925	170926.972065	36.933568
1705.709772	171174.711203	36.938586
1707.418955	171401.292388	36.943604
1708.519928	171684.317276	36.948621
1710.341956	171892.655358	36.953639
1712.061036	172167.644889	36.958656
1713.427895	172433.914225	36.963674
1715.131898	172689.615873	36.968692
1716.737242	172956.434397	36.973709
1718.489857	173213.653950	36.978727
1719.904989	173504.342034	36.983744
1721.475943	173760.680632	36.988762
1723.250924	174027.568232	36.993780
1724.950767	174316.479124	36.998797
1726.608106	174583.554030	37.003815
1728.167798	174868.266806	37.008832
1730.094104	175166.725655	37.013850
1731.790447	175456.748975	37.018868
1733.376045	175731.492536	37.023885
1735.292611	176017.526848	37.028903
1737.143277	176327.106655	37.033920
1738.715570	176623.983209	37.038938
1740.928422	176885.212797	37.043956
1742.280708	177213.819291	37.048973
1743.981581	177483.595886	37.053991
1746.083847	177765.400954	37.059008
1747.658113	178071.891472	37.064026
1749.695328	178356.755718	37.069044
1751.848050	178652.286013	37.074061
1753.376034	178932.172925	37.079079
1754.998805	179232.993148	37.084096
1756.654423	179534.990222	37.089114
1759.015329	179831.295062	37.094132
1760.420628	180131.445724	37.099149
1762.344575	180439.877244	37.104167
1764.522594	180735.303929	37.109184
1765.955921	181021.652300	37.114202
1768.179741	181313.599282	37.119220
1769.969493	181600.783079	37.124237
1772.721945	181871.753029	37.129255
1774.096961	182168.991855	37.134272
1775.999405	182432.106792	37.139290
1777.850916	182702.895068	37.144308
1779.271889	182988.344875	37.149325
1781.531926	183279.817196	37.154343
1783.482120	183547.765535	37.159360
1785.069516	183832.039762	37.164378
1786.808805	184090.508498	37.169396
1788.027053	184385.833196	37.174413
1790.238810	184663.149077	37.179431
1791.811474	184943.803783	37.184448
1793.248050	185236.929671	37.189466
1795.429206	185505.487602	37.194484
1796.917460	185795.525507	37.199501
1798.644575	186081.403388	37.204519
1800.622712	186344.707168	37.209536
1802.041023	186624.064472	37.214554
1803.641420	186888.408436	37.219572
1805.280179	187165.462665	37.224589
1806.661547	187436.290800	37.229607
1808.278478	187724.125270	37.234624
1809.906628	188009.282233	37.239642
1811.896643	188285.310338	37.244660
1813.390208	188594.958120	37.249677
1815.022801	188893.368001	37.254695
1817.221015	189180.789296	37.259712
1818.832346	189483.546292	37.264730
1820.440190	189789.757512	37.269748
1822.243717	190098.909174	37.274765
1824.284856	190390.969340	37.279783
1825.777186	190702.737771	37.284800
1827.774788	191019.237735	37.289818
1830.063493	191323.345660	37.294836
1831.551856	191644.346891	37.299853
1833.473467	191963.073301	37.304871
1835.500592	192268.586608	37.309888
1837.170455	192582.445695	37.314906
1839.004357	192908.717926	37.319924
1840.784705	193231.066597	37.324941
1842.803625	193536.779493	37.329959
1844.661617	193860.236775	37.334976
1846.597193	194196.032500	37.339994
1848.593828	194505.841510	37.345012
1850.325658	194829.858154	37.350029
1851.885874	195154.234106	37.355047
1854.557446	195482.243252	37.360064
1856.061234	195812.673610	37.365082
1858.344005	196122.878671	37.370100
1860.105476	196451.914258	37.375117
1862.128700	196760.933273	37.380135
1864.138138	197085.922914	37.385152
1865.596275	197423.579984	37.390170
1867.836963	197716.425835	37.395188
1869.877492	198070.266068	37.400205
1871.726491	198367.620037	37.405223
1873.511437	198685.014498	37.410240
1875.427061	199020.705414	37.415258
1877.668563	199318.814779	37.420276
1879.610724	199634.908038	37.425293
1881.283434	199955.996096	37.430311
1883.670766	200282.519422	37.435328
1885.476305	200588.879226	37.440346
1887.573389	200897.276143	37.445364
1889.491410	201205.449371	37.450381
1891.216566	201526.843073	37.455399
1893.381594	201839.347105	37.460416
1894.996545	202140.732080	37.465434
1896.776628	202442.422522	37.470452
1898.476854	202785.596551	37.475469
1900.541612	203072.470143	37.480487
1902.613791	203373.636931	37.485504
1904.224140	203666.653181	37.490522
1905.811259	203942.068552	37.495540
1907.579525	204252.592710	37.500557
1909.091368	204537.708226	37.505575
1911.256846	204819.573370	37.510592
1912.935010	205171.016397	37.515610
1915.383571	205433.087901	37.520628
1916.797553	205769.661079	37.525645
1918.312908	206045.910372	37.530663
1920.243285	206391.456104	37.535680
1921.886330	206683.175057	37.540698
1924.310275	207026.335854	37.545716
1926.008178	207336.354549	37.550733
1927.729161	207683.553268	37.555751
1929.688255	207985.206330	37.560768
1931.472102	208331.116686	37.565786
1933.296537	208692.662424	37.570804
1935.315033	208992.114925	37.575821
1937.461223	209338.125875	37.580839
1939.357339	209676.383809	37.585856
1941.459305	209994.387891	37.590874
1943.192315	210362.889449	37.595892
1945.832035	210685.686642	37.600909
1947.444822	211020.074090	37.605927
1949.356058	211377.952908	37.610944
1951.531271	211714.578032	37.615962
1953.736486	212047.467748	37.620980
1955.754590	212387.841106	37.625997
1957.532063	212725.994656	37.631015
1959.258829	213081.322424	37.636032
1961.787961	213422.356507	37.641050
1963.621289	213751.886216	37.646068
1965.618267	214121.421352	37.651085
1967.879800	214442.139202	37.656103
1969.893428	214774.743204	37.661120
1972.023788	215127.669266	37.666138
1974.130342	215448.937091	37.671156
1976.005519	215787.497131	37.676173
1978.056583	216141.951924	37.681191
1980.343627	216446.767036	37.686208
1982.077185	216805.389218	37.691226
1983.876495	217119.159391	37.696244
1986.025457	217484.714870	37.701261
1988.112801	217804.993782	37.706279
1990.322486	218146.457925	37.711296
1992.130366	218503.413811	37.716314
1994.313001	218802.631217	37.721332
1996.173592	219169.383883	37.726349
1997.930382	219484.466396	37.731367
2000.120376	219849.824413	37.736384
2002.052835	220156.971868	37.741402
2004.027459	220505.404328	37.746420
2006.158919	220857.609959	37.751437
2008.095545	221179.121322	37.756455
2009.845001	221502.479455	37.761472
2011.811327	221820.763809	37.766490
2013.758614	222124.399954	37.771508
2015.639318	222438.764364	37.776525
2017.099576	222784.292491	37.781543
2019.441776	223096.262786	37.786560
2021.600279	223421.608474	37.791578
2023.377706	223758.265942	37.796596
2025.429342	224080.152230	37.801613
2027.024795	224442.515909	37.806631
2029.032341	224814.504173	37.811648
2030.551586	225164.249079	37.816666
2032.928953	225504.221784	37.821684
2035.059076	225856.767878	37.826701
2036.994075	226222.539534	37.831719
2039.429862	226562.545490	37.836736
2041.147545	226919.212219	37.841754
2043.357257	227267.751879	37.846772
2045.383286	227622.747356	37.851789
2047.670359	227983.620247	37.856807
2049.645958	228333.623641	37.861824
2051.717802	228684.705249	37.866842
2054.013924	229050.101775	37.871860
2056.033327	229409.194563	37.876877
2057.923871	229774.404493	37.881895
2060.391928	230125.911592	37.886912
2062.077525	230484.375990	37.891930
2064.113464	230846.011678	37.896948
2066.188186	231221.128573	37.901965
2068.449459	231589.969686	37.906983
2070.758326	231951.490279	37.912000
2072.633371	232322.503569	37.917018
2075.096012	232680.192980	37.922036
2077.108052	233042.907774	37.927053
2079.037142	233414.348553	37.932071
2081.012517	233766.125465	37.937088
2083.457155	234146.376556	37.942106
2085.349642	234519.910025	37.947124
2087.577488	234890.166150	37.952141
2089.616022	235267.844582	37.957159
2091.723816	235632.763472	37.962176
2093.685696	235999.713302	37.967194
2096.053356	236376.861103	37.972212
2098.177624	236746.251509	37.977229
2100.332070	237123.512047	37.982247
2102.633806	237496.788364	37.987264
2104.773822	237858.687536	37.992282
2106.664735	238243.232548	37.997300
2108.863466	238601.569049	38.002317
2110.821726	238978.181468	38.007335
2113.020864	239347.848373	38.012352
2115.000069	239727.076140	38.017370
2117.246367	240097.627019	38.022388
2120.023301	240453.693429	38.027405
2121.565755	240828.041237	38.032423
2124.018462	241165.594175	38.037440
2126.278550	241509.909566	38.042458
2127.897492	241850.060476	38.047476
2130.184718	242191.350960	38.052493
2132.010890	242537.643121	38.057511
2134.072112	242876.532983	38.062528
2136.281931	243231.300665	38.067546
2138.405343	243580.063224	38.072564
2140.683409	243924.331782	38.077581
2142.614437	244291.338778	38.082599
2144.754787	244635.783494	38.087616
2146.655123	244985.880683	38.092634
2148.791509	245347.651000	38.097652
2151.090899	245719.074070	38.102669
2153.321413	246080.958445	38.107687
2155.158283	246453.320498	38.112704
2157.041140	246828.292543	38.117722
2159.120603	247198.128843	38.122740
2161.894321	247561.785192	38.127757
2163.785966	247947.274782	38.132775
2165.688107	248323.136731	38.137792
2168.125404	248714.688862	38.142810
2170.348119	249098.223874	38.147828
2172.312177	249471.995995	38.152845
2174.695112	249860.790972	38.157863
2176.521202	250261.842474	38.162880
2178.579429	250647.566518	38.167898
2180.845055	251052.970153	38.172916
2183.341506	251426.383039	38.177933
2185.280000	251846.700407	38.182951
2187.537388	252223.048762	38.187968
2190.223184	252631.844218	38.192986
2192.102018	253021.260021	38.198004
2194.392829	253415.691718	38.203021
2197.117814	253820.165384	38.208039
2199.072874	254208.885806	38.213056
2201.420362	254610.474428	38.218074
2203.474156	255004.210426	38.223092
2206.202564	255398.830932	38.228109
2208.236238	255787.669086	38.233127
2210.543785	256192.112320	38.238144
2213.001831	256579.182745	38.243162
2215.379577	256972.109145	38.248180
2217.675577	257350.646098	38.253197
2220.056191	257737.502273	38.258215
2222.100676	258132.134752	38.263232
2224.377025	258523.200206	38.268250
2226.674310	258905.041882	38.273268
2228.995777	259302.655321	38.278285
2231.014361	259682.561016	38.283303
2233.537037	260060.837802	38.288320
2235.740677	260452.730758	38.293338
2237.694915	260840.574005	38.298356
2240.031271	261227.798365	38.303373
2242.426772	261604.624154	38.308391
2244.478641	261978.075548	38.313408
2246.997781	262327.244428	38.318426
2248.629297	262685.216826	38.323444
2250.802095	263045.745725	38.328461
2253.064918	263417.641275	38.333479
2255.226527	263774.057495	38.338496
2257.488466	264144.302816	38.343514
2259.295944	264526.331374	38.348532
2261.464251	264901.444316	38.353549
2263.561205	265275.654442	38.358567
2265.861716	265661.873728	38.363584
2267.802943	266050.258811	38.368602
2269.711386	266452.214733	38.373620
2272.152332	266845.246311	38.378637
2274.489038	267252.926995	38.383655
2276.550493	267647.619829	38.388672
2279.424855	268051.786525	38.393690
2281.929083	268455.834396	38.398708
2284.369075	268853.186293	38.403725
2286.705228	269263.942455	38.408743
2288.905385	269658.894204	38.413760
2291.391198	270073.691700	38.418778
2293.224078	270465.425124	38.423796
2296.043060	270878.671477	38.428813
2298.226628	271279.698151	38.433831
2300.418281	271694.720980	38.438848
2302.756427	272092.344862	38.443866
2305.285344	272508.991189	38.448884
2307.505363	272919.894660	38.453901
2309.773076	273342.146016	38.458919
2312.251888	273748.893351	38.463936
2314.798289	274168.662012	38.468954
2317.234850	274577.854941	38.473972
2319.571254	274994.837250	38.478989
2322.084677	275408.692325	38.484007
2324.765028	275816.017689	38.489024
2327.185586	276209.234539	38.494042
2329.521565	276631.526296	38.499060
2331.918843	277031.478709	38.504077
2333.805254	277438.497997	38.509095
2336.278224	277855.483999	38.514112
2338.914750	278251.740225	38.519130
2340.568487	278666.595012	38.524148
2343.155960	279080.564980	38.529165
2345.573543	279496.949667	38.534183
2347.804343	279913.262198	38.539200
2350.200242	280327.719351	38.544218
2352.413479	280743.958106	38.549236
2354.989962	281163.746357	38.554253
2357.580399	281583.684593	38.559271
2359.848127	282003.648335	38.564288
2362.249880	282408.983684	38.569306
2364.347374	282836.264619	38.574324
2366.896648	283249.019191	38.579341
2369.280854	283663.069786	38.584359
2371.676801	284057.532321	38.589376
2374.113764	284436.085650	38.594394
2376.177032	284821.353542	38.599412
2378.432238	285212.179386	38.604429
2380.664465	285605.447228	38.609447
2382.640927	285993.903249	38.614464
2385.146703	286390.810444	38.619482
2387.183717	286799.934190	38.624500
2389.546970	287201.435687	38.629517
2391.947812	287612.812549	38.634535
2394.144747	288031.867538	38.639552
2396.607002	288447.044116	38.644570
2398.878518	288866.162445	38.649588
2401.254380	289283.231454	38.654605
2403.588828	289710.086549	38.659623
2405.549152	290163.520837	38.664640
2408.446234	290590.996757	38.669658
2410.740747	291016.179666	38.674676
2412.942333	291461.800384	38.679693
2415.569271	291903.237714	38.684711
2417.613282	292345.630353	38.689728
2420.496276	292796.145072	38.694746
2422.956356	293249.774277	38.699764
2425.107728	293689.454791	38.704781
2427.858690	294141.842251	38.709799
2429.917485	294598.987119	38.714816
2432.817557	295042.178873	38.719834
2435.337948	295507.174187	38.724852
2438.079187	295959.051352	38.729869
2440.922173	296399.785268	38.734887
2443.034509	296856.053048	38.739904
2445.845119	297305.452178	38.744922
2448.223677	297741.100065	38.749940
2450.905348	298204.412358	38.754957
2453.643933	298660.855974	38.759975
2455.989057	299099.960585	38.764992
2458.846369	299537.738259	38.770010
2461.153423	299993.484763	38.775028
2463.246655	300433.692777	38.780045
2466.032674	300874.882116	38.785063
2468.360485	301322.493229	38.790080
2471.258608	301769.428498	38.795098
2473.889429	302221.307307	38.800116
2476.276059	302666.187366	38.805133
2478.997681	303119.878042	38.810151
2481.194333	303564.328349	38.815168
2484.119277	303993.573747	38.820186
2486.271433	304441.279776	38.825204
2488.807828	304875.029280	38.830221
2491.550412	305334.856736	38.835239
2494.004966	305764.780945	38.840256
2496.486444	306209.558873	38.845274
2498.959784	306651.136164	38.850292
2501.367131	307092.874850	38.855309
2503.978561	307517.078895	38.860327
2506.245694	307942.250510	38.865344
2508.675441	308345.906417	38.870362
2511.056694	308757.544338	38.875380
2513.155648	309167.346028	38.880397
2516.047798	309584.386650	38.885415
2518.034735	310006.674622	38.890432
2520.461690	310421.169878	38.895450
2523.140994	310853.708241	38.900468
2525.431861	311272.209805	38.905485
2528.186703	311698.510173	38.910503
2530.241392	312151.487593	38.915520
2532.685706	312593.149602	38.920538
2535.154191	313044.483104	38.925556
2537.279005	313495.081834	38.930573
2539.858768	313942.228563	38.935591
2542.504977	314397.465130	38.940608
2544.856716	314854.854492	38.945626
2547.667738	315315.394721	38.950644
2550.097726	315781.809524	38.955661
2552.702685	316249.921574	38.960679
2555.047007	316725.108069	38.965696
2557.782920	317185.499359	38.970714
2560.697512	317663.867390	38.975732
2562.837244	318131.307759	38.980749
2565.642046	318608.164671	38.985767
2568.320466	319092.937892	38.990784
2570.937691	319564.943383	38.995802
2573.743305	320055.228154	39.000820
2576.408440	320527.297369	39.005837
2579.295051	321005.018018	39.010855
2581.504545	321485.992637	39.015872
2584.615738	321951.025007	39.020890
2587.477180	322436.564244	39.025908
2589.746648	322915.007345	39.030925
2592.708960	323384.119162	39.035943
2595.460836	323862.252040	39.040960
2597.995682	324340.010276	39.045978
2600.882353	324815.932357	39.050996
2603.385944	325296.229702	39.056013
2605.962704	325756.983376	39.061031
2608.634299	326239.737385	39.066048
2611.213334	326704.091517	39.071066
2613.915611	327189.907834	39.076084
2616.408855	327666.307322	39.081101
2619.280360	328127.762581	39.086119
2621.958320	328602.578043	39.091136
2624.765855	329083.033078	39.096154
2627.653058	329556.006513	39.101172
2629.756278	330020.644878	39.106189
2632.590723	330491.233769	39.111207
2635.073486	330977.238775	39.116224
2637.806658	331450.199292	39.121242
2640.524704	331920.543614	39.126260
2642.793334	332395.577703	39.131277
2645.943761	332861.073472	39.136295
2648.457476	333306.860382	39.141312
2650.652315	333745.153276	39.146330
2653.193343	334183.464797	39.151348
2655.561183	334633.583224	39.156365
2658.294044	335075.845415	39.161383
2660.727903	335530.492824	39.166400
2663.362342	335987.644668	39.171418
2665.843135	336452.613125	39.176436
2668.265424	336920.025261	39.181453
2670.908557	337373.636866	39.186471
2673.544098	337851.343113	39.191488
2676.287736	338336.671564	39.196506
2678.851042	338801.458161	39.201524
2681.371274	339279.070680	39.206541
2684.046100	339762.012623	39.211559
2686.346602	340253.820724	39.216576
2689.601571	340757.737397	39.221594
2692.331579	341248.022492	39.226612
2694.361546	341733.514340	39.231629
2697.321289	342253.588322	39.236647
2700.144037	342736.204650	39.241664
2702.805230	343243.571962	39.246682
2705.608994	343758.275294	39.251700
2708.389710	344279.858263	39.256717
2711.288804	344776.029253	39.261735
2713.914894	345288.183277	39.266752
2716.392354	345809.851580	39.271770
2719.666396	346319.253610	39.276788
2722.154725	346838.397556	39.281805
2724.837573	347354.992647	39.286823
2727.644199	347878.037234	39.291840
2730.408563	348396.412464	39.296858
2733.291298	348926.315195	39.301876
2735.949618	349450.434904	39.306893
2739.057916	349963.435337	39.311911
2741.541756	350490.009912	39.316928
2744.349256	351031.099667	39.321946
2747.435788	351550.511290	39.326964
2749.941233	352088.414328	39.331981
2752.733007	352602.963074	39.336999
2755.860968	353128.749886	39.342016
2758.513207	353664.735260	39.347034
2761.070859	354197.100170	39.352052
2764.154032	354741.027738	39.357069
2767.134152	355253.515321	39.362087
2769.646477	355791.023935	39.367104
2772.182658	356331.264513	39.372122
2774.916057	356854.969128	39.377140
2777.455626	357395.883136	39.382157
2780.723891	357932.208602	39.387175
2783.273939	358471.205604	39.392192
2786.032979	359010.265163	39.397210
2788.945971	359540.816947	39.402228
2791.532372	360091.339062	39.407245
2794.665605	360609.432810	39.412263
2797.236396	361132.483152	39.417280
2799.740395	361633.533396	39.422298
2802.903970	362130.387708	39.427316
2805.619957	362632.738990	39.432333
2808.157104	363134.529485	39.437351
2810.707027	363635.195872	39.442368
2813.445873	364156.384122	39.447386
2816.228279	364674.260336	39.452404
2819.298640	365182.187453	39.457421
2822.387612	365704.597016	39.462439
2825.493569	366210.781294	39.467456
2827.638597	366724.573091	39.472474
2830.615188	367253.580740	39.477492
2833.333349	367778.638813	39.482509
2836.157050	368321.666169	39.487527
2838.910705	368850.106406	39.492544
2841.618640	369377.177195	39.497562
2844.532715	369931.944887	39.502580
2847.126765	370472.748801	39.507597
2849.947011	371014.626635	39.512615
2852.883732	371587.360514	39.517632
2855.442334	372146.469628	39.522650
2858.655144	372691.156698	39.527668
2861.334683	373276.341849	39.532685
2864.079085	373831.593079	39.537703
2866.937493	374408.310006	39.542720
2869.996055	374947.359183	39.547738
2872.959690	375546.447823	39.552756
2875.497684	376116.163324	39.557773
2878.755104	376683.625730	39.562791
2881.638890	377253.118287	39.567808
2884.504533	377852.086883	39.572826
2887.565776	378409.052342	39.577844
2890.283297	379003.460345	39.582861
2892.987274	379596.567680	39.587879
2896.356699	380184.816615	39.592896
2899.242459	380763.873478	39.597914
2902.406193	381358.403445	39.602932
2905.126244	381944.496055	39.607949
2908.480475	382530.606185	39.612967
2911.489950	383108.694965	39.617984
2913.965032	383712.379020	39.623002
2917.392955	384294.949576	39.628020
2920.268492	384875.873604	39.633037
2923.415740	385463.036388	39.638055
2926.327214	386035.464377	39.643072
2929.322914	386653.908177	39.648090
2932.276735	387206.247347	39.653108
2934.895439	387802.866894	39.658125
2937.713478	388401.398144	39.663143
2941.005013	388976.763636	39.668160
2943.956446	389578.272534	39.673178
2947.538552	390139.674348	39.678196
2949.964998	390738.659784	39.683213
2952.915843	391317.592225	39.688231
2955.956896	391866.472768	39.693248
2958.325683	392406.473254	39.698266
2961.466108	392943.477504	39.703284
2964.054928	393516.826140	39.708301
2966.914885	394052.285264	39.713319
2970.181024	394600.300865	39.718336
2972.393869	395163.334876	39.723354
2975.414183	395731.861458	39.728372
2978.302830	396301.971574	39.733389
2981.388656	396869.226141	39.738407
2984.129185	397442.129784	39.743424
2987.257892	398023.608944	39.748442
2990.617619	398603.012868	39.753460
2993.185938	399189.606265	39.758477
2996.258526	399761.834183	39.763495
2999.238630	400365.253713	39.768512
3002.522529	400940.343458	39.773530
3005.100914	401559.093393	39.778548
3008.449033	402141.174831	39.783565
3011.135022	402733.111576	39.788583
3014.115288	403350.647963	39.793600
3016.969006	403955.059879	39.798618
3020.190522	404562.723195	39.803636
3022.936511	405207.716656	39.808653
3026.027911	405804.019204	39.813671
3029.308473	406444.212737	39.818688
3032.370070	407067.113785	39.823706
3035.212329	407676.399049	39.828724
3038.406259	408320.344600	39.833741
3041.587077	408947.295331	39.838759
3044.442394	409566.604307	39.843776
3047.490956	410212.991709	39.848794
3050.672372	410852.576702	39.853812
3053.719371	411499.697205	39.858829
3056.854207	412148.665417	39.863847
3060.207960	412758.274588	39.868864
3063.372522	413419.528117	39.873882
3066.337146	414053.376255	39.878900
3069.614031	414688.301786	39.883917
3072.705085	415331.504742	39.888935
3075.990568	415967.465506	39.893952
3079.016945	416643.696090	39.898970
3082.188427	417268.267840	39.903988
3085.249857	417914.839123	39.909005
3088.400630	418559.126390	39.914023
3091.833993	419208.143536	39.919040
3094.587271	419862.245179	39.924058
3097.420997	420500.558484	39.929076
3100.369186	421144.312132	39.934093
3103.718452	421802.100313	39.939111
3106.960457	422469.492474	39.944128
3109.951523	423109.494746	39.949146
3113.356985	423752.178168	39.954164
3116.074496	424424.242375	39.959181
3119.080829	425048.996168	39.964199
3122.365906	425696.314417	39.969216
3125.495601	426281.829266	39.974234
3128.111658	426934.264990	39.979252
3131.534692	427505.318021	39.984269
3134.500253	428151.665191	39.989287
3138.022428	428750.337642	39.994304
3140.522616	429367.319944	39.999322
3143.321762	430002.629781	40.004340
3146.482338	430635.055612	40.009357
3149.231248	431262.617623	40.014375
3152.464078	431935.779080	40.019392
3155.173993	432553.615688	40.024410
3158.307075	433240.106422	40.029428
3161.728448	433869.575776	40.034445
3164.574616	434571.221158	40.039463
3167.794925	435206.260979	40.044480
3170.620524	435922.358011	40.049498
3173.906269	436567.077755	40.054516
3177.267541	437276.366440	40.059533
3180.361162	437951.999664	40.064551
3183.575042	438647.016798	40.069568
3186.844875	439359.071530	40.074586
3189.718049	440025.770662	40.079604
3193.153496	440748.899811	40.084621
3196.535968	441455.154245	40.089639
3199.767935	442154.829602	40.094656
3202.535158	442880.229420	40.099674
3205.926631	443592.091436	40.104692
3209.218683	444292.151368	40.109709
3212.372152	445034.082792	40.114727
3215.696750	445737.841947	40.119744
3219.126559	446470.673448	40.124762
3222.273573	447204.590169	40.129780
3225.677508	447909.740523	40.134797
3228.726710	448663.420748	40.139815
3232.383975	449376.181407	40.144832
3235.756236	450117.210107	40.149850
3239.209210	450842.207713	40.154868
3242.531996	451559.914698	40.159885
3245.413050	452323.524556	40.164903
3249.121573	453029.736768	40.169920
3252.517657	453743.568036	40.174938
3255.413365	454504.825272	40.179956
3258.835030	455205.296629	40.184973
3262.189136	455973.112026	40.189991
3265.737691	456677.565916	40.195008
3269.086746	457443.914881	40.200026
3272.062949	458159.848467	40.205044
3275.437643	458915.263726	40.210061
3278.896842	459635.121115	40.215079
3282.069408	460362.943682	40.220096
3285.417809	461110.900938	40.225114
3288.718165	461828.788903	40.230132
3291.871336	462581.380986	40.235149
3295.360118	463294.839970	40.240167
3298.108626	463988.056714	40.245184
3301.165666	464692.583886	40.250202
3304.830054	465363.404691	40.255220
3308.064803	466053.999124	40.260237
3310.706962	466788.820973	40.265255
3313.707736	467468.531728	40.270272
3317.548475	468157.343272	40.275290
3320.544002	468892.390039	40.280308
3323.579407	469618.655593	40.285325
3327.020578	470307.661877	40.290343
3330.218063	471055.647885	40.295360
3333.434715	471761.531562	40.300378
3336.578621	472523.732997	40.305396
3340.017146	473226.750239	40.310413
3343.077387	474005.393732	40.315431
3346.219958	474744.254095	40.320448
3349.915774	475465.709104	40.325466
3352.659960	476233.447089	40.330484
3356.228609	477047.333538	40.335501
3359.396172	477799.778444	40.340519
3363.027238	478560.260437	40.345536
3366.283893	479367.176352	40.350554
3369.610175	480131.589224	40.355572
3373.255613	480948.084235	40.360589
3375.855934	481720.334185	40.365607
3379.532618	482516.188216	40.370624
3383.221285	483333.031952	40.375642
3386.605206	484115.828016	40.380660
3390.684025	484900.706121	40.385677
3393.873104	485693.020151	40.390695
3397.469003	486540.466716	40.395712
3400.588367	487328.681828	40.400730
3404.422086	488110.334656	40.405748
3408.068721	488915.983729	40.410765
3411.396998	489703.713643	40.415783
3414.801707	490547.424715	40.420800
3418.238464	491321.985215	40.425818
3421.833006	492172.008874	40.430836
3425.169995	492981.725263	40.435853
3428.582336	493781.797405	40.440871
3432.428307	494561.360956	40.445888
3436.060664	495366.077465	40.450906
3439.145662	496224.935054	40.455924
3443.028248	497021.862685	40.460941
3446.049370	497831.264003	40.465959
3449.249533	498624.845778	40.470976
3453.579509	499414.830981	40.475994
3456.879651	500274.220414	40.481012
3460.140718	501065.917789	40.486029
3463.240097	501883.859525	40.491047
3466.815549	502700.779723	40.496064
3470.740050	503517.354735	40.501082
3474.320343	504328.544952	40.506100
3477.929063	505135.200709	40.511117
3481.711327	505912.680661	40.516122
3485.086127	506644.902867	40.521127
3488.836243	507384.422819	40.526132
3491.710341	508009.644347	40.531136
3494.174465	508559.213625	40.536141
3497.135553	509071.751464	40.541146
3500.533154	509498.243921	40.546151
3503.012502	509890.669331	40.551156
3504.813278	510237.760474	40.556160
3507.288064	510509.811046	40.561165
3508.553754	510743.649391	40.566170
3509.861273	510970.901110	40.571175
3511.557589	511117.497886	40.576180
3513.402710	511199.516837	40.581184
3514.766864	511240.734623	40.586189
3515.621949	511306.417129	40.591194
3516.797728	511302.538248	40.596199
3517.792536	511292.161860	40.601204
3518.355525	511244.062927	40.606208
3519.467553	511147.563320	40.611213
3519.847969	511009.593189	40.616218
3520.475048	510853.673664	40.621223
3521.437150	510700.482323	40.626228
3521.501079	510524.766245	40.631232
3521.865538	510340.956623	40.636237
3521.702524	510153.939826	40.641242
3521.998473	509974.892889	40.646247
3522.151102	509776.438480	40.651252
3521.701503	509568.818064	40.656256
3522.022464	509335.471941	40.661261
3522.017254	509097.974706	40.666266
3521.884124	508846.124827	40.671271
3521.701346	508605.157672	40.676276
3521.794599	508345.270255	40.681280
3522.327848	508061.527671	40.686285
3521.874605	507880.249849	40.691290
3521.487868	507625.335697	40.696295
3521.614308	507365.630767	40.701300
3521.285604	507092.179470	40.706304
3521.270073	506808.503163	40.711309
3520.709527	506605.621469	40.716314
3520.889590	506346.044684	40.721319
3520.471529	506082.459546	40.726324
3520.215223	505829.269703	40.731328
3520.221875	505564.344495	40.736333
3520.289676	505305.174874	40.741338
3519.873839	505062.829171	40.746343
3519.692584	504814.521814	40.751348
3518.957905	504577.128864	40.756352
3518.489661	504364.995708	40.761357
3518.052542	504121.476370	40.766362
3518.514639	503872.345513	40.771367
3518.195254	503681.943587	40.776372
3518.090917	503431.276446	40.781376
3517.988893	503216.844661	40.786381
3517.160487	502992.807174	40.791386
3517.192949	502755.015438	40.796391
3516.899224	502590.714933	40.801396
3516.645464	502355.139534	40.806400
3516.509116	502163.072666	40.811405
3515.951151	501953.809952	40.816410
3516.177037	501737.081342	40.821415
3515.713953	501578.973620	40.826420
3515.411431	501357.363332	40.831424
3515.399483	501181.818561	40.836429
3514.728161	501008.704781	40.841434
3514.439042	500809.054530	40.846439
3514.703094	500607.036692	40.851444
3514.307289	500433.418222	40.856448
3514.269592	500277.965331	40.861453
3514.009350	500145.579365	40.866458
3513.755451	499975.831950	40.871463
3513.438502	499790.602215	40.876468
3513.349181	499628.216491	40.881472
3513.562112	499504.913904	40.886477
3512.684482	499320.831051	40.891482
3512.588657	499196.056413	40.896487
3512.767562	499019.599735	40.901492
3512.342909	498903.582598	40.906496
3512.114644	498753.664869	40.911501
3511.971087	498608.491399	40.916506
3511.444073	498490.513355	40.921511
3511.888716	498340.333975	40.926516
3511.194346	498218.583567	40.931520
3511.596529	498126.428226	40.936525
3511.132610	497982.869835	40.941530
3511.276160	497832.227553	40.946535
3511.306564	497751.469879	40.951540
3511.001325	497629.248986	40.956544
3510.917327	497477.728402	40.961549
3510.398165	497406.523788	40.966554
3510.445675	497302.370420	40.971559
3510.579830	497176.684825	40.976564
3509.876831	497047.839666	40.981568
3510.068920	496946.648634	40.986573
3509.628545	496840.595119	40.991578
3509.802880	496732.874255	40.996583
3509.978344	496619.026105	41.001588
3509.356351	496550.365997	41.006592
3509.319047	496483.891683	41.011597
3508.961399	496375.493302	41.016602
3509.385079	496262.110028	41.021607
3509.374112	496199.883691	41.026612
3508.826935	496106.804884	41.031616
3508.776931	496023.621864	41.036621
3509.032610	495919.427711	41.041626
3508.595282	495876.255381	41.046631
3508.389164	495768.487699	41.051636
3508.513862	495673.528303	41.056640
3508.623559	495584.900147	41.061645
3508.723711	495555.516067	41.066650
3508.356088	495493.141158	41.071655
3508.141403	495389.524685	41.076660
3507.934465	495313.907925	41.081664
3507.735203	495245.581198	41.086669
3507.874395	495148.844545	41.091674
3507.491553	495130.979870	41.096679
3507.508818	495046.161433	41.101684
3507.802501	494963.223110	41.106688
3507.567352	494938.549601	41.111693
3507.037835	494869.817943	41.116698
3507.245169	494795.348862	41.121703
3507.368994	494776.137840	41.126708
3507.263844	494691.995401	41.131712
3507.614909	494653.303592	41.136717
3507.155237	494576.508445	41.141722
3507.325630	494511.969036	41.146727
3507.165588	494493.967253	41.151732
3506.618780	494421.793279	41.156736
3507.199477	494351.162530	41.161741
3506.516532	494357.853438	41.166746
3506.665821	494266.630128	41.171751
3506.976660	494224.550999	41.176756
3506.629160	494206.122814	41.181760
3505.981841	494133.609127	41.186765
3506.593499	494067.783094	41.191770
3506.239537	494057.255471	41.196775
3506.091734	494033.326532	41.201780
3506.360454	493971.808044	41.206784
3506.570732	493948.379435	41.211789
3506.103410	493898.320245	41.216794
3506.297560	493864.006581	41.221799
3506.101233	493811.422985	41.226804
3505.854840	493790.547698	41.231808
3505.796840	493747.867460	41.236813
3506.218834	493684.956517	41.241818
3505.690942	493700.181328	41.246823
3506.037442	493626.141302	41.251828
3505.795824	493628.306379	41.256832
3505.706619	493571.096908	41.261837
3505.766145	493552.806305	41.266842
3505.829952	493519.829255	41.271847
3505.972516	493477.268617	41.276852
3505.408185	493466.976467	41.281856
3506.019649	493404.591677	41.286861
3505.868614	493416.465504	41.291866
3505.835992	493381.376533	41.296871
3506.105474	493307.347407	41.301876
3506.207115	493330.575605	41.306880
3505.988388	493286.704321	41.311885
3505.642002	493229.382518	41.316890
3505.819074	493191.930547	41.321895
3505.733246	493171.231751	41.326900
3505.394789	493141.001602	41.331904
3505.508667	493102.799814	41.336909
3505.052333	493090.971135	41.341914
3505.183508	493054.944109	41.346919
3505.698830	493015.868429	41.351924
3505.770769	492987.598846	41.356928
3505.609789	493001.297622	41.361933
3505.289860	492960.024300	41.366938
3505.550317	492906.606315	41.371943
3505.695849	492924.510651	41.376948
3505.091354	492886.776449	41.381952
3505.704786	492836.543583	41.386957
3505.873967	492798.433715	41.391962
3505.562152	492776.402847	41.396967
3505.568654	492793.670929	41.401972
3505.278918	492779.182309	41.406976
3505.566438	492731.431511	41.411981
3505.653347	492689.941363	41.416986
3505.434567	492668.857877	41.421991
3505.195306	492675.023476	41.426996
3504.898394	492653.749750	41.432000
3504.879536	492608.528560	41.437005
3505.624898	492560.856895	41.442010
3505.102780	492532.022146	41.447015
3505.581519	492532.604847	41.452020
3505.155294	492555.259078	41.457024
3505.311812	492526.874142	41.462029
3505.209494	492494.579891	41.467034
3504.893581	492459.837812	41.472039
3505.355385	492432.467996	41.477044
3504.623062	492411.819886	41.482048
3505.250992	492369.889014	41.487053
3505.358422	492354.071201	41.492058
3505.333376	492333.361866	41.497063
3505.066619	492299.827171	41.502068
3504.723997	492319.429843	41.507072
3504.904615	492316.970394	41.512077
3505.161455	492278.491102	41.517082
3505.105740	492228.564930	41.522087
3505.177993	492215.588626	41.527092
3505.126337	492194.832699	41.532096
3505.243230	492170.353082	41.537101
3504.733902	492182.689475	41.542106
3504.558847	492205.101859	41.547111
3504.965101	492183.058089	41.552116
3504.922975	492167.415687	41.557120
3504.859518	492124.175495	41.562125
3505.033959	492086.924295	41.567130
3504.903222	492079.398933	41.572135
3505.099596	492061.895549	41.577140
3504.635725	492089.873967	41.582144
3504.660871	492068.801894	41.587149
3504.819848	492022.183775	41.592154
3504.659871	492048.240376	41.597159
3504.751893	492033.690840	41.602164
3504.444630	492024.319505	41.607168
3504.877866	491979.683719	41.612173
3505.221615	491941.341931	41.617178
3504.899888	491962.714244	41.622183
3505.342197	491953.528277	41.627188
3504.569670	491921.896048	41.632192
3504.940805	491859.088264	41.637197
3504.947299	491899.704534	41.642202
3504.686257	491851.835603	41.647207
3504.762939	491859.268309	41.652212
3504.826407	491822.388636	41.657216
3504.811757	491813.679981	41.662221
3504.761296	491849.139553	41.667226
3504.198020	491819.601174	41.672231
3505.137243	491759.488756	41.677236
3504.737714	491781.430671	41.682240
3504.834825	491756.649767	41.687245
3505.351522	491753.326804	41.692250
3505.174576	491718.054927	41.697255
3505.244355	491715.764853	41.702260
3504.287517	491706.698601	41.707264
3505.301298	491650.929563	41.712269
3505.032512	491670.926409	41.717274
3504.673832	491625.300733	41.722279
3504.627846	491628.751908	41.727284
3504.532904	491611.142205	41.732288
3504.412355	491625.392703	41.737293
3504.900538	491583.279573	41.742298
3504.483685	491594.892696	41.747303
3504.877574	491562.569054	41.752308
3504.429948	491567.197926	41.757312
3505.142022	491538.419812	41.762317
3504.705518	491523.041782	41.767322
3504.474300	491516.393055	41.772327
3504.878384	491489.436151	41.777332
3504.838660	491506.104977	41.782336
3504.839708	491459.105246	41.787341
3504.913542	491466.437267	41.792346
3504.551129	491456.112085	41.797351
3505.072225	491410.802657	41.802356
3504.824464	491440.571156	41.807360
3504.470502	491393.475428	41.812365
3504.625299	491374.002765	41.817370
3504.358983	491419.272015	41.822375
3504.688136	491370.245001	41.827380
3504.457215	491385.222175	41.832384
3504.684733	491352.063477	41.837389
3505.156358	491312.332738	41.842394
3504.852618	491292.577933	41.847399
3504.756071	491284.337794	41.852404
3504.352728	491300.709745	41.857408
3504.809625	491317.350897	41.862413
3504.757303	491269.852660	41.867418
3504.667344	491230.818263	41.872423
3504.760065	491263.774624	41.877428
3504.527604	491221.166814	41.882432
3504.605561	491231.081261	41.887437
3504.634500	491218.769520	41.892442
3504.792400	491197.118370	41.897447
3504.709315	491179.202506	41.902452
3504.482914	491170.932193	41.907456
3504.199371	491145.805466	41.912461
3504.517920	491155.732576	41.917466
3504.155462	491157.461210	41.922471
3504.556238	491107.763781	41.927476
3504.595055	491134.094118	41.932480
3504.616735	491107.551631	41.937485
3504.617745	491123.049477	41.942490
3504.473760	491086.403729	41.947495
3504.998224	491059.325888	41.952500
3504.457105	491100.283676	41.957504
3504.707354	491060.435449	41.962509
3505.063533	491032.269927	41.967514
3504.751674	491050.045761	41.972519
3504.679627	491026.759397	41.977524
3504.980590	490983.864154	41.982528
3504.432078	490984.305374	41.987533
3504.308226	491007.977283	41.992538
3504.375524	490978.540504	41.997543
3504.929353	490954.901898	42.002548
3504.364148	490978.744892	42.007552
3504.523081	490930.300753	42.012557
3504.343676	490934.077027	42.017562
3504.013029	490927.342509	42.022567
3504.681640	490897.557331	42.027572
3504.467678	490876.116525	42.032576
3504.758142	490896.430992	42.037581
3504.838314	490906.142670	42.042586
3504.293679	490901.974344	42.047591
3504.462756	490845.728645	42.052596
3504.854626	490821.507694	42.057600
3504.677717	490819.611034	42.062605
3504.871088	490797.194099	42.067610
3504.436639	490807.088458	42.072615
3504.626851	490829.191518	42.077620
3504.239164	490791.570753	42.082624
3504.270070	490764.925028	42.087629
3504.886138	490744.112609	42.092634
3504.586573	490740.108107	42.097639
3504.736319	490756.038581	42.102644
3504.591557	490750.844711	42.107648
3503.953406	490719.341151	42.112653
3504.470749	490682.235557	42.117658
3504.336329	490723.180539	42.122663
3504.508853	490713.428828	42.127668
3504.283498	490706.728237	42.132672
3503.900482	490672.753164	42.137677
3504.538159	490653.254085	42.142682
3504.555624	490641.298316	42.147687
3504.305739	490641.489754	42.152692
3504.427309	490671.099805	42.157696
3504.307080	490677.297895	42.162701
3504.505881	490661.160322	42.167706
3503.850257	490638.472190	42.172711
3504.090214	490645.119849	42.177716
3503.883315	490656.497774	42.182720
3504.594717	490641.342785	42.187725
3504.640092	490628.724169	42.192730
3504.499152	490626.568563	42.197735
3504.038614	490608.509215	42.202740
3504.727472	490572.642509	42.207744
3504.685524	490546.007988	42.212749
3504.638132	490545.914181	42.217754
3504.738513	490538.250374	42.222759
3504.996591	490524.382504	42.227764
3503.745791	490545.092886	42.232768
3504.751346	490520.065478	42.237773
3504.840566	490487.686841	42.242778
3504.659492	490492.729686	42.247783
3504.947217	490462.953370	42.252788
3504.376424	490444.809991	42.257792
3504.877486	490439.311370	42.262797
3504.415543	490442.929800	42.267802
3504.132898	490445.456265	42.272807
3504.350009	490438.786947	42.277812
3504.514788	490449.599766	42.282816
3504.446594	490430.566559	42.287821
3504.579382	490416.059975	42.292826
3504.242058	490415.657446	42.297831
3504.130240	490408.482964	42.302836
3504.334409	490396.193639	42.307840
3504.430144	490388.631803	42.312845
3504.449950	490385.741678	42.317850
3503.901424	490386.841350	42.322855
3504.579945	490362.219962	42.327860
3504.500880	490335.692307	42.332864
3504.896950	490310.153156	42.337869
3505.127423	490300.898566	42.342874
3504.434552	490309.415848	42.347879
3504.234567	490332.391550	42.352884
3504.410833	490330.844216	42.357888
3504.585733	490303.617939	42.362893
3504.454419	490281.201055	42.367898
3504.064427	490273.563992	42.372903
3504.713792	490248.339271	42.377908
3504.521441	490288.129418	42.382912
3504.349928	490246.522749	42.387917
3504.722112	490230.053509	42.392922
3504.848769	490203.391856	42.397927
3504.711018	490164.869292	42.402932
3504.565170	490174.566420	42.407936
3504.688955	490144.055766	42.412941
3504.879738	490170.971231	42.417946
3504.251859	490160.484690	42.422951
3505.005823	490093.457225	42.427956
3504.451538	490139.230917	42.432960
3504.354846	490129.318853	42.437965
3504.449410	490084.428191	42.442970
3504.569499	490086.637805	42.447975
3504.654079	490104.807724	42.452980
3504.235915	490076.155354	42.457984
3503.752886	490056.224983	42.462989
3503.980654	490062.418925	42.467994
3504.534673	490054.885827	42.472999
3504.713010	490071.014963	42.478004
3504.463745	490050.085292	42.483008
3504.002176	490025.390401	42.488013
3504.780707	490001.867038	42.493018
3504.548192	490008.538944	42.498023
3504.558784	490034.115532	42.503028
3504.362798	489983.547099	42.508032
3504.461188	490006.020191	42.513037
3504.649259	490011.815224	42.518042
3504.056897	489970.223807	42.523047
3504.976695	489950.882018	42.528052
3504.450468	489983.786494	42.533056
3504.185123	489960.731959	42.538061
3504.357758	489959.641021	42.543066
3504.227171	489966.398134	42.548071
3504.754739	489955.424964	42.553076
3504.420964	489941.447605	42.558080
3504.582723	489901.965463	42.563085
3504.582568	489890.214604	42.568090
3504.318144	489872.072901	42.573095
3504.441400	489846.778843	42.578100
3504.309126	489855.460980	42.583104
3504.036493	489889.490502	42.588109
3504.100976	489854.227615	42.593114
3504.461622	489830.010326	42.598119
3504.646118	489800.857086	42.603124
3504.522879	489805.941624	42.608128
3504.411126	489786.053589	42.613133
3504.428032	489790.710777	42.618138
3504.007713	489817.672678	42.623143
3504.436208	489763.813974	42.628148
3504.170144	489808.074046	42.633152
3503.931543	489791.802256	42.638157
3505.141797	489749.267000	42.643162
3504.367924	489773.296446	42.648167
3504.314940	489752.031519	42.653172
3504.611344	489740.638903	42.658176
3504.237823	489725.705300	42.663181
3504.591090	489689.332797	42.668186
3504.163612	489735.340681	42.673191
3504.458291	489714.577924	42.678196
3504.306124	489668.256391	42.683200
3504.224777	489688.073767	42.688205
3504.353818	489666.628022	42.693210
3504.478853	489694.770182	42.698215
3504.366442	489672.096331	42.703220
3504.144267	489639.765453	42.708224
3504.532997	489658.140988	42.713229
3504.432844	489634.553437	42.718234
3504.133658	489633.131841	42.723239
3504.252576	489617.563163	42.728244
3504.364330	489597.082442	42.733248
3504.412264	489625.996658	42.738253
3503.695012	489610.914684	42.743258
3504.429439	489596.818896	42.748263
3504.275049	489586.662410	42.753268
3504.575185	489587.273441	42.758272
3504.358596	489571.707099	42.763277
3504.518766	489567.427081	42.768282
3504.464031	489534.309790	42.773287
3504.365535	489566.235668	42.778292
3504.540252	489538.653758	42.783296
3504.382966	489527.839230	42.788301
3504.104011	489533.606919	42.793306
3504.309606	489497.713249	42.798311
3504.311673	489509.717307	42.803316
3504.552628	489523.051189	42.808321
3504.533753	489486.686460	42.813325
3504.414135	489475.562041	42.818330
3504.483078	489487.150332	42.823335
3504.475182	489448.656433	42.828340
3504.246312	489469.358430	42.833345
3504.182020	489455.135513	42.838349
3504.195482	489425.907422	42.843354
3504.575143	489454.870775	42.848359
3504.611806	489404.365325	42.853364
3504.408915	489437.422256	42.858369
3504.569959	489404.068028	42.863373
3504.523659	489393.489142	42.868378
3504.520951	489410.204626	42.873383
3504.162624	489379.819583	42.878388
3504.225795	489362.942561	42.883393
3503.941427	489395.202015	42.888397
3504.321206	489338.209392	42.893402
3504.028431	489369.963699	42.898407
3504.319205	489319.164601	42.903412
3504.257832	489374.941968	42.908417
3503.809774	489342.393021	42.913421
3504.525682	489309.052236	42.918426
3504.259433	489347.285835	42.923431
3504.326894	489332.738091	42.928436
3504.415516	489300.002948	42.933441
3504.153015	489311.745034	42.938445
3504.204089	489330.224906	42.943450
3504.030893	489276.662517	42.948455
3504.194203	489307.990281	42.953460
3504.046076	489277.622505	42.958465
3503.918578	489274.654186	42.963469
3504.156282	489302.373908	42.968474
3503.733696	489298.084627	42.973479
3504.297615	489273.024068	42.978484
3504.236554	489258.952449	42.983489
3504.431910	489248.031376	42.988493
3504.121728	489281.561405	42.993498
3503.734776	489264.907391	42.998503
3503.801657	489249.346634	43.003508
3504.296630	489233.515598	43.008513
3504.309919	489258.788897	43.013517
3504.164515	489270.968370	43.018522
3504.069664	489231.778644	43.023527
3504.242281	489204.855057	43.028532
3504.480482	489240.020665	43.033537
3504.431805	489214.752934	43.038541
3504.187541	489219.046322	43.043546
3503.544807	489217.830946	43.048551
3503.882847	489190.020106	43.053556
3504.286037	489166.301767	43.058561
3504.096365	489161.671731	43.063565
3504.278232	489190.109574	43.068570
3504.016916	489200.686539	43.073575
3504.303828	489156.371099	43.078580
3504.342846	489161.582123	43.083585
3504.003913	489192.634889	43.088589
3504.428963	489190.035099	43.093594
3504.055314	489174.037382	43.098599
3504.601600	489175.065395	43.103604
3503.828135	489165.057175	43.108609
3504.138926	489126.816169	43.113613
3504.529236	489087.296205	43.118618
3504.340283	489120.047572	43.123623
3504.104526	489144.246030	43.128628
3504.063058	489132.653186	43.133633
3504.199791	489112.167993	43.138637
3504.432840	489097.745857	43.143642
3504.278455	489131.099572	43.148647
3504.090710	489102.105390	43.153652
3503.835947	489090.141011	43.158657
3503.506435	489096.828567	43.163661
3504.380831	489085.090947	43.168666
3504.506546	489074.991221	43.173671
3504.142879	489075.403265	43.178676
3504.533450	489089.726858	43.183681
3504.178799	489087.199630	43.188685
3504.291490	489065.299915	43.193690
3503.751137	489055.913279	43.198695
3504.684389	489015.547567	43.203700
3504.381576	489025.928577	43.208705
3504.303866	489069.248860	43.213709
3504.509568	489062.834124	43.218714
3503.944814	489016.626854	43.223719
3504.427763	488981.802731	43.228724
3504.465260	489002.564446	43.233729
3504.317090	489015.149742	43.238733
3504.147563	488979.365028	43.243738
3504.219597	488979.961477	43.248743
3504.674104	488952.283840	43.253748
3504.536609	488977.074816	43.258753
3504.354136	488950.814822	43.263757
3504.190688	488940.507462	43.268762
3504.065976	488903.043974	43.273767
3504.125722	488942.442540	43.278772
3503.933224	488955.338799	43.283777
3504.296949	488957.358082	43.288781
3504.387175	488948.682179	43.293786
3504.187008	488919.588375	43.298791
3504.577852	488879.257446	43.303796
3504.595663	488920.384890	43.308801
3504.270541	488909.697840	43.313805
3504.227613	488870.043282	43.318810
3504.512442	488839.606377	43.323815
3504.576968	488871.760927	43.328820
3504.393855	488874.221216	43.333825
3504.602110	488865.830539	43.338829
3504.551489	488839.093674	43.343834
3504.357380	488817.849999	43.348839
3504.499719	488812.204992	43.353844
3504.205227	488786.013127	43.358849
3504.510811	488765.754140	43.363853
3504.239501	488777.599255	43.368858
3504.156198	488806.687424	43.373863
3503.959256	488760.725317	43.378868
3504.183068	488757.144207	43.383873
3504.054523	488746.932531	43.388877
3504.508439	488754.205539	43.393882
3504.485544	488740.330116	43.398887
3504.101820	488750.318835	43.403892
3503.891209	488729.482898	43.408897
3504.397557	488686.955205	43.413901
3504.509109	488725.434269	43.418906
3504.022909	488715.988251	43.423911
3504.717934	488689.690518	43.428916
3504.197228	488700.359410	43.433921
3504.401998	488674.544367	43.438925
3504.579666	488697.361061	43.443930
3503.914892	488680.345211	43.448935
3504.279992	488639.916534	43.453940
3504.529070	488628.328117	43.458945
3504.165389	488672.910191	43.463949
3503.970913	488652.223579	43.468954
3504.270785	488625.481673	43.473959
3504.307048	488659.464585	43.478964
3504.045508	488634.432336	43.483969
3504.683960	488616.906538	43.488973
3504.169366	488620.837554	43.493978
3504.286062	488595.390900	43.498983
3504.315657	488619.294820	43.503988
3504.638376	488566.766430	43.508993
3503.995198	488602.173829	43.513997
3504.013420	488587.177411	43.519002
3504.185904	488560.455546	43.524007
3504.066900	488602.010535	43.529012
3504.204130	488549.865990	43.534017
3504.159830	488558.332201	43.539021
3504.194572	488549.208998	43.544026
3504.488597	488530.065975	43.549031
3504.008012	488558.153579	43.554036
3503.852322	488536.093054	43.559041
3504.052254	488506.884729	43.564045
3504.376848	488482.418147	43.569050
3504.123499	488535.796925	43.574055
3504.058883	488537.833297	43.579060
3504.130264	488540.050791	43.584065
3504.021351	488549.287028	43.589069
3504.210268	488523.524939	43.594074
3504.357961	488488.955515	43.599079
3504.362095	488506.025294	43.604084
3503.991952	488487.240466	43.609089
3504.433063	488474.811139	43.614093
3504.143561	488483.316136	43.619098
3504.196525	488433.970568	43.624103
3504.087553	488466.001264	43.629108
3504.124208	488483.623119	43.634113
3503.922792	488461.468426	43.639117
3503.922619	488437.762273	43.644122
3504.133203	488436.563943	43.649127
3503.641567	488482.027811	43.654132
3503.691316	488452.691176	43.659137
3504.385115	488423.202053	43.664141
3504.261865	488451.638573	43.669146
3504.122196	488441.884379	43.674151
3504.100895	488416.763221	43.679156
3504.691123	488399.143536	43.684161
3504.543746	488407.372833	43.689165
3504.309947	488415.362514	43.694170
3504.165175	488408.293788	43.699175
3503.913658	488364.922719	43.704180
3504.319242	488387.399838	43.709185
3504.037033	488396.207649	43.714189
3503.929204	488366.591859	43.719194
3504.059098	488401.877450	43.724199
3504.074789	488354.766359	43.729204
3504.290987	488378.489128	43.734209
3503.816476	488363.317135	43.739213
3504.466953	488331.352648	43.744218
3504.374569	488381.768455	43.749223
3503.947148	488354.533259	43.754228
3504.098247	488335.615246	43.759233
3504.478155	488325.728222	43.764237
3504.306565	488328.389377	43.769242
3504.474549	488328.666756	43.774247
3503.643435	488320.237487	43.779252
3504.529119	488302.115127	43.784257
3504.338414	488310.401968	43.789261
3504.568399	488302.514155	43.794266
3504.691162	488281.118490	43.799271
3504.083028	488294.334160	43.804276
3504.219807	488236.566161	43.809281
3504.126549	488251.726678	43.814285
3503.973278	488260.058280	43.819290
3504.323624	488226.216171	43.824295
3504.087210	488240.690155	43.829300
3504.300031	488269.529726	43.834305
3504.011993	488253.112461	43.839309
3504.377949	488229.044255	43.844314
3503.613815	488218.780781	43.849319
3503.512338	488231.257907	43.854324
3503.430066	488229.143408	43.859329
3504.245322	488219.339488	43.864333
3504.431479	488198.389604	43.869338
3504.075627	488255.077938	43.874343
3503.862166	488248.020009	43.879348
3504.587508	488210.471461	43.884353
3504.309892	488182.047280	43.889357
3504.210641	488215.748474	43.894362
3504.272778	488218.727289	43.899367
3503.946268	488198.162359	43.904372
3504.347419	488170.593328	43.909377
3504.399344	488181.475938	43.914381
3504.122860	488146.922276	43.919386
3504.091253	488166.429450	43.924391
3503.805192	488145.756760	43.929396
3504.532141	488156.228770	43.934401
3504.128080	488149.099617	43.939405
3504.176879	488158.412428	43.944410
3503.879938	488127.103883	43.949415
3504.272837	488096.901984	43.954420
3504.276420	488121.114574	43.959425
3504.139350	488149.047180	43.964429
3503.720706	488121.759608	43.969434
3503.695305	488124.296377	43.974439
3504.247907	488096.196752	43.979444
3504.367209	488093.290551	43.984449
3504.199220	488126.445560	43.989453
3504.170195	488119.966294	43.994458
3504.182091	488084.911046	43.999463
3504.539784	488088.501689	44.004468
3504.288832	488090.314282	44.009473
3504.626671	488044.519199	44.014477
3504.335516	488080.125208	44.019482
3503.852494	488053.252954	44.024487
3504.338080	488015.691260	44.029492
3504.176401	488043.070702	44.034497
3504.141286	488021.851663	44.039501
3503.893959	488000.514174	44.044506
3503.856704	488046.869721	44.049511
3503.964753	488029.477867	44.054516
3503.803189	487999.920654	44.059521
3504.076389	488035.032311	44.064525
3503.890510	488012.672017	44.069530
3504.020939	487995.428561	44.074535
3504.161364	488034.309706	44.079540
3504.232736	488001.220462	44.084545
3504.142644	488002.754363	44.089549
3503.802587	487992.626365	44.094554
3504.181515	487968.454469	44.099559
3503.929127	488010.285109	44.104564
3503.923959	487973.965968	44.109569
3503.874288	488005.076269	44.114573
3504.204780	487979.240412	44.119578
3504.448346	488005.644062	44.124583
3504.256199	487966.922999	44.129588
3504.351278	487987.474101	44.134593
3504.378864	487963.965592	44.139597
3504.231647	487936.634856	44.144602
3504.312591	487969.142929	44.149607
3504.237875	487936.026005	44.154612
3504.384420	487913.916990	44.159617
3504.119425	487911.780678	44.164621
3504.096823	487926.474387	44.169626
3503.895990	487923.618756	44.174631
3504.242874	487888.712826	44.179636
3504.449783	487911.373876	44.184641
3503.753509	487887.219840	44.189645
3503.297801	487884.556453	44.194650
3503.474086	487888.023838	44.199655
3504.109656	487869.180761	44.204660
3504.387464	487855.054543	44.209665
3503.930393	487857.608916	44.214669
3504.651029	487887.736516	44.219674
3504.125128	487918.263699	44.224679
3504.054689	487879.928469	44.229684
3504.175358	487838.371639	44.234689
3504.206674	487853.360818	44.239693
3504.267781	487880.603971	44.244698
3504.192584	487885.428151	44.249703
3504.277366	487869.863435	44.254708
3504.237731	487845.402944	44.259713
3504.083648	487813.969994	44.264717
3504.237484	487799.103489	44.269722
3504.218781	487850.775457	44.274727
3504.045859	487859.870177	44.279732
3503.944330	487847.830138	44.284737
3504.206814	487803.312781	44.289741
3504.336543	487780.193150	44.294746
3504.111293	487811.179548	44.299751
3503.790866	487827.440080	44.304756
3503.712097	487822.538908	44.309761
3503.735828	487828.208617	44.314765
3503.610410	487794.339621	44.319770
3503.406326	487793.257444	44.324775
3504.061775	487775.829501	44.329780
3503.823949	487814.517595	44.334785
3503.923864	487825.848727	44.339789
3504.100301	487828.454948	44.344794
3503.857574	487812.131452	44.349799
3504.252163	487791.350804	44.354804
3504.265870	487790.132894	44.359809
3503.745208	487810.832157	44.364813
3503.946507	487800.365218	44.369818
3504.119465	487770.400187	44.374823
3504.251934	487750.066168	44.379828
3504.428378	487762.752957	44.384833
3503.920351	487810.348572	44.389837
3504.194335	487800.123425	44.394842
3503.707842	487770.313273	44.399847
3504.236704	487720.789331	44.404852
3504.096122	487703.588443	44.409857
3503.807610	487709.966067	44.414861
3504.277470	487700.013846	44.419866
3504.413538	487717.114138	44.424871
3503.941108	487728.434472	44.429876
3504.476696	487717.914655	44.434881
3504.305063	487679.645671	44.439885
3503.993029	487708.417075	44.444890
3504.256660	487728.384600	44.449895
3503.423842	487704.251911	44.454900
3504.359057	487681.714044	44.459905
3503.369530	487707.705117	44.464909
3503.450938	487708.604062	44.469914
3503.754273	487706.884467	44.474919
3504.198502	487711.170692	44.479924
3503.937391	487707.564712	44.484929
3503.534278	487714.770946	44.489933
3503.915450	487698.551373	44.494938
3504.397082	487676.439781	44.499943
3504.448300	487696.592878	44.504948
3504.452180	487696.389640	44.509953
3503.904650	487713.648630	44.514957
3504.240427	487698.094762	44.519962
3504.180839	487694.406274	44.524967
3503.811627	487689.348345	44.529972
3503.753322	487653.442241	44.534977
3503.858834	487663.860771	44.539981
3503.896081	487652.203926	44.544986
3503.695287	487653.704695	44.549991
3503.642978	487642.771187	44.554996
3503.963055	487639.022685	44.560001
3504.160278	487633.469967	44.565005
3504.705097	487614.640983	44.570010
3504.450246	487617.315396	44.575015
3504.340236	487657.857896	44.580020
3504.370874	487645.492903	44.585025
3504.193373	487641.975010	44.590029
3504.156236	487630.127283	44.595034
3504.325249	487631.366981	44.600039
3504.202539	487638.174332	44.605044
3504.267344	487614.406228	44.610049
3503.969986	487615.263727	44.615053
3504.129752	487605.917688	44.620058
3504.264230	487588.217316	44.625063
3504.212818	487584.122262	44.630068
3504.527782	487536.404626	44.635073
3504.841334	487538.128053	44.640077
3503.801631	487545.536274	44.645082
3504.157820	487550.140389	44.650087
3504.305940	487562.223909	44.655092
3504.274312	487551.489707	44.660097
3504.301929	487541.809925	44.665101
3504.461889	487509.465677	44.670106
3504.597769	487496.577387	44.675111
3504.482494	487506.625643	44.680116
3504.504709	487493.147434	44.685121
3503.998335	487481.475088	44.690125
3503.944356	487491.361694	44.695130
3504.189853	487492.133403	44.700135
3503.748402	487494.989295	44.705140
3503.998754	487473.268617	44.710145
3503.497008	487456.479185	44.715149
3503.668303	487457.414593	44.720154
3504.261261	487457.726133	44.725159
3504.724062	487416.215626	44.730164
3504.384029	487440.736672	44.735169
3504.099392	487467.731116	44.740173
3504.271443	487434.726291	44.745178
3504.513770	487399.937307	44.750183
3504.006322	487435.933301	44.755188
3504.078680	487401.981694	44.760193
3504.473861	487384.087959	44.765197
3504.764923	487377.000625	44.770202
3504.109288	487356.233515	44.775207
3503.907650	487393.700971	44.780212
3504.172523	487390.974286	44.785217
3503.583901	487375.262310	44.790221
3504.028242	487349.103665	44.795226
3504.283752	487347.948826	44.800231
3503.591804	487370.853893	44.805236
3503.877348	487365.185825	44.810241
3503.490988	487372.237568	44.815245
3503.559444	487390.868551	44.820250
3504.079420	487383.187813	44.825255
3504.110986	487353.649731	44.830260
3503.716135	487397.530516	44.835265
3503.767471	487366.418961	44.840269
3504.096429	487392.100766	44.845274
3504.063456	487348.084955	44.850279
3503.776888	487355.931447	44.855284
3504.171965	487364.683347	44.860289
3504.311202	487341.662997	44.865293
3504.194649	487330.942093	44.870298
3503.946730	487364.111059	44.875303
3503.952416	487373.785667	44.880308
3504.245264	487352.007479	44.885313
3503.912595	487337.622762	44.890317
3503.734420	487318.097237	44.895322
3503.977760	487315.829860	44.900327
3503.579178	487322.478295	44.905332
3504.155614	487336.469896	44.910337
3503.931877	487355.704322	44.915341
3504.115843	487331.765062	44.920346
3504.009375	487336.037093	44.925351
3504.022813	487329.550847	44.930356
3504.390518	487299.047726	44.935361
3504.277946	487287.971568	44.940365
3504.108138	487284.148448	44.945370
3503.868619	487302.068332	44.950375
3503.980538	487320.439228	44.955380
3504.262110	487305.653466	44.960385
3504.002025	487323.829867	44.965389
3503.982570	487300.327975	44.970394
3504.302310	487291.412414	44.975399
3504.239154	487289.345445	44.980404
3504.007051	487285.937430	44.985409
3503.797069	487286.223903	44.990413
3503.950540	487283.261523	44.995418
3504.092271	487286.734478	45.000423
3504.093717	487287.696739	45.005428
3503.809377	487277.660868	45.010433
3503.712545	487284.362940	45.015437
3503.916996	487265.334120	45.020442
3503.904609	487233.016642	45.025447
3503.893137	487244.720325	45.030452
3504.315859	487258.888250	45.035457
3503.963072	487239.035639	45.040461
3503.918071	487191.171401	45.045466
3504.252833	487200.490143	45.050471
3503.278603	487229.164295	45.055476
3503.880428	487206.577247	45.060481
3503.724832	487219.063588	45.065485
3504.622270	487188.172623	45.070490
3504.248023	487198.312628	45.075495
3504.030483	487197.435172	45.080500
3504.105351	487215.812025	45.085505
3504.102520	487171.537757	45.090509
3503.874812	487162.100766	45.095514
3504.025806	487164.153865	45.100519
3503.862785	487182.213744	45.105524
3503.814449	487218.238903	45.110529
3503.933310	487224.197702	45.115533
3504.091102	487224.780654	45.120538
3504.097289	487221.081679	45.125543
3503.909626	487219.085038	45.130548
3503.706183	487196.219986	45.135553
3503.821465	487214.539796	45.140557
3503.614308	487204.238400	45.145562
3503.735318	487197.481820	45.150567
3503.617254	487204.187276	45.155572
3504.458192	487179.434789	45.160577
3504.294425	487189.794820	45.165581
3504.278784	487204.032067	45.170586
3503.830750	487170.820842	45.175591
3504.209451	487144.469662	45.180596
3504.559207	487138.639406	45.185601
3503.867647	487133.834904	45.190605
3503.842678	487130.039520	45.195610
3503.994758	487161.980491	45.200615
3503.727066	487147.534704	45.205620
3503.905074	487147.759859	45.210625
3503.912197	487167.869826	45.215629
3503.836462	487149.543722	45.220634
3503.949840	487163.811265	45.225639
3503.907368	487135.449673	45.230644
3504.081340	487100.164369	45.235649
3503.947295	487098.919109	45.240653
3504.019095	487112.484052	45.245658
3503.567758	487132.210594	45.250663
3503.468838	487154.059698	45.255668
3504.015063	487150.123386	45.260673
3503.618963	487150.489934	45.265677
3503.910792	487129.623492	45.270682
3504.353514	487117.902238	45.275687
3503.732334	487135.122731	45.280692
3503.605483	487140.005920	45.285697
3503.495456	487149.040380	45.290701
3503.729020	487159.692236	45.295706
3504.198502	487179.323856	45.300711
3503.840842	487144.781204	45.305716
3503.971353	487128.043530	45.310721
3503.915487	487152.773322	45.315725
3503.957403	487144.762782	45.320730
3504.230043	487113.869129	45.325735
3504.194538	487089.457674	45.330740
3503.635897	487109.049225	45.335745
3504.319319	487129.964186	45.340749
3504.025054	487126.768598	45.345754
3504.359448	487124.030888	45.350759
3503.859969	487118.942736	45.355764
3504.162098	487095.085820	45.360769
3503.899744	487095.887151	45.365773
3504.247342	487112.245345	45.370778
3504.432819	487090.433171	45.375783
3504.151865	487078.421003	45.380788
3504.257086	487060.268846	45.385793
3504.552530	487045.278059	45.390797
3504.267523	487041.929019	45.395802
3504.135390	487073.104529	45.400807
3504.311757	487077.078628	45.405812
3504.241951	487051.659388	45.410817
3504.266352	486998.920537	45.415821
3503.779055	487009.433115	45.420826
3503.889973	487028.057741	45.425831
3503.683260	487007.624564	45.430836
3503.912902	487002.775754	45.435841
3503.937324	487036.408827	45.440845
3503.953495	487047.854972	45.445850
3503.995429	487046.125974	45.450855
3504.155327	487043.517147	45.455860
3504.301230	486999.674895	45.460865
3504.236953	486992.998185	45.465869
3504.003842	486999.316631	45.470874
3504.434206	487001.274937	45.475879
3503.723261	487016.382084	45.480884
3504.145814	487005.575794	45.485889
3504.290707	486991.014023	45.490893
3504.183936	486946.553028	45.495898
3504.234715	486943.404193	45.500903
3503.818122	486941.393046	45.505908
3504.011242	486950.886270	45.510913
3503.705446	486956.962926	45.515917
3503.867049	486976.998021	45.520922
3504.026071	486953.011571	45.525927
3503.562619	486938.748539	45.530932
3503.323651	486956.466026	45.535937
3503.672037	486964.060352	45.540941
3503.950621	486977.136787	45.545946
3503.944685	486979.822606	45.550951
3503.732332	486982.439732	45.555956
3503.927222	486983.574067	45.560961
3503.355007	486998.507329	45.565965
3503.688037	486988.373733	45.570970
3504.125127	486990.229661	45.575975
3503.874592	486986.368582	45.580980
3504.035510	486988.521448	45.585985
3503.739247	486991.506441	45.590989
3503.972084	486993.799915	45.595994
3503.831115	487009.982122	45.600999
3504.021983	487008.381556	45.606004
3504.084367	487005.940109	45.611009
3503.855740	486991.589346	45.616013
3504.055242	486949.156934	45.621018
3504.416894	486902.595477	45.626023
3503.831107	486904.663733	45.631028
3504.238605	486900.901270	45.636033
3504.045012	486905.997701	45.641037
3504.073895	486915.212950	45.646042
3504.003470	486903.977933	45.651047
3503.585411	486933.831084	45.656052
3503.970383	486953.476293	45.661057
3504.062478	486943.228777	45.666061
3504.141275	486873.662443	45.671066
3504.161156	486873.811276	45.676071
3503.877688	486918.587407	45.681076
3504.030746	486889.130722	45.686081
3504.111876	486875.946718	45.691085
3503.894654	486880.894914	45.696090
3503.870404	486932.772876	45.701095
3503.861313	486938.346720	45.706100
3503.662799	486928.195784	45.711105
3503.807315	486923.664357	45.716109
3503.972263	486875.563515	45.721114
3503.864593	486887.333279	45.726119
3503.757373	486899.052308	45.731124
3503.710015	486911.521742	45.736129
3504.060423	486916.684168	45.741133
3503.812125	486910.695071	45.746138
3504.038592	486891.105157	45.751143
3503.932136	486884.637710	45.756148
3504.121485	486902.996770	45.761153
3503.861196	486910.130073	45.766157
3503.875062	486905.517974	45.771162
3504.295764	486889.950028	45.776167
3503.793972	486903.504456	45.781172
3503.879957	486911.342908	45.786177
3504.502889	486892.095602	45.791181
3504.255780	486871.060764	45.796186
3504.218590	486866.861992	45.801191
3503.778801	486858.370221	45.806196
3503.532096	486829.787161	45.811201
3504.317212	486812.033899	45.816205
3503.972365	486812.949596	45.821210
3504.294053	486847.751825	45.826215
3504.063901	486868.507509	45.831220
3504.238875	486851.255981	45.836225
3503.651042	486833.719727	45.841229
3503.733197	486822.764498	45.846234
3503.964747	486820.701560	45.851239
3503.742503	486810.554312	45.856244
3503.960743	486797.753853	45.861249
3503.644915	486800.741967	45.866253
3503.636855	486812.951962	45.871258
3504.215888	486826.791553	45.876263
3504.046534	486821.651146	45.881268
3504.047920	486769.725838	45.886273
3504.320395	486775.660499	45.891277
3504.555274	486767.923257	45.896282
3504.446108	486747.271750	45.901287
3503.913356	486781.246624	45.906292
3504.254890	486792.286890	45.911297
3503.903888	486796.850982	45.916301
3503.632789	486786.306173	45.921306
3503.816101	486789.215403	45.926311
3503.702692	486786.345784	45.931316
3503.703040	486755.545245	45.936321
3503.984670	486737.516877	45.941325
3503.441216	486751.128656	45.946330
3503.937919	486784.383578	45.951335
3503.828016	486809.628940	45.956340
3504.031758	486806.810517	45.961345
3503.989242	486789.238696	45.966349
3503.748350	486803.562499	45.971354
3503.828189	486787.288463	45.976359
3503.770557	486774.328953	45.981364
3503.925824	486747.202001	45.986369
3504.215008	486718.990009	45.991373
3504.632525	486705.094158	45.996378
3504.299639	486709.959360	46.001383
3503.613271	486732.611013	46.006388
3504.599771	486723.184540	46.011393
3504.399990	486706.751992	46.016397
3503.742510	486717.798214	46.021402
3503.937117	486731.344019	46.026407
3503.914788	486730.486348	46.031412
3504.163985	486673.303756	46.036417
3504.044367	486676.058244	46.041421
3504.031573	486677.782670	46.046426
3504.321924	486674.291973	46.051431
3503.712547	486680.568673	46.056436
3504.459771	486654.006598	46.061441
3504.492869	486649.897988	46.066445
3504.273816	486698.615854	46.071450
3504.004434	486687.361495	46.076455
3503.854977	486670.363714	46.081460
3504.312236	486658.690542	46.086465
3504.071282	486677.523099	46.091469
3503.538589	486639.511730	46.096474
3504.230033	486604.751638	46.101479
3503.937626	486623.339083	46.106484
3503.788652	486656.696273	46.111489
3504.117715	486654.465930	46.116493
3503.722483	486660.455496	46.121498
3503.860614	486658.660600	46.126503
3503.722973	486650.880868	46.131508
3504.291984	486663.506345	46.136513
3504.393159	486664.098263	46.141517
3504.014533	486643.033300	46.146522
3504.178711	486621.325276	46.151527
3503.743452	486631.829835	46.156532
3503.875394	486628.060211	46.161537
3504.020196	486622.464828	46.166541
3503.909775	486616.960439	46.171546
3503.676086	486602.711501	46.176551
3503.868709	486592.143955	46.181556
3503.999123	486586.905449	46.186561
3503.539978	486631.710015	46.191565
3503.625089	486623.844408	46.196570
3503.976636	486595.115788	46.201575
3504.321253	486573.733807	46.206580
3503.941067	486619.995038	46.211585
3503.967281	486605.502390	46.216589
3503.677408	486579.256098	46.221594
3503.451561	486572.047525	46.226599
3503.211976	486577.455267	46.231604
3503.974767	486588.479732	46.236609
3504.164717	486575.025026	46.241613
3504.043429	486604.274535	46.246618
3504.156224	486593.567629	46.251623
3503.952748	486558.138344	46.256628
3504.120024	486555.072351	46.261633
3504.522847	486593.712322	46.266637
3504.223855	486583.171809	46.271642
3503.701352	486551.795008	46.276647
3503.665732	486552.155253	46.281652
3503.950781	486557.328106	46.286657
3504.178071	486528.922980	46.291661
3504.016531	486553.568929	46.296666
3504.358144	486566.382387	46.301671
3503.922212	486566.552603	46.306676
3504.042147	486557.009710	46.311681
3503.778081	486544.639923	46.316685
3504.038127	486553.008263	46.321690
3504.006695	486550.176312	46.326695
3504.124769	486545.345019	46.331700
3503.970892	486524.953635	46.336705
3504.068648	486527.572471	46.341709
3504.250423	486494.969764	46.346714
3504.517135	486507.744440	46.351719
3504.359451	486522.764533	46.356724
3504.099300	486490.586278	46.361729
3504.689236	486455.740640	46.366733
3504.161632	486494.527861	46.371738
3504.076390	486476.101295	46.376743
3504.171237	486457.899547	46.381748
3504.688222	486428.891234	46.386753
3504.441973	486441.240430	46.391757
3504.021831	486440.192321	46.396762
3504.304998	486439.387674	46.401767
3503.912561	486458.801641	46.406772
3503.704897	486439.178560	46.411777
3503.389339	486434.821049	46.416781
3504.005704	486429.303060	46.421786
3504.249319	486398.868778	46.426791
3503.998789	486386.800707	46.431796
3504.661361	486376.868006	46.436801
3504.654486	486369.624749	46.441805
3503.893281	486368.174602	46.446810
3504.170658	486359.113325	46.451815
3504.197435	486389.808894	46.456820
3503.749505	486387.346702	46.461825
3503.945939	486365.329333	46.466829
3504.164043	486347.057339	46.471834
3503.989854	486382.040106	46.476839
3504.017497	486387.456326	46.481844
3504.259185	486367.508854	46.486849
3504.032387	486348.496621	46.491853
3503.900350	486324.656706	46.496858
3504.164265	486330.947478	46.501863
3503.758889	486363.028545	46.506868
3503.972890	486347.188869	46.511873
3504.071283	486341.904697	46.516877
3503.729097	486325.544989	46.521882
3503.878206	486315.946705	46.526887
3504.148818	486308.304951	46.531892
3503.977018	486340.298481	46.536897
3504.291918	486347.543726	46.541901
3503.761080	486350.869850	46.546906
3504.120327	486344.531256	46.551911
3504.070429	486341.296914	46.556916
3503.846882	486314.837138	46.561921
3503.941602	486337.821746	46.566925
3503.670741	486325.655530	46.571930
3503.819093	486306.482645	46.576935
3503.200261	486318.890804	46.581940
3503.479332	486311.045074	46.586945
3503.638004	486312.185174	46.591949
3503.615272	486331.490180	46.596954
3503.940916	486349.574931	46.601959
3504.104082	486364.088501	46.606964
3503.670589	486349.212376	46.611969
3503.926568	486340.407772	46.616973
3504.075642	486325.186257	46.621978
3503.456128	486305.830770	46.626983
3503.795992	486305.523756	46.631988
3504.285540	486286.550226	46.636993
3504.290834	486280.419532	46.641997
3503.780990	486297.977797	46.647002
3503.976592	486337.765554	46.652007
3504.068656	486308.013658	46.657012
3503.987795	486288.623681	46.662017
3503.949087	486316.999358	46.667021
3503.854196	486344.725294	46.672026
3504.162179	486310.734512	46.677031
3503.561187	486295.479538	46.682036
3503.240120	486284.334430	46.687041
3504.012958	486286.441325	46.692045
3504.095109	486271.078364	46.697050
3503.936967	486283.008457	46.702055
3504.065914	486309.635207	46.707060
3504.082297	486310.037897	46.712065
3503.531231	486293.559194	46.717069
3503.593265	486291.016392	46.722074
3503.748104	486274.628747	46.727079
3503.591222	486288.433056	46.732084
3503.568620	486290.513687	46.737089
3503.913384	486294.765294	46.742093
3503.685636	486294.851949	46.747098
3504.160839	486272.385135	46.752103
3503.902070	486290.460986	46.757108
3504.039669	486300.824528	46.762113
3503.650967	486287.461074	46.767117
3504.121507	486284.043149	46.772122
3504.081384	486293.117624	46.777127
3503.390477	486294.898596	46.782132
3504.157571	486272.284331	46.787137
3504.385521	486264.953262	46.792141
3504.065390	486245.449077	46.797146
3504.280070	486224.796485	46.802151
3504.206407	486266.400050	46.807156
3503.686267	486285.682395	46.812161
3503.919389	486286.912050	46.817165
3503.807030	486277.405731	46.822170
3504.190489	486283.576306	46.827175
3503.930729	486292.432193	46.832180
3504.056992	486263.840003	46.837185
3504.280113	486225.353739	46.842189
3503.994573	486210.200822	46.847194
3503.913043	486229.667203	46.852199
3503.848469	486247.408442	46.857204
3503.939313	486231.486815	46.862209
3503.857299	486232.766280	46.867213
3503.182281	486227.502991	46.872218
3504.070998	486229.996859	46.877223
3503.812779	486260.484376	46.882228
3503.839378	486239.101624	46.887233
3504.047511	486238.460809	46.892237
3503.695898	486247.736515	46.897242
3503.639901	486246.174902	46.902247
3503.827644	486223.449503	46.907252
3504.215810	486206.720963	46.912257
3504.449614	486214.485677	46.917261
3504.132684	486212.205399	46.922266
3504.352483	486176.860493	46.927271
3504.131743	486183.987815	46.932276
3503.729366	486215.308751	46.937281
3504.211784	486222.274267	46.942285
3503.939826	486234.475678	46.947290
3504.119215	486203.595297	46.952295
3504.007732	486171.950273	46.957300
3503.832635	486147.762321	46.962305
3504.519155	486142.537125	46.967309
3503.414751	486162.215895	46.972314
3504.083059	486166.923000	46.977319
3503.845646	486138.134798	46.982324
3503.522455	486167.416882	46.987329
3503.682672	486181.981717	46.992333
3503.817254	486193.764280	46.997338
3503.862469	486191.477424	47.002343
3503.587514	486197.498785	47.007348
3503.721615	486195.501842	47.012353
3503.645596	486196.527061	47.017357
3503.594928	486201.398448	47.022362
3504.055273	486186.938192	47.027367
3504.246890	486197.445233	47.032372
3504.069443	486198.891763	47.037377
3503.960820	486187.510382	47.042381
3504.004519	486203.917383	47.047386
3503.984940	486196.372108	47.052391
3503.952288	486176.467797	47.057396
3503.988809	486131.222359	47.062401
3504.042003	486121.892440	47.067405
3503.770527	486115.704115	47.072410
3503.602710	486127.787814	47.077415
3503.207033	486145.176194	47.082420
3503.624063	486200.127337	47.087425
3503.722330	486198.186719	47.092429
3504.053348	486155.782427	47.097434
3504.209090	486138.026694	47.102439
3503.902355	486146.788752	47.107444
3503.779508	486155.065801	47.112449
3503.908771	486156.615841	47.117453
3503.772514	486123.404182	47.122458
3503.335103	486142.217652	47.127463
3503.674233	486148.699238	47.132468
3503.988464	486175.246231	47.137473
3503.962318	486188.371367	47.142477
3503.816203	486180.187501	47.147482
3503.897520	486146.536214	47.152487
3504.017473	486136.334525	47.157492
3503.845077	486135.804507	47.162497
3504.225709	486146.889627	47.167501
3504.208772	486128.401272	47.172506
3504.653827	486128.280272	47.177511
3503.992384	486120.735090	47.182516
3503.560594	486129.770223	47.187521
3504.117749	486141.435372	47.192525
3504.002145	486143.784019	47.197530
3504.153943	486099.837457	47.202535
3503.911146	486104.435271	47.207540
3503.838595	486134.893644	47.212545
3504.162554	486117.060645	47.217549
3504.010168	486093.780923	47.222554
3504.110154	486084.190288	47.227559
3503.833205	486100.800036	47.232564
3503.892942	486097.953609	47.237569
3503.813425	486124.461582	47.242573
3504.004041	486129.548155	47.247578
3503.887026	486067.811542	47.252583
3503.444760	486083.890166	47.257588
3503.783308	486096.299140	47.262593
3504.254152	486091.158677	47.267597
3503.622660	486092.474333	47.272602
3504.169436	486099.683026	47.277607
3504.193998	486117.967562	47.282612
3504.220508	486080.322647	47.287617
3503.978294	486084.667071	47.292621
3503.810825	486091.178082	47.297626
3504.116209	486039.050768	47.302631
3504.265451	486023.575686	47.307636
3504.158446	486035.599170	47.312641
3503.975429	486040.440855	47.317645
3503.827775	486078.104993	47.322650
3504.117276	486037.429459	47.327655
3503.743390	486056.486276	47.332660
3504.049341	486072.244015	47.337665
3503.866202	486023.030856	47.342669
3503.594037	486050.683913	47.347674
3503.925036	486052.455381	47.352679
3504.181609	486070.500652	47.357684
3503.947329	486009.846257	47.362689
3503.831041	486025.214821	47.367693
3504.056936	486038.654850	47.372698
3504.219045	486018.820915	47.377703
3504.375561	485991.692698	47.382708
3504.245795	486009.191157	47.387713
3504.073966	486014.740329	47.392717
3503.922405	486019.222422	47.397722
3504.632569	485958.621243	47.402727
3504.460887	485946.287129	47.407732
3504.101839	485964.936404	47.412737
3503.840490	485982.506344	47.417741
3503.752419	486006.837418	47.422746
3503.860455	486007.124307	47.427751
3503.917186	485994.956768	47.432756
3503.985402	485978.633222	47.437761
3503.831475	485915.432790	47.442765
3504.051633	485919.906819	47.447770
3504.236471	485905.996504	47.452775
3504.110547	485931.549519	47.457780
3503.944554	485921.950179	47.462785
3504.223995	485906.606408	47.467789
3504.202307	485921.808121	47.472794
3504.127857	485896.489405	47.477799
3504.028125	485872.897127	47.482804
3504.197042	485878.696452	47.487809
3504.121470	485899.226107	47.492813
3503.709980	485919.758171	47.497818
3504.009002	485917.633813	47.502823
3503.844243	485938.329506	47.507828
3503.691270	485947.472640	47.512833
3504.178071	485940.860451	47.517837
3504.027573	485946.254289	47.522842
3503.865889	485931.385541	47.527847
3503.673262	485912.316814	47.532852
3503.994920	485913.735145	47.537857
3503.919466	485884.262373	47.542861
3503.706946	485868.844340	47.547866
3504.058879	485882.416542	47.552871
3504.181106	485899.672630	47.557876
3503.509727	485878.805077	47.562881
3504.296174	485854.616771	47.567885
3504.427220	485849.681932	47.572890
3503.804648	485865.231962	47.577895
3503.613691	485899.762306	47.582900
3503.652383	485852.489430	47.587905
3503.967630	485854.162084	47.592909
3503.958502	485873.668044	47.597914
3504.082177	485897.560502	47.602919
3503.786093	485883.878162	47.607924
3503.921371	485871.900775	47.612929
3504.270259	485866.120934	47.617933
3503.901971	485871.650536	47.622938
3503.599942	485846.165077	47.627943
3503.965415	485833.543351	47.632948
3503.790344	485880.584523	47.637953
3504.101090	485865.742381	47.642957
3503.485141	485858.645855	47.647962
3504.079052	485824.710346	47.652967
3503.957878	485867.031542	47.657972
3503.716643	485873.047674	47.662977
3503.685933	485855.878420	47.667981
3503.923667	485826.153417	47.672986
3503.844502	485838.881881	47.677991
3503.972467	485877.718720	47.682996
3503.972927	485879.542444	47.688001
3504.192717	485866.285171	47.693005
3503.751694	485834.438367	47.698010
3504.342852	485815.397654	47.703015
3504.540585	485799.610760	47.708020
3504.070662	485795.784112	47.713025
3504.023754	485813.877588	47.718029
3504.019769	485859.017307	47.723034
3503.787601	485855.710368	47.728039
3503.911671	485856.298692	47.733044
3503.726621	485830.794725	47.738049
3503.653848	485807.350090	47.743053
3504.099482	485795.627572	47.748058
3504.069847	485799.533173	47.753063
3504.247911	485821.745308	47.758068
3504.005241	485797.770239	47.763073
3504.066853	485772.531179	47.768077
3503.847691	485799.973573	47.773082
3504.134682	485770.038053	47.778087
3503.941694	485798.185572	47.783092
3504.003189	485766.816510	47.788097
3504.118308	485808.087263	47.793101
3503.989280	485786.627281	47.798106
3503.980862	485746.403507	47.803111
3504.445319	485720.036821	47.808116
3503.640751	485776.094152	47.813121
3503.642667	485756.791879	47.818125
3504.009840	485731.504472	47.823130
3504.139125	485731.129409	47.828135
3504.068165	485776.837182	47.833140
3503.707845	485773.449159	47.838145
3504.220021	485723.973360	47.843149
3503.770034	485737.875050	47.848154
3503.857192	485742.674108	47.853159
3503.970347	485703.038967	47.858164
3503.999674	485676.892976	47.863169
3503.842724	485728.643181	47.868173
3503.919745	485726.097936	47.873178
3504.180403	485686.236802	47.878183
3504.282815	485734.146384	47.883188
3503.778859	485723.232499	47.888193
3504.017401	485696.698840	47.893197
3503.718394	485748.623427	47.898202
3503.551349	485727.372033	47.903207
3504.624600	485693.715167	47.908212
3504.183292	485681.220850	47.913217
3504.303853	485661.899730	47.918221
3503.844037	485702.045698	47.923226
3503.886478	485709.638215	47.928231
3503.947579	485707.247468	47.933236
3503.582881	485690.941437	47.938241
3504.210712	485669.311045	47.943245
3504.069887	485663.203247	47.948250
3504.219527	485666.675248	47.953255
3504.383571	485676.072377	47.958260
3504.093339	485666.137914	47.963265
3503.668946	485643.153943	47.968269
3503.551787	485654.166038	47.973274
3503.833121	485659.289060	47.978279
3503.837685	485676.969237	47.983284
3503.834456	485682.491858	47.988289
3504.146149	485668.105369	47.993293
3504.059334	485659.000000	47.998298
3504.019282	485672.380993	48.003303
3504.173625	485679.449221	48.008308
3503.953927	485658.510042	48.013313
3503.966493	485611.088717	48.018317
3504.131116	485584.921219	48.023322
3504.048938	485603.476423	48.028327
3504.093266	485634.069101	48.033332
3503.719745	485622.931898	48.038337
3503.758191	485605.042227	48.043341
3503.799824	485603.769103	48.048346
3504.367312	485587.163670	48.053351
3504.161114	485598.747148	48.058356
3503.916814	485629.588097	48.063361
3503.892659	485639.065650	48.068365
3503.665463	485626.334811	48.073370
3503.575766	485598.890321	48.078375
3503.480563	485594.295145	48.083380
3503.677825	485604.446986	48.088385
3504.165462	485602.242123	48.093389
3504.064381	485591.416476	48.098394
3503.908548	485574.621379	48.103399
3503.523813	485578.583147	48.108404
3503.246723	485586.580846	48.113409
3503.802835	485601.083552	48.118413
3503.829465	485642.723277	48.123418
3503.925980	485635.868697	48.128423
3504.045350	485595.016471	48.133428
3503.815698	485591.050484	48.138433
3503.835513	485609.589563	48.143437
3503.793978	485605.036569	48.148442
3503.867767	485596.665713	48.153447
3504.173347	485552.440289	48.158452
3503.772191	485575.605504	48.163457
3504.090645	485604.584387	48.168461
3504.097957	485609.902716	48.173466
3504.140887	485565.668171	48.178471
3504.071924	485556.002651	48.183476
3503.869954	485605.328531	48.188481
3504.304020	485560.677524	48.193485
3503.958462	485566.456930	48.198490
3503.943746	485552.172604	48.203495
3504.207179	485520.720563	48.208500
3503.497694	485558.221204	48.213505
3504.163309	485578.988693	48.218509
3503.905932	485574.773776	48.223514
3504.042534	485534.931935	48.228519
3503.704545	485562.038815	48.233524
3503.723840	485581.996535	48.238529
3503.912021	485539.056179	48.243533
3504.145748	485525.492497	48.248538
3504.261818	485516.760291	48.253543
3503.911898	485515.903679	48.258548
3503.112044	485516.891346	48.263553
3503.551922	485520.824122	48.268557
3503.650411	485565.847010	48.273562
3503.835415	485558.623784	48.278567
3503.995931	485567.058948	48.283572
3503.766961	485538.724471	48.288577
3503.614310	485521.523529	48.293581
3503.896908	485539.869158	48.298586
3504.049550	485492.121430	48.303591
3503.691207	485521.055418	48.308596
3503.804703	485552.802519	48.313601
3504.044946	485506.662164	48.318605
3503.712942	485537.314473	48.323610
3503.887186	485518.643330	48.328615
3503.819331	485524.328197	48.333620
3503.844642	485554.721359	48.338625
3504.087777	485510.505707	48.343629
3503.671808	485525.212765	48.348634
3503.783019	485533.301103	48.353639
3503.748958	485554.635157	48.358644
3503.963740	485508.600154	48.363649
3503.496685	485535.119525	48.368653
3503.765431	485546.070691	48.373658
3503.707287	485501.092042	48.378663
3503.232280	485518.848158	48.383668
3503.662759	485556.573932	48.388673
3503.606308	485519.751622	48.393677
3503.509393	485551.177347	48.398682
3503.735073	485526.469315	48.403687
3503.908006	485524.922124	48.408692
3503.775431	485559.291866	48.413697
3504.139026	485557.714545	48.418701
3503.846259	485574.327246	48.423706
3503.791935	485557.617415	48.428711
3504.253597	485548.729280	48.433716
3503.939186	485569.752992	48.438721
3503.800704	485540.542964	48.443725
3503.904516	485551.013575	48.448730
3504.085658	485574.238747	48.453735
3504.060740	485564.059652	48.458740
3503.718534	485567.913376	48.463745
3503.830734	485573.873742	48.468749
3503.888135	485548.077772	48.473754
3504.166599	485500.158193	48.478759
3503.880690	485505.117597	48.483764
3503.500829	485511.155751	48.488769
3504.094435	485528.135024	48.493773
3504.091577	485513.544824	48.498778
3504.032112	485495.163905	48.503783
3503.839726	485522.399814	48.508788
3503.821724	485535.169475	48.513793
3504.200925	485477.152187	48.518797
3503.568778	485517.933719	48.523802
3503.858237	485535.974295	48.528807
3503.919677	485488.291634	48.533812
3503.523100	485524.071038	48.538817
3503.742917	485518.970099	48.543821
3503.370862	485508.136569	48.548826
3503.570436	485519.200006	48.553831
3504.061936	485541.413590	48.558836
3503.784898	485554.376163	48.563841
3503.904712	485539.969242	48.568845
3504.019376	485545.979889	48.573850
3503.936764	485516.001066	48.578855
3504.314647	485495.929843	48.583860
3504.406565	485477.119685	48.588865
3504.501497	485470.771917	48.593869
3504.442945	485459.838151	48.598874
3504.180704	485462.362042	48.603879
3504.173051	485465.757614	48.608884
3504.103075	485430.507798	48.613889
3504.408079	485420.580457	48.618893
3504.006213	485472.572706	48.623898
3504.001781	485485.593565	48.628903
3504.143537	485473.260272	48.633908
3503.880462	485451.821103	48.638913
3504.278398	485430.378764	48.643917
3503.211569	485417.729824	48.648922
3503.951003	485400.438447	48.653927
3504.647851	485380.823316	48.658932
3504.172729	485391.182862	48.663937
3504.460655	485385.057877	48.668941
3504.403390	485427.673911	48.673946
3503.922136	485408.852949	48.678951
3503.755238	485376.658089	48.683956
3503.241874	485366.758735	48.688961
3503.687300	485381.836387	48.693965
3503.596319	485392.287207	48.698970
3504.104820	485396.310489	48.703975
3504.235360	485375.112998	48.708980
3503.702994	485353.007006	48.713985
3503.917592	485362.750936	48.718989
3504.088879	485347.930437	48.723994
3503.705853	485348.041635	48.728999
3504.366164	485347.835951	48.734004
3504.099451	485347.675454	48.739009
3503.881319	485345.176806	48.744013
3504.016141	485390.650323	48.749018
3503.810035	485398.940855	48.754023
3504.295219	485398.560200	48.759028
3503.666693	485356.913749	48.764033
3504.177732	485327.448756	48.769037
3504.171492	485319.242417	48.774042
3503.523239	485368.031487	48.779047
3503.509711	485345.640836	48.784052
3503.646691	485319.730659	48.789057
3504.051466	485349.101585	48.794061
3503.491673	485340.172141	48.799066
3503.848873	485314.227152	48.804071
3504.086665	485312.163069	48.809076
3503.512745	485318.333278	48.814081
3503.785789	485303.851301	48.819085
3504.436675	485309.726612	48.824090
3504.080245	485302.335549	48.829095
3504.371532	485303.100113	48.834100
3503.953071	485327.889561	48.839105
3504.058268	485349.505808	48.844109
3503.791677	485341.593937	48.849114
3503.682292	485347.133432	48.854119
3503.839727	485337.533346	48.859124
3503.464032	485354.919279	48.864129
3503.842856	485343.511021	48.869133
3503.694887	485350.120525	48.874138
3503.749258	485354.772875	48.879143
3503.860341	485354.856644	48.884148
3503.652332	485328.190403	48.889153
3504.270456	485299.823020	48.894157
3503.605376	485314.822922	48.899162
3503.618886	485330.931463	48.904167
3503.796471	485326.749072	48.909172
3504.040729	485347.684731	48.914177
3504.114517	485351.928713	48.919181
3504.042306	485342.770224	48.924186
3503.776706	485331.463807	48.929191
3503.651624	485329.254427	48.934196
3503.741373	485336.434314	48.939201
3504.106036	485321.887209	48.944205
3503.810666	485334.244876	48.949210
3503.357371	485340.548001	48.954215
3503.604438	485331.997658	48.959220
3504.043709	485326.760659	48.964225
3504.067798	485328.732689	48.969229
3503.835391	485333.987656	48.974234
3503.752592	485335.824591	48.979239
3503.682993	485339.736600	48.984244
3503.974190	485367.757562	48.989249
3504.131294	485357.397602	48.994253
3504.253157	485312.136751	48.999258
3503.991427	485286.137556	49.004263
3504.167047	485318.989801	49.009268
3503.747051	485326.554231	49.014273
3503.770603	485305.373573	49.019277
3504.042404	485313.588610	49.024282
3503.987533	485326.718873	49.029287
3504.039770	485326.406642	49.034292
3503.780021	485331.463281	49.039297
3504.102580	485320.165227	49.044301
3504.074132	485315.964734	49.049306
3503.669651	485306.960066	49.054311
3503.902596	485287.012858	49.059316
3503.983733	485240.390386	49.064321
3504.208589	485231.438207	49.069325
3504.574547	485237.003933	49.074330
3504.372194	485224.471552	49.079335
3504.377281	485221.177668	49.084340
3503.271499	485228.445219	49.089345
3503.553397	485233.973568	49.094349
3503.355052	485254.472652	49.099354
3504.121896	485255.567360	49.104359
3504.399637	485234.599764	49.109364
3504.360252	485235.619243	49.114369
3504.013855	485243.932014	49.119373
3504.076647	485256.638427	49.124378
3503.990233	485246.924847	49.129383
3504.227948	485212.183292	49.134388
3504.057792	485251.777789	49.139393
3503.955460	485216.988660	49.144397
3503.864074	485180.120560	49.149402
3503.880961	485203.726780	49.154407
3504.003497	485174.474944	49.159412
3504.453280	485204.396269	49.164417
3504.125829	485201.661566	49.169421
3504.021605	485195.598498	49.174426
3504.347829	485171.178098	49.179431
3504.040063	485185.918976	49.184436
3503.704934	485153.193039	49.189441
3504.569433	485114.805842	49.194445
3504.423600	485106.824126	49.199450
3504.138020	485119.484361	49.204455
3503.888407	485126.211332	49.209460
3503.766342	485171.776628	49.214465
3503.477528	485179.877673	49.219469
3503.718841	485168.693697	49.224474
3503.542298	485150.482942	49.229479
3503.704763	485146.505554	49.234484
3503.805244	485156.976905	49.239489
3503.783947	485150.140773	49.244493
3503.972012	485168.552358	49.249498
3503.693448	485191.394681	49.254503
3504.097281	485181.198284	49.259508
3503.971978	485192.566569	49.264513
3503.970604	485170.680423	49.269517
3503.793607	485148.112727	49.274522
3504.080349	485105.307818	49.279527
3504.140937	485083.513106	49.284532
3503.864637	485106.709813	49.289537
3504.042402	485091.533453	49.294541
3503.588040	485116.480836	49.299546
3503.622260	485128.330577	49.304551
3503.995439	485135.567071	49.309556
3503.801965	485152.468419	49.314561
3503.928719	485121.239981	49.319565
3503.697433	485118.490068	49.324570
3503.728452	485113.114882	49.329575
3503.471729	485114.219380	49.334580
3503.532650	485122.822469	49.339585
3503.521716	485114.160816	49.344589
3503.435081	485112.350638	49.349594
3503.959658	485107.150761	49.354599
3504.320977	485097.670323	49.359604
3504.115773	485117.208037	49.364609
3503.990938	485127.867003	49.369613
3503.802121	485104.287864	49.374618
3504.163302	485127.181143	49.379623
3504.148560	485128.703363	49.384628
3503.812019	485131.543017	49.389633
3503.771105	485076.225398	49.394637
3504.000068	485050.958944	49.399642
3503.993900	485077.963396	49.404647
3504.313055	485105.878994	49.409652
3503.523124	485088.677059	49.414657
3503.408102	485079.423884	49.419661
3504.106475	485061.277420	49.424666
3504.005777	485050.502072	49.429671
3504.352920	485061.238471	49.434676
3503.682266	485117.479201	49.439681
3503.909510	485118.152569	49.444685
3503.979226	485107.755624	49.449690
3503.904617	485080.156021	49.454695
3504.088005	485097.453825	49.459700
3503.899770	485086.236364	49.464705
3504.023948	485053.235013	49.469709
3504.299464	485036.269948	49.474714
3503.955847	485081.363840	49.479719
3504.227936	485063.284750	49.484724
3504.222065	485041.905801	49.489729
3503.946313	485071.840673	49.494733
3504.309397	485062.207948	49.499738
3503.656087	485035.409028	49.504743
3503.739295	485010.874843	49.509748
3504.151291	484987.048614	49.514753
3504.095335	485001.192538	49.519757
3503.904967	485045.553006	49.524762
3503.863049	485035.274992	49.529767
3503.673977	485007.034753	49.534772
3503.921806	484994.177756	49.539777
3503.873017	484993.678833	49.544781
3504.004101	485029.679739	49.549786
3503.936721	485050.411657	49.554791
3504.077618	485035.595722	49.559796
3504.043849	485035.043763	49.564801
3503.815643	485008.076292	49.569805
3503.545194	484998.442336	49.574810
3503.840087	484989.326986	49.579815
3504.062947	485016.194001	49.584820
3503.832270	485009.998871	49.589825
3503.585719	484974.877455	49.594829
3503.785124	484980.520242	49.599834
3503.545575	485009.841528	49.604839
3503.305305	484986.017059	49.609844
3503.588770	485003.045814	49.614849
3503.937788	485040.582819	49.619853
3503.654163	485050.912281	49.624858
3503.485976	485033.916013	49.629863
3504.074705	485019.181277	49.634868
3503.962133	485015.044677	49.639873
3503.637677	485056.335850	49.644877
3503.621793	485067.788242	49.649882
3503.773643	485054.034517	49.654887
3504.057485	485055.357563	49.659892
3503.667488	485041.436150	49.664897
3503.969416	485041.844401	49.669901
3503.781468	485016.947772	49.674906
3503.384232	485025.977958	49.679911
3503.696674	485023.699393	49.684916
3503.555241	485039.326033	49.689921
3503.406959	485044.517119	49.694925
3504.097749	485022.724065	49.699930
3504.022666	485040.620066	49.704935
3503.856155	485056.402646	49.709940
3503.717308	485015.134032	49.714945
3504.129256	484996.424817	49.719949
3504.296283	484998.779597	49.724954
3503.934628	484972.187810	49.729959
3504.421998	484976.062531	49.734964
3503.750621	484991.772965	49.739969
3503.579462	485014.598521	49.744973
3503.531236	485003.156230	49.749978
3503.848411	484974.785271	49.754983
3504.098267	484982.193303	49.759988
3503.668790	485028.719463	49.764993
3503.521796	485007.362779	49.769997
3503.556130	484995.704782	49.775002
3504.072966	484977.637595	49.780007
3504.142358	484969.621807	49.785012
3504.217400	484978.273392	49.790017
3504.126879	484966.584447	49.795021
3504.380065	484955.702452	49.800026
3503.484778	484969.472417	49.805031
3504.023669	484948.260584	49.810036
3503.760572	484941.361265	49.815041
3503.959593	484972.183863	49.820045
3504.146759	484978.081902	49.825050
3503.587828	484964.693766	49.830055
3504.368164	484945.976943	49.835060
3503.896016	484971.383296	49.840065
3503.851015	484992.263729	49.845069
3503.931254	485006.284797	49.850074
3503.866095	484982.027341	49.855079
3504.078798	484929.050397	49.860084
3503.367115	484973.037452	49.865089
3503.808015	484993.081139	49.870093
3503.966184	484976.691864	49.875098
3503.611510	484936.369135	49.880103
3504.111543	484906.550597	49.885108
3504.111504	484902.193533	49.890113
3504.020448	484909.604809	49.895117
3504.332517	484946.995846	49.900122
3504.050139	484969.940359	49.905127
3503.983901	484962.452638	49.910132
3503.825898	484960.299081	49.915137
3503.391497	484950.589687	49.920141
3504.211310	484920.619303	49.925146
3503.735084	484939.592068	49.930151
3503.652804	484965.240793	49.935156
3503.608235	484955.824433	49.940161
3503.551987	484942.660816	49.945165
3504.250721	484920.815728	49.950170
3503.811904	484917.794604	49.955175
3504.203272	484898.733902	49.960180
3503.892768	484885.458439	49.965185
3503.939747	484871.670495	49.970189
3504.033217	484863.752185	49.975194
3503.648602	484885.193046	49.980199
3503.844618	484924.983659	49.985204
3503.812092	484914.349450	49.990209
3504.017832	484892.734237	49.995213
3503.943936	484909.464909	50.000218
3503.594811	484916.866306	50.005223
3503.871515	484897.469079	50.010228
3503.424187	484907.976481	50.015233
3503.080649	484912.590499	50.020237
3504.256958	484882.969023	50.025242
3503.910775	484922.490687	50.030247
3504.044452	484917.352540	50.035252
3504.256864	484891.936504	50.040257
3503.790567	484897.127227	50.045261
3504.023031	484906.919227	50.050266
3503.731807	484943.898981	50.055271
3503.981400	484906.925806	50.060276
3504.440954	484882.939942	50.065281
3504.143582	484847.876992	50.070285
3504.246136	484855.207026	50.075290
3504.076521	484854.879187	50.080295
3504.183369	484863.272478	50.085300
3504.150583	484892.763918	50.090305
3504.262761	484882.360141	50.095309
3504.021444	484851.290766	50.100314
3503.078306	484839.179195	50.105319
3504.187970	484810.885400	50.110324
3503.798277	484807.856495	50.115329
3503.674951	484851.548182	50.120333
3504.073318	484854.677037	50.125338
3503.873557	484826.235568	50.130343
3504.153802	484833.638855	50.135348
3504.031124	484865.627069	50.140353
3503.900448	484832.158983	50.145357
3504.137438	484831.310907	50.150362
3503.783296	484864.602299	50.155367
3504.176990	484859.676361	50.160372
3504.026251	484849.668765	50.165377
3503.947802	484832.303490	50.170381
3503.863608	484808.504798	50.175386
3503.944413	484792.026267	50.180391
3503.955935	484792.227101	50.185396
3503.854600	484844.224207	50.190401
3503.662017	484833.919234	50.195405
3503.790605	484844.690295	50.200410
3503.608059	484841.881975	50.205415
3503.651758	484827.385225	50.210420
3503.584075	484818.935064	50.215425
3503.292633	484825.972732	50.220429
3503.513262	484815.855762	50.225434
3503.359506	484825.556852	50.230439
3503.848260	484827.962133	50.235444
3504.083312	484823.111922	50.240449
3504.050911	484803.459472	50.245453
3504.210970	484851.058153	50.250458
3503.792699	484855.380013	50.255463
3503.860019	484856.179993	50.260468
3503.941623	484839.752040	50.265473
3503.845174	484846.505564	50.270477
3503.849109	484844.326401	50.275482
3503.770359	484845.706768	50.280487
3504.002802	484844.808747	50.285492
3503.887601	484797.354952	50.290497
3503.517203	484795.994903	50.295501
3503.972414	484806.967683	50.300506
3504.023752	484812.431265	50.305511
3504.445164	484791.997786	50.310516
3504.145772	484770.715590	50.315521
3503.802358	484766.311437	50.320525
3503.948522	484773.786602	50.325530
3503.995615	484773.069863	50.330535
3503.653774	484777.632981	50.335540
3503.736883	484789.829851	50.340545
3503.844549	484784.999763	50.345549
3503.881190	484769.845454	50.350554
3503.925338	484804.492593	50.355559
3503.848143	484815.498849	50.360564
3504.238302	484793.854379	50.365569
3503.980733	484769.120426	50.370573
3503.969823	484788.171790	50.375578
3503.868547	484818.636782	50.380583
3503.792504	484791.948943	50.385588
3503.954441	484791.923349	50.390593
3503.554975	484782.259012	50.395597
3503.999948	484780.364784	50.400602
3503.734457	484772.047194	50.405607
3503.663205	484759.544455	50.410612
3503.619651	484750.482482	50.415617
3504.169711	484724.962199	50.420621
3503.902368	484711.882451	50.425626
3503.592874	484738.074028	50.430631
3503.607853	484777.184261	50.435636
3503.651255	484780.166573	50.440641
3503.500527	484784.648820	50.445645
3503.767951	484749.040451	50.450650
3503.623728	484737.359855	50.455655
3504.122024	484776.393702	50.460660
3503.887284	484788.336824	50.465665
3503.876203	484784.944093	50.470669
3504.052233	484776.810044	50.475674
3504.217124	484786.815441	50.480679
3504.189236	484772.937931	50.485684
3504.044662	484768.097041	50.490689
3503.519357	484764.937569	50.495693
3503.630257	484758.992356	50.500698
3503.193191	484767.826300	50.505703
3503.412105	484751.477898	50.510708
3504.193844	484748.922475	50.515713
3504.095794	484780.805609	50.520717
3504.093236	484765.758820	50.525722
3503.742067	484771.843332	50.530727
3503.570097	484737.874969	50.535732
3504.204868	484710.770693	50.540737
3504.383525	484661.446213	50.545741
3504.265673	484590.889422	50.550746
3503.993439	484558.101871	50.555751
3503.972962	484519.752034	50.560756
3503.610626	484444.369545	50.565761
3503.279136	484336.758915	50.570765
3503.383245	484232.625419	50.575770
3503.576503	484129.642583	50.580775
3503.454329	484008.874648	50.585780
3503.158482	483893.301368	50.590785
3502.591432	483765.458286	50.595789
3502.956042	483606.560274	50.600794
3502.303071	483467.632736	50.605799
3501.811071	483365.463495	50.610804
3501.718091	483215.602778	50.615809
3501.434327	483033.799270	50.620813
3501.269046	482855.370162	50.625818
3500.753005	482683.683220	50.630823
3500.208844	482482.712022	50.635828
3499.896320	482287.731928	50.640833
3499.720770	482069.368932	50.645837
3499.740312	481890.293753	50.650842
3498.965788	481697.813034	50.655847
3498.911476	481446.487146	50.660852
3498.528081	481286.371011	50.665857
3497.761418	481034.696387	50.670861
3498.370943	480785.334755	50.675866
3497.527698	480572.128079	50.680871
3497.525224	480295.239170	50.685876
3497.206482	480088.886929	50.690881
3496.625570	479794.801882	50.695885
3496.263701	479557.943443	50.700890
3495.579040	479262.143858	50.705895
3495.243352	479008.956344	50.710900
3494.591816	478720.998688	50.715905
3494.061393	478463.324529	50.720909
3493.894748	478155.820852	50.725914
3493.110624	477907.961053	50.730919
3492.965543	477608.149151	50.735924
3492.768456	477279.299513	50.740929
3491.911667	477022.367939	50.745933
3491.379942	476711.199868	50.750938
3490.989032	476377.753806	50.755943
3490.269418	476117.950612	50.760948
3490.066221	475792.068122	50.765953
3489.225842	475469.322355	50.770957
3488.963199	475133.250404	50.775962
3487.883483	474864.161316	50.780967
3487.658043	474524.068946	50.785972
3487.460958	474180.113896	50.790977
3486.588856	473846.195335	50.795981
3486.038022	473559.618110	50.800986
3485.461538	473205.973648	50.805991
3484.900780	472862.560840	50.810996
3484.195999	472550.089042	50.816001
3483.875748	472185.943326	50.821005
3483.190179	471888.515130	50.826010
3482.194258	471530.396134	50.831015
3482.406010	471141.458184	50.836020
3481.706707	470825.765400	50.841025
3480.755737	470501.082980	50.846029
3480.077771	470108.311684	50.851034
3479.378047	469797.065026	50.856039
3478.739700	469435.709864	50.861044
3478.363302	469063.355086	50.866049
3477.490074	468750.193522	50.871053
3477.091957	468385.537185	50.876058
3476.327338	468014.391366	50.881063
3475.964019	467633.591954	50.886068
3475.143682	467315.989164	50.891073
3474.027326	466967.090497	50.896077
3474.011598	466584.239602	50.901082
3473.136910	466255.067714	50.906087
3472.140831	465872.764629	50.911092
3471.940232	465520.350500	50.916097
3470.961009	465179.362592	50.921101
3470.774682	464782.002385	50.926106
3469.585547	464478.513951	50.931111
3468.919698	464095.264727	50.936116
3468.386399	463720.508061	50.941121
3468.197073	463331.489690	50.946125
3467.369707	463005.100532	50.951130
3466.569857	462654.052769	50.956135
3466.206535	462282.794618	50.961140
3465.268617	461902.643405	50.966145
3464.118631	461517.244038	50.971149
3463.988321	461133.401242	50.976154
3463.115818	460816.826491	50.981159
3462.335282	460440.987121	50.986164
3461.965110	460044.837233	50.991169
3460.947038	459706.762113	50.996173
3460.385972	459364.703629	51.001178
3459.852036	458968.306631	51.006183
3458.959610	458636.586898	51.011188
3458.423713	458231.198134	51.016193
3457.427244	457903.948042	51.021197
3457.101520	457555.229549	51.026202
3456.353048	457188.258394	51.031207
3455.745552	456790.515164	51.036212
3455.387777	456453.808099	51.041217
3454.145605	456067.059958	51.046221
3453.706051	455718.736720	51.051226
3453.113420	455342.629212	51.056231
3451.925056	454992.282220	51.061236
3451.692094	454614.634385	51.066241
3450.644002	454266.740113	51.071245
3449.976723	453871.390256	51.076250
3448.879976	453551.855743	51.081255
3448.707905	453179.045435	51.086260
3448.020663	452817.118362	51.091265
3446.932136	452481.381123	51.096269
3446.296104	452100.507880	51.101274
3445.664587	451773.314322	51.106279
3444.485632	451407.586252	51.111284
3444.185036	451025.931799	51.116289
3443.468726	450692.342432	51.121293
3443.373889	450368.951586	51.126298
3442.319645	450004.044321	51.131303
3441.914223	449619.236967	51.136308
3441.037463	449281.694362	51.141313
3440.258729	448962.046023	51.146317
3439.853669	448579.860482	51.151322
3438.867884	448202.683394	51.156327
3438.143767	447843.171375	51.161332
3437.565394	447514.336289	51.166337
3436.823772	447146.695977	51.171341
3436.050793	446809.558263	51.176346
3434.852110	446454.363503	51.181351
3435.011398	446081.285735	51.186356
3433.957720	445763.566282	51.191361
3432.877004	445436.406030	51.196365
3432.623686	445089.720972	51.201370
3431.886799	444742.701273	51.206375
3431.314313	444381.691723	51.211380
3430.211398	444003.755931	51.216385
3429.683163	443650.088657	51.221389
3429.385944	443348.511937	51.226394
3428.572687	442990.565340	51.231399
3427.638810	442648.369095	51.236404
3426.781980	442282.093797	51.241409
3426.355371	441928.893016	51.246413
3425.670640	441613.852660	51.251418
3425.206780	441262.272626	51.256423
3424.167754	440897.934498	51.261428
3423.667783	440557.594908	51.266433
3422.406676	440240.495810	51.271437
3422.177154	439855.300902	51.276442
3421.286538	439555.421235	51.281447
3420.831145	439192.311053	51.286452
3419.931582	438844.877848	51.291457
3419.231840	438539.421706	51.296461
3418.983360	438162.174675	51.301466
3417.799625	437847.672948	51.306471
3417.354631	437471.360484	51.311476
3416.551955	437173.799256	51.316481
3415.690477	436817.877956	51.321485
3415.215344	436475.904661	51.326490
3414.442852	436166.039035	51.331495
3413.630674	435798.467791	51.336500
3413.138284	435511.018728	51.341505
3412.312033	435132.649816	51.346509
3411.780767	434818.413446	51.351514
3410.910661	434468.071626	51.356519
3410.308945	434140.229082	51.361524
3409.650881	433816.479128	51.366529
3409.155791	433465.099478	51.371533
3408.638150	433154.826934	51.376538
3407.211649	432813.869076	51.381543
3407.061701	432447.465409	51.386548
3406.256585	432154.365812	51.391553
3405.218962	431815.313922	51.396557
3405.183875	431466.449853	51.401562
3404.333131	431173.194063	51.406567
3403.316330	430804.517367	51.411572
3403.441318	430442.485909	51.416577
3402.138584	430127.095666	51.421581
3401.333995	429837.042691	51.426586
3400.242465	429493.423673	51.431591
3399.776178	429147.009463	51.436596
3399.232139	428840.905471	51.441601
3398.435747	428538.469423	51.446605
3397.938027	428177.318052	51.451610
3396.906842	427879.686085	51.456615
3396.436425	427554.051320	51.461620
3395.674974	427220.763349	51.466625
3395.119980	426884.670301	51.471629
3394.796650	426551.050783	51.476634
3393.614794	426272.574533	51.481639
3393.143499	425923.097021	51.486644
3392.475530	425606.359267	51.491649
3391.332186	425291.623272	51.496653
3390.914110	424968.641286	51.501658
3389.658674	424685.156760	51.506663
3389.472627	424360.937127	51.511668
3388.994491	424036.353434	51.516673
3387.657362	423707.202672	51.521677
3387.505304	423365.515967	51.526682
3387.015210	423089.310878	51.531687
3386.449811	422769.069555	51.536692
3385.792134	422441.853744	51.541697
3384.671283	422110.795445	51.546701
3384.609832	421773.596248	51.551706
3383.320718	421479.516855	51.556711
3382.697200	421140.900138	51.561716
3381.919155	420860.018941	51.566721
3380.960788	420529.170211	51.571725
3380.742564	420192.637221	51.576730
3379.773778	419916.654197	51.581735
3379.444115	419583.916700	51.586740
3378.573236	419263.556505	51.591745
3377.764219	418950.905877	51.596749
3377.438908	418631.747920	51.601754
3376.498783	418350.816581	51.606759
3375.861787	418008.125033	51.611764
3375.601513	417719.585418	51.616769
3374.296374	417391.371688	51.621773
3374.184287	417063.524511	51.626778
3373.242276	416776.048639	51.631783
3372.026124	416451.011323	51.636788
3372.149340	416109.980833	51.641793
3371.436623	415830.411700	51.646797
3370.518976	415516.140192	51.651802
3369.379225	415188.154777	51.656807
3368.674012	414903.544805	51.661812
3368.030340	414580.504929	51.666817
3367.453035	414291.092008	51.671821
3367.086614	413973.820185	51.676826
3366.520215	413677.971058	51.681831
3365.904627	413369.726959	51.686836
3365.121212	413044.278426	51.691841
3364.005087	412764.997957	51.696845
3363.583721	412418.877871	51.701850
3362.803611	412140.732690	51.706855
3362.089888	411823.111599	51.711860
3361.558484	411517.121949	51.716865
3360.526966	411206.710460	51.721869
3360.218848	410894.377168	51.726874
3359.182700	410618.087968	51.731879
3358.896851	410277.690195	51.736884
3357.859865	409967.419282	51.741889
3356.981448	409709.800279	51.746893
3356.568896	409421.559332	51.751898
3355.853264	409115.091640	51.756903
3355.047610	408795.750584	51.761908
3354.380366	408504.796618	51.766913
3353.817382	408219.643153	51.771917
3353.540731	407894.948427	51.776922
3352.311458	407619.755386	51.781927
3352.048555	407291.875358	51.786932
3351.287071	407026.590967	51.791937
3350.333271	406706.921286	51.796941
3350.299232	406379.961202	51.801946
3349.391956	406132.787888	51.806951
3348.306356	405822.635349	51.811956
3348.118935	405490.632485	51.816961
3347.152952	405237.336132	51.821965
3346.556706	404906.916713	51.826970
3345.784605	404621.255014	51.831975
3345.506664	404322.499139	51.836980
3344.602915	404015.883829	51.841985
3343.369681	403712.215239	51.846989
3343.027099	403433.947643	51.851994
3342.229677	403131.272144	51.856999
3341.792637	402824.825752	51.862004
3340.923257	402520.351168	51.867009
3340.192051	402252.149575	51.872013
3339.866690	401930.807134	51.877018
3338.598291	401655.314061	51.882023
3338.262881	401347.947876	51.887028
3337.548801	401075.870081	51.892033
3337.088759	400748.894085	51.897037
3336.193300	400488.406038	51.902042
3335.649945	400170.537757	51.907047
3334.709611	399909.416687	51.912052
3334.344571	399584.625601	51.917057
3333.614222	399337.244765	51.922061
3332.944692	398997.091001	51.927066
3331.954357	398741.866271	51.932071
3331.365764	398429.606443	51.937076
3330.867805	398131.794331	51.942081
3330.362280	397868.122463	51.947085
3329.718407	397547.067097	51.952090
3329.120269	397266.295976	51.957095
3328.350948	396986.083447	51.962100
3327.595288	396666.918604	51.967105
3326.767135	396412.260575	51.972109
3326.222442	396076.989410	51.977114
3325.454628	395813.419168	51.982119
3324.734075	395516.661446	51.987124
3324.029559	395227.729178	51.992129
3323.198593	394938.967002	51.997133
3322.570730	394669.925009	52.002138
3322.574315	394370.424107	52.007143
3321.530319	394075.128795	52.012148
3320.730843	393793.470944	52.017153
3319.941017	393500.978122	52.022157
3319.314031	393210.491114	52.027162
3318.819973	392932.693479	52.032167
3317.988155	392637.733732	52.037172
3317.468561	392337.560624	52.042177
3316.615582	392060.829842	52.047181
3316.076376	391780.309564	52.052186
3315.506470	391489.010984	52.057191
3314.572194	391186.884897	52.062196
3313.771518	390930.427618	52.067201
3313.225142	390619.869830	52.072205
3312.662465	390343.461071	52.077210
3311.894972	390068.862494	52.082215
3311.253541	389784.604688	52.087220
3310.783010	389484.450449	52.092225
3309.967878	389198.944054	52.097229
3309.215655	388924.537708	52.102234
3308.881722	388647.876256	52.107239
3308.082170	388354.528658	52.112244
3307.303047	388054.792740	52.117249
3306.488907	387778.531162	52.122253
3305.659551	387488.817673	52.127258
3305.030526	387202.198061	52.132263
3304.739143	386930.348455	52.137268
3304.585878	386638.741224	52.142273
3303.352063	386353.685568	52.147277
3302.447161	386081.519822	52.152282
3301.907212	385782.108938	52.157287
3301.174896	385492.745836	52.162292
3300.394256	385207.355374	52.167297
3299.541044	384925.534584	52.172301
3298.960632	384640.871062	52.177306
3298.182100	384351.684436	52.182311
3297.643326	384107.192320	52.187316
3297.275810	383781.390722	52.192321
3296.472259	383531.392551	52.197325
3296.276078	383240.630238	52.202330
3295.428033	382948.519124	52.207335
3294.210259	382692.833158	52.212340
3293.846748	382396.241308	52.217345
3293.016433	382113.810968	52.222349
3292.429373	381827.321604	52.227354
3291.633931	381559.429558	52.232359
3290.797284	381282.843830	52.237364
3290.463462	380979.064039	52.242369
3289.394168	380735.193780	52.247373
3288.896719	380434.462260	52.252378
3288.012609	380168.761971	52.257383
3287.603903	379873.963760	52.262388
3287.243266	379634.756264	52.267393
3286.269450	379329.996584	52.272397
3285.859883	379054.141433	52.277402
3284.808478	378790.162430	52.282407
3284.248168	378497.845124	52.287412
3283.598279	378198.366957	52.292417
3282.844268	377954.048051	52.297421
3282.021106	377665.327226	52.302426
3281.448062	377406.808460	52.307431
3280.597557	377125.540887	52.312436
3280.057140	376850.963004	52.317441
3279.519153	376579.002856	52.322445
3278.640817	376317.269477	52.327450
3278.210910	376031.374560	52.332455
3277.413348	375761.205142	52.337460
3276.951831	375484.188992	52.342465
3276.130405	375218.089747	52.347469
3275.110158	374929.711285	52.352474
3274.863641	374659.930774	52.357479
3274.298598	374379.285919	52.362484
3273.722882	374131.812378	52.367489
3272.932303	373833.494449	52.372493
3272.355649	373586.195875	52.377498
3271.937628	373269.753570	52.382503
3270.796117	373052.508071	52.387508
3270.298442	372742.841140	52.392513
3269.660071	372468.860081	52.397517
3268.807887	372186.516038	52.402522
3268.133552	371929.276330	52.407527
3267.568911	371653.751956	52.412532
3266.940831	371365.464977	52.417537
3266.086477	371095.884884	52.422541
3265.657426	370831.451085	52.427546
3265.249598	370540.528810	52.432551
3264.234631	370255.017680	52.437556
3263.640228	370003.223485	52.442561
3263.192537	369711.665912	52.447565
3262.362084	369451.866516	52.452570
3261.917234	369173.636011	52.457575
3261.229605	368886.893820	52.462580
3260.799996	368609.496885	52.467585
3260.074308	368327.565516	52.472589
3258.982434	368051.669104	52.477594
3258.593196	367767.874574	52.482599
3257.801707	367488.746890	52.487604
3257.299361	367210.818401	52.492609
3256.294473	366932.815008	52.497613
3255.638864	366646.078688	52.502618
3255.070217	366375.482995	52.507623
3254.346493	366098.193251	52.512628
3254.032184	365824.882514	52.517633
3253.210294	365546.561747	52.522637
3252.635043	365263.340565	52.527642
3252.094880	364986.116771	52.532647
3251.205072	364695.563168	52.537652
3250.615089	364420.837324	52.542657
3249.847710	364138.631893	52.547661
3248.665629	363873.716080	52.552666
3248.014140	363603.473289	52.557671
3247.516814	363321.169277	52.562676
3247.168115	363045.888229	52.567681
3246.239361	362769.730401	52.572685
3245.428308	362504.035667	52.577690
3244.604984	362233.659469	52.582695
3244.124293	361968.342031	52.587700
3243.799771	361688.545408	52.592705
3242.983770	361416.534881	52.597709
3242.326754	361138.365238	52.602714
3241.689161	360860.979728	52.607719
3240.970698	360594.750756	52.612724
3240.556735	360311.423229	52.617729
3239.373475	360044.679474	52.622733
3238.752472	359769.244423	52.627738
3238.001398	359490.164076	52.632743
3236.950258	359233.446371	52.637748
3236.825101	358956.808649	52.642753
3236.186942	358683.482279	52.647757
3235.309250	358427.012839	52.652762
3234.569195	358153.928676	52.657767
3233.775292	357900.776849	52.662772
3233.327911	357615.912178	52.667777
3232.620476	357355.720379	52.672781
3231.910961	357089.878141	52.677786
3231.544245	356812.426902	52.682791
3230.412748	356552.348910	52.687796
3230.324902	356279.609427	52.692801
3229.283902	356025.265713	52.697805
3228.709445	355745.474791	52.702810
3228.094025	355474.901220	52.707815
3227.766891	355210.490119	52.712820
3227.078108	354941.604959	52.717825
3226.332472	354683.365082	52.722829
3225.482853	354409.031050	52.727834
3225.248041	354124.927593	52.732839
3224.312454	353849.993429	52.737844
3223.550549	353575.539338	52.742849
3222.924004	353305.516099	52.747853
3222.137441	353026.914747	52.752858
3221.718188	352768.104792	52.757863
3220.906367	352494.441923	52.762868
3220.476654	352211.224278	52.767873
3219.454650	351952.785653	52.772877
3218.838172	351678.247844	52.777882
3218.344426	351400.838754	52.782887
3217.521765	351132.947937	52.787892
3216.828145	350858.290909	52.792897
3216.106043	350601.630842	52.797901
3215.402111	350323.740477	52.802906
3215.134180	350057.156437	52.807911
3214.119202	349791.300104	52.812916
3213.776405	349514.850158	52.817921
3212.725009	349247.571689	52.822925
3212.032071	348978.224548	52.827930
3211.734012	348706.981112	52.832935
3210.632782	348441.004706	52.837940
3210.185844	348164.462737	52.842945
3209.696449	347906.328078	52.847949
3209.268631	347630.391326	52.852954
3208.422113	347357.242877	52.857959
3207.346234	347093.801380	52.862964
3207.223850	346817.481500	52.867969
3206.231175	346559.471266	52.872973
3205.333775	346282.304206	52.877978
3205.127564	346009.073522	52.882983
3204.303195	345744.567961	52.887988
3203.865902	345474.222078	52.892993
3202.794365	345203.644381	52.897997
3202.191640	344926.678809	52.903002
3201.917269	344657.346997	52.908007
3200.740246	344401.316335	52.913012
3200.571873	344117.329404	52.918017
3199.778923	343848.050509	52.923021
3198.912059	343585.094714	52.928026
3198.258980	343305.202361	52.933031
3197.625454	343042.869104	52.938036
3197.049007	342761.994857	52.943041
3196.195967	342499.515801	52.948045
3195.487555	342224.234504	52.953050
3194.982314	341948.716198	52.958055
3194.362868	341685.840351	52.963060
3194.092497	341411.122509	52.968065
3192.949765	341142.268851	52.973069
3192.185039	340872.463308	52.978074
3191.626029	340607.995137	52.983079
3190.813278	340339.264028	52.988084
3190.342174	340066.786680	52.993089
3189.527803	339792.351470	52.998093
3188.835697	339518.226663	53.003098
3188.623920	339263.574804	53.008103
3187.340800	338991.781359	53.013108
3186.854535	338717.773319	53.018113
3186.312052	338453.471820	53.023117
3185.600447	338176.849707	53.028122
3185.042222	337904.962507	53.033127
3184.587112	337637.232737	53.038132
3183.963397	337361.433356	53.043137
3183.084292	337105.911307	53.048141
3182.091355	336820.978225	53.053146
3181.548750	336553.130649	53.058151
3180.832497	336288.007919	53.063156
3180.158776	336014.425661	53.068161
3179.466172	335752.479231	53.073165
3178.677026	335495.307584	53.078170
3178.059079	335226.550227	53.083175
3177.432949	334960.135205	53.088180
3177.175911	334691.725989	53.093185
3176.442313	334424.002109	53.098189
3175.616087	334146.948843	53.103194
3175.543675	333880.569380	53.108199
3174.548092	333613.596668	53.113204
3173.439430	333345.647972	53.118209
3172.776559	333074.572759	53.123213
3172.293164	332807.032284	53.128218
3171.712090	332545.361689	53.133223
3170.946292	332269.258956	53.138228
3170.631913	331999.091978	53.143233
3169.760752	331731.710697	53.148237
3169.178528	331462.373321	53.153242
3168.691683	331193.172622	53.158247
3167.754289	330921.776372	53.163252
3167.153074	330645.386892	53.168257
3166.522047	330377.071647	53.173261
3165.728376	330099.870445	53.178266
3164.990665	329827.191127	53.183271
3164.048433	329567.578394	53.188276
3163.761344	329290.064949	53.193281
3162.765688	329027.149093	53.198285
3162.037666	328754.286187	53.203290
3161.801586	328490.051726	53.208295
3160.999455	328244.593439	53.213300
3160.357057	327967.156907	53.218305
3159.731546	327700.613608	53.223309
3159.271089	327436.156482	53.228314
3158.555000	327161.605763	53.233319
3157.683480	326889.268269	53.238324
3157.298298	326612.015439	53.243329
3156.416464	326352.178790	53.248333
3155.809034	326093.494539	53.253338
3155.273346	325801.572019	53.258343
3154.470097	325543.426214	53.263348
3153.908082	325275.057123	53.268353
3153.146999	324993.911840	53.273357
3152.469702	324734.852453	53.278362
3151.488834	324466.674321	53.283367
3151.023722	324194.874643	53.288372
3150.200398	323923.181685	53.293377
3149.936607	323653.207086	53.298381
3148.996068	323396.273065	53.303386
3148.375804	323123.781599	53.308391
3147.535359	322859.828250	53.313396
3147.124912	322597.664765	53.318401
3146.440523	322332.437512	53.323405
3145.334454	322055.360080	53.328410
3145.193620	321790.885439	53.333415
3144.116003	321534.222248	53.338420
3143.628708	321266.541744	53.343425
3143.066476	320995.460386	53.348429
3141.996258	320732.020832	53.353434
3141.750422	320461.295215	53.358439
3141.188391	320195.583964	53.363444
3140.228063	319937.319039	53.368449
3139.846245	319678.987330	53.373453
3139.135773	319403.061405	53.378458
3138.346665	319136.262703	53.383463
3137.452521	318873.324722	53.388468
3137.257078	318605.488482	53.393473
3136.642449	318342.810365	53.398477
3135.446527	318077.549901	53.403482
3134.981193	317812.504138	53.408487
3134.399250	317545.591843	53.413492
3133.851458	317280.379441	53.418497
3133.086940	317010.337162	53.423501
3132.216016	316743.723048	53.428506
3131.897941	316469.967435	53.433511
3131.028781	316216.414285	53.438516
3130.583449	315942.473667	53.443521
3129.857384	315682.734407	53.448525
3128.978592	315419.912104	53.453530
3128.613344	315154.155961	53.458535
3127.643570	314893.409267	53.463540
3127.039075	314617.987963	53.468545
3126.233475	314353.063367	53.473549
3125.492189	314097.575017	53.478554
3125.197740	313818.868677	53.483559
3124.287094	313561.623372	53.488564
3123.817033	313294.402244	53.493569
3123.535076	313019.409618	53.498573
3121.969337	312759.617806	53.503578
3121.701700	312488.084713	53.508583
3120.997473	312235.590915	53.513588
3120.597411	311959.774032	53.518593
3119.872141	311703.972011	53.523597
3119.112795	311445.119073	53.528602
3118.683968	311168.897396	53.533607
3117.644054	310908.330594	53.538612
3117.211418	310636.004329	53.543617
3116.479278	310377.450282	53.548621
3115.798288	310113.692771	53.553626
3115.529141	309839.454416	53.558631
3114.863984	309578.748997	53.563636
3113.727218	309306.582036	53.568641
3113.455887	309030.636047	53.573645
3112.579062	308769.453091	53.578650
3112.296542	308498.524292	53.583655
3111.323900	308235.445498	53.588660
3110.683309	307960.192193	53.593665
3110.099046	307693.256511	53.598669
3109.486450	307423.370783	53.603674
3109.166024	307148.294266	53.608679
3108.131780	306872.999063	53.613684
3107.395731	306608.529847	53.618689
3106.683557	306335.550851	53.623693
3105.764684	306061.483522	53.628698
3105.730312	305788.599895	53.633703
3104.594024	305519.633527	53.638708
3103.881979	305247.747348	53.643713
3103.730660	304989.268760	53.648717
3102.751533	304722.313240	53.653722
3102.132999	304442.643638	53.658727
3101.386939	304174.555180	53.663732
3100.584085	303902.018672	53.668737
3099.969377	303632.915258	53.673741
3099.274646	303358.730807	53.678746
3098.719386	303091.959877	53.683751
3097.608808	302833.807491	53.688756
3097.122440	302566.999264	53.693761
3096.509062	302298.428033	53.698765
3095.806959	302041.737650	53.703770
3095.275820	301770.504003	53.708775
3094.882347	301515.062703	53.713780
3094.175182	301236.521690	53.718785
3093.710359	300973.552766	53.723789
3092.711031	300693.987459	53.728794
3092.102544	300421.821519	53.733799
3091.546826	300153.925165	53.738804
3090.587811	299879.929284	53.743809
3089.822250	299621.411529	53.748813
3089.141558	299350.579555	53.753818
3088.953861	299078.777815	53.758823
3088.330657	298821.407813	53.763828
3087.543663	298545.116068	53.768833
3086.721690	298267.785295	53.773837
3086.028617	297996.265614	53.778842
3085.527301	297725.810268	53.783847
3084.586984	297468.819604	53.788852
3084.167702	297195.370882	53.793857
3083.246058	296935.244105	53.798861
3082.525395	296670.373773	53.803866
3081.996655	296396.253634	53.808871
3081.472944	296135.884560	53.813876
3080.880253	295861.264465	53.818881
3080.205246	295589.458416	53.823885
3079.234266	295319.303278	53.828890
3078.843326	295048.826803	53.833895
3078.255337	294789.102887	53.838900
3077.794611	294517.541691	53.843905
3077.083391	294249.738027	53.848909
3076.092329	293970.467073	53.853914
3075.466342	293697.963266	53.858919
3074.730837	293439.330745	53.863924
3074.168494	293167.809470	53.868929
3073.660025	292898.240353	53.873933
3072.861602	292640.075327	53.878938
3072.549975	292351.271947	53.883943
3071.806916	292090.296152	53.888948
3070.677092	291819.015978	53.893953
3070.218308	291540.804006	53.898957
3069.791101	291275.702579	53.903962
3069.276683	290995.079406	53.908967
3068.368290	290727.022926	53.913972
3067.716176	290441.403834	53.918977
3067.370459	290174.123682	53.923981
3066.359607	289902.364335	53.928986
3065.764715	289621.803454	53.933991
3064.781577	289356.457101	53.938996
3064.168097	289093.395060	53.944001
3063.859918	288818.900346	53.949005
3062.876604	288553.222248	53.954010
3062.016654	288287.880959	53.959015
3061.890845	288016.056299	53.964020
3061.012510	287744.656118	53.969025
3059.896308	287467.996027	53.974029
3059.352518	287212.485439	53.979034
3058.822611	286932.803333	53.984039
3058.142552	286667.636083	53.989044
3057.198670	286406.381540	53.994049
3056.545814	286144.622340	53.999053
3056.000524	285865.654993	54.004058
3055.649067	285600.867979	54.009063
3054.684502	285349.624983	54.014068
3054.200097	285078.950080	54.019073
3053.727155	284810.387053	54.024077
3052.651955	284537.691462	54.029082
3052.303836	284274.151065	54.034087
3051.541228	284015.387733	54.039092
3050.716453	283739.621348	54.044097
3050.181551	283471.984240	54.049101
3049.487008	283204.983499	54.054106
3049.058145	282923.703842	54.059111
3048.141467	282674.132808	54.064116
3047.432985	282396.233488	54.069121
3046.937419	282128.080166	54.074125
3045.677379	281870.438771	54.079130
3045.571154	281598.530719	54.084135
3044.996447	281347.275087	54.089140
3044.485273	281069.496809	54.094145
3043.675387	280803.302851	54.099149
3042.674755	280545.314325	54.104154
3042.085300	280269.942188	54.109159
3041.307610	280017.190173	54.114164
3040.525078	279744.140589	54.119169
3040.082942	279483.669366	54.124173
3039.419023	279214.981433	54.129178
3038.605665	278954.110409	54.134183
3038.048339	278691.034004	54.139188
3037.361147	278431.874763	54.144193
3036.754059	278162.540921	54.149197
3035.869668	277915.102793	54.154202
3035.476994	277638.145365	54.159207
3035.269442	277382.857670	54.164212
3034.505356	277113.344794	54.169217
3033.894893	276845.386623	54.174221
3032.817982	276579.998156	54.179226
3032.392567	276308.699778	54.184231
3031.486453	276042.723956	54.189236
3030.865403	275781.414669	54.194241
3030.371282	275512.470245	54.199245
3029.842925	275235.101208	54.204250
3029.510211	274960.935705	54.209255
3028.238492	274708.745235	54.214260
3027.454353	274423.215906	54.219265
3027.042396	274152.297491	54.224269
3026.200119	273887.661495	54.229274
3025.677937	273625.470774	54.234279
3025.088133	273366.499807	54.239284
3023.865705	273097.492591	54.244289
3023.532342	272835.654138	54.249293
3022.768354	272565.504798	54.254298
3022.296801	272300.122753	54.259303
3021.519043	272048.338391	54.264308
3020.751568	271784.123910	54.269313
3020.590969	271513.038874	54.274317
3019.466676	271259.985200	54.279322
3018.890133	270992.913738	54.284327
3018.121257	270720.804606	54.289332
3017.635050	270463.218699	54.294337
3016.844411	270198.346192	54.299341
3016.390666	269938.692397	54.304346
3015.922483	269660.092589	54.309351
3014.981256	269402.324400	54.314356
3014.209951	269132.686685	54.319361
3013.706053	268864.254712	54.324365
3013.006400	268584.673290	54.329370
3012.396504	268315.443366	54.334375
3011.736864	268053.760036	54.339380
3011.062046	267787.444028	54.344385
3010.454550	267516.482297	54.349389
3009.571618	267257.763558	54.354394
3009.483065	266983.078045	54.359399
3008.654180	266720.989253	54.364404
3007.717881	266448.322878	54.369409
3007.333873	266174.143048	54.374413
3006.466453	265919.599396	54.379418
3005.965016	265629.291744	54.384423
3004.825342	265370.894912	54.389428
3004.278821	265101.809670	54.394433
3003.657453	264829.323750	54.399437
3002.840607	264577.956470	54.404442
3002.521864	264309.803534	54.409447
3001.903668	264036.298988	54.414452
3001.098800	263763.664646	54.419457
3001.064370	263496.180442	54.424461
2999.921370	263220.925928	54.429466
2999.058293	262960.526050	54.434471
2998.654921	262688.745900	54.439476
2997.904863	262414.117525	54.444481
2997.329805	262144.376988	54.449485
2996.435225	261886.529787	54.454490
2995.714081	261612.075849	54.459495
2994.922553	261351.334956	54.464500
2994.518006	261081.364677	54.469505
2994.158624	260815.182198	54.474509
2993.085927	260544.044816	54.479514
2992.770881	260270.979587	54.484519
2991.800546	260012.433029	54.489524
2991.291260	259742.939096	54.494529
2990.781532	259464.073458	54.499533
2989.912749	259197.998727	54.504538
2989.276655	258925.367773	54.509543
2988.518853	258658.817650	54.514548
2987.888230	258401.772521	54.519553
2987.140812	258130.178797	54.524557
2986.700864	257863.044453	54.529562
2986.187598	257589.580657	54.534567
2985.411953	257320.590038	54.539572
2984.638615	257055.648682	54.544577
2983.827419	256775.866226	54.549581
2983.143972	256519.162693	54.554586
2982.507408	256242.918709	54.559591
2981.677414	255990.390171	54.564596
2981.092291	255715.335705	54.569601
2981.094563	255449.433194	54.574605
2979.999583	255171.455053	54.579610
2979.625215	254901.079752	54.584615
2979.022793	254642.837744	54.589620
2978.297041	254364.267504	54.594625
2978.067962	254083.479834	54.599629
2976.751970	253814.553924	54.604634
2975.767416	253546.390882	54.609639
2975.254927	253274.358957	54.614644
2974.267054	253008.107244	54.619649
2974.002612	252736.342470	54.624653
2973.282248	252479.802962	54.629658
2972.682474	252206.309417	54.634663
2972.174398	251933.896854	54.639668
2971.341884	251663.344206	54.644673
2970.982200	251386.477848	54.649677
2969.774888	251130.068377	54.654682
2969.815884	250838.165212	54.659687
2968.994653	250581.313488	54.664692
2968.163051	250310.049851	54.669697
2967.657296	250034.787816	54.674701
2966.954174	249764.752621	54.679706
2966.406679	249484.939690	54.684711
2965.342245	249214.911707	54.689716
2964.887663	248948.149196	54.694721
2964.386167	248667.719286	54.699725
2963.500097	248415.006902	54.704730
2962.654183	248136.618857	54.709735
2962.225813	247863.436697	54.714740
2961.631052	247589.364613	54.719745
2961.204516	247320.945306	54.724749
2960.324807	247037.293283	54.729754
2960.022555	246758.236119	54.734759
2959.047462	246486.034429	54.739764
2958.181675	246217.101039	54.744769
2957.833288	245941.414282	54.749773
2956.964577	245672.533352	54.754778
2956.279727	245393.768701	54.759783
2955.745003	245116.050413	54.764788
2955.056883	244842.253194	54.769793
2954.585409	244568.524110	54.774797
2953.740777	244308.402206	54.779802
2953.016614	244026.463506	54.784807
2952.114221	243751.556564	54.789812
2951.628265	243480.964298	54.794817
2951.305353	243191.833692	54.799821
2950.056922	242937.813731	54.804826
2949.455105	242655.094775	54.809831
2949.077397	242403.178997	54.814836
2948.074302	242107.028422	54.819841
2947.388424	241856.283012	54.824845
2946.992650	241580.282108	54.829850
2946.598828	241299.443243	54.834855
2945.753312	241030.721313	54.839860
2944.971217	240763.212258	54.844865
2944.616679	240486.265198	54.849869
2943.412322	240216.430584	54.854874
2942.871309	239936.433168	54.859879
2942.140022	239680.479414	54.864884
2941.438121	239405.117821	54.869889
2940.709391	239126.476269	54.874893
2940.056513	238871.632374	54.879898
2939.604450	238587.448125	54.884903
2938.738331	238330.576649	54.889908
2938.244906	238059.488824	54.894913
2937.797281	237787.426800	54.899917
2936.920199	237527.732476	54.904922
2936.340496	237247.416990	54.909927
2935.779233	236968.041485	54.914932
2935.147071	236703.828800	54.919937
2934.556279	236432.174876	54.924941
2933.317382	236167.779503	54.929946
2933.180514	235884.341955	54.934951
2932.579151	235626.212908	54.939956
2931.458192	235344.460449	54.944961
2931.219553	235065.853856	54.949965
2930.290328	234806.174627	54.954970
2929.801014	234525.164762	54.959975
2928.827943	234255.996187	54.964980
2928.261888	233981.442162	54.969985
2927.789504	233718.103205	54.974989
2927.161306	233451.734093	54.979994
2926.593677	233174.559932	54.984999
2925.953150	232903.661926	54.990004
2925.152493	232627.493825	54.995009
2924.739616	232349.329991	55.000013
2923.583092	232085.823755	55.005018
2923.175896	231812.243854	55.010023
2922.629985	231539.857985	55.015028
2921.896803	231260.653233	55.020033
2921.394623	230988.542158	55.025037
2920.380815	230717.836919	55.030042
2920.142418	230443.317746	55.035047
2919.502318	230161.173512	55.040052
2918.379927	229889.342170	55.045057
2918.120185	229615.796465	55.050061
2917.545719	229332.753307	55.055066
2916.550429	229056.015770	55.060071
2915.750424	228790.273023	55.065076
2915.417618	228508.212739	55.070081
2914.789033	228225.614592	55.075085
2913.791978	227955.984565	55.080090
2913.229399	227680.074080	55.085095
2912.761245	227397.275050	55.090100
2912.051750	227128.735146	55.095105
2911.688224	226851.828339	55.100109
2910.843601	226580.332661	55.105114
2910.142870	226301.673351	55.110119
2909.840325	226016.472204	55.115124
2909.065673	225736.247951	55.120129
2908.267271	225446.837185	55.125133
2907.483505	225174.165348	55.130138
2906.834606	224896.075494	55.135143
2906.081939	224610.186745	55.140148
2905.682691	224331.601046	55.145153
2905.132077	224043.289094	55.150157
2904.309518	223776.725857	55.155162
2903.904867	223489.398494	55.160167
2903.123810	223203.264740	55.165172
2902.357165	222934.836964	55.170177
2902.008936	222656.783802	55.175181
2900.899254	222368.502916	55.180186
2900.468460	222071.243039	55.185191
2899.746483	221791.011774	55.190196
2898.427335	221513.943927	55.195201
2898.091537	221235.906725	55.200205
2897.299789	220967.298931	55.205210
2897.061813	220696.033081	55.210215
2896.214656	220415.393986	55.215220
2895.596207	220127.680412	55.220225
2894.879915	219847.048227	55.225229
2894.001796	219576.333383	55.230234
2893.609252	219288.307309	55.235239
2893.079071	219013.071530	55.240244
2892.104804	218738.734506	55.245249
2891.537044	218454.570978	55.250253
2890.982986	218187.297825	55.255258
2890.380066	217896.815773	55.260263
2889.728594	217619.046064	55.265268
2889.065928	217343.812273	55.270273
2888.374157	217054.964340	55.275277
2887.380682	216783.451038	55.280282
2887.172855	216502.318792	55.285287
2886.670891	216222.659873	55.290292
2885.670251	215945.715872	55.295297
2885.252586	215656.919508	55.300301
2884.755110	215370.479054	55.305306
2883.753669	215087.250804	55.310311
2883.297058	214811.052660	55.315316
2882.653177	214529.386661	55.320321
2881.857235	214229.060801	55.325325
2881.110728	213959.238047	55.330330
2880.405399	213680.360139	55.335335
2879.957032	213384.170665	55.340340
2879.088082	213104.786532	55.345345
2878.458959	212828.407621	55.350349
2877.873398	212555.039519	55.355354
2877.403712	212267.335334	55.360359
2876.760912	211976.566981	55.365364
2875.888049	211705.666272	55.370369
2875.299096	211410.488157	55.375373
2874.440157	211127.292723	55.380378
2873.329897	210843.489243	55.385383
2873.317451	210558.724118	55.390388
2872.420792	210278.758555	55.395393
2871.840429	209995.065938	55.400397
2871.517361	209726.148562	55.405402
2870.731288	209437.361934	55.410407
2869.802367	209147.975644	55.415412
2869.179129	208874.069522	55.420417
2868.515926	208587.329258	55.425421
2867.773269	208310.580971	55.430426
2867.230444	208034.667749	55.435431
2866.649891	207731.869664	55.440436
2865.830840	207465.509842	55.445441
2865.161366	207175.137399	55.450445
2864.489554	206902.113364	55.455450
2864.213114	206610.268779	55.460455
2863.450091	206328.047684	55.465460
2862.602390	206051.822862	55.470465
2862.232700	205750.108737	55.475469
2861.407683	205475.282971	55.480474
2860.791965	205182.544741	55.485479
2860.179794	204899.492192	55.490484
2859.183679	204610.456837	55.495489
2858.532761	204314.623380	55.500493
2857.806078	204039.508925	55.505498
2857.236209	203755.742672	55.510503
2856.683138	203473.502306	55.515508
2855.896979	203196.950594	55.520513
2855.443048	202912.533926	55.525517
2854.808591	202622.535187	55.530522
2853.818101	202342.622249	55.535527
2853.334605	202049.077554	55.540532
2852.562463	201779.555250	55.545537
2852.118890	201485.116434	55.550541
2851.211764	201218.799649	55.555546
2850.698204	200921.282642	55.560551
2850.142158	200639.222609	55.565556
2849.192465	200361.540257	55.570561
2848.648795	200070.777102	55.575565
2847.858568	199787.320640	55.580570
2847.217875	199508.104913	55.585575
2846.570060	199223.381822	55.590580
2845.790878	198950.184445	55.595585
2845.371573	198676.104368	55.600589
2844.405733	198398.498394	55.605594
2843.725661	198104.980821	55.610599
2843.500646	197828.164010	55.615604
2842.533253	197553.565783	55.620609
2842.015018	197258.194985	55.625613
2841.470024	196985.187068	55.630618
2840.583413	196697.970584	55.635623
2840.065503	196416.550528	55.640628
2839.443804	196133.099835	55.645633
2838.916928	195843.324478	55.650637
2838.083860	195568.461070	55.655642
2837.537835	195277.610409	55.660647
2836.832345	194982.549573	55.665652
2835.863221	194717.573440	55.670657
2835.436233	194426.365288	55.675661
2834.582375	194147.301311	55.680666
2833.731340	193868.989146	55.685671
2833.247751	193590.187748	55.690676
2832.480290	193312.565267	55.695681
2832.080250	193026.959412	55.700685
2831.110390	192740.592974	55.705690
2830.562455	192471.516071	55.710695
2829.914177	192182.659082	55.715700
2829.022825	191909.059271	55.720705
2828.669757	191626.304153	55.725709
2828.427294	191355.938172	55.730714
2827.672528	191071.684967	55.735719
2827.022314	190787.047920	55.740724
2826.372445	190510.046220	55.745729
2825.716450	190211.609212	55.750733
2824.913216	189931.848866	55.755738
2824.159819	189648.698058	55.760743
2823.524700	189370.072165	55.765748
2822.780849	189073.730007	55.770753
2821.943681	188796.513530	55.775757
2821.683056	188517.960606	55.780762
2820.615015	188233.786748	55.785767
2820.433986	187939.983427	55.790772
2819.327978	187663.821307	55.795777
2818.452129	187376.912457	55.800781
2818.221452	187106.301794	55.805786
2817.332057	186819.869273	55.810791
2816.855484	186536.222847	55.815796
2815.910694	186263.516657	55.820801
2815.285625	185984.171670	55.825805
2814.919241	185702.879206	55.830810
2814.353121	185420.755061	55.835815
2813.526779	185138.533953	55.840820
2812.442316	184854.294642	55.845825
2811.957630	184568.562820	55.850829
2811.366119	184291.080318	55.855834
2810.321829	184022.499666	55.860839
2810.057757	183734.817372	55.865844
2809.240325	183466.738442	55.870849
2808.846741	183190.338202	55.875853
2808.241624	182902.155625	55.880858
2807.634096	182614.496868	55.885863
2807.176165	182343.442108	55.890868
2806.382721	182066.641616	55.895873
2806.023671	181766.152285	55.900877
2805.100234	181486.959197	55.905882
2804.589876	181203.199530	55.910887
2803.941757	180903.728711	55.915892
2802.808155	180628.276037	55.920897
2802.403233	180347.787102	55.925901
2801.597089	180060.825516	55.930906
2800.952955	179774.158203	55.935911
2800.551281	179491.270350	55.940916
2799.810786	179211.439882	55.945921
2799.200212	178909.051628	55.950925
2798.449322	178629.315711	55.955930
2797.708576	178346.756348	55.960935
2797.504800	178056.812976	55.965940
2796.747346	177773.878556	55.970945
2796.248233	177478.173303	55.975949
2795.145539	177190.502425	55.980954
2794.655231	176900.905040	55.985959
2794.418179	176606.856138	55.990964
2793.332887	176327.328601	55.995969
2792.603906	176041.425359	56.000973
2792.173661	175748.608768	56.005978
2791.251126	175456.966036	56.010983
2790.645928	175167.208341	56.015988
2789.849474	174880.764334	56.020993
2789.389896	174584.145301	56.025997
2788.535360	174301.720847	56.031002
2787.830071	174014.454606	56.036007
2787.410541	173717.352348	56.041012
2786.883328	173427.950939	56.046017
2785.987365	173143.137559	56.051021
2785.290765	172852.139295	56.056026
2784.290363	172565.121018	56.061031
2784.113409	172275.977771	56.066036
2783.283594	171996.287328	56.071041
2782.629807	171695.612886	56.076045
2782.093411	171410.767798	56.081050
2781.579502	171130.092441	56.086055
2780.812875	170827.407820	56.091060
2780.043270	170546.166759	56.096065
2779.418976	170245.346247	56.101069
2778.704969	169967.635868	56.106074
2778.053561	169664.662338	56.111079
2777.439963	169378.369305	56.116084
2776.717226	169086.958255	56.121089
2776.215892	168792.920231	56.126093
2775.524496	168506.061110	56.131098
2774.795622	168220.837759	56.136103
2774.014030	167908.946632	56.141108
2773.576680	167578.158541	56.146113
2773.294170	167284.161158	56.151117
2772.511624	166993.792962	56.156122
2771.654160	166694.728674	56.161127
2771.066364	166396.361572	56.166132
2770.055219	166108.922892	56.171137
2769.407451	165816.825935	56.176141
2768.861432	165522.871458	56.181146
2768.417461	165230.365398	56.186151
2767.809394	164947.703656	56.191156
2766.801378	164639.906435	56.196161
2765.892601	164344.086163	56.201165
2765.376095	164067.494398	56.206170
2764.819589	163764.401066	56.211175
2764.334193	163473.899087	56.216180
2763.547770	163200.802302	56.221185
2762.810930	162888.310753	56.226189
2762.144972	162626.362404	56.231194
2761.526419	162303.876525	56.236199
2761.014155	162039.072868	56.241204
2760.306377	161734.596581	56.246209
2759.365435	161443.738161	56.251213
2758.872061	161156.599912	56.256218
2757.684787	160857.966374	56.261223
2757.015659	160579.569447	56.266228
2756.517620	160308.292544	56.271233
2756.085073	160004.219772	56.276237
2755.336210	159716.930274	56.281242
2754.484877	159450.801216	56.286247
2754.465829	159146.899217	56.291252
2753.786027	158861.525464	56.296257
2753.274990	158568.614076	56.301261
2752.042841	158294.837514	56.306266
2751.373455	157978.043680	56.311271
2750.877429	157696.248060	56.316276
2750.204157	157409.169058	56.321281
2749.645474	157105.764514	56.326285
2748.981025	156839.168283	56.331290
2747.775183	156545.036654	56.336295
2747.350364	156252.512675	56.341300
2746.406490	155981.327557	56.346305
2746.075442	155683.340255	56.351309
2745.534432	155381.397391	56.356314
2744.683545	155134.775820	56.361319
2744.018305	154821.811354	56.366324
2743.421144	154527.893191	56.371329
2742.707798	154240.834604	56.376333
2741.790880	153983.389333	56.381338
2741.348837	153672.522989	56.386343
2740.650137	153391.494366	56.391348
2739.804800	153110.211710	56.396353
2739.275871	152823.860630	56.401357
2738.906543	152557.607477	56.406362
2737.996996	152255.840210	56.411367
2737.543076	151994.956074	56.416372
2736.980700	151696.646986	56.421377
2736.628508	151400.061308	56.426381
2735.631214	151123.509701	56.431386
2734.508125	150842.709856	56.436391
2734.510835	150527.201781	56.441396
2733.147700	150271.788084	56.446401
2733.249841	149962.268691	56.451405
2732.154421	149699.737914	56.456410
2731.609901	149374.427132	56.461415
2731.079857	149128.689366	56.466420
2730.323158	148815.364472	56.471425
2729.614249	148529.257596	56.476429
2728.879955	148250.922392	56.481434
2728.247270	147957.729750	56.486439
2727.896017	147659.157625	56.491444
2726.783372	147389.607977	56.496449
2725.981418	147080.374030	56.501453
2725.464860	146823.023771	56.506458
2724.692809	146518.619726	56.511463
2723.770914	146240.153993	56.516468
2723.601100	145968.052632	56.521473
2723.072378	145665.880317	56.526477
2722.213017	145402.953744	56.531482
2721.520541	145077.634270	56.536487
2721.239045	144825.028519	56.541492
2720.538511	144523.834846	56.546497
2719.929909	144239.352210	56.551501
2719.096354	143952.404529	56.556506
2718.563607	143656.999861	56.561511
2717.870012	143357.226941	56.566516
2717.170329	143080.469776	56.571521
2716.419138	142793.430921	56.576525
2715.785628	142490.975866	56.581530
2714.489650	142228.780842	56.586535
2714.549686	141916.679145	56.591540
2713.473115	141640.935004	56.596545
2713.142513	141364.427200	56.601549
2712.376200	141047.103420	56.606554
2711.420321	140788.361104	56.611559
2710.927672	140498.050334	56.616564
2710.011252	140218.380489	56.621569
2709.776849	139890.731295	56.626573
2708.967510	139651.795969	56.631578
2708.090382	139348.953603	56.636583
2707.932927	139047.550327	56.641588
2707.072591	138794.451153	56.646593
2706.340016	138479.957040	56.651597
2705.944023	138234.297621	56.656602
2705.121057	137915.834557	56.661607
2704.541930	137615.668764	56.666612
2703.559466	137364.125723	56.671617
2702.947382	137034.357379	56.676621
2702.232755	136784.174342	56.681626
2701.236144	136480.186163	56.686631
2700.825804	136212.453829	56.691636
2700.204491	135914.865626	56.696641
2699.612092	135653.023674	56.701645
2698.996222	135346.573354	56.706650
2698.155538	135087.621411	56.711655
2697.897395	134760.935081	56.716660
2697.158415	134518.270301	56.721665
2696.215631	134210.473797	56.726669
2695.976779	133906.557756	56.731674
2695.058121	133670.584869	56.736679
2694.510507	133359.101946	56.741684
2693.967003	133069.584238	56.746689
2692.910876	132789.512266	56.751693
2692.347337	132509.695279	56.756698
2691.570652	132221.506071	56.761703
2691.118600	131919.969479	56.766708
2690.056167	131647.619854	56.771713
2689.678982	131366.692305	56.776717
2689.666524	131066.771817	56.781722
2688.578266	130789.735032	56.786727
2688.001590	130497.924585	56.791732
2687.173261	130203.489815	56.796737
2686.831752	129938.675958	56.801741
2686.132134	129622.724143	56.806746
2685.178574	129362.737448	56.811751
2684.735833	129044.643194	56.816756
2683.709228	128785.753037	56.821761
2683.172240	128472.061964	56.826765
2682.613649	128184.845081	56.831770
2681.696624	127944.081357	56.836775
2681.286663	127638.977614	56.841780
2680.627068	127323.198180	56.846785
2679.876007	127074.618127	56.851789
2679.163732	126784.189147	56.856794
2678.788054	126463.485351	56.861799
2678.150083	126219.555862	56.866804
2677.255690	125923.272458	56.871809
2676.582349	125616.467897	56.876813
2676.251936	125304.228173	56.881818
2675.793308	125006.527002	56.886823
2674.873891	124763.848912	56.891828
2673.925127	124454.180532	56.896833
2673.395491	124136.335109	56.901837
2672.689293	123884.996347	56.906842
2671.878387	123572.510025	56.911847
2671.616168	123286.606015	56.916852
2670.764347	123013.585135	56.921857
2670.133723	122719.784082	56.926861
2669.152748	122429.558993	56.931866
2668.695179	122150.351653	56.936871
2667.787157	121850.433282	56.941876
2667.472082	121555.719062	56.946881
2666.516475	121287.214515	56.951885
2665.982854	120982.993239	56.956890
2665.275057	120726.021956	56.961895
2664.864807	120419.610197	56.966900
2664.124409	120158.821653	56.971905
2663.537612	119854.418787	56.976909
2662.965986	119545.192560	56.981914
2662.343170	119281.601037	56.986919
2661.404369	118960.785051	56.991924
2660.330970	118701.155740	56.996929
2659.982082	118393.228326	57.001933
2659.560128	118104.594102	57.006938
2658.470227	117826.168009	57.011943
2658.411264	117555.471614	57.016948
2657.716940	117239.354572	57.021953
2656.877990	116981.457388	57.026957
2656.062307	116662.021623	57.031962
2655.448678	116377.067905	57.036967
2654.976150	116091.841135	57.041972
2654.315813	115809.421015	57.046977
2653.351535	115505.415100	57.051981
2653.113529	115225.511478	57.056986
2652.034680	114922.311404	57.061991
2651.654612	114656.679045	57.066996
2650.703874	114375.399925	57.072001
2649.980952	114064.512291	57.077005
2649.208495	113802.391034	57.082010
2648.639586	113489.195006	57.087015
2647.916983	113235.449224	57.092020
2647.560650	112925.120582	57.097025
2646.719312	112674.109237	57.102029
2645.999819	112351.812640	57.107034
2645.594895	112072.548207	57.112039
2645.022772	111804.330254	57.117044
2644.323000	111475.340444	57.122049
2643.502332	111205.575519	57.127053
2643.054173	110942.379633	57.132058
2642.017892	110636.204360	57.137063
2641.583886	110338.428068	57.142068
2640.766654	110087.908788	57.147073
2640.501058	109796.039259	57.152077
2639.561023	109506.850009	57.157082
2638.946049	109205.327917	57.162087
2638.289466	108898.619304	57.167092
2637.914059	108604.116401	57.172097
2636.994665	108336.905164	57.177101
2636.450273	108029.885190	57.182106
2635.130721	107749.235073	57.187111
2634.912376	107444.651797	57.192116
2634.193126	107195.377771	57.197121
2633.922836	106872.473183	57.202125
2633.468663	106609.705864	57.207130
2632.536609	106282.237990	57.212135
2631.840705	106018.278254	57.217140
2631.180527	105718.976779	57.222145
2630.608069	105397.573836	57.227149
2630.006104	105157.191024	57.232154
2629.050647	104836.440035	57.237159
2628.544298	104520.684897	57.242164
2627.600192	104286.043188	57.247169
2626.938202	103981.396775	57.252173
2626.379045	103666.175292	57.257178
2625.384693	103406.288627	57.262183
2625.101291	103084.528747	57.267188
2624.138274	102832.896764	57.272193
2622.979452	102529.921133	57.277197
2622.273720	102235.891866	57.282202
2622.273017	101944.012878	57.287207
2621.503079	101692.819314	57.292212
2620.716934	101428.633476	57.297217
2620.158272	101128.372048	57.302221
2619.661783	100796.509203	57.307226
2618.652594	100571.100025	57.312231
2617.767821	100266.106045	57.317236
2617.486703	99976.611447	57.322241
2616.677953	99686.639573	57.327245
2615.990045	99436.408945	57.332250
2615.447725	99119.571912	57.337255
2614.780283	98865.259551	57.342260
2614.213164	98568.483219	57.347265
2613.685239	98262.400093	57.352269
2613.004986	98023.137183	57.357274
2611.712356	97731.579662	57.362279
2611.691010	97437.832971	57.367284
2610.918758	97165.239737	57.372289
2610.079447	96876.595851	57.377293
2609.542054	96629.961803	57.382298
2608.688052	96341.688567	57.387303
2608.377218	96032.810654	57.392308
2607.010695	95748.158641	57.397313
2606.541644	95458.085382	57.402317
2606.065489	95179.406554	57.407322
2605.156148	94944.987780	57.412327
2604.716878	94663.005577	57.417332
2604.225256	94369.601684	57.422337
2603.630747	94059.356403	57.427341
2603.153321	93795.146882	57.432346
2602.333672	93530.639622	57.437351
2601.482714	93230.345090	57.442356
2601.303257	92920.848904	57.447361
2600.184139	92661.389823	57.452365
2599.894340	92398.302235	57.457370
2599.072056	92079.002633	57.462375
2598.499081	91818.794801	57.467380
2597.584607	91531.557164	57.472385
2597.140679	91221.651184	57.477389
2596.072839	90981.567660	57.482394
2595.286596	90702.208059	57.487399
2594.792280	90395.447545	57.492404
2594.710254	90100.444083	57.497409
2593.815962	89862.786323	57.502413
2593.314126	89561.801883	57.507418
2591.910556	89260.374889	57.512423
2591.753418	88958.412222	57.517428
2591.061561	88723.207396	57.522433
2589.986978	88428.358571	57.527437
2589.855783	88145.295402	57.532442
2589.049394	87865.252778	57.537447
2588.723037	87565.010035	57.542452
2587.950979	87303.676941	57.547457
2587.519356	87024.644552	57.552461
2586.732128	86725.614971	57.557466
2586.169776	86421.273472	57.562471
2585.423987	86165.851795	57.567476
2584.763688	85841.604231	57.572481
2583.857390	85582.227806	57.577485
2583.016515	85282.555040	57.582490
2582.124275	84981.252930	57.587495
2581.940819	84746.118984	57.592500
2580.917774	84425.271953	57.597505
2580.538897	84125.821232	57.602509
2579.908832	83844.047764	57.607514
2578.807166	83564.767667	57.612519
2578.329681	83306.492082	57.617524
2577.774742	83055.451021	57.622529
2576.889164	82752.265603	57.627533
2576.716953	82433.792263	57.632538
2575.842485	82168.850087	57.637543
2575.395749	81912.190286	57.642548
2574.423535	81621.425279	57.647553
2573.940463	81311.586824	57.652557
2573.440681	81051.473059	57.657562
2572.314991	80780.548750	57.662567
2571.410411	80468.691996	57.667572
2570.932851	80219.352219	57.672577
2570.202782	79902.755115	57.677581
2569.841273	79659.658444	57.682586
2569.035320	79359.196827	57.687591
2568.395211	79093.388659	57.692596
2568.141367	78788.532475	57.697601
2566.935893	78541.609606	57.702605
2566.744812	78229.255469	57.707610
2565.709544	77973.472917	57.712615
2565.018279	77666.966541	57.717620
2564.607596	77409.571331	57.722625
2563.726008	77114.293427	57.727629
2563.066063	76853.573859	57.732634
2562.099368	76564.020000	57.737639
2561.679580	76273.521907	57.742644
2561.314519	76013.970238	57.747649
2560.265340	75722.420326	57.752653
2559.727055	75454.451305	57.757658
2559.187265	75159.990380	57.762663
2558.308580	74901.053943	57.767668
2557.992841	74597.448862	57.772673
2557.019412	74341.949465	57.777677
2556.261650	74030.573463	57.782682
2555.518314	73786.809323	57.787687
2555.150399	73489.710216	57.792692
2554.618935	73213.331656	57.797697
2553.883393	72956.526252	57.802701
2553.270966	72663.329857	57.807706
2552.391973	72403.690966	57.812711
2551.989531	72098.249849	57.817716
2550.987792	71832.562931	57.822721
2550.308176	71560.500355	57.827725
2549.744543	71278.484439	57.832730
2549.173669	70979.922111	57.837735
2548.460537	70729.888067	57.842740
2547.985050	70418.802668	57.847745
2547.078492	70182.861691	57.852749
2546.991117	69869.240528	57.857754
2545.699512	69596.193639	57.862759
2545.273293	69326.832682	57.867764
2544.565942	69044.314230	57.872769
2543.930364	68746.885524	57.877773
2543.230483	68483.089809	57.882778
2542.271118	68218.388777	57.887783
2541.713582	67925.963649	57.892788
2541.246083	67652.249712	57.897793
2540.267485	67384.193816	57.902797
2539.819834	67107.941657	57.907802
2539.170657	66846.180403	57.912807
2538.354529	66560.916137	57.917812
2537.474488	66287.435718	57.922817
2536.952117	66004.951217	57.927821
2536.832757	65743.583250	57.932826
2535.864535	65469.881457	57.937831
2535.106484	65186.733928	57.942836
2534.557596	64901.917357	57.947841
2533.626958	64625.093501	57.952845
2533.153248	64356.480533	57.957850
2532.348246	64104.475889	57.962855
2531.967151	63817.511820	57.967860
2531.195410	63531.389646	57.972865
2530.600371	63275.883325	57.977869
2530.134292	62978.222493	57.982874
2529.163693	62743.246935	57.987879
2528.196218	62437.256181	57.992884
2528.124806	62138.298690	57.997889
2526.785457	61904.183435	58.002893
2526.009319	61621.034901	58.007898
2525.675062	61346.332823	58.012903
2525.132067	61093.956350	58.017908
2524.130575	60793.287289	58.022913
2523.779149	60527.725990	58.027917
2522.930516	60273.778792	58.032922
2522.284877	59983.075316	58.037927
2521.539968	59716.457866	58.042932
2521.325514	59444.132326	58.047937
2520.348727	59205.530312	58.052941
2519.812694	58912.635816	58.057946
2519.022388	58634.782557	58.062951
2518.361991	58392.124303	58.067956
2517.853453	58100.741665	58.072961
2517.027756	57848.393772	58.077965
2516.886452	57538.427646	58.082970
2515.731498	57305.312511	58.087975
2514.926869	57027.950882	58.092980
2514.793902	56738.505059	58.097985
2513.887241	56487.552638	58.102989
2513.588202	56197.094123	58.107994
2512.559169	55945.842536	58.112999
2512.455619	55638.101855	58.118004
2511.498412	55376.219962	58.123009
2510.711166	55110.096587	58.128013
2510.297868	54819.560941	58.133018
2509.204127	54544.463023	58.138023
2508.905591	54285.789698	58.143028
2507.936756	53997.181062	58.148033
2507.607934	53724.372860	58.153037
2506.517617	53471.646226	58.158042
2506.005078	53152.668592	58.163047
2505.353609	52927.889255	58.168052
2504.443791	52630.579012	58.173057
2503.803991	52368.750280	58.178061
2503.250472	52093.755815	58.183066
2502.320683	51837.989169	58.188071
2501.449207	51547.657715	58.193076
2501.158087	51295.303149	58.198081
2500.398731	51015.814517	58.203085
2499.716569	50761.314789	58.208090
2498.964009	50495.307624	58.213095
2498.133961	50212.283578	58.218100
2497.665225	49962.699854	58.223105
2496.845066	49695.971864	58.228109
2496.337828	49437.208290	58.233114
2495.793076	49161.507721	58.238119
2494.764661	48918.351124	58.243124
2494.442954	48633.598148	58.248129
2493.264762	48395.435796	58.253133
2493.094533	48107.519747	58.258138
2491.932212	47865.341489	58.263143
2491.954928	47580.202907	58.268148
2490.990691	47326.774499	58.273153
2490.353089	47071.137569	58.278157
2489.618113	46803.610915	58.283162
2489.266900	46533.588830	58.288167
2487.761877	46291.793349	58.293172
2487.473299	46010.661091	58.298177
2486.719419	45771.186002	58.303181
2486.212690	45481.104815	58.308186
2485.395355	45262.764825	58.313191
2484.963078	44998.057923	58.318196
2484.194412	44722.873504	58.323201
2482.774522	44465.981735	58.328205
2482.646195	44221.533017	58.333210
2481.654077	43972.348031	58.338215
2481.325991	43709.851657	58.343220
2480.769234	43451.231540	58.348225
2480.151470	43204.404866	58.353229
2479.589004	42945.695172	58.358234
2479.000279	42704.895295	58.363239
2477.980817	42443.432143	58.368244
2477.615689	42180.819382	58.373249
2476.640662	41926.446699	58.378253
2476.419440	41659.607081	58.383258
2475.541476	41425.726394	58.388263
2474.690873	41140.398503	58.393268
2474.033704	40910.828122	58.398273
2473.347811	40643.518295	58.403277
2472.608438	40401.609404	58.408282
2472.003546	40155.366718	58.413287
2471.598536	39890.085665	58.418292
2470.943210	39634.626085	58.423297
2470.054874	39384.653282	58.428301
2469.385863	39136.816693	58.433306
2468.560094	38885.832743	58.438311
2467.961945	38624.411763	58.443316
2467.464586	38375.313431	58.448321
2466.371417	38139.442740	58.453325
2465.879324	37862.375404	58.458330
2465.030743	37653.501183	58.463335
2464.518915	37373.841602	58.468340
2464.134378	37156.984035	58.473345
2463.045596	36875.140168	58.478349
2462.214102	36672.915538	58.483354
2461.533013	36412.208966	58.488359
2460.859463	36186.343598	58.493364
2460.463036	35913.766099	58.498369
2459.622102	35702.125284	58.503373
2459.184195	35423.649684	58.508378
2458.219551	35223.197430	58.513383
2457.585414	34958.901015	58.518388
2457.008424	34713.659420	58.523393
2456.206687	34492.676452	58.528397
2455.516221	34244.368518	58.533402
2454.759749	34005.447744	58.538407
2453.836221	33769.011120	58.543412
2453.652127	33520.412483	58.548417
2452.711583	33324.773886	58.553421
2452.057695	33043.584727	58.558426
2451.356149	32854.610889	58.563431
2450.399228	32594.440744	58.568436
2450.186796	32370.042601	58.573441
2448.853670	32140.514247	58.578445
2447.888801	31931.796467	58.583450
2447.610147	31683.995737	58.588455
2446.883965	31486.771142	58.593460
2446.387460	31223.432117	58.598465
2445.114029	31029.774347	58.603469
2444.354208	30831.046107	58.608474
2443.607386	30618.254495	58.613479
2442.472602	30393.315378	58.618484
2441.927562	30194.799389	58.623489
2440.585129	30016.395507	58.628493
2439.725558	29811.985495	58.633498
2438.885470	29629.313054	58.638503
2437.515586	29461.931635	58.643508
2436.741648	29284.046005	58.648513
2435.606907	29109.766326	58.653517
2434.923371	28966.162518	58.658522
2434.184834	28794.660824	58.663527
2433.138763	28648.551640	58.668532
2432.735366	28509.218800	58.673537
2431.751828	28349.621873	58.678541
2431.020534	28202.798548	58.683546
2430.233320	28062.595163	58.688551
2429.402979	27926.502451	58.693556
2428.642518	27786.399902	58.698561
2427.632332	27649.732991	58.703565
2426.999266	27517.842952	58.708570
2426.040758	27401.631209	58.713575
2425.436268	27273.323773	58.718580
2425.127907	27148.763216	58.723585
2424.020876	27029.524183	58.728589
2423.590289	26913.943897	58.733594
2422.914735	26806.470520	58.738599
2422.292949	26676.275793	58.743604
2421.825683	26555.667237	58.748609
2420.949939	26440.966527	58.753613
2420.593505	26323.027478	58.758618
2420.072407	26200.885270	58.763623
2419.195607	26080.931228	58.768628
2418.559776	25942.679367	58.773633
2417.820330	25844.577496	58.778637
2417.070783	25720.544950	58.783642
2416.262669	25586.533732	58.788647
2415.472542	25497.132571	58.793652
2415.041970	25374.706674	58.798657
2414.315184	25259.955254	58.803661
2413.884442	25164.660379	58.808666
2413.070748	25034.136640	58.813671
2412.229230	24936.407161	58.818676
2411.910309	24829.781300	58.823681
2411.146597	24707.899004	58.828685
2410.848652	24611.983813	58.833690
2410.340227	24491.952478	58.838695
2409.762196	24359.297846	58.843700
2408.910726	24254.814272	58.848705
2408.428679	24139.191076	58.853709
2407.793919	24010.653944	58.858714
2406.941923	23915.734972	58.863719
2406.416684	23789.341248	58.868724
2406.073015	23668.379500	58.873729
2405.359247	23553.357172	58.878733
2404.451099	23441.077386	58.883738
2403.862429	23324.587071	58.888743
2402.912939	23194.992236	58.893748
2402.620486	23077.044100	58.898753
2401.568356	22974.900183	58.903757
2401.272902	22845.885957	58.908762
2400.512403	22729.236958	58.913767
2399.750372	22627.412513	58.918772
2399.203833	22508.352106	58.923777
2398.682556	22399.127058	58.928781
2398.074896	22277.717950	58.933786
2397.367278	22163.446167	58.938791
2396.770021	22043.153695	58.943796
2396.317969	21911.526008	58.948801
2395.295919	21823.239533	58.953805
2394.801419	21690.338150	58.958810
2394.506607	21582.248247	58.963815
2393.398367	21468.388478	58.968820
2393.120023	21348.473151	58.973825
2392.561906	21233.259838	58.978829
2391.608070	21107.887144	58.983834
2390.790429	20990.449989	58.988839
2390.009475	20868.662331	58.993844
2389.697847	20749.212799	58.998849
2388.811754	20651.799079	59.003853
2388.173094	20524.338589	59.008858
2387.455656	20401.297453	59.013863
2387.047180	20295.536212	59.018868
2386.420253	20182.797249	59.023873
2385.822724	20051.758461	59.028877
2385.382589	19932.754734	59.033882
2384.233140	19827.111377	59.038887
2383.887471	19699.296533	59.043892
2383.310299	19577.415147	59.048897
2382.305976	19461.807571	59.053901
2381.740133	19344.011255	59.058906
2381.261356	19225.485206	59.063911
2380.249461	19115.754472	59.068916
2379.936211	18998.808040	59.073921
2379.264667	18884.390203	59.078925
2378.819842	18753.167176	59.083930
2378.058281	18631.476349	59.088935
2377.333415	18510.415339	59.093940
2376.818076	18389.221004	59.098945
2375.774669	18281.068508	59.103949
2375.431798	18149.055270	59.108954
2374.871610	18028.365805	59.113959
2374.306978	17908.166608	59.118964
2373.325006	17788.791918	59.123969
2372.780446	17672.547500	59.128973
2372.003555	17549.782784	59.133978
2371.399778	17428.950768	59.138983
2370.627865	17323.642250	59.143988
2370.097534	17193.980043	59.148993
2369.093905	17083.110112	59.153997
2368.499245	16965.351971	59.159002
2368.085209	16840.638777	59.164007
2367.280996	16738.704843	59.169012
2366.924787	16610.079578	59.174017
2366.073787	16494.101370	59.179021
2365.506827	16376.872154	59.184026
2364.681731	16256.637688	59.189031
2363.665360	16137.035138	59.194036
2363.097342	16019.551695	59.199041
2362.163262	15908.323110	59.204045
2362.005104	15810.053182	59.209050
2361.009915	15679.626167	59.214055
2360.552076	15580.101853	59.219060
2360.186186	15468.677530	59.224065
2359.637550	15345.588013	59.229069
2358.609949	15216.832810	59.234074
2357.987449	15125.725406	59.239079
2357.193762	15006.696451	59.244084
2356.468280	14886.139235	59.249089
2356.148203	14771.525249	59.254093
2355.211587	14642.360997	59.259098
2354.362135	14548.521299	59.264103
2353.995379	14425.949146	59.269108
2353.100271	14310.115551	59.274113
2352.074117	14226.091667	59.279117
2351.705346	14094.094433	59.284122
2350.834636	13993.154326	59.289127
2350.466772	13901.633120	59.294132
2349.912422	13762.290984	59.299137
2349.023982	13681.365270	59.304141
2348.386474	13570.604581	59.309146
2347.803595	13450.148718	59.314151
2347.136780	13365.691727	59.319156
2346.716108	13229.297587	59.324161
2345.690494	13141.413898	59.329165
2345.559179	13019.377852	59.334170
2344.864779	12894.301232	59.339175
2343.866060	12803.161291	59.344180
2343.442090	12690.519206	59.349185
2342.826000	12568.586330	59.354189
2341.966264	12452.990073	59.359194
2341.424256	12353.089478	59.364199
2340.530367	12250.536993	59.369204
2340.015466	12112.697730	59.374209
2339.058908	12042.667148	59.379213
2338.790118	11909.125109	59.384218
2337.726514	11806.464058	59.389223
2336.909400	11708.149026	59.394228
2336.381877	11606.944168	59.399233
2335.473904	11478.952544	59.404237
2335.036154	11397.852032	59.409242
2334.608675	11288.704734	59.414247
2333.520113	11185.195751	59.419252
2332.982755	11078.933355	59.424257
2332.179902	10974.670384	59.429261
2331.467637	10861.171356	59.434266
2330.634359	10798.025359	59.439271
2329.583785	10676.351183	59.444276
2329.459412	10603.156453	59.449281
2328.696010	10499.099598	59.454285
2327.729806	10395.732063	59.459290
2327.137970	10305.863417	59.464295
2326.515492	10221.839423	59.469300
2325.915269	10128.453910	59.474305
2325.044899	10041.013727	59.479309
2324.218742	9949.035209	59.484314
2323.820691	9854.679280	59.489319
2322.745837	9777.373367	59.494324
2322.644883	9689.314987	59.499329
2321.727996	9601.210185	59.504333
2321.150147	9503.929959	59.509338
2320.355999	9413.442723	59.514343
2319.365205	9340.563913	59.519348
2318.740291	9237.188489	59.524353
2317.927235	9172.250908	59.529357
2317.654696	9088.808110	59.534362
2317.001782	9004.768534	59.539367
2315.979813	8924.843369	59.544372
2315.816622	8838.063692	59.549377
2315.104323	8750.361404	59.554381
2314.229197	8666.496630	59.559386
2313.407544	8580.913915	59.564391
2312.641877	8516.652877	59.569396
2312.094801	8436.496839	59.574401
2311.182559	8367.692024	59.579405
2310.633125	8283.001885	59.584410
2310.097425	8196.861671	59.589415
2309.368175	8126.152214	59.594420
2308.859611	8054.470919	59.599425
2308.269480	7974.645257	59.604429
2307.615591	7883.417701	59.609434
2306.692956	7809.805856	59.614439
2305.612662	7745.955782	59.619444
2305.366173	7666.166414	59.624449
2304.134442	7591.420609	59.629453
2303.835811	7514.472272	59.634458
2303.454871	7437.998854	59.639463
2302.329292	7389.111856	59.644468
2301.982412	7297.873118	59.649473
2301.061928	7235.422545	59.654477
2300.344064	7171.887813	59.659482
2299.885378	7093.361783	59.664487
2299.049624	7028.663134	59.669492
2298.797143	6948.608786	59.674497
2297.961706	6884.688481	59.679501
2297.307545	6813.932333	59.684506
2296.955560	6739.815645	59.689511
2296.069568	6671.979211	59.694516
2295.512013	6600.946089	59.699521
2294.365227	6521.867258	59.704525
2293.548226	6458.149375	59.709530
2293.076962	6396.224259	59.714535
2292.238233	6336.722433	59.719540
2292.094259	6258.341004	59.724545
2291.242533	6202.311594	59.729549
2290.337581	6128.304589	59.734554
2289.902460	6057.204175	59.739559
2289.346654	5995.424288	59.744564
2289.020688	5936.228455	59.749569
2288.478389	5864.600144	59.754573
2287.549612	5791.765167	59.759578
2286.868689	5728.554152	59.764583
2285.974447	5655.845300	59.769588
2285.738453	5574.577149	59.774593
2284.672183	5503.475381	59.779597
2284.000746	5449.636573	59.784602
2283.437616	5367.155533	59.789607
2282.265102	5312.240425	59.794612
2281.770214	5243.727005	59.799617
2280.996624	5179.273455	59.804621
2280.671169	5123.708099	59.809626
2280.065985	5058.154143	59.814631
2279.216603	4998.691738	59.819636
2278.842925	4916.951368	59.824641
2277.982466	4863.675476	59.829645
2277.239938	4799.629573	59.834650
2276.475683	4739.799011	59.839655
2275.743529	4658.800724	59.844660
2275.259482	4606.358071	59.849665
2274.460379	4550.034782	59.854669
2274.167966	4488.748635	59.859674
2273.298569	4427.839755	59.864679
2272.362625	4369.772227	59.869684
2272.124598	4297.870610	59.874689
2271.570256	4240.855880	59.879693
2270.446960	4181.433126	59.884698
2270.077736	4112.958665	59.889703
2269.381045	4059.425486	59.894708
2268.632787	4006.010303	59.899713
2268.319338	3939.793603	59.904718
2267.367645	3884.422155	59.909722
2266.765914	3808.114514	59.914727
2265.960085	3753.322950	59.919732
2265.558404	3694.103178	59.924737
2264.676630	3633.309181	59.929742
2263.946643	3578.464445	59.934746
2263.582748	3491.960021	59.939751
2262.747840	3453.173044	59.944756
2262.224717	3398.848208	59.949761
2261.356082	3327.543458	59.954766
2260.632927	3259.879876	59.959770
2260.060567	3210.892993	59.964775
2259.083119	3149.699007	59.969780
2258.670752	3086.107408	59.974785
2258.109730	3028.068539	59.979790
2257.258823	2973.631665	59.984794
2256.870128	2920.989863	59.989799
2256.277726	2859.956037	59.994804
2255.893611	2798.507753	59.999809
2254.832125	2742.994806	60.004814
2254.378240	2680.546330	60.009818
2253.431871	2622.253972	60.014823
2252.648290	2563.210538	60.019828
2252.161900	2495.104463	60.024833
2251.186722	2449.283902	60.029838
2250.281936	2393.547925	60.034842
2250.135867	2335.905726	60.039847
2249.275513	2272.147425	60.044852
2248.569625	2222.733193	60.049857
2247.929675	2168.899075	60.054862
2247.170556	2105.291832	60.059866
2246.670060	2040.494145	60.064871
2245.935618	1992.553498	60.069876
2245.424135	1940.666478	60.074881
2244.566626	1894.485198	60.079886
2243.947464	1838.513640	60.084890
2243.151936	1792.665078	60.089895
2242.682528	1745.063283	60.094900
2242.305877	1682.354501	60.099905
2241.457701	1630.175041	60.104910
2240.773958	1580.344715	60.109914
2240.121176	1517.306684	60.114919
2239.264016	1474.392730	60.119924
2238.659456	1405.072525	60.124929
2238.061801	1356.494087	60.129934
2237.397254	1295.701406	60.134938
2236.678967	1247.699153	60.139943
2235.904682	1192.819169	60.144948
2235.233223	1141.268681	60.149953
2234.737745	1108.875364	60.154958
2233.987743	1059.651864	60.159962
2233.428727	999.985423	60.164967
2232.763432	949.099339	60.169972
2232.052562	889.895837	60.174977
2231.328523	844.412676	60.179982
2230.576427	804.007189	60.184986
2230.005180	751.039488	60.189991
2229.140994	712.631115	60.194996
2228.744369	661.528384	60.200001
2227.773050	613.240365	60.205006
2227.151264	563.238130	60.210010
2226.498779	507.966112	60.215015
2225.421091	475.486794	60.220020
2224.896547	427.289376	60.225025
2224.427391	375.663006	60.230030
2223.708551	341.707847	60.235034
2223.101353	297.709091	60.240039
2222.323276	262.423146	60.245044
2221.643662	207.735302	60.250049
2221.041270	177.682221	60.255054
2220.037887	147.489390	60.260058
2219.360875	95.739302	60.265063
2218.653720	77.189071	60.270068
2217.809245	32.733621	60.275073
2216.980941	11.827917	60.280078
2215.893565	-12.098947	60.285082
2213.310754	3.089198	60.290087
2208.981306	94.982589	60.295092
2209.364873	106.508686	60.300097
2210.642010	98.010112	60.305102
2211.575585	95.365817	60.310106
2211.486664	87.222708	60.315111
2210.027696	97.322270	60.320116
2210.289226	88.497547	60.325121
2209.450216	83.877914	60.330126
2208.498095	96.547816	60.335130
2207.784702	83.164442	60.340135
2206.788494	100.885787	60.345140
2205.860923	100.093103	60.350145
2205.219080	89.368039	60.355150
2204.838360	96.004033	60.360154
2204.129628	94.924334	60.365159
2203.002017	98.420967	60.370164
2202.850257	101.277124	60.375169
2202.344165	110.099650	60.380174
2201.773249	111.087461	60.385178
2201.237354	97.073551	60.390183
2200.434250	106.753708	60.395188
2199.921643	98.635228	60.400193
2199.678778	107.278808	60.405198
2198.485348	106.373764	60.410202
2197.824336	99.165034	60.415207
2196.945498	110.710047	60.420212
2196.226672	103.773826	60.425217
2195.820577	93.995340	60.430222
2195.184681	100.528319	60.435226
2194.938807	105.009404	60.440231
2194.102856	107.743871	60.445236
2193.372653	113.077616	60.450241
2192.600057	97.185342	60.455246
2191.514655	101.118389	60.460250
2191.385308	96.231647	60.465255
2191.044390	103.749117	60.470260
2190.608200	103.411475	60.475265
2189.521592	98.588281	60.480270
2188.667571	104.422614	60.485274
2188.408000	101.601748	60.490279
2187.236728	108.435694	60.495284
2186.640532	116.629150	60.500289
2186.128063	97.772069	60.505294
2184.864003	103.624143	60.510298
2184.703262	95.164435	60.515303
2183.761382	109.406458	60.520308
2183.810747	101.977812	60.525313
2183.508062	106.483678	60.530318
2182.475642	110.086641	60.535322
2181.287794	98.445297	60.540327
2180.834937	100.325822	60.545332
2180.128707	105.614764	60.550337
2179.813577	103.416120	60.555342
2178.902528	103.426611	60.560346
2178.322765	99.248384	60.565351
2177.311303	112.943233	60.570356
2176.583928	107.883289	60.575361
2176.293442	105.157210	60.580366
2175.142490	111.290956	60.585370
2175.537916	112.816148	60.590375
2174.430690	108.844592	60.595380
2173.240443	109.047605	60.600385
2173.348122	98.085375	60.605390
2172.831637	105.969728	60.610394
2171.812424	110.261275	60.615399
2170.708952	108.127773	60.620404
2170.654277	105.518820	60.625409
2170.343769	101.961747	60.630414
2168.719890	112.450183	60.635418
2168.493552	104.238987	60.640423
2168.167439	106.868926	60.645428
2167.507676	111.078221	60.650433
2166.186834	104.666428	60.655438
2165.429913	105.166537	60.660442
2165.820492	97.779953	60.665447
2164.236895	117.787955	60.670452
2164.156765	106.350911	60.675457
2163.443248	105.341365	60.680462
2162.042107	113.380261	60.685466
2161.902214	108.922526	60.690471
2161.414108	109.419413	60.695476
2160.638870	102.161009	60.700481
2159.927765	116.856843	60.705486
2159.472559	108.054355	60.710490
2158.830005	102.465322	60.715495
2157.352154	113.917726	60.720500
2157.236659	112.414356	60.725505
2157.150955	106.309643	60.730510
2156.062427	106.652638	60.735514
2154.886582	110.210559	60.740519
2154.656283	118.636119	60.745524
2154.293408	99.058333	60.750529
2153.161972	120.790679	60.755534
2152.545405	113.912359	60.760538
2152.462641	108.348051	60.765543
2151.142376	111.875272	60.770548
2150.288070	112.247338	60.775553
2150.362305	106.408976	60.780558
2149.868057	117.519267	60.785562
2148.491301	110.636979	60.790567
2147.706361	108.206958	60.795572
2147.730033	108.509118	60.800577
2147.056976	101.199817	60.805582
2145.752881	108.363920	60.810586
2145.461071	111.480408	60.815591
2144.630547	111.416637	60.820596
2144.223627	97.498974	60.825601
2143.469396	99.711157	60.830606
2142.539318	108.324999	60.835610
2142.540835	92.305209	60.840615
2141.957049	107.542206	60.845620
2141.073158	110.419907	60.850625
2140.569985	105.168294	60.855630
2139.866502	107.217892	60.860634
2139.482818	100.520245	60.865639
2138.078616	107.936765	60.870644
2137.043244	108.399061	60.875649
2137.107113	100.797814	60.880654
2136.211341	114.239364	60.885658
2135.862791	98.595216	60.890663
2134.689204	105.842690	60.895668
2134.006275	111.712971	60.900673
2133.360890	108.092343	60.905678
2133.070171	107.723747	60.910682
2132.535104	105.320316	60.915687
2131.498970	111.986194	60.920692
2130.935439	105.329695	60.925697
2130.517917	98.183277	60.930702
2129.821079	108.945677	60.935706
2129.461082	112.541319	60.940711
2128.581773	109.216414	60.945716
2127.863151	113.092872	60.950721
2127.580927	112.964192	60.955726
2125.998336	115.246307	60.960730
2125.381802	102.885172	60.965735
2125.477358	109.617493	60.970740
2124.443998	105.921234	60.975745
2123.371384	109.338215	60.980750
2122.845622	107.232918	60.985754
2122.170090	101.355828	60.990759
2121.476118	105.966356	60.995764
2121.544955	110.156250	61.000769
2120.890756	106.259493	61.005774
2119.699209	105.988094	61.010778
2119.558171	105.822822	61.015783
2119.141520	108.631127	61.020788
2118.076444	104.427416	61.025793
2117.245153	93.295643	61.030798
2115.937353	104.612272	61.035802
2115.337233	99.245168	61.040807
2115.433316	105.168462	61.045812
2114.812661	105.978110	61.050817
2113.869419	102.396863	61.055822
2112.973980	108.693508	61.060826
2112.769642	102.199212	61.065831
2112.209167	114.092683	61.070836
2111.418891	104.463473	61.075841
2111.096454	99.848638	61.080846
2110.049846	109.524873	61.085850
2108.961439	98.380280	61.090855
2108.013503	98.229499	61.095860
2107.992558	111.259447	61.100865
2107.680399	96.694431	61.105870
2106.559408	107.516247	61.110874
2106.035250	95.591456	61.115879
2105.180351	105.998907	61.120884
2104.615907	97.142814	61.125889
2104.447405	101.206366	61.130894
2103.898812	101.380138	61.135898
2103.315806	96.341468	61.140903
2101.807509	106.160341	61.145908
2101.234421	101.069637	61.150913
2100.625122	91.624604	61.155918
2099.239779	105.954349	61.160922
2099.208019	99.215064	61.165927
2098.715172	94.127400	61.170932
2098.026630	96.291325	61.175937
2097.708394	97.202796	61.180942
2097.179241	104.740676	61.185946
2096.702864	97.151040	61.190951
2095.423201	94.794805	61.195956
2094.768310	107.089588	61.200961
2093.948922	98.078416	61.205966
2093.399852	107.139571	61.210970
2093.076596	102.581636	61.215975
2092.410821	107.693875	61.220980
2091.836786	102.226448	61.225985
2091.374612	98.702914	61.230990
2089.961608	103.337655	61.235994
2089.177499	100.134850	61.240999
2088.292611	105.015363	61.246004
2088.164462	100.328705	61.251009
2087.734971	100.288048	61.256014
2087.052650	104.950347	61.261018
2086.668661	110.151912	61.266023
2085.996602	106.130271	61.271028
2085.142344	112.628539	61.276033
2084.140372	111.685284	61.281038
2083.101328	101.471115	61.286042
2082.862802	97.599874	61.291047
2082.586391	105.627485	61.296052
2081.761177	113.652298	61.301057
2081.749007	94.067781	61.306062
2080.106267	99.117429	61.311066
2079.222154	89.818508	61.316071
2078.562113	106.910980	61.321076
2078.357538	94.618536	61.326081
2077.427328	110.924444	61.331086
2076.523244	113.833752	61.336090
2076.364186	97.404228	61.341095
2075.837864	89.552880	61.346100
2075.331564	95.622210	61.351105
2075.131908	102.062336	61.356110
2074.117017	92.126607	61.361114
2073.116846	89.194626	61.366119
2072.043198	96.006810	61.371124
2071.332370	86.633092	61.376129
2071.213905	89.111822	61.381134
2070.312858	92.465327	61.386138
2070.156626	84.854865	61.391143
2069.478291	87.968035	61.396148
2068.639056	94.290458	61.401153
2067.799155	92.280753	61.406158
2066.968270	97.808682	61.411162
2066.663188	88.865721	61.416167
2066.260399	103.312364	61.421172
2065.673284	107.227888	61.426177
2064.180831	86.159477	61.431182
2063.419947	96.594587	61.436186
2062.949637	86.217655	61.441191
2062.337016	88.911987	61.446196
2061.615404	97.196310	61.451201
2061.242512	90.673583	61.456206
2060.519923	91.721758	61.461210
2060.155163	84.723102	61.466215
2059.734228	92.412534	61.471220
2058.476463	99.758542	61.476225
2057.554355	87.778656	61.481230
2056.551749	94.320963	61.486234
2056.558690	85.049385	61.491239
2056.168176	88.419646	61.496244
2055.491300	85.059498	61.501249
2055.134730	82.496883	61.506254
2054.082074	91.358837	61.511258
2053.294885	88.760480	61.516263
2052.468425	81.478718	61.521268
2051.425625	91.017166	61.526273
2051.185576	83.301742	61.531278
2050.871253	92.152185	61.536282
2050.851505	82.810731	61.541287
2049.799921	86.358431	61.546292
2048.772346	92.176184	61.551297
2048.265927	82.990802	61.556302
2047.414482	88.682838	61.561306
2046.922434	90.134381	61.566311
2045.906392	97.828371	61.571316
2044.810936	95.614809	61.576321
2044.418488	83.891488	61.581326
2043.507263	93.574633	61.586330
2043.216839	81.194911	61.591335
2042.995036	84.491094	61.596340
2042.341645	94.248436	61.601345
2042.307316	86.438868	61.606350
2040.782473	93.008862	61.611354
2040.046095	83.949857	61.616359
2039.164870	101.186229	61.621364
2038.571165	90.329012	61.626369
2038.294367	87.853084	61.631374
2037.600019	97.385127	61.636378
2037.420697	84.934158	61.641383
2036.144566	90.493328	61.646388
2035.041219	93.495765	61.651393
2035.070092	87.759226	61.656398
2034.182312	92.540865	61.661402
2033.689508	98.947089	61.666407
2032.958524	100.463360	61.671412
2032.027548	94.071777	61.676417
2031.376281	88.848430	61.681422
2030.594580	86.846848	61.686426
2030.184236	86.096720	61.691431
2030.046071	88.567539	61.696436
2029.135019	87.532612	61.701441
2028.165125	90.920707	61.706446
2026.997253	92.711306	61.711450
2026.674603	96.810359	61.716455
2026.135041	83.129829	61.721460
2025.585587	90.669354	61.726465
2024.992398	88.462824	61.731470
2024.359301	95.011153	61.736474
2024.096883	83.874301	61.741479
2023.086930	96.294813	61.746484
2021.833415	93.950235	61.751489
2021.692056	87.564230	61.756494
2020.977861	93.642905	61.761498
2020.857652	88.234363	61.766503
2019.900936	88.564379	61.771508
2018.583289	89.350624	61.776513
2018.135090	84.328434	61.781518
2017.355771	90.042146	61.786522
2017.193151	82.855310	61.791527
2016.845953	83.683080	61.796532
2015.977763	87.614831	61.801537
2015.063770	93.042426	61.806542
2013.807958	89.923969	61.811546
2013.873855	92.256753	61.816551
2013.617754	92.760999	61.821556
2012.471738	84.667411	61.826561
2011.607278	84.856638	61.831566
2010.283727	95.327438	61.836570
2010.138424	86.835351	61.841575
2010.037808	86.021881	61.846580
2009.104060	81.565583	61.851585
2009.205624	79.693479	61.856590
2008.085296	82.574046	61.861594
2006.844967	82.255250	61.866599
2006.302832	86.917389	61.871604
2005.721199	87.258842	61.876609
2005.524919	77.514925	61.881614
2004.874078	90.518656	61.886618
2003.834546	80.678340	61.891623
2003.166600	79.738875	61.896628
2002.297754	83.544583	61.901633
2001.953054	78.775619	61.906638
2001.273274	82.697970	61.911642
2000.656182	78.860018	61.916647
1999.890343	82.360810	61.921652
1998.747715	84.253064	61.926657
1998.399752	77.586057	61.931662
1997.909226	90.693650	61.936666
1997.443689	85.874479	61.941671
1996.936966	88.641900	61.946676
1995.919264	80.075395	61.951681
1995.301921	82.259581	61.956686
1994.270311	89.801518	61.961690
1994.028344	82.026488	61.966695
1993.412016	81.438362	61.971700
1992.339863	83.152284	61.976705
1991.644524	84.554103	61.981710
1990.871910	82.196294	61.986714
1990.598516	92.147211	61.991719
1990.048883	93.311451	61.996724
1989.715466	87.687604	62.001729
1989.295941	82.339186	62.006734
1988.066461	91.994009	62.011738
1987.145185	86.301044	62.016743
1986.707253	88.297493	62.021748
1985.768196	92.117504	62.026753
1985.606823	83.719431	62.031758
1984.892796	87.948407	62.036762
1983.257622	89.447353	62.041767
1982.763073	85.056971	62.046772
1982.237877	94.090688	62.051777
1981.723923	86.716776	62.056782
1981.150302	93.135830	62.061786
1980.981645	87.061655	62.066791
1980.603891	80.129733	62.071796
1979.941447	85.347109	62.076801
1979.150261	79.456892	62.081806
1978.118348	83.897161	62.086810
1977.353835	78.718615	62.091815
1977.078309	86.331357	62.096820
1975.413210	89.706812	62.101825
1975.047390	86.516504	62.106830
1974.635722	86.146623	62.111834
1973.708876	77.191990	62.116839
1973.525464	78.539369	62.121844
1972.862444	84.677734	62.126849
1972.636354	80.309399	62.131854
1971.996461	82.555513	62.136858
1970.949709	80.905086	62.141863
1970.173442	87.367340	62.146868
1969.310931	92.466671	62.151873
1969.150161	82.561010	62.156878
1968.354565	82.822895	62.161882
1967.230763	87.091683	62.166887
1966.757272	83.267215	62.171892
1965.794470	84.025550	62.176897
1965.739557	86.259240	62.181902
1965.197140	89.093830	62.186906
1964.276564	78.827819	62.191911
1963.620204	80.546718	62.196916
1962.360938	92.689860	62.201921
1961.924859	85.144330	62.206926
1961.521092	89.677287	62.211930
1961.079903	87.385149	62.216935
1960.884052	81.447753	62.221940
1959.418944	92.243799	62.226945
1958.973856	87.774612	62.231950
1958.051074	88.386255	62.236954
1957.799738	81.200895	62.241959
1957.521735	85.772234	62.246964
1956.585173	86.102227	62.251969
1955.774397	86.426447	62.256974
1954.948479	87.904192	62.261978
1954.501666	87.314399	62.266983
1953.529034	80.672436	62.271988
1952.506746	89.491754	62.276993
1951.790334	88.243042	62.281998
1951.440910	83.343955	62.287002
1950.900914	85.705099	62.292007
1950.668118	81.586977	62.297012
1950.163076	86.416694	62.302017
1949.516994	78.888734	62.307022
1948.328411	93.728160	62.312026
1947.919119	89.876159	62.317031
1947.480813	76.430315	62.322036
1946.239552	91.401097	62.327041
1945.258559	81.322871	62.332046
1944.727123	87.563352	62.337050
1944.369602	91.844555	62.342055
1944.052763	81.194155	62.347060
1943.263851	93.958050	62.352065
1942.903987	83.737081	62.357070
1941.602994	90.258978	62.362074
1940.564304	86.696107	62.367079
1940.598304	90.601367	62.372084
1939.752032	91.292331	62.377089
1939.664763	84.030470	62.382094
1938.253976	93.803973	62.387098
1937.655227	92.478244	62.392103
1937.330851	97.006489	62.397108
1936.569727	90.763021	62.402113
1936.390488	81.502087	62.407118
1935.007735	87.455096	62.412122
1934.065624	93.926339	62.417127
1933.662951	86.334514	62.422132
1933.157655	89.773469	62.427137
1932.717985	84.691600	62.432142
1932.244257	87.004383	62.437146
1931.425745	91.166382	62.442151
1930.752612	86.148377	62.447156
1929.907857	88.989965	62.452161
1929.703862	87.984760	62.457166
1928.336120	93.085454	62.462170
1927.694824	81.568816	62.467175
1927.459824	80.224774	62.472180
1926.755512	85.117662	62.477185
1926.386502	80.101846	62.482190
1925.261700	90.744545	62.487194
1924.762280	81.589628	62.492199
1924.136959	77.648930	62.497204
1923.242928	89.833451	62.502209
1922.858414	81.548076	62.507214
1921.698509	86.893310	62.512218
1920.875267	92.087341	62.517223
1920.257096	71.113665	62.522228
1919.502306	84.053479	62.527233
1919.687345	86.359462	62.532238
1919.192306	79.935002	62.537242
1918.568904	89.935168	62.542247
1917.866249	85.535259	62.547252
1916.547964	87.471199	62.552257
1916.148683	89.759553	62.557262
1914.843968	93.574555	62.562266
1913.719455	89.597985	62.567271
1914.191982	87.763182	62.572276
1913.368576	88.291261	62.577281
1912.852480	79.561598	62.582286
1912.490709	94.761774	62.587290
1911.932994	82.481281	62.592295
1910.975353	84.074560	62.597300
1910.062977	88.068545	62.602305
1909.754926	84.143716	62.607310
1908.662136	87.571858	62.612314
1907.635861	92.334519	62.617319
1907.420072	84.968489	62.622324
1906.466088	99.122596	62.627329
1906.349392	85.428594	62.632334
1905.742781	95.596403	62.637338
1905.072043	88.381435	62.642343
1904.398721	90.065195	62.647348
1903.301701	91.250116	62.652353
1902.862539	88.651753	62.657358
1902.510053	84.218339	62.662362
1901.547881	95.264143	62.667367
1900.966581	79.563998	62.672372
1899.999130	89.907350	62.677377
1899.662787	81.570182	62.682382
1898.987386	95.780983	62.687386
1897.954561	86.917316	62.692391
1897.330796	77.685958	62.697396
1896.916583	96.453469	62.702401
1896.531144	89.680469	62.707406
1895.955923	95.305044	62.712410
1894.791527	92.222595	62.717415
1893.933893	90.622599	62.722420
1893.460696	79.877190	62.727425
1892.981535	85.018181	62.732430
1892.373780	82.687847	62.737434
1891.697803	90.353124	62.742439
1890.809124	92.244532	62.747444
1889.884857	100.133724	62.752449
1889.814347	91.183523	62.757454
1889.299763	89.010277	62.762458
1888.635701	94.828721	62.767463
1887.479940	92.449769	62.772468
1886.595446	89.285046	62.777473
1886.187579	88.525088	62.782478
1885.950956	73.560254	62.787482
1885.142663	85.049958	62.792487
1884.750278	83.869670	62.797492
1883.306694	87.514351	62.802497
1883.042449	86.397296	62.807502
1882.718490	84.255289	62.812506
1881.902754	81.530641	62.817511
1881.004897	78.125205	62.822516
1880.222432	77.289105	62.827521
1879.665550	86.971222	62.832526
1879.567821	81.300522	62.837530
1878.537839	86.394923	62.842535
1877.734080	84.232897	62.847540
1876.825601	100.073351	62.852545
1876.549128	94.472020	62.857550
1876.214547	83.550075	62.862554
1874.866529	90.664486	62.867559
1874.032261	78.118845	62.872564
1873.148110	81.408227	62.877569
1872.720336	82.860634	62.882574
1872.364345	88.832011	62.887578
1872.069169	91.665212	62.892583
1872.135017	82.765907	62.897588
1870.558579	91.840371	62.902593
1870.155768	80.377355	62.907598
1869.600092	93.892671	62.912602
1868.713477	84.152718	62.917607
1868.033899	73.793306	62.922612
1866.943803	96.654455	62.927617
1866.701188	81.482422	62.932622
1865.532833	81.030847	62.937626
1864.757700	79.173348	62.942631
1864.474877	77.005892	62.947636
1863.627166	91.144705	62.952641
1863.077639	81.067404	62.957646
1863.081232	79.978789	62.962650
1862.008337	81.814299	62.967655
1861.366414	85.399527	62.972660
1860.437186	86.781743	62.977665
1860.049608	84.022243	62.982670
1859.644418	81.811139	62.987674
1858.156028	90.250341	62.992679
1857.746426	95.355067	62.997684
1857.172916	86.175660	63.002689
1856.920342	77.407332	63.007694
1856.163889	77.191552	63.012698
1855.286870	82.912925	63.017703
1854.746374	77.249447	63.022708
1854.030648	84.421169	63.027713
1853.554172	81.959622	63.032718
1852.719309	76.107924	63.037722
1851.229517	76.823815	63.042727
1850.975789	69.198911	63.047732
1850.350707	90.283203	63.052737
1850.073089	86.495469	63.057742
1849.735909	93.299607	63.062746
1849.255650	82.277801	63.067751
1848.272258	79.346405	63.072756
1847.198881	83.324971	63.077761
1846.864074	84.054605	63.082766
1846.325106	77.369071	63.087770
1845.122476	86.165013	63.092775
1844.655707	75.886934	63.097780
1844.025080	80.522146	63.102785
1843.803462	75.915012	63.107790
1843.107471	84.382947	63.112794
1842.212221	94.202369	63.117799
1841.657779	86.098523	63.122804
1840.603903	85.497904	63.127809
1840.109089	79.776716	63.132814
1839.164257	75.765350	63.137818
1838.134431	81.066309	63.142823
1838.114490	72.699425	63.147828
1837.602970	77.990630	63.152833
1837.137765	71.604035	63.157838
1836.845083	83.213724	63.162842
1835.397927	76.207206	63.167847
1834.821702	81.237463	63.172852
1834.020366	82.623036	63.177857
1833.643611	80.377461	63.182862
1832.771320	85.989286	63.187866
1831.925074	76.416401	63.192871
1831.589498	72.764026	63.197876
1830.791714	75.019469	63.202881
1830.593266	87.604477	63.207886
1829.134720	86.752736	63.212890
1828.602753	75.784880	63.217895
1828.140337	77.039377	63.222900
1827.287025	76.969864	63.227905
1827.041491	81.261678	63.232910
1826.885461	84.339281	63.237914
1825.856460	86.659821	63.242919
1825.038712	79.390958	63.247924
1824.519830	86.575586	63.252929
1823.910784	79.180553	63.257934
1822.719160	77.808643	63.262938
1822.131763	80.555785	63.267943
1821.703667	74.639516	63.272948
1821.026650	75.056076	63.277953
1820.660928	77.920978	63.282958
1819.944107	80.168301	63.287962
1818.856464	87.422735	63.292967
1818.785062	75.525514	63.297972
1817.512432	76.877115	63.302977
1816.727433	78.547089	63.307982
1816.346957	88.229589	63.312986
1815.829283	83.054481	63.317991
1815.497083	69.369499	63.322996
1814.113430	90.287243	63.328001
1813.378141	78.258898	63.333006
1812.787700	75.722419	63.338010
1812.157419	76.937343	63.343015
1811.951284	78.810284	63.348020
1811.415763	78.926849	63.353025
1810.426233	79.471875	63.358030
1809.992183	86.985217	63.363034
1809.095151	90.487966	63.368039
1808.917186	83.902809	63.373044
1807.555671	78.218322	63.378049
1806.693206	87.228336	63.383054
1806.474552	80.085120	63.388058
1805.750365	84.270018	63.393063
1805.277021	86.641105	63.398068
1804.048360	84.390457	63.403073
1803.962146	84.995474	63.408078
1803.398395	91.225338	63.413082
1802.715672	86.732418	63.418087
1802.219830	84.015348	63.423092
1800.847488	87.368076	63.428097
1800.481600	86.208824	63.433102
1799.985312	84.802209	63.438106
1799.156725	79.875159	63.443111
1798.117814	85.696368	63.448116
1797.367962	82.797292	63.453121
1797.022519	79.912848	63.458126
1796.741615	86.864161	63.463130
1796.097771	86.964815	63.468135
1795.785752	71.389113	63.473140
1794.665632	86.452659	63.478145
1793.923900	79.986982	63.483150
1793.633616	81.253575	63.488154
1792.221461	79.738509	63.493159
1791.488211	73.503290	63.498164
1790.712751	80.843772	63.503169
1790.228750	67.714309	63.508174
1790.184015	69.556892	63.513178
1789.608278	78.478800	63.518183
1789.210516	79.626848	63.523188
1788.190997	81.679404	63.528193
1787.691534	91.368186	63.533198
1786.492551	82.948831	63.538202
1785.208384	89.159054	63.543207
1784.630864	74.688323	63.548212
1784.243018	88.823509	63.553217
1784.139120	84.517794	63.558222
1783.872291	93.817995	63.563226
1783.250455	90.518568	63.568231
1782.334879	83.809276	63.573236
1781.546277	85.634366	63.578241
1780.999149	87.339117	63.583246
1779.942083	81.060704	63.588250
1779.059502	84.725161	63.593255
1778.450953	81.852538	63.598260
1778.023424	95.183518	63.603265
1777.770492	82.200272	63.608270
1777.045958	85.267229	63.613274
1775.991820	90.769181	63.618279
1775.705885	76.171732	63.623284
1774.975631	82.943672	63.628289
1773.583817	85.722369	63.633294
1772.738312	83.030869	63.638298
1772.185994	88.918316	63.643303
1772.026990	76.689676	63.648308
1771.571835	88.992186	63.653313
1771.249612	83.363450	63.658318
1770.696097	83.610608	63.663322
1769.489617	83.038980	63.668327
1769.702646	74.978866	63.673332
1768.301121	79.488937	63.678337
1767.342747	79.308399	63.683342
1766.741719	75.690301	63.688346
1766.010801	82.295201	63.693351
1766.034338	73.375821	63.698356
1764.806048	84.763514	63.703361
1764.249531	87.108392	63.708366
1763.622713	79.050759	63.713370
1762.964701	82.189152	63.718375
1762.252650	68.944530	63.723380
1760.885740	85.176313	63.728385
1760.490258	81.126627	63.733390
1760.190794	87.076420	63.738394
1759.828248	85.367891	63.743399
1759.255287	82.806573	63.748404
1758.309872	90.450008	63.753409
1757.419004	86.352836	63.758414
1756.430540	82.122938	63.763418
1756.100537	85.849457	63.768423
1755.961241	81.103111	63.773428
1754.441546	87.002258	63.778433
1754.273679	86.369782	63.783438
1753.780962	86.015960	63.788442
1752.980045	86.841700	63.793447
1752.870201	74.789753	63.798452
1751.837421	88.003963	63.803457
1750.945181	87.290984	63.808462
1750.472277	74.970278	63.813466
1749.694320	85.190537	63.818471
1748.903694	76.676399	63.823476
1747.984137	88.775127	63.828481
1747.556071	88.754799	63.833486
1747.483715	77.121077	63.838490
1746.670781	81.905101	63.843495
1745.525626	66.458569	63.848500
1744.619530	88.044776	63.853505
1744.508787	83.584041	63.858510
1744.234421	70.211576	63.863514
1742.859306	81.728240	63.868519
1742.118360	83.192554	63.873524
1741.396498	83.729790	63.878529
1740.955880	85.346674	63.883534
1740.761069	82.033062	63.888538
1740.070765	88.243609	63.893543
1739.487118	76.500282	63.898548
1738.747505	80.324964	63.903553
1737.610780	78.321511	63.908558
1736.729186	80.268608	63.913562
1735.811843	88.511533	63.918567
1735.503128	79.952405	63.923572
1735.187987	82.375646	63.928577
1734.741815	69.429417	63.933582
1734.327149	74.038236	63.938586
1733.375437	79.659545	63.943591
1732.983927	75.304898	63.948596
1731.751699	79.412805	63.953601
1730.534163	83.661876	63.958606
1730.109929	77.915316	63.963610
1729.301443	90.411128	63.968615
1729.261727	77.215851	63.973620
1728.763491	87.222968	63.978625
1728.464657	78.640198	63.983630
1727.491269	86.696491	63.988634
1726.833949	76.604818	63.993639
1726.204382	82.293236	63.998644
1725.210793	91.136446	64.003649
1724.006523	80.343194	64.008654
1723.678538	70.555598	64.013658
1723.058585	80.973106	64.018663
1723.233932	79.540265	64.023668
1722.466640	86.261332	64.028673
1721.400383	83.384146	64.033678
1720.808201	78.473196	64.038682
1719.788655	81.315794	64.043687
1719.116000	81.457311	64.048692
1717.972322	79.037100	64.053697
1717.421055	81.789563	64.058702
1717.485195	83.461900	64.063706
1717.165683	85.729726	64.068711
1716.595458	79.285723	64.073716
1715.416587	82.347581	64.078721
1714.577220	80.210187	64.083726
1714.511237	69.516857	64.088730
1713.275142	82.216186	64.093735
1712.798651	76.146786	64.098740
1711.961191	80.469537	64.103745
1711.110792	92.591983	64.108750
1710.298687	80.273120	64.113754
1709.424980	82.341969	64.118759
1709.241588	77.957428	64.123764
1708.704660	80.173055	64.128769
1708.280858	81.954422	64.133774
1708.091842	81.743179	64.138778
1706.633347	86.461015	64.143783
1705.988705	78.447230	64.148788
1705.578228	81.809661	64.153793
1705.039028	91.840634	64.158798
1703.701507	83.028609	64.163802
1702.975966	81.357241	64.168807
1702.787165	71.504968	64.173812
1702.320828	76.837899	64.178817
1701.871864	84.445076	64.183822
1701.105099	79.974999	64.188826
1699.987207	84.086838	64.193831
1699.495696	74.735202	64.198836
1699.132152	79.127761	64.203841
1697.915315	72.174634	64.208846
1697.228584	80.125485	64.213850
1696.569043	80.454149	64.218855
1696.445706	75.862963	64.223860
1695.900546	69.489102	64.228865
1694.816666	73.727996	64.233870
1693.947413	74.788522	64.238874
1693.268595	78.237724	64.243879
1693.053114	77.750002	64.248884
1692.395096	69.583818	64.253889
1691.257263	81.636798	64.258894
1690.799293	76.835422	64.263898
1690.236244	77.708552	64.268903
1690.087342	77.050992	64.273908
1688.774529	81.368825	64.278913
1688.061860	75.851003	64.283918
1687.871876	81.497995	64.288922
1687.095348	87.583482	64.293927
1686.321882	87.794631	64.298932
1685.068133	85.346187	64.303937
1684.000180	79.873755	64.308942
1684.164981	78.185557	64.313946
1683.240658	84.466395	64.318951
1683.018027	81.781650	64.323956
1682.691539	86.034293	64.328961
1682.137160	79.414327	64.333966
1681.369892	74.625810	64.338970
1680.393679	79.995573	64.343975
1680.025240	85.661448	64.348980
1678.730449	78.354876	64.353985
1678.093602	79.236576	64.358990
1677.759250	66.829243	64.363994
1677.295140	78.857217	64.368999
1676.551655	80.339297	64.374004
1675.520296	71.109682	64.379009
1675.183087	82.308569	64.384014
1674.720762	77.969911	64.389018
1673.726477	76.606151	64.394023
1672.891517	78.113799	64.399028
1672.586601	72.712560	64.404033
1672.039024	73.873381	64.409038
1671.201230	71.609603	64.414042
1670.173595	77.306063	64.419047
1669.785860	79.310353	64.424052
1668.904852	72.311787	64.429057
1668.421328	80.856385	64.434062
1667.665686	75.348549	64.439066
1666.966137	74.975560	64.444071
1666.531553	82.094779	64.449076
1666.401195	80.103395	64.454081
1665.035855	86.033262	64.459086
1664.430838	72.964056	64.464090
1663.655113	77.406316	64.469095
1663.153976	75.376059	64.474100
1662.864443	73.425728	64.479105
1661.564570	78.408534	64.484110
1661.168592	66.835697	64.489114
1660.410850	85.698745	64.494119
1660.270328	78.606218	64.499124
1659.176053	77.878056	64.504129
1658.144047	82.873509	64.509134
1658.010364	79.094481	64.514138
1657.193193	83.620595	64.519143
1656.717294	80.052033	64.524148
1655.576645	76.920202	64.529153
1654.879735	81.338909	64.534158
1654.808636	77.824317	64.539162
1653.774132	86.651967	64.544167
1654.068779	80.824354	64.549172
1652.499732	76.160044	64.554177
1651.944507	74.732861	64.559182
1651.455866	73.717704	64.564186
1650.144460	88.877902	64.569191
1649.693574	85.355827	64.574196
1648.941691	86.733599	64.579201
1648.382757	90.947477	64.584206
1648.532344	76.205195	64.589210
1647.600826	87.526868	64.594215
1646.712007	80.767656	64.599220
1646.094439	87.457074	64.604225
1645.311996	87.318019	64.609230
1644.909564	77.515455	64.614234
1643.785938	84.777238	64.619239
1643.049789	85.356192	64.624244
1642.549800	90.398028	64.629249
1641.972552	91.949902	64.634254
1641.828134	72.768121	64.639258
1640.754834	85.219279	64.644263
1640.300008	81.497571	64.649268
1639.611577	86.854751	64.654273
1638.035808	85.163920	64.659278
1637.528811	82.830262	64.664282
1636.858311	87.137553	64.669287
1636.659297	76.744467	64.674292
1636.103511	73.776774	64.679297
1635.456137	84.685903	64.684302
1635.351799	93.023631	64.689306
1634.388112	86.109165	64.694311
1633.771512	79.607900	64.699316
1633.187109	83.357494	64.704321
1631.881102	79.409890	64.709326
1631.597726	78.789463	64.714330
1630.880347	92.655314	64.719335
1630.329775	82.444218	64.724340
1628.979354	78.104723	64.729345
1628.227433	86.542159	64.734350
1627.893199	79.734283	64.739354
1627.443586	81.224886	64.744359
1627.040198	79.784628	64.749364
1626.894384	83.248523	64.754369
1625.659957	89.607022	64.759374
1625.406915	71.007024	64.764378
1624.042222	84.013801	64.769383
1623.321423	79.509642	64.774388
1622.665331	70.166830	64.779393
1622.353445	80.464454	64.784398
1622.098774	84.223170	64.789402
1620.748464	86.047651	64.794407
1620.062665	86.941872	64.799412
1619.637894	79.410403	64.804417
1618.950553	82.648099	64.809422
1618.132580	81.278429	64.814426
1617.143366	82.156196	64.819431
1617.041702	66.580251	64.824436
1616.518950	70.215978	64.829441
1615.653544	84.819660	64.834446
1615.249245	73.006892	64.839450
1613.948743	87.064713	64.844455
1613.478539	83.167266	64.849460
1613.133990	87.071141	64.854465
1612.408056	83.597498	64.859470
1611.547397	68.681410	64.864474
1610.813484	78.552513	64.869479
1610.746789	84.552063	64.874484
1610.126136	77.516892	64.879489
1608.796022	78.737382	64.884494
1608.483348	76.607816	64.889498
1607.728642	86.324540	64.894503
1606.795965	81.792546	64.899508
1606.059114	69.439708	64.904513
1605.573528	75.220384	64.909518
1605.025389	70.173170	64.914522
1604.128993	82.138940	64.919527
1603.717861	83.215025	64.924532
1603.420181	77.021059	64.929537
1602.227551	73.167420	64.934542
1601.936796	70.152903	64.939546
1600.990868	78.302632	64.944551
1600.525884	78.365459	64.949556
1599.364321	80.279809	64.954561
1598.582790	77.912505	64.959566
1598.564875	72.131391	64.964570
1597.901093	78.965343	64.969575
1597.189180	77.353339	64.974580
1596.533861	74.480311	64.979585
1595.657448	81.718607	64.984590
1595.238966	68.499956	64.989594
1594.575466	80.521766	64.994599
1593.524898	76.465799	64.999604
1592.745009	69.794959	65.004609
1592.025542	82.774937	65.009614
1592.106362	72.752126	65.014618
1591.402906	79.489885	65.019623
1591.121748	66.317227	65.024628
1590.416135	67.012763	65.029633
1589.309564	77.666852	65.034638
1588.561483	73.152849	65.039642
1587.559373	75.251595	65.044647
1587.087552	70.212761	65.049652
1586.528327	72.133923	65.054657
1585.823523	85.925240	65.059662
1585.363468	84.807787	65.064666
1584.224147	77.437150	65.069671
1583.840299	75.153324	65.074676
1583.373877	73.131761	65.079681
1583.201024	79.121366	65.084686
1582.241251	72.412878	65.089690
1581.087314	79.774109	65.094695
1580.653377	81.342649	65.099700
1580.007740	74.477029	65.104705
1578.823757	69.005738	65.109710
1578.487038	71.110737	65.114714
1578.056624	85.367792	65.119719
1577.694271	75.383847	65.124724
1576.798291	70.212137	65.129729
1575.789627	79.885635	65.134734
1575.435257	78.311448	65.139738
1574.976368	74.237183	65.144743
1574.096201	79.293692	65.149748
1573.438412	82.189253	65.154753
1572.727561	85.367620	65.159758
1572.211181	74.629173	65.164762
1570.866198	74.700929	65.169767
1570.166939	70.272212	65.174772
1570.012073	68.286308	65.179777
1569.378184	84.685538	65.184782
1569.073113	71.169769	65.189786
1567.870876	71.759715	65.194791
1567.336363	71.133465	65.199796
1566.787456	74.929466	65.204801
1566.346009	81.734410	65.209806
1565.597717	74.620189	65.214810
1564.564497	81.873943	65.219815
1563.791050	86.804700	65.224820
1563.455176	74.022338	65.229825
1563.050781	74.386189	65.234830
1562.400042	76.616770	65.239834
1561.197806	95.301310	65.244839
1560.662212	85.173006	65.249844
1560.642441	85.318066	65.254849
1559.636176	89.046392	65.259854
1558.685101	76.237195	65.264858
1557.915107	92.752671	65.269863
1557.783989	87.719630	65.274868
1557.152008	87.026869	65.279873
1555.853727	85.490689	65.284878
1555.302785	76.911742	65.289882
1554.786521	84.107023	65.294887
1554.378633	79.865394	65.299892
1553.557373	82.184566	65.304897
1552.423961	89.853195	65.309902
1552.190035	76.654112	65.314906
1551.632708	86.465637	65.319911
1550.949671	80.582048	65.324916
1550.207507	79.212972	65.329921
1549.191268	72.086138	65.334926
1548.925389	81.226916	65.339930
1548.653320	74.287763	65.344935
1547.369722	79.189191	65.349940
1546.898360	72.418890	65.354945
1546.070367	83.140695	65.359950
1546.245170	72.265638	65.364954
1544.760944	75.666224	65.369959
1544.060142	76.878221	65.374964
1543.547321	83.264022	65.379969
1543.062764	91.539157	65.384974
1542.859926	75.348545	65.389978
1541.665472	78.146460	65.394983
1540.784400	85.511662	65.399988
1540.636472	87.965122	65.404993
1539.660381	90.901803	65.409998
1538.671842	74.211584	65.415002
1537.914780	73.781539	65.420007
1537.518898	89.300914	65.425012
1537.500013	78.795653	65.430017
1536.792970	79.584466	65.435022
1535.713619	71.986720	65.440026
1534.759616	80.005294	65.445031
1534.302393	76.714476	65.450036
1533.942881	84.953972	65.455041
1533.204483	75.532806	65.460046
1532.487566	81.380209	65.465050
1531.986507	81.187020	65.470055
1530.990476	77.792586	65.475060
1530.237591	79.790258	65.480065
1529.639289	82.275853	65.485070
1529.038440	77.449908	65.490074
1528.806918	85.505075	65.495079
1527.640402	75.336692	65.500084
1527.125425	67.073726	65.505089
1526.070495	69.155656	65.510094
1526.167168	66.103248	65.515098
1525.193842	74.938556	65.520103
1524.224467	73.449478	65.525108
1523.533622	72.149523	65.530113
1523.013999	82.125360	65.535118
1522.813205	72.197759	65.540122
1521.926762	79.186944	65.545127
1521.200684	79.756447	65.550132
1520.691145	79.433727	65.555137
1519.875726	81.892323	65.560142
1519.252315	79.030015	65.565146
1518.396805	79.539663	65.570151
1517.638701	63.471987	65.575156
1517.625789	68.133682	65.580161
1516.119325	75.267111	65.585166
1515.729076	69.926766	65.590170
1515.077723	70.936958	65.595175
1514.560392	76.246475	65.600180
1514.247788	66.260955	65.605185
1512.970503	68.282032	65.610190
1512.534537	79.454033	65.615194
1511.831609	74.198060	65.620199
1511.752737	70.777750	65.625204
1511.057212	69.212052	65.630209
1509.616372	82.560536	65.635214
1509.185764	78.179031	65.640218
1508.516405	85.409682	65.645223
1508.011204	87.897834	65.650228
1507.354726	73.756708	65.655233
1506.201269	77.598319	65.660238
1506.074160	78.982507	65.665242
1505.659327	79.272336	65.670247
1504.860874	92.165541	65.675252
1504.177078	89.019532	65.680257
1503.375504	86.168190	65.685262
1502.912214	79.809754	65.690266
1501.998729	84.507323	65.695271
1501.095806	82.523596	65.700276
1500.743047	72.588607	65.705281
1500.238803	84.842156	65.710286
1498.998534	83.117025	65.715290
1498.210839	76.661913	65.720295
1497.482645	83.105595	65.725300
1497.293653	77.701734	65.730305
1496.646118	79.264806	65.735310
1496.518795	75.398056	65.740314
1495.643574	69.360534	65.745319
1494.528802	79.913461	65.750324
1494.142368	73.850307	65.755329
1493.715866	85.047616	65.760334
1493.074453	82.325362	65.765338
1492.002807	77.845459	65.770343
1491.390237	71.160685	65.775348
1491.092317	66.939444	65.780353
1489.963450	79.038364	65.785358
1489.120468	72.011755	65.790362
1488.485159	72.488000	65.795367
1488.042332	78.030097	65.800372
1487.675540	82.582456	65.805377
1487.072933	85.658493	65.810382
1486.538929	76.040873	65.815386
1485.757182	74.335926	65.820391
1484.898624	71.706525	65.825396
1483.877882	70.884757	65.830401
1483.269353	88.546192	65.835406
1483.126397	74.867495	65.840410
1482.515132	79.299437	65.845415
1481.598116	86.446451	65.850420
1480.607010	71.171128	65.855425
1480.071340	77.770289	65.860430
1479.889785	76.029893	65.865434
1479.013229	82.724222	65.870439
1478.024577	71.207767	65.875444
1477.707319	73.986162	65.880449
1476.739065	84.332898	65.885454
1476.578176	78.596586	65.890458
1475.942347	86.154634	65.895463
1474.637425	77.203540	65.900468
1474.570862	75.648287	65.905473
1473.544800	78.657580	65.910478
1472.716538	82.373418	65.915482
1471.823891	85.587005	65.920487
1471.353038	75.953047	65.925492
1470.909474	75.246136	65.930497
1470.738203	92.078043	65.935502
1470.144522	80.500398	65.940506
1469.194450	85.099717	65.945511
1468.657487	80.069682	65.950516
1467.513278	69.140896	65.955521
1466.740303	76.649775	65.960526
1466.150516	76.576349	65.965530
1465.705622	76.047836	65.970535
1465.259159	79.761348	65.975540
1464.387063	69.286035	65.980545
1463.740529	73.288368	65.985550
1463.151721	79.197424	65.990554
1462.698959	80.054653	65.995559
1461.533900	74.725484	66.000564
1460.989598	70.931309	66.005569
1459.843551	92.672372	66.010574
1459.721765	79.226842	66.015578
1459.279974	75.269727	66.020583
1458.264443	74.283146	66.025588
1457.655070	71.049639	66.030593
1457.035649	77.457119	66.035598
1457.038720	77.767274	66.040602
1455.821717	75.505487	66.045607
1454.926659	81.296064	66.050612
1454.810734	69.527400	66.055617
1453.647531	70.175847	66.060622
1452.951631	63.411296	66.065626
1452.263727	77.428580	66.070631
1451.410628	84.215379	66.075636
1451.173323	72.678880	66.080641
1450.567937	78.343004	66.085646
1450.084358	70.105029	66.090650
1448.931523	82.408036	66.095655
1447.988152	80.796590	66.100660
1447.992003	78.063266	66.105665
1447.342175	79.103193	66.110670
1446.818209	70.023283	66.115674
1445.925910	74.823149	66.120679
1445.126950	80.308313	66.125684
1444.878454	73.953605	66.130689
1443.609593	77.824618	66.135694
1443.051914	70.825225	66.140698
1442.656257	72.129095	66.145703
1442.342237	78.809726	66.150708
1441.631950	69.731044	66.155713
1440.604131	67.082829	66.160718
1440.483059	77.403742	66.165722
1439.683955	76.329161	66.170727
1438.365461	77.910569	66.175732
1437.886431	69.050590	66.180737
1437.461112	76.849560	66.185742
1436.598400	77.863400	66.190746
1435.452141	77.268168	66.195751
1434.361389	73.868329	66.200756
1434.601087	74.285951	66.205761
1433.660572	80.284019	66.210766
1433.699786	68.643662	66.215770
1433.282939	76.655740	66.220775
1432.093467	78.908891	66.225780
1431.622407	63.590380	66.230785
1430.434643	71.964655	66.235790
1429.821584	74.499919	66.240794
1429.161629	61.851106	66.245799
1428.619919	67.970285	66.250804
1428.561667	70.608179	66.255809
1427.605794	76.980829	66.260814
1426.297852	70.814995	66.265818
1425.744342	71.874311	66.270823
1425.302007	80.693068	66.275828
1425.106785	67.506794	66.280833
1424.053423	74.584028	66.285838
1423.186447	74.119449	66.290842
1422.663677	65.846715	66.295847
1422.111145	71.030958	66.300852
1421.735703	71.576300	66.305857
1420.964474	65.654739	66.310862
1420.166369	63.236517	66.315866
1419.464946	80.606797	66.320871
1419.023218	81.091715	66.325876
1418.353768	72.981053	66.330881
1417.367992	75.755319	66.335886
1416.759708	66.800778	66.340890
1416.258790	71.986280	66.345895
1415.050087	81.883994	66.350900
1414.437296	71.086809	66.355905
1413.591651	73.133945	66.360910
1413.583904	72.463431	66.365914
1413.353112	69.150846	66.370919
1412.447308	79.227488	66.375924
1411.812222	75.551825	66.380929
1410.661486	74.605674	66.385934
1410.516839	79.118003	66.390938
1409.039175	80.965983	66.395943
1408.449065	76.788036	66.400948
1408.290127	70.078499	66.405953
1407.751434	75.471846	66.410958
1407.248008	68.998400	66.415962
1406.200858	68.108324	66.420967
1405.467316	71.593093	66.425972
1405.479827	71.867056	66.430977
1404.076811	74.833788	66.435982
1403.306173	76.851661	66.440986
1402.975863	77.949620	66.445991
1402.263088	78.531233	66.450996
1402.094921	71.548788	66.456001
1400.587309	82.927385	66.461006
1400.249633	70.383464	66.466010
1399.494303	76.533449	66.471015
1398.994906	90.052462	66.476020
1398.780417	71.999884	66.481025
1397.474533	84.838138	66.486030
1396.865730	78.042411	66.491034
1396.959375	76.964720	66.496039
1395.583475	79.297977	66.501044
1395.320425	75.902215	66.506049
1394.490501	84.079295	66.511054
1393.992880	72.604682	66.516058
1392.982373	80.236482	66.521063
1392.051808	80.887403	66.526068
1391.904034	71.558494	66.531073
1391.282016	84.824194	66.536078
1390.260672	69.206819	66.541082
1389.624178	75.263805	66.546087
1388.849834	81.776342	66.551092
1388.777156	77.763728	66.556097
1387.428346	84.452722	66.561102
1386.915429	74.483295	66.566106
1386.380533	76.108909	66.571111
1385.600607	77.461249	66.576116
1385.387735	71.876708	66.581121
1384.607523	75.531318	66.586126
1383.507873	73.194148	66.591130
1382.837050	72.386186	66.596135
1382.401133	79.748478	66.601140
1382.152906	73.780070	66.606145
1381.151001	83.394206	66.611150
1380.344014	81.135093	66.616154
1379.932366	85.850702	66.621159
1379.253967	83.523845	66.626164
1378.940093	80.273350	66.631169
1377.503054	77.515171	66.636174
1377.087965	76.914131	66.641178
1376.781628	82.718385	66.646183
1375.704705	82.011239	66.651188
1374.969573	74.503934	66.656193
1374.546542	76.644751	66.661198
1374.102332	80.485643	66.666202
1373.853866	64.978814	66.671207
1372.470216	76.298294	66.676212
1372.182253	68.543309	66.681217
1371.270022	75.117185	66.686222
1370.404503	76.664473	66.691226
1369.550446	72.637295	66.696231
1368.996794	73.633571	66.701236
1368.738096	63.100231	66.706241
1368.294230	73.890312	66.711246
1367.307738	65.263970	66.716250
1366.477757	67.578274	66.721255
1365.430719	76.907864	66.726260
1365.261827	67.372596	66.731265
1364.878731	70.445300	66.736270
1364.339024	75.767856	66.741274
1363.296260	66.861894	66.746279
1362.237587	74.010951	66.751284
1362.452636	67.557350	66.756289
1361.255313	79.523696	66.761294
1360.385384	75.443853	66.766298
1360.285618	77.768243	66.771303
1359.279616	82.665053	66.776308
1358.651271	77.208051	66.781313
1357.556050	83.355306	66.786318
1356.844706	70.959096	66.791322
1356.735287	74.270560	66.796327
1356.116396	76.831998	66.801332
1355.952587	73.254897	66.806337
1354.906907	78.165898	66.811342
1354.059052	69.227381	66.816346
1353.677627	68.575266	66.821351
1352.629013	62.454985	66.826356
1352.132595	69.230836	66.831361
1351.568313	84.578285	66.836366
1350.754082	74.953214	66.841370
1350.246249	79.813417	66.846375
1349.396245	76.033169	66.851380
1349.272805	68.352956	66.856385
1348.148508	76.499568	66.861390
1347.132962	69.946700	66.866394
1346.679852	67.561968	66.871399
1346.221106	73.098726	66.876404
1346.108779	69.048268	66.881409
1344.732040	71.553562	66.886414
1343.875361	69.879494	66.891418
1343.619186	65.517608	66.896423
1342.670187	69.798266	66.901428
1342.412643	69.374029	66.906433
1341.299017	65.776032	66.911438
1340.771322	77.219649	66.916442
1340.238739	72.509059	66.921447
1339.764420	73.771835	66.926452
1338.677301	72.208511	66.931457
1337.938967	69.851774	66.936462
1337.308299	73.022180	66.941466
1336.847102	72.400093	66.946471
1336.414432	76.299075	66.951476
1335.633693	68.147792	66.956481
1334.503879	75.519468	66.961486
1334.213327	79.249212	66.966490
1333.737785	74.335601	66.971495
1332.834526	80.717263	66.976500
1332.138257	71.715236	66.981505
1331.658037	78.859082	66.986510
1331.378740	76.705329	66.991514
1330.678528	68.109186	66.996519
1329.236974	79.150901	67.001524
1329.014778	75.426974	67.006529
1328.487163	77.519771	67.011534
1327.896950	70.300091	67.016538
1327.060290	73.790233	67.021543
1326.266821	67.646750	67.026548
1325.716276	71.017298	67.031553
1325.233486	72.171043	67.036558
1323.982346	62.003621	67.041562
1323.721930	63.503616	67.046567
1323.039381	75.323490	67.051572
1322.809597	63.273350	67.056577
1321.536565	65.230766	67.061582
1320.693359	60.098080	67.066586
1320.512972	66.205566	67.071591
1319.854647	77.302541	67.076596
1319.155847	59.836317	67.081601
1318.140958	68.728745	67.086606
1317.526957	70.961424	67.091610
1317.413485	62.481741	67.096615
1316.484848	69.659023	67.101620
1315.744218	64.141045	67.106625
1315.159967	72.149781	67.111630
1314.464415	71.495571	67.116634
1314.043667	67.975089	67.121639
1312.575583	75.460467	67.126644
1312.183639	67.982206	67.131649
1311.691192	77.638366	67.136654
1311.307319	72.192977	67.141658
1311.107915	64.357700	67.146663
1309.794421	72.610089	67.151668
1309.307333	64.861543	67.156673
1308.623344	61.611556	67.161678
1307.372584	76.513071	67.166682
1306.776395	59.888356	67.171687
1306.049278	71.169719	67.176692
1305.822437	62.764827	67.181697
1305.370125	71.154689	67.186702
1304.841282	63.464819	67.191706
1303.908761	67.974668	67.196711
1303.240341	86.427753	67.201716
1302.954617	73.642221	67.206721
1301.932862	62.742949	67.211726
1300.972796	76.164885	67.216730
1300.403352	79.186803	67.221735
1299.964216	67.020144	67.226740
1299.550566	63.350313	67.231745
1298.570351	74.473230	67.236750
1297.683194	66.722059	67.241754
1297.335199	65.243092	67.246759
1296.835176	73.440279	67.251764
1296.154751	71.700363	67.256769
1295.283061	74.010282	67.261774
1294.600849	72.511911	67.266778
1294.150191	69.772005	67.271783
1293.281946	63.782342	67.276788
1292.608918	65.738997	67.281793
1292.032879	66.409282	67.286798
1291.526043	75.660899	67.291802
1290.490885	62.884141	67.296807
1289.889861	72.912355	67.301812
1289.348913	63.819428	67.306817
1288.713924	78.829628	67.311822
1287.798019	70.725080	67.316826
1286.787902	73.974743	67.321831
1286.113023	76.303836	67.326836
1285.841935	66.810058	67.331841
1285.754092	62.307886	67.336846
1285.265018	80.629957	67.341850
1284.660745	62.144256	67.346855
1283.284592	65.926746	67.351860
1283.192920	67.847748	67.356865
1282.213547	72.909071	67.361870
1281.189268	71.646425	67.366874
1280.820807	67.151020	67.371879
1280.284679	74.981810	67.376884
1279.443837	55.494576	67.381889
1278.594729	70.231320	67.386894
1277.667516	70.686218	67.391898
1277.646315	60.042607	67.396903
1276.611709	67.660922	67.401908
1276.177367	63.221722	67.406913
1275.153471	70.743725	67.411918
1274.703727	65.475966	67.416922
1274.219664	76.264560	67.421927
1273.489216	81.693146	67.426932
1273.050549	64.609758	67.431937
1272.289659	65.353588	67.436942
1271.575493	66.580394	67.441946
1270.751399	88.112617	67.446951
1269.669381	67.246113	67.451956
1269.263127	68.002944	67.456961
1269.156618	76.303144	67.461966
1268.580449	80.417327	67.466970
1267.938685	70.511000	67.471975
1266.696208	75.275134	67.476980
1266.238911	70.339717	67.481985
1265.901651	75.026163	67.486990
1264.846905	80.446388	67.491994
1264.212396	61.432524	67.496999
1263.663350	72.821194	67.502004
1263.232217	67.299757	67.507009
1262.037457	67.377751	67.512014
1260.968715	67.401019	67.517018
1260.808916	64.739450	67.522023
1260.114347	67.968913	67.527028
1260.186464	73.342437	67.532033
1259.431999	62.599376	67.537038
1258.418454	73.834829	67.542042
1257.884598	72.156772	67.547047
1256.742719	72.120711	67.552052
1256.231211	69.434640	67.557057
1255.905474	69.711920	67.562062
1255.101250	69.950164	67.567066
1254.167596	69.248676	67.572071
1253.149757	64.739834	67.577076
1252.508222	64.510691	67.582081
1252.408515	59.426970	67.587086
1251.869936	72.375070	67.592090
1251.689172	59.976553	67.597095
1250.679547	67.217188	67.602100
1249.995538	73.732736	67.607105
1248.679362	67.716541	67.612110
1247.820100	62.182758	67.617114
1247.553628	65.020903	67.622119
1246.763986	80.418374	67.627124
1246.741311	72.638579	67.632129
1246.126046	70.448373	67.637134
1245.068542	74.699009	67.642138
1244.856024	59.618566	67.647143
1243.890434	64.655632	67.652148
1243.056149	72.131730	67.657153
1242.343560	66.860040	67.662158
1241.623027	73.632118	67.667162
1241.453239	68.789759	67.672167
1240.584997	76.930388	67.677172
1239.632314	76.086859	67.682177
1238.882222	70.663445	67.687182
1238.220038	64.644194	67.692186
1237.907038	71.091293	67.697191
1237.326683	84.842364	67.702196
1236.282081	69.026937	67.707201
1235.428423	73.707186	67.712206
1235.312602	79.425964	67.717210
1235.243500	78.175459	67.722215
1234.125769	77.151606	67.727220
1233.383818	69.352143	67.732225
1232.585781	66.610716	67.737230
1231.474567	66.897778	67.742234
1230.749811	68.381731	67.747239
1229.910873	71.875417	67.752244
1229.775101	65.699933	67.757249
1229.196385	64.008517	67.762254
1228.946223	76.882381	67.767258
1228.575401	61.308323	67.772263
1227.318666	72.103085	67.777268
1226.975699	68.850935	67.782273
1225.741687	64.444282	67.787278
1224.969557	64.027765	67.792282
1224.688047	69.271441	67.797287
1223.943742	75.648357	67.802292
1223.405324	63.737194	67.807297
1222.582565	69.424878	67.812302
1221.693817	59.871642	67.817306
1221.215655	66.952092	67.822311
1220.665055	78.470321	67.827316
1220.196809	73.629690	67.832321
1219.380917	66.463275	67.837326
1218.376923	74.201317	67.842330
1218.328640	61.865313	67.847335
1217.594730	70.508103	67.852340
1216.763952	61.759312	67.857345
1216.154875	67.122877	67.862350
1215.299472	61.006633	67.867354
1215.021393	59.842972	67.872359
1213.835429	68.287997	67.877364
1213.144144	69.377148	67.882369
1212.650846	69.080292	67.887374
1212.228758	63.726154	67.892378
1211.431885	73.656216	67.897383
1210.570887	71.106147	67.902388
1209.932608	62.527010	67.907393
1209.685061	65.915627	67.912398
1208.984635	61.681168	67.917402
1208.082510	65.716309	67.922407
1206.949409	71.588955	67.927412
1206.828053	71.482102	67.932417
1206.417041	76.009979	67.937422
1205.170034	63.697437	67.942426
1204.846443	72.054225	67.947431
1203.891756	66.570322	67.952436
1203.519175	68.632181	67.957441
1203.109385	71.942525	67.962446
1201.901947	69.718767	67.967450
1201.323449	65.397117	67.972455
1201.006447	78.030888	67.977460
1200.494738	74.105446	67.982465
1199.371940	71.895036	67.987470
1198.622963	75.644070	67.992474
1198.636539	66.223311	67.997479
1197.298176	78.464436	68.002484
1196.111317	71.152024	68.007489
1195.807548	65.613505	68.012494
1195.403857	79.538320	68.017498
1195.196624	77.012023	68.022503
1194.634996	75.663230	68.027508
1194.027480	72.615569	68.032513
1193.208179	78.283792	68.037518
1192.565387	67.374773	68.042522
1191.563465	79.701166	68.047527
1190.754977	70.865261	68.052532
1190.327126	83.636505	68.057537
1190.106800	76.183016	68.062542
1188.890372	78.462637	68.067546
1188.225857	78.819026	68.072551
1187.254344	84.139317	68.077556
1186.892814	76.957426	68.082561
1186.509606	67.319082	68.087566
1185.342572	70.369818	68.092570
1184.822251	60.381142	68.097575
1184.390054	77.286025	68.102580
1183.866300	75.601648	68.107585
1182.925133	63.478592	68.112590
1182.009851	70.365223	68.117594
1181.645590	72.916166	68.122599
1180.900302	79.892457	68.127604
1180.692703	63.709017	68.132609
1179.633353	76.470295	68.137614
1178.715146	81.007871	68.142618
1178.444268	57.897881	68.147623
1178.347452	73.289254	68.152628
1177.115829	64.068087	68.157633
1176.601362	68.170895	68.162638
1175.746087	70.905570	68.167642
1174.932466	65.653123	68.172647
1173.879129	80.518560	68.177652
1173.296524	60.302800	68.182657
1172.656197	70.573806	68.187662
1172.289683	71.622359	68.192666
1172.418100	62.839317	68.197671
1171.491477	69.054434	68.202676
1170.986249	67.862249	68.207681
1170.211802	72.039516	68.212686
1169.254462	80.229024	68.217690
1168.648479	74.410577	68.222695
1167.672992	65.522399	68.227700
1167.337584	65.906878	68.232705
1166.200993	56.517655	68.237710
1165.463847	66.766211	68.242714
1165.237413	56.243558	68.247719
1164.373344	68.693098	68.252724
1163.979675	66.332065	68.257729
1163.122243	63.163317	68.262734
1162.207045	67.643649	68.267738
1161.898840	62.747625	68.272743
1161.450140	65.132235	68.277748
1160.934038	65.610101	68.282753
1159.966421	69.032812	68.287758
1159.161739	73.910286	68.292762
1159.046087	65.224401	68.297767
1157.423248	79.321018	68.302772
1156.670602	67.920155	68.307777
1156.382471	59.875102	68.312782
1155.635882	77.698833	68.317786
1155.405044	74.493513	68.322791
1154.853608	77.145186	68.327796
1153.969869	69.338341	68.332801
1153.538065	62.881959	68.337806
1152.786460	69.752029	68.342810
1152.222380	62.474639	68.347815
1151.105676	68.346274	68.352820
1150.866911	63.540127	68.357825
1149.973256	67.701665	68.362830
1148.985592	66.321294	68.367834
1148.302546	60.373197	68.372839
1147.822157	69.970681	68.377844
1147.414818	68.580018	68.382849
1147.142929	68.771481	68.387854
1146.282052	75.316755	68.392858
1145.589711	59.943658	68.397863
1144.862001	61.013388	68.402868
1143.781584	57.813883	68.407873
1143.126348	56.825323	68.412878
1142.156987	71.748363	68.417882
1142.023998	57.158320	68.422887
1141.756932	63.060406	68.427892
1141.176754	65.383932	68.432897
1140.013488	60.210759	68.437902
1139.388058	61.144383	68.442906
1139.255341	60.386520	68.447911
1137.810283	69.225996	68.452916
1137.139735	68.571013	68.457921
1136.783410	64.851099	68.462926
1135.859270	63.951035	68.467930
1135.943122	61.966624	68.472935
1134.413670	65.614304	68.477940
1133.720332	62.988718	68.482945
1133.682465	59.686487	68.487950
1132.897437	71.546334	68.492954
1132.295905	62.322751	68.497959
1131.125708	69.623653	68.502964
1130.667382	61.979388	68.507969
1130.459316	63.959901	68.512974
1129.521950	73.257926	68.517978
1128.898568	64.969744	68.522983
1128.095957	70.078694	68.527988
1127.783383	66.966799	68.532993
1127.160214	67.655654	68.537998
1125.810320	76.126787	68.543002
1125.584512	52.377335	68.548007
1125.172430	70.034325	68.553012
1124.440704	73.640293	68.558017
1123.850863	75.856558	68.563022
1122.841886	77.336860	68.568026
1122.457691	73.183012	68.573031
1121.089058	78.545982	68.578036
1120.415688	73.624464	68.583041
1120.216281	80.460337	68.588046
1119.492391	82.136559	68.593050
1119.050237	60.573922	68.598055
1118.652286	71.088645	68.603060
1117.717619	63.419222	68.608065
1117.277969	71.499598	68.613070
1116.257828	72.634768	68.618074
1115.410062	67.036134	68.623079
1114.586970	63.677450	68.628084
1114.240612	67.848142	68.633089
1113.650663	72.771896	68.638094
1113.104691	72.969110	68.643098
1112.200824	68.211982	68.648103
1111.587522	72.008840	68.653108
1110.963076	66.076663	68.658113
1110.852615	70.019038	68.663118
1109.564099	74.874135	68.668122
1108.981094	79.829902	68.673127
1108.159092	74.258707	68.678132
1107.774133	70.087638	68.683137
1107.334099	82.512335	68.688142
1106.301546	72.854288	68.693146
1105.801873	71.036796	68.698151
1105.146143	84.689485	68.703156
1104.573246	75.595382	68.708161
1103.578235	72.842751	68.713166
1103.065171	67.189311	68.718170
1102.421599	77.295277	68.723175
1101.928542	79.712183	68.728180
1100.912358	59.551226	68.733185
1100.353754	74.632861	68.738190
1099.709011	76.009511	68.743194
1099.691678	62.656258	68.748199
1098.383890	75.826057	68.753204
1097.542538	69.341790	68.758209
1097.264828	75.407992	68.763214
1096.448279	81.488941	68.768218
1095.770177	56.687127	68.773223
1094.572603	68.182112	68.778228
1094.275256	68.730848	68.783233
1094.189373	66.399716	68.788238
1093.734039	66.790664	68.793242
1092.696470	63.650594	68.798247
1092.046824	66.940756	68.803252
1091.561920	70.058069	68.808257
1090.501654	62.958959	68.813262
1089.511305	78.673786	68.818266
1089.177247	61.209575	68.823271
1088.806350	66.759194	68.828276
1087.849034	70.197637	68.833281
1086.993756	63.248841	68.838286
1086.364906	67.872874	68.843290
1086.287242	71.046832	68.848295
1085.510770	69.729084	68.853300
1084.663164	62.938331	68.858305
1083.953951	72.988509	68.863310
1083.158513	78.146793	68.868314
1083.095431	59.847901	68.873319
1081.745180	65.800860	68.878324
1080.941638	57.885109	68.883329
1080.645960	57.186285	68.888334
1080.091325	66.995843	68.893338
1079.302222	61.353203	68.898343
1078.605590	72.186656	68.903348
1077.808119	60.668390	68.908353
1077.698634	66.264734	68.913358
1076.902338	62.878149	68.918362
1076.082997	67.183998	68.923367
1075.429554	63.350515	68.928372
1074.814562	65.622825	68.933377
1073.719465	70.030881	68.938382
1072.920988	62.557423	68.943386
1072.833074	62.087310	68.948391
1072.233836	59.074636	68.953396
1071.409886	79.687531	68.958401
1071.037009	50.560746	68.963406
1069.852078	74.167162	68.968410
1069.607518	82.071445	68.973415
1068.544056	69.553180	68.978420
1067.274704	76.914033	68.983425
1067.167522	76.558943	68.988430
1066.621540	61.582044	68.993434
1066.809401	60.982916	68.998439
1065.592613	77.217860	69.003444
1064.686967	78.107771	69.008449
1064.062818	72.670692	69.013454
1063.737653	77.101357	69.018458
1063.220514	71.041743	69.023463
1061.923876	72.791739	69.028468
1061.243921	63.438737	69.033473
1061.072959	70.000438	69.038478
1059.883236	81.814299	69.043482
1059.192452	69.082226	69.048487
1058.570013	56.760315	69.053492
1057.917838	89.497179	69.058497
1057.736261	56.457724	69.063502
1056.871285	87.385085	69.068506
1055.992238	65.387366	69.073511
1055.636771	65.637863	69.078516
1054.950730	71.742211	69.083521
1054.792368	63.555116	69.088526
1053.642770	71.581281	69.093530
1052.780555	61.237047	69.098535
1052.083522	61.742138	69.103540
1051.641998	69.264608	69.108545
1050.528364	68.628094	69.113550
1049.545246	74.439098	69.118554
1049.459395	71.483526	69.123559
1048.912916	71.600415	69.128564
1048.838220	69.688528	69.133569
1048.129810	69.517380	69.138574
1047.058597	75.184713	69.143578
1046.584008	74.670461	69.148583
1045.523468	68.514377	69.153588
1044.542267	72.093821	69.158593
1044.114076	65.020337	69.163598
1043.563678	67.394336	69.168602
1043.244879	66.584083	69.173607
1042.078303	69.544926	69.178612
1041.248951	67.059267	69.183617
1040.866323	68.924060	69.188622
1040.577885	67.287434	69.193626
1040.013377	59.507129	69.198631
1039.365822	77.949014	69.203636
1038.385529	75.887888	69.208641
1038.108592	53.121099	69.213646
1036.732549	67.271538	69.218650
1036.282080	61.198177	69.223655
1035.617366	61.739129	69.228660
1035.080861	77.142087	69.233665
1034.591602	65.508580	69.238670
1033.341494	68.315567	69.243674
1032.889722	67.947490	69.248679
1032.903614	69.168922	69.253684
1031.903827	71.969205	69.258689
1031.130320	70.340361	69.263694
1029.907323	76.661013	69.268698
1030.042743	60.787304	69.273703
1029.595318	64.985118	69.278708
1028.262202	70.520665	69.283713
1027.570853	64.457240	69.288718
1026.859745	77.202583	69.293722
1026.460326	69.925840	69.298727
1026.219831	63.743389	69.303732
1024.628031	76.483761	69.308737
1024.552078	57.318084	69.313742
1023.730451	63.705762	69.318746
1023.785602	61.801605	69.323751
1022.581368	77.529970	69.328756
1021.832057	69.014287	69.333761
1021.539041	62.619431	69.338766
1020.606319	69.095745	69.343770
1019.714016	65.686607	69.348775
1019.094215	79.954867	69.353780
1018.365143	81.012235	69.358785
1017.839351	72.859939	69.363790
1016.693270	80.973866	69.368794
1016.141425	77.046969	69.373799
1015.665568	77.378121	69.378804
1015.072776	67.453060	69.383809
1015.191403	64.630533	69.388814
1014.087580	72.466515	69.393818
1013.618482	72.463874	69.398823
1013.179075	68.306217	69.403828
1011.944420	75.831874	69.408833
1010.975579	71.562911	69.413838
1010.399729	72.494986	69.418842
1009.986871	70.189070	69.423847
1009.423238	70.556263	69.428852
1008.209987	60.548576	69.433857
1007.935694	62.944884	69.438862
1007.170234	67.267410	69.443866
1006.794770	67.081151	69.448871
1006.497481	77.726518	69.453876
1005.220789	77.284687	69.458881
1004.703342	75.123135	69.463886
1004.351786	78.309130	69.468890
1003.110129	68.112006	69.473895
1002.442792	72.251776	69.478900
1001.530306	68.675555	69.483905
1001.375920	66.314329	69.488910
1000.939559	82.341567	69.493914
1000.325839	69.586220	69.498919
999.210429	72.890582	69.503924
998.555532	67.488378	69.508929
998.449310	56.483039	69.513934
997.260757	71.672779	69.518938
996.469548	64.381110	69.523943
996.113253	70.450355	69.528948
995.556092	67.281204	69.533953
995.177646	59.911256	69.538958
993.621032	68.743316	69.543962
993.545064	63.857680	69.548967
993.218515	70.636509	69.553972
991.736601	66.516987	69.558977
991.187776	69.299152	69.563982
990.440874	74.714649	69.568986
990.033256	63.323620	69.573991
989.981723	72.751971	69.578996
989.366226	75.751314	69.584001
988.897544	62.879868	69.589006
987.788999	70.767069	69.594010
986.850122	73.929817	69.599015
986.362506	71.821867	69.604020
985.344489	68.743384	69.609025
984.834065	66.568105	69.614030
983.613942	71.634715	69.619034
982.886204	59.208165	69.624039
982.290673	64.164364	69.629044
982.187901	68.977517	69.634049
981.890398	62.711109	69.639054
981.550814	67.636050	69.644058
980.650855	60.134624	69.649063
980.086399	61.312459	69.654068
978.490529	73.607248	69.659073
977.767110	61.479614	69.664078
976.725405	75.837074	69.669082
976.751866	56.768649	69.674087
976.597634	58.546652	69.679092
975.838360	67.366976	69.684097
975.265695	66.789498	69.689102
974.273440	74.275027	69.694106
973.722619	69.674662	69.699111
973.398483	67.922306	69.704116
972.263203	60.850960	69.709121
971.420918	58.198661	69.714126
970.931217	75.412289	69.719130
970.647570	74.161240	69.724135
969.603811	70.686336	69.729140
968.809870	65.924393	69.734145
968.468514	67.399453	69.739150
968.037673	68.415692	69.744154
966.950094	72.619178	69.749159
966.163826	65.530149	69.754164
965.494374	77.475714	69.759169
965.202148	60.176768	69.764174
964.670346	66.392202	69.769178
963.335956	68.012642	69.774183
962.923479	56.688627	69.779188
962.314405	63.127653	69.784193
962.172347	59.469870	69.789198
961.171915	68.356950	69.794202
960.191676	60.264369	69.799207
959.663330	61.890598	69.804212
958.872648	75.776064	69.809217
958.709041	58.398313	69.814222
957.338211	67.088876	69.819226
957.036799	70.538115	69.824231
956.903828	64.250263	69.829236
955.797371	67.510641	69.834241
954.714796	58.715298	69.839246
954.126380	74.099709	69.844250
953.669291	64.872127	69.849255
953.499130	69.181946	69.854260
952.655080	74.325920	69.859265
951.764015	71.569430	69.864270
951.017708	70.842978	69.869274
950.631850	67.471551	69.874279
950.076322	68.294757	69.879284
949.122855	69.841981	69.884289
948.622460	65.662506	69.889294
948.002848	71.469318	69.894298
947.294968	68.816140	69.899303
946.617548	47.220068	69.904308
945.635319	73.834435	69.909313
945.370450	62.759730	69.914318
944.833337	55.498615	69.919322
944.035643	60.351377	69.924327
943.537959	58.275001	69.929332
942.617583	71.578741	69.934337
942.115626	64.237916	69.939342
940.723913	70.818822	69.944346
940.579319	60.527605	69.949351
940.108317	55.756867	69.954356
939.322947	61.143800	69.959361
938.669844	52.843072	69.964366
938.001186	59.460305	69.969370
937.268779	55.098569	69.974375
936.811429	50.680454	69.979380
935.582726	72.486782	69.984385
935.279408	62.821602	69.989390
934.446105	71.018242	69.994394
934.335336	55.235759	69.999399
933.562582	70.614808	70.004404
932.341208	73.942365	70.009409
932.140848	70.882027	70.014414
931.491669	72.144312	70.019418
930.844499	65.421071	70.024423
930.009644	53.752716	70.029428
929.262058	62.563302	70.034433
929.028493	65.311084	70.039438
927.910501	74.027660	70.044442
926.976263	76.965776	70.049447
926.445445	72.641344	70.054452
926.144889	68.095781	70.059457
925.818388	66.389538	70.064462
924.436241	59.344884	70.069466
923.482477	66.559388	70.074471
923.416085	68.244575	70.079476
923.146286	69.033358	70.084481
922.760434	75.045816	70.089486
921.748452	69.725685	70.094490
921.144795	68.233844	70.099495
920.074139	62.815826	70.104500
918.490383	79.451386	70.109505
918.605837	65.857846	70.114510
917.827515	74.353230	70.119514
917.548119	67.446900	70.124519
917.718543	55.869307	70.129524
916.247095	71.752174	70.134529
915.696842	58.614632	70.139534
914.666075	69.472894	70.144538
914.214506	74.954948	70.149543
913.471063	69.582628	70.154548
912.750361	67.467633	70.159553
912.432592	69.268509	70.164558
911.700141	67.653670	70.169562
910.824233	55.938241	70.174567
909.886736	69.553775	70.179572
909.411065	70.783726	70.184577
909.430654	59.026718	70.189582
908.326560	69.180757	70.194586
907.416931	56.051524	70.199591
907.069520	61.371929	70.204596
906.508731	67.344417	70.209601
905.692388	66.796270	70.214606
904.780495	78.138642	70.219610
904.276309	71.916171	70.224615
903.769178	62.124168	70.229620
902.542348	58.052418	70.234625
902.010004	59.893746	70.239630
901.305652	62.765327	70.244634
900.885599	65.063421	70.249639
900.523196	70.871887	70.254644
899.718174	61.879450	70.259649
899.361294	67.359049	70.264654
898.445162	66.647023	70.269658
898.154898	64.525034	70.274663
897.307734	60.689319	70.279668
896.319365	68.087523	70.284673
896.060983	57.223101	70.289678
894.462101	58.259653	70.294682
893.920349	60.189207	70.299687
893.325037	64.781134	70.304692
892.814144	70.021908	70.309697
892.884077	69.127740	70.314702
891.911740	70.824636	70.319706
891.052568	60.520990	70.324711
890.404038	62.331928	70.329716
889.916329	72.632300	70.334721
889.215433	65.417759	70.339726
887.973520	87.489558	70.344730
887.444382	78.997229	70.349735
887.495458	79.477927	70.354740
886.656562	79.283437	70.359745
885.611355	73.418285	70.364750
884.938030	78.845752	70.369754
884.252192	72.956526	70.374759
884.461444	70.468060	70.379764
883.314546	71.623493	70.384769
882.638406	68.356617	70.389774
882.166296	72.985710	70.394778
881.117239	73.006005	70.399783
880.361240	67.776036	70.404788
879.719447	74.288092	70.409793
879.475883	71.920568	70.414798
878.417327	82.038995	70.419802
877.397684	75.849676	70.424807
876.884487	74.783392	70.429812
876.393868	72.880936	70.434817
876.121374	64.918599	70.439822
875.375198	61.531993	70.444826
874.671926	67.301671	70.449831
873.767404	67.789370	70.454836
873.221821	75.646945	70.459841
872.655040	64.954595	70.464846
871.935997	52.619749	70.469850
871.179008	67.505893	70.474855
870.444446	68.810164	70.479860
870.074384	76.458468	70.484865
869.361059	70.929993	70.489870
868.307422	81.128059	70.494874
868.141377	71.945637	70.499879
867.616791	65.325903	70.504884
866.165217	69.215216	70.509889
866.010687	69.779093	70.514894
865.626833	71.153702	70.519898
864.832406	69.903533	70.524903
864.054309	64.308104	70.529908
863.049168	65.352682	70.534913
862.821777	70.655570	70.539918
862.149061	69.770785	70.544922
860.909806	69.031353	70.549927
860.445454	77.467323	70.554932
859.717874	72.604976	70.559937
859.523412	65.096973	70.564942
858.731836	70.704101	70.569946
858.423506	66.426276	70.574951
857.515127	61.181148	70.579956
856.728099	71.035601	70.584961
856.063940	64.028102	70.589966
855.095110	65.134708	70.594970
854.472650	72.192437	70.599975
854.563381	66.324707	70.604980
853.564668	69.474945	70.609985
852.820984	58.176865	70.614990
852.233201	64.607791	70.619994
851.700840	64.919583	70.624999
851.152142	66.509650	70.630004
849.904227	67.302729	70.635009
848.996387	66.889003	70.640014
848.641430	61.005479	70.645018
848.316000	69.698441	70.650023
847.617267	56.444216	70.655028
846.594679	69.896699	70.660033
846.194075	68.932345	70.665038
845.751137	60.443666	70.670042
844.590541	70.491608	70.675047
843.704253	72.073908	70.680052
843.198258	72.028289	70.685057
842.791003	68.799052	70.690062
842.364752	64.699260	70.695066
841.907504	69.262917	70.700071
841.055099	68.340509	70.705076
840.268076	72.152455	70.710081
839.771695	55.706010	70.715086
838.720940	68.678882	70.720090
837.783536	75.488714	70.725095
837.544997	67.473673	70.730100
836.735196	66.290612	70.735105
836.729929	60.679422	70.740110
835.639259	61.267719	70.745114
834.708498	67.928267	70.750119
834.512456	65.958438	70.755124
833.845612	70.599607	70.760129
832.918138	71.061013	70.765134
832.443779	70.710759	70.770138
831.884004	73.756456	70.775143
831.113741	64.610289	70.780148
829.590409	80.827867	70.785153
829.144217	71.175984	70.790158
828.758059	64.461695	70.795162
828.782020	63.984824	70.800167
828.144176	60.557340	70.805172
827.036039	74.125943	70.810177
826.223827	60.629604	70.815182
825.725880	63.931948	70.820186
825.173369	64.663241	70.825191
824.016676	65.355086	70.830196
823.297555	68.978044	70.835201
823.002925	60.743293	70.840206
822.740982	73.406136	70.845210
821.873650	64.396840	70.850215
821.267000	71.819465	70.855220
820.176362	76.255294	70.860225
820.003511	63.887141	70.865230
818.713023	65.997377	70.870234
818.218061	68.525012	70.875239
817.651861	73.982747	70.880244
817.051459	78.143443	70.885249
816.617464	68.604734	70.890254
815.451027	70.583272	70.895258
814.963628	61.668042	70.900263
814.827199	62.072932	70.905268
813.909042	67.146740	70.910273
812.953456	58.525213	70.915278
812.511954	66.557024	70.920282
811.661981	67.171673	70.925287
811.412816	69.152440	70.930292
810.720337	74.508857	70.935297
810.005639	71.536704	70.940302
809.751531	73.598678	70.945306
808.169976	74.627796	70.950311
807.538351	71.806415	70.955316
806.551113	71.682869	70.960321
806.842553	67.397894	70.965326
806.176425	71.157493	70.970330
805.476562	60.566772	70.975335
804.656946	65.899271	70.980340
803.745205	67.532941	70.985345
803.424373	63.241348	70.990350
802.588558	67.196679	70.995354
801.438162	68.523005	71.000359
801.078012	60.815895	71.005364
800.598178	63.989212	71.010369
800.045887	69.482578	71.015374
799.004227	60.491582	71.020378
798.253425	67.847272	71.025383
797.893427	61.158788	71.030388
797.158847	71.120016	71.035393
797.021118	67.344871	71.040398
795.822457	64.055543	71.045402
794.989228	62.926684	71.050407
794.714738	58.857938	71.055412
794.162661	73.944857	71.060417
793.331364	71.141070	71.065422
792.699703	69.715216	71.070426
791.999888	66.568824	71.075431
791.625581	63.058404	71.080436
790.605369	67.369498	71.085441
789.882463	63.408395	71.090446
789.619973	63.406024	71.095450
788.858597	64.629436	71.100455
787.985456	53.637403	71.105460
787.005786	73.139768	71.110465
786.729993	64.895717	71.115470
786.421297	58.334680	71.120474
784.910533	76.027784	71.125479
784.465314	58.950354	71.130484
783.729139	76.378248	71.135489
783.748731	63.984201	71.140494
783.395242	69.723452	71.145498
782.127222	71.666138	71.150503
781.438938	67.187048	71.155508
780.453626	66.902366	71.160513
780.183333	70.105407	71.165518
779.324134	56.600805	71.170522
778.192055	66.289436	71.175527
778.245594	61.741150	71.180532
777.617070	79.134566	71.185537
777.328137	69.831381	71.190542
776.264800	66.782280	71.195546
775.421669	66.019257	71.200551
775.119624	56.831702	71.205556
773.884321	59.954976	71.210561
773.144593	71.736718	71.215566
772.736829	64.660050	71.220570
772.395885	71.195194	71.225575
771.959697	61.494435	71.230580
770.686681	62.523345	71.235585
770.070168	63.004657	71.240590
769.656280	59.046409	71.245594
768.782980	76.888768	71.250599
768.007351	62.836309	71.255604
767.562934	55.746559	71.260609
767.010990	57.212588	71.265614
766.439924	60.485581	71.270618
765.478826	59.492198	71.275623
765.351857	66.631905	71.280628
764.753886	63.754721	71.285633
763.363209	60.396634	71.290638
762.415157	65.601365	71.295642
761.615841	67.737516	71.300647
761.625432	61.848015	71.305652
760.916898	70.922065	71.310657
760.719772	69.523237	71.315662
759.953702	70.695369	71.320666
758.851042	63.221574	71.325671
758.666274	60.390574	71.330676
757.367814	63.115505	71.335681
756.739903	69.846131	71.340686
756.374681	63.833380	71.345690
755.403470	68.392137	71.350695
755.445516	65.190737	71.355700
754.170911	68.864293	71.360705
753.458807	67.353490	71.365710
753.215785	65.126236	71.370714
752.516538	72.543114	71.375719
751.716186	60.284330	71.380724
750.625541	69.282023	71.385729
750.354042	73.166460	71.390734
749.943439	68.026626	71.395738
749.004453	67.047074	71.400743
748.500030	64.536601	71.405748
747.605668	74.983717	71.410753
747.386744	69.598918	71.415758
746.596952	73.490173	71.420762
745.236359	71.754620	71.425767
744.984136	73.612884	71.430772
744.499125	70.112210	71.435777
744.024490	76.823172	71.440782
743.011793	65.351928	71.445786
742.149747	65.165904	71.450791
741.891334	62.830722	71.455796
741.361257	60.955077	71.460801
740.620498	70.862109	71.465806
739.796090	70.466678	71.470810
738.954612	67.544692	71.475815
738.794091	72.466378	71.480820
738.073334	71.841572	71.485825
736.959559	65.429204	71.490830
736.329657	71.614561	71.495834
735.735122	76.073941	71.500839
735.480498	69.250427	71.505844
734.396343	58.735104	71.510849
733.987760	62.955157	71.515854
733.343151	70.456374	71.520858
732.420763	67.960406	71.525863
731.585421	65.687109	71.530868
730.871547	71.977292	71.535873
730.683804	68.774629	71.540878
730.611010	67.955215	71.545882
729.489964	72.652945	71.550887
728.505378	64.435016	71.555892
728.006795	68.008697	71.560897
727.595116	64.602003	71.565902
726.576495	67.233517	71.570906
725.846650	64.429374	71.575911
725.745937	63.939237	71.580916
724.253823	67.973843	71.585921
723.828559	66.650759	71.590926
723.403224	67.907419	71.595930
722.632314	71.794098	71.600935
722.567631	54.987254	71.605940
721.297755	65.544611	71.610945
720.634041	57.641437	71.615950
720.049756	59.018013	71.620954
719.254683	63.745847	71.625959
718.703154	53.771753	71.630964
717.879051	64.226606	71.635969
717.350652	66.124109	71.640974
716.813893	68.347775	71.645978
715.696270	69.266823	71.650983
715.381732	65.634945	71.655988
714.714037	68.746726	71.660993
714.093708	63.052125	71.665998
713.129096	69.181968	71.671002
712.410629	61.593421	71.676007
711.961488	55.769074	71.681012
711.627205	72.191606	71.686017
711.105725	75.988119	71.691022
710.179794	50.699313	71.696026
709.446634	69.099643	71.701031
709.169206	57.404139	71.706036
708.209870	71.639746	71.711041
706.980052	61.205970	71.716046
706.416798	72.775136	71.721050
705.753843	71.240754	71.726055
705.950484	65.843415	71.731060
705.028709	58.999978	71.736065
703.715370	65.300452	71.741070
703.469268	65.409015	71.746074
702.956122	64.030545	71.751079
703.062232	53.846107	71.756084
701.497531	73.197215	71.761089
700.741331	74.735200	71.766094
700.407531	63.312003	71.771098
699.220213	63.885786	71.776103
698.767365	60.040981	71.781108
698.206102	71.114698	71.786113
697.533222	71.101985	71.791118
696.746865	61.589454	71.796122
696.037301	67.798537	71.801127
695.867921	64.001635	71.806132
695.214049	63.594837	71.811137
694.257217	58.139887	71.816142
693.132962	68.156864	71.821146
692.425846	66.981156	71.826151
692.324359	50.423019	71.831156
692.128983	68.742459	71.836161
691.033968	75.211598	71.841166
690.141595	62.235831	71.846170
689.452553	75.663638	71.851175
689.294377	61.074546	71.856180
688.020638	73.018589	71.861185
687.378799	80.355385	71.866190
686.914337	69.485967	71.871194
686.362177	60.669390	71.876199
686.158229	58.666145	71.881204
684.963304	72.188685	71.886209
684.455258	70.594954	71.891214
684.085062	65.013491	71.896218
682.620190	67.962061	71.901223
682.190850	58.205050	71.906228
681.493393	68.400068	71.911233
681.165890	64.787605	71.916238
680.921701	62.059107	71.921242
679.618954	69.944222	71.926247
679.250867	64.889093	71.931252
678.353673	71.678377	71.936257
677.616792	66.355557	71.941262
676.944200	64.827449	71.946266
676.158829	71.281981	71.951271
675.967549	46.404482	71.956276
675.372207	68.531045	71.961281
674.241858	60.867752	71.966286
673.899693	59.752207	71.971290
673.193368	66.172076	71.976295
672.576477	61.730539	71.981300
671.459759	69.237553	71.986305
670.850931	63.698818	71.991310
670.707803	53.492569	71.996314
669.943051	62.080450	72.001319
669.255523	57.326906	72.006324
668.137082	57.613788	72.011329
667.495281	66.270399	72.016334
667.690350	58.236815	72.021338
666.563995	68.066490	72.026343
665.931683	64.824240	72.031348
665.406357	73.479656	72.036353
664.625209	66.233821	72.041358
663.714396	65.421693	72.046362
662.805328	68.146168	72.051367
662.754716	60.919628	72.056372
661.961155	63.866970	72.061377
660.798811	62.897786	72.066382
660.372669	57.039829	72.071386
659.747757	66.075350	72.076391
659.421013	60.158990	72.081396
658.957241	57.030248	72.086401
657.973335	64.607575	72.091406
657.254014	63.697155	72.096410
656.379101	67.795939	72.101415
656.293229	56.003721	72.106420
655.197917	62.129161	72.111425
654.030273	65.577588	72.116430
653.855502	56.458098	72.121434
653.185582	63.400419	72.126439
653.014525	64.695445	72.131444
651.930128	61.727021	72.136449
651.193919	69.178186	72.141454
650.848005	60.259399	72.146458
650.075609	69.493438	72.151463
649.113260	69.184653	72.156468
648.508821	65.786592	72.161473
647.959773	77.172167	72.166478
647.868022	58.256662	72.171482
646.477819	62.178894	72.176487
645.886389	62.530093	72.181492
645.223266	80.209707	72.186497
645.122446	65.166815	72.191502
644.129543	71.723782	72.196506
643.190311	66.064212	72.201511
642.687162	51.121665	72.206516
642.075352	76.209034	72.211521
641.432402	65.817456	72.216526
640.804023	67.901194	72.221530
639.594255	65.037888	72.226535
639.433620	61.671658	72.231540
638.975941	75.324388	72.236545
638.230072	72.844501	72.241550
637.543931	72.403435	72.246554
636.904219	69.477741	72.251559
636.299738	64.991662	72.256564
635.173556	65.085838	72.261569
634.373178	65.036678	72.266574
634.064403	64.067199	72.271578
633.375025	67.329099	72.276583
633.256278	58.492409	72.281588
632.394716	57.401232	72.286593
632.372847	59.692725	72.291598
630.857826	60.520559	72.296602
629.901976	62.910317	72.301607
629.669350	60.075913	72.306612
629.152946	55.426013	72.311617
628.087710	59.493613	72.316622
627.305743	57.519342	72.321626
626.629430	62.010682	72.326631
626.420407	62.898620	72.331636
625.532003	58.134503	72.336641
624.689899	63.412286	72.341646
624.284728	55.562589	72.346650
623.389536	64.805146	72.351655
623.478436	60.869360	72.356660
622.008506	62.610900	72.361665
621.371679	62.827418	72.366670
620.998631	58.131039	72.371674
620.463994	61.420335	72.376679
619.511530	64.959083	72.381684
618.563096	73.503695	72.386689
617.776916	66.894151	72.391694
617.425107	64.572281	72.396698
617.224182	70.482781	72.401703
616.663185	59.458464	72.406708
615.739286	64.164264	72.411713
615.176980	60.067266	72.416718
614.486135	54.596803	72.421722
613.292613	64.484496	72.426727
613.026840	63.809350	72.431732
612.103739	63.644131	72.436737
611.811786	58.233141	72.441742
611.471834	54.006127	72.446746
609.943789	63.822519	72.451751
609.817747	56.202748	72.456756
609.381319	53.842320	72.461761
608.244978	70.903468	72.466766
607.845268	59.788819	72.471770
607.204182	65.326315	72.476775
606.561339	55.029352	72.481780
605.405686	53.283320	72.486785
604.316077	69.895508	72.491790
604.392535	52.724040	72.496794
603.838043	57.826725	72.501799
603.610397	58.616711	72.506804
602.720314	62.793615	72.511809
601.561686	64.370483	72.516814
601.536094	55.042755	72.521818
600.361506	66.017042	72.526823
599.621746	57.074262	72.531828
599.126525	55.040145	72.536833
598.391662	57.186577	72.541838
598.039763	51.379888	72.546842
596.521942	53.335635	72.551847
596.086370	53.444421	72.556852
595.625765	53.248130	72.561857
595.271810	60.433438	72.566862
595.038742	55.894534	72.571866
593.949590	69.472792	72.576871
593.341261	53.845311	72.581876
592.454537	61.668938	72.586881
591.910855	60.333200	72.591886
591.294374	53.371817	72.596890
590.408751	57.079689	72.601895
589.856630	46.345695	72.606900
589.328986	54.025408	72.611905
588.610881	61.696035	72.616910
588.005204	60.587776	72.621914
587.065362	58.914609	72.626919
586.957228	52.561356	72.631924
585.687057	58.093388	72.636929
585.184043	53.144920	72.641934
584.929938	45.974455	72.646938
583.867785	57.000216	72.651943
582.963958	59.999831	72.656948
582.208808	51.089472	72.661953
581.918937	67.288891	72.666958
581.680936	57.927186	72.671962
580.705061	60.354841	72.676967
579.904020	58.102944	72.681972
579.272289	58.299739	72.686977
578.639476	58.906687	72.691982
578.355533	56.269684	72.696986
577.024944	49.879320	72.701991
576.731788	57.507501	72.706996
576.137696	52.491544	72.712001
575.570009	53.099159	72.717006
574.908862	49.803187	72.722010
573.693188	66.656215	72.727015
572.945198	58.074277	72.732020
573.004466	50.894903	72.737025
571.837775	57.679825	72.742030
571.015761	52.756934	72.747034
570.369294	60.547034	72.752039
569.894951	57.870974	72.757044
569.519849	60.204530	72.762049
569.238030	55.611897	72.767054
568.372106	53.122773	72.772058
567.528637	59.777378	72.777063
566.887146	55.120610	72.782068
565.907665	53.311848	72.787073
565.266888	51.285153	72.792078
565.297536	43.072774	72.797082
564.311743	64.408439	72.802087
563.419689	52.235311	72.807092
562.774058	53.881871	72.812097
561.900170	64.754667	72.817102
561.445944	56.305711	72.822106
560.437777	51.164907	72.827111
559.835196	46.790510	72.832116
559.173284	46.005009	72.837121
558.617787	59.077256	72.842126
558.673463	47.467509	72.847130
557.664657	49.492011	72.852135
556.667974	55.352634	72.857140
556.210451	49.460281	72.862145
555.694867	46.464387	72.867150
555.519939	48.879596	72.872154
554.225829	57.841948	72.877159
553.935361	54.072233	72.882164
552.760391	66.254465	72.887169
551.880513	60.408876	72.892174
551.678219	50.044927	72.897178
550.767631	63.616828	72.902183
550.554374	43.974868	72.907188
549.543814	56.146675	72.912193
548.570393	56.443626	72.917198
548.669332	50.787479	72.922202
547.832031	44.585057	72.927207
546.694134	48.758869	72.932212
546.156312	52.389284	72.937217
545.557744	55.594164	72.942222
545.426597	52.106562	72.947226
544.426529	53.371214	72.952231
543.854337	52.377475	72.957236
543.220644	48.408557	72.962241
542.097608	57.247478	72.967246
541.519285	43.367132	72.972250
540.723952	56.245781	72.977255
540.317302	52.258046	72.982260
540.057834	60.741823	72.987265
538.948194	56.722561	72.992270
538.203296	47.451068	72.997274
537.752503	53.647347	73.002279
537.440501	57.904074	73.007284
536.270032	49.922421	73.012289
535.291001	61.332327	73.017294
535.128416	53.715233	73.022298
534.412100	57.878673	73.027303
533.999799	52.620899	73.032308
532.610695	48.031183	73.037313
531.953781	58.367985	73.042318
531.601262	47.602219	73.047322
531.083599	58.996983	73.052327
531.101074	59.639131	73.057332
530.227933	49.967047	73.062337
529.164866	49.469361	73.067342
528.887235	48.523320	73.072346
527.402557	58.154660	73.077351
526.751997	51.506212	73.082356
526.393168	55.253191	73.087361
525.792694	45.455686	73.092366
525.302863	54.159066	73.097370
524.494154	56.631073	73.102375
523.549436	58.091907	73.107380
523.113944	47.342513	73.112385
522.607523	41.752831	73.117390
521.857372	51.674001	73.122394
521.050354	56.545703	73.127399
520.689355	54.974318	73.132404
520.383103	54.277248	73.137409
519.074629	54.698536	73.142414
518.535060	46.351494	73.147418
517.944798	55.647998	73.152423
517.467387	46.810117	73.157428
516.023318	51.803788	73.162433
515.642602	45.615380	73.167438
515.146048	48.537529	73.172442
514.771715	61.030605	73.177447
514.351390	43.370626	73.182452
513.188384	57.668663	73.187457
512.235995	54.849579	73.192462
512.283496	42.041161	73.197466
511.513022	56.957873	73.202471
510.604195	47.316714	73.207476
509.884628	45.512305	73.212481
509.211053	56.608650	73.217486
509.099336	50.852026	73.222490
507.872666	50.750968	73.227495
506.815093	60.686424	73.232500
506.774508	50.690937	73.237505
505.887792	59.364506	73.242510
505.149373	55.347628	73.247514
504.400147	51.688840	73.252519
503.952755	45.509478	73.257524
503.469519	36.945329	73.262529
502.709855	56.512019	73.267534
501.882895	46.170317	73.272538
501.245565	49.245771	73.277543
500.910984	42.239519	73.282548
500.472974	62.533943	73.287553
499.552760	59.168879	73.292558
498.940181	60.501129	73.297562
498.329193	47.102207	73.302567
497.029706	41.629397	73.307572
496.338958	48.032623	73.312577
495.711090	57.762448	73.317582
495.413959	40.866548	73.322586
495.124480	53.049654	73.327591
494.326443	50.718468	73.332596
493.169252	52.771362	73.337601
492.663907	60.512189	73.342606
492.571592	48.795142	73.347610
491.300210	59.978833	73.352615
490.554292	57.588885	73.357620
489.803741	51.132985	73.362625
489.694708	52.426023	73.367630
489.297335	58.033520	73.372634
487.937335	58.114548	73.377639
487.499300	61.256026	73.382644
487.198921	64.099627	73.387649
486.117380	58.838088	73.392654
485.127803	47.342814	73.397658
484.306194	59.869294	73.402663
484.099535	52.582484	73.407668
483.687600	56.864595	73.412673
483.036602	58.598756	73.417678
482.338008	54.816800	73.422682
481.514400	64.235635	73.427687
481.027187	50.730274	73.432692
480.720494	59.465985	73.437697
479.467445	57.828562	73.442702
479.054192	48.110050	73.447706
478.228815	54.077443	73.452711
477.831517	54.694205	73.457716
477.002262	50.530969	73.462721
476.135302	59.141478	73.467726
475.945417	53.569185	73.472730
474.963531	60.110255	73.477735
473.822351	52.943931	73.482740
473.260505	53.984271	73.487745
472.922861	66.512506	73.492750
472.655105	52.015040	73.497754
471.324498	55.872676	73.502759
470.503270	53.163595	73.507764
470.407740	54.968535	73.512769
469.806804	54.881349	73.517774
469.570760	42.863954	73.522778
468.491217	47.113651	73.527783
467.713072	49.386853	73.532788
467.189621	52.669662	73.537793
465.986281	57.230801	73.542798
465.470652	44.975688	73.547802
464.628716	53.981152	73.552807
464.505271	53.731176	73.557812
464.003673	52.261041	73.562817
462.891032	59.906239	73.567822
462.289410	42.428115	73.572826
461.491617	53.578943	73.577831
461.227353	65.860538	73.582836
461.007573	48.938126	73.587841
459.755356	51.249007	73.592846
459.354134	44.341683	73.597850
458.424203	54.897016	73.602855
457.275235	48.657553	73.607860
456.288387	46.906778	73.612865
455.841021	58.183124	73.617870
456.006619	43.832662	73.622874
455.355223	52.534980	73.627879
454.871725	64.350060	73.632884
454.285683	52.889855	73.637889
453.718630	60.713052	73.642894
452.989364	55.587786	73.647898
451.469033	57.676474	73.652903
451.240378	49.298842	73.657908
450.626976	52.212811	73.662913
449.448100	54.430018	73.667918
449.159931	52.454407	73.672922
448.581975	58.349279	73.677927
447.971480	58.110668	73.682932
447.347242	61.448960	73.687937
446.124957	61.722524	73.692942
445.750121	48.161430	73.697946
444.842956	55.165236	73.702951
444.905053	51.011388	73.707956
444.241937	52.913058	73.712961
443.141018	59.061545	73.717966
442.383648	57.184336	73.722970
441.673067	54.640551	73.727975
441.806141	61.210574	73.732980
440.573802	57.083183	73.737985
439.439792	60.442770	73.742990
439.179068	48.946514	73.747994
438.709502	56.987553	73.752999
437.843595	68.073560	73.758004
437.237243	67.790139	73.763009
436.377444	48.694305	73.768014
436.253724	53.829307	73.773018
435.705349	54.408647	73.778023
434.599621	49.472667	73.783028
434.029024	51.703352	73.788033
433.308617	53.029142	73.793038
433.128885	45.717554	73.798042
432.254190	66.477340	73.803047
431.312321	60.912896	73.808052
430.850102	52.936728	73.813057
429.478456	61.711228	73.818062
428.754709	59.511720	73.823066
428.165049	58.635901	73.828071
428.039173	54.729605	73.833076
427.724241	52.725147	73.838081
426.797556	56.229891	73.843086
426.228600	59.721796	73.848090
425.438370	56.041184	73.853095
424.902195	54.217044	73.858100
424.497948	54.516398	73.863105
423.268289	52.730209	73.868110
422.697830	48.667679	73.873114
422.393393	46.792429	73.878119
421.289698	47.565894	73.883124
420.505801	49.117830	73.888129
419.747644	53.554449	73.893134
419.495749	43.520109	73.898138
419.270729	49.428134	73.903143
418.377220	55.720191	73.908148
417.761655	49.823092	73.913153
416.611675	51.808644	73.918158
416.374550	47.734007	73.923162
415.269895	56.196332	73.928167
414.524929	55.472985	73.933172
414.222920	40.093239	73.938177
413.927252	53.289664	73.943182
412.679559	44.489388	73.948186
412.223182	48.699744	73.953191
411.591411	47.693453	73.958196
411.083732	52.044438	73.963201
410.213445	62.647053	73.968206
409.724930	44.127556	73.973210
409.266608	57.455548	73.978215
408.131413	51.929804	73.983220
407.231043	37.939987	73.988225
406.375958	57.569194	73.993230
406.291742	52.153528	73.998234
405.969528	52.638498	74.003239
405.095372	42.058375	74.008244
404.560394	53.323449	74.013249
403.397103	54.711925	74.018254
403.489654	46.262629	74.023258
401.942137	53.450467	74.028263
401.024173	47.708780	74.033268
400.934611	45.472891	74.038273
400.200502	51.818396	74.043278
400.112683	50.637139	74.048282
398.987599	58.235460	74.053287
398.120286	54.598676	74.058292
397.986558	45.392279	74.063297
397.116823	56.518318	74.068302
396.293449	54.060323	74.073306
395.471516	58.045095	74.078311
395.030724	53.507780	74.083316
394.894871	57.376931	74.088321
393.629883	57.811856	74.093326
392.822078	58.889826	74.098330
392.648222	52.611716	74.103335
391.773533	52.823616	74.108340
390.669465	52.084959	74.113345
390.178597	63.101756	74.118350
389.785916	53.425716	74.123354
389.575253	51.201238	74.128359
388.466784	50.999410	74.133364
387.704523	43.458970	74.138369
387.064007	52.184794	74.143374
386.778040	40.921222	74.148378
385.737954	52.897516	74.153383
384.754641	51.519920	74.158388
384.341282	57.191471	74.163393
383.613410	61.613815	74.168398
383.340817	48.567846	74.173402
382.246672	48.907750	74.178407
381.773667	48.915312	74.183412
381.524584	44.583984	74.188417
380.602269	56.730739	74.193422
379.729640	41.627990	74.198426
379.081684	50.604141	74.203431
378.591164	52.538247	74.208436
378.170823	52.808636	74.213441
376.954010	60.528807	74.218446
376.403640	46.030675	74.223450
375.915819	51.278880	74.228455
375.679493	62.113203	74.233460
374.586073	47.905012	74.238465
373.847382	62.644809	74.243470
373.109821	51.052670	74.248474
372.991692	56.421731	74.253479
371.921081	53.246254	74.258484
371.259482	49.704428	74.263489
370.496810	55.248725	74.268494
370.422129	46.504400	74.273498
368.877737	47.075314	74.278503
368.226979	51.756589	74.283508
368.027795	50.660882	74.288513
367.527686	56.105000	74.293518
366.611316	48.308443	74.298522
366.037760	50.538037	74.303527
365.454632	57.425583	74.308532
365.109155	42.827006	74.313537
363.500131	47.847041	74.318542
363.265334	52.703294	74.323546
362.541186	56.582613	74.328551
362.444906	54.715200	74.333556
361.351324	47.076186	74.338561
360.474245	57.377136	74.343566
360.042833	57.272426	74.348570
359.679305	46.653530	74.353575
358.334390	46.811069	74.358580
357.925392	50.922425	74.363585
357.232763	60.028699	74.368590
357.024608	44.233491	74.373594
356.066478	59.192744	74.378599
355.007446	65.765071	74.383604
354.431483	52.020022	74.388609
353.998874	56.220293	74.393614
353.531472	56.507646	74.398618
352.782771	57.043237	74.403623
351.931401	54.329539	74.408628
351.542843	59.508320	74.413633
350.437051	58.194406	74.418638
350.491017	49.060601	74.423642
349.479531	53.834052	74.428647
348.736820	58.869008	74.433652
348.393676	49.420038	74.438657
347.483996	53.847707	74.443662
346.501276	56.926198	74.448666
345.748394	63.854992	74.453671
345.365172	44.973411	74.458676
345.338038	42.997218	74.463681
344.522878	50.738544	74.468686
343.492271	43.926810	74.473690
343.276509	59.387470	74.478695
341.869741	61.188486	74.483700
340.921150	52.011026	74.488705
339.983375	63.384451	74.493710
339.668302	49.600991	74.498714
339.376694	44.579480	74.503719
338.881640	53.605387	74.508724
338.783662	56.799920	74.513729
338.034386	55.869140	74.518734
337.177370	54.468284	74.523738
336.524949	55.748576	74.528743
335.597836	53.477434	74.533748
334.919751	49.339046	74.538753
334.245415	53.066941	74.543758
333.943827	48.414425	74.548762
332.945108	57.421255	74.553767
331.981594	48.794921	74.558772
331.504943	60.750831	74.563777
331.018095	62.312226	74.568782
330.542828	52.482217	74.573786
329.555977	46.007269	74.578791
328.344467	54.980204	74.583796
328.119392	42.737181	74.588801
327.913455	49.503124	74.593806
327.319379	54.766693	74.598810
326.126551	53.927099	74.603815
325.584869	62.285553	74.608820
325.301808	54.209905	74.613825
324.579430	50.796043	74.618830
323.282860	49.632384	74.623834
322.915213	45.409839	74.628839
322.287446	58.673382	74.633844
322.032856	54.242019	74.638849
320.814505	57.684477	74.643854
320.475526	50.652154	74.648858
320.118272	59.001715	74.653863
319.064237	59.667970	74.658868
318.788813	41.272239	74.663873
317.844049	52.394480	74.668878
317.462477	54.522532	74.673882
316.296353	52.743618	74.678887
315.524706	51.439545	74.683892
315.218096	61.845127	74.688897
314.507303	66.808780	74.693902
313.674610	60.785473	74.698906
312.766005	54.097799	74.703911
312.107573	49.897943	74.708916
311.812897	54.541406	74.713921
311.378766	64.948391	74.718926
310.686552	51.639750	74.723930
309.716692	72.566101	74.728935
309.034413	57.754714	74.733940
308.970438	56.227485	74.738945
307.476511	61.415283	74.743950
306.753723	56.309535	74.748954
306.105566	62.431648	74.753959
305.853319	58.189135	74.758964
305.838250	56.406547	74.763969
304.704589	63.437032	74.768974
303.869442	61.225356	74.773978
303.504543	60.304288	74.778983
302.586082	66.195110	74.783988
301.674004	59.963701	74.788993
301.041976	63.836241	74.793998
300.776037	65.586347	74.799002
300.245961	63.898449	74.804007
298.904466	61.018470	74.809012
298.687090	55.647687	74.814017
297.995079	55.668092	74.819022
297.465594	59.256226	74.824026
296.488216	62.184085	74.829031
295.872502	62.294825	74.834036
294.961922	62.477789	74.839041
294.644545	58.504260	74.844046
294.151019	53.158567	74.849050
293.018703	58.301356	74.854055
292.208699	62.405675	74.859060
292.035171	48.453024	74.864065
291.508298	50.579006	74.869070
291.050725	49.843009	74.874074
290.192595	48.130133	74.879079
289.200570	57.334591	74.884084
289.179533	54.753495	74.889089
288.056552	54.429454	74.894094
287.248557	54.305932	74.899098
287.063563	50.352306	74.904103
285.756505	55.791010	74.909108
285.296122	50.730177	74.914113
284.755470	62.699446	74.919118
284.110968	57.292666	74.924122
283.610010	55.885542	74.929127
282.516850	57.209284	74.934132
282.244403	55.339993	74.939137
281.401531	62.587474	74.944142
280.851009	60.005615	74.949146
279.997263	52.979653	74.954151
278.903575	57.608547	74.959156
278.657950	53.256182	74.964161
277.977957	72.138478	74.969166
277.653395	59.427217	74.974170
276.931419	63.181642	74.979175
276.115465	54.303172	74.984180
276.009568	52.337956	74.989185
274.995410	55.864577	74.994190
273.885981	54.877685	74.999194
273.330523	51.208594	75.004199
272.814048	59.838983	75.009204
272.925000	49.217021	75.014209
271.364318	57.734733	75.019214
271.025120	68.452999	75.024218
270.375275	63.862302	75.029223
268.851464	62.082076	75.034228
268.748320	52.263735	75.039233
268.066716	60.130445	75.044238
267.730006	57.249602	75.049242
267.303031	54.569214	75.054247
266.090642	65.732556	75.059252
265.828583	58.019400	75.064257
265.077700	55.228222	75.069262
264.170804	61.222860	75.074266
263.222262	56.509475	75.079271
262.441580	64.442439	75.084276
261.963601	59.099004	75.089281
261.637323	67.501980	75.094286
261.413889	50.490324	75.099290
260.438198	51.263956	75.104295
259.624215	55.547099	75.109300
259.291326	57.982769	75.114305
257.983858	58.306269	75.119310
257.047169	54.153933	75.124314
256.890791	59.806614	75.129319
256.204626	61.142765	75.134324
256.379080	65.005036	75.139329
255.068664	55.076364	75.144334
254.270510	60.030299	75.149338
253.887200	58.918221	75.154343
253.044185	69.114436	75.159348
252.268317	55.081186	75.164353
251.312712	58.738823	75.169358
251.137815	61.707515	75.174362
250.759663	58.945236	75.179367
249.440970	60.412165	75.184372
248.749004	57.064437	75.189377
247.796586	55.931114	75.194382
247.613416	55.449412	75.199386
247.496644	61.385921	75.204391
246.619922	56.287384	75.209396
245.644259	62.105344	75.214401
245.069837	60.287342	75.219406
244.808290	62.932401	75.224410
244.098772	51.772632	75.229415
243.194494	58.938452	75.234420
243.077823	48.735947	75.239425
241.792216	60.462860	75.244430
240.751873	54.857433	75.249434
240.238646	62.448170	75.254439
240.043791	61.235098	75.259444
239.463822	50.638116	75.264449
238.147058	65.343927	75.269454
237.583550	56.879365	75.274458
237.368421	58.099442	75.279463
236.757000	69.345191	75.284468
235.959075	50.747349	75.289473
234.676716	58.888005	75.294478
234.487867	49.816564	75.299482
234.105136	57.755481	75.304487
233.003513	60.219075	75.309492
232.447249	54.342540	75.314497
231.903316	64.226173	75.319502
231.948731	64.294623	75.324506
230.875844	57.686783	75.329511
229.565842	67.195822	75.334516
229.317582	52.215953	75.339521
228.624298	59.635131	75.344526
227.717383	56.195525	75.349530
227.197414	51.937356	75.354535
226.227261	66.841796	75.359540
226.497999	51.443333	75.364545
225.438070	58.477861	75.369550
224.209748	61.152453	75.374554
223.790178	54.845729	75.379559
223.111876	60.516955	75.384564
223.051739	54.469884	75.389569
221.966860	63.681283	75.394574
221.405144	55.068219	75.399578
220.950655	59.866465	75.404583
219.646769	67.635274	75.409588
219.222185	60.339090	75.414593
218.280448	58.105016	75.419598
217.985683	60.736449	75.424602
217.462652	48.878385	75.429607
217.127920	66.564009	75.434612
216.324841	52.268630	75.439617
215.252486	57.346703	75.444622
215.208770	48.561193	75.449626
214.093412	52.398837	75.454631
213.161901	56.861566	75.459636
212.843016	69.000486	75.464641
212.071114	54.239698	75.469646
211.201461	60.923803	75.474650
210.436914	58.401308	75.479655
209.769068	55.712022	75.484660
209.464619	50.908606	75.489665
208.995034	63.885194	75.494670
208.140603	54.915122	75.499674
207.420263	57.994414	75.504679
206.637137	71.356857	75.509684
206.379094	49.131379	75.514689
205.284642	71.824749	75.519694
204.743666	45.421588	75.524698
204.332815	50.594473	75.529703
203.635249	73.306575	75.534708
202.913593	53.823016	75.539713
202.105243	57.484003	75.544718
201.296005	51.431777	75.549722
200.759145	52.020369	75.554727
199.955926	65.143177	75.559732
199.412298	62.468782	75.564737
198.557061	58.503744	75.569742
198.176168	53.974272	75.574746
197.811178	47.485404	75.579751
197.058761	66.051259	75.584756
196.577674	49.791852	75.589761
195.709010	56.362268	75.594766
194.841513	58.712867	75.599770
194.014131	53.166549	75.604775
193.095132	64.708896	75.609780
192.713638	54.966474	75.614785
192.394762	62.245557	75.619790
191.715564	64.599255	75.624794
190.613986	62.613007	75.629799
190.263403	61.379036	75.634804
190.001590	48.605769	75.639809
189.419557	64.835966	75.644814
188.719495	61.937370	75.649818
187.944702	67.758020	75.654823
186.624588	71.098501	75.659828
186.005424	57.538582	75.664833
185.297857	82.023088	75.669838
184.755312	48.289427	75.674842
184.775096	52.740853	75.679847
183.812583	74.979567	75.684852
182.958864	50.425445	75.689857
182.236720	46.609499	75.694862
181.910752	69.590339	75.699866
181.361742	38.297114	75.704871
180.391151	53.141700	75.709876
179.724756	63.238813	75.714881
179.177118	69.225089	75.719886
177.974820	57.710269	75.724890
177.173582	55.745530	75.729895
176.549689	53.107591	75.734900
176.269115	63.885891	75.739905
176.013746	52.458222	75.744910
175.398719	67.134184	75.749914
174.870866	48.088075	75.754919
173.701219	62.158639	75.759924
173.564570	57.735302	75.764929
172.510442	67.687665	75.769934
171.670784	48.989288	75.774938
171.379970	58.085148	75.779943
170.447166	62.503948	75.784948
169.507475	74.908987	75.789953
168.973419	54.233403	75.794958
168.181663	46.590525	75.799962
168.049210	66.553971	75.804967
167.326195	61.722677	75.809972
166.581544	51.569838	75.814977
165.658123	55.345366	75.819982
165.252448	65.153354	75.824986
164.803593	60.477036	75.829991
163.498208	59.060996	75.834996
162.879825	53.091891	75.840001
162.775000	63.165706	75.845006
162.139298	58.855045	75.850010
160.899999	64.300354	75.855015
160.305536	67.592965	75.860020
159.917645	48.019959	75.865025
159.674026	71.698827	75.870030
158.875566	63.235477	75.875034
157.932403	47.833444	75.880039
157.031951	82.052587	75.885044
157.346336	47.028079	75.890049
155.567054	69.206205	75.895054
154.802826	66.688407	75.900058
154.341761	57.210974	75.905063
154.004498	59.297293	75.910068
153.713705	70.878263	75.915073
152.600446	64.945478	75.920078
151.767984	55.207160	75.925082
151.769194	55.831397	75.930087
150.895148	57.479783	75.935092
150.039935	46.581389	75.940097
149.080858	71.369307	75.945102
148.512251	65.065858	75.950106
148.131067	58.740416	75.955111
146.812844	69.652616	75.960116
146.478604	47.521306	75.965121
146.072903	41.475728	75.970126
145.452640	79.041977	75.975130
145.099092	41.919545	75.980135
143.912322	84.790742	75.985140
143.267781	37.469954	75.990145
142.811329	77.605562	75.995150
142.387182	65.110470	76.000154
141.567977	51.363287	76.005159
140.620694	58.372001	76.010164
140.212411	58.725657	76.015169
139.538755	55.546921	76.020174
138.371699	71.078824	76.025178
137.905432	60.968333	76.030183
137.427079	60.566815	76.035188
136.840318	43.745584	76.040193
135.674981	70.229954	76.045198
134.956808	57.103705	76.050202
134.938125	50.996422	76.055207
134.433474	64.647186	76.060212
133.856039	59.526207	76.065217
132.687066	75.580358	76.070222
131.869847	60.145632	76.075226
131.628326	53.681242	76.080231
130.852881	68.371748	76.085236
129.638782	61.890544	76.090241
129.268320	57.838781	76.095246
128.973785	66.566260	76.100250
128.565858	59.060877	76.105255
127.706988	57.611510	76.110260
126.807824	60.689375	76.115265
126.275528	69.569874	76.120270
125.806963	61.777711	76.125274
125.201798	60.630069	76.130279
124.171553	52.183197	76.135284
123.620689	62.176748	76.140289
123.073863	57.451412	76.145294
121.972673	59.434047	76.150298
121.538737	54.499914	76.155303
120.728451	61.849467	76.160308
120.447299	46.641504	76.165313
119.334791	60.890619	76.170318
118.697888	61.178235	76.175322
118.349701	46.772536	76.180327
117.548254	81.313335	76.185332
117.386478	42.545652	76.190337
116.333339	50.446394	76.195342
115.313223	67.314109	76.200346
115.461876	65.741948	76.205351
114.299899	65.298057	76.210356
113.446229	56.111878	76.215361
112.903468	62.496325	76.220366
112.423354	62.443576	76.225370
111.854968	60.963667	76.230375
110.469694	67.105585	76.235380
110.339757	46.469676	76.240385
109.433032	41.521055	76.245390
109.209640	62.949679	76.250394
108.982624	62.836076	76.255399
107.660182	58.611277	76.260404
106.934539	64.411494	76.265409
106.488877	65.031295	76.270414
105.783655	57.103422	76.275418
105.034362	54.515458	76.280423
104.315404	58.810301	76.285428
103.910882	58.549972	76.290433
103.044314	66.551857	76.295438
101.954169	55.741397	76.300442
101.625508	70.800609	76.305447
100.960065	55.478889	76.310452
100.665925	61.244994	76.315457
100.472111	53.853704	76.320462
99.384917	52.120655	76.325466
98.822962	72.929965	76.330471
97.821893	61.140272	76.335476
97.267956	37.862972	76.340481
96.049644	67.727074	76.345486
95.840325	66.636161	76.350490
94.952285	56.875193	76.355495
93.923713	58.541930	76.360500
93.224174	71.594618	76.365505
93.414664	54.515427	76.370510
92.655125	62.643739	76.375514
92.659911	49.247709	76.380519
91.258958	69.621555	76.385524
90.808044	53.705854	76.390529
89.898697	57.849722	76.395534
88.698504	68.962306	76.400538
88.309370	61.431859	76.405543
87.576408	66.195687	76.410548
87.204804	70.198624	76.415553
86.949600	60.019803	76.420558
86.114299	58.902560	76.425562
85.540148	65.102797	76.430567
84.931524	62.106082	76.435572
83.931548	57.423053	76.440577
83.185338	63.866753	76.445582
82.420684	65.090894	76.450586
82.368317	57.203998	76.455591
81.242063	62.049461	76.460596
80.121638	59.306234	76.465601
79.677788	62.234246	76.470606
79.218174	66.932413	76.475610
79.179221	53.466090	76.480615
78.098393	58.326385	76.485620
77.269938	54.294052	76.490625
76.553135	61.694936	76.495630
76.050025	79.486258	76.500634
75.397933	42.906597	76.505639
74.397418	74.777995	76.510644
73.926891	39.528630	76.515649
73.515772	71.518909	76.520654
72.437969	66.950788	76.525658
72.059561	34.644902	76.530663
70.813259	79.010957	76.535668
70.717030	40.537181	76.540673
70.254571	63.109286	76.545678
69.352818	44.904962	76.550682
68.815738	58.926722	76.555687
67.922021	44.532344	76.560692
67.404700	59.334643	76.565697
67.389855	64.628891	76.570702
66.124597	64.073768	76.575706
65.442509	58.278842	76.580711
64.734003	60.577325	76.585716
64.122512	55.928544	76.590721
63.185880	57.470254	76.595726
62.431377	55.774050	76.600730
62.135045	51.478685	76.605735
61.587191	49.929289	76.610740
61.049341	60.251907	76.615745
60.068775	49.775637	76.620750
59.236416	29.720100	76.625754
59.205014	60.099768	76.630759
58.306092	53.692919	76.635764
57.713029	39.594358	76.640769
57.191803	40.721344	76.645774
56.231927	61.586208	76.650778
55.328713	40.830802	76.655783
54.536878	57.688923	76.660788
54.166282	65.219095	76.665793
54.128966	35.772826	76.670798
53.283145	48.457771	76.675802
52.178384	59.192469	76.680807
51.417449	62.424922	76.685812
51.123088	30.614974	76.690817
50.233814	61.262323	76.695822
49.386817	49.971607	76.700826
48.873369	45.504304	76.705831
48.043861	58.087316	76.710836
47.674964	45.873597	76.715841
46.678940	61.428703	76.720846
46.519137	57.901564	76.725850
45.830727	43.416115	76.730855
44.339427	73.692753	76.735860
44.243883	60.011542	76.740865
43.575470	48.408520	76.745870
42.989967	63.489760	76.750874
42.976605	33.377407	76.755879
41.757475	66.459973	76.760884
41.085265	54.488571	76.765889
40.465779	41.242570	76.770894
39.485915	79.064830	76.775898
38.326419	46.405717	76.780903
37.871465	58.999957	76.785908
37.549647	54.103153	76.790913
37.197464	73.106641	76.795918
36.959520	50.438077	76.800922
36.334340	53.218406	76.805927
35.295273	64.112935	76.810932
34.497529	43.435328	76.815937
33.425558	48.940730	76.820942
32.886112	55.712560	76.825946
32.686841	37.095061	76.830951
31.937740	66.781849	76.835956
30.783463	55.790859	76.840961
30.159052	37.800939	76.845966
28.999067	68.642854	76.850970
29.184912	33.905396	76.855975
28.582749	73.097598	76.860980
28.112334	35.482989	76.865985
27.138374	66.952774	76.870990
26.664142	33.902159	76.875994
26.052907	59.839302	76.880999
25.059028	44.144259	76.886004
24.305814	51.880515	76.891009
24.386028	54.376475	76.896014
23.098275	48.009579	76.901018
22.256899	68.995900	76.906023
21.551753	50.591519	76.911028
20.911069	56.097526	76.916033
20.764786	56.693249	76.921038
20.123646	38.335443	76.926042
19.296841	69.201489	76.931047
18.232765	46.967444	76.936052
18.037868	59.826118	76.941057
17.956267	59.435460	76.946062
16.656741	41.531135	76.951066
16.015839	48.632936	76.956071
14.914710	56.793665	76.961076
13.899774	57.169981	76.966081
13.430811	33.402971	76.971086
12.915395	66.515225	76.976090
12.918829	53.944105	76.981095
12.385145	53.340141	76.986100
11.818233	60.108473	76.991105
11.175840	58.451171	76.996110
10.345724	57.579116	77.001114
9.190226	52.413185	77.006119
8.019176	47.495723	77.011124
7.754126	51.246721	77.016129
7.578264	47.566043	77.021134
6.820683	43.653314	77.026139
5.881757	45.605388	77.031143
4.768781	41.150143	77.036148
4.585086	59.166444	77.041153
4.210067	49.050909	77.046158