Mon Mar 08 19:56:47 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.520551	92.900835	0.000000
-0.974037	79.188405	0.005005
-1.561144	55.553735	0.010010
-3.116313	-5.147728	0.015014
-7.436376	-13.550687	0.020019
-12.412775	-11.766673	0.025024
-17.542896	-1.411684	0.030029
-22.154717	-4.000021	0.035034
-26.179085	-11.470898	0.040038
-30.453563	-4.324040	0.045043
-33.664345	-4.516712	0.050048
-37.031774	-6.568710	0.055053
-40.629098	-7.478670	0.060058
-44.632412	-5.487139	0.065062
-48.832691	9.188343	0.070067
-52.229378	-4.388784	0.075072
-55.815770	-12.637473	0.080077
-60.272270	-11.685291	0.085082
-62.968903	9.029298	0.090086
-67.115275	-5.546188	0.095091
-70.872980	-3.910738	0.100096
-74.697259	1.830376	0.105101
-78.677099	-3.168733	0.110106
-82.324170	-10.390643	0.115110
-86.124457	-4.913518	0.120115
-89.481900	-2.867268	0.125120
-93.526672	0.420807	0.130125
-97.436741	-2.694047	0.135130
-100.880556	-11.635566	0.140134
-105.059350	-5.918267	0.145139
-108.439459	-20.306852	0.150144
-112.421439	-14.365497	0.155149
-116.172064	3.052989	0.160154
-119.669004	-10.498571	0.165158
-123.666859	-3.286889	0.170163
-127.455288	-13.950474	0.175168
-131.258215	-11.063596	0.180173
-134.835191	0.384128	0.185178
-138.261421	-10.397151	0.190182
-142.470153	-9.006571	0.195187
-146.037914	-18.410751	0.200192
-149.910058	-25.092048	0.205197
-154.214823	-23.541057	0.210202
-157.610236	-15.252292	0.215206
-162.061183	-1.492206	0.220211
-165.602125	-12.706111	0.225216
-169.117272	-11.363084	0.230221
-172.877722	-15.818339	0.235226
-175.966055	-12.318501	0.240230
-180.270681	0.137882	0.245235
-183.684662	-7.767564	0.250240
-187.847350	-13.841087	0.255245
-191.851779	-10.653901	0.260250
-195.138895	5.426112	0.265254
-198.834303	-5.726829	0.270259
-202.810552	-12.853442	0.275264
-206.439524	-4.215122	0.280269
-210.017519	-7.701302	0.285274
-213.409840	-17.820872	0.290278
-217.685217	-9.806301	0.295283
-221.673459	-11.364755	0.300288
-225.287780	-16.771998	0.305293
-229.396057	-2.770042	0.310298
-232.547256	-13.495726	0.315302
-236.466998	-7.862127	0.320307
-240.461169	-3.236851	0.325312
-244.154803	-6.534226	0.330317
-247.914570	-13.622776	0.335322
-251.529088	-20.070653	0.340326
-255.482510	-5.416914	0.345331
-259.419792	-2.784340	0.350336
-262.688513	-7.084564	0.355341
-266.981704	-11.270151	0.360346
-270.112397	-11.246651	0.365350
-274.108613	-14.199238	0.370355
-277.784293	-22.417550	0.375360
-282.052306	-14.990630	0.380365
-285.741052	-1.843963	0.385370
-288.830024	-25.148398	0.390374
-292.829259	-4.274588	0.395379
-296.688554	-7.845035	0.400384
-300.588549	-19.386154	0.405389
-304.290902	-10.542037	0.410394
-307.994650	-9.220740	0.415398
-312.035117	-2.134413	0.420403
-315.410149	-11.116543	0.425408
-319.275697	-7.861439	0.430413
-323.135778	-6.590851	0.435418
-326.731650	-8.706888	0.440422
-330.812929	2.328059	0.445427
-334.657703	-10.499055	0.450432
-338.375417	-13.634753	0.455437
-342.139964	-15.438432	0.460442
-345.571575	-9.735943	0.465446
-349.761088	-8.887348	0.470451
-353.160679	-8.541713	0.475456
-356.546800	-12.553424	0.480461
-360.945847	-0.971001	0.485466
-364.220897	-15.040098	0.490470
-368.372455	-8.347499	0.495475
-372.206672	-7.311180	0.500480
-375.536844	-15.768987	0.505485
-379.889592	-10.926981	0.510490
-382.968346	-14.451604	0.515494
-386.845525	-6.413595	0.520499
-390.663225	-5.091324	0.525504
-394.850527	-7.816095	0.530509
-398.668341	-5.960825	0.535514
-401.720064	-8.149437	0.540518
-406.143891	-3.187233	0.545523
-409.594930	-7.071817	0.550528
-413.448939	-17.016448	0.555533
-417.336355	-9.208553	0.560538
-420.777618	-5.423416	0.565542
-424.669158	-2.042579	0.570547
-428.335754	-19.953279	0.575552
-432.199481	-9.424388	0.580557
-436.133062	-5.443933	0.585562
-439.753942	-22.384278	0.590566
-443.651475	-11.498341	0.595571
-447.278661	-14.891153	0.600576
-450.961438	-18.311348	0.605581
-454.779875	-8.089252	0.610586
-458.384161	-12.673054	0.615590
-462.412388	-10.864502	0.620595
-465.923489	-10.746886	0.625600
-469.621155	-6.696827	0.630605
-473.943354	-2.947541	0.635610
-477.151290	-16.475293	0.640614
-481.122771	-8.019990	0.645619
-484.785230	-13.843307	0.650624
-488.752157	-14.376625	0.655629
-492.448056	-3.445546	0.660634
-495.664479	-10.748185	0.665638
-499.819572	-8.160857	0.670643
-504.086309	-6.191151	0.675648
-507.633769	-12.838556	0.680653
-511.796627	-8.903358	0.685658
-514.742551	-20.579128	0.690662
-518.748503	-4.593652	0.695667
-522.476888	-12.823654	0.700672
-526.151861	-4.004084	0.705677
-530.341713	-8.382296	0.710682
-533.976194	-9.222506	0.715686
-537.260114	-19.032489	0.720691
-541.008227	-3.887612	0.725696
-544.953182	-17.953502	0.730701
-548.780519	-13.229808	0.735706
-552.489016	-13.591427	0.740710
-556.512874	-4.134239	0.745715
-560.230813	-15.517917	0.750720
-563.650667	-17.576558	0.755725
-567.828772	-7.329956	0.760730
-571.546483	-13.669391	0.765734
-575.174018	-12.257365	0.770739
-578.735998	-7.352101	0.775744
-582.434585	-15.298202	0.780749
-586.605756	-6.072881	0.785754
-589.944024	-10.913420	0.790758
-594.050893	-9.538327	0.795763
-598.082675	-15.419149	0.800768
-601.235747	-9.582623	0.805773
-605.475183	-5.964588	0.810778
-608.917020	-14.418401	0.815782
-612.597700	-4.180231	0.820787
-616.212290	-7.171126	0.825792
-620.013245	-7.416952	0.830797
-624.345457	-13.774815	0.835802
-627.707816	-11.156230	0.840806
-631.681099	-9.988479	0.845811
-635.549514	-6.271983	0.850816
-639.127988	-8.024498	0.855821
-643.045358	-6.747399	0.860826
-646.304954	-13.721251	0.865830
-650.149816	-4.708793	0.870835
-654.169421	-11.687356	0.875840
-657.940590	-0.381343	0.880845
-661.623299	-2.022562	0.885850
-665.271345	-19.382348	0.890854
-669.280957	-16.349658	0.895859
-673.161406	-1.214984	0.900864
-676.885211	-4.645614	0.905869
-680.698713	-14.881661	0.910874
-683.990355	-2.363967	0.915878
-687.741231	-4.591868	0.920883
-691.946627	-15.213095	0.925888
-695.697819	-19.047712	0.930893
-699.577245	-6.685219	0.935898
-702.994726	-13.986968	0.940902
-706.761126	-16.259661	0.945907
-710.531890	-15.414275	0.950912
-714.140555	-9.728714	0.955917
-718.365408	-12.735463	0.960922
-721.940574	-17.183166	0.965926
-725.744735	-2.894746	0.970931
-729.610797	-4.506557	0.975936
-733.098542	-6.655019	0.980941
-736.774382	-3.191467	0.985946
-740.224668	-10.532070	0.990950
-744.256745	-6.489651	0.995955
-748.354757	-6.094914	1.000960
-752.158838	-5.373437	1.005965
-755.716758	-6.433680	1.010970
-759.466663	-10.575881	1.015974
-763.222309	0.250029	1.020979
-767.064952	-2.160182	1.025984
-770.771344	-8.266155	1.030989
-774.494312	-14.716370	1.035994
-778.050088	-4.650876	1.040998
-782.038724	-7.252176	1.046003
-785.678076	-14.214012	1.051008
-789.639138	-16.745593	1.056013
-794.019020	1.786713	1.061018
-797.032462	-8.684234	1.066022
-801.063099	4.459462	1.071027
-804.685742	2.291670	1.076032
-808.373050	-11.535829	1.081037
-812.146537	-6.855019	1.086042
-815.505788	-7.502263	1.091046
-819.655626	7.827069	1.096051
-823.222201	0.803195	1.101056
-826.948407	-22.791176	1.106061
-830.993119	-8.831557	1.111066
-835.005256	-14.759251	1.116070
-838.561193	-9.190737	1.121075
-842.682738	-13.629756	1.126080
-845.973724	-6.714404	1.131085
-849.531902	-9.475852	1.136090
-853.235977	-17.858982	1.141094
-857.509120	-16.258177	1.146099
-861.168582	-22.371497	1.151104
-864.646741	-14.029142	1.156109
-868.890848	0.254131	1.161114
-871.894420	-15.137962	1.166118
-875.838854	-21.689786	1.171123
-879.967024	-14.241623	1.176128
-883.450400	-17.935836	1.181133
-887.386556	-12.096751	1.186138
-891.039298	-22.197293	1.191142
-894.638784	-12.862604	1.196147
-898.426705	-12.878272	1.201152
-902.534103	-18.714927	1.206157
-906.238170	-13.770706	1.211162
-909.702565	-25.616904	1.216166
-914.093289	-11.169790	1.221171
-917.755238	-4.923523	1.226176
-921.342312	-10.800764	1.231181
-924.889506	-11.129244	1.236186
-928.340840	-15.170682	1.241190
-932.368461	0.974995	1.246195
-936.222918	-14.719315	1.251200
-940.064821	-13.914224	1.256205
-943.830333	-27.528713	1.261210
-947.394677	-17.969355	1.266214
-951.368740	-11.371964	1.271219
-955.251533	-14.928094	1.276224
-958.618239	-19.205348	1.281229
-962.863257	-12.146757	1.286234
-966.259209	-19.320666	1.291238
-970.137108	-21.064212	1.296243
-973.955608	-21.248318	1.301248
-977.324117	-18.377548	1.306253
-981.480483	-10.672414	1.311258
-984.970507	-28.044286	1.316262
-989.365294	-10.767588	1.321267
-992.884340	-17.939117	1.326272
-996.313157	-32.551864	1.331277
-1000.437739	-1.402953	1.336282
-1003.631343	-18.852167	1.341286
-1007.880214	-20.698737	1.346291
-1011.554996	-14.007196	1.351296
-1015.336307	-23.561889	1.356301
-1018.950588	-14.428066	1.361306
-1022.779662	-27.999137	1.366310
-1026.348706	-15.230097	1.371315
-1030.408730	-13.424964	1.376320
-1034.031107	-9.632072	1.381325
-1037.898461	-18.081812	1.386330
-1041.393990	-33.243584	1.391334
-1045.394084	-9.478253	1.396339
-1049.461117	0.231038	1.401344
-1052.883687	-16.620134	1.406349
-1056.911336	-21.166813	1.411354
-1060.009283	-21.864957	1.416358
-1063.795261	-11.166212	1.421363
-1067.822281	-13.697805	1.426368
-1071.626445	-17.695206	1.431373
-1075.606497	-11.878755	1.436378
-1079.291001	-20.308786	1.441382
-1083.228877	-24.466112	1.446387
-1086.803530	-15.193463	1.451392
-1090.554874	-5.835775	1.456397
-1094.293885	-17.428040	1.461402
-1097.880500	-23.631466	1.466406
-1101.702685	-22.058203	1.471411
-1105.605736	-14.620442	1.476416
-1109.768719	-13.558728	1.481421
-1113.333538	-4.647121	1.486426
-1116.702929	-31.260852	1.491430
-1120.157437	-12.735714	1.496435
-1123.971355	-21.436679	1.501440
-1127.927753	-22.158242	1.506445
-1132.037019	-18.613716	1.511450
-1135.939934	-24.544151	1.516454
-1139.760049	-8.521238	1.521459
-1142.938785	-18.744494	1.526464
-1146.668012	-13.573550	1.531469
-1150.880953	-15.032979	1.536474
-1154.391747	-18.069590	1.541478
-1158.307900	-12.611702	1.546483
-1162.043191	-10.937135	1.551488
-1165.229078	-14.326882	1.556493
-1169.285769	-16.804667	1.561498
-1173.249078	-18.253535	1.566502
-1177.253839	-9.006549	1.571507
-1181.103636	-3.259643	1.576512
-1184.639091	-19.936427	1.581517
-1188.464187	-11.132871	1.586522
-1191.634711	-14.879822	1.591526
-1195.461771	-13.718751	1.596531
-1199.543524	-4.699083	1.601536
-1203.172244	-15.469942	1.606541
-1207.271742	-13.230872	1.611546
-1210.689352	-23.707513	1.616550
-1214.615753	-17.058979	1.621555
-1218.866493	-11.255746	1.626560
-1222.072634	-23.087575	1.631565
-1225.829623	-11.164889	1.636570
-1229.371373	-16.366125	1.641574
-1233.462893	-17.608310	1.646579
-1237.353305	-32.785407	1.651584
-1240.895032	-18.071506	1.656589
-1245.147110	4.495086	1.661594
-1248.534772	-15.734153	1.666598
-1252.238711	-22.196075	1.671603
-1255.418541	-16.665065	1.676608
-1259.677408	-23.172201	1.681613
-1263.464606	-9.942177	1.686618
-1267.167363	-15.087629	1.691622
-1270.935608	-2.273745	1.696627
-1274.987491	-21.381168	1.701632
-1278.585527	-19.383060	1.706637
-1282.154030	-19.436372	1.711642
-1285.555120	-26.285717	1.716646
-1289.955188	-10.502480	1.721651
-1294.098618	-10.260355	1.726656
-1297.368134	-10.602747	1.731661
-1301.628009	-9.745937	1.736666
-1304.874528	-22.758517	1.741670
-1308.335923	-27.203001	1.746675
-1312.090737	-13.402556	1.751680
-1315.972985	-14.110436	1.756685
-1319.991589	-17.004020	1.761690
-1323.283627	-23.490752	1.766694
-1327.545784	-20.250970	1.771699
-1331.267860	-15.080885	1.776704
-1334.956828	-17.385441	1.781709
-1338.755666	-13.401432	1.786714
-1342.562615	-18.817060	1.791718
-1346.258631	-16.003722	1.796723
-1349.847528	-19.849046	1.801728
-1353.733676	-23.779235	1.806733
-1357.523143	-12.470841	1.811738
-1361.221683	-18.514015	1.816742
-1365.143036	-18.354614	1.821747
-1368.870292	-9.689430	1.826752
-1372.167445	-28.305661	1.831757
-1376.335418	-15.840770	1.836762
-1380.055253	-31.265663	1.841766
-1383.666018	-25.984020	1.846771
-1388.208409	-21.199725	1.851776
-1391.513699	-29.128586	1.856781
-1395.176568	-18.460090	1.861786
-1398.769809	-24.490096	1.866790
-1402.900356	-27.302537	1.871795
-1406.555439	-18.205772	1.876800
-1410.165088	-28.009586	1.881805
-1414.310895	-9.548422	1.886810
-1417.631932	-20.475395	1.891814
-1420.955965	-18.229225	1.896819
-1425.054637	-13.582120	1.901824
-1428.801707	-26.774540	1.906829
-1433.047401	-16.247622	1.911834
-1436.762067	-23.546378	1.916838
-1440.233595	-8.233209	1.921843
-1444.162797	-16.640795	1.926848
-1447.864297	-33.668960	1.931853
-1451.746147	-19.997772	1.936858
-1455.213519	-26.120371	1.941862
-1459.064338	-20.281408	1.946867
-1462.626478	-11.136363	1.951872
-1466.218100	-17.841396	1.956877
-1470.737535	-8.029021	1.961882
-1474.373710	-8.753959	1.966886
-1477.959305	-16.789186	1.971891
-1481.697894	-27.032663	1.976896
-1485.149940	-19.904610	1.981901
-1489.205698	-9.089488	1.986906
-1493.130425	-19.470287	1.991910
-1496.812378	-17.767460	1.996915
-1500.889608	-16.826165	2.006912
-1501.552374	-16.869989	2.016909
-1498.876608	-8.692242	2.026906
-1496.196665	-9.184497	2.036902
-1494.070634	-17.032219	2.046899
-1492.042981	-15.471748	2.056896
-1490.440233	-12.704902	2.066893
-1488.611074	-10.369016	2.076890
-1486.603026	-17.841024	2.086886
-1484.569690	-16.197778	2.096883
-1482.610666	-17.326103	2.106880
-1480.877474	-18.842969	2.116877
-1479.031103	-13.210084	2.126874
-1477.081879	-7.860487	2.136870
-1475.156331	-21.265136	2.146867
-1473.090981	-16.810381	2.156864
-1471.408429	-10.652349	2.166861
-1469.607746	-13.340452	2.176858
-1467.478205	-20.951887	2.186854
-1465.636033	-23.231397	2.196851
-1463.605809	-18.777324	2.206848
-1461.976888	-15.004200	2.216845
-1459.956335	-14.031466	2.226842
-1458.165319	-15.186549	2.236838
-1456.377362	-14.096050	2.246835
-1454.187266	-14.680339	2.256832
-1452.512764	-12.943298	2.266829
-1450.603250	-9.977663	2.276826
-1448.868814	-22.417030	2.286822
-1446.810078	-13.346279	2.296819
-1445.009833	-14.826490	2.306816
-1442.963480	-18.493307	2.316813
-1441.169219	-22.973906	2.326810
-1439.497807	-23.577761	2.336806
-1437.150316	-10.606164	2.346803
-1435.409435	-14.293537	2.356800
-1433.517086	-17.732021	2.366797
-1431.631751	-12.931060	2.376794
-1430.124595	-17.274114	2.386790
-1428.082237	-12.081479	2.396787
-1426.261288	-14.128632	2.406784
-1424.331173	-23.525332	2.416781
-1422.322677	-17.932566	2.426778
-1420.373130	-15.350655	2.436774
-1418.565198	-10.873580	2.446771
-1416.599772	-15.242629	2.456768
-1414.886439	-22.942112	2.466765
-1413.248715	-10.860992	2.476762
-1410.880368	-16.570233	2.486758
-1409.044261	-12.023457	2.496755
-1407.268369	-11.019401	2.506752
-1405.618691	-19.327590	2.516749
-1403.763055	-12.643045	2.526746
-1401.772351	-24.562922	2.536742
-1399.630671	-17.178962	2.546739
-1397.867182	-20.276287	2.556736
-1396.067359	-16.383642	2.566733
-1394.189188	-16.876891	2.576730
-1392.468611	-9.548656	2.586726
-1390.640282	-19.547941	2.596723
-1388.405455	-15.612829	2.606720
-1386.490744	-10.500765	2.616717
-1384.762627	-15.648053	2.626714
-1382.926476	-22.735645	2.636710
-1380.932890	-11.762964	2.646707
-1379.408446	-12.177472	2.656704
-1377.403597	-16.968032	2.666701
-1375.515971	-11.900566	2.676698
-1373.258510	-10.228365	2.686694
-1371.505290	-10.570550	2.696691
-1369.649866	-18.591150	2.706688
-1368.006413	-17.922679	2.716685
-1366.007018	-15.385013	2.726682
-1364.183773	-19.519696	2.736678
-1362.277457	-21.788869	2.746675
-1360.349689	-22.466858	2.756672
-1358.460379	-11.041706	2.766669
-1356.561800	-18.480300	2.776666
-1354.801649	0.223414	2.786662
-1353.011796	-19.956296	2.796659
-1350.855404	-10.468481	2.806656
-1348.934982	-16.772231	2.816653
-1347.256270	-2.214111	2.826650
-1345.383414	-5.688879	2.836646
-1343.603595	-9.245062	2.846643
-1341.434204	-14.336647	2.856640
-1339.787102	-18.626262	2.866637
-1337.790979	-9.220140	2.876634
-1335.905761	-15.396676	2.886630
-1334.179258	-14.593064	2.896627
-1332.279387	-20.992977	2.906624
-1330.359904	-9.623149	2.916621
-1328.495384	-13.461278	2.926618
-1326.536637	-6.752116	2.936614
-1324.500305	-23.883064	2.946611
-1322.720621	-13.395525	2.956608
-1321.101750	-8.596025	2.966605
-1319.086913	-7.620671	2.976602
-1316.980232	-14.367862	2.986598
-1315.228044	-13.151536	2.996595
-1313.617093	-9.583829	3.006592
-1311.362454	-12.867061	3.016589
-1309.603123	-17.485648	3.026586
-1308.084892	-8.367720	3.036582
-1306.065593	-12.614260	3.046579
-1303.931939	-6.360934	3.056576
-1302.058180	-8.992717	3.066573
-1300.229018	-6.063036	3.076570
-1298.458664	-11.325966	3.086566
-1296.446376	-13.229970	3.096563
-1294.746078	-9.605501	3.106560
-1292.758305	0.174611	3.116557
-1290.875409	-9.961231	3.126554
-1289.005300	-21.365976	3.136550
-1287.032823	-6.523266	3.146547
-1285.104398	-11.282575	3.156544
-1283.576806	-8.588808	3.166541
-1281.831090	-6.582003	3.176538
-1279.625815	-9.641007	3.186534
-1277.632851	-9.790980	3.196531
-1275.534083	-7.131776	3.206528
-1274.166450	3.230722	3.216525
-1272.180091	-1.381547	3.226522
-1270.464040	3.220877	3.236518
-1268.385780	-6.674656	3.246515
-1266.509718	0.189891	3.256512
-1264.601392	-11.361477	3.266509
-1262.661218	-2.967828	3.276506
-1260.590474	-0.059405	3.286502
-1258.856109	-7.140100	3.296499
-1257.614445	-8.893912	3.306496
-1255.288479	-6.724171	3.316493
-1253.369089	-5.566129	3.326490
-1251.398744	-17.057940	3.336486
-1249.486637	-7.207265	3.346483
-1247.828348	-10.769192	3.356480
-1245.985676	-8.834714	3.366477
-1243.963464	-7.440504	3.376474
-1242.086767	-4.627321	3.386470
-1240.029827	-7.064174	3.396467
-1238.325912	-11.395971	3.406464
-1236.363901	-9.898972	3.416461
-1234.844094	-12.756674	3.426458
-1233.042927	-6.075892	3.436454
-1230.902026	-17.411834	3.446451
-1228.670904	-14.432739	3.456448
-1227.112766	-4.615396	3.466445
-1225.385786	-13.190037	3.476442
-1223.394295	-3.697803	3.486438
-1221.265604	-7.240252	3.496435
-1219.323561	-10.386544	3.506432
-1217.778488	-9.814320	3.516429
-1215.592912	-1.998275	3.526426
-1214.126114	-15.469865	3.536422
-1212.283223	-20.412782	3.546419
-1210.172689	-9.548637	3.556416
-1208.354723	-9.512667	3.566413
-1206.641653	-13.662761	3.576410
-1204.131960	-9.577245	3.586406
-1202.580000	-13.066869	3.596403
-1200.795971	-11.366111	3.606400
-1199.169182	-3.964290	3.616397
-1197.260307	-17.217676	3.626394
-1195.404945	-4.144948	3.636390
-1193.235317	-4.444685	3.646387
-1191.022112	-17.131014	3.656384
-1189.516614	-10.863909	3.666381
-1187.642975	-11.912015	3.676378
-1185.775031	-5.505541	3.686374
-1184.080681	-16.138468	3.696371
-1182.218213	-17.184782	3.706368
-1179.867733	-4.952252	3.716365
-1178.443688	-9.035562	3.726362
-1176.622422	-14.511798	3.736358
-1174.453658	-6.917218	3.746355
-1172.516039	-13.212535	3.756352
-1171.005933	-5.061026	3.766349
-1169.046465	-11.494038	3.776346
-1166.802170	-9.735846	3.786342
-1164.945970	-10.639049	3.796339
-1163.270562	-15.285157	3.806336
-1161.413506	-6.442360	3.816333
-1159.720960	-7.750399	3.826330
-1157.794333	-8.008069	3.836326
-1155.681444	-16.357055	3.846323
-1153.723316	-6.996776	3.856320
-1152.226470	-14.950384	3.866317
-1150.209391	-9.554509	3.876314
-1148.324042	-7.955176	3.886310
-1146.268265	-14.804600	3.896307
-1144.474456	-10.858683	3.906304
-1142.494694	-2.333897	3.916301
-1140.660077	-13.841808	3.926298
-1138.879602	-9.064866	3.936294
-1137.220749	-7.590331	3.946291
-1135.147246	-10.560231	3.956288
-1133.257065	-9.845805	3.966285
-1131.622949	-1.235716	3.976282
-1129.549225	-0.744844	3.986278
-1127.405092	-8.192559	3.996275
-1125.640380	-10.922015	4.006272
-1123.699983	1.654060	4.016269
-1121.882327	-14.199236	4.026266
-1120.341636	-8.807647	4.036262
-1118.397929	-9.649028	4.046259
-1116.321457	-6.896115	4.056256
-1114.247121	-4.509148	4.066253
-1112.682607	-3.387372	4.076250
-1110.785732	-1.330409	4.086246
-1108.851031	-10.236605	4.096243
-1107.238030	-9.360985	4.106240
-1105.122589	-16.625679	4.116237
-1103.351844	-10.956690	4.126234
-1101.190125	-12.682342	4.136230
-1099.674156	-6.004770	4.146227
-1097.432501	-23.942034	4.156224
-1095.846312	-9.031028	4.166221
-1093.847134	-10.468587	4.176218
-1092.008757	-16.842697	4.186214
-1090.074461	-18.599851	4.196211
-1087.898611	-18.232639	4.206208
-1086.472181	-20.680604	4.216205
-1084.387533	-19.757261	4.226202
-1082.517398	-21.630452	4.236198
-1080.880591	-23.400010	4.246195
-1078.909948	-23.899902	4.256192
-1076.747885	-15.754721	4.266189
-1075.107512	-15.497623	4.276186
-1073.271836	-21.020295	4.286182
-1071.467941	-21.010387	4.296179
-1069.264943	-14.962120	4.306176
-1067.551648	-10.461723	4.316173
-1065.544219	-11.523237	4.326170
-1063.708398	-15.833382	4.336166
-1062.115395	-11.811074	4.346163
-1060.019212	-17.997464	4.356160
-1058.132555	-8.996691	4.366157
-1056.827897	-9.289001	4.376154
-1054.560915	-4.705055	4.386150
-1052.560458	-8.296315	4.396147
-1050.511375	-8.710841	4.406144
-1048.742439	-14.972770	4.416141
-1047.051885	-13.383248	4.426138
-1044.928567	-13.970682	4.436134
-1043.235450	-10.090679	4.446131
-1041.397743	-16.761467	4.456128
-1039.238351	-15.774252	4.466125
-1037.531558	-14.209424	4.476122
-1035.709285	-10.781093	4.486118
-1033.893634	-18.007255	4.496115
-1032.219042	-21.191143	4.506112
-1030.172000	-15.567862	4.516109
-1028.056779	-9.549721	4.526106
-1026.217877	-20.133041	4.536102
-1024.258716	-16.562395	4.546099
-1022.343137	-20.076900	4.556096
-1020.909283	-11.909932	4.566093
-1019.065699	-16.012879	4.576090
-1016.982357	-19.944182	4.586086
-1014.958848	-6.334532	4.596083
-1012.831785	-17.868601	4.606080
-1011.094416	-15.740262	4.616077
-1009.435435	-13.103633	4.626074
-1007.657333	-18.961237	4.636070
-1005.732189	-17.069750	4.646067
-1003.929278	-16.530723	4.656064
-1001.987172	-17.081246	4.666061
-999.846703	-18.102404	4.676058
-998.090025	-12.026898	4.686054
-996.460156	-21.124241	4.696051
-994.349574	-18.190371	4.706048
-992.432843	-20.317242	4.716045
-990.622329	-17.591155	4.726042
-989.029848	-23.562735	4.736038
-986.757763	-27.284210	4.746035
-984.786542	-26.412109	4.756032
-983.036862	-24.050472	4.766029
-981.348436	-22.770014	4.776026
-979.495521	-19.393904	4.786022
-977.436052	-14.211477	4.796019
-975.733691	-16.851912	4.806016
-973.908534	-21.307116	4.816013
-971.908308	-14.059567	4.826010
-969.860407	-17.999373	4.836006
-968.018206	-18.871764	4.846003
-966.319928	-17.570765	4.856000
-964.435481	-12.833990	4.865997
-962.704287	-13.753359	4.875994
-960.522908	-22.062613	4.885990
-958.457793	-16.421630	4.895987
-956.781817	-17.736347	4.905984
-955.063637	-9.758468	4.915981
-953.481632	-15.035245	4.925978
-951.347428	-12.629284	4.935974
-949.237100	-10.598424	4.945971
-947.502531	-13.872367	4.955968
-945.472392	-9.820401	4.965965
-943.359303	-11.822325	4.975962
-942.028040	-4.245166	4.985958
-939.965701	-11.021270	4.995955
-938.377302	-9.833726	5.005952
-936.346142	-14.427624	5.015949
-934.324588	-14.177693	5.025946
-932.450644	-14.763047	5.035942
-930.333688	-13.750000	5.045939
-928.834329	-14.147574	5.055936
-926.723450	-12.375711	5.065933
-925.213830	-17.271449	5.075930
-923.485349	-16.922550	5.085926
-921.159430	-12.543670	5.095923
-919.029045	-13.282110	5.105920
-917.142069	-22.283154	5.115917
-915.723580	-6.091584	5.125914
-913.954409	-13.493379	5.135910
-911.888799	-15.985018	5.145907
-909.725547	-17.462864	5.155904
-908.006723	-14.363655	5.165901
-906.267809	-16.035743	5.175898
-904.247796	-17.601202	5.185894
-902.555747	-17.761164	5.195891
-900.704720	-17.082917	5.205888
-898.839403	-19.705143	5.215885
-896.694189	-14.264788	5.225882
-894.987639	-20.372962	5.235878
-893.154658	-12.934402	5.245875
-891.141788	-19.227325	5.255872
-889.216138	-21.494477	5.265869
-887.381938	-12.112559	5.275866
-885.682518	-23.096613	5.285862
-883.749394	-19.471160	5.295859
-881.947922	-22.642074	5.305856
-879.736417	-18.319066	5.315853
-877.923611	-22.704336	5.325850
-876.452102	-6.816455	5.335846
-874.375077	-8.577306	5.345843
-872.503944	-12.095644	5.355840
-870.419521	-7.873879	5.365837
-868.840666	-5.546418	5.375834
-866.817643	-11.981464	5.385830
-864.636431	-15.078870	5.395827
-863.045028	-6.013352	5.405824
-861.310545	-13.461669	5.415821
-859.325374	-12.424333	5.425818
-857.386575	-16.783943	5.435814
-855.598167	-14.242095	5.445811
-853.622782	-9.230833	5.455808
-851.601748	-7.398752	5.465805
-850.126299	-12.885786	5.475802
-848.321286	-7.259957	5.485798
-846.018989	-15.048485	5.495795
-844.163528	-16.164461	5.505792
-842.695952	-10.811509	5.515789
-840.412845	-16.236600	5.525786
-838.709085	-8.415782	5.535782
-836.639855	-14.520318	5.545779
-835.034635	-9.975623	5.555776
-833.212969	-18.262008	5.565773
-831.117480	-9.060742	5.575770
-829.092703	-5.025180	5.585766
-827.345041	-10.974106	5.595763
-825.569929	-16.951098	5.605760
-823.969895	-12.883955	5.615757
-821.982845	-12.581047	5.625754
-819.727655	-9.338571	5.635750
-817.887366	-16.194338	5.645747
-816.017461	-20.247661	5.655744
-814.277029	-18.631206	5.665741
-812.346044	-12.545517	5.675738
-810.556297	-18.392215	5.685734
-808.470120	-14.053841	5.695731
-806.870987	-13.177374	5.705728
-804.926467	-12.768187	5.715725
-803.029125	-11.683609	5.725722
-801.269397	-9.714988	5.735718
-799.260997	-19.231114	5.745715
-797.462286	-9.060339	5.755712
-795.553305	-10.778475	5.765709
-793.652668	-16.916025	5.775706
-791.761674	-13.285336	5.785702
-789.651379	-9.588648	5.795699
-787.879971	-16.482329	5.805696
-786.133305	-12.729100	5.815693
-784.310891	-13.752913	5.825690
-782.660009	-7.742420	5.835686
-780.092057	-16.706953	5.845683
-778.607654	-12.504462	5.855680
-776.628235	-11.775589	5.865677
-774.847152	-12.282823	5.875674
-772.932333	-12.555658	5.885670
-771.466896	-5.146664	5.895667
-769.075316	-10.465879	5.905664
-767.200060	-16.643561	5.915661
-765.410269	-19.146254	5.925658
-763.801832	-13.212644	5.935654
-761.923896	-6.226385	5.945651
-760.106472	-6.493117	5.955648
-757.711871	-6.286864	5.965645
-755.917301	-9.717094	5.975642
-754.345296	-5.834880	5.985638
-752.329679	-3.161901	5.995635
-750.120686	-9.915505	6.005632
-748.812771	-2.962866	6.015629
-746.846374	3.537201	6.025626
-745.071422	-6.598384	6.035622
-743.085178	0.471632	6.045619
-741.054965	-4.031965	6.055616
-739.098901	-4.914481	6.065613
-737.104679	-8.567643	6.075610
-735.364189	-4.169219	6.085606
-733.598346	-1.483149	6.095603
-731.849384	-7.403801	6.105600
-729.785401	-4.135415	6.115597
-727.863173	0.066618	6.125594
-726.105410	-6.846949	6.135590
-724.424729	-0.828540	6.145587
-722.123588	-5.896433	6.155584
-720.180920	-11.707513	6.165581
-718.747843	-4.457509	6.175578
-716.906916	-6.390484	6.185574
-714.782412	-8.881894	6.195571
-712.908842	-12.514178	6.205568
-711.094807	-13.913938	6.215565
-709.124284	-7.886576	6.225562
-707.460147	-7.022006	6.235558
-705.422050	-10.383752	6.245555
-703.654126	-12.661869	6.255552
-701.570165	-8.401981	6.265549
-699.873255	-5.696977	6.275546
-697.799418	-4.342113	6.285542
-695.850911	-4.988139	6.295539
-694.150133	-11.695222	6.305536
-692.844490	-6.534171	6.315533
-690.611830	-6.009888	6.325530
-688.529682	-6.014148	6.335526
-686.531355	-15.904346	6.345523
-684.418802	-11.745321	6.355520
-682.999369	-10.107474	6.365517
-681.182271	-5.719669	6.375514
-679.221875	-3.205160	6.385510
-677.016905	-9.274420	6.395507
-675.391239	-6.952725	6.405504
-673.698226	-1.479368	6.415501
-671.716906	-7.260275	6.425498
-669.897645	2.656301	6.435494
-667.805526	-8.271965	6.445491
-665.733294	-1.245615	6.455488
-663.999196	-7.689601	6.465485
-662.567216	-10.040321	6.475482
-660.491032	-6.426476	6.485478
-658.658533	-1.647981	6.495475
-656.780875	-7.772290	6.505472
-654.461462	-1.979026	6.515469
-653.001816	-0.835447	6.525466
-651.214959	-7.458368	6.535462
-649.026347	-7.574334	6.545459
-647.090543	-13.524777	6.555456
-645.572291	-8.096107	6.565453
-643.562451	-8.725049	6.575450
-641.327683	-5.188624	6.585446
-640.015692	-10.044730	6.595443
-637.906648	-7.956541	6.605440
-635.983053	-8.606432	6.615437
-634.440225	-13.303636	6.625434
-632.097179	-8.450381	6.635430
-630.423412	-7.191006	6.645427
-628.463039	-5.901632	6.655424
-626.594189	-10.238840	6.665421
-624.926561	-5.685014	6.675418
-622.851796	-9.998277	6.685414
-620.803737	-8.048740	6.695411
-619.265586	-9.050698	6.705408
-617.148805	-12.047598	6.715405
-615.309211	-12.177244	6.725402
-613.811134	-6.189576	6.735398
-611.784034	-1.625275	6.745395
-609.539759	-7.975474	6.755392
-607.848581	-2.061277	6.765389
-605.869484	-7.816516	6.775386
-604.040121	-8.102403	6.785382
-602.128538	-3.235449	6.795379
-600.568155	-8.216474	6.805376
-598.589107	-5.161754	6.815373
-596.566463	-3.264973	6.825370
-594.731437	-9.483472	6.835366
-592.847530	-8.966539	6.845363
-590.898535	-11.586111	6.855360
-588.969704	-14.197723	6.865357
-587.489845	-7.056150	6.875354
-585.555239	-15.894059	6.885350
-583.484605	-6.859091	6.895347
-581.442659	-13.042743	6.905344
-579.796646	-7.880734	6.915341
-577.833442	-14.594926	6.925338
-576.001892	-9.018898	6.935334
-574.219966	-5.312184	6.945331
-572.373683	-8.518453	6.955328
-570.078773	-8.545543	6.965325
-568.360853	-11.758144	6.975322
-566.614057	-8.511573	6.985318
-564.641856	-8.968658	6.995315
-562.795823	-4.242769	7.005312
-560.952306	-14.022891	7.015309
-559.395135	-8.480385	7.025306
-557.409687	-14.152921	7.035302
-555.241929	-16.947923	7.045299
-553.609971	-14.456633	7.055296
-551.543098	-6.278345	7.065293
-549.617528	-14.064855	7.075290
-547.550320	-8.744324	7.085286
-546.027841	-10.367375	7.095283
-544.064948	-8.478372	7.105280
-542.132707	-5.394024	7.115277
-540.509299	-10.503492	7.125274
-538.666896	-8.317364	7.135270
-536.498625	-10.182493	7.145267
-534.637621	-11.610149	7.155264
-532.909872	-10.630887	7.165261
-531.054697	-6.819004	7.175258
-528.886490	-5.944823	7.185254
-527.339821	-3.482519	7.195251
-525.240800	-12.761883	7.205248
-523.317293	-16.823550	7.215245
-521.469759	-8.569153	7.225242
-519.790281	-7.639010	7.235238
-517.919831	-13.215785	7.245235
-515.747335	-12.380169	7.255232
-513.954110	-13.497003	7.265229
-512.225902	-10.342152	7.275226
-510.359480	-12.095896	7.285222
-508.426984	-12.297136	7.295219
-506.742917	-14.388045	7.305216
-504.600491	-11.782469	7.315213
-502.896694	-4.509242	7.325210
-500.750305	-11.484724	7.335206
-498.887788	-10.741682	7.345203
-497.373544	-5.130700	7.355200
-495.271436	-6.099495	7.365197
-493.291408	-6.950904	7.375194
-491.553553	-9.416686	7.385190
-489.758672	-1.509088	7.395187
-488.009120	-11.826753	7.405184
-485.674744	-11.798490	7.415181
-483.990766	-8.401305	7.425178
-482.056481	-10.710567	7.435174
-480.490626	-8.292346	7.445171
-478.355107	-15.375012	7.455168
-476.544411	-12.778009	7.465165
-474.606576	-16.619310	7.475162
-472.774200	-11.273840	7.485158
-471.199609	-15.796031	7.495155
-468.724320	-18.147468	7.505152
-467.142505	-13.942957	7.515149
-465.503114	-8.759281	7.525146
-463.224358	-18.147817	7.535142
-461.504497	-19.677605	7.545139
-459.753266	-14.810189	7.555136
-457.656897	-13.498182	7.565133
-455.399157	-11.654610	7.575130
-454.282990	-15.795712	7.585126
-452.339088	-14.846171	7.595123
-450.425023	-18.868382	7.605120
-448.347283	-16.047175	7.615117
-446.378307	-13.754879	7.625114
-444.660744	-13.910694	7.635110
-442.680067	-15.785256	7.645107
-440.799872	-19.721530	7.655104
-438.970204	-20.564673	7.665101
-437.097006	-17.492914	7.675098
-435.137947	-14.613273	7.685094
-433.460426	-4.100741	7.695091
-431.298033	-18.864007	7.705088
-429.672307	-13.108161	7.715085
-428.071756	-15.733541	7.725082
-426.067001	-14.495293	7.735078
-423.834781	-13.574398	7.745075
-422.009993	-18.908563	7.755072
-420.318915	-16.425040	7.765069
-418.385789	-5.719640	7.775066
-416.350763	-23.162381	7.785062
-414.476823	-17.038816	7.795059
-412.651181	-14.889384	7.805056
-410.970613	-13.447791	7.815053
-408.894445	-9.726354	7.825050
-407.077005	-4.831572	7.835046
-405.124764	-12.982214	7.845043
-403.221288	-19.502012	7.855040
-401.444995	-14.636972	7.865037
-399.838553	-18.302154	7.875034
-397.768378	-7.678614	7.885030
-395.646891	-15.927319	7.895027
-394.046886	-17.082684	7.905024
-392.118030	-25.043273	7.915021
-390.345442	-18.008301	7.925018
-388.487886	-12.219968	7.935014
-386.743528	-13.810455	7.945011
-384.402845	-15.641401	7.955008
-382.469260	-10.938816	7.965005
-381.021449	-10.437347	7.975002
-378.938599	-7.526898	7.984998
-376.956815	-14.445999	7.994995
-374.822046	-15.334645	8.004992
-373.620332	-11.983535	8.014989
-371.550117	-11.810361	8.024986
-369.408776	-6.586757	8.034982
-367.684839	-14.841440	8.044979
-365.953097	-11.597049	8.054976
-363.999032	-11.762144	8.064973
-362.216190	-7.417556	8.074970
-360.337834	-16.592093	8.084966
-358.052567	-14.635987	8.094963
-356.270126	-14.461066	8.104960
-354.384631	-17.160307	8.114957
-352.541777	-7.921395	8.124954
-351.148031	-15.709696	8.134950
-348.842314	-19.972765	8.144947
-347.225670	-14.809054	8.154944
-345.268914	-12.491038	8.164941
-343.547177	-14.472595	8.174938
-341.177683	-10.952650	8.184934
-339.603913	-3.208564	8.194931
-337.574709	-18.533094	8.204928
-335.871677	-12.860567	8.214925
-333.988602	-4.084344	8.224922
-332.077169	-12.484193	8.234918
-330.220063	-4.737966	8.244915
-328.307634	-15.788855	8.254912
-326.221443	-12.968887	8.264909
-324.662582	-3.201485	8.274906
-322.652902	-9.435044	8.284902
-320.427093	-16.923548	8.294899
-319.069490	-13.567295	8.304896
-317.402286	-14.548612	8.314893
-315.214789	-11.676915	8.324890
-313.131036	-9.745436	8.334886
-311.380952	-9.881086	8.344883
-309.494582	-21.494605	8.354880
-307.688515	-14.404911	8.364877
-305.746652	-16.817869	8.374874
-303.993603	-4.124268	8.384870
-301.809706	-15.073218	8.394867
-300.258746	-11.282058	8.404864
-298.502817	-18.782376	8.414861
-295.967666	-16.041939	8.424858
-294.753985	-6.402566	8.434854
-292.861381	-13.604193	8.444851
-290.659166	-17.683330	8.454848
-288.544201	-7.249979	8.464845
-287.155048	-9.486286	8.474842
-285.261105	-11.188993	8.484838
-283.320706	-8.419920	8.494835
-281.131285	-7.585211	8.504832
-279.777259	-11.674212	8.514829
-277.718984	-13.204207	8.524826
-275.695182	-6.610259	8.534822
-273.906975	-15.899814	8.544819
-271.985702	-8.425870	8.554816
-269.836964	-14.353181	8.564813
-268.082978	-13.376333	8.574810
-266.370658	-8.115734	8.584807
-264.741292	-2.257717	8.594803
-262.907509	-10.449348	8.604800
-260.618938	-20.696592	8.614797
-258.764331	-14.961362	8.624794
-257.085894	-8.473319	8.634791
-255.132674	-15.899316	8.644787
-253.245948	-18.224491	8.654784
-251.518423	-16.075061	8.664781
-249.320218	-19.146217	8.674778
-247.599067	-20.753426	8.684775
-245.906380	-18.461072	8.694771
-243.702622	-13.850433	8.704768
-241.852168	-18.631235	8.714765
-240.197356	-17.731692	8.724762
-237.745995	-23.721480	8.734759
-236.398630	-13.348722	8.744755
-234.512372	-21.913416	8.754752
-232.571799	-19.479047	8.764749
-230.671644	-19.565961	8.774746
-228.878668	-19.190534	8.784743
-226.901163	-12.458112	8.794739
-225.009833	-19.908943	8.804736
-223.107180	-19.931517	8.814733
-221.480357	-15.528766	8.824730
-219.696173	-16.364485	8.834727
-217.526107	-18.932206	8.844723
-215.522460	-17.185214	8.854720
-214.019018	-24.501506	8.864717
-212.141195	-18.566272	8.874714
-210.251362	-19.740929	8.884711
-208.609478	-18.275652	8.894707
-206.062194	-28.789907	8.904704
-204.369087	-25.082944	8.914701
-202.796059	-24.726079	8.924698
-200.885043	-23.425317	8.934695
-198.562180	-23.832278	8.944691
-196.756896	-24.248215	8.954688
-195.138704	-23.448580	8.964685
-193.004691	-18.635724	8.974682
-191.470676	-10.511001	8.984679
-189.473471	-15.575695	8.994675
-187.782051	-21.257864	9.004672
-185.466274	-5.663618	9.014669
-184.059394	-15.897994	9.024666
-182.158545	-8.594384	9.034663
-180.103037	-10.944859	9.044659
-178.088976	-10.596778	9.054656
-176.254806	-11.382024	9.064653
-174.216408	-8.535346	9.074650
-172.661387	-12.258494	9.084647
-170.657708	-0.915212	9.094643
-168.787441	-9.584679	9.104640
-167.042202	-8.012713	9.114637
-165.069196	-10.217387	9.124634
-163.249582	-9.541443	9.134631
-161.296346	-17.308406	9.144627
-159.354275	-15.480492	9.154624
-157.580573	-18.782235	9.164621
-155.816116	-12.950434	9.174618
-153.847017	-12.661471	9.184615
-152.076820	-15.451104	9.194611
-150.081453	-11.902845	9.204608
-148.011834	-15.218643	9.214605
-146.227131	-16.537519	9.224602
-144.485439	-11.586231	9.234599
-142.674575	-11.949338	9.244595
-140.474426	-6.575437	9.254592
-138.745879	-12.288763	9.264589
-136.885437	-16.428492	9.274586
-135.061659	-4.271787	9.284583
-133.058128	-7.785438	9.294579
-131.215702	-7.837802	9.304576
-129.769300	-23.036045	9.314573
-127.628374	-14.787072	9.324570
-125.658361	-14.008788	9.334567
-123.643673	-3.505590	9.344563
-121.940218	-10.160635	9.354560
-120.208174	-10.975332	9.364557
-118.251564	-6.910892	9.374554
-116.138335	-16.586919	9.384551
-114.282050	-7.798336	9.394547
-112.439564	-7.538082	9.404544
-110.682233	-8.401015	9.414541
-109.189796	-13.175128	9.424538
-106.761042	-3.273205	9.434535
-105.067851	-6.325241	9.444531
-102.917261	-13.327909	9.454528
-101.492883	-11.879958	9.464525
-99.655079	-1.795330	9.474522
-97.652081	-12.273184	9.484519
-95.726270	-16.303320	9.494515
-93.664065	-11.990459	9.504512
-91.884143	-9.847691	9.514509
-89.780122	-12.295825	9.524506
-88.151230	-7.261764	9.534503
-86.163197	-10.768168	9.544499
-84.644299	-7.301724	9.554496
-82.737549	-11.643002	9.564493
-80.564327	-10.611326	9.574490
-78.709092	-8.060588	9.584487
-76.870008	-10.482234	9.594483
-75.037927	-20.681762	9.604480
-73.115551	-1.802192	9.614477
-71.253636	-11.668608	9.624474
-69.406601	-11.235374	9.634471
-67.302256	-5.023536	9.644467
-65.511362	-17.730023	9.654464
-63.798302	-16.902803	9.664461
-61.982709	-14.129426	9.674458
-59.888625	-5.703973	9.684455
-58.081655	-4.525435	9.694451
-56.275186	-9.922738	9.704448
-54.517139	-14.409210	9.714445
-52.641536	2.076414	9.724442
-50.850829	-2.671043	9.734439
-48.436887	-7.994728	9.744435
-46.754898	-7.670930	9.754432
-45.197598	-10.082339	9.764429
-43.175838	-7.174474	9.774426
-41.227193	-6.489021	9.784423
-39.239707	-5.626616	9.794419
-37.381539	-5.398805	9.804416
-35.574905	-8.154699	9.814413
-33.646755	-4.508778	9.824410
-32.010877	-1.621450	9.834407
-29.913638	-7.077748	9.844403
-28.176529	-7.567944	9.854400
-26.201276	-5.074200	9.864397
-24.133972	-5.588643	9.874394
-22.545600	0.634493	9.884391
-20.582203	-2.130607	9.894387
-18.756416	-7.745691	9.904384
-17.103530	-9.450793	9.914381
-14.700169	-7.630025	9.924378
-13.121343	-1.519038	9.934375
-11.286523	-8.370221	9.944371
-9.370432	-16.637962	9.954368
-7.454190	-9.114039	9.964365
-5.721873	-16.641981	9.974362
-3.988180	-4.093445	9.984359
-2.605327	18.888883	9.994355
-1.605489	67.849334	10.004352
-0.434178	138.504674	10.014349
0.000000	194.862683	10.019354
1.226005	241.528259	10.024359
1.417220	294.491471	10.029363
1.920322	334.044289	10.034368
2.718217	367.674757	10.039373
2.614007	396.832085	10.044378
3.235831	421.018454	10.049383
3.299126	459.099572	10.054387
3.751147	469.252023	10.059392
4.129171	478.575802	10.064397
3.963597	503.718916	10.069402
4.263236	522.544955	10.074407
4.103232	530.655223	10.079411
4.442213	527.931494	10.084416
4.620951	535.968814	10.089421
4.674119	559.930734	10.094426
4.934894	566.439589	10.099431
4.647234	565.397428	10.104435
4.690538	571.158830	10.109440
4.961716	564.360167	10.114445
4.644398	577.562122	10.119450
5.017875	580.274760	10.124455
4.983880	581.614256	10.129459
5.454447	595.595703	10.134464
5.575083	604.501738	10.139469
5.129733	607.892165	10.144474
5.600874	607.500080	10.149479
5.441939	621.354881	10.154483
5.424205	617.699313	10.159488
5.631311	622.042204	10.164493
5.506449	629.694350	10.169498
5.841277	622.220055	10.174503
5.557819	630.767948	10.179507
5.601856	628.053398	10.184512
5.659876	638.527422	10.189517
5.573930	644.918153	10.194522
5.728958	634.862750	10.199527
5.371500	633.990984	10.204531
5.891303	627.393904	10.209536
5.916501	629.895603	10.214541
5.812185	643.248143	10.219546
6.067115	646.339235	10.224551
5.698720	643.621079	10.229555
5.826544	636.726980	10.234560
5.978985	649.007277	10.239565
6.136673	679.120006	10.244570
6.210529	681.560338	10.249575
6.366647	684.586776	10.254579
6.663311	684.604131	10.259584
6.655538	681.815835	10.264589
6.330591	683.244322	10.269594
6.531551	683.396786	10.274599
6.434929	682.636375	10.279603
6.784672	675.892937	10.284608
6.732357	689.029073	10.289613
6.529072	693.960975	10.294618
6.892228	682.855236	10.299623
6.716082	694.546178	10.304627
6.595050	692.711052	10.309632
6.860304	687.528035	10.314637
6.885826	695.678187	10.319642
7.025272	695.730079	10.324647
6.977233	699.932343	10.329651
6.774413	705.386133	10.334656
7.013176	701.054137	10.339661
6.738246	702.815262	10.344666
6.845586	702.403931	10.349671
7.000478	710.973417	10.354675
6.935615	716.111902	10.359680
7.111853	724.258532	10.364685
7.308117	730.301522	10.369690
7.600555	735.496564	10.374695
7.340914	744.783452	10.379699
7.483918	746.812230	10.384704
7.699787	745.249785	10.389709
7.394647	747.356347	10.394714
7.848017	740.754043	10.399719
7.737508	742.616678	10.404723
7.606830	756.623216	10.409728
7.728112	749.821568	10.414733
7.781174	748.165244	10.419738
7.802166	745.992076	10.424743
7.443224	758.409222	10.429747
7.627153	745.083336	10.434752
7.535091	737.412148	10.439757
7.676955	754.672546	10.444762
7.758553	758.888843	10.449767
7.573925	756.420470	10.454771
7.991234	776.218377	10.459776
8.255413	786.173935	10.464781
8.634184	787.020271	10.469786
8.639916	777.275581	10.474791
8.342312	775.326684	10.479795
8.228600	778.359910	10.484800
8.878730	762.155888	10.489805
8.420659	761.476776	10.494810
8.310128	758.462008	10.499815
8.339380	763.416769	10.504819
8.478347	782.612542	10.509824
8.915837	791.482349	10.514829
8.541089	783.644915	10.519834
8.631253	793.300233	10.524839
8.630410	786.150623	10.529843
8.829246	795.665611	10.534848
8.974055	794.961302	10.539853
8.589128	795.180406	10.544858
8.931994	791.498818	10.549863
9.005272	784.996540	10.554867
8.966731	791.993197	10.559872
8.870786	795.115053	10.564877
8.523041	801.612262	10.569882
9.004878	796.082432	10.574887
8.780439	803.594436	10.579891
9.233761	793.390425	10.584896
9.380640	803.054050	10.589901
9.034835	810.293685	10.594906
9.068868	808.004889	10.599911
9.350314	815.127136	10.604915
9.876558	808.617256	10.609920
9.777820	802.464098	10.614925
9.426522	793.470188	10.619930
9.946064	787.292540	10.624935
9.696133	792.911569	10.629939
9.702623	800.432470	10.634944
9.968297	779.890134	10.639949
9.596701	796.738901	10.644954
9.753779	797.089173	10.649959
9.654518	804.007213	10.654963
9.603941	786.270193	10.659968
9.907819	798.695195	10.664973
10.149558	816.873277	10.669978
10.320517	819.520492	10.674983
9.996536	802.282789	10.679987
10.100793	796.724873	10.684992
9.985224	795.202670	10.689997
10.105131	815.041757	10.695002
10.488698	808.630325	10.700007
10.284618	812.300855	10.705011
10.245580	817.596103	10.710016
10.015771	819.734814	10.715021
10.214516	824.481216	10.720026
10.726880	818.134392	10.725031
10.586087	829.047111	10.730035
10.506490	820.902389	10.735040
10.518960	819.362916	10.740045
10.539548	828.852740	10.745050
10.515310	831.367089	10.750055
10.456463	837.209543	10.755059
10.686306	824.303609	10.760064
10.489421	829.351229	10.765069
10.309260	839.751426	10.770074
10.603187	830.424352	10.775079
10.584897	842.342544	10.780083
11.006033	852.675232	10.785088
10.900558	861.639566	10.790093
11.074287	867.459130	10.795098
11.304643	856.232517	10.800103
11.357125	859.141483	10.805107
11.672170	854.652198	10.810112
11.530811	844.320652	10.815117
11.243935	846.979393	10.820122
11.553916	828.063620	10.825127
11.472227	821.860427	10.830131
11.157691	839.417643	10.835136
11.755340	831.543361	10.840141
11.349429	836.534436	10.845146
11.386773	831.684180	10.850151
10.943704	842.638812	10.855155
11.425116	853.726697	10.860160
12.049758	845.472794	10.865165
12.115557	857.670896	10.870170
12.002187	851.584704	10.875175
11.849804	853.045608	10.880179
11.848723	849.939249	10.885184
11.980370	847.082953	10.890189
12.269087	861.615627	10.895194
12.071496	843.171867	10.900199
12.282481	835.516946	10.905203
11.895060	835.816870	10.910208
11.927642	834.499688	10.915213
11.951456	856.289047	10.920218
12.382372	849.354390	10.925223
12.277222	861.508799	10.930227
12.046056	868.154598	10.935232
12.252636	867.172355	10.940237
12.241344	867.260905	10.945242
12.183287	866.994220	10.950247
12.090222	865.749114	10.955251
12.345455	861.032827	10.960256
12.581949	856.470916	10.965261
12.151557	865.400344	10.970266
12.247186	856.956422	10.975271
12.638726	876.534654	10.980275
12.906052	885.419044	10.985280
12.997237	882.480887	10.990285
12.733869	872.845284	10.995290
13.355701	876.223256	11.000295
13.291335	864.643102	11.005299
13.007933	870.627038	11.010304
12.992700	858.269511	11.015309
12.873629	870.643763	11.020314
13.368527	861.309847	11.025319
13.107750	861.250533	11.030323
12.929204	867.973094	11.035328
13.231275	861.047943	11.040333
13.187403	868.753529	11.045338
13.280169	867.105051	11.050343
13.122900	874.737264	11.055347
13.358531	877.624907	11.060352
13.294432	892.650694	11.065357
13.462075	897.873584	11.070362
13.539301	896.442045	11.075367
13.750468	898.335395	11.080371
13.881491	897.655358	11.085376
13.695639	889.661583	11.090381
13.679347	898.551793	11.095386
13.944204	906.269659	11.100391
13.895777	893.866933	11.105395
13.929202	888.818589	11.110400
13.949186	878.350900	11.115405
13.845117	885.181437	11.120410
13.834645	869.293968	11.125415
13.976808	878.745511	11.130419
14.181028	894.849704	11.135424
13.932558	899.468764	11.140429
13.818398	900.716998	11.145434
13.909118	894.801662	11.150439
14.099216	900.380512	11.155443
13.976948	895.497345	11.160448
14.112236	906.771361	11.165453
13.858723	905.526610	11.170458
14.368964	899.962249	11.175463
14.130604	907.681529	11.180467
14.402881	921.346417	11.185472
14.656401	926.599775	11.190477
14.486747	928.438751	11.195482
14.894405	927.290395	11.200487
15.045104	917.672299	11.205491
14.798956	904.037974	11.210496
14.684957	889.080039	11.215501
14.623953	900.643975	11.220506
14.830555	909.456064	11.225511
14.869277	914.798869	11.230515
15.046680	916.286027	11.235520
15.070642	916.980805	11.240525
14.890083	910.787035	11.245530
15.139475	918.613029	11.250535
15.453370	915.880616	11.255539
15.023010	898.962535	11.260544
15.271379	891.150237	11.265549
15.098747	904.867147	11.270554
15.410039	915.901790	11.275559
15.580097	919.924255	11.280563
15.463395	911.515743	11.285568
15.303236	894.056262	11.290573
15.163436	901.001314	11.295578
15.346700	909.571124	11.300583
15.279534	918.191920	11.305587
14.965937	924.491350	11.310592
15.453736	928.381140	11.315597
15.219577	933.414240	11.320602
15.132842	932.396774	11.325607
15.562485	945.825278	11.330611
15.636417	955.525872	11.335616
15.636566	945.644766	11.340621
16.167343	949.493014	11.345626
16.284527	947.684516	11.350631
16.540652	953.907286	11.355635
16.397230	939.326150	11.360640
16.955186	916.732716	11.365645
16.426319	932.419290	11.370650
16.364501	920.660490	11.375655
15.981491	915.486169	11.380659
15.923645	916.124609	11.385664
16.252673	927.299934	11.390669
15.886820	925.598441	11.395674
16.265598	916.645705	11.400679
16.126939	921.860687	11.405683
15.897325	933.511464	11.410688
15.866176	937.900335	11.415693
15.984592	953.868470	11.420698
16.320003	948.007125	11.425703
16.478165	954.094134	11.430707
16.696231	949.226053	11.435712
17.018091	941.797818	11.440717
16.925725	955.449935	11.445722
17.068715	955.059720	11.450727
16.919609	946.634279	11.455731
17.030182	958.525707	11.460736
16.931281	953.839064	11.465741
16.637816	964.008264	11.470746
17.011639	956.426656	11.475751
16.907436	961.002227	11.480755
16.841584	960.265277	11.485760
17.394209	955.574069	11.490765
17.186101	964.105408	11.495770
17.057949	966.904434	11.500775
17.242026	979.156313	11.505779
17.273363	985.867532	11.510784
17.721237	980.276818	11.515789
17.683936	982.936779	11.520794
17.614008	963.819648	11.525799
17.446048	955.720482	11.530803
17.590565	946.877630	11.535808
17.775701	947.704397	11.540813
17.297515	957.810015	11.545818
17.641468	961.110904	11.550823
17.742230	984.186005	11.555827
17.640796	984.563320	11.560832
18.039613	984.547039	11.565837
18.016331	990.522653	11.570842
18.021269	979.524284	11.575847
18.038356	978.359370	11.580851
17.706289	975.797779	11.585856
18.060016	975.342414	11.590861
17.902617	990.529839	11.595866
18.028821	988.562203	11.600871
17.976456	978.440293	11.605875
17.815080	986.148912	11.610880
18.007940	980.184135	11.615885
17.989652	981.048080	11.620890
18.105268	980.389420	11.625895
18.321383	978.481562	11.630899
18.259888	978.508733	11.635904
18.421485	996.584708	11.640909
18.568685	1007.006930	11.645914
19.021090	1009.293904	11.650919
18.823027	992.777054	11.655923
18.796534	990.111531	11.660928
19.073103	988.695498	11.665933
18.729004	992.082478	11.670938
18.976136	988.610074	11.675943
18.738137	988.402047	11.680947
18.726817	994.669067	11.685952
18.991370	974.624949	11.690957
18.932825	981.232229	11.695962
19.297499	974.016345	11.700967
18.876835	991.502362	11.705971
18.982132	990.517343	11.710976
19.151975	983.822957	11.715981
19.078980	990.222812	11.720986
19.183690	981.534521	11.725991
18.832799	1000.122742	11.730995
19.145824	1008.545760	11.736000
19.580372	1012.105023	11.741005
19.195684	1020.510018	11.746010
19.629716	1011.346563	11.751015
20.074925	1008.578997	11.756019
19.844593	1009.028910	11.761024
19.638448	992.478656	11.766029
19.249907	985.846518	11.771034
19.721705	993.132460	11.776039
19.832570	1003.357049	11.781043
19.628021	996.667176	11.786048
20.001852	992.770867	11.791053
19.477896	993.630306	11.796058
19.829797	1009.455609	11.801063
19.643239	1008.657484	11.806067
19.956758	1013.877651	11.811072
19.772127	1015.070902	11.816077
19.864577	1011.451276	11.821082
19.998461	1001.534610	11.826087
20.026460	1010.846753	11.831091
19.672122	1013.782787	11.836096
20.343553	1010.821447	11.841101
20.000565	1008.837177	11.846106
19.933959	1004.328292	11.851111
20.171478	1020.335852	11.856115
20.483770	1038.468269	11.861120
20.940383	1034.388436	11.866125
20.761146	1036.001873	11.871130
20.726458	1006.461747	11.876135
20.833728	1002.489679	11.881139
20.589836	1008.749643	11.886144
20.850372	1000.933769	11.891149
20.698166	1009.476719	11.896154
20.983618	1003.202276	11.901159
21.026168	1010.115143	11.906163
20.810914	1004.907725	11.911168
20.795840	994.762509	11.916173
20.695026	999.108894	11.921178
20.786875	1011.135816	11.926183
20.926027	1006.743924	11.931187
20.878298	1010.468414	11.936192
21.168826	1013.692681	11.941197
21.344174	1028.130066	11.946202
21.005854	1027.663649	11.951207
21.231358	1029.955276	11.956211
21.197278	1037.555311	11.961216
21.296050	1029.270060	11.966221
21.392810	1038.768374	11.971226
21.467586	1039.828790	11.976231
21.519109	1044.196624	11.981235
21.370692	1039.629814	11.986240
21.548329	1032.181958	11.991245
21.262502	1040.585389	11.996250
21.484550	1026.012108	12.001255
21.676668	1031.002486	12.006259
21.756625	1037.718589	12.011264
21.436217	1037.124736	12.016269
21.526111	1037.380075	12.021274
21.541827	1029.696272	12.026279
21.829489	1043.406132	12.031283
21.280276	1051.826345	12.036288
21.660519	1038.222877	12.041293
21.665479	1060.343556	12.046298
22.245138	1065.065557	12.051303
22.152059	1046.639559	12.056307
21.970279	1045.963672	12.061312
22.133069	1038.910841	12.066317
22.089797	1042.021196	12.071322
21.995873	1039.610846	12.076327
22.141179	1033.264125	12.081331
22.175131	1033.558348	12.086336
22.217442	1037.150214	12.091341
21.949231	1033.594412	12.096346
22.127574	1010.343865	12.101351
22.344317	1018.544127	12.106355
22.002243	1002.889169	12.111360
22.006053	992.371938	12.116365
22.013181	997.700889	12.121370
21.858704	1003.542893	12.126375
21.985015	1002.647561	12.131379
21.654439	997.811773	12.136384
22.006185	985.640033	12.141389
21.926285	995.133378	12.146394
22.030218	1006.041892	12.151399
21.843008	1008.681612	12.156403
21.956040	999.665554	12.161408
22.048794	989.447951	12.166413
21.553899	989.239895	12.171418
21.533432	993.404731	12.176423
21.859597	990.522115	12.181427
21.290546	1003.215828	12.186432
21.889583	999.449179	12.191437
21.815743	1000.987455	12.196442
21.941640	1005.630420	12.201447
21.792567	1004.512505	12.206451
21.536316	1007.395047	12.211456
21.876246	1003.302293	12.216461
21.410580	1005.466031	12.221466
21.728367	1002.997908	12.226471
21.840472	1001.524526	12.231475
21.727675	1004.381035	12.236480
21.744599	999.779982	12.241485
21.709454	1002.854339	12.246490
21.665354	1001.079443	12.251495
22.009141	999.739420	12.256499
21.655427	1004.176604	12.261504
21.853020	998.417645	12.266509
21.802967	1006.890685	12.271514
22.041451	1000.566964	12.276519
22.226292	1003.077960	12.281523
21.977031	1007.646718	12.286528
22.153482	998.313042	12.291533
21.803196	1002.467406	12.296538
21.841316	993.991575	12.301543
21.980380	984.823142	12.306547
21.447053	987.590600	12.311552
21.602806	985.060014	12.316557
21.659611	1009.665494	12.321562
21.810367	1011.022872	12.326567
21.807943	1013.634699	12.331571
21.680269	1013.246650	12.336576
21.812736	1011.618633	12.341581
22.037593	1012.435916	12.346586
22.302421	1010.400437	12.351591
21.885174	994.453126	12.356595
21.620222	988.416283	12.361600
21.676970	976.272677	12.366605
21.757017	982.853124	12.371610
21.737952	983.666730	12.376615
21.754628	994.174416	12.381619
21.841902	1009.450570	12.386624
21.714484	1019.725790	12.391629
22.124710	1011.036062	12.396634
22.090194	997.196008	12.401639
21.959201	990.786140	12.406643
21.537988	995.584168	12.411648
21.688823	988.225764	12.416653
21.640248	984.636522	12.421658
21.912695	988.246864	12.426663
22.294419	980.996719	12.431667
21.913742	985.766201	12.436672
21.789867	985.762321	12.441677
21.938780	982.545280	12.446682
22.307335	978.056885	12.451687
22.176893	983.090807	12.456691
21.905454	990.564672	12.461696
21.925542	983.624513	12.466701
21.956367	989.884809	12.471706
21.872788	992.673577	12.476711
22.011892	998.180175	12.481715
21.653406	984.062222	12.486720
21.888379	970.780027	12.491725
21.347876	975.827307	12.496730
21.768388	985.931537	12.501735
22.084648	985.778613	12.506739
21.841938	995.156000	12.511744
21.815056	984.482821	12.516749
21.783583	990.590628	12.521754
21.825255	996.377691	12.526759
21.936248	997.817103	12.531763
21.468568	979.703246	12.536768
21.810002	981.925914	12.541773
21.596494	994.944534	12.546778
21.895654	996.142625	12.551783
21.980758	996.289918	12.556787
21.417668	1011.001175	12.561792
21.686716	990.292424	12.566797
21.826799	997.997125	12.571802
21.783817	995.756852	12.576807
21.711029	995.702247	12.581811
21.730884	997.711279	12.586816
22.099302	989.745741	12.591821
21.790459	1004.779140	12.596826
21.893839	994.424221	12.601831
22.067534	992.950479	12.606835
21.497793	998.093893	12.611840
21.775594	994.818445	12.616845
21.870841	995.558628	12.621850
21.870839	1000.641138	12.626855
22.080178	1001.640667	12.631859
21.581650	992.201759	12.636864
21.924132	984.243515	12.641869
21.716582	984.549446	12.646874
21.968463	983.712935	12.651879
21.800316	975.888174	12.656883
21.409917	980.657629	12.661888
21.970857	987.954583	12.666893
21.759989	1000.655822	12.671898
21.991419	1002.564879	12.676903
21.863496	980.452895	12.681907
21.924190	981.976021	12.686912
21.875288	970.287659	12.691917
21.563298	975.355264	12.696922
21.624976	974.159584	12.701927
21.737947	981.196823	12.706931
21.970479	990.031636	12.711936
21.710878	986.936516	12.716941
21.717113	987.479585	12.721946
21.671840	994.849573	12.726951
22.085239	999.771532	12.731955
21.618517	993.711674	12.736960
21.923705	995.599505	12.741965
21.654521	991.063009	12.746970
21.852050	990.312437	12.751975
21.963854	983.155802	12.756979
21.283355	985.443686	12.761984
21.274437	1000.350398	12.766989
21.526731	1003.798380	12.771994
21.747951	1011.354530	12.776999
21.913692	1012.107125	12.782003
21.839169	1015.910007	12.787008
22.061135	1008.828829	12.792013
21.590167	1014.114189	12.797018
21.535014	1010.669492	12.802023
22.264131	1011.180848	12.807027
21.834682	1016.177314	12.812032
21.891953	1010.607886	12.817037
21.879870	1013.120328	12.822042
21.842489	1015.900156	12.827047
21.924528	1008.410789	12.832051
21.720934	1019.913983	12.837056
22.023754	1010.656339	12.842061
21.821750	1014.839095	12.847066
21.937884	1008.489154	12.852071
21.866757	988.727210	12.857075
21.724941	985.209608	12.862080
21.378285	982.639304	12.867085
21.832463	1000.670198	12.872090
21.698858	1014.180714	12.877095
21.781957	1023.503002	12.882099
21.742253	1015.067957	12.887104
21.641055	1016.312555	12.892109
21.815052	1024.202672	12.897114
21.889553	1021.995697	12.902119
22.186302	1009.659244	12.907123
22.071917	1010.010241	12.912128
22.058603	995.969688	12.917133
21.985419	985.464741	12.922138
21.763646	988.903172	12.927143
21.752564	984.987831	12.932147
21.742414	984.571577	12.937152
21.905729	980.406073	12.942157
21.837558	991.774107	12.947162
21.514748	983.767430	12.952167
21.684658	976.976843	12.957171
21.565632	995.409807	12.962176
21.749558	988.255859	12.967181
21.878354	995.874050	12.972186
21.697544	997.412041	12.977191
21.917525	987.199379	12.982195
21.543680	997.583271	12.987200
22.049008	995.824826	12.992205
22.017283	993.718376	12.997210
21.705719	983.405990	13.002215
21.931615	993.698958	13.007219
21.909951	982.488787	13.012224
21.774684	985.009833	13.017229
22.113387	975.410599	13.022234
21.961458	993.353649	13.027239
22.233861	974.930953	13.032243
22.019378	990.652604	13.037248
22.251071	979.884572	13.042253
21.936795	989.643951	13.047258
21.748615	997.437275	13.052263
21.950360	985.387230	13.057267
21.733823	1000.538365	13.062272
21.806818	993.245990	13.067277
22.039871	986.557291	13.072282
21.930063	986.112777	13.077287
22.113770	975.607867	13.082291
21.847991	964.684223	13.087296
22.056365	964.690431	13.092301
21.754039	956.343036	13.097306
21.662696	975.807611	13.102311
21.609568	960.699544	13.107315
21.370948	965.108898	13.112320
21.631439	963.503045	13.117325
21.766259	985.322204	13.122330
21.727403	1001.388014	13.127335
22.007789	989.285999	13.132339
21.732421	987.980072	13.137344
22.054456	985.216386	13.142349
21.529115	978.339565	13.147354
21.577305	976.707647	13.152359
21.858855	995.992928	13.157363
21.708855	997.508658	13.162368
21.789221	991.326854	13.167373
22.054647	1001.891065	13.172378
21.921478	987.727711	13.177383
22.078504	970.990250	13.182387
21.580042	981.097541	13.187392
21.788506	966.233174	13.192397
21.741815	974.524311	13.197402
21.387227	972.920362	13.202407
21.755473	976.264689	13.207411
21.538870	995.200491	13.212416
21.700039	995.513846	13.217421
21.850574	1005.801496	13.222426
21.866417	1004.064347	13.227431
22.012789	996.102681	13.232435
21.754028	992.963273	13.237440
22.076851	1007.424424	13.242445
21.913930	999.048464	13.247450
21.796154	989.802720	13.252455
21.965123	970.931327	13.257459
21.749602	975.948853	13.262464
21.597560	970.734520	13.267469
21.563004	976.601541	13.272474
21.851829	991.003444	13.277479
22.149182	986.346631	13.282483
21.772025	988.240786	13.287488
21.850705	982.157025	13.292493
21.514858	973.031227	13.297498
21.647855	986.560698	13.302503
21.748897	1004.305721	13.307507
21.860514	999.888261	13.312512
22.193099	988.508047	13.317517
21.974365	995.935662	13.322522
21.541558	982.693729	13.327527
22.073784	967.192679	13.332531
21.703094	982.617539	13.337536
21.975471	972.827036	13.342541
21.742621	970.948207	13.347546
21.502721	978.524267	13.352551
21.692736	963.372689	13.357555
21.594694	974.568856	13.362560
21.886521	984.422374	13.367565
21.986080	982.313910	13.372570
21.857536	979.559010	13.377575
21.830348	977.945421	13.382579
21.603949	972.432289	13.387584
21.601362	971.607979	13.392589
22.019197	988.225406	13.397594
22.091444	990.661317	13.402599
21.960215	979.697280	13.407603
21.758012	971.903184	13.412608
21.814419	976.238680	13.417613
21.858060	980.270286	13.422618
21.638085	978.529750	13.427623
21.774194	975.065596	13.432627
21.528029	981.083061	13.437632
21.726958	973.299105	13.442637
21.536619	979.452745	13.447642
21.723913	989.297707	13.452647
22.151319	998.781108	13.457651
21.861470	996.085047	13.462656
21.932660	979.250881	13.467661
21.802401	979.095055	13.472666
21.841613	980.014484	13.477671
21.765878	967.236007	13.482675
21.604817	985.510084	13.487680
21.817693	973.784700	13.492685
21.654256	974.785334	13.497690
21.721431	976.310579	13.502695
22.002929	977.259175	13.507699
21.609852	984.856515	13.512704
22.050858	982.327743	13.517709
22.091092	989.065929	13.522714
21.665874	986.424576	13.527719
21.972022	990.543627	13.532723
21.838289	988.284714	13.537728
21.893224	993.621808	13.542733
21.751707	992.106876	13.547738
21.843793	993.953001	13.552743
21.804010	985.637833	13.557747
21.719739	995.614420	13.562752
21.864000	978.571482	13.567757
21.772908	980.465743	13.572762
21.792385	991.641603	13.577767
22.105679	987.387523	13.582771
21.721536	992.499757	13.587776
21.863020	989.487324	13.592781
21.985750	986.649770	13.597786
22.053352	985.073102	13.602791
21.827036	990.485014	13.607795
21.651903	987.105188	13.612800
21.672796	987.540264	13.617805
22.033362	987.788702	13.622810
21.741996	994.761126	13.627815
21.992560	983.640000	13.632819
21.770602	997.183516	13.637824
21.977610	990.664548	13.642829
21.966901	984.956162	13.647834
21.983318	998.311850	13.652839
22.271287	995.594597	13.657843
21.855118	976.786557	13.662848
22.057743	954.807973	13.667853
21.915511	962.970840	13.672858
21.800547	971.566175	13.677863
21.790429	940.405900	13.682867
21.519805	974.886293	13.687872
21.852432	954.847114	13.692877
21.524379	975.658300	13.697882
21.468775	975.351798	13.702887
21.382942	968.050073	13.707891
21.167507	1007.318797	13.712896
21.991378	988.271969	13.717901
21.862643	987.035695	13.722906
21.882416	1002.674266	13.727911
21.964379	994.073173	13.732915
21.783880	987.773703	13.737920
22.002817	995.104707	13.742925
22.059805	993.649578	13.747930
21.866401	997.078755	13.752935
21.902379	985.709579	13.757939
21.662905	972.993481	13.762944
21.987567	995.717504	13.767949
21.719390	977.377868	13.772954
21.461592	967.869043	13.777959
21.846846	985.964527	13.782963
21.780890	996.431777	13.787968
21.657030	1001.314845	13.792973
21.746850	996.771553	13.797978
21.723418	1000.517397	13.802983
21.935557	994.819197	13.807987
21.913149	1010.519697	13.812992
21.629948	995.298479	13.817997
21.861419	1004.511936	13.823002
21.546023	1001.234902	13.828007
21.981976	997.767075	13.833011
22.122743	1003.208755	13.838016
22.152059	987.198115	13.843021
21.942934	971.473102	13.848026
21.614061	975.108382	13.853031
21.693539	962.905969	13.858035
21.366067	973.014367	13.863040
21.848268	989.105870	13.868045
22.043583	990.481371	13.873050
21.849065	989.460591	13.878055
22.108811	968.111538	13.883059
21.823052	966.588075	13.888064
21.840152	961.718927	13.893069
21.545836	969.477125	13.898074
21.701655	968.074044	13.903079
21.725715	953.888801	13.908083
21.515388	969.453649	13.913088
21.746258	986.944557	13.918093
21.990964	998.207503	13.923098
21.550937	1005.725609	13.928103
21.900858	998.773839	13.933107
21.471655	998.489074	13.938112
21.966455	999.174995	13.943117
22.081763	995.304147	13.948122
21.578273	992.156462	13.953127
21.720698	1003.680150	13.958131
21.906244	1005.121865	13.963136
21.778577	1007.179657	13.968141
22.021547	997.742333	13.973146
21.596821	994.356582	13.978151
21.828805	992.969737	13.983155
22.281462	1007.170486	13.988160
21.761052	979.314790	13.993165
21.639704	974.253254	13.998170
21.640359	978.340601	14.003175
21.906876	966.378011	14.008179
21.605386	975.182868	14.013184
21.680817	987.529353	14.018189
21.921538	985.455133	14.023207
21.942207	994.722649	14.028224
21.828403	975.039993	14.033242
21.643642	979.586902	14.038259
22.075003	976.502836	14.043277
22.197561	971.009549	14.048295
21.799276	973.301915	14.053312
22.230119	964.879448	14.058330
21.869432	972.666312	14.063347
21.943386	967.333352	14.068365
21.798620	962.719496	14.073383
21.796723	969.434603	14.078400
21.786563	964.176403	14.083418
21.828658	975.271365	14.088435
22.464143	998.483855	14.093453
21.907383	992.269974	14.098471
21.763072	999.213861	14.103488
22.147161	1004.069575	14.108506
22.070442	1007.803362	14.113523
22.068753	1011.754831	14.118541
22.375975	1002.030804	14.123559
22.149944	1006.647221	14.128576
22.266106	1003.497024	14.133594
22.091033	1012.959353	14.138611
22.181221	1002.625042	14.143629
22.413847	1003.048825	14.148647
22.246708	1011.512655	14.153664
22.447630	1003.636464	14.158682
22.210928	1007.273079	14.163699
22.101413	1009.259862	14.168717
22.246520	1008.793172	14.173735
22.134671	1011.867218	14.178752
22.299130	1015.147291	14.183770
21.786735	1015.197571	14.188787
21.846032	1007.578330	14.193805
22.132822	999.417903	14.198823
21.947591	1015.698899	14.203840
22.495549	1020.887109	14.208858
22.427917	1034.123064	14.213875
22.019415	1043.320641	14.218893
22.412663	1036.749172	14.223911
22.530751	1036.805856	14.228928
22.586600	1040.534239	14.233946
22.660712	1043.534590	14.238963
22.485879	1047.733893	14.243981
22.639033	1038.750096	14.248999
22.433666	1048.797690	14.254016
22.652306	1038.570273	14.259034
22.509233	1043.637484	14.264051
22.507740	1046.067911	14.269069
22.501305	1037.614477	14.274087
22.515736	1050.208188	14.279104
22.639155	1045.861399	14.284122
22.295337	1056.255103	14.289139
22.703433	1060.256053	14.294157
23.143520	1061.102899	14.299175
22.843590	1056.436686	14.304192
22.881269	1038.705382	14.309210
22.908261	1038.392801	14.314227
22.969279	1046.535564	14.319245
23.002049	1036.243418	14.324263
22.785095	1040.575271	14.329280
23.100150	1039.807787	14.334298
22.874237	1046.690783	14.339315
22.839670	1035.547413	14.344333
22.902909	1034.201931	14.349351
22.662489	1045.920842	14.354368
22.737681	1060.757303	14.359386
23.225345	1064.226497	14.364403
23.237014	1068.759408	14.369421
23.268212	1052.274880	14.374439
23.009970	1045.679905	14.379456
23.030351	1030.889597	14.384474
22.913456	1069.775288	14.389491
23.003286	1068.557688	14.394509
23.426065	1060.112859	14.399527
22.936680	1065.708761	14.404544
23.226126	1071.899280	14.409562
23.435617	1060.839654	14.414579
23.289189	1073.438593	14.419597
23.263487	1067.232785	14.424615
22.974300	1078.132138	14.429632
23.073512	1070.047203	14.434650
23.015726	1070.813016	14.439667
22.925895	1074.816310	14.444685
23.603070	1074.063425	14.449703
23.691815	1069.590034	14.454720
23.171651	1077.729557	14.459738
23.548298	1073.046663	14.464755
23.590815	1072.481510	14.469773
23.927195	1074.922546	14.474791
23.820945	1069.509756	14.479808
23.647828	1072.330906	14.484826
23.709883	1062.982547	14.489843
23.471571	1049.460362	14.494861
23.599271	1056.999503	14.499879
23.315404	1062.285790	14.504896
23.390649	1067.245835	14.509914
23.473675	1071.437051	14.514931
23.681415	1065.480285	14.519949
23.913177	1068.442915	14.524967
23.528340	1076.070101	14.529984
23.747902	1066.897954	14.535002
23.763531	1075.228859	14.540019
23.388834	1067.493198	14.545037
23.393701	1062.735903	14.550055
23.415386	1066.790618	14.555072
23.513831	1072.115029	14.560090
23.929996	1067.570544	14.565107
23.576491	1069.365028	14.570125
23.693291	1060.352411	14.575143
23.678139	1062.657612	14.580160
23.760179	1069.568579	14.585178
23.796280	1071.374853	14.590195
23.298011	1075.732708	14.595213
23.708919	1085.276222	14.600231
23.901295	1100.149087	14.605248
23.880204	1105.328990	14.610266
24.547719	1099.622906	14.615283
24.145475	1109.126248	14.620301
24.237847	1097.934272	14.625319
24.069459	1102.164021	14.630336
24.297002	1093.147878	14.635354
24.528600	1080.439426	14.640371
23.932428	1081.262792	14.645389
24.179490	1073.291120	14.650407
23.644067	1066.579904	14.655424
24.014849	1078.133725	14.660442
24.346680	1088.693383	14.665459
24.204760	1098.134751	14.670477
24.401778	1098.627133	14.675495
24.448966	1100.782407	14.680512
24.463025	1094.345317	14.685530
24.236940	1065.969550	14.690547
24.253890	1077.197581	14.695565
24.793537	1065.599261	14.700583
24.084203	1072.538921	14.705600
24.215861	1069.183331	14.710618
24.349177	1071.889546	14.715635
24.210565	1088.565858	14.720653
24.846649	1092.517872	14.725671
24.449561	1084.409842	14.730688
24.251994	1078.961279	14.735706
24.543961	1083.786098	14.740723
24.354926	1097.252245	14.745741
24.274823	1106.111212	14.750759
24.526453	1104.691635	14.755776
24.677184	1103.056930	14.760794
24.478153	1093.701430	14.765811
24.269993	1103.076292	14.770829
24.563449	1101.970923	14.775847
24.535139	1108.290783	14.780864
24.440559	1103.566637	14.785882
24.712306	1099.836360	14.790899
24.543463	1109.653241	14.795917
24.658759	1101.694704	14.800935
24.630264	1103.394888	14.805952
24.716503	1107.620206	14.810970
24.903776	1092.260555	14.815987
24.747959	1094.586623	14.821005
24.872097	1094.054067	14.826023
24.624589	1100.585050	14.831040
24.813063	1107.899033	14.836058
25.137939	1111.853499	14.841075
24.739584	1114.238700	14.846093
25.090553	1105.602389	14.851111
25.205454	1104.366631	14.856128
24.817694	1101.719901	14.861146
25.076107	1096.148275	14.866163
25.067590	1104.322609	14.871181
25.014026	1107.263116	14.876199
24.834915	1099.568599	14.881216
25.035392	1103.395047	14.886234
25.439907	1116.508588	14.891251
25.170298	1117.331780	14.896269
25.473687	1092.607237	14.901287
25.037753	1090.690168	14.906304
25.027050	1089.927447	14.911322
25.292885	1079.234752	14.916339
25.341008	1084.872343	14.921357
25.333018	1089.798483	14.926375
25.287171	1104.316112	14.931392
25.308052	1098.566877	14.936410
25.183442	1089.127155	14.941427
24.940579	1104.541319	14.946445
25.214474	1114.704420	14.951463
25.682004	1121.748975	14.956480
25.486142	1133.309847	14.961498
25.811555	1114.406338	14.966515
25.820632	1103.271684	14.971533
25.578513	1100.409829	14.976551
25.553658	1083.122572	14.981568
25.237679	1079.493900	14.986586
25.391907	1094.607210	14.991603
25.052596	1100.610173	14.996621
25.625426	1104.877429	15.001639
25.633864	1099.608349	15.006656
25.470811	1125.145786	15.011674
25.755427	1122.741009	15.016691
25.822508	1124.149115	15.021709
26.134503	1115.780122	15.026727
25.993033	1103.716280	15.031744
25.482343	1087.689348	15.036762
25.590992	1089.803360	15.041779
25.523796	1093.803049	15.046797
25.815669	1111.022601	15.051815
25.958677	1119.866441	15.056832
25.731703	1123.451199	15.061850
25.893138	1116.622527	15.066867
26.094679	1126.188450	15.071885
25.885389	1114.001717	15.076903
26.044805	1113.907100	15.081920
25.754510	1119.126798	15.086938
25.808203	1113.875661	15.091955
25.713752	1113.854565	15.096973
25.729056	1126.352255	15.101991
25.851043	1131.528224	15.107008
26.128149	1119.682312	15.112026
25.952881	1112.287606	15.117043
26.126417	1134.889765	15.122061
26.199280	1121.415406	15.127079
26.148155	1131.682262	15.132096
25.783541	1133.154501	15.137114
26.247493	1123.578420	15.142131
25.976005	1123.571402	15.147149
25.776427	1129.739271	15.152167
26.227212	1130.313871	15.157184
26.233839	1111.867024	15.162202
26.430455	1120.321665	15.167219
25.969459	1133.102951	15.172237
26.033460	1134.280329	15.177255
26.331979	1136.532369	15.182272
26.237187	1151.723205	15.187290
26.702416	1138.990023	15.192307
26.822984	1148.767066	15.197325
26.535555	1142.293099	15.202343
26.693322	1120.202809	15.207360
26.683098	1128.512701	15.212378
26.605936	1129.239137	15.217395
26.374160	1129.076358	15.222413
26.705871	1111.656698	15.227431
26.690630	1116.546253	15.232448
26.024105	1121.070946	15.237466
26.376841	1112.210993	15.242483
26.649708	1128.835882	15.247501
26.542586	1149.236673	15.252519
26.975752	1147.118068	15.257536
26.626379	1146.314982	15.262554
26.882991	1147.151773	15.267571
26.946792	1144.958378	15.272589
26.730424	1138.594195	15.277607
27.242213	1142.276627	15.282624
26.751275	1148.978583	15.287642
26.666843	1111.730788	15.292659
27.005171	1118.580455	15.297677
26.532800	1141.244742	15.302695
27.111619	1131.548095	15.307712
26.989026	1138.645878	15.312730
27.111535	1138.134028	15.317747
26.889182	1138.389719	15.322765
27.118428	1146.397176	15.327783
27.132478	1137.523587	15.332800
26.644423	1139.860181	15.337818
26.833901	1132.185507	15.342835
27.477087	1133.970469	15.347853
26.977775	1139.887288	15.352871
27.297102	1133.885958	15.357888
27.258343	1136.438741	15.362906
27.390019	1133.061112	15.367923
27.281472	1134.799234	15.372941
27.300456	1134.373104	15.377959
27.632791	1124.585219	15.382976
27.301296	1127.312096	15.387994
27.395085	1118.874088	15.393011
27.203340	1113.169767	15.398029
26.946069	1124.688521	15.403047
27.110021	1127.521987	15.408064
27.037274	1135.031792	15.413082
27.305406	1141.686611	15.418099
27.253863	1147.687741	15.423117
27.182978	1141.352261	15.428135
27.403474	1136.898733	15.433152
27.111163	1139.045241	15.438170
27.134659	1146.478359	15.443187
27.746716	1145.215215	15.448205
27.351110	1156.894474	15.453223
27.396665	1154.177053	15.458240
27.906946	1165.046490	15.463258
28.141671	1157.407057	15.468275
27.782976	1148.677847	15.473293
27.765341	1142.495887	15.478311
27.980387	1140.177703	15.483328
27.464207	1144.703592	15.488346
27.443478	1141.985734	15.493363
27.585165	1141.810580	15.498381
27.719632	1157.474489	15.503399
27.807165	1162.191948	15.508416
27.788336	1168.842211	15.513434
28.016397	1170.073646	15.518451
28.066360	1170.476233	15.523469
27.944714	1170.014331	15.528487
28.193628	1156.798137	15.533504
28.015436	1167.300777	15.538522
28.199428	1165.492455	15.543539
28.568120	1147.163988	15.548557
27.935430	1138.377816	15.553575
28.134918	1124.112520	15.558592
27.829761	1133.472986	15.563610
27.893658	1126.235172	15.568627
28.219435	1143.532721	15.573645
27.808172	1155.662764	15.578663
28.498237	1158.687593	15.583680
28.248593	1174.568502	15.588698
28.366864	1158.433316	15.593715
28.536770	1155.922566	15.598733
28.344708	1165.392422	15.603751
28.527350	1146.035041	15.608768
28.516097	1137.531982	15.613786
28.209277	1122.463447	15.618803
28.464143	1132.074349	15.623821
28.094933	1129.478135	15.628839
28.268892	1148.994149	15.633856
28.350066	1165.795937	15.638874
28.442296	1164.621989	15.643891
28.541079	1159.642055	15.648909
28.712894	1160.363390	15.653927
28.625978	1157.495645	15.658944
28.427134	1164.994118	15.663962
28.421307	1180.114169	15.668979
28.822493	1165.218947	15.673997
28.640292	1159.749027	15.679015
28.655137	1159.469840	15.684032
28.820797	1162.167768	15.689050
28.840929	1167.350557	15.694067
28.853878	1160.146019	15.699085
28.874031	1164.073598	15.704103
28.665906	1162.362419	15.709120
28.645267	1165.631151	15.714138
28.658258	1157.138370	15.719155
28.707182	1154.215930	15.724173
28.497356	1166.106227	15.729191
28.981413	1156.701514	15.734208
28.639057	1156.281105	15.739226
28.732932	1162.413197	15.744243
29.006525	1160.798214	15.749261
28.794688	1169.610593	15.754279
28.425826	1171.383944	15.759296
28.735836	1189.302228	15.764314
28.975664	1191.080745	15.769331
29.245492	1182.922921	15.774349
29.053181	1195.219413	15.779367
29.224936	1194.806667	15.784384
29.233423	1191.914263	15.789402
29.329714	1187.036959	15.794419
29.408118	1197.012657	15.799437
29.241916	1196.694707	15.804455
29.504744	1185.672096	15.809472
29.163631	1190.715889	15.814490
29.084775	1192.782746	15.819507
29.217779	1191.069065	15.824525
28.944271	1197.788273	15.829543
29.222082	1192.233965	15.834560
29.374983	1179.970535	15.839578
28.910821	1181.609657	15.844595
29.543639	1199.119412	15.849613
29.877918	1210.889937	15.854631
30.257057	1213.484619	15.859648
29.657683	1203.197222	15.864666
29.696031	1177.107020	15.869683
29.796278	1180.933745	15.874701
29.770688	1186.804916	15.879719
29.970088	1172.678006	15.884736
30.024827	1171.969335	15.889754
29.942502	1178.065044	15.894771
29.947034	1182.389928	15.899789
29.674674	1182.467987	15.904807
29.695862	1173.804012	15.909824
29.988418	1178.979535	15.914842
29.796013	1190.192282	15.919859
29.735474	1171.853593	15.924877
29.561459	1183.373271	15.929895
30.134902	1174.493810	15.934912
29.887115	1169.183776	15.939930
29.821748	1171.633849	15.944947
29.870404	1175.242297	15.949965
29.866745	1176.054536	15.954983
29.939505	1170.087796	15.960000
30.141907	1167.334347	15.965018
30.285283	1194.001168	15.970035
30.485416	1175.089247	15.975053
30.154801	1177.696449	15.980071
29.831233	1174.525115	15.985088
30.069164	1181.629912	15.990106
30.096512	1193.027825	15.995123
30.226653	1196.878099	16.000141
30.171005	1205.423357	16.005159
30.303949	1206.253135	16.010176
30.379034	1209.011132	16.015194
30.032103	1222.865929	16.020211
30.604792	1200.434077	16.025229
30.365449	1208.050710	16.030247
30.559141	1203.798055	16.035264
30.517112	1211.304574	16.040282
30.257098	1214.721599	16.045299
30.532149	1209.678932	16.050317
30.550408	1207.901756	16.055335
30.668993	1212.115655	16.060352
30.651074	1207.588450	16.065370
30.756078	1206.657841	16.070387
31.261710	1206.220159	16.075405
30.843387	1205.761530	16.080423
30.695102	1205.239385	16.085440
30.828643	1201.490228	16.090458
31.013704	1199.291642	16.095475
31.086409	1198.307985	16.100493
30.828803	1190.726606	16.105511
31.048377	1175.430925	16.110528
31.058986	1175.446553	16.115546
30.733158	1172.022336	16.120563
31.294419	1165.685123	16.125581
30.939778	1175.295740	16.130599
31.017501	1174.058041	16.135616
31.425345	1162.559312	16.140634
31.089731	1167.836588	16.145651
30.888786	1169.940216	16.150669
31.109639	1166.178716	16.155687
30.892435	1164.745821	16.160704
31.202472	1161.811622	16.165722
31.191687	1181.994185	16.170739
31.187847	1172.058547	16.175757
31.138984	1176.446998	16.180775
31.005375	1186.756934	16.185792
31.399915	1194.192245	16.190810
31.476780	1202.828047	16.195827
31.529657	1192.693023	16.200845
31.487789	1197.505058	16.205863
31.571972	1191.379194	16.210880
31.614237	1167.927781	16.215898
30.931473	1170.073647	16.220915
31.278045	1185.271201	16.225933
31.139752	1195.330220	16.230951
30.932651	1201.861096	16.235968
31.509670	1199.820210	16.240986
31.478498	1199.450839	16.246003
31.376898	1185.758865	16.251021
31.533221	1202.608482	16.256039
31.724551	1201.937798	16.261056
31.591391	1210.342845	16.266074
31.545703	1201.346617	16.271091
31.524846	1196.371595	16.276109
31.708359	1209.993925	16.281127
31.512820	1214.927997	16.286144
31.719269	1223.193950	16.291162
31.665101	1224.596236	16.296179
32.107112	1216.450257	16.301197
32.034761	1224.581359	16.306215
32.059416	1224.137020	16.311232
32.162004	1226.868613	16.316250
31.893631	1233.148166	16.321267
31.999942	1224.115099	16.326285
32.000755	1231.624233	16.331303
31.923958	1225.670313	16.336320
32.141322	1211.274672	16.341338
32.182163	1226.725512	16.346355
32.367336	1217.012942	16.351373
32.362036	1220.312272	16.356391
32.222152	1232.779751	16.361408
32.077314	1209.885047	16.366426
32.329852	1247.531017	16.371443
32.570690	1215.944028	16.376461
32.082399	1224.729748	16.381479
31.942636	1232.115018	16.386496
32.107542	1215.140242	16.391514
31.918749	1218.424793	16.396531
32.571727	1238.481127	16.401549
32.447410	1221.237881	16.406567
32.169893	1219.323841	16.411584
32.635014	1233.731797	16.416602
32.271265	1219.167717	16.421619
32.449065	1256.146116	16.426637
32.343577	1249.567581	16.431655
32.731828	1251.839935	16.436672
32.725295	1249.657741	16.441690
32.687947	1269.668493	16.446707
32.948584	1239.928085	16.451725
32.866712	1256.359599	16.456743
32.766408	1268.874276	16.461760
32.946238	1248.884880	16.466778
32.690626	1259.097927	16.471795
32.872424	1250.825122	16.476813
33.104678	1248.167566	16.481831
32.773038	1252.316434	16.486848
32.952501	1250.032222	16.491866
32.820648	1257.678926	16.496883
33.218591	1250.167563	16.501901
32.997365	1252.373532	16.506919
33.214660	1241.760816	16.511936
33.260799	1232.037378	16.516954
32.764183	1253.433191	16.521971
33.002230	1237.099499	16.526989
33.493318	1250.136438	16.532007
33.301926	1243.883050	16.537024
33.329316	1251.543678	16.542042
33.179725	1234.623755	16.547059
33.225194	1247.962985	16.552077
33.298333	1254.897481	16.557095
32.935734	1241.037878	16.562112
33.216225	1238.783170	16.567130
32.822682	1257.111032	16.572147
33.012937	1243.374029	16.577165
33.481278	1252.906925	16.582183
33.294510	1282.516069	16.587200
33.473546	1267.406074	16.592218
33.474061	1268.019460	16.597235
33.747153	1275.752595	16.602253
33.745646	1285.552345	16.607271
33.679953	1273.794012	16.612288
33.823916	1267.732510	16.617306
33.922623	1283.696402	16.622323
33.868380	1253.365993	16.627341
33.848023	1273.353592	16.632359
33.978159	1274.768960	16.637376
34.250052	1272.072046	16.642394
33.692016	1244.442539	16.647411
33.613513	1260.667464	16.652429
34.010271	1242.707190	16.657447
34.102622	1292.797256	16.662464
34.085994	1255.692425	16.667482
34.065086	1285.089516	16.672499
34.013185	1273.256627	16.677517
34.081227	1275.666566	16.682535
34.305319	1276.804266	16.687552
34.042967	1269.055297	16.692570
34.306671	1281.216217	16.697587
34.296726	1257.257057	16.702605
34.216175	1287.609008	16.707623
34.079889	1266.450964	16.712640
34.138409	1257.565490	16.717658
33.824205	1287.960997	16.722675
33.845672	1265.401462	16.727693
34.346813	1270.561055	16.732711
34.276988	1277.312306	16.737728
34.356260	1261.482085	16.742746
34.299891	1276.015722	16.747763
34.228225	1280.657940	16.752781
34.577057	1289.995998	16.757799
34.403247	1281.597428	16.762816
34.752604	1295.039239	16.767834
34.798169	1288.636361	16.772851
34.283907	1282.867010	16.777869
34.798461	1293.429139	16.782887
35.109543	1292.599359	16.787904
34.923895	1280.089404	16.792922
34.846071	1278.137216	16.797939
34.737205	1264.425877	16.802957
34.698219	1274.670451	16.807975
34.750805	1273.551578	16.812992
34.950588	1267.429267	16.818010
35.012552	1272.924731	16.823027
34.773290	1288.980281	16.828045
35.037872	1282.665166	16.833063
34.563359	1292.607995	16.838080
35.107465	1286.567609	16.843098
34.868234	1294.001806	16.848115
35.064719	1290.426623	16.853133
35.238641	1292.866867	16.858151
35.379738	1297.273820	16.863168
35.503704	1288.442381	16.868186
35.439397	1296.630440	16.873203
35.447384	1292.045597	16.878221
35.367983	1267.985817	16.883239
34.974560	1272.649461	16.888256
35.040051	1278.924549	16.893274
35.101528	1302.304579	16.898291
35.172390	1294.318417	16.903309
35.163641	1284.469997	16.908327
34.975988	1289.695406	16.913344
35.235003	1282.017429	16.918362
35.353599	1298.468927	16.923379
35.847487	1302.379190	16.928397
36.167171	1287.295504	16.933415
35.880084	1282.721545	16.938432
36.151568	1290.448653	16.943450
36.243910	1274.414995	16.948467
36.080129	1269.190622	16.953485
36.016115	1283.058554	16.958503
35.877658	1287.234821	16.963520
35.879423	1284.727271	16.968538
35.858351	1277.627196	16.973555
35.832994	1301.516553	16.978573
36.009650	1264.295934	16.983591
35.819780	1291.252025	16.988608
36.281847	1283.359201	16.993626
36.078695	1277.769887	16.998643
35.940991	1299.177737	17.003661
36.346616	1287.389840	17.008679
36.132592	1276.226143	17.013696
36.002305	1290.070046	17.018714
36.530512	1282.405764	17.023731
36.113246	1269.295711	17.028749
36.277123	1304.105782	17.033767
36.111035	1285.228529	17.038784
36.320755	1282.426703	17.043802
36.529944	1284.103158	17.048819
36.570887	1293.277974	17.053837
36.269177	1279.012238	17.058855
35.953002	1292.788267	17.063872
35.840439	1288.351632	17.068890
36.078160	1285.993632	17.073907
35.967470	1286.067929	17.078925
36.078243	1288.651944	17.083943
35.948003	1307.324824	17.088960
36.184717	1310.167171	17.093978
36.173294	1317.843462	17.098995
36.615311	1313.384438	17.104013
36.613482	1293.051161	17.109031
36.519436	1329.149779	17.114048
36.788905	1327.684867	17.119066
37.065029	1330.833952	17.124083
36.689731	1353.347812	17.129101
37.055910	1348.660209	17.134119
37.082626	1336.520587	17.139136
36.994851	1328.822391	17.144154
36.830571	1328.027525	17.149171
36.754507	1339.330366	17.154189
36.887907	1322.330603	17.159207
36.786139	1350.531118	17.164224
37.045832	1339.381481	17.169242
37.498432	1326.241182	17.174259
37.160164	1342.866261	17.179277
37.500176	1334.958271	17.184295
37.466462	1331.087897	17.189312
37.620290	1323.558802	17.194330
37.545577	1329.139004	17.199347
37.454184	1334.270429	17.204365
37.840356	1306.644367	17.209383
37.419707	1304.778309	17.214400
36.967246	1310.692442	17.219418
37.590920	1316.395629	17.224435
37.466886	1310.963563	17.229453
37.729039	1323.035107	17.234471
37.619789	1339.299629	17.239488
37.563812	1314.042161	17.244506
37.546638	1321.857792	17.249523
37.360795	1320.662115	17.254541
37.949101	1319.935980	17.259559
37.893065	1325.390511	17.264576
37.837854	1327.143743	17.269594
37.993742	1315.269817	17.274611
37.830577	1320.132697	17.279629
37.742332	1315.594653	17.284647
37.832882	1314.524776	17.289664
37.798493	1323.927120	17.294682
37.870561	1336.162692	17.299699
37.483113	1334.211114	17.304717
37.913375	1327.971799	17.309735
37.830270	1320.544984	17.314752
37.518476	1327.677753	17.319770
37.906022	1332.265626	17.324787
38.058379	1350.239141	17.329805
37.686849	1342.540575	17.334823
37.707382	1340.994246	17.339840
38.056170	1363.886552	17.344858
38.304378	1345.644688	17.349875
38.564823	1338.259024	17.354893
38.197072	1349.331552	17.359911
38.201444	1356.347847	17.364928
38.312278	1349.044238	17.369946
38.807971	1360.034123	17.374963
38.548777	1358.510381	17.379981
38.546640	1359.465527	17.384999
38.789694	1353.934004	17.390016
38.759406	1349.772080	17.395034
38.820683	1347.736353	17.400051
38.267514	1344.548117	17.405069
38.578008	1358.096855	17.410087
39.082518	1350.829557	17.415104
38.813651	1366.410160	17.420122
38.999201	1367.163921	17.425139
38.930689	1347.424772	17.430157
39.201144	1344.473255	17.435175
39.113642	1351.055907	17.440192
38.835162	1348.129016	17.445210
38.672504	1352.222649	17.450227
38.742075	1364.567177	17.455245
38.906260	1358.496121	17.460263
38.899023	1396.575576	17.465280
38.661001	1383.795469	17.470298
38.952344	1374.916836	17.475315
39.178999	1388.107754	17.480333
38.851129	1392.646155	17.485351
39.180544	1378.753129	17.490368
39.130541	1372.615557	17.495386
39.520228	1393.565071	17.500403
39.533558	1407.832905	17.505421
39.863590	1395.456104	17.510439
39.640321	1370.118257	17.515456
39.171395	1377.696090	17.520474
39.241359	1377.197331	17.525491
39.365475	1393.866699	17.530509
39.883904	1401.036978	17.535527
40.170527	1405.438059	17.540544
39.794399	1391.224977	17.545562
40.067687	1393.781520	17.550579
39.852846	1375.272134	17.555597
39.714176	1349.142214	17.560615
40.129281	1386.702849	17.565632
39.580706	1364.296989	17.570650
39.841321	1362.781579	17.575667
39.708989	1363.795239	17.580685
39.747491	1390.144108	17.585703
40.213376	1394.861075	17.590720
39.989601	1397.237352	17.595738
40.625216	1393.442680	17.600755
40.349695	1373.778978	17.605773
40.303854	1358.885642	17.610791
40.666405	1368.284482	17.615808
40.087589	1372.096866	17.620826
40.103801	1344.026387	17.625843
40.533477	1375.435973	17.630861
40.022681	1343.556461	17.635879
40.195742	1371.809138	17.640896
40.112495	1357.245799	17.645914
40.563394	1365.073317	17.650931
40.479828	1380.391585	17.655949
40.143822	1385.002064	17.660967
40.805045	1385.280432	17.665984
40.561598	1388.064097	17.671002
40.598485	1389.911184	17.676019
40.490142	1393.774378	17.681037
40.559801	1386.389230	17.686055
40.652901	1393.709132	17.691072
40.349906	1381.375100	17.696090
40.771240	1382.553710	17.701107
40.600783	1399.683753	17.706125
40.390120	1380.967634	17.711143
40.884695	1389.989944	17.716160
40.604073	1386.627675	17.721178
40.784507	1408.610989	17.726195
40.641889	1419.082970	17.731213
40.914136	1421.995175	17.736231
41.050943	1418.212410	17.741248
40.693252	1425.055254	17.746266
41.162285	1422.559673	17.751283
40.973639	1413.353312	17.756301
40.963080	1417.270129	17.761319
41.493007	1419.279253	17.766336
41.304776	1425.366788	17.771354
41.449193	1418.628775	17.776371
41.373957	1421.324274	17.781389
41.340015	1416.573051	17.786407
41.295917	1419.861311	17.791424
41.105446	1435.467237	17.796442
41.603221	1439.645897	17.801459
41.689876	1442.032447	17.806477
41.811076	1447.199218	17.811495
42.138462	1440.067086	17.816512
41.788387	1424.341338	17.821530
41.894431	1410.825239	17.826547
41.676290	1414.458994	17.831565
41.328704	1405.988967	17.836583
41.797081	1426.537458	17.841600
41.780725	1436.787975	17.846618
42.057158	1439.487166	17.851635
42.090590	1446.569654	17.856653
41.850419	1450.510515	17.861671
42.209801	1442.670161	17.866688
42.262855	1450.646114	17.871706
42.377013	1441.986027	17.876723
42.171230	1433.018333	17.881741
42.278209	1437.684018	17.886759
42.351272	1426.369031	17.891776
42.192000	1444.922452	17.896794
42.315428	1440.589702	17.901811
42.135741	1442.306173	17.906829
42.009961	1433.388638	17.911847
42.059993	1421.444994	17.916864
42.319258	1428.107653	17.921882
42.264358	1440.412325	17.926899
42.089600	1426.085299	17.931917
42.178455	1430.038172	17.936935
42.695672	1423.140033	17.941952
42.433760	1445.319786	17.946970
42.878386	1440.614925	17.951987
42.735245	1449.427528	17.957005
42.368387	1445.654296	17.962023
42.752456	1453.083548	17.967040
42.652835	1460.876224	17.972058
42.752999	1463.619261	17.977075
42.925738	1461.743488	17.982093
43.254293	1477.342187	17.987111
43.315579	1456.923112	17.992128
43.174977	1469.236757	17.997146
43.169935	1457.445006	18.002163
43.255205	1465.606160	18.007181
43.210577	1462.346232	18.012199
43.543884	1446.247215	18.017216
43.253952	1449.632887	18.022234
43.142022	1430.754671	18.027251
43.286196	1442.761765	18.032269
42.987076	1453.944544	18.037287
43.579501	1455.591361	18.042304
43.273040	1450.948081	18.047322
43.173646	1451.047317	18.052339
43.504502	1448.460514	18.057357
43.311415	1470.476751	18.062375
43.571340	1454.095282	18.067392
43.555880	1451.963244	18.072410
43.847690	1449.742878	18.077427
43.969933	1452.108024	18.082445
43.568880	1454.817739	18.087463
43.816259	1454.995375	18.092480
43.681142	1454.098326	18.097498
43.737896	1435.646217	18.102515
43.753102	1442.171633	18.107533
43.409369	1457.253058	18.112551
43.848791	1450.639437	18.117568
43.866510	1471.731755	18.122586
44.160867	1477.902792	18.127603
44.151547	1475.043058	18.132621
44.107247	1482.309414	18.137639
44.619647	1471.696656	18.142656
44.229045	1478.167260	18.147674
44.089993	1480.781715	18.152691
44.457937	1474.676542	18.157709
44.742874	1482.873501	18.162727
44.684236	1459.192324	18.167744
44.590425	1448.380542	18.172762
44.361141	1452.967730	18.177779
44.395766	1455.795147	18.182797
44.466271	1443.456550	18.187815
44.487494	1439.641877	18.192832
44.494294	1449.105371	18.197850
44.664808	1459.178243	18.202867
44.705481	1469.990678	18.207885
44.571190	1481.315500	18.212903
44.656366	1478.596418	18.217920
44.800005	1475.492073	18.222938
44.677074	1474.504993	18.227955
44.762846	1467.208466	18.232973
44.609798	1480.002289	18.237991
44.917060	1460.498776	18.243008
44.909442	1469.758524	18.248026
44.958457	1466.707022	18.253043
45.200286	1465.498182	18.258061
44.889115	1472.885743	18.263079
44.833915	1462.369804	18.268096
44.881346	1477.642116	18.273114
44.700699	1489.381737	18.278131
45.166721	1496.368520	18.283149
44.976249	1505.844636	18.288167
45.398430	1480.038729	18.293184
45.197117	1490.015197	18.298202
45.625762	1499.738627	18.303219
45.590136	1487.737805	18.308237
45.378410	1502.466326	18.313255
45.682054	1499.471735	18.318272
45.726254	1489.017000	18.323290
45.720200	1495.907615	18.328307
45.708951	1492.294729	18.333325
45.466507	1500.893546	18.338343
45.479480	1492.428885	18.343360
45.805092	1486.772464	18.348378
45.833470	1527.239078	18.353395
46.079351	1517.444270	18.358413
46.295779	1513.077791	18.363431
46.153948	1528.473146	18.368448
46.195605	1515.747416	18.373466
46.162496	1510.956705	18.378483
46.629294	1505.752800	18.383501
46.114469	1501.988993	18.388519
46.411278	1487.303566	18.393536
46.374112	1480.084839	18.398554
46.008762	1486.261993	18.403571
46.697537	1477.912926	18.408589
46.179614	1493.542823	18.413607
46.506132	1493.866709	18.418624
46.478582	1488.003923	18.423642
46.034489	1519.166218	18.428659
46.228662	1519.119539	18.433677
46.384374	1520.999601	18.438695
46.500103	1507.514900	18.443712
46.390544	1510.761712	18.448730
46.326330	1517.576672	18.453747
46.692590	1516.483260	18.458765
46.413189	1527.176900	18.463783
46.568998	1537.484973	18.468800
46.978447	1554.251376	18.473818
46.923709	1549.158944	18.478835
47.099663	1554.669369	18.483853
47.464060	1555.177547	18.488871
47.563774	1545.133905	18.493888
47.015914	1532.620935	18.498906
46.851852	1529.026119	18.503923
47.306248	1529.140854	18.508941
47.484191	1534.087828	18.513959
47.352066	1528.652251	18.518976
47.121942	1514.904958	18.523994
47.330317	1537.440846	18.529011
47.458506	1543.050904	18.534029
47.243091	1552.340698	18.539047
47.347553	1551.027920	18.544064
47.414048	1547.217009	18.549082
47.349330	1556.020316	18.554099
47.796761	1553.215135	18.559117
47.384545	1550.771987	18.564135
47.733648	1548.729654	18.569152
47.766060	1548.785849	18.574170
47.492058	1537.821058	18.579187
48.166158	1545.594991	18.584205
47.930826	1539.736220	18.589223
47.714318	1538.430587	18.594240
48.190686	1544.458586	18.599258
47.907593	1541.142290	18.604275
47.945679	1538.727215	18.609293
47.919965	1534.981348	18.614311
48.105307	1550.768916	18.619328
48.163542	1561.924675	18.624346
47.988015	1563.448592	18.629363
48.271612	1568.787704	18.634381
48.459872	1572.804986	18.639399
48.479985	1570.673549	18.644416
48.798870	1554.395819	18.649434
48.417238	1576.656211	18.654451
48.758104	1568.724365	18.659469
48.397840	1564.732977	18.664487
48.634126	1569.483474	18.669504
48.570445	1571.813798	18.674522
48.334744	1573.863252	18.679539
48.779230	1560.826281	18.684557
48.451591	1566.203097	18.689575
48.349811	1562.562161	18.694592
49.134633	1559.379138	18.699610
48.619842	1572.699481	18.704627
48.579882	1561.138152	18.709645
49.210628	1577.034823	18.714663
49.313449	1585.559751	18.719680
49.116810	1568.846708	18.724698
49.159067	1568.687407	18.729715
49.452898	1547.498108	18.734733
49.144447	1555.649746	18.739751
49.207094	1551.545301	18.744768
49.614414	1548.276196	18.749786
49.201408	1559.271158	18.754803
49.049049	1557.540025	18.759821
49.482499	1566.128615	18.764839
49.535760	1573.796300	18.769856
49.869224	1577.082583	18.774874
49.860054	1570.318658	18.779891
49.747486	1559.747305	18.784909
49.563083	1555.117557	18.789927
49.527934	1550.965788	18.794944
49.732054	1556.680930	18.799962
49.847175	1584.545300	18.804979
49.806056	1585.764646	18.809997
49.990663	1585.521298	18.815015
49.962350	1588.163727	18.820032
49.956990	1585.427605	18.825050
49.890398	1592.167476	18.830067
50.342150	1571.805515	18.835085
49.827837	1577.043796	18.840103
49.585053	1580.020867	18.845120
50.025748	1575.184461	18.850138
49.783196	1575.360010	18.855155
49.797236	1586.104421	18.860173
50.078601	1608.306319	18.865191
50.182862	1604.851158	18.870208
50.540668	1609.233085	18.875226
50.349543	1622.135349	18.880243
50.624470	1612.444382	18.885261
50.560330	1608.119473	18.890279
50.338525	1601.357984	18.895296
50.842799	1610.443381	18.900314
50.683944	1605.076530	18.905331
50.816735	1592.694839	18.910349
50.998916	1603.478515	18.915367
50.674345	1609.098670	18.920384
50.715704	1594.375224	18.925402
50.680097	1604.392982	18.930419
51.162407	1622.259162	18.935437
51.337375	1632.948057	18.940455
50.978303	1623.465153	18.945472
51.305200	1625.682863	18.950490
51.655967	1633.384929	18.955507
51.378798	1616.181316	18.960525
51.524207	1600.606013	18.965543
51.179620	1603.476631	18.970560
51.216569	1589.310731	18.975578
51.301402	1610.392548	18.980595
51.371122	1615.174343	18.985613
51.730571	1626.871986	18.990631
51.337064	1636.487530	18.995648
51.596964	1625.065514	19.000666
51.497154	1629.460653	19.005683
51.501737	1620.234355	19.010701
51.786559	1618.828315	19.015719
51.673268	1631.398858	19.020736
51.739746	1634.968401	19.025754
51.609196	1635.712814	19.030771
51.924535	1633.394289	19.035789
52.059202	1627.972755	19.040807
51.543530	1627.910295	19.045824
51.920200	1636.791121	19.050842
52.233903	1638.177251	19.055859
52.212743	1639.780375	19.060877
52.179508	1641.303630	19.065895
52.559202	1657.855468	19.070912
52.722203	1653.604432	19.075930
52.516886	1635.330713	19.080947
52.682309	1622.509648	19.085965
52.219000	1617.829979	19.090983
52.246356	1630.450449	19.096000
52.531090	1632.854204	19.101018
52.737577	1647.240904	19.106035
52.516010	1642.563573	19.111053
52.698847	1641.332667	19.116071
52.759883	1639.671309	19.121088
52.754664	1644.071817	19.126106
52.809740	1640.416857	19.131123
52.857602	1636.667095	19.136141
53.047783	1634.108987	19.141159
52.788918	1644.292935	19.146176
53.116359	1624.867780	19.151194
53.317622	1638.594648	19.156211
53.043354	1632.914291	19.161229
53.308401	1634.525253	19.166247
53.271419	1627.026432	19.171264
53.447757	1623.393035	19.176282
53.367008	1628.305794	19.181299
53.273131	1628.610213	19.186317
53.450342	1637.129600	19.191335
53.176588	1638.021117	19.196352
53.210025	1646.325917	19.201370
53.566305	1670.183335	19.206387
53.774285	1662.709922	19.211405
53.877136	1663.844969	19.216423
53.553182	1661.169078	19.221440
53.736892	1661.067440	19.226458
53.549575	1666.969317	19.231475
53.674936	1662.173733	19.236493
54.057845	1657.936388	19.241511
53.851508	1663.254570	19.246528
53.767125	1663.873647	19.251546
54.052177	1660.902438	19.256563
53.988158	1684.565789	19.261581
54.521743	1681.112929	19.266599
54.448737	1676.743796	19.271616
54.534443	1670.781079	19.276634
54.257265	1669.507130	19.281651
54.246639	1668.623246	19.286669
54.654201	1663.785803	19.291687
54.438304	1670.113801	19.296704
54.749708	1681.117595	19.301722
54.882863	1674.315194	19.306739
54.586511	1669.014290	19.311757
54.717956	1650.103267	19.316775
54.476536	1665.700262	19.321792
54.913948	1670.763204	19.326810
54.784966	1670.352791	19.331827
54.931657	1688.366956	19.336845
55.312439	1661.632969	19.341863
55.119658	1675.809670	19.346880
54.707108	1673.836877	19.351898
55.114481	1679.088653	19.356915
54.989427	1666.601731	19.361933
55.189809	1681.668973	19.366951
54.818738	1686.675240	19.371968
54.784528	1677.425205	19.376986
54.958698	1667.279944	19.382003
55.320668	1700.898511	19.387021
55.586173	1712.848729	19.392039
55.824968	1695.441617	19.397056
55.454888	1694.044058	19.402074
55.565198	1703.480200	19.407091
55.719194	1703.078140	19.412109
55.790122	1691.330711	19.417127
55.763734	1689.829579	19.422144
55.628308	1700.406006	19.427162
55.698160	1709.891075	19.432179
55.610954	1703.759295	19.437197
55.935607	1699.594148	19.442215
55.715368	1706.372732	19.447232
55.679560	1708.118197	19.452250
56.108209	1715.438233	19.457267
56.218939	1723.015035	19.462285
56.360604	1724.145470	19.467303
56.274266	1726.499882	19.472320
56.476411	1722.972455	19.477338
56.529991	1732.611143	19.482355
56.494382	1730.380031	19.487373
56.557029	1717.705831	19.492391
56.652651	1707.747671	19.497408
56.545265	1730.964991	19.502426
56.951208	1693.064921	19.507443
56.716892	1728.519953	19.512461
56.901632	1721.964130	19.517479
56.968259	1706.934523	19.522496
57.103767	1722.296866	19.527514
57.104376	1706.840494	19.532531
56.875795	1702.979074	19.537549
57.059204	1700.890788	19.542567
56.799225	1721.324626	19.547584
57.030685	1726.060215	19.552602
57.239452	1692.901155	19.557619
57.006473	1717.753951	19.562637
56.987960	1703.093424	19.567655
57.212752	1708.132086	19.572672
57.369644	1693.544268	19.577690
57.510628	1709.185717	19.582707
57.088619	1738.683874	19.587725
57.677700	1727.118049	19.592743
57.426824	1739.883657	19.597760
57.633804	1747.410517	19.602778
57.725252	1743.776472	19.607795
57.696268	1736.406877	19.612813
57.869283	1736.593232	19.617831
57.780207	1739.418409	19.622848
58.030913	1738.271052	19.627866
58.090564	1739.938377	19.632883
57.879846	1746.984445	19.637901
58.111182	1738.434480	19.642919
57.897283	1730.701127	19.647936
57.742675	1759.313554	19.652954
58.129706	1726.797661	19.657971
58.122579	1773.290501	19.662989
58.326095	1759.115175	19.668007
58.297398	1786.836131	19.673024
58.434135	1770.936416	19.678042
58.601796	1752.285322	19.683059
58.345475	1762.272321	19.688077
58.279401	1762.097261	19.693095
58.652665	1770.044349	19.698112
58.587881	1756.888647	19.703130
58.617441	1751.469672	19.708147
58.497738	1787.222743	19.713165
58.845357	1778.898028	19.718183
58.977635	1769.755089	19.723200
59.178684	1800.972405	19.728218
59.696690	1770.928745	19.733235
59.570492	1788.344768	19.738253
59.656568	1775.701387	19.743271
59.620399	1762.066070	19.748288
59.420095	1754.555475	19.753306
59.589093	1741.230374	19.758323
59.280556	1764.176236	19.763341
59.366466	1751.783010	19.768359
59.304780	1751.083440	19.773376
59.113119	1780.706967	19.778394
59.654483	1764.273975	19.783411
59.605096	1780.466525	19.788429
59.787288	1785.128195	19.793447
59.698573	1786.178972	19.798464
59.740595	1788.830670	19.803482
60.065669	1771.793522	19.808499
59.488214	1785.663592	19.813517
59.764101	1786.796222	19.818535
60.016344	1782.101486	19.823552
59.932512	1784.328093	19.828570
60.202307	1792.242931	19.833587
59.862051	1803.217035	19.838605
60.173315	1807.103084	19.843623
60.342508	1803.285167	19.848640
60.547126	1810.722776	19.853658
60.344301	1810.704803	19.858675
60.294758	1817.331948	19.863693
60.599362	1801.908792	19.868711
60.734052	1806.265015	19.873728
60.363243	1810.851288	19.878746
60.950053	1800.298786	19.883763
60.679654	1799.758339	19.888781
60.754654	1805.122941	19.893799
61.097158	1798.431814	19.898816
60.907014	1803.700274	19.903834
60.935783	1795.805492	19.908851
60.904766	1811.117408	19.913869
61.160546	1823.118032	19.918887
61.006299	1831.577136	19.923904
61.209132	1828.244629	19.928922
61.605122	1820.146554	19.933939
61.442211	1829.480061	19.938957
61.345407	1828.084524	19.943975
61.569412	1819.625343	19.948992
61.623042	1818.166493	19.954010
61.904649	1815.540291	19.959027
61.557697	1821.952175	19.964045
61.378702	1815.227802	19.969063
61.509538	1811.949251	19.974080
61.315379	1819.625062	19.979098
61.704970	1817.547924	19.984115
61.821389	1838.563690	19.989133
61.949783	1840.210626	19.994151
62.022909	1848.416405	19.999168
61.969031	1853.035519	20.004186
62.457856	1847.618773	20.009203
62.396191	1845.660784	20.014221
62.459621	1847.730211	20.019239
62.250881	1850.544605	20.024256
62.203592	1845.180322	20.029274
62.863854	1838.510862	20.034291
62.729285	1847.778512	20.039309
62.437876	1845.987721	20.044327
62.689863	1839.238652	20.049344
62.602815	1837.759762	20.054362
62.867872	1835.710346	20.059379
62.822717	1846.714500	20.064397
62.963565	1839.294174	20.069415
63.097107	1834.368242	20.074432
62.545958	1842.662561	20.079450
63.023299	1857.100658	20.084467
63.215850	1873.026642	20.089485
63.124705	1881.430095	20.094503
63.409609	1882.389837	20.099520
63.261090	1873.588912	20.104538
63.293291	1877.646897	20.109555
63.202875	1876.371460	20.114573
63.313043	1881.132735	20.119591
63.465505	1881.844612	20.124608
63.680276	1878.805916	20.129626
63.403045	1877.580719	20.134643
63.617929	1871.921361	20.139661
63.382397	1876.122714	20.144679
63.644734	1873.296657	20.149696
63.845419	1885.476005	20.154714
63.746760	1893.013930	20.159731
63.668752	1907.240193	20.164749
63.957202	1907.729038	20.169767
64.193871	1900.914743	20.174784
63.433737	1910.993199	20.179802
64.239752	1900.341175	20.184819
64.417567	1898.167237	20.189837
64.465175	1900.934469	20.194855
64.486166	1888.899117	20.199872
64.637304	1880.591520	20.204890
64.931595	1886.935778	20.209907
64.868711	1889.272318	20.214925
64.629926	1899.624700	20.219943
64.982117	1877.046077	20.224960
65.056410	1885.935954	20.229978
64.732230	1894.585788	20.234995
64.610900	1894.817512	20.240013
64.941449	1890.328904	20.245031
65.010002	1901.790018	20.250048
65.053927	1918.713453	20.255066
64.894692	1922.471645	20.260083
65.163067	1917.852944	20.265101
65.349766	1915.698037	20.270119
65.766971	1911.003694	20.275136
65.268575	1914.086088	20.280154
65.713615	1914.998273	20.285171
65.417223	1906.044732	20.290189
65.667055	1911.145540	20.295207
65.875735	1906.314567	20.300224
65.749699	1909.999821	20.305242
65.906144	1904.680103	20.310259
65.625139	1914.067103	20.315277
65.524920	1911.715706	20.320295
65.976803	1905.936743	20.325312
65.442492	1914.428190	20.330330
65.652724	1931.748262	20.335347
66.203796	1938.627320	20.340365
66.205740	1949.325167	20.345383
66.575751	1947.534278	20.350400
67.046155	1951.678134	20.355418
67.073086	1949.020163	20.360435
66.916462	1931.666388	20.365453
66.888581	1921.397442	20.370471
67.248409	1899.508123	20.375488
66.935990	1905.032071	20.380506
66.949853	1908.698162	20.385523
67.163366	1901.448687	20.390541
66.834401	1902.638458	20.395559
67.280291	1904.720833	20.400576
67.090132	1905.098813	20.405594
67.077525	1903.540405	20.410611
67.085866	1904.545826	20.415629
66.657726	1908.985543	20.420647
67.059384	1900.900678	20.425664
66.953790	1914.041244	20.430682
67.098121	1906.250669	20.435699
67.221182	1900.058532	20.440717
66.903903	1911.721182	20.445735
67.079213	1929.276481	20.450752
67.270045	1933.114130	20.455770
67.338979	1924.398047	20.460787
67.219684	1933.795450	20.465805
67.456923	1948.180693	20.470823
67.674291	1951.018391	20.475840
67.689364	1955.300926	20.480858
67.984378	1958.108940	20.485875
68.371323	1967.422489	20.490893
68.201937	1971.852421	20.495911
68.252217	1963.222660	20.500928
67.974710	1967.301745	20.505946
68.039758	1966.924874	20.510963
68.423424	1957.928919	20.515981
68.295795	1961.573542	20.520999
68.725497	1964.912210	20.526016
68.478181	1955.101378	20.531034
68.714257	1960.224846	20.536051
68.942855	1959.527738	20.541069
68.980965	1968.111977	20.546087
68.637282	1956.065510	20.551104
68.687235	1955.282060	20.556122
68.878707	1967.955304	20.561139
68.932127	1975.395087	20.566157
68.654308	1989.746104	20.571175
68.891168	1980.207255	20.576192
69.027447	1978.492962	20.581210
68.896765	1974.512036	20.586227
69.204583	1975.076447	20.591245
68.996220	2000.581754	20.596263
69.279791	1998.678801	20.601280
69.174731	2011.007686	20.606298
69.713949	2005.239926	20.611315
69.718693	1998.220324	20.616333
69.548789	1997.306764	20.621351
69.872585	1987.142139	20.626368
70.303860	1989.330679	20.631386
69.759959	1987.823953	20.636403
70.382651	1992.803983	20.641421
69.949430	1997.573299	20.646439
69.927792	1992.544645	20.651456
70.161668	1991.204898	20.656474
70.049138	1994.024426	20.661491
70.099356	2003.865179	20.666509
70.292747	2018.535911	20.671527
70.575438	2022.871744	20.676544
70.643616	2028.780214	20.681562
70.302848	2034.363787	20.686579
70.950163	2011.841712	20.691597
70.829913	2030.031007	20.696615
70.807560	2017.510101	20.701632
70.925890	2031.967872	20.706650
70.914071	2018.188431	20.711667
71.374893	1997.668700	20.716685
71.055484	2017.443893	20.721703
71.103419	2007.466391	20.726720
71.265742	2009.178723	20.731738
71.073000	2009.785207	20.736755
71.355183	2003.866526	20.741773
71.168748	2007.168179	20.746791
70.894271	2015.223417	20.751808
71.065984	2019.860093	20.756826
71.431749	2047.801791	20.761843
71.377048	2040.186030	20.766861
71.408270	2051.856138	20.771879
71.426550	2034.128280	20.776896
71.743561	2033.025385	20.781914
71.393386	2033.254278	20.786931
71.521089	2035.961572	20.791949
71.984694	2051.658911	20.796967
71.784466	2048.905012	20.801984
72.120569	2059.307405	20.807002
72.141760	2062.898433	20.812019
72.742289	2046.340859	20.817037
72.303893	2054.040011	20.822055
72.217175	2052.051382	20.827072
72.360182	2059.752204	20.832090
72.875396	2083.023387	20.837107
72.954399	2070.082001	20.842125
72.861086	2060.932382	20.847143
72.634318	2060.406987	20.852160
72.958808	2065.129428	20.857178
72.915180	2075.040250	20.862195
73.344187	2068.429589	20.867213
73.247237	2073.367103	20.872231
73.148733	2067.181913	20.877248
73.335232	2071.473326	20.882266
73.210484	2073.196837	20.887283
73.316842	2064.141218	20.892301
72.730070	2061.409632	20.897319
73.180981	2057.140881	20.902336
72.997050	2075.024207	20.907354
73.348598	2092.658567	20.912371
73.653160	2088.372247	20.917389
73.445693	2100.256637	20.922407
73.649290	2105.597698	20.927424
73.836804	2098.550475	20.932442
73.401070	2098.533461	20.937459
73.996783	2103.985026	20.942477
74.146308	2122.642655	20.947495
74.308639	2129.248740	20.952512
74.410795	2129.010668	20.957530
74.240693	2128.388144	20.962547
74.951696	2109.867026	20.967565
74.728764	2118.225564	20.972583
74.388204	2108.775565	20.977600
74.631249	2110.707847	20.982618
74.348668	2116.329364	20.987635
74.669341	2115.814197	20.992653
74.468637	2118.674552	20.997671
75.034135	2111.104572	21.002688
75.135507	2097.354196	21.007706
74.895971	2103.914241	21.012723
75.179687	2098.136853	21.017741
75.376899	2098.453064	21.022759
75.498812	2103.813442	21.027776
75.555625	2096.315150	21.032794
75.049243	2104.089664	21.037811
75.416476	2099.194018	21.042829
75.313555	2093.572669	21.047847
75.296810	2109.308918	21.052864
75.705571	2118.683582	21.057882
75.730274	2136.557309	21.062899
75.868598	2126.854751	21.067917
75.776515	2129.317110	21.072935
75.618757	2124.690793	21.077952
76.217237	2122.290864	21.082970
75.857866	2130.307793	21.087987
75.770033	2125.105602	21.093005
76.121433	2135.625162	21.098023
76.139391	2152.693012	21.103040
76.326587	2149.808098	21.108058
76.327921	2165.107364	21.113075
76.558699	2156.226905	21.118093
76.842010	2155.969382	21.123111
76.547790	2162.063113	21.128128
76.887067	2146.846426	21.133146
76.565336	2150.517329	21.138163
76.610605	2159.284585	21.143181
77.004548	2173.962820	21.148199
76.798254	2176.712391	21.153216
77.068267	2179.448930	21.158234
76.959066	2184.566190	21.163251
77.478356	2172.284397	21.168269
77.288326	2184.696193	21.173287
76.988306	2179.972993	21.178304
77.492607	2180.600464	21.183322
77.520573	2188.629591	21.188339
77.507919	2203.069095	21.193357
77.695347	2201.061897	21.198375
77.945610	2207.996922	21.203392
78.188308	2205.564051	21.208410
78.153271	2206.132809	21.213427
78.070219	2208.386098	21.218445
78.306140	2202.745280	21.223463
78.336267	2206.275143	21.228480
78.014667	2206.065318	21.233498
78.311433	2198.903096	21.238515
78.375958	2194.425357	21.243533
78.374309	2204.442833	21.248551
78.410333	2196.587575	21.253568
78.649702	2185.723684	21.258586
78.743501	2201.829375	21.263603
78.810909	2191.757404	21.268621
78.733575	2189.023207	21.273639
78.248624	2190.036522	21.278656
78.948917	2190.225320	21.283674
78.843079	2214.750373	21.288691
79.031294	2214.003064	21.293709
79.135776	2220.050544	21.298727
79.221471	2225.155616	21.303744
79.435210	2217.594484	21.308762
79.231907	2228.057846	21.313779
79.710373	2216.380288	21.318797
79.581825	2211.598271	21.323815
79.687723	2221.626925	21.328832
79.970434	2214.935706	21.333850
79.569734	2210.816872	21.338867
79.935952	2208.704083	21.343885
79.999940	2223.419254	21.348903
79.706701	2225.567635	21.353920
80.279156	2229.544287	21.358938
80.216713	2236.102893	21.363955
80.476737	2235.606832	21.368973
80.860774	2233.455018	21.373991
80.666033	2240.745745	21.379008
80.995339	2230.850638	21.384026
80.587067	2210.017733	21.389043
80.600289	2202.403639	21.394061
80.673747	2212.574315	21.399079
80.601215	2233.192915	21.404096
81.055893	2224.482781	21.409114
80.854135	2235.052870	21.414131
80.880179	2232.517688	21.419149
81.275624	2219.209523	21.424167
81.194704	2225.582304	21.429184
81.138689	2227.301165	21.434202
81.129337	2224.485332	21.439219
80.995356	2226.708992	21.444237
81.140225	2246.306638	21.449255
80.888042	2251.184021	21.454272
81.624533	2249.235556	21.459290
81.421547	2259.214388	21.464307
81.452849	2262.191934	21.469325
82.062833	2270.582909	21.474343
81.866721	2290.974327	21.479360
82.072083	2294.886837	21.484378
81.873826	2298.923487	21.489395
81.903308	2287.504664	21.494413
82.076262	2286.607198	21.499431
82.137310	2297.201493	21.504448
82.571303	2280.630886	21.509466
82.504543	2287.602346	21.514483
82.401733	2285.480967	21.519501
82.609977	2272.773627	21.524519
82.554151	2287.684152	21.529536
82.995991	2295.985549	21.534554
82.883898	2305.478001	21.539571
82.702384	2301.299019	21.544589
83.225623	2303.897671	21.549607
82.769959	2321.777440	21.554624
83.092221	2295.605342	21.559642
82.945576	2307.211208	21.564659
82.951513	2304.510902	21.569677
83.291457	2318.939913	21.574695
83.037779	2337.103677	21.579712
83.477984	2334.406476	21.584730
83.901916	2336.762988	21.589747
83.533567	2327.718408	21.594765
84.007885	2337.054447	21.599783
83.921405	2329.792822	21.604800
84.127727	2321.226057	21.609818
84.260477	2322.433470	21.614835
83.938762	2326.052502	21.619853
84.136800	2321.460622	21.624871
84.276101	2339.698581	21.629888
84.602784	2349.720431	21.634906
84.406232	2351.169126	21.639923
84.483887	2356.207884	21.644941
85.118501	2349.359813	21.649959
84.773373	2355.364211	21.654976
84.750102	2352.806984	21.659994
84.959342	2344.722672	21.665011
84.824339	2347.264272	21.670029
85.297072	2338.176802	21.675047
85.197832	2336.769019	21.680064
85.150669	2328.749199	21.685082
85.300280	2331.368111	21.690099
85.418222	2339.084090	21.695117
85.331137	2330.287248	21.700135
85.351188	2358.890307	21.705152
85.823712	2364.825674	21.710170
85.929981	2355.920903	21.715187
85.918220	2365.329752	21.720205
86.201874	2356.006573	21.725223
85.986721	2364.802897	21.730240
86.088382	2361.654721	21.735258
85.839017	2363.472072	21.740275
85.872666	2359.219436	21.745293
86.432412	2346.959362	21.750311
86.024072	2356.835724	21.755328
86.311060	2354.713526	21.760346
86.505945	2358.582106	21.765363
86.134804	2372.136675	21.770381
86.742375	2378.091412	21.775399
86.398077	2381.607090	21.780416
86.755727	2376.576024	21.785434
86.688139	2389.700734	21.790451
86.655057	2387.303159	21.795469
87.092609	2380.066487	21.800487
87.008923	2393.075000	21.805504
87.093052	2399.336593	21.810522
87.326488	2409.737521	21.815539
87.278367	2408.070674	21.820557
87.344693	2409.447567	21.825575
87.651174	2408.427339	21.830592
87.563615	2402.797128	21.835610
87.627858	2417.132558	21.840627
87.508642	2416.579773	21.845645
87.746168	2412.208091	21.850663
88.016218	2440.657398	21.855680
87.891755	2429.674371	21.860698
88.183343	2424.264487	21.865715
88.196952	2441.797428	21.870733
88.672906	2431.524859	21.875751
88.538824	2420.410448	21.880768
88.269952	2427.271053	21.885786
88.424169	2424.142799	21.890803
88.475938	2427.969723	21.895821
88.820317	2429.575994	21.900839
88.995136	2449.148688	21.905856
88.838332	2447.953787	21.910874
89.321484	2447.610124	21.915891
89.114057	2454.496339	21.920909
89.178398	2446.628565	21.925927
89.581669	2444.782765	21.930944
89.640258	2451.756338	21.935962
89.706497	2441.012676	21.940979
89.634532	2442.387242	21.945997
89.563216	2450.129527	21.951015
89.504598	2436.182540	21.956032
89.517380	2434.138664	21.961050
89.888763	2443.848276	21.966067
89.587201	2445.093494	21.971085
89.553950	2452.752630	21.976103
89.754341	2462.990547	21.981120
90.072435	2475.017959	21.986138
90.423873	2472.061960	21.991155
90.318063	2469.573718	21.996173
90.166518	2471.437620	22.001191
90.468949	2504.748217	22.006208
90.579964	2499.685649	22.011226
91.128381	2498.494697	22.016243
90.689161	2503.671773	22.021261
90.634464	2500.937052	22.026279
91.038825	2496.220193	22.031296
90.866439	2501.476632	22.036314
90.897184	2486.919934	22.041331
90.767527	2524.240051	22.046349
91.177421	2522.169021	22.051367
91.228452	2528.341561	22.056384
91.208056	2525.101911	22.061402
91.869597	2535.098024	22.066419
91.703105	2526.519012	22.071437
91.573221	2523.744365	22.076455
91.625868	2538.497059	22.081472
92.030124	2553.550791	22.086490
92.464070	2544.452862	22.091507
92.337283	2540.661502	22.096525
92.487950	2544.143124	22.101543
92.751237	2552.219088	22.106560
92.785508	2542.124630	22.111578
92.856404	2521.876350	22.116595
92.422619	2510.232337	22.121613
92.501474	2525.715471	22.126631
92.670512	2556.506136	22.131648
92.877735	2542.918579	22.136666
92.949984	2540.227319	22.141683
92.725671	2553.084573	22.146701
93.091206	2549.611124	22.151719
92.925028	2543.006280	22.156736
92.936547	2552.678964	22.161754
93.310529	2567.043806	22.166771
93.229045	2566.907373	22.171789
93.465277	2568.188759	22.176807
93.479861	2583.020716	22.181824
93.252868	2560.722950	22.186842
93.352164	2585.673686	22.191859
93.592281	2605.576754	22.196877
94.170500	2598.463843	22.201895
94.297535	2605.895358	22.206912
93.966238	2606.837790	22.211930
94.263208	2603.098397	22.216947
94.358993	2607.635681	22.221965
94.477116	2593.033481	22.226983
94.499664	2598.251005	22.232000
94.464076	2611.901732	22.237018
95.112159	2617.803706	22.242035
94.980832	2628.239360	22.247053
95.233842	2617.583768	22.252071
95.450306	2612.058373	22.257088
95.433409	2623.123106	22.262106
95.614252	2612.750384	22.267123
95.665411	2611.379942	22.272141
95.516691	2594.249065	22.277159
95.413671	2594.879017	22.282176
95.578129	2609.332370	22.287194
95.869492	2612.867869	22.292211
95.670016	2615.043825	22.297229
95.731068	2621.966748	22.302247
95.668914	2604.795312	22.307264
95.572009	2610.865630	22.312282
95.800581	2609.053174	22.317299
96.073509	2618.463197	22.322317
95.820945	2628.776605	22.327335
96.108927	2639.885548	22.332352
95.990089	2635.071953	22.337370
96.544755	2625.673140	22.342387
96.541144	2638.664385	22.347405
96.656890	2635.019165	22.352423
96.765150	2640.266297	22.357440
96.587938	2657.724530	22.362458
96.926571	2658.265968	22.367475
96.951480	2655.004121	22.372493
97.176653	2658.346468	22.377511
97.276489	2657.975832	22.382528
96.831491	2663.297823	22.387546
97.161984	2668.820216	22.392563
97.468868	2692.960136	22.397581
97.772577	2688.824797	22.402599
97.994880	2680.586413	22.407616
98.121684	2699.403359	22.412634
98.103412	2684.365043	22.417651
98.072190	2682.820531	22.422669
97.730716	2680.786703	22.427687
98.055222	2688.032608	22.432704
98.052706	2695.687758	22.437722
98.429221	2700.110303	22.442739
98.188400	2704.878266	22.447757
98.506535	2715.651321	22.452775
98.430362	2703.786524	22.457792
98.284618	2721.355438	22.462810
98.888035	2736.142424	22.467827
98.808782	2732.618728	22.472845
98.827040	2746.787987	22.477863
99.042521	2745.212782	22.482880
99.082700	2738.423926	22.487898
99.613406	2742.064445	22.492915
99.660888	2743.817203	22.497933
99.638103	2753.998099	22.502951
100.196153	2746.849006	22.507968
100.061067	2756.844093	22.512986
100.202820	2746.885733	22.518003
100.190068	2744.315747	22.523021
100.039682	2754.208660	22.528039
100.166959	2752.704938	22.533056
99.890370	2771.221339	22.538074
100.270941	2764.604721	22.543091
100.090728	2759.642774	22.548109
99.866692	2768.385697	22.553127
100.338660	2764.215642	22.558144
100.435151	2783.622729	22.563162
100.538782	2784.858422	22.568179
100.664632	2798.997204	22.573197
100.592663	2802.818001	22.578215
100.895998	2800.486270	22.583232
101.106971	2810.648022	22.588250
101.629564	2799.633115	22.593267
101.744475	2807.063520	22.598285
101.764950	2811.747379	22.603303
102.098478	2799.211525	22.608320
101.837621	2809.817408	22.613338
101.896975	2803.386495	22.618355
102.224764	2809.350634	22.623373
102.297025	2798.070102	22.628391
102.231578	2796.910156	22.633408
101.728469	2805.696028	22.638426
102.161646	2799.036398	22.643443
102.104517	2792.626423	22.648461
102.329314	2799.003405	22.653479
102.531768	2787.764259	22.658496
102.608283	2814.155275	22.663514
102.957383	2828.273433	22.668531
102.838962	2831.396886	22.673549
102.583220	2825.671411	22.678567
102.834819	2826.979474	22.683584
102.484314	2837.385728	22.688602
102.815210	2852.123475	22.693619
103.260435	2855.402464	22.698637
103.159599	2856.390751	22.703655
103.289263	2853.725673	22.708672
103.350729	2869.831756	22.713690
103.573750	2878.903033	22.718707
103.817280	2887.536862	22.723725
103.926286	2892.887794	22.728743
103.955024	2883.827526	22.733760
104.080699	2893.333572	22.738778
103.944020	2884.903761	22.743795
104.506605	2897.871812	22.748813
104.505035	2908.996456	22.753831
104.685373	2904.309684	22.758848
105.137369	2908.369451	22.763866
105.397242	2908.177011	22.768883
105.210558	2901.979567	22.773901
105.181279	2897.489040	22.778919
105.329058	2890.664078	22.783936
105.007917	2904.362972	22.788954
105.181523	2903.749317	22.793971
105.320485	2902.930387	22.798989
105.608681	2897.817406	22.804007
105.625322	2894.829760	22.809024
105.437687	2897.425468	22.814042
105.307438	2903.760003	22.819059
106.165354	2909.226707	22.824077
105.977564	2923.086051	22.829095
106.011002	2920.384392	22.834112
105.926168	2935.116149	22.839130
106.314603	2927.640848	22.844147
106.482803	2922.965444	22.849165
106.303561	2921.420126	22.854183
106.499438	2912.801982	22.859200
106.691449	2938.227783	22.864218
106.371378	2950.300717	22.869235
106.588684	2945.980083	22.874253
106.690510	2949.957262	22.879271
107.230821	2943.994687	22.884288
106.835092	2944.469966	22.889306
106.928236	2951.799303	22.894323
107.269689	2971.393325	22.899341
107.161178	2990.134117	22.904359
107.588737	2972.406713	22.909376
107.638100	2952.931319	22.914394
107.803188	2959.101587	22.919411
108.229301	2963.175723	22.924429
107.938484	2968.911355	22.929447
108.262510	2976.922813	22.934464
108.272887	2999.358835	22.939482
108.501101	2989.545410	22.944499
108.678623	2987.908588	22.949517
108.433410	2995.624618	22.954535
108.817927	2995.322633	22.959552
108.875189	2985.939193	22.964570
109.079697	2989.985746	22.969587
109.233794	2989.525433	22.974605
108.818166	2999.308212	22.979623
109.387758	2974.729164	22.984640
109.281218	2986.805049	22.989658
109.050107	2992.761635	22.994675
109.386336	3004.348478	22.999693
109.445327	3013.180134	23.004711
109.774236	3008.897534	23.009728
109.801389	3013.268910	23.014746
109.695424	3010.991399	23.019763
109.907142	3015.144570	23.024781
110.214665	3038.365463	23.029799
110.329001	3031.971303	23.034816
110.331495	3034.487951	23.039834
110.221145	3042.530165	23.044851
110.569318	3029.896604	23.049869
110.507350	3040.618030	23.054887
110.519678	3041.715709	23.059904
110.873564	3048.614953	23.064922
110.606002	3060.773994	23.069939
111.218065	3061.324553	23.074957
111.154693	3058.240299	23.079975
111.332719	3055.844347	23.084992
111.449178	3054.815049	23.090010
111.355768	3066.601807	23.095027
111.812695	3070.579032	23.100045
111.868899	3079.957841	23.105063
112.109568	3084.372278	23.110080
112.299171	3085.273367	23.115098
112.234218	3089.484833	23.120115
112.159945	3082.081661	23.125133
112.149636	3077.033519	23.130151
112.514846	3068.007582	23.135168
112.313792	3076.213727	23.140186
112.432755	3079.970329	23.145203
112.927162	3067.609170	23.150221
113.034817	3083.598005	23.155239
113.001077	3088.314981	23.160256
112.982244	3098.633924	23.165274
112.936537	3090.842344	23.170291
113.334345	3092.483438	23.175309
113.084690	3105.691310	23.180327
113.521438	3099.807326	23.185344
113.437127	3099.032639	23.190362
113.213920	3104.033894	23.195379
113.669668	3113.483522	23.200397
113.696000	3125.228424	23.205415
113.596545	3130.241418	23.210432
113.998342	3133.194676	23.215450
113.599080	3146.344636	23.220467
114.247739	3141.716833	23.225485
113.745773	3157.279879	23.230503
113.924109	3155.644483	23.235520
114.229409	3168.766284	23.240538
114.303841	3179.942729	23.245555
114.775039	3174.570005	23.250573
114.801840	3192.957545	23.255591
114.861553	3212.954711	23.260608
115.558867	3202.025700	23.265626
115.516143	3197.066850	23.270643
115.614965	3219.090311	23.275661
115.479521	3205.091909	23.280679
115.812668	3195.636027	23.285696
116.300249	3205.893177	23.290714
115.945175	3196.203296	23.295731
116.294553	3202.602282	23.300749
116.428632	3198.169779	23.305767
116.365606	3203.135301	23.310784
116.651224	3199.513984	23.315802
116.593368	3204.000441	23.320819
116.570865	3192.914841	23.325837
116.616236	3232.192617	23.330855
117.110387	3216.566273	23.335872
117.249011	3223.633644	23.340890
117.067772	3221.414510	23.345907
117.368058	3200.474277	23.350925
117.452177	3232.518778	23.355943
117.551762	3219.071251	23.360960
117.463254	3216.070416	23.365978
117.597359	3212.825642	23.370995
117.919071	3213.350926	23.376013
117.719753	3228.717914	23.381031
117.654245	3230.089949	23.386048
118.150136	3237.571524	23.391066
118.296653	3251.065600	23.396083
118.626126	3230.028640	23.401101
118.254513	3241.710448	23.406119
118.287170	3253.679407	23.411136
118.532369	3230.414123	23.416154
118.608072	3238.442511	23.421171
118.907862	3281.991111	23.426189
118.948694	3258.287205	23.431207
118.754537	3273.186185	23.436224
119.003246	3266.665882	23.441242
118.783676	3263.689867	23.446259
119.211125	3274.375903	23.451277
119.462470	3294.502302	23.456295
119.165078	3311.385819	23.461312
119.814354	3303.414878	23.466330
119.856993	3292.906395	23.471347
120.168119	3294.770566	23.476365
119.599341	3315.929188	23.481383
119.966513	3317.445407	23.486400
120.375921	3317.476109	23.491418
120.565478	3314.787240	23.496435
120.445860	3319.700471	23.501453
120.485007	3323.063198	23.506471
120.856973	3346.734462	23.511488
121.177945	3343.489754	23.516506
121.123319	3347.981247	23.521523
121.233550	3344.144803	23.526541
121.139917	3355.035906	23.531559
121.288057	3350.140961	23.536576
121.431953	3350.452335	23.541594
121.393913	3365.358766	23.546611
121.655474	3374.915828	23.551629
121.877782	3369.182346	23.556647
121.915832	3376.659122	23.561664
122.176360	3377.978399	23.566682
121.988395	3372.457424	23.571699
122.461097	3383.232290	23.576717
122.855663	3403.311619	23.581735
122.589848	3394.402616	23.586752
123.235318	3392.223116	23.591770
123.106581	3404.821248	23.596787
123.393641	3385.555152	23.601805
123.623431	3386.875399	23.606823
123.315352	3392.972632	23.611840
123.503899	3383.240782	23.616858
123.323095	3387.703637	23.621875
123.823661	3385.684896	23.626893
123.813040	3388.461697	23.631911
123.617402	3379.856150	23.636928
124.183946	3371.022891	23.641946
123.482066	3385.459407	23.646963
123.838503	3386.096364	23.651981
124.286733	3403.317322	23.656999
124.208532	3405.530690	23.662016
124.288161	3411.294738	23.667034
124.250859	3427.532815	23.672051
124.421209	3429.439902	23.677069
124.592714	3435.726553	23.682087
124.423460	3436.170452	23.687104
124.820116	3450.641108	23.692122
124.936388	3460.945845	23.697139
125.094400	3457.034107	23.702157
125.207207	3459.105332	23.707175
125.208137	3467.668853	23.712192
125.293667	3481.653477	23.717210
125.638040	3487.093742	23.722227
125.606596	3492.003984	23.727245
125.779655	3504.519471	23.732263
125.870166	3523.213481	23.737280
126.392015	3528.183396	23.742298
126.442735	3522.593629	23.747315
126.355762	3509.905543	23.752333
126.869498	3513.688985	23.757351
126.822084	3520.733462	23.762368
126.870156	3519.154979	23.767386
126.968573	3534.452790	23.772403
127.236039	3536.306650	23.777421
127.502457	3532.394125	23.782439
127.628076	3534.667834	23.787456
127.926919	3539.237534	23.792474
127.842542	3548.353525	23.797491
127.743547	3539.169269	23.802509
128.129218	3531.077412	23.807527
127.681833	3532.502498	23.812544
128.049324	3544.600013	23.817562
127.872155	3564.383719	23.822579
128.604736	3565.088927	23.827597
128.480366	3560.029701	23.832615
128.284481	3567.720859	23.837632
128.855044	3579.797037	23.842650
128.763718	3587.182852	23.847667
128.902506	3591.568853	23.852685
129.028440	3597.044775	23.857703
128.700456	3606.316061	23.862720
129.427768	3603.979535	23.867738
129.449704	3604.005946	23.872755
129.609086	3617.639113	23.877773
129.754119	3612.565231	23.882791
129.922779	3623.173225	23.887808
130.488435	3625.533320	23.892826
130.693060	3634.358651	23.897843
130.764406	3636.743288	23.902861
130.549942	3637.033147	23.907879
130.954167	3631.483727	23.912896
130.746851	3625.846177	23.917914
130.798969	3623.043084	23.922931
130.707590	3642.766021	23.927949
131.257850	3636.589203	23.932967
130.986206	3634.033594	23.937984
131.079674	3651.932042	23.943002
131.300835	3665.121197	23.948019
131.058017	3666.693811	23.953037
131.561673	3661.263823	23.958055
131.830740	3669.286002	23.963072
132.120055	3678.500599	23.968090
132.131949	3698.646071	23.973107
132.044124	3692.143841	23.978125
132.365779	3691.584425	23.983143
132.055704	3700.675141	23.988160
132.416629	3699.451860	23.993178
132.453268	3699.265903	23.998195
132.594066	3720.224655	24.003213
132.670408	3721.170590	24.008231
132.677656	3725.065523	24.013248
133.009053	3720.778389	24.018266
132.771691	3732.466710	24.023283
133.097142	3744.545137	24.028301
133.476766	3752.992596	24.033319
133.471128	3761.702860	24.038336
133.990013	3762.631727	24.043354
134.393338	3771.946983	24.048371
134.199340	3776.765247	24.053389
134.330826	3770.160366	24.058407
134.524121	3775.322770	24.063424
134.749326	3771.362478	24.068442
134.725133	3771.411976	24.073459
134.872613	3774.896765	24.078477
135.100163	3767.383765	24.083495
135.121342	3793.073493	24.088512
135.112227	3793.568170	24.093530
135.243021	3806.399007	24.098547
135.067888	3789.988324	24.103565
135.466910	3805.828448	24.108583
135.265038	3815.219774	24.113600
135.880141	3810.115713	24.118618
135.845930	3829.021934	24.123635
135.481975	3826.574616	24.128653
136.172825	3837.864883	24.133671
136.017364	3862.742006	24.138688
136.338549	3845.747905	24.143706
136.659702	3837.384561	24.148723
136.583875	3862.956940	24.153741
136.616855	3870.767516	24.158759
137.007661	3869.644078	24.163776
137.166493	3869.416611	24.168794
137.080170	3875.343387	24.173811
137.336041	3900.926663	24.178829
137.938377	3900.471945	24.183847
137.856764	3900.487335	24.188864
137.818407	3903.609262	24.193882
138.307967	3896.285687	24.198899
138.077403	3905.014594	24.203917
138.664352	3902.135613	24.208935
138.288167	3898.594474	24.213952
138.678760	3916.189434	24.218970
138.641499	3927.457416	24.223987
138.784040	3927.399309	24.229005
139.134952	3915.632981	24.234023
139.005494	3926.848800	24.239040
138.828946	3927.282862	24.244058
139.180749	3930.103455	24.249075
139.067452	3941.348960	24.254093
139.349267	3947.242241	24.259111
139.277865	3959.980379	24.264128
139.460462	3953.169039	24.269146
139.925253	3979.705565	24.274163
139.973625	3980.132872	24.279181
140.849376	3965.056887	24.284199
140.877525	3965.478765	24.289216
140.887742	3975.909330	24.294234
140.887738	3967.501936	24.299251
140.657422	3966.040948	24.304269
140.953602	3956.303357	24.309287
140.768434	3966.116891	24.314304
141.521603	3981.095242	24.319322
141.825063	3989.751640	24.324339
141.358252	3997.245512	24.329357
141.695203	3982.126410	24.334375
141.769214	3984.159845	24.339392
141.961708	3997.909228	24.344410
141.864118	3989.029675	24.349427
141.719993	4015.109568	24.354445
142.185523	4009.892415	24.359463
142.146716	4013.694867	24.364480
142.429835	4020.075677	24.369498
142.971930	4036.152828	24.374515
142.987031	4044.085914	24.379533
143.209696	4042.769804	24.384551
143.223053	4044.764934	24.389568
143.317672	4038.868267	24.394586
143.553480	4039.706202	24.399603
143.759025	4038.587118	24.404621
143.888122	4066.262868	24.409639
143.501196	4066.713957	24.414656
143.841741	4062.093311	24.419674
143.821204	4065.182539	24.424691
143.839103	4087.265837	24.429709
144.439121	4100.174727	24.434727
144.633480	4108.651933	24.439744
144.448106	4096.704298	24.444762
145.055167	4100.172527	24.449779
144.810492	4125.360092	24.454797
145.392032	4108.656136	24.459815
145.371264	4125.579865	24.464832
145.400118	4116.355196	24.469850
145.799817	4125.089152	24.474867
145.445850	4119.725727	24.479885
145.757671	4134.116982	24.484903
146.077565	4154.665501	24.489920
146.179513	4160.958837	24.494938
146.477155	4147.799826	24.499955
145.991840	4158.786225	24.504973
146.183822	4165.965115	24.509991
146.322620	4185.075481	24.515008
146.472823	4180.777774	24.520026
146.803652	4183.534898	24.525043
146.564429	4194.326334	24.530061
147.086322	4206.715224	24.535079
147.426169	4203.166042	24.540096
147.545111	4208.230326	24.545114
147.927689	4193.880141	24.550131
147.795919	4213.489930	24.555149
147.918893	4219.801965	24.560167
148.074619	4216.945269	24.565184
147.910630	4226.527475	24.570202
148.376716	4224.179806	24.575219
148.037803	4236.451882	24.580237
148.629345	4252.426206	24.585255
148.899124	4258.199604	24.590272
148.405903	4256.634188	24.595290
148.560653	4261.385993	24.600307
148.742205	4281.921349	24.605325
149.175637	4281.243404	24.610343
149.087236	4290.307792	24.615360
149.255270	4310.485850	24.620378
149.720744	4317.654249	24.625395
149.716613	4324.081777	24.630413
150.115090	4335.913847	24.635431
150.276633	4335.281608	24.640448
150.612616	4337.599782	24.645466
150.791329	4318.308046	24.650483
150.748512	4328.182510	24.655501
151.059362	4334.256967	24.660519
151.143302	4348.225367	24.665536
151.165831	4353.488361	24.670554
151.820801	4355.521260	24.675571
151.507343	4352.505710	24.680589
151.484811	4346.355420	24.685607
151.919966	4357.792272	24.690624
151.704588	4367.995559	24.695642
151.975755	4367.997181	24.700659
152.160313	4386.438162	24.705677
152.457624	4375.026137	24.710695
152.635077	4378.488986	24.715712
152.752205	4389.987581	24.720730
152.786531	4404.347828	24.725747
152.976689	4421.662271	24.730765
153.191241	4421.630442	24.735783
153.467309	4410.533289	24.740800
153.305559	4417.940189	24.745818
153.498884	4428.004410	24.750835
153.576607	4437.910861	24.755853
153.374904	4433.518937	24.760871
153.669577	4456.757513	24.765888
154.047562	4462.879533	24.770906
154.295760	4473.170244	24.775923
154.528184	4466.906097	24.780941
154.402948	4459.443486	24.785959
154.954109	4472.894631	24.790976
155.144689	4483.445478	24.795994
155.590644	4485.893246	24.801011
155.353531	4492.239209	24.806029
155.509143	4489.567341	24.811047
155.610781	4476.726414	24.816064
155.508499	4498.234786	24.821082
156.022214	4480.158294	24.826099
155.606793	4497.983155	24.831117
155.829136	4498.414993	24.836135
156.163253	4498.678762	24.841152
156.182104	4519.322989	24.846170
156.371854	4512.743099	24.851187
156.222933	4524.000236	24.856205
156.568050	4534.570534	24.861223
156.830735	4552.344773	24.866240
156.863875	4552.565276	24.871258
157.376361	4553.525115	24.876275
157.304823	4573.810957	24.881293
157.266797	4572.745615	24.886311
157.843825	4562.962062	24.891328
157.906674	4590.504621	24.896346
158.115904	4592.420611	24.901363
157.880119	4599.198282	24.906381
158.285729	4591.680861	24.911399
158.797994	4597.886941	24.916416
158.720241	4612.877279	24.921434
159.046461	4615.308760	24.926451
159.138205	4621.141368	24.931469
159.325097	4626.253963	24.936487
159.640142	4617.421519	24.941504
159.631348	4621.106064	24.946522
159.799850	4632.014533	24.951539
159.973713	4634.802278	24.956557
159.832913	4643.556641	24.961575
160.482166	4637.153594	24.966592
159.806432	4647.232230	24.971610
160.604824	4647.809018	24.976627
160.863741	4662.722131	24.981645
160.541054	4674.880278	24.986663
160.893836	4667.725239	24.991680
160.561255	4671.580990	24.996698
160.699323	4695.500988	25.001715
161.208067	4691.118437	25.006733
160.987486	4701.824672	25.011751
161.542730	4717.716404	25.016768
161.587396	4726.224129	25.021786
161.982374	4727.476474	25.026803
162.303836	4734.678268	25.031821
162.416536	4751.674266	25.036839
162.904952	4751.129137	25.041856
162.908029	4757.668199	25.046874
162.999391	4746.918840	25.051891
162.892950	4756.329376	25.056909
162.654708	4754.556477	25.061927
163.138426	4767.261092	25.066944
162.800903	4784.725386	25.071962
163.464457	4786.103264	25.076979
163.732779	4802.715005	25.081997
163.600035	4816.421824	25.087015
163.826357	4813.297305	25.092032
164.226325	4816.808170	25.097050
164.453156	4830.079289	25.102067
164.489188	4847.989930	25.107085
164.684836	4837.396159	25.112103
164.586534	4832.021600	25.117120
165.046462	4844.000047	25.122138
165.605775	4854.979323	25.127155
165.742364	4849.271522	25.132173
165.671560	4861.083650	25.137191
165.778495	4861.071339	25.142208
165.788490	4859.581385	25.147226
165.808618	4861.131079	25.152243
166.057662	4860.367656	25.157261
166.106262	4886.210688	25.162279
166.335656	4879.664435	25.167296
166.203520	4894.898945	25.172314
166.713613	4904.444924	25.177331
167.002345	4914.663405	25.182349
166.987916	4921.980990	25.187367
167.373282	4914.525635	25.192384
167.910419	4927.242327	25.197402
168.077080	4936.054046	25.202419
168.231062	4949.362848	25.207437
168.192668	4936.588685	25.212455
168.774952	4939.758992	25.217472
168.345312	4945.962775	25.222490
168.465178	4941.074172	25.227507
169.159727	4931.091495	25.232525
168.823617	4943.939555	25.237543
168.752057	4937.276842	25.242560
168.941816	4952.781055	25.247578
169.179128	4957.540379	25.252595
169.382529	4962.184750	25.257613
169.714038	4978.715816	25.262631
169.763124	4997.695224	25.267648
169.981529	4995.547408	25.272666
170.301201	4983.421768	25.277683
170.725353	4984.652179	25.282701
170.363774	4987.039977	25.287719
170.597066	5002.799266	25.292736
170.917505	5010.357725	25.297754
170.978987	5008.105124	25.302771
170.926551	5004.343745	25.307789
171.043993	5036.237414	25.312807
171.309510	5032.599979	25.317824
171.615303	5052.543907	25.322842
171.176792	5048.877108	25.327859
171.776019	5058.276816	25.332877
171.760201	5071.376009	25.337895
171.846246	5072.368473	25.342912
172.107033	5086.936368	25.347930
172.465596	5093.141207	25.352947
172.767474	5094.496537	25.357965
172.753357	5106.244757	25.362983
173.323138	5118.581165	25.368000
173.422141	5133.049029	25.373018
173.109310	5119.192715	25.378035
173.296137	5115.853372	25.383053
173.446275	5153.388107	25.388071
173.782023	5154.928422	25.393088
173.830758	5153.599039	25.398106
174.170799	5168.255076	25.403123
174.284329	5181.558737	25.408141
173.932132	5191.785977	25.413159
174.496282	5186.913785	25.418176
175.137451	5208.811296	25.423194
174.674432	5217.735373	25.428211
175.033144	5224.950352	25.433229
174.888905	5243.795694	25.438247
175.608948	5245.511546	25.443264
175.501192	5255.673112	25.448282
176.048551	5272.572884	25.453299
176.563418	5259.004575	25.458317
176.680062	5261.461712	25.463335
176.929335	5264.061337	25.468352
177.329209	5260.419735	25.473370
176.772473	5267.864071	25.478387
177.139900	5276.598360	25.483405
177.313611	5293.139992	25.488423
177.498641	5288.852932	25.493440
177.618731	5293.447755	25.498458
177.621633	5318.646665	25.503475
177.975926	5306.820478	25.508493
177.931965	5324.547779	25.513511
178.612038	5313.275404	25.518528
178.940783	5322.995323	25.523546
178.830619	5341.706339	25.528563
179.045129	5343.031568	25.533581
179.206716	5346.063709	25.538599
179.448023	5339.895328	25.543616
179.740894	5353.697640	25.548634
179.577674	5341.210502	25.553651
179.208378	5340.537768	25.558669
179.579214	5382.130291	25.563687
179.818060	5373.559715	25.568704
179.784280	5380.765755	25.573722
179.543941	5416.457246	25.578739
179.914651	5419.002925	25.583757
180.469798	5440.071942	25.588775
180.506479	5441.069154	25.593792
180.926032	5461.582381	25.598810
181.150560	5469.805398	25.603827
181.704842	5467.668479	25.608845
181.526196	5483.454622	25.613863
181.921321	5499.292490	25.618880
182.462022	5495.666142	25.623898
182.475467	5496.309900	25.628915
182.829461	5489.859946	25.633933
182.535431	5498.984607	25.638951
182.885536	5495.974739	25.643968
182.726228	5488.590198	25.648986
183.085581	5497.321974	25.654003
183.521924	5503.443786	25.659021
183.203116	5513.320561	25.664039
183.385589	5505.563695	25.669056
183.564942	5508.663841	25.674074
183.805959	5531.151934	25.679092
184.035606	5545.114766	25.684109
184.296654	5540.931161	25.689127
184.706873	5544.949571	25.694144
184.537121	5565.648149	25.699162
184.412384	5564.739738	25.704180
185.114468	5564.316293	25.709197
184.953416	5589.000549	25.714215
184.906374	5594.225516	25.719232
185.389131	5596.250657	25.724250
185.392283	5622.300479	25.729268
185.592314	5627.184759	25.734285
185.590997	5631.799830	25.739303
185.846537	5656.814287	25.744320
186.313867	5657.694084	25.749338
186.215018	5677.648301	25.754356
186.615005	5677.557017	25.759373
186.754797	5695.233442	25.764391
187.009617	5710.305618	25.769408
187.399655	5715.482976	25.774426
187.442875	5726.195886	25.779444
187.834408	5735.242081	25.784461
188.179951	5740.393500	25.789479
188.135743	5748.680757	25.794496
188.586343	5747.943378	25.799514
188.321052	5758.876999	25.804532
188.942227	5758.444421	25.809549
188.986793	5781.834324	25.814567
189.014887	5778.677482	25.819584
189.368011	5773.573621	25.824602
189.444591	5797.509148	25.829620
189.536774	5801.483925	25.834637
189.686536	5804.059389	25.839655
190.002835	5827.775804	25.844672
190.569976	5830.739460	25.849690
190.293780	5832.437983	25.854708
190.810404	5832.233699	25.859725
191.420230	5819.583581	25.864743
191.178622	5811.793461	25.869760
191.893063	5816.003398	25.874778
191.986052	5826.117620	25.879796
192.347316	5812.371895	25.884813
192.551904	5798.104389	25.889831
192.460076	5800.055162	25.894848
192.674900	5786.221879	25.899866
192.322280	5788.432147	25.904884
192.750474	5779.968827	25.909901
192.721987	5790.187356	25.914919
192.752096	5806.053065	25.919936
193.171551	5812.059692	25.924954
193.308121	5824.819000	25.929972
193.271674	5812.760468	25.934989
193.286835	5835.330662	25.940007
193.356851	5843.463660	25.945024
193.942160	5845.903614	25.950042
193.809356	5855.978327	25.955060
194.092111	5879.027526	25.960077
194.457367	5880.088823	25.965095
194.307325	5888.074407	25.970112
194.756417	5908.050938	25.975130
194.654075	5925.929092	25.980148
195.075921	5929.549247	25.985165
194.905845	5944.588699	25.990183
194.785641	5949.060756	25.995200
195.121216	5965.664667	26.000218
195.403480	5991.914532	26.005236
195.649767	6000.320833	26.010253
196.091691	5998.053064	26.015271
195.961733	6028.339335	26.020288
196.482873	6036.044920	26.025306
196.907095	6049.564179	26.030324
197.094275	6056.777808	26.035341
197.270747	6054.462660	26.040359
197.477626	6083.339020	26.045376
198.130057	6079.766317	26.050394
198.151975	6081.062526	26.055412
198.331360	6085.373575	26.060429
198.641452	6090.320712	26.065447
198.420599	6112.382173	26.070464
198.779931	6111.402066	26.075482
198.855289	6122.483054	26.080500
199.280478	6135.775658	26.085517
199.476267	6140.988856	26.090535
199.394437	6141.274130	26.095552
199.551454	6142.686487	26.100570
200.057207	6167.595053	26.105588
200.323884	6156.159794	26.110605
200.416893	6169.932583	26.115623
200.071543	6180.716421	26.120640
200.554135	6192.890623	26.125658
200.937009	6196.721611	26.130676
201.153341	6224.775383	26.135693
201.262239	6227.965589	26.140711
201.824659	6223.441083	26.145728
202.350014	6205.173393	26.150746
202.320684	6217.892615	26.155764
202.669377	6222.010712	26.160781
202.795930	6225.434125	26.165799
202.729511	6236.706163	26.170816
202.978424	6228.891124	26.175834
203.288215	6234.310403	26.180852
203.174614	6247.164243	26.185869
203.830686	6241.797148	26.190887
203.614083	6239.010435	26.195904
203.765822	6233.708793	26.200922
203.584611	6253.337830	26.205940
203.852607	6261.991006	26.210957
204.047103	6263.041005	26.215975
204.098210	6280.210658	26.220992
204.487352	6295.409144	26.226010
204.394816	6297.194091	26.231028
204.847918	6312.375318	26.236045
205.026321	6325.546153	26.241063
205.091525	6339.754671	26.246080
205.527169	6349.502289	26.251098
205.718336	6366.640275	26.256116
205.848142	6373.724738	26.261133
206.341157	6375.045004	26.266151
206.283450	6381.700688	26.271168
206.620064	6384.513177	26.276186
206.574655	6411.782156	26.281204
206.689669	6410.618328	26.286221
207.297636	6432.784167	26.291239
207.592962	6445.418787	26.296256
207.680103	6434.977281	26.301274
207.762132	6451.903818	26.306292
207.926498	6470.405707	26.311309
208.498896	6472.884807	26.316327
208.384851	6480.270971	26.321344
208.795694	6489.592281	26.326362
208.765216	6491.785126	26.331380
208.954044	6507.567280	26.336397
209.564125	6522.868464	26.341415
209.430736	6530.127134	26.346432
209.829493	6527.103014	26.351450
210.099435	6543.865165	26.356468
210.192618	6554.933408	26.361485
210.832051	6550.300545	26.366503
210.763860	6554.439560	26.371520
211.045144	6561.379592	26.376538
211.343640	6580.262272	26.381556
211.420684	6570.403697	26.386573
212.179883	6576.880466	26.391591
211.661746	6579.582207	26.396608
212.031356	6593.747164	26.401626
212.121395	6602.222778	26.406644
212.093642	6600.285491	26.411661
212.697801	6607.410104	26.416679
212.582224	6633.056569	26.421696
212.462647	6629.195330	26.426714
213.102715	6644.469045	26.431732
213.244311	6638.607913	26.436749
213.491573	6668.893583	26.441767
213.684389	6668.832967	26.446784
213.575784	6682.688727	26.451802
213.752593	6687.256063	26.456820
213.830350	6704.528961	26.461837
214.399106	6708.885912	26.466855
214.256993	6728.129336	26.471872
214.668727	6742.262545	26.476890
215.224935	6761.958021	26.481908
215.153213	6770.217191	26.486925
215.722725	6763.624548	26.491943
215.828310	6775.533611	26.496960
216.094721	6791.533439	26.501978
216.642608	6776.008868	26.506996
216.333634	6785.582010	26.512013
216.952340	6802.587047	26.517031
216.812606	6810.862589	26.522048
216.847228	6806.409459	26.527066
217.063037	6805.861312	26.532084
217.341314	6821.056772	26.537101
217.483844	6839.546869	26.542119
217.480979	6857.547189	26.547136
217.611130	6850.635879	26.552154
217.883562	6895.542590	26.557172
218.030471	6886.545991	26.562189
218.693989	6914.168658	26.567207
218.837213	6923.022285	26.572224
219.055244	6935.058320	26.577242
219.397928	6954.483607	26.582260
219.461349	6956.685156	26.587277
219.952973	6963.873517	26.592295
220.064234	6977.001349	26.597312
220.364479	6973.641940	26.602330
221.016506	6990.481379	26.607348
221.177404	6998.319645	26.612365
221.260725	6996.131712	26.617383
221.233164	7002.486251	26.622400
221.488523	7016.848428	26.627418
221.880636	7030.081814	26.632436
222.069267	7032.700868	26.637453
222.580077	7032.912930	26.642471
222.212515	7036.784300	26.647488
222.535966	7046.110455	26.652506
222.691372	7048.780442	26.657524
222.564225	7073.546739	26.662541
223.125992	7081.192902	26.667559
223.357272	7092.791859	26.672576
223.623673	7099.017755	26.677594
224.052281	7113.390962	26.682612
224.332420	7108.616934	26.687629
224.411380	7110.585500	26.692647
224.386162	7144.055655	26.697664
224.588937	7141.195622	26.702682
225.029680	7140.867316	26.707700
224.905012	7172.915135	26.712717
225.428759	7190.341742	26.717735
225.291248	7180.516177	26.722752
225.547020	7201.626005	26.727770
225.710160	7213.434978	26.732788
226.136273	7219.332550	26.737805
226.106565	7230.165179	26.742823
225.948292	7246.888598	26.747840
226.214064	7255.301954	26.752858
226.972687	7267.691906	26.757876
226.918048	7296.673694	26.762893
227.507908	7287.542515	26.767911
227.725416	7299.167434	26.772928
227.692640	7326.916815	26.777946
228.431453	7321.493668	26.782964
228.148847	7336.461984	26.787981
228.746054	7345.647915	26.792999
228.792737	7353.591911	26.798016
229.182930	7373.448425	26.803034
229.484337	7373.266641	26.808052
229.514804	7386.154364	26.813069
229.706490	7393.974557	26.818087
229.958880	7400.595429	26.823104
230.164586	7414.162580	26.828122
230.964716	7418.900660	26.833140
230.732181	7435.275770	26.838157
231.151246	7438.384539	26.843175
231.473475	7438.555859	26.848192
231.481098	7446.800397	26.853210
231.807536	7460.224030	26.858228
231.840590	7471.645592	26.863245
232.260404	7472.397758	26.868263
232.461933	7491.072032	26.873280
232.465991	7488.771560	26.878298
232.895069	7497.571311	26.883316
232.926175	7510.717901	26.888333
233.267730	7511.055306	26.893351
233.374980	7531.505541	26.898368
233.397119	7554.559559	26.903386
233.978329	7551.218969	26.908404
233.896016	7559.562881	26.913421
234.529171	7580.568247	26.918439
235.050764	7578.012166	26.923456
235.308812	7590.797697	26.928474
235.366144	7596.104297	26.933492
235.559355	7602.855076	26.938509
235.779542	7603.082006	26.943527
235.867172	7620.140383	26.948544
235.935196	7633.782399	26.953562
236.139443	7637.307846	26.958580
236.307083	7665.628616	26.963597
236.430769	7668.541391	26.968615
236.825660	7683.769507	26.973632
237.069828	7701.641776	26.978650
237.439340	7717.297281	26.983668
237.759966	7719.921384	26.988685
237.645931	7734.616167	26.993703
238.083748	7733.881532	26.998720
238.009660	7743.254186	27.003738
238.344410	7740.429656	27.008756
238.513434	7774.019764	27.013773
238.983079	7782.724309	27.018791
239.295228	7777.343833	27.023808
239.630810	7792.890738	27.028826
239.793145	7802.269806	27.033844
239.982352	7820.003055	27.038861
240.215790	7819.794335	27.043879
240.515291	7826.220624	27.048896
240.688581	7842.310395	27.053914
240.911128	7842.654977	27.058932
240.884548	7856.106128	27.063949
241.402587	7867.560844	27.068967
241.190449	7879.995898	27.073984
241.518508	7892.228405	27.079002
241.885948	7909.815327	27.084020
241.827096	7930.451528	27.089037
242.541184	7949.118641	27.094055
242.785862	7958.875740	27.099072
242.917751	7977.584545	27.104090
243.506002	7984.497566	27.109108
243.819384	7998.122052	27.114125
243.883852	7996.303644	27.119143
244.107195	8016.307216	27.124160
244.329130	8027.402461	27.129178
244.456831	8036.511804	27.134196
244.859349	8046.355532	27.139213
245.350608	8041.976385	27.144231
245.270284	8050.977265	27.149248
245.525037	8082.282801	27.154266
245.836000	8066.454745	27.159284
246.089168	8103.843638	27.164301
246.300081	8094.839257	27.169319
246.452546	8102.009064	27.174336
246.837760	8111.091177	27.179354
247.267539	8118.901342	27.184372
247.438548	8126.194100	27.189389
247.383085	8147.825419	27.194407
247.951978	8153.428363	27.199424
248.190391	8151.836361	27.204442
248.229482	8156.573246	27.209460
248.800632	8171.030202	27.214477
248.908109	8164.167535	27.219495
249.085029	8185.817734	27.224512
249.452275	8193.916451	27.229530
249.791286	8192.042456	27.234548
249.661862	8210.407652	27.239565
249.879287	8218.537345	27.244583
250.284302	8224.623596	27.249600
250.132108	8243.136456	27.254618
250.577522	8257.947949	27.259636
250.644991	8257.720829	27.264653
250.673591	8297.984173	27.269671
250.933563	8298.089107	27.274688
251.178068	8311.813774	27.279706
251.598745	8318.715109	27.284724
251.907627	8330.599312	27.289741
252.046751	8348.176722	27.294759
252.526834	8366.907630	27.299776
252.459366	8377.280508	27.304794
252.992697	8386.496160	27.309812
253.039366	8389.567709	27.314829
253.480655	8418.006027	27.319847
254.141283	8409.803188	27.324864
254.191744	8435.349970	27.329882
254.611639	8438.543017	27.334900
254.466898	8451.890003	27.339917
254.427772	8463.489859	27.344935
255.230402	8467.123925	27.349952
255.225222	8491.089425	27.354970
255.507571	8496.565852	27.359988
255.881299	8502.233874	27.365005
256.121075	8510.869264	27.370023
256.282127	8520.995725	27.375040
256.321976	8549.126093	27.380058
256.965246	8552.523556	27.385076
257.282805	8566.003902	27.390093
257.268893	8578.661312	27.395111
257.868838	8583.906170	27.400128
257.965822	8597.860774	27.405146
258.122058	8615.289415	27.410164
258.599388	8621.047984	27.415181
258.666594	8626.134628	27.420199
258.977036	8649.178224	27.425216
259.200666	8656.519510	27.430234
259.686648	8651.628778	27.435252
259.652662	8665.254951	27.440269
259.689009	8672.926682	27.445287
260.125632	8694.973728	27.450304
260.307162	8702.302076	27.455322
260.262638	8702.446106	27.460340
261.094245	8735.850942	27.465357
261.198752	8744.545012	27.470375
261.610360	8762.783735	27.475392
261.759735	8772.209547	27.480410
262.179971	8797.009492	27.485428
262.318526	8806.879277	27.490445
262.544160	8805.057903	27.495463
262.853921	8820.560428	27.500480
263.085552	8835.420738	27.505498
263.611073	8849.174292	27.510516
263.853698	8859.649947	27.515533
263.858132	8856.780287	27.520551
264.061558	8882.477355	27.525568
264.051730	8896.307624	27.530586
264.627259	8896.876105	27.535604
264.648305	8915.465265	27.540621
264.582546	8944.099505	27.545639
265.479140	8940.434515	27.550656
265.903221	8948.384522	27.555674
265.715884	8958.765892	27.560692
266.480067	8963.089626	27.565709
266.457593	8975.221522	27.570727
266.758740	8984.157047	27.575744
266.897603	9014.427797	27.580762
267.523761	9016.835831	27.585780
267.925688	9003.146007	27.590797
267.508918	9027.390430	27.595815
268.085601	9038.504250	27.600832
268.330050	9032.731625	27.605850
268.615556	9056.781539	27.610868
268.881869	9075.555677	27.615885
268.769578	9081.434766	27.620903
269.274221	9092.499125	27.625920
269.455762	9101.057977	27.630938
269.688087	9134.519489	27.635956
269.966614	9124.974132	27.640973
270.049251	9145.957336	27.645991
270.368443	9149.652108	27.651008
270.626520	9194.408706	27.656026
270.932531	9186.171085	27.661044
271.121839	9203.826885	27.666061
271.418444	9241.748377	27.671079
272.051573	9234.855736	27.676096
272.164058	9251.109774	27.681114
272.404999	9261.708344	27.686132
272.878832	9278.982877	27.691149
272.961045	9322.698094	27.696167
273.231997	9301.326641	27.701184
273.425110	9319.358112	27.706202
273.849255	9356.701651	27.711220
274.473947	9335.614499	27.716237
274.114448	9393.310087	27.721255
274.850252	9373.215959	27.726272
275.040389	9409.258789	27.731290
274.981189	9396.045397	27.736308
275.349906	9435.161432	27.741325
275.915270	9434.029075	27.746343
276.010964	9459.776963	27.751360
276.450055	9457.310847	27.756378
276.476509	9494.705526	27.761396
276.728277	9471.731975	27.766413
277.085160	9521.424674	27.771431
277.324136	9510.471682	27.776448
277.906518	9536.334927	27.781466
278.011679	9567.376266	27.786484
278.485179	9558.189478	27.791501
278.423526	9585.504628	27.796519
278.707548	9599.568463	27.801536
279.236602	9606.840688	27.806554
279.266979	9644.429091	27.811572
279.625907	9625.995690	27.816589
279.446118	9666.634704	27.821607
279.615720	9646.673737	27.826624
279.829621	9683.538135	27.831642
280.037176	9698.111193	27.836660
280.682479	9696.153184	27.841677
280.566314	9754.518430	27.846695
281.113551	9742.844101	27.851712
281.501086	9766.976476	27.856730
281.869355	9787.168258	27.861748
282.341685	9782.228980	27.866765
282.214404	9826.756937	27.871783
282.807861	9813.785012	27.876800
283.094837	9861.431368	27.881818
283.417884	9872.833731	27.886836
284.015143	9868.836148	27.891853
284.086089	9890.366030	27.896871
284.383432	9905.129190	27.901888
284.924069	9899.795355	27.906906
285.133215	9915.653440	27.911924
285.421191	9933.566263	27.916941
285.093855	9935.126225	27.921959
285.789755	9959.632349	27.926976
286.109466	9972.417973	27.931994
286.383578	9991.706287	27.937012
287.168721	10000.048264	27.942029
286.774475	10007.255761	27.947047
286.879289	10014.291648	27.952064
287.094154	10028.850880	27.957082
287.068947	10069.666231	27.962100
288.028025	10082.018744	27.967117
287.983929	10098.681507	27.972135
287.961210	10112.407142	27.977152
288.649696	10153.080249	27.982170
288.574594	10157.813541	27.987188
289.320407	10166.858726	27.992205
289.711174	10200.861614	27.997223
289.745333	10213.090936	28.002240
290.308088	10225.825844	28.007258
290.725837	10239.813882	28.012276
290.923940	10254.008496	28.017293
291.454778	10272.156092	28.022311
291.611182	10278.349708	28.027328
291.867574	10284.003672	28.032346
292.074371	10313.255769	28.037364
292.596168	10320.562949	28.042381
292.597093	10336.511719	28.047399
292.892639	10358.937056	28.052416
293.481604	10361.435848	28.057434
293.606432	10386.021491	28.062452
293.863116	10383.874690	28.067469
293.980938	10401.894282	28.072487
294.286679	10415.013429	28.077504
294.678647	10428.810587	28.082522
294.782678	10464.043365	28.087540
295.396565	10471.751854	28.092557
295.475843	10478.215970	28.097575
295.813562	10493.210153	28.102592
296.234798	10506.852407	28.107610
296.508892	10520.065225	28.112628
296.484831	10518.641516	28.117645
296.972089	10543.942065	28.122663
297.457321	10544.085494	28.127680
297.491797	10558.292703	28.132698
297.587010	10568.843813	28.137716
298.034450	10590.658209	28.142733
297.889119	10603.603876	28.147751
298.457825	10628.241547	28.152768
298.878247	10648.039776	28.157786
298.903188	10660.739969	28.162804
299.587961	10675.219823	28.167821
299.439319	10689.495688	28.172839
299.913458	10712.599011	28.177856
300.458636	10725.031800	28.182874
300.053359	10740.299286	28.187892
300.431249	10758.270381	28.192909
300.876742	10776.914218	28.197927
301.181847	10811.889507	28.202944
301.613674	10840.197013	28.207962
301.943896	10845.710358	28.212980
302.474187	10880.712485	28.217997
302.514290	10892.534146	28.223015
302.887589	10911.336036	28.228032
303.372184	10916.161766	28.233050
303.467915	10943.118255	28.238068
303.890160	10971.226852	28.243085
304.683578	10984.380136	28.248103
304.823749	10991.874387	28.253120
305.348482	11016.905333	28.258138
305.545567	11020.404400	28.263156
305.995660	11037.015413	28.268173
305.841013	11048.106029	28.273191
305.781140	11066.572239	28.278208
306.692756	11084.769530	28.283226
306.953877	11102.943805	28.288244
307.271814	11123.409844	28.293261
307.576362	11116.292097	28.298279
307.745803	11157.999775	28.303296
307.997880	11167.786524	28.308314
308.534094	11176.669376	28.313332
308.704510	11187.442675	28.318349
308.759240	11207.791014	28.323367
309.153904	11221.255571	28.328384
309.567067	11234.923387	28.333402
309.575303	11259.435385	28.338420
310.123954	11285.081161	28.343437
310.558479	11293.391213	28.348455
310.407216	11307.938418	28.353472
310.948482	11343.551773	28.358490
311.103140	11334.016503	28.363508
311.451560	11389.326158	28.368525
311.918651	11399.854591	28.373543
311.702660	11411.820179	28.378560
312.223199	11433.429758	28.383578
312.376208	11448.490143	28.388596
312.919958	11470.533658	28.393613
313.523436	11483.098271	28.398631
313.678579	11503.519546	28.403648
313.954614	11522.441982	28.408666
314.297424	11539.619203	28.413684
314.358402	11555.416455	28.418701
314.686269	11567.003506	28.423719
315.111802	11595.099760	28.428736
315.403664	11602.321835	28.433754
315.606791	11638.424608	28.438772
315.665861	11644.839322	28.443789
316.381084	11673.469595	28.448807
316.866084	11699.854618	28.453824
317.303167	11700.642056	28.458842
317.460587	11734.807592	28.463860
317.933491	11739.017242	28.468877
318.055048	11762.462489	28.473895
318.081561	11789.973001	28.478912
318.780741	11795.056812	28.483930
319.027843	11813.642652	28.488948
319.351492	11826.729093	28.493965
320.201579	11841.324614	28.498983
320.237928	11857.615251	28.504000
320.807388	11875.128218	28.509018
320.927338	11889.964497	28.514036
321.612115	11900.936129	28.519053
321.471290	11908.243441	28.524071
321.569458	11932.759120	28.529088
322.195013	11940.170588	28.534106
322.568392	11961.395905	28.539124
322.470217	11994.920395	28.544141
323.071326	11986.592122	28.549159
323.010504	12005.259538	28.554176
323.282734	12044.710204	28.559194
323.778090	12056.673123	28.564212
324.410051	12076.491863	28.569229
324.663173	12097.023074	28.574247
324.127907	12127.444911	28.579264
325.311387	12125.535829	28.584282
325.457687	12165.516888	28.589300
325.951014	12191.616532	28.594317
326.575074	12192.732706	28.599335
326.889953	12208.087205	28.604352
326.965591	12215.187015	28.609370
327.190529	12230.550361	28.614388
327.737115	12239.801325	28.619405
327.974781	12266.574243	28.624423
327.959843	12272.187986	28.629440
328.789356	12305.766420	28.634458
329.088072	12316.156064	28.639476
329.193296	12331.217862	28.644493
329.648283	12329.494507	28.649511
329.597829	12359.457232	28.654528
329.881966	12375.980279	28.659546
330.348646	12393.373281	28.664564
330.372694	12403.755992	28.669581
330.782199	12408.339956	28.674599
330.988192	12447.507864	28.679616
331.721159	12460.435377	28.684634
331.689429	12489.035710	28.689652
331.545582	12511.954575	28.694669
332.268013	12521.207993	28.699687
332.615255	12553.844181	28.704704
332.816171	12571.245896	28.709722
333.198527	12596.107358	28.714740
333.387193	12630.842143	28.719757
334.066288	12652.981524	28.724775
334.244044	12683.378998	28.729792
334.820415	12688.062390	28.734810
335.270247	12715.051402	28.739828
335.247763	12744.374663	28.744845
335.806004	12751.978687	28.749863
335.933007	12765.972914	28.754880
336.041039	12793.979141	28.759898
336.535279	12819.986457	28.764916
336.848390	12849.108467	28.769933
337.428932	12872.043488	28.774951
337.517402	12898.997537	28.779968
337.846930	12925.348086	28.784986
338.647016	12945.910367	28.790004
338.826541	12982.231640	28.795021
339.450120	12997.677851	28.800039
339.601573	13017.603526	28.805056
340.147690	13025.191518	28.810074
339.830536	13041.805800	28.815092
340.189958	13069.526506	28.820109
340.900339	13090.973421	28.825127
341.127219	13132.900337	28.830144
341.615347	13139.960823	28.835162
341.934045	13158.182316	28.840180
342.205737	13178.869850	28.845197
342.775636	13209.374722	28.850215
342.890109	13238.681441	28.855232
343.526999	13247.495566	28.860250
344.150889	13272.328111	28.865268
344.254721	13276.014157	28.870285
344.718970	13287.350373	28.875303
344.890374	13312.664389	28.880320
345.174249	13328.410063	28.885338
345.366219	13344.663526	28.890356
345.789989	13373.137052	28.895373
346.022790	13382.778761	28.900391
346.332268	13403.936001	28.905408
346.706331	13424.237611	28.910426
347.122155	13451.250672	28.915444
347.293465	13474.256936	28.920461
347.645041	13490.569934	28.925479
347.753857	13522.316609	28.930496
348.117353	13535.306089	28.935514
348.794274	13562.088043	28.940532
348.710157	13585.339437	28.945549
349.463271	13597.365426	28.950567
349.653050	13631.684358	28.955584
349.805840	13645.920675	28.960602
350.273456	13674.286830	28.965620
350.807718	13707.273325	28.970637
351.181004	13712.810582	28.975655
351.268099	13738.181836	28.980672
351.507134	13744.533341	28.985690
352.140063	13774.148500	28.990708
352.216687	13809.246239	28.995725
352.846059	13825.838846	29.000743
352.994848	13853.511309	29.005760
353.300103	13874.954626	29.010778
353.666551	13901.913188	29.015796
353.899483	13932.253991	29.020813
354.440988	13945.694633	29.025831
354.716711	13976.281477	29.030848
355.028486	14009.954562	29.035866
355.489803	14030.704645	29.040884
355.677496	14060.832018	29.045901
356.311769	14087.215427	29.050919
356.453693	14114.245860	29.055936
356.815215	14142.543503	29.060954
357.484052	14164.454817	29.065972
357.751205	14201.896577	29.070989
358.348340	14209.663007	29.076007
358.382357	14230.736493	29.081024
358.870246	14255.451222	29.086042
359.521033	14266.661824	29.091060
359.731319	14298.178288	29.096077
360.150362	14326.521126	29.101095
360.598377	14337.984795	29.106112
360.710976	14362.791774	29.111130
361.447595	14385.183111	29.116148
361.583286	14402.018059	29.121165
362.119169	14422.800385	29.126183
362.201237	14443.521825	29.131200
362.140214	14463.699035	29.136218
362.731395	14485.429740	29.141236
362.979016	14521.784275	29.146253
363.669696	14540.122118	29.151271
364.209864	14563.020575	29.156288
364.569126	14584.953194	29.161306
364.786385	14604.689409	29.166324
365.139563	14638.298443	29.171341
365.950705	14652.195427	29.176359
365.954867	14680.441397	29.181376
366.168105	14701.361812	29.186394
366.931688	14705.052693	29.191412
367.176769	14726.847947	29.196429
367.363670	14748.380232	29.201447
367.510780	14771.256028	29.206464
367.855913	14788.823472	29.211482
368.534449	14802.268920	29.216500
368.345483	14827.180006	29.221517
369.054295	14852.473527	29.226535
369.279250	14867.929772	29.231552
369.279814	14890.574834	29.236570
369.809732	14913.076835	29.241588
370.087852	14935.172455	29.246605
370.241280	14964.446860	29.251623
370.693235	14993.327582	29.256640
370.834768	15022.205375	29.261658
371.365013	15054.045721	29.266676
371.835120	15083.675304	29.271693
372.465092	15119.156241	29.276711
372.959073	15137.181058	29.281728
372.691702	15164.212540	29.286746
373.392440	15188.269035	29.291764
373.775992	15221.334879	29.296781
374.112757	15254.063155	29.301799
374.847819	15285.073603	29.306816
375.271459	15299.161835	29.311834
376.180006	15305.578926	29.316852
376.210193	15339.834728	29.321869
376.611872	15379.836079	29.326887
377.453619	15372.035725	29.331904
377.266636	15389.010754	29.336922
378.185608	15425.094360	29.341940
378.111445	15439.380224	29.346957
378.301981	15443.148334	29.351975
378.774832	15469.888725	29.356992
379.057503	15501.087025	29.362010
379.390865	15523.027283	29.367028
379.647572	15553.038062	29.372045
380.357327	15556.122221	29.377063
380.588947	15595.900108	29.382080
380.719036	15627.396836	29.387098
381.666930	15647.944356	29.392116
381.831744	15662.447807	29.397133
381.845635	15699.290319	29.402151
382.507250	15713.925244	29.407168
382.617171	15747.736467	29.412186
383.388968	15756.325494	29.417204
383.233369	15801.882649	29.422221
383.612122	15831.213340	29.427239
384.450506	15844.545481	29.432256
384.532181	15885.538422	29.437274
385.336690	15919.501305	29.442292
385.480817	15934.650605	29.447309
385.520339	15969.506601	29.452327
386.013205	15978.245297	29.457344
386.136740	16014.769872	29.462362
386.759269	16045.673835	29.467380
387.270122	16073.838487	29.472397
387.210294	16095.874985	29.477415
388.231284	16122.426047	29.482432
388.157022	16154.049213	29.487450
388.511376	16179.840115	29.492468
389.264384	16213.268056	29.497485
389.695657	16223.233422	29.502503
389.798551	16256.649710	29.507520
389.542021	16292.997257	29.512538
390.654430	16303.887041	29.517556
390.828825	16339.510735	29.522573
391.025521	16364.681311	29.527591
391.802469	16393.792669	29.532608
391.859584	16432.704414	29.537626
392.526765	16451.269137	29.542644
393.131316	16491.036369	29.547661
393.423575	16512.670863	29.552679
394.167275	16525.854641	29.557696
394.350826	16546.384630	29.562714
394.922567	16573.236663	29.567732
395.184473	16610.159438	29.572749
395.247283	16623.250638	29.577767
396.439475	16636.161506	29.582784
396.454970	16674.267818	29.587802
397.018361	16686.762262	29.592820
397.142567	16712.463189	29.597837
397.255932	16742.307228	29.602855
397.706400	16774.821053	29.607872
398.020122	16803.258873	29.612890
398.538001	16822.076543	29.617908
399.065390	16865.796268	29.622925
399.128363	16888.469067	29.627943
399.746399	16926.278843	29.632960
399.903776	16942.260972	29.637978
400.745596	16971.432767	29.642996
401.240755	16998.897474	29.648013
401.743904	17029.000003	29.653031
402.414101	17050.443557	29.658048
402.218999	17075.982998	29.663066
403.266068	17096.371216	29.668084
403.131942	17116.735284	29.673101
403.315304	17144.943747	29.678119
404.120261	17166.128027	29.683136
404.246319	17200.090145	29.688154
404.627627	17230.561851	29.693172
404.911990	17248.233522	29.698189
405.182098	17283.818954	29.703207
405.559128	17303.580031	29.708224
405.982570	17346.379394	29.713242
406.873261	17371.585318	29.718260
407.086655	17393.607397	29.723277
407.510618	17431.940626	29.728295
407.798852	17457.270039	29.733312
408.145076	17483.181733	29.738330
408.476583	17522.793580	29.743348
409.142946	17551.330320	29.748365
409.099726	17575.216610	29.753383
409.892533	17606.268320	29.758400
410.076639	17645.649067	29.763418
410.548374	17655.840595	29.768436
410.677988	17679.512319	29.773453
410.884073	17708.934234	29.778471
411.717562	17727.500186	29.783488
412.268295	17774.019336	29.788506
412.595095	17780.242014	29.793524
413.427620	17810.114273	29.798541
413.898041	17835.827455	29.803559
414.358343	17857.220150	29.808576
414.389665	17881.181446	29.813594
414.773127	17894.924753	29.818612
415.109535	17927.140108	29.823629
415.443466	17966.796011	29.828647
415.861136	17986.452479	29.833664
416.342068	18013.452982	29.838682
416.500184	18041.861581	29.843700
417.070308	18067.632684	29.848717
417.345429	18107.950447	29.853735
418.108263	18134.125187	29.858752
418.266096	18166.651170	29.863770
418.813995	18197.853718	29.868788
419.220031	18231.469766	29.873805
419.607942	18263.064847	29.878823
420.403384	18276.711165	29.883840
420.725070	18312.829307	29.888858
421.540674	18318.050349	29.893876
421.616354	18355.890396	29.898893
422.244486	18382.261815	29.903911
422.664057	18403.987140	29.908928
422.941714	18446.624592	29.913946
423.223779	18451.871631	29.918964
423.873001	18491.756786	29.923981
423.920612	18525.442389	29.928999
424.296494	18545.800894	29.934016
424.715765	18574.134215	29.939034
425.171343	18600.287834	29.944052
425.273101	18636.705937	29.949069
425.773993	18669.149184	29.954087
426.828667	18699.197612	29.959104
426.982301	18738.104107	29.964122
427.385161	18760.602270	29.969140
428.202327	18780.723457	29.974157
428.231024	18804.982854	29.979175
428.663391	18852.809723	29.984192
429.366756	18869.678309	29.989210
429.453106	18911.017206	29.994228
429.604618	18939.630468	29.999245
429.768212	18952.394588	30.004263
430.542885	19000.063043	30.009280
430.860173	19042.885976	30.014298
431.265452	19064.195604	30.019316
432.042956	19105.132381	30.024333
432.224627	19133.514420	30.029351
432.927915	19156.672390	30.034368
433.438742	19190.082087	30.039386
433.828307	19210.640076	30.044404
434.383569	19236.934009	30.049421
434.446558	19258.387020	30.054439
435.333689	19274.549593	30.059456
435.623228	19306.601852	30.064474
435.758374	19331.765211	30.069492
436.400191	19353.482051	30.074509
436.571608	19381.437818	30.079527
437.210160	19409.337325	30.084544
437.856838	19437.216295	30.089562
437.880732	19466.300872	30.094580
438.199898	19500.164225	30.099597
438.477014	19525.248584	30.104615
439.403792	19550.189323	30.109632
439.676970	19589.845073	30.114650
439.847479	19627.785708	30.119668
440.522226	19651.246616	30.124685
440.655650	19698.686683	30.129703
441.245363	19736.722617	30.134720
441.420525	19760.244775	30.139738
441.941937	19796.101856	30.144756
442.815244	19836.975297	30.149773
442.654131	19873.596840	30.154791
443.399115	19904.934426	30.159808
443.672934	19947.320287	30.164826
443.915050	19978.759789	30.169844
444.910737	20014.860340	30.174861
445.204839	20060.923848	30.179879
445.453481	20094.768623	30.184896
445.934612	20127.787791	30.189914
446.299481	20172.307952	30.194932
446.839746	20206.664430	30.199949
447.214588	20248.365667	30.204967
448.177355	20285.232784	30.209984
448.761964	20312.623956	30.215002
448.986879	20354.169030	30.220020
449.718798	20385.699447	30.225037
450.059463	20421.443833	30.230055
450.274443	20455.926310	30.235072
451.107377	20478.188742	30.240090
451.662479	20514.672485	30.245108
452.080636	20539.922639	30.250125
452.377588	20574.322232	30.255143
452.762492	20590.973717	30.260160
453.570288	20620.627757	30.265178
453.350331	20654.224739	30.270196
454.242892	20674.650587	30.275213
454.532710	20712.495705	30.280231
454.767695	20744.944299	30.285248
455.744904	20775.992283	30.290266
456.025656	20807.916332	30.295284
456.602418	20841.109592	30.300301
456.932566	20873.156236	30.305319
457.552172	20884.452663	30.310336
457.924453	20910.423412	30.315354
457.767060	20946.298742	30.320372
458.773114	20971.773696	30.325389
458.694476	21005.067382	30.330407
458.952674	21036.765933	30.335424
459.687128	21057.171403	30.340442
459.835385	21096.922147	30.345460
460.116877	21126.510972	30.350477
460.607738	21181.742605	30.355495
461.318595	21209.651144	30.360512
461.901532	21247.043712	30.365530
461.900194	21282.420075	30.370548
462.801909	21316.105177	30.375565
463.316437	21356.386114	30.380583
463.699835	21393.805700	30.385600
464.440064	21427.624659	30.390618
464.726768	21467.766556	30.395636
465.388034	21492.195141	30.400653
465.488032	21538.712882	30.405671
465.947185	21570.741188	30.410688
466.616281	21616.497521	30.415706
466.539294	21648.513740	30.420724
467.637515	21675.781381	30.425741
468.024617	21718.669826	30.430759
468.352132	21746.152509	30.435776
468.872375	21779.037805	30.440794
469.353841	21827.666892	30.445812
470.073845	21858.997419	30.450829
470.484441	21900.714684	30.455847
471.149532	21931.683954	30.460864
471.667657	21961.652091	30.465882
471.914955	22000.077670	30.470900
472.420262	22026.121220	30.475917
472.599060	22073.700641	30.480935
473.008703	22104.584149	30.485952
473.668855	22144.287102	30.490970
474.382127	22187.084700	30.495988
474.643579	22216.364138	30.501005
475.016902	22258.041034	30.506023
475.725121	22291.300694	30.511040
476.051011	22321.275724	30.516058
476.368654	22368.664590	30.521076
477.149338	22399.069792	30.526093
477.798791	22427.975936	30.531111
478.001518	22472.499312	30.536128
478.955546	22510.677304	30.541146
479.038544	22542.413888	30.546164
479.586684	22578.578271	30.551181
479.921800	22608.110543	30.556199
480.438121	22645.785226	30.561216
481.223669	22678.692362	30.566234
481.319981	22720.986399	30.571252
481.974334	22749.876602	30.576269
482.309415	22791.764199	30.581287
482.589188	22820.351119	30.586304
483.317048	22847.271039	30.591322
483.321085	22873.278491	30.596340
484.108879	22904.040321	30.601357
484.727398	22945.456296	30.606375
484.805691	22983.099173	30.611392
485.519119	23006.093092	30.616410
485.806685	23047.467542	30.621428
486.492821	23086.008585	30.626445
487.143007	23124.941380	30.631463
487.430139	23169.437523	30.636480
487.770953	23202.661546	30.641498
488.198135	23239.006598	30.646516
488.805954	23275.770327	30.651533
489.193717	23317.761981	30.656551
489.907096	23351.931188	30.661568
490.244079	23388.512273	30.666586
490.953596	23438.374926	30.671604
491.487742	23466.321535	30.676621
491.952033	23501.776773	30.681639
491.980154	23540.464700	30.686656
492.469444	23577.379546	30.691674
493.121414	23627.179498	30.696692
493.967959	23655.064864	30.701709
494.103080	23704.955267	30.706727
494.291141	23752.077493	30.711744
495.487440	23771.245647	30.716762
496.024164	23818.672485	30.721780
496.481403	23853.774407	30.726797
497.097548	23886.590540	30.731815
497.783042	23920.052595	30.736832
498.319842	23950.170404	30.741850
498.638822	23985.790863	30.746868
498.926837	24021.617186	30.751885
499.444999	24056.623998	30.756903
499.530518	24100.546798	30.761920
500.572801	24130.645082	30.766938
500.687280	24174.946278	30.771956
501.322684	24210.574338	30.776973
502.051143	24258.880918	30.781991
502.105154	24296.456738	30.787008
502.419251	24329.657449	30.792026
503.250311	24386.017769	30.797044
503.643004	24425.528035	30.802061
504.632623	24470.316857	30.807079
504.633684	24506.986326	30.812096
505.470345	24546.278090	30.817114
505.653586	24584.750868	30.822132
506.235427	24621.666794	30.827149
506.873082	24658.846455	30.832167
507.193122	24695.354484	30.837184
507.785925	24755.012736	30.842202
508.424287	24787.445165	30.847220
508.883225	24824.961671	30.852237
509.843338	24857.967636	30.857255
509.900385	24887.264092	30.862272
510.489337	24925.729784	30.867290
511.196349	24961.125991	30.872308
511.172027	24991.998402	30.877325
511.649792	25032.969633	30.882343
512.051493	25068.709313	30.887360
512.935915	25099.641988	30.892378
513.218006	25134.660421	30.897396
513.676796	25173.658669	30.902413
514.328659	25212.727875	30.907431
514.434377	25264.179647	30.912448
515.037176	25296.452571	30.917466
515.602666	25336.080939	30.922484
515.816794	25380.646104	30.927501
516.542497	25424.653334	30.932519
517.293504	25479.505244	30.937536
517.793353	25512.871041	30.942554
517.967244	25569.229158	30.947572
518.698180	25599.178955	30.952589
519.397342	25644.082734	30.957607
520.084696	25699.505620	30.962624
520.728378	25735.038886	30.967642
521.240116	25778.692031	30.972660
521.089661	25819.937863	30.977677
522.317606	25861.625168	30.982695
522.753048	25902.854303	30.987712
523.289176	25943.991883	30.992730
523.756638	25984.661552	30.997748
524.395044	26018.382883	31.002765
524.728308	26057.058247	31.007783
525.121290	26102.386267	31.012800
526.050878	26130.192654	31.017818
526.702153	26182.548334	31.022836
526.885665	26218.203238	31.027853
527.549222	26263.023836	31.032871
528.028982	26307.217622	31.037888
528.590327	26343.382181	31.042906
528.781638	26385.667668	31.047924
529.266352	26430.971767	31.052941
529.840489	26469.894149	31.057959
530.401108	26524.384507	31.062976
531.012002	26553.117615	31.067994
531.876766	26604.202279	31.073012
532.414743	26641.370142	31.078029
533.302396	26686.070364	31.083047
533.459045	26724.324854	31.088064
534.114281	26758.444476	31.093082
534.501354	26789.410019	31.098100
534.729362	26827.755016	31.103117
535.782748	26875.905119	31.108135
535.997065	26916.552087	31.113152
536.662452	26956.215829	31.118170
537.165771	26995.512369	31.123188
537.327047	27024.304543	31.128205
537.861801	27082.376758	31.133223
538.165508	27132.692183	31.138240
538.827913	27155.987801	31.143258
539.353769	27196.810384	31.148276
539.827744	27246.152883	31.153293
540.779745	27283.203507	31.158311
541.040013	27321.877003	31.163328
541.596944	27366.048810	31.168346
541.980858	27403.067292	31.173364
542.500473	27447.216903	31.178381
542.952094	27484.949588	31.183399
543.283435	27529.077415	31.188416
544.152308	27580.215743	31.193434
544.706726	27634.364996	31.198452
545.176346	27670.661392	31.203469
545.690915	27710.181632	31.208487
546.242211	27760.465101	31.213504
546.481562	27818.551568	31.218522
547.438662	27872.550036	31.223540
547.849233	27911.018226	31.228557
548.647522	27962.162707	31.233575
549.010066	28008.227350	31.238592
549.820960	28046.433566	31.243610
550.327748	28102.692397	31.248628
550.802292	28143.859606	31.253645
551.543196	28182.365648	31.258663
552.118460	28234.498250	31.263680
552.617560	28279.052855	31.268698
553.798070	28313.146484	31.273716
553.699307	28365.799702	31.278733
554.655683	28389.004594	31.283751
555.220422	28446.036960	31.288768
555.758417	28490.712015	31.293786
556.124665	28520.129727	31.298804
556.900667	28558.389988	31.303821
557.846176	28580.878344	31.308839
558.426997	28627.095928	31.313856
558.767306	28671.229388	31.318874
559.861868	28684.359301	31.323892
560.197871	28723.955375	31.328909
560.957413	28761.364671	31.333927
561.438236	28789.392124	31.338944
561.528937	28809.558724	31.343962
562.254526	28847.999463	31.348980
562.501724	28895.478000	31.353997
563.250776	28924.205166	31.359015
563.709084	28953.152025	31.364032
563.634113	29004.186760	31.369050
564.369826	29056.824355	31.374068
564.902806	29101.779240	31.379085
565.506250	29145.749173	31.384103
565.621386	29201.464362	31.389120
566.370787	29246.909930	31.394138
567.121397	29299.140953	31.399156
567.288809	29351.909411	31.404173
568.137721	29390.500412	31.409191
568.763869	29443.142529	31.414208
568.927671	29486.625556	31.419226
569.882838	29519.218026	31.424244
570.165582	29564.524489	31.429261
570.572643	29614.578255	31.434279
571.431457	29660.341640	31.439296
571.744897	29700.963277	31.444314
572.510501	29740.365770	31.449332
572.780297	29804.070129	31.454349
573.548108	29838.908766	31.459367
574.225047	29898.278015	31.464384
574.309230	29954.167756	31.469402
575.100480	29995.327056	31.474420
575.450815	30047.714061	31.479437
576.426570	30086.089531	31.484455
577.006612	30141.002678	31.489472
577.616727	30198.327100	31.494490
578.524653	30241.094788	31.499508
578.926612	30297.693116	31.504525
579.637297	30333.038329	31.509543
580.368156	30378.417527	31.514560
580.913226	30430.993807	31.519578
581.730651	30476.841731	31.524596
581.987211	30518.810867	31.529613
582.518323	30569.175611	31.534631
583.274688	30611.607518	31.539648
583.580094	30675.520790	31.544666
584.319186	30698.620201	31.549684
584.603407	30758.962886	31.554701
585.102034	30794.598180	31.559719
586.071538	30848.710981	31.564736
586.180193	30913.052086	31.569754
587.253403	30963.813969	31.574772
587.499001	31018.721870	31.579789
588.336998	31059.299604	31.584807
589.013779	31111.653799	31.589824
589.251901	31168.052715	31.594842
590.510961	31201.750660	31.599860
590.905129	31259.144721	31.604877
591.531412	31311.761338	31.609895
592.050325	31342.537294	31.614912
592.910826	31390.891540	31.619930
593.410333	31436.316829	31.624948
594.043877	31485.331607	31.629965
594.705965	31526.780124	31.634983
595.154131	31579.884598	31.640000
595.902684	31625.658461	31.645018
596.297614	31661.011133	31.650036
596.888421	31715.752921	31.655053
597.351050	31756.797215	31.660071
598.321797	31790.718813	31.665088
598.420574	31861.437266	31.670106
599.099999	31887.725239	31.675124
599.516582	31950.569811	31.680141
600.603368	31984.627790	31.685159
601.118817	32034.243019	31.690176
601.226630	32081.434654	31.695194
602.082869	32124.040567	31.700212
602.462088	32159.853887	31.705229
603.045033	32214.248696	31.710247
603.567027	32266.267152	31.715264
603.566874	32313.416753	31.720282
604.274576	32369.492843	31.725300
604.858961	32431.562297	31.730317
605.382659	32478.550144	31.735335
606.231716	32523.470430	31.740352
606.777962	32597.818416	31.745370
607.473284	32641.921845	31.750388
608.352898	32705.773657	31.755405
608.643009	32749.902500	31.760423
609.554843	32799.398599	31.765440
610.002717	32859.182322	31.770458
610.784003	32908.404795	31.775476
611.362690	32971.774388	31.780493
612.260802	33022.405044	31.785511
612.926227	33070.021401	31.790528
613.395153	33118.843453	31.795546
614.285472	33160.389002	31.800564
614.608218	33219.074853	31.805581
615.500650	33270.964991	31.810599
616.099613	33317.183514	31.815616
616.720177	33370.050376	31.820634
617.655614	33422.017682	31.825652
618.197523	33463.644698	31.830669
618.561018	33501.211479	31.835687
619.500512	33560.586875	31.840704
619.805712	33610.197776	31.845722
620.339631	33645.488448	31.850740
621.064826	33702.277180	31.855757
621.393586	33751.881602	31.860775
622.380105	33789.259983	31.865792
622.974923	33854.113658	31.870810
623.804922	33894.869923	31.875828
624.207096	33952.609427	31.880845
624.662590	34007.084043	31.885863
625.485379	34051.397934	31.890880
625.695053	34104.260066	31.895898
626.664099	34157.091296	31.900916
627.642427	34214.325402	31.905933
627.878546	34260.350558	31.910951
628.914614	34294.104574	31.915968
629.658344	34347.498778	31.920986
630.214711	34393.142282	31.926004
631.100003	34443.716291	31.931021
631.572564	34478.525124	31.936039
631.901898	34526.073092	31.941056
632.497025	34573.303014	31.946074
633.287921	34610.641896	31.951092
633.666503	34659.875394	31.956109
634.088887	34727.654113	31.961127
634.526267	34761.639983	31.966144
635.646398	34812.087871	31.971162
636.329132	34848.438797	31.976180
636.853846	34876.865358	31.981197
637.307283	34932.068469	31.986215
637.869301	34969.203421	31.991232
638.286794	35024.726261	31.996250
638.797137	35067.555657	32.001268
639.889457	35113.435809	32.006285
640.172687	35164.418433	32.011303
640.943202	35210.561331	32.016320
641.295961	35275.574186	32.021338
642.018543	35321.743942	32.026356
642.789065	35369.124759	32.031373
643.170630	35426.190084	32.036391
643.864953	35477.041998	32.041408
644.373320	35536.439530	32.046426
645.072254	35588.930535	32.051444
645.899559	35648.760072	32.056461
646.179059	35716.493053	32.061479
647.321864	35770.900275	32.066496
647.617261	35834.243948	32.071514
648.400976	35881.379772	32.076532
649.163337	35948.570179	32.081549
649.868167	36005.707403	32.086567
650.599348	36066.001461	32.091584
651.248752	36117.284977	32.096602
651.690322	36168.399954	32.101620
652.795516	36224.485722	32.106637
653.092189	36282.224888	32.111655
653.856748	36337.515542	32.116672
654.281139	36398.673125	32.121690
654.797197	36452.638472	32.126708
655.576645	36524.770845	32.131725
656.245405	36578.769040	32.136743
657.542570	36628.368156	32.141760
658.044945	36703.086781	32.146778
658.788008	36747.914018	32.151796
659.251798	36797.406696	32.156813
659.566619	36859.677531	32.161831
660.518890	36918.634079	32.166848
661.141445	36977.446262	32.171866
661.778011	37032.266129	32.176884
662.328933	37098.692351	32.181901
662.754601	37157.962191	32.186919
663.927737	37209.725354	32.191936
664.137330	37280.053506	32.196954
664.846415	37345.646733	32.201972
665.833134	37399.246943	32.206989
666.237185	37461.747024	32.212007
667.073082	37506.315560	32.217024
667.558399	37574.939296	32.222042
668.400006	37634.258108	32.227060
669.101469	37684.357245	32.232077
669.180627	37749.227767	32.237095
670.258231	37806.732746	32.242112
670.570648	37866.538677	32.247130
671.559906	37908.974314	32.252148
672.610004	37967.565805	32.257165
672.816289	38026.930397	32.262183
673.789183	38078.184177	32.267200
673.894310	38139.413123	32.272218
674.639895	38185.489372	32.277236
675.417221	38246.260082	32.282253
675.951783	38312.950705	32.287271
676.538205	38367.543255	32.292288
677.098986	38440.062391	32.297306
677.689851	38510.090583	32.302324
678.615271	38569.320512	32.307341
679.345395	38638.866668	32.312359
679.722594	38690.420552	32.317376
680.404820	38761.149495	32.322394
681.292274	38827.462736	32.327412
682.043282	38888.780771	32.332429
682.754864	38964.292876	32.337447
683.536364	39026.205720	32.342464
683.832016	39091.770657	32.347482
684.561600	39163.414570	32.352500
685.393311	39223.133166	32.357517
686.074407	39293.159697	32.362535
686.641418	39356.309403	32.367552
687.359903	39417.711797	32.372570
688.515078	39498.273920	32.377588
689.383830	39549.924033	32.382605
689.988154	39624.275134	32.387623
691.157673	39670.830366	32.392640
691.855219	39730.758179	32.397658
692.577708	39776.290561	32.402676
693.037590	39838.058899	32.407693
694.070976	39897.626351	32.412711
694.432527	39959.418670	32.417728
695.049809	40015.405552	32.422746
695.716842	40061.270782	32.427764
696.380097	40116.558441	32.432781
696.982788	40208.212040	32.437799
697.771137	40248.805932	32.442816
697.902862	40315.330467	32.447834
698.735193	40389.022596	32.452852
699.686572	40452.255528	32.457869
700.256971	40520.220103	32.462887
700.828506	40584.004412	32.467904
701.360794	40648.159472	32.472922
701.965478	40718.364890	32.477940
702.945836	40782.053316	32.482957
703.400585	40875.055510	32.487975
704.771707	40927.855109	32.492992
705.444522	40984.741497	32.498010
706.074838	41066.623052	32.503028
706.886934	41124.271472	32.508045
707.672075	41172.284467	32.513063
708.145576	41245.521764	32.518080
708.742397	41274.745612	32.523098
708.995667	41338.137129	32.528116
709.956606	41412.865048	32.533133
710.430062	41473.872323	32.538151
711.400349	41523.370731	32.543168
711.928802	41611.878682	32.548186
712.168175	41670.479584	32.553204
713.270495	41741.594032	32.558221
713.933366	41813.617706	32.563239
714.576727	41863.490858	32.568256
715.134150	41957.383067	32.573274
715.977817	42010.385115	32.578292
716.634591	42076.894419	32.583309
717.108970	42158.708248	32.588327
718.172099	42232.625496	32.593344
718.812856	42300.024518	32.598362
719.416178	42393.362990	32.603380
720.539041	42448.227040	32.608397
721.054008	42526.446750	32.613415
721.462470	42597.334562	32.618432
722.231346	42678.753872	32.623450
723.221773	42754.526985	32.628468
724.168841	42818.425434	32.633485
724.827075	42893.873539	32.638503
725.469772	42965.775936	32.643520
726.136584	43056.562434	32.648538
726.947950	43120.445757	32.653556
727.884848	43191.176189	32.658573
728.576021	43266.008752	32.663591
729.365162	43337.728520	32.668608
730.308405	43414.884174	32.673626
730.805280	43486.099081	32.678644
731.704476	43548.727206	32.683661
732.479747	43605.779468	32.688679
733.181413	43689.384449	32.693696
734.221115	43760.832667	32.698714
734.825812	43801.715004	32.703732
735.602582	43892.242353	32.708749
736.487150	43945.067212	32.713767
737.163417	44006.842945	32.718784
738.129606	44078.881442	32.723802
738.472385	44158.243171	32.728820
739.074978	44218.356374	32.733837
739.700104	44281.283143	32.738855
740.318809	44377.342749	32.743872
741.356983	44431.491611	32.748890
741.893323	44508.259521	32.753908
742.632929	44570.181753	32.758925
743.510030	44650.410190	32.763943
744.166594	44722.393399	32.768960
744.835235	44794.557950	32.773978
745.483488	44876.681903	32.778996
746.133750	44942.219064	32.784013
746.881891	45029.431971	32.789031
747.630710	45103.307458	32.794048
748.519801	45158.034383	32.799066
749.066684	45226.267355	32.804084
749.693962	45284.780920	32.809101
750.294471	45365.381619	32.814119
750.957175	45437.972513	32.819136
751.875625	45498.752831	32.824154
752.305698	45564.163343	32.829172
753.191933	45658.988659	32.834189
754.035060	45736.612255	32.839207
754.982455	45812.695853	32.844224
756.163921	45866.715972	32.849242
756.518931	45951.033756	32.854260
757.252019	46022.969155	32.859277
757.917455	46108.724191	32.864295
758.542557	46177.995835	32.869312
759.480721	46264.424367	32.874330
760.117163	46343.626277	32.879348
761.126674	46404.502525	32.884365
761.794523	46497.723482	32.889383
762.187449	46581.284255	32.894400
763.391784	46654.961305	32.899418
763.869458	46730.846044	32.904436
764.994227	46809.306644	32.909453
765.669916	46893.145698	32.914471
766.407624	46971.715962	32.919488
767.254761	47047.101567	32.924506
767.679844	47118.926442	32.929524
768.903895	47204.695736	32.934541
769.704553	47291.397318	32.939559
770.150204	47366.567407	32.944576
771.178378	47443.642236	32.949594
771.835888	47534.134926	32.954612
772.847592	47610.317072	32.959629
773.949950	47678.509059	32.964647
774.406287	47767.078816	32.969664
775.200932	47832.149501	32.974682
775.917271	47913.620622	32.979700
776.675233	47986.238475	32.984717
777.917153	48064.783856	32.989735
778.195172	48142.662669	32.994752
778.860762	48216.047104	32.999770
779.668250	48297.429767	33.004788
780.521162	48377.758046	33.009805
781.498967	48457.363196	33.014823
782.090640	48541.744096	33.019840
782.784290	48615.766241	33.024858
783.497678	48710.402083	33.029876
784.721106	48787.502205	33.034893
785.181770	48865.885224	33.039911
785.488647	48954.279634	33.044928
786.637648	49033.292175	33.049946
787.238522	49119.788439	33.054964
787.902728	49203.971633	33.059981
789.173442	49280.952790	33.064999
789.671793	49355.242614	33.070016
790.940454	49420.578182	33.075034
791.320487	49501.652625	33.080052
792.372538	49579.786903	33.085069
793.413810	49633.607442	33.090087
793.555953	49730.135100	33.095104
794.492760	49793.161430	33.100122
795.445567	49872.616002	33.105140
795.878662	49933.694033	33.110157
796.687367	50013.408833	33.115175
797.637115	50088.898393	33.120192
798.517591	50176.945689	33.125210
799.279144	50246.804853	33.130228
800.014983	50321.130340	33.135245
800.667614	50405.709210	33.140263
801.730812	50497.881745	33.145280
802.740162	50550.899164	33.150298
803.349893	50649.979687	33.155316
804.431653	50717.760675	33.160333
804.510923	50798.677471	33.165351
805.670056	50879.861397	33.170368
806.765006	50957.262794	33.175386
807.332712	51063.364200	33.180404
808.171481	51128.452599	33.185421
809.397172	51206.194018	33.190439
809.827628	51293.529528	33.195456
810.504222	51365.296880	33.200474
811.262894	51461.817830	33.205492
812.017711	51550.633513	33.210509
813.109443	51626.835975	33.215527
813.467268	51705.935831	33.220544
814.247136	51798.715599	33.225562
815.501241	51909.904099	33.230580
816.023507	51960.453316	33.235597
817.207806	52075.150629	33.240615
817.740457	52150.645869	33.245632
818.510694	52240.806923	33.250650
819.764770	52328.691754	33.255668
820.708375	52400.209309	33.260685
821.228834	52497.897258	33.265703
822.389845	52587.568652	33.270720
823.357690	52653.200656	33.275738
824.255090	52741.772314	33.280756
825.038179	52828.547902	33.285773
825.716438	52901.621408	33.290791
826.333791	52980.710817	33.295808
827.444714	53066.236086	33.300826
828.587394	53154.193182	33.305844
829.033558	53222.769677	33.310861
829.595904	53294.026391	33.315879
830.406364	53382.520354	33.320896
831.447285	53449.683809	33.325914
832.465360	53542.848117	33.330932
833.013305	53635.948856	33.335949
833.937496	53706.224861	33.340967
834.388644	53782.071305	33.345984
835.214869	53852.890551	33.351002
836.162228	53936.157748	33.356020
836.849928	54008.580902	33.361037
838.021619	54084.762123	33.366055
838.562636	54163.748926	33.371072
839.443165	54238.613642	33.376090
840.171962	54328.914825	33.381108
840.827093	54408.812475	33.386125
842.107927	54474.991523	33.391143
842.698951	54575.614822	33.396160
843.384554	54658.668182	33.401178
844.592582	54732.273948	33.406196
845.316400	54817.225220	33.411213
846.076485	54897.155662	33.416231
846.440277	54990.179033	33.421248
847.704970	55081.519188	33.426266
848.268586	55171.942386	33.431284
848.498947	55274.849060	33.436301
849.882993	55361.042437	33.441319
850.679146	55454.782170	33.446336
851.289987	55541.471913	33.451354
852.482420	55648.072168	33.456372
853.277088	55761.346074	33.461389
854.479926	55823.243287	33.466407
855.137889	55955.059454	33.471424
856.492677	56018.511421	33.476442
857.361540	56110.017581	33.481460
857.925877	56204.350454	33.486477
859.062094	56286.509343	33.491495
859.618705	56382.081749	33.496512
860.495012	56485.151285	33.501530
861.305596	56571.927768	33.506548
862.338931	56662.697116	33.511565
862.990713	56753.404522	33.516583
863.665847	56859.895296	33.521600
864.995983	56950.978704	33.526618
865.895160	57041.648166	33.531636
866.265544	57142.661646	33.536653
867.265604	57238.912939	33.541671
868.143285	57335.054783	33.546688
869.053870	57435.598781	33.551706
870.221745	57529.744564	33.556724
870.803399	57628.141660	33.561741
871.975969	57709.650836	33.566759
872.583017	57818.285706	33.571776
873.742081	57901.174272	33.576794
874.784687	58002.716872	33.581812
875.299021	58110.064418	33.586829
876.414343	58195.155320	33.591847
877.384604	58288.600866	33.596864
877.771657	58383.528753	33.601882
878.597753	58482.121962	33.606900
879.555199	58579.599319	33.611917
880.593810	58672.477142	33.616935
881.039554	58772.202648	33.621952
881.990512	58853.647964	33.626970
883.438350	58933.155067	33.631988
883.891129	59024.704051	33.637005
884.822178	59116.003741	33.642023
885.749661	59189.905689	33.647040
886.313135	59300.554640	33.652058
887.422399	59390.046709	33.657076
887.948791	59476.746330	33.662093
889.054992	59567.818316	33.667111
889.779554	59673.635502	33.672128
890.840259	59762.148896	33.677146
891.705966	59864.983265	33.682164
892.439922	59968.306437	33.687181
893.078000	60068.317703	33.692199
894.114857	60158.481702	33.697216
894.704117	60273.284129	33.702234
895.834384	60383.479926	33.707252
896.848297	60486.246781	33.712269
897.966770	60583.513281	33.717287
898.858333	60687.330003	33.722304
899.821120	60776.962557	33.727322
901.404150	60875.157541	33.732340
902.284419	60989.959114	33.737357
902.942207	61069.436890	33.742375
903.885136	61155.910695	33.747392
904.629370	61243.777374	33.752410
905.572784	61356.048347	33.757428
906.637317	61455.004578	33.762445
907.394746	61550.653780	33.767463
908.656080	61638.181113	33.772480
909.466618	61732.926062	33.777498
910.602711	61827.720729	33.782516
911.316910	61935.260599	33.787533
911.979452	62016.244630	33.792551
912.929279	62123.823868	33.797568
913.682712	62223.120989	33.802586
914.973862	62316.137820	33.807604
915.866086	62416.680086	33.812621
917.054116	62500.089753	33.817639
917.607647	62597.674475	33.822656
918.443637	62706.983457	33.827674
919.368762	62800.881922	33.832692
920.136900	62905.712597	33.837709
921.106637	63007.275096	33.842727
922.264817	63106.389318	33.847744
922.852645	63205.699016	33.852762
923.963882	63311.828879	33.857780
924.451865	63422.441540	33.862797
925.739732	63509.506001	33.867815
926.548654	63620.444534	33.872832
927.600404	63730.416671	33.877850
928.843231	63822.867573	33.882868
929.387375	63939.079539	33.887885
930.516907	64024.981038	33.892903
931.762270	64113.633993	33.897920
932.215947	64207.203918	33.902938
933.037550	64294.061956	33.907956
933.859500	64387.188901	33.912973
935.003374	64471.160620	33.917991
935.885454	64560.779805	33.923008
936.443076	64676.359375	33.928026
937.752745	64758.335382	33.933044
938.850568	64847.991071	33.938061
939.367969	64949.904375	33.943079
940.560501	65047.194757	33.948096
941.196162	65144.485809	33.953114
942.370328	65235.091233	33.958132
943.032101	65346.495907	33.963149
943.884308	65443.226620	33.968167
945.028810	65538.108011	33.973184
945.619862	65659.233936	33.978202
946.766694	65759.244934	33.983220
947.847897	65866.805547	33.988237
948.674245	65971.928102	33.993255
949.517141	66080.361602	33.998272
950.508311	66196.689895	34.003290
951.315746	66302.739486	34.008308
952.304046	66419.739143	34.013325
953.465396	66523.140678	34.018343
954.374343	66648.132268	34.023360
955.331934	66754.950051	34.028378
956.345514	66852.202278	34.033396
957.339303	66978.837506	34.038413
958.185908	67090.380815	34.043431
959.291096	67202.471099	34.048448
960.249855	67312.513388	34.053466
961.445754	67415.503623	34.058484
962.023581	67534.590461	34.063501
963.217378	67644.493020	34.068519
964.019223	67762.847595	34.073536
964.641926	67878.117073	34.078554
965.977793	67986.868218	34.083572
966.943068	68112.413080	34.088589
967.877934	68224.204738	34.093607
968.843716	68334.198029	34.098624
969.818138	68452.706246	34.103642
970.933515	68576.050773	34.108660
972.061980	68686.367632	34.113677
972.661947	68795.436229	34.118695
973.837904	68902.916576	34.123712
975.045509	69022.307197	34.128730
976.048846	69134.099519	34.133748
977.101109	69243.957854	34.138765
977.701627	69362.720629	34.143783
978.963384	69481.562142	34.148800
979.932768	69584.385139	34.153818
981.039729	69686.074881	34.158836
982.141677	69805.247039	34.163853
982.714869	69922.880381	34.168871
983.784280	70020.420763	34.173888
984.310214	70125.142990	34.178906
985.326368	70236.762693	34.183924
986.430429	70334.899326	34.188941
987.415159	70442.330129	34.193959
988.151729	70548.777492	34.198976
989.054151	70673.578065	34.203994
990.163306	70759.730799	34.209012
990.816595	70882.556886	34.214029
991.848663	71005.936339	34.219047
993.066307	71115.330294	34.224064
994.169427	71239.066359	34.229082
995.519277	71349.956949	34.234100
996.599734	71468.574001	34.239117
997.077630	71573.975010	34.244135
998.040816	71691.967598	34.249152
998.953845	71822.409709	34.254170
1000.054388	71923.600288	34.259188
1000.958058	72049.117044	34.264205
1001.530780	72174.396593	34.269223
1002.876697	72302.479408	34.274240
1003.855044	72437.066446	34.279258
1004.668805	72545.199369	34.284276
1006.019750	72681.144158	34.289293
1006.795401	72798.907803	34.294311
1007.953755	72927.397299	34.299328
1009.057574	73061.393615	34.304346
1010.163718	73177.072294	34.309364
1011.326192	73300.603304	34.314381
1012.295512	73418.118655	34.319399
1013.309481	73539.583230	34.324416
1014.228738	73686.073994	34.329434
1015.234601	73807.503578	34.334452
1016.667294	73924.069867	34.339469
1017.593433	74037.955988	34.344487
1018.526073	74180.884308	34.349504
1019.289125	74277.748802	34.354522
1020.777070	74402.631402	34.359540
1021.951127	74543.331160	34.364557
1022.763816	74663.153681	34.369575
1023.965857	74768.273185	34.374592
1024.729448	74884.123685	34.379610
1025.675236	75025.735210	34.384628
1027.252007	75138.974321	34.389645
1028.463962	75245.188008	34.394663
1029.574350	75363.349584	34.399680
1030.409283	75470.534441	34.404698
1031.666802	75593.552631	34.409716
1032.718035	75684.115410	34.414733
1033.461540	75819.994937	34.419751
1034.661908	75932.748593	34.424768
1035.125047	76055.820130	34.429786
1036.208726	76175.659125	34.434804
1037.262971	76291.964443	34.439821
1038.144750	76412.816526	34.444839
1039.380687	76537.796735	34.449856
1039.999479	76637.400446	34.454874
1040.861518	76770.910205	34.459892
1042.705961	76862.211617	34.464909
1043.446012	76981.819335	34.469927
1044.613844	77078.588695	34.474944
1045.715189	77197.716779	34.479962
1046.551823	77295.709066	34.484980
1047.634713	77421.837733	34.489997
1048.037359	77551.462989	34.495015
1049.326885	77666.392588	34.500032
1050.095953	77777.284829	34.505050
1051.104897	77898.214026	34.510068
1052.447153	78033.305298	34.515085
1053.048789	78166.416910	34.520103
1054.035376	78288.540206	34.525120
1054.915766	78450.582019	34.530138
1055.885943	78565.491642	34.535156
1057.458139	78689.344490	34.540173
1058.389772	78833.051706	34.545191
1059.140555	78976.061827	34.550208
1060.349415	79105.973242	34.555226
1061.355816	79246.940954	34.560244
1062.451984	79399.462293	34.565261
1063.477568	79530.530640	34.570279
1064.787362	79663.160106	34.575296
1065.590923	79818.259421	34.580314
1066.527480	79936.702802	34.585332
1067.954524	80101.647862	34.590349
1069.091944	80231.274355	34.595367
1070.133679	80376.239057	34.600384
1071.255900	80520.901208	34.605402
1072.267174	80662.655340	34.610420
1073.418523	80796.556249	34.615437
1074.232104	80959.412296	34.620455
1075.779079	81087.265980	34.625472
1076.808282	81226.612732	34.630490
1078.003912	81366.964330	34.635508
1079.164848	81522.854024	34.640525
1080.082235	81631.606857	34.645543
1081.133754	81795.240769	34.650560
1082.446021	81910.215794	34.655578
1083.472789	82068.160122	34.660596
1084.772430	82202.305711	34.665613
1085.673928	82330.876594	34.670631
1086.801752	82470.980927	34.675648
1087.579352	82621.193425	34.680666
1088.629950	82755.451722	34.685684
1090.407238	82863.758147	34.690701
1090.957190	83056.966576	34.695719
1092.151959	83169.817813	34.700736
1093.152767	83327.706262	34.705754
1094.022542	83453.804585	34.710772
1095.638298	83601.336748	34.715789
1096.380305	83741.966143	34.720807
1098.117371	83860.747131	34.725824
1098.993450	83990.318503	34.730842
1100.224173	84106.247942	34.735860
1101.106500	84238.728047	34.740877
1102.115867	84357.210310	34.745895
1103.125616	84489.330325	34.750912
1104.456640	84624.422144	34.755930
1105.078580	84734.610042	34.760948
1106.671825	84878.184314	34.765965
1107.046278	84995.904971	34.770983
1108.261197	85137.758251	34.776000
1109.492277	85255.761406	34.781018
1110.016769	85424.704559	34.786036
1111.461213	85535.056662	34.791053
1112.617491	85713.948243	34.796071
1113.221869	85848.961121	34.801088
1114.979722	85971.816186	34.806106
1115.811847	86143.472842	34.811124
1117.195895	86285.528203	34.816141
1118.271844	86412.660996	34.821159
1119.251402	86571.588734	34.826176
1120.571103	86718.551142	34.831194
1121.681508	86870.732694	34.836212
1123.030737	87002.643663	34.841229
1124.080073	87165.238404	34.846247
1125.304635	87297.689513	34.851264
1126.426626	87434.236187	34.856282
1127.376117	87596.824793	34.861300
1128.991906	87725.839749	34.866317
1129.860122	87875.708397	34.871335
1130.769810	88017.110887	34.876352
1132.036436	88176.118713	34.881370
1133.199277	88326.847898	34.886388
1134.464955	88462.006082	34.891405
1135.722337	88624.578799	34.896423
1136.809963	88743.540965	34.901440
1138.014231	88922.382193	34.906458
1139.027513	89050.855910	34.911476
1140.570257	89188.851845	34.916493
1141.405566	89361.532893	34.921511
1143.077437	89488.639742	34.926528
1144.108068	89635.990593	34.931546
1144.975398	89786.757992	34.936564
1146.015145	89932.060481	34.941581
1147.216275	90076.263213	34.946599
1148.686976	90209.900957	34.951616
1149.925542	90353.644253	34.956634
1150.978524	90509.231334	34.961652
1151.999921	90637.934508	34.966669
1153.246091	90776.386125	34.971687
1154.179381	90936.675147	34.976704
1155.643474	91069.332649	34.981722
1156.566964	91204.341003	34.986740
1157.608533	91376.075580	34.991757
1158.957930	91502.170352	34.996775
1160.232579	91627.240540	35.001792
1161.609169	91781.994686	35.006810
1162.285428	91885.114582	35.011828
1163.585235	92037.612265	35.016845
1164.946257	92125.186325	35.021863
1165.719387	92289.786093	35.026880
1167.523972	92399.211672	35.031898
1168.561689	92524.413195	35.036916
1169.721210	92666.508233	35.041933
1170.695086	92771.684758	35.046951
1171.894174	92929.865254	35.051968
1172.944181	93035.884776	35.056986
1174.230561	93165.648519	35.062004
1176.118763	93314.791564	35.067021
1176.966269	93415.013586	35.072039
1178.482791	93551.453710	35.077056
1179.467251	93708.674571	35.082074
1180.576391	93808.002902	35.087092
1181.688793	93959.873227	35.092109
1182.487122	94085.849043	35.097127
1183.810060	94193.127356	35.102144
1184.732557	94368.907973	35.107162
1185.755960	94480.182198	35.112180
1186.891237	94657.411356	35.117197
1188.128340	94777.400899	35.122215
1188.956092	94928.077015	35.127232
1190.217894	95066.913643	35.132250
1191.213822	95247.079305	35.137268
1192.431528	95386.019809	35.142285
1193.347678	95549.893598	35.147303
1194.604815	95703.903461	35.152320
1196.156330	95852.554091	35.157338
1197.176502	96033.765946	35.162356
1198.586507	96175.622190	35.167373
1199.522337	96333.856080	35.172391
1200.537089	96506.020509	35.177408
1201.636274	96666.463757	35.182426
1202.698428	96832.967877	35.187444
1204.150202	97004.345481	35.192461
1205.173771	97170.630494	35.197479
1206.418907	97330.036777	35.202496
1207.672898	97495.205796	35.207514
1208.702532	97665.947016	35.212532
1210.357603	97824.241474	35.217549
1211.213027	98008.025820	35.222567
1212.641776	98180.453482	35.227584
1213.776837	98331.217373	35.232602
1215.157034	98529.042739	35.237620
1216.502976	98679.895612	35.242637
1217.912497	98840.140423	35.247655
1219.161044	99021.162740	35.252672
1220.697721	99166.199793	35.257690
1221.363269	99343.559410	35.262708
1222.679721	99515.711350	35.267725
1224.135407	99651.862837	35.272743
1225.125991	99799.160760	35.277760
1226.168290	99966.405883	35.282778
1227.698400	100109.166007	35.287796
1228.883568	100252.848631	35.292813
1230.072857	100422.452581	35.297831
1231.011813	100552.231848	35.302848
1232.148012	100713.906146	35.307866
1233.356892	100886.022183	35.312884
1234.800621	101040.487744	35.317901
1236.291361	101192.371750	35.322919
1236.902811	101370.856494	35.327936
1238.179692	101510.495675	35.332954
1239.165971	101674.389716	35.337972
1240.707667	101851.161125	35.342989
1241.628675	102029.285358	35.348007
1243.054061	102183.875350	35.353024
1244.817958	102344.929748	35.358042
1245.856499	102521.229433	35.363060
1247.016663	102690.709089	35.368077
1248.186612	102853.417982	35.373095
1249.296484	103031.741314	35.378112
1250.496895	103218.815350	35.383130
1251.974542	103390.837603	35.388148
1253.115067	103553.068811	35.393165
1254.902482	103726.942598	35.398183
1255.569732	103913.790549	35.403200
1257.345041	104082.568691	35.408218
1257.842799	104271.496646	35.413236
1259.336167	104443.334273	35.418253
1260.930265	104610.980671	35.423271
1262.074637	104794.722326	35.428288
1263.257891	104976.459555	35.433306
1264.882887	105155.495456	35.438324
1266.279272	105320.438238	35.443341
1267.349181	105518.764810	35.448359
1268.528460	105688.054184	35.453376
1269.989140	105853.351163	35.458394
1271.230919	106060.318399	35.463412
1272.527116	106215.157933	35.468429
1274.167998	106387.631712	35.473447
1274.946912	106571.824921	35.478464
1276.564462	106738.267551	35.483482
1277.670095	106924.664507	35.488500
1279.300630	107111.068077	35.493517
1280.512255	107271.731276	35.498535
1281.439892	107461.331375	35.503552
1283.277604	107639.421801	35.508570
1284.682515	107801.671664	35.513588
1285.853428	107966.586300	35.518605
1287.332178	108122.763531	35.523623
1288.683917	108319.264784	35.528640
1290.192823	108468.148493	35.533658
1291.133006	108635.768893	35.538676
1292.590571	108803.732262	35.543693
1293.709815	108975.307550	35.548711
1294.862879	109135.859574	35.553728
1296.467743	109289.150853	35.558746
1297.498552	109446.331904	35.563764
1298.518973	109600.091472	35.568781
1299.844385	109746.993164	35.573799
1301.307842	109904.336262	35.578816
1302.503130	110069.065130	35.583834
1303.536745	110233.827138	35.588852
1304.756027	110398.731643	35.593869
1306.119168	110554.139060	35.598887
1307.290724	110733.250584	35.603904
1308.360616	110896.928933	35.608922
1309.622366	111084.162268	35.613940
1310.928793	111253.831261	35.618957
1312.576207	111420.301331	35.623975
1313.292543	111593.940284	35.628992
1314.871717	111796.427757	35.634010
1316.168331	111964.349836	35.639028
1317.510983	112139.247679	35.644045
1318.820855	112329.192053	35.649063
1320.052407	112526.474204	35.654080
1321.727834	112706.368219	35.659098
1322.788201	112876.638199	35.664116
1323.849770	113087.169169	35.669133
1325.741273	113236.711067	35.674151
1326.845209	113464.754263	35.679168
1328.446938	113627.157081	35.684186
1329.670778	113818.955990	35.689204
1331.012093	114007.249634	35.694221
1332.591257	114192.170733	35.699239
1333.590077	114369.227972	35.704256
1334.949070	114566.689612	35.709274
1336.653479	114754.342423	35.714292
1337.814142	114950.426877	35.719309
1339.499295	115133.907346	35.724327
1340.498345	115305.140559	35.729344
1341.789169	115518.770276	35.734362
1343.605992	115676.081206	35.739380
1344.844866	115883.707962	35.744397
1346.197708	116065.937530	35.749415
1347.627176	116263.268315	35.754432
1348.767892	116431.580717	35.759450
1350.184928	116624.281966	35.764468
1351.492821	116825.827626	35.769485
1353.160200	117006.830039	35.774503
1354.472648	117202.762202	35.779520
1355.822102	117378.537540	35.784538
1357.249957	117560.544306	35.789556
1358.849286	117747.621865	35.794573
1360.457778	117918.370633	35.799591
1361.479119	118103.136714	35.804608
1362.752602	118290.795536	35.809626
1364.378471	118471.808589	35.814644
1365.434649	118661.397784	35.819661
1366.793101	118822.492312	35.824679
1368.213006	118996.323732	35.829696
1369.342254	119180.459895	35.834714
1370.938283	119340.601805	35.839732
1371.829102	119516.565968	35.844749
1373.522142	119676.447601	35.849767
1374.429271	119858.673684	35.854784
1375.825354	120037.176152	35.859802
1377.238507	120209.642768	35.864820
1378.108094	120393.714839	35.869837
1379.631317	120568.414207	35.874855
1381.504099	120764.968259	35.879872
1382.720413	120947.976006	35.884890
1384.263582	121139.582866	35.889908
1385.436067	121318.484247	35.894925
1386.979316	121502.596386	35.899943
1388.149200	121696.001683	35.904960
1389.280715	121889.997079	35.909978
1390.968410	122078.155685	35.914996
1391.736696	122286.510332	35.920013
1393.600613	122472.642692	35.925031
1395.315857	122671.148484	35.930048
1396.461403	122866.276030	35.935066
1397.947741	123053.270394	35.940084
1399.364272	123253.208541	35.945101
1401.192563	123449.549090	35.950119
1402.200033	123644.121689	35.955136
1403.769707	123843.001362	35.960154
1405.278625	124023.159501	35.965172
1406.644058	124221.415834	35.970189
1407.814397	124429.292771	35.975207
1409.375544	124628.204984	35.980224
1410.568150	124825.910625	35.985242
1412.353421	125014.023867	35.990260
1413.505467	125231.751601	35.995277
1415.521508	125436.778700	36.000295
1416.883083	125626.204868	36.005312
1417.937038	125823.610547	36.010330
1419.594118	126024.721845	36.015348
1420.733512	126243.777099	36.020365
1422.434983	126428.455496	36.025383
1423.849018	126617.766275	36.030400
1425.195432	126835.881395	36.035418
1426.696167	127027.613336	36.040436
1428.008153	127208.786788	36.045453
1429.584493	127427.186794	36.050471
1431.007810	127631.665990	36.055488
1432.153270	127842.942673	36.060506
1434.087057	128026.328244	36.065524
1435.494057	128237.655088	36.070541
1437.036156	128443.692274	36.075559
1438.847139	128631.218451	36.080576
1439.885980	128822.111606	36.085594
1441.705754	129029.819244	36.090612
1442.799087	129226.736558	36.095629
1444.862248	129399.507463	36.100647
1446.363281	129584.973777	36.105664
1447.512431	129758.690261	36.110682
1449.164804	129914.921345	36.115700
1450.432441	130085.023192	36.120717
1451.760340	130268.494615	36.125735
1452.871649	130459.374874	36.130752
1454.359314	130623.756786	36.135770
1455.859253	130803.011013	36.140788
1456.606853	130987.048116	36.145805
1458.024126	131189.413538	36.150823
1459.209894	131398.861268	36.155840
1460.591360	131573.160266	36.160858
1462.373587	131780.020229	36.165876
1463.468615	131992.628802	36.170893
1464.660684	132206.857932	36.175911
1466.412830	132406.125551	36.180928
1467.667464	132612.315272	36.185946
1469.092934	132829.096661	36.190964
1470.489991	133049.317770	36.195981
1472.321628	133260.817922	36.200999
1474.124614	133463.125706	36.206016
1475.394256	133683.245272	36.211034
1477.064556	133879.786817	36.216052
1478.355520	134117.201290	36.221069
1480.381664	134314.766278	36.226087
1481.827866	134515.237637	36.231104
1483.474276	134752.448859	36.236122
1485.277515	134921.797861	36.241140
1486.587213	135160.079604	36.246157
1488.144960	135337.845493	36.251175
1489.635244	135571.401031	36.256192
1491.101470	135768.342721	36.261210
1492.814838	135970.581066	36.266228
1494.578229	136180.694424	36.271245
1495.826328	136378.042382	36.276263
1497.253542	136600.756862	36.281280
1498.928533	136780.743165	36.286298
1500.294131	137007.664833	36.291316
1501.629081	137202.989789	36.296333
1503.084834	137404.873537	36.301351
1504.807391	137639.295811	36.306368
1505.943451	137822.567476	36.311386
1507.521289	138065.683803	36.316404
1508.847906	138249.599480	36.321421
1510.146948	138493.283188	36.326439
1511.737144	138712.807080	36.331456
1513.056941	138927.572686	36.336474
1515.104673	139146.596249	36.341492
1516.365528	139375.136886	36.346509
1517.665249	139586.945051	36.351527
1519.251662	139822.268027	36.356544
1520.437985	140051.041133	36.361562
1522.139361	140266.516171	36.366580
1523.879662	140489.349678	36.371597
1525.103241	140716.892663	36.376615
1526.618927	140923.834818	36.381632
1528.312779	141137.213540	36.386650
1529.984761	141337.911068	36.391668
1531.064938	141554.799408	36.396685
1532.385885	141770.637162	36.401703
1534.317636	141974.415385	36.406720
1535.362115	142198.360628	36.411738
1537.023545	142402.184669	36.416756
1538.577607	142621.857009	36.421773
1539.791324	142849.709120	36.426791
1541.466822	143064.536516	36.431808
1543.030724	143301.613908	36.436826
1544.587964	143511.634316	36.441844
1545.736687	143779.187282	36.446861
1547.566804	143978.635017	36.451879
1549.750499	144195.823146	36.456896
1551.085902	144444.619056	36.461914
1552.728049	144659.399541	36.466932
1554.450804	144877.274083	36.471949
1555.817811	145117.311982	36.476967
1557.156659	145343.641681	36.481984
1558.838544	145577.054708	36.487002
1560.534565	145807.678663	36.492020
1562.092297	146045.196382	36.497037
1563.501465	146276.655244	36.502055
1565.285190	146504.038146	36.507072
1566.825524	146746.938421	36.512090
1568.448270	146978.431917	36.517108
1569.940895	147212.482966	36.522125
1571.573439	147452.750127	36.527143
1573.309545	147679.946275	36.532160
1574.644229	147933.967276	36.537178
1576.191752	148158.724952	36.542196
1577.708153	148411.453280	36.547213
1579.229141	148657.261518	36.552231
1580.863927	148905.487482	36.557248
1582.160879	149144.286869	36.562266
1583.909170	149400.370868	36.567284
1585.565205	149648.117495	36.572301
1587.260539	149899.586823	36.577319
1588.865385	150154.292466	36.582336
1590.289016	150405.251101	36.587354
1592.211792	150636.444591	36.592372
1593.856817	150882.452979	36.597389
1595.154098	151135.237520	36.602407
1597.380587	151376.935703	36.607424
1598.586824	151641.871064	36.612442
1599.971512	151876.378958	36.617460
1601.549511	152121.811490	36.622477
1603.116106	152378.974771	36.627495
1604.981653	152630.235325	36.632512
1606.105512	152897.970402	36.637530
1608.075025	153133.763623	36.642548
1609.734049	153402.305266	36.647565
1611.241661	153642.359324	36.652583
1612.951065	153886.719123	36.657600
1614.102955	154120.785475	36.662618
1615.880195	154354.817544	36.667636
1617.574753	154579.608868	36.672653
1618.803918	154820.057955	36.677671
1620.563773	155069.375837	36.682688
1621.915090	155310.202083	36.687706
1623.933175	155542.251615	36.692724
1625.406326	155784.570720	36.697741
1626.580053	156052.716210	36.702759
1628.776982	156288.622344	36.707776
1630.195623	156533.630823	36.712794
1631.417155	156787.712936	36.717812
1633.305577	157046.547360	36.722829
1634.914231	157317.537396	36.727847
1636.891854	157561.614933	36.732864
1637.700614	157826.015670	36.737882
1639.471598	158070.066237	36.742900
1641.087019	158353.882944	36.747917
1642.993953	158611.572323	36.752935
1644.689424	158874.648324	36.757952
1646.590208	159151.667608	36.762970
1648.041910	159408.940663	36.767988
1649.996295	159676.774874	36.773005
1651.448827	159944.018754	36.778023
1653.302436	160227.559305	36.783040
1655.209368	160484.932830	36.788058
1656.696103	160743.871332	36.793076
1658.671420	161007.502262	36.798093
1660.231047	161276.400483	36.803111
1661.751703	161533.044070	36.808128
1663.435876	161818.615274	36.813146
1665.563502	162069.992322	36.818164
1667.113733	162330.936005	36.823181
1668.571844	162618.591249	36.828199
1670.665583	162875.546621	36.833216
1671.847196	163138.051167	36.838234
1673.867742	163399.295707	36.843252
1675.574254	163683.546605	36.848269
1677.073963	163959.208676	36.853287
1678.803321	164210.778067	36.858304
1680.676099	164484.545951	36.863322
1682.416245	164758.933029	36.868340
1683.981789	165015.632342	36.873357
1685.704204	165285.320949	36.878375
1687.256496	165570.232491	36.883392
1689.008696	165851.943779	36.888410
1690.656956	166093.887326	36.893428
1692.324988	166387.804367	36.898445
1694.171141	166656.329186	36.903463
1695.712038	166914.009530	36.908480
1697.723134	167193.914248	36.913498
1699.017700	167477.435458	36.918516
1700.993990	167740.049624	36.923533
1702.068018	167989.833587	36.928551
1703.915281	168273.666235	36.933568
1706.073471	168523.268901	36.938586
1707.446209	168771.640759	36.943604
1708.855792	169019.437616	36.948621
1710.710010	169304.684799	36.953639
1712.223126	169542.118460	36.958656
1713.943080	169819.894511	36.963674
1715.704893	170077.104714	36.968692
1717.186674	170345.979978	36.973709
1718.726537	170599.487029	36.978727
1720.729967	170897.812719	36.983744
1722.278804	171157.651594	36.988762
1723.780300	171437.122982	36.993780
1725.602250	171713.907057	36.998797
1727.328756	171982.678709	37.003815
1728.988824	172259.682627	37.008832
1731.115922	172563.291076	37.013850
1732.547765	172821.865715	37.018868
1734.581672	173117.818709	37.023885
1736.302711	173403.764105	37.028903
1738.013605	173667.881527	37.033920
1739.864766	173975.223404	37.038938
1741.577137	174241.526308	37.043956
1743.114090	174529.107399	37.048973
1744.902432	174823.133084	37.053991
1746.916530	175107.839001	37.059008
1748.696027	175389.907433	37.064026
1750.099572	175694.174718	37.069044
1752.246135	175970.733904	37.074061
1754.233652	176266.730190	37.079079
1756.160423	176549.912371	37.084096
1757.871185	176840.742666	37.089114
1759.788311	177126.835559	37.094132
1761.770281	177395.425315	37.099149
1763.474285	177691.654502	37.104167
1765.286236	177973.354991	37.109184
1767.439434	178234.069891	37.114202
1768.724798	178540.203911	37.119220
1770.872500	178822.998672	37.124237
1772.442366	179091.106580	37.129255
1774.374938	179398.856888	37.134272
1776.099454	179644.423974	37.139290
1777.682413	179974.132242	37.144308
1779.867839	180229.195842	37.149325
1781.188250	180551.363171	37.154343
1783.215098	180824.522598	37.159360
1784.998590	181103.863260	37.164378
1786.746787	181393.260085	37.169396
1788.470906	181681.305075	37.174413
1790.068397	181983.049728	37.179431
1792.102297	182250.723197	37.184448
1793.899696	182549.559868	37.189466
1795.403754	182850.170755	37.194484
1797.386229	183113.937029	37.199501
1799.101016	183409.531800	37.204519
1801.019623	183687.573418	37.209536
1802.783996	183924.263920	37.214554
1804.659242	184208.482333	37.219572
1806.652054	184483.522662	37.224589
1808.354217	184744.424777	37.229607
1809.865568	185001.361719	37.234624
1811.723645	185278.851910	37.239642
1813.518232	185543.284223	37.244660
1815.300602	185802.048012	37.249677
1816.876112	186094.193210	37.254695
1818.353784	186367.550376	37.259712
1820.459888	186638.347707	37.264730
1822.250046	186933.293943	37.269748
1824.042685	187222.658322	37.274765
1825.821309	187504.730260	37.279783
1827.764184	187800.076584	37.284800
1829.242737	188092.186486	37.289818
1830.843458	188389.900413	37.294836
1832.959073	188670.847341	37.299853
1834.476081	188969.390412	37.304871
1836.268475	189281.774567	37.309888
1838.177576	189593.152446	37.314906
1839.966984	189887.787631	37.319924
1841.737833	190194.432597	37.324941
1843.363564	190516.013749	37.329959
1845.335826	190829.394802	37.334976
1847.729381	191140.591722	37.339994
1849.199248	191451.226597	37.345012
1851.372699	191750.025603	37.350029
1853.404177	192067.072933	37.355047
1855.040553	192385.200314	37.360064
1857.530758	192675.743766	37.365082
1859.183060	192977.285437	37.370100
1861.391409	193303.006067	37.375117
1863.272226	193601.329833	37.380135
1865.460496	193887.384936	37.385152
1867.092258	194220.221379	37.390170
1869.057179	194508.676094	37.395188
1871.520057	194809.998744	37.400205
1873.269124	195101.295947	37.405223
1874.884180	195416.742883	37.410240
1877.008977	195709.202360	37.415258
1878.573253	196010.954020	37.420276
1880.612502	196310.106406	37.425293
1882.246331	196624.605966	37.430311
1884.360077	196909.776221	37.435328
1886.443601	197209.726422	37.440346
1887.828315	197537.673919	37.445364
1889.945241	197833.713248	37.450381
1891.796345	198139.226823	37.455399
1893.446881	198444.812090	37.460416
1895.153595	198757.904146	37.465434
1897.071039	199088.556455	37.470452
1899.484545	199390.370666	37.475469
1900.907110	199683.585912	37.480487
1902.835036	199995.393586	37.485504
1904.850873	200249.868399	37.490522
1905.977885	200573.991627	37.495540
1908.116663	200844.252371	37.500557
1910.048366	201133.117194	37.505575
1911.650192	201443.296807	37.510592
1913.522049	201730.321100	37.515610
1915.304761	202039.345692	37.520628
1917.457223	202345.063858	37.525645
1919.476389	202654.536715	37.530663
1921.318403	202956.512205	37.535680
1923.170516	203262.498872	37.540698
1925.043830	203572.456931	37.545716
1926.794088	203888.656108	37.550733
1929.114395	204202.062833	37.555751
1930.840499	204512.684095	37.560768
1932.755706	204824.622588	37.565786
1934.630392	205153.249018	37.570804
1936.929255	205459.595534	37.575821
1938.425143	205794.721580	37.580839
1940.358403	206118.660097	37.585856
1942.782796	206433.281100	37.590874
1944.327667	206757.094371	37.595892
1946.327456	207096.006971	37.600909
1948.825550	207419.126759	37.605927
1950.442493	207727.116669	37.610944
1952.609097	208089.467860	37.615962
1954.832737	208385.355841	37.620980
1956.768179	208726.293653	37.625997
1958.907467	209041.303737	37.631015
1960.618224	209370.258886	37.636032
1962.684165	209703.869248	37.641050
1964.480554	210039.326875	37.646068
1966.389732	210366.211977	37.651085
1968.816363	210691.302857	37.656103
1970.648426	211021.352018	37.661120
1972.605593	211357.134000	37.666138
1974.626258	211688.159656	37.671156
1976.776999	212013.047238	37.676173
1978.771774	212349.209369	37.681191
1980.518540	212686.859900	37.686208
1982.697581	213012.560574	37.691226
1984.788083	213349.347515	37.696244
1986.266269	213681.167773	37.701261
1988.639832	214016.389762	37.706279
1990.427060	214359.501720	37.711296
1992.197924	214692.004298	37.716314
1994.164155	215028.908423	37.721332
1996.308134	215378.888324	37.726349
1998.420165	215694.621115	37.731367
2000.136260	216051.210867	37.736384
2002.517970	216386.951293	37.741402
2004.229379	216720.260464	37.746420
2006.084935	217081.492984	37.751437
2008.210475	217401.903760	37.756455
2010.216985	217733.545854	37.761472
2012.436438	218038.036010	37.766490
2014.247000	218376.834969	37.771508
2016.174442	218689.106468	37.776525
2018.099972	218998.103900	37.781543
2019.626146	219335.009947	37.786560
2021.958751	219668.615432	37.791578
2023.981663	219996.913518	37.796596
2025.404857	220316.420399	37.801613
2027.899390	220659.895622	37.806631
2029.798910	221001.130593	37.811648
2031.796446	221332.003468	37.816666
2033.409025	221677.616765	37.821684
2035.581577	222030.189757	37.826701
2037.870285	222371.686661	37.831719
2039.379661	222726.983735	37.836736
2041.931534	223079.831545	37.841754
2043.897777	223438.525811	37.846772
2045.448657	223793.275222	37.851789
2047.768760	224207.569978	37.856807
2049.694888	224576.802096	37.861824
2051.885378	224936.877069	37.866842
2053.844009	225302.386979	37.871860
2055.743316	225673.837823	37.876877
2058.471957	226027.559603	37.881895
2060.292903	226409.590838	37.886912
2062.534817	226770.453068	37.891930
2064.749103	227138.394042	37.896948
2066.890877	227517.954171	37.901965
2069.325251	227873.013017	37.906983
2071.277346	228233.940220	37.912000
2073.505626	228598.355244	37.917018
2075.455066	228961.546215	37.922036
2077.830967	229324.569470	37.927053
2080.212482	229690.361592	37.932071
2082.227814	230050.346641	37.937088
2084.419611	230406.876565	37.942106
2086.471673	230760.484015	37.947124
2088.806613	231128.651356	37.952141
2090.736878	231478.344365	37.957159
2092.980552	231845.513183	37.962176
2095.141743	232202.664540	37.967194
2097.523926	232558.639323	37.972212
2099.263100	232913.650747	37.977229
2101.838907	233272.645233	37.982247
2103.758797	233637.764400	37.987264
2105.873716	233990.637602	37.992282
2108.028446	234333.041778	37.997300
2109.973392	234707.659858	38.002317
2111.991164	235061.619047	38.007335
2114.001735	235420.939679	38.012352
2115.921104	235795.870683	38.017370
2118.170673	236152.971747	38.022388
2119.887432	236521.257748	38.027405
2122.368142	236874.997442	38.032423
2123.649169	237228.776222	38.037440
2125.801242	237561.387793	38.042458
2127.800532	237913.886596	38.047476
2129.744417	238268.833651	38.052493
2132.043918	238621.033164	38.057511
2134.048775	238980.824099	38.062528
2135.847071	239334.883338	38.067546
2137.831584	239706.922298	38.072564
2139.917987	240074.679226	38.077581
2142.263543	240427.131141	38.082599
2144.029359	240811.298564	38.087616
2146.501740	241180.293196	38.092634
2148.871438	241556.137807	38.097652
2150.345115	241932.303514	38.102669
2152.572716	242319.958588	38.107687
2155.037186	242703.081537	38.112704
2157.456421	243090.683271	38.117722
2159.664752	243474.738243	38.122740
2162.126029	243860.430689	38.127757
2163.976848	244234.587785	38.132775
2166.055739	244633.119555	38.137792
2168.362187	245022.573896	38.142810
2170.755391	245404.573277	38.147828
2172.586933	245809.396358	38.152845
2174.888670	246186.256146	38.157863
2177.235541	246591.330036	38.162880
2179.262166	246970.394659	38.167898
2181.804296	247374.957240	38.172916
2183.791556	247762.717327	38.177933
2186.075323	248159.042379	38.182951
2187.996603	248564.671981	38.187968
2190.201441	248972.340617	38.192986
2192.746538	249372.767846	38.198004
2194.850976	249769.506610	38.203021
2197.114048	250178.210668	38.208039
2199.269867	250579.439371	38.213056
2201.300169	250982.797303	38.218074
2203.687895	251392.805560	38.223092
2205.869994	251799.875448	38.228109
2208.604259	252207.595409	38.233127
2211.114104	252608.468057	38.238144
2212.933348	253012.981983	38.243162
2215.513821	253407.901234	38.248180
2218.146530	253804.743609	38.253197
2220.317997	254199.678627	38.258215
2222.606473	254594.316502	38.263232
2224.710966	254986.190140	38.268250
2227.148626	255367.368257	38.273268
2229.160843	255775.820275	38.278285
2231.451994	256161.062079	38.283303
2234.018173	256547.099269	38.288320
2236.233936	256940.788019	38.293338
2238.692900	257335.531230	38.298356
2240.877352	257718.227144	38.303373
2242.839105	258097.580501	38.308391
2245.211476	258461.729508	38.313408
2247.142161	258819.725504	38.318426
2249.891719	259171.444785	38.323444
2251.462142	259537.653188	38.328461
2254.051831	259890.592771	38.333479
2256.258780	260245.244703	38.338496
2258.397301	260615.149582	38.343514
2260.674398	260978.301283	38.348532
2262.444919	261341.305162	38.353549
2264.731770	261720.333018	38.358567
2266.871777	262087.597749	38.363584
2268.983889	262479.736755	38.368602
2271.398922	262851.709157	38.373620
2273.392337	263243.080469	38.378637
2275.573981	263626.649114	38.383655
2277.925682	264013.137988	38.388672
2280.092870	264406.896410	38.393690
2282.285046	264803.369434	38.398708
2284.894418	265202.291649	38.403725
2286.912654	265600.037849	38.408743
2289.202988	266007.546913	38.413760
2291.577544	266416.541816	38.418778
2294.081227	266814.466265	38.423796
2295.991854	267232.756830	38.428813
2298.624696	267641.457877	38.433831
2301.053653	268041.249654	38.438848
2302.909853	268464.884575	38.443866
2305.346858	268871.941032	38.448884
2307.881750	269297.831494	38.453901
2310.414657	269709.979383	38.458919
2312.444374	270116.567769	38.463936
2314.929015	270544.016614	38.468954
2317.475026	270958.982934	38.473972
2319.373933	271383.781533	38.478989
2321.623525	271800.370262	38.484007
2324.345987	272223.158840	38.489024
2326.475389	272663.011058	38.494042
2329.217666	273077.769340	38.499060
2331.520026	273501.361653	38.504077
2333.566687	273928.982944	38.509095
2336.340526	274358.521326	38.514112
2338.407062	274779.229901	38.519130
2341.041988	275199.924639	38.524148
2343.217163	275629.507274	38.529165
2345.675495	276059.146653	38.534183
2348.291470	276478.244026	38.539200
2350.540804	276899.812819	38.544218
2352.940354	277337.057070	38.549236
2355.358566	277759.818356	38.554253
2357.724984	278180.682519	38.559271
2360.313425	278597.624674	38.564288
2362.399279	279025.264999	38.569306
2364.966886	279435.884771	38.574324
2367.207639	279870.943444	38.579341
2369.643485	280285.521309	38.584359
2372.230613	280682.394285	38.589376
2374.165996	281074.518347	38.594394
2376.276106	281460.797161	38.599412
2379.017168	281854.190307	38.604429
2381.157467	282249.126441	38.609447
2383.307583	282641.723677	38.614464
2385.489060	283043.003605	38.619482
2387.940519	283446.348932	38.624500
2389.877799	283862.197633	38.629517
2392.327051	284267.778170	38.634535
2395.184537	284681.829139	38.639552
2397.074929	285102.155182	38.644570
2399.619867	285527.051264	38.649588
2401.969417	285941.765843	38.654605
2404.630712	286372.688564	38.659623
2406.794329	286796.017968	38.664640
2409.181880	287234.477009	38.669658
2411.816622	287639.745441	38.674676
2414.030333	288085.953494	38.679693
2416.474789	288523.893839	38.684711
2418.969266	288954.128591	38.689728
2421.103918	289401.160262	38.694746
2423.513597	289832.118511	38.699764
2426.624481	290267.689917	38.704781
2429.014696	290717.702017	38.709799
2431.575600	291156.890189	38.714816
2433.707103	291595.942474	38.719834
2436.641719	292040.023475	38.724852
2439.290134	292477.290364	38.729869
2441.546036	292918.403659	38.734887
2444.561932	293351.952782	38.739904
2446.541627	293795.470653	38.744922
2449.460384	294224.740529	38.749940
2451.753510	294665.920810	38.754957
2454.653516	295106.318164	38.759975
2456.864180	295544.029606	38.764992
2459.307837	295990.771780	38.770010
2461.995386	296422.563287	38.775028
2464.399530	296862.552831	38.780045
2466.508450	297306.779497	38.785063
2469.314967	297745.814198	38.790080
2471.511023	298196.096032	38.795098
2473.969291	298633.024660	38.800116
2476.506624	299073.826168	38.805133
2479.049583	299520.544278	38.810151
2481.662738	299968.977423	38.815168
2483.938423	300416.319792	38.820186
2486.495297	300847.816682	38.825204
2489.065232	301314.542131	38.830221
2491.160165	301775.651595	38.835239
2493.942888	302212.290915	38.840256
2496.610023	302664.340451	38.845274
2499.308584	303106.324827	38.850292
2501.609741	303561.173000	38.855309
2504.070413	303993.540046	38.860327
2506.269657	304425.007398	38.865344
2508.696488	304851.357229	38.870362
2511.194904	305259.228093	38.875380
2513.886401	305674.331761	38.880397
2516.138527	306105.252155	38.885415
2518.647181	306518.451781	38.890432
2520.972925	306942.245688	38.895450
2523.306165	307372.234729	38.900468
2525.829453	307816.568780	38.905485
2527.942005	308252.000109	38.910503
2530.677378	308694.240080	38.915520
2533.154875	309140.126138	38.920538
2535.192413	309591.998463	38.925556
2537.718754	310035.841523	38.930573
2539.818774	310499.333655	38.935591
2542.679164	310959.909543	38.940608
2545.554592	311446.515714	38.945626
2547.907718	311912.070287	38.950644
2550.403950	312384.458084	38.955661
2552.981105	312849.236716	38.960679
2555.818685	313318.620166	38.965696
2558.061095	313803.589257	38.970714
2561.231368	314276.878093	38.975732
2563.635820	314750.717931	38.980749
2566.080836	315237.502502	38.985767
2569.064595	315711.373203	38.990784
2571.424208	316203.424240	38.995802
2574.194635	316675.901951	39.000820
2576.896349	317156.388732	39.005837
2579.315876	317639.737066	39.010855
2582.173480	318118.467393	39.015872
2584.549520	318624.142463	39.020890
2587.378091	319092.078503	39.025908
2590.173026	319591.713629	39.030925
2592.367914	320074.729683	39.035943
2595.137078	320562.985658	39.040960
2597.468879	321049.251148	39.045978
2600.294435	321542.216794	39.050996
2603.217802	322041.411845	39.056013
2606.026153	322528.787458	39.061031
2608.563734	323013.511221	39.066048
2610.955762	323506.407568	39.071066
2613.657628	323995.442570	39.076084
2616.599818	324476.614694	39.081101
2619.384703	324980.030428	39.086119
2622.255741	325461.741472	39.091136
2624.887731	325949.557123	39.096154
2627.595704	326431.694631	39.101172
2630.186971	326910.774914	39.106189
2632.710226	327395.500834	39.111207
2635.342651	327880.511240	39.116224
2638.006927	328374.224046	39.121242
2640.742374	328840.191429	39.126260
2643.634322	329331.627339	39.131277
2645.987918	329800.722116	39.136295
2648.808776	330258.185603	39.141312
2651.579398	330694.983475	39.146330
2653.977806	331148.927862	39.151348
2656.399483	331585.191705	39.156365
2658.666480	332033.996512	39.161383
2661.500633	332481.769161	39.166400
2663.853358	332951.478922	39.171418
2666.181261	333411.362387	39.176436
2669.338956	333867.404073	39.181453
2671.520044	334348.609400	39.186471
2674.093677	334817.738527	39.191488
2676.444676	335304.826812	39.196506
2678.824555	335782.613500	39.201524
2682.006387	336275.733612	39.206541
2684.169438	336763.374477	39.211559
2687.135597	337244.003448	39.216576
2689.742629	337744.948269	39.221594
2692.391518	338242.581786	39.226612
2695.300183	338742.480975	39.231629
2698.014393	339250.125960	39.236647
2700.547650	339756.297550	39.241664
2703.570526	340275.412939	39.246682
2705.940831	340779.799471	39.251700
2708.964760	341291.898606	39.256717
2711.342735	341805.466893	39.261735
2714.281698	342332.703300	39.266752
2717.212291	342853.969979	39.271770
2719.314145	343359.672873	39.276788
2722.896436	343901.798889	39.281805
2725.031298	344422.060950	39.286823
2727.971260	344928.912730	39.291840
2730.673487	345478.374126	39.296858
2733.781529	346004.078979	39.301876
2736.544020	346526.228720	39.306893
2739.676356	347064.766393	39.311911
2742.209773	347578.945741	39.316928
2745.137301	348100.902686	39.321946
2747.592028	348626.280761	39.326964
2750.637493	349148.640896	39.331981
2753.422435	349698.048619	39.336999
2756.024782	350216.457805	39.342016
2759.040757	350737.538289	39.347034
2761.653434	351274.264509	39.352052
2764.665025	351824.097317	39.357069
2767.193688	352326.911329	39.362087
2770.009490	352879.582066	39.367104
2773.176417	353398.328199	39.372122
2775.929955	353925.435405	39.377140
2778.603592	354463.592089	39.382157
2781.726574	355004.845042	39.387175
2784.476783	355523.534457	39.392192
2787.606857	356054.900965	39.397210
2790.156928	356578.586504	39.402228
2793.308369	357102.831358	39.407245
2796.001539	357617.624802	39.412263
2798.672133	358109.775408	39.417280
2801.662407	358564.431825	39.422298
2804.027608	359073.957212	39.427316
2806.802667	359525.745278	39.432333
2809.572349	360050.856935	39.437351
2811.980535	360521.780638	39.442368
2814.929945	361041.979887	39.447386
2817.728355	361518.847300	39.452404
2820.291280	362009.655663	39.457421
2822.982053	362539.650936	39.462439
2825.863958	363046.133666	39.467456
2828.796796	363543.770771	39.472474
2830.765571	364064.574165	39.477492
2833.700269	364597.755979	39.482509
2836.534214	365090.925392	39.487527
2839.232576	365657.556004	39.492544
2842.262569	366170.604705	39.497562
2844.948746	366708.952902	39.502580
2847.611589	367262.093400	39.507597
2850.683097	367795.190524	39.512615
2853.266831	368357.592585	39.517632
2855.853302	368918.439071	39.522650
2858.597240	369463.647091	39.527668
2861.859125	370052.412783	39.532685
2864.737533	370583.780986	39.537703
2867.655510	371181.137277	39.542720
2870.788814	371725.316207	39.547738
2873.274659	372314.630447	39.552756
2876.450725	372852.469886	39.557773
2879.375254	373472.274377	39.562791
2882.331191	374012.671146	39.567808
2885.276889	374609.390861	39.572826
2888.418273	375177.095283	39.577844
2891.479225	375737.801796	39.582861
2894.327360	376338.672886	39.587879
2896.973263	376909.171816	39.592896
2899.750108	377491.769442	39.597914
2902.881489	378078.970739	39.602932
2906.205330	378652.737257	39.607949
2908.894362	379251.610974	39.612967
2912.404630	379801.813123	39.617984
2915.196925	380407.274412	39.623002
2917.962500	380977.543631	39.628020
2920.777718	381542.215487	39.633037
2924.057929	382153.407073	39.638055
2926.935662	382704.378443	39.643072
2930.309611	383302.827476	39.648090
2933.165241	383860.584087	39.653108
2936.299714	384440.053013	39.658125
2938.966025	385029.936568	39.663143
2941.977171	385592.919011	39.668160
2944.777902	386158.488142	39.673178
2947.598851	386754.914862	39.678196
2950.880780	387333.934789	39.683213
2953.600241	387898.297845	39.688231
2956.666088	388442.864116	39.693248
2959.395411	389000.005080	39.698266
2961.943893	389511.106380	39.703284
2964.858994	390083.292273	39.708301
2968.051303	390600.211008	39.713319
2970.410340	391171.199277	39.718336
2973.686161	391680.226774	39.723354
2976.072221	392285.633894	39.728372
2979.257053	392818.093078	39.733389
2981.955890	393401.544879	39.738407
2984.741123	393961.337615	39.743424
2987.357696	394548.688509	39.748442
2990.273967	395106.894917	39.753460
2993.165226	395726.920833	39.758477
2995.997332	396305.712196	39.763495
2999.057784	396912.122941	39.768512
3002.041447	397534.104338	39.773530
3005.124607	398103.214572	39.778548
3007.915181	398750.383295	39.783565
3011.390576	399328.969828	39.788583
3013.933790	399972.603907	39.793600
3017.502160	400566.646154	39.798618
3020.203071	401216.620269	39.803636
3023.867142	401831.415003	39.808653
3026.445179	402451.542014	39.813671
3029.791770	403077.544128	39.818688
3033.022359	403683.878723	39.823706
3035.994114	404337.752562	39.828724
3039.239144	404938.762311	39.833741
3042.517604	405576.387649	39.838759
3045.173727	406216.126537	39.843776
3048.416476	406836.645542	39.848794
3051.312645	407490.288138	39.853812
3054.344099	408118.369051	39.858829
3057.611589	408753.193182	39.863847
3060.556145	409400.957345	39.868864
3064.144626	410042.497115	39.873882
3067.327517	410680.513562	39.878900
3070.462577	411308.993849	39.883917
3073.434964	411960.855549	39.888935
3076.626642	412594.090254	39.893952
3079.743567	413215.309896	39.898970
3082.576160	413885.577121	39.903988
3085.844332	414505.503814	39.909005
3089.103575	415155.399662	39.914023
3092.020245	415815.269486	39.919040
3095.210753	416447.280903	39.924058
3098.203899	417086.836111	39.929076
3101.389106	417732.149760	39.934093
3104.664401	418368.413491	39.939111
3107.769016	419017.562572	39.944128
3110.731759	419676.702842	39.949146
3113.909250	420331.714262	39.954164
3117.129841	420959.186642	39.959181
3120.204216	421591.304821	39.964199
3123.061590	422219.262425	39.969216
3126.250529	422815.407096	39.974234
3129.246257	423405.210215	39.979252
3131.978811	424026.280533	39.984269
3135.344063	424642.955151	39.989287
3138.070223	425245.073897	39.994304
3140.947999	425870.386052	39.999322
3144.258225	426500.555247	40.004340
3147.304793	427115.653411	40.009357
3150.362290	427764.502806	40.014375
3153.275204	428374.678861	40.019392
3156.508939	429039.073274	40.024410
3159.390075	429667.513187	40.029428
3162.290084	430333.346338	40.034445
3166.173352	430949.515119	40.039463
3169.078649	431638.337940	40.044480
3172.292648	432288.115094	40.049498
3174.908697	432980.569899	40.054516
3178.094944	433613.653267	40.059533
3181.664708	434313.392559	40.064551
3184.257788	434964.416057	40.069568
3187.747324	435680.566269	40.074586
3190.862563	436348.337476	40.079604
3193.770469	437051.727350	40.084621
3196.904698	437740.552350	40.089639
3200.258062	438425.728148	40.094656
3203.732860	439165.558040	40.099674
3206.595253	439854.924691	40.104692
3210.033971	440568.740374	40.109709
3213.152373	441282.839201	40.114727
3216.351660	441995.030934	40.119744
3219.948634	442711.797264	40.124762
3222.944244	443430.308412	40.129780
3226.165449	444146.737319	40.134797
3229.736519	444886.885190	40.139815
3232.818632	445587.091892	40.144832
3236.287568	446332.881456	40.149850
3239.278197	447059.587282	40.154868
3242.926324	447771.486209	40.159885
3246.227363	448531.660529	40.164903
3248.819185	449252.742848	40.169920
3252.689108	449968.083422	40.174938
3255.974695	450714.421057	40.179956
3259.172671	451451.739069	40.184973
3262.512947	452165.728933	40.189991
3265.954762	452926.951784	40.195008
3269.482109	453658.579591	40.200026
3272.842387	454389.805445	40.205044
3275.944383	455118.771266	40.210061
3279.443543	455850.231610	40.215079
3282.472643	456600.111518	40.220096
3285.810531	457316.216769	40.225114
3289.143951	458064.987373	40.230132
3292.203188	458818.582934	40.235149
3295.686664	459535.605576	40.240167
3298.630229	460244.898624	40.245184
3301.913704	460941.770207	40.250202
3305.211115	461613.270862	40.255220
3308.284842	462340.536622	40.260237
3311.616706	462997.166150	40.265255
3314.400562	463716.640880	40.270272
3317.642201	464442.392926	40.275290
3320.869386	465125.480742	40.280308
3323.792774	465864.437222	40.285325
3327.509502	466598.235173	40.290343
3330.412987	467317.974358	40.295360
3333.953786	468050.384144	40.300378
3336.951778	468792.412904	40.305396
3339.951808	469562.887688	40.310413
3343.274082	470277.503040	40.315431
3346.266606	471055.206073	40.320448
3349.611321	471812.748917	40.325466
3353.009393	472598.926209	40.330484
3356.343375	473369.257113	40.335501
3359.137338	474154.256740	40.340519
3362.493503	474960.372347	40.345536
3366.126507	475733.650720	40.350554
3369.092215	476547.247445	40.355572
3372.402625	477362.172292	40.360589
3376.212274	478174.963011	40.365607
3379.349558	478987.928029	40.370624
3382.949912	479787.593679	40.375642
3386.624440	480640.338587	40.380660
3389.979748	481434.517412	40.385677
3393.665530	482288.149445	40.390695
3396.970382	483084.291026	40.395712
3400.885977	483896.172131	40.400730
3404.358141	484747.759184	40.405748
3407.462592	485565.762663	40.410765
3411.043194	486372.792042	40.415783
3415.264358	487176.907113	40.420800
3418.724944	488003.946384	40.425818
3422.313293	488833.708303	40.430836
3425.685723	489675.189041	40.435853
3429.359873	490516.736101	40.440871
3432.573970	491310.478331	40.445888
3435.998576	492120.520533	40.450906
3439.776619	492942.847335	40.455924
3442.644262	493779.071032	40.460941
3447.114265	494563.131503	40.465959
3450.155041	495410.214289	40.470976
3453.134951	496261.610939	40.475994
3456.817455	497092.454288	40.481012
3460.204261	497904.268258	40.486029
3463.382871	498712.847002	40.491047
3466.437587	499552.059447	40.496064
3469.855519	500385.065802	40.501082
3473.371535	501231.246338	40.506100
3477.101951	502089.217481	40.511117
3481.028700	502900.262277	40.516122
3484.377964	503664.802529	40.521127
3487.363229	504413.475702	40.526132
3490.564558	505056.868891	40.531136
3493.433207	505691.131343	40.536141
3496.107284	506234.363880	40.541146
3498.161517	506726.112786	40.546151
3500.663799	507168.440095	40.551156
3503.650821	507541.103381	40.556160
3505.864193	507868.239804	40.561165
3507.904304	508191.804904	40.566170
3509.470022	508408.626012	40.571175
3510.272095	508583.568885	40.576180
3512.761871	508694.541026	40.581184
3513.757853	508804.028231	40.586189
3514.752136	508899.702041	40.591194
3515.795822	508947.654765	40.596199
3516.688425	508931.879285	40.601204
3517.643875	508882.699857	40.606208
3518.153466	508834.197920	40.611213
3519.008370	508760.140214	40.616218
3519.302581	508662.693504	40.621223
3519.593870	508543.185987	40.626228
3520.880615	508412.135688	40.631232
3520.944191	508256.686687	40.636237
3521.558531	508086.070650	40.641242
3521.124634	507910.457416	40.646247
3521.132119	507740.338688	40.651252
3521.808289	507554.881750	40.656256
3521.321421	507353.565982	40.661261
3521.128958	507138.235179	40.666266
3521.331706	506923.294678	40.671271
3521.530600	506713.564281	40.676276
3521.604960	506488.163815	40.681280
3521.787614	506255.102023	40.686285
3522.384114	505996.719636	40.691290
3521.896472	505754.951772	40.696295
3521.369826	505516.779819	40.701300
3521.731703	505277.705093	40.706304
3521.240944	505042.557480	40.711309
3521.192907	504798.885072	40.716314
3521.411051	504537.909350	40.721319
3521.317198	504306.889775	40.726324
3520.587287	504062.606404	40.731328
3520.585857	503817.698402	40.736333
3519.633179	503581.085938	40.741338
3519.577202	503351.971156	40.746343
3519.453768	503122.256707	40.751348
3519.812113	502884.111775	40.756352
3519.370849	502648.418314	40.761357
3519.390430	502405.107151	40.766362
3518.913150	502203.174128	40.771367
3518.351106	502012.995319	40.776372
3518.139230	501752.046528	40.781376
3518.139431	501566.481529	40.786381
3517.975572	501327.385946	40.791386
3517.627006	501137.315920	40.796391
3516.926629	500925.279826	40.801396
3517.374222	500696.962459	40.806400
3516.909669	500519.913688	40.811405
3517.046694	500288.501702	40.816410
3516.654871	500085.771928	40.821415
3516.210058	499939.998860	40.826420
3515.772596	499730.741967	40.831424
3515.904835	499528.024328	40.836429
3515.645850	499358.018961	40.841434
3515.381057	499187.354788	40.846439
3515.002849	499032.755133	40.851444
3514.896898	498840.901218	40.856448
3514.829700	498640.787051	40.861453
3514.766447	498500.915955	40.866458
3514.664905	498313.105885	40.871463
3514.366152	498150.385769	40.876468
3514.242680	498029.860329	40.881472
3513.817675	497861.031577	40.886477
3513.713094	497694.226401	40.891482
3513.187829	497542.978786	40.896487
3512.906823	497393.108942	40.901492
3513.450093	497238.652129	40.906496
3512.920554	497129.829851	40.911501
3512.691326	497006.833447	40.916506
3512.652555	496870.236936	40.921511
3512.197225	496701.959167	40.926516
3512.749560	496552.051966	40.931520
3511.664366	496447.617169	40.936525
3512.120880	496322.431843	40.941530
3511.823741	496219.086377	40.946535
3511.465599	496056.812642	40.951540
3511.137272	495947.748983	40.956544
3510.930468	495866.463582	40.961549
3510.985132	495773.085536	40.966554
3511.145251	495664.348068	40.971559
3510.905733	495503.974804	40.976564
3510.890928	495397.288802	40.981568
3510.161618	495329.451329	40.986573
3510.249774	495240.825021	40.991578
3510.222215	495127.607453	40.996583
3509.571938	495010.031604	41.001588
3510.408252	494902.195485	41.006592
3510.060321	494820.320119	41.011597
3509.789368	494731.545568	41.016602
3509.773023	494643.591184	41.021607
3509.144896	494561.201939	41.026612
3509.176832	494496.583163	41.031616
3509.367156	494409.557118	41.036621
3509.319802	494331.379290	41.041626
3509.523940	494233.513639	41.046631
3509.134815	494153.515448	41.051636
3509.205851	494108.486325	41.056640
3509.268869	494053.533111	41.061645
3509.019984	493971.688962	41.066650
3508.739623	493899.065810	41.071655
3508.655439	493814.257845	41.076660
3508.421277	493724.611763	41.081664
3508.529127	493639.570087	41.086669
3508.746112	493606.113269	41.091674
3508.211458	493522.742452	41.096679
3508.521134	493429.565435	41.101684
3508.427311	493378.281139	41.106688
3508.423574	493345.010658	41.111693
3508.283257	493255.701961	41.116698
3508.699702	493160.936843	41.121703
3507.934698	493114.416912	41.126708
3507.940227	493098.008169	41.131712
3507.631083	493032.425356	41.136717
3507.984716	492939.492142	41.141722
3507.989403	492926.881537	41.146727
3507.574715	492853.465244	41.151732
3507.306513	492775.670252	41.156736
3507.435664	492715.739654	41.161741
3507.420889	492722.528125	41.166746
3507.330051	492650.325912	41.171751
3507.488607	492584.313099	41.176756
3507.724365	492520.516151	41.181760
3507.289167	492473.132194	41.186765
3507.241021	492421.382248	41.191770
3507.519797	492387.001888	41.196775
3507.097022	492325.840533	41.201780
3507.288927	492293.803344	41.206784
3506.979007	492273.544155	41.211789
3506.742614	492247.196048	41.216794
3506.866254	492213.903412	41.221799
3506.856485	492176.529625	41.226804
3507.017773	492110.160191	41.231808
3506.552349	492066.325079	41.236813
3507.106030	491995.689731	41.241818
3506.834121	491956.938886	41.246823
3506.665991	491965.271213	41.251828
3506.705899	491918.215912	41.256832
3506.640409	491884.547422	41.261837
3506.397094	491869.949500	41.266842
3506.267078	491838.823374	41.271847
3506.483228	491805.363453	41.276852
3506.797756	491749.603999	41.281856
3506.068353	491727.992447	41.286861
3506.044867	491689.961465	41.291866
3505.985296	491659.938108	41.296871
3505.911709	491628.448194	41.301876
3506.812533	491576.697857	41.306880
3506.129937	491561.105561	41.311885
3506.179411	491562.617133	41.316890
3506.262159	491522.543187	41.321895
3506.090917	491504.692249	41.326900
3506.394587	491495.021534	41.331904
3506.530671	491452.963815	41.336909
3506.146280	491418.787780	41.341914
3506.205963	491380.236561	41.346919
3505.757252	491359.643791	41.351924
3505.978286	491317.521695	41.356928
3506.387828	491264.733923	41.361933
3506.301925	491283.436112	41.366938
3506.032825	491254.306212	41.371943
3506.152185	491202.273181	41.376948
3506.562985	491191.724382	41.381952
3506.152906	491169.352657	41.386957
3506.314808	491103.941848	41.391962
3506.024475	491122.119390	41.396967
3505.962365	491121.166931	41.401972
3505.971543	491078.419371	41.406976
3505.779046	491038.539834	41.411981
3506.058072	490990.532758	41.416986
3506.306695	490961.472518	41.421991
3505.644876	490980.620565	41.426996
3505.915784	490922.839650	41.432000
3505.862638	490887.496046	41.437005
3505.877267	490913.425327	41.442010
3505.540850	490859.538772	41.447015
3505.856893	490835.532453	41.452020
3505.854619	490842.927404	41.457024
3505.644733	490812.369321	41.462029
3505.850189	490754.750177	41.467034
3505.896116	490782.447372	41.472039
3505.261753	490737.926775	41.477044
3505.803467	490728.927116	41.482048
3505.475514	490711.404077	41.487053
3505.721330	490660.109278	41.492058
3505.679108	490669.384597	41.497063
3505.604566	490686.009009	41.502068
3505.563444	490662.717345	41.507072
3505.512847	490633.602594	41.512077
3506.003367	490577.305357	41.517082
3505.725874	490569.093528	41.522087
3505.451655	490582.406789	41.527092
3505.775158	490564.122220	41.532096
3505.378774	490527.312731	41.537101
3504.928329	490509.353026	41.542106
3505.813553	490473.657739	41.547111
3505.433496	490503.549920	41.552116
3505.568800	490473.392565	41.557120
3505.051082	490457.722637	41.562125
3505.521589	490414.090271	41.567130
3505.212953	490421.533809	41.572135
3505.039796	490449.468717	41.577140
3505.421023	490393.542745	41.582144
3505.328896	490404.649445	41.587149
3505.220223	490382.178494	41.592154
3505.392292	490332.261980	41.597159
3505.573795	490362.014981	41.602164
3505.745377	490365.178770	41.607168
3505.356590	490352.172776	41.612173
3505.224044	490334.973046	41.617178
3505.690855	490310.182491	41.622183
3505.487954	490302.465248	41.627188
3505.296609	490255.796869	41.632192
3504.980511	490239.233854	41.637197
3505.611335	490210.618541	41.642202
3505.894716	490184.387978	41.647207
3505.815065	490193.618797	41.652212
3505.829712	490199.339894	41.657216
3505.102000	490153.110580	41.662221
3505.740214	490106.361369	41.667226
3505.504588	490095.255680	41.672231
3505.256463	490120.113287	41.677236
3505.302268	490130.337304	41.682240
3505.325562	490108.452964	41.687245
3504.965933	490069.560130	41.692250
3505.654950	490040.428864	41.697255
3505.347010	490036.729457	41.702260
3505.341472	490050.962976	41.707264
3505.605766	489995.003653	41.712269
3505.308699	489965.369672	41.717274
3505.587678	489992.474045	41.722279
3505.376507	489995.394491	41.727284
3505.239230	489966.444357	41.732288
3505.925018	489924.549587	41.737293
3505.433548	489900.011252	41.742298
3505.413814	489873.321660	41.747303
3505.344599	489858.542703	41.752308
3505.681014	489843.395720	41.757312
3505.277479	489867.873020	41.762317
3505.477457	489867.740130	41.767322
3505.497749	489835.270013	41.772327
3504.835882	489811.619552	41.777332
3505.828091	489772.107240	41.782336
3505.394446	489747.610217	41.787341
3505.300412	489743.319786	41.792346
3505.489858	489746.531507	41.797351
3505.085855	489759.106099	41.802356
3505.417872	489751.253435	41.807360
3505.406857	489733.426138	41.812365
3505.448778	489719.895776	41.817370
3505.204427	489677.235753	41.822375
3505.203557	489657.279443	41.827380
3505.673502	489637.198049	41.832384
3504.746916	489632.482016	41.837389
3504.731690	489626.710223	41.842394
3505.414737	489632.477804	41.847399
3505.393636	489619.210584	41.852404
3505.053915	489582.947454	41.857408
3504.631802	489593.954833	41.862413
3504.807318	489575.388789	41.867418
3505.456680	489562.825982	41.872423
3505.043114	489584.215510	41.877428
3505.285159	489573.945737	41.882432
3505.254818	489541.888328	41.887437
3505.550363	489505.423342	41.892442
3505.595635	489477.355330	41.897447
3505.383345	489475.666751	41.902452
3505.522662	489464.653383	41.907456
3505.471475	489445.261969	41.912461
3505.555790	489468.396391	41.917466
3505.449908	489454.939850	41.922471
3505.336818	489422.135544	41.927476
3505.425130	489425.971124	41.932480
3505.035041	489409.267117	41.937485
3505.300781	489404.717140	41.942490
3505.618978	489365.462464	41.947495
3505.317449	489361.508650	41.952500
3505.350398	489321.843102	41.957504
3505.469481	489306.172870	41.962509
3505.285015	489335.478814	41.967514
3505.356769	489323.412355	41.972519
3505.348476	489309.028553	41.977524
3504.962120	489272.164373	41.982528
3505.156619	489246.908945	41.987533
3505.460412	489226.954680	41.992538
3505.426207	489201.380773	41.997543
3505.409883	489189.074888	42.002548
3505.506522	489198.582244	42.007552
3505.251059	489177.804580	42.012557
3505.465256	489139.730875	42.017562
3505.458404	489134.514783	42.022567
3505.262985	489124.921737	42.027572
3505.577706	489109.220421	42.032576
3505.412296	489078.753800	42.037581
3505.129092	489065.325008	42.042586
3505.053944	489058.904029	42.047591
3504.991580	489085.455824	42.052596
3505.151002	489058.483503	42.057600
3504.987478	489020.114689	42.062605
3505.091325	489011.132771	42.067610
3505.094055	489021.668112	42.072615
3505.021321	489021.679625	42.077620
3505.264731	489037.090225	42.082624
3505.274883	489023.766995	42.087629
3505.066243	488995.738400	42.092634
3504.837030	488971.765238	42.097639
3505.009805	488969.965101	42.102644
3505.010200	488950.615679	42.107648
3505.524177	488957.777817	42.112653
3505.291985	488952.192068	42.117658
3505.053138	488938.401605	42.122663
3505.071326	488927.407070	42.127668
3505.083659	488913.931460	42.132672
3505.184721	488912.953099	42.137677
3505.061662	488897.776676	42.142682
3504.820348	488872.589629	42.147687
3504.574684	488867.867087	42.152692
3505.254391	488838.330221	42.157696
3504.813165	488874.515633	42.162701
3504.738333	488868.246498	42.167706
3505.330121	488804.178054	42.172711
3505.177562	488837.481330	42.177716
3505.141926	488805.879390	42.182720
3505.010058	488803.418240	42.187725
3504.681073	488794.403323	42.192730
3505.096243	488765.870567	42.197735
3504.870240	488818.383091	42.202740
3505.108566	488760.144826	42.207744
3505.075216	488770.483396	42.212749
3504.650857	488787.418034	42.217754
3505.051444	488776.565586	42.222759
3504.731795	488769.170086	42.227764
3504.972891	488752.770966	42.232768
3504.800142	488739.729711	42.237773
3504.533471	488727.108520	42.242778
3504.696176	488730.476602	42.247783
3504.999917	488716.904141	42.252788
3505.042621	488709.755269	42.257792
3504.661976	488729.823565	42.262797
3504.562226	488708.970121	42.267802
3505.314478	488672.937885	42.272807
3505.298020	488673.447040	42.277812
3504.846583	488692.310878	42.282816
3505.268990	488640.830726	42.287821
3504.993061	488684.487116	42.292826
3505.226653	488628.376644	42.297831
3504.651399	488625.479013	42.302836
3505.236707	488655.728072	42.307840
3505.210675	488637.952770	42.312845
3504.624532	488609.932615	42.317850
3504.888101	488594.796150	42.322855
3505.073128	488587.675391	42.327860
3504.962850	488612.411883	42.332864
3504.939172	488604.311041	42.337869
3504.663233	488583.029422	42.342874
3504.865188	488546.476076	42.347879
3504.967527	488541.039947	42.352884
3504.784651	488579.920400	42.357888
3504.902990	488536.997867	42.362893
3505.016503	488512.108838	42.367898
3504.927963	488551.835556	42.372903
3504.606519	488543.376520	42.377908
3504.730091	488498.832147	42.382912
3505.044125	488533.987064	42.387917
3504.665972	488513.076099	42.392922
3505.122955	488482.358187	42.397927
3504.853284	488539.234636	42.402932
3504.796153	488482.815106	42.407936
3505.301366	488466.677919	42.412941
3504.928317	488497.939820	42.417946
3505.127472	488468.782258	42.422951
3505.232925	488432.142635	42.427956
3505.406451	488460.734845	42.432960
3504.652670	488441.402794	42.437965
3505.121038	488399.741637	42.442970
3505.185527	488389.853868	42.447975
3505.097760	488432.822590	42.452980
3505.133120	488438.692909	42.457984
3505.191053	488414.774967	42.462989
3504.598106	488403.370176	42.467994
3504.969916	488394.497577	42.472999
3505.048215	488381.973596	42.478004
3504.790594	488372.035418	42.483008
3504.843322	488370.507470	42.488013
3504.653452	488353.770885	42.493018
3505.221191	488310.371576	42.498023
3505.064727	488347.070185	42.503028
3505.066842	488338.357299	42.508032
3504.883747	488309.462525	42.513037
3504.511236	488302.075197	42.518042
3505.370128	488279.144893	42.523047
3505.149443	488260.538874	42.528052
3505.380841	488253.157388	42.533056
3505.117968	488270.725473	42.538061
3504.870288	488285.454482	42.543066
3505.172923	488249.593817	42.548071
3504.780320	488240.487380	42.553076
3505.038699	488204.836245	42.558080
3505.184652	488233.585119	42.563085
3504.611498	488211.742201	42.568090
3505.590889	488181.549094	42.573095
3505.191150	488193.972081	42.578100
3504.875999	488173.456023	42.583104
3504.630751	488163.059886	42.588109
3505.071547	488139.840910	42.593114
3505.010163	488166.799075	42.598119
3504.823555	488144.489746	42.603124
3505.117448	488102.956826	42.608128
3505.019341	488114.926951	42.613133
3505.050936	488139.742945	42.618138
3505.017046	488115.585864	42.623143
3504.782281	488132.187188	42.628148
3504.668941	488113.006854	42.633152
3504.931662	488066.362617	42.638157
3504.358199	488085.347653	42.643162
3505.160521	488047.229459	42.648167
3504.934671	488091.943054	42.653172
3504.681635	488055.511332	42.658176
3504.827940	488083.095307	42.663181
3504.816859	488034.468061	42.668186
3505.401578	488029.664720	42.673191
3504.762592	488062.792958	42.678196
3504.756683	488022.725593	42.683200
3505.279983	488022.693558	42.688205
3504.844435	487996.674906	42.693210
3505.102866	488016.440326	42.698215
3505.042685	487979.775355	42.703220
3504.871364	487993.580723	42.708224
3504.723979	487966.706000	42.713229
3505.011150	487960.581972	42.718234
3504.969929	487975.278590	42.723239
3504.326161	487948.178362	42.728244
3504.809549	487930.423195	42.733248
3504.801054	487941.568776	42.738253
3504.985686	487914.236258	42.743258
3504.906223	487964.803066	42.748263
3504.556435	487940.645035	42.753268
3504.986490	487905.320794	42.758272
3504.909635	487921.036198	42.763277
3504.807558	487880.375866	42.768282
3504.801772	487900.031199	42.773287
3504.717950	487906.123142	42.778292
3504.846729	487888.373326	42.783296
3505.087907	487878.153431	42.788301
3504.590377	487887.400764	42.793306
3504.607251	487863.893865	42.798311
3504.755356	487884.335383	42.803316
3504.761664	487876.837360	42.808321
3504.746873	487870.406439	42.813325
3504.370440	487854.458736	42.818330
3505.086119	487820.862147	42.823335
3504.449743	487868.325913	42.828340
3504.478060	487830.633553	42.833345
3505.079281	487849.382507	42.838349
3504.608655	487846.873462	42.843354
3504.892583	487814.763464	42.848359
3504.779864	487830.585922	42.853364
3504.935684	487799.610574	42.858369
3504.778805	487811.083619	42.863373
3504.471034	487826.683630	42.868378
3504.837715	487818.014198	42.873383
3504.477859	487779.471283	42.878388
3504.598709	487805.894597	42.883393
3504.489107	487783.572673	42.888397
3504.526844	487802.866636	42.893402
3504.733775	487779.582873	42.898407
3505.002612	487786.733546	42.903412
3504.764696	487804.956643	42.908417
3504.910629	487766.890977	42.913421
3504.918243	487768.764063	42.918426
3504.976098	487773.972504	42.923431
3504.879472	487743.340899	42.928436
3504.707594	487741.595120	42.933441
3504.926615	487766.837882	42.938445
3504.698853	487755.172358	42.943450
3504.366876	487733.037490	42.948455
3504.819534	487712.652860	42.953460
3504.850543	487744.662634	42.958465
3504.425123	487742.399710	42.963469
3504.683917	487719.360957	42.968474
3505.032704	487715.101389	42.973479
3504.717361	487723.256228	42.978484
3504.848125	487679.164705	42.983489
3504.663046	487725.797653	42.988493
3504.635039	487699.663526	42.993498
3504.957164	487697.333103	42.998503
3504.814892	487700.546946	43.003508
3505.227869	487657.677174	43.008513
3505.371259	487692.202088	43.013517
3505.020743	487641.398613	43.018522
3505.214692	487647.244110	43.023527
3505.121417	487658.200631	43.028532
3504.548165	487623.895601	43.033537
3505.274972	487575.961061	43.038541
3504.889818	487588.990015	43.043546
3505.124381	487611.495076	43.048551
3504.830687	487574.866234	43.053556
3505.062763	487593.572471	43.058561
3504.779799	487560.234574	43.063565
3504.979150	487544.651517	43.068570
3504.907248	487520.702316	43.073575
3505.082981	487502.438154	43.078580
3505.241942	487504.540629	43.083585
3505.480162	487492.497354	43.088589
3505.235338	487466.954401	43.093594
3505.512908	487470.963091	43.098599
3505.272009	487496.228246	43.103604
3505.114797	487482.981046	43.108609
3504.848705	487460.024939	43.113613
3504.948753	487433.464954	43.118618
3505.593196	487397.447350	43.123623
3504.871867	487397.054804	43.128628
3504.592264	487432.406898	43.133633
3504.943928	487435.137463	43.138637
3504.482006	487404.309765	43.143642
3504.815228	487368.138667	43.148647
3505.284090	487359.148935	43.153652
3504.916983	487403.481214	43.158657
3504.619900	487382.708161	43.163661
3504.222393	487371.575800	43.168666
3504.597764	487356.673968	43.173671
3505.319591	487327.634679	43.178676
3504.973723	487380.777999	43.183681
3504.616003	487365.485470	43.188685
3504.933395	487340.056115	43.193690
3504.885527	487313.114084	43.198695
3504.522229	487334.650164	43.203700
3504.727255	487350.828058	43.208705
3504.922159	487354.596553	43.213709
3504.657849	487356.056744	43.218714
3504.749725	487334.310335	43.223719
3504.732127	487319.521240	43.228724
3504.270233	487296.849169	43.233729
3505.071748	487266.885363	43.238733
3505.147218	487253.601228	43.243738
3504.966755	487286.303739	43.248743
3504.741269	487295.153759	43.253748
3505.065222	487238.974256	43.258753
3505.033508	487272.058541	43.263757
3504.466452	487249.808294	43.268762
3504.849651	487240.072185	43.273767
3504.511533	487260.033990	43.278772
3504.881374	487245.943463	43.283777
3504.622578	487222.023426	43.288781
3505.093527	487210.500423	43.293786
3504.856764	487245.896748	43.298791
3504.258956	487229.882195	43.303796
3504.573339	487214.685947	43.308801
3504.912440	487245.280112	43.313805
3504.839083	487193.266518	43.318810
3504.852457	487189.566422	43.323815
3504.947667	487221.414953	43.328820
3504.654168	487205.301625	43.333825
3504.804467	487178.277426	43.338829
3504.759774	487190.037058	43.343834
3504.578090	487176.033649	43.348839
3504.186067	487156.592452	43.353844
3505.004855	487123.788865	43.358849
3504.985764	487168.016028	43.363853
3504.256628	487156.125434	43.368858
3504.512701	487129.641681	43.373863
3504.672845	487174.093790	43.378868
3504.317671	487171.971667	43.383873
3504.587414	487132.973332	43.388877
3504.552618	487160.637925	43.393882
3504.693462	487151.092048	43.398887
3504.491467	487136.331956	43.403892
3504.019992	487123.134176	43.408897
3504.771952	487106.450266	43.413901
3504.455301	487112.173998	43.418906
3504.696213	487150.281179	43.423911
3504.508869	487172.600154	43.428916
3504.481054	487155.634271	43.433921
3504.653940	487124.655130	43.438925
3504.630474	487161.638946	43.443930
3505.376772	487122.008035	43.448935
3504.708520	487141.464907	43.453940
3504.778173	487106.094835	43.458945
3505.057836	487099.363827	43.463949
3504.925412	487130.539279	43.468954
3504.714195	487090.654378	43.473959
3504.949890	487057.841522	43.478964
3504.564666	487103.139860	43.483969
3504.541385	487084.349518	43.488973
3504.818279	487079.290648	43.493978
3504.905467	487067.169661	43.498983
3504.763771	487030.414433	43.503988
3504.644630	487062.905003	43.508993
3504.532509	487036.833921	43.513997
3504.444533	487046.067586	43.519002
3504.603620	487068.787849	43.524007
3504.677314	487053.781488	43.529012
3504.762560	487045.865400	43.534017
3504.987289	487004.442337	43.539021
3504.639939	487008.752527	43.544026
3504.796448	487018.352828	43.549031
3504.693497	487036.403352	43.554036
3504.895276	487027.860942	43.559041
3505.062305	487026.568112	43.564045
3504.658086	486997.858271	43.569050
3504.793488	486950.522218	43.574055
3504.707822	486967.607570	43.579060
3504.546300	486972.243005	43.584065
3505.304961	486959.914506	43.589069
3504.464311	486963.745434	43.594074
3505.424141	486918.406641	43.599079
3505.162903	486910.798551	43.604084
3504.777026	486926.816905	43.609089
3504.956586	486939.959678	43.614093
3504.554822	486939.060689	43.619098
3504.601305	486913.572270	43.624103
3504.724390	486913.907441	43.629108
3504.399316	486912.844356	43.634113
3504.854791	486897.017657	43.639117
3504.694298	486878.654066	43.644122
3504.917740	486906.024919	43.649127
3504.805930	486912.273576	43.654132
3504.634725	486871.672679	43.659137
3505.426389	486845.914417	43.664141
3504.995101	486901.098908	43.669146
3504.780757	486853.969869	43.674151
3504.205367	486848.133792	43.679156
3504.343247	486850.644939	43.684161
3504.525300	486846.766141	43.689165
3504.111798	486852.302624	43.694170
3504.116780	486848.705106	43.699175
3505.007171	486830.378008	43.704180
3504.869440	486823.560897	43.709185
3504.945266	486826.132514	43.714189
3504.772405	486867.497140	43.719194
3504.790891	486857.311898	43.724199
3504.703054	486852.462590	43.729204
3504.896149	486829.331832	43.734209
3504.732464	486815.173338	43.739213
3504.894965	486794.884251	43.744218
3504.847374	486794.638497	43.749223
3504.917271	486804.303254	43.754228
3504.503403	486766.881317	43.759233
3505.003480	486752.212599	43.764237
3504.598064	486790.270674	43.769242
3504.761579	486801.237759	43.774247
3504.610061	486764.230279	43.779252
3504.671290	486752.974394	43.784257
3505.070923	486724.643679	43.789261
3505.115936	486725.345804	43.794266
3504.821513	486730.812843	43.799271
3504.660445	486758.092704	43.804276
3504.385993	486718.166362	43.809281
3504.842337	486677.060596	43.814285
3504.657179	486721.922944	43.819290
3504.430596	486724.238418	43.824295
3504.771585	486690.800385	43.829300
3504.751582	486727.581857	43.834305
3504.847939	486735.621386	43.839309
3504.457968	486672.714127	43.844314
3505.010170	486666.091869	43.849319
3504.723323	486701.699751	43.854324
3504.146728	486686.339952	43.859329
3504.262260	486684.244696	43.864333
3504.354548	486694.665852	43.869338
3504.771530	486690.496598	43.874343
3504.538414	486695.143415	43.879348
3504.328698	486685.146125	43.884353
3504.576352	486687.184014	43.889357
3504.073813	486702.765064	43.894362
3504.159470	486690.441446	43.899367
3504.841645	486669.766138	43.904372
3504.730004	486705.396981	43.909377
3505.032211	486661.985239	43.914381
3504.689959	486677.490317	43.919386
3504.604660	486694.018607	43.924391
3504.551311	486686.732181	43.929396
3504.666060	486685.194296	43.934401
3505.030653	486653.829482	43.939405
3504.629011	486626.891740	43.944410
3504.997191	486611.534535	43.949415
3505.050382	486604.889807	43.954420
3504.769433	486657.416965	43.959425
3504.816225	486652.900940	43.964429
3504.766934	486604.782681	43.969434
3505.052517	486582.143598	43.974439
3504.885920	486634.196814	43.979444
3504.603697	486629.378172	43.984449
3504.842901	486603.858881	43.989453
3504.699776	486590.710153	43.994458
3504.672784	486559.255098	43.999463
3505.035110	486565.378271	44.004468
3504.771811	486562.785625	44.009473
3505.130424	486563.184896	44.014477
3504.511000	486555.329320	44.019482
3504.917182	486506.986849	44.024487
3504.747383	486548.756954	44.029492
3504.605515	486520.460864	44.034497
3504.696637	486518.774722	44.039501
3504.505149	486540.436517	44.044506
3504.667076	486510.927235	44.049511
3505.212330	486488.348318	44.054516
3504.965148	486521.873230	44.059521
3504.656136	486492.691649	44.064525
3505.173696	486465.405760	44.069530
3505.412376	486449.511639	44.074535
3504.631839	486481.449156	44.079540
3504.415860	486466.437459	44.084545
3504.878787	486453.192850	44.089549
3504.834660	486471.031971	44.094554
3504.875545	486422.493726	44.099559
3504.848363	486448.081102	44.104564
3504.972711	486406.773933	44.109569
3504.823425	486436.382731	44.114573
3504.573366	486444.629113	44.119578
3504.771983	486399.257428	44.124583
3504.995439	486403.274897	44.129588
3504.520377	486386.682979	44.134593
3505.162286	486350.714470	44.139597
3504.890391	486410.333238	44.144602
3504.838199	486388.051269	44.149607
3504.763690	486349.764326	44.154612
3504.939746	486353.080061	44.159617
3504.694991	486358.336716	44.164621
3505.095493	486328.688126	44.169626
3504.927873	486334.996452	44.174631
3504.900943	486341.282539	44.179636
3504.381194	486318.618450	44.184641
3504.693192	486353.068474	44.189645
3504.738263	486344.854487	44.194650
3504.349666	486333.466812	44.199655
3504.834951	486297.067020	44.204660
3504.752053	486312.480741	44.209665
3504.888744	486317.423819	44.214669
3504.526658	486292.353767	44.219674
3504.985813	486258.339047	44.224679
3504.907928	486315.343786	44.229684
3504.781873	486300.925665	44.234689
3504.572988	486261.291966	44.239693
3504.597112	486247.609969	44.244698
3504.494688	486225.133111	44.249703
3505.164758	486222.798178	44.254708
3504.867236	486247.466008	44.259713
3504.196984	486257.349342	44.264717
3504.101884	486266.027248	44.269722
3504.778229	486239.678482	44.274727
3504.794728	486279.798606	44.279732
3504.386643	486247.491394	44.284737
3504.512268	486220.013802	44.289741
3504.800990	486193.878218	44.294746
3504.603044	486244.873582	44.299751
3505.055257	486252.907730	44.304756
3504.894230	486259.316358	44.309761
3505.029879	486237.460466	44.314765
3504.925759	486226.382385	44.319770
3504.822244	486231.414111	44.324775
3504.643316	486220.803791	44.329780
3504.597415	486235.654465	44.334785
3504.832344	486221.027250	44.339789
3504.805052	486195.701517	44.344794
3504.370700	486191.210769	44.349799
3504.474705	486178.833262	44.354804
3504.331329	486130.120760	44.359809
3504.780058	486115.054390	44.364813
3504.561485	486141.179028	44.369818
3504.813753	486117.936740	44.374823
3504.952088	486124.804702	44.379828
3504.886983	486111.997937	44.384833
3504.655577	486118.468396	44.389837
3504.649535	486127.790874	44.394842
3504.567930	486139.354343	44.399847
3504.568121	486134.186978	44.404852
3504.770390	486146.972084	44.409857
3504.457213	486143.019436	44.414861
3504.434314	486136.893176	44.419866
3504.630011	486118.016616	44.424871
3504.674084	486103.115513	44.429876
3504.495388	486123.053304	44.434881
3504.711148	486116.028090	44.439885
3504.682013	486113.043750	44.444890
3504.586708	486117.618264	44.449895
3504.906265	486085.753037	44.454900
3504.412514	486108.830924	44.459905
3505.002341	486108.889700	44.464909
3504.744436	486070.377883	44.469914
3504.737979	486043.123557	44.474919
3504.885834	486068.987737	44.479924
3504.625052	486065.736039	44.484929
3504.624056	486074.348497	44.489933
3504.525935	486085.711968	44.494938
3504.309622	486071.206619	44.499943
3504.547252	486055.008375	44.504948
3504.674681	486055.697499	44.509953
3504.914352	486060.371065	44.514957
3504.754904	486043.576984	44.519962
3504.589402	486024.605439	44.524967
3505.188761	486015.898420	44.529972
3504.727852	486041.554889	44.534977
3504.674564	486000.122939	44.539981
3504.116618	485991.193538	44.544986
3504.759671	485967.990626	44.549991
3504.748713	486008.723586	44.554996
3504.389543	485995.000667	44.560001
3504.694729	485988.062594	44.565005
3504.941499	485978.195429	44.570010
3504.542428	485955.562497	44.575015
3504.716033	485972.050489	44.580020
3504.581336	485994.058549	44.585025
3504.587673	485982.101637	44.590029
3504.602419	485981.998003	44.595034
3504.499260	485984.598021	44.600039
3504.636157	485975.356149	44.605044
3504.360867	485974.538444	44.610049
3504.488341	485958.762815	44.615053
3504.427623	485955.074192	44.620058
3504.403275	485997.177133	44.625063
3504.805936	485987.589298	44.630068
3504.151507	485959.626695	44.635073
3504.156065	485952.888107	44.640077
3504.452415	485961.858906	44.645082
3504.925317	485935.389896	44.650087
3504.508912	485973.704630	44.655092
3504.436302	485947.676482	44.660097
3504.951263	485920.542214	44.665101
3504.495246	485947.616539	44.670106
3504.486722	485939.258868	44.675111
3504.900421	485959.609806	44.680116
3504.959417	485925.252457	44.685121
3504.658221	485917.650285	44.690125
3504.665088	485937.052330	44.695130
3504.478022	485912.916676	44.700135
3504.350657	485908.681307	44.705140
3504.489970	485898.932407	44.710145
3504.873850	485864.827566	44.715149
3504.659077	485901.590744	44.720154
3504.627857	485942.124403	44.725159
3504.887575	485928.404942	44.730164
3504.326094	485873.121296	44.735169
3505.027884	485839.118147	44.740173
3504.647080	485845.561649	44.745178
3504.426857	485866.620812	44.750183
3504.436301	485899.143690	44.755188
3504.061819	485896.011255	44.760193
3504.949773	485860.560214	44.765197
3504.754633	485871.989805	44.770202
3504.616969	485907.322276	44.775207
3504.507957	485865.189589	44.780212
3504.870974	485831.797242	44.785217
3504.713896	485825.286801	44.790221
3504.257682	485827.436030	44.795226
3504.523720	485833.777301	44.800231
3504.504046	485847.357603	44.805236
3504.391556	485828.782774	44.810241
3504.691596	485834.054787	44.815245
3504.635429	485864.460327	44.820250
3504.275878	485826.724003	44.825255
3504.676347	485808.473369	44.830260
3504.490465	485819.749545	44.835265
3504.818166	485793.201967	44.840269
3504.596570	485786.701710	44.845274
3504.889751	485779.664137	44.850279
3504.929379	485777.175489	44.855284
3504.509374	485804.548292	44.860289
3504.578526	485836.149938	44.865293
3504.531163	485819.793896	44.870298
3504.424538	485775.938157	44.875303
3504.560805	485759.451718	44.880308
3504.388125	485795.499187	44.885313
3504.311979	485759.693726	44.890317
3504.312800	485791.407568	44.895322
3504.270078	485764.867836	44.900327
3504.886765	485780.981993	44.905332
3504.107577	485784.398144	44.910337
3504.979411	485762.020066	44.915341
3504.687474	485759.938450	44.920346
3504.473280	485786.366846	44.925351
3504.477032	485806.073483	44.930356
3504.615621	485810.661764	44.935361
3504.621094	485810.103643	44.940365
3504.263152	485774.342748	44.945370
3504.564985	485739.693380	44.950375
3504.809367	485720.200798	44.955380
3504.502752	485727.747165	44.960385
3504.409851	485729.940305	44.965389
3504.415801	485737.487928	44.970394
3504.317500	485741.556391	44.975399
3504.316032	485746.470792	44.980404
3504.913651	485722.109554	44.985409
3504.779740	485730.945820	44.990413
3504.803740	485779.880882	44.995418
3504.375202	485780.455243	45.000423
3504.817995	485738.437710	45.005428
3504.443227	485718.080418	45.010433
3504.637576	485710.703811	45.015437
3504.851452	485698.967229	45.020442
3504.436652	485710.887587	45.025447
3504.418984	485745.390806	45.030452
3504.330694	485765.821291	45.035457
3504.574887	485748.507204	45.040461
3504.412786	485752.129796	45.045466
3504.570754	485757.626931	45.050471
3504.648374	485755.588228	45.055476
3504.475961	485743.304790	45.060481
3504.311741	485694.645140	45.065485
3504.587508	485698.857136	45.070490
3504.530665	485708.846444	45.075495
3504.289751	485674.232079	45.080500
3504.589925	485655.338553	45.085505
3504.802497	485680.889057	45.090509
3504.576374	485715.931891	45.095514
3504.465101	485732.718420	45.100519
3504.892521	485728.496649	45.105524
3504.414700	485735.006183	45.110529
3504.590381	485717.449589	45.115533
3504.395305	485730.044468	45.120538
3504.463692	485695.330593	45.125543
3504.828353	485651.248098	45.130548
3504.614773	485660.350296	45.135553
3505.079408	485643.254581	45.140557
3504.852334	485636.856462	45.145562
3504.674961	485683.797130	45.150567
3504.932046	485688.569357	45.155572
3504.808627	485678.355256	45.160577
3504.960372	485670.580075	45.165581
3504.776505	485663.668520	45.170586
3504.699066	485655.676248	45.175591
3504.832408	485655.604529	45.180596
3504.560734	485635.433502	45.185601
3504.616898	485619.871513	45.190605
3504.626860	485615.665036	45.195610
3504.678778	485623.560070	45.200615
3504.775199	485614.476407	45.205620
3504.749126	485630.185664	45.210625
3504.932634	485617.795230	45.215629
3504.908027	485602.904596	45.220634
3504.700583	485590.727921	45.225639
3504.774758	485540.307702	45.230644
3504.717672	485536.162467	45.235649
3504.541548	485559.140148	45.240653
3504.630123	485575.185962	45.245658
3504.793851	485508.894357	45.250663
3504.833617	485492.321618	45.255668
3504.434419	485527.898769	45.260673
3504.568688	485523.267330	45.265677
3504.565882	485530.208474	45.270682
3504.378942	485544.980650	45.275687
3504.580552	485549.305723	45.280692
3504.422869	485550.647871	45.285697
3504.494727	485561.123534	45.290701
3504.733642	485561.896379	45.295706
3504.352055	485539.260193	45.300711
3504.256007	485523.519537	45.305716
3504.412299	485514.527688	45.310721
3504.439815	485490.661560	45.315725
3504.313690	485471.936556	45.320730
3504.451316	485475.461165	45.325735
3504.681223	485458.351724	45.330740
3504.578099	485466.575300	45.335745
3504.728404	485479.267739	45.340749
3504.017732	485494.274717	45.345754
3504.765194	485476.830181	45.350759
3504.920448	485500.312840	45.355764
3504.403063	485514.427998	45.360769
3504.644204	485492.909221	45.365773
3505.022532	485479.829301	45.370778
3504.623951	485443.212958	45.375783
3504.821264	485447.741382	45.380788
3504.747890	485480.886002	45.385793
3504.552108	485490.137453	45.390797
3504.726902	485485.904896	45.395802
3504.455180	485489.139567	45.400807
3504.573529	485438.002830	45.405812
3504.336722	485429.326382	45.410817
3504.490855	485442.524863	45.415821
3504.515521	485449.461695	45.420826
3503.979087	485435.057123	45.425831
3504.271872	485444.383364	45.430836
3504.379782	485452.573591	45.435841
3504.555575	485466.376577	45.440845
3504.508087	485435.074908	45.445850
3504.812384	485400.475203	45.450855
3504.750088	485425.664191	45.455860
3504.330387	485439.966613	45.460865
3504.490308	485443.133070	45.465869
3504.485460	485441.816638	45.470874
3504.580488	485436.735420	45.475879
3505.190751	485410.243981	45.480884
3504.672685	485399.534821	45.485889
3504.746629	485414.417850	45.490893
3504.696001	485404.901370	45.495898
3504.686759	485373.036270	45.500903
3504.603497	485387.741517	45.505908
3504.548734	485416.019726	45.510913
3504.423476	485426.881252	45.515917
3504.473133	485421.807202	45.520922
3504.338940	485406.477776	45.525927
3504.841335	485353.608262	45.530932
3504.609246	485360.484382	45.535937
3504.468215	485397.135542	45.540941
3504.752607	485395.216106	45.545946
3504.518021	485402.092606	45.550951
3504.345692	485401.663900	45.555956
3504.524241	485406.245962	45.560961
3504.856029	485406.294864	45.565965
3504.715407	485391.878363	45.570970
3504.422999	485367.809336	45.575975
3504.250069	485344.329345	45.580980
3504.744847	485330.116346	45.585985
3504.819430	485324.481043	45.590989
3504.837566	485326.808667	45.595994
3504.532224	485319.814863	45.600999
3504.467047	485315.316221	45.606004
3504.410720	485373.080282	45.611009
3504.505316	485367.391167	45.616013
3504.174256	485352.700761	45.621018
3504.328848	485326.737188	45.626023
3504.319762	485370.308300	45.631028
3504.311848	485388.142702	45.636033
3504.364140	485357.635732	45.641037
3504.100856	485362.591612	45.646042
3504.371186	485346.032968	45.651047
3504.500831	485333.904177	45.656052
3504.671586	485386.870037	45.661057
3504.408071	485390.914024	45.666061
3504.207369	485379.242772	45.671066
3503.892736	485366.778923	45.676071
3504.849556	485347.426674	45.681076
3504.761848	485356.255809	45.686081
3504.315054	485342.242299	45.691085
3504.853462	485319.308459	45.696090
3504.883036	485315.656105	45.701095
3504.623437	485318.179613	45.706100
3504.536139	485359.179325	45.711105
3504.751935	485369.125719	45.716109
3504.535578	485352.795990	45.721114
3504.147502	485352.604031	45.726119
3505.030950	485308.844058	45.731124
3504.548949	485292.049638	45.736129
3504.553141	485302.890773	45.741133
3504.508155	485323.922832	45.746138
3504.207679	485345.501873	45.751143
3504.372326	485337.724518	45.756148
3504.256515	485322.290795	45.761153
3504.644172	485271.111051	45.766157
3504.367519	485293.800961	45.771162
3503.619877	485306.179475	45.776167
3504.495903	485307.712897	45.781172
3504.479867	485318.303909	45.786177
3504.729298	485339.086768	45.791181
3504.922354	485329.886373	45.796186
3504.873188	485333.288544	45.801191
3504.631929	485326.943226	45.806196
3504.604957	485324.465046	45.811201
3504.958057	485306.728050	45.816205
3504.911029	485289.864880	45.821210
3504.353780	485288.078457	45.826215
3504.230451	485275.837626	45.831220
3504.112970	485279.959880	45.836225
3504.459752	485270.532509	45.841229
3504.935281	485245.126053	45.846234
3504.530102	485270.217450	45.851239
3504.865563	485248.936807	45.856244
3505.244374	485235.755320	45.861249
3504.871759	485219.703488	45.866253
3504.868103	485209.014245	45.871258
3504.392226	485211.318637	45.876263
3504.603852	485247.762354	45.881268
3504.336082	485255.100114	45.886273
3504.654596	485214.722288	45.891277
3505.033287	485191.002936	45.896282
3504.904769	485176.533698	45.901287
3504.739374	485173.165446	45.906292
3504.360565	485187.309603	45.911297
3504.484302	485233.950461	45.916301
3504.408286	485241.460570	45.921306
3503.954813	485216.758196	45.926311
3504.600502	485196.492380	45.931316
3504.974661	485191.620295	45.936321
3504.569113	485187.631386	45.941325
3504.683073	485158.279599	45.946330
3503.794196	485180.965079	45.951335
3504.657252	485152.964111	45.956340
3504.414238	485142.971279	45.961345
3504.502349	485158.460221	45.966349
3504.564361	485164.935287	45.971354
3504.436357	485186.892548	45.976359
3504.410633	485202.703423	45.981364
3504.693372	485208.332983	45.986369
3504.315767	485191.015347	45.991373
3504.590575	485168.933597	45.996378
3504.712973	485158.325728	46.001383
3504.321860	485178.500719	46.006388
3504.172008	485196.357733	46.011393
3504.186906	485201.067034	46.016397
3504.199896	485191.641719	46.021402
3503.576216	485196.553277	46.026407
3504.352237	485182.498369	46.031412
3504.613901	485168.980713	46.036417
3504.315631	485205.505100	46.041421
3504.512131	485220.723548	46.046426
3504.246418	485212.963500	46.051431
3504.582366	485219.952541	46.056436
3504.318613	485225.617807	46.061441
3504.442837	485222.963730	46.066445
3504.901964	485210.428147	46.071450
3504.681190	485178.089531	46.076455
3504.662146	485150.987920	46.081460
3504.828416	485158.409104	46.086465
3504.515012	485146.603535	46.091469
3504.417037	485165.313647	46.096474
3504.257349	485169.695911	46.101479
3504.013772	485164.972116	46.106484
3504.247925	485165.391091	46.111489
3503.982277	485170.144742	46.116493
3504.289285	485159.811672	46.121498
3504.034789	485177.938556	46.126503
3504.686834	485183.357765	46.131508
3504.651633	485200.284723	46.136513
3504.843049	485158.254994	46.141517
3504.619094	485155.959915	46.146522
3504.431699	485178.990493	46.151527
3504.986263	485189.592716	46.156532
3504.754128	485207.260073	46.161537
3504.796196	485147.471288	46.166541
3504.842465	485151.314374	46.171546
3504.700473	485179.961357	46.176551
3504.850112	485162.763014	46.181556
3505.159101	485111.595282	46.186561
3505.170547	485088.744457	46.191565
3505.411359	485072.139581	46.196570
3504.929711	485083.817574	46.201575
3504.573420	485077.085049	46.206580
3504.622261	485078.293262	46.211585
3504.785677	485088.146754	46.216589
3504.916256	485087.214197	46.221594
3504.665499	485089.584349	46.226599
3504.438264	485093.521337	46.231604
3504.452682	485085.716963	46.236609
3504.694380	485031.823847	46.241613
3504.919245	485025.506084	46.246618
3505.122858	485004.094020	46.251623
3504.721404	485018.495196	46.256628
3504.532184	485020.956956	46.261633
3505.010688	485003.655831	46.266637
3505.402492	484964.481818	46.271642
3505.067839	484965.953303	46.276647
3505.018017	485007.555799	46.281652
3505.091059	484975.879691	46.286657
3504.638891	484936.585696	46.291661
3504.795252	484968.478962	46.296666
3504.714754	484947.466384	46.301671
3505.269636	484910.293024	46.306676
3504.946963	484896.766206	46.311681
3504.433699	484896.442037	46.316685
3504.584553	484932.895955	46.321690
3504.535312	484927.584088	46.326695
3504.549181	484901.692849	46.331700
3504.660286	484904.411138	46.336705
3504.432011	484911.185487	46.341709
3504.911542	484877.823739	46.346714
3504.638882	484889.418154	46.351719
3504.701797	484900.199571	46.356724
3504.666694	484899.951819	46.361729
3504.600143	484898.797093	46.366733
3504.952242	484875.638857	46.371738
3505.210888	484852.191382	46.376743
3504.968499	484850.709799	46.381748
3504.731993	484835.902727	46.386753
3505.002077	484806.475067	46.391757
3504.852752	484855.693187	46.396762
3504.119130	484826.018885	46.401767
3504.904861	484799.144230	46.406772
3504.776781	484836.351709	46.411777
3504.173432	484810.456573	46.416781
3504.626640	484788.599511	46.421786
3504.654488	484806.479462	46.426791
3504.791410	484818.009185	46.431796
3504.466969	484800.226821	46.436801
3504.619384	484784.496954	46.441805
3504.801548	484817.652989	46.446810
3504.810565	484806.049570	46.451815
3504.760453	484761.067987	46.456820
3505.155119	484752.240764	46.461825
3504.894373	484789.925276	46.466829
3504.761018	484755.038941	46.471834
3504.824647	484707.354066	46.476839
3504.839218	484704.362600	46.481844
3504.573405	484756.031261	46.486849
3504.336622	484721.465196	46.491853
3504.714084	484725.458677	46.496858
3504.425665	484722.464438	46.501863
3504.744906	484725.757824	46.506868
3504.318993	484717.313600	46.511873
3504.451910	484690.136660	46.516877
3504.667539	484711.685500	46.521882
3504.705092	484706.663839	46.526887
3504.675070	484681.691196	46.531892
3505.001607	484654.382276	46.536897
3504.727278	484661.569305	46.541901
3504.590680	484702.223553	46.546906
3504.111805	484693.939681	46.551911
3504.913501	484656.118854	46.556916
3504.702400	484641.915589	46.561921
3504.524950	484674.470071	46.566925
3504.410065	484655.742498	46.571930
3504.293328	484632.252758	46.576935
3504.743854	484622.656684	46.581940
3504.260763	484639.046951	46.586945
3503.806646	484654.419342	46.591949
3504.239430	484654.046971	46.596954
3504.320500	484668.220150	46.601959
3504.491831	484675.539393	46.606964
3504.694119	484669.377074	46.611969
3504.639347	484659.202246	46.616973
3504.738456	484688.926463	46.621978
3504.524832	484677.915462	46.626983
3504.080867	484653.312191	46.631988
3504.303033	484647.298716	46.636993
3504.651593	484650.942132	46.641997
3505.065144	484634.309579	46.647002
3504.628567	484616.798090	46.652007
3504.626801	484620.902195	46.657012
3504.714468	484628.234679	46.662017
3504.246861	484656.477923	46.667021
3504.725819	484654.882314	46.672026
3504.704493	484657.722897	46.677031
3504.752726	484644.086616	46.682036
3504.703592	484636.089447	46.687041
3504.589135	484624.910750	46.692045
3504.769099	484605.275233	46.697050
3504.435173	484609.431839	46.702055
3504.522049	484554.903229	46.707060
3504.708656	484547.274080	46.712065
3504.387330	484558.825720	46.717069
3504.430690	484602.390274	46.722074
3504.464469	484589.212218	46.727079
3504.736374	484592.969088	46.732084
3504.506350	484582.213947	46.737089
3504.412761	484604.369087	46.742093
3504.711317	484615.670727	46.747098
3504.382327	484599.104840	46.752103
3504.351902	484581.681119	46.757108
3504.774760	484552.836900	46.762113
3504.669508	484536.539583	46.767117
3504.699117	484520.220938	46.772122
3504.501401	484548.168360	46.777127
3504.633763	484564.714739	46.782132
3504.814013	484538.340737	46.787137
3504.595698	484573.536402	46.792141
3504.735393	484534.198707	46.797146
3504.706943	484512.518790	46.802151
3504.793897	484495.076440	46.807156
3504.772079	484542.805929	46.812161
3504.636274	484532.441184	46.817165
3504.778624	484507.998382	46.822170
3504.387173	484524.272934	46.827175
3504.471179	484501.207288	46.832180
3504.345590	484475.996160	46.837185
3504.562866	484479.913681	46.842189
3504.756226	484504.303494	46.847194
3504.615776	484488.366352	46.852199
3504.310584	484481.777536	46.857204
3504.573375	484481.685354	46.862209
3504.178987	484482.862328	46.867213
3504.327690	484472.756572	46.872218
3503.841656	484476.582595	46.877223
3504.194500	484483.822557	46.882228
3504.301371	484482.235078	46.887233
3503.936947	484491.614990	46.892237
3504.549100	484495.672755	46.897242
3504.535321	484514.826171	46.902247
3504.580556	484513.299101	46.907252
3504.351399	484508.167549	46.912257
3504.507331	484502.873802	46.917261
3504.469879	484497.357296	46.922266
3504.288736	484505.238959	46.927271
3504.550842	484488.528888	46.932276
3504.640730	484487.450741	46.937281
3504.361293	484511.205966	46.942285
3504.644653	484496.975107	46.947290
3504.959718	484475.696838	46.952295
3504.600081	484451.333305	46.957300
3505.110198	484447.300847	46.962305
3504.738838	484435.655997	46.967309
3504.887274	484425.955577	46.972314
3504.342574	484461.912339	46.977319
3504.485951	484480.686296	46.982324
3504.123998	484469.293303	46.987329
3504.053224	484454.358415	46.992333
3504.691523	484426.999899	46.997338
3504.704790	484431.658982	47.002343
3504.199337	484442.834474	47.007348
3504.422074	484458.657353	47.012353
3504.730058	484462.611206	47.017357
3504.567838	484426.056904	47.022362
3503.986785	484423.767512	47.027367
3504.542035	484414.408107	47.032372
3504.690604	484398.830530	47.037377
3504.560649	484392.213986	47.042381
3504.507368	484444.103213	47.047386
3504.305326	484441.399266	47.052391
3504.022002	484426.903269	47.057396
3503.464896	484429.321919	47.062401
3503.791033	484436.667450	47.067405
3504.292862	484459.691279	47.072410
3504.387800	484486.275253	47.077415
3504.527280	484487.621171	47.082420
3504.587291	484477.580100	47.087425
3504.124262	484459.160685	47.092429
3504.835047	484434.222630	47.097434
3504.657881	484443.015656	47.102439
3504.149823	484456.876784	47.107444
3505.077985	484414.728996	47.112449
3504.647902	484408.818537	47.117453
3504.720462	484423.905208	47.122458
3504.219932	484413.750040	47.127463
3504.350406	484408.561621	47.132468
3504.923956	484422.555812	47.137473
3504.491375	484410.971288	47.142477
3504.739104	484409.108216	47.147482
3504.203301	484401.947843	47.152487
3504.090923	484403.384239	47.157492
3504.751289	484397.453423	47.162497
3504.732187	484379.267757	47.167501
3505.098649	484416.955192	47.172506
3504.596761	484409.485473	47.177511
3504.266217	484407.257815	47.182516
3504.440847	484407.686215	47.187521
3504.182157	484407.575125	47.192525
3504.948983	484389.163921	47.197530
3504.401284	484425.881197	47.202535
3504.510504	484382.900144	47.207540
3504.781658	484351.850346	47.212545
3504.531625	484380.870243	47.217549
3504.727891	484396.444032	47.222554
3504.322411	484381.004675	47.227559
3504.202714	484373.981184	47.232564
3504.949656	484345.338759	47.237569
3504.774442	484364.416508	47.242573
3504.695284	484393.713369	47.247578
3504.806263	484358.787701	47.252583
3504.656255	484319.495358	47.257588
3504.623880	484361.147151	47.262593
3504.866677	484319.462135	47.267597
3504.899388	484354.567858	47.272602
3504.757411	484354.184995	47.277607
3504.627682	484332.723545	47.282612
3504.469774	484302.248133	47.287617
3504.542748	484335.624912	47.292621
3504.473309	484301.639628	47.297626
3504.881271	484289.060873	47.302631
3504.702930	484330.533142	47.307636
3504.502755	484309.234795	47.312641
3504.404255	484313.607580	47.317645
3504.692407	484312.295427	47.322650
3504.416111	484314.264387	47.327655
3504.112787	484313.045718	47.332660
3504.791426	484304.021414	47.337665
3504.976478	484269.742526	47.342669
3504.799008	484291.607290	47.347674
3504.500367	484305.992744	47.352679
3504.691296	484289.293751	47.357684
3504.724982	484268.059727	47.362689
3504.873391	484255.876631	47.367693
3504.597190	484265.901355	47.372698
3504.685278	484224.037925	47.377703
3504.398477	484261.474256	47.382708
3504.490194	484237.444438	47.387713
3503.886881	484235.462533	47.392717
3504.216566	484230.495908	47.397722
3504.757790	484217.794714	47.402727
3504.617464	484252.117325	47.407732
3504.443588	484233.854655	47.412737
3504.485519	484234.810686	47.417741
3505.112445	484214.597477	47.422746
3505.075687	484275.502976	47.427751
3504.482441	484227.363422	47.432756
3505.077626	484180.201220	47.437761
3504.481435	484225.438334	47.442765
3504.546111	484184.997149	47.447770
3504.754864	484176.604373	47.452775
3504.573859	484218.330630	47.457780
3505.051526	484172.656279	47.462785
3504.707122	484202.147348	47.467789
3504.887816	484148.616073	47.472794
3504.583435	484184.940689	47.477799
3504.045109	484169.623490	47.482804
3504.894796	484152.414937	47.487809
3504.955984	484138.066935	47.492813
3504.810263	484149.033742	47.497818
3504.652230	484138.925627	47.502823
3504.578816	484150.691655	47.507828
3504.675212	484156.148313	47.512833
3504.428797	484154.464650	47.517837
3504.899505	484131.945432	47.522842
3504.304649	484135.434061	47.527847
3504.659839	484113.895726	47.532852
3504.862557	484102.666596	47.537857
3504.696411	484088.455819	47.542861
3504.660021	484066.827325	47.547866
3504.407940	484084.448192	47.552871
3504.839634	484110.320802	47.557876
3504.850047	484123.086910	47.562881
3504.433011	484125.787452	47.567885
3504.633800	484119.371868	47.572890
3504.707678	484116.066944	47.577895
3504.462789	484069.189244	47.582900
3504.906411	484039.783658	47.587905
3504.799053	484032.352767	47.592909
3504.627558	484037.598470	47.597914
3504.330423	484061.053048	47.602919
3504.452257	484055.713903	47.607924
3504.107164	484052.829848	47.612929
3504.007078	484070.325373	47.617933
3504.396912	484055.570706	47.622938
3504.284913	484058.324377	47.627943
3504.095204	484057.746389	47.632948
3503.939244	484062.786967	47.637953
3504.411176	484066.157666	47.642957
3504.481937	484087.122109	47.647962
3504.184426	484096.643632	47.652967
3504.353208	484075.033385	47.657972
3504.736764	484037.632102	47.662977
3504.438858	484039.553840	47.667981
3504.691467	484048.583112	47.672986
3504.707232	484064.591023	47.677991
3504.775641	484040.564645	47.682996
3504.177724	484049.323018	47.688001
3504.334398	484075.695134	47.693005
3504.567867	484082.194129	47.698010
3504.459132	484055.409153	47.703015
3504.450517	484026.379019	47.708020
3504.327189	484019.811966	47.713025
3504.571805	484035.277072	47.718029
3504.549606	484005.387734	47.723034
3504.679795	484006.937818	47.728039
3504.560226	484013.593966	47.733044
3504.270677	484039.428668	47.738049
3504.332180	484054.872034	47.743053
3504.576682	484045.916228	47.748058
3504.268046	484074.185859	47.753063
3504.316111	484055.127955	47.758068
3504.778387	484046.644387	47.763073
3504.647840	484055.430220	47.768077
3504.675769	484068.142930	47.773082
3504.469896	484019.536308	47.778087
3504.513700	483982.340616	47.783092
3504.647631	484014.796325	47.788097
3504.255108	484045.308555	47.793101
3504.527363	484030.876448	47.798106
3504.461812	484040.817328	47.803111
3504.691838	484028.570524	47.808116
3504.828248	484032.044924	47.813121
3504.127267	484036.158335	47.818125
3504.660580	483995.085361	47.823130
3504.662940	483976.541263	47.828135
3504.422918	483980.936491	47.833140
3504.519811	483981.225190	47.838145
3504.445121	483979.159707	47.843149
3504.407789	483984.181557	47.848154
3504.451878	484005.200970	47.853159
3504.353472	483952.675920	47.858164
3504.925904	483949.444168	47.863169
3503.829884	483963.753239	47.868173
3504.149614	483975.761231	47.873178
3504.132391	483981.843888	47.878183
3504.249838	483997.025128	47.883188
3504.282535	484013.233069	47.888193
3504.097246	484027.398150	47.893197
3504.588571	483996.971643	47.898202
3504.730374	483960.115080	47.903207
3504.790701	483955.900282	47.908212
3504.286112	483973.966487	47.913217
3504.473022	483994.254015	47.918221
3504.465966	483979.258024	47.923226
3503.931210	483979.342561	47.928231
3504.252314	483976.657196	47.933236
3504.731400	483976.125499	47.938241
3504.858346	483947.276484	47.943245
3505.103373	483946.984444	47.948250
3504.733650	483951.146848	47.953255
3504.560945	483977.773821	47.958260
3504.947096	483982.475408	47.963265
3504.483728	483948.805096	47.968269
3504.963957	483921.318856	47.973274
3505.075089	483926.519919	47.978279
3504.696356	483908.390652	47.983284
3504.735165	483941.824175	47.988289
3504.418607	483951.196781	47.993293
3504.518509	483941.250459	47.998298
3504.936963	483939.259028	48.003303
3504.506556	483913.031358	48.008308
3504.733021	483899.873044	48.013313
3504.802326	483882.686263	48.018317
3504.481560	483873.211725	48.023322
3504.468941	483911.416056	48.028327
3504.672342	483899.781372	48.033332
3504.738123	483874.691214	48.038337
3504.749147	483854.372312	48.043341
3504.792278	483890.085224	48.048346
3504.667338	483888.483670	48.053351
3503.838069	483870.678907	48.058356
3504.698175	483859.751065	48.063361
3504.370943	483899.170470	48.068365
3504.429022	483854.220348	48.073370
3504.697032	483874.596516	48.078375
3504.299801	483863.056742	48.083380
3504.063299	483835.632994	48.088385
3504.337688	483837.514965	48.093389
3504.431815	483856.499977	48.098394
3504.167936	483889.474768	48.103399
3504.196027	483891.851657	48.108404
3503.761769	483868.309844	48.113409
3504.412656	483857.820399	48.118413
3504.511777	483841.490196	48.123418
3504.590207	483876.690890	48.128423
3504.526140	483897.626182	48.133428
3504.369152	483877.739188	48.138433
3504.892428	483847.459396	48.143437
3504.816306	483839.364832	48.148442
3504.967472	483853.274196	48.153447
3504.752075	483868.913474	48.158452
3504.820621	483843.417509	48.163457
3504.695013	483807.514916	48.168461
3504.927000	483784.729028	48.173466
3505.052365	483779.085251	48.178471
3504.578084	483777.082903	48.183476
3504.639434	483823.027690	48.188481
3504.209166	483841.994265	48.193485
3504.138702	483841.093426	48.198490
3504.639098	483805.750550	48.203495
3504.465680	483796.252685	48.208500
3504.439210	483828.328727	48.213505
3504.599354	483834.940727	48.218509
3504.655545	483797.894722	48.223514
3504.081873	483776.857488	48.228519
3504.925013	483754.430969	48.233524
3504.988605	483726.351638	48.238529
3504.662266	483744.237883	48.243533
3504.494067	483738.184493	48.248538
3504.822767	483722.729904	48.253543
3505.194979	483740.353744	48.258548
3504.918521	483717.344139	48.263553
3504.651461	483715.410366	48.268557
3504.670811	483706.439323	48.273562
3504.763922	483713.720626	48.278567
3504.587638	483699.105832	48.283572
3504.717987	483702.935917	48.288577
3504.289845	483723.726272	48.293581
3503.939091	483703.565725	48.298586
3504.547554	483681.682881	48.303591
3504.281696	483690.540932	48.308596
3504.296527	483730.666615	48.313601
3504.147351	483709.663549	48.318605
3504.546255	483713.957852	48.323610
3504.222829	483709.144987	48.328615
3504.715733	483679.477734	48.333620
3504.882052	483710.155497	48.338625
3504.399853	483717.629061	48.343629
3504.145058	483712.248016	48.348634
3504.724681	483679.831057	48.353639
3504.467140	483679.871779	48.358644
3504.274871	483689.478201	48.363649
3504.173132	483725.872980	48.368653
3504.498915	483723.034841	48.373658
3504.148470	483711.234248	48.378663
3504.063991	483708.866284	48.383668
3504.893566	483679.247152	48.388673
3503.460640	483719.095014	48.393677
3503.553878	483710.416294	48.398682
3503.976759	483719.368141	48.403687
3504.075599	483749.499174	48.408692
3504.641166	483764.863102	48.413697
3504.537892	483749.983475	48.418701
3505.024554	483725.991935	48.423706
3504.622061	483726.207568	48.428711
3504.584863	483695.712124	48.433716
3504.819145	483697.195114	48.438721
3504.745537	483742.046756	48.443725
3504.353783	483736.079365	48.448730
3504.519148	483698.205249	48.453735
3504.627994	483704.977401	48.458740
3504.545133	483724.750516	48.463745
3504.343887	483712.014342	48.468749
3504.248705	483708.837403	48.473754
3504.303114	483695.300811	48.478759
3504.196582	483690.402994	48.483764
3504.370961	483679.228766	48.488769
3504.031486	483691.797125	48.493773
3504.932413	483676.404057	48.498778
3504.535062	483660.000170	48.503783
3504.528831	483694.201240	48.508788
3504.406913	483695.588528	48.513793
3504.848101	483673.022779	48.518797
3504.888965	483668.658994	48.523802
3504.656941	483723.365071	48.528807
3504.240844	483695.006845	48.533812
3505.054673	483669.696858	48.538817
3504.642604	483693.879379	48.543821
3504.470217	483650.029211	48.548826
3504.954308	483634.347325	48.553831
3504.566175	483678.387488	48.558836
3505.028055	483680.594508	48.563841
3504.739569	483672.026771	48.568845
3503.997561	483636.778620	48.573850
3505.039696	483602.920426	48.578855
3504.587612	483617.735977	48.583860
3504.629964	483634.449377	48.588865
3504.637724	483649.344224	48.593869
3504.325092	483619.348195	48.598874
3504.702373	483604.696505	48.603879
3504.493423	483642.729727	48.608884
3504.504623	483647.997326	48.613889
3504.448393	483658.950266	48.618893
3504.360471	483632.161417	48.623898
3504.332031	483624.971230	48.628903
3503.841495	483637.512832	48.633908
3503.945731	483631.720351	48.638913
3504.076321	483632.662399	48.643917
3504.551753	483599.197769	48.648922
3504.455007	483648.207975	48.653927
3504.346398	483664.742542	48.658932
3504.305873	483662.620959	48.663937
3503.932968	483668.455930	48.668941
3504.189766	483656.001992	48.673946
3504.231671	483648.800696	48.678951
3504.066846	483638.896062	48.683956
3503.665350	483634.450185	48.688961
3504.349732	483624.917992	48.693965
3504.529938	483608.068109	48.698970
3504.314060	483640.833066	48.703975
3504.099115	483621.106970	48.708980
3504.007446	483629.633516	48.713985
3503.849061	483656.005332	48.718989
3504.307525	483681.671616	48.723994
3504.848891	483683.258072	48.728999
3504.446960	483644.156178	48.734004
3504.517938	483635.784945	48.739009
3504.597007	483639.116479	48.744013
3503.914517	483640.440370	48.749018
3503.916947	483650.168039	48.754023
3504.559819	483665.063826	48.759028
3504.377239	483675.124725	48.764033
3504.182774	483689.950169	48.769037
3504.211828	483693.390932	48.774042
3504.453412	483691.376765	48.779047
3504.177375	483702.415087	48.784052
3504.254529	483688.469563	48.789057
3504.171995	483693.245298	48.794061
3504.476021	483688.687924	48.799066
3504.528382	483699.066344	48.804071
3504.560860	483716.237235	48.809076
3504.821565	483665.073315	48.814081
3504.869274	483654.121761	48.819085
3504.939930	483659.481294	48.824090
3505.043265	483672.081011	48.829095
3504.883382	483657.210260	48.834100
3504.945106	483601.061606	48.839105
3504.499820	483620.081437	48.844109
3504.513859	483616.633885	48.849114
3504.483159	483602.148009	48.854119
3504.591475	483631.163054	48.859124
3504.958026	483607.545021	48.864129
3504.559361	483602.592020	48.869133
3504.146362	483602.961315	48.874138
3504.868658	483616.071243	48.879143
3504.580704	483555.620370	48.884148
3504.749572	483538.924219	48.889153
3504.959735	483544.160401	48.894157
3504.743788	483554.327969	48.899162
3504.360863	483564.623257	48.904167
3504.266640	483563.776827	48.909172
3504.219815	483563.632244	48.914177
3504.553654	483590.838358	48.919181
3505.147434	483551.477569	48.924186
3504.775653	483559.389745	48.929191
3504.711969	483528.036884	48.934196
3504.260766	483543.409690	48.939201
3504.390064	483565.226786	48.944205
3504.669962	483521.558179	48.949210
3504.823344	483511.299183	48.954215
3504.171784	483548.997206	48.959220
3504.725457	483543.285665	48.964225
3504.681038	483557.783492	48.969229
3504.591959	483568.691008	48.974234
3504.907356	483529.880844	48.979239
3504.943208	483485.186718	48.984244
3504.285816	483512.802944	48.989249
3504.327841	483533.164521	48.994253
3504.848847	483469.748162	48.999258
3505.262331	483470.240167	49.004263
3504.086382	483477.012795	49.009268
3504.486162	483471.781562	49.014273
3504.529775	483455.054470	49.019277
3504.341193	483462.228387	49.024282
3504.850758	483481.097437	49.029287
3504.443830	483465.961582	49.034292
3504.795485	483434.644260	49.039297
3503.900690	483461.892741	49.044301
3503.768359	483460.140317	49.049306
3503.934726	483461.735394	49.054311
3504.216095	483473.851096	49.059316
3504.809386	483476.848047	49.064321
3504.730140	483484.207345	49.069325
3504.672088	483480.264490	49.074330
3504.895852	483474.351736	49.079335
3504.927900	483455.599780	49.084340
3504.797741	483439.204143	49.089345
3504.576569	483448.460579	49.094349
3504.846676	483439.804452	49.099354
3504.707592	483400.356519	49.104359
3504.827748	483411.433722	49.109364
3504.458269	483429.732413	49.114369
3504.852529	483445.478343	49.119373
3504.222822	483439.345800	49.124378
3504.547828	483393.541745	49.129383
3504.777351	483359.355558	49.134388
3505.232347	483352.443536	49.139393
3504.894797	483343.174061	49.144397
3504.965624	483347.013624	49.149402
3504.887777	483325.137518	49.154407
3504.549006	483324.025723	49.159412
3504.833249	483303.409723	49.164417
3505.070955	483324.297936	49.169421
3504.675645	483310.477482	49.174426
3504.704649	483290.661827	49.179431
3504.620675	483286.267020	49.184436
3504.546966	483325.596848	49.189441
3504.319061	483343.163896	49.194445
3504.488913	483331.280838	49.199450
3504.781275	483330.525299	49.204455
3504.302656	483338.251780	49.209460
3504.730116	483330.178746	49.214465
3504.557450	483331.523413	49.219469
3504.714664	483326.178477	49.224474
3504.673765	483297.507030	49.229479
3504.742740	483279.559753	49.234484
3504.701502	483241.312060	49.239489
3504.828743	483237.238534	49.244493
3504.198378	483263.634811	49.249498
3504.448440	483277.782296	49.254503
3504.363579	483286.713258	49.259508
3504.345905	483275.822492	49.264513
3504.350772	483271.768315	49.269517
3504.437497	483276.112058	49.274522
3504.820288	483296.622694	49.279527
3504.657296	483292.139042	49.284532
3504.890406	483226.031333	49.289537
3504.736771	483221.242178	49.294541
3503.985696	483230.633138	49.299546
3504.315205	483217.103402	49.304551
3503.981174	483223.945720	49.309556
3504.238598	483231.353238	49.314561
3504.433109	483230.663829	49.319565
3504.492281	483240.180062	49.324570
3504.898805	483258.153593	49.329575
3504.295813	483272.081235	49.334580
3504.493328	483269.364640	49.339585
3504.486637	483272.101778	49.344589
3504.618738	483245.530960	49.349594
3504.822902	483205.623038	49.354599
3504.495901	483257.305356	49.359604
3504.597481	483254.907929	49.364609
3504.378899	483260.870634	49.369613
3504.194597	483250.208861	49.374618
3504.299889	483247.861514	49.379623
3504.287614	483264.735870	49.384628
3504.855915	483261.453992	49.389633
3504.748152	483255.897577	49.394637
3504.507426	483238.657893	49.399642
3504.482450	483231.264342	49.404647
3504.397541	483245.312790	49.409652
3504.313657	483238.891243	49.414657
3504.134499	483245.658407	49.419661
3504.179733	483232.781627	49.424666
3504.294219	483229.115458	49.429671
3504.306671	483216.091845	49.434676
3504.244076	483182.458196	49.439681
3504.290072	483176.624117	49.444685
3504.040695	483204.024287	49.449690
3504.081125	483211.668781	49.454695
3503.961531	483221.517286	49.459700
3504.252384	483241.333161	49.464705
3504.282178	483253.742101	49.469709
3503.684818	483255.356569	49.474714
3504.372367	483226.519217	49.479719
3504.329140	483220.293909	49.484724
3504.673328	483249.474915	49.489729
3504.433907	483288.273663	49.494733
3504.221647	483284.659148	49.499738
3504.604318	483247.965838	49.504743
3504.538354	483245.290883	49.509748
3504.330987	483271.468290	49.514753
3504.090681	483241.612250	49.519757
3504.266696	483246.245894	49.524762
3504.812995	483228.375130	49.529767
3504.344083	483224.547829	49.534772
3504.388640	483209.543086	49.539777
3504.360005	483218.414525	49.544781
3504.295902	483257.692304	49.549786
3504.354080	483242.229423	49.554791
3504.122494	483225.646966	49.559796
3504.887681	483202.776124	49.564801
3504.942395	483228.506821	49.569805
3504.611240	483253.690458	49.574810
3504.100251	483239.837570	49.579815
3504.060444	483242.934621	49.584820
3504.266654	483238.392603	49.589825
3504.570417	483227.299002	49.594829
3504.560971	483215.292208	49.599834
3504.528714	483250.460862	49.604839
3504.617650	483250.193484	49.609844
3504.071084	483241.058331	49.614849
3503.830881	483239.424273	49.619853
3504.511066	483229.943220	49.624858
3505.088547	483219.059693	49.629863
3504.452244	483236.792721	49.634868
3503.706162	483241.774778	49.639873
3504.143781	483249.204476	49.644877
3504.195821	483255.023074	49.649882
3504.282814	483258.961435	49.654887
3504.365358	483269.639321	49.659892
3504.082193	483270.038768	49.664897
3504.500696	483267.337913	49.669901
3504.354695	483248.461895	49.674906
3504.536398	483214.840359	49.679911
3504.159267	483271.850698	49.684916
3504.580235	483291.899295	49.689921
3504.530641	483270.728012	49.694925
3503.930856	483258.358538	49.699930
3504.692343	483260.011575	49.704935
3504.698193	483284.736565	49.709940
3504.635799	483262.148597	49.714945
3504.403830	483256.865153	49.719949
3504.406704	483233.760158	49.724954
3505.079992	483191.852681	49.729959
3504.478556	483202.790712	49.734964
3504.545913	483226.391358	49.739969
3504.762922	483247.738935	49.744973
3504.571024	483249.846666	49.749978
3504.447354	483234.969868	49.754983
3503.870512	483228.828902	49.759988
3504.803902	483202.080711	49.764993
3504.475597	483203.399318	49.769997
3504.746313	483237.962761	49.775002
3504.701380	483234.321790	49.780007
3504.291366	483233.322585	49.785012
3504.284629	483211.536449	49.790017
3504.867416	483196.395960	49.795021
3504.419924	483183.445019	49.800026
3504.562276	483170.350176	49.805031
3504.892902	483174.047375	49.810036
3504.932642	483201.655193	49.815041
3504.650714	483211.529360	49.820045
3504.462482	483183.489048	49.825050
3504.777979	483138.851264	49.830055
3504.269512	483110.456115	49.835060
3504.521052	483108.490982	49.840065
3504.796247	483102.215309	49.845069
3504.588309	483112.229837	49.850074
3504.875591	483123.584799	49.855079
3504.636180	483147.234026	49.860084
3504.582134	483128.394026	49.865089
3504.705286	483110.336693	49.870093
3504.639251	483092.005236	49.875098
3504.611521	483081.217287	49.880103
3504.471999	483101.709346	49.885108
3504.570719	483126.977208	49.890113
3504.604485	483130.214653	49.895117
3504.444225	483131.050691	49.900122
3504.571142	483118.008920	49.905127
3503.913612	483113.046039	49.910132
3504.599137	483087.907583	49.915137
3504.400282	483089.205738	49.920141
3504.115871	483135.004126	49.925146
3504.711495	483136.987398	49.930151
3504.357546	483133.648590	49.935156
3504.375127	483120.421429	49.940161
3504.686272	483083.637778	49.945165
3505.039496	483068.229463	49.950170
3504.936163	483050.917229	49.955175
3504.547581	483042.669044	49.960180
3504.710780	483080.593876	49.965185
3504.378184	483097.873682	49.970189
3503.920574	483072.510535	49.975194
3505.081602	483049.576951	49.980199
3504.689855	483070.716928	49.985204
3504.327845	483039.866447	49.990209
3504.777608	483004.935471	49.995213
3504.673800	483007.890669	50.000218
3504.379843	483009.507871	50.005223
3504.326446	483036.978638	50.010228
3504.436128	483048.159040	50.015233
3504.330075	483038.751494	50.020237
3504.059306	483070.816727	50.025242
3504.094246	483065.339040	50.030247
3504.285446	483069.666317	50.035252
3504.051377	483042.342402	50.040257
3504.921834	483009.422347	50.045261
3504.149479	483019.526130	50.050266
3504.434123	483067.666822	50.055271
3504.213296	483049.917142	50.060276
3504.316948	483033.028192	50.065281
3504.793479	483017.448343	50.070285
3504.538040	483050.879235	50.075290
3504.630162	483065.963869	50.080295
3504.338103	483067.226087	50.085300
3504.500031	483032.036642	50.090305
3504.788765	483036.145837	50.095309
3504.564131	483068.305119	50.100314
3504.674532	483049.388383	50.105319
3504.255843	483025.589745	50.110324
3504.143606	483018.615252	50.115329
3504.039910	483017.618290	50.120333
3503.840915	483027.327437	50.125338
3504.664672	483010.932675	50.130343
3504.471689	483072.069310	50.135348
3504.353613	483063.221027	50.140353
3504.369480	483043.761875	50.145357
3503.983141	483049.143138	50.150362
3504.249108	483066.936387	50.155367
3503.889063	483070.945442	50.160372
3503.920974	483059.337362	50.165377
3504.569123	483044.794445	50.170381
3504.030551	483087.238332	50.175386
3504.270248	483052.137968	50.180391
3504.241698	483065.924296	50.185396
3503.953227	483081.930433	50.190401
3503.821817	483055.451673	50.195405
3504.055312	483040.467607	50.200410
3504.199896	483032.185817	50.205415
3504.152608	483095.174084	50.210420
3504.523095	483097.750296	50.215425
3504.769783	483057.734014	50.220429
3504.065737	483092.350443	50.225434
3504.623687	483092.768958	50.230439
3504.244618	483065.062647	50.235444
3504.512077	483038.976837	50.240449
3504.494820	483080.426312	50.245453
3504.252520	483078.184551	50.250458
3504.915810	483044.486605	50.255463
3504.372937	483082.725702	50.260468
3504.285782	483084.411549	50.265473
3504.398856	483074.057357	50.270477
3503.858461	483078.905608	50.275482
3504.850388	483047.334463	50.280487
3504.760085	483043.700627	50.285492
3504.685404	483073.150775	50.290497
3504.719332	483101.367674	50.295501
3504.668095	483078.271047	50.300506
3504.268756	483035.874079	50.305511
3504.672943	483026.487219	50.310516
3504.183756	483033.202121	50.315521
3504.263479	483040.587129	50.320525
3503.600571	483053.865706	50.325530
3504.168855	483055.650635	50.330535
3504.628639	483044.633609	50.335540
3504.934788	483043.166523	50.340545
3504.800110	483023.528471	50.345549
3504.698078	483005.506632	50.350554
3505.050875	482999.573340	50.355559
3504.261161	483030.301942	50.360564
3504.402252	483073.347795	50.365569
3504.517254	483063.854654	50.370573
3504.189188	483063.551845	50.375578
3504.444283	483041.065446	50.380583
3504.528662	483033.198520	50.385588
3504.202485	483059.040311	50.390593
3504.673194	483029.578251	50.395597
3504.305740	483073.819186	50.400602
3504.735435	483040.918179	50.405607
3504.075823	483013.256135	50.410612
3504.341405	482985.599827	50.415617
3504.551798	483014.447652	50.420621
3504.227150	482995.092940	50.425626
3504.159106	483009.442904	50.430631
3504.033745	483044.423971	50.435636
3503.810370	483033.058898	50.440641
3504.698412	483015.741948	50.445645
3504.258858	483033.646737	50.450650
3504.469728	483070.601353	50.455655
3504.320328	483092.817706	50.460660
3504.399682	483066.710996	50.465665
3505.108293	483015.423910	50.470669
3504.507903	483027.932596	50.475674
3504.530892	483038.670690	50.480679
3504.541142	483009.433382	50.485684
3504.844496	483001.481165	50.490689
3504.744390	482996.936837	50.495693
3504.681279	483038.494985	50.500698
3504.854398	483025.445850	50.505703
3504.226519	482986.277008	50.510708
3504.768751	482952.496700	50.515713
3505.042428	482987.617474	50.520717
3504.335465	482976.835485	50.525722
3504.365437	482973.841319	50.530727
3504.219503	482954.863669	50.535732
3504.618585	482914.113645	50.540737
3504.935591	482877.278010	50.545741
3504.408560	482825.932379	50.550746
3504.358441	482773.396514	50.555751
3504.105560	482739.893516	50.560756
3503.772996	482694.698445	50.565761
3503.700454	482583.439781	50.570765
3504.058173	482492.481768	50.575770
3503.923832	482380.268989	50.580775
3503.893092	482259.273205	50.585780
3503.500000	482143.096996	50.590785
3503.172296	482053.968085	50.595789
3502.659894	481928.131297	50.600794
3502.902375	481748.817088	50.605799
3503.029305	481588.825616	50.610804
3502.250045	481443.569769	50.615809
3502.037126	481309.168686	50.620813
3501.477876	481106.767130	50.625818
3501.973747	480903.588638	50.630823
3501.094166	480760.269209	50.635828
3500.848364	480567.237988	50.640833
3500.813657	480340.016326	50.645837
3500.584489	480130.610048	50.650842
3500.170015	479951.636699	50.655847
3499.413127	479712.613019	50.660852
3499.423861	479469.512273	50.665857
3499.115812	479269.282005	50.670861
3498.286335	479035.582843	50.675866
3498.292000	478759.178254	50.680871
3498.000017	478561.725692	50.685876
3497.480563	478317.985153	50.690881
3497.329467	478038.858608	50.695885
3496.466748	477763.489743	50.700890
3496.319608	477499.813041	50.705895
3496.004551	477232.662263	50.710900
3495.343775	476947.062913	50.715905
3494.821987	476681.660738	50.720909
3494.509202	476374.507933	50.725914
3493.873429	476132.381150	50.730919
3493.077629	475842.681904	50.735924
3493.097774	475516.607924	50.740929
3492.679743	475246.608592	50.745933
3491.507694	474946.919709	50.750938
3490.961437	474631.616406	50.755943
3490.913098	474319.777856	50.760948
3490.234942	473998.149261	50.765953
3489.933789	473716.908343	50.770957
3489.036758	473434.997347	50.775962
3488.893383	473101.965619	50.780967
3488.026558	472781.868522	50.785972
3487.769489	472460.960322	50.790977
3487.487435	472140.710112	50.795981
3486.207380	471800.486038	50.800986
3486.111483	471440.297081	50.805991
3485.881040	471113.736261	50.810996
3484.906211	470804.120119	50.816001
3484.596936	470434.973634	50.821005
3483.858908	470143.612965	50.826010
3483.023460	469793.703194	50.831015
3482.300948	469444.175319	50.836020
3481.691963	469087.829391	50.841025
3481.367095	468746.745184	50.846029
3480.286564	468423.977995	50.851034
3479.971256	468075.985488	50.856039
3479.631367	467723.630334	50.861044
3478.691998	467374.254382	50.866049
3478.246330	467025.200280	50.871053
3477.389074	466644.106498	50.876058
3477.328481	466256.946843	50.881063
3476.063934	465904.149746	50.886068
3475.941515	465558.975903	50.891073
3475.455038	465191.083993	50.896077
3474.135571	464837.060816	50.901082
3473.661890	464521.035335	50.906087
3473.006674	464140.270585	50.911092
3472.399727	463794.181293	50.916097
3471.272034	463442.792760	50.921101
3470.792262	463067.306580	50.926106
3471.087159	462678.656724	50.931111
3469.838275	462318.646891	50.936116
3469.300650	461997.421162	50.941121
3468.779475	461627.952317	50.946125
3468.185185	461229.323584	50.951130
3467.444245	460868.195030	50.956135
3466.791024	460534.285292	50.961140
3465.659031	460154.844802	50.966145
3465.626349	459765.789049	50.971149
3464.354664	459410.807463	50.976154
3464.100097	459006.200400	50.981159
3462.776477	458694.637963	50.986164
3461.991461	458340.475354	50.991169
3461.842789	457960.131498	50.996173
3461.024070	457576.995418	51.001178
3460.112318	457204.977620	51.006183
3459.841530	456890.534713	51.011188
3458.909014	456497.048749	51.016193
3458.940891	456105.382051	51.021197
3457.756104	455730.440361	51.026202
3457.213134	455399.784497	51.031207
3455.994990	455024.988547	51.036212
3455.643118	454642.438880	51.041217
3455.283067	454283.629402	51.046221
3453.911639	453957.700576	51.051226
3453.288095	453595.370178	51.056231
3452.663127	453225.118764	51.061236
3452.104065	452831.915947	51.066241
3451.512267	452505.335716	51.071245
3450.476325	452120.568481	51.076250
3450.039896	451765.334257	51.081255
3449.106278	451407.077748	51.086260
3448.394290	451050.861191	51.091265
3447.962756	450684.445641	51.096269
3447.288001	450310.907466	51.101274
3446.235870	449993.600358	51.106279
3445.754198	449616.823424	51.111284
3445.379758	449238.297987	51.116289
3444.523530	448871.261295	51.121293
3443.628031	448568.779750	51.126298
3443.006632	448191.342193	51.131303
3442.426700	447812.217204	51.136308
3441.770155	447485.525938	51.141313
3441.474982	447129.995770	51.146317
3440.159206	446754.066088	51.151322
3439.949779	446378.919899	51.156327
3438.840318	446062.888446	51.161332
3438.214973	445688.964516	51.166337
3437.633143	445308.987713	51.171341
3436.847766	444948.782009	51.176346
3435.674210	444624.671107	51.181351
3435.396856	444248.487040	51.186356
3434.499182	443913.511122	51.191361
3433.896804	443565.336740	51.196365
3433.322768	443191.873444	51.201370
3432.767251	442871.651476	51.206375
3432.452406	442488.643774	51.211380
3430.902673	442165.523874	51.216385
3430.714424	441783.551119	51.221389
3429.441173	441466.926925	51.226394
3429.322997	441071.428349	51.231399
3428.415802	440752.858709	51.236404
3427.461097	440402.308817	51.241409
3427.269247	440050.389513	51.246413
3426.206395	439700.506737	51.251418
3425.482214	439376.915022	51.256423
3425.077879	439011.712853	51.261428
3424.272695	438686.728761	51.266433
3423.815861	438304.668467	51.271437
3422.934744	437983.215866	51.276442
3422.473427	437616.783741	51.281447
3421.788211	437299.734071	51.286452
3420.722146	436919.526060	51.291457
3420.055301	436609.319383	51.296461
3419.279085	436241.139868	51.301466
3418.335698	435928.404354	51.306471
3417.600650	435576.634955	51.311476
3417.156717	435214.785966	51.316481
3416.358901	434914.658732	51.321485
3415.329921	434575.388165	51.326490
3415.465052	434206.984343	51.331495
3414.731619	433901.325382	51.336500
3413.578861	433554.926163	51.341505
3412.962766	433228.394831	51.346509
3411.981139	432891.151199	51.351514
3411.688720	432545.516495	51.356519
3410.925706	432211.631938	51.361524
3410.279195	431878.918111	51.366529
3409.767401	431560.728757	51.371533
3408.538061	431198.769789	51.376538
3407.826928	430893.427308	51.381543
3407.708965	430551.268237	51.386548
3406.976433	430212.833214	51.391553
3405.716840	429902.436321	51.396557
3404.751581	429562.556862	51.401562
3404.253008	429212.415860	51.406567
3403.492805	428952.490202	51.411572
3402.971112	428607.779445	51.416577
3402.950219	428264.102460	51.421581
3401.762413	427964.718720	51.426586
3401.255713	427613.059566	51.431591
3400.439178	427306.219366	51.436596
3399.900772	426967.331333	51.441601
3399.387878	426676.105939	51.446605
3398.365738	426314.149125	51.451610
3397.856327	425985.530234	51.456615
3397.162507	425678.652086	51.461620
3396.382006	425341.839185	51.466625
3395.785904	425026.150278	51.471629
3395.096570	424670.290835	51.476634
3394.077995	424393.090459	51.481639
3393.355179	424050.181988	51.486644
3392.894382	423734.888564	51.491649
3392.176834	423399.133961	51.496653
3391.371821	423104.563689	51.501658
3390.849967	422763.995073	51.506663
3389.655164	422466.609308	51.511668
3389.280531	422121.589684	51.516673
3388.627461	421835.593031	51.521677
3387.587654	421510.027214	51.526682
3387.184073	421185.576322	51.531687
3386.582696	420884.904517	51.536692
3386.052151	420558.180180	51.541697
3385.242690	420259.719234	51.546701
3384.824621	419911.884845	51.551706
3383.571250	419632.794191	51.556711
3383.314399	419317.240698	51.561716
3382.387205	418981.135860	51.566721
3382.123597	418695.985647	51.571725
3381.190749	418359.645710	51.576730
3380.367384	418059.639477	51.581735
3379.961295	417718.889806	51.586740
3378.783934	417443.144591	51.591745
3378.439835	417103.597286	51.596749
3378.167021	416794.624030	51.601754
3376.979335	416496.132630	51.606759
3376.405799	416150.233305	51.611764
3375.956123	415873.036854	51.616769
3375.489413	415549.217735	51.621773
3374.030189	415226.949371	51.626778
3374.018609	414898.858778	51.631783
3373.254351	414598.832680	51.636788
3372.182796	414327.919500	51.641793
3371.477702	413987.401936	51.646797
3370.927899	413669.215915	51.651802
3370.082113	413403.314938	51.656807
3369.724861	413061.715313	51.661812
3368.715377	412776.802758	51.666817
3368.328121	412449.811513	51.671821
3367.604535	412129.171647	51.676826
3366.926154	411855.937545	51.681831
3366.187060	411507.163823	51.686836
3365.452440	411203.896879	51.691841
3365.150770	410926.757644	51.696845
3364.214380	410592.260321	51.701850
3363.858370	410289.762892	51.706855
3362.940185	409993.831453	51.711860
3362.075240	409656.923737	51.716865
3361.880218	409344.810901	51.721869
3360.718027	409061.513704	51.726874
3360.514166	408720.602908	51.731879
3359.834844	408421.162209	51.736884
3358.817436	408145.889736	51.741889
3358.372237	407797.814746	51.746893
3357.357541	407525.382670	51.751898
3356.701869	407198.961763	51.756903
3356.371336	406874.290456	51.761908
3355.262446	406597.239608	51.766913
3355.077282	406255.739497	51.771917
3353.833456	405993.597998	51.776922
3352.984303	405679.492864	51.781927
3352.724362	405341.095315	51.786932
3352.061039	405082.997224	51.791937
3351.077686	404753.095110	51.796941
3350.496680	404481.127051	51.801946
3349.934718	404158.268788	51.806951
3349.105399	403872.101222	51.811956
3348.495331	403552.243638	51.816961
3348.077467	403273.046274	51.821965
3347.206499	402951.139662	51.826970
3346.570342	402673.979606	51.831975
3346.106584	402342.165637	51.836980
3344.900399	402068.496567	51.841985
3344.638135	401736.186956	51.846989
3343.722633	401461.653370	51.851994
3343.522526	401151.671369	51.856999
3342.956009	400834.525168	51.862004
3341.412251	400554.770550	51.867009
3341.188796	400228.540147	51.872013
3340.317198	399958.689665	51.877018
3339.840577	399643.271689	51.882023
3339.074198	399343.733678	51.887028
3338.439108	399073.228428	51.892033
3337.630585	398745.626828	51.897037
3337.038486	398474.855672	51.902042
3336.579453	398156.115922	51.907047
3336.071550	397856.015146	51.912052
3334.917749	397573.046667	51.917057
3334.389537	397249.580670	51.922061
3333.598844	396982.540477	51.927066
3333.119657	396666.662472	51.932071
3332.434152	396368.711987	51.937076
3331.477285	396090.911614	51.942081
3330.909884	395765.149466	51.947085
3330.228638	395499.809040	51.952090
3329.450842	395189.354304	51.957095
3328.912523	394916.512086	51.962100
3328.024697	394610.340745	51.967105
3327.925566	394296.668807	51.972109
3326.739248	394039.812471	51.977114
3326.171812	393729.260394	51.982119
3325.638264	393429.073677	51.987124
3324.474025	393155.172335	51.992129
3324.314933	392844.217214	51.997133
3323.515923	392571.016282	52.002138
3322.327320	392274.253970	52.007143
3322.033913	391954.641857	52.012148
3321.258826	391716.366242	52.017153
3320.540357	391397.350230	52.022157
3320.378051	391098.839225	52.027162
3319.455270	390834.416649	52.032167
3319.135590	390514.337941	52.037172
3318.208708	390256.777098	52.042177
3317.376574	389929.959581	52.047181
3316.870648	389642.144917	52.052186
3315.342138	389380.782407	52.057191
3315.529841	389045.556801	52.062196
3314.580321	388814.790706	52.067201
3313.828817	388502.467151	52.072205
3313.254085	388189.248355	52.077210
3312.478377	387944.463248	52.082215
3312.001846	387630.410366	52.087220
3311.204446	387359.330724	52.092225
3310.520884	387058.681631	52.097229
3309.917264	386786.117595	52.102234
3309.096609	386500.565596	52.107239
3309.039399	386211.584696	52.112244
3307.924796	385945.859733	52.117249
3307.362813	385630.379144	52.122253
3306.554195	385356.209396	52.127258
3305.475334	385060.921619	52.132263
3305.408949	384756.265220	52.137268
3304.293404	384517.207724	52.142273
3303.863762	384195.132722	52.147277
3302.997410	383902.726857	52.152282
3302.363856	383665.520549	52.157287
3302.102780	383370.700516	52.162292
3301.258802	383101.072274	52.167297
3300.632014	382792.572025	52.172301
3300.361863	382469.338074	52.177306
3299.360770	382218.726832	52.182311
3298.874539	381899.973037	52.187316
3298.115735	381638.561393	52.192321
3297.450974	381336.642695	52.197325
3296.895103	381025.853422	52.202330
3295.837733	380771.808089	52.207335
3295.179389	380465.227149	52.212340
3294.861609	380151.875238	52.217345
3294.042749	379910.376621	52.222349
3293.275337	379595.972243	52.227354
3292.390009	379335.607955	52.232359
3291.965575	379031.547731	52.237364
3290.976773	378749.219928	52.242369
3290.566300	378468.706313	52.247373
3290.049739	378197.873071	52.252378
3289.083661	377908.210204	52.257383
3288.873087	377615.627780	52.262388
3287.897963	377356.053230	52.267393
3287.706621	377031.820789	52.272397
3286.434615	376778.979254	52.277402
3286.041402	376462.277964	52.282407
3285.214527	376168.205413	52.287412
3284.153225	375926.593823	52.292417
3283.803763	375610.336839	52.297421
3283.406884	375344.527539	52.302426
3282.183779	375066.764283	52.307431
3281.746802	374755.983648	52.312436
3280.985480	374500.477991	52.317441
3280.515511	374196.897328	52.322445
3279.877896	373917.609195	52.327450
3279.078219	373635.902714	52.332455
3278.529832	373376.260847	52.337460
3277.672729	373084.028088	52.342465
3277.225299	372795.417166	52.347469
3276.645291	372520.765941	52.352474
3275.785416	372238.423608	52.357479
3275.218447	371942.143047	52.362484
3274.702900	371664.245236	52.367489
3273.765475	371375.447724	52.372493
3273.113186	371097.695044	52.377498
3272.311554	370820.294906	52.382503
3271.772263	370528.681161	52.387508
3270.713778	370270.423861	52.392513
3270.248125	369978.642106	52.397517
3269.720485	369700.860700	52.402522
3269.052683	369417.706175	52.407527
3268.349528	369137.150410	52.412532
3267.510071	368860.481496	52.417537
3266.895365	368578.712415	52.422541
3266.508255	368312.068804	52.427546
3265.699879	368036.789085	52.432551
3264.838561	367746.708752	52.437556
3264.124531	367456.247036	52.442561
3263.500906	367218.231297	52.447565
3262.924455	366902.454501	52.452570
3262.048294	366657.555348	52.457575
3261.781257	366378.923103	52.462580
3261.009896	366094.186255	52.467585
3260.425064	365810.639380	52.472589
3259.604861	365555.242812	52.477594
3259.060774	365265.350705	52.482599
3258.682586	364977.694999	52.487604
3257.586481	364702.389490	52.492609
3257.119384	364428.636697	52.497613
3256.337478	364128.470223	52.502618
3255.571757	363878.042728	52.507623
3255.064399	363572.180601	52.512628
3254.476267	363313.198097	52.517633
3253.920295	363030.036617	52.522637
3253.424918	362758.263129	52.527642
3252.413551	362462.880393	52.532647
3251.969861	362178.245650	52.537652
3250.892181	361902.818888	52.542657
3250.515532	361627.992116	52.547661
3249.917381	361339.559950	52.552666
3248.978001	361067.923316	52.557671
3248.290755	360776.702813	52.562676
3247.516049	360515.444373	52.567681
3246.928043	360231.177084	52.572685
3246.292964	359953.429830	52.577690
3245.499338	359662.346660	52.582695
3244.989921	359392.413839	52.587700
3244.390936	359126.692410	52.592705
3243.826880	358842.031514	52.597709
3243.409010	358553.579682	52.602714
3242.222181	358291.407518	52.607719
3241.696363	358004.827202	52.612724
3240.557904	357736.715220	52.617729
3240.586873	357460.197557	52.622733
3239.787195	357170.805626	52.627738
3238.659348	356897.343431	52.632743
3238.147746	356623.858619	52.637748
3237.555030	356344.303040	52.642753
3236.729018	356059.616811	52.647757
3236.036180	355809.721419	52.652762
3235.360798	355547.224995	52.657767
3234.981861	355246.405452	52.662772
3234.264991	355011.550164	52.667777
3233.803382	354713.947141	52.672781
3233.151137	354429.631561	52.677786
3232.026502	354170.914762	52.682791
3232.079381	353865.107177	52.687796
3230.861025	353622.588307	52.692801
3230.479734	353315.930009	52.697805
3229.519947	353078.635812	52.702810
3229.087226	352789.517492	52.707815
3228.696118	352475.729890	52.712820
3227.868977	352245.715157	52.717825
3227.107137	351935.011588	52.722829
3226.428232	351694.307343	52.727834
3225.883762	351394.611760	52.732839
3225.020116	351107.334057	52.737844
3224.241306	350853.203879	52.742849
3223.807428	350561.477762	52.747853
3223.033863	350269.218442	52.752858
3222.042601	350022.473378	52.757863
3221.878456	349725.940765	52.762868
3220.927308	349478.194315	52.767873
3220.888250	349175.199738	52.772877
3219.727853	348923.691621	52.777882
3218.798745	348623.710885	52.782887
3218.498105	348362.901571	52.787892
3217.456045	348059.830546	52.792897
3217.093762	347810.023746	52.797901
3216.676599	347528.256359	52.802906
3215.969236	347238.312326	52.807911
3215.330381	346986.738536	52.812916
3214.517382	346681.994975	52.817921
3213.927715	346410.634096	52.822925
3213.627247	346117.514797	52.827930
3212.324389	345866.855657	52.832935
3212.118978	345553.635978	52.837940
3211.172855	345287.722335	52.842945
3210.507511	345012.803451	52.847949
3210.012275	344719.173437	52.852954
3209.155151	344456.194585	52.857959
3208.621140	344172.265864	52.862964
3207.478703	343902.558983	52.867969
3206.950326	343615.139536	52.872973
3206.491442	343348.860155	52.877978
3205.579687	343074.353140	52.882983
3205.115267	342792.570520	52.887988
3204.378888	342525.338702	52.892993
3203.675791	342245.424040	52.897997
3203.195666	341964.811008	52.903002
3202.423783	341691.013850	52.908007
3201.750628	341419.847184	52.913012
3201.017650	341148.128788	52.918017
3200.394099	340860.940588	52.923021
3200.060069	340601.146112	52.928026
3199.047156	340319.617204	52.933031
3198.702673	340031.642873	52.938036
3197.901583	339769.449682	52.943041
3196.804866	339485.995710	52.948045
3196.287029	339213.522215	52.953050
3195.472888	338945.345590	52.958055
3194.879217	338675.834715	52.963060
3194.367818	338409.975398	52.968065
3193.606909	338119.029106	52.973069
3192.995854	337857.638161	52.978074
3192.454797	337595.853257	52.983079
3192.046709	337292.348354	52.988084
3191.278215	337022.985637	52.993089
3190.945933	336745.508469	52.998093
3189.959266	336471.519446	53.003098
3189.298790	336203.918335	53.008103
3188.510665	335902.071051	53.013108
3187.634114	335646.797723	53.018113
3187.129010	335353.227750	53.023117
3186.734233	335071.731359	53.028122
3185.975918	334808.391650	53.033127
3185.234194	334530.613828	53.038132
3184.479455	334268.162521	53.043137
3183.831464	333976.671394	53.048141
3183.092597	333705.279760	53.053146
3182.249760	333426.036993	53.058151
3181.798782	333147.978583	53.063156
3180.806742	332877.234827	53.068161
3180.459973	332607.940924	53.073165
3180.086855	332345.243916	53.078170
3178.927923	332070.195591	53.083175
3178.325314	331770.999802	53.088180
3177.841278	331529.855397	53.093185
3176.959396	331250.101203	53.098189
3176.680058	330967.959321	53.103194
3175.591000	330686.453644	53.108199
3175.318283	330418.183786	53.113204
3174.574443	330153.169898	53.118209
3173.742902	329875.159256	53.123213
3173.199840	329602.753935	53.128218
3172.203020	329326.804179	53.133223
3171.807184	329041.363767	53.138228
3171.120387	328776.106914	53.143233
3170.396224	328496.419386	53.148237
3169.895956	328221.456417	53.153242
3169.177425	327950.855196	53.158247
3168.546742	327677.947742	53.163252
3167.673333	327404.975902	53.168257
3167.165154	327118.756961	53.173261
3166.987868	326850.561441	53.178266
3165.884055	326574.593433	53.183271
3165.104230	326304.480046	53.188276
3164.617674	326033.937452	53.193281
3163.962937	325752.879868	53.198285
3163.175274	325470.772999	53.203290
3162.429780	325209.663647	53.208295
3162.050924	324933.779079	53.213300
3161.162193	324658.330718	53.218305
3160.558944	324389.838070	53.223309
3160.436346	324111.746061	53.228314
3159.346320	323831.972988	53.233319
3158.899083	323548.430873	53.238324
3158.244390	323278.058710	53.243329
3157.677581	322983.305179	53.248333
3156.869222	322711.886175	53.253338
3155.720045	322433.772916	53.258343
3155.431940	322154.351305	53.263348
3154.528312	321877.674217	53.268353
3153.844521	321603.023896	53.273357
3153.308769	321328.527541	53.278362
3152.548456	321052.894623	53.283367
3152.107866	320783.855886	53.288372
3150.922553	320514.679557	53.293377
3150.806734	320235.784883	53.298381
3150.065752	319961.698804	53.303386
3149.230794	319693.584983	53.308391
3148.882828	319402.426191	53.313396
3148.196181	319123.363866	53.318401
3147.492866	318849.446803	53.323405
3147.001328	318570.886695	53.328410
3146.004228	318297.014525	53.333415
3145.933137	318020.779798	53.338420
3144.801787	317736.589364	53.343425
3144.089211	317449.709155	53.348429
3143.148736	317170.554012	53.353434
3142.164523	316906.759270	53.358439
3141.838248	316622.387315	53.363444
3140.964628	316360.152349	53.368449
3140.474921	316093.960068	53.373453
3139.888342	315823.046222	53.378458
3139.143272	315542.709784	53.383463
3138.671001	315270.859708	53.388468
3137.763177	315015.858349	53.393473
3137.557683	314722.014998	53.398477
3136.726090	314446.451001	53.403482
3135.833205	314179.528215	53.408487
3135.569498	313903.491000	53.413492
3134.672298	313629.921454	53.418497
3133.807253	313348.503214	53.423501
3133.269174	313080.859503	53.428506
3132.497099	312807.573662	53.433511
3131.862913	312526.524212	53.438516
3130.894448	312257.265967	53.443521
3130.690917	311988.140687	53.448525
3129.670891	311717.819808	53.453530
3129.135497	311449.917121	53.458535
3128.878424	311172.038617	53.463540
3127.914443	310906.086851	53.468545
3127.111999	310634.252057	53.473549
3126.861932	310369.026442	53.478554
3126.090602	310094.689942	53.483559
3125.359632	309811.382819	53.488564
3124.491897	309548.621336	53.493569
3123.758675	309266.230024	53.498573
3123.266260	308983.545307	53.503578
3122.534542	308720.887848	53.508583
3121.826410	308442.616011	53.513588
3121.447970	308187.133611	53.518593
3120.648396	307910.402973	53.523597
3119.946218	307636.330172	53.528602
3119.059722	307366.869704	53.533607
3118.711585	307091.262739	53.538612
3118.100829	306820.738896	53.543617
3117.216270	306555.911151	53.548621
3117.019843	306283.003295	53.553626
3115.904613	306008.814194	53.558631
3115.640100	305728.454581	53.563636
3114.966510	305455.747887	53.568641
3113.980837	305179.499370	53.573645
3113.676463	304898.584132	53.578650
3112.882949	304633.509064	53.583655
3112.206028	304343.254788	53.588660
3111.664949	304082.238754	53.593665
3110.826214	303804.003434	53.598669
3110.080864	303525.065226	53.603674
3109.200654	303247.472063	53.608679
3108.682454	302983.241734	53.613684
3108.000769	302716.592060	53.618689
3107.537154	302432.514008	53.623693
3106.683850	302162.579919	53.628698
3106.083008	301891.612227	53.633703
3105.808416	301599.557263	53.638708
3104.445878	301335.763314	53.643713
3104.207551	301064.813245	53.648717
3103.536598	300786.978839	53.653722
3102.531278	300513.016844	53.658727
3102.080986	300246.504664	53.663732
3101.664760	299972.372164	53.668737
3100.813678	299695.379369	53.673741
3100.188205	299414.657761	53.678746
3099.459907	299142.687046	53.683751
3098.854417	298868.149803	53.688756
3097.760514	298592.110480	53.693761
3097.412334	298328.024001	53.698765
3096.924017	298060.725022	53.703770
3095.949580	297790.344684	53.708775
3095.096407	297509.681594	53.713780
3094.739714	297247.199334	53.718785
3094.079926	296970.146619	53.723789
3093.471284	296690.385908	53.728794
3092.882458	296425.850969	53.733799
3092.464941	296145.575367	53.738804
3091.627059	295871.325203	53.743809
3090.745532	295595.349810	53.748813
3090.592410	295321.678168	53.753818
3089.385683	295043.919865	53.758823
3089.114615	294769.247482	53.763828
3088.164665	294494.554840	53.768833
3087.342296	294218.848439	53.773837
3086.939624	293948.168756	53.778842
3086.305857	293673.246793	53.783847
3085.713764	293389.226034	53.788852
3084.589717	293128.286223	53.793857
3083.916317	292847.461105	53.798861
3083.769646	292582.265766	53.803866
3082.994855	292305.530867	53.808871
3082.407466	292028.867874	53.813876
3081.481363	291753.327816	53.818881
3080.938197	291472.506001	53.823885
3080.739104	291200.670453	53.828890
3079.406698	290926.900153	53.833895
3079.000363	290647.380132	53.838900
3078.487949	290372.766420	53.843905
3077.424554	290097.959484	53.848909
3077.289446	289815.899875	53.853914
3076.371497	289546.926989	53.858919
3075.705928	289267.523048	53.863924
3075.125790	288990.626648	53.868929
3074.659764	288712.362146	53.873933
3073.793044	288428.634276	53.878938
3073.237953	288149.619342	53.883943
3072.571825	287864.815056	53.888948
3071.789865	287599.078895	53.893953
3071.068116	287326.940539	53.898957
3070.861088	287042.674157	53.903962
3069.764976	286768.557182	53.908967
3069.215643	286482.740053	53.913972
3068.637555	286217.250770	53.918977
3067.761190	285914.294039	53.923981
3067.546256	285651.446525	53.928986
3066.298366	285364.847760	53.933991
3065.987275	285091.267573	53.938996
3065.648328	284799.583776	53.944001
3064.808528	284517.911636	53.949005
3064.033218	284250.363955	53.954010
3063.055374	283967.414459	53.959015
3062.332107	283681.342864	53.964020
3061.645153	283416.276639	53.969025
3061.039500	283135.458056	53.974029
3060.391230	282863.305276	53.979034
3059.621531	282584.167816	53.984039
3059.205280	282306.629730	53.989044
3058.494085	282037.491791	53.994049
3057.866472	281761.082055	53.999053
3056.717953	281478.005546	54.004058
3056.363247	281206.493251	54.009063
3055.513644	280928.488356	54.014068
3054.938749	280664.574807	54.019073
3054.377122	280388.103190	54.024077
3053.706056	280101.563347	54.029082
3052.939386	279842.417016	54.034087
3052.256206	279550.377768	54.039092
3051.577310	279282.634575	54.044097
3050.685075	279015.892882	54.049101
3050.383295	278747.147561	54.054106
3049.566667	278478.305389	54.059111
3049.017714	278209.064250	54.064116
3048.570168	277935.681143	54.069121
3047.740060	277653.368204	54.074125
3047.497320	277380.614789	54.079130
3046.332093	277107.956403	54.084135
3045.832758	276826.380545	54.089140
3045.200313	276549.257235	54.094145
3044.422534	276280.663354	54.099149
3043.521334	275996.196722	54.104154
3043.334799	275724.987887	54.109159
3042.452703	275451.164017	54.114164
3041.854417	275182.618131	54.119169
3041.220903	274896.479175	54.124173
3040.793674	274627.549688	54.129178
3039.979285	274362.348943	54.134183
3039.317619	274073.030963	54.139188
3038.841334	273798.047845	54.144193
3037.932998	273514.422959	54.149197
3037.495099	273229.653992	54.154202
3036.113245	272962.556709	54.159207
3035.643381	272679.753970	54.164212
3035.345657	272411.237264	54.169217
3034.637254	272139.398325	54.174221
3033.913604	271848.587949	54.179226
3033.279727	271586.950161	54.184231
3032.808247	271314.157081	54.189236
3032.383839	271018.409677	54.194241
3031.360643	270750.008237	54.199245
3030.636271	270472.263662	54.204250
3030.017041	270188.466562	54.209255
3029.365177	269907.017820	54.214260
3028.589291	269635.750662	54.219265
3027.878842	269370.229086	54.224269
3027.149856	269073.766630	54.229274
3026.314478	268804.113745	54.234279
3025.509266	268516.399238	54.239284
3025.113643	268222.940641	54.244289
3024.417483	267953.393473	54.249293
3023.635907	267677.620258	54.254298
3022.657256	267421.616220	54.259303
3022.566648	267145.835813	54.264308
3021.928288	266876.662106	54.269313
3021.134945	266608.073387	54.274317
3020.764480	266333.050871	54.279322
3019.804251	266059.853706	54.284327
3019.173521	265776.009847	54.289332
3018.803723	265488.686699	54.294337
3017.853921	265212.279477	54.299341
3017.159335	264954.245441	54.304346
3016.600758	264671.002197	54.309351
3016.123341	264399.181451	54.314356
3015.077069	264124.547600	54.319361
3014.399959	263853.879471	54.324365
3013.914176	263575.286216	54.329370
3013.141169	263303.614990	54.334375
3012.459386	263026.861441	54.339380
3011.850007	262763.492768	54.344385
3011.295107	262486.031978	54.349389
3010.565961	262215.755475	54.354394
3009.968940	261945.611109	54.359399
3009.598052	261658.749810	54.364404
3008.681148	261386.007945	54.369409
3007.718902	261102.857223	54.374413
3007.369607	260829.134689	54.379418
3006.673451	260562.292666	54.384423
3006.143622	260275.152340	54.389428
3005.468037	260006.041000	54.394433
3005.117366	259736.929448	54.399437
3004.328424	259438.650793	54.404442
3003.375369	259166.757362	54.409447
3002.965380	258889.582905	54.414452
3002.407464	258612.381245	54.419457
3001.236128	258334.691251	54.424461
3000.930807	258050.268453	54.429466
3000.127404	257783.369999	54.434471
2999.348199	257494.260501	54.439476
2998.657606	257225.358401	54.444481
2998.155981	256946.418076	54.449485
2997.696899	256670.833054	54.454490
2996.804435	256385.715843	54.459495
2996.211704	256109.210419	54.464500
2995.472617	255839.731995	54.469505
2994.767064	255554.611809	54.474509
2994.241984	255272.315773	54.479514
2993.834649	254994.330898	54.484519
2992.769669	254718.258669	54.489524
2992.257523	254444.009351	54.494529
2991.810381	254156.660133	54.499533
2991.031905	253876.596396	54.504538
2990.195202	253600.005790	54.509543
2989.655603	253307.731946	54.514548
2988.988620	253042.091517	54.519553
2988.094261	252758.711688	54.524557
2988.008643	252474.236564	54.529562
2987.180790	252202.485384	54.534567
2986.277215	251911.748522	54.539572
2985.551437	251637.919281	54.544577
2984.718828	251360.847677	54.549581
2984.363304	251077.257995	54.554586
2983.632923	250807.912944	54.559591
2982.988918	250513.801323	54.564596
2982.699561	250238.581068	54.569601
2981.093698	249961.685170	54.574605
2980.836834	249679.304706	54.579610
2980.342726	249399.177867	54.584615
2979.386877	249134.378863	54.589620
2979.179635	248845.880183	54.594625
2978.608148	248563.729830	54.599629
2977.753046	248289.442975	54.604634
2976.777239	248018.511777	54.609639
2976.391609	247726.605589	54.614644
2975.975740	247442.853856	54.619649
2975.086387	247162.742849	54.624653
2974.959152	246886.127895	54.629658
2974.000263	246595.256987	54.634663
2973.417307	246311.075583	54.639668
2972.600345	246026.779009	54.644673
2971.512995	245748.535703	54.649677
2971.135616	245462.999303	54.654682
2970.458061	245190.982259	54.659687
2969.644707	244904.395581	54.664692
2969.180352	244619.460459	54.669697
2968.369153	244342.806154	54.674701
2967.936132	244057.485320	54.679706
2967.105700	243781.115380	54.684711
2966.557070	243504.625035	54.689716
2965.907862	243229.882843	54.694721
2965.265077	242934.742747	54.699725
2964.814385	242646.091975	54.704730
2963.840274	242371.530436	54.709735
2963.288850	242087.378749	54.714740
2962.780349	241807.244370	54.719745
2961.816109	241513.992058	54.724749
2961.264875	241242.752956	54.729754
2960.612196	240943.825040	54.734759
2959.677826	240666.230838	54.739764
2959.026686	240377.540877	54.744769
2958.703935	240107.872505	54.749773
2957.926328	239816.861246	54.754778
2957.328314	239542.475951	54.759783
2956.525523	239266.417638	54.764788
2955.963001	238977.182461	54.769793
2955.243037	238696.783540	54.774797
2954.907516	238406.317108	54.779802
2954.190242	238122.481585	54.784807
2953.309890	237839.080044	54.789812
2952.567631	237554.205951	54.794817
2951.761094	237275.097604	54.799821
2951.396394	236989.324949	54.804826
2950.697827	236704.802713	54.809831
2949.796243	236430.396961	54.814836
2949.487496	236130.154495	54.819841
2948.591629	235862.166146	54.824845
2948.011159	235576.355150	54.829850
2947.031778	235289.946064	54.834855
2946.483335	235010.853901	54.839860
2945.975174	234719.686613	54.844865
2944.854032	234460.446046	54.849869
2944.495561	234167.168712	54.854874
2943.945937	233891.772021	54.859879
2943.226468	233617.039567	54.864884
2942.894838	233324.524404	54.869889
2941.985275	233052.904645	54.874893
2941.272814	232751.259487	54.879898
2940.678623	232482.545093	54.884903
2940.221202	232203.039187	54.889908
2939.573461	231908.159498	54.894913
2938.719581	231633.173980	54.899917
2938.080278	231338.702162	54.904922
2937.166973	231044.580212	54.909927
2936.902216	230766.881422	54.914932
2936.054868	230492.076532	54.919937
2935.396438	230217.828195	54.924941
2934.839311	229915.607565	54.929946
2934.026894	229645.637491	54.934951
2933.419434	229356.310382	54.939956
2933.078868	229062.969964	54.944961
2931.818529	228772.627832	54.949965
2931.654392	228493.112460	54.954970
2930.762539	228221.173371	54.959975
2930.199080	227927.337399	54.964980
2929.596301	227646.646625	54.969985
2928.677901	227364.759154	54.974989
2928.177128	227080.756899	54.979994
2927.391580	226782.084285	54.984999
2926.755483	226511.115914	54.990004
2926.007822	226225.335211	54.995009
2925.285770	225950.334030	55.000013
2924.815875	225664.129396	55.005018
2924.106446	225376.919809	55.010023
2923.312980	225092.805252	55.015028
2922.525464	224802.822159	55.020033
2922.074820	224538.297904	55.025037
2921.532551	224245.070022	55.030042
2920.708809	223969.213332	55.035047
2920.034850	223680.387520	55.040052
2919.807233	223394.203580	55.045057
2918.590736	223125.528065	55.050061
2918.232067	222823.327336	55.055066
2917.595607	222540.457381	55.060071
2917.075150	222266.302699	55.065076
2916.376072	221965.381298	55.070081
2915.691820	221687.181138	55.075085
2915.105805	221403.199948	55.080090
2914.238365	221120.855580	55.085095
2913.858631	220839.937145	55.090100
2912.899582	220535.791155	55.095105
2912.042372	220273.739115	55.100109
2911.798160	219968.196624	55.105114
2911.134341	219681.675753	55.110119
2910.205581	219405.712310	55.115124
2909.678544	219114.614953	55.120129
2908.973039	218826.029211	55.125133
2908.551528	218537.552416	55.130138
2907.424585	218261.382894	55.135143
2907.101756	217967.699339	55.140148
2906.389871	217679.399296	55.145153
2905.428802	217404.148807	55.150157
2905.063355	217113.568688	55.155162
2904.579946	216831.702213	55.160167
2903.577550	216551.968381	55.165172
2903.359793	216263.481413	55.170177
2902.623450	215962.094573	55.175181
2901.753422	215681.961475	55.180186
2901.086527	215388.292420	55.185191
2900.611985	215108.710044	55.190196
2899.928437	214809.547453	55.195201
2899.277148	214536.168721	55.200205
2898.238740	214238.935938	55.205210
2897.745704	213948.504115	55.210215
2897.122146	213657.597836	55.215220
2896.636880	213371.087608	55.220225
2896.437219	213081.567775	55.225229
2895.769677	212780.158979	55.230234
2894.711278	212501.354674	55.235239
2894.153783	212193.821771	55.240244
2893.682663	211904.095633	55.245249
2892.612952	211609.845402	55.250253
2891.998343	211328.646754	55.255258
2891.268825	211026.466907	55.260263
2890.521794	210735.147924	55.265268
2889.877347	210450.877838	55.270273
2888.817160	210162.958445	55.275277
2888.573491	209862.374591	55.280282
2887.855856	209594.296564	55.285287
2886.997225	209294.589211	55.290292
2886.628672	208992.540275	55.295297
2885.593116	208720.672776	55.300301
2884.987517	208427.776837	55.305306
2884.409678	208149.908581	55.310311
2884.079773	207853.930000	55.315316
2883.081685	207574.260072	55.320321
2882.607733	207284.530586	55.325325
2882.194872	206990.058458	55.330330
2881.188566	206704.679573	55.335335
2880.566634	206420.895677	55.340340
2880.024874	206130.431700	55.345345
2879.035950	205838.194613	55.350349
2878.232945	205563.466681	55.355354
2877.702854	205267.889093	55.360359
2877.306909	204988.594269	55.365364
2876.698222	204693.566573	55.370369
2875.955538	204415.283909	55.375373
2875.442244	204108.077823	55.380378
2874.738831	203827.386560	55.385383
2873.547065	203534.607898	55.390388
2873.539877	203249.622385	55.395393
2872.769098	202960.636023	55.400397
2872.254868	202652.369024	55.405402
2871.595791	202376.666518	55.410407
2870.520590	202076.674220	55.415412
2870.212491	201791.654717	55.420417
2869.373336	201503.450298	55.425421
2868.810848	201213.142047	55.430426
2868.191528	200933.686429	55.435431
2867.529483	200631.167867	55.440436
2866.804731	200331.473217	55.445441
2865.700547	200051.640804	55.450445
2865.218688	199749.582202	55.455450
2864.660694	199475.710765	55.460455
2864.031749	199178.895971	55.465460
2863.670258	198878.235712	55.470465
2862.831163	198606.334728	55.475469
2861.996876	198302.075107	55.480474
2861.289959	198019.950896	55.485479
2860.921530	197725.431645	55.490484
2860.119339	197429.010421	55.495489
2858.921758	197150.951406	55.500493
2858.678490	196862.474106	55.505498
2858.017996	196570.883378	55.510503
2857.474803	196290.333183	55.515508
2856.969327	195990.895726	55.520513
2856.007253	195709.129892	55.525517
2855.275186	195412.505586	55.530522
2854.527129	195117.539672	55.535527
2853.514153	194837.682622	55.540532
2853.645747	194540.010545	55.545537
2852.545322	194269.128139	55.550541
2852.532396	193965.298573	55.555546
2851.740201	193689.586368	55.560551
2851.073133	193391.729508	55.565556
2850.352026	193096.745794	55.570561
2849.518835	192801.654358	55.575565
2848.962170	192506.482735	55.580570
2848.547147	192217.435820	55.585575
2847.465222	191922.999786	55.590580
2847.111796	191630.307755	55.595585
2846.305146	191335.806246	55.600589
2845.545401	191050.510559	55.605594
2845.091682	190749.264445	55.610599
2843.998633	190468.605247	55.615604
2843.926327	190171.373682	55.620609
2842.914019	189883.147818	55.625613
2842.815230	189585.287972	55.630618
2841.851821	189296.981595	55.635623
2841.057832	188997.161773	55.640628
2840.420779	188702.229850	55.645633
2839.428214	188406.719967	55.650637
2838.808056	188114.422593	55.655642
2838.357638	187821.400458	55.660647
2837.658545	187528.953880	55.665652
2836.907277	187237.191681	55.670657
2835.754018	186950.710965	55.675661
2835.528778	186655.116200	55.680666
2835.196482	186363.725747	55.685671
2834.093259	186071.059857	55.690676
2833.396465	185787.720009	55.695681
2833.131095	185492.749779	55.700685
2832.488404	185205.194200	55.705690
2831.878030	184913.195598	55.710695
2830.985315	184626.408431	55.715700
2830.830298	184316.608198	55.720705
2829.659490	184045.541268	55.725709
2829.113724	183734.051459	55.730714
2828.520572	183442.326904	55.735719
2827.696346	183154.011888	55.740724
2827.108143	182851.668575	55.745729
2826.405158	182566.505677	55.750733
2825.909700	182270.359366	55.755738
2824.963602	181974.260991	55.760743
2824.555514	181688.064940	55.765748
2823.884945	181380.147903	55.770753
2822.938885	181095.936291	55.775757
2822.643586	180808.761469	55.780762
2822.162343	180504.903872	55.785767
2821.350050	180220.536954	55.790772
2820.472092	179909.661399	55.795777
2819.874100	179613.447843	55.800781
2819.319483	179325.497287	55.805786
2818.658866	179026.384948	55.810791
2817.634501	178734.887729	55.815796
2817.509637	178429.614860	55.820801
2816.753169	178144.731576	55.825805
2815.781647	177850.306701	55.830810
2815.543449	177547.500325	55.835815
2814.611005	177260.336078	55.840820
2814.064874	176968.355750	55.845825
2813.501701	176664.589783	55.850829
2812.641592	176364.396190	55.855834
2812.023071	176064.891500	55.860839
2811.266519	175767.038847	55.865844
2811.004447	175477.237188	55.870849
2809.916288	175165.298475	55.875853
2809.448109	174877.492377	55.880858
2809.001784	174578.518262	55.885863
2808.000420	174278.654972	55.890868
2807.310993	173983.831737	55.895873
2806.770010	173691.645215	55.900877
2806.194590	173389.584514	55.905882
2805.386516	173096.528970	55.910887
2804.665719	172802.253589	55.915892
2804.099055	172488.828770	55.920897
2803.015940	172198.824780	55.925901
2802.214830	171902.152515	55.930906
2801.743927	171607.884633	55.935911
2800.993003	171321.064713	55.940916
2800.472349	171027.597547	55.945921
2799.719194	170734.143984	55.950925
2799.159494	170438.423829	55.955930
2798.622834	170150.421383	55.960935
2797.767793	169860.932790	55.965940
2797.508577	169578.168115	55.970945
2796.853253	169225.527477	55.975949
2796.499907	168918.036294	55.980954
2795.441005	168622.816108	55.985959
2794.790757	168317.665730	55.990964
2794.310509	167995.629354	55.995969
2793.338883	167728.034373	56.000973
2792.609231	167418.491380	56.005978
2792.290881	167131.964947	56.010983
2791.265657	166835.926879	56.015988
2791.125323	166528.510428	56.020993
2790.261321	166246.438647	56.025997
2789.705373	165939.487063	56.031002
2789.137658	165640.970114	56.036007
2787.887288	165330.751294	56.041012
2787.330861	165049.618987	56.046017
2786.644876	164744.808631	56.051021
2786.220947	164455.967323	56.056026
2785.639375	164150.903789	56.061031
2784.713164	163851.606273	56.066036
2784.250871	163550.088983	56.071041
2783.408583	163260.280821	56.076045
2782.952398	162984.615763	56.081050
2782.315993	162669.287454	56.086055
2781.137542	162369.304723	56.091060
2781.011354	162087.504194	56.096065
2780.358923	161782.065024	56.101069
2779.252852	161470.216267	56.106074
2778.688522	161196.756143	56.111079
2777.864971	160894.301272	56.116084
2777.334450	160578.402537	56.121089
2776.710446	160322.681234	56.126093
2775.472439	160000.860855	56.131098
2774.906321	159725.759667	56.136103
2774.617345	159443.726243	56.141108
2774.026196	159143.893920	56.146113
2773.271393	158853.268788	56.151117
2772.661191	158560.385732	56.156122
2772.292957	158273.123956	56.161127
2771.111390	157989.324074	56.166132
2770.750581	157683.302284	56.171137
2770.016363	157386.596936	56.176141
2769.158362	157101.990372	56.181146
2768.795082	156805.994021	56.186151
2767.966517	156521.921524	56.191156
2767.396916	156228.988310	56.196161
2766.727476	155934.433606	56.201165
2765.874290	155649.469752	56.206170
2765.802815	155338.096933	56.211175
2764.659417	155061.751598	56.216180
2764.484109	154756.692764	56.221185
2763.640625	154458.314242	56.226189
2762.845923	154173.760359	56.231194
2762.047767	153868.757407	56.236199
2761.366955	153592.122113	56.241204
2760.697653	153290.535989	56.246209
2759.800650	153003.745773	56.251213
2759.468922	152704.501114	56.256218
2758.745084	152411.002845	56.261223
2758.200134	152152.241670	56.266228
2757.410523	151828.088927	56.271233
2756.712805	151552.058050	56.276237
2756.117795	151246.983555	56.281242
2755.501643	150947.634708	56.286247
2754.745773	150686.427383	56.291252
2754.423635	150360.156169	56.296257
2753.715306	150090.214571	56.301261
2752.898337	149786.269247	56.306266
2752.271824	149497.014011	56.311271
2751.309435	149191.000294	56.316276
2750.564689	148911.110319	56.321281
2750.313151	148603.833074	56.326285
2749.462185	148338.287944	56.331290
2748.889417	148032.795477	56.336295
2748.393218	147750.385385	56.341300
2747.831506	147443.816588	56.346305
2746.786562	147147.049217	56.351309
2745.880268	146878.297125	56.356314
2745.673305	146552.376903	56.361319
2744.646020	146287.779162	56.366324
2744.273509	145970.240381	56.371329
2743.431582	145699.226163	56.376333
2742.714975	145400.606053	56.381338
2742.338047	145102.303514	56.386343
2741.588084	144830.430871	56.391348
2740.915946	144509.561528	56.396353
2740.263367	144255.544993	56.401357
2739.545933	143934.409228	56.406362
2739.051237	143667.347766	56.411367
2738.301578	143358.091426	56.416372
2737.718074	143062.090403	56.421377
2737.091716	142769.631462	56.426381
2736.604072	142487.521834	56.431386
2735.877667	142184.410901	56.436391
2735.184489	141877.320672	56.441396
2734.248965	141599.775518	56.446401
2733.517964	141286.115502	56.451405
2732.796177	141010.498616	56.456410
2732.789508	140700.033471	56.461415
2731.845502	140434.748698	56.466420
2731.265647	140125.142621	56.471425
2730.397499	139852.062520	56.476429
2730.041566	139524.550724	56.481434
2728.812465	139250.898036	56.486439
2728.436577	138935.465738	56.491444
2727.947857	138650.050828	56.496449
2727.106796	138336.604311	56.501453
2726.339168	138064.121827	56.506458
2726.100956	137739.304457	56.511463
2725.174007	137479.595201	56.516468
2724.233370	137146.053419	56.521473
2723.811429	136886.028037	56.526477
2723.053733	136570.351212	56.531482
2722.578543	136275.759520	56.536487
2721.519148	135990.028912	56.541492
2721.591231	135685.549235	56.546497
2720.676770	135397.591074	56.551501
2720.150080	135069.558899	56.556506
2719.266222	134816.053076	56.561511
2718.556024	134495.487868	56.566516
2718.053578	134225.323936	56.571521
2716.890356	133901.559762	56.576525
2716.398124	133602.780699	56.581530
2715.987143	133346.253228	56.586535
2715.159347	133022.268043	56.591540
2714.955432	132723.846285	56.596545
2713.880120	132418.516019	56.601549
2713.004369	132146.550996	56.606554
2712.724006	131811.772415	56.611559
2711.940778	131560.604030	56.616564
2711.250130	131248.087096	56.621569
2710.594125	130945.094248	56.626573
2709.949104	130669.309199	56.631578
2709.359550	130335.168741	56.636583
2708.541653	130087.092731	56.641588
2708.050014	129751.165602	56.646593
2707.055550	129482.534756	56.651597
2706.539128	129166.635091	56.656602
2706.179145	128898.049099	56.661607
2705.147771	128572.013868	56.666612
2705.031225	128264.646619	56.671617
2704.007722	128008.747642	56.676621
2703.247702	127669.916480	56.681626
2702.816843	127395.387384	56.686631
2702.161911	127088.359889	56.691636
2701.101940	126807.599210	56.696641
2700.633108	126479.772593	56.701645
2699.698208	126234.988175	56.706650
2699.133803	125912.326760	56.711655
2698.711039	125594.878735	56.716660
2697.994817	125350.702614	56.721665
2696.946652	125031.455454	56.726669
2696.500623	124732.993171	56.731674
2695.987148	124454.062419	56.736679
2695.403235	124153.482378	56.741684
2694.806073	123862.964770	56.746689
2694.437128	123547.297439	56.751693
2693.336359	123283.392128	56.756698
2693.065926	122963.132165	56.761703
2692.270865	122663.135674	56.766708
2691.459678	122370.674732	56.771713
2690.285491	122066.516805	56.776717
2689.828414	121769.194131	56.781722
2689.295931	121482.806214	56.786727
2688.844338	121177.185487	56.791732
2688.004589	120899.867399	56.796737
2687.503089	120596.610243	56.801741
2686.747440	120308.981788	56.806746
2686.420069	119984.862884	56.811751
2685.258754	119726.417799	56.816756
2684.742033	119401.790217	56.821761
2683.601552	119121.199631	56.826765
2683.577700	118820.001362	56.831770
2682.922395	118508.750160	56.836775
2681.529311	118243.367670	56.841780
2681.410844	117941.515431	56.846785
2681.045140	117642.955866	56.851789
2680.083754	117364.076228	56.856794
2679.545913	117043.321926	56.861799
2678.767209	116756.288906	56.866804
2678.434921	116460.340262	56.871809
2677.549314	116164.362122	56.876813
2676.851525	115876.850152	56.881818
2676.562925	115564.186640	56.886823
2675.510754	115260.762239	56.891828
2675.174514	114967.694120	56.896833
2674.252493	114684.985062	56.901837
2673.171843	114385.929634	56.906842
2673.121231	114074.592387	56.911847
2671.748074	113801.764035	56.916852
2671.429839	113485.824424	56.921857
2670.835070	113198.193435	56.926861
2670.118010	112912.412899	56.931866
2669.653575	112595.111519	56.936871
2668.609247	112336.266118	56.941876
2667.964490	112002.316594	56.946881
2667.669897	111733.852144	56.951885
2666.910687	111424.322959	56.956890
2666.116384	111143.556675	56.961895
2665.494857	110840.803163	56.966900
2665.057192	110533.068187	56.971905
2664.121598	110256.046710	56.976909
2662.739367	109954.579576	56.981914
2662.963149	109650.742289	56.986919
2662.008341	109387.839873	56.991924
2661.602118	109056.284847	56.996929
2660.685690	108804.740923	57.001933
2660.325692	108480.788139	57.006938
2659.464563	108191.804845	57.011943
2658.516892	107926.277533	57.016948
2657.904698	107608.213888	57.021953
2657.647032	107332.691891	57.026957
2656.734137	107026.396355	57.031962
2656.564537	106741.400631	57.036967
2655.605162	106432.302952	57.041972
2654.850382	106162.538977	57.046977
2654.530846	105871.226379	57.051981
2653.582247	105560.856663	57.056986
2652.877001	105271.782317	57.061991
2651.857650	104990.387138	57.066996
2651.169009	104668.035176	57.072001
2650.502173	104395.282823	57.077005
2650.198034	104100.075149	57.082010
2649.600296	103812.156204	57.087015
2648.797612	103521.780082	57.092020
2648.111261	103214.774553	57.097025
2647.660883	102939.594086	57.102029
2646.989321	102639.616303	57.107034
2646.297990	102335.794921	57.112039
2645.496551	102060.477418	57.117044
2644.872937	101760.484293	57.122049
2644.356738	101462.374684	57.127053
2643.780168	101185.636351	57.132058
2642.969127	100882.334993	57.137063
2642.248093	100598.528496	57.142068
2641.508333	100301.166983	57.147073
2640.687111	100002.680472	57.152077
2640.411285	99712.211289	57.157082
2639.679217	99421.995660	57.162087
2638.784117	99139.078310	57.167092
2638.480686	98836.617766	57.172097
2637.945723	98550.726652	57.177101
2636.754868	98249.644942	57.182106
2636.639222	97954.973917	57.187111
2635.877358	97660.504231	57.192116
2635.335186	97366.783645	57.197121
2634.639169	97067.072521	57.202125
2633.643208	96763.677404	57.207130
2633.388795	96483.367879	57.212135
2632.579907	96189.463829	57.217140
2631.833569	95882.787587	57.222145
2631.182804	95585.904720	57.227149
2629.938857	95294.040899	57.232154
2629.985135	95001.278860	57.237159
2629.115534	94712.413596	57.242164
2628.147036	94407.549318	57.247169
2627.474892	94118.692151	57.252173
2626.987975	93814.558677	57.257178
2626.440135	93533.267195	57.262183
2625.383848	93246.302137	57.267188
2625.029460	92942.907841	57.272193
2624.589399	92644.781551	57.277197
2623.626426	92362.283508	57.282202
2623.316667	92062.628967	57.287207
2622.483696	91774.056110	57.292212
2622.061297	91476.101334	57.297217
2620.909404	91192.006037	57.302221
2620.354773	90901.663243	57.307226
2619.964294	90597.292514	57.312231
2619.029408	90311.735004	57.317236
2618.201109	90024.902651	57.322241
2617.799132	89732.338497	57.327245
2616.895134	89436.935094	57.332250
2616.625251	89143.242099	57.337255
2615.643057	88854.319376	57.342260
2615.093445	88555.797013	57.347265
2614.643386	88269.149821	57.352269
2613.870048	87966.062142	57.357274
2613.103069	87682.135586	57.362279
2612.276882	87393.435925	57.367284
2611.542860	87087.127655	57.372289
2611.320721	86793.091416	57.377293
2610.158007	86522.453824	57.382298
2609.750690	86221.773343	57.387303
2609.098542	85934.745619	57.392308
2608.328576	85646.643806	57.397313
2607.576122	85364.558624	57.402317
2606.994520	85067.655598	57.407322
2606.388410	84774.728578	57.412327
2605.586794	84496.446879	57.417332
2604.986035	84197.930081	57.422337
2604.421864	83907.182516	57.427341
2603.692052	83617.745537	57.432346
2602.839251	83330.702505	57.437351
2602.420310	83042.060824	57.442356
2601.821761	82748.989625	57.447361
2600.701470	82464.301529	57.452365
2600.455106	82177.621836	57.457370
2599.882444	81889.147164	57.462375
2598.948185	81598.559972	57.467380
2598.151178	81320.275304	57.472385
2597.874299	81032.291647	57.477389
2596.897977	80734.137248	57.482394
2596.528216	80448.616303	57.487399
2595.663325	80170.604970	57.492404
2595.122162	79883.255851	57.497409
2594.719826	79595.172647	57.502413
2593.825142	79294.130062	57.507418
2593.456708	79009.123101	57.512423
2592.552138	78718.071067	57.517428
2592.213074	78420.482812	57.522433
2591.785878	78127.544887	57.527437
2590.390655	77841.658667	57.532442
2589.998067	77546.974707	57.537447
2589.324432	77250.806157	57.542452
2588.433485	76947.307335	57.547457
2587.714288	76670.137770	57.552461
2586.926592	76387.901340	57.557466
2586.526268	76077.437827	57.562471
2585.376219	75826.217758	57.567476
2585.499310	75517.884766	57.572481
2584.639918	75226.691788	57.577485
2583.866340	74948.756140	57.582490
2583.265024	74653.817895	57.587495
2582.152077	74370.837611	57.592500
2581.649388	74070.995030	57.597505
2580.880711	73786.295919	57.602509
2580.038715	73516.354338	57.607514
2579.627057	73221.242415	57.612519
2579.203636	72953.966174	57.617524
2578.320212	72664.239624	57.622529
2577.543372	72376.312150	57.627533
2576.901698	72099.421453	57.632538
2576.338746	71809.612242	57.637543
2575.648254	71533.510009	57.642548
2574.985475	71245.454200	57.647553
2574.503818	70963.233136	57.652557
2573.394891	70681.818620	57.657562
2573.193939	70399.681490	57.662567
2572.341941	70117.474232	57.667572
2571.751781	69827.647786	57.672577
2570.997041	69544.476929	57.677581
2570.267259	69258.532021	57.682586
2569.338620	68967.378524	57.687591
2568.609762	68692.563694	57.692596
2568.081777	68402.400175	57.697601
2567.548418	68141.027155	57.702605
2566.569268	67873.901643	57.707610
2566.339686	67578.256472	57.712615
2565.945050	67291.242356	57.717620
2564.945881	67019.445272	57.722625
2564.353355	66747.666725	57.727629
2563.611724	66466.618990	57.732634
2563.353844	66171.332283	57.737639
2562.165855	65904.191090	57.742644
2561.922911	65616.930858	57.747649
2561.351150	65324.980834	57.752653
2560.389946	65047.648814	57.757658
2560.138825	64767.159269	57.762663
2559.177288	64478.465906	57.767668
2558.526235	64195.347450	57.772673
2558.055180	63916.599090	57.777677
2556.986876	63625.206468	57.782682
2556.258714	63345.734723	57.787687
2555.297724	63073.158098	57.792692
2554.775709	62792.215029	57.797697
2554.480275	62521.354871	57.802701
2553.339126	62245.950511	57.807706
2552.916334	61960.416924	57.812711
2552.350199	61693.182432	57.817716
2551.368190	61414.985551	57.822721
2551.159236	61129.449655	57.827725
2550.266179	60854.716402	57.832730
2549.856123	60578.682425	57.837735
2549.228676	60308.058659	57.842740
2548.242700	60027.790640	57.847745
2547.984897	59746.237084	57.852749
2547.063606	59465.546263	57.857754
2546.368462	59176.819000	57.862759
2545.424945	58901.682489	57.867764
2544.755265	58620.046640	57.872769
2544.228492	58357.667702	57.877773
2543.421652	58083.110362	57.882778
2542.890546	57798.540540	57.887783
2542.327223	57535.273861	57.892788
2541.967989	57247.963429	57.897793
2540.937577	56985.731249	57.902797
2540.282735	56717.309905	57.907802
2539.752994	56425.700386	57.912807
2539.283128	56145.937781	57.917812
2538.662465	55870.149655	57.922817
2538.017028	55593.758836	57.927821
2536.937381	55321.763791	57.932826
2536.691550	55041.523680	57.937831
2535.633091	54763.710899	57.942836
2534.982553	54478.822208	57.947841
2534.422813	54204.574808	57.952845
2533.460614	53931.034524	57.957850
2532.718120	53662.928221	57.962855
2532.294882	53385.741439	57.967860
2531.601008	53130.906022	57.972865
2531.007421	52843.565909	57.977869
2530.192313	52578.581680	57.982874
2529.986128	52292.714008	57.987879
2528.763407	52023.771571	57.992884
2527.976831	51746.224577	57.997889
2527.854079	51474.024851	58.002893
2526.890694	51211.134444	58.007898
2526.084166	50933.827799	58.012903
2525.345506	50666.882258	58.017908
2524.502891	50404.253469	58.022913
2523.993625	50141.173920	58.027917
2523.443805	49882.641276	58.032922
2523.078493	49595.924366	58.037927
2521.950584	49336.646607	58.042932
2521.229921	49068.118240	58.047937
2520.958481	48793.002947	58.052941
2519.760824	48535.645982	58.057946
2519.608347	48272.249653	58.062951
2518.762425	48000.328279	58.067956
2517.801082	47731.352196	58.072961
2517.326521	47470.770855	58.077965
2516.711123	47207.871814	58.082970
2516.172602	46933.539486	58.087975
2515.203347	46690.970074	58.092980
2514.551387	46416.587880	58.097985
2513.907286	46149.062801	58.102989
2513.391195	45890.165676	58.107994
2512.501007	45620.998686	58.112999
2511.752236	45387.040590	58.118004
2510.997007	45100.354169	58.123009
2510.241274	44859.455704	58.128013
2509.507712	44606.855235	58.133018
2509.030543	44341.542066	58.138023
2508.367847	44084.744330	58.143028
2507.546777	43826.583990	58.148033
2507.132542	43580.345582	58.153037
2506.400086	43331.109378	58.158042
2505.926949	43042.207982	58.163047
2505.319645	42823.428693	58.168052
2504.528619	42537.293078	58.173057
2503.800425	42298.509765	58.178061
2503.097606	42041.293356	58.183066
2502.846642	41771.521890	58.188071
2501.818081	41510.851915	58.193076
2500.966388	41281.670770	58.198081
2500.663723	41001.472200	58.203085
2499.682009	40731.121469	58.208090
2499.239264	40510.008855	58.213095
2498.822200	40253.741491	58.218100
2497.747634	39984.070217	58.223105
2497.151287	39740.016680	58.228109
2496.529043	39486.446081	58.233114
2496.076148	39213.847654	58.238119
2495.125446	38997.851146	58.243124
2494.437235	38712.348067	58.248129
2493.588705	38472.219303	58.253133
2492.737952	38210.465049	58.258138
2492.116341	37959.104906	58.263143
2491.426949	37731.686175	58.268148
2490.557555	37461.322217	58.273153
2490.057342	37235.460849	58.278157
2489.128148	36976.331998	58.283162
2488.530821	36763.227433	58.288167
2487.865747	36500.251633	58.293172
2486.690630	36273.713550	58.298177
2486.379394	36049.096278	58.303181
2485.707263	35795.585818	58.308186
2485.250254	35572.437886	58.313191
2484.402617	35332.325310	58.318196
2483.692846	35092.110564	58.323201
2483.143610	34858.698088	58.328205
2481.971339	34624.801315	58.333210
2481.378021	34387.563632	58.338215
2480.581387	34167.105430	58.343220
2479.529315	33938.024086	58.348225
2479.044693	33714.257458	58.353229
2477.990396	33518.571156	58.358234
2477.260767	33284.136351	58.363239
2476.127078	33110.637116	58.368244
2475.243650	32866.736846	58.373249
2474.720177	32686.867056	58.378253
2473.685070	32493.419522	58.383258
2473.155634	32284.469974	58.388263
2472.324544	32092.562333	58.393268
2471.175383	31903.828128	58.398273
2470.410248	31710.762557	58.403277
2469.501592	31537.658185	58.408282
2468.682857	31370.822237	58.413287
2467.735067	31200.159384	58.418292
2467.045487	31025.151717	58.423297
2466.530030	30851.323884	58.428301
2465.288225	30693.673983	58.433306
2464.701101	30519.074183	58.438311
2463.827090	30373.544602	58.443316
2463.009114	30226.245757	58.448321
2462.351965	30058.392689	58.453325
2461.294975	29921.394768	58.458330
2460.774286	29777.411814	58.463335
2460.359449	29644.289537	58.468340
2459.515367	29489.710133	58.473345
2458.821181	29354.882387	58.478349
2457.862846	29229.068206	58.483354
2457.172782	29081.135372	58.488359
2456.819749	28935.633982	58.493364
2455.802790	28806.178165	58.498369
2455.029236	28672.899522	58.503373
2454.221817	28545.321000	58.508378
2453.434950	28423.481232	58.513383
2452.805017	28298.843384	58.518388
2451.784606	28182.791316	58.523393
2451.753587	28052.479047	58.528397
2450.674244	27944.493272	58.533402
2449.776325	27814.724769	58.538407
2448.909695	27698.176295	58.543412
2448.165323	27586.991394	58.548417
2447.652153	27481.702425	58.553421
2447.159083	27367.207611	58.558426
2446.636523	27246.157041	58.563431
2446.191841	27138.341426	58.568436
2445.367068	27049.019956	58.573441
2445.092376	26908.610893	58.578445
2444.275970	26791.627388	58.583450
2443.743801	26677.032306	58.588455
2443.038218	26560.242214	58.593460
2442.552981	26454.530603	58.598465
2441.632740	26336.807073	58.603469
2440.950825	26213.543334	58.608474
2440.582690	26105.382098	58.613479
2440.113376	25989.932923	58.618484
2439.131137	25881.192924	58.623489
2438.871591	25754.104035	58.628493
2437.997381	25648.535216	58.633498
2437.414448	25522.171527	58.638503
2436.491285	25412.059060	58.643508
2435.956879	25289.661189	58.648513
2435.320211	25177.247023	58.653517
2434.391296	25070.874883	58.658522
2434.135135	24939.925357	58.663527
2433.433963	24832.160359	58.668532
2432.943984	24721.200563	58.673537
2432.213043	24606.689695	58.678541
2431.212203	24492.488572	58.683546
2430.951626	24373.241571	58.688551
2430.318011	24258.117600	58.693556
2429.482916	24137.113980	58.698561
2428.742615	24028.695694	58.703565
2428.329339	23912.140754	58.708570
2427.696244	23795.625468	58.713575
2427.404040	23679.951682	58.718580
2426.373486	23564.597954	58.723585
2425.890336	23452.709367	58.728589
2424.926917	23331.248163	58.733594
2424.325229	23224.030241	58.738599
2423.829784	23099.544915	58.743604
2423.146824	22976.774586	58.748609
2422.663067	22857.703828	58.753613
2421.756388	22744.653983	58.758618
2421.309601	22630.180206	58.763623
2420.809595	22515.749647	58.768628
2419.655496	22395.242589	58.773633
2419.281237	22273.977180	58.778637
2418.311320	22163.691688	58.783642
2417.723040	22054.954061	58.788647
2416.965478	21937.189087	58.793652
2416.172186	21834.831356	58.798657
2416.058247	21719.624464	58.803661
2414.969961	21600.052634	58.808666
2414.648012	21478.272612	58.813671
2414.235700	21358.462002	58.818676
2413.300283	21269.060213	58.823681
2412.606911	21145.290406	58.828685
2412.011613	21024.115441	58.833690
2411.182565	20904.765574	58.838695
2410.731457	20783.160232	58.843700
2409.878485	20675.082819	58.848705
2409.595772	20554.476553	58.853709
2408.643266	20445.416190	58.858714
2408.026230	20334.718075	58.863719
2407.496623	20216.499163	58.868724
2406.797916	20109.611879	58.873729
2406.278006	19987.952947	58.878733
2405.329547	19863.429995	58.883738
2404.612123	19748.064020	58.888743
2404.031584	19640.820543	58.893748
2403.212873	19520.261824	58.898753
2403.174887	19402.445179	58.903757
2401.970788	19309.849351	58.908762
2401.638029	19182.019562	58.913767
2401.185064	19055.165886	58.918772
2400.199505	18951.935783	58.923777
2399.496132	18830.944122	58.928781
2399.115721	18710.986855	58.933786
2398.351268	18590.724720	58.938791
2397.750454	18494.259949	58.943796
2396.810681	18364.800746	58.948801
2396.351496	18234.282436	58.953805
2395.520141	18132.337402	58.958810
2394.613518	18017.013442	58.963815
2393.833610	17922.087159	58.968820
2393.094085	17808.456340	58.973825
2392.883427	17699.300310	58.978829
2391.843801	17581.272027	58.983834
2391.195882	17472.528522	58.988839
2390.698228	17369.102314	58.993844
2389.909018	17257.700304	58.998849
2389.286259	17128.341257	59.003853
2388.168003	17038.926006	59.008858
2387.408171	16930.508538	59.013863
2387.205789	16832.567562	59.018868
2386.503829	16738.284408	59.023873
2385.694781	16629.499363	59.028877
2385.155533	16522.298280	59.033882
2384.395811	16418.739031	59.038887
2383.567331	16313.809911	59.043892
2382.822980	16218.830624	59.048897
2382.159732	16108.403939	59.053901
2381.462779	16022.193949	59.058906
2380.610268	15918.104619	59.063911
2380.069957	15816.295633	59.068916
2379.155622	15738.439358	59.073921
2378.646781	15641.423518	59.078925
2377.743366	15559.528544	59.083930
2377.218020	15462.545850	59.088935
2376.549776	15369.729001	59.093940
2375.981476	15274.132633	59.098945
2375.456570	15175.246839	59.103949
2374.338872	15095.790270	59.108954
2373.831167	15005.826437	59.113959
2373.249653	14911.534089	59.118964
2372.231875	14828.105094	59.123969
2371.951883	14719.145018	59.128973
2371.062663	14648.916886	59.133978
2370.430148	14556.350361	59.138983
2370.045264	14462.057614	59.143988
2369.018816	14393.677545	59.148993
2368.710917	14304.531773	59.153997
2367.926055	14203.620942	59.159002
2367.222656	14107.939725	59.164007
2366.814345	14015.437102	59.169012
2365.996646	13936.819190	59.174017
2365.308771	13840.741018	59.179021
2364.418348	13768.658131	59.184026
2363.710843	13672.984235	59.189031
2363.098934	13586.098443	59.194036
2362.504934	13514.550376	59.199041
2361.895099	13421.410159	59.204045
2361.003532	13339.232416	59.209050
2360.421100	13262.036479	59.214055
2359.835032	13184.733002	59.219060
2359.320826	13095.972146	59.224065
2358.589935	13000.179526	59.229069
2357.696457	12929.675110	59.234074
2356.910686	12832.746834	59.239079
2356.887726	12755.921446	59.244084
2355.770210	12679.558437	59.249089
2355.317624	12586.758027	59.254093
2354.524666	12509.484477	59.259098
2354.154175	12422.189854	59.264103
2353.494262	12346.290965	59.269108
2352.532863	12261.356263	59.274113
2352.242957	12177.487541	59.279117
2351.297046	12098.448722	59.284122
2350.693662	12011.230480	59.289127
2350.210524	11916.668323	59.294132
2349.146088	11848.014067	59.299137
2348.505134	11754.669440	59.304141
2347.863426	11679.955583	59.309146
2347.204045	11600.178372	59.314151
2346.696744	11516.648411	59.319156
2345.930418	11437.194382	59.324161
2345.244048	11352.117999	59.329165
2344.432189	11275.480638	59.334170
2344.095656	11202.971079	59.339175
2343.421946	11123.706004	59.344180
2342.164158	11054.626999	59.349185
2341.683506	10959.472742	59.354189
2341.102881	10890.916939	59.359194
2339.993248	10817.803566	59.364199
2339.691001	10742.066870	59.369204
2338.885152	10665.118025	59.374209
2338.536695	10585.100012	59.379213
2337.989886	10516.529108	59.384218
2337.102806	10445.916512	59.389223
2336.587804	10362.878203	59.394228
2335.643103	10287.800727	59.399233
2335.430840	10218.099977	59.404237
2334.583901	10151.626531	59.409242
2333.686743	10075.090856	59.414247
2333.336832	10005.416076	59.419252
2332.497992	9924.820941	59.424257
2331.612565	9848.012763	59.429261
2330.626052	9778.279833	59.434266
2330.311748	9707.738452	59.439271
2329.957251	9640.657023	59.444276
2329.024380	9565.834929	59.449281
2328.550784	9481.298286	59.454285
2327.734085	9431.509812	59.459290
2326.988862	9357.091736	59.464295
2326.425989	9282.968574	59.469300
2325.475732	9213.302738	59.474305
2325.192432	9126.397554	59.479309
2324.374811	9074.291763	59.484314
2323.693229	9003.368959	59.489319
2323.237761	8925.108825	59.494324
2322.448635	8856.068771	59.499329
2321.748869	8781.498031	59.504333
2320.953691	8731.629584	59.509338
2320.042482	8654.052179	59.514343
2319.372303	8583.367412	59.519348
2318.368288	8528.430967	59.524353
2317.947969	8456.253244	59.529357
2317.447551	8401.184545	59.534362
2316.842113	8342.925889	59.539367
2316.343634	8266.195416	59.544372
2315.617963	8213.446154	59.549377
2315.107230	8139.683666	59.554381
2314.526529	8070.806279	59.559386
2313.861398	8013.740891	59.564391
2313.127704	7929.470808	59.569396
2312.426520	7866.489711	59.574401
2312.025112	7801.271473	59.579405
2310.929006	7747.368956	59.584410
2310.479806	7675.291885	59.589415
2309.924986	7605.935287	59.594420
2309.360806	7543.897796	59.599425
2308.739472	7472.951805	59.604429
2307.778756	7396.232855	59.609434
2306.900416	7330.794926	59.614439
2306.542043	7268.443542	59.619444
2305.755973	7203.667565	59.624449
2305.230023	7136.794161	59.629453
2304.082430	7079.214104	59.634458
2303.664518	7008.457359	59.639463
2303.325106	6940.487200	59.644468
2302.417406	6888.369425	59.649473
2301.816602	6826.318651	59.654477
2301.215940	6763.432774	59.659482
2300.754422	6695.716585	59.664487
2299.829899	6630.415277	59.669492
2298.914896	6564.430444	59.674497
2298.778199	6488.952470	59.679501
2297.978927	6431.767718	59.684506
2297.294943	6366.572194	59.689511
2296.655139	6306.847215	59.694516
2295.408881	6239.706383	59.699521
2295.148264	6175.349278	59.704525
2294.640587	6113.314326	59.709530
2294.123058	6054.350274	59.714535
2293.351158	5988.816991	59.719540
2292.379873	5932.029805	59.724545
2292.116173	5861.119197	59.729549
2290.933615	5801.763136	59.734554
2290.679296	5742.234853	59.739559
2289.991144	5676.546909	59.744564
2289.168383	5610.718916	59.749569
2288.661983	5558.643930	59.754573
2287.787594	5489.289548	59.759578
2287.222416	5412.686930	59.764583
2286.389853	5356.118944	59.769588
2285.622598	5310.457537	59.774593
2285.218774	5236.550549	59.779597
2284.359081	5181.789761	59.784602
2283.304527	5117.081277	59.789607
2283.048975	5056.947852	59.794612
2282.592266	5018.870446	59.799617
2281.773901	4954.566892	59.804621
2281.069227	4890.269249	59.809626
2280.777737	4829.673173	59.814631
2280.007308	4788.869115	59.819636
2279.370069	4719.773348	59.824641
2278.575577	4640.549277	59.829645
2277.808253	4595.060458	59.834650
2276.909768	4539.234814	59.839655
2276.673248	4464.640302	59.844660
2275.877343	4420.036725	59.849665
2275.178010	4362.672216	59.854669
2274.581891	4306.199320	59.859674
2273.933619	4243.251283	59.864679
2273.693533	4179.686709	59.869684
2272.250902	4125.832272	59.874689
2271.981515	4064.854917	59.879693
2271.280876	4002.014014	59.884698
2270.740516	3940.341975	59.889703
2269.965785	3880.559900	59.894708
2269.470123	3839.166005	59.899713
2268.678282	3774.739592	59.904718
2267.933457	3715.844611	59.909722
2267.415239	3648.104872	59.914727
2266.821231	3590.984559	59.919732
2265.859956	3541.171008	59.924737
2265.570400	3477.700915	59.929742
2264.855821	3424.176005	59.934746
2263.987941	3365.173407	59.939751
2263.494328	3301.987221	59.944756
2263.057697	3237.962649	59.949761
2262.442600	3175.383794	59.954766
2261.425672	3119.457748	59.959770
2260.773568	3051.808246	59.964775
2260.436496	2984.844062	59.969780
2259.233061	2941.326925	59.974785
2258.798797	2879.353898	59.979790
2258.118062	2818.913029	59.984794
2257.560431	2767.894637	59.989799
2256.927466	2708.093291	59.994804
2255.814024	2657.439450	59.999809
2255.325773	2597.412150	60.004814
2254.751983	2542.190835	60.009818
2254.199876	2480.952639	60.014823
2253.595147	2420.202496	60.019828
2252.730984	2367.537126	60.024833
2251.950038	2303.606746	60.029838
2251.519762	2248.732826	60.034842
2250.344773	2201.548957	60.039847
2250.399618	2142.328453	60.044852
2249.223759	2093.358211	60.049857
2248.586584	2025.645648	60.054862
2247.738259	1983.351711	60.059866
2247.064969	1923.573385	60.064871
2246.465897	1869.901016	60.069876
2245.953866	1822.871860	60.074881
2245.216813	1769.243828	60.079886
2244.653113	1738.113677	60.084890
2243.776208	1673.645372	60.089895
2243.425968	1608.609658	60.094900
2242.277889	1581.907847	60.099905
2241.959657	1527.031490	60.104910
2241.173459	1468.037812	60.109914
2240.606317	1420.310613	60.114919
2240.092739	1370.668452	60.119924
2239.178886	1333.527902	60.124929
2238.668040	1272.267745	60.129934
2237.948545	1213.313409	60.134938
2237.046148	1166.324646	60.139943
2236.493154	1124.017121	60.144948
2235.697694	1073.490262	60.149953
2235.171288	1023.972750	60.154958
2234.421181	987.721767	60.159962
2233.539815	926.996513	60.164967
2233.200224	887.671793	60.169972
2232.256609	847.033185	60.174977
2231.609500	801.362880	60.179982
2231.045069	764.564183	60.184986
2230.222844	719.079612	60.189991
2229.380463	672.947102	60.194996
2228.795915	637.944909	60.200001
2228.494802	585.258195	60.205006
2227.883952	550.186270	60.210010
2227.162192	501.616156	60.215015
2226.479660	454.131213	60.220020
2225.805046	413.370732	60.225025
2225.165846	360.131353	60.230030
2224.270103	325.027899	60.235034
2223.618122	289.294522	60.240039
2222.839628	248.114184	60.245044
2221.866382	205.692300	60.250049
2221.222866	167.756534	60.255054
2220.510951	151.113426	60.260058
2219.887426	124.070927	60.265063
2219.327926	68.648606	60.270068
2218.360088	47.389683	60.275073
2217.286751	6.327767	60.280078
2216.677393	5.252830	60.285082
2214.848182	4.689928	60.290087
2211.890572	35.193892	60.295092
2211.121808	64.210611	60.300097
2211.177543	69.757142	60.305102
2211.629559	56.263040	60.310106
2211.341878	71.867784	60.315111
2211.253790	65.769780	60.320116
2210.835056	65.976565	60.325121
2210.234673	66.940685	60.330126
2209.321530	68.951010	60.335130
2208.047097	73.811306	60.340135
2207.140775	72.368754	60.345140
2206.117431	86.683637	60.350145
2205.668045	82.205633	60.355150
2205.350518	66.323199	60.360154
2204.748102	85.372913	60.365159
2204.521504	74.567805	60.370164
2203.626568	87.719079	60.375169
2203.206287	80.948400	60.380174
2202.363595	67.975051	60.385178
2201.507746	75.567914	60.390183
2201.094097	77.469043	60.395188
2200.165341	82.640346	60.400193
2199.592079	76.884221	60.405198
2199.358213	74.609629	60.410202
2198.174635	91.018807	60.415207
2197.760366	81.399323	60.420212
2196.936659	89.609964	60.425217
2197.027701	66.603009	60.430222
2196.353810	83.596767	60.435226
2195.160617	85.296726	60.440231
2195.045036	75.338140	60.445236
2194.097080	84.085707	60.450241
2193.533082	83.042995	60.455246
2192.677335	87.442661	60.460250
2191.549572	82.362681	60.465255
2191.215221	78.922944	60.470260
2190.395662	81.527106	60.475265
2189.247490	81.825961	60.480270
2189.607386	76.202487	60.485274
2189.081546	87.226340	60.490279
2188.626511	86.399722	60.495284
2187.228805	78.730750	60.500289
2186.707980	77.802611	60.505294
2186.343776	74.082196	60.510298
2185.382446	85.093137	60.515303
2184.676419	79.760183	60.520308
2183.944109	87.437532	60.525313
2183.227461	78.249207	60.530318
2183.086091	73.701847	60.535322
2181.908067	85.639682	60.540327
2181.206054	79.864565	60.545332
2180.728687	84.845997	60.550337
2179.830371	79.642894	60.555342
2180.082520	88.804023	60.560346
2179.266769	78.251649	60.565351
2178.043342	74.836274	60.570356
2177.396852	82.254013	60.575361
2177.253421	83.331720	60.580366
2176.903137	85.374181	60.585370
2175.338432	85.191944	60.590375
2174.872994	78.989808	60.595380
2174.371069	79.428984	60.600385
2173.891505	83.407868	60.605390
2173.093361	71.178058	60.610394
2171.937704	83.025617	60.615399
2171.816038	73.586795	60.620404
2171.358094	77.874471	60.625409
2170.564722	76.519663	60.630414
2169.581256	76.327215	60.635418
2168.924187	87.359274	60.640423
2168.672372	79.303524	60.645428
2167.752223	80.479227	60.650433
2167.002885	71.680858	60.655438
2166.477302	67.471988	60.660442
2165.891906	87.167102	60.665447
2165.392103	61.365051	60.670452
2163.878869	83.785562	60.675457
2163.682162	82.667239	60.680462
2163.467777	75.285192	60.685466
2163.083654	80.631860	60.690471
2161.832696	74.864998	60.695476
2160.375804	84.934324	60.700481
2160.444004	80.293794	60.705486
2160.207933	76.466326	60.710490
2159.390109	77.958520	60.715495
2158.824647	79.964161	60.720500
2157.633189	86.990571	60.725505
2156.959960	76.443980	60.730510
2157.034752	73.038682	60.735514
2155.590281	79.950696	60.740519
2155.281650	72.588334	60.745524
2154.685841	77.572789	60.750529
2154.288221	70.981450	60.755534
2153.200459	79.330178	60.760538
2151.953779	82.801596	60.765543
2152.526299	71.641069	60.770548
2151.707054	78.469657	60.775553
2150.376225	76.020619	60.780558
2149.967077	63.844221	60.785562
2149.088451	82.723299	60.790567
2148.593839	76.584143	60.795572
2147.750545	82.471998	60.800577
2147.027894	78.915687	60.805582
2146.983391	77.300154	60.810586
2146.049825	85.299586	60.815591
2145.271027	78.910641	60.820596
2144.751466	76.922645	60.825601
2144.054190	87.939010	60.830606
2143.851789	79.279364	60.835610
2142.916270	85.279620	60.840615
2142.720854	83.495650	60.845620
2141.692345	80.762117	60.850625
2141.180665	79.323203	60.855630
2140.671517	80.283902	60.860634
2138.991526	90.152105	60.865639
2138.767551	79.275631	60.870644
2137.793118	78.197131	60.875649
2137.397475	76.164245	60.880654
2137.099031	80.860262	60.885658
2135.921269	83.617463	60.890663
2135.758842	73.015068	60.895668
2134.906800	81.673317	60.900673
2134.480446	86.280825	60.905678
2133.747333	66.257229	60.910682
2133.243376	86.202759	60.915687
2132.498742	74.916911	60.920692
2131.830472	86.963109	60.925697
2130.931634	79.899387	60.930702
2130.263055	73.723187	60.935706
2129.115808	83.323946	60.940711
2129.153075	85.005315	60.945716
2128.472544	81.987927	60.950721
2127.509604	76.694179	60.955726
2126.960644	74.460128	60.960730
2126.124600	90.129816	60.965735
2126.015648	75.204585	60.970740
2125.456451	69.163991	60.975745
2124.802772	73.490612	60.980750
2124.096427	76.575124	60.985754
2122.862211	80.246416	60.990759
2121.805922	79.920468	60.995764
2121.655427	78.693896	61.000769
2121.428206	75.894733	61.005774
2120.440671	73.651427	61.010778
2119.909360	73.395140	61.015783
2119.216981	72.186743	61.020788
2118.802897	83.210212	61.025793
2117.822270	75.514530	61.030798
2117.776141	71.390438	61.035802
2116.239023	76.517948	61.040807
2115.625377	68.877578	61.045812
2114.643525	69.927476	61.050817
2114.187242	81.325053	61.055822
2114.318081	76.497975	61.060826
2113.297381	80.942757	61.065831
2112.921223	76.918336	61.070836
2112.025154	77.060533	61.075841
2111.199627	75.054863	61.080846
2111.177799	57.802545	61.085850
2109.406059	77.547119	61.090855
2108.747186	76.765474	61.095860
2108.311765	72.163859	61.100865
2108.221069	76.352271	61.105870
2107.069276	74.406257	61.110874
2106.179333	72.801876	61.115879
2105.892992	65.491182	61.120884
2105.438987	76.595094	61.125889
2104.885830	80.849003	61.130894
2104.151360	61.867961	61.135898
2103.589411	71.970333	61.140903
2103.044800	70.766877	61.145908
2101.348873	70.540854	61.150913
2101.118886	66.371825	61.155918
2100.571570	77.384893	61.160922
2099.607961	76.506531	61.165927
2099.376107	80.157550	61.170932
2098.522646	69.475588	61.175937
2098.216114	68.472465	61.180942
2098.014392	67.610400	61.185946
2097.442834	79.218646	61.190951
2096.344429	80.036322	61.195956
2095.096629	79.095828	61.200961
2094.177751	79.684753	61.205966
2093.920588	74.949204	61.210970
2093.013423	80.864553	61.215975
2092.385033	65.797845	61.220980
2092.004969	74.630355	61.225985
2091.746824	73.258449	61.230990
2091.545583	69.188933	61.235994
2090.644762	72.994985	61.240999
2089.886797	66.664258	61.246004
2088.732040	68.809150	61.251009
2087.502929	70.816037	61.256014
2087.440623	61.301588	61.261018
2086.556202	70.214127	61.266023
2086.571168	70.766831	61.271028
2085.811972	76.928347	61.276033
2085.186471	74.983982	61.281038
2084.074004	74.813613	61.286042
2083.266272	72.267413	61.291047
2082.709735	71.799103	61.296052
2082.007379	72.892968	61.301057
2081.329826	92.503370	61.306062
2081.143372	63.557789	61.311066
2080.339516	83.833164	61.316071
2080.392714	71.952404	61.321076
2079.390175	66.696502	61.326081
2078.204656	81.926503	61.331086
2077.471064	63.073061	61.336090
2076.695236	70.202265	61.341095
2076.234171	66.588701	61.346100
2075.962554	64.482533	61.351105
2075.208192	82.725341	61.356110
2074.090750	69.644267	61.361114
2073.026370	70.905963	61.366119
2072.404895	71.671620	61.371124
2072.476252	70.288429	61.376129
2071.613511	67.681580	61.381134
2071.230367	75.032313	61.386138
2070.590271	70.993017	61.391143
2070.282516	68.194026	61.396148
2069.461469	72.230264	61.401153
2068.102278	78.393960	61.406158
2067.530802	71.361895	61.411162
2066.873672	78.201046	61.416167
2066.514218	61.516372	61.421172
2066.113265	78.422668	61.426177
2065.626629	83.069710	61.431182
2064.758365	78.298680	61.436186
2063.868996	81.210409	61.441191
2063.079086	70.529416	61.446196
2062.773821	73.329531	61.451201
2061.788706	81.743998	61.456206
2060.876691	76.620385	61.461210
2059.982291	72.859556	61.466215
2059.346161	76.596807	61.471220
2059.158988	71.845426	61.476225
2058.443667	77.180008	61.481230
2058.273680	65.708394	61.486234
2057.455921	73.591699	61.491239
2056.821711	63.844748	61.496244
2055.936349	72.598180	61.501249
2054.601594	74.957722	61.506254
2054.311048	81.030684	61.511258
2053.431864	72.347576	61.516263
2053.075399	68.633843	61.521268
2053.130031	72.015482	61.526273
2052.186826	69.993816	61.531278
2052.171452	69.154219	61.536282
2050.633174	80.220478	61.541287
2049.921430	75.214891	61.546292
2048.996278	68.303612	61.551297
2048.385174	67.222679	61.556302
2048.292504	66.355928	61.561306
2047.567477	63.424473	61.566311
2046.461061	65.744628	61.571316
2045.757229	70.590131	61.576321
2044.678122	77.663401	61.581326
2044.571631	62.849768	61.586330
2043.986781	71.240136	61.591335
2043.822890	62.397795	61.596340
2043.220493	67.471617	61.601345
2041.641611	77.276510	61.606350
2041.248703	69.634247	61.611354
2040.475747	68.348778	61.616359
2040.030306	81.739389	61.621364
2039.656812	78.955564	61.626369
2039.020792	72.072515	61.631374
2038.050714	85.987916	61.636378
2037.006995	75.042871	61.641383
2036.789753	66.674175	61.646388
2036.241804	73.407697	61.651393
2035.563527	78.860979	61.656398
2035.292492	67.268216	61.661402
2034.052537	72.695521	61.666407
2032.768471	69.586297	61.671412
2032.344737	82.520900	61.676417
2031.707531	78.107434	61.681422
2031.516774	70.742160	61.686426
2030.979673	77.267391	61.691431
2030.411985	76.561177	61.696436
2030.216478	70.164861	61.701441
2028.816680	84.840710	61.706446
2028.137937	77.969173	61.711450
2027.320968	74.946662	61.716455
2027.077116	72.033461	61.721460
2026.736095	72.432936	61.726465
2025.253812	79.437740	61.731470
2024.435505	70.992555	61.736474
2023.557479	70.802350	61.741479
2023.518808	69.755150	61.746484
2022.804633	73.000191	61.751489
2022.218491	80.990245	61.756494
2022.130165	66.716177	61.761498
2021.068259	74.783310	61.766503
2019.847376	71.435417	61.771508
2019.445508	83.690070	61.776513
2018.983021	81.890153	61.781518
2018.590755	68.386531	61.786522
2018.198284	66.409932	61.791527
2017.029623	71.187294	61.796532
2016.403307	77.788185	61.801537
2015.409015	71.310495	61.806542
2014.986611	80.436723	61.811546
2014.364776	76.523848	61.816551
2013.481782	66.513634	61.821556
2012.702649	73.569265	61.826561
2011.803128	78.024808	61.831566
2011.521315	77.850365	61.836570
2010.800435	77.639955	61.841575
2010.593489	74.290411	61.846580
2010.268463	69.825831	61.851585
2009.434514	78.359816	61.856590
2008.425916	74.320677	61.861594
2007.642675	79.543054	61.866599
2007.120830	67.449233	61.871604
2006.885847	69.836094	61.876609
2005.784700	80.224321	61.881614
2005.072003	66.413609	61.886618
2004.288313	65.492537	61.891623
2003.588929	76.372059	61.896628
2003.094327	75.968050	61.901633
2002.574518	73.272106	61.906638
2001.476711	66.191140	61.911642
2000.520188	76.769292	61.916647
2000.166945	77.719464	61.921652
1999.854585	70.294650	61.926657
1999.079974	66.874363	61.931662
1998.798605	59.835702	61.936666
1998.466412	71.875870	61.941671
1997.254144	71.962640	61.946676
1996.463468	68.612708	61.951681
1995.703121	74.750772	61.956686
1995.221278	68.759436	61.961690
1994.697753	77.966365	61.966695
1993.537695	71.246925	61.971700
1992.468140	71.916568	61.976705
1992.046601	84.194843	61.981710
1992.042735	69.043243	61.986714
1991.067614	65.541247	61.991719
1990.831260	71.291807	61.996724
1990.516383	72.071895	62.001729
1989.253823	71.229985	62.006734
1988.598145	63.332990	62.011738
1987.752393	78.106982	62.016743
1987.108906	72.925011	62.021748
1986.913105	62.707975	62.026753
1986.082186	74.953452	62.031758
1985.000488	66.703047	62.036762
1984.137888	77.763012	62.041767
1983.426930	60.861356	62.046772
1983.048419	70.888895	62.051777
1982.298776	71.503035	62.056782
1982.431255	66.505398	62.061786
1981.840324	76.396353	62.066791
1981.322937	68.903166	62.071796
1980.192943	65.998162	62.076801
1979.267516	81.368250	62.081806
1978.817465	70.888803	62.086810
1978.061852	69.373529	62.091815
1976.630710	73.145522	62.096820
1975.954692	71.243895	62.101825
1975.706620	75.480937	62.106830
1975.412481	64.196195	62.111834
1974.767506	67.583220	62.116839
1974.413590	66.535597	62.121844
1974.358069	72.979667	62.126849
1972.786437	72.950030	62.131854
1972.142661	68.931847	62.136858
1971.593495	77.259796	62.141863
1970.851171	66.254339	62.146868
1969.617182	69.093067	62.151873
1968.695759	65.421715	62.156878
1968.738899	69.972062	62.161882
1968.029404	72.145673	62.166887
1967.908566	60.481785	62.171892
1967.599755	65.226759	62.176897
1966.399440	71.887226	62.181902
1965.622182	56.561947	62.186906
1964.965597	62.659890	62.191911
1964.278780	70.978147	62.196916
1963.205801	70.941904	62.201921
1962.194168	70.131137	62.206926
1961.809852	59.147708	62.211930
1960.981451	70.911839	62.216935
1961.066747	62.648094	62.221940
1960.410060	61.459307	62.226945
1960.142126	68.432229	62.231950
1959.305168	66.398465	62.236954
1958.387850	72.799560	62.241959
1957.523343	72.670307	62.246964
1957.185571	60.304452	62.251969
1956.040948	68.646494	62.256974
1955.419204	70.591724	62.261978
1954.490393	75.763105	62.266983
1953.935609	67.175201	62.271988
1953.621177	63.669270	62.276993
1953.098848	76.897050	62.281998
1952.837376	61.023145	62.287002
1951.673990	71.072772	62.292007
1950.560893	71.566425	62.297012
1950.370124	65.011683	62.302017
1949.460185	77.130946	62.307022
1949.532829	74.951225	62.312026
1948.326806	79.283559	62.317031
1947.486949	81.126226	62.322036
1946.583201	70.816571	62.327041
1946.005154	67.013456	62.332046
1945.706040	68.965821	62.337050
1945.201908	79.571522	62.342055
1944.830563	63.327145	62.347060
1944.185039	70.867759	62.352065
1942.823839	69.426547	62.357070
1942.332325	64.042282	62.362074
1941.675060	64.484081	62.367079
1940.628718	67.307227	62.372084
1940.247116	61.019312	62.377089
1939.356610	70.563602	62.382094
1939.239273	72.936523	62.387098
1938.570808	75.426889	62.392103
1937.999261	68.673983	62.397108
1937.137157	61.978240	62.402113
1936.286286	71.891536	62.407118
1936.066103	69.464999	62.412122
1935.644506	80.210557	62.417127
1934.340504	65.072971	62.422132
1933.754145	67.091432	62.427137
1933.110897	71.258747	62.432142
1933.041015	68.354211	62.437146
1931.651905	77.611819	62.442151
1930.814775	69.868217	62.447156
1929.992461	58.982707	62.452161
1929.430125	61.984480	62.457166
1929.319834	69.880081	62.462170
1928.772183	78.028031	62.467175
1928.284338	72.763027	62.472180
1927.302371	66.601952	62.477185
1926.452963	78.744727	62.482190
1925.828749	66.574148	62.487194
1925.183921	75.680496	62.492199
1924.788126	67.302317	62.497204
1923.762387	62.755031	62.502209
1922.728754	71.423226	62.507214
1922.541115	73.258554	62.512218
1922.131231	75.032973	62.517223
1921.481595	70.282486	62.522228
1921.087247	67.820523	62.527233
1919.823454	77.875065	62.532238
1919.157988	70.356518	62.537242
1919.012023	76.288266	62.542247
1918.052482	81.067164	62.547252
1917.019242	70.528933	62.552257
1915.998483	79.064210	62.557262
1915.594339	65.322822	62.562266
1915.324792	77.977493	62.567271
1914.973843	73.903379	62.572276
1914.584785	67.812183	62.577281
1913.103715	69.764532	62.582286
1912.754350	67.658111	62.587290
1912.309645	66.210191	62.592295
1911.497208	66.668747	62.597300
1910.778345	69.772639	62.602305
1909.420116	77.388556	62.607310
1909.436922	65.786398	62.612314
1909.021966	69.701444	62.617319
1908.286908	76.198195	62.622324
1907.596044	71.763325	62.627329
1906.413635	72.600721	62.632334
1905.961957	73.656412	62.637338
1905.389879	74.754871	62.642343
1904.926007	64.411679	62.647348
1904.250736	65.009303	62.652353
1902.708469	74.571919	62.657358
1902.248133	78.803241	62.662362
1901.825180	73.702974	62.667367
1901.454355	74.275922	62.672372
1901.189377	63.863312	62.677377
1900.641926	68.136844	62.682382
1899.721888	58.066338	62.687386
1899.133976	71.367602	62.692391
1898.519783	80.921657	62.697396
1897.519942	65.433049	62.702401
1896.214749	70.686272	62.707406
1896.095025	62.412504	62.712410
1895.660553	70.436835	62.717415
1895.060113	75.980284	62.722420
1894.448588	60.355924	62.727425
1893.463805	75.623485	62.732430
1892.810395	67.454938	62.737434
1892.169234	68.118109	62.742439
1891.787710	59.420726	62.747444
1890.732270	67.250338	62.752449
1889.757817	64.415297	62.757454
1889.560922	64.156427	62.762458
1889.154987	69.427734	62.767463
1888.408733	78.107088	62.772468
1887.873259	63.684849	62.777473
1886.802348	73.838084	62.782478
1886.237280	73.145678	62.787482
1885.861761	82.136744	62.792487
1885.146004	69.528147	62.797492
1884.371084	65.658538	62.802497
1883.641296	73.075351	62.807502
1883.043005	72.328299	62.812506
1882.777782	64.829800	62.817511
1881.565604	73.743962	62.822516
1880.601726	69.918543	62.827521
1880.062962	82.310042	62.832526
1879.773766	58.865243	62.837530
1879.495544	62.359634	62.842535
1878.088660	62.619274	62.847540
1877.494313	66.512343	62.852545
1876.852568	75.632400	62.857550
1876.505096	61.457851	62.862554
1875.976598	64.540990	62.867559
1874.989029	66.796615	62.872564
1874.275823	72.812109	62.877569
1873.363284	74.045046	62.882574
1872.962260	69.455368	62.887578
1872.694559	65.741767	62.892583
1871.983245	70.151700	62.897588
1870.875038	56.093203	62.902593
1869.947258	77.340692	62.907598
1869.825061	64.759291	62.912602
1869.339802	70.197727	62.917607
1868.703575	74.747122	62.922612
1867.673766	68.270408	62.927617
1866.928869	68.218385	62.932622
1866.411819	67.076835	62.937626
1865.942805	61.610174	62.942631
1865.157665	62.805541	62.947636
1864.587991	69.224004	62.952641
1863.631681	71.529862	62.957646
1863.275791	66.426844	62.962650
1862.439867	61.827373	62.967655
1861.852111	62.677605	62.972660
1860.847604	64.611088	62.977665
1859.970793	72.201051	62.982670
1859.699573	62.033859	62.987674
1859.310221	62.220265	62.992679
1858.782704	63.914024	62.997684
1858.767623	63.906974	63.002689
1857.442009	76.994224	63.007694
1856.724702	68.198775	63.012698
1855.959233	71.401539	63.017703
1854.933245	75.456181	63.022708
1854.390097	62.900619	63.027713
1853.255846	76.067869	63.032718
1853.305162	70.581988	63.037722
1853.043818	66.626118	63.042727
1852.000936	73.285287	63.047732
1851.189717	68.066915	63.052737
1850.143131	73.514055	63.057742
1849.925495	67.431925	63.062746
1849.369555	69.311539	63.067751
1848.926522	66.876242	63.072756
1847.918540	63.634976	63.077761
1846.582742	64.305949	63.082766
1846.364939	64.707959	63.087770
1845.868912	62.938634	63.092775
1845.551262	69.028517	63.097780
1845.421242	59.002907	63.102785
1844.225674	70.609322	63.107790
1843.349973	76.049834	63.112794
1843.246001	68.869497	63.117799
1841.818763	70.028054	63.122804
1841.224614	68.871943	63.127809
1840.326278	68.817482	63.132814
1840.073260	67.837434	63.137818
1839.611818	64.097831	63.142823
1838.720446	68.438594	63.147828
1838.157292	64.514878	63.152833
1837.446390	78.518467	63.157838
1837.057708	56.628515	63.162842
1836.700873	61.147743	63.167847
1835.365493	69.434962	63.172852
1834.658631	57.427351	63.177857
1834.020151	69.981325	63.182862
1833.578384	63.835442	63.187866
1832.619756	61.261249	63.192871
1831.762126	73.648182	63.197876
1831.359231	59.009386	63.202881
1831.055241	73.069782	63.207886
1830.541301	62.439687	63.212890
1829.361465	74.040459	63.217895
1828.419933	74.224662	63.222900
1828.206689	56.562846	63.227905
1827.625806	66.501100	63.232910
1827.099351	65.518739	63.237914
1826.247722	63.887877	63.242919
1825.158585	63.165161	63.247924
1824.882982	62.850987	63.252929
1824.174202	68.761714	63.257934
1823.749467	66.094868	63.262938
1822.950390	59.523200	63.267943
1822.002344	54.711325	63.272948
1821.529716	61.166419	63.277953
1820.975018	68.175415	63.282958
1820.658845	60.290801	63.287962
1819.556732	61.875538	63.292967
1818.880474	69.561393	63.297972
1818.805927	63.237363	63.302977
1817.404594	59.733732	63.307982
1816.268250	64.077129	63.312986
1816.072339	63.105361	63.317991
1815.276353	76.799202	63.322996
1814.957717	67.689744	63.328001
1814.735100	61.151118	63.333006
1813.919013	66.121721	63.338010
1812.898388	71.840705	63.343015
1812.284270	62.558982	63.348020
1812.042323	55.455754	63.353025
1811.507783	71.788763	63.358030
1810.293654	59.697710	63.363034
1809.695421	67.420060	63.368039
1809.228561	63.331259	63.373044
1808.666148	50.999544	63.378049
1807.494954	63.464645	63.383054
1807.042357	65.767806	63.388058
1806.478727	55.293841	63.393063
1805.421380	66.971354	63.398068
1804.650666	64.234877	63.403073
1803.469150	76.217529	63.408078
1803.582760	65.350606	63.413082
1803.511900	57.808648	63.418087
1802.649776	61.097730	63.423092
1802.384344	62.857111	63.428097
1801.082793	64.539753	63.433102
1800.354704	68.163928	63.438106
1799.910071	59.678428	63.443111
1799.125389	57.625381	63.448116
1798.266962	66.549627	63.453121
1797.254269	61.043162	63.458126
1796.732912	61.217424	63.463130
1796.620731	66.528822	63.468135
1795.753185	58.194052	63.473140
1795.733702	59.890726	63.478145
1794.356984	71.685188	63.483150
1793.884908	64.380393	63.488154
1793.447801	68.158628	63.493159
1792.738690	62.369005	63.498164
1791.582074	60.409711	63.503169
1790.842995	66.454558	63.508174
1790.605558	63.770593	63.513178
1789.915440	60.322768	63.518183
1789.411595	65.101877	63.523188
1788.734244	62.222853	63.528193
1787.557675	74.996314	63.533198
1787.155591	73.007089	63.538202
1786.883078	68.124222	63.543207
1786.089912	62.865164	63.548212
1785.209191	54.688603	63.553217
1784.809659	69.366531	63.558222
1783.863734	64.839746	63.563226
1783.531246	63.146961	63.568231
1782.410043	61.752876	63.573236
1782.191646	58.849859	63.578241
1781.389773	66.823734	63.583246
1780.873290	63.433490	63.588250
1779.985158	56.584258	63.593255
1779.053081	68.440574	63.598260
1778.715768	65.367214	63.603265
1778.120124	66.258139	63.608270
1777.225635	60.983637	63.613274
1776.312614	65.138629	63.618279
1775.684167	71.591669	63.623284
1775.564270	66.851719	63.628289
1775.229945	69.214947	63.633294
1774.329735	60.197855	63.638298
1772.953434	66.077404	63.643303
1772.400027	67.062543	63.648308
1772.369417	52.664259	63.653313
1771.272505	65.595371	63.658318
1770.683042	51.571248	63.663322
1769.939990	61.312918	63.668327
1769.404058	58.226949	63.673332
1769.272487	50.040237	63.678337
1767.957572	67.459058	63.683342
1766.848183	62.034191	63.688346
1766.450687	50.073675	63.693351
1765.836734	69.454773	63.698356
1765.584793	65.180471	63.703361
1765.306472	66.675410	63.708366
1763.998309	63.347815	63.713370
1763.340574	66.998672	63.718375
1762.644006	51.140311	63.723380
1762.420213	57.082832	63.728385
1761.776458	50.133306	63.733390
1760.546530	57.657943	63.738394
1760.034306	60.989239	63.743399
1759.634706	70.901868	63.748404
1759.199622	59.338381	63.753409
1758.103881	61.942368	63.758414
1757.404718	63.735940	63.763418
1757.123393	57.370643	63.768423
1756.338974	72.068697	63.773428
1755.724548	55.546041	63.778433
1754.710577	63.011158	63.783438
1754.399519	55.067404	63.788442
1753.888131	68.979389	63.793447
1752.661665	62.035669	63.798452
1751.777347	56.518301	63.803457
1750.972623	67.206435	63.808462
1750.665328	68.497830	63.813466
1750.343337	57.857780	63.818471
1749.811075	59.273205	63.823476
1749.302057	57.182704	63.828481
1748.319697	64.699572	63.833486
1747.699456	55.176010	63.838490
1747.107851	68.797974	63.843495
1746.053011	63.045926	63.848500
1745.466105	55.880803	63.853505
1745.012738	52.811690	63.858510
1744.281354	56.890538	63.863514
1744.025312	55.158813	63.868519
1742.667130	52.685955	63.873524
1742.066312	52.319365	63.878529
1741.634210	58.704956	63.883534
1741.037692	59.912979	63.888538
1740.820207	47.644779	63.893543
1739.260151	68.197939	63.898548
1738.936472	58.289829	63.903553
1738.041430	57.340794	63.908558
1737.783467	56.049322	63.913562
1737.296884	54.228060	63.918567
1736.148032	61.090162	63.923572
1735.696139	51.481526	63.928577
1735.299757	56.620445	63.933582
1734.723686	55.488297	63.938586
1734.064995	61.416314	63.943591
1733.105512	61.163454	63.948596
1732.962365	50.053487	63.953601
1731.514182	72.821740	63.958606
1730.558689	65.929609	63.963610
1730.330307	56.518852	63.968615
1729.809618	66.624166	63.973620
1729.422455	45.386858	63.978625
1728.803597	55.033117	63.983630
1727.503692	60.222496	63.988634
1727.258893	52.692405	63.993639
1726.272537	60.899004	63.998644
1726.134917	49.507478	64.003649
1724.828957	47.745391	64.008654
1724.137301	60.173779	64.013658
1723.753543	54.938030	64.018663
1723.167269	62.497649	64.023668
1722.935215	56.804165	64.028673
1721.903376	61.238228	64.033678
1721.072008	57.223107	64.038682
1720.518689	53.411397	64.043687
1719.877425	55.414967	64.048692
1719.489152	49.577573	64.053697
1718.354606	55.497590	64.058702
1717.619511	52.353384	64.063706
1717.067470	50.977740	64.068711
1716.630666	54.033726	64.073716
1716.149858	50.412341	64.078721
1715.333282	65.065040	64.083726
1714.627992	64.653550	64.088730
1714.146208	52.573977	64.093735
1713.363849	60.158431	64.098740
1712.465922	43.933132	64.103745
1711.534135	44.210441	64.108750
1710.922015	64.278757	64.113754
1710.811730	53.764361	64.118759
1710.400883	61.032781	64.123764
1709.685786	59.355045	64.128769
1708.557922	56.514483	64.133774
1708.093978	54.110920	64.138778
1707.314459	60.550116	64.143783
1705.836601	58.438466	64.148788
1705.531258	58.785008	64.153793
1705.136788	52.451885	64.158798
1704.720588	64.749802	64.163802
1704.535588	59.291686	64.168807
1704.057994	58.943379	64.173812
1703.217258	49.393358	64.178817
1702.250086	55.515445	64.183822
1701.029269	59.344049	64.188826
1700.509627	49.378774	64.193831
1699.677511	61.608712	64.198836
1699.261958	53.679990	64.203841
1698.802010	62.052137	64.208846
1698.507851	61.015563	64.213850
1697.383703	50.815156	64.218855
1696.485992	58.037908	64.223860
1696.217586	53.417746	64.228865
1695.650736	48.501230	64.233870
1694.808947	52.433629	64.238874
1694.051193	52.110899	64.243879
1693.390745	56.016075	64.248884
1693.277052	45.713529	64.253889
1692.005834	62.007425	64.258894
1691.495942	54.101572	64.263898
1691.020097	49.929077	64.268903
1690.258273	52.074798	64.273908
1689.535957	51.546177	64.278913
1688.577470	60.188308	64.283918
1687.747742	50.261249	64.288922
1687.794818	52.439333	64.293927
1686.990127	51.816569	64.298932
1686.441457	62.918181	64.303937
1685.787514	57.020491	64.308942
1684.906394	54.754153	64.313946
1684.684157	51.064899	64.318951
1683.353272	47.255284	64.323956
1682.915577	49.955042	64.328961
1682.419694	61.270607	64.333966
1681.329603	57.462166	64.338970
1680.717663	53.215100	64.343975
1679.674304	60.033658	64.348980
1679.430419	46.896078	64.353985
1679.099729	46.582787	64.358990
1678.614830	60.541019	64.363994
1677.828997	56.906592	64.368999
1676.770771	62.046569	64.374004
1676.021702	57.412874	64.379009
1675.759167	57.006760	64.384014
1675.104362	68.027469	64.389018
1674.301041	60.469407	64.394023
1673.400083	64.133685	64.399028
1673.107484	55.843257	64.404033
1672.487087	55.142343	64.409038
1671.991548	70.341695	64.414042
1671.141965	59.574164	64.419047
1669.928013	63.974096	64.424052
1669.685880	63.123218	64.429057
1669.161906	65.492927	64.434062
1667.987796	60.507298	64.439066
1667.653386	52.821149	64.444071
1666.767342	64.403684	64.449076
1666.819575	62.484236	64.454081
1665.743924	61.217002	64.459086
1664.942080	55.852141	64.464090
1664.521167	49.367118	64.469095
1664.128222	64.513901	64.474100
1663.395053	58.261390	64.479105
1662.330633	59.280414	64.484110
1661.664807	69.694204	64.489114
1661.406364	56.294018	64.494119
1659.949129	55.978330	64.499124
1659.415556	51.198455	64.504129
1658.723472	61.649525	64.509134
1658.518259	52.113685	64.514138
1658.550202	54.213751	64.519143
1657.381970	71.525737	64.524148
1656.478519	57.384378	64.529153
1655.595453	56.482353	64.534158
1655.089432	45.400083	64.539162
1654.719410	42.629972	64.544167
1653.584749	63.804679	64.549172
1652.795980	52.404637	64.554177
1652.623624	53.370270	64.559182
1652.106522	57.850319	64.564186
1651.506609	44.895450	64.569191
1650.302040	59.567209	64.574196
1649.546902	53.158931	64.579201
1649.182300	54.005299	64.584206
1648.779759	55.173068	64.589210
1648.171480	59.885210	64.594215
1647.261360	63.396417	64.599220
1646.831448	53.852118	64.604225
1645.817340	62.086803	64.609230
1644.516543	60.469008	64.614234
1643.989563	56.350374	64.619239
1643.662179	61.095164	64.624244
1643.778937	64.536291	64.629249
1643.054731	57.293666	64.634254
1642.025922	59.885489	64.639258
1641.120615	52.435104	64.644263
1640.443791	58.539473	64.649268
1640.157873	55.763886	64.654273
1640.018913	50.886641	64.659278
1638.959506	56.381613	64.664282
1638.283894	45.755197	64.669287
1637.012923	62.422789	64.674292
1636.411689	52.809519	64.679297
1635.843970	50.821405	64.684302
1635.196732	63.081909	64.689306
1635.005047	55.467706	64.694311
1634.190669	61.906149	64.699316
1633.001008	57.320381	64.704321
1632.802212	51.788779	64.709326
1632.066211	61.880995	64.714330
1631.793343	48.678647	64.719335
1630.231071	57.632735	64.724340
1629.857318	51.296338	64.729345
1629.389275	54.879242	64.734350
1628.649880	58.338104	64.739354
1628.505735	47.045400	64.744359
1627.722263	55.790622	64.749364
1626.950978	48.563371	64.754369
1626.130745	56.488154	64.759374
1625.080843	53.953775	64.764378
1624.480367	50.725139	64.769383
1623.516161	68.081986	64.774388
1623.161609	63.120721	64.779393
1622.655764	57.541705	64.784398
1622.421568	55.972095	64.789402
1621.908631	57.414435	64.794407
1620.995634	54.360018	64.799412
1620.307481	57.276182	64.804417
1620.009841	58.657514	64.809422
1618.397604	67.107069	64.814426
1618.037235	58.556195	64.819431
1617.275420	69.362111	64.824436
1616.904540	61.211854	64.829441
1616.756902	62.064760	64.834446
1615.635291	58.335469	64.839450
1615.202952	53.238340	64.844455
1614.147976	55.410152	64.849460
1612.685698	51.678215	64.854465
1612.464184	58.249548	64.859470
1611.894044	63.802418	64.864474
1611.807405	56.098995	64.869479
1610.975186	58.713213	64.874484
1610.696582	64.204001	64.879489
1609.986874	45.813770	64.884494
1608.560120	60.998630	64.889498
1608.476968	57.952728	64.894503
1607.831091	59.023549	64.899508
1606.712586	53.802051	64.904513
1606.211429	59.224119	64.909518
1605.619035	53.811816	64.914522
1605.474318	46.530764	64.919527
1604.171638	61.375811	64.924532
1603.444135	57.577610	64.929537
1602.951123	46.327718	64.934542
1602.211346	51.817652	64.939546
1602.105603	47.602151	64.944551
1600.722682	53.637359	64.949556
1600.029330	54.643188	64.954561
1599.702849	47.614928	64.959566
1599.432369	50.767501	64.964570
1598.615743	42.290702	64.969575
1597.337296	49.707995	64.974580
1596.802329	43.055040	64.979585
1596.544218	40.519459	64.984590
1595.669725	55.771117	64.989594
1594.976975	48.449403	64.994599
1594.128447	47.355842	64.999604
1593.679663	52.991928	65.004609
1593.125668	40.409816	65.009614
1592.608744	59.236200	65.014618
1591.958965	55.770989	65.019623
1591.108980	66.849522	65.024628
1591.008494	51.576171	65.029633
1589.591639	52.053581	65.034638
1588.372516	52.933217	65.039642
1588.181013	51.976538	65.044647
1587.760487	58.921670	65.049652
1587.403404	56.072246	65.054657
1586.932900	53.039002	65.059662
1585.839769	61.795588	65.064666
1585.363881	48.295939	65.069671
1584.727246	48.565824	65.074676
1583.461139	45.551753	65.079681
1582.957990	44.802274	65.084686
1581.909403	51.944949	65.089690
1581.968578	47.534524	65.094695
1581.509162	60.023799	65.099700
1580.674360	51.918877	65.104705
1580.124244	57.758712	65.109710
1579.133797	60.681914	65.114714
1578.995246	47.204365	65.119719
1577.376051	53.247161	65.124724
1576.954031	50.084798	65.129729
1576.629652	66.657215	65.134734
1576.005837	58.121399	65.139738
1575.602095	60.806319	65.144743
1574.393457	61.509263	65.149748
1573.802528	54.083073	65.154753
1573.475479	75.954207	65.159758
1572.419377	67.266304	65.164762
1572.049515	55.892775	65.169767
1571.238632	57.587454	65.174772
1570.781510	59.821985	65.179777
1570.310011	50.929256	65.184782
1569.178407	61.043336	65.189786
1568.636945	49.492083	65.194791
1567.876035	52.501815	65.199796
1567.567160	57.412394	65.204801
1566.383478	60.151847	65.209806
1565.325219	59.160999	65.214810
1565.131794	54.953122	65.219815
1564.599204	64.757581	65.224820
1564.194188	61.349679	65.229825
1563.873620	52.942300	65.234830
1562.376523	56.191995	65.239834
1561.837542	53.961224	65.244839
1561.464587	55.390796	65.249844
1561.025405	39.805441	65.254849
1560.358220	58.589468	65.259854
1559.053820	59.287135	65.264858
1558.724137	45.458357	65.269863
1558.374518	51.903393	65.274868
1557.259697	52.878429	65.279873
1556.519859	51.994681	65.284878
1555.758016	58.380642	65.289882
1555.535987	54.689794	65.294887
1554.876946	51.237105	65.299892
1554.164020	59.271007	65.304897
1553.424372	45.086342	65.309902
1552.822440	60.053445	65.314906
1552.490867	50.354786	65.319911
1551.575758	59.259706	65.324916
1550.729371	60.907995	65.329921
1550.234300	56.169335	65.334926
1549.768568	47.338773	65.339930
1548.935529	55.478485	65.344935
1547.714973	63.413282	65.349940
1547.485504	56.733871	65.354945
1547.041795	46.214139	65.359950
1545.955294	70.230625	65.364954
1545.334727	47.048343	65.369959
1544.608062	54.862089	65.374964
1544.301210	54.300613	65.379969
1543.929798	60.291824	65.384974
1543.057125	63.965839	65.389978
1542.266991	61.174189	65.394983
1541.299187	59.995523	65.399988
1540.778081	64.332732	65.404993
1540.497710	59.052209	65.409998
1539.289839	52.223922	65.415002
1538.924930	52.106886	65.420007
1538.247574	64.107274	65.425012
1537.813414	53.444103	65.430017
1536.843653	52.172716	65.435022
1536.128867	63.163547	65.440026
1535.813025	53.281050	65.445031
1535.160407	55.759526	65.450036
1534.370131	58.217299	65.455041
1533.719896	52.751132	65.460046
1532.614955	58.920392	65.465050
1532.442134	57.088740	65.470055
1531.784624	60.175089	65.475060
1530.921162	52.491034	65.480065
1530.265480	57.163422	65.485070
1529.646723	65.491435	65.490074
1529.400903	47.625167	65.495079
1528.490487	53.992163	65.500084
1527.447480	56.401791	65.505089
1527.191225	56.835165	65.510094
1526.601423	52.972535	65.515098
1525.847183	54.292393	65.520103
1524.862696	54.352649	65.525108
1524.225434	54.129089	65.530113
1524.009568	48.625445	65.535118
1523.009052	54.369706	65.540122
1522.384306	55.680027	65.545127
1521.615176	57.246666	65.550132
1521.167609	55.181143	65.555137
1520.832589	40.888051	65.560142
1519.174426	56.710497	65.565146
1518.929327	49.576286	65.570151
1518.325732	44.938456	65.575156
1518.134003	51.298485	65.580161
1517.202515	53.699857	65.585166
1515.903676	50.306266	65.590170
1515.417984	37.752752	65.595175
1514.997873	53.088330	65.600180
1514.790046	60.256701	65.605185
1514.110280	41.324052	65.610190
1512.969366	48.229120	65.615194
1512.451271	54.991074	65.620199
1511.681862	59.545927	65.625204
1511.125026	48.042867	65.630209
1510.785273	35.992841	65.635214
1510.006174	52.140779	65.640218
1509.514550	46.744031	65.645223
1508.774144	42.760267	65.650228
1507.796561	57.370768	65.655233
1506.989985	41.310828	65.660238
1506.445397	52.867514	65.665242
1506.059565	38.029023	65.670247
1504.997535	57.720993	65.675252
1504.500416	53.228662	65.680257
1503.869431	59.152319	65.685262
1503.133259	53.764468	65.690266
1502.957797	54.749526	65.695271
1501.874388	47.903061	65.700276
1501.180141	54.732429	65.705281
1500.604232	41.158828	65.710286
1499.947802	51.523828	65.715290
1499.612675	59.817811	65.720295
1498.879683	49.645240	65.725300
1498.257325	51.846117	65.730305
1497.629411	47.571681	65.735310
1496.504524	49.016672	65.740314
1496.143295	43.493558	65.745319
1495.635687	49.356609	65.750324
1494.405297	50.551875	65.755329
1493.545450	48.914551	65.760334
1492.809960	51.265863	65.765338
1492.631418	46.385464	65.770343
1492.350553	55.033501	65.775348
1491.738524	49.075602	65.780353
1490.615225	58.117693	65.785358
1489.518405	56.842861	65.790362
1489.507393	45.765557	65.795367
1489.088031	50.152830	65.800372
1488.028252	43.042436	65.805377
1487.543371	49.269286	65.810382
1486.586192	50.566213	65.815386
1486.371696	45.560648	65.820391
1485.295056	46.652643	65.825396
1484.419802	53.551776	65.830401
1484.038871	41.932473	65.835406
1483.647243	58.935009	65.840410
1483.084350	44.370647	65.845415
1482.093807	49.099408	65.850420
1481.211151	50.486990	65.855425
1481.127938	50.754107	65.860430
1480.041629	49.802444	65.865434
1479.341355	53.515307	65.870439
1478.426698	53.769478	65.875444
1477.808661	52.041696	65.880449
1477.771087	49.564118	65.885454
1476.915488	50.955287	65.890458
1476.175913	53.422364	65.895463
1475.504068	39.532877	65.900468
1475.172483	45.028930	65.905473
1474.474621	35.815837	65.910478
1473.433689	45.620655	65.915482
1472.708871	46.855431	65.920487
1472.011673	46.583064	65.925492
1471.594246	45.014206	65.930497
1471.007095	48.042078	65.935502
1469.786268	43.144401	65.940506
1469.489338	44.555594	65.945511
1469.022416	44.767000	65.950516
1468.524281	51.937348	65.955521
1467.407976	49.423052	65.960526
1466.550810	52.044429	65.965530
1466.647144	42.145337	65.970535
1465.992119	49.381616	65.975540
1465.064835	47.181039	65.980545
1464.215574	47.155178	65.985550
1463.405133	42.302668	65.990554
1463.201006	45.219213	65.995559
1462.505264	46.537675	66.000564
1461.386225	35.207561	66.005569
1460.928724	48.488113	66.010574
1460.252094	51.889734	66.015578
1460.081777	35.231997	66.020583
1459.042076	52.020565	66.025588
1458.128318	47.392620	66.030593
1458.122442	34.745531	66.035598
1456.622126	48.311648	66.040602
1455.683727	36.987519	66.045607
1455.020884	49.941180	66.050612
1454.551336	45.518595	66.055617
1454.277645	43.412839	66.060622
1453.823877	44.866304	66.065626
1453.947541	46.907633	66.070631
1453.217099	44.407712	66.075636
1452.126500	53.387849	66.080641
1451.369424	39.759484	66.085646
1450.193612	63.709748	66.090650
1449.770768	53.694473	66.095655
1449.438324	38.868013	66.100660
1448.638107	42.232509	66.105665
1447.556031	46.419194	66.110670
1446.723478	44.815394	66.115674
1446.691221	58.491972	66.120679
1445.927488	55.615740	66.125684
1444.807606	48.248426	66.130689
1444.331052	44.566508	66.135694
1443.743346	44.265710	66.140698
1443.474687	42.012507	66.145703
1442.267101	51.542642	66.150708
1441.185425	52.096167	66.155713
1441.281116	41.285751	66.160718
1440.497958	60.441435	66.165722
1440.217619	44.875025	66.170727
1439.200781	45.236906	66.175732
1438.198509	46.495287	66.180737
1437.911399	40.574074	66.185742
1437.570697	58.156685	66.190746
1436.707905	43.523315	66.195751
1436.023519	47.687799	66.200756
1434.958542	49.689390	66.205761
1435.100814	45.223188	66.210766
1433.585204	38.910625	66.215770
1433.115835	46.733956	66.220775
1432.498966	45.404948	66.225780
1431.864856	61.517249	66.230785
1431.344011	45.602731	66.235790
1430.506042	55.455731	66.240794
1430.037855	56.540929	66.245799
1429.548011	47.636966	66.250804
1428.921794	58.634234	66.255809
1427.518908	46.642804	66.260814
1426.843154	49.583848	66.265818
1426.742269	56.825102	66.270823
1426.335556	46.051956	66.275828
1425.473950	43.375782	66.280833
1424.686080	41.268176	66.285838
1423.986354	46.431679	66.290842
1423.496084	46.271510	66.295847
1422.755575	46.860701	66.300852
1421.600978	53.916205	66.305857
1421.172071	44.537386	66.310862
1420.748144	56.770302	66.315866
1420.242111	46.392968	66.320871
1419.404544	45.190498	66.325876
1418.508796	45.925782	66.330881
1418.406831	56.052871	66.335886
1417.614245	52.466914	66.340890
1416.854255	43.542818	66.345895
1415.873226	53.177296	66.350900
1415.258366	50.782011	66.355905
1414.926991	48.111449	66.360910
1414.093547	50.014751	66.365914
1413.302426	52.310274	66.370919
1412.795598	41.937802	66.375924
1412.215561	51.309863	66.380929
1411.532471	43.147788	66.385934
1410.642224	41.827545	66.390938
1409.800355	44.750842	66.395943
1409.311018	50.074865	66.400948
1408.894403	50.663042	66.405953
1408.607427	45.872423	66.410958
1407.481801	53.248162	66.415962
1406.573416	58.980972	66.420967
1406.418509	46.371758	66.425972
1405.785269	53.281329	66.430977
1404.901521	53.333505	66.435982
1403.979149	52.373164	66.440986
1403.604491	55.780417	66.445991
1402.905656	40.526528	66.450996
1401.797035	51.359207	66.456001
1401.719952	44.890559	66.461006
1400.880102	55.380917	66.466010
1400.461845	47.329707	66.471015
1399.231577	52.095022	66.476020
1398.452843	58.078448	66.481025
1398.328006	46.442115	66.486030
1397.673131	49.592724	66.491034
1397.204606	49.496908	66.496039
1396.346856	44.353913	66.501044
1395.767843	52.276675	66.506049
1395.251342	47.976677	66.511054
1394.021560	51.455195	66.516058
1393.398006	51.215296	66.521063
1392.753409	52.473612	66.526068
1392.324178	63.568880	66.531073
1392.024844	39.102520	66.536078
1390.765516	52.040618	66.541082
1390.355400	46.586792	66.546087
1389.776290	50.352953	66.551092
1389.246186	49.951553	66.556097
1388.414070	46.975830	66.561102
1387.377746	45.188409	66.566106
1386.695977	43.893381	66.571111
1386.572409	45.854160	66.576116
1385.617528	45.342093	66.581121
1385.144706	34.453326	66.586126
1384.057303	35.056667	66.591130
1383.803346	46.051528	66.596135
1383.563076	35.070607	66.601140
1382.269286	58.169198	66.606145
1381.662780	38.999478	66.611150
1380.672647	50.401499	66.616154
1380.617055	42.396725	66.621159
1379.856352	53.465831	66.626164
1378.697915	46.413746	66.631169
1378.411861	52.104409	66.636174
1377.650979	44.238547	66.641178
1377.394934	46.012237	66.646183
1376.520439	39.761801	66.651188
1375.316970	44.551248	66.656193
1375.261657	47.909318	66.661198
1374.666771	40.947424	66.666202
1374.127275	54.245747	66.671207
1373.072842	37.889402	66.676212
1372.233701	46.324994	66.681217
1372.129136	41.836530	66.686222
1370.948010	41.975408	66.691226
1370.290383	30.267670	66.696231
1369.446492	43.445644	66.701236
1369.015217	46.584370	66.706241
1368.931529	39.612181	66.711246
1368.026107	53.017551	66.716250
1366.963630	42.099516	66.721255
1366.668961	47.238069	66.726260
1365.932435	44.732834	66.731265
1365.537023	37.575243	66.736270
1364.688870	36.790767	66.741274
1364.075527	38.641752	66.746279
1363.564962	41.648009	66.751284
1362.335988	44.948225	66.756289
1362.061620	42.284379	66.761294
1361.641442	42.284958	66.766298
1360.643575	38.335862	66.771303
1359.783604	37.523306	66.776308
1359.192433	45.495308	66.781313
1358.828620	50.014106	66.786318
1358.056437	49.514007	66.791322
1356.917759	44.421990	66.796327
1356.319171	35.749795	66.801332
1355.791558	44.168984	66.806337
1355.552448	41.425421	66.811342
1354.830387	44.375419	66.816346
1353.633374	44.007503	66.821351
1353.363830	36.539764	66.826356
1352.484229	50.037219	66.831361
1352.360237	44.006517	66.836366
1351.254349	46.965492	66.841370
1350.713499	45.709572	66.846375
1350.145795	57.864427	66.851380
1349.339287	57.984763	66.856385
1348.802350	40.270483	66.861390
1347.839605	50.827691	66.866394
1347.065968	61.304387	66.871399
1346.816464	58.212410	66.876404
1346.258075	57.517488	66.881409
1345.283606	35.025483	66.886414
1344.566617	52.070265	66.891418
1343.997775	48.626953	66.896423
1343.762584	44.936650	66.901428
1342.873733	54.561227	66.906433
1342.005964	50.851637	66.911438
1341.743499	43.232970	66.916442
1341.020499	50.193087	66.921447
1340.026621	45.385549	66.926452
1339.170536	55.618320	66.931457
1338.778536	40.927507	66.936462
1337.983873	49.239350	66.941466
1337.824281	48.192470	66.946471
1337.231894	48.848020	66.951476
1336.050262	50.204333	66.956481
1335.628266	48.119014	66.961486
1334.545171	47.742459	66.966490
1333.737320	48.176810	66.971495
1333.192084	37.551866	66.976500
1332.500305	56.167932	66.981505
1332.553073	42.715215	66.986510
1332.008428	54.759176	66.991514
1331.208619	44.890593	66.996519
1330.390052	40.512484	67.001524
1329.501562	48.478142	67.006529
1328.698670	50.122738	67.011534
1328.140177	39.157723	67.016538
1327.452300	39.500467	67.021543
1326.961290	53.376101	67.026548
1326.146648	47.428387	67.031553
1325.514503	42.071370	67.036558
1324.655254	49.172991	67.041562
1324.478049	61.197968	67.046567
1324.160360	38.740326	67.051572
1322.775954	52.434727	67.056577
1322.029581	49.707156	67.061582
1321.609101	49.728289	67.066586
1321.184738	51.916651	67.071591
1320.765576	40.029098	67.076596
1319.675617	56.426744	67.081601
1319.155540	40.619379	67.086606
1318.128165	62.010471	67.091610
1317.519219	45.113424	67.096615
1317.126208	53.746177	67.101620
1316.301913	40.817648	67.106625
1316.177260	49.475542	67.111630
1314.690667	52.618050	67.116634
1313.975236	41.504532	67.121639
1313.663743	46.890176	67.126644
1313.076329	52.564100	67.131649
1312.968127	46.218672	67.136654
1311.772805	50.035503	67.141658
1310.623435	58.003224	67.146663
1310.458184	53.801938	67.151668
1309.849545	47.028317	67.156673
1308.939669	55.366370	67.161678
1307.911995	53.150275	67.166682
1307.364258	53.909115	67.171687
1307.247240	36.754114	67.176692
1306.781313	51.160315	67.181697
1306.110884	34.525358	67.186702
1305.199317	44.222931	67.191706
1304.615920	46.345119	67.196711
1303.869522	55.579650	67.201716
1302.794949	49.485620	67.206721
1302.450389	43.029545	67.211726
1301.862234	51.138265	67.216730
1301.343302	50.435504	67.221735
1300.297838	44.270622	67.226740
1299.430704	56.737996	67.231745
1299.395379	47.209909	67.236750
1298.719934	46.287617	67.241754
1298.032826	41.969040	67.246759
1297.080210	55.683111	67.251764
1296.448909	56.067329	67.256769
1296.365098	40.674712	67.261774
1294.994601	49.827122	67.266778
1294.334616	41.005442	67.271783
1293.996465	37.886571	67.276788
1293.251358	50.829677	67.281793
1293.138477	39.822212	67.286798
1291.702167	44.002197	67.291802
1291.001365	46.231358	67.296807
1290.706878	49.476074	67.301812
1289.728166	54.466356	67.306817
1288.927957	36.281481	67.311822
1288.241869	51.561576	67.316826
1287.904520	51.588420	67.321831
1287.538044	43.071718	67.326836
1286.859168	57.350942	67.331841
1286.080298	40.942950	67.336846
1285.302908	58.244914	67.341850
1284.698984	47.594619	67.346855
1284.224507	45.941829	67.351860
1283.063424	45.355357	67.356865
1282.322660	48.087586	67.361870
1281.835896	48.332140	67.366874
1281.253861	49.159513	67.371879
1281.045284	49.307802	67.376884
1279.713405	60.286401	67.381889
1279.287558	56.861368	67.386894
1278.880857	51.695588	67.391898
1278.225163	43.308444	67.396903
1277.322246	48.851195	67.401908
1276.212388	55.015020	67.406913
1276.102925	43.808326	67.411918
1275.820061	48.080886	67.416922
1275.126907	46.899657	67.421927
1274.210896	36.992812	67.426932
1273.366218	50.382234	67.431937
1272.932262	46.879651	67.436942
1271.828992	53.029815	67.441946
1271.237610	41.437723	67.446951
1271.206370	46.182758	67.451956
1270.296845	51.892133	67.456961
1269.376558	39.838279	67.461966
1268.737892	54.670895	67.466970
1268.022020	50.785805	67.471975
1267.889238	50.136767	67.476980
1266.370003	49.615130	67.481985
1266.449262	38.129293	67.486990
1265.598577	47.678433	67.491994
1264.993992	41.881840	67.496999
1263.964276	40.158072	67.502004
1263.081165	54.249006	67.507009
1262.720116	35.131777	67.512014
1262.363208	41.962741	67.517018
1261.631414	54.817011	67.522023
1260.759591	51.828723	67.527028
1259.670166	41.484279	67.532033
1259.703061	43.237268	67.537038
1259.178282	47.295994	67.542042
1258.584041	48.174195	67.547047
1257.451307	36.560959	67.552052
1256.943503	51.467378	67.557057
1256.624228	39.095634	67.562062
1255.339663	50.613884	67.567066
1254.317778	47.047098	67.572071
1253.958534	46.296881	67.577076
1253.430431	52.946924	67.582081
1253.411699	49.277405	67.587086
1252.495122	54.078057	67.592090
1251.646657	54.198788	67.597095
1251.080173	45.286565	67.602100
1250.268030	48.626205	67.607105
1249.822097	43.556553	67.612110
1249.075041	47.417248	67.617114
1248.247583	47.957239	67.622119
1247.555691	40.118304	67.627124
1246.341003	44.395531	67.632129
1245.767347	49.482261	67.637134
1245.747356	52.058898	67.642138
1245.242305	51.707159	67.647143
1244.830096	43.888404	67.652148
1243.773775	57.303606	67.657153
1243.050750	45.868063	67.662158
1242.557452	50.027437	67.667162
1241.829766	45.663292	67.672167
1241.015071	49.853269	67.677172
1240.250065	53.726283	67.682177
1239.686187	52.707424	67.687182
1238.996244	49.414275	67.692186
1238.389222	44.389162	67.697191
1237.962827	47.564974	67.702196
1237.070161	53.462479	67.707201
1236.620613	52.075378	67.712206
1235.292180	47.948674	67.717210
1234.949522	48.162439	67.722215
1234.521082	47.637680	67.727220
1233.825436	45.591162	67.732225
1233.271771	50.819787	67.737230
1232.103042	48.840608	67.742234
1231.586546	42.366158	67.747239
1231.198095	38.258720	67.752244
1230.734617	48.096363	67.757249
1230.201773	47.815275	67.762254
1229.324630	41.418671	67.767258
1228.635437	48.218902	67.772263
1228.121058	50.945108	67.777268
1226.753495	54.196464	67.782273
1226.305408	44.453339	67.787278
1225.989010	59.423943	67.792282
1225.369098	54.814018	67.797287
1224.724636	53.954624	67.802292
1223.470671	53.625785	67.807297
1223.244667	40.047111	67.812302
1222.671587	45.024949	67.817306
1222.086280	46.231301	67.822311
1221.175924	53.691140	67.827316
1220.241126	52.354396	67.832321
1220.069522	43.697920	67.837326
1219.276529	46.171980	67.842330
1218.398587	47.286101	67.847335
1217.635424	55.369051	67.852340
1216.843064	53.188113	67.857345
1216.873223	54.734968	67.862350
1216.396345	59.550866	67.867354
1215.009224	59.164361	67.872359
1214.392756	56.223790	67.877364
1213.884564	46.561182	67.882369
1213.498156	55.538225	67.887374
1212.723661	56.057191	67.892378
1211.630195	61.086248	67.897383
1211.261124	46.902727	67.902388
1210.776485	54.217609	67.907393
1210.314917	50.115490	67.912398
1209.337428	47.300135	67.917402
1208.806632	53.332482	67.922407
1208.313710	46.576760	67.927412
1207.317630	53.372184	67.932417
1206.592970	53.996761	67.937422
1206.033981	50.734834	67.942426
1205.498682	51.222074	67.947431
1205.133835	41.812629	67.952436
1204.003363	50.977370	67.957441
1202.975259	56.172643	67.962446
1202.679725	43.945360	67.967450
1202.257948	48.342510	67.972455
1201.127544	51.245524	67.977460
1200.167930	54.272759	67.982465
1200.145400	48.938680	67.987470
1199.381579	48.260690	67.992474
1198.928598	48.547194	67.997479
1198.365981	39.063552	68.002484
1197.371284	54.399042	68.007489
1197.166074	41.586574	68.012494
1196.372920	51.935515	68.017498
1195.316131	48.658140	68.022503
1195.097636	43.591755	68.027508
1194.328425	47.408680	68.032513
1193.529946	47.890467	68.037518
1192.457442	44.923081	68.042522
1191.703873	51.071276	68.047527
1191.276218	51.419981	68.052532
1190.709359	54.603946	68.057537
1190.637860	45.436420	68.062542
1189.188827	46.977239	68.067546
1188.619501	41.525125	68.072551
1188.696449	44.625630	68.077556
1187.715312	53.145347	68.082561
1186.539481	49.508459	68.087566
1186.006618	56.326417	68.092570
1185.399818	46.367281	68.097575
1185.356548	45.833316	68.102580
1184.165819	61.703009	68.107585
1183.581033	51.221581	68.112590
1183.288462	48.193244	68.117594
1182.585405	47.860391	68.122599
1181.614583	50.105713	68.127604
1180.922645	53.374222	68.132609
1180.443633	48.607872	68.137614
1180.049541	50.171733	68.142618
1178.728855	46.281935	68.147623
1178.487121	40.552237	68.152628
1177.873353	54.204563	68.157633
1176.789481	44.497907	68.162638
1176.025971	36.735041	68.167642
1175.357240	41.417455	68.172647
1175.066545	45.479967	68.177652
1174.695946	56.056589	68.182657
1173.577761	47.601111	68.187662
1172.671952	41.223281	68.192666
1172.007372	39.640169	68.197671
1171.991983	39.595328	68.202676
1171.374178	45.785009	68.207681
1170.282955	46.674459	68.212686
1169.622980	41.227306	68.217690
1168.890497	44.718293	68.222695
1168.785977	34.829094	68.227700
1167.687021	44.370432	68.232705
1166.609167	44.861966	68.237710
1166.167965	29.940938	68.242714
1165.971265	41.458086	68.247719
1165.402575	32.095267	68.252724
1164.095701	40.307262	68.257729
1163.782389	35.333230	68.262734
1163.503616	42.421417	68.267738
1162.651120	33.382837	68.272743
1161.796266	27.924108	68.277748
1160.874762	43.586978	68.282753
1160.488951	39.501210	68.287758
1160.129620	41.111581	68.292762
1158.728222	50.213774	68.297767
1158.382199	36.002963	68.302772
1157.776836	49.436342	68.307777
1157.329528	43.193746	68.312782
1156.692459	32.854689	68.317786
1155.507022	37.983536	68.322791
1155.185116	33.677884	68.327796
1154.312701	43.134315	68.332801
1154.053963	37.850424	68.337806
1153.319633	41.787959	68.342810
1152.096495	45.267103	68.347815
1152.164194	33.869846	68.352820
1151.645477	39.267954	68.357825
1150.646394	36.992192	68.362830
1150.064696	40.005066	68.367834
1149.033995	41.077277	68.372839
1148.874754	33.021213	68.377844
1147.597349	38.300300	68.382849
1146.823076	43.377952	68.387854
1146.278036	36.066025	68.392858
1145.896021	41.149098	68.397863
1145.727698	39.428724	68.402868
1144.486664	39.791687	68.407873
1143.709945	35.600946	68.412878
1143.346105	38.538175	68.417882
1142.775381	51.590756	68.422887
1142.401473	40.069775	68.427892
1141.442113	41.474398	68.432897
1140.853105	39.526058	68.437902
1139.970435	41.752644	68.442906
1138.551076	45.568911	68.447911
1138.334520	32.751962	68.452916
1137.842746	40.739721	68.457921
1137.307618	39.512900	68.462926
1136.987617	41.672073	68.467930
1136.442321	41.616899	68.472935
1135.881928	34.107157	68.477940
1134.868469	38.931133	68.482945
1134.087828	33.955744	68.487950
1133.285031	38.415075	68.492954
1132.487989	46.542847	68.497959
1132.408512	35.895931	68.502964
1131.086234	43.161123	68.507969
1130.491627	41.716694	68.512974
1129.948385	44.778648	68.517978
1129.264172	42.925873	68.522983
1129.259930	32.188151	68.527988
1128.008822	39.372641	68.532993
1127.515300	33.350282	68.537998
1127.021911	32.701840	68.543002
1126.199091	37.848715	68.548007
1125.348467	39.325930	68.553012
1124.380872	45.959160	68.558017
1124.009857	49.321710	68.563022
1123.539085	42.896785	68.568026
1122.997336	43.739860	68.573031
1122.041559	42.395453	68.578036
1121.466282	40.195791	68.583041
1121.213095	42.689672	68.588046
1120.367431	39.793467	68.593050
1118.988061	45.224397	68.598055
1118.664604	47.112903	68.603060
1118.299975	47.013229	68.608065
1117.874688	37.310664	68.613070
1116.842967	45.865250	68.618074
1116.032055	45.442343	68.623079
1115.874380	39.405990	68.628084
1114.972656	51.557219	68.633089
1114.216611	38.578510	68.638094
1113.576744	37.117633	68.643098
1112.909310	44.007458	68.648103
1112.579997	34.985027	68.653108
1111.532934	49.515200	68.658113
1110.571286	41.096359	68.663118
1110.224992	33.054284	68.668122
1109.646661	36.175434	68.673127
1109.334544	33.295291	68.678132
1107.962782	42.839040	68.683137
1107.146631	42.388586	68.688142
1106.837027	44.992361	68.693146
1106.448041	43.471081	68.698151
1106.205618	37.124953	68.703156
1104.888829	44.501241	68.708161
1104.505808	29.000158	68.713166
1103.901120	43.004251	68.718170
1102.835225	34.180978	68.723175
1102.375887	28.489062	68.728180
1101.242150	42.638802	68.733185
1100.988895	39.720914	68.738190
1100.762732	42.792359	68.743194
1099.451364	32.749799	68.748199
1098.757149	32.666283	68.753204
1098.277454	44.844995	68.758209
1097.992325	45.670911	68.763214
1097.121862	41.577092	68.768218
1096.012527	41.097586	68.773223
1095.619512	40.158811	68.778228
1095.127669	45.385507	68.783233
1094.755970	33.813734	68.788238
1094.043765	41.839713	68.793242
1093.064898	34.943716	68.798247
1092.658544	34.424931	68.803252
1091.754517	42.869331	68.808257
1091.278783	37.943222	68.813262
1090.644141	48.531879	68.818266
1089.732299	53.984649	68.823271
1089.175002	40.219019	68.828276
1088.310847	42.124151	68.833281
1087.689010	44.470104	68.838286
1087.283633	46.209228	68.843290
1086.681705	36.342393	68.848295
1085.886833	39.114815	68.853300
1084.624158	39.052343	68.858305
1084.464719	45.025635	68.863310
1084.461573	37.583377	68.868314
1083.121912	42.801438	68.873319
1082.292839	29.356579	68.878324
1081.815693	38.994563	68.883329
1081.304253	35.004484	68.888334
1080.380165	33.735474	68.893338
1079.397647	44.276969	68.898343
1079.203875	45.969819	68.903348
1078.766218	40.965120	68.908353
1078.403691	42.792039	68.913358
1077.199924	29.069337	68.918362
1076.440892	38.261757	68.923367
1076.133467	32.099430	68.928372
1075.189405	45.060019	68.933377
1074.485168	39.309295	68.938382
1074.075376	32.327517	68.943386
1073.372492	48.668374	68.948391
1072.707331	32.608240	68.953396
1071.549431	42.898530	68.958401
1070.904951	39.449978	68.963406
1070.399038	33.953123	68.968410
1069.891001	38.485425	68.973415
1069.871759	38.106904	68.978420
1068.977419	40.142991	68.983425
1067.873057	39.899236	68.988430
1067.513919	28.590388	68.993434
1066.641651	42.376867	68.998439
1065.745719	35.101859	69.003444
1064.915768	34.284629	69.008449
1064.530467	33.549624	69.013454
1064.520833	43.982094	69.018458
1063.544194	48.262532	69.023463
1062.787317	30.173384	69.028468
1062.461525	42.606718	69.033473
1061.593263	41.708856	69.038478
1060.663148	33.068998	69.043482
1059.535873	41.657722	69.048487
1059.237593	32.833783	69.053492
1058.952352	39.520901	69.058497
1058.438973	36.743740	69.063502
1057.544289	30.133974	69.068506
1056.599864	42.599488	69.073511
1056.120896	37.191384	69.078516
1055.249916	33.048783	69.083521
1054.424647	38.845732	69.088526
1053.864759	27.989844	69.093530
1053.441903	34.090185	69.098535
1053.317103	27.230226	69.103540
1052.025502	32.473767	69.108545
1051.114333	41.007616	69.113550
1050.547771	45.853567	69.118554
1049.984328	39.790313	69.123559
1050.281458	31.480328	69.128564
1049.046502	33.840248	69.133569
1048.366907	36.121285	69.138574
1047.936769	32.865712	69.143578
1047.229428	32.032137	69.148583
1046.436045	32.894758	69.153588
1045.580531	38.199810	69.158593
1044.272978	39.267221	69.163598
1043.723266	35.327391	69.168602
1043.042903	30.769719	69.173607
1042.668764	36.723549	69.178612
1042.288797	41.610775	69.183617
1042.195350	36.133461	69.188622
1041.441367	31.161750	69.193626
1040.186411	47.243524	69.198631
1039.611027	35.831892	69.203636
1038.976764	47.442299	69.208641
1038.140475	39.773059	69.213646
1037.681784	40.856812	69.218650
1036.797820	39.243987	69.223655
1036.527395	35.305458	69.228660
1035.394215	46.955813	69.233665
1034.535055	51.085116	69.238670
1034.367433	34.903271	69.243674
1033.825780	37.372089	69.248679
1033.152280	32.387576	69.253684
1032.071209	44.922143	69.258689
1031.525764	33.974079	69.263694
1031.180073	38.934696	69.268698
1030.586407	47.238282	69.273703
1029.871544	44.948891	69.278708
1029.177992	35.736857	69.283713
1028.461414	29.871430	69.288718
1027.907838	28.172935	69.293722
1026.489316	46.086234	69.298727
1026.101190	36.805112	69.303732
1025.705385	38.542720	69.308737
1025.423022	32.933047	69.313742
1024.832423	36.008859	69.318746
1023.404694	38.850441	69.323751
1023.198358	34.338780	69.328756
1022.902285	36.520965	69.333761
1021.716594	23.372557	69.338766
1020.935546	26.180640	69.343770
1020.215600	39.711094	69.348775
1019.762117	24.334787	69.353780
1019.293905	26.331480	69.358785
1018.154400	44.687641	69.363790
1017.940793	33.268923	69.368794
1016.919495	35.825088	69.373799
1016.839008	37.952477	69.378804
1015.664190	31.294260	69.383809
1014.979258	25.830633	69.388814
1014.894332	32.211508	69.393818
1014.005968	41.200605	69.398823
1013.212714	24.224231	69.403828
1012.071934	38.401920	69.408833
1011.481887	41.966474	69.413838
1011.771355	33.389639	69.418842
1010.333461	31.428162	69.423847
1009.925363	29.596146	69.428852
1009.022722	36.764666	69.433857
1008.313559	35.904586	69.438862
1008.320848	29.357911	69.443866
1007.304816	37.031720	69.448871
1006.733460	25.912763	69.453876
1006.186139	30.951185	69.458881
1005.353725	37.506175	69.463886
1004.763080	30.269353	69.468890
1003.900294	37.710638	69.473895
1003.609125	25.722408	69.478900
1002.423607	39.777917	69.483905
1001.822440	34.897016	69.488910
1001.302405	40.675378	69.493914
1000.503526	36.663244	69.498919
1000.295372	33.724003	69.503924
998.933318	38.248694	69.508929
998.484424	36.437362	69.513934
998.366174	33.337169	69.518938
997.173667	45.682907	69.523943
996.044961	32.492326	69.528948
995.622548	33.243905	69.533953
995.287211	26.363837	69.538958
995.177309	39.683703	69.543962
994.274816	38.736122	69.548967
993.611839	39.130184	69.553972
992.859286	35.492282	69.558977
992.115697	47.963707	69.563982
991.065376	33.565399	69.568986
990.558495	32.461842	69.573991
990.174469	42.479235	69.578996
989.540629	36.479236	69.584001
988.843289	39.502657	69.589006
988.015343	31.409516	69.594010
987.359439	47.105855	69.599015
986.894386	27.786098	69.604020
986.349453	33.653571	69.609025
985.397836	34.875680	69.614030
984.752464	36.487430	69.619034
984.098933	39.953286	69.624039
983.800264	29.502111	69.629044
982.482414	31.607185	69.634049
981.954407	31.024200	69.639054
982.009117	19.408279	69.644058
980.571762	38.128777	69.649063
979.787914	30.077507	69.654068
979.345144	31.450455	69.659073
978.620116	33.841233	69.664078
978.723940	25.098410	69.669082
977.754687	25.296793	69.674087
976.865345	24.384971	69.679092
976.118598	37.441906	69.684097
975.621671	29.378101	69.689102
974.631204	35.783214	69.694106
973.329163	35.093165	69.699111
972.998449	23.147505	69.704116
972.963375	30.701511	69.709121
972.546182	26.743771	69.714126
972.362582	35.511938	69.719130
971.203924	32.775970	69.724135
970.417724	33.315792	69.729140
969.832295	28.299943	69.734145
968.416274	26.019639	69.739150
967.907140	28.456487	69.744154
967.446533	35.892133	69.749159
967.025548	30.285605	69.754164
966.466329	36.896478	69.759169
965.520269	29.910173	69.764174
965.097542	33.752444	69.769178
964.241015	32.706102	69.774183
963.881770	28.783296	69.779188
962.734966	27.360544	69.784193
961.935476	45.638966	69.789198
961.660983	27.071021	69.794202
961.006685	39.285401	69.799207
960.887328	26.166045	69.804212
959.853476	29.842219	69.809217
958.921492	28.181874	69.814222
958.812180	31.376649	69.819226
957.612443	30.466916	69.824231
956.884511	33.104151	69.829236
956.434266	31.696718	69.834241
955.684311	41.745529	69.839246
954.930414	26.243589	69.844250
953.913249	41.180595	69.849255
953.574602	20.926171	69.854260
953.155925	37.854124	69.859265
952.692550	34.102418	69.864270
952.111112	31.192618	69.869274
950.843812	31.356439	69.874279
950.467691	22.764099	69.879284
950.089143	40.106689	69.884289
949.088421	30.801648	69.889294
948.598174	35.641777	69.894298
947.820230	37.470161	69.899303
946.727045	27.340948	69.904308
945.688335	45.958616	69.909313
945.059335	29.848636	69.914318
945.425317	33.095508	69.919322
944.393757	34.095400	69.924327
944.267656	40.490713	69.929332
943.963892	39.129355	69.934337
942.614700	31.198018	69.939342
942.104908	29.833177	69.944346
940.873613	38.019047	69.949351
940.400841	34.968964	69.954356
939.692642	25.773493	69.959361
939.037524	36.915742	69.964366
939.153590	27.508693	69.969370
937.783088	33.394005	69.974375
937.030109	27.162265	69.979380
936.541667	27.478110	69.984385
935.953076	29.328402	69.989390
935.717277	20.212298	69.994394
934.371584	44.809365	69.999399
934.280335	29.936804	70.004404
933.414439	31.635692	70.009409
931.979030	32.726658	70.014414
931.895757	32.350443	70.019418
931.146691	31.983983	70.024423
930.780953	31.231695	70.029428
930.007201	26.863952	70.034433
928.875856	38.919294	70.039438
928.463238	33.180564	70.044442
927.666114	37.049303	70.049447
927.658752	29.208789	70.054452
927.102038	26.705045	70.059457
925.955852	32.234567	70.064462
925.572373	21.916747	70.069466
924.746149	27.253436	70.074471
923.957501	36.854273	70.079476
923.404737	22.206539	70.084481
922.550587	32.790716	70.089486
922.500076	34.702036	70.094490
921.149658	26.480768	70.099495
920.555829	24.626288	70.104500
919.998842	15.780484	70.109505
919.283672	42.650381	70.114510
919.111975	35.343763	70.119514
917.769185	37.247848	70.124519
917.352687	26.314000	70.129524
916.775404	40.204942	70.134529
916.048146	35.353593	70.139534
915.476960	28.272966	70.144538
914.664020	31.497714	70.149543
914.259306	24.974034	70.154548
913.482802	24.917857	70.159553
912.768498	37.547041	70.164558
911.985200	28.022929	70.169562
911.590025	40.431033	70.174567
911.276797	22.618280	70.179572
910.543750	31.525914	70.184577
909.723489	39.089759	70.189582
908.950285	30.984787	70.194586
907.623006	36.112654	70.199591
907.272977	20.308369	70.204596
906.911264	28.387405	70.209601
906.050359	37.001595	70.214606
906.015525	37.417138	70.219610
904.222576	34.365850	70.224615
903.859036	29.776728	70.229620
903.347988	34.859855	70.234625
902.880547	37.528187	70.239630
902.889899	28.469260	70.244634
901.638264	45.143444	70.249639
900.873333	31.371515	70.254644
900.412184	36.260634	70.259649
899.293901	35.076208	70.264654
898.528145	31.224411	70.269658
897.834559	30.500648	70.274663
898.158661	28.414946	70.279668
897.434541	31.319655	70.284673
896.322789	34.489465	70.289678
895.747841	28.292482	70.294682
894.651204	32.063822	70.299687
894.641014	20.480313	70.304692
893.638030	37.471290	70.309697
892.567337	31.621264	70.314702
892.197672	20.910196	70.319706
891.635923	34.905889	70.324711
891.135400	31.527517	70.329716
890.383695	33.646613	70.334721
889.947499	39.711251	70.339726
889.355905	33.441228	70.344730
888.025835	39.380052	70.349735
887.425714	34.301912	70.354740
887.208258	38.923608	70.359745
886.367938	36.310474	70.364750
885.582569	28.302060	70.369754
884.471314	29.011902	70.374759
883.928245	32.054948	70.379764
883.644331	32.953227	70.384769
883.097258	36.506234	70.389774
883.110615	34.973000	70.394778
882.170291	42.420351	70.399783
881.433349	35.222616	70.404788
880.285313	28.687936	70.409793
879.165172	31.805475	70.414798
879.033902	40.560584	70.419802
878.226829	37.079621	70.424807
878.015937	37.338692	70.429812
877.417426	36.684953	70.434817
876.125324	34.085379	70.439822
875.900727	32.252567	70.444826
875.361040	32.076716	70.449831
874.206947	33.562886	70.454836
873.607292	34.049397	70.459841
873.090694	29.796857	70.464846
872.905869	31.969234	70.469850
872.282400	35.182763	70.474855
871.472345	28.867095	70.479860
870.435381	32.108586	70.484865
869.605361	43.084732	70.489870
868.979344	29.793728	70.494874
868.039895	39.770216	70.499879
867.680083	34.622300	70.504884
867.253990	35.374485	70.509889
866.804369	38.415277	70.514894
865.973513	32.156533	70.519898
865.290320	40.032868	70.524903
864.400061	24.943734	70.529908
864.056042	20.594351	70.534913
863.137523	34.124887	70.539918
862.295035	29.462198	70.544922
861.398118	38.082131	70.549927
861.495526	32.755799	70.554932
861.034637	26.949079	70.559937
859.953893	21.274128	70.564942
859.108319	27.495375	70.569946
858.458396	31.348588	70.574951
858.212238	21.456759	70.579956
857.906597	38.675783	70.584961
856.844212	32.405009	70.589966
856.470098	29.820184	70.594970
855.026873	33.482708	70.599975
854.327132	32.537601	70.604980
853.715882	28.487776	70.609985
853.300835	28.631116	70.614990
853.071614	30.156165	70.619994
851.899970	37.518921	70.624999
851.146297	34.299112	70.630004
850.539572	41.947251	70.635009
849.978625	40.776639	70.640014
849.813964	29.741230	70.645018
848.694328	34.944879	70.650023
848.252270	34.031296	70.655028
847.796618	35.185556	70.660033
846.459728	39.718932	70.665038
845.542082	29.251194	70.670042
845.182690	31.588543	70.675047
844.768335	35.664448	70.680052
844.460393	31.706691	70.685057
843.248066	31.637904	70.690062
842.468715	31.569586	70.695066
842.003627	38.402024	70.700071
841.684840	23.706043	70.705076
841.335715	31.505554	70.710081
839.863791	23.300524	70.715086
839.612297	36.370111	70.720090
838.920858	42.733985	70.725095
837.851622	35.950254	70.730100
837.174234	27.215090	70.735105
836.262190	42.944319	70.740110
836.343857	34.263369	70.745114
835.557664	40.916696	70.750119
835.295036	46.160559	70.755124
834.204696	38.041438	70.760129
833.491083	38.512982	70.765134
833.135213	36.797257	70.770138
831.865768	43.126981	70.775143
831.174710	36.620508	70.780148
830.775175	29.424282	70.785153
830.082348	40.429057	70.790158
829.883825	30.091281	70.795162
828.966865	40.989814	70.800167
828.074041	44.976310	70.805172
828.037872	33.239249	70.810177
827.063431	50.955796	70.815182
825.880550	41.094789	70.820186
825.105993	46.267180	70.825191
824.866973	38.006255	70.830196
824.756185	47.920247	70.835201
823.616515	51.674817	70.840206
823.505849	40.406896	70.845210
822.550082	47.172370	70.850215
821.749249	37.835572	70.855220
820.693194	40.931898	70.860225
819.721141	48.933066	70.865230
819.902725	33.369010	70.870234
819.276544	44.766857	70.875239
818.528208	30.030444	70.880244
817.724081	40.543613	70.885249
816.854843	38.550080	70.890254
816.709782	33.702285	70.895258
815.673066	42.141070	70.900263
814.890476	42.281422	70.905268
814.345164	33.703423	70.910273
813.548913	43.436376	70.915278
813.256940	37.624854	70.920282
812.088556	45.507471	70.925287
811.595266	28.527600	70.930292
811.263636	42.048312	70.935297
810.407853	44.434718	70.940302
809.456492	31.077258	70.945306
808.607503	38.007073	70.950311
808.439363	42.203057	70.955316
808.246837	37.648227	70.960321
807.493508	31.807648	70.965326
806.588963	35.239385	70.970330
805.891276	41.443420	70.975335
805.245793	29.074846	70.980340
804.347633	37.676069	70.985345
803.540258	40.885773	70.990350
803.010688	31.993057	70.995354
802.401863	29.560712	71.000359
801.892490	32.065433	71.005364
801.188522	31.765946	71.010369
800.353115	34.250028	71.015374
800.155713	40.808066	71.020378
799.410234	30.551049	71.025383
798.323527	27.247085	71.030388
797.954256	36.096838	71.035393
797.317841	37.216806	71.040398
796.459052	22.061204	71.045402
795.502627	36.285298	71.050407
794.894054	37.227381	71.055412
794.788809	36.309077	71.060417
794.210018	26.711464	71.065422
793.636331	25.438822	71.070426
792.425252	41.458494	71.075431
791.860591	35.166867	71.080436
791.559751	32.980371	71.085441
790.252292	39.454926	71.090446
789.862536	32.446374	71.095450
789.002685	32.556457	71.100455
788.836906	40.621662	71.105460
787.881824	30.664504	71.110465
786.601740	41.406398	71.115470
786.308275	29.298744	71.120474
785.806894	39.544545	71.125479
785.619743	36.775439	71.130484
784.968880	31.470456	71.135489
783.816131	32.086028	71.140494
783.551540	23.165335	71.145498
783.022798	40.306337	71.150503
782.160544	42.886157	71.155508
781.288622	34.193014	71.160513
780.547875	49.030877	71.165518
780.297241	25.148349	71.170522
779.302621	29.499545	71.175527
778.665545	40.397689	71.180532
778.440435	45.764884	71.185537
777.504944	32.166808	71.190542
776.498951	38.963940	71.195546
775.457194	50.566714	71.200551
775.155876	38.047170	71.205556
774.795214	27.773060	71.210561
774.202647	53.997449	71.215566
774.096842	42.837565	71.220570
772.784250	44.995521	71.225575
772.110413	49.899596	71.230580
771.239766	36.903016	71.235585
770.256402	45.290750	71.240590
769.637235	38.996766	71.245594
768.899678	33.046464	71.250599
768.858526	47.408707	71.255604
768.779968	43.129033	71.260609
767.761175	52.131077	71.265614
767.107670	41.082035	71.270618
766.305794	49.879247	71.275623
765.458439	37.456091	71.280628
764.271639	44.231552	71.285633
763.496625	43.221187	71.290638
763.462309	34.881960	71.295642
763.035680	39.410810	71.300647
762.816868	38.977335	71.305652
762.021960	38.488922	71.310657
761.192838	37.991765	71.315662
760.347040	30.666336	71.320666
759.107064	29.182824	71.325671
758.395793	39.052058	71.330676
758.100929	35.333491	71.335681
757.850060	53.852595	71.340686
757.203987	36.556457	71.345690
756.251363	38.031106	71.350695
755.672973	34.252026	71.355700
755.334918	36.721598	71.360705
753.868743	40.983882	71.365710
753.436607	32.914556	71.370714
752.697636	39.118866	71.375719
752.283715	39.260466	71.380724
752.115351	40.197131	71.385729
750.769412	56.165765	71.390734
750.356390	36.435711	71.395738
749.826831	35.253819	71.400743
749.045439	29.217470	71.405748
748.028366	32.134163	71.410753
747.279737	48.077081	71.415758
747.206573	38.111994	71.420762
746.625900	40.320590	71.425767
745.300324	39.099854	71.430772
745.035210	37.260892	71.435777
744.366413	38.441217	71.440782
744.043227	33.238613	71.445786
742.832129	40.077870	71.450791
741.848740	36.470494	71.455796
741.834806	28.121721	71.460801
741.086028	44.342185	71.465806
740.864363	37.174427	71.470810
739.823284	43.226577	71.475815
738.857920	39.501222	71.480820
738.527294	32.011790	71.485825
737.653281	49.135235	71.490830
736.826503	39.140324	71.495834
736.292942	37.929112	71.500839
735.780698	36.518978	71.505844
735.584890	40.799786	71.510849
734.356619	41.678125	71.515854
733.963550	35.001251	71.520858
733.347121	44.562100	71.525863
732.597858	40.602083	71.530868
731.438853	35.325977	71.535873
730.789182	39.724772	71.540878
730.750846	36.255509	71.545882
730.252869	39.182602	71.550887
729.251121	41.313168	71.555892
728.468740	38.191005	71.560897
727.639599	38.034462	71.565902
727.533073	41.604088	71.570906
726.558859	32.906756	71.575911
725.735850	35.819368	71.580916
725.478724	40.452116	71.585921
724.491021	44.808542	71.590926
723.571106	39.041817	71.595930
722.737707	30.569636	71.600935
722.196825	38.066970	71.605940
722.214425	37.488635	71.610945
721.652576	42.195127	71.615950
721.238570	37.673993	71.620954
719.938721	42.285106	71.625959
719.259391	46.035810	71.630964
718.354867	25.642912	71.635969
717.406173	51.201794	71.640974
717.083941	13.796577	71.645978
716.612883	58.709383	71.650983
716.206658	39.952751	71.655988
715.339236	39.901648	71.660993
714.133253	49.253609	71.665998
713.883054	37.252613	71.671002
713.337610	38.138935	71.676007
713.224909	37.505656	71.681012
712.355039	35.020284	71.686017
711.125089	23.952675	71.691022
710.911949	42.205571	71.696026
709.975407	48.196938	71.701031
709.073256	40.349098	71.706036
708.861453	34.365570	71.711041
708.066854	35.125992	71.716046
707.600171	37.663355	71.721050
706.718612	35.665516	71.726055
705.691536	38.176991	71.731060
705.443612	37.563665	71.736065
704.548636	33.700971	71.741070
703.875046	23.935569	71.746074
703.157643	33.659139	71.751079
702.282361	35.771156	71.756084
702.247705	31.676877	71.761089
701.459618	39.907388	71.766094
701.135417	37.634744	71.771098
700.247659	38.922478	71.776103
699.979522	29.458348	71.781108
698.918188	33.355024	71.786113
697.980842	35.752873	71.791118
697.302915	31.373109	71.796122
697.084545	37.836719	71.801127
696.115487	36.470942	71.806132
695.160352	31.298007	71.811137
694.420015	37.582966	71.816142
694.247415	31.471781	71.821146
693.854663	47.939902	71.826151
692.806064	37.549849	71.831156
692.003865	36.394034	71.836161
691.424274	43.492288	71.841166
691.618651	39.150243	71.846170
690.372162	42.324246	71.851175
689.954441	37.406343	71.856180
689.227218	30.036836	71.861185
687.812966	44.329126	71.866190
687.259517	38.994470	71.871194
686.650849	32.181637	71.876199
686.461211	45.731777	71.881204
685.550226	37.934238	71.886209
684.661623	44.361074	71.891214
684.077720	43.233578	71.896218
683.798253	44.815524	71.901223
683.123541	33.205384	71.906228
682.072459	34.109148	71.911233
681.270950	43.109730	71.916238
680.606503	34.476630	71.921242
680.241151	41.570733	71.926247
680.237215	41.531956	71.931252
679.311996	35.622603	71.936257
678.265138	43.744524	71.941262
677.684169	34.511544	71.946266
676.520733	30.497656	71.951271
675.706410	31.817857	71.956276
675.427339	37.761310	71.961281
674.565584	43.094269	71.966286
674.516527	28.751173	71.971290
674.453744	27.800885	71.976295
673.104713	45.919276	71.981300
672.902259	18.454402	71.986305
671.577614	42.833731	71.991310
670.918894	31.765066	71.996314
670.024687	18.450627	72.001319
669.286147	41.963974	72.006324
669.357383	36.605545	72.011329
668.618694	36.907674	72.016334
667.526863	35.564612	72.021338
666.808495	33.469846	72.026343
666.069689	36.438450	72.031348
665.947267	39.488669	72.036353
665.500335	35.764371	72.041358
664.683888	39.169511	72.046362
664.076214	42.110929	72.051367
663.467082	36.160714	72.056372
662.453736	30.705344	72.061377
661.353126	30.402827	72.066382
660.885529	49.374290	72.071386
660.892065	17.430999	72.076391
659.742174	53.569475	72.081396
659.392145	32.596331	72.086401
658.435031	39.453523	72.091406
657.931196	34.388502	72.096410
656.963805	34.624557	72.101415
656.092505	44.729016	72.106420
655.744980	29.846859	72.111425
655.203968	30.543265	72.116430
654.983979	27.224352	72.121434
654.184237	41.193313	72.126439
652.990651	41.224128	72.131444
652.605258	39.317603	72.136449
651.774743	28.378799	72.141454
650.696504	36.258156	72.146458
650.274505	42.946570	72.151463
649.789171	37.034988	72.156468
649.730822	35.552596	72.161473
648.973349	37.338385	72.166478
648.074117	36.794086	72.171482
647.303674	47.142669	72.176487
646.799451	36.560308	72.181492
646.116100	19.818921	72.186497
644.941243	42.160767	72.191502
644.948039	33.264686	72.196506
644.261555	41.023322	72.201511
642.896158	36.284720	72.206516
642.509652	27.473347	72.211521
641.720843	29.921674	72.216526
641.655478	32.907617	72.221530
640.831228	33.551364	72.226535
640.105772	33.777283	72.231540
639.631566	28.332260	72.236545
638.565259	35.549021	72.241550
637.479016	28.577304	72.246554
636.914749	33.780901	72.251559
636.691533	42.798207	72.256564
636.396471	29.918188	72.261569
635.674160	38.985008	72.266574
634.434419	33.952030	72.271578
633.904479	35.271111	72.276583
633.255671	41.538356	72.281588
633.171412	27.517822	72.286593
631.705195	38.789277	72.291598
631.409095	28.731989	72.296602
631.023278	25.095733	72.301607
630.205993	39.955256	72.306612
629.887046	33.682893	72.311617
628.824617	45.008317	72.316622
628.078056	30.438855	72.321626
627.498070	29.916261	72.326631
626.664159	35.462401	72.331636
626.086094	27.104134	72.336641
625.476726	35.342467	72.341646
624.882303	35.741476	72.346650
624.042072	38.554367	72.351655
622.999864	40.279858	72.356660
622.840317	29.333558	72.361665
622.265239	34.977244	72.366670
621.818886	34.296184	72.371674
620.635143	29.716316	72.376679
620.081275	40.238554	72.381684
619.771446	21.420902	72.386689
618.935160	33.106096	72.391694
617.738229	42.379383	72.396698
617.450165	31.295864	72.401703
616.895140	36.190508	72.406708
616.458318	21.095526	72.411713
615.535424	43.165459	72.416718
614.770673	34.070571	72.421722
614.181684	33.708676	72.426727
613.892145	35.971854	72.431732
613.555160	28.723144	72.436737
612.139781	38.521619	72.441742
611.900426	31.353549	72.446746
610.662296	35.313104	72.451751
609.645192	41.091839	72.456756
609.177302	36.107833	72.461761
608.858177	49.915120	72.466766
608.619928	31.213785	72.471770
608.242360	32.443954	72.476775
606.774882	33.704201	72.481780
606.446747	36.506501	72.486785
606.012030	42.939918	72.491790
605.224865	39.522111	72.496794
604.062731	38.188696	72.501799
603.557462	34.372783	72.506804
603.233101	32.702537	72.511809
602.156128	31.850692	72.516814
601.611521	42.021398	72.521818
601.012189	33.986622	72.526823
600.659288	38.571555	72.531828
600.160987	24.218025	72.536833
598.831438	34.903215	72.541838
598.474438	34.608450	72.546842
597.968758	32.681671	72.551847
596.524335	34.941128	72.556852
595.870105	33.664016	72.561857
595.428919	46.251335	72.566862
595.602435	35.081693	72.571866
594.913221	35.024327	72.576871
593.404602	40.882922	72.581876
593.112360	30.044487	72.586881
592.227699	36.352454	72.591886
591.880780	34.373585	72.596890
591.211831	36.936871	72.601895
590.048547	36.295883	72.606900
589.934996	30.941658	72.611905
589.081759	26.662385	72.616910
588.440826	29.956020	72.621914
587.715282	44.308967	72.626919
586.802972	33.375331	72.631924
586.570246	23.631218	72.636929
586.140350	32.722431	72.641934
585.516202	38.965258	72.646938
584.588721	37.477795	72.651943
583.845446	34.336840	72.656948
583.453459	27.926320	72.661953
581.959620	37.478700	72.666958
581.461728	32.477404	72.671962
580.909215	37.489918	72.676967
580.308338	40.569034	72.681972
580.414784	32.349326	72.686977
579.516380	37.412197	72.691982
578.514916	28.481176	72.696986
577.935420	32.473034	72.701991
577.620567	34.984659	72.706996
577.038768	30.141798	72.712001
575.651771	39.440639	72.717006
575.002341	44.608932	72.722010
574.868865	39.872850	72.727015
573.518490	34.404970	72.732020
573.266551	34.080861	72.737025
572.701679	35.675159	72.742030
572.360538	37.348933	72.747034
571.333923	23.454848	72.752039
570.301831	26.500147	72.757044
570.143281	25.240285	72.762049
569.392707	28.349550	72.767054
568.678517	34.283465	72.772058
568.041439	28.184778	72.777063
567.278463	29.142044	72.782068
566.811339	25.689050	72.787073
565.836677	35.472541	72.792078
564.848873	22.027989	72.797082
564.506738	27.702385	72.802087
563.873849	36.245653	72.807092
563.990667	29.552263	72.812097
562.902704	40.900692	72.817102
562.186204	28.195043	72.822106
561.776927	27.120185	72.827111
560.803087	33.246833	72.832116
559.869155	31.930707	72.837121
559.221505	40.681320	72.842126
558.578155	34.291916	72.847130
558.242800	33.416582	72.852135
557.675076	35.730380	72.857140
556.970955	33.899866	72.862145
556.487607	32.893573	72.867150
555.513766	31.683147	72.872154
554.721474	20.459202	72.877159
553.798237	27.657932	72.882164
553.608059	20.106755	72.887169
552.600852	27.568001	72.892174
551.823198	26.244333	72.897178
550.977752	25.322521	72.902183
550.707552	30.540791	72.907188
550.507007	35.005272	72.912193
549.934557	32.202950	72.917198
549.033082	31.132377	72.922202
548.083512	31.446055	72.927207
547.502111	34.823252	72.932212
546.982626	26.985501	72.937217
545.990936	33.201724	72.942222
545.168137	33.769582	72.947226
544.956444	34.183339	72.952231
544.575377	42.218179	72.957236
544.019546	30.299022	72.962241
542.694240	31.697500	72.967246
542.159062	25.476944	72.972250
541.635220	20.574406	72.977255
540.701434	29.100949	72.982260
540.180867	32.802749	72.987265
539.844343	30.071654	72.992270
538.877156	36.220904	72.997274
538.389038	22.818193	73.002279
537.272274	39.904636	73.007284
537.392456	23.150418	73.012289
536.457369	34.925479	73.017294
535.367656	20.910589	73.022298
534.555541	30.042186	73.027303
533.834990	40.964697	73.032308
534.034222	23.994473	73.037313
533.497021	27.055569	73.042318
532.379632	24.196559	73.047322
531.899010	32.753420	73.052327
531.252218	29.313283	73.057332
529.961867	27.243440	73.062337
529.092787	29.062809	73.067342
528.592753	38.699753	73.072346
528.243958	28.721841	73.077351
527.858100	30.528891	73.082356
527.446265	29.791892	73.087361
526.769459	22.559488	73.092366
525.915651	34.548671	73.097370
525.207958	30.988934	73.102375
524.078119	34.773595	73.107380
523.247243	24.367884	73.112385
523.085474	41.627045	73.117390
522.519344	36.821124	73.122394
522.490567	34.988696	73.127399
521.310892	37.902992	73.132404
520.582176	24.328890	73.137409
519.940530	32.895633	73.142414
518.908875	39.577097	73.147418
518.486323	30.470317	73.152423
517.769681	33.134251	73.157428
517.399880	27.913887	73.162433
516.347170	38.179726	73.167438
515.318396	38.072399	73.172442
514.726047	28.675722	73.177447
514.420297	37.337187	73.182452
514.258171	31.738412	73.187457
513.537727	37.731680	73.192462
512.485657	37.214930	73.197466
512.045223	28.120463	73.202471
511.283987	40.481236	73.207476
510.443665	35.882987	73.212481
509.476456	43.618562	73.217486
508.790701	38.992538	73.222490
508.412973	32.264392	73.227495
508.065913	40.689606	73.232500
507.822087	29.491842	73.237505
506.668639	35.997179	73.242510
506.067168	30.621344	73.247514
505.273501	40.413869	73.252519
504.026534	38.304014	73.257524
503.681140	24.504866	73.262529
503.508729	24.649034	73.267534
502.892457	29.398920	73.272538
502.010343	32.746762	73.277543
500.965509	37.423003	73.282548
500.862595	37.019973	73.287553
500.131008	40.290226	73.292558
499.130124	32.617475	73.297562
498.514119	30.831287	73.302567
497.893066	40.394479	73.307572
497.082032	29.747512	73.312577
497.006839	39.102332	73.317582
496.083695	35.669958	73.322586
495.246077	34.511968	73.327591
494.803968	40.366292	73.332596
494.297380	21.925356	73.337601
493.199905	27.590780	73.342606
492.281503	30.569116	73.347610
491.871289	32.469931	73.352615
491.711350	37.153436	73.357620
491.027152	29.075452	73.362625
489.883225	26.302685	73.367630
489.089019	39.520210	73.372634
489.089746	37.353522	73.377639
488.071149	35.699274	73.382644
486.988325	30.332320	73.387649
486.486098	33.670110	73.392654
486.260205	39.720212	73.397658
486.068788	29.267838	73.402663
484.595563	32.638892	73.407668
484.196149	25.605148	73.412673
483.797724	35.557046	73.417678
483.120598	32.843951	73.422682
482.357869	35.393819	73.427687
481.430561	32.264870	73.432692
481.055169	36.900701	73.437697
479.819385	42.832581	73.442702
479.281947	33.028223	73.447706
478.897585	22.926692	73.452711
478.226908	36.354757	73.457716
477.185424	43.629120	73.462721
476.292353	33.034650	73.467726
475.731863	31.074055	73.472730
475.599431	26.142293	73.477735
474.811952	37.919086	73.482740
474.854003	37.207554	73.487745
473.873352	44.752907	73.492750
472.928385	38.900402	73.497754
472.382008	36.522848	73.502759
471.119401	30.240011	73.507764
470.461991	33.481108	73.512769
469.859373	36.251461	73.517774
469.238791	28.052972	73.522778
469.335787	27.864084	73.527783
468.459530	38.689992	73.532788
467.934568	35.925853	73.537793
467.195905	32.941887	73.542798
466.671523	39.160958	73.547802
465.630265	33.910386	73.552807
464.489010	31.115129	73.557812
464.562890	27.754154	73.562817
463.690883	40.812203	73.567822
462.609943	32.890466	73.572826
462.251501	29.172616	73.577831
461.619939	37.663653	73.582836
461.366559	33.683076	73.587841
460.275719	27.240427	73.592846
459.314213	29.347337	73.597850
459.333614	35.844028	73.602855
458.671472	32.791108	73.607860
457.580377	29.230977	73.612865
456.857965	34.973852	73.617870
456.173127	36.760739	73.622874
456.077576	32.646216	73.627879
455.001728	39.277975	73.632884
454.172513	24.548315	73.637889
453.410154	34.178173	73.642894
452.770322	36.785736	73.647898
452.927482	30.418636	73.652903
451.757858	36.280065	73.657908
451.276015	31.107524	73.662913
450.714345	38.485212	73.667918
449.973805	48.344978	73.672922
448.954236	28.907213	73.677927
447.814182	38.059543	73.682932
447.861912	32.425765	73.687937
447.422201	33.650088	73.692942
446.373519	36.180873	73.697946
445.717671	27.384078	73.702951
444.975183	34.077838	73.707956
444.607338	34.823966	73.712961
444.055825	29.318773	73.717966
443.144307	37.159026	73.722970
442.329518	29.015139	73.727975
441.880165	31.327446	73.732980
441.105798	25.999677	73.737985
439.943791	25.405864	73.742990
439.390473	39.907993	73.747994
439.128399	24.529780	73.752999
438.523095	27.890306	73.758004
438.418735	27.287250	73.763009
437.563394	33.825538	73.768014
436.348249	32.497497	73.773018
436.152024	14.661538	73.778023
435.155638	35.391834	73.783028
434.319242	25.573629	73.788033
433.613511	30.866026	73.793038
433.382043	36.874440	73.798042
433.380920	37.511683	73.803047
432.052796	33.757531	73.808052
431.339030	26.608314	73.813057
430.655423	37.815093	73.818062
429.957771	34.588078	73.823066
429.231789	25.028232	73.828071
428.501947	28.711358	73.833076
428.099748	37.239968	73.838081
427.474952	33.260229	73.843086
426.025476	33.648869	73.848090
425.789078	31.136790	73.853095
425.026439	45.129841	73.858100
425.183551	33.861905	73.863105
424.547030	39.047091	73.868110
423.542874	38.428135	73.873114
423.159526	28.269687	73.878119
421.825920	42.829914	73.883124
421.178265	32.888605	73.888129
420.519373	31.356836	73.893134
419.823470	41.572165	73.898138
419.828332	23.287873	73.903143
418.696179	39.318734	73.908148
417.959994	32.994628	73.913153
417.468190	29.553483	73.918158
416.931853	33.245202	73.923162
415.922879	28.930890	73.928167
414.862171	31.585019	73.933172
414.583949	34.592261	73.938177
414.197863	33.548424	73.943182
413.938810	33.375265	73.948186
413.103425	37.005831	73.953191
411.791452	37.411993	73.958196
411.776542	35.541092	73.963201
410.850135	36.718397	73.968206
409.925602	47.380140	73.973210
409.329963	31.370723	73.978215
408.783948	34.999336	73.983220
408.598117	32.266327	73.988225
407.321304	41.038368	73.993230
406.414090	40.273095	73.998234
406.247496	33.025662	74.003239
405.664809	36.822534	74.008244
404.979657	28.402558	74.013249
403.937093	32.020408	74.018254
403.681680	38.675993	74.023258
403.117609	22.904393	74.028263
401.736444	37.174175	74.033268
401.109954	19.941327	74.038273
400.719236	29.669662	74.043278
400.333257	17.441248	74.048282
400.194168	33.794815	74.053287
398.975374	43.439074	74.058292
398.305660	28.918973	74.063297
397.673442	30.240205	74.068302
396.982922	30.015957	74.073306
395.882475	25.388246	74.078311
395.331578	37.726558	74.083316
395.065194	30.247465	74.088321
394.837202	33.552612	74.093326
393.709637	30.636945	74.098330
393.301720	35.672179	74.103335
392.510619	43.818092	74.108340
391.324213	25.425595	74.113345
390.247648	30.240962	74.118350
390.088118	33.254522	74.123354
389.952941	38.769812	74.128359
389.140968	34.242782	74.133364
388.670912	25.101036	74.138369
387.573213	29.956039	74.143374
386.849282	34.879212	74.148378
386.716514	24.436437	74.153383
386.048842	32.773976	74.158388
384.870950	26.195437	74.163393
384.114112	41.600420	74.168398
383.772660	32.160653	74.173402
383.093486	30.860769	74.178407
381.917275	36.549824	74.183412
381.301930	32.123921	74.188417
381.151643	33.459822	74.193422
380.423115	35.551714	74.198426
380.073210	25.391105	74.203431
379.077305	43.558972	74.208436
378.746246	30.705255	74.213441
378.425512	29.293068	74.218446
377.069214	32.126768	74.223450
376.507833	21.071099	74.228455
375.719519	36.224066	74.233460
374.859851	30.227139	74.238465
373.872946	29.892440	74.243470
373.414185	27.111470	74.248474
373.342754	27.168598	74.253479
372.692793	29.700527	74.258484
372.351102	32.979641	74.263489
371.069076	16.936137	74.268494
370.357149	29.659626	74.273498
370.086496	25.032156	74.278503
369.140515	27.992852	74.283508
368.377380	32.144891	74.288513
367.734996	23.232449	74.293518
367.427919	30.714646	74.298522
367.281233	25.387802	74.303527
365.902810	22.523163	74.308532
365.115235	21.877604	74.313537
364.744722	24.538456	74.318542
363.527155	34.045341	74.323546
363.107313	17.895989	74.328551
362.122252	34.597233	74.333556
361.946905	29.620285	74.338561
361.508207	30.969032	74.343566
360.731487	22.533707	74.348570
360.180612	30.133596	74.353575
359.421825	30.237183	74.358580
358.952969	24.362479	74.363585
357.826934	26.976581	74.368590
356.784181	19.130819	74.373594
356.659455	13.784713	74.378599
356.061971	28.019503	74.383604
355.359854	29.692482	74.388609
354.487430	35.839305	74.393614
353.618254	33.379189	74.398618
353.588812	26.456818	74.403623
352.447660	29.888561	74.408628
351.923067	35.875884	74.413633
351.106510	37.418879	74.418638
350.265830	36.128972	74.423642
350.225998	26.486622	74.428647
349.960243	34.195610	74.433652
348.962082	16.731877	74.438657
348.111079	28.641803	74.443662
347.265583	45.757608	74.448666
346.426610	34.533300	74.453671
345.409323	35.010800	74.458676
344.855390	28.876860	74.463681
344.742118	28.349340	74.468686
344.182716	41.583087	74.473690
344.083320	29.879828	74.478695
343.025386	30.430034	74.483700
342.132244	29.933760	74.488705
341.849000	42.010246	74.493710
341.064392	33.393266	74.498714
340.422213	35.450910	74.503719
339.099609	35.820959	74.508724
338.791213	30.630267	74.513729
337.604455	31.968927	74.518734
336.801540	32.667717	74.523738
336.933697	17.212522	74.528743
335.957190	36.012766	74.533748
336.041940	29.616209	74.538753
335.251851	33.048780	74.543758
334.579792	39.807033	74.548762
334.195750	24.941838	74.553767
332.634974	21.975400	74.558772
331.962424	34.419829	74.563777
331.518663	27.591870	74.568782
330.555453	34.920033	74.573786
329.964359	24.879869	74.578791
328.951605	23.604779	74.583796
328.705552	23.677122	74.588801
328.378857	41.326793	74.593806
327.785328	37.452478	74.598810
327.657052	26.452370	74.603815
326.214890	28.486128	74.608820
325.685085	17.914268	74.613825
325.454820	26.071727	74.618830
323.993076	44.274425	74.623834
323.375839	34.509640	74.628839
322.784857	26.809498	74.633844
322.436510	32.984765	74.638849
321.408879	29.723647	74.643854
320.534770	26.453832	74.648858
320.445466	22.869724	74.653863
319.755880	39.068185	74.658868
318.910109	31.027051	74.663873
317.954646	35.369016	74.668878
317.052975	27.131804	74.673882
317.237153	15.279297	74.678887
316.573457	31.653384	74.683892
316.177030	27.020738	74.688897
315.097234	24.116420	74.693902
314.267180	21.839307	74.698906
314.553447	23.889327	74.703911
313.166186	34.016169	74.708916
312.525914	23.543911	74.713921
311.727114	26.850151	74.718926
310.515195	26.071979	74.723930
310.075570	16.778765	74.728935
309.316283	31.610166	74.733940
308.821135	26.465012	74.738945
308.692981	27.614474	74.743950
307.870074	24.415347	74.748954
307.118082	30.672289	74.753959
306.324883	25.543101	74.758964
305.767133	24.211273	74.763969
305.435204	27.725364	74.768974
304.319732	21.174768	74.773978
303.691665	20.576342	74.778983
303.124484	32.319629	74.783988
302.906843	28.792242	74.788993
301.483058	29.228897	74.793998
300.855851	33.499629	74.799002
300.583791	25.069047	74.804007
299.894427	36.164806	74.809012
299.685077	36.078349	74.814017
298.548944	32.605891	74.819022
297.496650	33.774917	74.824026
297.508507	27.049381	74.829031
296.237100	30.473525	74.834036
295.444608	31.754099	74.839041
295.209325	34.059117	74.844046
294.559027	38.910658	74.849050
294.209291	36.227437	74.854055
293.155581	38.363296	74.859060
292.318506	37.090180	74.864065
292.032122	29.473955	74.869070
291.356689	26.910450	74.874074
291.006296	32.616145	74.879079
290.085076	35.823642	74.884084
289.780946	35.418001	74.889089
288.689138	32.583413	74.894094
287.526399	30.198493	74.899098
287.142093	33.169039	74.904103
286.583133	41.175482	74.909108
286.260167	34.872290	74.914113
285.393813	33.737876	74.919118
284.501014	29.619558	74.924122
284.389527	26.466312	74.929127
283.116113	40.504521	74.934132
282.404595	34.860883	74.939137
281.996465	35.813714	74.944142
281.153873	36.856289	74.949146
281.046870	20.762750	74.954151
279.998099	35.257126	74.959156
279.356903	33.812456	74.964161
278.517439	31.371285	74.969166
277.978409	35.069766	74.974170
277.569311	22.747305	74.979175
276.331350	27.452830	74.984180
275.727233	30.135159	74.989185
275.351666	28.528313	74.994190
274.957287	34.513815	74.999194
274.440913	27.281158	75.004199
273.725030	27.092524	75.009204
272.915448	28.636007	75.014209
271.792764	26.049184	75.019214
270.861097	26.836319	75.024218
270.938046	22.358453	75.029223
270.306965	40.097631	75.034228
269.611577	23.651626	75.039233
268.833079	21.192859	75.044238
267.870543	22.036952	75.049242
267.677256	25.981501	75.054247
267.023355	34.036189	75.059252
266.059704	26.748679	75.064257
265.492794	23.562377	75.069262
264.708819	25.748286	75.074266
264.382756	20.528890	75.079271
263.254349	34.104048	75.084276
262.686512	28.648815	75.089281
262.047528	22.750794	75.094286
261.238438	28.578485	75.099290
261.588905	14.364172	75.104295
260.442786	32.671102	75.109300
259.349860	23.288078	75.114305
259.406633	25.999100	75.119310
258.119152	30.961669	75.124314
257.346164	33.787606	75.129319
256.510041	36.336622	75.134324
256.078694	31.996538	75.139329
256.002036	26.540282	75.144334
254.716352	33.749569	75.149338
254.288293	26.897052	75.154343
253.996010	24.655659	75.159348
252.943760	26.293017	75.164353
252.157794	24.228080	75.169358
251.135040	30.397316	75.174362
251.145544	29.408555	75.179367
250.525675	30.302106	75.184372
249.825206	20.484398	75.189377
248.877927	9.490293	75.194382
248.220095	24.871610	75.199386
247.793474	14.642852	75.204391
246.556677	29.077321	75.209396
246.100815	16.423308	75.214401
245.910130	15.244283	75.219406
245.240168	31.807019	75.224410
244.851406	20.805876	75.229415
243.470802	23.178350	75.234420
242.940335	19.038564	75.239425
242.614635	21.960351	75.244430
241.411685	22.081161	75.249434
240.804576	23.388966	75.254439
240.226299	20.370052	75.259444
239.795174	25.613988	75.264449
239.362806	16.756422	75.269454
238.029323	24.071095	75.274458
237.821436	19.457297	75.279463
236.943785	27.311126	75.284468
236.975434	31.178824	75.289473
236.250029	22.358506	75.294478
235.277915	28.234266	75.299482
234.500818	22.730404	75.304487
233.541220	28.110617	75.309492
233.111023	27.061228	75.314497
232.357860	16.058260	75.319502
231.717629	19.651460	75.324506
231.383851	15.177571	75.329511
230.134161	24.782656	75.334516
229.584325	21.786017	75.339521
229.323204	19.143874	75.344526
228.573699	32.144592	75.349530
228.284161	23.371483	75.354535
226.913589	21.874374	75.359540
226.467059	25.930251	75.364545
226.166713	22.471249	75.369550
225.019651	27.911308	75.374554
224.303966	19.220324	75.379559
223.565515	31.501818	75.384564
223.231242	30.269994	75.389569
223.108125	23.912887	75.394574
221.942201	25.998856	75.399578
221.208492	24.966315	75.404583
220.678066	29.508621	75.409588
219.979510	20.723451	75.414593
219.011489	16.889948	75.419598
218.309497	24.392526	75.424602
217.978767	15.353197	75.429607
217.615214	17.927807	75.434612
216.594319	21.682611	75.439617
215.996258	16.831414	75.444622
215.155235	22.282609	75.449626
214.899062	18.335631	75.454631
213.302130	24.331498	75.459636
212.795719	15.897300	75.464641
212.461025	19.033396	75.469646
211.945895	22.584583	75.474650
211.853266	10.627989	75.479655
210.822748	19.195270	75.484660
209.854097	22.566459	75.489665
209.360970	24.764363	75.494670
209.144107	20.293915	75.499674
208.277173	13.427805	75.504679
207.165210	36.007278	75.509684
206.798428	25.075174	75.514689
206.418932	26.031335	75.519694
205.291681	25.074150	75.524698
204.719600	17.823592	75.529703
204.009400	20.663184	75.534708
203.061281	21.281092	75.539713
202.552021	20.911317	75.544718
202.396380	33.125135	75.549722
201.795636	17.682722	75.554727
201.032215	23.725480	75.559732
199.740449	22.515424	75.564737
199.311263	22.561785	75.569742
198.827565	31.434537	75.574746
198.376690	22.543662	75.579751
197.436175	20.307854	75.584756
196.647052	19.840780	75.589761
196.320712	16.527843	75.594766
195.763973	24.204375	75.599770
194.871806	12.673267	75.604775
193.813626	27.698977	75.609780
193.205403	17.500760	75.614785
192.964363	26.344286	75.619790
191.968869	36.161164	75.624794
191.548437	29.129263	75.629799
190.557011	25.422495	75.634804
190.493978	21.512533	75.639809
189.950858	9.820136	75.644814
188.589449	29.467026	75.649818
188.387430	19.770138	75.654823
187.741023	25.666522	75.659828
186.773778	27.164209	75.664833
186.073854	17.038957	75.669838
185.256401	27.634791	75.674842
184.974990	16.529828	75.679847
184.505902	16.867961	75.684852
183.526451	19.684257	75.689857
183.180774	21.133311	75.694862
182.036294	28.141933	75.699866
181.707801	19.542192	75.704871
180.925130	25.422457	75.709876
179.776819	27.201307	75.714881
179.802312	18.247110	75.719886
179.105674	35.161014	75.724890
178.592902	9.521348	75.729895
177.364409	16.037194	75.734900
176.731202	19.225616	75.739905
176.573083	25.403676	75.744910
175.654690	32.909230	75.749914
174.788826	34.591019	75.754919
174.032348	29.120158	75.759924
173.614793	21.504374	75.764929
173.466717	22.305382	75.769934
172.575593	25.405624	75.774938
171.720924	22.448137	75.779943
170.901411	32.612251	75.784948
170.335523	28.498628	75.789953
169.694789	24.702845	75.794958
168.624629	31.141423	75.799962
168.327120	24.815279	75.804967
167.960935	19.291660	75.809972
167.323696	22.510687	75.814977
166.271317	26.620589	75.819982
165.521610	24.486827	75.824986
165.060937	23.242051	75.829991
164.798452	26.549555	75.834996
163.805999	30.850164	75.840001
163.135360	18.331336	75.845006
162.377392	25.052854	75.850010
162.100800	26.389979	75.855015
160.971945	28.436953	75.860020
160.090120	42.158904	75.865025
159.998180	21.841782	75.870030
159.398239	28.834553	75.875034
158.482912	28.188930	75.880039
157.563223	28.015479	75.885044
157.020094	23.920307	75.890049
156.870916	30.106404	75.895054
155.800593	38.178624	75.900058
154.788934	24.976202	75.905063
154.339875	33.231623	75.910068
153.942767	25.458052	75.915073
153.645339	31.352418	75.920078
152.339763	30.876242	75.925082
151.694217	20.986742	75.930087
151.265137	29.713604	75.935092
150.880221	30.519261	75.940097
150.295363	34.385908	75.945102
149.244418	29.154380	75.950106
148.358201	38.586447	75.955111
148.242723	25.681082	75.960116
146.761578	31.981782	75.965121
146.272193	42.386566	75.970126
145.728337	39.463103	75.975130
145.314114	17.104906	75.980135
145.033312	28.561290	75.985140
143.984916	40.423899	75.990145
143.423860	30.394777	75.995150
142.660227	39.725304	76.000154
142.199352	30.306216	76.005159
140.838791	34.660795	76.010164
140.320506	53.247699	76.015169
140.275964	23.816751	76.020174
139.677486	25.039632	76.025178
138.996891	21.650733	76.030183
137.941036	32.598383	76.035188
137.399665	30.879234	76.040193
136.853813	27.349010	76.045198
135.837689	32.195837	76.050202
135.143567	35.815000	76.055207
134.831184	34.936065	76.060212
134.238614	34.620586	76.065217
133.644473	14.568044	76.070222
132.531816	32.995819	76.075226
132.168777	26.546099	76.080231
131.355083	29.492093	76.085236
130.200224	33.244639	76.090241
129.942676	35.321424	76.095246
129.166204	27.357628	76.100250
128.911960	33.032237	76.105255
128.409632	33.654782	76.110260
127.616648	32.291123	76.115265
127.155094	22.752313	76.120270
126.276171	42.246622	76.125274
125.407383	19.360132	76.130279
124.581951	29.096297	76.135284
123.897489	23.082579	76.140289
123.913333	25.047967	76.145294
122.813021	42.098784	76.150298
121.866555	27.580358	76.155303
121.306529	29.651760	76.160308
120.923593	33.735358	76.165313
120.759737	19.213571	76.170318
119.618957	18.979200	76.175322
118.910102	20.475133	76.180327
118.429970	29.301595	76.185332
117.103101	24.757431	76.190337
116.603287	22.867671	76.195342
115.627771	25.402688	76.200346
115.667212	19.872746	76.205351
114.950010	32.819450	76.210356
114.595594	25.665087	76.215361
113.944700	25.390449	76.220366
113.151813	30.155959	76.225370
112.335928	23.083065	76.230375
111.330125	23.637671	76.235380
110.716147	32.572203	76.240385
110.806745	31.852927	76.245390
109.388074	38.738157	76.250394
108.840955	29.935185	76.255399
107.931716	29.198731	76.260404
107.217674	27.590696	76.265409
107.000449	27.614313	76.270414
106.470787	34.148067	76.275418
106.166497	24.797058	76.280423
105.318093	25.290301	76.285428
104.317962	33.302461	76.290433
103.751506	26.800033	76.295438
102.363191	40.637448	76.300442
102.167123	19.673098	76.305447
101.784807	29.045318	76.310452
101.536989	29.977344	76.315457
100.274349	35.260857	76.320462
99.496907	17.978105	76.325466
99.386966	22.552720	76.330471
98.669355	35.021711	76.335476
97.238358	28.840055	76.340481
97.086383	28.307682	76.345486
96.481634	35.644985	76.350490
95.954520	18.725988	76.355495
94.883836	15.807709	76.360500
93.854232	30.513523	76.365505
93.923548	25.164883	76.370510
93.264954	23.197953	76.375514
92.406356	18.378877	76.380519
91.676311	23.948019	76.385524
90.865630	26.393687	76.390529
90.826550	21.891751	76.395534
90.212162	34.049414	76.400538
88.980247	29.797608	76.405543
88.269191	22.594475	76.410548
87.827710	27.078467	76.415553
87.385356	25.518571	76.420558
86.190474	38.902553	76.425562
85.558505	18.766180	76.430567
85.392020	27.954183	76.435572
84.612416	28.824365	76.440577
83.802872	25.927520	76.445582
82.734515	28.232944	76.450586
82.437223	15.735035	76.455591
82.013665	28.716910	76.460596
81.510528	35.749450	76.465601
80.571789	29.634377	76.470606
79.722438	30.583486	76.475610
79.331777	25.672448	76.480615
78.992766	34.632520	76.485620
77.819703	21.214627	76.490625
77.312122	21.494269	76.495630
76.648995	25.294568	76.500634
76.038258	29.564296	76.505639
74.890789	33.911734	76.510644
74.166619	27.040254	76.515649
73.741811	23.530166	76.520654
73.529722	25.681701	76.525658
73.011575	22.342605	76.530663
71.777585	32.534993	76.535668
71.442957	37.340971	76.540673
70.896423	26.664633	76.545678
70.050774	30.697454	76.550682
69.584794	26.947945	76.555687
68.905456	29.576087	76.560692
68.068064	35.857744	76.565697
67.412619	19.490618	76.570702
66.488105	21.454588	76.575706
66.064059	16.827980	76.580711
65.184708	30.212102	76.585716
64.457298	33.245275	76.590721
63.872158	34.434510	76.595726
63.174281	29.578774	76.600730
62.768243	25.933240	76.605735
62.424713	23.381526	76.610740
61.392704	23.689614	76.615745
60.660371	31.756844	76.620750
59.861909	36.857550	76.625754
59.609596	26.296710	76.630759
58.558470	29.811986	76.635764
57.684276	23.177313	76.640769
57.620845	24.882548	76.645774
56.923812	31.080326	76.650778
56.090706	29.754627	76.655783
55.094608	19.941567	76.660788
54.569262	17.795715	76.665793
54.521052	12.407481	76.670798
53.413296	31.783750	76.675802
52.904619	25.270547	76.680807
52.149387	22.664652	76.685812
51.517178	33.847520	76.690817
51.115304	28.861010	76.695822
49.865172	25.750610	76.700826
49.051771	21.655996	76.705831
48.916414	29.188085	76.710836
48.487685	20.691086	76.715841
48.120629	21.911771	76.720846
46.989330	27.918628	76.725850
46.338148	21.220012	76.730855
45.129545	9.291624	76.735860
44.200884	26.371834	76.740865
43.867782	27.743212	76.745870
43.061002	30.864737	76.750874
43.475904	20.093426	76.755879
42.811885	15.680123	76.760884
41.668228	36.795072	76.765889
41.401357	29.926361	76.770894
40.166892	27.780071	76.775898
38.950574	23.943669	76.780903
38.177502	32.526721	76.785908
37.589111	27.768642	76.790913
37.373109	31.024591	76.795918
37.387217	23.324230	76.800922
37.319216	23.372937	76.805927
36.520971	24.675006	76.810932
35.307657	27.391470	76.815937
34.241998	27.433720	76.820942
32.876944	32.921240	76.825946
32.618444	25.677487	76.830951
32.499797	28.790186	76.835956
31.826130	26.800447	76.840961
31.292515	20.133546	76.845966
30.326055	24.641351	76.850970
29.520884	31.591189	76.855975
29.057187	35.652987	76.860980
28.546658	35.773849	76.865985
27.747848	19.596751	76.870990
26.662485	33.623976	76.875994
26.550830	38.430664	76.880999
25.852740	34.199402	76.886004
24.736855	26.964668	76.891009
24.711945	31.722829	76.896014
24.232428	21.715440	76.901018
23.176329	19.688934	76.906023
22.144245	26.719113	76.911028
21.580307	31.678352	76.916033
21.371697	28.685686	76.921038
20.590036	38.159453	76.926042
19.712467	34.568631	76.931047
19.254083	22.038083	76.936052
18.594802	53.605937	76.941057
17.891577	28.980642	76.946062
16.967973	38.688345	76.951066
16.422152	27.280257	76.956071
16.152855	31.533385	76.961076
14.723829	38.469197	76.966081
14.281961	26.724433	76.971086
13.720022	38.526838	76.976090
13.137539	31.123462	76.981095
12.869834	26.836178	76.986100
11.813390	24.243647	76.991105
11.235132	22.727518	76.996110
10.473872	29.621474	77.001114
9.908317	30.966858	77.006119
9.099274	29.239974	77.011124
8.301904	27.022409	77.016129
8.140753	24.589839	77.021134
7.518228	30.012553	77.026139
6.790005	27.396058	77.031143
5.815639	30.651548	77.036148
5.024988	28.106507	77.041153
4.817910	28.970546	77.046158