Mon Mar 08 19:59:56 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.816041	95.128959	0.000000
-0.344516	94.963872	0.005005
-1.623479	48.764577	0.010010
-2.978059	-4.321159	0.015014
-7.149125	-25.606855	0.020019
-13.098886	-15.396958	0.025024
-18.584343	-32.254910	0.030029
-23.354388	-16.296419	0.035034
-27.040649	-25.246585	0.040038
-30.194341	-27.610130	0.045043
-34.361036	-19.844905	0.050048
-37.620341	-28.752789	0.055053
-41.435518	-14.723690	0.060058
-44.963821	-13.220978	0.065062
-48.681634	-22.500365	0.070067
-52.408136	-9.868275	0.075072
-55.811679	-27.682724	0.080077
-59.810103	-17.293650	0.085082
-64.308199	-17.403811	0.090086
-67.643018	-28.492976	0.095091
-71.684689	-15.801118	0.100096
-75.421687	-29.191350	0.105101
-78.981684	-23.643693	0.110106
-82.459809	-20.594178	0.115110
-86.324233	-30.512375	0.120115
-90.289841	-21.828316	0.125120
-93.991547	-25.343725	0.130125
-98.261879	-26.664904	0.135130
-101.813901	-22.444600	0.140134
-105.623258	-27.871277	0.145139
-109.698106	-17.069417	0.150144
-113.266315	-17.272678	0.155149
-117.074494	-22.749984	0.160154
-120.287117	-10.970870	0.165158
-123.889542	-12.830636	0.170163
-128.038676	-14.868063	0.175168
-131.496640	-25.666268	0.180173
-135.538408	-14.723000	0.185178
-139.221756	-9.775263	0.190182
-142.720097	-21.453191	0.195187
-146.844497	-14.703701	0.200192
-150.532237	-18.547655	0.205197
-154.221374	-15.212071	0.210202
-157.766055	-13.665585	0.215206
-161.216211	-10.577847	0.220211
-165.605183	-13.836821	0.225216
-169.295807	-21.079932	0.230221
-173.841323	-18.339296	0.235226
-176.980361	-20.345469	0.240230
-180.298857	-16.233279	0.245235
-184.240551	-11.253706	0.250240
-187.909646	-20.901735	0.255245
-191.981675	-20.258131	0.260250
-196.051443	-17.945017	0.265254
-199.477188	-14.766513	0.270259
-203.365385	-18.898487	0.275264
-206.642488	-21.347748	0.280269
-210.769076	-15.548633	0.285274
-214.601348	-20.597767	0.290278
-218.284990	-24.046483	0.295283
-221.939787	-24.492785	0.300288
-225.633994	-25.090474	0.305293
-230.018735	-24.095717	0.310298
-233.371163	-32.651008	0.315302
-236.589362	-26.433923	0.320307
-240.649909	-20.039799	0.325312
-244.320391	-23.930510	0.330317
-248.452736	-13.708986	0.335322
-252.515860	-15.092926	0.340326
-255.749470	-22.766788	0.345331
-259.761775	-10.178664	0.350336
-263.435135	-18.681112	0.355341
-267.148173	-19.559560	0.360346
-270.564396	-24.277655	0.365350
-274.752433	-23.910259	0.370355
-278.670710	-20.657750	0.375360
-282.080882	-20.613198	0.380365
-285.675956	-25.551857	0.385370
-289.458597	-14.272854	0.390374
-293.154200	-12.273180	0.395379
-297.068656	-21.307895	0.400384
-301.204431	-21.694635	0.405389
-305.360725	-17.721318	0.410394
-308.798147	-19.384812	0.415398
-312.154776	-28.259414	0.420403
-316.197631	-18.137220	0.425408
-319.879283	-20.200064	0.430413
-323.899071	-20.181116	0.435418
-327.531049	-13.943575	0.440422
-330.652311	-22.527751	0.445427
-334.440969	-7.475948	0.450432
-338.580351	-23.829002	0.455437
-342.567064	-21.637706	0.460442
-346.251935	-20.125329	0.465446
-349.908049	-17.967884	0.470451
-353.995501	-5.783896	0.475456
-357.370330	-24.447626	0.480461
-360.983584	-23.121689	0.485466
-365.064469	-19.128775	0.490470
-368.436972	-18.848860	0.495475
-372.664475	-18.703632	0.500480
-376.459393	-24.103786	0.505485
-380.273913	-22.879713	0.510490
-383.828271	-26.620025	0.515494
-387.337725	-21.173033	0.520499
-391.214940	-17.441238	0.525504
-394.914189	-23.834272	0.530509
-398.506745	-27.801832	0.535514
-402.711808	-23.454741	0.540518
-406.557883	-20.942051	0.545523
-410.499799	-18.596960	0.550528
-413.672646	-24.239885	0.555533
-417.689791	-18.882071	0.560538
-421.668585	-26.187551	0.565542
-425.169613	-25.823958	0.570547
-429.150409	-22.405119	0.575552
-432.881104	-14.956428	0.580557
-436.404728	-27.585401	0.585562
-440.217988	-23.121060	0.590566
-443.731726	-21.072938	0.595571
-447.898628	-16.047519	0.600576
-451.402284	-24.065869	0.605581
-455.377187	-14.889363	0.610586
-459.324820	-6.496153	0.615590
-462.504525	-19.474886	0.620595
-466.534049	-18.714613	0.625600
-470.290969	-16.339053	0.630605
-473.562468	-20.633722	0.635610
-477.928392	-19.441262	0.640614
-481.949192	-25.049572	0.645619
-485.757679	-13.534362	0.650624
-488.781132	-23.887367	0.655629
-492.979658	-20.061516	0.660634
-496.676175	-10.240336	0.665638
-500.194985	-27.491649	0.670643
-504.328437	-4.356919	0.675648
-507.802445	-17.058361	0.680653
-511.761520	-14.541645	0.685658
-515.415014	-15.306224	0.690662
-518.963384	-10.204458	0.695667
-522.944492	-12.887724	0.700672
-526.350242	-15.809536	0.705677
-530.782347	-17.922469	0.710682
-535.042989	-10.757945	0.715686
-538.354412	-15.585420	0.720691
-541.697901	-15.686756	0.725696
-545.316208	-20.812096	0.730701
-549.492015	-19.266709	0.735706
-552.970012	-9.392054	0.740710
-556.717396	-11.499216	0.745715
-560.698536	-8.679298	0.750720
-564.242183	-30.814685	0.755725
-568.178844	-11.957691	0.760730
-571.542355	-20.848153	0.765734
-575.585103	-15.599522	0.770739
-579.389457	-19.551888	0.775744
-583.203146	-25.068541	0.780749
-587.029115	-3.253730	0.785754
-590.888407	-16.278229	0.790758
-594.282476	-26.813126	0.795763
-598.326558	-18.446869	0.800768
-601.784143	-19.159044	0.805773
-605.869703	-17.200658	0.810778
-609.474456	-19.332100	0.815782
-612.926090	-23.716050	0.820787
-617.657620	-12.092583	0.825792
-620.672956	-26.324107	0.830797
-624.591487	-16.421544	0.835802
-628.482306	-17.796102	0.840806
-631.996031	-25.002073	0.845811
-636.049880	-8.567170	0.850816
-639.548188	-22.942252	0.855821
-643.311544	-16.514541	0.860826
-647.661025	-14.324693	0.865830
-650.718396	-23.604545	0.870835
-654.193186	-21.723176	0.875840
-658.104103	-25.451819	0.880845
-662.038786	-29.611859	0.885850
-665.904766	-14.389553	0.890854
-669.904060	-15.499147	0.895859
-674.060033	-6.064717	0.900864
-677.350608	-19.895820	0.905869
-681.176174	-21.260218	0.910874
-684.801234	-15.009072	0.915878
-688.362759	-18.211654	0.920883
-692.313348	-10.271733	0.925888
-695.820855	-19.331366	0.930893
-699.350600	-22.619427	0.935898
-703.259900	-15.699984	0.940902
-707.318848	-22.262086	0.945907
-711.071288	-14.681783	0.950912
-714.707802	-14.185733	0.955917
-718.886391	-18.286200	0.960922
-722.811668	-17.969473	0.965926
-725.893221	-29.337790	0.970931
-730.275818	-15.377850	0.975936
-733.744381	-11.081670	0.980941
-737.169217	-17.992630	0.985946
-741.018914	-11.771723	0.990950
-744.666633	-17.391899	0.995955
-748.496659	-10.130269	1.000960
-752.122073	-24.819134	1.005965
-756.158302	-23.167973	1.010970
-760.568186	-11.408009	1.015974
-763.846576	-17.104532	1.020979
-767.607867	-16.747716	1.025984
-771.286578	-14.492988	1.030989
-774.872212	-14.060167	1.035994
-779.089184	-13.088068	1.040998
-782.218328	-20.998623	1.046003
-786.668421	-3.036856	1.051008
-789.916448	-23.221284	1.056013
-793.497203	-19.621386	1.061018
-797.797246	-22.319423	1.066022
-801.684276	-16.483506	1.071027
-805.613105	-15.417084	1.076032
-808.684163	-24.983083	1.081037
-812.016411	-31.311109	1.086042
-816.326741	-19.902830	1.091046
-819.745220	-29.384888	1.096051
-824.141190	-24.366362	1.101056
-827.805844	-23.841988	1.106061
-831.510971	-21.568753	1.111066
-835.532846	-23.185342	1.116070
-839.001086	-35.716859	1.121075
-842.735266	-27.932720	1.126080
-846.295588	-34.731965	1.131085
-850.247126	-17.870016	1.136090
-854.048984	-17.957546	1.141094
-857.689093	-26.486404	1.146099
-861.725286	-18.545145	1.151104
-865.249034	-31.190741	1.156109
-868.536791	-20.997603	1.161114
-872.719016	-16.730614	1.166118
-876.625647	-26.437284	1.171123
-880.899651	-10.660607	1.176128
-884.288087	-11.815470	1.181133
-887.797755	-20.461325	1.186138
-891.434393	-15.704423	1.191142
-895.119925	-19.564888	1.196147
-899.130035	-12.767774	1.201152
-902.769926	-12.332391	1.206157
-906.713426	-13.493075	1.211162
-910.630542	-19.109326	1.216166
-914.019289	-31.975107	1.221171
-917.810827	-17.970601	1.226176
-921.758680	-20.344712	1.231181
-925.259290	-22.850253	1.236186
-929.248543	-24.268486	1.241190
-932.893573	-26.902294	1.246195
-936.991427	-18.102725	1.251200
-940.636852	-24.669038	1.256205
-944.472807	-14.009697	1.261210
-948.286912	-16.791471	1.266214
-951.838146	-18.200873	1.271219
-955.796965	-4.770315	1.276224
-959.237658	-16.236978	1.281229
-963.234649	-23.775115	1.286234
-966.999327	-14.114225	1.291238
-970.049159	-21.838516	1.296243
-974.478636	-9.223562	1.301248
-978.258092	-11.974563	1.306253
-981.808352	-13.570140	1.311258
-985.759338	-20.312996	1.316262
-989.253941	-31.640100	1.321267
-993.307719	3.269318	1.326272
-996.935538	-18.959090	1.331277
-1000.543067	-20.635356	1.336282
-1004.579832	-23.124402	1.341286
-1008.488574	-23.390110	1.346291
-1012.088104	-18.419786	1.351296
-1015.605373	-13.762207	1.356301
-1019.397633	-19.571689	1.361306
-1023.454086	-21.737459	1.366310
-1026.807691	-29.649601	1.371315
-1030.947321	-16.186862	1.376320
-1034.719301	-16.717232	1.381325
-1038.492676	-16.179869	1.386330
-1041.881652	-13.699856	1.391334
-1045.619836	-22.340440	1.396339
-1049.683163	-17.664845	1.401344
-1053.424112	-22.977894	1.406349
-1057.006913	-18.268777	1.411354
-1060.879180	-21.416341	1.416358
-1064.433153	-28.424395	1.421363
-1068.284752	-22.380853	1.426368
-1072.095654	-25.498793	1.431373
-1075.960065	-27.671539	1.436378
-1080.154275	-21.510096	1.441382
-1083.177245	-29.235369	1.446387
-1086.923556	-24.895831	1.451392
-1090.905049	-25.378400	1.456397
-1094.783108	-23.017171	1.461402
-1098.793096	-16.438928	1.466406
-1102.225262	-26.320442	1.471411
-1106.145269	-14.606712	1.476416
-1109.518468	-17.427220	1.481421
-1113.258312	-32.633266	1.486426
-1117.721688	-19.345654	1.491430
-1121.473481	-20.937154	1.496435
-1124.874717	-17.135269	1.501440
-1128.703991	-22.624856	1.506445
-1132.369018	-31.125617	1.511450
-1136.411934	-26.330152	1.516454
-1139.759696	-27.530567	1.521459
-1143.495477	-17.106129	1.526464
-1147.166525	-30.415181	1.531469
-1151.300267	-29.545610	1.536474
-1155.068089	-30.847509	1.541478
-1158.648541	-31.342095	1.546483
-1162.351367	-17.706208	1.551488
-1166.277338	-23.265405	1.556493
-1169.833528	-21.124274	1.561498
-1173.881268	-18.114500	1.566502
-1177.208680	-27.946430	1.571507
-1181.236900	-15.243951	1.576512
-1184.951255	-13.511110	1.581517
-1188.872220	-12.197747	1.586522
-1192.625427	-16.893648	1.591526
-1196.132014	-24.339545	1.596531
-1200.036331	-20.971089	1.601536
-1203.643566	-31.183935	1.606541
-1207.790758	-20.452314	1.611546
-1211.847738	-11.285122	1.616550
-1214.957462	-30.970635	1.621555
-1219.030322	-21.695249	1.626560
-1222.579269	-31.879548	1.631565
-1225.803702	-30.477339	1.636570
-1230.153214	-20.742959	1.641574
-1234.013175	-18.549961	1.646579
-1238.136037	-12.763903	1.651584
-1241.456755	-17.964139	1.656589
-1244.908320	-22.835948	1.661594
-1248.495855	-15.951365	1.666598
-1252.246354	-26.866537	1.671603
-1256.889346	-19.379395	1.676608
-1260.724055	-21.379981	1.681613
-1264.279941	-26.522042	1.686618
-1267.777400	-24.060610	1.691622
-1271.041978	-28.076138	1.696627
-1275.319615	-27.650051	1.701632
-1279.136943	-19.889781	1.706637
-1282.647671	-13.692316	1.711642
-1286.677745	-12.421242	1.716646
-1290.628251	-17.332958	1.721651
-1294.260369	-21.051525	1.726656
-1297.685729	-23.306789	1.731661
-1301.570084	-21.034089	1.736666
-1305.591416	-18.712651	1.741670
-1308.837859	-21.967853	1.746675
-1312.625183	-21.665911	1.751680
-1316.385050	-22.713375	1.756685
-1320.189214	-18.400476	1.761690
-1324.522342	-16.316072	1.766694
-1328.345624	-22.727132	1.771699
-1332.160519	-16.167119	1.776704
-1335.684308	-27.962030	1.781709
-1339.018780	-32.622221	1.786714
-1342.991533	-31.633015	1.791718
-1346.469030	-28.110317	1.796723
-1350.596432	-23.107015	1.801728
-1354.540654	-18.648648	1.806733
-1357.764671	-28.433778	1.811738
-1361.543831	-18.795204	1.816742
-1365.132111	-33.564635	1.821747
-1369.234367	-31.725250	1.826752
-1373.316290	-26.498978	1.831757
-1377.072964	-23.503918	1.836762
-1380.873252	-21.009602	1.841766
-1384.230427	-24.609631	1.846771
-1388.010144	-20.179123	1.851776
-1391.569797	-29.815855	1.856781
-1395.630921	-28.281026	1.861786
-1399.822327	-24.527260	1.866790
-1403.327080	-23.385823	1.871795
-1406.950629	-20.479833	1.876800
-1410.600356	-26.286238	1.881805
-1414.407480	-25.209900	1.886810
-1418.298717	-16.631828	1.891814
-1421.859670	-18.113056	1.896819
-1425.855307	-20.857077	1.901824
-1429.878158	-25.848413	1.906829
-1432.988787	-29.724367	1.911834
-1436.763770	-26.551256	1.916838
-1440.637793	-29.637968	1.921843
-1444.878818	-16.306535	1.926848
-1448.475980	-26.047545	1.931853
-1451.685790	-25.710132	1.936858
-1455.986835	-26.393187	1.941862
-1459.605602	-24.736713	1.946867
-1463.336568	-21.515419	1.951872
-1467.226899	-31.365549	1.956877
-1470.635602	-20.015381	1.961882
-1474.398931	-21.826783	1.966886
-1478.095478	-36.115097	1.971891
-1482.047713	-26.647302	1.976896
-1486.044746	-31.576444	1.981901
-1490.060637	-24.709630	1.986906
-1493.846701	-16.632360	1.991910
-1497.158738	-28.153438	1.996915
-1501.217816	-15.698557	2.006912
-1502.224437	-20.033809	2.016909
-1499.377937	-16.533133	2.026906
-1496.713273	-23.961958	2.036902
-1494.445987	-22.943577	2.046899
-1492.943293	-24.148875	2.056896
-1490.931387	-22.202291	2.066893
-1489.029029	-25.427758	2.076890
-1487.071319	-22.621504	2.086886
-1485.083510	-18.015471	2.096883
-1483.261933	-32.278191	2.106880
-1481.538983	-20.922892	2.116877
-1479.193286	-25.351369	2.126874
-1477.381665	-17.111076	2.136870
-1475.578695	-11.509189	2.146867
-1473.642318	-19.770233	2.156864
-1471.876742	-14.503382	2.166861
-1469.697067	-26.987271	2.176858
-1468.227344	-15.422470	2.186854
-1466.251809	-20.903150	2.196851
-1464.336388	-26.336309	2.206848
-1462.431065	-18.854635	2.216845
-1460.503999	-29.697132	2.226842
-1458.675970	-21.606283	2.236838
-1456.590136	-31.223771	2.246835
-1454.972182	-16.891336	2.256832
-1452.910553	-26.176552	2.266829
-1450.918635	-24.525129	2.276826
-1449.308961	-23.039845	2.286822
-1447.456243	-26.595198	2.296819
-1445.700833	-11.424301	2.306816
-1443.530976	-19.260114	2.316813
-1441.333670	-29.757480	2.326810
-1439.725446	-16.165520	2.336806
-1437.859526	-16.424813	2.346803
-1436.035094	-20.591372	2.356800
-1434.259889	-14.512936	2.366797
-1432.271171	-22.131853	2.376794
-1430.481348	-21.111158	2.386790
-1428.366965	-28.311277	2.396787
-1426.442912	-24.061270	2.406784
-1424.839069	-25.401133	2.416781
-1422.806560	-27.460111	2.426778
-1420.852123	-30.237581	2.436774
-1419.137213	-22.373303	2.446771
-1417.334058	-21.823643	2.456768
-1415.239556	-25.286645	2.466765
-1413.165742	-24.079321	2.476762
-1411.884220	-26.431694	2.486758
-1409.522036	-16.154396	2.496755
-1407.807091	-27.542322	2.506752
-1406.171587	-23.023481	2.516749
-1404.212461	-26.428484	2.526746
-1401.995594	-26.616055	2.536742
-1400.430638	-20.800749	2.546739
-1398.429572	-21.995789	2.556736
-1396.545377	-23.475251	2.566733
-1394.439405	-24.336585	2.576730
-1392.843730	-28.464905	2.586726
-1391.002543	-31.486303	2.596723
-1388.952309	-23.096259	2.606720
-1387.182027	-24.322230	2.616717
-1385.238894	-26.125304	2.626714
-1383.365079	-15.215616	2.636710
-1381.472610	-21.589176	2.646707
-1379.672823	-24.820238	2.656704
-1377.909282	-22.922203	2.666701
-1375.793985	-19.198520	2.676698
-1373.716878	-29.262933	2.686694
-1372.133994	-23.325750	2.696691
-1370.126366	-25.257550	2.706688
-1368.377651	-24.995956	2.716685
-1366.654404	-18.924935	2.726682
-1364.824906	-19.442002	2.736678
-1362.601584	-23.470277	2.746675
-1360.642336	-23.577094	2.756672
-1358.976966	-26.889244	2.766669
-1357.159020	-29.179058	2.776666
-1355.303440	-27.671501	2.786662
-1353.554666	-27.179396	2.796659
-1351.555426	-20.803627	2.806656
-1349.537238	-22.424493	2.816653
-1347.677920	-31.268318	2.826650
-1345.634835	-27.967226	2.836646
-1344.010902	-18.031106	2.846643
-1342.253533	-24.239335	2.856640
-1340.068051	-23.807658	2.866637
-1337.962101	-23.170631	2.876634
-1336.479584	-28.586489	2.886630
-1334.527903	-26.323831	2.896627
-1333.031209	-23.980441	2.906624
-1330.725106	-32.201093	2.916621
-1328.859405	-28.402678	2.926618
-1327.001785	-26.906476	2.936614
-1325.104940	-22.792539	2.946611
-1323.533889	-19.862670	2.956608
-1321.225272	-26.760660	2.966605
-1319.653965	-16.847672	2.976602
-1317.469077	-25.850956	2.986598
-1315.866476	-24.369180	2.996595
-1313.989182	-23.202934	3.006592
-1312.061382	-27.990636	3.016589
-1310.031369	-28.306091	3.026586
-1308.390863	-22.093894	3.036582
-1306.405553	-21.467524	3.046579
-1304.812193	-26.440090	3.056576
-1302.609995	-18.710551	3.066573
-1300.606814	-20.698419	3.076570
-1298.919121	-32.282423	3.086566
-1296.737956	-27.792428	3.096563
-1295.351909	-17.636625	3.106560
-1293.346262	-20.749007	3.116557
-1291.506055	-22.462904	3.126554
-1289.531819	-18.023454	3.136550
-1287.524983	-26.444043	3.146547
-1285.563714	-20.504207	3.156544
-1284.084974	-15.595469	3.166541
-1282.154442	-23.815961	3.176538
-1279.915782	-23.282221	3.186534
-1278.199624	-24.049480	3.196531
-1276.474257	-24.139315	3.206528
-1274.723578	-26.053590	3.216525
-1272.358583	-22.114005	3.226522
-1270.687424	-22.659335	3.236518
-1268.797051	-23.236593	3.246515
-1266.991749	-18.950070	3.256512
-1265.121821	-18.875153	3.266509
-1263.264389	-30.235271	3.276506
-1261.301821	-28.111651	3.286502
-1259.440350	-22.392643	3.296499
-1257.670399	-30.026928	3.306496
-1256.068718	-18.674124	3.316493
-1253.813603	-25.323507	3.326490
-1251.819415	-21.000893	3.336486
-1249.931876	-27.796689	3.346483
-1248.287038	-26.934212	3.356480
-1246.170293	-24.459492	3.366477
-1244.449622	-25.271655	3.376474
-1242.578988	-20.883472	3.386470
-1240.735108	-25.798204	3.396467
-1238.679004	-23.716373	3.406464
-1236.910399	-21.561688	3.416461
-1235.032738	-21.562190	3.426458
-1233.476646	-22.212227	3.436454
-1231.462604	-24.354920	3.446451
-1229.369261	-21.271747	3.456448
-1227.712273	-20.152270	3.466445
-1225.759998	-24.695947	3.476442
-1223.675029	-28.248828	3.486438
-1221.820031	-26.463194	3.496435
-1220.088046	-13.481333	3.506432
-1218.157391	-17.942604	3.516429
-1216.250830	-18.707133	3.526426
-1214.471819	-14.795277	3.536422
-1212.368416	-25.302689	3.546419
-1210.718316	-20.702357	3.556416
-1208.932597	-24.399953	3.566413
-1207.026222	-27.101669	3.576410
-1204.985025	-24.706392	3.586406
-1203.239120	-23.938997	3.596403
-1201.350377	-21.700885	3.606400
-1199.313410	-27.360117	3.616397
-1197.439828	-20.315196	3.626394
-1195.973815	-24.949969	3.636390
-1193.764741	-24.690864	3.646387
-1191.650041	-26.222836	3.656384
-1190.174586	-19.497854	3.666381
-1188.341334	-15.649916	3.676378
-1186.162322	-13.455082	3.686374
-1184.398698	-20.872009	3.696371
-1182.667727	-17.730805	3.706368
-1180.444410	-14.346301	3.716365
-1178.801088	-23.175973	3.726362
-1176.812796	-19.040227	3.736358
-1175.033844	-19.048568	3.746355
-1173.313808	-14.964622	3.756352
-1171.367990	-14.514959	3.766349
-1169.392275	-14.272169	3.776346
-1167.312323	-17.307923	3.786342
-1165.620679	-23.609716	3.796339
-1163.839615	-18.053007	3.806336
-1161.862734	-21.831680	3.816333
-1159.782927	-25.674186	3.826330
-1158.243568	-17.798965	3.836326
-1156.376759	-25.117127	3.846323
-1154.357514	-22.285692	3.856320
-1152.358873	-25.930481	3.866317
-1150.842416	-16.090681	3.876314
-1148.778143	-26.555468	3.886310
-1146.876885	-17.669276	3.896307
-1144.812452	-24.624343	3.906304
-1143.259362	-16.571320	3.916301
-1141.561825	-20.347911	3.926298
-1139.232664	-25.223380	3.936294
-1137.349182	-26.928293	3.946291
-1135.636844	-31.089322	3.956288
-1133.454020	-28.394560	3.966285
-1132.009751	-22.076623	3.976282
-1130.043016	-32.852603	3.986278
-1128.014093	-24.550466	3.996275
-1126.148280	-22.365461	4.006272
-1124.611300	-24.865915	4.016269
-1122.495731	-22.274057	4.026266
-1120.273795	-28.556458	4.036262
-1118.806828	-18.642407	4.046259
-1116.930231	-24.062773	4.056256
-1115.111318	-16.331711	4.066253
-1113.044158	-21.747829	4.076250
-1111.307764	-21.657739	4.086246
-1109.056068	-20.357027	4.096243
-1107.636467	-22.515032	4.106240
-1105.777111	-27.135320	4.116237
-1103.761413	-26.207343	4.126234
-1101.892458	-25.794269	4.136230
-1099.748958	-30.831035	4.146227
-1097.957271	-20.444748	4.156224
-1096.359775	-17.877342	4.166221
-1094.175554	-29.652759	4.176218
-1092.294919	-21.137402	4.186214
-1090.554392	-23.215695	4.196211
-1088.869115	-30.471610	4.206208
-1086.716256	-27.419929	4.216205
-1084.869635	-15.926181	4.226202
-1083.069742	-34.702219	4.236198
-1081.447434	-26.800745	4.246195
-1079.418117	-25.200764	4.256192
-1077.494204	-21.005687	4.266189
-1075.495824	-24.819305	4.276186
-1073.720116	-28.677821	4.286182
-1071.829667	-23.597976	4.296179
-1069.893251	-23.547748	4.306176
-1068.018188	-13.342123	4.316173
-1066.248697	-17.366998	4.326170
-1064.205099	-22.406700	4.336166
-1062.214856	-22.099833	4.346163
-1060.444723	-19.661063	4.356160
-1058.957112	-21.673614	4.366157
-1056.792061	-20.469508	4.376154
-1055.126108	-18.470352	4.386150
-1053.090790	-22.875609	4.396147
-1051.002995	-17.786262	4.406144
-1049.363140	-23.651831	4.416141
-1047.386133	-22.427110	4.426138
-1045.370653	-23.390489	4.436134
-1043.685754	-26.713442	4.446131
-1042.069511	-23.465363	4.456128
-1039.975530	-18.939060	4.466125
-1037.774469	-23.050313	4.476122
-1036.064882	-24.624706	4.486118
-1034.301084	-31.522120	4.496115
-1032.365438	-26.984695	4.506112
-1030.917835	-22.714968	4.516109
-1028.554860	-24.501229	4.526106
-1026.628089	-30.755280	4.536102
-1024.866288	-19.802082	4.546099
-1023.050623	-30.699075	4.556096
-1021.060349	-20.911285	4.566093
-1019.289695	-29.344412	4.576090
-1017.462056	-24.134482	4.586086
-1015.302331	-27.176548	4.596083
-1013.593220	-23.905409	4.606080
-1011.755690	-17.710284	4.616077
-1009.794149	-34.810153	4.626074
-1008.107922	-19.913560	4.636070
-1006.136348	-22.873423	4.646067
-1004.447427	-18.078630	4.656064
-1002.432877	-29.991034	4.666061
-1000.694699	-21.733843	4.676058
-998.390145	-35.317243	4.686054
-996.733764	-15.193083	4.696051
-995.003449	-22.940847	4.706048
-993.127120	-28.788940	4.716045
-991.226401	-25.221611	4.726042
-988.967076	-26.092899	4.736038
-987.358625	-28.252617	4.746035
-985.668012	-29.291872	4.756032
-983.535019	-16.601290	4.766029
-981.854226	-27.069349	4.776026
-980.049631	-30.004062	4.786022
-977.909274	-25.886144	4.796019
-975.735859	-29.127718	4.806016
-974.466625	-24.286307	4.816013
-972.430945	-32.125517	4.826010
-970.450373	-24.699642	4.836006
-968.676754	-29.225595	4.846003
-966.687345	-24.125172	4.856000
-964.998919	-16.549942	4.865997
-963.062540	-20.028315	4.875994
-960.894198	-33.482541	4.885990
-959.374686	-24.721433	4.895987
-957.125203	-35.416198	4.905984
-955.474966	-27.099122	4.915981
-953.718684	-28.205694	4.925978
-951.947981	-27.955196	4.935974
-949.843050	-19.432951	4.945971
-947.856000	-23.716726	4.955968
-946.035884	-20.156993	4.965965
-944.169997	-22.487316	4.975962
-942.664527	-10.435228	4.985958
-940.261044	-23.502343	4.995955
-938.399686	-22.499018	5.005952
-936.687225	-14.171344	5.015949
-934.820760	-26.923644	5.025946
-933.082149	-10.574930	5.035942
-931.075116	-21.560888	5.045939
-928.975074	-27.053158	5.055936
-927.568887	-17.980237	5.065933
-925.586842	-21.465883	5.075930
-923.349196	-10.869714	5.085926
-921.902839	-18.652545	5.095923
-920.057308	-20.090711	5.105920
-917.720930	-22.316262	5.115917
-916.224777	-17.620040	5.125914
-914.038801	-28.511445	5.135910
-912.154900	-26.918062	5.145907
-910.488875	-28.201209	5.155904
-908.389097	-18.132419	5.165901
-906.699996	-17.704638	5.175898
-904.836731	-20.055037	5.185894
-902.970965	-12.733885	5.195891
-901.320693	-26.564673	5.205888
-899.295965	-23.331283	5.215885
-897.110332	-16.176528	5.225882
-895.368541	-25.809612	5.235878
-893.725641	-18.558601	5.245875
-891.592225	-17.546637	5.255872
-889.644729	-16.628092	5.265869
-887.929838	-18.290064	5.275866
-886.146443	-18.777282	5.285862
-884.208959	-23.304116	5.295859
-882.313973	-20.743074	5.305856
-880.688744	-20.623987	5.315853
-878.324619	-25.953190	5.325850
-876.620781	-20.396527	5.335846
-875.020579	-23.734243	5.345843
-872.935673	-15.854462	5.355840
-870.939096	-18.085633	5.365837
-869.031830	-24.064890	5.375834
-867.213580	-23.261442	5.385830
-865.543520	-19.991840	5.395827
-863.410551	-20.017074	5.405824
-861.673582	-20.417909	5.415821
-859.726126	-19.955616	5.425818
-857.901757	-29.440835	5.435814
-856.106214	-24.500356	5.445811
-854.109624	-21.462938	5.455808
-852.248358	-19.603799	5.465805
-850.423188	-21.594406	5.475802
-848.720721	-26.809902	5.485798
-846.595872	-20.202710	5.495795
-844.918169	-24.435367	5.505792
-842.921959	-21.775220	5.515789
-840.847674	-25.067137	5.525786
-839.385791	-19.541232	5.535782
-837.357317	-20.468619	5.545779
-835.190121	-17.919479	5.555776
-833.383344	-13.639149	5.565773
-831.493621	-20.251846	5.575770
-829.986686	-21.785800	5.585766
-827.981535	-20.104370	5.595763
-825.906377	-17.022648	5.605760
-823.961976	-24.520334	5.615757
-822.396932	-23.625850	5.625754
-820.387807	-18.016901	5.635750
-818.346430	-24.601729	5.645747
-816.528025	-20.481130	5.655744
-814.785971	-17.837166	5.665741
-812.983020	-17.081752	5.675738
-810.866971	-18.199947	5.685734
-808.928993	-15.614138	5.695731
-807.556432	-12.150101	5.705728
-805.375614	-18.473021	5.715725
-803.440474	-15.122597	5.725722
-801.575468	-22.677044	5.735718
-799.568809	-18.932290	5.745715
-797.941140	-24.551030	5.755712
-796.247018	-16.049797	5.765709
-794.201524	-13.627994	5.775706
-792.377882	-20.575865	5.785702
-790.293584	-17.020342	5.795699
-788.474062	-26.187396	5.805696
-786.549637	-20.861699	5.815693
-784.511185	-24.627807	5.825690
-782.593654	-25.859496	5.835686
-780.919140	-25.192468	5.845683
-779.510658	-14.632543	5.855680
-777.383540	-25.563376	5.865677
-775.409870	-20.098709	5.875674
-772.968709	-24.357044	5.885670
-771.760616	-21.463498	5.895667
-770.201187	-20.847534	5.905664
-767.802674	-27.505195	5.915661
-765.823409	-15.636068	5.925658
-764.085963	-25.708870	5.935654
-762.139017	-16.079680	5.945651
-760.157381	-18.658875	5.955648
-758.323171	-21.332915	5.965645
-756.674170	-18.160911	5.975642
-754.483742	-19.391989	5.985638
-752.810378	-17.636936	5.995635
-751.005545	-17.167545	6.005632
-749.183862	-23.868773	6.015629
-747.129426	-20.400010	6.025626
-745.315169	-18.208029	6.035622
-743.742283	-19.161986	6.045619
-741.604310	-18.755307	6.055616
-739.537275	-12.201919	6.065613
-737.881624	-21.178551	6.075610
-735.797178	-14.037457	6.085606
-733.954049	-27.245338	6.095603
-732.185867	-23.366100	6.105600
-730.472156	-21.211718	6.115597
-728.741182	-19.524272	6.125594
-726.421957	-23.362048	6.135590
-724.451225	-23.231762	6.145587
-722.798565	-20.046108	6.155584
-720.909440	-14.694185	6.165581
-719.067108	-20.257192	6.175578
-717.284203	-27.373748	6.185574
-715.395034	-26.849919	6.195571
-713.562510	-24.763457	6.205568
-711.585065	-25.947827	6.215565
-709.497418	-20.554997	6.225562
-707.620294	-24.819434	6.235558
-705.910112	-22.923399	6.245555
-704.206416	-19.717469	6.255552
-702.173921	-19.775443	6.265549
-700.411586	-16.138385	6.275546
-698.371562	-21.402993	6.285542
-696.355360	-24.739186	6.295539
-694.340588	-25.860038	6.305536
-692.805169	-19.188495	6.315533
-691.451549	-18.103828	6.325530
-689.112190	-12.307548	6.335526
-687.098834	-26.995137	6.345523
-685.194587	-22.968670	6.355520
-683.413320	-20.771368	6.365517
-681.343587	-22.971445	6.375514
-679.449116	-17.445090	6.385510
-677.984466	-19.379534	6.395507
-675.969828	-17.410559	6.405504
-674.044403	-14.663167	6.415501
-672.196304	-24.265734	6.425498
-670.428989	-26.318008	6.435494
-668.261610	-18.474890	6.445491
-666.555517	-20.575795	6.455488
-664.809397	-29.509997	6.465485
-662.989752	-16.576387	6.475482
-660.674124	-19.251500	6.485478
-658.826854	-24.859459	6.495475
-657.340808	-18.513136	6.505472
-655.241103	-23.918289	6.515469
-653.226535	-20.072043	6.525466
-651.354879	-22.125188	6.535462
-649.741403	-20.466273	6.545459
-647.853585	-24.923413	6.555456
-645.804904	-28.575786	6.565453
-643.851508	-21.060007	6.575450
-642.027613	-14.107700	6.585446
-640.350857	-25.015408	6.595443
-638.719616	-20.719503	6.605440
-636.690750	-19.801118	6.615437
-634.593271	-17.649568	6.625434
-632.444067	-22.904728	6.635430
-630.867655	-23.409204	6.645427
-628.992871	-19.919523	6.655424
-627.096369	-16.283319	6.665421
-625.158824	-19.769508	6.675418
-623.474294	-11.552368	6.685414
-621.698457	-14.485385	6.695411
-619.552286	-19.705316	6.705408
-617.664801	-16.864978	6.715405
-615.832347	-17.418249	6.725402
-613.860253	-21.634637	6.735398
-612.255776	-16.623957	6.745395
-610.450968	-15.522917	6.755392
-608.169261	-15.486427	6.765389
-606.617886	-15.506919	6.775386
-604.572474	-19.313464	6.785382
-602.774215	-21.577461	6.795379
-600.667004	-16.200284	6.805376
-598.973634	-19.660071	6.815373
-597.077875	-28.892856	6.825370
-595.045199	-20.508706	6.835366
-593.467677	-21.990637	6.845363
-591.717181	-22.581318	6.855360
-589.532761	-21.392501	6.865357
-587.635394	-35.294166	6.875354
-585.930184	-27.078730	6.885350
-584.232652	-21.871334	6.895347
-582.030849	-18.694368	6.905344
-579.997709	-22.876274	6.915341
-578.410662	-25.054408	6.925338
-576.595185	-27.160094	6.935334
-574.544292	-26.306750	6.945331
-572.586343	-21.576709	6.955328
-570.732147	-24.730612	6.965325
-568.987311	-21.164862	6.975322
-567.023777	-29.660082	6.985318
-565.143532	-25.677045	6.995315
-563.362939	-19.900308	7.005312
-561.517136	-22.367647	7.015309
-559.821955	-16.773038	7.025306
-557.291464	-30.201134	7.035302
-555.768690	-22.646480	7.045299
-554.106551	-25.592859	7.055296
-552.311432	-30.581396	7.065293
-550.106540	-21.460557	7.075290
-548.103412	-20.994269	7.085286
-546.281511	-22.390481	7.095283
-544.736991	-26.786387	7.105280
-542.901516	-19.313252	7.115277
-540.511745	-17.225677	7.125274
-538.904272	-12.900637	7.135270
-536.987734	-20.452080	7.145267
-535.154430	-20.531772	7.155264
-533.574904	-20.255154	7.165261
-531.678746	-20.055956	7.175258
-529.441996	-15.834591	7.185254
-527.402145	-20.349085	7.195251
-525.844414	-26.060687	7.205248
-523.898848	-17.338890	7.215245
-521.887784	-20.929894	7.225242
-520.082546	-18.538939	7.235238
-518.544156	-24.177978	7.245235
-516.574211	-19.184558	7.255232
-514.281318	-18.860837	7.265229
-512.539516	-19.314290	7.275226
-510.786788	-21.600946	7.285222
-508.921215	-25.943910	7.295219
-507.023158	-23.171482	7.305216
-505.361011	-17.824169	7.315213
-503.363682	-12.400927	7.325210
-501.477370	-30.869947	7.335206
-499.463444	-23.576851	7.345203
-497.682575	-21.721950	7.355200
-495.693930	-21.318037	7.365197
-493.869229	-27.045422	7.375194
-492.108677	-17.544094	7.385190
-489.975403	-23.172354	7.395187
-488.107176	-16.389620	7.405184
-486.498461	-25.183350	7.415181
-484.572260	-19.257713	7.425178
-482.652427	-17.102912	7.435174
-480.701782	-23.642984	7.445171
-479.041287	-22.618261	7.455168
-477.274711	-23.156167	7.465165
-475.248522	-21.621466	7.475162
-473.013025	-23.794162	7.485158
-471.265048	-19.284688	7.495155
-469.412732	-29.599848	7.505152
-467.695551	-27.322675	7.515149
-465.865792	-15.625155	7.525146
-463.827859	-20.592419	7.535142
-461.920429	-18.760862	7.545139
-459.814605	-23.661602	7.555136
-458.347871	-21.248112	7.565133
-456.477746	-17.863326	7.575130
-454.429885	-20.506531	7.585126
-452.677853	-24.202940	7.595123
-450.695601	-22.845926	7.605120
-449.065527	-20.437992	7.615117
-447.051146	-26.047226	7.625114
-445.079137	-22.506610	7.635110
-443.040118	-18.823544	7.645107
-441.288817	-22.401416	7.655104
-439.582107	-18.377926	7.665101
-437.740050	-19.804117	7.675098
-435.545009	-13.564550	7.685094
-433.909341	-24.236644	7.695091
-431.980828	-24.284096	7.705088
-430.126935	-9.189563	7.715085
-428.272047	-11.481424	7.725082
-426.317139	-23.226010	7.735078
-424.393471	-21.881721	7.745075
-422.447760	-18.377933	7.755072
-420.968266	-29.751344	7.765069
-419.029714	-12.872021	7.775066
-416.808888	-18.269483	7.785062
-414.797445	-24.782901	7.795059
-413.289512	-15.425888	7.805056
-411.541548	-23.130307	7.815053
-409.527775	-14.676647	7.825050
-407.442100	-34.284216	7.835046
-405.654165	-15.468851	7.845043
-403.630457	-21.928961	7.855040
-401.930237	-19.559036	7.865037
-400.239116	-22.966227	7.875034
-398.419986	-16.968156	7.885030
-396.112259	-22.433156	7.895027
-394.189230	-24.331686	7.905024
-392.549021	-27.615486	7.915021
-391.007321	-26.150180	7.925018
-388.805158	-22.134720	7.935014
-386.828277	-24.614965	7.945011
-385.096429	-23.279485	7.955008
-383.196045	-27.367406	7.965005
-381.338863	-22.306917	7.975002
-379.445217	-28.351526	7.984998
-377.486059	-27.036549	7.994995
-375.632036	-26.863654	8.004992
-373.826398	-24.395286	8.014989
-372.140421	-25.572308	8.024986
-370.121750	-26.050922	8.034982
-368.243236	-12.592790	8.044979
-366.262020	-19.936556	8.054976
-364.173694	-25.347547	8.064973
-362.725391	-21.527460	8.074970
-360.740042	-22.750697	8.084966
-358.917596	-20.926011	8.094963
-357.024373	-23.380244	8.104960
-355.029488	-22.991419	8.114957
-352.930815	-25.423193	8.124954
-351.149885	-25.469120	8.134950
-349.297580	-24.566503	8.144947
-347.485928	-24.521023	8.154944
-346.005851	-20.769152	8.164941
-343.936628	-29.822629	8.174938
-341.764718	-20.407380	8.184934
-340.066523	-22.304706	8.194931
-338.346176	-22.192539	8.204928
-336.064720	-29.108983	8.214925
-334.392347	-19.953421	8.224922
-332.707639	-19.649256	8.234918
-330.592566	-26.769643	8.244915
-328.554228	-15.615268	8.254912
-326.806702	-18.459874	8.264909
-324.987754	-19.182861	8.274906
-323.309443	-18.805041	8.284902
-321.095640	-19.633694	8.294899
-319.671151	-25.567045	8.304896
-317.849105	-19.801464	8.314893
-315.681229	-23.213666	8.324890
-313.564011	-23.355883	8.334886
-311.905149	-20.248283	8.344883
-309.990094	-24.090614	8.354880
-307.909926	-20.660297	8.364877
-306.304146	-17.912089	8.374874
-304.471792	-17.670946	8.384870
-302.489774	-19.839333	8.394867
-300.361637	-14.133654	8.404864
-298.904597	-18.780696	8.414861
-297.011630	-17.057214	8.424858
-294.774624	-13.129324	8.434854
-293.022604	-17.184021	8.444851
-291.341917	-14.870891	8.454848
-289.603377	-21.722729	8.464845
-287.651296	-18.639817	8.474842
-285.895003	-10.634377	8.484838
-283.494775	-22.015774	8.494835
-281.701703	-24.289761	8.504832
-279.944462	-10.240642	8.514829
-278.174305	-19.402639	8.524826
-276.149730	-21.686739	8.534822
-274.410000	-18.997784	8.544819
-272.480056	-15.128216	8.554816
-270.589266	-25.454126	8.564813
-268.589848	-23.771298	8.574810
-266.702653	-15.077839	8.584807
-265.056456	-17.612561	8.594803
-263.675483	-22.886873	8.604800
-261.328444	-15.588310	8.614797
-259.147798	-19.741403	8.624794
-257.413157	-22.482858	8.634791
-255.482476	-25.475064	8.644787
-253.744226	-22.572713	8.654784
-252.084941	-20.162987	8.664781
-249.963615	-21.267322	8.674778
-248.210634	-20.951892	8.684775
-245.965814	-22.672740	8.694771
-244.354786	-14.441988	8.704768
-242.322640	-17.581426	8.714765
-240.589314	-19.212729	8.724762
-238.717315	-18.758404	8.734759
-237.202840	-21.074726	8.744755
-235.063518	-18.414790	8.754752
-233.143267	-18.588651	8.764749
-231.229603	-19.776657	8.774746
-229.254622	-20.614472	8.784743
-227.473963	-18.882481	8.794739
-225.425591	-16.768509	8.804736
-223.563991	-22.301083	8.814733
-221.796447	-23.882575	8.824730
-220.085479	-19.431731	8.834727
-218.106185	-17.961950	8.844723
-215.771760	-24.635708	8.854720
-214.379363	-18.209397	8.864717
-212.552913	-24.216322	8.874714
-210.869814	-21.511965	8.884711
-208.891849	-22.721269	8.894707
-206.877062	-23.246492	8.904704
-204.877945	-24.517586	8.914701
-202.771420	-21.647136	8.924698
-201.333319	-15.559667	8.934695
-199.429994	-22.450378	8.944691
-197.487779	-19.523700	8.954688
-195.526238	-20.071992	8.964685
-193.627077	-14.391242	8.974682
-191.716278	-22.618846	8.984679
-189.882882	-20.262125	8.994675
-187.886548	-19.371318	9.004672
-186.400883	-21.302509	9.014669
-183.880539	-29.074790	9.024666
-182.087745	-31.285506	9.034663
-180.853942	-31.851843	9.044659
-178.879334	-33.412669	9.054656
-176.930895	-32.086342	9.064653
-174.891621	-26.015862	9.074650
-172.912766	-42.462733	9.084647
-171.193359	-27.730172	9.094643
-169.017100	-31.524086	9.104640
-167.324520	-31.282636	9.114637
-165.833568	-24.914654	9.124634
-163.466005	-26.378716	9.134631
-161.792640	-27.591473	9.144627
-159.944912	-31.580828	9.154624
-157.896728	-28.787865	9.164621
-156.593334	-26.455478	9.174618
-154.498640	-29.011178	9.184615
-152.312774	-33.436571	9.194611
-150.403766	-33.120708	9.204608
-148.730403	-27.939120	9.214605
-146.619268	-25.757733	9.224602
-144.830628	-28.255111	9.234599
-142.935056	-24.597832	9.244595
-141.126215	-36.762560	9.254592
-139.620244	-22.008535	9.264589
-137.294146	-23.743833	9.274586
-135.390118	-22.910879	9.284583
-133.856985	-22.208198	9.294579
-131.788510	-28.667346	9.304576
-129.850998	-31.804220	9.314573
-128.174364	-31.174958	9.324570
-126.085444	-23.059852	9.334567
-124.213218	-25.346357	9.344563
-122.297453	-29.730203	9.354560
-120.782721	-23.007585	9.364557
-118.741904	-32.662635	9.374554
-116.704430	-23.702521	9.384551
-114.690890	-37.350858	9.394547
-112.874625	-19.659143	9.404544
-111.184350	-32.000714	9.414541
-109.552716	-21.749068	9.424538
-107.595728	-25.656354	9.434535
-105.221347	-24.791067	9.444531
-103.551288	-24.767017	9.454528
-101.922045	-27.933623	9.464525
-100.172281	-19.702798	9.474522
-98.126536	-21.601733	9.484519
-95.938746	-21.365044	9.494515
-94.030880	-14.378310	9.504512
-92.441560	-21.945113	9.514509
-90.383747	-18.616816	9.524506
-88.588687	-19.845783	9.534503
-86.699310	-21.516087	9.544499
-85.089785	-17.814697	9.554496
-83.072607	-23.957748	9.564493
-80.912579	-20.565230	9.574490
-79.287532	-20.627134	9.584487
-77.186907	-20.455462	9.594483
-75.668780	-21.760227	9.604480
-73.899557	-19.143717	9.614477
-71.570008	-18.182827	9.624474
-69.851582	-17.107062	9.634471
-67.844042	-13.200757	9.644467
-66.216004	-13.863093	9.654464
-64.471785	-13.692963	9.664461
-62.299404	-22.407449	9.674458
-60.292311	-16.418563	9.684455
-58.343646	-21.328634	9.694451
-56.556308	-13.872665	9.704448
-54.846952	-15.946829	9.714445
-53.187419	-11.272925	9.724442
-51.017824	-19.165956	9.734439
-49.079702	-11.577730	9.744435
-47.403383	-17.487964	9.754432
-45.978960	-21.217086	9.764429
-43.580470	-22.011798	9.774426
-41.686689	-20.766633	9.784423
-39.580161	-24.932974	9.794419
-37.988094	-17.232693	9.804416
-36.236554	-15.296976	9.814413
-34.179875	-19.955857	9.824410
-32.354443	-8.296724	9.834407
-30.235908	-13.229141	9.844403
-28.658951	-15.627934	9.854400
-26.514083	-14.918572	9.864397
-24.915846	-13.866229	9.874394
-23.106381	-7.297916	9.884391
-21.038681	-23.428905	9.894387
-19.271744	-24.820693	9.904384
-17.359186	-22.005969	9.914381
-15.691892	-16.081249	9.924378
-13.339759	-24.417026	9.934375
-11.931599	-12.770254	9.944371
-9.481399	-22.165295	9.954368
-8.041865	-19.906643	9.964365
-6.211808	-17.154532	9.974362
-4.803277	-2.266422	9.984359
-3.417806	29.154429	9.994355
-2.353843	88.231463	10.004352
-1.394390	174.208858	10.014349
0.000000	230.660389	10.019354
0.761222	283.619334	10.024359
1.158989	327.728707	10.029363
1.474521	362.688111	10.034368
1.952650	389.343054	10.039373
2.052601	431.901298	10.044378
2.447546	456.978561	10.049383
3.096297	481.583313	10.054387
3.068822	513.516562	10.059392
3.603404	520.908916	10.064397
3.647203	528.292835	10.069402
3.530472	542.074594	10.074407
3.855777	542.603011	10.079411
3.988543	572.257445	10.084416
4.519067	578.442574	10.089421
4.193049	585.369870	10.094426
4.060592	581.256384	10.099431
4.494474	602.568364	10.104435
4.164496	587.273049	10.109440
4.382621	604.171018	10.114445
4.436048	600.649173	10.119450
4.570666	601.729965	10.124455
4.791853	618.898689	10.129459
5.037356	628.677337	10.134464
5.069256	607.461347	10.139469
4.491227	623.180667	10.144474
4.941919	622.706675	10.149479
5.072744	644.261019	10.154483
5.178270	648.926030	10.159488
5.035848	628.005893	10.164493
5.245707	648.841183	10.169498
4.932460	638.869933	10.174503
5.523174	639.761280	10.179507
5.081549	629.189215	10.184512
5.372562	652.230269	10.189517
5.235743	648.588955	10.194522
4.997330	666.351430	10.199527
5.550442	643.226185	10.204531
5.054614	692.692466	10.209536
5.252857	662.409437	10.214541
5.473311	690.507911	10.219546
5.781908	664.819735	10.224551
5.422304	677.225879	10.229555
5.183518	683.281469	10.234560
5.746986	681.280383	10.239565
5.520727	683.079473	10.244570
5.665058	690.307093	10.249575
5.551472	682.141063	10.254579
5.434780	695.861462	10.259584
6.157127	718.195165	10.264589
6.218827	714.411783	10.269594
6.016019	717.490744	10.274599
6.105519	729.259179	10.279603
5.996797	711.269760	10.284608
6.144618	731.616762	10.289613
6.496116	731.735742	10.294618
6.124329	724.558602	10.299623
6.746644	724.208614	10.304627
6.345907	716.717560	10.309632
6.512577	725.685700	10.314637
6.517054	739.883539	10.319642
5.996382	694.458474	10.324647
6.431970	732.829404	10.329651
6.138588	730.796266	10.334656
6.422226	734.336937	10.339661
6.196961	739.535705	10.344666
6.380512	758.513013	10.349671
6.624508	733.765402	10.354675
6.561941	748.921672	10.359680
6.309763	756.857535	10.364685
6.474025	767.019812	10.369690
6.719708	777.757298	10.374695
6.897358	778.679855	10.379699
6.626002	778.857193	10.384704
6.707729	776.634904	10.389709
6.612504	789.733814	10.394714
7.162319	787.567739	10.399719
7.226398	778.952276	10.404723
7.136718	792.239535	10.409728
7.116820	793.057990	10.414733
7.175073	805.541086	10.419738
7.269544	815.914800	10.424743
7.611242	828.434701	10.429747
7.397519	832.095735	10.434752
7.611438	824.697383	10.439757
7.351339	839.722834	10.444762
7.277554	841.196428	10.449767
7.628990	830.371552	10.454771
7.738051	818.640770	10.459776
8.015926	843.190186	10.464781
7.920245	837.344026	10.469786
7.905597	831.434480	10.474791
8.330480	827.132671	10.479795
7.512484	823.549512	10.484800
7.930013	825.480885	10.489805
8.015239	830.229616	10.494810
7.799207	839.842338	10.499815
8.099859	847.062447	10.504819
7.863495	832.259710	10.509824
8.078090	842.245279	10.514829
7.876914	847.755628	10.519834
7.808893	852.768506	10.524839
7.946284	838.607873	10.529843
7.861365	849.588959	10.534848
8.031866	845.392378	10.539853
8.092694	851.521666	10.544858
8.328763	870.694167	10.549863
8.298939	862.008480	10.554867
8.125379	884.579971	10.559872
8.472908	878.450208	10.564877
8.462131	872.811260	10.569882
8.348157	871.364486	10.574887
8.636184	868.264040	10.579891
8.450660	890.553602	10.584896
8.420431	867.756019	10.589901
8.703546	890.503826	10.594906
9.131148	902.948588	10.599911
8.614508	907.845393	10.604915
8.405139	917.177986	10.609920
8.579799	909.136156	10.614925
8.570781	920.466306	10.619930
8.794547	926.375671	10.624935
9.193562	918.323278	10.629939
8.974377	921.666665	10.634944
9.055820	919.876480	10.639949
9.355565	934.610875	10.644954
9.433167	936.186485	10.649959
9.511698	932.673171	10.654963
9.340011	932.769956	10.659968
9.764224	923.355799	10.664973
9.393890	927.459727	10.669978
9.540635	928.581186	10.674983
9.605046	929.282123	10.679987
9.547480	934.405323	10.684992
9.554923	945.337055	10.689997
9.594563	945.527862	10.695002
9.652947	961.496105	10.700007
9.611223	972.068273	10.705011
9.537779	958.297546	10.710016
9.917319	966.257330	10.715021
9.920916	965.837303	10.720026
9.701060	965.285765	10.725031
10.268222	963.854906	10.730035
9.883340	969.137564	10.735040
9.812731	969.478420	10.740045
9.880716	967.218871	10.745050
10.369831	958.871389	10.750055
10.458156	962.608851	10.755059
9.735994	970.876843	10.760064
10.236652	968.355888	10.765069
10.131152	983.519250	10.770074
10.208317	991.894711	10.775079
10.447563	1000.124474	10.780083
10.318588	1007.906781	10.785088
10.390163	1011.251114	10.790093
10.477715	1002.661736	10.795098
10.352049	1007.884135	10.800103
10.736418	993.803802	10.805107
10.551620	1012.535851	10.810112
10.805206	1010.084264	10.815117
10.730623	1017.673396	10.820122
10.622583	1014.596676	10.825127
10.947625	1013.095626	10.830131
10.603513	1021.642383	10.835136
10.655370	1016.822862	10.840141
10.830543	1021.506846	10.845146
10.772642	1038.179695	10.850151
11.057593	1038.520605	10.855155
11.130878	1038.048459	10.860160
11.364146	1040.613226	10.865165
11.366214	1041.281534	10.870170
10.933285	1048.181949	10.875175
11.401205	1046.183442	10.880179
11.433473	1042.819407	10.885184
11.282890	1030.570055	10.890189
11.196921	1040.684132	10.895194
11.451174	1042.132226	10.900199
11.223866	1043.051589	10.905203
11.265022	1044.626716	10.910208
11.657747	1046.117377	10.915213
11.613577	1045.667121	10.920218
11.784603	1051.726875	10.925223
11.819991	1047.316824	10.930227
11.680701	1054.772795	10.935232
11.603442	1061.506094	10.940237
11.772679	1067.823184	10.945242
11.938411	1068.405463	10.950247
12.118020	1074.962175	10.955251
11.750778	1094.005707	10.960256
11.935392	1086.842132	10.965261
12.180084	1092.961116	10.970266
11.830167	1091.891001	10.975271
12.185633	1070.069210	10.980275
12.232401	1087.685783	10.985280
12.297239	1084.061076	10.990285
12.603920	1088.296750	10.995290
12.214101	1092.459025	11.000295
12.381073	1091.164532	11.005299
11.802534	1091.652647	11.010304
12.014775	1079.446303	11.015309
12.408041	1104.662153	11.020314
12.121262	1129.418822	11.025319
12.724807	1126.873543	11.030323
12.626086	1128.083061	11.035328
12.950610	1120.012478	11.040333
12.668805	1123.730177	11.045338
12.493292	1128.389711	11.050343
12.846765	1129.225897	11.055347
12.875076	1131.856490	11.060352
12.918682	1128.495358	11.065357
13.077697	1124.530764	11.070362
12.789287	1122.302811	11.075367
13.008170	1125.805024	11.080371
12.661019	1136.493841	11.085376
12.945454	1136.394865	11.090381
13.246721	1126.747876	11.095386
12.591029	1159.452965	11.100391
13.305494	1152.069220	11.105395
13.619761	1170.586245	11.110400
13.480809	1168.935266	11.115405
13.604733	1165.372077	11.120410
13.548118	1169.050711	11.125415
13.748801	1163.314840	11.130419
13.697968	1171.732901	11.135424
13.694788	1164.398970	11.140429
13.637107	1141.468139	11.145434
13.634289	1154.448559	11.150439
13.770839	1151.391141	11.155443
13.745855	1168.503591	11.160448
13.871368	1173.577171	11.165453
13.501878	1166.566602	11.170458
13.733370	1163.238568	11.175463
13.937887	1171.328889	11.180467
13.685719	1178.000255	11.185472
13.811577	1176.415844	11.190477
14.016231	1179.390480	11.195482
13.873194	1185.155034	11.200487
13.936216	1165.874507	11.205491
13.941758	1173.551865	11.210496
14.193413	1186.308793	11.215501
14.504394	1195.082316	11.220506
14.483413	1197.539433	11.225511
14.278001	1181.226976	11.230515
14.316423	1190.629027	11.235520
14.484561	1199.843235	11.240525
14.569016	1195.950441	11.245530
13.955699	1212.300500	11.250535
14.526497	1202.935321	11.255539
14.700403	1213.228839	11.260544
14.768434	1209.676132	11.265549
14.658650	1209.236336	11.270554
14.615314	1219.793172	11.275559
14.700880	1208.080017	11.280563
14.143886	1217.633835	11.285568
14.937456	1204.536708	11.290573
14.551359	1222.682968	11.295578
14.641468	1229.858007	11.300583
15.104132	1226.026301	11.305587
14.868721	1230.622882	11.310592
15.025789	1240.657328	11.315597
15.167712	1250.322032	11.320602
15.085648	1237.334591	11.325607
15.174364	1240.485431	11.330611
15.082208	1255.060315	11.335616
15.060321	1240.483147	11.340621
15.031086	1240.719638	11.345626
14.994568	1269.172466	11.350631
15.551267	1263.994785	11.355635
15.563715	1277.162116	11.360640
15.435886	1268.472895	11.365645
15.651818	1291.180009	11.370650
15.950628	1261.947300	11.375655
15.906508	1287.192238	11.380659
15.762468	1272.383784	11.385664
16.064556	1273.775386	11.390669
16.362053	1289.486649	11.395674
15.781191	1252.968305	11.400679
15.786200	1258.999436	11.405683
15.708403	1260.409056	11.410688
15.768702	1253.845555	11.415693
16.265631	1286.463263	11.420698
16.091048	1276.206097	11.425703
15.994608	1267.819379	11.430707
15.872191	1290.200413	11.435712
15.995947	1283.213609	11.440717
16.008611	1266.599760	11.445722
15.566043	1301.581436	11.450727
15.999537	1290.408812	11.455731
16.166908	1310.606850	11.460736
16.404887	1303.592354	11.465741
16.683802	1310.642696	11.470746
16.661120	1326.722046	11.475751
16.894553	1319.233597	11.480755
16.838984	1306.599842	11.485760
16.676546	1333.164739	11.490765
17.013243	1296.848432	11.495770
16.593111	1321.147298	11.500775
17.078405	1278.128830	11.505779
16.610249	1324.875722	11.510784
16.632643	1305.792304	11.515789
16.669098	1315.721461	11.520794
16.620235	1337.106800	11.525799
17.002296	1311.825240	11.530803
17.024967	1318.094856	11.535808
16.935456	1323.751577	11.540813
17.134426	1315.710376	11.545818
16.885192	1325.290867	11.550823
17.232104	1310.314172	11.555827
17.109420	1308.553347	11.560832
17.078773	1329.338095	11.565837
17.305368	1328.529242	11.570842
17.301637	1333.076283	11.575847
17.519457	1359.063321	11.580851
17.521469	1350.000095	11.585856
17.339788	1339.450698	11.590861
17.576636	1362.380096	11.595866
17.574531	1346.053946	11.600871
17.903685	1349.395118	11.605875
17.499547	1362.955414	11.610880
17.679649	1356.505223	11.615885
18.000090	1350.958337	11.620890
17.734440	1357.180919	11.625895
17.605747	1358.388928	11.630899
17.709165	1351.537802	11.635904
17.693574	1354.418294	11.640909
17.885556	1358.194519	11.645914
18.054697	1357.306519	11.650919
17.985743	1350.224264	11.655923
18.042765	1363.354601	11.660928
18.234074	1376.741077	11.665933
18.359111	1383.770269	11.670938
18.169328	1381.811976	11.675943
18.181691	1380.382845	11.680947
18.207764	1396.224254	11.685952
18.031861	1403.918062	11.690957
18.238223	1400.633408	11.695962
17.967520	1391.194180	11.700967
18.420218	1384.072853	11.705971
18.267911	1383.012195	11.710976
18.234225	1425.582059	11.715981
18.604207	1401.428242	11.720986
18.420156	1423.920241	11.725991
18.587433	1412.357894	11.730995
18.805647	1435.298264	11.736000
18.795295	1415.513434	11.741005
19.035602	1428.297617	11.746010
18.788948	1440.099751	11.751015
19.071295	1433.366705	11.756019
19.236090	1418.202902	11.761024
19.032980	1437.662259	11.766029
19.213499	1419.537511	11.771034
19.009013	1428.809726	11.776039
19.118875	1439.197201	11.781043
19.146045	1426.376675	11.786048
18.940972	1415.676408	11.791053
19.285837	1425.900228	11.796058
19.458298	1428.574115	11.801063
19.219094	1425.404686	11.806067
19.315208	1443.122632	11.811072
19.488062	1459.929471	11.816077
19.652940	1456.913204	11.821082
19.480824	1474.820635	11.826087
20.103678	1470.072312	11.831091
20.045360	1459.145171	11.836096
19.903896	1452.700499	11.841101
19.893563	1436.567953	11.846106
19.713056	1440.189146	11.851111
19.604613	1430.347108	11.856115
19.645443	1459.420344	11.861120
19.964945	1444.258645	11.866125
20.149701	1457.761363	11.871130
19.945046	1463.605243	11.876135
20.126352	1462.697949	11.881139
19.835618	1460.285805	11.886144
19.844387	1459.391840	11.891149
19.919731	1461.945604	11.896154
19.795233	1469.065104	11.901159
20.071642	1457.833829	11.906163
19.963691	1463.200225	11.911168
20.165199	1479.546765	11.916173
20.131829	1492.183844	11.921178
20.240072	1484.161754	11.926183
20.396160	1478.510146	11.931187
20.285215	1497.003952	11.936192
20.208100	1482.649822	11.941197
20.519576	1483.331876	11.946202
20.463950	1500.235134	11.951207
20.747634	1519.709204	11.956211
20.921503	1521.482417	11.961216
21.401614	1505.977269	11.966221
21.222525	1498.854160	11.971226
20.750445	1487.705985	11.976231
21.113973	1470.887697	11.981235
21.098878	1488.970377	11.986240
20.765558	1483.579766	11.991245
20.906737	1490.701055	11.996250
20.879112	1522.859694	12.001255
21.536571	1512.326920	12.006259
21.286144	1523.701568	12.011264
21.404748	1512.254930	12.016269
21.244386	1503.758419	12.021274
21.057746	1524.031360	12.026279
21.495400	1515.174516	12.031283
21.336312	1512.111351	12.036288
21.421781	1523.869248	12.041293
21.692556	1512.587577	12.046298
21.240844	1492.668033	12.051303
21.536656	1490.086625	12.056307
20.869442	1489.869784	12.061312
21.167991	1495.414206	12.066317
21.771176	1489.798512	12.071322
21.236008	1498.144204	12.076327
21.372695	1491.208856	12.081331
21.441143	1489.483755	12.086336
21.348124	1493.087851	12.091341
21.279825	1497.284110	12.096346
21.181712	1488.970073	12.101351
21.438695	1486.312855	12.106355
21.277999	1496.730913	12.111360
21.163935	1491.721652	12.116365
21.390953	1497.648081	12.121370
20.996766	1492.432760	12.126375
21.587266	1491.308801	12.131379
21.435356	1490.869408	12.136384
21.258249	1490.561772	12.141389
21.258523	1498.858325	12.146394
21.153559	1499.698274	12.151399
21.176706	1497.884201	12.156403
21.109779	1509.818576	12.161408
21.167312	1523.403940	12.166413
21.567932	1522.795983	12.171418
21.586682	1521.507749	12.176423
21.316783	1508.385232	12.181427
21.405244	1503.337353	12.186432
21.048409	1506.573515	12.191437
21.419354	1483.427111	12.196442
21.019616	1502.577288	12.201447
21.371440	1504.721093	12.206451
21.266185	1506.001071	12.211456
21.136639	1529.358985	12.216461
21.674987	1518.890150	12.221466
21.518924	1516.152153	12.226471
21.611053	1499.411029	12.231475
21.442019	1496.689298	12.236480
21.271925	1501.710796	12.241485
21.413399	1499.794267	12.246490
21.676620	1502.414265	12.251495
21.772497	1503.312066	12.256499
21.863218	1499.749362	12.261504
21.389090	1502.745605	12.266509
21.707005	1491.222246	12.271514
21.661712	1505.969685	12.276519
21.399440	1486.199710	12.281523
21.250582	1483.591461	12.286528
21.381386	1476.977188	12.291533
21.464373	1472.860621	12.296538
21.351965	1476.387379	12.301543
21.330716	1471.885305	12.306547
21.562220	1478.378728	12.311552
21.355413	1482.571845	12.316557
21.263336	1472.476426	12.321562
21.297149	1480.274019	12.326567
21.471899	1483.166754	12.331571
21.313667	1477.579478	12.336576
21.398652	1486.389228	12.341581
21.452123	1485.265775	12.346586
21.369556	1488.988055	12.351591
21.511354	1476.762651	12.356595
21.280607	1482.864598	12.361600
21.251428	1490.377346	12.366605
21.695304	1486.821391	12.371610
21.476268	1483.770161	12.376615
21.332543	1495.475494	12.381619
21.677146	1492.605597	12.386624
21.505884	1484.669094	12.391629
21.504717	1493.921535	12.396634
21.343678	1465.586539	12.401639
21.116053	1458.368688	12.406643
21.182550	1468.190653	12.411648
21.141720	1485.993575	12.416653
21.156913	1498.684416	12.421658
21.080951	1492.399594	12.426663
21.267153	1495.123343	12.431667
21.267515	1492.240546	12.436672
21.205203	1497.183347	12.441677
21.493137	1485.675814	12.446682
21.575262	1481.636655	12.451687
21.561828	1482.476195	12.456691
21.415382	1493.393463	12.461696
21.177029	1475.430081	12.466701
21.520725	1476.387700	12.471706
21.103019	1471.217141	12.476711
21.127788	1482.900319	12.481715
21.254332	1493.786657	12.486720
21.364559	1491.349973	12.491725
21.307692	1488.042631	12.496730
21.290570	1495.696966	12.501735
21.492272	1495.798850	12.506739
21.570898	1481.107633	12.511744
21.457904	1481.840049	12.516749
21.538077	1468.487468	12.521754
21.114712	1458.389708	12.526759
21.001505	1454.537837	12.531763
21.419376	1469.517294	12.536768
21.425689	1469.891624	12.541773
21.478702	1457.189954	12.546778
21.320880	1459.571170	12.551783
21.454938	1462.755828	12.556787
21.416794	1450.715271	12.561792
20.871559	1464.500023	12.566797
21.248225	1457.229936	12.571802
21.375684	1448.321684	12.576807
21.001839	1455.239673	12.581811
21.065150	1471.116226	12.586816
21.498693	1484.442085	12.591821
21.545771	1486.869471	12.596826
21.286067	1479.163127	12.601831
21.036283	1494.473044	12.606835
21.528543	1486.334502	12.611840
21.507325	1489.149684	12.616845
21.450937	1463.024720	12.621850
21.300575	1470.058459	12.626855
21.375473	1461.015077	12.631859
21.300938	1458.704067	12.636864
21.185752	1463.986459	12.641869
21.396812	1462.181841	12.646874
21.104159	1466.353953	12.651879
21.365684	1461.723195	12.656883
21.503904	1467.192254	12.661888
21.175161	1468.364372	12.666893
21.187413	1463.421707	12.671898
21.386126	1469.280097	12.676903
21.424365	1460.553231	12.681907
21.213915	1464.128742	12.686912
20.964198	1475.656996	12.691917
21.724925	1470.658016	12.696922
21.190131	1478.437496	12.701927
21.561384	1465.869563	12.706931
21.450838	1464.120976	12.711936
21.268016	1470.019725	12.716941
21.299858	1473.439892	12.721946
21.092468	1473.607031	12.726951
21.146627	1470.214173	12.731955
20.993256	1475.671399	12.736960
21.027670	1498.511875	12.741965
21.606167	1499.619705	12.746970
21.219988	1508.044143	12.751975
21.355904	1509.638899	12.756979
21.443047	1505.360806	12.761984
21.369889	1512.010078	12.766989
21.687529	1504.583798	12.771994
21.449434	1492.365361	12.776999
21.387051	1480.232450	12.782003
21.561076	1479.315277	12.787008
21.324014	1474.122210	12.792013
21.345711	1469.595940	12.797018
21.362997	1481.570476	12.802023
21.514709	1470.278655	12.807027
21.719884	1473.710598	12.812032
21.616019	1469.202780	12.817037
21.544089	1473.989408	12.822042
21.345069	1478.655957	12.827047
21.461907	1468.658106	12.832051
21.505025	1475.858109	12.837056
21.245344	1481.617731	12.842061
21.509203	1477.133257	12.847066
21.367394	1479.798936	12.852071
21.337651	1473.438938	12.857075
21.424554	1452.342253	12.862080
21.115727	1452.793661	12.867085
21.624520	1460.105460	12.872090
21.205433	1459.480022	12.877095
21.568366	1441.110102	12.882099
21.355777	1445.472869	12.887104
21.059595	1446.401665	12.892109
21.743427	1441.320341	12.897114
21.522528	1458.271992	12.902119
21.185610	1442.376042	12.907123
21.306508	1440.954824	12.912128
21.166260	1454.755392	12.917133
20.925252	1449.405264	12.922138
20.879561	1450.027592	12.927143
20.975004	1476.127404	12.932147
21.374666	1476.970438	12.937152
21.262418	1485.163504	12.942157
21.037714	1485.792311	12.947162
21.202097	1481.074538	12.952167
21.378742	1486.004450	12.957171
21.398472	1484.459013	12.962176
21.320378	1488.767222	12.967181
21.535775	1481.619044	12.972186
21.387700	1477.824770	12.977191
21.560350	1485.127121	12.982195
21.652511	1483.063914	12.987200
21.088519	1473.720302	12.992205
21.272210	1472.883592	12.997210
21.342230	1477.368449	13.002215
21.496301	1482.137954	13.007219
21.285231	1465.789807	13.012224
21.114114	1464.998655	13.017229
21.373546	1477.038644	13.022234
21.463371	1489.561450	13.027239
21.470312	1471.801802	13.032243
21.708345	1472.083975	13.037248
21.267798	1458.565300	13.042253
21.313681	1450.529521	13.047258
21.136717	1457.370372	13.052263
21.204467	1461.611153	13.057267
21.047408	1456.701806	13.062272
21.160846	1481.308498	13.067277
21.243206	1476.914478	13.072282
21.254302	1489.676930	13.077287
21.365452	1495.661265	13.082291
21.717959	1495.543545	13.087296
21.239770	1476.467211	13.092301
21.320124	1457.929449	13.097306
21.221563	1458.886649	13.102311
21.290752	1467.083880	13.107315
21.429792	1472.537041	13.112320
21.447892	1469.779156	13.117325
21.565400	1457.538719	13.122330
21.135671	1461.994476	13.127335
21.470633	1461.458497	13.132339
21.619481	1464.323820	13.137344
21.426114	1470.244753	13.142349
21.418688	1468.117007	13.147354
21.392641	1459.838800	13.152359
21.174143	1478.064302	13.157363
21.335196	1468.573499	13.162368
21.301136	1471.209372	13.167373
21.362881	1464.913635	13.172378
21.116477	1468.964826	13.177383
21.583061	1465.365829	13.182387
21.711329	1457.687499	13.187392
21.330431	1471.608473	13.192397
21.400966	1470.403450	13.197402
21.589346	1464.917011	13.202407
21.760546	1465.826450	13.207411
21.592045	1469.660206	13.212416
21.371232	1457.029024	13.217421
21.606653	1441.633152	13.222426
21.393155	1441.235124	13.227431
21.211709	1437.684309	13.232435
21.191116	1426.052568	13.237440
20.925274	1439.920466	13.242445
21.482452	1437.738934	13.247450
21.401712	1452.192343	13.252455
21.199288	1444.836435	13.257459
21.469409	1438.226766	13.262464
21.330592	1442.494183	13.267469
21.168959	1428.560452	13.272474
21.037868	1444.441178	13.277479
21.306448	1462.257796	13.282483
21.830630	1446.252870	13.287488
21.346718	1446.893060	13.292493
20.945171	1438.102315	13.297498
21.125465	1453.458705	13.302503
21.660751	1452.537526	13.307507
21.533701	1451.248901	13.312512
21.125631	1451.115305	13.317517
21.570269	1434.131153	13.322522
21.034210	1445.055338	13.327527
21.290602	1437.156303	13.332531
21.465672	1432.200292	13.337536
21.184714	1448.108081	13.342541
21.437276	1432.512360	13.347546
21.310993	1438.652820	13.352551
20.967510	1437.614768	13.357555
21.310286	1449.783369	13.362560
21.328135	1460.906223	13.367565
21.495697	1445.235735	13.372570
21.446450	1438.973483	13.377575
21.121276	1440.875177	13.382579
21.546769	1430.807616	13.387584
21.285212	1436.953883	13.392589
21.420084	1440.132098	13.397594
21.155047	1449.098587	13.402599
21.227236	1446.614360	13.407603
21.460829	1445.031659	13.412608
21.159111	1455.576264	13.417613
21.423663	1435.313882	13.422618
21.235497	1438.262920	13.427623
21.387388	1443.881181	13.432627
21.274907	1445.064533	13.437632
21.220496	1445.399663	13.442637
21.372419	1432.560808	13.447642
21.409466	1431.775878	13.452647
21.477191	1437.282979	13.457651
21.112943	1449.296271	13.462656
21.555298	1443.135378	13.467661
21.545718	1434.452426	13.472666
21.489350	1447.570963	13.477671
21.217461	1446.054700	13.482675
21.661170	1442.751102	13.487680
21.578169	1445.904146	13.492685
21.416559	1449.117039	13.497690
21.317454	1445.988337	13.502695
21.423550	1451.038304	13.507699
21.648421	1434.445607	13.512704
21.379267	1448.421277	13.517709
21.607908	1454.342698	13.522714
21.607609	1450.007604	13.527719
21.288185	1441.968598	13.532723
21.051224	1432.941863	13.537728
21.313708	1441.584498	13.542733
21.618882	1438.318768	13.547738
21.338152	1435.471359	13.552743
21.110683	1429.243848	13.557747
21.157679	1425.658173	13.562752
21.232304	1444.027691	13.567757
21.506867	1439.279740	13.572762
21.474582	1455.180987	13.577767
21.296420	1433.153607	13.582771
21.459531	1426.682441	13.587776
21.262006	1426.628804	13.592781
21.346032	1414.800607	13.597786
21.257964	1425.631239	13.602791
21.513970	1435.500225	13.607795
21.792316	1425.019313	13.612800
21.340136	1427.900075	13.617805
21.260511	1422.256125	13.622810
21.432545	1416.989937	13.627815
21.446746	1421.366984	13.632819
21.320325	1412.989695	13.637824
21.109794	1421.598958	13.642829
21.213723	1420.114215	13.647834
21.231418	1422.879022	13.652839
21.070530	1423.770466	13.657843
21.471692	1417.431646	13.662848
21.017868	1431.394178	13.667853
21.108997	1428.440144	13.672858
21.328130	1426.676821	13.677863
21.069835	1425.428057	13.682867
21.335026	1426.287807	13.687872
21.144854	1451.912728	13.692877
21.207982	1453.339312	13.697882
21.095191	1458.674938	13.702887
21.311095	1472.847655	13.707891
21.477062	1465.731025	13.712896
21.052166	1457.953268	13.717901
21.042818	1451.373979	13.722906
21.213815	1462.407748	13.727911
21.049099	1460.508526	13.732915
21.554223	1464.786776	13.737920
21.320288	1464.674290	13.742925
21.034445	1462.210901	13.747930
21.111380	1464.808567	13.752935
21.389649	1456.898146	13.757939
21.440013	1446.981878	13.762944
21.095017	1466.645260	13.767949
21.225757	1461.355680	13.772954
21.207126	1459.023136	13.777959
21.286310	1459.441038	13.782963
21.496642	1452.602773	13.787968
21.314430	1462.484907	13.792973
21.039151	1458.742468	13.797978
20.769276	1455.404455	13.802983
21.199064	1464.599173	13.807987
21.028924	1469.691632	13.812992
21.431605	1474.550791	13.817997
21.564393	1474.750401	13.823002
21.211437	1463.517009	13.828007
21.262677	1468.228793	13.833011
21.421079	1467.664206	13.838016
21.209063	1467.477259	13.843021
21.338332	1459.507023	13.848026
21.609482	1473.431225	13.853031
21.379872	1461.854875	13.858035
21.737747	1458.512923	13.863040
21.431194	1465.336602	13.868045
21.428578	1455.920801	13.873050
21.215978	1457.845542	13.878055
21.140936	1467.347875	13.883059
21.569827	1465.633092	13.888064
21.375474	1474.272922	13.893069
21.553094	1469.136715	13.898074
21.449197	1467.131593	13.903079
21.118962	1468.109979	13.908083
21.802540	1462.186573	13.913088
21.413498	1463.901333	13.918093
21.382533	1461.848308	13.923098
21.584970	1465.745899	13.928103
21.651326	1468.417795	13.933107
21.632799	1448.746189	13.938112
21.287313	1444.604934	13.943117
21.356912	1434.999427	13.948122
21.468690	1436.350439	13.953127
21.173254	1444.739864	13.958131
21.619341	1430.467911	13.963136
21.201297	1441.764363	13.968141
21.289927	1434.005633	13.973146
21.618089	1443.773226	13.978151
21.087887	1447.051222	13.983155
21.280336	1435.399684	13.988160
20.993095	1447.326572	13.993165
21.325843	1434.190783	13.998170
21.117138	1441.260623	14.003175
20.670957	1446.099055	14.008179
21.459744	1451.353944	14.013184
21.184323	1463.780444	14.018189
21.570044	1473.894243	14.023207
21.405308	1467.770213	14.028224
21.401634	1471.009561	14.033242
21.813458	1462.898132	14.038259
21.515259	1458.231517	14.043277
21.626598	1443.898170	14.048295
21.337338	1442.825943	14.053312
21.270665	1453.380206	14.058330
21.144733	1447.221681	14.063347
21.303220	1444.693819	14.068365
21.717967	1457.859497	14.073383
21.456143	1453.165060	14.078400
21.516577	1455.978915	14.083418
21.411807	1444.687559	14.088435
21.363819	1457.533808	14.093453
21.633015	1456.196325	14.098471
21.678841	1466.454238	14.103488
21.496793	1481.664047	14.108506
22.001381	1466.432700	14.113523
22.032091	1468.988612	14.118541
21.637043	1451.923559	14.123559
21.580743	1450.433512	14.128576
21.308357	1450.725503	14.133594
21.689181	1451.635292	14.138611
21.530365	1475.712943	14.143629
21.493518	1479.025222	14.148647
21.823549	1468.756134	14.153664
21.528263	1481.709489	14.158682
21.969544	1486.501173	14.163699
21.791061	1476.722168	14.168717
21.632429	1474.815874	14.173735
21.749813	1481.927449	14.178752
21.774310	1481.656149	14.183770
21.834457	1472.663319	14.188787
21.736284	1486.875074	14.193805
21.857904	1476.551139	14.198823
21.870536	1468.550572	14.203840
21.665031	1480.128984	14.208858
21.863871	1472.770372	14.213875
21.586179	1488.446888	14.218893
21.791563	1504.225683	14.223911
21.886171	1512.794335	14.228928
21.834833	1514.803363	14.233946
22.354069	1523.898874	14.238963
22.104871	1519.658565	14.243981
22.006976	1524.880750	14.248999
22.304643	1512.235305	14.254016
22.119818	1520.633038	14.259034
22.275837	1519.398544	14.264051
22.242807	1518.150163	14.269069
22.102149	1520.837236	14.274087
22.252982	1523.786117	14.279104
21.933021	1515.366684	14.284122
21.975045	1514.246326	14.289139
22.010909	1522.459424	14.294157
22.020298	1523.044660	14.299175
22.493859	1522.999020	14.304192
22.154783	1531.298672	14.309210
22.339281	1517.516708	14.314227
22.398572	1517.165928	14.319245
22.317505	1521.374002	14.324263
22.193673	1521.824764	14.329280
21.940880	1525.481376	14.334298
22.565532	1537.666712	14.339315
22.390484	1550.837682	14.344333
22.295913	1546.125187	14.349351
23.013916	1545.409791	14.354368
22.501183	1547.511298	14.359386
22.619718	1547.983173	14.364403
22.697119	1549.572920	14.369421
22.343998	1535.083129	14.374439
22.341282	1531.973795	14.379456
22.529377	1544.570110	14.384474
22.589740	1548.717095	14.389491
22.606871	1553.485226	14.394509
22.451911	1554.581157	14.399527
22.855798	1554.828195	14.404544
22.529060	1550.553056	14.409562
22.459882	1546.539632	14.414579
22.504004	1549.586549	14.419597
22.726410	1551.817750	14.424615
22.896230	1548.035183	14.429632
22.597535	1551.460817	14.434650
22.321034	1548.191452	14.439667
22.757683	1545.315617	14.444685
22.638218	1550.167668	14.449703
23.057955	1553.331630	14.454720
22.984355	1570.707531	14.459738
22.830578	1565.113379	14.464755
22.647233	1570.044052	14.469773
22.884580	1579.019399	14.474791
22.934860	1588.649066	14.479808
22.987767	1589.401964	14.484826
22.858237	1581.346936	14.489843
23.157515	1574.832674	14.494861
22.955720	1594.251909	14.499879
23.521171	1584.745837	14.504896
23.431507	1587.287939	14.509914
23.243548	1590.638504	14.514931
23.405615	1579.018197	14.519949
23.293875	1562.370280	14.524967
23.381209	1545.238395	14.529984
22.737164	1562.671460	14.535002
23.171900	1568.816980	14.540019
23.131940	1567.052189	14.545037
23.163522	1578.081641	14.550055
23.475693	1583.861337	14.555072
23.298905	1592.322321	14.560090
23.640532	1580.402817	14.565107
23.399706	1558.578357	14.570125
23.211195	1563.989610	14.575143
23.286822	1568.268656	14.580160
23.525501	1576.449433	14.585178
23.597750	1555.241983	14.590195
23.749152	1553.660594	14.595213
23.439570	1550.320215	14.600231
23.696585	1540.513383	14.605248
23.404209	1557.621368	14.610266
23.448104	1545.097383	14.615283
23.658325	1548.655764	14.620301
23.261428	1540.505771	14.625319
23.216358	1559.947936	14.630336
23.416237	1552.244636	14.635354
23.318428	1569.575635	14.640371
23.482297	1583.380753	14.645389
23.377836	1574.066489	14.650407
23.784982	1582.844871	14.655424
23.818114	1596.422324	14.660442
23.583153	1564.485771	14.665459
23.939904	1589.637513	14.670477
23.988364	1575.093848	14.675495
23.749346	1575.012441	14.680512
23.703354	1595.850824	14.685530
23.691064	1572.972166	14.690547
24.007747	1570.694320	14.695565
23.574598	1581.967787	14.700583
23.951017	1561.405495	14.705600
23.829874	1583.487493	14.710618
23.497050	1579.861386	14.715635
23.731316	1577.591966	14.720653
23.723072	1579.186726	14.725671
23.670887	1569.011569	14.730688
23.806605	1577.727855	14.735706
23.767108	1582.605699	14.740723
24.041249	1587.249477	14.745741
24.138808	1591.350429	14.750759
24.290000	1597.432655	14.755776
24.432949	1602.537800	14.760794
24.369697	1591.993168	14.765811
24.214067	1574.515409	14.770829
24.073028	1577.775119	14.775847
24.017002	1590.558275	14.780864
24.001289	1564.296686	14.785882
23.914770	1589.004769	14.790899
24.377177	1593.627956	14.795917
24.255071	1608.598680	14.800935
24.352165	1597.490505	14.805952
24.516306	1612.108840	14.810970
24.231683	1585.638429	14.815987
24.362420	1599.455140	14.821005
24.595725	1601.091594	14.826023
24.564396	1583.800058	14.831040
24.300396	1578.722119	14.836058
24.353050	1589.652266	14.841075
24.332054	1570.171076	14.846093
24.204882	1596.490099	14.851111
24.523779	1614.118041	14.856128
24.347556	1591.116070	14.861146
24.288800	1608.035055	14.866163
24.379987	1615.669960	14.871181
24.268831	1584.669990	14.876199
24.273831	1611.493334	14.881216
24.503131	1608.180238	14.886234
24.475743	1598.383341	14.891251
24.668266	1598.156021	14.896269
24.485449	1614.523809	14.901287
24.826082	1593.098892	14.906304
24.918753	1596.038189	14.911322
24.656444	1614.103324	14.916339
24.808321	1599.562015	14.921357
24.701701	1595.965887	14.926375
25.043857	1606.510103	14.931392
24.713801	1575.425523	14.936410
24.518356	1613.376673	14.941427
25.019615	1588.515904	14.946445
24.707485	1607.394346	14.951463
24.401427	1613.400082	14.956480
25.022858	1602.329385	14.961498
24.726931	1619.915410	14.966515
24.958171	1634.475875	14.971533
25.018706	1627.345309	14.976551
25.146480	1645.651847	14.981568
25.442732	1629.041018	14.986586
24.831373	1620.194536	14.991603
24.951916	1621.300007	14.996621
25.070506	1627.813725	15.001639
25.321971	1625.197071	15.006656
25.459844	1615.960525	15.011674
25.087542	1620.727878	15.016691
25.091565	1615.976825	15.021709
25.295738	1606.668363	15.026727
24.831337	1591.836838	15.031744
25.254401	1629.145117	15.036762
25.062689	1629.608282	15.041779
25.330314	1626.990622	15.046797
25.304114	1652.118616	15.051815
25.309246	1634.671770	15.056832
25.092309	1637.853940	15.061850
25.281925	1640.807669	15.066867
25.356967	1627.610911	15.071885
25.194379	1654.950267	15.076903
25.245334	1623.161455	15.081920
25.425706	1648.690638	15.086938
25.390077	1640.362628	15.091955
25.475378	1627.535459	15.096973
25.258461	1633.136882	15.101991
25.168720	1644.363485	15.107008
25.291647	1646.753711	15.112026
25.033638	1660.752037	15.117043
25.729309	1663.291575	15.122061
25.496355	1666.257660	15.127079
25.722732	1666.153924	15.132096
25.706749	1664.783263	15.137114
25.968788	1668.183187	15.142131
26.528556	1657.513960	15.147149
26.384248	1644.912160	15.152167
25.798063	1634.641242	15.157184
26.175768	1613.364535	15.162202
26.368850	1617.189142	15.167219
26.318422	1609.247319	15.172237
26.190113	1611.580090	15.177255
25.896771	1610.555690	15.182272
26.095818	1605.342533	15.187290
26.035935	1597.035720	15.192307
25.861898	1590.305948	15.197325
26.076204	1579.111451	15.202343
25.704819	1589.830820	15.207360
26.197358	1603.898128	15.212378
26.037661	1615.837420	15.217395
26.128215	1606.070467	15.222413
26.225986	1587.817686	15.227431
26.136298	1583.048559	15.232448
26.234784	1567.384823	15.237466
25.990429	1580.279806	15.242483
26.221789	1588.540407	15.247501
26.052819	1586.374632	15.252519
25.924104	1596.666769	15.257536
26.154711	1613.413765	15.262554
26.182305	1615.795599	15.267571
26.433204	1616.488603	15.272589
26.212376	1615.770379	15.277607
26.335756	1621.149206	15.282624
26.664132	1612.182717	15.287642
26.327403	1632.823716	15.292659
26.720464	1611.541416	15.297677
26.743191	1609.057202	15.302695
26.060262	1600.912689	15.307712
26.516553	1608.693840	15.312730
26.518700	1616.578897	15.317747
26.410989	1615.858360	15.322765
26.563211	1619.159388	15.327783
26.438241	1615.207540	15.332800
26.759890	1618.881082	15.337818
26.142802	1619.929612	15.342835
26.474929	1615.071168	15.347853
26.616112	1616.734904	15.352871
26.470534	1617.075881	15.357888
26.956956	1613.482676	15.362906
26.877821	1619.655133	15.367923
26.920823	1619.505145	15.372941
26.399352	1622.580162	15.377959
26.785977	1615.946559	15.382976
27.020575	1625.425730	15.387994
26.598498	1626.029458	15.393011
26.780401	1617.413511	15.398029
26.946610	1612.988938	15.403047
26.668736	1617.906391	15.408064
26.853210	1615.188741	15.413082
26.860389	1621.570795	15.418099
26.742634	1620.153453	15.423117
26.967440	1618.760117	15.428135
26.687045	1620.151334	15.433152
26.892754	1619.536528	15.438170
26.699018	1634.081414	15.443187
26.616313	1637.094311	15.448205
27.174736	1640.709641	15.453223
27.028287	1647.264072	15.458240
26.901441	1655.948357	15.463258
26.802198	1657.085744	15.468275
27.214554	1645.744776	15.473293
27.393339	1655.320958	15.478311
27.015236	1654.177943	15.483328
27.232784	1646.644804	15.488346
27.196194	1644.667111	15.493363
27.199513	1643.431797	15.498381
27.152296	1647.763494	15.503399
27.266671	1649.648582	15.508416
27.266300	1631.969813	15.513434
27.167949	1661.136186	15.518451
27.413455	1643.070552	15.523469
27.603336	1663.990956	15.528487
27.556274	1661.966169	15.533504
27.540660	1651.467376	15.538522
27.508566	1651.247570	15.543539
27.240147	1665.098127	15.548557
27.956279	1667.258457	15.553575
27.500967	1664.348701	15.558592
27.748798	1667.245961	15.563610
27.606945	1670.508967	15.568627
27.969244	1668.909656	15.573645
27.957404	1646.571919	15.578663
27.683280	1643.356420	15.583680
28.129848	1629.151885	15.588698
27.957751	1641.513163	15.593715
27.731874	1642.319971	15.598733
27.875230	1643.141813	15.603751
27.769015	1647.497078	15.608768
27.823571	1637.185299	15.613786
27.881549	1641.276850	15.618803
27.650179	1635.717069	15.623821
27.830054	1638.744709	15.628839
27.371659	1660.094124	15.633856
27.869002	1664.444353	15.638874
28.090236	1681.932231	15.643891
28.110989	1678.765640	15.648909
28.417104	1669.256838	15.653927
27.944698	1683.676340	15.658944
27.958763	1678.401431	15.663962
28.168327	1682.965880	15.668979
28.178984	1681.630293	15.673997
28.115390	1682.618852	15.679015
28.002790	1680.733502	15.684032
28.170061	1689.392914	15.689050
28.031850	1689.584856	15.694067
27.858815	1678.884642	15.699085
28.094857	1682.505790	15.704103
27.681947	1691.249882	15.709120
27.983969	1685.491745	15.714138
28.314861	1703.323945	15.719155
28.350762	1718.829566	15.724173
28.403985	1704.417145	15.729191
28.253905	1710.350850	15.734208
28.662941	1708.943849	15.739226
28.701425	1714.414903	15.744243
28.569848	1714.349389	15.749261
28.764951	1705.323878	15.754279
28.715700	1702.943937	15.759296
28.683093	1696.155377	15.764314
28.628426	1690.962211	15.769331
28.869321	1705.595140	15.774349
28.808409	1682.931699	15.779367
28.472951	1684.501588	15.784384
28.679119	1674.624914	15.789402
28.667612	1683.611708	15.794419
28.688429	1701.159891	15.799437
28.948481	1702.683555	15.804455
28.715349	1713.255121	15.809472
28.509132	1703.859478	15.814490
28.666364	1703.247683	15.819507
28.873779	1723.312812	15.824525
28.916614	1703.827552	15.829543
28.875799	1703.354311	15.834560
29.064237	1694.635031	15.839578
28.834032	1711.790694	15.844595
28.664237	1707.196323	15.849613
28.950484	1709.428377	15.854631
29.078914	1708.383882	15.859648
29.039498	1702.118641	15.864666
28.769626	1713.268638	15.869683
28.770865	1712.736780	15.874701
28.956446	1712.018218	15.879719
28.729197	1735.713965	15.884736
29.150898	1728.587086	15.889754
29.737826	1740.445137	15.894771
29.382545	1731.645826	15.899789
29.746913	1725.695260	15.904807
29.792330	1724.335249	15.909824
29.732744	1713.127710	15.914842
29.519631	1703.160596	15.919859
29.195724	1704.363709	15.924877
29.401322	1696.577625	15.929895
29.368167	1705.309914	15.934912
29.366672	1704.023453	15.939930
29.783981	1690.087789	15.944947
29.284610	1698.836240	15.949965
29.675608	1696.607868	15.954983
29.568449	1693.821894	15.960000
29.576298	1697.965501	15.965018
29.702501	1691.725755	15.970035
29.382880	1690.107802	15.975053
29.465974	1706.337325	15.980071
29.500952	1730.587402	15.985088
29.406986	1734.745687	15.990106
30.129527	1718.644050	15.995123
29.794395	1719.713677	16.000141
30.270107	1721.349232	16.005159
29.904380	1727.150603	16.010176
29.972669	1722.964982	16.015194
30.111782	1721.651372	16.020211
29.861720	1718.697855	16.025229
29.699685	1710.912203	16.030247
29.793914	1722.513781	16.035264
29.659229	1738.174046	16.040282
29.872614	1730.831861	16.045299
29.646335	1734.691931	16.050317
29.750640	1726.129196	16.055335
29.985409	1726.788600	16.060352
30.238669	1726.362830	16.065370
29.977397	1729.375915	16.070387
29.900845	1725.512267	16.075405
30.030407	1732.546519	16.080423
30.319557	1757.317659	16.085440
30.250078	1759.875447	16.090458
30.329715	1748.290175	16.095475
30.303473	1767.360746	16.100493
30.465912	1756.413483	16.105511
30.408352	1762.947496	16.110528
30.564672	1763.720087	16.115546
30.833479	1756.880274	16.120563
29.983525	1737.337607	16.125581
30.656474	1733.945852	16.130599
30.576381	1739.118083	16.135616
30.518876	1745.568710	16.140634
30.550403	1750.564268	16.145651
30.572203	1759.278386	16.150669
30.553766	1748.158637	16.155687
30.868058	1744.632182	16.160704
30.667545	1754.745551	16.165722
30.707955	1749.954044	16.170739
30.855134	1753.559497	16.175757
31.061010	1741.683538	16.180775
30.860961	1726.608361	16.185792
30.421274	1717.149278	16.190810
30.665662	1747.307199	16.195827
30.656226	1751.931771	16.200845
30.898368	1742.645480	16.205863
31.127812	1747.702274	16.210880
31.264713	1748.517287	16.215898
30.945509	1752.382747	16.220915
30.910028	1751.172488	16.225933
31.171631	1750.352137	16.230951
31.173355	1747.860239	16.235968
30.922310	1747.617155	16.240986
31.167852	1744.197620	16.246003
31.149659	1754.745943	16.251021
31.234400	1751.342618	16.256039
31.157610	1740.491728	16.261056
30.963196	1757.279945	16.266074
31.047496	1745.975498	16.271091
30.894437	1746.624407	16.276109
31.157369	1743.790401	16.281127
31.077528	1757.150075	16.286144
30.823168	1758.257157	16.291162
31.316183	1745.924839	16.296179
31.192767	1750.628938	16.301197
31.473730	1751.081204	16.306215
31.174557	1755.201441	16.311232
31.251935	1772.748554	16.316250
31.539719	1776.333158	16.321267
31.342198	1784.360265	16.326285
31.587518	1775.158390	16.331303
31.408408	1772.429494	16.336320
31.297846	1789.487514	16.341338
31.754727	1785.386181	16.346355
31.710097	1788.243600	16.351373
31.799996	1780.699292	16.356391
31.829769	1782.229810	16.361408
31.725238	1782.804913	16.366426
31.703430	1784.139168	16.371443
31.330343	1785.170809	16.376461
31.522681	1779.117103	16.381479
31.657879	1778.840723	16.386496
31.681099	1789.075729	16.391514
32.258899	1802.539754	16.396531
32.255065	1793.780299	16.401549
32.254378	1785.147761	16.406567
32.531672	1778.920057	16.411584
32.000945	1788.640960	16.416602
32.211402	1780.844618	16.421619
31.970769	1780.736724	16.426637
32.211668	1767.217659	16.431655
32.276734	1771.589683	16.436672
31.867119	1772.874112	16.441690
32.319872	1765.234182	16.446707
32.283050	1775.849985	16.451725
32.093674	1761.740467	16.456743
32.360745	1771.002200	16.461760
32.151892	1777.834054	16.466778
32.332063	1774.302245	16.471795
32.117912	1776.919292	16.476813
32.332702	1801.733830	16.481831
32.841089	1802.846663	16.486848
32.506563	1804.211925	16.491866
32.748059	1799.581806	16.496883
32.927872	1784.351598	16.501901
32.418066	1774.612656	16.506919
33.002780	1778.831009	16.511936
32.735876	1781.797813	16.516954
32.730628	1784.974562	16.521971
32.379359	1789.670974	16.526989
32.401866	1774.053740	16.532007
32.975264	1770.932684	16.537024
32.700168	1775.294475	16.542042
32.925892	1772.526173	16.547059
32.961072	1776.884091	16.552077
32.453715	1773.227571	16.557095
32.597065	1769.171534	16.562112
32.414821	1792.001335	16.567130
32.487008	1794.154291	16.572147
32.761107	1793.992607	16.577165
32.826031	1810.822888	16.582183
32.912859	1800.587642	16.587200
32.734074	1807.156741	16.592218
33.001066	1803.074681	16.597235
33.002800	1798.119442	16.602253
32.899820	1811.034549	16.607271
33.322711	1822.936137	16.612288
33.394625	1825.504417	16.617306
33.438835	1817.404240	16.622323
33.302712	1822.994421	16.627341
33.323823	1807.045470	16.632359
33.328138	1790.834950	16.637376
33.149654	1820.207904	16.642394
33.172790	1802.413494	16.647411
33.316380	1842.068213	16.652429
33.100825	1818.650586	16.657447
33.517217	1840.401844	16.662464
33.527188	1821.742780	16.667482
33.689540	1848.884381	16.672499
33.625488	1823.628896	16.677517
33.361916	1822.769615	16.682535
33.889545	1840.031062	16.687552
33.750787	1841.044205	16.692570
33.418044	1823.789450	16.697587
33.893537	1840.467760	16.702605
34.001854	1840.522854	16.707623
34.080163	1816.262413	16.712640
33.703006	1839.365621	16.717658
34.071496	1829.635982	16.722675
33.983803	1826.732047	16.727693
33.997665	1840.130333	16.732711
34.077628	1824.381186	16.737728
33.978027	1827.277268	16.742746
34.243713	1821.504425	16.747763
34.326452	1827.259469	16.752781
33.643941	1823.316273	16.757799
34.122974	1815.044494	16.762816
34.133813	1825.677899	16.767834
34.518507	1820.779543	16.772851
34.241439	1815.882927	16.777869
33.820474	1825.784546	16.782887
34.102956	1816.598739	16.787904
34.095184	1816.252356	16.792922
34.204342	1823.604509	16.797939
34.046493	1815.590046	16.802957
34.575534	1827.043702	16.807975
34.731423	1819.905696	16.812992
34.191218	1818.263138	16.818010
34.525318	1819.016813	16.823027
34.316342	1822.356626	16.828045
33.967206	1826.264632	16.833063
34.349884	1812.178648	16.838080
34.535180	1825.371826	16.843098
34.201030	1822.488328	16.848115
34.298874	1813.926571	16.853133
34.283442	1826.410880	16.858151
34.588696	1837.815297	16.863168
34.577676	1853.408770	16.868186
34.520103	1853.839534	16.873203
34.940338	1845.289256	16.878221
34.843305	1851.639270	16.883239
34.885665	1847.567860	16.888256
34.806248	1843.141498	16.893274
34.975890	1844.550612	16.898291
35.070829	1848.960367	16.903309
34.806912	1844.947249	16.908327
35.073325	1838.076320	16.913344
34.797797	1854.103665	16.918362
35.022825	1843.825896	16.923379
35.075547	1850.987292	16.928397
34.760888	1851.624229	16.933415
34.910233	1853.179726	16.938432
35.228312	1846.379203	16.943450
35.075931	1852.115132	16.948467
35.276603	1837.114348	16.953485
35.158872	1844.217987	16.958503
35.214086	1848.829131	16.963520
35.438270	1858.195287	16.968538
35.385515	1864.791500	16.973555
35.537609	1863.406595	16.978573
35.493404	1859.496852	16.983591
35.641815	1864.915823	16.988608
35.535279	1852.608262	16.993626
35.357550	1851.452145	16.998643
35.430094	1859.187680	17.003661
35.668532	1868.993586	17.008679
35.797897	1868.991841	17.013696
35.765907	1871.060752	17.018714
35.564199	1879.300936	17.023731
36.043529	1865.693411	17.028749
35.863582	1876.465823	17.033767
35.856288	1869.273598	17.038784
35.638381	1871.450816	17.043802
35.716906	1875.023206	17.048819
36.197667	1869.041433	17.053837
35.835865	1873.767866	17.058855
36.240237	1874.568538	17.063872
36.016086	1865.392726	17.068890
35.596462	1878.150762	17.073907
36.113802	1858.372531	17.078925
35.878106	1875.258704	17.083943
36.227222	1867.959293	17.088960
36.139740	1874.528015	17.093978
36.189301	1870.563988	17.098995
35.988827	1869.589248	17.104013
35.856913	1874.919230	17.109031
36.234788	1864.447180	17.114048
36.272599	1863.594880	17.119066
36.362951	1876.181907	17.124083
36.661871	1866.584463	17.129101
36.385348	1864.525462	17.134119
36.309714	1873.955182	17.139136
36.499953	1861.299830	17.144154
36.780898	1866.694515	17.149171
36.838375	1867.877705	17.154189
36.629896	1875.356055	17.159207
36.687827	1866.056598	17.164224
36.668887	1871.613949	17.169242
36.493589	1869.219479	17.174259
36.570535	1856.819727	17.179277
36.453963	1875.632718	17.184295
36.249761	1866.837539	17.189312
36.318339	1865.892242	17.194330
36.285122	1866.147663	17.199347
36.623572	1883.579335	17.204365
36.711150	1906.490545	17.209383
36.770485	1890.167319	17.214400
37.066393	1881.462246	17.219418
36.616863	1896.677401	17.224435
37.115558	1889.239291	17.229453
37.090179	1883.737791	17.234471
36.838941	1886.219201	17.239488
36.948261	1900.673541	17.244506
36.890498	1892.819249	17.249523
37.048865	1886.829119	17.254541
37.314192	1925.684432	17.259559
37.263506	1921.799302	17.264576
37.243322	1921.895343	17.269594
37.398561	1931.664226	17.274611
37.880526	1915.297155	17.279629
37.502244	1913.155278	17.284647
37.543906	1905.245794	17.289664
37.624289	1901.105383	17.294682
37.535349	1886.621075	17.299699
37.897003	1882.368166	17.304717
37.573964	1878.551657	17.309735
37.365877	1874.416369	17.314752
37.683192	1876.127545	17.319770
37.530509	1882.316564	17.324787
37.746968	1892.374529	17.329805
37.736184	1911.283949	17.334823
37.785919	1908.282572	17.339840
37.880113	1912.601230	17.344858
37.767503	1918.063428	17.349875
37.851863	1917.692909	17.354893
37.761295	1919.141963	17.359911
37.719751	1916.095369	17.364928
38.095847	1910.775213	17.369946
37.796902	1925.544809	17.374963
38.077211	1913.543580	17.379981
38.278734	1910.728776	17.384999
37.711343	1920.870892	17.390016
37.633880	1911.033006	17.395034
37.865415	1911.716531	17.400051
37.850183	1905.533860	17.405069
38.154551	1913.396040	17.410087
37.850077	1919.403220	17.415104
38.208235	1933.915430	17.420122
38.047019	1946.912306	17.425139
38.463199	1939.625758	17.430157
38.257757	1940.050223	17.435175
38.318795	1939.511964	17.440192
38.231476	1940.933760	17.445210
38.434387	1948.260011	17.450227
38.684634	1934.059754	17.455245
38.451128	1940.277419	17.460263
38.691758	1936.976600	17.465280
38.762367	1931.730331	17.470298
38.644894	1935.989950	17.475315
39.201835	1929.686116	17.480333
38.779206	1939.636841	17.485351
38.560182	1939.825946	17.490368
38.791202	1929.048512	17.495386
38.855589	1933.231932	17.500403
38.940299	1929.883626	17.505421
38.855675	1935.791251	17.510439
38.858360	1942.863147	17.515456
39.009388	1935.754174	17.520474
38.700925	1939.231005	17.525491
38.953987	1946.478470	17.530509
39.124957	1964.246840	17.535527
39.021697	1973.905974	17.540544
39.462204	1960.373767	17.545562
39.115729	1962.676898	17.550579
39.681768	1958.506196	17.555597
39.524572	1972.754582	17.560615
39.673568	1963.827502	17.565632
39.717639	1962.063415	17.570650
39.376136	1951.934137	17.575667
39.497179	1931.490709	17.580685
39.304687	1933.105459	17.585703
39.493865	1953.894261	17.590720
39.737980	1967.353466	17.595738
39.821989	1968.741645	17.600755
39.897309	1947.789535	17.605773
39.438110	1956.827458	17.610791
39.349603	1964.945815	17.615808
40.058975	1955.413404	17.620826
39.753909	1958.638013	17.625843
39.894432	1960.100548	17.630861
39.975225	1962.687884	17.635879
39.951313	1972.104699	17.640896
39.852570	1947.982390	17.645914
39.773890	1948.558095	17.650931
39.770174	1964.103332	17.655949
39.706277	1964.318030	17.660967
39.633886	1961.485559	17.665984
39.704350	1962.581742	17.671002
39.886707	1975.342944	17.676019
39.604011	1960.590592	17.681037
40.191031	1972.382755	17.686055
40.142506	1984.811131	17.691072
40.419699	1986.107149	17.696090
40.400231	1996.136752	17.701107
40.371375	1984.884775	17.706125
40.538312	1983.057044	17.711143
40.473175	1994.943810	17.716160
40.431078	1992.734140	17.721178
40.049785	1996.367320	17.726195
40.145095	1985.529694	17.731213
40.578817	1983.506825	17.736231
40.309775	1982.344812	17.741248
40.671360	1984.328940	17.746266
40.413790	1986.599017	17.751283
40.433308	1986.529849	17.756301
40.448221	1986.093328	17.761319
40.493683	1996.913245	17.766336
40.862747	2008.381552	17.771354
40.598860	2012.875333	17.776371
40.948023	2005.522364	17.781389
41.084699	2011.591350	17.786407
41.233621	2010.125140	17.791424
41.246565	2006.550736	17.796442
41.491898	2009.599475	17.801459
41.451550	1996.169103	17.806477
41.175812	1984.336732	17.811495
40.960946	1983.117314	17.816512
41.351291	1990.501780	17.821530
41.691728	1992.701641	17.826547
41.394199	1974.704910	17.831565
41.628921	1970.569749	17.836583
41.375263	1974.254924	17.841600
41.388400	1970.387915	17.846618
41.427329	1970.293629	17.851635
41.415757	1958.563862	17.856653
41.687855	1968.809634	17.861671
41.149012	1974.852646	17.866688
41.391812	1964.598699	17.871706
41.543934	1982.771220	17.876723
41.402230	1991.907961	17.881741
41.899126	1995.792749	17.886759
41.963518	1998.746078	17.891776
41.920854	1997.395371	17.896794
41.865006	2005.002025	17.901811
42.010291	1993.130807	17.906829
42.085566	1993.062184	17.911847
41.882207	1980.527711	17.916864
42.020631	1974.153761	17.921882
41.994316	1978.641098	17.926899
41.779698	1975.820300	17.931917
41.826451	1993.254588	17.936935
42.068647	1997.386069	17.941952
41.996666	1991.481402	17.946970
42.271939	1994.468733	17.951987
42.356426	1987.788775	17.957005
42.271187	1990.953160	17.962023
42.213890	1999.530601	17.967040
42.509104	1988.222212	17.972058
42.381992	1988.715981	17.977075
42.159243	1994.540268	17.982093
42.283269	1985.496034	17.987111
42.338986	1990.574333	17.992128
42.599721	1989.879951	17.997146
42.338570	1996.344295	18.002163
42.195570	1992.750723	18.007181
42.705733	1987.558593	18.012199
42.481219	1997.281128	18.017216
42.807952	2005.555071	18.022234
42.791115	2009.148998	18.027251
42.604866	2029.456669	18.032269
42.854497	2018.651032	18.037287
43.061658	2028.119116	18.042304
43.276856	2020.512226	18.047322
43.178126	2030.648877	18.052339
42.991320	2028.537789	18.057357
43.313103	2012.480877	18.062375
42.841550	2013.284418	18.067392
43.273564	2022.433487	18.072410
43.081645	2020.721193	18.077427
43.114433	2021.362492	18.082445
42.923063	2027.389427	18.087463
43.201429	2015.899659	18.092480
42.996412	2019.342706	18.097498
43.167016	2021.758425	18.102515
43.024000	2021.861474	18.107533
43.460634	2004.420860	18.112551
43.037500	2024.911028	18.117568
43.154007	2046.850431	18.122586
43.598066	2043.872647	18.127603
43.748375	2045.206213	18.132621
43.859333	2051.066958	18.137639
43.485007	2047.801282	18.142656
43.469862	2059.851588	18.147674
43.626995	2047.171468	18.152691
43.743758	2061.377816	18.157709
43.941619	2044.535241	18.162727
43.458671	2056.477689	18.167744
43.596578	2049.666485	18.172762
43.671866	2060.598097	18.177779
43.610320	2053.574884	18.182797
43.934495	2066.953771	18.187815
44.213419	2069.314468	18.192832
44.294923	2078.174985	18.197850
44.548763	2075.688436	18.202867
44.118627	2062.705569	18.207885
44.376435	2052.983998	18.212903
44.162110	2059.506968	18.217920
44.501028	2055.447973	18.222938
44.806122	2047.543585	18.227955
44.312259	2039.288435	18.232973
44.577406	2045.382562	18.237991
44.545360	2048.757126	18.243008
44.523900	2036.091345	18.248026
44.493211	2044.755804	18.253043
44.398734	2049.670890	18.258061
44.849927	2048.134440	18.263079
44.654283	2070.430410	18.268096
44.853327	2066.488104	18.273114
45.031172	2062.833901	18.278131
44.714922	2049.928835	18.283149
44.821435	2055.179954	18.288167
45.033293	2061.208654	18.293184
45.019944	2060.740458	18.298202
44.950198	2057.569344	18.303219
44.680414	2063.640263	18.308237
44.997124	2060.173124	18.313255
44.896801	2055.580144	18.318272
44.780970	2064.690781	18.323290
45.213102	2061.427030	18.328307
45.132020	2057.065363	18.333325
44.919106	2057.775741	18.338343
45.239450	2058.600839	18.343360
45.366190	2057.691871	18.348378
45.460788	2058.958819	18.353395
45.305320	2055.884749	18.358413
45.315094	2063.235573	18.363431
45.751774	2078.795632	18.368448
45.346501	2096.700123	18.373466
45.680078	2092.168485	18.378483
45.530356	2090.183608	18.383501
45.607374	2093.598989	18.388519
45.750441	2101.011942	18.393536
46.029426	2092.265399	18.398554
45.911441	2092.392770	18.403571
45.481517	2094.998670	18.408589
45.757915	2087.723334	18.413607
45.845544	2082.406656	18.418624
45.606925	2098.799620	18.423642
46.016362	2087.074956	18.428659
46.381949	2090.365657	18.433677
46.028172	2089.012655	18.438695
46.284286	2081.861682	18.443712
46.138667	2090.800906	18.448730
46.247347	2079.303547	18.453747
46.215194	2081.614762	18.458765
46.471602	2083.813884	18.463783
46.221958	2085.075967	18.468800
45.968702	2082.015915	18.473818
46.133432	2085.991463	18.478835
46.313872	2110.242571	18.483853
46.576805	2111.127166	18.488871
46.769311	2114.646829	18.493888
46.505714	2127.254351	18.498906
46.982269	2114.238503	18.503923
46.481500	2123.780240	18.508941
46.655360	2102.903425	18.513959
46.849813	2108.371774	18.518976
46.591615	2114.022436	18.523994
46.811277	2111.904705	18.529011
46.811889	2103.753120	18.534029
47.225388	2110.366311	18.539047
47.165994	2112.321650	18.544064
46.932720	2116.939569	18.549082
47.086045	2112.485440	18.554099
47.243498	2112.795396	18.559117
47.201485	2115.353584	18.564135
47.344626	2111.637263	18.569152
47.194814	2104.889229	18.574170
47.214641	2110.476667	18.579187
47.035809	2109.742279	18.584205
47.045421	2098.973294	18.589223
47.302168	2126.374069	18.594240
47.364326	2127.817659	18.599258
47.643548	2126.064810	18.604275
47.515995	2139.462333	18.609293
47.758273	2125.120014	18.614311
48.015055	2135.329022	18.619328
47.697339	2140.550309	18.624346
47.702801	2123.824848	18.629363
47.909806	2129.866936	18.634381
47.703875	2132.234192	18.639399
48.114380	2132.368505	18.644416
47.743105	2139.154074	18.649434
48.265874	2135.709108	18.654451
48.113460	2126.779666	18.659469
48.073907	2137.853924	18.664487
48.382968	2133.746187	18.669504
48.109005	2137.566777	18.674522
48.109509	2123.454934	18.679539
48.314492	2132.563207	18.684557
48.448109	2115.117310	18.689575
48.222521	2130.125527	18.694592
48.095816	2136.115451	18.699610
48.421029	2123.452501	18.704627
48.254240	2131.405682	18.709645
47.993953	2127.972358	18.714663
48.481419	2114.350721	18.719680
48.170720	2129.753189	18.724698
48.413706	2141.274747	18.729715
48.274586	2150.159487	18.734733
48.570069	2154.381617	18.739751
48.721776	2156.054749	18.744768
48.332955	2169.832178	18.749786
48.978765	2159.951120	18.754803
48.871910	2150.558213	18.759821
48.778916	2150.772835	18.764839
49.384974	2148.477062	18.769856
49.015819	2150.820018	18.774874
49.058425	2137.812017	18.779891
48.890203	2149.158494	18.784909
48.801485	2158.812285	18.789927
49.277364	2160.301576	18.794944
49.386518	2176.250613	18.799962
49.465618	2176.514866	18.804979
49.326542	2189.003478	18.809997
49.303311	2179.019905	18.815015
49.654288	2172.627696	18.820032
49.971340	2179.681026	18.825050
49.773526	2173.418823	18.830067
49.614924	2156.719492	18.835085
49.616976	2156.181196	18.840103
50.053237	2176.072025	18.845120
49.530123	2161.905234	18.850138
49.659283	2152.438501	18.855155
49.990697	2163.444171	18.860173
49.741597	2163.872458	18.865191
50.135017	2171.536530	18.870208
49.755906	2179.166522	18.875226
49.818093	2173.221503	18.880243
49.862115	2166.639153	18.885261
49.860197	2168.442185	18.890279
50.385188	2162.866952	18.895296
50.136633	2184.507710	18.900314
50.434452	2169.278727	18.905331
50.345769	2162.959795	18.910349
49.597428	2174.147134	18.915367
50.325698	2165.451583	18.920384
50.201008	2168.386341	18.925402
50.146765	2184.575384	18.930419
50.816950	2202.670269	18.935437
50.743758	2203.492078	18.940455
50.788042	2184.267069	18.945472
50.546300	2209.052876	18.950490
50.983865	2201.259412	18.955507
50.885834	2195.635673	18.960525
50.658472	2191.286285	18.965543
50.948307	2193.053796	18.970560
50.902458	2211.217282	18.975578
50.652676	2201.655226	18.980595
50.948113	2196.159067	18.985613
50.261758	2204.029989	18.990631
50.484833	2207.769746	18.995648
50.736467	2217.216703	19.000666
51.126951	2215.864529	19.005683
51.229027	2229.071350	19.010701
51.153474	2233.469090	19.015719
51.227567	2222.954001	19.020736
51.644173	2218.759872	19.025754
51.795398	2227.290031	19.030771
51.793705	2222.630928	19.035789
51.729557	2236.683829	19.040807
51.776273	2212.552036	19.045824
51.326732	2221.587007	19.050842
51.291659	2225.871321	19.055859
51.644023	2219.834381	19.060877
51.546472	2228.176127	19.065895
51.711958	2231.017423	19.070912
51.576193	2223.792029	19.075930
51.791049	2211.827737	19.080947
51.587327	2220.633160	19.085965
51.964731	2224.411228	19.090983
52.150829	2224.184926	19.096000
51.948001	2219.391162	19.101018
51.999346	2239.670668	19.106035
52.555923	2240.127756	19.111053
52.039993	2250.568635	19.116071
52.595749	2241.249311	19.121088
52.687772	2245.200319	19.126106
52.492900	2245.492542	19.131123
52.335597	2224.372639	19.136141
52.334022	2229.328023	19.141159
52.449575	2236.809931	19.146176
52.604016	2239.245569	19.151194
52.680058	2260.063868	19.156211
52.596649	2243.303680	19.161229
52.272492	2252.144062	19.166247
52.890005	2237.414586	19.171264
52.766077	2245.313802	19.176282
52.430391	2242.235402	19.181299
52.629407	2240.803652	19.186317
52.692280	2241.169597	19.191335
53.138466	2255.833263	19.196352
53.068743	2277.109000	19.201370
52.970589	2277.791646	19.206387
53.498818	2261.207593	19.211405
53.018795	2268.664959	19.216423
53.208582	2266.525229	19.221440
53.651067	2278.229012	19.226458
53.275923	2267.588912	19.231475
53.797092	2266.601290	19.236493
53.550094	2265.056629	19.241511
53.849238	2253.955052	19.246528
54.008202	2261.783986	19.251546
53.654464	2254.217383	19.256563
54.045065	2251.477752	19.261581
54.049370	2232.831648	19.266599
53.812684	2230.355670	19.271616
54.029540	2223.937641	19.276634
53.857271	2221.816339	19.281651
53.804856	2219.315692	19.286669
53.619310	2220.169579	19.291687
53.871772	2230.818226	19.296704
54.455919	2254.410570	19.301722
53.827673	2241.553522	19.306739
54.276314	2241.485122	19.311757
54.066775	2252.976699	19.316775
54.068104	2251.084112	19.321792
54.538557	2251.027965	19.326810
54.273476	2252.391626	19.331827
54.358817	2255.448634	19.336845
54.151631	2258.476794	19.341863
54.358535	2242.648743	19.346880
54.414536	2250.978595	19.351898
54.218099	2256.087768	19.356915
54.283653	2248.718564	19.361933
54.534371	2270.583416	19.366951
54.664651	2287.591022	19.371968
54.884037	2284.686780	19.376986
54.799692	2292.606450	19.382003
54.759679	2282.336039	19.387021
54.702457	2290.790941	19.392039
54.663307	2281.660862	19.397056
54.806694	2297.175127	19.402074
54.464631	2284.160708	19.407091
55.233676	2298.214485	19.412109
55.293146	2306.185157	19.417127
55.265846	2310.937029	19.422144
55.484551	2315.188756	19.427162
55.469250	2312.779703	19.432179
55.560694	2307.816274	19.437197
55.721140	2301.158664	19.442215
56.154698	2311.707698	19.447232
56.212260	2295.632842	19.452250
55.841851	2294.949450	19.457267
56.008384	2271.723408	19.462285
55.906245	2267.420092	19.467303
55.863797	2276.755116	19.472320
55.657406	2263.882673	19.477338
55.877852	2282.639289	19.482355
55.926500	2293.540720	19.487373
55.682946	2312.484643	19.492391
56.037938	2298.811604	19.497408
56.301044	2290.891759	19.502426
56.206497	2298.350580	19.507443
56.222359	2302.601622	19.512461
56.274999	2308.677846	19.517479
56.171296	2304.294542	19.522496
56.357125	2297.137371	19.527514
56.260492	2293.062836	19.532531
56.351566	2302.129609	19.537549
56.130438	2307.909716	19.542567
56.515753	2305.844189	19.547584
56.550307	2313.609623	19.552602
56.544255	2316.778751	19.557619
56.662279	2314.398770	19.562637
56.988106	2325.326802	19.567655
56.858758	2326.738035	19.572672
57.074473	2313.485183	19.577690
57.073624	2317.340910	19.582707
57.382441	2309.961191	19.587725
57.064960	2312.343121	19.592743
57.157063	2308.831524	19.597760
57.280922	2307.408609	19.602778
57.132579	2305.763263	19.607795
57.403573	2299.364880	19.612813
57.288232	2304.042700	19.617831
57.251858	2310.296721	19.622848
57.457225	2307.824157	19.627866
57.504244	2300.377657	19.632883
57.493584	2300.731736	19.637901
57.119482	2309.311125	19.642919
57.317814	2308.927138	19.647936
57.511047	2307.697656	19.652954
57.381642	2338.581836	19.657971
57.390732	2331.053279	19.662989
57.452482	2336.796144	19.668007
57.568153	2342.881205	19.673024
57.610554	2344.880115	19.678042
57.592084	2346.047144	19.683059
58.053459	2372.010997	19.688077
58.068812	2364.788172	19.693095
58.139517	2369.208244	19.698112
58.707619	2364.488102	19.703130
58.416543	2374.613198	19.708147
58.667394	2365.677492	19.713165
58.659177	2369.677558	19.718183
58.301163	2369.794449	19.723200
58.592699	2357.990845	19.728218
58.554517	2374.330126	19.733235
58.799816	2375.031930	19.738253
58.529587	2370.712921	19.743271
58.501181	2367.341657	19.748288
59.062048	2362.566039	19.753306
58.958203	2366.965186	19.758323
59.072416	2364.241303	19.763341
59.163612	2357.207737	19.768359
59.014567	2357.848165	19.773376
59.201974	2350.755212	19.778394
59.102297	2357.411043	19.783411
59.127527	2358.489302	19.788429
59.022542	2352.371094	19.793447
59.079849	2362.398143	19.798464
59.471532	2369.065273	19.803482
59.479138	2390.723684	19.808499
59.516327	2389.599311	19.813517
59.798299	2388.616799	19.818535
59.678187	2389.499585	19.823552
59.426012	2393.333283	19.828570
59.487948	2386.552129	19.833587
59.820566	2393.323076	19.838605
59.606155	2385.244955	19.843623
59.418250	2397.006909	19.848640
60.023615	2376.244928	19.853658
60.036786	2383.348400	19.858675
59.651410	2384.509456	19.863693
59.687754	2380.992578	19.868711
59.858161	2399.659797	19.873728
59.965944	2412.800593	19.878746
59.893755	2409.644735	19.883763
60.309243	2413.308237	19.888781
60.446288	2406.604759	19.893799
60.293586	2412.783780	19.898816
60.601143	2406.100299	19.903834
60.474596	2413.057751	19.908851
60.454939	2400.105065	19.913869
60.582330	2397.007829	19.918887
60.697605	2403.698612	19.923904
60.630015	2403.368834	19.928922
61.053844	2416.440348	19.933939
61.137393	2419.770606	19.938957
60.979673	2415.181946	19.943975
60.811130	2433.116733	19.948992
61.297924	2429.155965	19.954010
61.013482	2436.567276	19.959027
60.731633	2431.478507	19.964045
60.920987	2436.132940	19.969063
60.956857	2435.785088	19.974080
61.162362	2433.112700	19.979098
60.965598	2444.824194	19.984115
61.060001	2445.178823	19.989133
61.281915	2447.033494	19.994151
60.922561	2467.537705	19.999168
61.564391	2455.210947	20.004186
61.438655	2465.835929	20.009203
61.486200	2467.390427	20.014221
61.954580	2482.761817	20.019239
61.975334	2486.949210	20.024256
62.258430	2483.046873	20.029274
62.348000	2491.949617	20.034291
62.321485	2474.693217	20.039309
62.472253	2454.547132	20.044327
61.979488	2462.892270	20.049344
62.239435	2452.431533	20.054362
62.634276	2458.000979	20.059379
62.309090	2467.138966	20.064397
62.469486	2456.896244	20.069415
62.544591	2469.348575	20.074432
62.757048	2475.739163	20.079450
62.537750	2478.731546	20.084467
62.638971	2474.879456	20.089485
63.054066	2476.704106	20.094503
62.489088	2469.557272	20.099520
62.775160	2473.392447	20.104538
62.834169	2480.844173	20.109555
62.643189	2480.114848	20.114573
62.704453	2470.680761	20.119591
62.960266	2484.852762	20.124608
62.748967	2474.499419	20.129626
62.801084	2478.923275	20.134643
62.866503	2481.561137	20.139661
63.045281	2491.224395	20.144679
62.746851	2505.129299	20.149696
63.368053	2508.152805	20.154714
63.682427	2502.171362	20.159731
63.368644	2509.947626	20.164749
63.995211	2503.621435	20.169767
63.991568	2501.915233	20.174784
64.077789	2495.077457	20.179802
63.738886	2502.951322	20.184819
63.848277	2505.090586	20.189837
63.918909	2494.932156	20.194855
64.001395	2504.774383	20.199872
63.922698	2498.006169	20.204890
64.150966	2493.913579	20.209907
63.955864	2495.753755	20.214925
64.014647	2496.201373	20.219943
63.797698	2513.999256	20.224960
63.937021	2511.197406	20.229978
64.259048	2515.665530	20.234995
64.367069	2533.351828	20.240013
64.410637	2525.013824	20.245031
64.215925	2533.608777	20.250048
64.410817	2533.555683	20.255066
64.706760	2526.114985	20.260083
64.333693	2533.096083	20.265101
64.545213	2533.563387	20.270119
64.670320	2540.056816	20.275136
64.875241	2550.523725	20.280154
64.986471	2554.776148	20.285171
64.819289	2557.170326	20.290189
65.078946	2548.380187	20.295207
64.754712	2549.945226	20.300224
64.904385	2533.911260	20.305242
64.933563	2558.398037	20.310259
65.096489	2581.063906	20.315277
65.311916	2584.185183	20.320295
65.649687	2579.499351	20.325312
65.563605	2583.918540	20.330330
65.979467	2577.246023	20.335347
65.769659	2579.321372	20.340365
66.073904	2576.451519	20.345383
66.046958	2579.438412	20.350400
65.887227	2581.561620	20.355418
65.883747	2569.812764	20.360435
65.637709	2570.451367	20.365453
66.155334	2568.787864	20.370471
65.844649	2575.534080	20.375488
66.331027	2562.436042	20.380506
66.257109	2563.117981	20.385523
66.151185	2575.558376	20.390541
66.368884	2567.892600	20.395559
66.243045	2566.422180	20.400576
66.352045	2566.709201	20.405594
66.682076	2573.753577	20.410611
66.480493	2579.284484	20.415629
66.715574	2582.021151	20.420647
66.694756	2592.866243	20.425664
66.912791	2603.061312	20.430682
66.799193	2584.267600	20.435699
66.785957	2593.422768	20.440717
67.184132	2591.513248	20.445735
66.996125	2598.515200	20.450752
66.757393	2596.654564	20.455770
66.999191	2584.315993	20.460787
66.918710	2585.145278	20.465805
66.985129	2591.169083	20.470823
66.915517	2598.796333	20.475840
67.281781	2614.623044	20.480858
67.348399	2628.918175	20.485875
67.542262	2629.205820	20.490893
68.020280	2620.211703	20.495911
67.882185	2615.265903	20.500928
68.023977	2623.424190	20.505946
68.058230	2608.384658	20.510963
67.773961	2617.961399	20.515981
68.135156	2604.733845	20.520999
68.318428	2623.520429	20.526016
68.231885	2621.287076	20.531034
68.259738	2612.269591	20.536051
67.925810	2607.691670	20.541069
68.238683	2612.575009	20.546087
68.340303	2609.349699	20.551104
68.228427	2605.089522	20.556122
68.214841	2608.651616	20.561139
68.289348	2612.218538	20.566157
68.402286	2604.090445	20.571175
68.564510	2616.806659	20.576192
68.934340	2624.787784	20.581210
69.085469	2632.271301	20.586227
68.913353	2639.683676	20.591245
69.146150	2628.744201	20.596263
69.339737	2612.309085	20.601280
69.051778	2617.674450	20.606298
69.330819	2612.592117	20.611315
69.495905	2598.930210	20.616333
69.474036	2596.673174	20.621351
69.277138	2585.302809	20.626368
69.390037	2587.032521	20.631386
69.441334	2604.948187	20.636403
69.421699	2617.676103	20.641421
69.596884	2619.326669	20.646439
69.415663	2608.694713	20.651456
69.352212	2621.681317	20.656474
69.634013	2611.193384	20.661491
69.380588	2620.564637	20.666509
69.647426	2624.176395	20.671527
69.668024	2622.478897	20.676544
69.718978	2633.568987	20.681562
69.902613	2650.582667	20.686579
69.802396	2654.371744	20.691597
70.161302	2645.846517	20.696615
70.368324	2650.694053	20.701632
69.995664	2654.584001	20.706650
70.591463	2647.164634	20.711667
70.227672	2644.962912	20.716685
70.399652	2650.247066	20.721703
70.745293	2639.778820	20.726720
70.854431	2665.578361	20.731738
71.028970	2653.515526	20.736755
70.633075	2669.339583	20.741773
70.599726	2667.332131	20.746791
70.893603	2664.268850	20.751808
70.941639	2667.532466	20.756826
71.116632	2665.804832	20.761843
71.187795	2662.195025	20.766861
71.114138	2664.927464	20.771879
71.096884	2661.800544	20.776896
71.070726	2656.243817	20.781914
71.235188	2648.429180	20.786931
71.014454	2673.168378	20.791949
71.434036	2690.277400	20.796967
71.317152	2691.151824	20.801984
71.477137	2699.916830	20.807002
71.615295	2686.645334	20.812019
71.659516	2690.793648	20.817037
71.631643	2706.204312	20.822055
72.005599	2705.499709	20.827072
72.191085	2713.592086	20.832090
72.284045	2711.245928	20.837107
72.399207	2725.471274	20.842125
72.427794	2714.119116	20.847143
72.592541	2709.548935	20.852160
72.380339	2725.032278	20.857178
72.422405	2715.299844	20.862195
72.538447	2709.821882	20.867213
72.559280	2716.342246	20.872231
72.633765	2712.598183	20.877248
72.544954	2717.470901	20.882266
72.894655	2714.332636	20.887283
72.761985	2710.955898	20.892301
72.445100	2713.602078	20.897319
73.128025	2722.370214	20.902336
73.026813	2736.234444	20.907354
73.359007	2736.354516	20.912371
73.234285	2741.753669	20.917389
73.732089	2737.102043	20.922407
73.805399	2736.364374	20.927424
73.418055	2728.198805	20.932442
73.532747	2707.622372	20.937459
73.191574	2715.225352	20.942477
73.552330	2725.954626	20.947495
73.754842	2729.072489	20.952512
73.590924	2743.648333	20.957530
73.642043	2742.244058	20.962547
73.680233	2733.486771	20.967565
73.467142	2730.719850	20.972583
73.759021	2736.817088	20.977600
73.861186	2746.243398	20.982618
74.234714	2740.073877	20.987635
74.092912	2761.552952	20.992653
74.099887	2773.149625	20.997671
74.384837	2756.680897	21.002688
74.222993	2760.766924	21.007706
74.515131	2766.472428	21.012723
74.921082	2744.244916	21.017741
74.488349	2752.185791	21.022759
74.817560	2756.831394	21.027776
74.334732	2772.092094	21.032794
74.463109	2774.870987	21.037811
74.713051	2791.851447	21.042829
74.485915	2784.645065	21.047847
75.063595	2776.543433	21.052864
74.997833	2795.476144	21.057882
75.286965	2804.515575	21.062899
75.632535	2806.422149	21.067917
75.518955	2814.530819	21.072935
75.843947	2808.428002	21.077952
75.725443	2816.648364	21.082970
76.032768	2810.371388	21.087987
75.981326	2807.608560	21.093005
75.882366	2810.709238	21.098023
76.080171	2781.775633	21.103040
76.111035	2782.893927	21.108058
76.113727	2775.262335	21.113075
76.029376	2788.071512	21.118093
76.200208	2801.229347	21.123111
76.476152	2808.211675	21.128128
76.126307	2817.920134	21.133146
76.536031	2804.678368	21.138163
76.441685	2804.462967	21.143181
76.080500	2806.860597	21.148199
76.701640	2802.725712	21.153216
76.433100	2801.913566	21.158234
76.446721	2807.113703	21.163251
76.906026	2805.702525	21.168269
76.702235	2802.308793	21.173287
76.739349	2811.103689	21.178304
76.871133	2831.991788	21.183322
76.989436	2826.769054	21.188339
77.018503	2839.183424	21.193357
77.033443	2850.959798	21.198375
77.055733	2839.352128	21.203392
76.904173	2843.770039	21.208410
76.917411	2848.327632	21.213427
77.355153	2856.321652	21.218445
77.216358	2872.014467	21.223463
77.294337	2864.207216	21.228480
77.712406	2870.168760	21.233498
77.651765	2866.645995	21.238515
77.747061	2863.216345	21.243533
77.962142	2874.242687	21.248551
78.184012	2872.534296	21.253568
78.227060	2889.484156	21.258586
77.992436	2893.614077	21.263603
78.267051	2897.716266	21.268621
78.213125	2885.242911	21.273639
78.499748	2889.522519	21.278656
78.152750	2887.560341	21.283674
78.758871	2880.479794	21.288691
78.800924	2873.220209	21.293709
78.726665	2878.082794	21.298727
78.341852	2881.979459	21.303744
79.147942	2875.637853	21.308762
78.993968	2877.587141	21.313779
79.003734	2867.809416	21.318797
78.756067	2880.677757	21.323815
79.213909	2888.843206	21.328832
79.061871	2903.779921	21.333850
79.102680	2895.955771	21.338867
79.760751	2899.572060	21.343885
79.402749	2895.907152	21.348903
79.639324	2896.416095	21.353920
79.814189	2898.573292	21.358938
79.410210	2895.988589	21.363955
79.814094	2903.858253	21.368973
79.411941	2896.057556	21.373991
79.712610	2899.877934	21.379008
79.762447	2915.115967	21.384026
79.854702	2923.644930	21.389043
80.461606	2915.389900	21.394061
80.288273	2916.049955	21.399079
80.541792	2926.405560	21.404096
80.653286	2926.604882	21.409114
80.723260	2923.579618	21.414131
80.605729	2921.747589	21.419149
80.701321	2928.894029	21.424167
80.814489	2919.210685	21.429184
80.772523	2925.354955	21.434202
80.271903	2929.576076	21.439219
80.765059	2923.433806	21.444237
80.802539	2937.799960	21.449255
80.711461	2942.426133	21.454272
80.964816	2945.682236	21.459290
80.697617	2946.498058	21.464307
81.164733	2944.297484	21.469325
81.143921	2951.458567	21.474343
81.556796	2955.510406	21.479360
81.789935	2977.152597	21.484378
81.622948	2981.668185	21.489395
81.772248	2966.226877	21.494413
81.814912	2973.964627	21.499431
81.830451	2971.360982	21.504448
81.858447	2969.480567	21.509466
82.227394	2971.510073	21.514483
82.563387	2963.461044	21.519501
82.411522	2969.556002	21.524519
82.724524	2959.600857	21.529536
82.602124	2949.221983	21.534554
82.092684	2958.222122	21.539571
82.480403	2950.181368	21.544589
82.356021	2955.052759	21.549607
82.342718	2948.386385	21.554624
82.734556	2948.801349	21.559642
82.494231	2949.309271	21.564659
83.046813	2956.019447	21.569677
82.851660	2962.791461	21.574695
82.795765	2947.174458	21.579712
82.719421	2967.440737	21.584730
82.930845	2982.796225	21.589747
83.319626	2987.846924	21.594765
83.347072	2977.001293	21.599783
83.101727	2985.112982	21.604800
83.314909	2984.334115	21.609818
83.022422	2989.166256	21.614835
83.715012	3001.747095	21.619853
83.840457	3011.431005	21.624871
83.923950	3011.195103	21.629888
84.323643	3011.965133	21.634906
84.054652	3014.260782	21.639923
84.169309	2997.424872	21.644941
84.148835	3000.399021	21.649959
84.076751	3004.410233	21.654976
84.435339	3013.573222	21.659994
84.510811	3008.343883	21.665011
84.503460	2998.781961	21.670029
84.532198	3003.126330	21.675047
84.792262	3001.127095	21.680064
84.743641	2992.859373	21.685082
84.367143	3022.096434	21.690099
84.698338	3016.426730	21.695117
84.709559	3031.389451	21.700135
84.723984	3031.700218	21.705152
85.133344	3027.624220	21.710170
84.850840	3029.571216	21.715187
84.791986	3031.908077	21.720205
84.654895	3049.908610	21.725223
85.317048	3060.854353	21.730240
85.368320	3050.652216	21.735258
85.372062	3064.699808	21.740275
85.564450	3080.735674	21.745293
85.628654	3088.905811	21.750311
85.727004	3101.679046	21.755328
85.838845	3091.561610	21.760346
85.787821	3093.057171	21.765363
85.868537	3092.131099	21.770381
86.103294	3089.288749	21.775399
86.242112	3103.209434	21.780416
86.475984	3113.956874	21.785434
86.516617	3124.773682	21.790451
86.611985	3111.446486	21.795469
86.808740	3124.543846	21.800487
86.430902	3125.183825	21.805504
86.586920	3106.921424	21.810522
86.774195	3107.436665	21.815539
87.070909	3107.478239	21.820557
87.166579	3107.166455	21.825575
87.038240	3110.678541	21.830592
87.417236	3106.078000	21.835610
86.729227	3105.138450	21.840627
87.151870	3110.341108	21.845645
87.104050	3127.802067	21.850663
87.284225	3132.952160	21.855680
87.599203	3131.044046	21.860698
87.528539	3137.800219	21.865715
87.839366	3139.732045	21.870733
87.695659	3139.582717	21.875751
87.939368	3140.328078	21.880768
88.143370	3130.200636	21.885786
88.063688	3155.518313	21.890803
88.423195	3168.205120	21.895821
88.809432	3155.089492	21.900839
88.687401	3158.838916	21.905856
88.631920	3148.714304	21.910874
88.670873	3143.706262	21.915891
88.857407	3155.146391	21.920909
88.683167	3142.467042	21.925927
88.591772	3156.138180	21.930944
88.653883	3152.786120	21.935962
88.744022	3165.755005	21.940979
88.645135	3154.035052	21.945997
89.067591	3148.506485	21.951015
88.940749	3159.545887	21.956032
89.233170	3175.897840	21.961050
89.418259	3177.281028	21.966067
89.543003	3177.013374	21.971085
89.529615	3177.823338	21.976103
89.485311	3175.259092	21.981120
89.693370	3167.560718	21.986138
89.698285	3178.606652	21.991155
89.443309	3189.044328	21.996173
89.877223	3189.432141	22.001191
89.874497	3205.931094	22.006208
89.947499	3200.775232	22.011226
90.294459	3220.231820	22.016243
90.291779	3217.063913	22.021261
90.366855	3206.317490	22.026279
90.214477	3204.602677	22.031296
90.822159	3217.288490	22.036314
90.479228	3240.959510	22.041331
90.790473	3237.368693	22.046349
90.854105	3231.713261	22.051367
90.979758	3241.092885	22.056384
90.982547	3227.190411	22.061402
91.358931	3233.913874	22.066419
91.647396	3219.525361	22.071437
91.327753	3220.156062	22.076455
91.354396	3227.675472	22.081472
91.695799	3218.814476	22.086490
91.609460	3217.472194	22.091507
91.729455	3224.404084	22.096525
91.765441	3226.341999	22.101543
91.719859	3218.363126	22.106560
91.762354	3215.338251	22.111578
91.475330	3231.460181	22.116595
91.851434	3249.633966	22.121613
91.910785	3256.590488	22.126631
91.851791	3249.336606	22.131648
91.989421	3247.919272	22.136666
91.893762	3277.845935	22.141683
92.133732	3289.169099	22.146701
92.857220	3281.955590	22.151719
92.576685	3293.141525	22.156736
92.748686	3276.393685	22.161754
92.861453	3280.804967	22.166771
92.842418	3276.696541	22.171789
93.222183	3290.555382	22.176807
93.196944	3308.094760	22.181824
93.335740	3296.339932	22.186842
93.512926	3295.009889	22.191859
93.701965	3302.665475	22.196877
94.069597	3296.941084	22.201895
93.891271	3305.140584	22.206912
93.911572	3303.898487	22.211930
93.992146	3299.520101	22.216947
93.914970	3295.316327	22.221965
94.239925	3288.115247	22.226983
93.959003	3304.781388	22.232000
93.954617	3289.501115	22.237018
93.856175	3288.123786	22.242035
94.062595	3286.593222	22.247053
94.295009	3303.245925	22.252071
94.051649	3329.142189	22.257088
94.369786	3328.595915	22.262106
94.945237	3335.028104	22.267123
94.871423	3323.279631	22.272141
94.545707	3319.627556	22.277159
94.337889	3339.439434	22.282176
94.857267	3331.618958	22.287194
94.956957	3342.373809	22.292211
95.050932	3358.111828	22.297229
94.907405	3344.203473	22.302247
95.382860	3355.167418	22.307264
95.780882	3365.873134	22.312282
95.855997	3366.093998	22.317299
95.900671	3376.916642	22.322317
96.306275	3358.988538	22.327335
95.873004	3354.162712	22.332352
95.944004	3341.020107	22.337370
96.349774	3355.911585	22.342387
96.261505	3367.288731	22.347405
96.645674	3356.116128	22.352423
96.283729	3357.130356	22.357440
96.633404	3357.802196	22.362458
96.516192	3360.363155	22.367475
96.513143	3371.227229	22.372493
96.696898	3363.624660	22.377511
96.661188	3367.633318	22.382528
96.852980	3367.450145	22.387546
97.212867	3361.225908	22.392563
96.964767	3358.775149	22.397581
96.905702	3361.423586	22.402599
97.332478	3377.563198	22.407616
97.187162	3388.408285	22.412634
97.217368	3394.207728	22.417651
97.601145	3405.681098	22.422669
97.709097	3402.696088	22.427687
97.511563	3402.019672	22.432704
97.414548	3399.699770	22.437722
97.934262	3406.086605	22.442739
97.763365	3421.394194	22.447757
98.064040	3414.248053	22.452775
97.949126	3428.024667	22.457792
98.335316	3415.022084	22.462810
98.309591	3421.049130	22.467827
98.158586	3428.265034	22.472845
98.582708	3442.308088	22.477863
98.454765	3447.650592	22.482880
98.382314	3449.758430	22.487898
98.421284	3444.728258	22.492915
98.603926	3448.614016	22.497933
98.687054	3466.093826	22.502951
98.716104	3479.768868	22.507968
98.881068	3476.145475	22.512986
99.008928	3489.542833	22.518003
99.246693	3504.226064	22.523021
99.701720	3495.946955	22.528039
99.556649	3510.092648	22.533056
99.850127	3511.407455	22.538074
99.992075	3491.212578	22.543091
99.977347	3498.949533	22.548109
100.150893	3485.999679	22.553127
99.903323	3490.086993	22.558144
100.037131	3514.072575	22.563162
100.497962	3520.275350	22.568179
100.665160	3515.718686	22.573197
100.885322	3510.533740	22.578215
100.819662	3520.721212	22.583232
100.962244	3511.817022	22.588250
101.228343	3505.623414	22.593267
100.834366	3512.280296	22.598285
100.941119	3504.991200	22.603303
101.237473	3517.877170	22.608320
101.110215	3511.154771	22.613338
101.319289	3498.272393	22.618355
100.956249	3507.049721	22.623373
101.302386	3504.526979	22.628391
101.348609	3520.355381	22.633408
101.255075	3525.005727	22.638426
101.805493	3531.442785	22.643443
101.877289	3542.822071	22.648461
102.016789	3541.037856	22.653479
102.181459	3546.440708	22.658496
102.281269	3545.996894	22.663514
102.282511	3533.212131	22.668531
102.031205	3535.604936	22.673549
102.466395	3556.170379	22.678567
102.414311	3565.386627	22.683584
102.293295	3568.804049	22.688602
102.709769	3566.282666	22.693619
102.774719	3567.213093	22.698637
102.636751	3569.365220	22.703655
102.955110	3583.214469	22.708672
103.052161	3596.752134	22.713690
103.505497	3586.155131	22.718707
103.013732	3603.774772	22.723725
103.242540	3594.067819	22.728743
103.394670	3598.874087	22.733760
102.988485	3619.117572	22.738778
103.555502	3621.239083	22.743795
103.574776	3626.455130	22.748813
103.803296	3625.761098	22.753831
104.178788	3638.794234	22.758848
104.024570	3644.742752	22.763866
104.319794	3644.652420	22.768883
104.223125	3647.925962	22.773901
104.483340	3640.859319	22.778919
104.509335	3648.141495	22.783936
104.277258	3648.338986	22.788954
104.764680	3648.575121	22.793971
104.966837	3671.904260	22.798989
105.051988	3671.626393	22.804007
105.142345	3665.910683	22.809024
104.922325	3674.788798	22.814042
105.504555	3677.147020	22.819059
105.208818	3689.276460	22.824077
105.532731	3680.021528	22.829095
105.728370	3680.155528	22.834112
105.722277	3705.432530	22.839130
105.930855	3706.785280	22.844147
105.927704	3717.806163	22.849165
105.907618	3703.037683	22.854183
106.167685	3710.899261	22.859200
106.138775	3709.499791	22.864218
106.592424	3702.120665	22.869235
106.153012	3712.670719	22.874253
106.326820	3704.234184	22.879271
106.484570	3699.305333	22.884288
106.271805	3705.761134	22.889306
106.418375	3722.671856	22.894323
106.773547	3727.306556	22.899341
106.608532	3727.560215	22.904359
106.764128	3729.569582	22.909376
107.256562	3749.175159	22.914394
107.310978	3748.919499	22.919411
107.438516	3765.269306	22.924429
107.537612	3751.214104	22.929447
107.762307	3750.202888	22.934464
107.490644	3749.122947	22.939482
107.913581	3744.184040	22.944499
107.889082	3753.251271	22.949517
108.220743	3764.115749	22.954535
108.262992	3772.495863	22.959552
108.421344	3789.932599	22.964570
109.076307	3777.661646	22.969587
108.969212	3774.676245	22.974605
109.014389	3776.171479	22.979623
109.200489	3761.366912	22.984640
108.696276	3751.263886	22.989658
109.358081	3764.152362	22.994675
108.944024	3773.021363	22.999693
109.299732	3771.953854	23.004711
109.174299	3771.029938	23.009728
109.094543	3774.395991	23.014746
109.460386	3765.322319	23.019763
109.327958	3767.645859	23.024781
109.580379	3771.179187	23.029799
109.970547	3779.151418	23.034816
109.872430	3788.287048	23.039834
110.176900	3797.481978	23.044851
110.186003	3803.410807	23.049869
110.024378	3797.296301	23.054887
109.810681	3803.931642	23.059904
109.811287	3803.133933	23.064922
110.234486	3805.159631	23.069939
110.416220	3812.897673	23.074957
110.226287	3819.050970	23.079975
110.712139	3821.699115	23.084992
110.548922	3832.695268	23.090010
110.725142	3846.339318	23.095027
110.822416	3850.974283	23.100045
110.902193	3845.370317	23.105063
111.010791	3864.696659	23.110080
111.017082	3881.010869	23.115098
111.326726	3867.672411	23.120115
111.529637	3877.625366	23.125133
111.351360	3889.389341	23.130151
111.775749	3900.645027	23.135168
112.103880	3911.973495	23.140186
112.436584	3904.124281	23.145203
112.271275	3903.588225	23.150221
112.479356	3903.260072	23.155239
112.830853	3903.688586	23.160256
112.502202	3906.863096	23.165274
112.609174	3901.705503	23.170291
112.604935	3902.125459	23.175309
112.464058	3898.870104	23.180327
113.155834	3909.252487	23.185344
112.981527	3916.223775	23.190362
113.110060	3922.498597	23.195379
113.362506	3927.230767	23.200397
113.283188	3917.678933	23.205415
113.466266	3923.387345	23.210432
113.219978	3932.842462	23.215450
113.653586	3932.590043	23.220467
113.967184	3962.269558	23.225485
113.601364	3964.181188	23.230503
113.895556	3947.313195	23.235520
114.092931	3949.735986	23.240538
114.053199	3947.580703	23.245555
114.325896	3969.407637	23.250573
114.388176	3975.616745	23.255591
115.043232	3982.849900	23.260608
114.785408	3976.704250	23.265626
114.698957	3986.535089	23.270643
114.770195	3977.947203	23.275661
114.857786	3978.881913	23.280679
115.256303	4012.204991	23.285696
115.118857	4012.322891	23.290714
115.140399	4007.980455	23.295731
115.447053	4010.210411	23.300749
115.628921	4012.856727	23.305767
115.563304	4026.645706	23.310784
115.625844	4026.337615	23.315802
115.807119	4028.656792	23.320819
115.912191	4026.382437	23.325837
115.833139	4044.602270	23.330855
116.149052	4053.632706	23.335872
116.273540	4055.016207	23.340890
116.400730	4059.658267	23.345907
116.579846	4064.025382	23.350925
116.582176	4064.291689	23.355943
116.790385	4071.132039	23.360960
117.454624	4090.196225	23.365978
117.076930	4083.131986	23.370995
117.482643	4083.513316	23.376013
117.418303	4083.113756	23.381031
117.564596	4072.288478	23.386048
117.454137	4073.165103	23.391066
117.632126	4085.367207	23.396083
117.974638	4085.955273	23.401101
117.900966	4105.821522	23.406119
118.483901	4103.526013	23.411136
117.974154	4116.453749	23.416154
118.284613	4106.803448	23.421171
118.900645	4104.591550	23.426189
118.491081	4106.606142	23.431207
118.659171	4108.084956	23.436224
118.961648	4101.956881	23.441242
118.649365	4102.357531	23.446259
118.864772	4104.422703	23.451277
118.882082	4101.592813	23.456295
119.118798	4099.548388	23.461312
118.923532	4107.635401	23.466330
119.002220	4130.640420	23.471347
119.460925	4141.394457	23.476365
119.365878	4134.841266	23.481383
119.450915	4133.526632	23.486400
119.457182	4154.779614	23.491418
119.358316	4157.688622	23.496435
119.479300	4157.036103	23.501453
119.741824	4174.693462	23.506471
120.042664	4193.100687	23.511488
120.046250	4203.714959	23.516506
120.287137	4213.729738	23.521523
121.107516	4209.412457	23.526541
120.954236	4231.060710	23.531559
120.998508	4226.583216	23.536576
121.493484	4222.819697	23.541594
121.349256	4217.276484	23.546611
121.611543	4227.948634	23.551629
121.307666	4225.405144	23.556647
121.710984	4225.758542	23.561664
121.556863	4222.953607	23.566682
121.811756	4221.552094	23.571699
121.668322	4213.580415	23.576717
121.741634	4239.833689	23.581735
122.053438	4236.735765	23.586752
122.223126	4241.925685	23.591770
122.457777	4239.342725	23.596787
122.161706	4237.219625	23.601805
122.475544	4251.869454	23.606823
122.520110	4256.746585	23.611840
122.669320	4263.561822	23.616858
122.605033	4274.104372	23.621875
123.056386	4254.364911	23.626893
122.941104	4269.891065	23.631911
123.227135	4289.922033	23.636928
123.414608	4295.117789	23.641946
123.490485	4302.784869	23.646963
123.461465	4297.872230	23.651981
123.434918	4305.137940	23.656999
123.863987	4317.939737	23.662016
123.978668	4331.745089	23.667034
123.790656	4332.505873	23.672051
124.513250	4333.042779	23.677069
124.244810	4331.925305	23.682087
124.386220	4328.509986	23.687104
124.669611	4345.194297	23.692122
124.753153	4346.150129	23.697139
125.007244	4354.548712	23.702157
125.038339	4359.011892	23.707175
125.280387	4347.681064	23.712192
125.556172	4355.065354	23.717210
125.205551	4351.048836	23.722227
125.321355	4357.027738	23.727245
125.404472	4353.727120	23.732263
125.279173	4353.801393	23.737280
125.762033	4373.320448	23.742298
125.416341	4377.761910	23.747315
125.740853	4384.826933	23.752333
125.855805	4415.375248	23.757351
125.794809	4408.678054	23.762368
126.119076	4408.764805	23.767386
126.119895	4421.122094	23.772403
126.822963	4431.660383	23.777421
126.804289	4450.274641	23.782439
126.590170	4444.030572	23.787456
126.947064	4437.564076	23.792474
126.822204	4440.646414	23.797491
127.379976	4455.709870	23.802509
127.418732	4466.943321	23.807527
127.660562	4468.200378	23.812544
127.664075	4469.124929	23.817562
127.431165	4471.746222	23.822579
127.913321	4460.491081	23.827597
127.854089	4498.902358	23.832615
127.954414	4502.610371	23.837632
128.286173	4499.928495	23.842650
128.569119	4492.798036	23.847667
128.935614	4487.721570	23.852685
128.590796	4496.952047	23.857703
128.774455	4495.687732	23.862720
129.130618	4507.491264	23.867738
128.867383	4516.851913	23.872755
129.112080	4522.345418	23.877773
129.408196	4506.288302	23.882791
129.189661	4515.305136	23.887808
129.435572	4531.211345	23.892826
129.358111	4551.908719	23.897843
129.614425	4548.379055	23.902861
129.648347	4554.686543	23.907879
129.745664	4555.602434	23.912896
130.099758	4569.319485	23.917914
130.027609	4584.419807	23.922931
130.652107	4576.816341	23.927949
130.776141	4583.810380	23.932967
130.645887	4590.159011	23.937984
131.008921	4606.262168	23.943002
130.955481	4615.067084	23.948019
131.154778	4604.815875	23.953037
131.060928	4603.788535	23.958055
130.803749	4610.092909	23.963072
131.235012	4602.456526	23.968090
131.250141	4620.085436	23.973107
131.445256	4627.199532	23.978125
131.698173	4636.172724	23.983143
131.683369	4628.093774	23.988160
132.202139	4636.124637	23.993178
131.993728	4656.748642	23.998195
132.452919	4660.711771	24.003213
132.184199	4662.444377	24.008231
132.423792	4663.428839	24.013248
132.883552	4655.506260	24.018266
132.347829	4668.498405	24.023283
132.616769	4665.449708	24.028301
133.030765	4675.408094	24.033319
133.153139	4678.796399	24.038336
133.311940	4684.575061	24.043354
133.215641	4697.056627	24.048371
133.558516	4702.058615	24.053389
133.681571	4714.216512	24.058407
133.609116	4718.749807	24.063424
134.087197	4713.703457	24.068442
133.961864	4730.968649	24.073459
134.362632	4742.598486	24.078477
134.564260	4736.175501	24.083495
134.363298	4743.057030	24.088512
134.582965	4732.581431	24.093530
134.625129	4752.131938	24.098547
134.899114	4768.400513	24.103565
135.102306	4768.186404	24.108583
134.959894	4765.993881	24.113600
135.180983	4765.617226	24.118618
135.380039	4780.246556	24.123635
135.556881	4790.551211	24.128653
135.925179	4799.924610	24.133671
135.829288	4803.209297	24.138688
135.911551	4799.987382	24.143706
135.665014	4814.656337	24.148723
136.177504	4826.101653	24.153741
135.993682	4840.089605	24.158759
135.945582	4843.252612	24.163776
136.633475	4846.236108	24.168794
136.546556	4862.879368	24.173811
136.842580	4870.267772	24.178829
137.121733	4875.039260	24.183847
137.451881	4890.762507	24.188864
137.109692	4891.074328	24.193882
137.150294	4898.290290	24.198899
137.633076	4893.494078	24.203917
137.748503	4892.710253	24.208935
137.539286	4916.992769	24.213952
137.926107	4906.888448	24.218970
138.233419	4915.557350	24.223987
138.357186	4908.265634	24.229005
138.674077	4912.223991	24.234023
138.656016	4922.556673	24.239040
139.125361	4927.099608	24.244058
139.168926	4944.531638	24.249075
139.371636	4934.029494	24.254093
139.320819	4915.575985	24.259111
139.021836	4926.381416	24.264128
139.821070	4921.201970	24.269146
139.567941	4926.244010	24.274163
139.662203	4928.125658	24.279181
139.884340	4937.200705	24.284199
139.830322	4933.398688	24.289216
140.177904	4923.944111	24.294234
140.270556	4924.588580	24.299251
140.216392	4922.232494	24.304269
140.394943	4943.437118	24.309287
140.315420	4956.223818	24.314304
140.686924	4949.733531	24.319322
140.881110	4954.601196	24.324339
140.593833	4962.369798	24.329357
140.786283	4967.416319	24.334375
140.574746	4985.405136	24.339392
141.082290	4985.993675	24.344410
141.093822	5001.724582	24.349427
141.090442	5019.219254	24.354445
141.198399	5032.210554	24.359463
141.331266	5039.315897	24.364480
141.823197	5045.186328	24.369498
142.035878	5064.918529	24.374515
141.848664	5079.133812	24.379533
142.363878	5077.910980	24.384551
142.462336	5085.691298	24.389568
142.668984	5099.861889	24.394586
143.121142	5108.413406	24.399603
143.103050	5113.892399	24.404621
143.583968	5102.150014	24.409639
143.788636	5105.846262	24.414656
143.870843	5096.590442	24.419674
144.087172	5098.547836	24.424691
143.904842	5095.556854	24.429709
144.351188	5100.667562	24.434727
144.197877	5116.198314	24.439744
144.131745	5108.692122	24.444762
144.186847	5120.899740	24.449779
144.329092	5126.053444	24.454797
144.448731	5117.671940	24.459815
144.227657	5136.623001	24.464832
144.578511	5145.510088	24.469850
144.936546	5143.516978	24.474867
145.212691	5166.351318	24.479885
145.470656	5167.719149	24.484903
145.187263	5186.741573	24.489920
145.115374	5179.380227	24.494938
145.562608	5185.601625	24.499955
145.448794	5209.904811	24.504973
145.974325	5209.002080	24.509991
146.019435	5213.069155	24.515008
146.400660	5229.860810	24.520026
146.493694	5228.709223	24.525043
146.579687	5235.774935	24.530061
147.003373	5220.093192	24.535079
146.983676	5224.325582	24.540096
147.070358	5229.123159	24.545114
147.329111	5223.176241	24.550131
147.406028	5230.514805	24.555149
147.489435	5223.120020	24.560167
147.397989	5261.317365	24.565184
147.703668	5257.791463	24.570202
147.968208	5246.754515	24.575219
147.569561	5254.144538	24.580237
148.075936	5254.095271	24.585255
148.322900	5284.393844	24.590272
148.465307	5278.280583	24.595290
148.714989	5281.179860	24.600307
148.477258	5278.796346	24.605325
148.708516	5304.708515	24.610343
149.055549	5310.825581	24.615360
149.060081	5310.206531	24.620378
149.166865	5316.408324	24.625395
149.153409	5332.015338	24.630413
149.581578	5332.836826	24.635431
149.650841	5343.196786	24.640448
149.563574	5335.850401	24.645466
149.890356	5360.399828	24.650483
150.046533	5364.060606	24.655501
150.364668	5378.432390	24.660519
150.535278	5378.607378	24.665536
150.759717	5392.800589	24.670554
151.184971	5378.440082	24.675571
150.930855	5405.775864	24.680589
151.389398	5397.345667	24.685607
151.372171	5397.836180	24.690624
151.674769	5395.315350	24.695642
151.572025	5396.712400	24.700659
151.757685	5410.846517	24.705677
151.661698	5413.033123	24.710695
151.766224	5427.560168	24.715712
151.674512	5446.551575	24.720730
152.407979	5418.598844	24.725747
152.248102	5453.867707	24.730765
152.475649	5454.779409	24.735783
152.586090	5459.120133	24.740800
152.823753	5472.890429	24.745818
152.939463	5482.727791	24.750835
153.187164	5482.513658	24.755853
153.607371	5480.714347	24.760871
153.643114	5491.624941	24.765888
153.415107	5510.030042	24.770906
154.057034	5508.051406	24.775923
154.008604	5512.928836	24.780941
153.844803	5505.124909	24.785959
154.099871	5517.034277	24.790976
154.379251	5530.097807	24.795994
154.466132	5538.276710	24.801011
154.573242	5546.441378	24.806029
154.922272	5537.304010	24.811047
154.795062	5536.551763	24.816064
154.745651	5552.719371	24.821082
155.073077	5550.580829	24.826099
154.914895	5575.923850	24.831117
154.924044	5570.760820	24.836135
155.372805	5586.976474	24.841152
155.544851	5593.562906	24.846170
156.051316	5611.807747	24.851187
155.762057	5632.330360	24.856205
156.077200	5626.750337	24.861223
156.367294	5630.938951	24.866240
156.501402	5647.217433	24.871258
157.176506	5650.138633	24.876275
157.134495	5655.092185	24.881293
157.206683	5656.126226	24.886311
157.476186	5658.430811	24.891328
157.418729	5652.473567	24.896346
157.761583	5658.832180	24.901363
157.482041	5670.755330	24.906381
157.824911	5677.088774	24.911399
158.054339	5671.490146	24.916416
158.236120	5693.968239	24.921434
158.459860	5694.537558	24.926451
158.467987	5698.275524	24.931469
158.858880	5705.377809	24.936487
158.707899	5706.324712	24.941504
159.048166	5714.157277	24.946522
159.256484	5724.614913	24.951539
159.162560	5734.695925	24.956557
159.488868	5726.917574	24.961575
159.518954	5729.246187	24.966592
159.347726	5748.614124	24.971610
159.829327	5750.633941	24.976627
159.838339	5761.610362	24.981645
159.972232	5767.192024	24.986663
160.285206	5782.068526	24.991680
160.512125	5792.531898	24.996698
160.922774	5779.515474	25.001715
160.891188	5801.758696	25.006733
161.244828	5808.945644	25.011751
161.320087	5805.330481	25.016768
161.469568	5813.030671	25.021786
161.654596	5808.538906	25.026803
161.631242	5824.437532	25.031821
161.986250	5829.554411	25.036839
162.227238	5837.087398	25.041856
162.132729	5837.023022	25.046874
162.616896	5836.395914	25.051891
162.562114	5836.187527	25.056909
162.704613	5836.086145	25.061927
163.065989	5848.716776	25.066944
163.080757	5874.255374	25.071962
163.342309	5864.115308	25.076979
163.547504	5864.610493	25.081997
163.506571	5860.574853	25.087015
163.457111	5868.232841	25.092032
163.334299	5865.706603	25.097050
163.791994	5861.078511	25.102067
163.636630	5882.138693	25.107085
164.036059	5894.714519	25.112103
164.157162	5889.043397	25.117120
163.817528	5912.336618	25.122138
164.454562	5910.498751	25.127155
164.239615	5925.018224	25.132173
164.495040	5944.999691	25.137191
164.580905	5952.278184	25.142208
164.832153	5979.813734	25.147226
165.121483	5981.514149	25.152243
165.262929	6002.620796	25.157261
165.460986	6015.161962	25.162279
165.923931	6016.071570	25.167296
165.801703	6021.234718	25.172314
166.224987	6031.991869	25.177331
166.599023	6043.839426	25.182349
166.787424	6034.246672	25.187367
166.740755	6038.900564	25.192384
166.828810	6053.892665	25.197402
167.445748	6055.563667	25.202419
167.141909	6062.601462	25.207437
167.525843	6064.356035	25.212455
167.793617	6070.539558	25.217472
167.816611	6087.293337	25.222490
168.230591	6090.098133	25.227507
168.263886	6103.499585	25.232525
168.136664	6105.197203	25.237543
168.522195	6098.409944	25.242560
168.464023	6110.687582	25.247578
169.035851	6118.215165	25.252595
168.995731	6120.298558	25.257613
169.220335	6119.587738	25.262631
169.586846	6112.210306	25.267648
169.511966	6139.997200	25.272666
169.910379	6141.884794	25.277683
169.779512	6144.200586	25.282701
169.820055	6142.945582	25.287719
170.176895	6144.096338	25.292736
170.083936	6167.409632	25.297754
170.648767	6165.942002	25.302771
170.950080	6174.017048	25.307789
170.656036	6178.457098	25.312807
171.026040	6178.048800	25.317824
170.940134	6198.028391	25.322842
171.357549	6202.997772	25.327859
171.354570	6205.181465	25.332877
171.357646	6198.190798	25.337895
171.603840	6226.052537	25.342912
171.796618	6236.801751	25.347930
171.785152	6229.785065	25.352947
172.081154	6238.558047	25.357965
172.510244	6262.609609	25.362983
172.495728	6252.859465	25.368000
172.607488	6265.033821	25.373018
173.091614	6263.304478	25.378035
173.218589	6273.260158	25.383053
173.309583	6280.132036	25.388071
173.731765	6297.499002	25.393088
173.150477	6305.739240	25.398106
173.419256	6300.613231	25.403123
173.722735	6311.543895	25.408141
173.466149	6326.626630	25.413159
174.364497	6330.926162	25.418176
174.418243	6350.113465	25.423194
174.397281	6340.324954	25.428211
174.675567	6347.760207	25.433229
174.803495	6362.403242	25.438247
174.957996	6372.326277	25.443264
175.280209	6386.744818	25.448282
175.411900	6390.784251	25.453299
175.784295	6402.707100	25.458317
175.434869	6407.701267	25.463335
175.901530	6421.419416	25.468352
175.825655	6436.002970	25.473370
175.746456	6440.913935	25.478387
176.270104	6457.760603	25.483405
176.347157	6466.146932	25.488423
176.762152	6463.779517	25.493440
176.814229	6484.270912	25.498458
177.229397	6490.224194	25.503475
177.946537	6482.322554	25.508493
177.816334	6481.168701	25.513511
177.983174	6492.012714	25.518528
178.330307	6511.581441	25.523546
178.166798	6515.542097	25.528563
178.212917	6515.648049	25.533581
178.542567	6512.681352	25.538599
178.884362	6518.280503	25.543616
179.181321	6540.336342	25.548634
179.178959	6547.712593	25.553651
179.815673	6534.218094	25.558669
179.668722	6549.857121	25.563687
179.737468	6536.516121	25.568704
179.698236	6533.571260	25.573722
180.193308	6526.328117	25.578739
180.367738	6553.866760	25.583757
180.355069	6551.121430	25.588775
180.813942	6547.252165	25.593792
180.720265	6561.839468	25.598810
180.517369	6566.641169	25.603827
181.171164	6573.849871	25.608845
181.236864	6582.284495	25.613863
181.328347	6582.295097	25.618880
181.339782	6598.182714	25.623898
181.514213	6598.759147	25.628915
181.447176	6606.074931	25.633933
181.572881	6611.839963	25.638951
181.882541	6617.113049	25.643968
181.792209	6641.340101	25.648986
181.936115	6651.396403	25.654003
182.305509	6669.121549	25.659021
182.278528	6679.481273	25.664039
182.715722	6685.179358	25.669056
182.941912	6702.938393	25.674074
183.113332	6721.562972	25.679092
183.475370	6725.924536	25.684109
183.600795	6750.502095	25.689127
184.068863	6751.103311	25.694144
184.223860	6754.165108	25.699162
184.198692	6764.227989	25.704180
184.676305	6766.305239	25.709197
184.491659	6780.216477	25.714215
184.898257	6786.934416	25.719232
184.673252	6799.485485	25.724250
184.890915	6806.880284	25.729268
185.235493	6802.160581	25.734285
185.506599	6826.638722	25.739303
185.537122	6834.444172	25.744320
186.063066	6842.969996	25.749338
186.121449	6842.884383	25.754356
186.405181	6858.041221	25.759373
186.539494	6860.578412	25.764391
186.724013	6866.716538	25.769408
186.627557	6872.026146	25.774426
187.253016	6886.670623	25.779444
187.387681	6887.450103	25.784461
187.255467	6889.327990	25.789479
187.891083	6902.072371	25.794496
188.130343	6906.171112	25.799514
187.783819	6916.522942	25.804532
188.496433	6902.085252	25.809549
188.472674	6927.172332	25.814567
188.518676	6939.717288	25.819584
188.964778	6942.984479	25.824602
188.992114	6939.685099	25.829620
189.276964	6949.482312	25.834637
189.006201	6972.516804	25.839655
189.339847	6970.891630	25.844672
189.658943	6975.380493	25.849690
189.648187	6997.927464	25.854708
190.132678	6990.838421	25.859725
190.073606	7003.241254	25.864743
190.326226	7020.199445	25.869760
190.711251	7027.762006	25.874778
190.801652	7038.002556	25.879796
190.981660	7043.630852	25.884813
191.150717	7060.948599	25.889831
191.232468	7061.007175	25.894848
191.399573	7064.122968	25.899866
191.330518	7067.134794	25.904884
191.532135	7089.053230	25.909901
191.691161	7084.798905	25.914919
191.742039	7098.537561	25.919936
192.380757	7117.647538	25.924954
192.466627	7124.948640	25.929972
192.771302	7137.815229	25.934989
192.789174	7157.437312	25.940007
192.863617	7148.957225	25.945024
193.349137	7168.521282	25.950042
193.341848	7177.234605	25.955060
193.748930	7189.390961	25.960077
194.037033	7196.726731	25.965095
193.768203	7211.914598	25.970112
194.283324	7211.150329	25.975130
194.267911	7219.914540	25.980148
194.796228	7229.803728	25.985165
195.194894	7237.557774	25.990183
195.472952	7244.182333	25.995200
195.715856	7232.975841	26.000218
195.577287	7261.631026	26.005236
196.052266	7272.666456	26.010253
196.004864	7269.833688	26.015271
196.286526	7264.872098	26.020288
196.427244	7262.623039	26.025306
196.507017	7282.844400	26.030324
196.615749	7288.608468	26.035341
196.608627	7308.100193	26.040359
197.009970	7317.935726	26.045376
197.352956	7325.483114	26.050394
197.117736	7330.187929	26.055412
197.417405	7338.398421	26.060429
197.984635	7350.639529	26.065447
198.075209	7364.304437	26.070464
198.578784	7361.446748	26.075482
198.699444	7369.978490	26.080500
199.083611	7364.169660	26.085517
199.006055	7369.024020	26.090535
199.130545	7371.753272	26.095552
199.531079	7371.794068	26.100570
199.356893	7405.376660	26.105588
199.728670	7392.601071	26.110605
199.896069	7395.288080	26.115623
199.877980	7413.010596	26.120640
200.150985	7422.403233	26.125658
200.317273	7423.097447	26.130676
200.543530	7434.675423	26.135693
200.956519	7458.756682	26.140711
201.097047	7460.481001	26.145728
201.334819	7453.387018	26.150746
201.218006	7483.395617	26.155764
201.666025	7487.502152	26.160781
202.221018	7481.536217	26.165799
201.591457	7490.398507	26.170816
202.047597	7498.138807	26.175834
202.004384	7517.152674	26.180852
202.433385	7523.109681	26.185869
202.318595	7536.565940	26.190887
202.550388	7547.116333	26.195904
203.099244	7549.230337	26.200922
203.060361	7567.811617	26.205940
203.348044	7579.493214	26.210957
203.714044	7574.262361	26.215975
203.611379	7597.540896	26.220992
204.132532	7610.988673	26.226010
203.993096	7616.428141	26.231028
204.600191	7628.380657	26.236045
204.777105	7633.823197	26.241063
204.993529	7641.923601	26.246080
205.717625	7642.106370	26.251098
205.639218	7648.242681	26.256116
205.838653	7658.793592	26.261133
206.303941	7657.600566	26.266151
206.106914	7663.256166	26.271168
206.511091	7657.811477	26.276186
206.404921	7680.267689	26.281204
206.551515	7688.747484	26.286221
206.561374	7694.771388	26.291239
206.719504	7705.387142	26.296256
207.225836	7698.402081	26.301274
207.004755	7723.339425	26.306292
207.259415	7751.969841	26.311309
207.357516	7746.884715	26.316327
207.655911	7761.966969	26.321344
207.855177	7778.908572	26.326362
208.163328	7796.372595	26.331380
208.592939	7805.114982	26.336397
208.906624	7821.552920	26.341415
208.850007	7822.868878	26.346432
209.363498	7825.890266	26.351450
209.234186	7850.308835	26.356468
209.351865	7873.182074	26.361485
209.947947	7878.566529	26.366503
209.567144	7888.053474	26.371520
210.352796	7894.308631	26.376538
210.370671	7902.899556	26.381556
210.794443	7919.275202	26.386573
210.879831	7939.585473	26.391591
210.670669	7940.324622	26.396608
211.600426	7936.661619	26.401626
211.927900	7956.738182	26.406644
211.931133	7955.639260	26.411661
212.412433	7949.833604	26.416679
212.430870	7962.477452	26.421696
212.817219	7966.909476	26.426714
212.901789	7982.332911	26.431732
213.092541	7976.634154	26.436749
213.357431	7982.429461	26.441767
213.273968	7977.831143	26.446784
213.771357	7989.338786	26.451802
213.828425	8007.201887	26.456820
213.725371	8005.314186	26.461837
214.349908	8014.204232	26.466855
214.163267	8020.043217	26.471872
214.048342	8030.011895	26.476890
214.413864	8041.488672	26.481908
214.568977	8051.787273	26.486925
214.925265	8061.318900	26.491943
215.107888	8070.393527	26.496960
215.341288	8080.996763	26.501978
215.340670	8101.671112	26.506996
215.617706	8119.719986	26.512013
215.857417	8129.344993	26.517031
216.145264	8131.014430	26.522048
216.615578	8144.331529	26.527066
216.540108	8159.494252	26.532084
216.577716	8172.516842	26.537101
217.161211	8182.312897	26.542119
217.022550	8196.365264	26.547136
217.444249	8195.072925	26.552154
217.355235	8224.626935	26.557172
217.449477	8238.886133	26.562189
218.294998	8250.134684	26.567207
218.419868	8257.221610	26.572224
218.964984	8279.818026	26.577242
219.014299	8292.267600	26.582260
219.059543	8296.172624	26.587277
219.448394	8299.296604	26.592295
219.616158	8316.183255	26.597312
219.847773	8304.984055	26.602330
220.151524	8321.803395	26.607348
220.224909	8344.374400	26.612365
220.538362	8337.912367	26.617383
220.623045	8348.269614	26.622400
220.936035	8359.676328	26.627418
220.960377	8368.279080	26.632436
221.248959	8379.887202	26.637453
222.016909	8386.101332	26.642471
222.224733	8397.468188	26.647488
222.244921	8400.104887	26.652506
222.442785	8397.138378	26.657524
222.534850	8414.702891	26.662541
222.820797	8421.726446	26.667559
223.033565	8425.604797	26.672576
223.087586	8434.604940	26.677594
223.295223	8457.291626	26.682612
223.476410	8466.109422	26.687629
223.632607	8478.460278	26.692647
223.455167	8493.633302	26.697664
223.962610	8516.943475	26.702682
224.183019	8521.508350	26.707700
224.443958	8528.421061	26.712717
224.924261	8546.267692	26.717735
224.842363	8565.032545	26.722752
224.965485	8558.839969	26.727770
225.137791	8578.664349	26.732788
225.576295	8596.090435	26.737805
226.231806	8602.277733	26.742823
226.095238	8614.371646	26.747840
226.419981	8619.026145	26.752858
226.593404	8613.865767	26.757876
226.612196	8634.557432	26.762893
226.942089	8643.673454	26.767911
226.898137	8656.440360	26.772928
227.122372	8668.701840	26.777946
227.420477	8675.713349	26.782964
227.646968	8694.367822	26.787981
227.931473	8703.593411	26.792999
228.394283	8725.895174	26.798016
228.170767	8732.400502	26.803034
228.777197	8735.727524	26.808052
229.121544	8764.639883	26.813069
229.364137	8776.067583	26.818087
229.300829	8776.471914	26.823104
229.700416	8787.899775	26.828122
230.027444	8780.524971	26.833140
230.198160	8808.899332	26.838157
230.593648	8814.282281	26.843175
230.403620	8823.991201	26.848192
231.035241	8841.890391	26.853210
231.496655	8841.801892	26.858228
231.145725	8848.844563	26.863245
231.270852	8869.050619	26.868263
231.727495	8883.548526	26.873280
231.896849	8900.504045	26.878298
232.203689	8906.557421	26.883316
232.405769	8919.297917	26.888333
233.043726	8931.291427	26.893351
233.140298	8942.039059	26.898368
232.983806	8946.298252	26.903386
233.552308	8966.664707	26.908404
233.535742	8975.945152	26.913421
233.820884	8983.001365	26.918439
234.308408	9008.353524	26.923456
234.366178	9006.777238	26.928474
234.591309	9023.832989	26.933492
234.421803	9046.582272	26.938509
234.961657	9051.507928	26.943527
235.094581	9075.846168	26.948544
235.378096	9080.466862	26.953562
235.895310	9096.403203	26.958580
235.996966	9104.358244	26.963597
236.421823	9106.958882	26.968615
236.404305	9128.718147	26.973632
236.728161	9131.077576	26.978650
237.465700	9144.271924	26.983668
237.396967	9157.794694	26.988685
237.418609	9150.875222	26.993703
237.760107	9144.902938	26.998720
237.543093	9168.507467	27.003738
238.156782	9162.131778	27.008756
238.386105	9181.430878	27.013773
238.667075	9177.656201	27.018791
238.643840	9199.493597	27.023808
239.108977	9204.841191	27.028826
239.222928	9208.885800	27.033844
239.260978	9226.154955	27.038861
239.561383	9238.306399	27.043879
240.121219	9247.323970	27.048896
239.897364	9261.667908	27.053914
240.570725	9259.317114	27.058932
240.338879	9271.053361	27.063949
240.952715	9287.772817	27.068967
240.950936	9296.719818	27.073984
241.185045	9306.322874	27.079002
241.586625	9322.146086	27.084020
241.482871	9342.130773	27.089037
242.176496	9350.780447	27.094055
242.611573	9358.774537	27.099072
242.597536	9361.769790	27.104090
242.891475	9378.826782	27.109108
242.837930	9396.312185	27.114125
243.203147	9405.924701	27.119143
243.364101	9424.596438	27.124160
243.639661	9440.073165	27.129178
243.940502	9447.901812	27.134196
243.910629	9469.985783	27.139213
244.386966	9482.917933	27.144231
244.694138	9489.741884	27.149248
244.819402	9504.857445	27.154266
245.223502	9518.106071	27.159284
245.130357	9533.049520	27.164301
245.362999	9542.433806	27.169319
245.719005	9556.205171	27.174336
246.097932	9581.847105	27.179354
246.362064	9582.765052	27.184372
246.403097	9604.102934	27.189389
246.817575	9613.898166	27.194407
246.979659	9621.053387	27.199424
247.304403	9645.408403	27.204442
247.914958	9662.246056	27.209460
248.022276	9671.446589	27.214477
248.137553	9667.361796	27.219495
248.535922	9688.084903	27.224512
248.606524	9696.506348	27.229530
249.127438	9725.314515	27.234548
249.272573	9728.723178	27.239565
249.661393	9733.261188	27.244583
249.916579	9731.801296	27.249600
249.775109	9751.285759	27.254618
250.206725	9755.979848	27.259636
250.320226	9771.757786	27.264653
250.552095	9790.913260	27.269671
250.706042	9790.784069	27.274688
250.916585	9805.461396	27.279706
251.262238	9809.190263	27.284724
251.590850	9819.118540	27.289741
251.964877	9835.042695	27.294759
252.139249	9841.985952	27.299776
251.884603	9861.258029	27.304794
252.439726	9867.688507	27.309812
252.529370	9881.599822	27.314829
252.552089	9904.936325	27.319847
253.208724	9909.632364	27.324864
253.307943	9934.790280	27.329882
253.740086	9936.250815	27.334900
254.034949	9954.400194	27.339917
254.043272	9978.701533	27.344935
254.472163	9986.319218	27.349952
254.654055	10001.495110	27.354970
254.667043	10015.050087	27.359988
254.959920	10031.306493	27.365005
255.382218	10039.106647	27.370023
255.398920	10060.524604	27.375040
255.649603	10078.168481	27.380058
256.240409	10095.557488	27.385076
256.472693	10116.553587	27.390093
256.722035	10123.968996	27.395111
257.469143	10127.748447	27.400128
257.423920	10159.596396	27.405146
257.642452	10154.830826	27.410164
258.047792	10168.715689	27.415181
257.970181	10185.865099	27.420199
258.401328	10187.631943	27.425216
258.836436	10218.964721	27.430234
259.357253	10217.325116	27.435252
259.248152	10230.676256	27.440269
259.634781	10239.806644	27.445287
259.984126	10245.335583	27.450304
259.877628	10252.288393	27.455322
260.060593	10264.624263	27.460340
260.310186	10280.256310	27.465357
260.509237	10303.786851	27.470375
261.025716	10312.409851	27.475392
261.086892	10331.444493	27.480410
261.471907	10341.802462	27.485428
261.767512	10362.536592	27.490445
261.811103	10376.329400	27.495463
262.062297	10385.860389	27.500480
261.960592	10416.208887	27.505498
262.360680	10425.810602	27.510516
262.783368	10445.322500	27.515533
263.199057	10468.081772	27.520551
263.349626	10480.453282	27.525568
263.292899	10506.427524	27.530586
263.741409	10515.029211	27.535604
263.995051	10534.347822	27.540621
264.058996	10552.870774	27.545639
264.871690	10555.459034	27.550656
264.935454	10579.161885	27.555674
265.335648	10594.747430	27.560692
265.759354	10607.827456	27.565709
266.014946	10608.254186	27.570727
266.382878	10622.442910	27.575744
266.530066	10635.036226	27.580762
266.755267	10643.491795	27.585780
267.120179	10656.125971	27.590797
267.247779	10667.737144	27.595815
267.493180	10670.117988	27.600832
267.716734	10687.203827	27.605850
267.811287	10701.054521	27.610868
268.276570	10721.060901	27.615885
268.576148	10724.760751	27.620903
268.412961	10737.873064	27.625920
268.961822	10756.354379	27.630938
269.557266	10760.677189	27.635956
269.785604	10772.973585	27.640973
269.587186	10794.082968	27.645991
270.159426	10797.999470	27.651008
269.932577	10833.975619	27.656026
270.307571	10839.934321	27.661044
270.501622	10853.894426	27.666061
270.807249	10882.780458	27.671079
271.279036	10892.949873	27.676096
271.278763	10925.374648	27.681114
271.749640	10933.244653	27.686132
272.083320	10953.973924	27.691149
272.084521	10979.258605	27.696167
272.459988	10980.831774	27.701184
272.766142	11002.792421	27.706202
273.326568	11018.499246	27.711220
273.818424	11038.750898	27.716237
274.246238	11060.368387	27.721255
274.321328	11054.654248	27.726272
274.350194	11078.499205	27.731290
274.800897	11082.610658	27.736308
275.312214	11099.143874	27.741325
275.386849	11129.689599	27.746343
275.937451	11129.632929	27.751360
276.051814	11141.690053	27.756378
276.369410	11158.593805	27.761396
276.434739	11152.951621	27.766413
276.484124	11177.599747	27.771431
276.998283	11193.517572	27.776448
277.088527	11207.775514	27.781466
277.412841	11221.864333	27.786484
277.872960	11232.577300	27.791501
277.720228	11253.137795	27.796519
278.276433	11267.911772	27.801536
278.749210	11270.491784	27.806554
278.808890	11286.901630	27.811572
279.156918	11293.279959	27.816589
279.101375	11311.320780	27.821607
279.596943	11322.304007	27.826624
279.653180	11341.478834	27.831642
279.678695	11358.137783	27.836660
280.333878	11366.473670	27.841677
280.225075	11392.840621	27.846695
280.598624	11405.941146	27.851712
281.133411	11426.200447	27.856730
281.516673	11438.082333	27.861748
281.709020	11459.559279	27.866765
281.682182	11469.678320	27.871783
282.553598	11482.821931	27.876800
282.520039	11503.122942	27.881818
282.525822	11519.015902	27.886836
283.114085	11524.502119	27.891853
283.248306	11555.547624	27.896871
283.831398	11566.420670	27.901888
284.233648	11577.757774	27.906906
284.493231	11594.273818	27.911924
284.724721	11610.422882	27.916941
284.814780	11621.289953	27.921959
285.220009	11629.345118	27.926976
285.399178	11662.210366	27.931994
285.342014	11681.476502	27.937012
285.831001	11687.748319	27.942029
286.040863	11719.497513	27.947047
286.522023	11722.912097	27.952064
286.982802	11749.849591	27.957082
287.127524	11763.764886	27.962100
288.078429	11769.383063	27.967117
287.959852	11782.335304	27.972135
288.297269	11791.335969	27.977152
288.504238	11807.848828	27.982170
288.752042	11821.371542	27.987188
288.786254	11828.537183	27.992205
289.099652	11851.852799	27.997223
289.243611	11865.699838	28.002240
289.737073	11879.935461	28.007258
289.853076	11905.473349	28.012276
289.974730	11918.769915	28.017293
290.306083	11944.326666	28.022311
290.771271	11964.605068	28.027328
291.448356	11975.417781	28.032346
291.251173	12015.462998	28.037364
291.938850	12011.457910	28.042381
291.995748	12029.641827	28.047399
292.289240	12048.781702	28.052416
292.404641	12062.969543	28.057434
292.873763	12083.432828	28.062452
292.934406	12098.397198	28.067469
293.440781	12118.849871	28.072487
293.714203	12136.509464	28.077504
294.120907	12148.507020	28.082522
294.085775	12173.642082	28.087540
294.701062	12191.016245	28.092557
294.912684	12212.762331	28.097575
295.278907	12222.308816	28.102592
295.247662	12240.327981	28.107610
295.562027	12252.389924	28.112628
296.051413	12265.478244	28.117645
296.338891	12286.383375	28.122663
296.553308	12291.632157	28.127680
297.156962	12300.886821	28.132698
296.877844	12335.026654	28.137716
297.547278	12334.173038	28.142733
297.690245	12365.486414	28.147751
298.100298	12373.655926	28.152768
298.388568	12384.782182	28.157786
298.471841	12399.812111	28.162804
298.660614	12423.065046	28.167821
298.944826	12441.568389	28.172839
299.318466	12463.205188	28.177856
299.652334	12473.947629	28.182874
299.776075	12507.406571	28.187892
300.138119	12517.172519	28.192909
300.511656	12562.279204	28.197927
300.680311	12568.174088	28.202944
301.353902	12588.042118	28.207962
301.577391	12602.867493	28.212980
302.181729	12629.524334	28.217997
302.503353	12640.428622	28.223015
302.764207	12655.077101	28.228032
303.259959	12657.336112	28.233050
303.107687	12683.290560	28.238068
303.382868	12709.359127	28.243085
303.711066	12720.122128	28.248103
303.746015	12734.766550	28.253120
304.338192	12757.781949	28.258138
304.871457	12781.729632	28.263156
305.013959	12786.772420	28.268173
305.359165	12811.032296	28.273191
305.644312	12828.141638	28.278208
306.223850	12847.010838	28.283226
306.368260	12849.164922	28.288244
306.842234	12862.357754	28.293261
307.180227	12886.511463	28.298279
307.411721	12891.678630	28.303296
308.049357	12892.464847	28.308314
308.584211	12920.163186	28.313332
308.977140	12907.710939	28.318349
308.920735	12938.084037	28.323367
308.766462	12944.976432	28.328384
309.465535	12956.973290	28.333402
309.344942	12977.861580	28.338420
309.759318	12989.352679	28.343437
310.195102	12989.267292	28.348455
310.131150	13022.487314	28.353472
310.614710	13044.487397	28.358490
310.665440	13058.536931	28.363508
311.058321	13053.527199	28.368525
311.295526	13101.581888	28.373543
311.422675	13107.812411	28.378560
312.149100	13120.105321	28.383578
312.132738	13137.655639	28.388596
312.592482	13154.037588	28.393613
313.004258	13181.754450	28.398631
313.032967	13194.815274	28.403648
313.404574	13201.192826	28.408666
313.529575	13246.262451	28.413684
314.307306	13238.502353	28.418701
314.039992	13280.470037	28.423719
314.782937	13294.748111	28.428736
315.189055	13299.148289	28.433754
315.255805	13322.054667	28.438772
315.491263	13348.231809	28.443789
316.050000	13348.381851	28.448807
316.183109	13379.944670	28.453824
316.454669	13387.005722	28.458842
316.918841	13422.468568	28.463860
317.409720	13429.738886	28.468877
317.393769	13457.709795	28.473895
317.615439	13463.066256	28.478912
318.055741	13492.985835	28.483930
318.466209	13514.123954	28.488948
318.799517	13514.749736	28.493965
319.070523	13569.284452	28.498983
319.529890	13565.417296	28.504000
319.628880	13592.240801	28.509018
319.882905	13635.696687	28.514036
320.340394	13639.587770	28.519053
320.589354	13655.137228	28.524071
320.556074	13693.412521	28.529088
321.546793	13700.438004	28.534106
321.491890	13728.529359	28.539124
321.972833	13755.790530	28.544141
322.413615	13759.238197	28.549159
322.640338	13798.671123	28.554176
323.321935	13813.949492	28.559194
323.455825	13835.753589	28.564212
324.242973	13833.450910	28.569229
324.527329	13850.597939	28.574247
324.801714	13874.265689	28.579264
325.117333	13862.453720	28.584282
325.331709	13883.789893	28.589300
325.207094	13914.432911	28.594317
326.013523	13902.564624	28.599335
325.896888	13960.380174	28.604352
326.765850	13951.937386	28.609370
326.830632	13960.658106	28.614388
326.834177	13984.857621	28.619405
327.717569	14003.642449	28.624423
327.496028	14021.620358	28.629440
328.160899	14037.740525	28.634458
328.151641	14055.569322	28.639476
328.488130	14079.637107	28.644493
329.047636	14089.752502	28.649511
329.219509	14120.279605	28.654528
329.183108	14137.514191	28.659546
329.575965	14152.260266	28.664564
330.034625	14158.111320	28.669581
330.420632	14175.877553	28.674599
330.617452	14225.055662	28.679616
331.233468	14221.961755	28.684634
331.417677	14243.620073	28.689652
331.733280	14247.808059	28.694669
331.851468	14267.648357	28.699687
332.115010	14293.044662	28.704704
332.732224	14316.371734	28.709722
332.985152	14350.490711	28.714740
332.934310	14361.380629	28.719757
333.764304	14383.827490	28.724775
333.608078	14409.587237	28.729792
334.323520	14423.988842	28.734810
334.342804	14450.113777	28.739828
334.508854	14464.931826	28.744845
334.937925	14499.688617	28.749863
335.516272	14525.478191	28.754880
335.941731	14544.851590	28.759898
336.088209	14570.921430	28.764916
336.453141	14593.650735	28.769933
337.009284	14606.460348	28.774951
337.606202	14640.941370	28.779968
337.572717	14659.890859	28.784986
338.190954	14679.254956	28.790004
338.245464	14694.959073	28.795021
338.565807	14714.080223	28.800039
339.082171	14751.588569	28.805056
339.539840	14770.037391	28.810074
339.889937	14780.897752	28.815092
340.326763	14802.707888	28.820109
340.806523	14811.010293	28.825127
340.720275	14828.906972	28.830144
341.450829	14851.153995	28.835162
341.647498	14874.818761	28.840180
341.953270	14889.032430	28.845197
341.913287	14915.371981	28.850215
342.705317	14925.479708	28.855232
342.585601	14953.586301	28.860250
343.200433	14968.329967	28.865268
343.681594	14991.706033	28.870285
344.121533	15008.819336	28.875303
344.068381	15034.248333	28.880320
344.618360	15045.403223	28.885338
345.208622	15074.071022	28.890356
345.218246	15101.336316	28.895373
345.779459	15116.341439	28.900391
345.982534	15129.084764	28.905408
346.283217	15143.662187	28.910426
346.637552	15166.538981	28.915444
346.863569	15203.432176	28.920461
347.349324	15217.415349	28.925479
347.381269	15241.544036	28.930496
348.022945	15251.240026	28.935514
348.477796	15271.555305	28.940532
348.313264	15291.467182	28.945549
349.066408	15306.552827	28.950567
349.314506	15313.678740	28.955584
349.699155	15350.775497	28.960602
350.076920	15368.849779	28.965620
350.104154	15393.981685	28.970637
350.892678	15411.932495	28.975655
350.949560	15422.826172	28.980672
350.927340	15459.068463	28.985690
351.351496	15476.815177	28.990708
351.509716	15502.305237	28.995725
351.939867	15524.472606	29.000743
352.374015	15561.449412	29.005760
352.462842	15582.851759	29.010778
353.180465	15608.840213	29.015796
353.308475	15638.377749	29.020813
353.911620	15663.544564	29.025831
354.286267	15697.408516	29.030848
354.492094	15723.186372	29.035866
355.545404	15738.873784	29.040884
355.461404	15765.626057	29.045901
356.123427	15792.423521	29.050919
356.474531	15803.055758	29.055936
356.798730	15831.135030	29.060954
357.256905	15859.963813	29.065972
357.327077	15876.500042	29.070989
358.062415	15884.280313	29.076007
357.980074	15919.562795	29.081024
358.116749	15939.663778	29.086042
358.764882	15964.205928	29.091060
359.004933	15983.554022	29.096077
359.239802	16014.436999	29.101095
359.540374	16031.685942	29.106112
360.238198	16068.095374	29.111130
360.699329	16081.418526	29.116148
360.879024	16108.758387	29.121165
361.468204	16124.454531	29.126183
362.027283	16157.530894	29.131200
362.023723	16172.865927	29.136218
362.569028	16189.994072	29.141236
362.939747	16217.577552	29.146253
363.269217	16237.697404	29.151271
363.588651	16261.977019	29.156288
363.858404	16294.026056	29.161306
364.498252	16307.846720	29.166324
364.365490	16334.827597	29.171341
365.323730	16348.621567	29.176359
365.576592	16368.216783	29.181376
365.623707	16391.465280	29.186394
366.014863	16404.053040	29.191412
366.074246	16439.398462	29.196429
366.942567	16448.296822	29.201447
367.126863	16479.725617	29.206464
367.361579	16502.271852	29.211482
368.182197	16511.041062	29.216500
368.161253	16529.392330	29.221517
368.201359	16539.940018	29.226535
368.846209	16573.219127	29.231552
368.703589	16596.719791	29.236570
369.486181	16607.879402	29.241588
369.571569	16654.153386	29.246605
369.901298	16682.500421	29.251623
370.016866	16694.095286	29.256640
370.458909	16720.436591	29.261658
371.146671	16755.000999	29.266676
371.441850	16786.603470	29.271693
372.339080	16795.945594	29.276711
372.450252	16836.299711	29.281728
372.779031	16858.732476	29.286746
373.443325	16873.636422	29.291764
373.860303	16897.464645	29.296781
374.422396	16917.469881	29.301799
374.507190	16943.782097	29.306816
374.853611	16966.500163	29.311834
375.182966	16970.884918	29.316852
375.434042	17006.719923	29.321869
375.854776	17032.234356	29.326887
376.143969	17061.876384	29.331904
376.347207	17086.723489	29.336922
377.096751	17106.291273	29.341940
377.263414	17147.278229	29.346957
377.422474	17175.232945	29.351975
377.915159	17191.172702	29.356992
378.339300	17218.902007	29.362010
378.897408	17252.339701	29.367028
379.129244	17276.829838	29.372045
379.525766	17300.993603	29.377063
380.160347	17327.826470	29.382080
379.900412	17358.425778	29.387098
380.361518	17395.220435	29.392116
380.969438	17425.626854	29.397133
381.294734	17452.145678	29.402151
381.928450	17482.757527	29.407168
382.103769	17504.501189	29.412186
382.760449	17528.560865	29.417204
383.227256	17564.100210	29.422221
383.502888	17587.308579	29.427239
384.168683	17620.893480	29.432256
383.908042	17650.095367	29.437274
384.631940	17661.940444	29.442292
384.894411	17685.452608	29.447309
385.510415	17702.417254	29.452327
385.571400	17734.127289	29.457344
386.532229	17757.747546	29.462362
386.712351	17774.679577	29.467380
387.173905	17814.518044	29.472397
387.200581	17827.010146	29.477415
387.726250	17839.682956	29.482432
387.937454	17869.679490	29.487450
388.442589	17892.599400	29.492468
388.514024	17912.161520	29.497485
389.069831	17940.563416	29.502503
389.562815	17969.624352	29.507520
389.826471	17993.811951	29.512538
390.158158	18011.910369	29.517556
390.446836	18044.841964	29.522573
390.646433	18066.649472	29.527591
391.533115	18084.815036	29.532608
391.478281	18118.910129	29.537626
392.017417	18157.858424	29.542644
392.843647	18178.008829	29.547661
393.100709	18198.695216	29.552679
393.446063	18218.198324	29.557696
393.968268	18242.297474	29.562714
394.325183	18265.159278	29.567732
394.527423	18286.656846	29.572749
394.288547	18317.226736	29.577767
395.258197	18358.277315	29.582784
395.372854	18381.110575	29.587802
396.300376	18422.161345	29.592820
396.703019	18443.272876	29.597837
396.851430	18461.622280	29.602855
397.524013	18478.892143	29.607872
397.436844	18528.829044	29.612890
398.118265	18547.446752	29.617908
398.852563	18584.173343	29.622925
398.883307	18602.784573	29.627943
399.422477	18620.858121	29.632960
399.629802	18653.080759	29.637978
400.046803	18686.832229	29.642996
400.410828	18718.593031	29.648013
400.935362	18731.841947	29.653031
401.141139	18762.730431	29.658048
401.130103	18807.811271	29.663066
402.015421	18828.155865	29.668084
402.442781	18864.641878	29.673101
402.633873	18901.821925	29.678119
402.982928	18914.530458	29.683136
403.654313	18952.083694	29.688154
404.019700	18981.796785	29.693172
404.638648	19012.862053	29.698189
405.113010	19039.537798	29.703207
405.627658	19073.934790	29.708224
405.827140	19108.233654	29.713242
406.576746	19121.837595	29.718260
406.902036	19150.923927	29.723277
406.731729	19173.341944	29.728295
407.295173	19192.752470	29.733312
407.677103	19239.164087	29.738330
408.007412	19269.246710	29.743348
408.615197	19298.837921	29.748365
409.007967	19322.691657	29.753383
409.441721	19349.527558	29.758400
409.685530	19363.333968	29.763418
410.540011	19382.604258	29.768436
410.853750	19408.336126	29.773453
410.733373	19434.906529	29.778471
411.508492	19455.329750	29.783488
411.853947	19477.213639	29.788506
412.521839	19506.625584	29.793524
412.265900	19535.990302	29.798541
412.652993	19562.324144	29.803559
413.228066	19591.168340	29.808576
413.454342	19630.324523	29.813594
413.566017	19662.616070	29.818612
414.461109	19697.754645	29.823629
414.801607	19729.618510	29.828647
415.183056	19759.604164	29.833664
415.436190	19796.137056	29.838682
415.732009	19831.847436	29.843700
416.409012	19859.766781	29.848717
416.909459	19894.878524	29.853735
417.405309	19922.223661	29.858752
417.611181	19956.696220	29.863770
418.327866	19985.903252	29.868788
418.564500	20013.065036	29.873805
419.024556	20046.762594	29.878823
419.405352	20078.985345	29.883840
419.846450	20104.574832	29.888858
420.628091	20138.532392	29.893876
420.892133	20172.063408	29.898893
421.633845	20210.043945	29.903911
422.177590	20233.616338	29.908928
422.304363	20267.606870	29.913946
422.452504	20281.500999	29.918964
423.099386	20310.906002	29.923981
423.153599	20350.457976	29.928999
424.088927	20372.629873	29.934016
424.272607	20400.220885	29.939034
424.865933	20435.876185	29.944052
425.342001	20477.277584	29.949069
425.242010	20501.187233	29.954087
426.008465	20520.137894	29.959104
426.398329	20550.935621	29.964122
426.773122	20591.062382	29.969140
427.408590	20626.743297	29.974157
427.418017	20672.754704	29.979175
428.222476	20682.038206	29.984192
428.528824	20711.669505	29.989210
428.722239	20746.625372	29.994228
428.975856	20791.068513	29.999245
429.155536	20822.275507	30.004263
429.700862	20855.784431	30.009280
430.340898	20899.302815	30.014298
430.682621	20935.520278	30.019316
431.380099	20968.155090	30.024333
431.663424	21008.119912	30.029351
432.293423	21034.933745	30.034368
432.487211	21057.053888	30.039386
433.075306	21078.590296	30.044404
433.599463	21117.181013	30.049421
433.770978	21155.859515	30.054439
434.359975	21179.722232	30.059456
434.755431	21200.861884	30.064474
435.116108	21240.309781	30.069492
435.848636	21267.773129	30.074509
435.917219	21295.389570	30.079527
436.973595	21313.606711	30.084544
437.337771	21353.904466	30.089562
437.453881	21366.004384	30.094580
437.939961	21408.279226	30.099597
438.271766	21434.993599	30.104615
438.923475	21457.210661	30.109632
439.252929	21489.946155	30.114650
439.498284	21521.151556	30.119668
440.477402	21565.588002	30.124685
440.458752	21589.053200	30.129703
440.686326	21628.781200	30.134720
441.096371	21642.583616	30.139738
441.535950	21682.872563	30.144756
442.155883	21731.153987	30.149773
442.529750	21762.934773	30.154791
442.906083	21792.206900	30.159808
443.232970	21834.991809	30.164826
443.694100	21874.573747	30.169844
444.379145	21907.734645	30.174861
445.031947	21941.855265	30.179879
445.212178	21978.406830	30.184896
445.951564	22005.395879	30.189914
446.356192	22042.170157	30.194932
446.785910	22080.236057	30.199949
447.136182	22107.254991	30.204967
447.569753	22145.628372	30.209984
448.602048	22167.317989	30.215002
448.408653	22198.847451	30.220020
449.037879	22229.417384	30.225037
449.805787	22256.214093	30.230055
450.178683	22293.184604	30.235072
450.716761	22321.849932	30.240090
450.798568	22357.695857	30.245108
451.351951	22384.055209	30.250125
451.919067	22414.177030	30.255143
452.108036	22449.788718	30.260160
452.680015	22483.602848	30.265178
453.054775	22523.904277	30.270196
453.958290	22544.257935	30.275213
454.104259	22581.155018	30.280231
454.639237	22608.402136	30.285248
455.012349	22625.415988	30.290266
455.388905	22663.008190	30.295284
455.917255	22692.935098	30.300301
456.300046	22727.226459	30.305319
456.752147	22752.314067	30.310336
457.366298	22773.852988	30.315354
457.412454	22812.132988	30.320372
458.118238	22829.955687	30.325389
458.524328	22853.522062	30.330407
458.727498	22886.060054	30.335424
459.335951	22927.301115	30.340442
459.480638	22963.696018	30.345460
460.070933	22978.407351	30.350477
460.538359	23024.516476	30.355495
460.889682	23054.918063	30.360512
461.431816	23103.304304	30.365530
461.672460	23131.890904	30.370548
462.311004	23163.184982	30.375565
462.479860	23210.871767	30.380583
462.712378	23245.631624	30.385600
463.349752	23286.078247	30.390618
463.662694	23331.652096	30.395636
464.229810	23365.544505	30.400653
464.806825	23410.240051	30.405671
464.887752	23448.664912	30.410688
465.592754	23494.761972	30.415706
465.906527	23535.399414	30.420724
466.831870	23571.958033	30.425741
467.320528	23619.104397	30.430759
467.897446	23650.457306	30.435776
468.834578	23693.743116	30.440794
468.879362	23734.112807	30.445812
469.682694	23763.931773	30.450829
470.291661	23806.934643	30.455847
470.796461	23833.330940	30.460864
471.469221	23857.080017	30.465882
471.818170	23897.268550	30.470900
472.090784	23913.074221	30.475917
472.743749	23944.713329	30.480935
473.046728	23973.480554	30.485952
473.656538	24017.688184	30.490970
474.274852	24049.017172	30.495988
474.801854	24066.368808	30.501005
474.622700	24105.750379	30.506023
475.194239	24145.303880	30.511040
476.247465	24168.795106	30.516058
476.215470	24202.650859	30.521076
476.496577	24242.456455	30.526093
477.078639	24263.623657	30.531111
477.907443	24307.755459	30.536128
478.441265	24341.824614	30.541146
478.599033	24373.179570	30.546164
479.192329	24405.594724	30.551181
479.446516	24448.116301	30.556199
479.729239	24483.028407	30.561216
480.357754	24516.146299	30.566234
480.397401	24559.394725	30.571252
481.005073	24600.756061	30.576269
481.634808	24635.722704	30.581287
481.963085	24672.877600	30.586304
482.503639	24707.831828	30.591322
483.060652	24752.250777	30.596340
483.816953	24772.381079	30.601357
483.916135	24813.885423	30.606375
484.455027	24846.455869	30.611392
484.914699	24878.657758	30.616410
485.390861	24925.192437	30.621428
486.016305	24947.035790	30.626445
486.681560	24969.995307	30.631463
487.077357	25008.073657	30.636480
487.851929	25046.016919	30.641498
487.878476	25079.632046	30.646516
488.707058	25109.466856	30.651533
488.866868	25138.978179	30.656551
489.255155	25185.988432	30.661568
490.181931	25218.181182	30.666586
490.368364	25261.419942	30.671604
490.922852	25303.576146	30.676621
491.423588	25342.401876	30.681639
492.046324	25367.164745	30.686656
492.480065	25392.011329	30.691674
493.019355	25444.922757	30.696692
493.451933	25486.280420	30.701709
493.903802	25519.297783	30.706727
494.227914	25551.757373	30.711744
494.869178	25593.932029	30.716762
495.514833	25645.432101	30.721780
495.591148	25683.510971	30.726797
496.165931	25703.554002	30.731815
496.866787	25748.835082	30.736832
497.509306	25775.612841	30.741850
497.979599	25823.743106	30.746868
498.560545	25857.812726	30.751885
499.012876	25891.388510	30.756903
499.131495	25935.411889	30.761920
499.804413	25980.042667	30.766938
500.319210	26019.736696	30.771956
500.671011	26064.335365	30.776973
501.377651	26103.349139	30.781991
501.889245	26144.220111	30.787008
502.227876	26178.061179	30.792026
502.798326	26210.860989	30.797044
503.117538	26261.839986	30.802061
503.910966	26294.713157	30.807079
504.138628	26349.245670	30.812096
504.647902	26381.361550	30.817114
505.246211	26427.262747	30.822132
505.393664	26470.617332	30.827149
506.376144	26511.982213	30.832167
506.631731	26559.845600	30.837184
507.670106	26597.638666	30.842202
507.770134	26642.812384	30.847220
508.249354	26690.995827	30.852237
509.222459	26707.277217	30.857255
509.521027	26762.528542	30.862272
510.270326	26788.596947	30.867290
510.547037	26825.357775	30.872308
510.749307	26854.483417	30.877325
511.559782	26870.203187	30.882343
511.673241	26919.609948	30.887360
512.018995	26961.133359	30.892378
512.469685	26986.212912	30.897396
513.023718	27042.729890	30.902413
513.929886	27068.320773	30.907431
514.124174	27110.778617	30.912448
514.796861	27152.197657	30.917466
515.326733	27192.498015	30.922484
515.593808	27247.563011	30.927501
516.594729	27285.688249	30.932519
516.960633	27320.052068	30.937536
517.504685	27357.314331	30.942554
517.837749	27394.741858	30.947572
518.610487	27434.528290	30.952589
519.311368	27462.762568	30.957607
519.288402	27518.571920	30.962624
520.030405	27554.555187	30.967642
520.332386	27596.075394	30.972660
520.675000	27643.624828	30.977677
521.576714	27684.651868	30.982695
521.792519	27727.709028	30.987712
522.761870	27774.416864	30.992730
523.254002	27821.562479	30.997748
523.905787	27857.859389	31.002765
524.673528	27886.840093	31.007783
524.713767	27937.831028	31.012800
525.447231	27975.738948	31.017818
526.013001	28013.336471	31.022836
526.308983	28055.366981	31.027853
527.007222	28088.898736	31.032871
527.480723	28140.949502	31.037888
528.037760	28167.211501	31.042906
528.373647	28217.612599	31.047924
529.175936	28266.803456	31.052941
529.720977	28296.504241	31.057959
529.835846	28351.179682	31.062976
530.398745	28399.302911	31.067994
531.242539	28427.413695	31.073012
531.611800	28486.257880	31.078029
532.451254	28523.414330	31.083047
532.650898	28554.117639	31.088064
533.122545	28597.951030	31.093082
533.643410	28658.163087	31.098100
534.064380	28689.063033	31.103117
534.862951	28726.735437	31.108135
535.367161	28780.239385	31.113152
536.084485	28825.491852	31.118170
536.723684	28864.984784	31.123188
537.190856	28910.704376	31.128205
537.866792	28951.081988	31.133223
538.064494	28989.659106	31.138240
538.523508	29029.311933	31.143258
539.218792	29068.654606	31.148276
539.497926	29103.077803	31.153293
540.100475	29139.129371	31.158311
540.594566	29183.416183	31.163328
541.035006	29221.726692	31.168346
541.598629	29261.456397	31.173364
541.832785	29305.038006	31.178381
542.753387	29344.722082	31.183399
543.153488	29390.081814	31.188416
543.831909	29427.973549	31.193434
544.194043	29471.862995	31.198452
544.534465	29522.839464	31.203469
545.333256	29565.198792	31.208487
545.852137	29618.666926	31.213504
546.051659	29656.964836	31.218522
546.870870	29701.588936	31.223540
547.494793	29756.936561	31.228557
547.986271	29799.082283	31.233575
548.865703	29840.983513	31.238592
549.749222	29874.243624	31.243610
550.616941	29935.141110	31.248628
550.601060	29954.407347	31.253645
551.422058	29995.139517	31.258663
552.041549	30025.277597	31.263680
552.642360	30075.119071	31.268698
553.199431	30116.252893	31.273716
553.880826	30142.347006	31.278733
554.472143	30182.002063	31.283751
554.989124	30221.197858	31.288768
555.149780	30258.174876	31.293786
555.917738	30293.266566	31.298804
556.482711	30334.743233	31.303821
557.286603	30365.802858	31.308839
557.626898	30407.195728	31.313856
558.134243	30449.948921	31.318874
558.637786	30475.109001	31.323892
558.835634	30524.582655	31.328909
559.546012	30558.440667	31.333927
560.160645	30599.689466	31.338944
560.923924	30634.541518	31.343962
561.625647	30695.053814	31.348980
561.776750	30730.537835	31.353997
562.419226	30768.956919	31.359015
562.964823	30821.397217	31.364032
563.036960	30872.034530	31.369050
563.985355	30891.975667	31.374068
564.299595	30971.645327	31.379085
565.233658	31002.252037	31.384103
565.515527	31041.230368	31.389120
566.045095	31097.079835	31.394138
566.475272	31140.015761	31.399156
567.048274	31181.696609	31.404173
567.627452	31225.088133	31.409191
568.470962	31260.158842	31.414208
568.761334	31325.605742	31.419226
569.563621	31337.088539	31.424244
570.222892	31389.463697	31.429261
570.528996	31421.246072	31.434279
570.760280	31469.270460	31.439296
571.465442	31503.758531	31.444314
572.290674	31553.039226	31.449332
572.238329	31605.422829	31.454349
573.383492	31655.598505	31.459367
574.040106	31688.671521	31.464384
574.133595	31740.167068	31.469402
574.860113	31781.670540	31.474420
575.474460	31834.534979	31.479437
575.916954	31871.155538	31.484455
576.654001	31929.917334	31.489472
577.260435	31989.866451	31.494490
577.840322	32016.274466	31.499508
578.432312	32073.527922	31.504525
578.994534	32120.562151	31.509543
579.853956	32169.755725	31.514560
580.037072	32220.708931	31.519578
580.951115	32254.777593	31.524596
581.085567	32313.072495	31.529613
581.877689	32357.288934	31.534631
582.562272	32409.529351	31.539648
583.078361	32460.096125	31.544666
584.150014	32495.158366	31.549684
584.485139	32560.486427	31.554701
584.680742	32609.744495	31.559719
585.407474	32652.247839	31.564736
585.782253	32707.913091	31.569754
586.418882	32757.840575	31.574772
587.086347	32818.842176	31.579789
587.578297	32865.435794	31.584807
588.274283	32923.810492	31.589824
589.095182	32963.843959	31.594842
589.522607	33014.765438	31.599860
589.969181	33073.563405	31.604877
590.553146	33123.394781	31.609895
591.801386	33173.814035	31.614912
591.800224	33222.421201	31.619930
592.736261	33271.254378	31.624948
593.383195	33332.675695	31.629965
593.977658	33381.380761	31.634983
594.620823	33427.619301	31.640000
595.022495	33473.322687	31.645018
595.927654	33512.414094	31.650036
596.338707	33568.503632	31.655053
596.944634	33610.927815	31.660071
597.900828	33652.643753	31.665088
598.142588	33694.717904	31.670106
598.768740	33755.699604	31.675124
599.090289	33804.772519	31.680141
599.802181	33845.296794	31.685159
600.113172	33890.695796	31.690176
600.701949	33936.998019	31.695194
601.433966	33982.706945	31.700212
601.894572	34041.219239	31.705229
602.349754	34091.964651	31.710247
603.079138	34125.691449	31.715264
603.711219	34187.567554	31.720282
604.174581	34227.159774	31.725300
604.828900	34289.784615	31.730317
605.662246	34334.490031	31.735335
606.351000	34372.006952	31.740352
606.589206	34435.480470	31.745370
607.107926	34479.758762	31.750388
607.590368	34527.356397	31.755405
607.791532	34595.306898	31.760423
608.858951	34646.946439	31.765440
609.156548	34707.756979	31.770458
610.082906	34759.157663	31.775476
610.759860	34823.199630	31.780493
611.112125	34881.125244	31.785511
611.947169	34929.474973	31.790528
612.652740	35004.285985	31.795546
613.631825	35057.006503	31.800564
614.178415	35109.526508	31.805581
614.309030	35160.175546	31.810599
615.508333	35208.854291	31.815616
615.981894	35277.338002	31.820634
616.560581	35326.748071	31.825652
617.018844	35376.601521	31.830669
617.870852	35420.216018	31.835687
618.653766	35486.124327	31.840704
618.780530	35543.846969	31.845722
620.019742	35580.088755	31.850740
620.684064	35623.998518	31.855757
620.828995	35688.636161	31.860775
621.817565	35735.693176	31.865792
622.570522	35795.374220	31.870810
623.279157	35843.499239	31.875828
623.774768	35899.531161	31.880845
624.161269	35946.233790	31.885863
624.667456	35996.086190	31.890880
625.306486	36042.687389	31.895898
626.242322	36092.211532	31.900916
626.911973	36146.548654	31.905933
627.197871	36206.707557	31.910951
628.262540	36260.308977	31.915968
628.584345	36310.349330	31.920986
629.041620	36358.080751	31.926004
630.004031	36409.203332	31.931021
630.725246	36467.854495	31.936039
631.323410	36510.000398	31.941056
631.677454	36566.556860	31.946074
632.576815	36623.449176	31.951092
633.212923	36662.240875	31.956109
633.536735	36724.021004	31.961127
634.338772	36757.418390	31.966144
634.669895	36806.895918	31.971162
635.567969	36858.392726	31.976180
635.903654	36902.192653	31.981197
636.681224	36946.854068	31.986215
637.212876	36996.336481	31.991232
638.009775	37048.627233	31.996250
638.545277	37086.133693	32.001268
639.452510	37131.175400	32.006285
640.224735	37191.350255	32.011303
640.846104	37231.621302	32.016320
641.222081	37283.281393	32.021338
642.121653	37319.048174	32.026356
642.555909	37373.442534	32.031373
642.940749	37425.215166	32.036391
643.944749	37466.382840	32.041408
644.142213	37530.205692	32.046426
644.824493	37582.779659	32.051444
645.415267	37639.918498	32.056461
645.863311	37689.432036	32.061479
646.717181	37737.908310	32.066496
646.856997	37799.281815	32.071514
647.515801	37877.608542	32.076532
648.349994	37930.082147	32.081549
648.721799	37993.021291	32.086567
649.716180	38052.526884	32.091584
650.485188	38123.827369	32.096602
651.264324	38182.248264	32.101620
651.856248	38240.153644	32.106637
652.085936	38319.145168	32.111655
652.948286	38379.443943	32.116672
653.723517	38445.037170	32.121690
654.249919	38512.429880	32.126708
655.034814	38568.314279	32.131725
655.539709	38625.244666	32.136743
656.617753	38670.025218	32.141760
656.915211	38763.225311	32.146778
657.308573	38824.302006	32.151796
658.722975	38879.879061	32.156813
658.996033	38942.392829	32.161831
660.021895	39001.078429	32.166848
660.688756	39055.004414	32.171866
661.177961	39118.520340	32.176884
661.788522	39167.947691	32.181901
662.236416	39236.237201	32.186919
663.411036	39300.872969	32.191936
663.826471	39354.376374	32.196954
664.153683	39423.441135	32.201972
665.379724	39477.862835	32.206989
665.864876	39542.626664	32.212007
666.703155	39603.865534	32.217024
667.504645	39669.177082	32.222042
667.806217	39708.207259	32.227060
668.611606	39766.392930	32.232077
669.536367	39849.193000	32.237095
670.245524	39874.796611	32.242112
671.045740	39918.697542	32.247130
671.211164	39965.932194	32.252148
671.980916	40022.779376	32.257165
672.375455	40073.536782	32.262183
672.837889	40139.545911	32.267200
673.206709	40196.055419	32.272218
673.910575	40259.237099	32.277236
675.163058	40314.346370	32.282253
675.099286	40375.408408	32.287271
676.365608	40434.177375	32.292288
676.944072	40484.364271	32.297306
677.095430	40564.000015	32.302324
678.157920	40614.174871	32.307341
678.597121	40690.810261	32.312359
679.389585	40751.462918	32.317376
680.317608	40813.450354	32.322394
681.187366	40886.208228	32.327412
681.846754	40935.639259	32.332429
682.369663	41007.285953	32.337447
683.177831	41063.868726	32.342464
683.503180	41127.229018	32.347482
684.113709	41197.794965	32.352500
684.920384	41254.197258	32.357517
685.707410	41326.842451	32.362535
686.066823	41395.206755	32.367552
687.240669	41467.513404	32.372570
687.847691	41523.733910	32.377588
688.590914	41597.557351	32.382605
689.081583	41668.876053	32.387623
690.133797	41727.394989	32.392640
690.481498	41793.835653	32.397658
691.112935	41856.159542	32.402676
692.064892	41917.707193	32.407693
692.679051	41990.225028	32.412711
693.370556	42066.156170	32.417728
693.875555	42123.177099	32.422746
694.829701	42212.206961	32.427764
695.577324	42268.353905	32.432781
696.478549	42335.443435	32.437799
697.490056	42381.897139	32.442816
698.099310	42455.736148	32.447834
698.156965	42530.947044	32.452852
699.372837	42587.752239	32.457869
699.899569	42653.726141	32.462887
700.711266	42711.293174	32.467904
701.512835	42770.675676	32.472922
701.839651	42838.047885	32.477940
703.054383	42900.326850	32.482957
703.544316	42965.468785	32.487975
704.128300	43027.183099	32.492992
705.390254	43079.484636	32.498010
705.765305	43158.710414	32.503028
706.442211	43205.184929	32.508045
706.923139	43271.685795	32.513063
707.360176	43327.153858	32.518080
708.288002	43394.688046	32.523098
708.890692	43458.864445	32.528116
709.781749	43494.741822	32.533133
710.018279	43554.945649	32.538151
710.719917	43623.062446	32.543168
711.777510	43681.098269	32.548186
711.956076	43742.977483	32.553204
712.982882	43798.444634	32.558221
713.718648	43869.033160	32.563239
714.233014	43942.764321	32.568256
715.139803	44006.556815	32.573274
715.449281	44078.103617	32.578292
716.530437	44154.656979	32.583309
716.979825	44219.775404	32.588327
717.644709	44290.714465	32.593344
718.273089	44372.659327	32.598362
718.913852	44429.691509	32.603380
719.706938	44507.033604	32.608397
720.776397	44586.596992	32.613415
721.317224	44654.746612	32.618432
722.082335	44719.110027	32.623450
722.814478	44808.813246	32.628468
723.374958	44876.742944	32.633485
723.918967	44967.170943	32.638503
724.485011	45024.216976	32.643520
725.761118	45098.472154	32.648538
726.161063	45184.397341	32.653556
727.084499	45263.725249	32.658573
728.181274	45331.542946	32.663591
728.569367	45408.357307	32.668608
729.125762	45493.596629	32.673626
729.922810	45561.346220	32.678644
731.190102	45636.734487	32.683661
731.741903	45715.413814	32.688679
732.626558	45779.705340	32.693696
733.476839	45856.697316	32.698714
733.812834	45938.617243	32.703732
734.701054	45990.144774	32.708749
735.614909	46071.777726	32.713767
736.584635	46148.786677	32.718784
737.231069	46213.379581	32.723802
737.949877	46282.807025	32.728820
738.947483	46340.990655	32.733837
739.652701	46408.865426	32.738855
740.116636	46480.394356	32.743872
741.007377	46541.712681	32.748890
741.557374	46615.809156	32.753908
742.322110	46684.628299	32.758925
743.176085	46754.897389	32.763943
743.665605	46833.232005	32.768960
744.725623	46906.491325	32.773978
745.271421	46980.820324	32.778996
746.097197	47045.832599	32.784013
746.793259	47103.022480	32.789031
747.438057	47172.638763	32.794048
748.409148	47232.949741	32.799066
748.479446	47300.149766	32.804084
749.485153	47364.658169	32.809101
750.366404	47437.998655	32.814119
750.901670	47507.393921	32.819136
751.836338	47565.067906	32.824154
752.249135	47631.662533	32.829172
753.135609	47690.963158	32.834189
753.708570	47778.369051	32.839207
754.421158	47851.214367	32.844224
755.591331	47920.235687	32.849242
756.225642	47994.734727	32.854260
756.623123	48059.935685	32.859277
757.675532	48142.433361	32.864295
758.333557	48226.574957	32.869312
759.482864	48289.098217	32.874330
759.830194	48365.045417	32.879348
760.761273	48427.029662	32.884365
761.595426	48496.747249	32.889383
761.958359	48581.076347	32.894400
763.353443	48654.194959	32.899418
764.083054	48722.267260	32.904436
764.611895	48811.344970	32.909453
765.598070	48868.708966	32.914471
766.434493	48957.202043	32.919488
766.903083	49015.683860	32.924506
767.738177	49109.898516	32.929524
768.228495	49173.637349	32.934541
769.198171	49253.581781	32.939559
769.330852	49349.427265	32.944576
770.449813	49412.527309	32.949594
771.236746	49509.563214	32.954612
771.741851	49596.480883	32.959629
772.850706	49672.463920	32.964647
773.399632	49763.187202	32.969664
774.243849	49838.723986	32.974682
774.916675	49930.135221	32.979700
775.968492	50012.540745	32.984717
777.000569	50084.233667	32.989735
777.440489	50167.747087	32.994752
778.579440	50246.236437	32.999770
779.349873	50321.559821	33.004788
779.622291	50412.589191	33.009805
780.918375	50503.014280	33.014823
781.346881	50569.365012	33.019840
782.504366	50667.853473	33.024858
783.162517	50765.563637	33.029876
784.087116	50821.627859	33.034893
784.451194	50921.575708	33.039911
785.003048	51003.020886	33.044928
786.496560	51070.261092	33.049946
786.864028	51158.928149	33.054964
787.773580	51248.916800	33.059981
788.378413	51301.839849	33.064999
789.145587	51411.755178	33.070016
790.077982	51442.529965	33.075034
790.670490	51562.174812	33.080052
791.554297	51618.554144	33.085069
792.547751	51689.852580	33.090087
792.874926	51784.178025	33.095104
793.869014	51842.216244	33.100122
794.568616	51924.020794	33.105140
795.271885	52019.979139	33.110157
796.153572	52083.315778	33.115175
796.907769	52174.791826	33.120192
797.831209	52242.622671	33.125210
798.396093	52341.372483	33.130228
799.057098	52425.041137	33.135245
800.668347	52493.972163	33.140263
800.940282	52575.964533	33.145280
801.835281	52649.983958	33.150298
802.792042	52752.372437	33.155316
803.637970	52829.326009	33.160333
804.431311	52909.602092	33.165351
804.907102	53001.745243	33.170368
806.088780	53077.472388	33.175386
806.341969	53158.327905	33.180404
806.981946	53248.060202	33.185421
807.994570	53355.786446	33.190439
808.902277	53445.120467	33.195456
809.629987	53528.815191	33.200474
810.731190	53615.685888	33.205492
811.287516	53716.414022	33.210509
812.381189	53798.704066	33.215527
813.097311	53882.743140	33.220544
813.586014	53975.088040	33.225562
814.547692	54080.024008	33.230580
815.440352	54170.061531	33.235597
816.593925	54251.573981	33.240615
817.016973	54342.409893	33.245632
817.884189	54434.071940	33.250650
818.549405	54537.397546	33.255668
819.309183	54631.722669	33.260685
820.242863	54733.573692	33.265703
820.954829	54821.519003	33.270720
822.006532	54910.868898	33.275738
822.946939	55011.183261	33.280756
823.627072	55110.428556	33.285773
824.825849	55190.091538	33.290791
825.662454	55282.640221	33.295808
826.582087	55357.806278	33.300826
827.321858	55475.133616	33.305844
828.173421	55520.406930	33.310861
828.968893	55646.981265	33.315879
830.143650	55699.056314	33.320896
830.837215	55813.741729	33.325914
832.112527	55881.034643	33.330932
832.528555	55966.579967	33.335949
833.567004	56051.524726	33.340967
834.290021	56126.545326	33.345984
835.064247	56201.599118	33.351002
835.873354	56274.321256	33.356020
836.372896	56357.784390	33.361037
837.333200	56441.676468	33.366055
837.959064	56497.610176	33.371072
838.586494	56583.209962	33.376090
840.192467	56663.382768	33.381108
840.207053	56754.750267	33.386125
841.418482	56836.435545	33.391143
841.875996	56923.244567	33.396160
842.709906	57013.898953	33.401178
843.606586	57090.774111	33.406196
844.362055	57188.178318	33.411213
845.274597	57281.697313	33.416231
845.935924	57373.905664	33.421248
846.471984	57463.709995	33.426266
847.407366	57562.075624	33.431284
848.046494	57675.616482	33.436301
849.275804	57753.738930	33.441319
849.787618	57863.055246	33.446336
850.723798	57972.573000	33.451354
851.777065	58064.877115	33.456372
852.679797	58149.935272	33.461389
853.519732	58268.543082	33.466407
854.180095	58367.212493	33.471424
855.785633	58456.980873	33.476442
856.664025	58558.015897	33.481460
857.419232	58636.230174	33.486477
858.428582	58749.573489	33.491495
859.334793	58838.062784	33.496512
859.848249	58925.244854	33.501530
860.799274	59018.551849	33.506548
861.746850	59133.116499	33.511565
862.664453	59211.777766	33.516583
863.328841	59311.821750	33.521600
864.567668	59413.959581	33.526618
865.603375	59496.085573	33.531636
866.019490	59592.779811	33.536653
866.858668	59683.105490	33.541671
868.216691	59780.919980	33.546688
868.617098	59878.016007	33.551706
869.812595	59965.785838	33.556724
870.714093	60052.920912	33.561741
871.570083	60151.098246	33.566759
872.203875	60242.122352	33.571776
873.347330	60338.553152	33.576794
874.122977	60432.788675	33.581812
874.599406	60539.202723	33.586829
875.552778	60631.598661	33.591847
876.237819	60737.434417	33.596864
877.286387	60824.874900	33.601882
878.071723	60924.188412	33.606900
878.896107	61030.897193	33.611917
880.004046	61124.546560	33.616935
880.588748	61230.862060	33.621952
881.599995	61323.144852	33.626970
882.664416	61403.891717	33.631988
883.156050	61493.485789	33.637005
884.187541	61571.150598	33.642023
884.985978	61683.961196	33.647040
885.857475	61763.729911	33.652058
886.902063	61852.397790	33.657076
887.882250	61964.707519	33.662093
888.657377	62048.783909	33.667111
889.627870	62136.362928	33.672128
890.157321	62235.259940	33.677146
891.199311	62331.619271	33.682164
892.187907	62433.706079	33.687181
892.878543	62515.192947	33.692199
894.036715	62629.066615	33.697216
894.783314	62725.613910	33.702234
895.345880	62827.375940	33.707252
896.490361	62931.215265	33.712269
897.385451	63024.667992	33.717287
897.978192	63147.290138	33.722304
899.049038	63235.777204	33.727322
900.255053	63353.676950	33.732340
900.983095	63456.830725	33.737357
902.070832	63548.733320	33.742375
903.080740	63649.484391	33.747392
903.863624	63753.392093	33.752410
904.684045	63860.218587	33.757428
905.423083	63962.779684	33.762445
906.765572	64066.912680	33.767463
907.887314	64183.182569	33.772480
908.413123	64278.484483	33.777498
909.742275	64357.881850	33.782516
910.409900	64475.621616	33.787533
911.115536	64578.305038	33.792551
912.431901	64694.995522	33.797568
913.302947	64804.721485	33.802586
914.021037	64890.411228	33.807604
914.837081	65003.977805	33.812621
915.953456	65088.430256	33.817639
916.847127	65193.503001	33.822656
917.420348	65311.954578	33.827674
918.977441	65401.801828	33.832692
919.745273	65515.732832	33.837709
920.031296	65627.391508	33.842727
921.636324	65727.875704	33.847744
922.384198	65828.307340	33.852762
923.518940	65928.804268	33.857780
924.373191	66048.690570	33.862797
925.148578	66149.381645	33.867815
926.384563	66250.628448	33.872832
927.262556	66344.438133	33.877850
928.699311	66447.896414	33.882868
929.232516	66546.316230	33.887885
930.053775	66636.115825	33.892903
931.218765	66724.796777	33.897920
932.154998	66808.091628	33.902938
932.771291	66905.789429	33.907956
933.698996	66994.010358	33.912973
934.320219	67076.235266	33.917991
934.998098	67169.411238	33.923008
935.837623	67269.816874	33.928026
937.111016	67378.050136	33.933044
937.974971	67474.754397	33.938061
938.824529	67584.651292	33.943079
939.811692	67682.729884	33.948096
940.801113	67790.347360	33.953114
941.583340	67870.973929	33.958132
942.935515	67980.770987	33.963149
943.534449	68077.112981	33.968167
944.570535	68191.137163	33.973184
945.279766	68302.870340	33.978202
946.478322	68404.418692	33.983220
947.280600	68505.278878	33.988237
947.902872	68624.867496	33.993255
948.814162	68728.889110	33.998272
949.552694	68843.741510	34.003290
950.545620	68959.735469	34.008308
951.830084	69069.928516	34.013325
952.887195	69188.585915	34.018343
953.930062	69282.595264	34.023360
955.100413	69414.679743	34.028378
956.151198	69517.685201	34.033396
957.017098	69614.737813	34.038413
957.772385	69740.661350	34.043431
958.911884	69842.473000	34.048448
959.521915	69968.989715	34.053466
960.702748	70080.961306	34.058484
961.943297	70192.494424	34.063501
962.916162	70299.578770	34.068519
963.831362	70407.102495	34.073536
964.647542	70527.777553	34.078554
965.827964	70634.281043	34.083572
966.801287	70750.585704	34.088589
967.218223	70860.800536	34.093607
968.386071	70978.377112	34.098624
969.385708	71087.527514	34.103642
970.323178	71203.935336	34.108660
971.320231	71333.059210	34.113677
971.813659	71451.352471	34.118695
973.139869	71556.605709	34.123712
973.883150	71682.998536	34.128730
974.685907	71806.236171	34.133748
976.057666	71928.859615	34.138765
977.089322	72044.480255	34.143783
978.168922	72168.876606	34.148800
979.238159	72300.971327	34.153818
980.114389	72412.846705	34.158836
981.070825	72517.917485	34.163853
981.771539	72653.997033	34.168871
983.008946	72734.855560	34.173888
983.556403	72869.425540	34.178906
985.065829	72954.449929	34.183924
985.914919	73058.175812	34.188941
986.747001	73192.614234	34.193959
988.073280	73303.563677	34.198976
988.907534	73400.197668	34.203994
989.772371	73526.361756	34.209012
990.739956	73623.291561	34.214029
991.506110	73728.771842	34.219047
992.862009	73843.030719	34.224064
993.541793	73967.761038	34.229082
994.449133	74093.106796	34.234100
995.431993	74203.957922	34.239117
996.368019	74321.635472	34.244135
997.751741	74436.379896	34.249152
998.086632	74549.579343	34.254170
999.265386	74682.550829	34.259188
1000.266388	74809.150027	34.264205
1001.287219	74939.026609	34.269223
1002.486683	75067.807635	34.274240
1003.548433	75185.059499	34.279258
1004.670786	75301.177543	34.284276
1005.674921	75415.697277	34.289293
1006.367655	75561.018051	34.294311
1007.592679	75676.439419	34.299328
1008.381106	75802.623693	34.304346
1009.322576	75927.014907	34.309364
1010.406468	76063.246291	34.314381
1011.223123	76179.999456	34.319399
1012.788123	76339.874130	34.324416
1013.378439	76466.485902	34.329434
1014.558552	76567.402898	34.334452
1015.613587	76730.774519	34.339469
1016.758940	76817.769236	34.344487
1017.849509	76981.617543	34.349504
1019.074256	77103.190141	34.354522
1020.154394	77196.510561	34.359540
1020.967796	77364.564651	34.364557
1022.115616	77467.640108	34.369575
1023.426246	77612.763563	34.374592
1024.309565	77728.592305	34.379610
1025.031933	77855.716320	34.384628
1026.309036	77980.743023	34.389645
1027.360615	78092.754895	34.394663
1028.085309	78236.743554	34.399680
1029.305904	78376.489183	34.404698
1030.339715	78480.915201	34.409716
1031.214965	78607.197921	34.414733
1032.107224	78773.734172	34.419751
1034.000900	78868.525615	34.424768
1034.869899	78990.747577	34.429786
1035.389361	79118.771338	34.434804
1036.555647	79244.670379	34.439821
1037.560517	79380.702707	34.444839
1038.711917	79476.127034	34.449856
1040.007507	79593.108028	34.454874
1040.809082	79702.178758	34.459892
1041.900431	79833.105746	34.464909
1042.754145	79914.408100	34.469927
1043.568996	80054.602661	34.474944
1045.019819	80145.014213	34.479962
1045.950140	80310.811009	34.484980
1046.766630	80394.877143	34.489997
1048.048305	80502.839093	34.495015
1048.590415	80661.431236	34.500032
1049.156843	80751.714336	34.505050
1050.411337	80914.474509	34.510068
1051.873549	81025.394077	34.515085
1052.205956	81150.027793	34.520103
1053.654602	81306.217654	34.525120
1054.616848	81413.261694	34.530138
1055.411842	81583.673198	34.535156
1056.923296	81685.485660	34.540173
1057.782157	81856.034632	34.545191
1058.792059	81958.187399	34.550208
1060.119500	82109.313773	34.555226
1061.305938	82253.181189	34.560244
1062.553339	82359.622124	34.565261
1063.493654	82537.648538	34.570279
1064.385537	82640.961334	34.575296
1065.915530	82772.248044	34.580314
1066.409969	82948.901209	34.585332
1067.704068	83053.169875	34.590349
1068.951163	83208.312400	34.595367
1069.869107	83324.040623	34.600384
1070.788359	83495.193966	34.605402
1071.794837	83602.084166	34.610420
1073.125815	83757.331210	34.615437
1073.873498	83884.835993	34.620455
1074.750806	84030.718340	34.625472
1076.078830	84209.007071	34.630490
1076.972836	84316.038917	34.635508
1078.386025	84469.014785	34.640525
1079.195839	84644.386556	34.645543
1080.466312	84757.506058	34.650560
1081.632567	84906.345303	34.655578
1082.669977	85093.652907	34.660596
1083.574073	85217.568684	34.665613
1084.631929	85350.470335	34.670631
1086.232009	85499.402813	34.675648
1087.346979	85666.780723	34.680666
1088.310160	85808.008236	34.685684
1089.550444	85924.426571	34.690701
1090.419913	86064.469384	34.695719
1092.092616	86188.047282	34.700736
1092.538860	86373.721457	34.705754
1093.534694	86488.379757	34.710772
1095.130711	86605.377527	34.715789
1095.988849	86794.751982	34.720807
1096.855617	86893.284155	34.725824
1098.295211	87040.564724	34.730842
1099.099440	87173.385328	34.735860
1100.058641	87298.569083	34.740877
1101.232504	87415.809171	34.745895
1101.885110	87583.326264	34.750912
1103.061289	87690.911976	34.755930
1104.253160	87863.631701	34.760948
1105.584960	87971.276272	34.765965
1106.407273	88150.234956	34.770983
1107.677869	88245.705526	34.776000
1109.192363	88423.538325	34.781018
1110.011239	88567.001256	34.786036
1110.965690	88670.504234	34.791053
1112.174815	88856.097539	34.796071
1113.232976	89000.043824	34.801088
1114.629538	89099.848793	34.806106
1115.763859	89274.131955	34.811124
1116.868829	89390.419922	34.816141
1117.867886	89569.653159	34.821159
1119.124647	89678.241468	34.826176
1120.454431	89815.737642	34.831194
1121.184262	89996.693050	34.836212
1122.633014	90099.675255	34.841229
1123.482699	90287.981406	34.846247
1124.520288	90400.276100	34.851264
1126.091001	90580.931880	34.856282
1127.006075	90705.396176	34.861300
1128.081925	90864.112486	34.866317
1129.852562	90993.836857	34.871335
1130.190373	91169.944141	34.876352
1131.786823	91281.465150	34.881370
1132.481179	91469.976962	34.886388
1133.170062	91621.715021	34.891405
1134.882398	91756.531664	34.896423
1136.148910	91924.711964	34.901440
1137.434910	92051.654713	34.906458
1138.287838	92246.333332	34.911476
1139.581891	92361.727967	34.916493
1140.548360	92537.537530	34.921511
1141.785900	92668.817601	34.926528
1142.838319	92840.397356	34.931546
1143.613544	93000.966835	34.936564
1145.008083	93119.809110	34.941581
1146.542777	93312.845467	34.946599
1147.721286	93454.619891	34.951616
1148.697002	93610.348664	34.956634
1149.647111	93775.247510	34.961652
1151.192541	93920.616081	34.966669
1152.130693	94067.227023	34.971687
1152.934344	94243.493493	34.976704
1154.362038	94370.933053	34.981722
1155.066876	94567.869455	34.986740
1156.645637	94708.544574	34.991757
1157.541059	94863.150025	34.996775
1158.752318	95019.698801	35.001792
1159.823387	95179.933367	35.006810
1160.682828	95306.956297	35.011828
1162.097076	95457.998047	35.016845
1163.178918	95618.632548	35.021863
1164.501113	95776.408780	35.026880
1166.064455	95907.282970	35.031898
1166.627639	96083.652803	35.036916
1167.962291	96225.084760	35.041933
1168.990549	96365.699709	35.046951
1170.185998	96516.119181	35.051968
1171.589958	96677.361583	35.056986
1172.440663	96834.429497	35.062004
1173.746901	96993.070795	35.067021
1175.029483	97140.633926	35.072039
1175.651724	97317.775785	35.077056
1177.353759	97451.825200	35.082074
1178.358971	97644.160759	35.087092
1179.740105	97779.604276	35.092109
1180.719532	97962.862339	35.097127
1181.888161	98123.216202	35.102144
1183.217697	98281.926087	35.107162
1184.254289	98447.180775	35.112180
1185.483156	98625.653460	35.117197
1187.081293	98758.582050	35.122215
1188.437925	98917.095937	35.127232
1189.831973	99095.539707	35.132250
1191.221564	99234.432149	35.137268
1192.207617	99411.507145	35.142285
1193.225106	99537.877061	35.147303
1194.302982	99724.113448	35.152320
1195.851390	99858.435558	35.157338
1196.564693	100046.668503	35.162356
1197.966925	100192.473547	35.167373
1199.077843	100344.159172	35.172391
1200.302420	100535.547823	35.177408
1201.852040	100678.036205	35.182426
1203.055518	100866.223210	35.187444
1204.060262	101008.958456	35.192461
1205.258988	101193.877823	35.197479
1206.410695	101328.967573	35.202496
1207.732035	101504.841167	35.207514
1208.789242	101667.616527	35.212532
1209.885816	101849.843012	35.217549
1211.475914	101984.322730	35.222567
1212.519864	102209.250547	35.227584
1213.359951	102350.128358	35.232602
1214.950628	102484.421058	35.237620
1216.108112	102691.840204	35.242637
1216.844314	102843.728324	35.247655
1218.129632	103018.752224	35.252672
1220.349779	103161.427654	35.257690
1220.976383	103373.138781	35.262708
1222.079070	103513.532590	35.267725
1223.681107	103686.397674	35.272743
1224.484156	103850.152521	35.277760
1225.802830	103994.539331	35.282778
1227.428698	104138.169464	35.287796
1228.216520	104294.140236	35.292813
1229.505060	104466.326869	35.297831
1230.747157	104596.441059	35.302848
1231.694470	104763.526818	35.307866
1232.639566	104926.570476	35.312884
1233.991519	105084.937376	35.317901
1235.252423	105263.253495	35.322919
1236.244990	105419.300388	35.327936
1237.268736	105591.151295	35.332954
1238.928290	105761.225356	35.337972
1240.192158	105919.681449	35.342989
1241.491911	106117.103041	35.348007
1242.241075	106261.347434	35.353024
1243.773652	106446.552530	35.358042
1245.185263	106636.467730	35.363060
1246.519152	106789.051934	35.368077
1247.676836	106966.992202	35.373095
1248.748562	107155.915020	35.378112
1250.348810	107311.643521	35.383130
1251.462254	107514.030001	35.388148
1252.135513	107665.845130	35.393165
1253.585669	107876.623737	35.398183
1254.977007	108038.105115	35.403200
1256.247650	108236.004478	35.408218
1257.347794	108416.603797	35.413236
1258.600566	108592.794177	35.418253
1260.129721	108781.036776	35.423271
1261.362306	108996.511632	35.428288
1262.235749	109151.677706	35.433306
1263.875719	109367.407547	35.438324
1264.990795	109520.550182	35.443341
1266.132847	109730.495171	35.448359
1267.662603	109917.360366	35.453376
1268.901853	110113.590101	35.458394
1270.436214	110273.133157	35.463412
1271.781254	110499.502796	35.468429
1273.045150	110649.185596	35.473447
1274.597549	110837.731572	35.478464
1275.548857	111061.137114	35.483482
1277.017514	111229.495102	35.488500
1278.156663	111421.769844	35.493517
1279.478262	111585.507602	35.498535
1280.512071	111797.101620	35.503552
1282.583773	111958.716041	35.508570
1283.368968	112163.149292	35.513588
1284.887556	112348.730814	35.518605
1286.393029	112507.229535	35.523623
1287.584576	112730.295501	35.528640
1288.677492	112880.886273	35.533658
1290.246527	113077.922797	35.538676
1291.619493	113252.443746	35.543693
1292.665880	113422.276459	35.548711
1293.475347	113606.119019	35.553728
1294.816151	113779.351057	35.558746
1296.538479	113940.236316	35.563764
1297.311649	114114.200289	35.568781
1299.075333	114274.922869	35.573799
1300.248932	114464.797463	35.578816
1301.222180	114621.292513	35.583834
1302.467187	114795.129228	35.588852
1303.838842	114991.022066	35.593869
1305.139638	115136.636473	35.598887
1306.220254	115369.796806	35.603904
1307.722486	115501.466272	35.608922
1309.167665	115720.226295	35.613940
1310.101563	115870.917309	35.618957
1311.626626	116086.166814	35.623975
1313.093299	116263.776985	35.628992
1313.648323	116467.313323	35.634010
1315.360547	116646.393927	35.639028
1316.493055	116838.800022	35.644045
1317.857368	117044.833421	35.649063
1319.155841	117241.198491	35.654080
1320.137047	117427.928642	35.659098
1321.466082	117648.521814	35.664116
1322.765134	117830.468539	35.669133
1324.352052	118054.905358	35.674151
1325.965943	118237.887603	35.679168
1327.158398	118464.543414	35.684186
1329.241801	118637.475371	35.689204
1329.804267	118849.659423	35.694221
1331.901537	119042.466901	35.699239
1332.978731	119237.920010	35.704256
1334.567398	119444.456217	35.709274
1336.098085	119613.949452	35.714292
1337.108642	119841.779666	35.719309
1338.960096	120008.324494	35.724327
1340.532963	120185.735993	35.729344
1341.680842	120391.722947	35.734362
1343.320885	120571.310941	35.739380
1344.279850	120769.175226	35.744397
1345.761798	120949.620461	35.749415
1346.987861	121131.855301	35.754432
1348.138954	121347.296911	35.759450
1349.926589	121536.575409	35.764468
1350.888714	121719.223561	35.769485
1352.639551	121932.155693	35.774503
1354.250568	122106.471300	35.779520
1355.068360	122298.797034	35.784538
1356.365360	122494.936163	35.789556
1357.550361	122695.641333	35.794573
1359.168275	122881.258263	35.799591
1360.178736	123078.625133	35.804608
1361.206703	123307.008288	35.809626
1362.998306	123459.646259	35.814644
1363.952978	123699.532042	35.819661
1365.429285	123869.105741	35.824679
1366.736827	124088.420533	35.829696
1367.928584	124248.124559	35.834714
1369.328350	124460.132207	35.839732
1370.913415	124643.182799	35.844749
1372.348967	124823.294531	35.849767
1373.581114	125039.424571	35.854784
1374.565055	125201.079915	35.859802
1376.516035	125413.197484	35.864820
1377.508161	125596.513485	35.869837
1378.927024	125787.185530	35.874855
1380.037022	125992.386035	35.879872
1381.346073	126202.863843	35.884890
1382.463293	126407.673679	35.889908
1383.919784	126598.345462	35.894925
1385.225803	126807.916429	35.899943
1386.683082	127027.142689	35.904960
1388.040352	127245.107215	35.909978
1389.883379	127434.279358	35.914996
1391.124659	127672.128160	35.920013
1392.444341	127861.741133	35.925031
1394.089464	128075.536913	35.930048
1395.232336	128301.689245	35.935066
1396.916542	128505.829336	35.940084
1398.093791	128711.495663	35.945101
1399.773950	128928.016121	35.950119
1401.225409	129150.769353	35.955136
1402.696817	129356.938474	35.960154
1404.354892	129565.562459	35.965172
1405.590673	129773.000957	35.970189
1406.827894	129995.605013	35.975207
1408.106497	130214.935766	35.980224
1409.691853	130429.278690	35.985242
1411.084162	130644.072016	35.990260
1412.520270	130861.216455	35.995277
1413.925445	131070.183306	36.000295
1415.438367	131292.905931	36.005312
1417.135673	131507.340688	36.010330
1418.424089	131725.592186	36.015348
1420.078318	131932.954890	36.020365
1421.436702	132142.405931	36.025383
1423.266810	132364.313798	36.030400
1424.836828	132567.551594	36.035418
1425.880121	132770.532475	36.040436
1427.012377	132989.743462	36.045453
1428.592976	133215.397264	36.050471
1430.510520	133421.968847	36.055488
1431.693059	133641.189540	36.060506
1433.275047	133836.984462	36.065524
1434.448921	134058.236979	36.070541
1435.967431	134269.806893	36.075559
1437.592609	134479.473507	36.080576
1438.983544	134689.432294	36.085594
1440.823320	134897.724776	36.090612
1441.672757	135135.927257	36.095629
1443.929252	135300.910905	36.100647
1444.894256	135520.028483	36.105664
1446.069782	135685.110084	36.110682
1447.440877	135890.620560	36.115700
1448.939920	136060.138484	36.120717
1450.125537	136297.270740	36.125735
1451.458326	136454.424817	36.130752
1452.839307	136695.812217	36.135770
1454.319736	136861.447621	36.140788
1455.642314	137113.998766	36.145805
1456.928031	137300.474541	36.150823
1458.532578	137523.269105	36.155840
1459.917300	137726.927606	36.160858
1461.403722	137936.856699	36.165876
1462.882902	138148.499181	36.170893
1463.984286	138373.572433	36.175911
1465.725243	138591.652018	36.180928
1467.029539	138827.531336	36.185946
1468.852345	139031.864247	36.190964
1470.569569	139249.483573	36.195981
1472.248258	139473.523011	36.200999
1474.114726	139668.779712	36.206016
1475.136660	139883.143198	36.211034
1476.939615	140101.642241	36.216052
1478.293257	140294.525973	36.221069
1479.396651	140544.023676	36.226087
1480.776021	140738.832504	36.231104
1482.212528	140961.020599	36.236122
1483.749329	141200.924541	36.241140
1485.537570	141412.198941	36.246157
1487.176881	141625.640328	36.251175
1488.547908	141862.331426	36.256192
1490.016317	142085.245137	36.261210
1491.634454	142293.092773	36.266228
1493.070029	142536.090479	36.271245
1494.319014	142734.266157	36.276263
1495.955878	142975.131486	36.281280
1497.783937	143185.182518	36.286298
1498.878758	143431.245301	36.291316
1501.011185	143635.344808	36.296333
1501.952656	143876.631913	36.301351
1503.950894	144108.880745	36.306368
1505.064854	144321.702027	36.311386
1506.570443	144566.010213	36.316404
1508.592171	144759.690706	36.321421
1509.415969	145003.489605	36.326439
1510.741409	145238.439535	36.331456
1512.395691	145468.129484	36.336474
1514.025247	145696.304021	36.341492
1515.325109	145952.748051	36.346509
1517.199430	146150.136504	36.351527
1518.878311	146402.150961	36.356544
1519.918967	146614.162995	36.361562
1521.502589	146875.551038	36.366580
1523.388635	147076.999715	36.371597
1524.372218	147308.039287	36.376615
1525.877771	147542.876488	36.381632
1527.124244	147746.015558	36.386650
1528.879246	147998.119424	36.391668
1530.489123	148207.529154	36.396685
1531.792179	148411.728308	36.401703
1533.220336	148654.343987	36.406720
1534.874175	148872.802124	36.411738
1536.524695	149101.898004	36.416756
1538.194522	149294.343975	36.421773
1539.871529	149560.188821	36.426791
1541.085251	149754.953821	36.431808
1543.021500	149953.902714	36.436826
1544.414249	150196.484981	36.441844
1545.493013	150466.336896	36.446861
1547.253884	150664.126373	36.451879
1548.953489	150920.711749	36.456896
1550.298540	151135.316984	36.461914
1552.089584	151395.289140	36.466932
1553.545167	151610.361693	36.471949
1554.904307	151870.609094	36.476967
1556.522708	152062.686685	36.481984
1557.976875	152338.224839	36.487002
1559.555703	152594.043839	36.492020
1561.135554	152816.749415	36.497037
1562.673782	153051.748285	36.502055
1564.652170	153290.228823	36.507072
1566.189903	153547.114035	36.512090
1567.835276	153758.658563	36.517108
1569.569320	154024.239070	36.522125
1571.193824	154248.887001	36.527143
1572.793744	154506.479745	36.532160
1574.510088	154729.594868	36.537178
1576.026234	154992.124048	36.542196
1577.532405	155209.075749	36.547213
1578.942337	155450.426062	36.552231
1581.027022	155705.478571	36.557248
1582.433484	155925.506412	36.562266
1584.220900	156185.529332	36.567284
1585.857456	156426.305398	36.572301
1587.389072	156639.597869	36.577319
1589.214871	156911.602432	36.582336
1590.361669	157135.432535	36.587354
1592.107941	157355.111331	36.592372
1593.896360	157628.091200	36.597389
1595.248086	157856.306071	36.602407
1597.197337	158069.731317	36.607424
1598.668957	158349.360879	36.612442
1600.224742	158552.935711	36.617460
1602.333072	158821.689731	36.622477
1603.541611	159042.656659	36.627495
1604.953738	159309.673702	36.632512
1606.373397	159531.218862	36.637530
1608.426106	159744.967689	36.642548
1610.305860	160022.491608	36.647565
1611.278301	160249.273440	36.652583
1613.027003	160461.401054	36.657600
1614.586563	160722.762430	36.662618
1615.858595	160913.423385	36.667636
1617.993757	161104.138489	36.672653
1619.414535	161386.831222	36.677671
1620.967826	161576.005407	36.682688
1622.266902	161827.448772	36.687706
1623.750645	162029.698308	36.692724
1625.510527	162278.471951	36.697741
1626.559923	162508.489823	36.702759
1628.859822	162720.771667	36.707776
1630.294215	163002.878997	36.712794
1631.352597	163227.408802	36.717812
1633.596589	163443.330830	36.722829
1635.213360	163727.532758	36.727847
1636.765639	163937.150455	36.732864
1638.550427	164200.555988	36.737882
1640.001510	164452.602300	36.742900
1642.193344	164654.804830	36.747917
1643.047102	164949.004429	36.752935
1645.274847	165142.757387	36.757952
1647.102731	165419.177222	36.762970
1648.487659	165685.447157	36.767988
1650.414602	165901.751176	36.773005
1651.839904	166173.865024	36.778023
1653.783912	166411.514746	36.783040
1655.412925	166660.237654	36.788058
1656.998481	166919.661077	36.793076
1658.474795	167168.551149	36.798093
1660.473531	167394.745440	36.803111
1661.899784	167674.911365	36.808128
1663.744622	167913.639135	36.813146
1665.025589	168193.882735	36.818164
1667.009662	168410.217596	36.823181
1668.443668	168685.582676	36.828199
1670.125602	168949.304611	36.833216
1671.743038	169194.215591	36.838234
1673.709590	169484.392876	36.843252
1675.278508	169712.977808	36.848269
1676.645945	169999.448906	36.853287
1678.302901	170250.968873	36.858304
1680.526069	170502.869886	36.863322
1681.808908	170813.435499	36.868340
1683.756980	171029.549905	36.873357
1685.586243	171294.875509	36.878375
1686.972183	171604.974439	36.883392
1688.007253	171848.891210	36.888410
1690.484972	172088.724177	36.893428
1692.277303	172398.384318	36.898445
1693.344308	172647.945829	36.903463
1696.029264	172889.628181	36.908480
1697.431524	173200.003518	36.913498
1698.860198	173449.918592	36.918516
1701.390051	173672.500838	36.923533
1702.619925	173962.587451	36.928551
1704.065151	174196.203685	36.933568
1705.883877	174412.851967	36.938586
1707.242103	174706.399468	36.943604
1709.282272	174943.629826	36.948621
1710.568378	175174.080192	36.953639
1712.224195	175429.299642	36.958656
1714.171230	175671.927934	36.963674
1715.522426	175922.314729	36.968692
1717.075912	176204.906648	36.973709
1718.975966	176451.847690	36.978727
1720.434814	176710.417586	36.983744
1722.360622	176976.108190	36.988762
1723.982645	177227.576382	36.993780
1725.620526	177513.982576	36.998797
1727.667566	177758.028263	37.003815
1729.373806	178049.501994	37.008832
1731.475893	178271.035581	37.013850
1732.793798	178575.274219	37.018868
1734.557763	178825.930284	37.023885
1736.181530	179112.235539	37.028903
1738.220196	179374.827911	37.033920
1739.834720	179647.918217	37.038938
1741.443483	179889.445048	37.043956
1743.546122	180196.082895	37.048973
1745.074340	180462.937248	37.053991
1746.849075	180736.021807	37.059008
1748.910328	181022.372006	37.064026
1750.343576	181281.836940	37.069044
1752.427169	181582.207316	37.074061
1753.963769	181840.885250	37.079079
1755.831530	182145.100194	37.084096
1757.788532	182409.081804	37.089114
1759.194553	182708.108445	37.094132
1761.293536	182975.471379	37.099149
1762.992004	183270.788527	37.104167
1764.459718	183542.835650	37.109184
1766.257682	183841.363692	37.114202
1768.044302	184103.136694	37.119220
1770.057646	184416.721157	37.124237
1771.700912	184687.275556	37.129255
1773.635741	184977.186533	37.134272
1775.500306	185245.767787	37.139290
1777.032254	185555.401605	37.144308
1779.325065	185831.176474	37.149325
1781.317694	186098.245173	37.154343
1782.804257	186384.911834	37.159360
1784.841866	186676.390888	37.164378
1786.511660	186933.135895	37.169396
1788.725608	187242.406469	37.174413
1790.546660	187491.009328	37.179431
1792.200272	187774.257381	37.184448
1794.246377	188056.213957	37.189466
1795.534196	188325.234866	37.194484
1797.585967	188607.384241	37.199501
1799.397564	188881.071209	37.204519
1801.033173	189140.892179	37.209536
1802.894325	189368.750601	37.214554
1804.379169	189644.790804	37.219572
1806.381758	189887.476732	37.224589
1808.023812	190150.715914	37.229607
1809.732741	190399.567796	37.234624
1811.436462	190675.591948	37.239642
1813.054883	190941.846884	37.244660
1815.480428	191190.132265	37.249677
1816.814006	191470.268044	37.254695
1818.181583	191743.610537	37.259712
1820.081916	192006.247837	37.264730
1821.599667	192286.156052	37.269748
1823.315518	192566.415155	37.274765
1825.213239	192866.660658	37.279783
1826.505076	193148.132595	37.284800
1828.520631	193428.234830	37.289818
1830.262129	193756.088377	37.294836
1832.074548	194029.918742	37.299853
1833.958853	194357.537840	37.304871
1835.578989	194624.777114	37.309888
1837.598376	194957.671027	37.314906
1839.480575	195248.262477	37.319924
1841.169718	195565.665648	37.324941
1843.406619	195879.595158	37.329959
1845.374211	196173.820894	37.334976
1847.272043	196475.687225	37.339994
1848.891604	196799.962751	37.345012
1851.477335	197104.693503	37.350029
1853.105496	197393.674841	37.355047
1854.787715	197725.599578	37.360064
1856.952152	198019.931530	37.365082
1858.970348	198321.662605	37.370100
1860.258877	198625.503951	37.375117
1862.262227	198946.089203	37.380135
1864.304029	199263.116377	37.385152
1866.132454	199559.452235	37.390170
1867.880031	199895.111901	37.395188
1869.928704	200195.046441	37.400205
1872.146000	200514.045950	37.405223
1873.657860	200822.560720	37.410240
1875.931685	201136.757001	37.415258
1877.932728	201447.583957	37.420276
1879.237862	201752.684294	37.425293
1881.450834	202074.778074	37.430311
1883.111709	202380.053900	37.435328
1885.322498	202704.322252	37.440346
1887.236704	203017.773987	37.445364
1889.157514	203315.676885	37.450381
1890.975895	203644.595340	37.455399
1893.085469	203974.611926	37.460416
1894.975109	204266.469927	37.465434
1897.242363	204588.759973	37.470452
1898.759217	204892.079378	37.475469
1901.095068	205203.724550	37.480487
1902.454697	205484.438768	37.485504
1904.463067	205776.780684	37.490522
1906.341932	206066.605806	37.495540
1907.727487	206328.634254	37.500557
1910.050934	206628.280363	37.505575
1911.496176	206919.841479	37.510592
1913.282558	207231.305435	37.515610
1915.243375	207509.623571	37.520628
1916.879034	207827.131731	37.525645
1919.027659	208137.210011	37.530663
1920.618788	208433.426982	37.535680
1922.667638	208759.963845	37.540698
1924.895018	209062.709547	37.545716
1926.405622	209366.116392	37.550733
1928.409992	209683.778897	37.555751
1930.433605	210020.799789	37.560768
1932.068614	210324.712113	37.565786
1934.203707	210633.967355	37.570804
1936.007536	210980.422695	37.575821
1938.040897	211282.372191	37.580839
1939.714698	211620.257039	37.585856
1941.915916	211946.976951	37.590874
1943.679130	212282.451712	37.595892
1945.649155	212593.570886	37.600909
1947.957705	212941.150198	37.605927
1949.587170	213281.805785	37.610944
1951.629746	213602.465395	37.615962
1953.831333	213938.907529	37.620980
1955.852193	214291.960780	37.625997
1957.544195	214606.396506	37.631015
1959.488900	214975.500357	37.636032
1961.695341	215304.191442	37.641050
1963.308572	215644.265069	37.646068
1965.528622	215984.142538	37.651085
1967.904437	216296.903341	37.656103
1969.406388	216668.981434	37.661120
1972.072281	217002.280043	37.666138
1974.050041	217323.539039	37.671156
1975.951994	217683.878460	37.676173
1978.543317	218004.205263	37.681191
1979.983837	218367.643186	37.686208
1982.004828	218683.899112	37.691226
1983.965339	219027.819389	37.696244
1985.915504	219365.089872	37.701261
1987.615221	219707.670846	37.706279
1990.156469	220040.229054	37.711296
1991.927962	220394.127465	37.716314
1994.213301	220711.124833	37.721332
1995.824958	221085.989235	37.726349
1998.058061	221394.592386	37.731367
1999.526348	221766.080141	37.736384
2001.899019	222095.830178	37.741402
2004.040908	222424.069208	37.746420
2005.834295	222789.885517	37.751437
2008.175441	223102.313082	37.756455
2010.223515	223434.850343	37.761472
2011.916631	223812.851544	37.766490
2013.710262	224132.480726	37.771508
2015.942342	224435.687144	37.776525
2018.037285	224764.565710	37.781543
2019.311909	225096.001054	37.786560
2021.322302	225405.099977	37.791578
2023.257591	225746.591365	37.796596
2024.933866	226093.826621	37.801613
2027.083801	226415.490816	37.806631
2029.195742	226768.043707	37.811648
2031.086581	227108.684359	37.816666
2033.367319	227442.509174	37.821684
2035.028625	227797.106112	37.826701
2037.132679	228136.955216	37.831719
2039.215102	228510.256190	37.836736
2041.126142	228844.170568	37.841754
2043.042528	229211.075601	37.846772
2045.063025	229578.245023	37.851789
2047.493624	229937.909637	37.856807
2049.373844	230292.609045	37.861824
2051.559143	230667.096548	37.866842
2053.423088	231030.385658	37.871860
2055.534745	231403.998999	37.876877
2057.851991	231764.704790	37.881895
2059.801833	232145.407282	37.886912
2061.844233	232512.178786	37.891930
2064.347585	232880.935801	37.896948
2065.931845	233249.713083	37.901965
2068.365744	233631.157507	37.906983
2070.358335	234006.450959	37.912000
2072.506483	234384.337179	37.917018
2074.864364	234743.701734	37.922036
2076.449033	235128.258322	37.927053
2078.950520	235499.692390	37.932071
2080.698287	235885.419726	37.937088
2082.840382	236257.218371	37.942106
2085.317950	236647.683922	37.947124
2087.115652	237018.244615	37.952141
2089.316070	237398.902251	37.957159
2091.590788	237775.917429	37.962176
2093.781776	238166.637272	37.967194
2096.198765	238531.034639	37.972212
2098.083164	238917.945170	37.977229
2100.752087	239271.561195	37.982247
2102.723411	239658.155734	37.987264
2104.692015	240020.927389	37.992282
2107.055131	240400.096489	37.997300
2108.822082	240768.617396	38.002317
2111.243734	241137.619810	38.007335
2113.384480	241511.697095	38.012352
2115.449519	241881.698202	38.017370
2117.732918	242253.799406	38.022388
2119.747346	242627.798619	38.027405
2121.636496	242977.612608	38.032423
2123.888297	243326.836658	38.037440
2126.171734	243663.661378	38.042458
2128.721583	243993.916875	38.047476
2130.360867	244347.914558	38.052493
2132.585478	244675.734173	38.057511
2134.797472	245020.244706	38.062528
2136.550224	245356.167413	38.067546
2138.663486	245698.536329	38.072564
2140.761502	246041.035536	38.077581
2143.158037	246408.634951	38.082599
2145.119419	246754.764516	38.087616
2147.082133	247109.505609	38.092634
2149.054287	247464.931920	38.097652
2150.617773	247822.811626	38.102669
2152.677310	248190.951749	38.107687
2154.890646	248568.238194	38.112704
2157.108164	248941.740159	38.117722
2159.553124	249318.636138	38.122740
2161.187174	249705.517363	38.127757
2163.723632	250083.340547	38.132775
2165.855699	250481.372089	38.137792
2167.556003	250844.571495	38.142810
2170.387681	251235.940360	38.147828
2172.083889	251630.970267	38.152845
2174.298194	252013.573734	38.157863
2176.731806	252405.719716	38.162880
2178.759328	252802.528713	38.167898
2180.925543	253208.385052	38.172916
2183.273862	253606.084831	38.177933
2185.529616	253996.560611	38.182951
2187.712981	254400.283123	38.187968
2189.730456	254798.291948	38.192986
2192.441579	255191.949435	38.198004
2194.176716	255596.990245	38.203021
2196.408200	255997.787196	38.208039
2199.064146	256397.450721	38.213056
2201.147668	256797.180396	38.218074
2203.733284	257203.943844	38.223092
2205.973300	257593.336836	38.228109
2208.367357	257999.090641	38.233127
2210.603155	258401.237718	38.238144
2212.969649	258802.196249	38.243162
2215.563629	259175.506814	38.248180
2217.634146	259584.185159	38.253197
2219.874894	259965.402342	38.258215
2222.089114	260360.722781	38.263232
2224.229412	260756.639803	38.268250
2226.623942	261144.184994	38.273268
2228.549447	261549.307623	38.278285
2231.137091	261926.509752	38.283303
2233.666967	262318.455180	38.288320
2235.488338	262718.362968	38.293338
2237.934489	263099.043808	38.298356
2239.895272	263490.242683	38.303373
2242.401090	263885.293054	38.308391
2244.576957	264244.705006	38.313408
2246.841688	264612.791071	38.318426
2248.720194	264971.920679	38.323444
2250.657813	265339.322661	38.328461
2252.791288	265709.005618	38.333479
2254.929737	266079.932883	38.338496
2257.028461	266467.505837	38.343514
2259.296316	266831.224158	38.348532
2261.244904	267216.535299	38.353549
2263.061762	267611.495461	38.358567
2265.364299	268003.203525	38.363584
2267.558056	268407.173500	38.368602
2269.390481	268816.078499	38.373620
2271.678023	269223.844688	38.378637
2274.312560	269637.957760	38.383655
2276.234870	270039.177539	38.388672
2278.560114	270477.244691	38.393690
2281.130313	270885.652969	38.398708
2283.496431	271305.550726	38.403725
2285.596440	271734.331249	38.408743
2287.930931	272153.065855	38.413760
2289.925389	272586.131242	38.418778
2292.698479	273007.768817	38.423796
2295.007110	273448.456504	38.428813
2297.217184	273884.638132	38.433831
2299.782775	274296.909688	38.438848
2301.990203	274742.846818	38.443866
2304.506477	275168.310693	38.448884
2306.718628	275610.970130	38.453901
2309.129581	276039.753203	38.458919
2311.649258	276476.495707	38.463936
2313.962302	276901.102715	38.468954
2316.579283	277351.979427	38.473972
2318.698602	277777.353745	38.478989
2321.231972	278207.997050	38.484007
2323.889259	278635.445184	38.489024
2326.186413	279080.758071	38.494042
2328.739938	279504.792938	38.499060
2331.076274	279935.136716	38.504077
2333.266673	280360.422780	38.509095
2335.853222	280791.996680	38.514112
2337.844176	281226.662380	38.519130
2340.606310	281655.388215	38.524148
2342.815433	282083.744209	38.529165
2345.292785	282515.283622	38.534183
2347.585873	282933.743865	38.539200
2350.000561	283375.606324	38.544218
2352.604985	283802.475851	38.549236
2354.754210	284235.285334	38.554253
2357.223511	284658.212664	38.559271
2359.361492	285095.722744	38.564288
2361.590193	285509.923344	38.569306
2364.321413	285956.407436	38.574324
2366.593410	286379.338980	38.579341
2368.919400	286814.048524	38.584359
2371.421551	287211.971470	38.589376
2373.561676	287616.708567	38.594394
2375.602362	288017.548905	38.599412
2378.234736	288407.295502	38.604429
2380.486361	288814.121940	38.609447
2382.846594	289225.426948	38.614464
2384.766056	289644.955588	38.619482
2387.241849	290039.678527	38.624500
2389.392403	290468.339771	38.629517
2391.043771	290890.805020	38.634535
2393.907232	291310.689627	38.639552
2396.202087	291755.990138	38.644570
2398.603976	292184.481801	38.649588
2401.330564	292621.202498	38.654605
2403.293177	293053.775897	38.659623
2405.758926	293502.348515	38.664640
2408.363709	293937.409553	38.669658
2410.576724	294374.310023	38.674676
2412.759878	294832.196672	38.679693
2415.111565	295286.753346	38.684711
2417.821054	295738.737511	38.689728
2420.288847	296194.035874	38.694746
2422.467753	296663.629568	38.699764
2424.866774	297122.238985	38.704781
2427.327577	297582.742666	38.709799
2430.036606	298046.457324	38.714816
2432.617521	298506.025226	38.719834
2435.218159	298983.827304	38.724852
2437.760113	299440.223767	38.729869
2439.969145	299918.949029	38.734887
2442.514946	300370.922532	38.739904
2444.886693	300851.524478	38.744922
2447.177945	301326.905083	38.749940
2449.976313	301799.435164	38.754957
2452.359100	302274.773036	38.759975
2455.056147	302744.420583	38.764992
2457.539637	303225.175410	38.770010
2459.716940	303698.280714	38.775028
2462.397116	304167.545458	38.780045
2464.784100	304643.154561	38.785063
2467.610561	305123.670975	38.790080
2470.151138	305596.331438	38.795098
2472.666964	306076.004765	38.800116
2475.279966	306559.521872	38.805133
2477.729310	307034.020618	38.810151
2480.034604	307508.464279	38.815168
2482.459014	307984.081134	38.820186
2485.153705	308450.864936	38.825204
2487.777769	308928.656413	38.830221
2490.404271	309420.314023	38.835239
2493.099283	309882.520393	38.840256
2495.334782	310355.846693	38.845274
2497.790409	310842.064632	38.850292
2500.372511	311301.489411	38.855309
2502.753256	311773.389989	38.860327
2505.171787	312211.831721	38.865344
2507.429153	312668.610126	38.870362
2510.202764	313100.947092	38.875380
2513.014385	313546.941007	38.880397
2514.684198	313989.177197	38.885415
2517.364634	314428.127363	38.890432
2519.774756	314875.398527	38.895450
2522.238361	315338.457232	38.900468
2524.850767	315787.114752	38.905485
2526.865455	316251.383424	38.910503
2529.549857	316726.566684	38.915520
2531.803019	317193.561634	38.920538
2534.093557	317654.554529	38.925556
2536.991799	318134.344983	38.930573
2539.121147	318623.728256	38.935591
2541.788269	319109.290362	38.940608
2544.411381	319591.707662	38.945626
2546.644031	320074.616099	38.950644
2549.402196	320554.848230	38.955661
2552.015890	321049.297706	38.960679
2554.334074	321543.308763	38.965696
2557.119040	322043.770114	38.970714
2559.891380	322554.719457	38.975732
2562.414772	323047.115019	38.980749
2565.017268	323558.974263	38.985767
2567.663809	324049.770011	38.990784
2570.369591	324557.670484	38.995802
2572.809381	325064.060880	39.000820
2575.672691	325567.003452	39.005837
2578.058251	326073.929566	39.010855
2580.929468	326574.452113	39.015872
2583.810869	327092.746636	39.020890
2585.861793	327588.009026	39.025908
2588.759134	328087.959252	39.030925
2591.550019	328615.044789	39.035943
2594.295922	329114.834654	39.040960
2597.115581	329631.623863	39.045978
2599.124269	330155.648440	39.050996
2602.083055	330659.178171	39.056013
2604.780747	331179.302711	39.061031
2607.331798	331693.733228	39.066048
2610.053888	332206.431664	39.071066
2612.237664	332727.236070	39.076084
2615.211871	333227.266803	39.081101
2617.640715	333756.683975	39.086119
2620.311948	334259.980338	39.091136
2623.141994	334781.352881	39.096154
2625.578708	335308.471728	39.101172
2628.653208	335810.728039	39.106189
2631.201156	336340.030447	39.111207
2633.872697	336852.702845	39.116224
2636.616683	337374.399281	39.121242
2639.040055	337892.181340	39.126260
2642.274588	338389.898672	39.131277
2644.488142	338903.389469	39.136295
2647.373776	339378.911912	39.141312
2650.194268	339861.398214	39.146330
2652.034952	340336.520487	39.151348
2654.745557	340811.349052	39.156365
2657.398435	341294.384190	39.161383
2659.714007	341783.714946	39.166400
2662.422275	342271.100792	39.171418
2664.806353	342763.637424	39.176436
2667.730401	343256.693894	39.181453
2669.878054	343762.056109	39.186471
2672.088929	344273.548176	39.191488
2674.764413	344782.296456	39.196506
2677.295548	345304.874552	39.201524
2679.996238	345833.108109	39.206541
2682.906246	346361.760713	39.211559
2685.833950	346877.457932	39.216576
2688.571249	347410.520369	39.221594
2691.018131	347943.090694	39.226612
2694.043437	348457.463424	39.231629
2696.515800	349010.354672	39.236647
2699.198525	349550.234594	39.241664
2702.198046	350083.991748	39.246682
2704.476165	350621.437420	39.251700
2707.912500	351154.251839	39.256717
2710.394470	351707.419088	39.261735
2713.417316	352239.399799	39.266752
2716.064591	352782.324887	39.271770
2719.047508	353315.011959	39.276788
2721.668273	353862.042497	39.281805
2724.636893	354403.478453	39.286823
2727.382859	354943.547912	39.291840
2730.340890	355486.243425	39.296858
2732.761329	356025.845401	39.301876
2735.838838	356569.652737	39.306893
2738.507287	357128.164952	39.311911
2741.280986	357664.850603	39.316928
2744.360830	358216.711412	39.321946
2747.014715	358761.323497	39.326964
2750.169353	359299.504802	39.331981
2752.486591	359847.914646	39.336999
2755.059922	360403.562154	39.342016
2758.280795	360953.643816	39.347034
2761.201346	361498.030702	39.352052
2763.949424	362040.585915	39.357069
2766.527827	362591.435679	39.362087
2769.440407	363121.947639	39.367104
2772.410429	363667.469133	39.372122
2775.098506	364215.033825	39.377140
2778.132722	364749.187920	39.382157
2781.476747	365295.620726	39.387175
2783.997026	365832.559063	39.392192
2787.009018	366355.074617	39.397210
2789.952150	366898.227073	39.402228
2793.017410	367436.582659	39.407245
2795.500462	367945.865674	39.412263
2798.295539	368442.202014	39.417280
2800.784540	368942.641469	39.422298
2803.027703	369432.202361	39.427316
2805.806415	369941.719936	39.432333
2808.369518	370432.716075	39.437351
2811.114561	370955.904491	39.442368
2813.896648	371456.217761	39.447386
2816.692483	371979.588610	39.452404
2819.283243	372492.226724	39.457421
2822.221052	373010.259088	39.462439
2824.510736	373531.940011	39.467456
2827.500215	374066.976917	39.472474
2830.005941	374607.462624	39.477492
2832.924325	375142.192412	39.482509
2835.763933	375679.388836	39.487527
2838.039404	376238.030841	39.492544
2841.072543	376781.271393	39.497562
2843.637388	377350.888950	39.502580
2846.379238	377903.319565	39.507597
2849.044333	378478.283879	39.512615
2851.870329	379049.840140	39.517632
2854.838827	379631.488183	39.522650
2857.608727	380211.281704	39.527668
2860.576350	380795.728614	39.532685
2863.663372	381389.001542	39.537703
2866.157696	381970.486767	39.542720
2869.405725	382551.590178	39.547738
2872.358167	383157.617209	39.552756
2875.413630	383745.353842	39.557773
2878.197777	384338.730354	39.562791
2881.329413	384946.475985	39.567808
2884.481505	385524.606322	39.572826
2887.047627	386130.063125	39.577844
2890.073170	386730.541786	39.582861
2893.265521	387330.654481	39.587879
2896.014978	387944.067640	39.592896
2899.368798	388530.133879	39.597914
2902.275675	389133.736853	39.602932
2905.201544	389721.195742	39.607949
2908.192884	390315.989801	39.612967
2911.592169	390921.336129	39.617984
2914.718675	391496.889751	39.623002
2917.417421	392089.620649	39.628020
2920.307974	392691.720083	39.633037
2923.553794	393265.906977	39.638055
2926.176659	393870.615144	39.643072
2929.692888	394454.832821	39.648090
2932.358167	395048.710338	39.653108
2935.583342	395621.491791	39.658125
2938.823936	396210.490526	39.663143
2941.614361	396794.782964	39.668160
2944.645803	397372.180578	39.673178
2947.478787	397948.560010	39.678196
2950.684482	398531.437850	39.683213
2953.705103	399091.767725	39.688231
2956.361006	399637.439467	39.693248
2959.615703	400166.475668	39.698266
2962.614184	400694.935352	39.703284
2965.163061	401243.994816	39.708301
2968.000245	401773.425977	39.713319
2970.627594	402323.392819	39.718336
2973.543456	402860.957553	39.723354
2976.510858	403417.621146	39.728372
2978.649882	403970.552571	39.733389
2981.907700	404535.238055	39.738407
2984.781687	405103.472705	39.743424
2987.244526	405667.122931	39.748442
2989.547592	406259.333032	39.753460
2992.468174	406843.702386	39.758477
2995.429635	407445.798978	39.763495
2998.160557	408062.166508	39.768512
3001.240074	408660.392987	39.773530
3004.224748	409287.798413	39.778548
3007.016264	409910.405461	39.783565
3010.651501	410516.517368	39.788583
3013.307413	411148.093258	39.793600
3016.287383	411778.083830	39.798618
3019.477802	412420.142941	39.803636
3022.617683	413039.284427	39.808653
3025.664403	413687.548375	39.813671
3028.564336	414334.021895	39.818688
3031.945573	414961.296212	39.823706
3034.801301	415613.577423	39.828724
3037.462192	416266.660442	39.833741
3040.608317	416909.033835	39.838759
3043.723749	417562.319717	39.843776
3046.812091	418217.926317	39.848794
3050.017938	418877.984406	39.853812
3053.029844	419546.875890	39.858829
3056.667964	420201.513515	39.863847
3059.553406	420878.020365	39.868864
3063.101213	421525.648117	39.873882
3066.306365	422190.569417	39.878900
3069.374784	422844.677866	39.883917
3072.625634	423486.378184	39.888935
3075.518955	424154.063161	39.893952
3078.695503	424805.802380	39.898970
3081.786909	425463.188925	39.903988
3084.880246	426127.804528	39.909005
3088.084155	426787.370443	39.914023
3091.066896	427453.060174	39.919040
3094.481827	428110.989591	39.924058
3097.469900	428777.000134	39.929076
3100.462472	429441.954724	39.934093
3103.648024	430099.263233	39.939111
3106.748196	430766.320402	39.944128
3109.796628	431408.445908	39.949146
3112.667478	432111.597591	39.954164
3116.378123	432755.687261	39.959181
3119.310404	433401.125022	39.964199
3122.054679	434042.473616	39.969216
3125.193835	434659.988914	39.974234
3128.632757	435278.682749	39.979252
3131.484486	435901.784796	39.984269
3134.701193	436513.798237	39.989287
3137.690411	437137.633105	39.994304
3140.286001	437771.010461	39.999322
3143.479627	438421.495588	40.004340
3146.673029	439054.264749	40.009357
3149.597737	439694.149870	40.014375
3152.300767	440340.130130	40.019392
3155.247932	440993.245307	40.024410
3158.781476	441644.883179	40.029428
3161.522605	442320.022118	40.034445
3164.577180	442988.257310	40.039463
3167.722786	443667.345470	40.044480
3171.055026	444345.423042	40.049498
3174.406403	445029.148881	40.054516
3177.386826	445716.154032	40.059533
3180.540118	446392.278144	40.064551
3183.581919	447103.837653	40.069568
3186.919411	447799.737187	40.074586
3190.268445	448497.740437	40.079604
3193.294372	449201.747166	40.084621
3196.807566	449900.998735	40.089639
3200.274167	450608.892117	40.094656
3203.202153	451321.151367	40.099674
3206.528304	452027.555712	40.104692
3209.696778	452729.560048	40.109709
3212.977905	453441.090416	40.114727
3216.267389	454165.198863	40.119744
3219.490485	454885.246144	40.124762
3223.213180	455603.976941	40.129780
3225.992789	456307.247938	40.134797
3229.241944	457034.661178	40.139815
3232.842904	457764.474526	40.144832
3235.975909	458496.210118	40.149850
3239.674662	459218.117362	40.154868
3242.807146	459935.233365	40.159885
3246.140800	460685.332090	40.164903
3249.494431	461406.564324	40.169920
3252.787879	462122.470198	40.174938
3256.353950	462847.870682	40.179956
3258.886099	463572.044512	40.184973
3262.551034	464289.792816	40.189991
3265.605568	465019.247961	40.195008
3268.989031	465746.350000	40.200026
3272.299200	466494.884910	40.205044
3275.461365	467227.383385	40.210061
3278.886626	467949.345436	40.215079
3281.551045	468679.798532	40.220096
3284.750460	469442.255662	40.225114
3288.749438	470165.517284	40.230132
3291.728856	470904.996192	40.235149
3294.804148	471644.989800	40.240167
3297.946738	472352.836709	40.245184
3300.919816	473031.965416	40.250202
3304.118006	473739.957963	40.255220
3307.257488	474461.687847	40.260237
3310.769091	475154.716738	40.265255
3313.774240	475869.895666	40.270272
3316.591751	476581.893933	40.275290
3319.993445	477298.071712	40.280308
3322.996348	478054.071444	40.285325
3326.367343	478781.878482	40.290343
3329.833562	479521.927079	40.295360
3332.783890	480264.405310	40.300378
3336.219843	481000.359691	40.305396
3339.022881	481774.697892	40.310413
3342.650616	482538.160513	40.315431
3345.512903	483305.252023	40.320448
3348.901489	484079.001968	40.325466
3352.528663	484851.318865	40.330484
3355.696372	485652.885282	40.335501
3359.038276	486424.325190	40.340519
3362.302996	487218.635574	40.345536
3365.099501	488022.081650	40.350554
3368.694940	488843.252950	40.355572
3372.472141	489629.802969	40.360589
3376.090804	490448.172685	40.365607
3379.654728	491272.375443	40.370624
3382.670562	492075.260611	40.375642
3386.612819	492859.325385	40.380660
3389.632618	493718.057047	40.385677
3393.619361	494503.560567	40.390695
3397.124359	495343.098175	40.395712
3400.487596	496155.044570	40.400730
3404.052518	496955.004586	40.405748
3407.574173	497803.718980	40.410765
3411.362268	498580.695885	40.415783
3414.985449	499426.742834	40.420800
3417.837640	500244.596029	40.425818
3421.726522	501028.368944	40.430836
3425.039944	501838.957277	40.435853
3428.076161	502673.129484	40.440871
3431.802032	503539.109500	40.445888
3435.244859	504376.570095	40.450906
3438.789707	505182.173188	40.455924
3441.845222	506002.757666	40.460941
3445.791577	506833.913764	40.465959
3449.199132	507677.682788	40.470976
3452.675715	508483.649000	40.475994
3456.249328	509308.083615	40.481012
3459.565144	510180.056865	40.486029
3462.705869	510989.945601	40.491047
3466.586407	511794.279884	40.496064
3469.860563	512659.422227	40.501082
3473.587655	513516.174392	40.506100
3476.842935	514323.464504	40.511117
3480.732567	515108.459572	40.516122
3484.552734	515926.450005	40.521127
3486.971658	516620.463227	40.526132
3490.568666	517241.690535	40.531136
3493.863273	517842.158070	40.536141
3496.745707	518427.397348	40.541146
3499.537322	518881.156284	40.546151
3502.099288	519295.244904	40.551156
3504.063790	519670.887301	40.556160
3506.156110	519981.526628	40.561165
3507.798492	520213.605861	40.566170
3510.187260	520394.192433	40.571175
3511.369138	520608.490304	40.576180
3513.028628	520711.980556	40.581184
3513.965850	520778.118432	40.586189
3515.806651	520789.153214	40.591194
3516.350466	520820.263544	40.596199
3516.829599	520816.345175	40.601204
3518.169945	520729.471233	40.606208
3518.813019	520665.055309	40.611213
3519.630416	520606.375630	40.616218
3520.182551	520458.444917	40.621223
3520.529229	520341.236904	40.626228
3520.699734	520158.677806	40.631232
3521.678657	520003.445009	40.636237
3521.615404	519809.997236	40.641242
3521.837324	519594.304127	40.646247
3521.535515	519423.087513	40.651252
3521.688405	519205.428180	40.656256
3521.666410	518972.168477	40.661261
3521.916923	518724.501220	40.666266
3522.238610	518494.467357	40.671271
3521.834325	518305.758734	40.676276
3521.736856	518074.622214	40.681280
3521.897905	517813.706262	40.686285
3521.821567	517553.076594	40.691290
3521.570316	517294.543940	40.696295
3521.428869	517038.619700	40.701300
3521.590772	516771.365690	40.706304
3521.373899	516565.412694	40.711309
3521.246577	516281.153056	40.716314
3521.242686	516003.443943	40.721319
3520.848246	515789.113862	40.726324
3520.363656	515515.923380	40.731328
3520.643145	515252.723307	40.736333
3520.150824	515042.951198	40.741338
3519.915146	514753.270869	40.746343
3519.564947	514552.625091	40.751348
3519.698659	514285.841746	40.756352
3519.265651	514020.256562	40.761357
3518.941163	513802.096476	40.766362
3518.345899	513569.256678	40.771367
3518.551447	513313.423175	40.776372
3518.051616	513120.725721	40.781376
3517.909939	512909.303559	40.786381
3517.470559	512663.476876	40.791386
3517.689990	512429.480937	40.796391
3517.299134	512247.581872	40.801396
3517.303869	512011.034174	40.806400
3517.205565	511783.706586	40.811405
3516.217890	511581.811107	40.816410
3516.558111	511416.987902	40.821415
3515.769331	511198.716014	40.826420
3516.021173	510978.657947	40.831424
3515.628129	510825.934981	40.836429
3515.315957	510597.967742	40.841434
3515.308349	510440.020029	40.846439
3514.792667	510261.913990	40.851444
3514.852535	510043.341462	40.856448
3514.715346	509892.593491	40.861453
3514.179978	509731.079907	40.866458
3514.071983	509526.643219	40.871463
3513.773087	509374.398415	40.876468
3513.548142	509218.548258	40.881472
3513.419587	509049.678150	40.886477
3512.744189	508913.730275	40.891482
3513.311198	508741.306615	40.896487
3512.821607	508634.015898	40.901492
3512.619583	508442.180067	40.906496
3512.626243	508337.642577	40.911501
3512.282582	508154.883103	40.916506
3512.653306	508038.395456	40.921511
3512.228713	507896.935199	40.926516
3511.712055	507763.837393	40.931520
3511.816974	507629.577701	40.936525
3511.785014	507489.620685	40.941530
3511.468764	507359.271161	40.946535
3511.125818	507259.285968	40.951540
3511.524320	507098.814639	40.956544
3511.125710	507023.277753	40.961549
3510.747558	506871.984934	40.966554
3510.900623	506773.841462	40.971559
3511.005713	506654.451552	40.976564
3510.595525	506517.026078	40.981568
3510.389183	506436.395864	40.986573
3510.439055	506335.736032	40.991578
3510.299689	506204.692057	40.996583
3509.975034	506117.348627	41.001588
3510.224247	505995.198758	41.006592
3509.833022	505926.133449	41.011597
3509.306353	505799.398530	41.016602
3509.827069	505697.091813	41.021607
3509.465449	505624.781832	41.026612
3509.735034	505518.414642	41.031616
3509.629003	505421.974565	41.036621
3509.360251	505340.083988	41.041626
3509.610490	505243.485401	41.046631
3509.034488	505162.502890	41.051636
3509.051252	505042.660483	41.056640
3508.963572	504987.764390	41.061645
3508.826593	504894.717068	41.066650
3508.814745	504789.857602	41.071655
3508.408004	504740.527540	41.076660
3508.318037	504652.532411	41.081664
3508.744415	504555.092453	41.086669
3508.372798	504526.303719	41.091674
3508.180304	504422.179153	41.096679
3508.050781	504374.575595	41.101684
3507.935743	504289.264949	41.106688
3507.854384	504215.335947	41.111693
3507.703466	504163.585135	41.116698
3507.682088	504100.274416	41.121703
3507.988123	504017.477053	41.126708
3507.588608	503976.747599	41.131712
3507.824154	503879.081018	41.136717
3507.732384	503844.882113	41.141722
3507.899033	503770.912048	41.146727
3507.473825	503713.635971	41.151732
3507.235803	503678.498233	41.156736
3507.128744	503591.816430	41.161741
3506.788456	503528.807134	41.166746
3506.760847	503511.502018	41.171751
3507.015573	503447.183677	41.176756
3506.871501	503394.518500	41.181760
3506.908272	503335.143656	41.186765
3506.581628	503317.025195	41.191770
3506.647557	503238.058123	41.196775
3506.457852	503225.536005	41.201780
3506.843432	503170.356997	41.206784
3506.113485	503127.855730	41.211789
3506.267579	503077.318867	41.216794
3506.278558	503043.152785	41.221799
3505.920867	503035.516020	41.226804
3506.240199	502967.237839	41.231808
3506.347237	502959.628810	41.236813
3506.097305	502901.563187	41.241818
3506.524609	502861.965829	41.246823
3505.908124	502849.915821	41.251828
3506.029889	502801.711549	41.256832
3506.165611	502756.946743	41.261837
3506.072697	502750.330911	41.266842
3506.280703	502685.561661	41.271847
3505.832307	502682.342580	41.276852
3506.273083	502611.614318	41.281856
3506.318549	502598.953353	41.286861
3505.978884	502563.373933	41.291866
3506.456734	502510.860903	41.296871
3506.002199	502485.422567	41.301876
3505.816110	502457.967755	41.306880
3505.901589	502417.461744	41.311885
3505.710401	502392.690268	41.316890
3505.682334	502379.230918	41.321895
3505.605446	502325.640864	41.326900
3505.673218	502318.898241	41.331904
3505.655174	502262.514816	41.336909
3505.532067	502263.192298	41.341914
3506.050925	502225.451850	41.346919
3505.613498	502194.898153	41.351924
3505.444006	502173.817934	41.356928
3505.450355	502148.559346	41.361933
3505.478852	502111.807265	41.366938
3505.517095	502091.807677	41.371943
3505.837187	502046.961325	41.376948
3505.575938	502045.129813	41.381952
3505.506213	501989.512946	41.386957
3505.474179	501992.150101	41.391962
3505.494017	501943.301596	41.396967
3505.526939	501942.081596	41.401972
3505.532544	501893.994461	41.406976
3505.259329	501912.816626	41.411981
3505.066968	501871.543418	41.416986
3505.307154	501831.770879	41.421991
3505.333126	501834.145802	41.426996
3505.410159	501783.111271	41.432000
3505.376601	501796.884543	41.437005
3505.642681	501738.682940	41.442010
3505.492375	501747.159852	41.447015
3504.954391	501694.349431	41.452020
3505.453416	501673.416037	41.457024
3505.242098	501679.776678	41.462029
3504.908010	501632.603036	41.467034
3505.552314	501594.537719	41.472039
3505.189782	501621.979372	41.477044
3505.345460	501563.997122	41.482048
3505.378731	501562.878277	41.487053
3505.220114	501539.821482	41.492058
3505.403836	501537.059071	41.497063
3504.608657	501508.939801	41.502068
3505.339699	501454.814474	41.507072
3505.308446	501465.094966	41.512077
3505.064184	501453.288879	41.517082
3505.263249	501397.020255	41.522087
3505.296759	501427.689813	41.527092
3505.254805	501382.949640	41.532096
3504.990230	501346.444783	41.537101
3505.099555	501336.000052	41.542106
3505.446160	501339.235496	41.547111
3504.771217	501318.689731	41.552116
3504.693234	501291.975316	41.557120
3505.095992	501262.451445	41.562125
3504.617069	501248.758794	41.567130
3504.791582	501227.167508	41.572135
3504.852017	501266.843279	41.577140
3505.220499	501246.385592	41.582144
3504.952341	501212.158882	41.587149
3504.877101	501193.897277	41.592154
3505.458409	501154.828600	41.597159
3504.669490	501146.854230	41.602164
3504.813850	501170.318765	41.607168
3505.093733	501130.285295	41.612173
3504.973405	501104.690919	41.617178
3504.889365	501111.740314	41.622183
3505.046087	501076.130078	41.627188
3505.150517	501086.338720	41.632192
3505.098291	501056.532094	41.637197
3504.953732	501009.023128	41.642202
3504.974207	501020.358712	41.647207
3504.946337	501035.599641	41.652212
3504.736107	500992.403680	41.657216
3504.874238	500956.593666	41.662221
3504.708048	500981.575513	41.667226
3504.976106	500965.132341	41.672231
3504.534616	500931.286830	41.677236
3505.025499	500910.708173	41.682240
3505.115471	500932.106198	41.687245
3504.902308	500883.899066	41.692250
3504.983741	500864.650579	41.697255
3504.662148	500874.825443	41.702260
3504.196300	500851.411363	41.707264
3505.197177	500823.412070	41.712269
3505.025753	500817.870955	41.717274
3504.765597	500819.430697	41.722279
3504.439422	500811.332410	41.727284
3505.069264	500757.980280	41.732288
3504.670431	500799.450777	41.737293
3504.041829	500786.237012	41.742298
3504.294269	500765.088435	41.747303
3504.796512	500720.361826	41.752308
3504.711867	500729.588148	41.757312
3504.613859	500764.734233	41.762317
3504.391494	500722.906289	41.767322
3505.303897	500678.924671	41.772327
3504.994815	500718.052620	41.777332
3504.500315	500710.942684	41.782336
3504.765069	500684.375667	41.787341
3504.669134	500655.233349	41.792346
3504.933541	500627.299544	41.797351
3504.577158	500659.297568	41.802356
3504.597207	500620.215203	41.807360
3504.487040	500584.899283	41.812365
3504.301427	500576.272461	41.817370
3504.642549	500621.220490	41.822375
3504.285499	500606.951252	41.827380
3504.909387	500558.205966	41.832384
3504.512599	500587.122625	41.837389
3504.702576	500558.491786	41.842394
3504.344898	500569.128115	41.847399
3504.627727	500529.042217	41.852404
3504.756311	500551.193910	41.857408
3504.306330	500525.802677	41.862413
3504.300505	500497.557038	41.867418
3504.528057	500525.463927	41.872423
3503.930488	500509.359651	41.877428
3504.494758	500486.642823	41.882432
3504.701721	500507.921619	41.887437
3504.456543	500510.744548	41.892442
3504.180367	500469.127002	41.897447
3504.354952	500458.772687	41.902452
3504.168363	500501.425232	41.907456
3504.536975	500515.439646	41.912461
3504.194004	500474.794472	41.917466
3504.427261	500443.625548	41.922471
3504.395696	500485.899277	41.927476
3504.270897	500478.427082	41.932480
3504.682131	500480.184454	41.937485
3504.298220	500451.137946	41.942490
3504.424179	500411.076580	41.947495
3504.394728	500399.083977	41.952500
3504.914900	500440.663142	41.957504
3504.197988	500412.479149	41.962509
3504.193956	500372.691353	41.967514
3504.735999	500359.697201	41.972519
3504.319502	500403.348129	41.977524
3504.407719	500407.232045	41.982528
3504.819543	500365.859858	41.987533
3504.483508	500347.486749	41.992538
3504.354180	500387.852542	41.997543
3504.349548	500361.580737	42.002548
3504.067592	500328.721300	42.007552
3504.674827	500303.314503	42.012557
3504.575676	500316.238713	42.017562
3504.934330	500352.275232	42.022567
3504.312007	500304.333704	42.027572
3504.825250	500266.893748	42.032576
3505.033664	500260.128118	42.037581
3504.653511	500259.428894	42.042586
3504.322762	500297.346261	42.047591
3504.177623	500290.434041	42.052596
3504.080365	500258.253984	42.057600
3504.771969	500232.985617	42.062605
3504.772850	500205.295299	42.067610
3504.815052	500220.272735	42.072615
3504.500902	500242.494792	42.077620
3504.523276	500199.260151	42.082624
3504.561869	500219.705330	42.087629
3504.469482	500203.470303	42.092634
3504.968774	500147.454033	42.097639
3504.851337	500177.997724	42.102644
3504.734832	500174.978830	42.107648
3505.235218	500128.023671	42.112653
3504.569877	500109.955482	42.117658
3505.002765	500105.381690	42.122663
3504.710515	500115.856077	42.127668
3504.904525	500084.895224	42.132672
3504.973865	500070.102559	42.137677
3504.267530	500079.478107	42.142682
3504.816864	500052.915797	42.147687
3504.483536	500056.917044	42.152692
3504.937367	500023.130784	42.157696
3504.598322	500037.054942	42.162701
3504.717716	500020.178804	42.167706
3504.584551	499997.014754	42.172711
3504.883110	499989.829793	42.177716
3504.384127	499979.429805	42.182720
3504.903806	499944.215556	42.187725
3504.537433	499944.070990	42.192730
3504.674663	499969.512509	42.197735
3504.548574	499958.952321	42.202740
3504.767911	499936.896795	42.207744
3504.593713	499909.081828	42.212749
3504.441411	499884.655088	42.217754
3504.966529	499864.525431	42.222759
3504.653816	499917.981975	42.227764
3504.242539	499884.382825	42.232768
3504.405917	499869.575130	42.237773
3503.728643	499866.442333	42.242778
3504.070089	499860.465491	42.247783
3504.284253	499870.201874	42.252788
3504.292705	499856.886722	42.257792
3504.142988	499837.369934	42.262797
3504.485958	499814.585994	42.267802
3504.865160	499793.011253	42.272807
3504.917726	499796.698444	42.277812
3504.443252	499802.746982	42.282816
3504.108741	499800.977439	42.287821
3504.142531	499798.440956	42.292826
3504.430975	499795.864219	42.297831
3504.408689	499794.450307	42.302836
3504.559121	499765.216979	42.307840
3504.741611	499795.207677	42.312845
3504.455904	499778.749708	42.317850
3505.070883	499738.457677	42.322855
3504.441558	499768.576743	42.327860
3504.207413	499739.556033	42.332864
3504.799179	499709.847867	42.337869
3504.524094	499685.490889	42.342874
3504.927651	499702.031586	42.347879
3504.549552	499732.262872	42.352884
3504.553960	499698.597668	42.357888
3504.428422	499673.963918	42.362893
3504.975496	499645.781415	42.367898
3504.598634	499667.204117	42.372903
3504.267423	499657.283657	42.377908
3503.983242	499629.688136	42.382912
3504.848429	499596.089171	42.387917
3504.630867	499598.047274	42.392922
3504.601410	499621.996922	42.397927
3504.406885	499616.155344	42.402932
3503.824664	499600.756555	42.407936
3504.664394	499576.729447	42.412941
3504.694379	499571.763594	42.417946
3504.655715	499550.406486	42.422951
3504.516705	499548.707263	42.427956
3503.939838	499561.758151	42.432960
3504.650452	499567.568817	42.437965
3504.441476	499563.450714	42.442970
3504.615664	499519.026095	42.447975
3504.602059	499506.979768	42.452980
3504.258465	499530.321083	42.457984
3504.482573	499510.491731	42.462989
3504.246093	499503.289903	42.467994
3503.885360	499498.385790	42.472999
3503.978352	499496.295522	42.478004
3504.871003	499475.297352	42.483008
3504.515703	499460.267564	42.488013
3504.337177	499499.529397	42.493018
3504.517915	499471.657649	42.498023
3504.394915	499463.982251	42.503028
3503.974459	499447.444030	42.508032
3504.594925	499401.986723	42.513037
3504.466506	499451.061836	42.518042
3504.446860	499438.712674	42.523047
3504.723542	499401.004570	42.528052
3504.549599	499384.781695	42.533056
3504.694739	499368.609617	42.538061
3504.193160	499418.250048	42.543066
3504.434747	499423.628659	42.548071
3504.229669	499392.172834	42.553076
3504.356454	499354.640200	42.558080
3504.577850	499387.460391	42.563085
3504.460664	499397.451903	42.568090
3504.602060	499347.868375	42.573095
3504.939255	499345.182619	42.578100
3504.420121	499359.642009	42.583104
3504.676146	499322.342001	42.588109
3504.570036	499289.705991	42.593114
3504.897644	499319.826416	42.598119
3504.633452	499285.899151	42.603124
3504.534220	499245.364544	42.608128
3504.912707	499275.932621	42.613133
3504.580491	499268.796457	42.618138
3504.442941	499222.648524	42.623143
3504.638942	499207.582006	42.628148
3504.609443	499247.985198	42.633152
3504.708869	499215.974687	42.638157
3504.494502	499191.658068	42.643162
3504.519992	499206.740238	42.648167
3504.210799	499191.196689	42.653172
3504.564993	499159.601430	42.658176
3504.745266	499157.649201	42.663181
3504.252548	499171.800815	42.668186
3504.291731	499149.114680	42.673191
3504.484598	499129.340474	42.678196
3504.349501	499146.928702	42.683200
3504.537249	499117.890926	42.688205
3504.188947	499159.711585	42.693210
3504.356896	499147.433820	42.698215
3504.539749	499105.639311	42.703220
3504.239423	499131.505553	42.708224
3504.161123	499093.296044	42.713229
3504.701907	499077.162416	42.718234
3504.613290	499077.277686	42.723239
3504.579296	499045.692964	42.728244
3504.529498	499077.139081	42.733248
3504.514821	499067.978263	42.738253
3504.285080	499041.740115	42.743258
3504.665098	499046.033828	42.748263
3504.464817	499033.156064	42.753268
3504.406747	498998.335048	42.758272
3504.714024	498998.742117	42.763277
3504.660718	499021.633199	42.768282
3504.503298	498987.941624	42.773287
3504.993356	498963.563974	42.778292
3504.805073	498964.656883	42.783296
3504.690426	498970.800696	42.788301
3504.362803	498983.812601	42.793306
3504.611090	498965.801343	42.798311
3504.426165	498955.502994	42.803316
3504.581661	498944.442071	42.808321
3504.587774	498934.670393	42.813325
3504.440772	498914.190291	42.818330
3504.547722	498901.668874	42.823335
3504.022805	498887.070424	42.828340
3503.717903	498886.460499	42.833345
3504.426054	498871.413997	42.838349
3504.543810	498876.559217	42.843354
3503.928374	498852.862421	42.848359
3504.634087	498854.117777	42.853364
3504.794108	498824.223275	42.858369
3504.842659	498849.123508	42.863373
3504.665551	498840.848888	42.868378
3504.508117	498819.155309	42.873383
3504.470782	498792.633257	42.878388
3504.271710	498821.420240	42.883393
3504.399133	498808.136134	42.888397
3503.814309	498789.750133	42.893402
3504.054595	498776.296286	42.898407
3504.663894	498762.885351	42.903412
3503.945900	498777.326012	42.908417
3504.499280	498788.123132	42.913421
3504.277573	498790.689487	42.918426
3504.315523	498775.546340	42.923431
3504.317183	498769.369721	42.928436
3504.428755	498751.734243	42.933441
3504.329758	498749.927367	42.938445
3503.654114	498742.440270	42.943450
3504.365129	498739.442206	42.948455
3504.665156	498717.423063	42.953460
3504.018345	498740.003308	42.958465
3504.524305	498705.396328	42.963469
3504.126217	498748.896469	42.968474
3504.060059	498727.593360	42.973479
3504.277791	498707.966641	42.978484
3504.196002	498713.497833	42.983489
3504.283636	498691.157848	42.988493
3504.169795	498694.820942	42.993498
3503.967706	498692.878477	42.998503
3504.854249	498677.347980	43.003508
3504.589632	498654.152358	43.008513
3504.559909	498645.094956	43.013517
3504.745955	498682.934023	43.018522
3504.547215	498659.525489	43.023527
3503.992388	498632.882497	43.028532
3504.090408	498616.869074	43.033537
3504.288518	498590.410762	43.038541
3504.184872	498603.843173	43.043546
3504.232544	498646.463075	43.048551
3504.417737	498640.206774	43.053556
3504.192895	498625.459426	43.058561
3504.025707	498597.742581	43.063565
3503.926257	498604.187874	43.068570
3503.859530	498603.287158	43.073575
3504.017007	498604.983578	43.078580
3504.102763	498607.551984	43.083585
3504.699092	498582.903892	43.088589
3504.776117	498602.484180	43.093594
3504.633480	498606.911240	43.098599
3504.475500	498564.612466	43.103604
3504.553387	498539.388120	43.108609
3504.507727	498579.694107	43.113613
3504.188349	498557.519547	43.118618
3504.984582	498516.183612	43.123623
3504.543785	498514.076353	43.128628
3504.352979	498551.772757	43.133633
3504.363495	498505.700842	43.138637
3504.177853	498502.793848	43.143642
3504.287256	498487.183525	43.148647
3504.549807	498482.231238	43.153652
3504.528043	498465.527841	43.158657
3504.298918	498452.856730	43.163661
3504.350514	498497.096423	43.168666
3504.365672	498464.794142	43.173671
3504.634357	498449.918012	43.178676
3504.420506	498419.778180	43.183681
3504.682142	498394.777722	43.188685
3504.418809	498403.679090	43.193690
3503.947223	498433.724814	43.198695
3504.155861	498462.549174	43.203700
3504.200463	498443.000162	43.208705
3504.513793	498431.711470	43.213709
3504.149157	498424.529468	43.218714
3503.871360	498401.133096	43.223719
3504.514050	498379.363140	43.228724
3504.270714	498385.071849	43.233729
3504.860277	498357.437524	43.238733
3504.410876	498335.587007	43.243738
3504.452360	498331.479658	43.248743
3504.724476	498334.727426	43.253748
3504.345557	498315.143967	43.258753
3504.554957	498325.793229	43.263757
3504.140519	498339.224337	43.268762
3504.438925	498358.111741	43.273767
3504.188169	498330.306441	43.278772
3504.275303	498282.247385	43.283777
3504.438929	498255.085252	43.288781
3504.363373	498257.476696	43.293786
3504.140411	498282.116863	43.298791
3504.373097	498272.612778	43.303796
3504.352761	498250.593081	43.308801
3504.371628	498258.690500	43.313805
3504.274844	498283.158839	43.318810
3504.183408	498292.589989	43.323815
3504.317500	498281.177654	43.328820
3504.118528	498258.123029	43.333825
3503.884253	498229.302420	43.338829
3503.984959	498223.717488	43.343834
3504.608258	498208.633225	43.348839
3504.361769	498236.770473	43.353844
3504.124132	498259.691656	43.358849
3504.209527	498240.743507	43.363853
3504.595047	498208.331598	43.368858
3504.306238	498195.315347	43.373863
3503.968165	498207.772556	43.378868
3504.067830	498218.894875	43.383873
3504.607026	498204.532687	43.388877
3504.612383	498210.404650	43.393882
3504.041330	498176.827575	43.398887
3503.797951	498161.171481	43.403892
3504.148274	498165.065077	43.408897
3504.423381	498150.542081	43.413901
3503.752974	498165.380726	43.418906
3504.088269	498156.113498	43.423911
3505.038411	498152.014360	43.428916
3504.960733	498124.839547	43.433921
3504.602799	498119.478964	43.438925
3504.665060	498151.972158	43.443930
3504.470607	498144.763143	43.448935
3504.324744	498122.560622	43.453940
3504.527429	498109.972897	43.458945
3504.521869	498109.062488	43.463949
3504.115234	498116.974090	43.468954
3504.277853	498099.532421	43.473959
3504.352289	498083.319744	43.478964
3503.980408	498052.444861	43.483969
3504.287907	498036.752210	43.488973
3504.501353	498040.009305	43.493978
3504.181737	498052.868726	43.498983
3504.193254	498058.233485	43.503988
3504.695159	498027.878605	43.508993
3504.990766	497996.796861	43.513997
3504.786687	497991.563804	43.519002
3504.744774	497978.913397	43.524007
3505.038124	497964.488625	43.529012
3504.505780	497957.991113	43.534017
3504.486995	497980.270515	43.539021
3504.206620	497956.367693	43.544026
3504.910834	497925.221239	43.549031
3504.692298	497911.636765	43.554036
3504.501433	497952.574638	43.559041
3504.598905	497929.827134	43.564045
3504.151798	497916.481307	43.569050
3504.635812	497872.256815	43.574055
3504.739613	497854.419180	43.579060
3504.417607	497896.744880	43.584065
3504.100958	497882.416466	43.589069
3503.906794	497847.665378	43.594074
3504.586639	497816.876991	43.599079
3504.424747	497813.915503	43.604084
3504.193987	497816.331538	43.609089
3504.457501	497818.112529	43.614093
3504.321345	497865.674302	43.619098
3503.918679	497832.272484	43.624103
3504.562746	497786.351740	43.629108
3504.458685	497824.997887	43.634113
3504.516983	497799.826238	43.639117
3504.706321	497780.354891	43.644122
3504.451942	497802.165464	43.649127
3504.413896	497767.895834	43.654132
3504.388164	497779.898933	43.659137
3504.416132	497756.554653	43.664141
3503.869475	497764.184769	43.669146
3504.245917	497720.938860	43.674151
3504.347493	497746.186630	43.679156
3504.071570	497745.167052	43.684161
3504.701241	497711.601830	43.689165
3504.231404	497760.431719	43.694170
3504.181859	497712.696533	43.699175
3504.526832	497693.808040	43.704180
3504.079862	497730.685947	43.709185
3504.478401	497683.588661	43.714189
3504.551852	497675.172643	43.719194
3504.067666	497699.095456	43.724199
3504.532871	497655.632846	43.729204
3504.371774	497680.466566	43.734209
3504.668979	497642.549044	43.739213
3504.198547	497689.759084	43.744218
3504.543657	497637.252819	43.749223
3504.730580	497605.681295	43.754228
3504.131457	497646.785650	43.759233
3504.476010	497629.162883	43.764237
3504.503881	497592.097897	43.769242
3504.376667	497586.396909	43.774247
3504.412763	497580.366329	43.779252
3504.171972	497606.174704	43.784257
3504.340305	497567.467329	43.789261
3503.991112	497587.318602	43.794266
3504.277906	497591.019848	43.799271
3504.518422	497546.326762	43.804276
3504.320702	497573.697886	43.809281
3504.354588	497547.061496	43.814285
3504.568367	497549.812333	43.819290
3504.044637	497547.920586	43.824295
3504.504839	497488.712618	43.829300
3504.245763	497537.813565	43.834305
3504.324829	497501.347854	43.839309
3504.159373	497544.763477	43.844314
3504.211499	497512.554917	43.849319
3504.294223	497515.934029	43.854324
3504.139564	497484.365660	43.859329
3503.842692	497506.892117	43.864333
3504.211068	497493.518333	43.869338
3503.937012	497517.408170	43.874343
3504.379939	497470.505834	43.879348
3504.148949	497504.160393	43.884353
3504.193714	497505.165920	43.889357
3504.158595	497510.588842	43.894362
3504.119686	497482.039942	43.899367
3504.580766	497456.804151	43.904372
3503.999671	497471.224204	43.909377
3504.322104	497485.855831	43.914381
3504.381411	497476.176218	43.919386
3503.809009	497463.558676	43.924391
3504.590376	497428.348807	43.929396
3504.014519	497419.073342	43.934401
3504.164226	497451.452708	43.939405
3504.042312	497462.306737	43.944410
3504.189132	497452.410760	43.949415
3503.984032	497431.077461	43.954420
3503.887586	497421.624957	43.959425
3504.469287	497414.090445	43.964429
3504.842820	497396.057835	43.969434
3504.635075	497379.990395	43.974439
3504.779243	497379.157541	43.979444
3504.444501	497365.135357	43.984449
3504.393253	497332.588410	43.989453
3504.508363	497337.329446	43.994458
3504.457614	497343.109298	43.999463
3504.893506	497320.105018	44.004468
3504.625395	497336.247755	44.009473
3504.366410	497349.908168	44.014477
3504.259676	497315.699172	44.019482
3504.505439	497307.812678	44.024487
3504.201040	497306.443165	44.029492
3503.792209	497295.622333	44.034497
3503.773912	497290.055926	44.039501
3503.487644	497287.063381	44.044506
3503.586403	497293.882849	44.049511
3503.825478	497284.782279	44.054516
3504.221223	497306.845091	44.059521
3504.131834	497303.720169	44.064525
3504.233186	497261.225474	44.069530
3503.752621	497288.489846	44.074535
3503.945710	497279.092761	44.079540
3504.426403	497270.156513	44.084545
3504.340026	497273.815551	44.089549
3503.824349	497324.020869	44.094554
3503.436411	497305.500975	44.099559
3503.563035	497292.165258	44.104564
3503.475697	497300.431782	44.109569
3504.530696	497286.848052	44.114573
3504.408899	497271.678273	44.119578
3504.479389	497307.462637	44.124583
3504.334304	497299.840441	44.129588
3504.386317	497285.453281	44.134593
3504.263741	497262.638466	44.139597
3504.438475	497233.144061	44.144602
3504.428236	497239.322585	44.149607
3504.654812	497256.096021	44.154612
3504.238975	497238.238661	44.159617
3504.101503	497221.603040	44.164621
3504.814845	497206.250565	44.169626
3504.522543	497173.943959	44.174631
3504.634375	497165.369748	44.179636
3503.987056	497205.115693	44.184641
3504.012813	497187.644154	44.189645
3504.580216	497161.429170	44.194650
3503.854619	497189.289358	44.199655
3504.501462	497150.505458	44.204660
3503.917536	497159.761892	44.209665
3504.271507	497142.997886	44.214669
3504.408383	497168.342138	44.219674
3504.711538	497127.080993	44.224679
3504.465575	497151.270652	44.229684
3504.223096	497148.119271	44.234689
3504.463326	497136.638811	44.239693
3504.359172	497108.605944	44.244698
3504.447425	497091.630740	44.249703
3504.404677	497105.459677	44.254708
3504.013044	497105.774749	44.259713
3504.049856	497086.681185	44.264717
3504.078710	497087.841142	44.269722
3504.174397	497092.382790	44.274727
3504.344029	497072.508757	44.279732
3504.311978	497075.804832	44.284737
3504.069422	497089.159058	44.289741
3504.051460	497050.935710	44.294746
3504.496526	497045.549138	44.299751
3504.811979	497062.561857	44.304756
3503.853822	497044.384985	44.309761
3504.647083	497030.234870	44.314765
3504.383411	497022.631303	44.319770
3504.484960	497038.462716	44.324775
3504.500688	496992.689926	44.329780
3504.123256	497010.571683	44.334785
3504.132615	497007.228577	44.339789
3504.517433	496968.941389	44.344794
3504.219513	496953.343505	44.349799
3504.328743	496940.516591	44.354804
3504.438270	496960.650453	44.359809
3504.463079	497000.088076	44.364813
3504.351369	496984.764570	44.369818
3503.938249	496965.944525	44.374823
3503.859646	496943.324883	44.379828
3504.027113	496949.424784	44.384833
3504.018851	496944.413626	44.389837
3504.474651	496932.848332	44.394842
3504.436231	496921.209259	44.399847
3504.441530	496930.322037	44.404852
3504.020964	496945.476595	44.409857
3504.321725	496947.555572	44.414861
3504.155950	496947.328633	44.419866
3503.868109	496928.438115	44.424871
3504.504605	496912.895017	44.429876
3504.105998	496925.666456	44.434881
3504.040445	496921.727602	44.439885
3504.314030	496922.747623	44.444890
3503.826074	496906.369640	44.449895
3504.108719	496885.464915	44.454900
3504.338832	496860.315440	44.459905
3504.273850	496841.642761	44.464909
3504.306957	496852.118229	44.469914
3503.725933	496846.893794	44.474919
3504.250857	496847.215882	44.479924
3504.254430	496873.442350	44.484929
3504.313045	496873.635622	44.489933
3504.410489	496867.949528	44.494938
3503.913591	496853.142480	44.499943
3504.530923	496808.641179	44.504948
3504.432761	496850.326348	44.509953
3503.807851	496837.210356	44.514957
3504.049227	496807.603467	44.519962
3503.860618	496781.456810	44.524967
3504.175585	496818.114859	44.529972
3504.076281	496806.687862	44.534977
3503.991265	496792.524499	44.539981
3504.501402	496776.798734	44.544986
3504.489633	496795.382373	44.549991
3503.472036	496811.795939	44.554996
3503.778508	496831.696287	44.560001
3504.191559	496835.732150	44.565005
3503.874416	496839.174596	44.570010
3503.626230	496829.543245	44.575015
3503.843923	496818.167411	44.580020
3503.218093	496826.620532	44.585025
3503.522903	496820.040911	44.590029
3503.987711	496819.410505	44.595034
3504.344230	496801.936944	44.600039
3503.705662	496818.341223	44.605044
3503.895260	496838.816982	44.610049
3504.111368	496841.820717	44.615053
3504.308682	496858.801670	44.620058
3504.162643	496860.191812	44.625063
3504.429709	496808.049916	44.630068
3504.174120	496783.787214	44.635073
3503.363386	496808.269127	44.640077
3504.016133	496814.748047	44.645082
3504.073280	496790.689078	44.650087
3503.978364	496788.375044	44.655092
3504.277068	496819.415562	44.660097
3504.434606	496784.454956	44.665101
3504.036069	496815.403167	44.670106
3503.574213	496836.386957	44.675111
3503.748320	496785.778632	44.680116
3504.080030	496784.460423	44.685121
3503.757475	496801.776763	44.690125
3504.168589	496827.027510	44.695130
3504.214030	496824.488769	44.700135
3504.529367	496758.466089	44.705140
3503.909601	496789.246788	44.710145
3504.350365	496786.594922	44.715149
3504.149597	496763.741210	44.720154
3503.669094	496806.043865	44.725159
3504.264748	496776.735345	44.730164
3504.575816	496783.369549	44.735169
3504.325386	496753.182102	44.740173
3504.648407	496714.600360	44.745178
3504.446211	496709.670425	44.750183
3504.408299	496719.954669	44.755188
3503.740591	496728.819508	44.760193
3504.009659	496712.726741	44.765197
3504.547324	496671.680656	44.770202
3504.396255	496686.995356	44.775207
3504.078788	496712.361429	44.780212
3504.325309	496719.714704	44.785217
3504.391988	496736.058209	44.790221
3504.469006	496693.869829	44.795226
3504.275392	496653.243087	44.800231
3503.958963	496670.102896	44.805236
3504.204229	496692.595294	44.810241
3504.619060	496646.657287	44.815245
3504.638823	496636.375896	44.820250
3504.406026	496622.337025	44.825255
3504.331488	496623.817147	44.830260
3504.385179	496629.580716	44.835265
3504.728975	496614.995009	44.840269
3505.140644	496588.348134	44.845274
3504.200312	496595.484009	44.850279
3504.620987	496599.316192	44.855284
3504.169736	496606.121594	44.860289
3504.119384	496574.737688	44.865293
3503.989738	496557.593903	44.870298
3503.678067	496556.529275	44.875303
3504.395664	496535.352868	44.880308
3504.310557	496537.087829	44.885313
3503.939549	496530.108609	44.890317
3504.151650	496588.352694	44.895322
3504.105287	496578.031091	44.900327
3504.187972	496551.841222	44.905332
3504.174453	496545.970040	44.910337
3504.026015	496528.930463	44.915341
3503.990607	496511.467944	44.920346
3504.065468	496511.000433	44.925351
3503.991687	496484.227613	44.930356
3504.200803	496525.561157	44.935361
3503.928356	496551.426659	44.940365
3504.148831	496558.530955	44.945370
3503.922948	496542.212482	44.950375
3503.784445	496525.880182	44.955380
3503.695923	496528.375167	44.960385
3504.252825	496513.654429	44.965389
3504.795657	496501.973842	44.970394
3504.180801	496494.425565	44.975399
3503.900220	496499.836955	44.980404
3503.946997	496507.880110	44.985409
3503.808489	496499.750216	44.990413
3504.548589	496485.456188	44.995418
3503.997169	496475.720685	45.000423
3504.267582	496518.107837	45.005428
3503.921344	496528.440925	45.010433
3503.996326	496507.619226	45.015437
3504.678338	496474.802945	45.020442
3504.423454	496448.210596	45.025447
3504.299824	496447.166869	45.030452
3504.323123	496484.479281	45.035457
3503.568016	496463.130524	45.040461
3504.173341	496451.946351	45.045466
3504.039001	496441.284150	45.050471
3503.905630	496454.368418	45.055476
3504.000312	496454.758524	45.060481
3504.109150	496438.741475	45.065485
3504.161890	496457.922851	45.070490
3503.920559	496436.644747	45.075495
3504.870307	496395.937967	45.080500
3504.615711	496399.168077	45.085505
3504.416844	496394.237530	45.090509
3504.478377	496373.620335	45.095514
3504.257854	496369.351429	45.100519
3504.567175	496382.416405	45.105524
3503.834202	496424.607950	45.110529
3503.976208	496428.939912	45.115533
3504.154767	496419.494051	45.120538
3504.223204	496406.065619	45.125543
3504.181656	496368.907855	45.130548
3504.492463	496335.593042	45.135553
3504.212546	496379.080162	45.140557
3503.797338	496364.057273	45.145562
3504.206530	496348.093933	45.150567
3504.644929	496326.961420	45.155572
3504.726777	496321.581418	45.160577
3504.265329	496294.667068	45.165581
3504.147873	496331.546345	45.170586
3504.314316	496353.697191	45.175591
3504.050221	496342.954178	45.180596
3503.819574	496334.484346	45.185601
3503.932898	496296.542462	45.190605
3503.506909	496292.812345	45.195610
3503.361891	496304.632739	45.200615
3504.565084	496296.594469	45.205620
3504.234066	496278.824025	45.210625
3503.812588	496318.688095	45.215629
3504.251117	496311.226397	45.220634
3504.139332	496318.079511	45.225639
3504.391635	496316.672555	45.230644
3504.071874	496309.583884	45.235649
3504.466286	496300.255740	45.240653
3504.146212	496291.749391	45.245658
3504.086444	496277.784169	45.250663
3503.997956	496280.228550	45.255668
3503.965539	496277.145078	45.260673
3503.788256	496279.856659	45.265677
3503.681883	496267.164619	45.270682
3503.977355	496267.168559	45.275687
3503.849313	496272.809068	45.280692
3503.640630	496285.905361	45.285697
3503.782238	496264.363993	45.290701
3504.442794	496231.905100	45.295706
3503.798189	496284.564038	45.300711
3504.012353	496273.492221	45.305716
3503.942505	496244.541211	45.310721
3503.626318	496271.122886	45.315725
3504.223755	496271.889221	45.320730
3504.065671	496283.964858	45.325735
3504.015682	496260.225923	45.330740
3504.166998	496249.822254	45.335745
3504.297472	496253.345953	45.340749
3504.486028	496227.493316	45.345754
3504.207678	496219.436035	45.350759
3504.117245	496202.133819	45.355764
3504.266940	496213.097556	45.360769
3504.256191	496267.327242	45.365773
3503.792081	496265.881628	45.370778
3503.743456	496242.598151	45.375783
3504.037538	496239.665595	45.380788
3503.565459	496262.271915	45.385793
3504.002413	496220.633143	45.390797
3504.521939	496222.829523	45.395802
3503.928346	496263.125984	45.400807
3504.210855	496243.688904	45.405812
3504.197733	496213.260521	45.410817
3503.855554	496212.403226	45.415821
3503.936248	496215.074038	45.420826
3504.194677	496187.995106	45.425831
3504.294036	496200.840234	45.430836
3503.969986	496223.575101	45.435841
3504.351466	496207.362855	45.440845
3504.235914	496210.469753	45.445850
3504.228307	496159.078288	45.450855
3504.414205	496193.985827	45.455860
3504.367831	496181.790575	45.460865
3504.117068	496164.716199	45.465869
3504.187965	496177.819009	45.470874
3503.863178	496183.389379	45.475879
3504.025472	496162.654753	45.480884
3503.993715	496142.811543	45.485889
3504.479746	496110.025588	45.490893
3504.946118	496091.268151	45.495898
3504.314148	496136.127967	45.500903
3504.333602	496123.162770	45.505908
3504.296430	496111.522984	45.510913
3504.314427	496083.114801	45.515917
3504.361220	496104.373459	45.520922
3504.026588	496112.882144	45.525927
3504.698411	496074.699619	45.530932
3504.657342	496089.136661	45.535937
3504.191295	496071.083559	45.540941
3504.610239	496030.257339	45.545946
3504.463959	496084.964690	45.550951
3504.335604	496026.148819	45.555956
3504.650106	496011.820432	45.560961
3504.154920	496017.113985	45.565965
3504.477257	496016.759243	45.570970
3504.005447	496006.808371	45.575975
3504.258941	496026.920505	45.580980
3503.962740	496016.283641	45.585985
3503.704430	495989.843068	45.590989
3503.990234	495970.455811	45.595994
3504.223002	495954.520018	45.600999
3504.371078	495998.193558	45.606004
3504.490981	495996.301170	45.611009
3504.139424	495966.786647	45.616013
3504.406443	495982.795355	45.621018
3504.057444	495973.989627	45.626023
3504.818114	495934.830725	45.631028
3504.208196	495961.408645	45.636033
3504.338151	495928.526750	45.641037
3504.386459	495949.380277	45.646042
3503.828887	495944.556943	45.651047
3503.947605	495893.397933	45.656052
3504.017606	495887.057631	45.661057
3503.828511	495937.924005	45.666061
3504.080703	495927.858646	45.671066
3503.731610	495911.002112	45.676071
3504.126437	495919.952553	45.681076
3503.972357	495928.483417	45.686081
3503.294401	495918.210644	45.691085
3503.496522	495916.558421	45.696090
3503.827405	495925.316432	45.701095
3504.464320	495901.569720	45.706100
3504.114700	495919.549412	45.711105
3503.847710	495940.300888	45.716109
3503.946864	495911.221370	45.721114
3503.924626	495948.187635	45.726119
3504.265441	495933.703126	45.731124
3503.799067	495938.840245	45.736129
3503.843515	495921.415175	45.741133
3504.362279	495902.699898	45.746138
3503.908052	495953.101800	45.751143
3504.053662	495947.559708	45.756148
3503.934783	495931.122507	45.761153
3504.005562	495907.212123	45.766157
3503.859721	495884.348629	45.771162
3503.471041	495914.233490	45.776167
3503.911697	495919.936115	45.781172
3504.650614	495905.540557	45.786177
3504.265448	495884.082010	45.791181
3504.498333	495874.272843	45.796186
3504.250560	495909.401378	45.801191
3504.525859	495916.649160	45.806196
3504.265539	495907.120508	45.811201
3504.015689	495884.881063	45.816205
3504.434183	495869.320910	45.821210
3503.897129	495872.494492	45.826215
3504.018614	495870.095501	45.831220
3504.469863	495848.403431	45.836225
3504.030056	495858.042809	45.841229
3504.407197	495852.818529	45.846234
3504.559609	495830.667335	45.851239
3504.060922	495800.922631	45.856244
3504.129141	495801.063763	45.861249
3504.225846	495810.365187	45.866253
3504.534386	495815.784923	45.871258
3504.476990	495830.376653	45.876263
3504.201094	495826.167006	45.881268
3504.188502	495815.738367	45.886273
3503.699021	495792.220199	45.891277
3504.054502	495788.923427	45.896282
3504.329181	495778.196185	45.901287
3504.236990	495771.121966	45.906292
3504.235071	495784.236568	45.911297
3503.936560	495797.904385	45.916301
3503.867390	495783.687101	45.921306
3503.800874	495747.797881	45.926311
3503.618894	495770.865292	45.931316
3503.913225	495786.464780	45.936321
3503.900197	495821.455108	45.941325
3504.102374	495805.220215	45.946330
3504.104977	495795.092967	45.951335
3504.171013	495802.323239	45.956340
3503.986827	495803.516954	45.961345
3504.124784	495796.963342	45.966349
3504.344795	495796.574137	45.971354
3503.693381	495806.601431	45.976359
3503.995286	495803.161227	45.981364
3504.263818	495807.422703	45.986369
3503.941845	495806.207754	45.991373
3504.117036	495805.015487	45.996378
3504.131596	495798.835821	46.001383
3504.330795	495775.765748	46.006388
3504.013841	495771.360042	46.011393
3503.814409	495772.961243	46.016397
3504.060666	495772.517255	46.021402
3503.965611	495766.000464	46.026407
3504.533499	495769.303211	46.031412
3504.555479	495739.273566	46.036417
3504.215276	495739.833699	46.041421
3504.224229	495720.084865	46.046426
3504.029402	495717.229510	46.051431
3503.843342	495722.524918	46.056436
3503.937391	495735.219309	46.061441
3504.048439	495714.593545	46.066445
3504.591644	495674.607679	46.071450
3503.853009	495699.535381	46.076455
3503.769777	495709.776721	46.081460
3504.050013	495712.061623	46.086465
3503.720314	495725.076176	46.091469
3503.999073	495732.120947	46.096474
3504.393081	495730.337107	46.101479
3504.213138	495719.428522	46.106484
3504.428037	495707.242289	46.111489
3504.381887	495698.489825	46.116493
3504.207252	495669.453202	46.121498
3503.624407	495674.558171	46.126503
3503.857811	495663.331041	46.131508
3504.028752	495664.164821	46.136513
3503.881602	495676.694841	46.141517
3504.016519	495680.420486	46.146522
3503.504739	495680.602665	46.151527
3503.799679	495680.150980	46.156532
3503.985758	495690.197857	46.161537
3504.210874	495691.529418	46.166541
3504.361589	495675.100007	46.171546
3504.099473	495653.166027	46.176551
3504.339631	495655.659810	46.181556
3504.246234	495651.674449	46.186561
3504.198355	495623.478505	46.191565
3504.937941	495608.069915	46.196570
3504.431745	495635.087623	46.201575
3504.499590	495625.709489	46.206580
3504.597510	495622.453401	46.211585
3504.450473	495617.160008	46.216589
3504.859278	495553.244869	46.221594
3504.113352	495534.374684	46.226599
3503.695049	495551.150353	46.231604
3503.636769	495553.843230	46.236609
3504.145453	495563.636642	46.241613
3504.282336	495585.185471	46.246618
3503.862788	495575.479275	46.251623
3504.095463	495531.947108	46.256628
3504.425076	495555.237732	46.261633
3503.397726	495548.615058	46.266637
3504.189576	495549.198791	46.271642
3504.073357	495546.381618	46.276647
3504.255396	495517.794724	46.281652
3504.429392	495521.564859	46.286657
3504.630138	495511.912485	46.291661
3504.093224	495512.351813	46.296666
3504.101033	495534.680630	46.301671
3504.417078	495528.098772	46.306676
3504.078577	495502.125885	46.311681
3503.567872	495492.484690	46.316685
3504.429840	495469.410739	46.321690
3504.497459	495450.918221	46.326695
3503.845796	495460.692565	46.331700
3504.196824	495504.487105	46.336705
3503.966651	495499.713170	46.341709
3504.052271	495515.092705	46.346714
3504.156255	495528.494559	46.351719
3504.263596	495493.944505	46.356724
3504.754708	495484.347488	46.361729
3504.089770	495484.604513	46.366733
3504.184904	495452.790608	46.371738
3504.077914	495422.122573	46.376743
3504.588484	495424.016656	46.381748
3504.768728	495394.366513	46.386753
3504.831174	495381.191455	46.391757
3504.968107	495365.472842	46.396762
3504.740047	495360.647901	46.401767
3504.533823	495362.452753	46.406772
3504.128546	495399.835118	46.411777
3503.914658	495386.146755	46.416781
3503.841533	495363.423024	46.421786
3503.791095	495364.950073	46.426791
3503.771471	495370.219273	46.431796
3504.069330	495348.955945	46.436801
3503.769180	495346.826076	46.441805
3504.263262	495321.379588	46.446810
3504.186699	495320.885347	46.451815
3504.032457	495308.858472	46.456820
3504.046867	495340.098346	46.461825
3503.697535	495375.294591	46.466829
3504.051956	495369.820589	46.471834
3503.853908	495364.282009	46.476839
3503.684649	495373.119342	46.481844
3503.628879	495358.140079	46.486849
3503.787903	495334.164364	46.491853
3503.695260	495371.902453	46.496858
3503.567317	495353.440749	46.501863
3504.008725	495357.371190	46.506868
3503.726173	495365.770716	46.511873
3503.688089	495341.016000	46.516877
3503.956152	495364.265961	46.521882
3503.885145	495371.112981	46.526887
3504.181066	495340.178580	46.531892
3503.781097	495390.320271	46.536897
3503.771065	495362.776204	46.541901
3504.043116	495363.594016	46.546906
3503.775538	495380.194110	46.551911
3504.260160	495350.799596	46.556916
3504.077383	495379.488162	46.561921
3503.891948	495362.402711	46.566925
3504.109322	495383.027616	46.571930
3503.958428	495370.341992	46.576935
3504.168249	495346.307628	46.581940
3504.121097	495400.849443	46.586945
3503.917342	495376.222234	46.591949
3504.413029	495323.128537	46.596954
3504.172205	495318.103060	46.601959
3504.496328	495303.063702	46.606964
3504.431531	495321.302770	46.611969
3503.895576	495361.895909	46.616973
3503.898022	495348.223957	46.621978
3503.680012	495338.890863	46.626983
3504.303241	495310.031365	46.631988
3504.292373	495296.361479	46.636993
3503.823424	495324.943459	46.641997
3503.885147	495320.427150	46.647002
3504.148997	495326.107274	46.652007
3504.019116	495328.862136	46.657012
3504.162953	495307.724378	46.662017
3503.786919	495320.341456	46.667021
3503.889694	495312.881793	46.672026
3503.884019	495298.907275	46.677031
3504.097187	495305.101773	46.682036
3503.643689	495313.427073	46.687041
3503.689709	495311.900743	46.692045
3503.920375	495303.560055	46.697050
3503.952356	495299.352256	46.702055
3503.805593	495303.730131	46.707060
3504.030550	495308.454332	46.712065
3504.178786	495316.583242	46.717069
3504.054133	495324.654014	46.722074
3503.624257	495312.316262	46.727079
3503.781008	495304.392343	46.732084
3504.011671	495309.925811	46.737089
3504.120052	495290.819062	46.742093
3504.256064	495277.125945	46.747098
3503.856074	495285.695977	46.752103
3504.055623	495306.222515	46.757108
3504.214916	495300.121074	46.762113
3504.153738	495290.813800	46.767117
3504.112547	495276.439794	46.772122
3504.313154	495280.864036	46.777127
3504.117873	495273.654014	46.782132
3504.257444	495273.480057	46.787137
3503.760015	495284.698549	46.792141
3504.089813	495281.861468	46.797146
3504.128339	495263.322725	46.802151
3503.969405	495263.449132	46.807156
3504.188944	495265.034785	46.812161
3504.139987	495260.535957	46.817165
3504.256465	495263.201251	46.822170
3503.887702	495264.170997	46.827175
3503.782282	495256.339135	46.832180
3503.940051	495278.391380	46.837185
3503.569893	495284.627457	46.842189
3504.022369	495257.921566	46.847194
3503.990688	495259.395023	46.852199
3503.615576	495257.378264	46.857204
3504.099680	495253.352166	46.862209
3503.840821	495252.329746	46.867213
3504.130169	495220.636646	46.872218
3504.155602	495268.584719	46.877223
3504.201935	495268.476137	46.882228
3503.995227	495221.215009	46.887233
3504.078635	495198.972689	46.892237
3504.397483	495232.898960	46.897242
3503.797276	495220.182984	46.902247
3504.155748	495206.049562	46.907252
3503.913653	495240.773390	46.912257
3503.767124	495226.517267	46.917261
3504.292325	495208.762349	46.922266
3504.095632	495244.035989	46.927271
3503.608397	495221.529448	46.932276
3504.420394	495194.108369	46.937281
3504.441027	495182.509492	46.942285
3504.612538	495157.265674	46.947290
3504.197310	495162.445559	46.952295
3504.306197	495159.592744	46.957300
3504.293547	495152.404441	46.962305
3503.944259	495171.144351	46.967309
3503.944467	495191.753163	46.972314
3503.935575	495192.109033	46.977319
3503.979192	495162.075025	46.982324
3503.434451	495140.337015	46.987329
3504.079922	495145.855599	46.992333
3504.444282	495139.822962	46.997338
3504.567813	495131.802948	47.002343
3504.129952	495117.694064	47.007348
3504.135267	495120.478223	47.012353
3503.861596	495137.484587	47.017357
3504.191883	495113.734694	47.022362
3504.165846	495114.852817	47.027367
3504.551929	495101.120040	47.032372
3504.365380	495083.831962	47.037377
3504.646806	495089.357473	47.042381
3504.559280	495074.585543	47.047386
3504.073454	495060.028470	47.052391
3503.954085	495058.832080	47.057396
3503.882971	495037.474808	47.062401
3503.815380	495036.624687	47.067405
3504.181009	495046.947353	47.072410
3503.646806	495061.564426	47.077415
3503.731402	495067.779328	47.082420
3503.723785	495070.616175	47.087425
3503.719365	495084.997577	47.092429
3503.914730	495089.169514	47.097434
3504.092477	495103.015745	47.102439
3503.804153	495103.770239	47.107444
3504.022249	495041.351917	47.112449
3504.490345	495048.974658	47.117453
3504.578566	495062.936344	47.122458
3504.246856	495105.472577	47.127463
3504.406748	495087.117016	47.132468
3504.335531	495060.240439	47.137473
3503.912681	495078.232528	47.142477
3504.042941	495061.907075	47.147482
3504.237255	495005.264925	47.152487
3504.136398	495002.495875	47.157492
3504.260960	495019.388763	47.162497
3503.486698	495049.133432	47.167501
3504.205219	495036.006330	47.172506
3504.243635	495052.305167	47.177511
3504.122913	495046.855541	47.182516
3504.456306	495007.053299	47.187521
3504.336733	494976.538419	47.192525
3504.426667	494978.448404	47.197530
3504.596013	494972.243992	47.202535
3504.938250	494949.302183	47.207540
3504.384878	494936.224150	47.212545
3503.985183	494965.150196	47.217549
3504.004971	494964.286260	47.222554
3503.760989	494988.630366	47.227559
3503.906836	494932.299471	47.232564
3504.511055	494935.394082	47.237569
3503.876351	494939.646626	47.242573
3503.942913	494955.536008	47.247578
3504.034876	494914.657724	47.252583
3503.830705	494920.918321	47.257588
3504.263138	494944.750470	47.262593
3504.322333	494915.068053	47.267597
3503.864552	494943.750132	47.272602
3504.124537	494913.681517	47.277607
3503.685976	494931.524322	47.282612
3504.287609	494936.644807	47.287617
3504.238304	494968.604296	47.292621
3504.021220	494961.650780	47.297626
3503.934053	494924.902395	47.302631
3503.908409	494878.776409	47.307636
3504.025843	494854.148366	47.312641
3504.160240	494877.571981	47.317645
3504.288016	494881.400191	47.322650
3504.072162	494893.384599	47.327655
3504.391922	494872.978085	47.332660
3504.679980	494863.412844	47.337665
3503.935821	494851.327007	47.342669
3504.178140	494836.047015	47.347674
3504.058928	494820.115241	47.352679
3504.483437	494826.327131	47.357684
3504.182576	494847.338377	47.362689
3503.844586	494848.961559	47.367693
3504.147271	494846.229972	47.372698
3503.562678	494852.094994	47.377703
3503.985768	494878.106092	47.382708
3504.225937	494882.473540	47.387713
3503.943750	494878.973584	47.392717
3503.899295	494840.547265	47.397722
3503.945152	494838.008185	47.402727
3504.013694	494841.440671	47.407732
3504.344796	494824.019886	47.412737
3503.902228	494815.785397	47.417741
3504.246896	494809.958314	47.422746
3503.757974	494832.872871	47.427751
3503.847640	494847.796592	47.432756
3503.847084	494848.758793	47.437761
3503.923575	494811.781766	47.442765
3503.832485	494840.861773	47.447770
3503.923848	494868.343154	47.452775
3503.892176	494872.956122	47.457780
3504.224193	494830.824424	47.462785
3503.690255	494851.973781	47.467789
3503.795577	494856.413189	47.472794
3503.645212	494876.337239	47.477799
3503.691325	494877.190788	47.482804
3504.027864	494867.921706	47.487809
3503.941420	494871.682506	47.492813
3503.964730	494854.766134	47.497818
3503.943972	494823.931561	47.502823
3504.001165	494814.301513	47.507828
3504.581702	494823.020589	47.512833
3504.056092	494810.748268	47.517837
3504.095466	494780.207939	47.522842
3504.430981	494774.382291	47.527847
3503.930763	494807.476714	47.532852
3504.172791	494801.463304	47.537857
3504.259359	494786.410439	47.542861
3504.161672	494787.033537	47.547866
3504.421145	494792.410697	47.552871
3504.226447	494766.667224	47.557876
3504.218536	494754.819404	47.562881
3503.752144	494767.552416	47.567885
3504.295092	494748.123226	47.572890
3504.081597	494743.295820	47.577895
3504.250936	494757.903197	47.582900
3503.810120	494778.531547	47.587905
3503.837805	494787.135482	47.592909
3503.858695	494778.928991	47.597914
3503.859874	494778.523720	47.602919
3503.926355	494799.578229	47.607924
3504.161317	494796.705428	47.612929
3503.557853	494807.839696	47.617933
3503.768588	494802.590788	47.622938
3503.866660	494798.473701	47.627943
3503.863783	494784.042617	47.632948
3504.075311	494799.656033	47.637953
3503.871143	494817.259350	47.642957
3504.022416	494803.766016	47.647962
3504.065226	494801.429960	47.652967
3504.055615	494790.898994	47.657972
3503.889299	494775.734182	47.662977
3503.426691	494774.541393	47.667981
3503.726203	494775.354892	47.672986
3503.699070	494793.892351	47.677991
3503.736891	494808.571114	47.682996
3503.918827	494805.352238	47.688001
3503.884964	494813.915252	47.693005
3504.229909	494798.213911	47.698010
3504.011561	494772.372910	47.703015
3503.732381	494758.643763	47.708020
3503.936416	494757.244322	47.713025
3503.578685	494778.062088	47.718029
3503.907932	494775.427566	47.723034
3503.905119	494749.552463	47.728039
3504.049340	494728.464617	47.733044
3504.274448	494732.328110	47.738049
3503.506695	494761.667115	47.743053
3503.809944	494759.340523	47.748058
3503.935744	494780.031218	47.753063
3503.774365	494779.449095	47.758068
3504.187930	494727.227493	47.763073
3504.059930	494735.957335	47.768077
3504.165260	494756.144920	47.773082
3503.907969	494772.288200	47.778087
3503.825460	494779.542355	47.783092
3503.941518	494765.193730	47.788097
3503.969109	494771.417743	47.793101
3503.722270	494744.619102	47.798106
3503.725671	494741.479074	47.803111
3504.116416	494732.657090	47.808116
3504.685778	494725.528533	47.813121
3504.392115	494737.525342	47.818125
3504.219833	494706.815798	47.823130
3504.376587	494710.234366	47.828135
3504.160595	494736.296047	47.833140
3504.054373	494729.679379	47.838145
3504.205996	494703.678526	47.843149
3504.105781	494710.024036	47.848154
3504.607955	494683.663920	47.853159
3504.312696	494676.013730	47.858164
3504.730350	494657.313173	47.863169
3504.345950	494661.171752	47.868173
3503.849628	494669.453473	47.873178
3503.797554	494660.853364	47.878183
3503.455797	494677.010079	47.883188
3503.796275	494706.528454	47.888193
3503.917282	494665.138653	47.893197
3503.853320	494676.440906	47.898202
3504.010425	494703.912140	47.903207
3503.901605	494710.056462	47.908212
3504.452054	494674.219534	47.913217
3503.895712	494689.599960	47.918221
3503.788357	494683.439190	47.923226
3503.922246	494679.265778	47.928231
3503.909186	494651.265389	47.933236
3503.851514	494632.234842	47.938241
3503.748226	494667.190997	47.943245
3504.038300	494674.740760	47.948250
3504.183931	494679.882761	47.953255
3503.884129	494635.622447	47.958260
3504.437796	494622.014736	47.963265
3503.885163	494638.711193	47.968269
3503.615110	494665.996817	47.973274
3504.143608	494677.914342	47.978279
3504.196606	494631.775307	47.983284
3504.046959	494644.306423	47.988289
3503.817999	494671.737456	47.993293
3504.304281	494656.216203	47.998298
3504.082834	494631.286967	48.003303
3503.874062	494659.018652	48.008308
3504.243194	494635.667103	48.013313
3504.159983	494643.984809	48.018317
3504.025408	494640.613386	48.023322
3504.126146	494647.585440	48.028327
3504.027288	494595.140639	48.033332
3503.897286	494605.643173	48.038337
3503.695886	494639.855325	48.043341
3503.862187	494657.805333	48.048346
3504.137193	494649.102879	48.053351
3503.866385	494641.600722	48.058356
3503.721322	494620.710392	48.063361
3504.096320	494631.335637	48.068365
3504.269148	494599.052238	48.073370
3504.422551	494586.115422	48.078375
3504.175292	494609.751619	48.083380
3504.057283	494604.605258	48.088385
3503.955599	494624.521885	48.093389
3504.072741	494621.768956	48.098394
3504.317728	494574.080305	48.103399
3503.959330	494570.693611	48.108404
3504.455135	494560.285172	48.113409
3504.148875	494577.499753	48.118413
3503.855061	494577.748760	48.123418
3503.768762	494546.620257	48.128423
3504.646614	494526.580882	48.133428
3504.511528	494515.158112	48.138433
3504.194694	494559.111112	48.143437
3504.157147	494575.776842	48.148442
3504.526894	494559.058626	48.153447
3504.159493	494549.141092	48.158452
3503.973393	494513.521554	48.163457
3504.567891	494492.260987	48.168461
3503.913715	494502.694523	48.173466
3504.133468	494517.192847	48.178471
3504.111875	494524.184284	48.183476
3504.599486	494516.106453	48.188481
3504.051992	494509.255631	48.193485
3503.894814	494500.418872	48.198490
3504.220192	494439.348775	48.203495
3503.711309	494476.749388	48.208500
3503.946544	494501.828592	48.213505
3503.724703	494500.192623	48.218509
3503.994070	494465.361839	48.223514
3504.313428	494445.562571	48.228519
3503.527517	494475.310004	48.233524
3503.761168	494476.944134	48.238529
3503.834181	494470.450954	48.243533
3504.076064	494450.157559	48.248538
3504.194665	494443.302699	48.253543
3504.032576	494471.533666	48.258548
3503.927835	494508.060126	48.263553
3504.034883	494489.712324	48.268557
3503.550567	494471.609895	48.273562
3504.166195	494452.371458	48.278567
3504.088583	494458.510930	48.283572
3504.163376	494470.753497	48.288577
3504.156861	494453.638920	48.293581
3504.172892	494463.510796	48.298586
3504.034773	494478.116358	48.303591
3503.955613	494472.102974	48.308596
3503.739519	494456.084924	48.313601
3503.891921	494456.010208	48.318605
3503.942483	494479.751409	48.323610
3503.919456	494469.374293	48.328615
3503.621874	494460.205243	48.333620
3504.023231	494441.608320	48.338625
3504.382955	494431.879613	48.343629
3504.341186	494422.163728	48.348634
3504.293928	494423.285247	48.353639
3504.273602	494411.337893	48.358644
3504.148647	494395.913041	48.363649
3503.917167	494388.708392	48.368653
3503.869096	494389.171747	48.373658
3504.264694	494383.083289	48.378663
3503.960399	494394.170514	48.383668
3503.669282	494425.004491	48.388673
3503.463434	494436.329320	48.393677
3503.538462	494422.999674	48.398682
3504.279147	494417.261783	48.403687
3503.701625	494442.672093	48.408692
3503.855453	494425.937248	48.413697
3503.604849	494419.343292	48.418701
3503.471868	494411.667340	48.423706
3503.610294	494415.747154	48.428711
3503.729055	494429.451302	48.433716
3504.374374	494423.222107	48.438721
3504.562298	494409.672055	48.443725
3504.237801	494394.633209	48.448730
3503.986998	494399.686039	48.453735
3503.848248	494450.548565	48.458740
3503.916306	494430.130711	48.463745
3503.621531	494429.316473	48.468749
3504.227229	494395.495791	48.473754
3504.354158	494416.996925	48.478759
3503.626801	494451.950858	48.483764
3503.866556	494418.491891	48.488769
3504.154302	494449.740706	48.493773
3503.969628	494440.958903	48.498778
3504.082303	494415.976561	48.503783
3503.732731	494386.611098	48.508788
3504.167511	494360.868832	48.513793
3504.218167	494374.381233	48.518797
3504.366115	494353.950667	48.523802
3504.047116	494355.165783	48.528807
3503.846452	494393.935713	48.533812
3504.003211	494420.040195	48.538817
3503.873739	494425.327029	48.543821
3503.710795	494431.530637	48.548826
3503.676121	494401.609042	48.553831
3503.478952	494403.564468	48.558836
3503.886513	494386.283099	48.563841
3504.257748	494379.287004	48.568845
3503.974067	494405.157300	48.573850
3503.903579	494423.195603	48.578855
3503.766579	494405.848418	48.583860
3503.914537	494399.900386	48.588865
3503.802556	494405.792118	48.593869
3504.630960	494385.659131	48.598874
3504.764035	494362.547103	48.603879
3504.002928	494359.122750	48.608884
3503.870139	494366.283739	48.613889
3503.527708	494373.376587	48.618893
3503.889805	494378.332541	48.623898
3504.044041	494389.347288	48.628903
3503.697878	494403.985794	48.633908
3503.927975	494409.114519	48.638913
3503.918869	494402.229192	48.643917
3504.076226	494397.798817	48.648922
3504.091723	494377.591765	48.653927
3503.853027	494380.060140	48.658932
3504.229383	494368.455159	48.663937
3503.991885	494377.303755	48.668941
3504.039460	494367.117975	48.673946
3504.464275	494364.670841	48.678951
3504.312157	494343.123016	48.683956
3504.213422	494356.051386	48.688961
3503.961579	494382.220510	48.693965
3503.864839	494359.347358	48.698970
3503.694010	494357.956503	48.703975
3503.643345	494357.306228	48.708980
3503.283786	494353.160104	48.713985
3503.467343	494359.460879	48.718989
3503.545959	494355.194854	48.723994
3503.952132	494377.208914	48.728999
3503.865375	494410.441244	48.734004
3503.952044	494419.187941	48.739009
3504.158045	494423.003881	48.744013
3503.921777	494401.621340	48.749018
3504.221205	494390.585552	48.754023
3504.123834	494373.080157	48.759028
3503.925123	494354.679276	48.764033
3503.952880	494336.698324	48.769037
3504.040924	494366.054593	48.774042
3504.458121	494386.497115	48.779047
3504.160618	494372.162918	48.784052
3504.054355	494362.457196	48.789057
3503.966575	494373.915314	48.794061
3503.786943	494347.409301	48.799066
3503.709795	494354.105756	48.804071
3503.865438	494361.727536	48.809076
3503.855913	494356.108213	48.814081
3503.565233	494361.066080	48.819085
3504.042935	494360.433561	48.824090
3504.744895	494335.206047	48.829095
3504.580291	494314.926119	48.834100
3504.567914	494299.128922	48.839105
3504.167337	494303.547154	48.844109
3503.947198	494324.546234	48.849114
3504.180526	494291.999544	48.854119
3503.805740	494298.945620	48.859124
3504.207187	494283.994487	48.864129
3504.044349	494300.123249	48.869133
3503.971577	494307.122859	48.874138
3504.354018	494291.972183	48.879143
3504.159188	494284.711062	48.884148
3504.138251	494301.425054	48.889153
3504.301997	494291.727252	48.894157
3504.260117	494267.680631	48.899162
3504.212122	494258.573305	48.904167
3503.872390	494258.424466	48.909172
3504.420980	494220.358859	48.914177
3504.133400	494241.419332	48.919181
3504.255312	494271.783169	48.924186
3504.289247	494234.355965	48.929191
3504.115505	494220.356557	48.934196
3504.172850	494204.193788	48.939201
3503.991143	494206.045514	48.944205
3503.896794	494209.807698	48.949210
3503.863694	494225.409631	48.954215
3503.212026	494220.701989	48.959220
3503.829562	494202.982149	48.964225
3503.962105	494228.584343	48.969229
3503.787566	494238.486463	48.974234
3503.907373	494222.870861	48.979239
3503.728147	494236.723532	48.984244
3503.513501	494227.338702	48.989249
3503.851480	494238.577688	48.994253
3503.993634	494230.706255	48.999258
3504.120749	494238.687065	49.004263
3504.070512	494258.190847	49.009268
3503.787026	494218.838885	49.014273
3504.245083	494201.954471	49.019277
3503.806569	494245.572980	49.024282
3503.916881	494220.388193	49.029287
3503.531356	494229.108343	49.034292
3503.294910	494236.994707	49.039297
3503.767513	494232.109353	49.044301
3504.285342	494231.824957	49.049306
3504.117563	494216.356085	49.054311
3504.204716	494212.392510	49.059316
3504.085711	494206.233422	49.064321
3504.064562	494252.267235	49.069325
3503.857308	494241.767196	49.074330
3503.851956	494225.411802	49.079335
3504.286025	494210.202260	49.084340
3503.998175	494214.653333	49.089345
3504.197075	494246.878669	49.094349
3503.756880	494229.376690	49.099354
3503.638605	494230.306892	49.104359
3503.382242	494236.221501	49.109364
3503.622178	494221.397125	49.114369
3503.890991	494231.532999	49.119373
3504.070085	494214.338222	49.124378
3504.195272	494203.177950	49.129383
3504.238920	494210.918773	49.134388
3503.933755	494254.212351	49.139393
3504.153917	494252.962238	49.144397
3503.969726	494225.798471	49.149402
3504.061903	494210.440418	49.154407
3504.138531	494171.993567	49.159412
3504.005843	494197.283259	49.164417
3504.193088	494212.495903	49.169421
3503.827373	494194.982117	49.174426
3503.499560	494194.426284	49.179431
3503.438157	494201.221582	49.184436
3503.628832	494185.392191	49.189441
3504.182710	494179.025453	49.194445
3504.070489	494193.475230	49.199450
3503.914993	494233.149853	49.204455
3503.756785	494217.679469	49.209460
3504.009993	494206.701517	49.214465
3504.003475	494221.742226	49.219469
3503.703524	494238.854848	49.224474
3504.130343	494233.369068	49.229479
3503.896714	494233.203457	49.234484
3503.925421	494227.021027	49.239489
3503.800850	494217.318122	49.244493
3503.450641	494208.461097	49.249498
3503.880423	494196.594371	49.254503
3503.703412	494179.354574	49.259508
3503.855263	494228.652614	49.264513
3503.860623	494214.979361	49.269517
3503.758982	494207.095816	49.274522
3504.143736	494185.918691	49.279527
3503.777747	494207.903093	49.284532
3503.907427	494239.734275	49.289537
3503.850235	494240.148436	49.294541
3503.530110	494215.335513	49.299546
3504.288210	494188.883599	49.304551
3503.791700	494235.904089	49.309556
3504.135698	494207.137646	49.314561
3504.088989	494238.946072	49.319565
3503.817711	494202.529182	49.324570
3503.997127	494226.452895	49.329575
3503.978499	494251.015544	49.334580
3504.129269	494226.938418	49.339585
3503.671015	494227.973000	49.344589
3503.386518	494236.170791	49.349594
3503.575942	494227.279113	49.354599
3503.544634	494232.601124	49.359604
3504.144610	494209.972126	49.364609
3504.057341	494198.592241	49.369613
3503.867485	494204.597624	49.374618
3503.931434	494201.751764	49.379623
3504.132712	494203.897422	49.384628
3504.021803	494201.231118	49.389633
3503.917587	494259.026206	49.394637
3503.870857	494261.869360	49.399642
3503.953075	494236.385205	49.404647
3503.878982	494246.018251	49.409652
3503.808657	494210.227911	49.414657
3504.309730	494189.943899	49.419661
3504.041977	494167.097541	49.424666
3504.124111	494197.214594	49.429671
3504.178460	494229.716003	49.434676
3504.052898	494205.125504	49.439681
3504.206830	494205.253101	49.444685
3503.589611	494201.299587	49.449690
3504.086041	494186.789109	49.454695
3504.336511	494173.026442	49.459700
3504.234642	494175.574493	49.464705
3504.141334	494169.563247	49.469709
3503.871092	494162.465915	49.474714
3504.099979	494159.340783	49.479719
3503.749494	494166.029873	49.484724
3504.167255	494174.268601	49.489729
3504.060996	494168.968344	49.494733
3503.878828	494163.325613	49.499738
3503.751430	494152.863540	49.504743
3504.282352	494142.196122	49.509748
3503.980278	494132.268037	49.514753
3504.244040	494133.036578	49.519757
3503.983643	494146.952786	49.524762
3504.293063	494145.992390	49.529767
3504.470338	494130.924652	49.534772
3504.539446	494103.872583	49.539777
3504.669516	494096.661309	49.544781
3504.271580	494102.750255	49.549786
3504.198802	494099.672798	49.554791
3503.457009	494094.726174	49.559796
3503.723044	494097.722470	49.564801
3503.991744	494100.465149	49.569805
3504.290995	494062.590548	49.574810
3504.070878	494081.665617	49.579815
3504.070466	494109.517108	49.584820
3504.216073	494092.631345	49.589825
3503.752506	494089.109269	49.594829
3503.758579	494076.246023	49.599834
3504.080627	494058.674032	49.604839
3503.975999	494071.704811	49.609844
3503.800307	494071.378122	49.614849
3504.018394	494080.205484	49.619853
3504.163464	494107.628869	49.624858
3504.124100	494119.484603	49.629863
3504.017538	494121.577653	49.634868
3504.402051	494103.286886	49.639873
3504.415554	494069.711136	49.644877
3503.873041	494067.923261	49.649882
3504.101245	494083.484009	49.654887
3503.962912	494066.896300	49.659892
3504.113997	494037.299224	49.664897
3504.182294	494026.603590	49.669901
3504.352458	494025.462643	49.674906
3504.184782	494057.746255	49.679911
3503.747972	494056.549339	49.684916
3503.954330	494032.716368	49.689921
3503.774074	494021.654907	49.694925
3503.566643	494015.205898	49.699930
3504.360319	494009.864620	49.704935
3504.053579	494001.962768	49.709940
3503.720171	494002.319318	49.714945
3503.848177	494007.059180	49.719949
3503.769858	494028.137457	49.724954
3503.766494	494045.962962	49.729959
3503.551222	494046.351476	49.734964
3503.826063	494036.635980	49.739969
3504.007155	493994.981985	49.744973
3503.327017	494018.282251	49.749978
3503.892785	494063.869284	49.754983
3503.856127	494047.670597	49.759988
3503.699334	494068.508038	49.764993
3504.334151	494031.542471	49.769997
3503.704820	494044.048540	49.775002
3503.989075	494054.739100	49.780007
3503.676868	494068.359722	49.785012
3503.767052	494076.194524	49.790017
3504.102283	494039.276328	49.795021
3503.722537	494058.781767	49.800026
3504.080274	494069.713898	49.805031
3504.078438	494058.117866	49.810036
3504.032711	494004.599569	49.815041
3504.256995	493998.993818	49.820045
3503.815449	494025.142794	49.825050
3503.998485	494039.799215	49.830055
3503.844143	494053.141699	49.835060
3504.189763	494057.847149	49.840065
3504.475745	494003.516830	49.845069
3503.537306	494041.847088	49.850074
3504.017960	494020.350780	49.855079
3504.499195	493999.867139	49.860084
3504.258062	493999.095041	49.865089
3504.317229	493979.538961	49.870093
3504.013215	493979.485751	49.875098
3504.370577	493956.945434	49.880103
3503.993767	493967.588623	49.885108
3504.071785	493962.968128	49.890113
3504.381235	493963.223061	49.895117
3504.237698	493969.018641	49.900122
3504.180247	493942.087619	49.905127
3504.091576	493932.834644	49.910132
3503.863821	493951.505940	49.915137
3504.178548	493963.305802	49.920141
3503.954142	493992.661415	49.925146
3504.167202	493964.978717	49.930151
3504.090489	493934.455339	49.935156
3503.660808	493955.234764	49.940161
3503.993547	493971.893147	49.945165
3503.626331	493986.282114	49.950170
3503.848698	493926.847063	49.955175
3504.223458	493926.484000	49.960180
3504.120492	493940.780593	49.965185
3503.961962	493933.361677	49.970189
3503.805038	493929.183426	49.975194
3503.925195	493955.902023	49.980199
3503.746051	493988.542044	49.985204
3504.056393	493978.618348	49.990209
3503.608465	493946.988966	49.995213
3503.610396	493970.029559	50.000218
3503.928120	493993.678514	50.005223
3503.826461	493949.891627	50.010228
3503.660470	493956.298432	50.015233
3503.617103	493977.371242	50.020237
3503.680073	493985.463581	50.025242
3503.863484	493984.421816	50.030247
3503.626329	493977.623018	50.035252
3503.540823	493991.309141	50.040257
3503.826799	493963.462997	50.045261
3503.675324	493974.982070	50.050266
3503.842442	493997.996516	50.055271
3504.219063	493956.362166	50.060276
3504.046282	493950.363411	50.065281
3503.515811	493982.653862	50.070285
3503.598183	494016.822310	50.075290
3503.868869	493980.623148	50.080295
3503.985079	493947.132219	50.085300
3504.412948	493953.293235	50.090305
3504.291776	493960.503184	50.095309
3503.755896	493980.185303	50.100314
3504.189804	493957.025216	50.105319
3504.228972	494002.442444	50.110324
3503.815055	493973.491607	50.115329
3504.055835	493954.868939	50.120333
3504.143037	493938.853137	50.125338
3504.087286	493935.823600	50.130343
3504.379968	493926.814177	50.135348
3504.300172	493921.762863	50.140353
3504.581720	493912.603275	50.145357
3504.059977	493905.191123	50.150362
3504.008372	493901.553252	50.155367
3504.014399	493936.037754	50.160372
3504.121125	493920.069489	50.165377
3503.768691	493896.932345	50.170381
3504.288544	493880.341707	50.175386
3504.250421	493876.448503	50.180391
3503.913212	493897.061457	50.185396
3503.997786	493941.762704	50.190401
3504.101515	493937.897729	50.195405
3503.903529	493934.789396	50.200410
3504.063045	493937.802556	50.205415
3504.056347	493927.270637	50.210420
3504.136303	493883.151047	50.215425
3504.035275	493912.791121	50.220429
3503.843751	493920.062845	50.225434
3503.985543	493886.263925	50.230439
3504.082740	493855.105252	50.235444
3503.779390	493849.633499	50.240449
3504.225926	493852.094907	50.245453
3503.915263	493897.415773	50.250458
3504.266023	493909.463171	50.255463
3503.996714	493889.604442	50.260468
3504.111964	493866.393333	50.265473
3504.133527	493916.421755	50.270477
3503.932444	493901.616196	50.275482
3504.131905	493868.061324	50.280487
3503.906058	493876.908317	50.285492
3503.590062	493857.816527	50.290497
3504.203320	493840.907252	50.295501
3503.881186	493875.241182	50.300506
3504.112205	493847.454191	50.305511
3503.622688	493839.125405	50.310516
3504.019946	493821.693219	50.315521
3504.203296	493806.877457	50.320525
3503.876307	493845.415306	50.325530
3503.812891	493839.500506	50.330535
3503.743208	493849.386260	50.335540
3503.871118	493858.683739	50.340545
3503.952899	493859.075941	50.345549
3503.683239	493858.662823	50.350554
3503.934636	493858.623097	50.355559
3503.732823	493855.008960	50.360564
3504.416493	493840.468615	50.365569
3504.344970	493829.187292	50.370573
3504.107459	493885.333508	50.375578
3503.967210	493857.149463	50.380583
3504.616706	493857.198728	50.385588
3503.958416	493838.566141	50.390593
3504.209718	493806.522152	50.395597
3504.094501	493845.684842	50.400602
3504.138460	493849.172039	50.405607
3503.924935	493837.457412	50.410612
3503.780345	493832.872072	50.415617
3504.092360	493807.806759	50.420621
3504.375577	493821.333443	50.425626
3504.095526	493828.467278	50.430631
3503.940499	493818.262581	50.435636
3504.352674	493781.382349	50.440641
3503.956252	493770.051067	50.445645
3503.961394	493817.854199	50.450650
3504.051185	493816.827224	50.455655
3503.940236	493816.743495	50.460660
3503.904250	493798.265698	50.465665
3503.707126	493778.091601	50.470669
3504.065853	493767.349907	50.475674
3504.298846	493766.199014	50.480679
3504.197732	493809.208179	50.485684
3503.766795	493790.286407	50.490689
3504.105903	493760.102130	50.495693
3503.677156	493817.291578	50.500698
3504.055945	493791.911851	50.505703
3503.876267	493788.800600	50.510708
3503.973825	493765.288322	50.515713
3503.993125	493772.729338	50.520717
3503.907313	493800.746712	50.525722
3503.432815	493760.208614	50.530727
3503.475465	493755.593658	50.535732
3503.856061	493720.541331	50.540737
3503.930428	493742.254118	50.545741
3503.360000	493688.210167	50.550746
3503.552834	493619.309106	50.555751
3503.715999	493584.645373	50.560756
3503.376142	493521.651789	50.565761
3503.304433	493402.860137	50.570765
3503.509668	493291.214990	50.575770
3502.995000	493242.832731	50.580775
3503.020738	493124.530306	50.585780
3502.192180	492991.979860	50.590785
3502.365251	492854.053979	50.595789
3502.181146	492720.234951	50.600794
3501.888130	492621.578420	50.605799
3501.606569	492498.003073	50.610804
3501.137448	492324.521868	50.615809
3501.071508	492139.631004	50.620813
3501.080821	491963.639889	50.625818
3500.890020	491781.348095	50.630823
3500.527809	491636.255548	50.635828
3500.173900	491463.457167	50.640833
3500.082631	491263.367801	50.645837
3499.589433	491064.606012	50.650842
3499.626772	490822.201166	50.655847
3499.360845	490580.398264	50.660852
3498.447156	490366.349051	50.665857
3498.509311	490160.095137	50.670861
3498.157593	489955.626492	50.675866
3497.578212	489704.035744	50.680871
3497.152675	489431.143674	50.685876
3497.013769	489200.496979	50.690881
3496.874375	488921.423404	50.695885
3496.181161	488687.261719	50.700890
3496.189679	488406.586923	50.705895
3495.586107	488139.985527	50.710900
3494.772712	487869.209134	50.715905
3494.816556	487555.184681	50.720909
3494.020922	487309.827114	50.725914
3493.142988	486991.886521	50.730919
3492.826680	486694.723321	50.735924
3492.592753	486424.645377	50.740929
3492.210246	486135.133557	50.745933
3491.436789	485837.928021	50.750938
3490.927805	485515.041144	50.755943
3490.471291	485199.638653	50.760948
3490.034130	484881.390782	50.765953
3489.579813	484585.990041	50.770957
3488.951496	484276.274044	50.775962
3488.140797	483940.995565	50.780967
3487.715386	483625.765162	50.785972
3487.283015	483297.762473	50.790977
3487.216277	482977.347420	50.795981
3486.511872	482665.084344	50.800986
3486.030118	482335.654534	50.805991
3485.415791	481981.461940	50.810996
3484.381470	481615.725422	50.816001
3484.707838	481245.510450	50.821005
3483.662847	480916.753922	50.826010
3482.838244	480586.234123	50.831015
3482.437077	480200.912096	50.836020
3481.924056	479847.678601	50.841025
3481.185994	479526.603937	50.846029
3480.310014	479200.224655	50.851034
3479.720185	478829.146386	50.856039
3479.625786	478442.272008	50.861044
3478.885179	478072.774578	50.866049
3478.385180	477735.770178	50.871053
3477.457343	477406.075393	50.876058
3476.763556	477027.428342	50.881063
3475.957940	476660.043852	50.886068
3475.714407	476278.574544	50.891073
3475.404363	475881.294286	50.896077
3474.138275	475551.166403	50.901082
3473.556461	475183.770347	50.906087
3473.779659	474775.131243	50.911092
3472.309818	474415.971991	50.916097
3471.963534	474090.642597	50.921101
3471.160221	473716.056891	50.926106
3469.953126	473326.877853	50.931111
3469.434014	472945.186759	50.936116
3468.901779	472573.933799	50.941121
3468.747074	472238.152217	50.946125
3467.526361	471851.380755	50.951130
3467.437561	471442.217503	50.956135
3466.647000	471108.241780	50.961140
3465.432706	470742.032139	50.966145
3464.772577	470349.719137	50.971149
3464.558722	469958.646416	50.976154
3464.186936	469593.246674	50.981159
3463.109836	469244.177034	50.986164
3462.331162	468841.206745	50.991169
3461.780333	468459.133856	50.996173
3460.898834	468107.377696	51.001178
3460.279952	467701.774282	51.006183
3459.841862	467359.366995	51.011188
3458.897327	466972.714991	51.016193
3458.811456	466569.236748	51.021197
3458.161806	466196.418365	51.026202
3457.365372	465821.689620	51.031207
3456.493866	465473.133626	51.036212
3455.638068	465109.609126	51.041217
3454.805618	464697.490822	51.046221
3454.106037	464318.460421	51.051226
3454.039849	463926.137090	51.056231
3453.230067	463548.378428	51.061236
3452.204750	463214.923617	51.066241
3451.259241	462846.252545	51.071245
3450.808694	462450.970786	51.076250
3450.237186	462066.960826	51.081255
3449.596300	461699.236502	51.086260
3448.390255	461320.233619	51.091265
3447.864282	460942.232535	51.096269
3446.796309	460585.918871	51.101274
3446.472226	460206.351456	51.106279
3446.502482	459816.627116	51.111284
3445.293706	459496.637371	51.116289
3444.496938	459104.951423	51.121293
3443.999373	458716.711452	51.126298
3443.797515	458323.345045	51.131303
3442.442817	457965.563232	51.136308
3441.878661	457630.986658	51.141313
3440.875623	457238.133564	51.146317
3440.118237	456856.142130	51.151322
3439.796167	456474.836344	51.156327
3438.977881	456159.302785	51.161332
3438.103263	455798.721484	51.166337
3437.385299	455414.365487	51.171341
3436.906047	455042.547788	51.176346
3436.198713	454673.601310	51.181351
3435.505291	454279.176194	51.186356
3434.528800	453970.943328	51.191361
3434.222592	453582.026139	51.196365
3433.462677	453200.176218	51.201370
3432.539834	452837.779541	51.206375
3431.963307	452510.080577	51.211380
3431.125412	452129.239956	51.216385
3430.890190	451737.996795	51.221389
3429.808975	451380.625773	51.226394
3429.473125	451047.996477	51.231399
3428.721371	450697.311891	51.236404
3427.785906	450343.403262	51.241409
3427.354024	449971.089798	51.246413
3425.837193	449595.998520	51.251418
3425.517074	449217.514805	51.256423
3424.695954	448898.278489	51.261428
3424.013237	448518.013800	51.266433
3423.761352	448145.135289	51.271437
3422.779679	447837.379743	51.276442
3422.258873	447440.476105	51.281447
3421.760362	447125.072689	51.286452
3420.487138	446750.760271	51.291457
3420.448995	446399.238757	51.296461
3419.285916	446048.295960	51.301466
3418.656445	445691.984930	51.306471
3418.131974	445317.683849	51.311476
3417.403062	444997.415947	51.316481
3416.615983	444646.240831	51.321485
3415.759078	444275.529163	51.326490
3414.904609	443943.338538	51.331495
3414.653298	443565.870594	51.336500
3413.393000	443269.115355	51.341505
3412.969752	442897.704825	51.346509
3412.322973	442529.268231	51.351514
3411.727609	442214.577033	51.356519
3411.098270	441850.594644	51.361524
3410.305773	441502.674519	51.366529
3409.554953	441152.712212	51.371533
3408.571130	440820.093262	51.376538
3407.646193	440492.740324	51.381543
3407.413750	440123.262811	51.386548
3406.417851	439814.010976	51.391553
3405.815885	439462.148053	51.396557
3405.282326	439096.078999	51.401562
3404.404015	438795.122205	51.406567
3403.783716	438449.644991	51.411572
3402.922636	438121.971406	51.416577
3402.800137	437778.030907	51.421581
3401.839920	437436.832999	51.426586
3401.040595	437118.275800	51.431591
3400.743079	436761.782387	51.436596
3399.669909	436422.975021	51.441601
3399.483319	436094.914480	51.446605
3398.467597	435744.029522	51.451610
3397.977378	435415.652763	51.456615
3397.077498	435082.614142	51.461620
3396.546682	434726.332114	51.466625
3395.916355	434383.542916	51.471629
3395.087343	434074.778111	51.476634
3394.756822	433703.469927	51.481639
3394.090369	433392.766921	51.486644
3392.993085	433027.003879	51.491649
3392.125027	432729.579009	51.496653
3391.788355	432363.203862	51.501658
3390.882933	432053.766753	51.506663
3390.519916	431707.167060	51.511668
3389.027856	431391.746012	51.516673
3389.267932	431026.225773	51.521677
3387.988624	430731.052293	51.526682
3387.554827	430377.107422	51.531687
3387.063633	430055.976154	51.536692
3386.360560	429719.612385	51.541697
3385.554791	429387.095185	51.546701
3384.695314	429048.436672	51.551706
3383.970159	428726.665967	51.556711
3383.227991	428404.233765	51.561716
3382.680168	428057.488275	51.566721
3381.809313	427732.960424	51.571725
3381.103343	427420.567580	51.576730
3380.420632	427072.941767	51.581735
3379.620264	426769.470620	51.586740
3378.720738	426429.235987	51.591745
3378.512080	426124.648104	51.596749
3377.978777	425783.026725	51.601754
3377.267928	425474.294827	51.606759
3376.820980	425142.887333	51.611764
3375.624438	424813.219884	51.616769
3375.481026	424492.906705	51.621773
3375.008155	424135.939226	51.626778
3373.694457	423857.256062	51.631783
3372.954618	423511.905086	51.636788
3371.916889	423192.276944	51.641793
3372.060726	422849.165580	51.646797
3371.109991	422555.780890	51.651802
3370.743465	422200.168574	51.656807
3369.862554	421921.270412	51.661812
3369.143543	421563.927568	51.666817
3368.284901	421256.975259	51.671821
3367.349266	420912.435742	51.676826
3366.913538	420623.928191	51.681831
3366.536520	420275.431255	51.686836
3365.318692	419975.685449	51.691841
3364.943072	419649.637299	51.696845
3363.900482	419336.875616	51.701850
3363.568380	418992.750660	51.706855
3362.993491	418706.100041	51.711860
3362.310269	418372.057955	51.716865
3361.440739	418059.661327	51.721869
3361.057255	417731.077288	51.726874
3359.875649	417425.658810	51.731879
3359.741822	417089.634838	51.736884
3358.925228	416772.617305	51.741889
3358.557548	416457.252952	51.746893
3357.546251	416118.587101	51.751898
3356.984769	415826.163626	51.756903
3355.897262	415485.266594	51.761908
3355.212022	415160.029411	51.766913
3354.630052	414872.859021	51.771917
3353.889974	414533.776126	51.776922
3352.967535	414231.154166	51.781927
3352.709007	413904.056945	51.786932
3351.662625	413606.682399	51.791937
3351.470409	413293.695423	51.796941
3350.707167	412993.525708	51.801946
3350.432159	412659.937847	51.806951
3349.347540	412336.181003	51.811956
3348.446096	412048.398396	51.816961
3348.169643	411706.312971	51.821965
3347.396450	411406.154244	51.826970
3346.443115	411100.710035	51.831975
3345.853185	410788.547418	51.836980
3344.547636	410466.609529	51.841985
3344.199425	410163.398012	51.846989
3343.347612	409865.955471	51.851994
3342.830041	409537.352107	51.856999
3342.285049	409247.783732	51.862004
3341.334477	408943.892921	51.867009
3340.856179	408648.336225	51.872013
3340.476958	408319.748701	51.877018
3339.361215	408042.686453	51.882023
3338.573841	407718.172438	51.887028
3337.749266	407426.115076	51.892033
3337.444371	407103.271888	51.897037
3336.732996	406847.432429	51.902042
3335.840028	406519.288216	51.907047
3335.873638	406197.195362	51.912052
3334.864599	405925.968261	51.917057
3334.444297	405599.874538	51.922061
3333.690616	405321.307457	51.927066
3333.015150	404997.255700	51.932071
3332.206073	404708.855824	51.937076
3331.831619	404368.076708	51.942081
3331.193856	404093.292977	51.947085
3330.045129	403777.614951	51.952090
3329.413799	403433.307993	51.957095
3328.609205	403167.743825	51.962100
3328.025824	402832.624058	51.967105
3327.192755	402565.534310	51.972109
3326.567114	402245.996513	51.977114
3326.059744	401961.260589	51.982119
3325.373323	401658.299619	51.987124
3324.619099	401362.413087	51.992129
3324.333974	401032.362120	51.997133
3323.246835	400757.544654	52.002138
3322.918735	400432.197046	52.007143
3322.222178	400139.594872	52.012148
3321.434164	399842.708495	52.017153
3320.474110	399547.829453	52.022157
3320.052600	399229.348260	52.027162
3319.236443	398950.583386	52.032167
3318.818032	398611.682579	52.037172
3317.991932	398328.490718	52.042177
3317.064820	398046.685198	52.047181
3316.930756	397719.398931	52.052186
3315.632407	397455.086657	52.057191
3315.105590	397121.246865	52.062196
3314.343943	396859.387259	52.067201
3314.052033	396546.605453	52.072205
3313.093976	396252.586720	52.077210
3312.668068	395952.786424	52.082215
3311.685373	395658.359651	52.087220
3311.250992	395357.563916	52.092225
3310.634163	395051.277357	52.097229
3309.592679	394781.767887	52.102234
3308.999324	394483.354052	52.107239
3308.958755	394167.993602	52.112244
3308.125816	393880.189107	52.117249
3307.333306	393565.120043	52.122253
3306.727639	393270.282597	52.127258
3305.935593	392970.259874	52.132263
3305.226957	392670.984143	52.137268
3304.214537	392393.391448	52.142273
3303.760344	392082.399876	52.147277
3303.379809	391781.259366	52.152282
3302.386699	391511.564260	52.157287
3302.175731	391201.441778	52.162292
3300.788138	390911.539235	52.167297
3300.432754	390613.842862	52.172301
3299.606226	390315.175983	52.177306
3299.209795	390015.497743	52.182311
3298.506991	389718.789658	52.187316
3297.495475	389422.941641	52.192321
3297.359530	389135.089773	52.197325
3296.164996	388837.180750	52.202330
3295.748763	388543.621628	52.207335
3295.312258	388248.690162	52.212340
3294.060315	387961.666606	52.217345
3293.357698	387666.619924	52.222349
3292.946008	387372.491161	52.227354
3292.380056	387083.063513	52.232359
3291.592271	386792.498885	52.237364
3290.708818	386507.211142	52.242369
3290.477463	386205.390002	52.247373
3290.095454	385915.390029	52.252378
3288.827763	385629.673095	52.257383
3288.383122	385332.023790	52.262388
3287.744712	385042.947640	52.267393
3287.100597	384746.164436	52.272397
3286.424565	384460.624697	52.277402
3285.694260	384164.206557	52.282407
3284.888936	383871.358427	52.287412
3284.198571	383581.134789	52.292417
3283.740534	383284.946426	52.297421
3282.971803	382985.752983	52.302426
3282.186480	382704.159302	52.307431
3281.642090	382413.623889	52.312436
3280.920379	382128.150084	52.317441
3280.333503	381823.984737	52.322445
3279.708514	381562.475086	52.327450
3278.633450	381249.328075	52.332455
3278.442138	380970.578033	52.337460
3277.581942	380675.399611	52.342465
3276.711795	380386.502798	52.347469
3276.561622	380093.242397	52.352474
3275.306367	379795.856132	52.357479
3274.996077	379504.880339	52.362484
3274.255129	379226.611743	52.367489
3273.547299	378940.323841	52.372493
3273.353222	378656.979417	52.377498
3272.307505	378351.689561	52.382503
3271.399613	378069.725637	52.387508
3270.496380	377783.231376	52.392513
3270.037252	377496.359579	52.397517
3269.293440	377209.276398	52.402522
3268.609039	376916.483984	52.407527
3268.320302	376639.448497	52.412532
3267.548856	376359.028051	52.417537
3266.793955	376065.502958	52.422541
3266.075089	375787.842891	52.427546
3265.170431	375485.968454	52.432551
3264.808456	375196.623005	52.437556
3263.847501	374928.483627	52.442561
3263.610186	374636.468985	52.447565
3262.878617	374353.560999	52.452570
3262.206506	374062.348783	52.457575
3261.712102	373781.816017	52.462580
3260.961989	373505.010415	52.467585
3260.292404	373199.927698	52.472589
3259.585911	372914.919981	52.477594
3258.850280	372622.486697	52.482599
3258.209983	372339.728699	52.487604
3257.232675	372053.689541	52.492609
3256.938222	371760.849790	52.497613
3256.153163	371488.615610	52.502618
3255.454388	371202.653863	52.507623
3254.913365	370899.722065	52.512628
3254.523107	370619.965916	52.517633
3253.703322	370323.637771	52.522637
3252.952882	370038.617747	52.527642
3252.158852	369751.720115	52.532647
3251.792897	369462.208764	52.537652
3250.766025	369169.594443	52.542657
3250.360209	368893.315063	52.547661
3249.986922	368611.151796	52.552666
3249.283526	368313.392274	52.557671
3248.252428	368032.881305	52.562676
3247.428480	367733.508663	52.567681
3247.082972	367452.045974	52.572685
3246.393290	367156.184672	52.577690
3245.473701	366855.829002	52.582695
3245.159899	366575.398919	52.587700
3244.130193	366299.761826	52.592705
3243.885789	366002.245017	52.597709
3243.023082	365713.856404	52.602714
3242.072147	365424.563953	52.607719
3241.422207	365140.870513	52.612724
3240.938238	364851.627773	52.617729
3240.640216	364558.638990	52.622733
3239.431574	364283.119767	52.627738
3238.793437	363994.150461	52.632743
3238.297734	363704.469820	52.637748
3237.607996	363422.629524	52.642753
3236.758382	363130.838516	52.647757
3236.281594	362845.220682	52.652762
3235.378326	362562.416629	52.657767
3234.741890	362268.398263	52.662772
3234.247437	361988.808512	52.667777
3233.568655	361692.299628	52.672781
3232.861415	361420.679159	52.677786
3232.062823	361135.916162	52.682791
3231.588984	360840.209264	52.687796
3230.903115	360566.417664	52.692801
3230.085273	360276.258056	52.697805
3229.853062	359986.131291	52.702810
3229.168407	359683.478361	52.707815
3228.485705	359413.089563	52.712820
3227.590819	359115.810155	52.717825
3226.920675	358828.926628	52.722829
3226.414706	358551.761682	52.727834
3225.330956	358263.973308	52.732839
3225.084884	357972.233634	52.737844
3223.788432	357697.351984	52.742849
3223.451317	357407.735547	52.747853
3222.906694	357127.540497	52.752858
3222.033804	356838.514486	52.757863
3221.694941	356555.331736	52.762868
3220.646436	356273.328492	52.767873
3220.056333	355992.269094	52.772877
3219.545977	355709.235993	52.777882
3218.722131	355433.351092	52.782887
3218.319656	355136.530038	52.787892
3217.329637	354855.883951	52.792897
3217.037709	354572.046560	52.797901
3216.039351	354289.591835	52.802906
3215.289369	354013.764010	52.807911
3214.637600	353726.212429	52.812916
3213.841788	353448.785557	52.817921
3213.418425	353167.302686	52.822925
3212.902072	352884.611431	52.827930
3211.793983	352611.912342	52.832935
3211.513018	352324.701661	52.837940
3210.610096	352046.749936	52.842945
3209.938158	351762.143116	52.847949
3209.398441	351487.846795	52.852954
3208.975042	351197.649450	52.857959
3208.519454	350912.214946	52.862964
3207.501155	350634.325100	52.867969
3207.112363	350361.500814	52.872973
3206.564998	350061.721970	52.877978
3205.506363	349782.103498	52.882983
3205.116378	349493.495255	52.887988
3204.222400	349218.429148	52.892993
3203.639576	348925.878013	52.897997
3203.005565	348651.786050	52.903002
3202.294403	348354.390924	52.908007
3201.850368	348068.481781	52.913012
3200.771490	347796.975798	52.918017
3200.658239	347491.489526	52.923021
3199.693099	347205.480312	52.928026
3198.733104	346929.293573	52.933031
3198.287149	346639.406949	52.938036
3197.692198	346360.258108	52.943041
3196.837639	346068.320674	52.948045
3196.361753	345792.993671	52.953050
3195.627038	345503.070693	52.958055
3195.142565	345216.873791	52.963060
3194.156425	344945.161554	52.968065
3193.371077	344652.137066	52.973069
3192.747460	344373.721451	52.978074
3191.939852	344099.355356	52.983079
3191.587375	343807.454556	52.988084
3190.732370	343537.649653	52.993089
3190.355146	343254.964475	52.998093
3189.524951	342979.018684	53.003098
3188.897079	342678.170620	53.008103
3188.423364	342405.907638	53.013108
3187.353291	342118.134073	53.018113
3186.961261	341835.902854	53.023117
3186.744277	341547.457104	53.028122
3185.175552	341269.049534	53.033127
3184.875707	340984.203446	53.038132
3184.451587	340711.008788	53.043137
3183.646908	340420.996233	53.048141
3182.882898	340143.550933	53.053146
3182.306180	339857.674434	53.058151
3181.897467	339567.442598	53.063156
3180.932451	339295.982054	53.068161
3180.259613	339008.665991	53.073165
3179.953077	338721.417975	53.078170
3179.119050	338433.182989	53.083175
3178.427085	338142.811379	53.088180
3177.351268	337857.615954	53.093185
3176.841411	337579.864873	53.098189
3176.180428	337300.405487	53.103194
3175.599839	337025.488959	53.108199
3175.341966	336726.769013	53.113204
3174.367680	336446.821032	53.118209
3173.876853	336154.092324	53.123213
3173.334892	335880.386938	53.128218
3172.554403	335592.207554	53.133223
3171.960996	335305.321137	53.138228
3171.052644	335009.751439	53.143233
3169.978897	334737.882196	53.148237
3169.570894	334437.241198	53.153242
3168.859560	334171.294952	53.158247
3168.497918	333886.529904	53.163252
3167.500752	333613.065776	53.168257
3166.891960	333316.855980	53.173261
3166.201476	333040.718934	53.178266
3165.452705	332749.824231	53.183271
3165.106172	332478.645878	53.188276
3164.434162	332195.908933	53.193281
3163.668014	331909.366992	53.198285
3163.155384	331623.369359	53.203290
3162.316229	331351.297314	53.208295
3162.072795	331058.431930	53.213300
3161.116903	330779.095004	53.218305
3159.906717	330495.392845	53.223309
3159.833637	330214.055600	53.228314
3159.017855	329926.724595	53.233319
3158.370108	329643.744920	53.238324
3157.575356	329365.421072	53.243329
3156.956925	329084.547814	53.248333
3156.195576	328807.795145	53.253338
3155.596340	328530.532095	53.258343
3155.263531	328241.768973	53.263348
3154.405195	327956.754166	53.268353
3153.659934	327675.768573	53.273357
3153.195052	327391.045896	53.278362
3152.146118	327105.752648	53.283367
3151.652931	326831.878491	53.288372
3151.089814	326555.239281	53.293377
3150.422191	326269.780877	53.298381
3149.923295	325987.604641	53.303386
3148.922042	325705.532378	53.308391
3148.512890	325411.195223	53.313396
3147.713007	325136.370910	53.318401
3146.986605	324853.284726	53.323405
3146.612463	324564.362196	53.328410
3145.744961	324286.439539	53.333415
3145.309489	324006.869011	53.338420
3144.537358	323724.601019	53.343425
3143.851567	323427.780012	53.348429
3143.044448	323158.322737	53.353434
3141.943383	322874.881851	53.358439
3141.762411	322589.919521	53.363444
3141.079698	322304.806502	53.368449
3140.213145	322038.716107	53.373453
3139.861760	321737.355157	53.378458
3138.658305	321468.973876	53.383463
3138.145650	321178.839795	53.388468
3137.456367	320922.571808	53.393473
3136.875908	320640.925593	53.398477
3136.304085	320354.999489	53.403482
3135.211450	320088.429863	53.408487
3135.074278	319794.947327	53.413492
3134.465210	319522.112194	53.418497
3133.632713	319250.381047	53.423501
3133.129797	318964.388835	53.428506
3132.019060	318688.855249	53.433511
3131.839195	318409.175913	53.438516
3130.886629	318137.180492	53.443521
3130.425018	317838.268729	53.448525
3129.745898	317564.802509	53.453530
3128.786405	317296.421573	53.458535
3128.441846	317005.535063	53.463540
3127.636249	316725.797141	53.468545
3126.785560	316447.160491	53.473549
3126.297541	316180.127879	53.478554
3125.490476	315890.075221	53.483559
3125.204006	315611.728939	53.488564
3124.362622	315335.990605	53.493569
3123.711457	315044.739567	53.498573
3123.421410	314776.220552	53.503578
3122.211692	314501.913335	53.508583
3122.005213	314207.941376	53.513588
3121.185465	313935.277057	53.518593
3120.376696	313654.156281	53.523597
3119.648197	313372.054440	53.528602
3119.231877	313092.576192	53.533607
3118.363210	312807.362994	53.538612
3117.696695	312531.895320	53.543617
3117.319116	312254.675135	53.548621
3116.235793	311966.769077	53.553626
3115.374045	311701.897954	53.558631
3114.668654	311415.000193	53.563636
3114.146286	311152.365890	53.568641
3113.643993	310868.745014	53.573645
3113.202965	310588.424154	53.578650
3112.645150	310313.545086	53.583655
3112.041896	310026.474957	53.588660
3111.145303	309740.952985	53.593665
3110.656356	309462.266804	53.598669
3109.944561	309176.332281	53.603674
3108.999982	308900.721784	53.608679
3108.518170	308617.525250	53.613684
3107.651553	308341.290012	53.618689
3106.922052	308062.740603	53.623693
3106.367670	307785.232408	53.628698
3105.450411	307505.973004	53.633703
3105.429418	307235.102038	53.638708
3104.310371	306973.877399	53.643713
3103.618709	306673.215060	53.648717
3103.130577	306401.525012	53.653722
3102.050532	306119.563615	53.658727
3101.727087	305842.727802	53.663732
3101.001368	305571.710323	53.668737
3100.092880	305291.171601	53.673741
3099.701488	305024.327441	53.678746
3099.132307	304741.671191	53.683751
3098.582277	304460.157307	53.688756
3097.546627	304199.576282	53.693761
3096.974703	303917.326286	53.698765
3096.244003	303636.323239	53.703770
3095.418067	303375.249160	53.708775
3094.948481	303078.669451	53.713780
3094.432769	302818.691275	53.718785
3093.431700	302540.326496	53.723789
3092.991144	302261.337712	53.728794
3092.191952	301989.306539	53.733799
3091.901204	301700.055604	53.738804
3091.319503	301438.328376	53.743809
3090.839550	301156.236970	53.748813
3090.429827	300867.614549	53.753818
3089.233724	300579.549002	53.758823
3088.917928	300305.655819	53.763828
3088.145308	300026.079042	53.768833
3087.375022	299725.389613	53.773837
3086.956700	299445.424743	53.778842
3086.087430	299160.310116	53.783847
3085.345407	298883.400641	53.788852
3084.607538	298598.951912	53.793857
3083.855219	298323.214669	53.798861
3083.211993	298037.960606	53.803866
3082.501026	297764.278791	53.808871
3081.913559	297483.115218	53.813876
3081.302551	297196.173950	53.818881
3080.789493	296917.850065	53.823885
3080.055553	296645.087085	53.828890
3079.293156	296356.411308	53.833895
3078.969939	296073.726778	53.838900
3078.129102	295799.655269	53.843905
3077.528693	295511.767595	53.848909
3076.843690	295219.538016	53.853914
3075.914507	294956.252009	53.858919
3075.351621	294661.150002	53.863924
3074.683460	294388.017084	53.868929
3074.040981	294104.871095	53.873933
3073.340670	293827.082050	53.878938
3072.330721	293548.679519	53.883943
3071.912030	293254.316856	53.888948
3071.209482	292989.362748	53.893953
3070.491811	292706.507085	53.898957
3069.974328	292428.076226	53.903962
3069.265021	292136.330409	53.908967
3068.646148	291854.527769	53.913972
3068.213632	291582.398484	53.918977
3067.583192	291284.221371	53.923981
3067.008271	291006.180065	53.928986
3065.790750	290730.888818	53.933991
3065.398851	290433.666249	53.938996
3065.027186	290161.678703	53.944001
3063.958294	289887.305409	53.949005
3063.432290	289598.609432	53.954010
3062.677125	289310.484267	53.959015
3061.997889	289044.223693	53.964020
3061.233552	288768.756990	53.969025
3060.518808	288480.955738	53.974029
3059.867626	288201.726857	53.979034
3059.279613	287936.062150	53.984039
3058.722393	287648.235240	53.989044
3057.992640	287366.878797	53.994049
3057.166949	287101.531216	53.999053
3056.717579	286811.700052	54.004058
3055.996006	286534.925911	54.009063
3055.405045	286246.135444	54.014068
3054.757142	285975.181426	54.019073
3054.222192	285697.613114	54.024077
3053.584152	285400.425024	54.029082
3052.644000	285128.345177	54.034087
3051.957226	284847.871508	54.039092
3051.343663	284564.482709	54.044097
3050.472441	284291.601937	54.049101
3049.964434	284020.344421	54.054106
3049.131003	283744.222904	54.059111
3048.670465	283455.053431	54.064116
3047.903263	283184.091184	54.069121
3047.282624	282905.184986	54.074125
3046.695285	282614.761734	54.079130
3045.829878	282348.831884	54.084135
3044.991978	282077.651104	54.089140
3044.715818	281796.728820	54.094145
3044.069861	281529.847045	54.099149
3043.513096	281252.152493	54.104154
3042.598200	280977.112293	54.109159
3041.984881	280694.078148	54.114164
3041.175373	280416.346904	54.119169
3040.555436	280140.215541	54.124173
3039.982434	279865.808516	54.129178
3039.006111	279593.477255	54.134183
3038.521178	279306.194628	54.139188
3038.023426	279043.363585	54.144193
3037.220663	278760.486227	54.149197
3036.569047	278490.955781	54.154202
3035.986335	278209.953612	54.159207
3035.557928	277933.740497	54.164212
3034.708567	277671.270494	54.169217
3033.918821	277385.665732	54.174221
3033.847928	277102.061029	54.179226
3033.061934	276822.084130	54.184231
3032.363563	276544.334561	54.189236
3031.677087	276251.709555	54.194241
3030.808732	275978.520244	54.199245
3030.131023	275690.834706	54.204250
3029.404925	275429.389274	54.209255
3028.898759	275139.206160	54.214260
3028.106995	274852.964930	54.219265
3027.642350	274583.379202	54.224269
3027.152854	274294.950825	54.229274
3025.875803	274027.709494	54.234279
3025.467704	273735.244294	54.239284
3025.155723	273462.883939	54.244289
3024.329571	273186.733823	54.249293
3023.821132	272900.040499	54.254298
3022.883474	272611.428644	54.259303
3022.470786	272324.058109	54.264308
3021.849273	272029.793311	54.269313
3020.818499	271761.138121	54.274317
3020.534473	271455.868677	54.279322
3019.791025	271191.319501	54.284327
3018.825296	270904.495345	54.289332
3018.487738	270617.571853	54.294337
3017.786215	270334.093362	54.299341
3017.212754	270051.817186	54.304346
3016.277678	269766.924195	54.309351
3015.832447	269489.365049	54.314356
3015.532032	269191.383027	54.319361
3014.308919	268921.103847	54.324365
3013.948409	268630.695682	54.329370
3013.061125	268346.254211	54.334375
3012.298603	268059.220850	54.339380
3011.557735	267768.262116	54.344385
3010.659110	267495.385458	54.349389
3010.397718	267209.241040	54.354394
3009.742241	266933.295498	54.359399
3009.292928	266649.422367	54.364404
3008.392164	266364.754965	54.369409
3007.466251	266092.469227	54.374413
3007.102774	265798.446765	54.379418
3006.311934	265533.678564	54.384423
3005.461575	265249.258631	54.389428
3005.192756	264970.629963	54.394433
3004.496841	264688.223442	54.399437
3004.067468	264398.032677	54.404442
3003.051238	264126.450258	54.409447
3002.418326	263828.320707	54.414452
3001.828098	263557.791889	54.419457
3000.718204	263276.267017	54.424461
3000.856260	262990.011552	54.429466
3000.040456	262699.756082	54.434471
2999.116431	262423.474387	54.439476
2998.656985	262128.680704	54.444481
2998.039082	261844.889011	54.449485
2997.581814	261558.729131	54.454490
2996.515126	261276.460702	54.459495
2995.985709	260980.380411	54.464500
2995.157104	260716.488013	54.469505
2994.520161	260424.551110	54.474509
2994.156767	260119.200722	54.479514
2993.516783	259832.511289	54.484519
2992.630413	259542.575866	54.489524
2991.905007	259255.416725	54.494529
2991.455237	258982.425154	54.499533
2990.840842	258688.372877	54.504538
2990.172750	258402.886526	54.509543
2989.441048	258115.882548	54.514548
2988.725825	257821.490776	54.519553
2988.175288	257543.678028	54.524557
2987.678134	257243.980747	54.529562
2986.743360	256965.338195	54.534567
2986.178070	256666.594782	54.539572
2985.623224	256385.295177	54.544577
2984.888183	256095.874976	54.549581
2984.098135	255801.319525	54.554586
2983.489564	255518.603441	54.559591
2983.074609	255213.013140	54.564596
2982.495774	254938.595434	54.569601
2981.292845	254640.847277	54.574605
2980.974852	254341.482400	54.579610
2980.395903	254064.748462	54.584615
2979.439416	253769.534813	54.589620
2978.635699	253474.424783	54.594625
2978.107578	253197.887827	54.599629
2977.479776	252902.954609	54.604634
2976.545480	252618.715489	54.609639
2975.979420	252325.632527	54.614644
2975.619080	252045.912939	54.619649
2974.397052	251766.559424	54.624653
2974.004569	251468.408059	54.629658
2973.307135	251183.013287	54.634663
2972.913153	250907.222752	54.639668
2972.113887	250621.768673	54.644673
2971.654545	250323.910092	54.649677
2970.876871	250039.013886	54.654682
2970.075036	249753.714557	54.659687
2969.517976	249467.765806	54.664692
2968.865569	249175.695328	54.669697
2968.107450	248890.696260	54.674701
2967.430852	248605.175500	54.679706
2966.810211	248318.958841	54.684711
2966.080998	248042.895386	54.689716
2965.498046	247745.392437	54.694721
2964.596122	247465.613922	54.699725
2964.111577	247175.889126	54.704730
2963.588911	246889.965355	54.709735
2962.677281	246597.941036	54.714740
2962.220254	246314.223563	54.719745
2961.236881	246029.902430	54.724749
2960.667985	245745.032421	54.729754
2960.148348	245461.453952	54.734759
2959.454252	245169.907543	54.739764
2958.954154	244893.126463	54.744769
2958.442072	244593.097988	54.749773
2957.947901	244308.601197	54.754778
2956.897735	244025.160736	54.759783
2956.289826	243739.842853	54.764788
2955.806433	243432.758675	54.769793
2954.764826	243160.854487	54.774797
2954.175852	242866.317225	54.779802
2953.369041	242586.890402	54.784807
2953.033361	242293.180213	54.789812
2952.568203	242005.551861	54.794817
2951.652240	241726.526265	54.799821
2951.337850	241424.411441	54.804826
2950.053653	241134.928606	54.809831
2949.774463	240847.248137	54.814836
2948.952631	240562.404459	54.819841
2948.337728	240273.963695	54.824845
2947.817712	239981.663508	54.829850
2946.977021	239690.917237	54.834855
2946.498834	239393.595468	54.839860
2945.754963	239108.615758	54.844865
2944.921512	238819.474844	54.849869
2944.523205	238522.219147	54.854874
2943.655987	238240.342359	54.859879
2942.679055	237950.309752	54.864884
2942.364351	237668.805323	54.869889
2941.500436	237372.543200	54.874893
2941.047260	237091.953450	54.879898
2940.240802	236800.241837	54.884903
2939.758280	236509.549219	54.889908
2939.395822	236234.549389	54.894913
2938.168903	235940.691435	54.899917
2938.000117	235647.023276	54.904922
2937.158225	235361.992742	54.909927
2936.488383	235070.977378	54.914932
2936.022729	234771.069353	54.919937
2935.357099	234490.622218	54.924941
2934.579977	234185.901831	54.929946
2933.770060	233904.537080	54.934951
2933.210221	233612.490075	54.939956
2932.572345	233318.877615	54.944961
2931.658635	233030.453190	54.949965
2931.358017	232731.441966	54.954970
2930.373046	232450.643903	54.959975
2929.721152	232159.481643	54.964980
2929.079191	231858.923101	54.969985
2928.440582	231575.246500	54.974989
2927.547614	231288.071797	54.979994
2926.936749	231005.029117	54.984999
2926.325879	230717.607842	54.990004
2925.693056	230421.432035	54.995009
2924.841860	230146.272380	55.000013
2924.700067	229857.557407	55.005018
2923.686892	229564.398233	55.010023
2923.090985	229278.175916	55.015028
2922.657091	228990.477570	55.020033
2921.763035	228697.506123	55.025037
2921.383103	228402.697425	55.030042
2920.370251	228120.389607	55.035047
2919.958254	227828.388701	55.040052
2919.527987	227528.320510	55.045057
2918.446937	227241.494325	55.050061
2918.167353	226950.213853	55.055066
2917.315212	226665.301157	55.060071
2916.472312	226359.497408	55.065076
2916.175509	226068.604663	55.070081
2915.446913	225779.041619	55.075085
2914.882887	225485.367132	55.080090
2913.830123	225192.764052	55.085095
2913.033764	224904.296927	55.090100
2912.423064	224617.392705	55.095105
2911.414057	224328.146601	55.100109
2911.121433	224039.106368	55.105114
2910.641359	223750.606074	55.110119
2909.948351	223461.122164	55.115124
2909.168456	223173.473458	55.120129
2908.367029	222889.609990	55.125133
2907.981238	222586.217910	55.130138
2907.166952	222306.801322	55.135143
2906.434891	222020.715110	55.140148
2905.925244	221729.401064	55.145153
2905.145640	221439.480225	55.150157
2904.791489	221156.532573	55.155162
2904.232824	220857.350083	55.160167
2903.017616	220566.470520	55.165172
2902.477919	220281.837104	55.170177
2901.997258	219994.929618	55.175181
2901.611675	219700.052393	55.180186
2900.764020	219411.703257	55.185191
2900.034645	219120.370638	55.190196
2899.119109	218829.539654	55.195201
2898.213141	218538.020965	55.200205
2897.899254	218246.791583	55.205210
2897.363676	217963.490471	55.210215
2896.817710	217672.732986	55.215220
2896.247318	217375.094250	55.220225
2895.639308	217094.952143	55.225229
2894.778077	216785.867848	55.230234
2894.057545	216492.495345	55.235239
2893.761220	216207.292362	55.240244
2893.155795	215911.345653	55.245249
2892.373923	215610.604049	55.250253
2891.953147	215316.450872	55.255258
2890.887996	215019.791685	55.260263
2890.306645	214728.784971	55.265268
2889.690960	214428.353269	55.270273
2889.105823	214137.451561	55.275277
2888.447147	213838.213067	55.280282
2887.452655	213546.793287	55.285287
2886.736130	213252.454234	55.290292
2886.327206	212952.301995	55.295297
2885.600996	212663.872948	55.300301
2884.897272	212367.092106	55.305306
2884.124707	212078.062079	55.310311
2883.645368	211780.535655	55.315316
2882.981848	211482.428854	55.320321
2882.161751	211200.232408	55.325325
2881.525872	210898.509313	55.330330
2881.033874	210610.154288	55.335335
2880.346695	210309.676723	55.340340
2879.479592	210018.481957	55.345345
2878.385015	209733.382821	55.350349
2877.983515	209426.436959	55.355354
2877.586161	209145.188331	55.360359
2876.796648	208854.343142	55.365364
2876.253287	208561.093110	55.370369
2875.688497	208268.967872	55.375373
2875.157386	207965.944376	55.380378
2873.956663	207680.617111	55.385383
2873.312660	207394.426702	55.390388
2873.139822	207088.398266	55.395393
2872.095470	206806.932104	55.400397
2871.684921	206511.240256	55.405402
2871.009207	206209.801258	55.410407
2870.509947	205913.108335	55.415412
2869.695990	205626.164365	55.420417
2868.860910	205332.365594	55.425421
2868.559926	205029.931597	55.430426
2867.689607	204739.386652	55.435431
2866.938967	204440.552154	55.440436
2866.444728	204146.947258	55.445441
2865.545031	203862.074581	55.450445
2865.186210	203557.646797	55.455450
2864.340450	203271.941354	55.460455
2863.803069	202966.616041	55.465460
2862.890479	202676.241072	55.470465
2862.607106	202384.151790	55.475469
2861.872318	202083.303876	55.480474
2860.621618	201788.685794	55.485479
2860.291496	201504.752978	55.490484
2859.631966	201201.492820	55.495489
2858.877743	200910.694834	55.500493
2858.252094	200617.549293	55.505498
2857.562561	200330.307275	55.510503
2856.937565	200036.184927	55.515508
2856.304646	199740.283914	55.520513
2855.622592	199456.150318	55.525517
2855.106747	199148.997758	55.530522
2854.734147	198854.867376	55.535527
2853.709226	198566.199116	55.540532
2853.234289	198272.304502	55.545537
2852.499168	197977.091185	55.550541
2851.893908	197680.077508	55.555546
2851.264109	197389.533511	55.560551
2850.408250	197079.202101	55.565556
2849.863361	196785.390555	55.570561
2849.006703	196496.974302	55.575565
2848.624453	196197.452544	55.580570
2847.624287	195904.596110	55.585575
2847.402196	195617.534872	55.590580
2846.700472	195314.417050	55.595585
2846.118089	195024.171580	55.600589
2845.437058	194718.547418	55.605594
2844.632677	194426.202926	55.610599
2843.729028	194128.201045	55.615604
2843.397187	193828.812562	55.620609
2842.702774	193535.348904	55.625613
2842.142038	193236.789106	55.630618
2841.141958	192942.652130	55.635623
2840.388488	192641.543590	55.640628
2839.959118	192341.403436	55.645633
2839.290594	192045.107257	55.650637
2838.668199	191749.123655	55.655642
2838.061168	191444.284141	55.660647
2837.690594	191153.480768	55.665652
2836.649319	190847.874076	55.670657
2835.830763	190555.185937	55.675661
2835.182858	190250.258681	55.680666
2834.455871	189959.239101	55.685671
2833.639848	189669.634894	55.690676
2833.033105	189371.933213	55.695681
2832.591143	189087.171515	55.700685
2832.107852	188774.785039	55.705690
2831.134924	188492.312018	55.710695
2830.827599	188182.815035	55.715700
2830.361215	187886.818057	55.720705
2829.332254	187599.652133	55.725709
2828.726824	187292.485553	55.730714
2828.036461	186999.951942	55.735719
2827.388637	186696.243695	55.740724
2826.727358	186401.648360	55.745729
2826.145033	186104.625307	55.750733
2825.669346	185793.937058	55.755738
2825.083602	185500.226110	55.760743
2824.223272	185195.785533	55.765748
2823.743349	184897.800080	55.770753
2822.838256	184599.158837	55.775757
2822.495697	184296.728637	55.780762
2821.552767	183992.767284	55.785767
2820.735487	183694.588874	55.790772
2820.259117	183392.504049	55.795777
2819.649324	183096.433921	55.800781
2819.149119	182782.221411	55.805786
2818.331610	182479.408204	55.810791
2817.781489	182180.052893	55.815796
2817.157713	181865.090598	55.820801
2816.359944	181568.742584	55.825805
2815.411048	181273.285515	55.830810
2814.745252	180966.871716	55.835815
2814.193528	180668.099527	55.840820
2813.702241	180370.502808	55.845825
2813.037759	180072.770235	55.850829
2812.361138	179763.988140	55.855834
2811.600502	179470.968626	55.860839
2811.136822	179171.671480	55.865844
2810.336762	178872.607811	55.870849
2809.431306	178571.578726	55.875853
2809.023531	178267.801906	55.880858
2808.327142	177962.699326	55.885863
2807.544280	177662.051672	55.890868
2807.033182	177356.936905	55.895873
2806.118300	177056.454464	55.900877
2805.944488	176755.996737	55.905882
2805.060054	176458.897059	55.910887
2804.264922	176159.966610	55.915892
2803.449585	175857.823733	55.920897
2802.853258	175555.940932	55.925901
2802.003263	175259.963753	55.930906
2801.307498	174964.651096	55.935911
2800.843678	174663.148223	55.940916
2800.077968	174363.552275	55.945921
2799.626500	174066.528708	55.950925
2799.089029	173760.096950	55.955930
2798.213827	173460.385202	55.960935
2797.319235	173171.895862	55.965940
2797.046374	172867.425750	55.970945
2796.204426	172573.120449	55.975949
2795.470459	172274.984991	55.980954
2794.897999	171976.495556	55.985959
2794.310262	171676.726363	55.990964
2793.496541	171385.426767	55.995969
2792.825162	171082.712272	56.000973
2792.152053	170783.879093	56.005978
2791.576551	170486.902140	56.010983
2790.563768	170205.295059	56.015988
2790.345563	169831.838557	56.020993
2789.409873	169528.046311	56.025997
2789.127192	169251.035707	56.031002
2788.767055	168934.135310	56.036007
2787.945804	168639.284342	56.041012
2787.550321	168335.225273	56.046017
2786.207416	168042.661473	56.051021
2786.086663	167730.196554	56.056026
2785.460542	167414.126669	56.061031
2784.462192	167116.390981	56.066036
2784.056746	166813.045134	56.071041
2783.179408	166523.051563	56.076045
2782.665347	166198.225875	56.081050
2781.781010	165913.845683	56.086055
2781.260387	165593.336839	56.091060
2780.316311	165303.643104	56.096065
2779.766344	164987.518185	56.101069
2779.176747	164693.856861	56.106074
2778.358187	164395.059215	56.111079
2777.444584	164116.241223	56.116084
2777.078113	163794.617478	56.121089
2776.816936	163521.434993	56.126093
2775.791866	163194.161203	56.131098
2775.362935	162911.435927	56.136103
2774.736601	162578.268678	56.141108
2773.811518	162302.492451	56.146113
2773.225118	161973.354860	56.151117
2772.632250	161695.369301	56.156122
2771.907937	161374.128980	56.161127
2771.349060	161102.283421	56.166132
2771.141933	160779.186633	56.171137
2770.175637	160476.961417	56.176141
2769.528840	160164.835328	56.181146
2768.498421	159865.206325	56.186151
2767.995346	159553.317161	56.191156
2767.460952	159250.678100	56.196161
2766.253796	158946.393851	56.201165
2766.019776	158662.819812	56.206170
2765.193585	158326.279118	56.211175
2764.399563	158058.765856	56.216180
2763.849803	157761.278081	56.221185
2763.124677	157435.116144	56.226189
2762.523911	157161.057795	56.231194
2761.853610	156823.248561	56.236199
2761.068665	156538.266518	56.241204
2760.384961	156250.219957	56.246209
2759.660022	155944.487536	56.251213
2758.945215	155649.090863	56.256218
2758.380188	155353.495076	56.261223
2757.808247	155026.416681	56.266228
2757.216802	154775.243995	56.271233
2756.066078	154454.542257	56.276237
2755.722447	154161.108198	56.281242
2754.889394	153872.686119	56.286247
2754.440109	153583.392238	56.291252
2754.081817	153275.859177	56.296257
2753.318495	152978.256609	56.301261
2752.824936	152672.136035	56.306266
2752.209693	152360.622924	56.311271
2751.508191	152061.442723	56.316276
2750.754790	151773.267797	56.321281
2749.987653	151472.095148	56.326285
2749.466802	151151.617932	56.331290
2748.517263	150869.430304	56.336295
2747.677408	150572.624244	56.341300
2747.428909	150248.465071	56.346305
2746.389382	149971.764632	56.351309
2745.697723	149658.993032	56.356314
2745.092887	149363.101324	56.361319
2744.607964	149067.142503	56.366324
2743.943536	148765.737253	56.371329
2743.187926	148470.983339	56.376333
2742.598691	148175.278044	56.381338
2741.855524	147876.092282	56.386343
2740.658749	147574.719073	56.391348
2740.595774	147269.470953	56.396353
2739.472188	146985.603983	56.401357
2739.413227	146689.307485	56.406362
2738.909447	146396.922083	56.411367
2738.173444	146090.686386	56.416372
2737.298547	145792.011431	56.421377
2736.835264	145505.918300	56.426381
2736.041560	145189.445433	56.431386
2735.138703	144912.500611	56.436391
2734.663649	144603.556882	56.441396
2734.110270	144291.184980	56.446401
2733.345364	144006.258969	56.451405
2732.813523	143691.322883	56.456410
2732.125170	143387.482483	56.461415
2731.626733	143100.845329	56.466420
2730.891613	142801.503619	56.471425
2730.131168	142484.811794	56.476429
2729.373139	142176.991907	56.481434
2728.897326	141894.924066	56.486439
2727.889438	141589.373305	56.491444
2727.549232	141270.289630	56.496449
2726.732706	140996.034779	56.501453
2726.133817	140688.204804	56.506458
2725.569053	140363.740949	56.511463
2724.354100	140095.224127	56.516468
2724.047753	139781.842918	56.521473
2723.078696	139472.635655	56.526477
2722.814086	139184.308791	56.531482
2721.829619	138892.833592	56.536487
2721.643714	138591.706108	56.541492
2721.087503	138283.131871	56.546497
2720.075595	137989.433880	56.551501
2719.640261	137687.440391	56.556506
2718.860148	137388.172531	56.561511
2718.068448	137081.426791	56.566516
2717.622303	136776.420785	56.571521
2716.857995	136485.163197	56.576525
2716.319275	136178.310626	56.581530
2715.821483	135883.955206	56.586535
2714.677357	135588.447520	56.591540
2714.320579	135297.073745	56.596545
2713.619429	134969.642066	56.601549
2712.723741	134685.918279	56.606554
2712.570344	134361.252226	56.611559
2711.578561	134092.920139	56.616564
2711.029894	133763.000973	56.621569
2710.117087	133468.939204	56.626573
2709.805994	133166.604742	56.631578
2708.843942	132872.048831	56.636583
2708.170796	132574.249245	56.641588
2708.048680	132261.059493	56.646593
2706.987419	131965.347425	56.651597
2706.307692	131644.987341	56.656602
2705.578978	131365.677682	56.661607
2704.771670	131047.072040	56.666612
2704.320193	130747.757826	56.671617
2703.574162	130458.400450	56.676621
2702.822835	130148.280594	56.681626
2702.235824	129850.254873	56.686631
2701.493005	129559.814026	56.691636
2700.901670	129245.817820	56.696641
2700.214792	128948.884450	56.701645
2699.587909	128658.714086	56.706650
2698.774078	128362.594557	56.711655
2698.547917	128064.988081	56.716660
2697.702067	127752.293800	56.721665
2696.543674	127464.328444	56.726669
2696.289049	127162.913599	56.731674
2695.772000	126855.981235	56.736679
2694.785067	126564.912192	56.741684
2694.512422	126263.268851	56.746689
2693.519617	125966.721042	56.751693
2692.862724	125667.634242	56.756698
2692.376478	125360.383721	56.761703
2691.544081	125064.950584	56.766708
2691.224858	124752.524830	56.771713
2690.163134	124459.674394	56.776717
2689.388847	124158.222941	56.781722
2688.860357	123861.180299	56.786727
2688.179727	123573.701294	56.791732
2687.729870	123258.304230	56.796737
2686.927204	122979.853777	56.801741
2686.129224	122671.781949	56.806746
2685.616998	122370.156829	56.811751
2684.740918	122069.646677	56.816756
2684.193748	121793.441033	56.821761
2683.419689	121484.211111	56.826765
2682.691704	121194.060963	56.831770
2682.508004	120890.419999	56.836775
2681.460498	120591.820315	56.841780
2680.676265	120298.667199	56.846785
2680.425083	119999.643388	56.851789
2679.826721	119700.900202	56.856794
2679.165537	119403.465396	56.861799
2678.182894	119110.541193	56.866804
2677.924642	118800.962969	56.871809
2677.233970	118508.799144	56.876813
2676.337567	118204.153515	56.881818
2675.827477	117896.257412	56.886823
2675.000029	117609.825645	56.891828
2674.207193	117302.254412	56.896833
2673.681888	117003.035776	56.901837
2672.745114	116722.058314	56.906842
2672.175517	116427.379106	56.911847
2671.339840	116131.558543	56.916852
2671.081105	115826.510131	56.921857
2670.239568	115541.462109	56.926861
2669.333400	115241.074176	56.931866
2669.153406	114930.635488	56.936871
2668.389514	114657.517322	56.941876
2667.720611	114357.514859	56.946881
2667.052447	114055.148546	56.951885
2666.462273	113758.536241	56.956890
2666.036365	113471.503732	56.961895
2665.111804	113182.776524	56.966900
2664.664049	112871.282417	56.971905
2663.497519	112552.436502	56.976909
2663.091170	112273.341227	56.981914
2662.502437	111974.585859	56.986919
2661.659953	111668.563622	56.991924
2660.937699	111373.752199	56.996929
2660.122116	111089.569480	57.001933
2659.796763	110787.905681	57.006938
2659.105561	110491.126344	57.011943
2657.939586	110199.699107	57.016948
2657.710649	109904.027581	57.021953
2657.022111	109619.505440	57.026957
2656.339058	109314.166252	57.031962
2656.008537	109003.463936	57.036967
2655.131776	108718.804471	57.041972
2654.528257	108425.640497	57.046977
2653.810820	108134.883904	57.051981
2653.209931	107836.498236	57.056986
2652.785363	107535.030023	57.061991
2651.733410	107241.786504	57.066996
2651.151934	106932.781199	57.072001
2650.521855	106644.236754	57.077005
2650.035555	106339.335421	57.082010
2649.341470	106040.783785	57.087015
2648.377232	105755.481661	57.092020
2647.844276	105445.580605	57.097025
2647.047971	105146.130083	57.102029
2646.149228	104847.974771	57.107034
2645.734526	104577.293084	57.112039
2645.107591	104279.038417	57.117044
2644.491629	103974.175267	57.122049
2643.751884	103675.419544	57.127053
2643.125562	103390.022574	57.132058
2643.006244	103086.018426	57.137063
2641.782329	102785.695001	57.142068
2641.242898	102486.294631	57.147073
2640.442242	102212.294768	57.152077
2640.296328	101892.914460	57.157082
2639.296392	101602.403173	57.162087
2638.421918	101315.142451	57.167092
2637.927412	100994.630824	57.172097
2637.585247	100709.836882	57.177101
2636.514890	100412.196564	57.182106
2636.023730	100105.404140	57.187111
2635.415445	99817.789985	57.192116
2634.848818	99515.863363	57.197121
2634.115104	99207.465859	57.202125
2633.382179	98908.516617	57.207130
2632.734106	98623.657416	57.212135
2632.138911	98303.731978	57.217140
2631.544205	98006.846621	57.222145
2630.764849	97737.615309	57.227149
2629.946779	97401.926381	57.232154
2629.333815	97136.481176	57.237159
2628.739626	96811.940424	57.242164
2627.800474	96539.622003	57.247169
2626.949673	96222.912026	57.252173
2626.410361	95935.989150	57.257178
2625.847824	95649.853647	57.262183
2625.206317	95339.490058	57.267188
2624.644466	95064.840336	57.272193
2624.033819	94747.770635	57.277197
2623.534441	94461.678332	57.282202
2622.627361	94163.364779	57.287207
2621.897010	93871.292374	57.292212
2621.357213	93570.766181	57.297217
2620.352581	93301.433464	57.302221
2619.896569	92970.312686	57.307226
2619.264572	92704.409380	57.312231
2618.096181	92414.866830	57.317236
2617.681967	92100.504967	57.322241
2617.224346	91845.033940	57.327245
2616.180228	91521.744699	57.332250
2615.599076	91247.652534	57.337255
2615.109992	90957.298690	57.342260
2614.551960	90648.813578	57.347265
2613.675468	90388.106364	57.352269
2613.268479	90077.221447	57.357274
2612.671998	89780.097268	57.362279
2611.777225	89500.827134	57.367284
2611.466587	89205.979599	57.372289
2610.661512	88910.295155	57.377293
2610.233305	88607.188244	57.382298
2609.568313	88318.824761	57.387303
2608.978278	88030.738532	57.392308
2608.126795	87717.206535	57.397313
2607.352250	87432.853463	57.402317
2606.377161	87133.365977	57.407322
2606.040136	86832.875040	57.412327
2604.986051	86549.268963	57.417332
2604.301947	86269.905888	57.422337
2603.599073	85982.086924	57.427341
2603.155178	85677.166548	57.432346
2602.366475	85389.933350	57.437351
2601.883526	85106.667976	57.442356
2601.088204	84807.590334	57.447361
2600.383594	84541.830527	57.452365
2600.110152	84231.357696	57.457370
2599.552538	83953.038223	57.462375
2598.474501	83661.424814	57.467380
2597.910357	83358.616831	57.472385
2597.385772	83062.797851	57.477389
2596.693135	82787.696918	57.482394
2596.033569	82488.763779	57.487399
2595.194971	82202.798791	57.492404
2594.951247	81907.997352	57.497409
2594.132738	81622.880045	57.502413
2593.466067	81310.351633	57.507418
2592.929679	81028.081350	57.512423
2592.214577	80730.158207	57.517428
2591.241112	80440.956046	57.522433
2590.820794	80161.708390	57.527437
2589.911814	79860.501460	57.532442
2589.507756	79562.881700	57.537447
2588.536098	79275.362217	57.542452
2588.173935	78993.700451	57.547457
2587.054678	78694.692100	57.552461
2586.628425	78408.834574	57.557466
2585.905522	78123.433598	57.562471
2585.266146	77837.807924	57.567476
2584.601315	77545.733489	57.572481
2583.607413	77241.961545	57.577485
2583.051496	76979.994439	57.582490
2582.333617	76675.141735	57.587495
2581.398714	76408.958841	57.592500
2581.372281	76108.940832	57.597505
2580.419557	75847.887586	57.602509
2579.992532	75538.241319	57.607514
2579.321390	75275.174086	57.612519
2578.837339	74966.895131	57.617524
2578.231038	74678.134606	57.622529
2577.263315	74401.086343	57.627533
2576.776740	74086.644264	57.632538
2575.885265	73842.915418	57.637543
2575.067412	73518.290697	57.642548
2574.658277	73269.126537	57.647553
2573.705625	72956.790653	57.652557
2572.837777	72709.194916	57.657562
2572.541894	72399.132928	57.662567
2571.473602	72111.344265	57.667572
2571.029060	71850.199262	57.672577
2570.305119	71534.669523	57.677581
2569.962653	71283.948741	57.682586
2569.500199	70974.296517	57.687591
2568.481523	70714.556059	57.692596
2568.102546	70415.996968	57.697601
2567.390915	70121.244893	57.702605
2566.341740	69850.847811	57.707610
2565.946627	69559.246326	57.712615
2564.925312	69287.927853	57.717620
2564.565836	68987.360610	57.722625
2563.780867	68738.116876	57.727629
2563.032755	68430.538845	57.732634
2562.542340	68160.811274	57.737639
2561.633820	67878.081735	57.742644
2561.449920	67581.618682	57.747649
2560.345864	67332.573376	57.752653
2559.738350	67019.586904	57.757658
2559.252179	66774.095513	57.762663
2558.691416	66454.059037	57.767668
2557.802844	66188.677725	57.772673
2556.897388	65904.501025	57.777677
2556.257819	65621.362918	57.782682
2555.734647	65366.941059	57.787687
2554.600341	65076.296752	57.792692
2554.831090	64777.439612	57.797697
2553.956181	64540.802274	57.802701
2553.148231	64232.107059	57.807706
2552.502402	63932.863846	57.812711
2551.438953	63701.842153	57.817716
2551.253756	63387.388487	57.822721
2550.187470	63136.302191	57.827725
2549.563604	62828.195762	57.832730
2548.956418	62579.845820	57.837735
2548.100051	62311.442501	57.842740
2547.937154	61996.353070	57.847745
2547.205680	61769.417718	57.852749
2546.187823	61473.153063	57.857754
2546.160109	61197.058967	57.862759
2545.298150	60915.289293	57.867764
2544.691168	60619.162898	57.872769
2543.764690	60382.031795	57.877773
2543.403373	60068.781914	57.882778
2542.563738	59788.858391	57.887783
2541.434934	59545.119648	57.892788
2541.245985	59259.533202	57.897793
2540.384968	58977.653310	57.902797
2539.400631	58713.851154	57.907802
2539.003559	58421.676440	57.912807
2538.286761	58162.606326	57.917812
2537.837226	57872.417237	57.922817
2536.658975	57633.667797	57.927821
2536.309647	57326.684504	57.932826
2535.648077	57088.983741	57.937831
2534.934675	56793.552297	57.942836
2534.184996	56523.091781	57.947841
2533.593821	56268.142531	57.952845
2532.769883	55988.318281	57.957850
2532.132015	55720.994369	57.962855
2531.574416	55470.199706	57.967860
2530.954591	55184.301548	57.972865
2529.838197	54939.460290	57.977869
2529.311219	54647.916699	57.982874
2528.683842	54398.486373	57.987879
2528.135153	54128.598984	57.992884
2527.323216	53858.792140	57.997889
2526.628289	53606.098853	58.002893
2526.159160	53339.444446	58.007898
2525.187375	53069.965785	58.012903
2524.368319	52824.109194	58.017908
2524.087355	52533.639526	58.022913
2523.444798	52296.014030	58.027917
2523.008410	52014.781502	58.032922
2522.347921	51755.584516	58.037927
2521.380375	51502.242506	58.042932
2520.904190	51221.322935	58.047937
2520.005612	50977.256935	58.052941
2519.333894	50708.231134	58.057946
2518.378331	50423.651026	58.062951
2517.600434	50194.895182	58.067956
2517.384921	49908.424825	58.072961
2516.358711	49681.540327	58.077965
2515.698475	49403.282112	58.082970
2515.166429	49155.174746	58.087975
2514.363529	48905.592175	58.092980
2513.721457	48637.959521	58.097985
2513.178306	48404.820856	58.102989
2512.600452	48143.021852	58.107994
2511.953776	47873.633199	58.112999
2510.979440	47636.356421	58.118004
2510.659754	47379.016386	58.123009
2510.059118	47124.261457	58.128013
2509.163486	46872.131712	58.133018
2508.702710	46587.344960	58.138023
2507.742490	46359.350777	58.143028
2507.064872	46100.023941	58.148033
2506.244125	45841.963480	58.153037
2505.720111	45599.895331	58.158042
2504.978956	45344.369345	58.163047
2503.869564	45104.349139	58.168052
2503.638788	44847.949333	58.173057
2502.788404	44607.341436	58.178061
2501.757887	44357.208023	58.183066
2501.706487	44117.125408	58.188071
2500.924461	43864.205103	58.193076
2500.023466	43610.953150	58.198081
2499.395641	43372.502855	58.203085
2498.427744	43122.529113	58.208090
2498.110233	42895.091888	58.213095
2496.958621	42657.287904	58.218100
2496.263124	42400.172589	58.223105
2495.438545	42188.048145	58.228109
2494.762171	41951.965198	58.233114
2494.258875	41712.974194	58.238119
2493.477450	41496.101934	58.243124
2492.772708	41271.153885	58.248129
2492.023880	41044.274308	58.253133
2491.460561	40802.521358	58.258138
2490.732342	40580.673745	58.263143
2489.713311	40372.058553	58.268148
2489.337291	40135.845491	58.273153
2488.450890	39898.753848	58.278157
2487.255764	39709.543801	58.283162
2486.309215	39502.375840	58.288167
2485.244870	39280.002453	58.293172
2484.440135	39089.801552	58.298177
2483.534167	38883.042558	58.303181
2482.899997	38710.599708	58.308186
2482.271851	38515.914691	58.313191
2480.421738	38345.128971	58.318196
2479.724462	38157.113997	58.323201
2478.979642	38002.403272	58.328205
2477.921092	37839.457660	58.333210
2477.460787	37656.672841	58.338215
2476.296247	37519.384277	58.343220
2475.230575	37372.263684	58.348225
2474.648743	37215.560090	58.353229
2474.044937	37072.788366	58.358234
2473.488885	36936.388073	58.363239
2472.432599	36799.450180	58.368244
2471.638990	36643.139549	58.373249
2471.181804	36518.149903	58.378253
2470.028348	36396.646090	58.383258
2469.899196	36250.083864	58.388263
2468.600617	36109.828180	58.393268
2468.084433	35984.908760	58.398273
2467.164575	35861.244404	58.403277
2466.527924	35735.811728	58.408282
2465.979813	35618.048732	58.413287
2465.193044	35479.555299	58.418292
2464.658415	35409.470055	58.423297
2464.094804	35237.739103	58.428301
2463.042667	35139.620728	58.433306
2462.761093	35049.098042	58.438311
2462.113179	34893.287972	58.443316
2461.357875	34793.370301	58.448321
2460.738124	34699.854508	58.453325
2459.992029	34559.133894	58.458330
2460.052231	34446.799867	58.463335
2458.723363	34313.239626	58.468340
2458.212726	34231.211103	58.473345
2457.592285	34088.789879	58.478349
2457.172016	33987.289411	58.483354
2456.668202	33860.574451	58.488359
2455.955176	33749.126293	58.493364
2455.253503	33641.096865	58.498369
2454.654491	33505.587927	58.503373
2453.883829	33403.399109	58.508378
2453.390393	33283.471072	58.513383
2452.583487	33161.250080	58.518388
2451.823115	33053.485054	58.523393
2451.393936	32914.919942	58.528397
2450.315544	32809.275464	58.533402
2449.904738	32695.977118	58.538407
2449.226932	32574.327838	58.543412
2448.411017	32463.301287	58.548417
2447.828130	32356.509771	58.553421
2447.156245	32254.641077	58.558426
2446.717787	32127.665140	58.563431
2445.925944	32020.167839	58.568436
2445.325696	31906.595245	58.573441
2445.133992	31784.290067	58.578445
2444.091508	31672.418322	58.583450
2443.502024	31569.409439	58.588455
2442.781129	31460.635721	58.593460
2442.262626	31343.157536	58.598465
2441.366194	31231.772844	58.603469
2440.466036	31119.796975	58.608474
2440.389271	31000.748557	58.613479
2439.293338	30881.853124	58.618484
2438.879188	30766.813165	58.623489
2438.311307	30666.089674	58.628493
2437.677159	30549.599324	58.633498
2436.848154	30431.668143	58.638503
2436.108503	30329.512462	58.643508
2435.377971	30222.290564	58.648513
2434.812041	30118.636116	58.653517
2433.910915	29986.341882	58.658522
2433.581359	29888.688423	58.663527
2432.693171	29793.015313	58.668532
2431.982768	29675.938170	58.673537
2431.687331	29566.570828	58.678541
2430.866195	29451.144910	58.683546
2430.077205	29349.477162	58.688551
2429.750153	29249.920201	58.693556
2428.932433	29139.331980	58.698561
2428.079007	29041.005171	58.703565
2427.435411	28921.426677	58.708570
2427.086395	28805.197430	58.713575
2426.480267	28711.298035	58.718580
2425.723445	28589.664038	58.723585
2424.984029	28489.753729	58.728589
2424.025165	28391.967330	58.733594
2423.897248	28278.629424	58.738599
2423.066213	28165.792429	58.743604
2422.177939	28061.624005	58.748609
2421.384116	27971.112510	58.753613
2420.759264	27849.418911	58.758618
2420.289415	27733.319191	58.763623
2419.691383	27649.062644	58.768628
2418.981026	27546.398505	58.773633
2418.337772	27407.642303	58.778637
2417.505851	27345.541889	58.783642
2416.582750	27223.009352	58.788647
2415.671974	27126.776606	58.793652
2415.342064	27035.986692	58.798657
2414.675000	26937.707880	58.803661
2413.768837	26832.009272	58.808666
2413.453851	26732.980044	58.813671
2412.631261	26651.794066	58.818676
2412.067090	26533.776568	58.823681
2411.286242	26443.064662	58.828685
2410.593789	26343.322100	58.833690
2409.826750	26249.186896	58.838695
2409.421398	26149.084094	58.843700
2408.492060	26049.833469	58.848705
2407.762447	25968.949744	58.853709
2407.291017	25866.567235	58.858714
2406.808432	25764.851347	58.863719
2406.003489	25679.474590	58.868724
2405.238269	25572.635713	58.873729
2404.676134	25504.665664	58.878733
2404.116246	25393.955610	58.883738
2403.754571	25288.902656	58.888743
2402.776756	25199.473665	58.893748
2402.334749	25097.499703	58.898753
2401.903136	24995.391277	58.903757
2400.475977	24891.196966	58.908762
2400.041838	24804.165301	58.913767
2399.607615	24712.269449	58.918772
2399.082103	24608.206457	58.923777
2398.158069	24520.393238	58.928781
2397.500682	24432.574544	58.933786
2396.738974	24334.231943	58.938791
2395.920687	24232.332653	58.943796
2395.476639	24139.736458	58.948801
2394.760467	24051.718339	58.953805
2394.314036	23964.611078	58.958810
2393.794647	23853.804992	58.963815
2392.834435	23757.804079	58.968820
2392.173502	23673.527079	58.973825
2391.371788	23585.900197	58.978829
2390.673626	23494.981868	58.983834
2390.425543	23383.346377	58.988839
2389.411546	23303.317238	58.993844
2388.988577	23223.149766	58.998849
2388.374253	23115.114224	59.003853
2387.669268	23024.568435	59.008858
2386.821095	22935.577757	59.013863
2386.125751	22837.305754	59.018868
2385.402217	22742.419204	59.023873
2385.177731	22649.992701	59.028877
2384.032064	22562.245202	59.033882
2383.506261	22456.231791	59.038887
2382.647578	22391.948740	59.043892
2381.767404	22295.304418	59.048897
2381.617163	22204.026299	59.053901
2380.529191	22132.548765	59.058906
2380.082260	22034.419226	59.063911
2379.485698	21938.249291	59.068916
2378.633633	21850.868191	59.073921
2378.020938	21784.772055	59.078925
2377.277704	21684.220316	59.083930
2376.778954	21593.451050	59.088935
2376.040354	21508.364911	59.093940
2375.459495	21424.640677	59.098945
2375.288633	21339.026422	59.103949
2374.345124	21252.894843	59.108954
2373.617582	21148.579473	59.113959
2372.942467	21066.594084	59.118964
2372.156391	20984.179450	59.123969
2371.205350	20904.501077	59.128973
2370.643911	20810.117591	59.133978
2369.973506	20731.010633	59.138983
2368.888033	20639.666063	59.143988
2368.397620	20559.417418	59.148993
2367.568609	20485.914365	59.153997
2367.390734	20400.332782	59.159002
2366.595353	20315.214347	59.164007
2365.907935	20253.800872	59.169012
2365.428969	20162.468690	59.174017
2364.783533	20084.900545	59.179021
2363.767767	20003.493433	59.184026
2363.595993	19901.812066	59.189031
2362.499077	19831.633680	59.194036
2361.820361	19754.573373	59.199041
2361.206168	19684.628958	59.204045
2360.969789	19599.689444	59.209050
2360.067405	19507.591009	59.214055
2359.220202	19430.521917	59.219060
2358.741156	19352.462081	59.224065
2358.306371	19276.005695	59.229069
2357.523915	19197.609897	59.234074
2356.984640	19107.817856	59.239079
2356.112053	19029.292337	59.244084
2355.525924	18939.965777	59.249089
2354.955710	18867.103077	59.254093
2353.811936	18779.396975	59.259098
2353.338131	18708.408817	59.264103
2352.691227	18625.045927	59.269108
2351.908067	18544.022805	59.274113
2351.062448	18471.504823	59.279117
2350.471983	18399.394700	59.284122
2350.162900	18307.924856	59.289127
2349.282475	18255.701765	59.294132
2348.667178	18169.423827	59.299137
2348.149812	18089.565137	59.304141
2347.796010	18010.308477	59.309146
2346.997519	17927.595405	59.314151
2345.967387	17850.693402	59.319156
2345.163720	17764.603491	59.324161
2344.945780	17693.598333	59.329165
2343.885249	17618.466345	59.334170
2343.437230	17540.922580	59.339175
2342.812097	17462.724500	59.344180
2341.792957	17385.447529	59.349185
2341.011066	17299.485612	59.354189
2340.186082	17236.380745	59.359194
2339.736152	17170.491056	59.364199
2338.923650	17102.841701	59.369204
2338.379663	17022.188596	59.374209
2337.926478	16957.496763	59.379213
2337.129471	16893.848365	59.384218
2336.704980	16813.148784	59.389223
2336.165673	16746.640066	59.394228
2334.967109	16662.316750	59.399233
2334.749603	16610.031767	59.404237
2334.099427	16528.027442	59.409242
2333.975802	16444.594274	59.414247
2332.833572	16375.428309	59.419252
2332.246651	16296.208322	59.424257
2331.906272	16224.771532	59.429261
2330.630929	16155.736392	59.434266
2330.056626	16069.272459	59.439271
2329.497593	16000.865837	59.444276
2328.788586	15923.165682	59.449281
2328.079621	15868.499997	59.454285
2327.343788	15784.652499	59.459290
2327.197476	15700.033285	59.464295
2325.932056	15638.499296	59.469300
2325.713346	15562.478125	59.474305
2324.986766	15490.841396	59.479309
2323.783707	15418.479979	59.484314
2323.758598	15328.711374	59.489319
2323.003705	15261.922829	59.494324
2322.037533	15194.494667	59.499329
2321.536893	15121.915704	59.504333
2320.907379	15050.523222	59.509338
2320.579316	14947.995055	59.514343
2319.475591	14908.034600	59.519348
2318.963786	14837.412681	59.524353
2318.371365	14744.784523	59.529357
2317.521458	14664.748296	59.534362
2316.578983	14600.792317	59.539367
2316.093958	14537.038101	59.544372
2315.333187	14467.368122	59.549377
2314.705295	14399.806050	59.554381
2314.056597	14333.195306	59.559386
2313.068286	14256.980088	59.564391
2312.656053	14199.021724	59.569396
2312.041526	14124.958298	59.574401
2311.603867	14046.873228	59.579405
2310.724186	13991.424815	59.584410
2310.475424	13916.053908	59.589415
2309.729776	13846.609670	59.594420
2308.770068	13778.899766	59.599425
2308.396725	13708.214538	59.604429
2307.434296	13641.521132	59.609434
2307.123298	13558.748218	59.614439
2306.232699	13498.050415	59.619444
2305.437348	13426.577692	59.624449
2304.993256	13355.155334	59.629453
2304.160004	13286.834024	59.634458
2303.289691	13200.422781	59.639463
2302.478932	13144.835621	59.644468
2302.084113	13079.889482	59.649473
2301.738815	13024.773037	59.654477
2300.884017	12951.692683	59.659482
2300.512067	12866.455444	59.664487
2299.791173	12820.742107	59.669492
2298.951740	12736.254841	59.674497
2298.462298	12656.836610	59.679501
2297.614429	12604.486746	59.684506
2297.063646	12543.143475	59.689511
2296.668525	12444.365744	59.694516
2295.472138	12396.609197	59.699521
2295.188825	12321.229787	59.704525
2294.119257	12245.437310	59.709530
2293.532504	12177.472689	59.714535
2292.702535	12121.135399	59.719540
2292.199036	12049.950724	59.724545
2291.873081	11977.424215	59.729549
2290.858453	11918.881522	59.734554
2290.131646	11856.626800	59.739559
2289.625721	11778.526819	59.744564
2289.106938	11727.399364	59.749569
2288.344372	11655.079571	59.754573
2287.486532	11590.485870	59.759578
2287.384998	11523.586807	59.764583
2286.736734	11440.933470	59.769588
2285.740215	11367.491871	59.774593
2285.094319	11312.458525	59.779597
2284.218408	11223.497823	59.784602
2283.454324	11184.091205	59.789607
2283.256644	11110.024291	59.794612
2282.405825	11032.350363	59.799617
2281.814378	10975.947356	59.804621
2280.927019	10916.843347	59.809626
2280.556286	10821.748371	59.814631
2279.822561	10780.671596	59.819636
2279.405279	10704.329307	59.824641
2278.882758	10631.478872	59.829645
2278.042345	10563.660568	59.834650
2277.310543	10484.132806	59.839655
2276.482607	10423.002269	59.844660
2275.761863	10352.934266	59.849665
2275.095467	10297.223037	59.854669
2274.490383	10217.241854	59.859674
2273.811317	10140.810609	59.864679
2272.866688	10099.941149	59.869684
2272.295658	10030.762560	59.874689
2272.200058	9951.776943	59.879693
2270.937858	9889.292194	59.884698
2270.790231	9809.913598	59.889703
2269.967038	9765.366191	59.894708
2269.369568	9691.977557	59.899713
2268.851618	9619.750625	59.904718
2268.010462	9545.672766	59.909722
2267.392201	9471.361100	59.914727
2266.633499	9399.621934	59.919732
2265.537981	9354.774972	59.924737
2265.215795	9274.777598	59.929742
2264.332262	9206.307197	59.934746
2263.601746	9159.883046	59.939751
2262.952100	9094.482848	59.944756
2262.291491	9025.113253	59.949761
2262.097734	8943.288676	59.954766
2261.218022	8893.387814	59.959770
2260.492615	8843.616479	59.964775
2260.118437	8767.563567	59.969780
2259.108086	8704.163400	59.974785
2258.779850	8629.618200	59.979790
2258.060610	8578.631865	59.984794
2257.410334	8498.011447	59.989799
2256.743645	8437.275629	59.994804
2256.266566	8359.964692	59.999809
2255.556271	8309.793169	60.004814
2254.573173	8236.343468	60.009818
2254.099058	8165.781920	60.014823
2253.306668	8103.415499	60.019828
2252.451436	8040.216008	60.024833
2251.860762	7962.270391	60.029838
2250.818666	7910.267466	60.034842
2250.620168	7858.735161	60.039847
2249.880857	7792.697375	60.044852
2249.128016	7727.829133	60.049857
2249.079941	7654.216617	60.054862
2247.972513	7598.945907	60.059866
2247.387397	7539.430616	60.064871
2246.584721	7472.753508	60.069876
2245.976949	7400.173698	60.074881
2245.332834	7337.757776	60.079886
2244.939301	7267.401471	60.084890
2244.400886	7184.550652	60.089895
2243.406961	7147.592710	60.094900
2242.865686	7057.233484	60.099905
2242.108275	6991.869464	60.104910
2241.078679	6968.444977	60.109914
2240.419998	6888.843491	60.114919
2239.773954	6810.058416	60.119924
2239.020225	6766.584096	60.124929
2238.542208	6713.875092	60.129934
2237.616731	6646.867005	60.134938
2237.414272	6595.135406	60.139943
2236.920188	6529.360918	60.144948
2236.078235	6466.786792	60.149953
2235.738206	6392.744885	60.154958
2234.722504	6329.633348	60.159962
2234.297844	6257.848034	60.164967
2233.527230	6183.876270	60.169972
2232.713842	6153.517838	60.174977
2232.254425	6054.578617	60.179982
2231.726746	6012.296389	60.184986
2230.840977	5917.003544	60.189991
2230.049696	5884.356346	60.194996
2229.489748	5800.554396	60.200001
2229.121042	5755.022489	60.205006
2228.597002	5685.420039	60.210010
2227.391359	5630.176998	60.215015
2227.104636	5542.756226	60.220020
2226.397123	5483.000440	60.225025
2225.766270	5436.809921	60.230030
2224.509658	5351.571188	60.235034
2224.555689	5289.431418	60.240039
2223.665207	5228.795505	60.245044
2222.725200	5162.761845	60.250049
2222.064658	5101.094620	60.255054
2221.558956	5025.577035	60.260058
2220.480525	4992.824363	60.265063
2220.082730	4899.117743	60.270068
2219.407486	4882.817547	60.275073
2218.978829	4809.062634	60.280078
2218.568693	4719.095958	60.285082
2217.617497	4683.791304	60.290087
2216.813218	4598.000916	60.295092
2215.693640	4554.692899	60.300097
2215.414853	4485.224405	60.305102
2214.913357	4417.718304	60.310106
2214.005955	4384.066008	60.315111
2213.840860	4300.727304	60.320116
2212.679160	4238.969696	60.325121
2211.933855	4192.323311	60.330126
2211.334670	4131.929626	60.335130
2210.486463	4073.473995	60.340135
2210.595758	3984.068215	60.345140
2209.792871	3965.449364	60.350145
2208.751802	3878.103730	60.355150
2208.078897	3848.993552	60.360154
2207.728959	3758.287398	60.365159
2206.673039	3732.750822	60.370164
2205.734890	3650.372047	60.375169
2205.281024	3613.637774	60.380174
2204.660211	3553.014892	60.385178
2204.309679	3483.176878	60.390183
2203.565075	3416.835376	60.395188
2203.122947	3364.822697	60.400193
2202.480398	3307.220748	60.405198
2201.605054	3235.102123	60.410202
2200.892980	3195.562979	60.415207
2200.128259	3124.816089	60.420212
2199.744921	3056.072014	60.425217
2198.978623	3020.146648	60.430222
2198.040066	2975.256319	60.435226
2197.580878	2891.761720	60.440231
2197.268063	2837.131985	60.445236
2196.226051	2791.270533	60.450241
2195.845886	2733.947803	60.455246
2194.979045	2658.988614	60.460250
2194.088361	2612.683401	60.465255
2193.615495	2546.816887	60.470260
2192.816702	2490.353262	60.475265
2192.263508	2420.888404	60.480270
2191.472228	2392.331411	60.485274
2190.660262	2310.334452	60.490279
2189.956508	2257.656730	60.495284
2188.866776	2207.503101	60.500289
2188.964866	2165.611324	60.505294
2188.129993	2095.901730	60.510298
2187.714557	2056.522057	60.515303
2187.009638	1983.812457	60.520308
2186.034562	1941.393735	60.525313
2185.234047	1877.633229	60.530318
2184.737854	1822.225772	60.535322
2184.153723	1769.142879	60.540327
2183.461290	1711.833497	60.545332
2182.588549	1658.408845	60.550337
2182.045377	1616.220609	60.555342
2181.408477	1557.076804	60.560346
2180.596889	1500.788582	60.565351
2180.077821	1453.260305	60.570356
2179.415303	1397.414056	60.575361
2178.948942	1347.960098	60.580366
2178.000710	1296.750275	60.585370
2177.310902	1257.956427	60.590375
2176.899779	1204.613171	60.595380
2175.920369	1138.950097	60.600385
2175.388395	1092.305014	60.605390
2174.478523	1046.596847	60.610394
2174.069296	1005.355827	60.615399
2173.344600	958.363279	60.620404
2172.820984	904.058098	60.625409
2172.276839	831.613398	60.630414
2170.974621	805.661383	60.635418
2170.611641	768.546914	60.640423
2170.302849	716.029737	60.645428
2169.384537	650.747901	60.650433
2168.589863	616.942938	60.655438
2167.875134	579.205106	60.660442
2167.177065	522.464286	60.665447
2166.666471	482.749961	60.670452
2166.020293	431.547312	60.675457
2165.504624	393.295843	60.680462
2164.428439	330.401148	60.685466
2163.425987	287.947466	60.690471
2162.961005	263.918291	60.695476
2161.992282	225.854268	60.700481
2161.521908	183.822651	60.705486
2160.840649	150.905923	60.710490
2160.097576	104.441018	60.715495
2159.260217	86.775612	60.720500
2158.294131	40.392031	60.725505
2158.453593	23.916762	60.730510
2157.184996	-25.972883	60.735514
2155.864777	-15.081658	60.740519
2151.723235	36.607908	60.745524
2150.127292	62.083333	60.750529
2150.657064	56.682045	60.755534
2151.075103	84.078680	60.760538
2151.593591	34.073989	60.765543
2151.286551	64.360944	60.770548
2150.838298	48.081424	60.775553
2150.269164	49.789623	60.780558
2149.178485	53.914362	60.785562
2147.786543	55.790969	60.790567
2146.853754	65.032862	60.795572
2146.372389	80.870183	60.800577
2146.153869	49.348345	60.805582
2145.247766	71.149003	60.810586
2145.273183	66.414341	60.815591
2144.968097	61.974964	60.820596
2144.149933	71.454127	60.825601
2143.687488	45.550009	60.830606
2142.374934	88.639982	60.835610
2141.358558	64.411652	60.840615
2140.829295	68.089359	60.845620
2140.161605	67.118313	60.850625
2140.250074	72.173958	60.855630
2139.551860	67.598276	60.860634
2138.828911	67.474900	60.865639
2138.029152	77.788470	60.870644
2136.963155	72.077449	60.875649
2136.428748	69.863172	60.880654
2135.348768	60.429784	60.885658
2135.489747	75.662165	60.890663
2135.355446	65.509456	60.895668
2134.317917	54.711643	60.900673
2133.434829	72.911792	60.905678
2132.951364	75.170926	60.910682
2131.847130	62.641240	60.915687
2131.300937	73.952159	60.920692
2130.439278	70.305968	60.925697
2129.590111	60.203628	60.930702
2128.674087	60.424691	60.935706
2128.972005	84.637737	60.940711
2128.850393	47.791171	60.945716
2127.460263	95.830682	60.950721
2126.865404	54.399510	60.955726
2126.399526	83.013405	60.960730
2125.548153	51.987794	60.965735
2125.012431	73.641377	60.970740
2124.100853	70.909817	60.975745
2123.340342	61.138746	60.980750
2122.408805	74.332112	60.985754
2121.974439	78.901472	60.990759
2121.474877	50.149092	60.995764
2120.464904	86.861457	61.000769
2120.854439	47.011821	61.005774
2120.016454	89.845148	61.010778
2118.769048	65.705529	61.015783
2118.079137	86.719734	61.020788
2117.917643	58.599635	61.025793
2117.429867	89.902443	61.030798
2116.395274	60.522199	61.035802
2115.599691	83.390233	61.040807
2115.247214	53.646303	61.045812
2114.220259	78.145269	61.050817
2114.144268	61.303646	61.055822
2112.555395	79.188474	61.060826
2112.810965	57.221415	61.065831
2112.164481	59.213121	61.070836
2110.730569	75.379786	61.075841
2110.552222	60.344168	61.080846
2109.683222	68.634552	61.085850
2109.208533	72.049727	61.090855
2108.749162	64.719188	61.095860
2107.774076	72.384621	61.100865
2107.338439	68.978323	61.105870
2106.202112	77.960811	61.110874
2105.959408	63.868917	61.115879
2105.537663	68.707496	61.120884
2104.271859	75.753623	61.125889
2103.970492	58.958810	61.130894
2103.366936	70.113259	61.135898
2102.271063	75.795226	61.140903
2102.038772	71.481489	61.145908
2101.349589	79.052671	61.150913
2100.898713	65.742832	61.155918
2099.292852	74.076046	61.160922
2098.939104	63.767367	61.165927
2098.777252	64.261398	61.170932
2098.297277	64.525231	61.175937
2097.944693	61.179870	61.180942
2096.243160	71.844702	61.185946
2095.497048	73.503734	61.190951
2095.802173	68.619033	61.195956
2094.210332	67.009375	61.200961
2094.211645	63.271975	61.205966
2093.813676	65.158018	61.210970
2092.474107	55.161907	61.215975
2091.812050	63.444681	61.220980
2090.892879	78.768035	61.225985
2091.400397	66.881403	61.230990
2090.138226	67.365562	61.235994
2089.188359	65.046927	61.240999
2088.686514	69.215431	61.246004
2087.629638	69.558206	61.251009
2087.978229	59.220068	61.256014
2086.965302	60.265463	61.261018
2086.211049	72.464072	61.266023
2085.871797	63.293181	61.271028
2084.588500	65.335498	61.276033
2084.014703	60.180298	61.281038
2083.667477	64.343186	61.286042
2082.627163	72.044206	61.291047
2082.489385	59.140407	61.296052
2081.679916	64.083096	61.301057
2081.299077	62.494135	61.306062
2080.858270	63.929682	61.311066
2079.385676	65.046455	61.316071
2078.597244	66.172914	61.321076
2077.799150	67.617860	61.326081
2077.939707	55.988162	61.331086
2076.606442	60.961944	61.336090
2076.002270	58.895942	61.341095
2075.610565	53.235631	61.346100
2075.045164	67.807428	61.351105
2074.650514	68.483480	61.356110
2073.682085	65.166478	61.361114
2073.080888	64.218012	61.366119
2072.380812	69.815094	61.371124
2071.815902	59.368059	61.376129
2071.722185	56.341147	61.381134
2070.723507	70.232694	61.386138
2069.284891	64.252855	61.391143
2068.683389	58.187467	61.396148
2068.463137	69.355199	61.401153
2067.583240	69.002873	61.406158
2066.809467	70.442386	61.411162
2066.293765	68.316614	61.416167
2065.880672	60.846286	61.421172
2064.810506	63.517074	61.426177
2064.595254	54.036368	61.431182
2064.043688	70.135543	61.436186
2063.522522	56.371700	61.441191
2063.158349	58.881556	61.446196
2062.253844	57.244829	61.451201
2060.788989	55.646577	61.456206
2060.040991	57.331145	61.461210
2059.425470	63.845166	61.466215
2059.277178	61.926000	61.471220
2058.069967	59.917868	61.476225
2057.959945	55.450702	61.481230
2056.948485	58.955805	61.486234
2056.473045	60.037324	61.491239
2056.364207	60.005728	61.496244
2055.710673	53.134936	61.501249
2055.265947	54.399229	61.506254
2053.934589	49.331163	61.511258
2052.850810	62.797842	61.516263
2052.490132	52.580164	61.521268
2051.870190	63.973747	61.526273
2051.292915	59.306364	61.531278
2050.579508	59.727097	61.536282
2050.111666	59.916475	61.541287
2049.804966	63.837979	61.546292
2049.217822	62.303843	61.551297
2048.349758	55.413487	61.556302
2046.993071	57.678770	61.561306
2046.201991	56.861368	61.566311
2045.681566	60.137159	61.571316
2044.918147	60.393951	61.576321
2044.383967	65.210959	61.581326
2044.241169	56.858838	61.586330
2043.443419	61.812291	61.591335
2043.188602	58.766798	61.596340
2042.291333	65.043280	61.601345
2041.820807	66.226519	61.606350
2041.118967	60.404135	61.611354
2039.306151	53.867152	61.616359
2039.200651	64.991436	61.621364
2038.274393	78.483592	61.626369
2038.279422	49.187565	61.631374
2037.593489	61.017377	61.636378
2036.920641	66.725256	61.641383
2036.438223	64.778703	61.646388
2035.890084	70.242873	61.651393
2035.171388	57.620514	61.656398
2034.173827	59.617501	61.661402
2033.154326	66.842168	61.666407
2032.464265	59.430001	61.671412
2031.726024	63.992408	61.676417
2031.457309	62.732570	61.681422
2030.698868	66.771507	61.686426
2030.367543	72.571832	61.691431
2030.202401	67.582005	61.696436
2029.254904	69.127946	61.701441
2028.482060	66.984653	61.706446
2027.674495	67.015080	61.711450
2026.502339	67.100222	61.716455
2026.449146	58.144128	61.721460
2025.615425	67.930119	61.726465
2025.439782	76.369082	61.731470
2024.666433	63.813742	61.736474
2023.175766	68.907147	61.741479
2022.961158	58.549598	61.746484
2022.013004	62.408924	61.751489
2021.338307	66.672679	61.756494
2021.023512	61.157857	61.761498
2020.589302	55.994712	61.766503
2020.342040	62.737277	61.771508
2019.087321	68.452367	61.776513
2018.055286	59.339421	61.781518
2017.190709	59.908731	61.786522
2016.625087	53.989046	61.791527
2016.413409	64.114672	61.796532
2015.748294	65.729330	61.801537
2015.505685	46.755447	61.806542
2015.080816	78.522869	61.811546
2013.739011	47.513689	61.816551
2012.937513	67.120085	61.821556
2012.502120	69.388952	61.826561
2011.784453	46.048412	61.831566
2011.246958	71.642883	61.836570
2010.728869	56.005239	61.841575
2009.919727	70.407583	61.846580
2008.696718	56.857661	61.851585
2008.096006	55.590605	61.856590
2007.400538	52.820057	61.861594
2006.805771	50.024064	61.866599
2006.473570	63.461338	61.871604
2006.205362	70.845868	61.876609
2005.841122	47.526495	61.881614
2005.169693	72.481515	61.886618
2003.968816	77.139444	61.891623
2003.026473	53.708410	61.896628
2001.942197	76.606495	61.901633
2002.188144	55.238620	61.906638
2001.251471	47.515549	61.911642
2000.620876	77.253067	61.916647
2000.151354	62.180119	61.921652
1998.895596	64.758973	61.926657
1998.317269	52.672566	61.931662
1997.762787	61.119618	61.936666
1997.045545	59.664491	61.941671
1996.350224	64.224823	61.946676
1995.783361	66.538215	61.951681
1995.691319	58.561224	61.956686
1995.150785	69.547993	61.961690
1993.724414	59.873210	61.966695
1993.285513	59.454061	61.971700
1992.571973	69.856465	61.976705
1992.176349	64.259864	61.981710
1991.595729	55.068969	61.986714
1990.820725	61.490050	61.991719
1990.000487	54.273598	61.996724
1988.749777	71.751567	62.001729
1988.404894	68.980561	62.006734
1988.085714	58.393627	62.011738
1987.248395	65.253512	62.016743
1987.007632	57.878845	62.021748
1986.384301	53.668203	62.026753
1985.649133	66.387315	62.031758
1984.782430	58.648408	62.036762
1983.820786	67.147483	62.041767
1983.701493	56.271790	62.046772
1982.985309	60.792861	62.051777
1982.027401	56.800902	62.056782
1981.092442	71.585905	62.061786
1980.053167	70.126711	62.066791
1979.709091	44.998627	62.071796
1979.284028	75.969745	62.076801
1978.763855	44.371302	62.081806
1978.267233	67.981874	62.086810
1977.985547	64.117524	62.091815
1977.393308	47.096137	62.096820
1975.718278	77.672777	62.101825
1975.535726	47.493539	62.106830
1974.704340	64.151191	62.111834
1973.900444	66.554252	62.116839
1973.994206	54.712806	62.121844
1973.274780	57.372102	62.126849
1972.487276	62.341292	62.131854
1971.408873	66.729065	62.136858
1970.563676	55.793576	62.141863
1970.535778	60.836137	62.146868
1969.664227	65.563217	62.151873
1969.306737	55.196826	62.156878
1968.293312	51.428142	62.161882
1966.877109	67.841186	62.166887
1966.892779	61.026603	62.171892
1966.274861	58.707357	62.176897
1965.835507	63.460440	62.181902
1965.104734	39.801910	62.186906
1963.820509	74.775909	62.191911
1963.564647	46.768638	62.196916
1962.452453	61.375200	62.201921
1962.261394	52.827337	62.206926
1961.727523	61.378349	62.211930
1961.332944	61.177663	62.216935
1961.025444	65.979197	62.221940
1959.331868	54.609141	62.226945
1958.934000	58.780077	62.231950
1958.416604	56.703484	62.236954
1957.855674	58.970210	62.241959
1957.292281	43.188413	62.246964
1956.202068	74.981018	62.251969
1955.563883	56.136169	62.256974
1954.918741	55.929531	62.261978
1954.223456	64.480941	62.266983
1953.833769	53.788522	62.271988
1953.457031	59.577133	62.276993
1953.034582	58.070488	62.281998
1952.070076	77.453634	62.287002
1951.001731	67.458698	62.292007
1950.959271	57.848082	62.297012
1949.316959	57.990552	62.302017
1948.810863	68.098267	62.307022
1948.251026	71.255759	62.312026
1947.585737	76.107791	62.317031
1947.369506	45.981221	62.322036
1946.351172	77.896457	62.327041
1946.481048	57.989856	62.332046
1945.184663	61.228010	62.337050
1943.893357	67.368388	62.342055
1943.796781	65.072032	62.347060
1942.717530	49.291708	62.352065
1942.734254	77.595573	62.357070
1942.474527	57.372375	62.362074
1941.025290	59.499446	62.367079
1940.516121	57.503548	62.372084
1939.614097	57.648341	62.377089
1939.045077	57.972067	62.382094
1938.686176	59.197523	62.387098
1938.112684	65.058373	62.392103
1937.436636	66.367293	62.397108
1936.119122	58.181185	62.402113
1935.821252	64.654257	62.407118
1935.373310	65.135373	62.412122
1934.923045	60.425781	62.417127
1934.313811	45.162175	62.422132
1932.911105	70.882960	62.427137
1932.476144	59.179069	62.432142
1931.778923	52.782008	62.437146
1931.221715	71.971183	62.442151
1931.308263	54.219176	62.447156
1930.038156	62.658430	62.452161
1928.983445	59.640602	62.457166
1928.545410	59.457858	62.462170
1927.959219	55.993504	62.467175
1927.973220	57.303254	62.472180
1926.635424	58.822888	62.477185
1925.862239	54.311218	62.482190
1925.191153	67.482190	62.487194
1924.102088	56.833007	62.492199
1924.182707	67.970310	62.497204
1923.574187	71.608599	62.502209
1923.268958	63.135631	62.507214
1922.205838	53.644490	62.512218
1921.235470	67.288734	62.517223
1920.980465	59.886378	62.522228
1920.020711	60.571750	62.527233
1919.221434	48.356460	62.532238
1918.299754	79.111543	62.537242
1917.626261	58.648129	62.542247
1917.578129	50.802946	62.547252
1916.629406	78.367574	62.552257
1916.239319	52.884126	62.557262
1916.101125	67.627790	62.562266
1914.887149	67.760621	62.567271
1914.368582	47.168554	62.572276
1913.288507	57.247551	62.577281
1912.937547	62.718275	62.582286
1912.469577	55.699801	62.587290
1910.727033	67.140754	62.592295
1910.196441	46.126420	62.597300
1909.860959	53.668273	62.602305
1909.498920	54.782272	62.607310
1909.045553	67.965986	62.612314
1908.536443	54.856266	62.617319
1908.461744	53.048425	62.622324
1906.971052	65.002875	62.627329
1906.454237	44.290695	62.632334
1905.706248	55.280437	62.637338
1904.488510	57.514267	62.642343
1903.680932	51.166276	62.647348
1903.217250	63.829678	62.652353
1902.527208	51.751583	62.657358
1902.177680	44.515625	62.662362
1901.876389	51.301457	62.667367
1901.874028	48.154404	62.672372
1900.542472	61.747190	62.677377
1899.565043	65.781506	62.682382
1899.058891	61.930731	62.687386
1898.404487	54.993898	62.692391
1897.413188	55.178110	62.697396
1896.323248	46.802942	62.702401
1895.871166	54.368040	62.707406
1895.646431	61.521748	62.712410
1895.122497	57.881946	62.717415
1894.554435	49.557950	62.722420
1894.278115	58.971624	62.727425
1893.130790	54.834744	62.732430
1892.540089	55.316456	62.737434
1891.690340	57.597515	62.742439
1891.253188	49.408846	62.747444
1890.370739	50.231757	62.752449
1889.353724	59.603772	62.757454
1888.873642	48.659236	62.762458
1888.233890	58.786593	62.767463
1887.966285	53.770482	62.772468
1887.419244	57.810577	62.777473
1886.470620	51.932819	62.782478
1885.372970	54.122360	62.787482
1884.686641	61.437665	62.792487
1884.199483	51.907131	62.797492
1883.797989	58.155394	62.802497
1883.425293	57.478182	62.807502
1882.692054	51.898948	62.812506
1881.634017	59.434113	62.817511
1881.250081	49.045141	62.822516
1880.717907	53.615859	62.827521
1880.211708	58.026343	62.832526
1879.133024	54.570819	62.837530
1878.317476	56.786530	62.842535
1877.932076	44.273744	62.847540
1877.257158	45.552538	62.852545
1876.633907	50.041528	62.857550
1875.629324	57.522477	62.862554
1874.652130	57.105245	62.867559
1874.397004	50.016720	62.872564
1873.884799	51.119876	62.877569
1873.573523	47.618194	62.882574
1873.105166	47.605846	62.887578
1871.647898	55.511894	62.892583
1871.263612	61.867808	62.897588
1870.756983	50.184783	62.902593
1870.246002	55.674609	62.907598
1869.136187	49.738880	62.912602
1868.081774	50.691600	62.917607
1867.699034	61.561859	62.922612
1867.222857	44.190949	62.927617
1866.978896	53.173725	62.932622
1866.480109	47.049518	62.937626
1865.120230	61.138797	62.942631
1864.529481	42.587658	62.947636
1863.854388	62.888312	62.952641
1863.473008	54.921015	62.957646
1862.799068	43.624092	62.962650
1861.396718	54.940084	62.967655
1860.913957	39.492437	62.972660
1860.243083	72.085736	62.977665
1860.076726	60.534747	62.982670
1859.837287	43.402202	62.987674
1859.069576	65.983534	62.992679
1858.033945	52.276229	62.997684
1857.420637	56.134472	63.002689
1856.673079	46.333078	63.007694
1856.502660	44.054763	63.012698
1855.275737	57.738174	63.017703
1854.501896	53.568814	63.022708
1853.637719	51.933644	63.027713
1853.113467	47.768806	63.032718
1853.131438	49.271879	63.037722
1852.096428	64.544272	63.042727
1851.677055	40.177222	63.047732
1850.444771	53.960825	63.052737
1850.062781	50.705329	63.057742
1849.980323	58.836182	63.062746
1849.024088	61.138894	63.067751
1848.020215	39.852837	63.072756
1847.058801	66.815520	63.077761
1846.831087	54.965213	63.082766
1846.416186	46.236887	63.087770
1845.244569	51.508360	63.092775
1844.370955	68.611111	63.097780
1843.918880	60.245054	63.102785
1843.443380	48.192838	63.107790
1842.837374	44.815231	63.112794
1842.513798	65.652975	63.117799
1841.825897	45.810039	63.122804
1840.543934	70.937692	63.127809
1840.020746	44.712220	63.132814
1839.496478	75.475148	63.137818
1839.256440	35.671987	63.142823
1838.508144	71.292555	63.147828
1837.516380	39.858970	63.152833
1836.995012	73.704218	63.157838
1836.683767	40.429582	63.162842
1835.595634	56.770064	63.167847
1834.957579	61.579944	63.172852
1834.097499	39.615083	63.177857
1833.466089	90.959058	63.182862
1832.980100	88.011794	63.187866
1832.617229	69.541136	63.192871
1831.963268	44.990576	63.197876
1831.023206	55.933565	63.202881
1830.186184	54.415509	63.207886
1829.812693	46.450126	63.212890
1828.735846	49.502088	63.217895
1827.864553	61.375554	63.222900
1827.370451	57.691609	63.227905
1826.660597	52.570704	63.232910
1826.549596	56.707137	63.237914
1825.839305	56.607067	63.242919
1825.392799	52.330546	63.247924
1823.996484	54.441389	63.252929
1823.666228	54.992139	63.257934
1823.182143	64.758916	63.262938
1822.584872	62.579923	63.267943
1821.687959	54.254556	63.272948
1820.883674	56.697142	63.277953
1820.026424	62.912137	63.282958
1820.018820	52.789829	63.287962
1819.412371	50.237001	63.292967
1818.344262	63.797443	63.297972
1817.895859	40.046845	63.302977
1817.053944	60.984239	63.307982
1816.874402	53.325506	63.312986
1815.566708	54.976026	63.317991
1814.600258	58.187073	63.322996
1814.094567	50.991700	63.328001
1813.725833	44.589823	63.333006
1813.506108	50.564808	63.338010
1812.861356	46.397040	63.343015
1812.076748	43.350564	63.348020
1810.893023	63.668920	63.353025
1810.614459	54.340234	63.358030
1809.875688	44.040749	63.363034
1809.063524	63.497471	63.368039
1808.250340	60.256844	63.373044
1807.276506	59.809144	63.378049
1806.742897	52.052108	63.383054
1806.553613	56.065362	63.388058
1806.060515	65.896646	63.393063
1805.917531	50.743536	63.398068
1805.035784	48.202895	63.403073
1803.769619	58.598469	63.408078
1803.711098	52.260862	63.413082
1802.367712	49.730459	63.418087
1801.514908	50.622804	63.423092
1800.754356	46.662655	63.428097
1800.060999	57.785659	63.433102
1800.017985	59.662675	63.438106
1799.337867	56.948094	63.443111
1799.359635	50.198788	63.448116
1798.059100	51.818219	63.453121
1797.261479	56.801671	63.458126
1796.976417	42.439073	63.463130
1796.336655	65.020585	63.468135
1795.390432	55.192415	63.473140
1794.601165	58.110416	63.478145
1793.769107	41.316423	63.483150
1793.713031	69.825742	63.488154
1792.492993	53.383498	63.493159
1791.671913	42.978827	63.498164
1791.072458	66.071153	63.503169
1790.720265	53.972560	63.508174
1790.596573	41.941761	63.513178
1789.220152	50.489406	63.518183
1788.527031	59.474137	63.523188
1787.775735	52.166396	63.528193
1787.288427	56.430398	63.533198
1787.231189	43.807178	63.538202
1786.386674	47.199130	63.543207
1785.449426	49.984523	63.548212
1784.695391	69.853049	63.553217
1784.301088	39.521463	63.558222
1783.482029	53.480721	63.563226
1782.211637	57.519026	63.568231
1781.958239	40.609486	63.573236
1781.135768	39.866535	63.578241
1780.627653	56.420826	63.583246
1780.670613	42.425584	63.588250
1779.260321	50.843003	63.593255
1778.777935	43.965623	63.598260
1778.201660	43.830090	63.603265
1777.406565	44.533514	63.608270
1777.278704	36.352528	63.613274
1776.145706	48.007374	63.618279
1775.679419	39.753985	63.623284
1774.978404	46.500807	63.628289
1774.607026	49.235754	63.633294
1773.377789	47.604977	63.638298
1772.372220	41.526593	63.643303
1772.275668	51.805797	63.648308
1771.734899	48.884601	63.653313
1770.859432	40.882270	63.658318
1770.053399	44.547220	63.663322
1768.948531	47.855954	63.668327
1768.378244	48.652980	63.673332
1768.238756	51.264370	63.678337
1767.678962	54.816102	63.683342
1767.675663	47.503107	63.688346
1766.464528	53.346985	63.693351
1765.830971	69.839217	63.698356
1765.401781	42.103981	63.703361
1764.126715	59.685210	63.708366
1763.233592	52.401580	63.713370
1762.670466	54.815341	63.718375
1762.264055	44.792654	63.723380
1761.727470	49.266323	63.728385
1761.197807	57.550194	63.733390
1760.582209	47.488194	63.738394
1759.631036	30.609076	63.743399
1759.212635	66.737017	63.748404
1758.506050	50.970147	63.753409
1756.834446	41.703469	63.758414
1756.853395	46.677077	63.763418
1755.654825	65.942880	63.768423
1755.491764	47.107821	63.773428
1755.446636	44.128408	63.778433
1754.807795	50.676136	63.783438
1754.125354	53.678100	63.788442
1752.908529	55.888198	63.793447
1752.635303	44.243835	63.798452
1752.180383	42.504278	63.803457
1750.829643	51.241816	63.808462
1750.212609	50.262829	63.813466
1749.843330	42.457638	63.818471
1749.494341	45.551711	63.823476
1747.964134	46.572165	63.828481
1747.550415	45.201359	63.833486
1746.863929	38.227105	63.838490
1746.215158	61.122262	63.843495
1746.353163	56.615730	63.848500
1745.656726	53.541077	63.853505
1744.261968	45.788383	63.858510
1743.579645	39.365373	63.863514
1742.913653	54.194412	63.868519
1742.746180	43.312229	63.873524
1741.924786	38.177536	63.878529
1740.798521	45.652617	63.883534
1740.316692	57.398009	63.888538
1740.214519	45.150921	63.893543
1739.743954	32.375761	63.898548
1739.071189	50.036353	63.903553
1738.006391	43.959506	63.908558
1737.417158	48.175050	63.913562
1736.181727	53.936071	63.918567
1735.646183	41.445601	63.923572
1735.174775	55.450569	63.928577
1734.772028	53.669612	63.933582
1734.244366	44.781040	63.938586
1732.665859	45.905363	63.943591
1732.094729	39.504117	63.948596
1731.556137	45.326332	63.953601
1731.031453	43.750816	63.958606
1730.661197	58.010942	63.963610
1730.281804	53.179760	63.968615
1729.809325	55.162835	63.973620
1728.865205	42.209012	63.978625
1727.852898	76.651018	63.983630
1727.640387	50.146020	63.988634
1726.149126	45.958203	63.993639
1725.464448	56.288249	63.998644
1725.251266	38.262222	64.003649
1724.642465	42.378378	64.008654
1724.315725	48.518587	64.013658
1723.446073	48.312978	64.018663
1722.409395	54.493420	64.023668
1722.006264	52.729873	64.028673
1720.966892	56.794583	64.033678
1721.224666	36.692703	64.038682
1720.201730	66.194464	64.043687
1719.230913	28.546362	64.048692
1718.529773	67.596991	64.053697
1718.064983	34.999640	64.058702
1717.912135	54.198675	64.063706
1716.698061	48.987597	64.068711
1716.103959	35.238636	64.073716
1715.509316	51.516523	64.078721
1715.001272	45.324443	64.083726
1714.028878	31.867375	64.088730
1713.016745	63.720105	64.093735
1712.774867	36.388791	64.098740
1712.387372	57.577266	64.103745
1711.474988	61.336396	64.108750
1710.740759	51.165528	64.113754
1709.772231	54.264982	64.118759
1709.481238	38.604011	64.123764
1709.367716	61.608102	64.128769
1707.907481	38.666374	64.133774
1707.151276	55.606984	64.138778
1706.805079	47.796557	64.143783
1706.180625	49.655549	64.148788
1705.715330	68.213563	64.153793
1705.097955	53.761846	64.158798
1704.097712	39.735219	64.163802
1703.186642	59.603451	64.168807
1702.827693	51.869161	64.173812
1702.486364	54.094745	64.178817
1701.465646	46.889757	64.183822
1700.674283	38.248080	64.188826
1699.544290	33.853094	64.193831
1699.337331	48.087270	64.198836
1699.443046	49.568517	64.203841
1698.747006	53.700115	64.208846
1697.792189	51.682026	64.213850
1697.173245	59.541718	64.218855
1696.739589	52.573041	64.223860
1695.440701	55.619327	64.228865
1694.592723	52.045242	64.233870
1694.168921	40.096826	64.238874
1693.368974	53.222052	64.243879
1693.452805	48.093380	64.248884
1692.445078	49.882379	64.253889
1691.568901	52.407379	64.258894
1691.312675	43.769000	64.263898
1690.265648	57.291429	64.268903
1689.237614	43.289721	64.273908
1688.559240	41.232453	64.278913
1688.011694	40.371747	64.283918
1687.768977	56.625273	64.288922
1687.452176	46.593100	64.293927
1686.907977	41.911107	64.298932
1685.700457	42.708457	64.303937
1685.048439	57.896388	64.308942
1684.796142	38.353329	64.313946
1683.126344	39.487453	64.318951
1682.745972	58.700556	64.323956
1682.286295	32.830928	64.328961
1681.679801	65.413966	64.333966
1681.631926	33.089437	64.338970
1680.465486	56.817411	64.343975
1679.539612	37.225247	64.348980
1678.745032	40.479993	64.353985
1678.520778	62.948188	64.358990
1678.164255	30.515010	64.363994
1676.812484	60.524716	64.368999
1676.276520	37.217003	64.374004
1675.783337	59.041976	64.379009
1675.148890	53.887065	64.384014
1674.993816	41.739854	64.389018
1673.381418	37.454628	64.394023
1673.029937	47.717552	64.399028
1672.664071	45.612220	64.404033
1672.278445	49.844314	64.409038
1671.394685	49.762382	64.414042
1670.131397	69.415364	64.419047
1669.463320	42.579094	64.424052
1669.296455	61.349872	64.429057
1669.062249	42.393688	64.434062
1668.029046	46.400668	64.439066
1667.186546	60.866697	64.444071
1666.724937	38.625754	64.449076
1665.603192	58.797103	64.454081
1664.727171	43.948131	64.459086
1664.158265	38.946812	64.464090
1663.699611	61.313476	64.469095
1663.578200	34.827172	64.474100
1662.791436	31.345875	64.479105
1662.338302	65.851980	64.484110
1661.598407	25.529141	64.489114
1660.984604	61.243410	64.494119
1660.115322	38.712438	64.499124
1659.387558	44.000197	64.504129
1658.316810	48.481475	64.509134
1658.018642	52.554605	64.514138
1657.427602	48.834065	64.519143
1656.385719	33.825387	64.524148
1655.433994	56.130034	64.529153
1655.268216	52.160593	64.534158
1655.059500	34.991699	64.539162
1654.173164	53.263362	64.544167
1653.243493	38.449732	64.549172
1652.378979	34.853064	64.554177
1651.635307	44.432434	64.559182
1651.621616	48.528174	64.564186
1651.117333	30.780224	64.569191
1649.925446	54.937998	64.574196
1649.474366	49.129525	64.579201
1648.592578	38.204736	64.584206
1648.279615	59.136953	64.589210
1646.884062	42.881963	64.594215
1646.401721	37.251918	64.599220
1645.790247	53.387411	64.604225
1645.267929	39.400000	64.609230
1645.284714	50.109018	64.614234
1644.586637	50.902719	64.619239
1643.406927	36.819489	64.624244
1642.824222	51.616380	64.629249
1642.324335	50.856915	64.634254
1641.690831	37.052743	64.639258
1639.996157	51.193708	64.644263
1639.720586	52.760757	64.649268
1639.503816	42.864086	64.654273
1639.207218	35.304406	64.659278
1638.800573	30.534347	64.664282
1637.879531	58.693765	64.669287
1637.297265	56.091413	64.674292
1636.408720	44.964282	64.679297
1635.109237	55.347864	64.684302
1634.660147	37.901787	64.689306
1634.252429	50.923707	64.694311
1633.647317	43.837217	64.699316
1632.801960	41.207285	64.704321
1632.196390	44.760003	64.709326
1631.363216	42.933916	64.714330
1630.757444	56.116610	64.719335
1630.524429	49.120804	64.724340
1629.310924	39.229538	64.729345
1628.478921	56.770371	64.734350
1628.235885	48.196135	64.739354
1627.745742	45.172319	64.744359
1627.120666	46.643517	64.749364
1626.468521	59.325830	64.754369
1625.644435	52.475968	64.759374
1625.203828	32.160228	64.764378
1624.123711	54.335471	64.769383
1623.100942	49.243851	64.774388
1622.929255	42.489028	64.779393
1622.090444	56.740020	64.784398
1621.725722	53.724660	64.789402
1621.447769	52.745445	64.794407
1620.314598	49.790679	64.799412
1619.620482	46.633701	64.804417
1618.847035	50.049101	64.809422
1618.689419	35.022947	64.814426
1617.368100	65.699582	64.819431
1616.547113	49.268168	64.824436
1616.107299	47.045292	64.829441
1615.596066	59.274732	64.834446
1615.783828	51.215492	64.839450
1614.655098	47.810616	64.844455
1613.611370	54.711267	64.849460
1613.272702	45.783241	64.854465
1612.284413	58.731840	64.859470
1611.504224	50.072648	64.864474
1610.355509	42.230488	64.869479
1609.953739	38.894608	64.874484
1609.516352	48.546743	64.879489
1609.155751	38.095799	64.884494
1609.306289	50.412466	64.889498
1607.852804	36.224530	64.894503
1607.249639	31.950878	64.899508
1606.870212	69.901763	64.904513
1605.835203	48.778478	64.909518
1604.876736	46.423556	64.914522
1604.466526	54.656926	64.919527
1603.479488	42.832716	64.924532
1603.229800	48.129680	64.929537
1602.653189	49.596338	64.934542
1601.702678	32.114837	64.939546
1600.646870	51.878343	64.944551
1600.187808	47.230150	64.949556
1600.288381	15.411932	64.954561
1599.319986	51.748603	64.959566
1598.487409	13.928867	64.964570
1597.406989	65.430743	64.969575
1597.422074	31.520953	64.974580
1597.052020	56.549470	64.979585
1596.408238	42.491491	64.984590
1595.383394	22.848892	64.989594
1594.569666	62.666388	64.994599
1593.842014	25.463856	64.999604
1592.831043	47.531919	65.004609
1591.885716	22.299306	65.009614
1591.479672	52.835220	65.014618
1591.363561	36.432177	65.019623
1591.006018	20.799179	65.024628
1590.568901	63.034091	65.029633
1589.698133	40.946494	65.034638
1589.171628	55.352860	65.039642
1587.938675	23.949931	65.044647
1586.970440	61.412482	65.049652
1586.480320	31.879939	65.054657
1585.980331	60.136453	65.059662
1585.750264	41.340479	65.064666
1584.474221	36.162975	65.069671
1583.882847	47.698705	65.074676
1583.343044	28.899926	65.079681
1582.591959	36.605588	65.084686
1582.274157	43.977493	65.089690
1580.901032	36.338157	65.094695
1580.281881	45.289084	65.099700
1580.246521	46.841623	65.104705
1579.718026	32.658115	65.109710
1578.945929	39.949247	65.114714
1578.346175	47.457414	65.119719
1577.184705	25.215777	65.124724
1576.866029	46.965692	65.129729
1575.589321	40.436921	65.134734
1575.292064	36.567229	65.139738
1574.369335	41.212663	65.144743
1573.576813	41.631903	65.149748
1573.619804	46.136503	65.154753
1572.994718	44.264755	65.159758
1572.482561	37.026330	65.164762
1571.372759	33.405593	65.169767
1570.941633	60.443285	65.174772
1570.388187	24.529777	65.179777
1569.189714	46.660750	65.184782
1568.238455	41.214037	65.189786
1568.094324	25.089840	65.194791
1567.734771	59.768687	65.199796
1567.220279	33.132003	65.204801
1566.399355	40.024066	65.209806
1565.826738	20.771651	65.214810
1564.971571	48.526368	65.219815
1564.041933	39.536154	65.224820
1563.595445	25.331743	65.229825
1562.850567	36.825631	65.234830
1562.433861	43.293939	65.239834
1561.112391	28.444860	65.244839
1560.270303	43.251426	65.249844
1560.405423	50.914045	65.254849
1559.648179	25.310957	65.259854
1558.934415	39.969403	65.264858
1558.483498	54.843127	65.269863
1557.328609	37.778876	65.274868
1556.795771	25.344819	65.279873
1556.167114	50.100617	65.284878
1556.161643	33.063449	65.289882
1554.821709	46.900514	65.294887
1554.214642	40.199117	65.299892
1553.831861	40.611597	65.304897
1553.084958	49.046696	65.309902
1552.332180	31.633145	65.314906
1551.334169	18.377355	65.319911
1550.624025	49.336871	65.324916
1550.392454	16.155421	65.329921
1549.784453	53.100261	65.334926
1549.275055	29.398912	65.339930
1548.502953	35.710816	65.344935
1547.377645	39.117495	65.349940
1547.148055	37.696966	65.354945
1546.167313	39.915368	65.359950
1545.312034	30.159610	65.364954
1544.597223	30.378862	65.369959
1544.400680	31.025085	65.374964
1544.172162	28.609385	65.379969
1543.390054	33.368090	65.384974
1542.665798	29.914747	65.389978
1542.185755	23.215252	65.394983
1541.286120	42.848290	65.399988
1540.175608	48.127517	65.404993
1539.400430	36.214488	65.409998
1539.183963	22.998498	65.415002
1538.588074	49.731207	65.420007
1537.678009	31.833329	65.425012
1536.974465	21.244536	65.430017
1535.749838	52.405657	65.435022
1535.816501	22.265891	65.440026
1535.575395	43.287572	65.445031
1534.692169	37.502075	65.450036
1533.897139	40.821583	65.455041
1532.917737	37.426132	65.460046
1532.884405	35.923958	65.465050
1531.555032	43.404580	65.470055
1530.945430	46.283061	65.475060
1530.478569	42.632704	65.480065
1530.055854	50.904333	65.485070
1529.816108	29.544365	65.490074
1528.532876	34.176141	65.495079
1527.766042	43.849095	65.500084
1527.309769	42.787849	65.505089
1526.332505	37.465130	65.510094
1525.622733	32.678615	65.515098
1524.618030	29.235154	65.520103
1524.466048	49.277637	65.525108
1524.189560	32.102206	65.530113
1523.481304	27.517291	65.535118
1522.661570	47.886650	65.540122
1521.944579	33.589623	65.545127
1521.472874	26.775273	65.550132
1520.744175	43.257379	65.555137
1519.742720	18.193003	65.560142
1518.863009	45.705626	65.565146
1518.359074	34.999957	65.570151
1517.905295	28.964884	65.575156
1517.946336	28.950490	65.580161
1516.648942	35.350611	65.585166
1515.935065	41.202289	65.590170
1515.130854	41.841012	65.595175
1514.942563	31.908309	65.600180
1513.573312	21.270786	65.605185
1512.713677	58.131050	65.610190
1512.608321	24.920077	65.615194
1512.132528	53.510174	65.620199
1511.471660	40.503563	65.625204
1511.465685	38.509790	65.630209
1510.271112	43.701466	65.635214
1509.586264	39.743578	65.640218
1508.370791	44.984306	65.645223
1507.452605	39.073496	65.650228
1507.152380	39.923846	65.655233
1506.348860	35.250000	65.660238
1506.269830	40.953482	65.665242
1506.182201	24.943315	65.670247
1505.094411	35.305905	65.675252
1504.275729	31.907002	65.680257
1503.456117	47.917889	65.685262
1502.554168	31.724911	65.690266
1501.471925	29.381820	65.695271
1500.688597	47.518862	65.700276
1500.723481	43.176948	65.705281
1500.111147	38.611483	65.710286
1500.039962	33.674605	65.715290
1499.178620	45.327359	65.720295
1497.995587	41.879133	65.725300
1497.744268	41.245765	65.730305
1497.246713	41.463617	65.735310
1496.391894	30.851568	65.740314
1495.484075	45.955584	65.745319
1495.067872	28.389231	65.750324
1493.907533	29.073521	65.755329
1493.072313	45.250881	65.760334
1492.938630	35.134469	65.765338
1492.173261	42.262135	65.770343
1491.649444	43.218981	65.775348
1491.241470	40.499088	65.780353
1490.073936	42.827617	65.785358
1489.698048	22.515850	65.790362
1489.102717	33.826716	65.795367
1487.990710	46.342435	65.800372
1487.220420	34.293044	65.805377
1486.742324	32.379037	65.810382
1486.368483	30.073167	65.815386
1486.101570	34.488247	65.820391
1484.905403	38.082821	65.825396
1484.480757	34.600800	65.830401
1483.638435	30.606452	65.835406
1483.035417	33.750383	65.840410
1481.962702	35.191839	65.845415
1481.291884	44.305523	65.850420
1481.139731	41.721582	65.855425
1480.255854	41.169828	65.860430
1479.983511	32.119343	65.865434
1478.831757	36.115268	65.870439
1477.957856	40.940618	65.875444
1477.758899	26.777313	65.880449
1477.250104	40.412922	65.885454
1476.382103	37.554846	65.890458
1475.590786	36.371828	65.895463
1474.841061	36.068399	65.900468
1474.770178	26.973284	65.905473
1473.724382	36.726849	65.910478
1473.233621	21.198635	65.915482
1472.694110	23.712765	65.920487
1471.873214	33.263436	65.925492
1470.724138	32.061592	65.930497
1469.689254	45.176881	65.935502
1469.761023	26.495405	65.940506
1469.047356	35.492901	65.945511
1468.424150	36.448203	65.950516
1468.171496	21.790420	65.955521
1466.874080	23.343284	65.960526
1466.425706	28.604019	65.965530
1466.250715	34.598700	65.970535
1464.995579	40.963746	65.975540
1464.362267	26.866327	65.980545
1463.609381	33.924206	65.985550
1463.324885	27.832281	65.990554
1462.802201	30.958717	65.995559
1461.630204	37.308971	66.000564
1460.863349	38.265030	66.005569
1460.117797	39.821643	66.010574
1460.116109	33.817222	66.015578
1459.444649	39.100805	66.020583
1458.338484	48.083429	66.025588
1457.851402	39.470753	66.030593
1457.232555	38.238252	66.035598
1456.918903	39.128586	66.040602
1455.826418	37.958753	66.045607
1455.256183	27.586905	66.050612
1454.930250	27.246083	66.055617
1453.684028	38.866981	66.060622
1452.856525	28.827744	66.065626
1451.879863	37.032885	66.070631
1451.584116	38.101713	66.075636
1451.585591	32.886800	66.080641
1450.852728	41.959890	66.085646
1450.480853	34.962539	66.090650
1449.497156	31.525232	66.095655
1449.026139	39.549085	66.100660
1448.393265	37.923023	66.105665
1446.989274	41.850251	66.110670
1446.628251	37.650112	66.115674
1446.185792	24.126307	66.120679
1444.964397	45.379481	66.125684
1444.221430	33.226424	66.130689
1443.582764	39.168657	66.135694
1443.276010	30.896314	66.140698
1442.897778	28.599034	66.145703
1441.878386	36.536595	66.150708
1441.300053	39.763340	66.155713
1440.697744	31.569512	66.160718
1440.684455	35.701445	66.165722
1439.620831	43.087830	66.170727
1438.635026	49.162512	66.175732
1438.092206	39.529008	66.180737
1437.643367	32.613277	66.185742
1436.731455	31.550361	66.190746
1435.619604	27.097431	66.195751
1434.883762	41.432991	66.200756
1434.602737	19.008941	66.205761
1434.102566	48.958995	66.210766
1433.689480	38.119068	66.215770
1432.457956	38.297488	66.220775
1432.079310	28.612668	66.225780
1431.727240	27.649989	66.230785
1430.943936	52.537594	66.235790
1430.158124	26.045038	66.240794
1428.912020	32.861220	66.245799
1428.705565	28.310106	66.250804
1428.517222	31.660931	66.255809
1427.569473	40.962136	66.260814
1427.095285	29.720368	66.265818
1426.197847	20.474390	66.270823
1425.614741	24.209643	66.275828
1424.503942	34.421382	66.280833
1423.279844	49.514191	66.285838
1423.476322	26.627899	66.290842
1422.738328	22.616993	66.295847
1422.226148	41.060998	66.300852
1422.275370	29.228283	66.305857
1421.083428	36.554648	66.310862
1420.139557	38.196409	66.315866
1419.933528	34.260204	66.320871
1418.892457	38.717927	66.325876
1418.061521	27.376762	66.330881
1417.149192	36.442114	66.335886
1416.987816	33.679883	66.340890
1416.725394	37.690577	66.345895
1415.791425	41.115776	66.350900
1415.161377	35.438309	66.355905
1414.299749	27.233677	66.360910
1413.479236	32.384851	66.365914
1412.553017	38.979892	66.370919
1411.745164	39.223432	66.375924
1411.779905	27.626397	66.380929
1411.036264	23.588008	66.385934
1410.468180	36.898746	66.390938
1409.610585	39.988550	66.395943
1408.476915	41.646294	66.400948
1408.534617	33.077916	66.405953
1408.150414	39.973131	66.410958
1407.261055	29.212081	66.415962
1406.387369	39.353023	66.420967
1405.631229	32.596530	66.425972
1405.004673	29.758445	66.430977
1403.910230	47.055602	66.435982
1403.403562	37.411632	66.440986
1403.091466	42.948744	66.445991
1402.391643	40.786165	66.450996
1402.048025	35.190897	66.456001
1400.995198	38.444193	66.461006
1400.195658	36.734258	66.466010
1399.537591	38.281711	66.471015
1399.395677	33.960023	66.476020
1398.470119	32.877213	66.481025
1397.231913	41.795692	66.486030
1397.076215	33.565573	66.491034
1396.921934	39.927527	66.496039
1396.042166	35.822475	66.501044
1395.173425	28.658134	66.506049
1394.381826	41.624385	66.511054
1393.971050	30.566501	66.516058
1392.895870	40.504525	66.521063
1391.878311	31.342302	66.526068
1391.415656	41.249184	66.531073
1390.915011	25.650031	66.536078
1390.710791	28.337945	66.541082
1390.486050	28.643328	66.546087
1389.061503	40.426631	66.551092
1388.530905	29.930238	66.556097
1387.935394	26.044917	66.561102
1387.468958	27.442066	66.566106
1386.432365	29.202651	66.571111
1385.679369	33.966229	66.576116
1385.586026	31.081229	66.581121
1384.445989	41.444282	66.586126
1383.571731	34.071098	66.591130
1383.023712	39.464376	66.596135
1382.310892	36.692046	66.601140
1382.336575	29.513248	66.606145
1381.547292	31.641350	66.611150
1380.560592	27.919138	66.616154
1380.070632	25.943966	66.621159
1379.418532	23.554625	66.626164
1378.715265	31.129728	66.631169
1377.486428	29.218405	66.636174
1377.069871	15.840314	66.641178
1376.573434	27.417723	66.646183
1376.282083	25.787849	66.651188
1375.739622	35.819372	66.656193
1374.419729	37.407393	66.661198
1374.109531	38.306648	66.666202
1373.425347	33.125053	66.671207
1372.192808	30.695532	66.676212
1372.069207	20.364670	66.681217
1371.145180	30.255012	66.686222
1370.325515	41.325609	66.691226
1370.138379	27.471092	66.696231
1369.513821	44.163727	66.701236
1368.766456	31.856869	66.706241
1368.099124	32.172695	66.711246
1367.688961	19.066385	66.716250
1366.562778	37.792491	66.721255
1365.616649	30.402358	66.726260
1365.539564	24.597581	66.731265
1364.928028	32.128143	66.736270
1364.075342	37.502054	66.741274
1363.271058	39.585241	66.746279
1362.834226	32.200869	66.751284
1362.250011	24.384218	66.756289
1361.584477	26.361772	66.761294
1360.752596	27.515844	66.766298
1359.917870	39.806174	66.771303
1359.633341	26.033373	66.776308
1358.996515	31.636301	66.781313
1357.950648	38.474293	66.786318
1357.522312	37.455944	66.791322
1356.994076	34.102375	66.796327
1356.365907	34.044569	66.801332
1355.340185	41.377650	66.806337
1354.362809	41.785346	66.811342
1354.154809	32.928072	66.816346
1353.818955	29.387811	66.821351
1352.486869	33.652139	66.826356
1351.873814	43.570321	66.831361
1351.386209	45.618934	66.836366
1350.861688	41.011168	66.841370
1350.704508	41.305813	66.846375
1349.321906	31.674975	66.851380
1348.908014	33.601487	66.856385
1348.022151	51.590858	66.861390
1348.004612	41.722490	66.866394
1346.911041	39.163660	66.871399
1345.935934	36.843025	66.876404
1345.509640	40.223802	66.881409
1344.914385	30.653860	66.886414
1344.661541	43.908183	66.891418
1343.693971	40.105676	66.896423
1342.591585	38.560595	66.901428
1342.474940	35.704532	66.906433
1341.977366	29.979222	66.911438
1341.029714	28.871563	66.916442
1340.058986	31.752304	66.921447
1339.456163	45.461217	66.926452
1339.299702	28.574251	66.931457
1338.103572	36.506829	66.936462
1337.594731	32.385403	66.941466
1337.046306	29.993782	66.946471
1336.551474	33.776517	66.951476
1335.779850	27.514495	66.956481
1334.560031	33.586988	66.961486
1334.309049	38.469450	66.966490
1334.012746	24.649646	66.971495
1333.315499	33.365449	66.976500
1332.562924	34.208894	66.981505
1331.699433	31.471574	66.986510
1331.156179	31.193704	66.991514
1330.137080	35.591197	66.996519
1328.965920	39.271743	67.001524
1328.917644	27.646918	67.006529
1328.411964	28.701830	67.011534
1328.002419	27.235825	67.016538
1327.432137	29.515192	67.021543
1326.343803	34.757854	67.026548
1325.840694	28.833167	67.031553
1325.125733	27.893510	67.036558
1324.557886	27.121264	67.041562
1323.472854	38.549432	67.046567
1322.798192	32.953201	67.051572
1322.563677	37.082458	67.056577
1322.106847	32.314137	67.061582
1321.242743	34.941403	67.066586
1320.783431	33.939024	67.071591
1319.833865	40.288660	67.076596
1319.701831	29.180172	67.081601
1318.267109	35.174884	67.086606
1317.458636	29.137911	67.091610
1317.207790	24.567065	67.096615
1316.462383	40.086806	67.101620
1315.740368	34.419262	67.106625
1314.569183	34.603913	67.111630
1314.161246	29.523487	67.116634
1314.089101	32.389090	67.121639
1313.349192	38.982920	67.126644
1313.340565	28.632206	67.131649
1311.987196	29.180120	67.136654
1311.321659	35.246490	67.141658
1310.884238	37.679768	67.146663
1309.849625	37.311305	67.151668
1309.036000	32.959241	67.156673
1308.639078	33.519076	67.161678
1307.953992	37.631671	67.166682
1306.948166	37.667038	67.171687
1306.407933	38.535072	67.176692
1305.788745	32.032792	67.181697
1305.404558	32.516490	67.186702
1304.883492	37.807728	67.191706
1304.063479	27.071970	67.196711
1303.005955	32.995675	67.201716
1302.723938	24.274758	67.206721
1302.464176	33.873429	67.211726
1301.388648	36.119604	67.216730
1300.735492	31.555960	67.221735
1299.948124	38.923694	67.226740
1299.362608	31.006347	67.231745
1298.246629	33.247917	67.236750
1297.403196	41.950708	67.241754
1296.788101	35.502968	67.246759
1296.605182	37.720750	67.251764
1296.484360	27.624407	67.256769
1295.934782	37.757990	67.261774
1294.903016	35.102630	67.266778
1294.333785	33.518526	67.271783
1293.271023	38.818633	67.276788
1292.363036	35.730454	67.281793
1291.612261	36.043799	67.286798
1291.136283	28.850164	67.291802
1290.860237	34.659075	67.296807
1290.414121	30.543457	67.301812
1289.986196	35.414633	67.306817
1289.074945	41.021791	67.311822
1288.356571	39.347869	67.316826
1287.243110	33.572278	67.321831
1286.092628	37.445084	67.326836
1285.769631	25.827682	67.331841
1285.336516	37.964284	67.336846
1284.774246	27.132361	67.341850
1284.653157	36.040395	67.346855
1283.506581	47.035269	67.351860
1283.105569	30.363810	67.356865
1282.428776	25.201571	67.361870
1281.691028	31.873904	67.366874
1280.825187	26.986138	67.371879
1279.757465	45.534254	67.376884
1279.464936	37.327485	67.381889
1279.351320	31.203689	67.386894
1278.189854	42.527339	67.391898
1277.757940	27.484968	67.396903
1276.782541	30.683422	67.401908
1276.404747	33.991843	67.406913
1274.850547	33.398527	67.411918
1274.240204	40.343902	67.416922
1274.154880	42.150375	67.421927
1273.797740	30.897926	67.426932
1273.893129	30.807081	67.431937
1272.335075	37.955192	67.436942
1271.337686	33.651285	67.441946
1270.991404	29.494566	67.446951
1270.523309	38.339515	67.451956
1269.534977	26.526735	67.456961
1268.783596	38.475841	67.461966
1268.095149	39.928814	67.466970
1267.910627	33.483575	67.471975
1266.967395	33.263014	67.476980
1266.406606	31.450507	67.481985
1265.852138	31.212279	67.486990
1265.116079	36.078844	67.491994
1264.363588	33.642423	67.496999
1263.490179	31.717212	67.502004
1263.038872	35.600264	67.507009
1262.619273	33.558737	67.512014
1261.552171	39.611709	67.517018
1260.827208	35.132029	67.522023
1259.993254	40.346881	67.527028
1259.937116	33.245753	67.532033
1259.357227	23.876816	67.537038
1258.362303	32.083336	67.542042
1257.875120	33.373427	67.547047
1257.074720	38.559290	67.552052
1256.435259	27.810610	67.557057
1255.487188	25.132498	67.562062
1254.726249	43.007394	67.567066
1254.294992	27.703167	67.572071
1253.669291	38.238345	67.577076
1253.529218	35.075372	67.582081
1252.585288	30.488600	67.587086
1251.568877	33.550092	67.592090
1251.404190	34.243305	67.597095
1250.531525	50.511811	67.602100
1250.168871	35.942523	67.607105
1249.204841	36.455363	67.612110
1248.434605	30.073310	67.617114
1248.002132	30.884798	67.622119
1246.915846	32.115629	67.627124
1246.197470	32.017005	67.632129
1245.500288	32.634059	67.637134
1245.131780	31.908974	67.642138
1244.909463	34.473625	67.647143
1243.925491	38.629034	67.652148
1243.290199	31.566395	67.657153
1242.643110	38.046137	67.662158
1242.148678	27.492006	67.667162
1241.517893	30.331336	67.672167
1240.453297	42.122113	67.677172
1240.028692	27.955326	67.682177
1239.204204	42.547846	67.687182
1238.489373	33.424284	67.692186
1237.511530	37.651255	67.697191
1236.770192	37.742355	67.702196
1236.979855	21.752776	67.707201
1236.071822	32.921020	67.712206
1235.198092	32.372469	67.717210
1234.819578	28.272919	67.722215
1233.949534	41.347860	67.727220
1233.374375	41.697945	67.732225
1232.310813	37.775141	67.737230
1231.876810	46.554756	67.742234
1231.739232	39.646341	67.747239
1230.630346	43.115186	67.752244
1229.553703	29.943022	67.757249
1229.009836	26.871076	67.762254
1228.560783	28.128300	67.767258
1228.501634	33.041755	67.772263
1227.540142	36.748919	67.777268
1226.813524	20.190770	67.782273
1225.872994	42.309174	67.787278
1225.500027	33.560155	67.792282
1225.134404	27.925849	67.797287
1223.610427	49.288700	67.802292
1223.212810	38.891047	67.807297
1223.098539	33.831742	67.812302
1221.948316	40.599649	67.817306
1221.419837	28.497730	67.822311
1220.201792	37.126079	67.827316
1220.310302	30.720974	67.832321
1219.747904	42.778800	67.837326
1218.878238	41.184149	67.842330
1218.192605	35.036218	67.847335
1217.375945	41.680121	67.852340
1217.148347	41.788865	67.857345
1216.043324	41.441098	67.862350
1215.218124	39.992333	67.867354
1214.641987	18.416342	67.872359
1214.218786	33.820194	67.877364
1213.904337	29.943835	67.882369
1212.458830	36.608903	67.887374
1211.848407	33.568044	67.892378
1211.518753	35.402337	67.897383
1210.966097	31.514978	67.902388
1210.376270	26.994904	67.907393
1209.324262	39.887488	67.912398
1208.539557	37.815733	67.917402
1208.510659	40.860529	67.922407
1207.138651	39.637494	67.927412
1206.281446	31.665621	67.932417
1205.905385	35.115691	67.937422
1205.389996	39.800527	67.942426
1205.176893	31.598491	67.947431
1204.659838	38.193169	67.952436
1203.762829	28.646037	67.957441
1202.984888	27.517748	67.962446
1202.253780	32.200623	67.967450
1202.062826	19.542019	67.972455
1200.727140	29.622446	67.977460
1200.445064	25.029777	67.982465
1199.745800	32.866037	67.987470
1198.832708	29.783439	67.992474
1198.354025	29.656168	67.997479
1197.237862	35.273865	68.002484
1196.904401	30.547450	68.007489
1196.873862	27.415947	68.012494
1195.429838	34.582228	68.017498
1195.462022	26.795320	68.022503
1194.226874	28.257994	68.027508
1193.530127	24.899731	68.032513
1192.542241	23.161478	68.037518
1192.027235	29.200773	68.042522
1191.747689	20.181462	68.047527
1190.983741	41.904376	68.052532
1190.686000	34.460080	68.057537
1189.503360	28.233523	68.062542
1188.879434	24.761183	68.067546
1188.980399	22.941211	68.072551
1187.901099	44.624405	68.077556
1187.164618	27.858112	68.082561
1186.290542	35.733217	68.087566
1185.956251	29.210894	68.092570
1185.092071	45.626280	68.097575
1184.115819	33.160374	68.102580
1183.406700	25.105040	68.107585
1183.126372	43.914270	68.112590
1182.898964	39.489514	68.117594
1182.084944	15.213949	68.122599
1180.731359	45.280772	68.127604
1180.281564	39.237260	68.132609
1180.013428	30.917832	68.137614
1179.119232	31.589891	68.142618
1178.379484	19.846430	68.147623
1177.578476	30.983471	68.152628
1177.086846	24.590249	68.157633
1176.826945	27.943003	68.162638
1176.016161	37.813810	68.167642
1175.619912	31.744440	68.172647
1174.711403	27.532091	68.177652
1173.813651	20.648412	68.182657
1172.951922	33.463430	68.187662
1172.185155	37.951724	68.192666
1172.004407	18.559891	68.197671
1171.406006	32.856270	68.202676
1170.685831	37.319808	68.207681
1169.666032	22.292141	68.212686
1169.329316	30.028165	68.217690
1168.966784	7.560426	68.222695
1167.668218	40.486793	68.227700
1167.490937	27.611563	68.232705
1166.643517	28.090117	68.237710
1165.944184	26.387975	68.242714
1165.272809	28.748105	68.247719
1164.359977	29.952959	68.252724
1163.766195	31.110219	68.257729
1163.467698	36.660949	68.262734
1162.819645	22.887680	68.267738
1161.658581	41.274054	68.272743
1161.194643	40.045373	68.277748
1160.777744	28.196948	68.282753
1160.405509	24.179988	68.287758
1159.032393	28.460393	68.292762
1158.767095	25.807753	68.297767
1157.848970	30.764797	68.302772
1157.531189	26.564145	68.307777
1156.263988	28.837710	68.312782
1155.437384	33.775468	68.317786
1155.200513	28.905972	68.322791
1154.566785	42.996683	68.327796
1154.458474	32.709146	68.332801
1153.894988	27.636151	68.337806
1152.599751	34.070777	68.342810
1152.416618	27.617453	68.347815
1151.121806	38.380491	68.352820
1150.005115	26.195553	68.357825
1149.487921	22.174847	68.362830
1148.862446	37.415346	68.367834
1148.921420	29.247309	68.372839
1148.286652	34.436813	68.377844
1147.986035	30.253930	68.382849
1147.417891	27.947489	68.387854
1146.392685	34.990409	68.392858
1145.431538	38.426326	68.397863
1144.220678	40.899082	68.402868
1143.786274	32.757487	68.407873
1143.232322	23.206278	68.412878
1142.827886	47.633097	68.417882
1142.869397	25.698701	68.422887
1141.660376	22.325751	68.427892
1140.990528	27.501912	68.432897
1140.140648	28.862330	68.437902
1139.370371	20.381531	68.442906
1138.677943	26.373365	68.447911
1138.122814	36.580382	68.452916
1137.734513	32.250608	68.457921
1137.193816	15.029037	68.462926
1136.177450	26.119919	68.467930
1135.585589	27.645865	68.472935
1134.661831	46.322490	68.477940
1134.435879	24.345493	68.482945
1133.147035	23.229113	68.487950
1132.370780	43.047569	68.492954
1132.258394	39.580599	68.497959
1131.619285	25.477932	68.502964
1131.366726	32.684940	68.507969
1130.633392	27.085492	68.512974
1129.808057	47.659193	68.517978
1129.426723	21.052027	68.522983
1127.905161	28.596504	68.527988
1127.604147	20.752226	68.532993
1126.881483	39.234439	68.537998
1126.582652	30.561958	68.543002
1125.446720	19.991649	68.548007
1124.375032	34.603002	68.553012
1124.201411	31.738674	68.558017
1124.108816	23.664135	68.563022
1123.252777	23.377722	68.568026
1122.284387	12.667235	68.573031
1121.678905	39.871326	68.578036
1121.249587	14.853399	68.583041
1120.366411	42.100091	68.588046
1119.266612	33.782090	68.593050
1118.800748	23.933042	68.598055
1118.311856	19.899958	68.603060
1118.084947	27.257415	68.608065
1117.472166	32.758799	68.613070
1116.015611	22.435026	68.618074
1115.653667	21.573308	68.623079
1114.989480	22.076344	68.628084
1114.544351	39.607717	68.633089
1113.704427	26.131477	68.638094
1112.543867	29.531320	68.643098
1112.407744	34.215757	68.648103
1112.171704	23.251580	68.653108
1111.095983	13.814927	68.658113
1110.432455	32.532139	68.663118
1109.874820	24.436966	68.668122
1109.324848	27.624569	68.673127
1108.493851	29.130219	68.678132
1107.789106	8.858313	68.683137
1107.229034	32.929839	68.688142
1106.440468	23.985210	68.693146
1106.070706	38.718286	68.698151
1104.692666	15.402917	68.703156
1104.352704	43.761609	68.708161
1104.067016	7.208208	68.713166
1103.246980	41.643203	68.718170
1102.565712	11.824413	68.723175
1101.334895	37.686732	68.728180
1101.120379	18.885305	68.733185
1100.780451	25.552732	68.738190
1100.087183	36.204326	68.743194
1099.456147	15.666815	68.748199
1098.501021	25.943769	68.753204
1097.836236	25.623786	68.758209
1096.928715	25.030200	68.763214
1095.981214	41.100904	68.768218
1095.631345	7.176880	68.773223
1095.220734	40.545436	68.778228
1094.682574	29.017500	68.783233
1094.697447	33.203281	68.788238
1093.360339	33.408122	68.793242
1092.821562	14.166309	68.798247
1092.151220	26.018968	68.803252
1091.356903	29.015225	68.808257
1090.808370	29.515638	68.813262
1089.546221	43.009356	68.818266
1089.801957	26.165684	68.823271
1088.680738	28.408173	68.828276
1087.621746	14.936846	68.833281
1087.136412	27.332473	68.838286
1086.536173	35.069429	68.843290
1086.255080	44.192135	68.848295
1085.136630	33.623787	68.853300
1084.995957	13.079236	68.858305
1084.326868	31.131898	68.863310
1083.403762	33.256146	68.868314
1082.833088	27.149896	68.873319
1082.062703	34.169643	68.878324
1081.463547	27.929161	68.883329
1080.641829	30.475645	68.888334
1079.591833	32.539661	68.893338
1079.370046	27.283024	68.898343
1078.592367	33.014063	68.903348
1078.297041	43.315369	68.908353
1077.762734	35.948151	68.913358
1076.499105	32.073018	68.918362
1076.290585	33.318808	68.923367
1075.379332	31.174195	68.928372
1074.449903	32.457410	68.933377
1073.635590	39.309118	68.938382
1073.079171	40.734829	68.943386
1072.889893	22.728858	68.948391
1072.426297	40.611654	68.953396
1071.680898	24.706227	68.958401
1070.781769	15.370802	68.963406
1069.671824	21.176775	68.968410
1069.590507	31.325761	68.973415
1069.331317	33.289199	68.978420
1068.365882	29.817611	68.983425
1067.645078	21.209127	68.988430
1066.987890	44.239627	68.993434
1066.019329	34.396451	68.998439
1065.030236	15.473858	69.003444
1064.653681	58.599347	69.008449
1064.856852	27.331044	69.013454
1063.801216	30.083473	69.018458
1062.973003	37.065120	69.023463
1062.225579	24.307429	69.028468
1061.753990	27.761674	69.033473
1061.391748	18.291951	69.038478
1059.902121	28.067364	69.043482
1059.498538	31.770972	69.048487
1058.976903	32.527293	69.053492
1058.202899	27.918300	69.058497
1057.299399	27.196364	69.063502
1056.275630	28.135070	69.068506
1056.096738	17.311620	69.073511
1055.824365	39.905597	69.078516
1055.494450	26.006065	69.083521
1054.329318	23.474526	69.088526
1053.283034	26.405231	69.093530
1053.088902	12.088319	69.098535
1052.623217	20.866665	69.103540
1051.682143	14.056162	69.108545
1050.847114	23.437287	69.113550
1050.491423	25.731450	69.118554
1049.973355	24.227571	69.123559
1048.811286	23.311824	69.128564
1047.943928	28.522583	69.133569
1047.826570	22.804664	69.138574
1047.286565	29.199595	69.143578
1046.564171	18.842640	69.148583
1045.404707	16.497850	69.153588
1044.782266	12.393000	69.158593
1044.372704	25.221244	69.163598
1043.896218	30.005562	69.168602
1043.836300	26.303187	69.173607
1042.620079	25.894346	69.178612
1041.985892	29.092207	69.183617
1041.058675	26.131760	69.188622
1040.349414	29.934464	69.193626
1039.862237	20.639155	69.198631
1039.285755	31.649043	69.203636
1038.058527	26.336354	69.208641
1037.557094	26.906550	69.213646
1036.888117	22.257203	69.218650
1036.623319	22.917474	69.223655
1036.156737	21.392792	69.228660
1034.980554	25.345475	69.233665
1034.333916	20.877067	69.238670
1033.614077	29.631207	69.243674
1033.593576	22.478708	69.248679
1032.531228	19.691144	69.253684
1031.365012	25.285327	69.258689
1031.057699	21.748465	69.263694
1030.621564	29.765226	69.268698
1030.428168	21.186375	69.273703
1029.300371	18.057588	69.278708
1028.418650	29.144424	69.283713
1028.104115	24.194272	69.288718
1027.228753	25.039995	69.293722
1026.542698	18.521642	69.298727
1025.454509	28.386153	69.303732
1025.202358	26.611324	69.308737
1024.928396	28.208130	69.313742
1023.847525	23.912889	69.318746
1023.116931	12.568564	69.323751
1022.405748	25.607217	69.328756
1021.971744	23.017706	69.333761
1021.505084	27.251716	69.338766
1020.314503	22.917166	69.343770
1020.078341	2.495067	69.348775
1019.543031	19.872040	69.353780
1018.896931	17.790911	69.358785
1018.117126	16.134732	69.363790
1017.314960	23.637333	69.368794
1016.719344	14.939572	69.373799
1015.444185	30.010652	69.378804
1014.558177	23.617150	69.383809
1014.385515	30.023019	69.388814
1013.885885	21.809845	69.393818
1013.773702	19.424580	69.398823
1013.157673	23.751739	69.403828
1012.229346	25.861072	69.408833
1011.602681	22.204727	69.413838
1011.111672	34.946599	69.418842
1009.973696	20.283160	69.423847
1009.260242	20.792486	69.428852
1008.673863	22.882101	69.433857
1008.367126	17.314163	69.438862
1007.026493	30.941805	69.443866
1006.639415	24.710177	69.448871
1005.944704	37.028752	69.453876
1005.734288	29.564293	69.458881
1004.980227	11.271354	69.463886
1003.538845	19.348723	69.468890
1003.111036	27.247472	69.473895
1002.317286	37.583931	69.478900
1002.314531	22.098079	69.483905
1001.997418	8.166582	69.488910
1000.727927	27.838023	69.493914
1000.130261	30.393032	69.498919
999.738810	19.690140	69.503924
999.220478	23.205444	69.508929
997.992210	28.672328	69.513934
997.196399	14.979414	69.518938
997.112741	11.429048	69.523943
996.260950	22.602581	69.528948
995.170093	32.547949	69.533953
995.021476	32.229432	69.538958
994.430606	40.597233	69.543962
994.233863	24.188249	69.548967
993.062946	26.891243	69.553972
991.966911	29.266952	69.558977
991.828699	19.987088	69.563982
990.663171	17.648020	69.568986
990.150148	30.478542	69.573991
989.590853	28.741554	69.578996
988.950716	20.930768	69.584001
988.254058	28.918029	69.589006
987.345192	25.286097	69.594010
986.751545	16.897095	69.599015
986.309243	24.582122	69.604020
986.089668	14.971454	69.609025
985.138004	21.815073	69.614030
984.118032	28.330540	69.619034
984.072263	19.302456	69.624039
982.687201	28.911466	69.629044
981.716336	27.181628	69.634049
981.411889	15.146649	69.639054
980.956839	22.393761	69.644058
980.681863	15.772166	69.649063
979.673298	34.102772	69.654068
978.797853	26.274242	69.659073
978.764893	18.855667	69.664078
978.023112	22.977353	69.669082
977.305137	34.298329	69.674087
976.069995	30.084424	69.679092
975.316840	24.885553	69.684097
975.268874	27.845072	69.689102
974.635326	33.021800	69.694106
973.492145	23.621178	69.699111
972.889456	25.316028	69.704116
972.324890	17.458534	69.709121
972.175848	22.148176	69.714126
970.818973	31.875702	69.719130
970.709505	24.811477	69.724135
969.818866	20.315690	69.729140
969.123121	34.484083	69.734145
968.292611	19.238766	69.739150
967.471057	24.423335	69.744154
967.303747	31.462247	69.749159
966.321171	9.944757	69.754164
965.959988	23.982634	69.759169
964.901444	14.997458	69.764174
964.367462	23.267897	69.769178
964.243559	9.657301	69.774183
963.522580	25.021802	69.779188
962.012668	30.686478	69.784193
961.730865	25.814701	69.789198
961.207747	25.060651	69.794202
960.849212	9.150496	69.799207
959.710661	26.899425	69.804212
958.929931	27.160867	69.809217
958.849466	21.897529	69.814222
957.973096	13.821595	69.819226
957.250835	43.537272	69.824231
956.404777	39.602058	69.829236
955.525664	27.054591	69.834241
955.414889	29.405977	69.839246
954.378482	30.261585	69.844250
953.683909	24.851562	69.849255
952.939649	21.195026	69.854260
952.446442	22.752617	69.859265
952.127616	27.663234	69.864270
951.720065	34.768763	69.869274
950.826287	33.364117	69.874279
950.391257	27.734605	69.879284
949.013458	21.912952	69.884289
948.311654	33.679185	69.889294
947.508450	28.545055	69.894298
947.245531	24.149640	69.899303
946.521805	25.274015	69.904308
946.287401	29.581454	69.909313
945.794512	21.425571	69.914318
944.614883	33.635254	69.919322
944.406377	20.952692	69.924327
943.281197	19.884478	69.929332
942.111162	27.477179	69.934337
942.059120	30.449961	69.939342
941.315436	31.579091	69.944346
940.976769	34.460302	69.949351
940.089570	44.202984	69.954356
939.154087	38.137483	69.959361
938.613085	29.393204	69.964366
938.236466	36.651498	69.969370
937.494896	18.544241	69.974375
936.430502	28.646253	69.979380
935.866683	46.456700	69.984385
935.836382	39.353067	69.989390
934.685179	37.043280	69.994394
933.989942	30.321424	69.999399
933.071505	33.711194	70.004404
932.696534	47.762326	70.009409
932.457831	24.637897	70.014414
931.448228	32.720704	70.019418
930.761608	20.998851	70.024423
930.040419	27.679661	70.029428
929.437603	41.598325	70.034433
929.409050	34.319385	70.039438
928.313112	31.146152	70.044442
927.802374	29.745205	70.049447
926.648089	37.150918	70.054452
925.447593	34.275006	70.059457
924.741059	34.237663	70.064462
924.270394	34.539649	70.069466
923.909941	29.719816	70.074471
923.316437	23.390181	70.079476
922.937308	38.222508	70.084481
922.956264	36.805065	70.089486
922.310837	37.489658	70.094490
921.369068	27.544529	70.099495
920.092671	34.097677	70.104500
919.201875	33.433690	70.109505
919.025941	30.768435	70.114510
918.374538	39.300411	70.119514
917.792664	32.685089	70.124519
916.700434	41.951082	70.129524
915.794483	34.630446	70.134529
915.832159	28.323351	70.139534
915.192152	51.734304	70.144538
914.436551	39.018965	70.149543
913.314352	31.958239	70.154548
912.797051	49.854322	70.159553
912.804359	29.018179	70.164558
911.413535	37.333545	70.169562
910.752516	39.487098	70.174567
910.411608	35.995021	70.179572
909.784526	39.861945	70.184577
909.482154	28.640300	70.189582
908.129977	26.635310	70.194586
907.871028	18.814345	70.199591
907.312414	36.325926	70.204596
906.172010	39.643808	70.209601
905.698521	31.965784	70.214606
905.106262	32.520502	70.219610
904.923465	34.104387	70.224615
903.864556	31.339984	70.229620
902.825938	25.022855	70.234625
902.479919	25.599879	70.239630
901.554730	41.394273	70.244634
900.530618	29.185280	70.249639
899.790858	32.125603	70.254644
899.142238	32.873784	70.259649
899.327939	25.884006	70.264654
898.693159	39.020907	70.269658
898.285730	47.417872	70.274663
897.253386	41.542836	70.279668
896.428229	42.951435	70.284673
896.234764	29.832847	70.289678
894.697825	37.430355	70.294682
894.085445	29.014398	70.299687
893.847663	42.282069	70.304692
893.522352	41.165409	70.309697
892.702264	36.163286	70.314702
891.448892	31.709492	70.319706
891.127712	30.519641	70.324711
890.987471	35.594216	70.329716
889.773447	43.193947	70.334721
889.302819	31.270578	70.339726
888.583943	36.013078	70.344730
888.178883	37.160862	70.349735
887.028336	37.560031	70.354740
886.199468	29.862888	70.359745
886.194004	29.616205	70.364750
885.303576	34.907949	70.369754
884.578848	37.432748	70.374759
883.452208	47.360205	70.379764
882.949404	40.987754	70.384769
882.576860	34.892599	70.389774
881.875856	42.256145	70.394778
881.348929	34.151420	70.399783
880.134970	40.548003	70.404788
879.940451	34.003492	70.409793
879.797000	30.372767	70.414798
878.930735	39.878754	70.419802
877.731586	34.984278	70.424807
877.290766	28.603545	70.429812
876.703498	42.783075	70.434817
876.015360	28.227871	70.439822
874.790945	30.775440	70.444826
874.344396	28.150111	70.449831
874.073732	29.531954	70.454836
873.490250	30.583567	70.459841
872.991567	40.256538	70.464846
871.991451	36.484641	70.469850
871.412418	23.399053	70.474855
870.798740	39.342551	70.479860
870.168597	40.712233	70.484865
869.286594	29.693238	70.489870
868.641554	35.119383	70.494874
868.344008	25.374495	70.499879
867.661392	32.161136	70.504884
866.613238	33.304060	70.509889
866.198827	35.132959	70.514894
865.288858	41.824915	70.519898
864.865602	33.594891	70.524903
863.885374	40.537713	70.529908
863.198218	40.651834	70.534913
863.033427	32.330210	70.539918
862.121961	30.206213	70.544922
861.159961	30.556459	70.549927
860.721980	32.307114	70.554932
860.528378	31.827043	70.559937
860.096702	20.323243	70.564942
858.990016	37.373323	70.569946
858.023015	19.399753	70.574951
857.754202	24.201496	70.579956
856.416982	42.306925	70.584961
855.719750	23.166113	70.589966
855.044410	27.668315	70.594970
854.595855	23.240966	70.599975
854.217369	37.382528	70.604980
853.614342	27.424510	70.609985
852.742967	20.226131	70.614990
851.856735	20.728313	70.619994
851.803902	31.741593	70.624999
851.609150	47.842330	70.630004
850.044881	25.988578	70.635009
849.408976	42.410252	70.640014
848.994644	30.615122	70.645018
848.390142	37.745704	70.650023
847.291483	40.307960	70.655028
846.352335	27.188244	70.660033
846.033598	43.452205	70.665038
845.454952	32.419622	70.670042
845.523227	34.059732	70.675047
844.444813	28.210982	70.680052
843.337937	39.567083	70.685057
843.388704	28.216706	70.690062
842.293396	35.643023	70.695066
841.095374	40.647876	70.700071
840.851001	30.697420	70.705076
840.281502	34.241397	70.710081
839.895140	22.096493	70.715086
839.143242	37.754508	70.720090
838.438815	38.295559	70.725095
838.000009	32.762861	70.730100
837.077942	30.905473	70.735105
835.939298	34.920072	70.740110
834.900718	34.276486	70.745114
834.760293	34.778216	70.750119
834.819683	31.350156	70.755124
834.091472	30.917345	70.760129
832.986424	26.048914	70.765134
832.292399	24.461137	70.770138
831.802122	36.442860	70.775143
831.247837	37.984967	70.780148
830.059772	39.164370	70.785153
829.910179	21.459636	70.790158
829.009637	32.757661	70.795162
828.640015	33.574980	70.800167
827.963230	26.889646	70.805172
826.774530	41.421946	70.810177
826.481212	37.761468	70.815182
826.126355	43.381112	70.820186
825.012778	30.544621	70.825191
824.196572	21.528821	70.830196
823.435825	30.970713	70.835201
823.261830	41.609072	70.840206
822.817777	44.101822	70.845210
821.785345	45.409409	70.850215
821.125593	30.253658	70.855220
820.575718	32.588221	70.860225
820.176562	25.098652	70.865230
818.902244	43.523643	70.870234
818.607112	42.637141	70.875239
817.951131	35.372943	70.880244
817.319703	35.359942	70.885249
816.632848	42.782745	70.890254
816.024849	31.972451	70.895258
815.294452	28.832537	70.900263
814.420199	30.075523	70.905268
813.469558	38.421778	70.910273
813.269207	28.517934	70.915278
812.705499	40.747880	70.920282
811.968800	36.073113	70.925287
811.186505	30.117318	70.930292
810.164560	28.015660	70.935297
810.155793	22.901760	70.940302
809.489128	31.887159	70.945306
808.613139	33.348029	70.950311
807.962498	23.006551	70.955316
807.069909	20.004418	70.960321
806.915750	22.840499	70.965326
805.918054	49.477864	70.970330
805.016420	26.868995	70.975335
804.210453	30.917372	70.980340
803.788603	46.775154	70.985345
804.040553	7.113490	70.990350
803.170993	53.206151	70.995354
802.390304	28.846640	71.000359
801.302197	14.752524	71.005364
800.104221	39.989976	71.010369
799.511291	11.399868	71.015374
799.074281	42.842504	71.020378
798.338625	24.355923	71.025383
798.806236	35.666366	71.030388
797.349529	43.115547	71.035393
796.570553	23.618794	71.040398
796.041133	22.269733	71.045402
795.709849	29.326863	71.050407
794.919205	38.633185	71.055412
793.470995	55.490108	71.060417
793.324237	21.213771	71.065422
792.824834	32.421135	71.070426
792.292208	29.779566	71.075431
791.066697	47.479332	71.080436
790.063033	22.847851	71.085441
789.907003	33.484919	71.090446
789.427031	37.489286	71.095450
789.056890	45.427764	71.100455
788.924519	10.344969	71.105460
787.540247	37.813362	71.110465
787.027672	31.978627	71.115470
786.224879	35.083547	71.120474
785.215272	35.558088	71.125479
784.866246	27.568567	71.130484
784.199246	31.079194	71.135489
783.892710	21.665321	71.140494
782.461175	35.652855	71.145498
781.761899	26.369312	71.150503
781.714814	28.708984	71.155508
780.997520	24.513660	71.160513
780.018547	31.707023	71.165518
779.318108	34.078181	71.170522
778.595764	30.148570	71.175527
778.520275	29.857846	71.180532
777.616498	23.121944	71.185537
777.227798	43.184638	71.190542
776.395193	33.535990	71.195546
776.038421	33.614880	71.200551
774.941319	23.601521	71.205556
773.736010	39.317542	71.210561
773.410712	28.746090	71.215566
773.020803	42.017475	71.220570
772.748090	36.937711	71.225575
771.614900	18.697358	71.230580
770.497161	41.241396	71.235585
770.896954	13.224907	71.240590
769.334990	23.865049	71.245594
768.347373	36.878377	71.250599
768.072139	8.480547	71.255604
767.506899	57.870840	71.260609
767.430152	10.129674	71.265614
766.806547	33.178463	71.270618
765.987371	40.306972	71.275623
765.145679	19.848884	71.280628
764.301556	41.343330	71.285633
763.140606	12.205051	71.290638
762.382774	17.746933	71.295642
762.007185	34.053045	71.300647
762.013011	31.516552	71.305652
761.624546	35.244596	71.310657
761.080920	26.008814	71.315662
759.687512	20.850463	71.320666
759.078706	38.806831	71.325671
758.452801	30.842475	71.330676
757.348738	29.126051	71.335681
756.987312	22.757940	71.340686
756.309801	42.403021	71.345690
755.998070	26.149592	71.350695
755.074579	32.235064	71.355700
754.185261	38.384479	71.360705
753.659240	17.328973	71.365710
753.491068	40.254801	71.370714
752.323721	13.549054	71.375719
751.575136	33.555500	71.380724
751.161768	21.996780	71.385729
750.656212	27.951058	71.390734
750.180983	20.043140	71.395738
749.270660	19.812804	71.400743
748.722708	39.419907	71.405748
747.760045	14.851321	71.410753
746.826673	42.164366	71.415758
746.261734	3.613600	71.420762
745.393810	50.238956	71.425767
745.183412	6.357158	71.430772
744.741097	27.582618	71.435777
744.081740	33.386357	71.440782
743.135442	37.133841	71.445786
742.573809	29.381594	71.450791
742.321950	32.285271	71.455796
741.020239	31.623702	71.460801
740.299408	19.543122	71.465806
739.363145	38.973949	71.470810
739.140047	27.922639	71.475815
739.052671	25.933963	71.480820
738.177957	38.495689	71.485825
737.089961	27.493790	71.490830
736.572151	29.884761	71.495834
736.099079	32.356913	71.500839
735.584994	14.303422	71.505844
734.633205	37.565311	71.510849
733.983108	17.073585	71.515854
733.395927	29.583214	71.520858
732.826670	29.744826	71.525863
731.844209	19.307990	71.530868
731.144995	30.072540	71.535873
730.679623	36.947614	71.540878
729.654728	26.668908	71.545882
728.902820	22.286737	71.550887
728.610744	26.939237	71.555892
728.181182	32.624393	71.560897
727.970006	24.513595	71.565902
726.852500	17.633565	71.570906
726.385448	29.543786	71.575911
725.873086	37.314110	71.580916
724.626671	30.840930	71.585921
724.170070	13.355419	71.590926
723.480979	29.817093	71.595930
722.788625	30.253758	71.600935
721.598188	14.266418	71.605940
720.973105	25.063314	71.610945
720.919351	26.435862	71.615950
719.915061	36.868975	71.620954
719.637372	33.324291	71.625959
718.566107	15.706433	71.630964
717.651366	44.700593	71.635969
717.260113	10.900035	71.640974
716.953827	30.952738	71.645978
716.562381	41.860668	71.650983
715.543954	24.414150	71.655988
714.862523	28.102120	71.660993
714.434443	30.373158	71.665998
713.468055	35.267068	71.671002
712.289766	15.803995	71.676007
712.283839	39.708431	71.681012
711.805529	44.078376	71.686017
711.214194	23.548911	71.691022
710.034321	29.955901	71.696026
709.519025	28.694490	71.701031
709.071838	40.204191	71.706036
708.075172	24.414637	71.711041
707.354283	23.796206	71.716046
706.802190	25.257569	71.721050
706.549447	32.068825	71.726055
705.855176	34.308141	71.731060
704.393463	32.355398	71.736065
703.959117	24.433096	71.741070
703.432163	12.498272	71.746074
702.905499	30.968220	71.751079
702.520000	25.524834	71.756084
701.360164	38.694906	71.761089
701.081551	32.908088	71.766094
700.669903	30.086438	71.771098
699.762036	24.174336	71.776103
698.798166	32.812869	71.781108
697.998171	16.436960	71.786113
697.911682	21.780496	71.791118
697.020412	33.925422	71.796122
696.044098	28.142484	71.801127
695.459841	20.433280	71.806132
694.657673	36.983930	71.811137
694.469581	34.684885	71.816142
694.119738	28.296018	71.821146
692.963956	21.865195	71.826151
692.283335	22.030358	71.831156
691.624958	34.138198	71.836161
691.336307	46.057869	71.841166
690.002674	25.436897	71.846170
689.368876	42.257189	71.851175
689.104562	30.878158	71.856180
688.539608	14.936305	71.861185
687.943553	41.186452	71.866190
686.698441	29.572551	71.871194
686.190830	29.137769	71.876199
686.007563	47.915729	71.881204
685.248238	15.671801	71.886209
684.501903	31.592276	71.891214
683.860348	41.702728	71.896218
683.478338	29.823658	71.901223
682.635576	31.517383	71.906228
681.740099	42.787837	71.911233
681.626939	34.287719	71.916238
680.338927	19.927480	71.921242
679.240443	36.630968	71.926247
679.157126	16.219311	71.931252
678.361825	34.845577	71.936257
678.192184	35.459193	71.941262
677.067972	13.470881	71.946266
676.240660	49.783478	71.951271
675.837828	13.985330	71.956276
675.223958	30.312036	71.961281
674.801655	15.388192	71.966286
673.422714	30.367112	71.971290
672.718044	36.288462	71.976295
672.798688	17.820180	71.981300
672.020529	41.361918	71.986305
671.558099	25.586648	71.991310
670.689765	20.508726	71.996314
669.991876	35.909016	72.001319
669.344642	31.297319	72.006324
668.234481	12.797924	72.011329
667.596592	5.138277	72.016334
666.887727	49.525969	72.021338
666.333430	22.514498	72.026343
666.715609	9.638598	72.031348
665.692861	54.814258	72.036353
664.839750	24.261455	72.041358
663.909723	31.330372	72.046362
662.810348	42.185476	72.051367
662.426915	-1.974602	72.056372
661.586737	41.632940	72.061377
661.044775	25.562853	72.066382
660.944423	29.748038	72.071386
660.256098	49.232440	72.076391
659.409250	19.109134	72.081396
658.811329	26.180350	72.086401
658.155023	31.696633	72.091406
657.154703	20.789623	72.096410
656.137680	37.667790	72.101415
656.020463	25.483227	72.106420
655.316724	35.064299	72.111425
655.251629	-0.598366	72.116430
654.158314	41.876315	72.121434
653.282512	17.454792	72.126439
652.836135	44.046935	72.131444
652.308815	30.508515	72.136449
650.963555	41.662962	72.141454
650.536513	13.074897	72.146458
649.735670	44.050363	72.151463
649.954175	7.812691	72.156468
648.908149	53.920817	72.161473
648.126196	52.589929	72.166478
647.371873	21.732845	72.171482
646.893483	3.143898	72.176487
646.204906	53.944560	72.181492
645.125110	36.586685	72.186497
644.187115	32.505396	72.191502
644.162437	10.830821	72.196506
643.918064	-1.029135	72.201511
643.072628	24.820758	72.206516
641.913181	32.009793	72.211521
641.886419	4.862314	72.216526
641.145866	46.907115	72.221530
639.925903	63.199510	72.226535
638.921268	29.446181	72.231540
638.745039	3.126704	72.236545
638.530262	26.583423	72.241550
637.690163	20.971197	72.246554
637.093294	29.060895	72.251559
636.698685	21.681027	72.256564
635.762896	41.472896	72.261569
634.534812	26.991180	72.266574
634.455235	5.893024	72.271578
633.850043	40.177083	72.276583
633.052785	9.151843	72.281588
631.885253	28.722002	72.286593
631.632155	31.348358	72.291598
631.178129	22.782702	72.296602
630.498414	25.749799	72.301607
629.521127	25.877078	72.306612
628.812570	23.241494	72.311617
628.276509	23.093511	72.316622
627.888059	34.778348	72.321626
626.703691	23.211582	72.326631
626.321341	31.825321	72.331636
625.433897	25.324987	72.336641
625.226830	22.335160	72.341646
624.388623	31.243839	72.346650
623.535056	25.214320	72.351655
622.959006	25.277697	72.356660
622.220838	34.272940	72.361665
621.652532	15.214216	72.366670
620.647493	25.434595	72.371674
619.922061	34.877212	72.376679
619.904532	20.872866	72.381684
619.569566	27.993665	72.386689
618.097317	27.403474	72.391694
618.028288	26.093082	72.396698
617.327935	22.213638	72.401703
616.522465	27.208096	72.406708
615.421104	31.795550	72.411713
614.924476	26.224812	72.416718
614.237642	37.637076	72.421722
613.875065	28.672105	72.426727
612.971719	25.435234	72.431732
611.736536	47.916023	72.436737
611.381155	8.335387	72.441742
611.261461	36.950609	72.446746
610.694774	21.674486	72.451751
610.536737	18.396174	72.456756
609.180118	28.901199	72.461761
608.649519	42.786313	72.466766
608.263348	20.284697	72.471770
606.821440	18.291017	72.476775
606.399498	24.109000	72.481780
606.040882	36.295256	72.486785
604.885711	25.162215	72.491790
604.305559	29.097414	72.496794
603.923222	16.832101	72.501799
603.513354	30.258033	72.506804
602.886536	42.042341	72.511809
601.811467	22.987066	72.516814
601.032492	27.423834	72.521818
600.153580	43.997766	72.526823
600.257976	28.928543	72.531828
599.098408	17.138667	72.536833
598.451951	34.057160	72.541838
598.075126	23.326817	72.546842
597.307062	30.984927	72.551847
596.384495	20.062411	72.556852
595.360732	40.448578	72.561857
595.331691	21.709212	72.566862
594.789427	21.302044	72.571866
594.153096	29.071627	72.576871
593.053564	31.167377	72.581876
592.681697	30.204824	72.586881
592.210127	6.516857	72.591886
591.519266	46.391876	72.596890
590.337606	25.049805	72.601895
589.841189	14.370058	72.606900
588.962425	38.225843	72.611905
588.860952	25.701339	72.616910
588.400803	34.031026	72.621914
587.064542	17.726399	72.626919
586.721333	25.133921	72.631924
586.080939	39.116940	72.636929
585.501934	13.090265	72.641934
584.386955	36.233094	72.646938
583.652869	44.292629	72.651943
583.493193	27.524631	72.656948
583.024790	23.737553	72.661953
581.830291	24.429271	72.666958
581.407552	37.737420	72.671962
580.255749	25.523715	72.676967
580.660638	18.544756	72.681972
579.431006	28.132341	72.686977
578.449891	30.928278	72.691982
578.105239	17.138465	72.696986
577.438182	14.890500	72.701991
577.320039	30.102259	72.706996
575.936070	8.609535	72.712001
575.320962	33.656410	72.717006
574.744832	21.831952	72.722010
574.186194	38.965106	72.727015
573.492434	13.122286	72.732020
572.274874	29.166716	72.737025
572.126111	30.391984	72.742030
571.797093	2.797547	72.747034
570.981476	38.368704	72.752039
570.208813	3.935182	72.757044
569.256366	37.337894	72.762049
569.237967	7.415424	72.767054
568.231113	44.393644	72.772058
567.060120	7.205738	72.777063
566.965584	35.955701	72.782068
566.286177	15.534955	72.787073
565.455220	47.286301	72.792078
564.812928	8.844150	72.797082
563.517129	43.733347	72.802087
563.500553	13.515704	72.807092
563.209513	33.159140	72.812097
562.730396	33.391582	72.817102
561.965563	-6.669351	72.822106
560.971112	44.869059	72.827111
560.141926	39.482184	72.832116
558.719778	23.121871	72.837121
558.644068	4.870908	72.842126
558.383082	45.535246	72.847130
557.654269	34.730098	72.852135
557.794729	30.283099	72.857140
556.305575	14.442793	72.862145
555.588278	30.566801	72.867150
555.316086	9.355852	72.872154
553.852914	44.142411	72.877159
553.085214	9.736480	72.882164
552.781224	20.693543	72.887169
552.001310	33.144014	72.892174
552.184181	23.574965	72.897178
551.125912	19.121821	72.902183
550.296569	20.226862	72.907188
549.425243	34.431159	72.912193
549.558261	21.531865	72.917198
548.793331	13.772652	72.922202
547.701065	28.835254	72.927207
547.395847	13.331445	72.932212
546.078504	35.525719	72.937217
545.538468	14.797373	72.942222
544.915280	14.095623	72.947226
544.687597	27.747980	72.952231
544.445734	24.689593	72.957236
543.061624	39.663090	72.962241
542.326105	5.879636	72.967246
542.025717	38.522508	72.972250
541.244133	35.116465	72.977255
540.075551	4.497358	72.982260
538.754648	37.123037	72.987265
538.682725	23.010681	72.992270
538.836546	26.627130	72.997274
538.029136	30.346249	73.002279
537.312364	17.484571	73.007284
536.240275	37.846907	73.012289
535.669623	29.069633	73.017294
535.520765	30.499908	73.022298
534.632801	22.009716	73.027303
533.739158	25.827722	73.032308
533.395767	38.643871	73.037313
532.684431	16.351778	73.042318
531.535489	34.939787	73.047322
530.640306	25.107270	73.052327
530.720449	25.767829	73.057332
529.869302	20.677765	73.062337
529.439887	13.544730	73.067342
528.351848	37.224138	73.072346
527.639622	12.625266	73.077351
527.542677	43.827612	73.082356
526.931258	25.422293	73.087361
526.211031	43.757525	73.092366
525.376357	10.056097	73.097370
524.609797	53.024339	73.102375
523.519090	11.815316	73.107380
522.537037	51.146986	73.112385
522.086772	27.597539	73.117390
522.123877	12.151160	73.122394
521.298177	52.358303	73.127399
520.955894	21.657996	73.132404
520.174057	20.054340	73.137409
519.614408	7.030463	73.142414
519.104240	10.199214	73.147418
517.734381	39.701088	73.152423
516.845197	59.108708	73.157428
516.355210	58.817799	73.162433
515.806829	57.077606	73.167438
515.850826	54.593378	73.172442
514.701742	63.759774	73.177447
514.093615	40.456218	73.182452
513.170166	21.892476	73.187457
512.957344	3.251813	73.192462
512.147755	48.696234	73.197466
511.130386	34.493238	73.202471
511.025461	-1.036872	73.207476
510.384945	40.774346	73.212481
509.146923	44.341322	73.217486
508.818630	-2.579040	73.222490
508.108410	9.362033	73.227495
507.947573	-4.267802	73.232500
506.597410	22.662224	73.237505
505.425738	41.537701	73.242510
505.561805	-0.678793	73.247514
505.141834	35.892112	73.252519
503.983322	27.456072	73.257524
503.557146	4.457883	73.262529
502.865821	5.058435	73.267534
502.600762	37.260457	73.272538
501.208314	65.521852	73.277543
500.763342	50.076551	73.282548
500.017226	30.249881	73.287553
499.559971	12.482305	73.292558
498.448625	60.754815	73.297562
497.476185	20.514058	73.302567
497.606751	30.963531	73.307572
496.829043	40.556420	73.312577
496.802359	7.205650	73.317582
495.911033	34.994514	73.322586
494.596159	54.209772	73.327591
494.242902	35.320230	73.332596
493.409624	33.070386	73.337601
492.670138	9.420414	73.342606
492.409567	4.059672	73.347610
491.570565	56.071626	73.352615
491.051459	28.605226	73.357620
490.129052	37.035379	73.362625
489.337692	24.272326	73.367630
488.927501	36.244464	73.372634
488.394742	29.481111	73.377639
488.028640	9.141375	73.382644
486.988849	35.350243	73.387649
486.201555	26.307903	73.392654
485.825771	23.110023	73.397658
484.613427	38.611225	73.402663
484.476969	10.256052	73.407668
483.417569	58.827764	73.412673
482.955302	10.563170	73.417678
482.515316	38.152406	73.422682
481.364452	19.661187	73.427687
480.653033	41.027290	73.432692
480.617299	21.398098	73.437697
479.754087	44.928172	73.442702
478.890952	-0.615521	73.447706
478.151963	47.766340	73.452711
477.814183	38.745409	73.457716
477.655036	6.601543	73.462721
476.514517	37.769873	73.467726
475.896759	5.932453	73.472730
475.093340	50.976950	73.477735
474.199716	24.584153	73.482740
473.397140	6.792772	73.487745
472.443865	51.093222	73.492750
472.449248	13.503499	73.497754
471.698695	52.366230	73.502759
471.767602	7.191221	73.507764
470.313493	48.085058	73.512769
469.655715	10.432284	73.517774
469.232080	39.170011	73.522778
468.224115	9.988674	73.527783
467.316627	49.002548	73.532788
466.290973	24.478859	73.537793
466.552375	9.040906	73.542798
466.440451	23.586226	73.547802
465.535288	48.013909	73.552807
464.770099	15.523497	73.557812
464.538893	8.852452	73.562817
462.833949	38.341498	73.567822
462.481517	6.020293	73.572826
461.399312	36.452406	73.577831
461.351293	10.820556	73.582836
460.435195	32.167225	73.587841
459.962988	22.489684	73.592846
459.223352	11.667396	73.597850
458.807999	32.831784	73.602855
458.152058	22.035575	73.607860
456.757929	16.600003	73.612865
456.152652	37.411486	73.617870
456.394925	13.986693	73.622874
455.602554	23.995050	73.627879
454.704758	22.594384	73.632884
453.729790	33.470723	73.637889
452.949132	24.523528	73.642894
453.108203	26.190151	73.647898
451.314552	21.619278	73.652903
451.054417	16.953857	73.657908
450.375835	31.903267	73.662913
449.895352	42.207270	73.667918
449.522518	29.771755	73.672922
448.889916	16.928242	73.677927
447.920417	39.281574	73.682932
447.377370	6.495618	73.687937
446.625770	40.995356	73.692942
445.434621	16.300960	73.697946
445.060433	33.023125	73.702951
444.450999	1.113450	73.707956
444.049506	50.592630	73.712961
443.384536	14.191452	73.717966
443.140189	39.802109	73.722970
442.082649	20.785145	73.727975
441.771762	37.642298	73.732980
440.857207	13.760065	73.737985
439.607486	26.182916	73.742990
439.084362	21.127346	73.747994
438.513212	18.667033	73.752999
438.695219	20.027245	73.758004
437.575636	16.277737	73.763009
436.744724	23.293080	73.768014
436.136513	17.907318	73.773018
435.215379	34.831748	73.778023
434.268487	31.699650	73.783028
433.537660	21.290672	73.788033
433.278492	34.911779	73.793038
433.190325	22.118699	73.798042
432.623261	34.434357	73.803047
431.827748	38.336104	73.808052
430.783826	11.136311	73.813057
430.067519	30.462745	73.818062
429.463502	31.079366	73.823066
428.508305	18.433911	73.828071
427.787666	22.183384	73.833076
427.561964	40.512353	73.838081
427.373116	26.391840	73.843086
426.233924	25.414401	73.848090
425.176563	30.955217	73.853095
425.222794	23.811060	73.858100
424.302610	29.560236	73.863105
423.297306	22.723982	73.868110
422.925810	32.996422	73.873114
422.146294	27.519695	73.878119
421.782711	12.268060	73.883124
420.524123	22.391713	73.888129
419.667385	21.921163	73.893134
419.604125	19.413035	73.898138
419.080639	24.873508	73.903143
418.728972	26.047543	73.908148
417.714092	38.707361	73.913153
416.747136	8.310089	73.918158
416.394924	36.167580	73.923162
415.412242	30.844647	73.928167
414.728510	4.631352	73.933172
414.039466	41.863251	73.938177
413.794331	26.892329	73.943182
413.272517	7.698574	73.948186
412.086922	40.285374	73.953191
411.466548	3.033526	73.958196
410.963278	27.149571	73.963201
410.993317	24.837872	73.968206
409.949749	-0.184317	73.973210
408.970100	34.280785	73.978215
408.340456	20.943260	73.983220
407.194336	9.786830	73.988225
406.758778	26.107208	73.993230
406.082400	29.439656	73.998234
405.246732	35.342518	74.003239
405.340342	27.790290	74.008244
404.894330	15.650294	74.013249
403.701355	25.066535	74.018254
403.171067	29.851629	74.023258
402.729995	38.545701	74.028263
401.672427	24.989382	74.033268
400.699937	31.465944	74.038273
400.242398	23.276201	74.043278
399.971544	35.005378	74.048282
399.312872	32.484909	74.053287
398.485782	16.840395	74.058292
397.479877	24.749323	74.063297
397.092930	22.849405	74.068302
396.785160	12.983269	74.073306
395.790958	19.181032	74.078311
394.967750	14.917568	74.083316
394.283027	18.677094	74.088321
393.979030	27.719874	74.093326
393.489893	24.365046	74.098330
392.154117	22.619491	74.103335
391.500739	5.983857	74.108340
391.581313	21.862458	74.113345
390.794322	16.915181	74.118350
389.923521	17.121773	74.123354
389.275982	31.038139	74.128359
388.618517	16.924521	74.133364
387.360674	33.778047	74.138369
386.498890	30.201927	74.143374
386.494172	26.394611	74.148378
385.931294	40.049929	74.153383
385.722809	25.010102	74.158388
384.786518	21.121029	74.163393
384.139870	17.725079	74.168398
383.663234	22.559967	74.173402
382.523753	33.665957	74.178407
381.749133	19.902148	74.183412
381.064773	19.522404	74.188417
380.337186	31.726461	74.193422
380.160952	24.444307	74.198426
378.811674	31.053458	74.203431
378.060941	14.356071	74.208436
377.589345	23.892304	74.213441
377.615033	26.931533	74.218446
377.193052	21.594951	74.223450
375.809399	38.493766	74.228455
375.348250	22.368343	74.233460
374.797946	23.195598	74.238465
374.026278	24.717252	74.243470
373.421697	21.653622	74.248474
372.304155	19.338749	74.253479
371.948253	16.041536	74.258484
371.821513	27.304645	74.263489
370.574366	33.113832	74.268494
370.427524	25.617274	74.273498
369.435354	40.108935	74.278503
368.996052	27.830684	74.283508
368.095478	17.992801	74.288513
367.295079	26.190664	74.293518
366.949347	17.347647	74.298522
365.560003	30.727849	74.303527
364.853950	25.198439	74.308532
364.370856	26.385543	74.313537
363.868466	22.359521	74.318542
363.563720	8.032024	74.323546
363.097366	29.390596	74.328551
362.701201	35.456797	74.333556
361.552769	24.713884	74.338561
360.626429	20.771200	74.343566
359.951339	36.040166	74.348570
358.651782	31.608220	74.353575
358.495032	23.148215	74.358580
357.941336	24.299267	74.363585
357.727228	27.692082	74.368590
357.587240	25.826923	74.373594
356.253978	24.513043	74.378599
355.937621	32.726800	74.383604
355.258769	29.124691	74.388609
354.061082	35.282371	74.393614
353.499878	17.078858	74.398618
353.007286	21.646653	74.403623
351.756344	27.320843	74.408628
351.138696	30.677057	74.413633
350.604231	32.263409	74.418638
350.489830	31.012295	74.423642
349.706533	35.604351	74.428647
348.984400	23.809551	74.433652
348.276562	32.192929	74.438657
347.589848	35.642148	74.443662
347.193540	19.848579	74.448666
345.784883	22.203422	74.453671
345.173591	39.344977	74.458676
344.615944	10.888263	74.463681
344.037266	33.985079	74.468686
343.743878	27.125274	74.473690
343.200672	22.317341	74.478695
342.946215	16.756962	74.483700
342.052864	30.692013	74.488705
340.808975	29.527888	74.493710
340.182349	13.346866	74.498714
339.117860	31.954574	74.503719
338.687544	27.130225	74.508724
338.437417	28.554573	74.513729
337.936606	25.977426	74.518734
337.140835	31.128098	74.523738
335.891456	33.430755	74.528743
335.665696	31.158250	74.533748
335.379138	13.978498	74.538753
334.198664	26.311509	74.543758
333.596133	22.878581	74.548762
333.196609	16.943962	74.553767
332.654911	9.918755	74.558772
331.574520	21.956710	74.563777
330.714007	31.767816	74.568782
330.545516	7.935471	74.573786
329.842273	35.336422	74.578791
329.485876	30.503446	74.583796
328.383496	19.311700	74.588801
327.656595	27.220333	74.593806
327.168539	23.830658	74.598810
326.290538	15.898756	74.603815
325.370123	9.504732	74.608820
324.934894	28.184016	74.613825
324.692962	28.301433	74.618830
324.653024	15.128556	74.623834
322.945705	23.847848	74.628839
322.561563	29.098482	74.633844
321.854640	19.086261	74.638849
320.633221	29.677087	74.643854
320.285877	32.075654	74.648858
319.650534	36.631521	74.653863
319.245297	28.348312	74.658868
319.012331	11.205755	74.663873
317.520433	31.895221	74.668878
317.321920	20.368612	74.673882
316.504138	18.464847	74.678887
315.804526	18.336694	74.683892
314.875843	33.190375	74.688897
313.920477	25.753319	74.693902
313.917939	26.029684	74.698906
313.323433	22.877738	74.703911
312.983689	17.479182	74.708916
312.115823	22.624004	74.713921
310.809569	19.213375	74.718926
311.012970	14.950298	74.723930
309.796717	28.933669	74.728935
309.022646	22.371250	74.733940
308.405873	22.240932	74.738945
307.697400	25.763009	74.743950
307.568334	18.500157	74.748954
306.713666	22.151184	74.753959
305.839442	24.692079	74.758964
305.253737	21.789450	74.763969
304.599021	25.060125	74.768974
304.640252	20.515411	74.773978
303.255085	17.481615	74.778983
302.544234	19.728405	74.783988
302.301411	18.798943	74.788993
301.289572	24.502845	74.793998
300.307150	17.625161	74.799002
299.835375	32.765534	74.804007
299.431175	21.773151	74.809012
299.059664	28.896640	74.814017
297.890175	27.534611	74.819022
297.574487	33.712559	74.824026
296.731070	27.791935	74.829031
295.846808	27.194938	74.834036
294.893998	24.704042	74.839041
294.210935	34.108429	74.844046
293.977273	26.699833	74.849050
293.419673	30.486427	74.854055
293.364963	33.563698	74.859060
292.360208	27.408614	74.864065
291.238688	27.242073	74.869070
291.012409	29.561425	74.874074
290.154833	35.319587	74.879079
289.063769	32.078077	74.884084
288.532406	28.116612	74.889089
287.678477	28.372585	74.894094
287.496682	24.789030	74.899098
287.612038	21.061920	74.904103
286.551460	14.702869	74.909108
285.760986	25.821056	74.914113
284.395068	36.963178	74.919118
284.027900	16.664676	74.924122
283.304347	23.557297	74.929127
282.821034	19.380033	74.934132
282.348789	26.718262	74.939137
281.574816	33.778186	74.944142
281.233046	16.818546	74.949146
280.391021	23.704823	74.954151
279.667903	25.050044	74.959156
278.697883	31.595632	74.964161
278.169310	30.847331	74.969166
277.865945	33.180549	74.974170
276.989118	27.659470	74.979175
275.927273	27.037176	74.984180
275.437961	27.071039	74.989185
274.847059	26.099302	74.994190
274.422551	26.321517	74.999194
273.364551	33.431450	75.004199
272.580711	23.551347	75.009204
272.551871	39.087864	75.014209
271.609520	35.759581	75.019214
271.459822	26.614114	75.024218
270.378455	43.343369	75.029223
269.502550	31.580994	75.034228
269.484497	28.315089	75.039233
268.270205	37.443071	75.044238
267.584161	19.603245	75.049242
267.113242	28.702598	75.054247
266.426402	32.979700	75.059252
265.719219	29.970298	75.064257
264.713627	31.549776	75.069262
264.594969	22.109225	75.074266
263.540567	39.870164	75.079271
262.696987	19.773762	75.084276
261.875602	36.138312	75.089281
261.071700	39.546315	75.094286
261.165565	24.086186	75.099290
260.797044	24.381473	75.104295
260.412012	27.563438	75.109300
259.675666	23.297215	75.114305
258.526597	16.114981	75.119310
257.714904	20.293721	75.124314
256.604576	35.581624	75.129319
256.006019	34.041871	75.134324
255.859318	31.447711	75.139329
255.352134	30.396405	75.144334
254.365138	13.757243	75.149338
253.659806	31.399452	75.154343
252.768215	16.526911	75.159348
252.818697	11.465100	75.164353
251.439666	40.531712	75.169358
251.289948	17.927900	75.174362
250.387554	23.136589	75.179367
249.910109	20.087416	75.184372
249.302903	28.010098	75.189377
248.336423	29.529734	75.194382
247.950871	24.948988	75.199386
247.131285	37.497298	75.204391
246.473458	33.623807	75.209396
245.778522	25.743170	75.214401
244.686041	11.683202	75.219406
244.493999	32.321576	75.224410
244.321106	25.174518	75.229415
243.340289	26.344805	75.234420
242.274765	21.874042	75.239425
241.752713	27.447847	75.244430
241.245570	31.335209	75.249434
241.056730	21.312958	75.254439
239.859689	24.367353	75.259444
239.408568	35.579679	75.264449
238.790693	5.651980	75.269454
238.275605	46.178534	75.274458
236.968288	8.608981	75.279463
236.526983	35.695377	75.284468
236.482931	18.972117	75.289473
234.925404	26.179044	75.294478
234.463375	36.733990	75.299482
233.542722	61.176801	75.304487
233.325823	19.932781	75.309492
233.280406	-3.326241	75.314497
231.757715	39.661541	75.319502
231.449132	25.476592	75.324506
230.634673	30.411091	75.329511
230.277717	14.541913	75.334516
229.263019	31.558558	75.339521
228.304555	19.926062	75.344526
228.259641	43.847630	75.349530
227.119127	19.202089	75.354535
226.505287	16.438000	75.359540
226.028764	37.935385	75.364545
224.686232	33.015238	75.369550
225.223538	-7.823853	75.374554
224.260868	15.233232	75.379559
223.425701	55.296789	75.384564
222.676707	47.155126	75.389569
221.938715	38.328942	75.394574
221.384403	15.469550	75.399578
220.561285	25.012959	75.404583
219.604548	44.046622	75.409588
219.651182	5.466500	75.414593
218.811445	48.810593	75.419598
218.532648	12.896744	75.424602
217.245892	40.345005	75.429607
216.897709	29.676423	75.434612
216.443906	4.511452	75.439617
215.386651	46.836890	75.444622
214.713269	24.985151	75.449626
214.286916	1.257043	75.454631
213.443693	52.391289	75.459636
213.177351	11.144150	75.464641
211.888064	32.673346	75.469646
211.317810	29.117042	75.474650
210.819550	22.179551	75.479655
210.301807	37.390333	75.484660
209.502756	10.572679	75.489665
208.362226	41.507677	75.494670
208.441792	21.852280	75.499674
207.653080	34.692120	75.504679
207.025456	30.829595	75.509684
206.105077	46.539791	75.514689
205.417978	32.025713	75.519694
205.392505	32.643178	75.524698
204.146995	33.431514	75.529703
203.164802	43.284134	75.534708
202.786060	28.586863	75.539713
201.875007	21.609542	75.544718
201.939288	23.879418	75.549722
201.046370	47.193499	75.554727
200.149698	35.648917	75.559732
199.786930	29.943412	75.564737
198.894293	34.418910	75.569742
198.685136	22.096140	75.574746
197.702348	36.598957	75.579751
197.009929	25.297766	75.584756
196.535019	27.303553	75.589761
195.389164	36.980430	75.594766
195.042619	34.979495	75.599770
194.376548	31.703382	75.604775
193.718875	29.226966	75.609780
192.966588	26.333583	75.614785
192.160134	30.557237	75.619790
191.997165	20.770552	75.624794
191.533759	33.637366	75.629799
190.140867	21.993737	75.634804
189.471023	20.787045	75.639809
188.735843	26.416915	75.644814
188.470673	24.029296	75.649818
187.727724	36.524399	75.654823
186.936465	22.689220	75.659828
186.463295	8.596770	75.664833
185.597289	29.385167	75.669838
185.268946	30.563398	75.674842
184.170226	15.665578	75.679847
183.464331	27.349001	75.684852
183.044937	35.014685	75.689857
182.832324	26.737066	75.694862
182.330748	16.387830	75.699866
181.513612	31.980637	75.704871
180.323178	12.327500	75.709876
180.077117	32.619689	75.714881
178.901363	26.376816	75.719886
177.943152	16.150851	75.724890
177.875676	34.955991	75.729895
177.294937	20.478590	75.734900
176.448050	49.249090	75.739905
175.264899	14.945923	75.744910
174.954424	40.696376	75.749914
174.495362	20.038852	75.754919
173.742568	32.825663	75.759924
173.725924	24.989851	75.764929
172.406066	33.215403	75.769934
171.996451	13.828823	75.774938
171.676825	38.711893	75.779943
170.363585	40.627449	75.784948
169.760878	12.797712	75.789953
168.889963	27.672168	75.794958
168.844029	34.729563	75.799962
168.142292	19.349008	75.804967
167.005667	33.843246	75.809972
166.539224	33.014105	75.814977
166.323597	30.574436	75.819982
165.350551	23.307416	75.824986
164.586862	33.022704	75.829991
164.067627	31.106077	75.834996
163.501209	24.510603	75.840001
162.304328	28.391273	75.845006
161.679051	23.758892	75.850010
160.974940	23.092221	75.855015
160.534104	35.096061	75.860020
160.550647	21.209351	75.865025
159.463536	32.035849	75.870030
158.977878	16.133602	75.875034
157.979114	23.346081	75.880039
156.987576	33.135548	75.885044
156.218141	33.201487	75.890049
155.359809	23.002177	75.895054
155.278873	38.873388	75.900058
154.766246	22.087674	75.905063
154.443489	37.032417	75.910068
153.840764	22.858129	75.915073
152.767998	34.147511	75.920078
152.552686	26.351264	75.925082
151.365065	31.092996	75.930087
150.207139	19.113906	75.935092
149.949428	10.457168	75.940097
149.035595	42.645880	75.945102
149.291921	27.842628	75.950106
148.193974	35.573944	75.955111
147.481249	29.642001	75.960116
146.796091	26.171843	75.965121
146.377184	28.359506	75.970126
145.864971	23.284930	75.975130
144.927081	17.032532	75.980135
144.310122	22.034899	75.985140
143.367346	26.888966	75.990145
142.497468	34.312698	75.995150
142.005894	28.698704	76.000154
141.394098	32.041415	76.005159
140.662362	13.204497	76.010164
140.257428	34.788221	76.015169
139.410567	25.794947	76.020174
139.125842	24.935258	76.025178
138.525554	28.058530	76.030183
137.521372	30.202341	76.035188
136.679182	31.355295	76.040193
136.273785	26.634244	76.045198
135.642359	17.996102	76.050202
134.750365	30.754656	76.055207
133.678446	38.538596	76.060212
133.528875	33.133396	76.065217
132.549279	26.335756	76.070222
132.521532	31.647839	76.075226
132.006465	23.609260	76.080231
130.730449	38.508915	76.085236
130.520069	24.524362	76.090241
129.716657	24.718722	76.095246
128.923973	22.177131	76.100250
127.897174	34.135654	76.105255
127.230020	19.509640	76.110260
127.531706	32.948257	76.115265
126.414438	22.326662	76.120270
125.608024	32.020388	76.125274
124.989181	6.853391	76.130279
124.494257	49.402948	76.135284
123.768658	14.044488	76.140289
122.515258	31.644810	76.145294
121.995415	25.989602	76.150298
121.690643	6.434955	76.155303
120.739072	43.281360	76.160308
121.086941	16.200428	76.165313
119.602674	15.183556	76.170318
118.961776	19.792381	76.175322
118.568624	39.589250	76.180327
117.433314	9.750439	76.185332
116.994770	30.781314	76.190337
116.169535	23.637391	76.195342
115.537633	15.868172	76.200346
115.634450	17.901058	76.205351
114.559681	22.870793	76.210356
113.812281	30.456336	76.215361
113.122881	36.135693	76.220366
112.312056	21.933113	76.225370
111.328524	25.024475	76.230375
110.582224	24.829715	76.235380
110.498722	23.748718	76.240385
110.155009	15.340649	76.245390
109.644673	24.831049	76.250394
108.373166	22.173453	76.255399
107.740927	30.937453	76.260404
107.763487	20.209780	76.265409
106.368273	22.035946	76.270414
105.569532	21.516838	76.275418
105.039280	20.683695	76.280423
104.732814	24.633683	76.285428
103.982779	20.331855	76.290433
103.232756	22.157621	76.295438
103.002285	23.947835	76.300442
102.095682	24.789397	76.305447
100.863657	31.190760	76.310452
100.358021	20.105811	76.315457
99.613395	26.065191	76.320462
99.535758	33.299513	76.325466
98.825056	23.477202	76.330471
97.563126	28.571405	76.335476
97.473922	23.861432	76.340481
96.839279	28.980164	76.345486
95.920689	14.895703	76.350490
95.205917	29.688507	76.355495
94.369230	24.143758	76.360500
94.100635	17.412508	76.365505
92.991145	26.139088	76.370510
92.470550	18.118752	76.375514
91.783810	24.849437	76.380519
91.178276	30.110174	76.385524
90.877888	13.848848	76.390529
89.771322	30.465466	76.395534
89.310474	21.574646	76.400538
88.786425	23.722320	76.405543
88.150696	29.322162	76.410548
87.507790	11.420364	76.415553
86.489671	30.361328	76.420558
86.085894	29.563207	76.425562
85.697437	22.743847	76.430567
84.390463	32.430689	76.435572
83.873552	15.197873	76.440577
82.906614	22.938272	76.445582
82.501006	29.841727	76.450586
82.532590	28.766029	76.455591
81.433521	24.307000	76.460596
80.821994	15.391336	76.465601
80.151829	13.062018	76.470606
79.601426	17.132908	76.475610
78.599043	23.374658	76.480615
77.783245	21.946867	76.485620
77.286973	20.138555	76.490625
76.849976	27.972620	76.495630
76.460463	22.794920	76.500634
75.648528	15.533788	76.505639
74.995113	22.243392	76.510644
73.967295	15.511820	76.515649
72.803303	30.954974	76.520654
72.339115	23.534304	76.525658
72.095320	14.900589	76.530663
71.584661	20.191923	76.535668
71.442782	16.745520	76.540673
70.185546	22.493372	76.545678
69.434262	20.385137	76.550682
69.151134	23.475183	76.555687
67.678303	19.529906	76.560692
66.998235	15.119168	76.565697
66.198628	21.188241	76.570702
66.109585	7.674765	76.575706
65.873171	19.795792	76.580711
65.063931	31.875738	76.585716
65.129987	21.532189	76.590721
63.802785	31.485598	76.595726
63.073958	21.186834	76.600730
61.929294	16.085433	76.605735
61.156277	24.879775	76.610740
60.959422	23.725403	76.615745
60.399224	26.799722	76.620750
59.882477	19.286523	76.625754
59.252703	22.212679	76.630759
58.378569	28.334642	76.635764
58.012437	8.685730	76.640769
56.388031	30.810850	76.645774
56.046083	22.402509	76.650778
55.426764	27.930359	76.655783
55.161439	26.187710	76.660788
54.370746	22.542040	76.665793
53.582396	28.856888	76.670798
52.630099	18.434514	76.675802
52.485834	28.456270	76.680807
51.677452	23.403729	76.685812
50.972663	19.750667	76.690817
49.931617	33.348243	76.695822
49.739668	17.421264	76.700826
49.551513	20.295904	76.705831
48.167166	26.237494	76.710836
47.848831	15.228339	76.715841
47.064920	41.882128	76.720846
46.389341	27.150260	76.725850
45.139600	24.361503	76.730855
44.313430	16.870859	76.735860
44.070203	12.368375	76.740865
43.632935	30.598580	76.745870
43.115838	27.399670	76.750874
43.016775	24.182965	76.755879
42.165384	23.013157	76.760884
41.513172	17.104718	76.765889
40.591995	23.491213	76.770894
39.456060	39.830286	76.775898
38.935342	27.413751	76.780903
38.096031	26.391817	76.785908
38.036164	15.344591	76.790913
37.494100	30.370032	76.795918
36.915410	26.020396	76.800922
35.967967	28.066894	76.805927
35.272422	28.947349	76.810932
34.208742	34.068303	76.815937
33.334045	26.566476	76.820942
32.854728	23.874017	76.825946
32.661235	38.555305	76.830951
32.235576	33.115314	76.835956
31.760925	23.357872	76.840961
30.202126	28.800635	76.845966
29.915583	32.283863	76.850970
29.199064	28.172241	76.855975
27.758111	25.702554	76.860980
27.688054	42.376202	76.865985
27.053246	29.845413	76.870990
26.747012	21.445574	76.875994
26.284430	19.206154	76.880999
25.357449	29.639747	76.886004
24.803942	28.944362	76.891009
24.050106	28.643606	76.896014
23.113460	20.607659	76.901018
22.460660	26.781052	76.906023
21.512175	23.201563	76.911028
21.138404	25.106098	76.916033
20.837913	27.662793	76.921038
20.319326	35.448386	76.926042
19.395166	29.398839	76.931047
18.609121	20.268198	76.936052
18.165480	5.327493	76.941057
16.966897	21.157766	76.946062
16.408752	22.636006	76.951066
15.760447	23.275559	76.956071
15.171361	22.552738	76.961076
15.203491	18.170325	76.966081
14.221639	23.503718	76.971086
13.664174	28.876640	76.976090
13.166078	21.611197	76.981095
11.826075	22.305899	76.986100
11.328551	15.412502	76.991105
11.117074	27.936380	76.996110
10.195462	27.943068	77.001114
9.174969	20.704192	77.006119
8.431818	25.212668	77.011124
8.187432	16.432413	77.016129
7.569896	26.963293	77.021134
6.371559	31.523883	77.026139
5.707137	28.435210	77.031143
5.168888	18.246411	77.036148
4.856506	26.604612	77.041153
4.415318	19.063609	77.046158