Mon Mar 08 20:03:04 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.109797	106.618505	0.000000
0.097655	92.871909	0.005005
-0.348747	51.040101	0.010010
-2.531545	26.013785	0.015014
-6.403229	-0.061313	0.020019
-12.104876	11.310467	0.025024
-17.294463	4.347143	0.030029
-21.152809	0.452861	0.035034
-24.994115	15.086823	0.040038
-28.699006	1.118907	0.045043
-32.315694	8.272811	0.050048
-36.161911	8.758640	0.055053
-39.605929	-1.239405	0.060058
-43.827552	12.592725	0.065062
-47.342754	-4.566967	0.070067
-50.926774	5.399550	0.075072
-54.980168	6.568115	0.080077
-58.784153	0.511268	0.085082
-62.688741	8.433336	0.090086
-66.329678	-5.125275	0.095091
-69.862157	7.270829	0.100096
-74.072650	9.401129	0.105101
-77.334147	13.847774	0.110106
-81.325810	13.494350	0.115110
-84.511848	-0.450603	0.120115
-88.852503	-0.297358	0.125120
-92.672468	8.322405	0.130125
-96.164935	7.777404	0.135130
-100.026480	13.497712	0.140134
-103.692769	-0.528270	0.145139
-107.534930	-2.991651	0.150144
-111.299469	4.638505	0.155149
-115.218456	-6.154046	0.160154
-119.261673	-5.106837	0.165158
-123.063703	9.569873	0.170163
-127.149040	13.499959	0.175168
-130.532176	6.868333	0.180173
-134.015219	3.395284	0.185178
-137.939196	3.657156	0.190182
-141.565714	4.554338	0.195187
-145.514374	5.783606	0.200192
-149.092184	5.528246	0.205197
-152.484050	-0.491717	0.210202
-156.411527	-2.660728	0.215206
-160.656146	-0.960040	0.220211
-164.403562	12.474934	0.225216
-167.721390	13.777021	0.230221
-171.294864	10.334224	0.235226
-175.369455	14.989595	0.240230
-179.101761	-4.855269	0.245235
-182.991919	-2.293394	0.250240
-186.904169	6.957776	0.255245
-190.302752	-5.767318	0.260250
-194.250634	10.012898	0.265254
-198.099338	-4.204566	0.270259
-201.340706	7.547634	0.275264
-205.451199	5.538787	0.280269
-209.325344	7.095285	0.285274
-213.278455	13.293968	0.290278
-216.802707	7.017704	0.295283
-220.669825	11.919134	0.300288
-224.452544	5.507529	0.305293
-228.150633	8.254847	0.310298
-231.672875	10.573590	0.315302
-235.404338	5.394788	0.320307
-239.196680	6.868896	0.325312
-243.226240	12.685622	0.330317
-246.774516	-0.051764	0.335322
-250.426621	5.034570	0.340326
-254.142299	11.059811	0.345331
-258.055294	3.872758	0.350336
-262.339218	4.037758	0.355341
-265.475249	-7.874485	0.360346
-269.619758	17.805031	0.365350
-273.453446	-12.080497	0.370355
-277.032127	13.942329	0.375360
-280.802406	10.781830	0.380365
-284.238078	-6.901057	0.385370
-288.441842	21.301415	0.390374
-291.705571	6.683242	0.395379
-295.665073	-5.453869	0.400384
-299.413619	13.161356	0.405389
-303.058837	1.497589	0.410394
-306.999599	11.698016	0.415398
-310.593177	0.476992	0.420403
-314.734698	-10.462593	0.425408
-318.794598	21.633794	0.430413
-321.752858	-13.918183	0.435418
-326.352921	6.928615	0.440422
-329.608028	0.294193	0.445427
-333.382391	-11.482926	0.450432
-337.281900	6.166197	0.455437
-340.825094	4.350843	0.460442
-344.869827	6.139780	0.465446
-348.257258	-9.820920	0.470451
-351.921443	4.458816	0.475456
-355.935633	9.456471	0.480461
-359.633492	-4.464695	0.485466
-363.630012	-5.070742	0.490470
-367.502085	2.990089	0.495475
-371.214167	3.783014	0.500480
-374.543834	7.823070	0.505485
-378.234120	1.595642	0.510490
-382.363018	4.205415	0.515494
-385.984636	6.852459	0.520499
-389.897589	14.244975	0.525504
-393.647625	14.793280	0.530509
-397.611793	-8.755981	0.535514
-401.319381	4.898447	0.540518
-404.632017	-4.672192	0.545523
-409.079465	-5.045322	0.550528
-412.500500	12.909104	0.555533
-415.915325	4.466458	0.560538
-419.790047	11.588008	0.565542
-423.504940	3.027723	0.570547
-427.593369	4.019594	0.575552
-431.472171	-4.161288	0.580557
-434.641446	-9.591952	0.585562
-438.884690	2.673735	0.590566
-442.636454	-5.442266	0.595571
-446.675835	5.327586	0.600576
-450.337800	14.375203	0.605581
-453.816974	4.676698	0.610586
-457.599370	13.060791	0.615590
-461.137211	-1.614255	0.620595
-465.128987	-0.945237	0.625600
-468.989607	9.073917	0.630605
-472.307636	7.885068	0.635610
-476.496901	8.727559	0.640614
-480.182421	14.406150	0.645619
-483.743984	-0.058508	0.650624
-487.767928	3.956978	0.655629
-491.253947	7.397740	0.660634
-495.201071	4.188570	0.665638
-498.708782	-1.987404	0.670643
-502.718831	2.472128	0.675648
-506.947997	9.048077	0.680653
-510.175236	1.371911	0.685658
-513.977748	-0.026477	0.690662
-517.505204	7.385078	0.695667
-521.081352	-0.512861	0.700672
-525.224011	0.587178	0.705677
-528.878791	-7.624588	0.710682
-533.057257	7.778251	0.715686
-536.718167	3.082215	0.720691
-540.424594	3.959646	0.725696
-544.009958	12.224093	0.730701
-547.728331	10.746090	0.735706
-551.593788	-12.123256	0.740710
-555.442420	15.459934	0.745715
-559.109096	5.812045	0.750720
-563.001956	9.101875	0.755725
-566.822829	6.142294	0.760730
-570.534340	-3.501561	0.765734
-574.120488	-2.542375	0.770739
-577.888585	3.009211	0.775744
-582.251992	4.166690	0.780749
-585.009763	2.779694	0.785754
-589.279952	-1.323798	0.790758
-593.099526	-11.164794	0.795763
-596.654599	-2.573987	0.800768
-600.652098	-1.471780	0.805773
-604.096400	-10.147520	0.810778
-608.125658	6.448905	0.815782
-611.793900	-5.850856	0.820787
-615.192096	-9.417157	0.825792
-619.090092	-1.853230	0.830797
-623.007940	-16.549274	0.835802
-627.280219	-2.116820	0.840806
-630.871093	4.762599	0.845811
-634.762913	-3.630301	0.850816
-638.216577	-4.045100	0.855821
-641.381987	-0.216995	0.860826
-645.642450	-10.078912	0.865830
-649.308937	-0.191426	0.870835
-653.200307	-4.746380	0.875840
-657.169461	-3.601302	0.880845
-660.547438	-9.099220	0.885850
-664.153595	-6.943048	0.890854
-668.010840	-11.232214	0.895859
-671.922019	-8.098543	0.900864
-676.115060	-3.800283	0.905869
-679.654779	-6.411974	0.910874
-683.598554	-0.958301	0.915878
-687.127614	-3.535417	0.920883
-690.545344	4.801785	0.925888
-694.612608	-9.643196	0.930893
-698.184558	-4.138542	0.935898
-702.368582	2.460483	0.940902
-705.968830	-4.974452	0.945907
-709.558493	-11.204802	0.950912
-713.565610	-12.111313	0.955917
-717.300832	-8.611484	0.960922
-720.562578	-9.602412	0.965926
-724.245803	-0.364948	0.970931
-727.957110	0.327491	0.975936
-732.205901	-3.279304	0.980941
-735.816806	0.618545	0.985946
-739.854268	-1.859894	0.990950
-743.270457	1.415539	0.995955
-747.073768	-5.286768	1.000960
-751.253248	-0.683064	1.005965
-754.766147	-9.024360	1.010970
-758.693117	-1.088185	1.015974
-762.353000	-2.357592	1.020979
-765.981039	-2.914630	1.025984
-769.916887	0.702497	1.030989
-773.259325	-6.502322	1.035994
-777.266120	4.921954	1.040998
-781.080397	4.189720	1.046003
-784.995918	0.895574	1.051008
-788.722297	5.173052	1.056013
-792.299425	-0.628703	1.061018
-796.208326	6.090496	1.066022
-799.894227	0.764995	1.071027
-803.697574	-3.296038	1.076032
-807.774089	-0.632416	1.081037
-811.199665	-5.961665	1.086042
-814.716559	0.379534	1.091046
-818.512580	-4.346486	1.096051
-822.435666	0.706745	1.101056
-826.537415	-3.815861	1.106061
-829.885477	-7.538080	1.111066
-833.654323	-12.506515	1.116070
-837.228948	6.658750	1.121075
-840.814562	-8.581984	1.126080
-845.359378	4.393274	1.131085
-848.966179	0.881163	1.136090
-852.853312	0.442944	1.141094
-856.332753	-11.627983	1.146099
-859.942379	-4.287962	1.151104
-863.943944	14.352720	1.156109
-867.202423	9.279086	1.161114
-871.430359	9.220208	1.166118
-875.296001	-5.661914	1.171123
-878.811163	-7.766336	1.176128
-882.732149	7.922296	1.181133
-886.244914	-4.811832	1.186138
-889.905436	-0.715026	1.191142
-893.836645	-6.795867	1.196147
-897.781327	6.504543	1.201152
-901.608205	3.585897	1.206157
-905.066244	-4.740282	1.211162
-909.108556	-1.400770	1.216166
-912.964505	-1.180035	1.221171
-916.075845	-11.581531	1.226176
-920.330672	4.791260	1.231181
-924.201368	9.601336	1.236186
-927.920072	9.708694	1.241190
-931.707897	6.276117	1.246195
-935.201395	-1.891395	1.251200
-938.630922	0.375708	1.256205
-942.730896	-1.086372	1.261210
-946.584693	-7.433367	1.266214
-950.266120	-5.543823	1.271219
-953.831627	-6.146836	1.276224
-957.741572	4.882225	1.281229
-961.457246	-5.402070	1.286234
-965.474367	2.720724	1.291238
-969.393423	-2.346460	1.296243
-972.710480	5.099894	1.301248
-976.755264	8.182896	1.306253
-980.601109	-1.317373	1.311258
-984.481234	-4.976352	1.316262
-987.989195	3.697355	1.321267
-991.481670	2.451993	1.326272
-995.562938	5.714311	1.331277
-999.289063	9.317196	1.336282
-1003.175680	9.068362	1.341286
-1006.758422	0.333390	1.346291
-1010.225421	0.246095	1.351296
-1014.492294	-0.474866	1.356301
-1018.269598	4.821849	1.361306
-1021.743387	5.766895	1.366310
-1025.924982	1.831378	1.371315
-1029.148299	-5.086208	1.376320
-1033.286145	4.197620	1.381325
-1036.593440	-1.798278	1.386330
-1040.736928	0.584745	1.391334
-1044.636098	7.917741	1.396339
-1048.034408	1.513830	1.401344
-1051.894429	4.650977	1.406349
-1055.258976	-8.790915	1.411354
-1059.170320	-10.317649	1.416358
-1063.367805	5.639386	1.421363
-1066.928773	7.915085	1.426368
-1070.761369	3.245794	1.431373
-1074.004406	-1.243432	1.436378
-1077.970030	0.043701	1.441382
-1082.279930	-2.556124	1.446387
-1085.725421	-2.845425	1.451392
-1089.945932	-0.539874	1.456397
-1093.243916	-8.628030	1.461402
-1097.330614	-7.915955	1.466406
-1101.119634	-11.488391	1.471411
-1104.346491	-8.875038	1.476416
-1108.150519	-10.067227	1.481421
-1111.900982	-0.995041	1.486426
-1115.590916	-9.249097	1.491430
-1119.607634	-7.616282	1.496435
-1123.315539	4.405641	1.501440
-1127.410452	-7.701989	1.506445
-1130.733436	0.483470	1.511450
-1134.813352	-2.348574	1.516454
-1138.576215	-13.411840	1.521459
-1142.305650	-8.051638	1.526464
-1146.166812	8.537640	1.531469
-1149.575655	-3.244518	1.536474
-1153.121156	6.089806	1.541478
-1157.105000	5.967162	1.546483
-1160.444257	-4.988822	1.551488
-1164.711497	-3.437261	1.556493
-1168.591564	0.286702	1.561498
-1172.419198	13.519932	1.566502
-1175.962298	4.395726	1.571507
-1179.682226	0.698832	1.576512
-1183.936120	-4.811098	1.581517
-1187.347268	3.065300	1.586522
-1191.164687	7.775823	1.591526
-1194.842414	4.051701	1.596531
-1198.198408	-0.669983	1.601536
-1202.058950	9.097989	1.606541
-1206.294800	2.943449	1.611546
-1210.308790	0.025302	1.616550
-1214.092439	0.835730	1.621555
-1217.388000	-1.060487	1.626560
-1221.217741	10.351933	1.631565
-1224.340271	-3.027507	1.636570
-1228.306883	-1.481365	1.641574
-1232.501040	3.480306	1.646579
-1236.245954	6.183054	1.651584
-1240.334570	7.209472	1.656589
-1243.507624	-0.589400	1.661594
-1247.446295	-1.559557	1.666598
-1251.327942	-2.455263	1.671603
-1254.584047	-1.867956	1.676608
-1258.868254	5.998469	1.681613
-1262.704298	3.383066	1.686618
-1266.359997	1.098319	1.691622
-1269.919755	3.066652	1.696627
-1273.445292	-2.919193	1.701632
-1277.367320	11.221775	1.706637
-1281.582658	2.197451	1.711642
-1285.254211	-1.948518	1.716646
-1289.292118	4.885148	1.721651
-1292.822576	-2.523738	1.726656
-1296.538574	2.867669	1.731661
-1299.933636	-2.858344	1.736666
-1303.738838	1.963932	1.741670
-1307.868734	-0.318957	1.746675
-1311.333329	0.177233	1.751680
-1315.217383	1.112697	1.756685
-1319.230215	4.230588	1.761690
-1322.644497	0.637956	1.766694
-1326.277800	4.761032	1.771699
-1329.594064	-6.166831	1.776704
-1334.179509	0.570068	1.781709
-1337.949821	2.706238	1.786714
-1341.679659	1.980330	1.791718
-1345.254620	-3.726276	1.796723
-1348.624291	-20.388287	1.801728
-1352.595805	-0.510750	1.806733
-1356.374496	3.031728	1.811738
-1360.123519	0.651695	1.816742
-1364.325380	-2.644497	1.821747
-1367.722524	-4.811213	1.826752
-1371.871978	-2.133366	1.831757
-1375.600260	-0.016480	1.836762
-1379.331659	-6.358669	1.841766
-1383.085734	-2.451117	1.846771
-1386.601979	-11.535117	1.851776
-1390.221015	1.748605	1.856781
-1393.684321	1.375891	1.861786
-1397.846215	1.165485	1.866790
-1401.745938	-6.436393	1.871795
-1405.612340	1.205716	1.876800
-1409.522940	3.175245	1.881805
-1412.801269	-10.849103	1.886810
-1416.448529	9.955825	1.891814
-1420.474348	8.624637	1.896819
-1424.148869	-4.161542	1.901824
-1427.669159	6.801134	1.906829
-1431.952625	-1.619109	1.911834
-1435.824102	7.870307	1.916838
-1439.737786	-2.230089	1.921843
-1442.827686	-12.957494	1.926848
-1446.803206	4.238685	1.931853
-1450.719599	-7.291419	1.936858
-1454.344596	3.322240	1.941862
-1458.063488	-1.355134	1.946867
-1461.644987	-6.578001	1.951872
-1465.760056	5.826563	1.956877
-1469.406194	1.832929	1.961882
-1473.053171	4.129323	1.966886
-1477.040237	3.909986	1.971891
-1480.655521	-2.654035	1.976896
-1484.645247	-0.892463	1.981901
-1488.407611	-3.806260	1.986906
-1492.027608	-8.784814	1.991910
-1495.854901	-6.364902	1.996915
-1499.255950	4.705058	2.006912
-1500.609246	-2.434017	2.016909
-1498.272659	0.325708	2.026906
-1495.205205	2.096879	2.036902
-1493.125109	5.019255	2.046899
-1491.232780	1.023287	2.056896
-1489.484232	6.035449	2.066893
-1487.409493	-0.995813	2.076890
-1485.484701	4.251791	2.086886
-1483.922003	-6.578223	2.096883
-1481.741878	-4.320754	2.106880
-1479.554914	-0.221887	2.116877
-1478.138434	-1.945495	2.126874
-1476.195243	-2.491965	2.136870
-1474.109773	8.568420	2.146867
-1472.070365	9.307500	2.156864
-1470.503124	2.783801	2.166861
-1468.795244	-0.587394	2.176858
-1466.523116	-0.060827	2.186854
-1464.519717	3.195938	2.196851
-1462.931126	6.986462	2.206848
-1461.043884	-3.172407	2.216845
-1459.068602	-0.908954	2.226842
-1457.120846	3.021414	2.236838
-1454.996955	4.953204	2.246835
-1453.058623	-2.251961	2.256832
-1451.439134	-1.316160	2.266829
-1449.696728	-4.359738	2.276826
-1447.787749	8.740361	2.286822
-1445.827520	8.622208	2.296819
-1443.698068	-2.434316	2.306816
-1442.289981	-0.533150	2.316813
-1440.231879	-3.016265	2.326810
-1438.463765	7.474493	2.336806
-1436.377855	5.479523	2.346803
-1434.681988	-2.054672	2.356800
-1432.524356	2.805197	2.366797
-1430.541648	6.665262	2.376794
-1428.741554	0.505328	2.386790
-1427.269223	3.749273	2.396787
-1425.131632	-0.925338	2.406784
-1423.096180	0.966961	2.416781
-1421.405614	7.816745	2.426778
-1419.830782	2.924371	2.436774
-1417.674197	2.476404	2.446771
-1415.563640	-3.516927	2.456768
-1413.770617	0.154064	2.466765
-1412.054859	6.701423	2.476762
-1410.328735	-4.850980	2.486758
-1408.137444	1.918642	2.496755
-1406.335290	1.641108	2.506752
-1404.454392	-7.312058	2.516749
-1402.526637	-2.143797	2.526746
-1400.953652	7.064650	2.536742
-1398.689243	4.177516	2.546739
-1396.609241	-3.640769	2.556736
-1394.926460	-2.672433	2.566733
-1393.469105	-5.291414	2.576730
-1391.522512	-2.881214	2.586726
-1389.624936	8.210920	2.596723
-1387.513733	-5.324554	2.606720
-1385.428885	-4.398477	2.616717
-1383.732386	-10.612836	2.626714
-1382.059500	-0.462024	2.636710
-1379.782091	-0.638794	2.646707
-1378.160997	1.761955	2.656704
-1376.376547	1.016788	2.666701
-1374.362604	2.688382	2.676698
-1372.713281	-1.104391	2.686694
-1370.749984	-5.269508	2.696691
-1368.754852	4.376607	2.706688
-1366.884408	-6.103165	2.716685
-1364.972582	-2.651665	2.726682
-1362.762940	-10.302792	2.736678
-1361.412752	-1.936481	2.746675
-1359.584238	-2.210303	2.756672
-1357.491630	-8.675937	2.766669
-1355.536767	-11.852922	2.776666
-1353.576105	-5.531028	2.786662
-1351.832559	-4.551863	2.796659
-1349.958319	-4.588279	2.806656
-1348.573478	-12.036311	2.816653
-1346.138803	-3.949376	2.826650
-1344.188275	-10.011757	2.836646
-1342.387728	-8.864880	2.846643
-1340.625316	-11.910001	2.856640
-1338.747809	-10.557563	2.866637
-1336.725359	-6.250656	2.876634
-1335.080921	-3.095776	2.886630
-1333.074091	-2.998678	2.896627
-1331.181962	-2.954265	2.906624
-1329.208280	-8.475645	2.916621
-1327.325906	-5.721977	2.926618
-1325.815153	-7.773191	2.936614
-1324.258229	-1.921865	2.946611
-1321.625756	-5.793034	2.956608
-1319.922871	2.755256	2.966605
-1318.096288	-3.388312	2.976602
-1316.330195	-0.538658	2.986598
-1313.889957	-7.208310	2.996595
-1312.394761	-1.250785	3.006592
-1310.846572	3.498351	3.016589
-1308.432249	-3.877623	3.026586
-1306.973204	3.438751	3.036582
-1304.933149	-2.323745	3.046579
-1302.940902	-9.794771	3.056576
-1301.396129	-8.204321	3.066573
-1299.408184	-6.639018	3.076570
-1297.456068	-0.607786	3.086566
-1295.421152	-4.429069	3.096563
-1293.611842	-11.829757	3.106560
-1291.361381	-2.756504	3.116557
-1289.985192	-4.617224	3.126554
-1288.176714	-0.905976	3.136550
-1286.040568	-7.031176	3.146547
-1284.330421	-8.738517	3.156544
-1282.433258	-4.239414	3.166541
-1280.693283	-2.405476	3.176538
-1278.429958	-2.733038	3.186534
-1276.701440	-10.217093	3.196531
-1275.350634	-11.085394	3.206528
-1273.124452	-3.651798	3.216525
-1270.902833	-6.276190	3.226522
-1269.437358	-3.158929	3.236518
-1267.304228	-6.658037	3.246515
-1265.490627	-7.770915	3.256512
-1263.570273	-11.202809	3.266509
-1261.616865	-6.269040	3.276506
-1259.828688	-1.585117	3.286502
-1258.034741	-9.254882	3.296499
-1256.126762	-5.928979	3.306496
-1254.178260	-6.768196	3.316493
-1252.252508	-3.511444	3.326490
-1250.864736	4.507904	3.336486
-1248.608100	0.540657	3.346483
-1246.727447	-8.050804	3.356480
-1244.827467	-10.593699	3.366477
-1242.779000	-8.079683	3.376474
-1241.162767	0.769886	3.386470
-1239.405106	-5.056302	3.396467
-1237.400599	-2.732598	3.406464
-1235.401750	0.913495	3.416461
-1233.597102	-5.397015	3.426458
-1231.882892	-2.425316	3.436454
-1229.800159	-4.039096	3.446451
-1227.702292	-5.407421	3.456448
-1226.319228	-4.439940	3.466445
-1224.685954	-2.827287	3.476442
-1222.404800	0.596812	3.486438
-1220.250143	-5.078171	3.496435
-1218.602311	-1.060126	3.506432
-1216.800282	-1.812720	3.516429
-1214.827139	-3.749978	3.526426
-1212.870666	0.142898	3.536422
-1211.267276	-2.601967	3.546419
-1209.085333	-9.159135	3.556416
-1207.072614	-2.706498	3.566413
-1205.256354	0.793590	3.576410
-1203.557902	-2.195412	3.586406
-1201.952507	-4.144861	3.596403
-1199.769145	-1.646074	3.606400
-1197.945213	5.000983	3.616397
-1195.951196	-1.327174	3.626394
-1194.221778	1.305831	3.636390
-1192.108025	6.000869	3.646387
-1190.518745	-1.741886	3.656384
-1188.602128	-13.577239	3.666381
-1186.876134	-1.947505	3.676378
-1184.856967	-2.283273	3.686374
-1183.030794	-2.351334	3.696371
-1180.812436	-7.324422	3.706368
-1179.161781	-0.696991	3.716365
-1177.325084	-5.624796	3.726362
-1175.471208	-6.101464	3.736358
-1173.539814	-7.100497	3.746355
-1171.664741	0.572532	3.756352
-1169.926741	1.675873	3.766349
-1168.040921	2.889765	3.776346
-1165.962391	-1.688334	3.786342
-1164.082946	-6.553500	3.796339
-1162.538616	0.774591	3.806336
-1160.162041	-3.477006	3.816333
-1158.510242	3.050793	3.826330
-1156.462765	-4.163715	3.836326
-1154.960762	-3.189960	3.846323
-1152.977222	-4.775172	3.856320
-1150.977871	-4.695665	3.866317
-1149.124394	-0.317340	3.876314
-1147.293085	2.373604	3.886310
-1145.551039	-4.572570	3.896307
-1143.614268	-4.487781	3.906304
-1141.637011	0.068100	3.916301
-1139.689792	0.247529	3.926298
-1137.799447	3.828971	3.936294
-1136.108243	-0.177171	3.946291
-1134.243963	-0.868614	3.956288
-1132.305266	-0.998845	3.966285
-1130.267477	-5.062011	3.976282
-1128.389370	3.879954	3.986278
-1126.776584	9.259896	3.996275
-1125.042484	1.389807	4.006272
-1122.813121	6.890567	4.016269
-1121.066619	4.675456	4.026266
-1119.194388	2.023421	4.036262
-1117.190887	-0.924330	4.046259
-1115.255397	-6.755197	4.056256
-1113.597499	7.275855	4.066253
-1111.496115	-6.186790	4.076250
-1109.682927	-0.780482	4.086246
-1107.924216	-4.161135	4.096243
-1106.021654	-7.394284	4.106240
-1104.090014	-3.473657	4.116237
-1101.895315	-9.450184	4.126234
-1100.367200	-1.963149	4.136230
-1098.773442	8.432653	4.146227
-1096.776050	-6.690066	4.156224
-1094.840448	-6.118769	4.166221
-1092.595765	-1.076716	4.176218
-1091.003847	-10.891257	4.186214
-1088.970623	-5.794850	4.196211
-1087.322304	2.569745	4.206208
-1085.515247	-4.131018	4.216205
-1083.502615	-3.033652	4.226202
-1081.560018	-5.436405	4.236198
-1079.597271	0.667531	4.246195
-1077.741906	-8.383941	4.256192
-1075.943001	-7.397633	4.266189
-1074.218456	0.279037	4.276186
-1072.354220	-2.595876	4.286182
-1070.370028	-5.609967	4.296179
-1068.478821	-6.610380	4.306176
-1066.488647	-10.064339	4.316173
-1064.410849	-6.089695	4.326170
-1062.671303	3.474450	4.336166
-1061.021508	-5.709907	4.346163
-1059.219938	0.135639	4.356160
-1057.162219	0.592704	4.366157
-1055.286893	-1.636649	4.376154
-1053.741273	-3.956935	4.386150
-1051.632205	-0.724595	4.396147
-1049.685327	-2.768033	4.406144
-1048.014170	1.036425	4.416141
-1045.846072	-5.799421	4.426138
-1043.933959	-7.442586	4.436134
-1042.041231	-2.827309	4.446131
-1040.267618	-5.400355	4.456128
-1038.373385	-4.200333	4.466125
-1036.709453	4.687558	4.476122
-1034.728411	-0.009039	4.486118
-1032.611667	-4.261582	4.496115
-1031.010025	-6.930263	4.506112
-1029.196202	-6.802032	4.516109
-1027.010324	-5.951784	4.526106
-1025.218731	-1.309265	4.536102
-1023.623633	-4.891040	4.546099
-1021.746871	-6.094353	4.556096
-1019.579106	0.455233	4.566093
-1017.868225	-5.333322	4.576090
-1016.068291	-2.158866	4.586086
-1013.845533	-1.976035	4.596083
-1011.978387	-6.673342	4.606080
-1010.320779	-2.299887	4.616077
-1008.633759	-4.661706	4.626074
-1006.680731	-4.034705	4.636070
-1004.480961	-5.344924	4.646067
-1002.582908	-5.451180	4.656064
-1001.044238	-1.131322	4.666061
-999.027207	-9.509171	4.676058
-997.432213	-1.453324	4.686054
-995.333308	-2.106396	4.696051
-993.401234	0.101223	4.706048
-991.429467	-10.231872	4.716045
-989.573200	-7.694781	4.726042
-987.742962	-2.259522	4.736038
-985.852355	8.081003	4.746035
-984.228066	-2.384404	4.756032
-982.349374	5.359266	4.766029
-980.011612	-0.730031	4.776026
-978.414070	-1.042401	4.786022
-976.453984	3.022201	4.796019
-974.661813	-4.307639	4.806016
-972.682299	-2.759647	4.816013
-971.123077	-4.628931	4.826010
-969.373190	-5.096701	4.836006
-966.955285	-1.749471	4.846003
-965.372574	-6.170747	4.856000
-963.300187	-4.858637	4.865997
-961.549219	-5.579188	4.875994
-959.579278	-11.165988	4.885990
-957.677675	-4.641669	4.895987
-955.935604	-6.398087	4.905984
-954.020281	1.377639	4.915981
-952.113632	-4.494279	4.925978
-950.276622	0.051046	4.935974
-948.126633	1.262346	4.945971
-946.395455	6.452977	4.955968
-944.657942	-12.556221	4.965965
-942.695234	1.756210	4.975962
-941.003626	1.143054	4.985958
-938.971965	4.998890	4.995955
-937.102902	-5.791397	5.005952
-935.066841	7.352031	5.015949
-933.249207	-2.283797	5.025946
-931.614386	8.920253	5.035942
-929.840866	10.081251	5.045939
-927.793444	7.410823	5.055936
-925.682808	-0.707224	5.065933
-924.007604	5.583350	5.075930
-922.229885	4.204912	5.085926
-920.291206	7.878279	5.095923
-918.567922	8.532617	5.105920
-916.521118	2.196238	5.115917
-914.605239	13.705867	5.125914
-912.864801	-2.970271	5.135910
-910.968340	12.421667	5.145907
-908.742022	2.720507	5.155904
-906.887657	5.117456	5.165901
-905.215527	-1.856852	5.175898
-903.483758	5.779336	5.185894
-901.163439	2.721111	5.195891
-899.644731	-5.970117	5.205888
-897.761364	5.161063	5.215885
-895.909000	-9.908330	5.225882
-894.153707	8.652811	5.235878
-892.069810	-2.028123	5.245875
-890.174633	4.805161	5.255872
-888.487860	-5.712806	5.265869
-886.597219	4.414659	5.275866
-884.435403	4.005820	5.285862
-882.619613	4.375413	5.295859
-880.991721	-0.987707	5.305856
-878.993614	3.923474	5.315853
-876.834198	11.011348	5.325850
-875.051564	-1.683371	5.335846
-873.484793	8.817973	5.345843
-871.473231	-5.255354	5.355840
-869.334352	2.631541	5.365837
-868.132701	4.993937	5.375834
-866.010914	-1.414384	5.385830
-863.872603	-2.289940	5.395827
-862.105614	-1.988313	5.405824
-860.209739	-1.628349	5.415821
-858.592622	1.229696	5.425818
-856.583338	0.731592	5.435814
-854.505022	6.773052	5.445811
-852.605006	7.135518	5.455808
-850.540563	6.219682	5.465805
-848.803087	2.692618	5.475802
-847.063352	6.765721	5.485798
-844.976458	1.269248	5.495795
-843.395921	3.691078	5.505792
-841.744587	0.203052	5.515789
-839.548305	12.226834	5.525786
-837.756629	-2.382859	5.535782
-835.562201	7.672409	5.545779
-833.901533	3.628723	5.555776
-832.215873	8.144663	5.565773
-830.114123	1.267501	5.575770
-828.181505	4.071976	5.585766
-826.409354	11.963862	5.595763
-824.459894	5.208936	5.605760
-822.760405	10.943117	5.615757
-820.914389	4.716273	5.625754
-818.787061	13.096090	5.635750
-817.132101	5.823021	5.645747
-815.219479	7.479730	5.655744
-813.180861	9.987819	5.665741
-811.505779	8.973215	5.675738
-809.805792	14.217887	5.685734
-807.521657	11.208162	5.695731
-805.626311	12.395569	5.705728
-803.754697	15.389805	5.715725
-802.039867	11.736927	5.725722
-799.981495	17.611117	5.735718
-798.305135	6.378065	5.745715
-796.737321	9.425604	5.755712
-794.310549	3.161209	5.765709
-792.469607	2.810059	5.775706
-791.003988	8.145886	5.785702
-789.158136	11.420549	5.795699
-786.905610	-0.532964	5.805696
-785.098967	3.614750	5.815693
-783.101032	13.540443	5.825690
-781.556839	3.809481	5.835686
-779.299087	14.677266	5.845683
-777.603734	8.060878	5.855680
-775.992490	14.098129	5.865677
-774.020267	0.905830	5.875674
-772.032564	13.165115	5.885670
-769.926223	10.621182	5.895667
-767.940112	16.840086	5.905664
-766.153896	-0.176426	5.915661
-764.655872	9.052395	5.925658
-762.796008	12.449568	5.935654
-760.721663	6.088385	5.945651
-758.857930	2.489103	5.955648
-757.239395	14.946345	5.965645
-755.023960	12.407092	5.975642
-753.137238	13.196473	5.985638
-751.380479	15.471791	5.995635
-749.241900	8.587227	6.005632
-747.651042	13.075757	6.015629
-745.957216	3.305111	6.025626
-743.952695	17.633177	6.035622
-741.587047	11.440173	6.045619
-740.038439	6.781343	6.055616
-738.233946	6.652362	6.065613
-736.424051	6.929859	6.075610
-734.642417	12.188381	6.085606
-732.442755	9.710087	6.095603
-730.717166	4.663002	6.105600
-728.817037	8.906342	6.115597
-726.919423	10.892343	6.125594
-725.231948	13.608199	6.135590
-723.460478	13.733963	6.145587
-721.199575	11.631129	6.155584
-719.257938	13.078032	6.165581
-717.566569	10.049446	6.175578
-715.739440	11.547808	6.185574
-713.990324	13.971208	6.195571
-712.174553	2.205965	6.205568
-710.156428	11.402234	6.215565
-708.190159	12.448920	6.225562
-706.062920	12.850979	6.235558
-704.415693	8.531649	6.245555
-702.541658	16.244740	6.255552
-700.474919	9.460111	6.265549
-699.093464	13.164300	6.275546
-696.964443	13.542399	6.285542
-695.059034	10.555409	6.295539
-693.175462	12.584733	6.305536
-691.295175	13.522024	6.315533
-689.472100	13.183282	6.325530
-687.577115	10.269011	6.335526
-685.756928	8.274529	6.345523
-684.001810	14.456216	6.355520
-681.631619	12.853815	6.365517
-679.915075	6.668285	6.375514
-678.434429	16.889885	6.385510
-676.475172	13.415915	6.395507
-674.059072	8.479566	6.405504
-672.399928	7.513392	6.415501
-670.863494	3.022328	6.425498
-668.889516	17.762691	6.435494
-666.908752	7.598895	6.445491
-664.859422	9.732799	6.455488
-663.347757	7.454496	6.465485
-661.268589	15.815326	6.475482
-659.207746	11.647814	6.485478
-657.811659	8.535408	6.495475
-655.962619	13.600078	6.505472
-653.830787	14.486154	6.515469
-651.477361	9.795088	6.525466
-649.983620	8.016993	6.535462
-648.230396	12.929622	6.545459
-646.390170	5.882829	6.555456
-644.472189	9.452380	6.565453
-642.279447	10.049280	6.575450
-640.649738	10.292487	6.585446
-638.799240	12.305036	6.595443
-636.939834	14.311427	6.605440
-635.025532	2.882571	6.615437
-633.104639	5.968540	6.625434
-631.200712	6.679485	6.635430
-629.447261	9.196988	6.645427
-627.582488	6.947547	6.655424
-625.610565	14.820316	6.665421
-623.899846	3.932382	6.675418
-621.858603	9.590013	6.685414
-620.078359	12.065350	6.695411
-618.135646	4.446451	6.705408
-616.265858	13.196015	6.715405
-614.258727	9.573929	6.725402
-612.359820	14.649615	6.735398
-610.650407	13.348631	6.745395
-608.782332	13.852179	6.755392
-606.805547	8.687681	6.765389
-605.143318	11.718691	6.775386
-603.223681	16.170588	6.785382
-601.196120	11.261648	6.795379
-599.488008	15.827863	6.805376
-597.250829	4.093254	6.815373
-595.807518	3.851569	6.825370
-593.754111	8.889955	6.835366
-592.038230	12.845500	6.845363
-590.090330	11.473275	6.855360
-588.094051	1.676510	6.865357
-586.297266	11.610843	6.875354
-584.250907	5.541623	6.885350
-582.319969	8.029228	6.895347
-580.547310	9.378513	6.905344
-578.985037	9.013630	6.915341
-576.900968	5.930300	6.925338
-575.022454	7.273730	6.935334
-573.120303	13.217295	6.945331
-571.082876	9.989851	6.955328
-569.359914	8.574634	6.965325
-567.368139	6.094965	6.975322
-565.784620	6.817677	6.985318
-563.867450	17.132249	6.995315
-561.722595	1.852125	7.005312
-560.106377	0.854994	7.015309
-558.121218	7.394742	7.025306
-556.300209	2.070445	7.035302
-554.215289	3.155145	7.045299
-552.463297	11.939371	7.055296
-550.713686	4.790286	7.065293
-548.810810	13.858288	7.075290
-546.780156	6.798512	7.085286
-545.027156	8.092547	7.095283
-542.963970	4.452092	7.105280
-540.973142	-5.758998	7.115277
-539.482248	3.638481	7.125274
-537.396104	4.509857	7.135270
-535.748479	10.239916	7.145267
-533.643935	-0.767707	7.155264
-531.905886	-2.245302	7.165261
-529.815441	-2.808197	7.175258
-527.773490	1.619486	7.185254
-526.499401	-0.488160	7.195251
-524.295448	2.115346	7.205248
-522.519322	0.660095	7.215245
-520.566923	-1.022246	7.225242
-518.667360	-4.609703	7.235238
-516.849374	6.514906	7.245235
-514.960774	-1.185266	7.255232
-513.133818	0.100137	7.265229
-511.223260	-6.514134	7.275226
-509.357900	-0.908832	7.285222
-507.371075	4.306045	7.295219
-505.553942	-3.840568	7.305216
-503.691252	-5.082279	7.315213
-501.706806	0.199293	7.325210
-499.836285	-1.804668	7.335206
-498.473969	-0.066118	7.345203
-496.683908	2.393536	7.355200
-494.170137	1.542021	7.365197
-492.425375	0.500721	7.375194
-490.327623	-0.360128	7.385190
-488.411946	-4.422211	7.395187
-486.838747	3.629618	7.405184
-484.931123	0.830320	7.415181
-483.025745	-3.419575	7.425178
-481.154413	-0.115578	7.435174
-479.199520	-4.619677	7.445171
-477.414863	3.988874	7.455168
-475.478305	2.863274	7.465165
-473.642682	5.342510	7.475162
-472.069055	3.228102	7.485158
-470.087908	-4.112631	7.495155
-467.878464	1.444070	7.505152
-466.081541	7.625569	7.515149
-464.277019	8.453571	7.525146
-462.246562	11.072216	7.535142
-460.717493	4.436802	7.545139
-458.894725	13.244538	7.555136
-456.735867	1.451505	7.565133
-454.592841	7.579319	7.575130
-452.993831	18.791067	7.585126
-451.529924	11.862923	7.595123
-449.040890	8.200323	7.605120
-447.229605	5.269606	7.615117
-445.664525	4.350186	7.625114
-444.132849	8.758391	7.635110
-441.476063	13.225328	7.645107
-439.710842	9.218884	7.655104
-437.808451	9.289219	7.665101
-436.004064	2.354081	7.675098
-434.524969	8.223226	7.685094
-432.516321	10.308573	7.695091
-430.455126	6.311709	7.705088
-428.477182	12.146985	7.715085
-426.980953	11.786432	7.725082
-424.832972	11.162339	7.735078
-422.717596	8.550951	7.745075
-421.105843	8.410359	7.755072
-419.474114	3.757395	7.765069
-417.552475	10.642131	7.775066
-415.540000	12.232702	7.785062
-413.431270	5.223717	7.795059
-411.801787	13.921841	7.805056
-409.788902	4.002561	7.815053
-407.820355	6.185905	7.825050
-406.074032	8.237378	7.835046
-404.247115	9.492875	7.845043
-402.203929	6.520424	7.855040
-400.441663	13.934277	7.865037
-398.569778	5.981079	7.875034
-396.894423	6.717660	7.885030
-394.899334	15.540566	7.895027
-393.090911	11.978805	7.905024
-391.283620	10.171325	7.915021
-389.399000	5.178018	7.925018
-387.183116	0.640209	7.935014
-385.739285	9.337996	7.945011
-383.492854	1.495522	7.955008
-381.379078	1.115335	7.965005
-380.039759	15.106322	7.975002
-377.857741	5.761599	7.984998
-376.010796	17.715349	7.994995
-374.334687	11.629625	8.004992
-372.353962	2.313891	8.014989
-370.408640	5.021994	8.024986
-368.365244	12.348357	8.034982
-366.868748	2.843116	8.044979
-364.960170	1.303678	8.054976
-363.080915	9.925644	8.064973
-361.185065	10.601784	8.074970
-359.208362	5.235399	8.084966
-357.048840	4.775302	8.094963
-355.465090	6.647519	8.104960
-353.695972	8.332258	8.114957
-351.596219	4.206152	8.124954
-349.758584	7.555111	8.134950
-348.144606	7.884710	8.144947
-345.764370	6.652064	8.154944
-344.171763	7.572408	8.164941
-342.420135	7.802671	8.174938
-340.258346	6.788053	8.184934
-338.926275	2.997666	8.194931
-336.861411	0.621770	8.204928
-334.783820	4.750273	8.214925
-332.898452	1.103646	8.224922
-331.115207	5.143364	8.234918
-328.953585	5.895513	8.244915
-327.142897	7.662050	8.254912
-325.436227	0.363664	8.264909
-323.576770	11.666552	8.274906
-321.743930	16.759350	8.284902
-319.966690	10.518576	8.294899
-317.669840	11.381770	8.304896
-316.009934	4.027700	8.314893
-314.279722	9.092677	8.324890
-312.637471	17.520438	8.334886
-310.486776	9.554367	8.344883
-308.544028	11.452985	8.354880
-306.593310	14.806031	8.364877
-304.767216	9.645296	8.374874
-303.100312	6.650895	8.384870
-300.811488	14.001297	8.394867
-298.890027	5.462395	8.404864
-297.394618	7.405593	8.414861
-295.760684	12.823829	8.424858
-293.132771	8.071913	8.434854
-291.607970	12.175025	8.444851
-289.860019	-1.783196	8.454848
-287.784637	6.843841	8.464845
-285.960748	6.653688	8.474842
-284.103962	2.028037	8.484838
-282.384919	7.499006	8.494835
-280.690198	10.618219	8.504832
-278.575724	3.158454	8.514829
-276.415159	1.943573	8.524826
-274.856769	9.410597	8.534822
-272.965302	5.208864	8.544819
-270.897847	10.319510	8.554816
-269.241322	16.356227	8.564813
-266.953860	11.966557	8.574810
-265.354486	16.375134	8.584807
-263.503112	13.038700	8.594803
-261.616254	7.487794	8.604800
-259.712783	3.789387	8.614797
-258.168817	11.340826	8.624794
-256.494273	12.401300	8.634791
-253.761361	5.531217	8.644787
-252.249679	9.368045	8.654784
-250.526063	3.650585	8.664781
-248.625984	6.564947	8.674778
-246.660665	8.794730	8.684775
-244.591077	8.860636	8.694771
-242.866405	15.188056	8.704768
-241.003344	6.900080	8.714765
-239.104958	4.004555	8.724762
-237.123063	5.873301	8.734759
-235.301130	7.278136	8.744755
-233.385798	4.594635	8.754752
-231.562016	6.959118	8.764749
-230.086864	7.658302	8.774746
-228.054225	8.906363	8.784743
-225.959129	13.711079	8.794739
-223.941785	6.336328	8.804736
-222.262909	8.866043	8.814733
-220.239413	-1.607386	8.824730
-218.556205	14.060827	8.834727
-216.444249	3.366448	8.844723
-214.753172	9.640832	8.854720
-212.722585	7.003684	8.864717
-211.100155	5.716863	8.874714
-209.144798	5.504207	8.884711
-207.322018	9.905587	8.894707
-205.419158	8.343502	8.904704
-202.974303	3.990347	8.914701
-201.193928	7.744855	8.924698
-200.111041	10.680738	8.934695
-198.233106	4.098735	8.944691
-195.952205	2.964189	8.954688
-194.035310	7.385292	8.964685
-192.290005	4.337403	8.974682
-190.131470	-1.432058	8.984679
-188.473311	8.611576	8.994675
-186.602619	14.487868	9.004672
-184.735705	11.403207	9.014669
-182.763274	11.694659	9.024666
-180.939043	14.460140	9.034663
-179.299903	8.094668	9.044659
-177.261102	3.672137	9.054656
-175.564554	7.343733	9.064653
-173.319386	2.048324	9.074650
-171.585313	6.623351	9.084647
-169.631647	4.967928	9.094643
-167.913566	5.620488	9.104640
-166.027406	-1.670127	9.114637
-163.999809	-1.074851	9.124634
-162.001026	2.723774	9.134631
-160.198506	-1.672087	9.144627
-158.468719	2.298933	9.154624
-156.372919	7.746191	9.164621
-154.713275	3.922572	9.174618
-152.809799	5.053948	9.184615
-151.074327	6.698421	9.194611
-149.274914	-1.353555	9.204608
-147.146706	0.632435	9.214605
-145.320992	0.686819	9.224602
-143.619660	2.654094	9.234599
-141.425231	5.104757	9.244595
-139.620456	-1.048711	9.254592
-137.553084	-3.623776	9.264589
-135.769577	6.570413	9.274586
-134.167433	-0.573813	9.284583
-132.505489	3.595936	9.294579
-130.239065	5.280431	9.304576
-128.486216	4.380198	9.314573
-126.640632	-0.721943	9.324570
-124.565060	0.552510	9.334567
-122.924788	2.142725	9.344563
-120.955125	-1.768232	9.354560
-119.027165	9.670742	9.364557
-117.002502	4.776859	9.374554
-115.428026	-0.613575	9.384551
-113.601401	3.646747	9.394547
-111.342638	-2.206531	9.404544
-109.569415	3.244873	9.414541
-107.762257	3.973258	9.424538
-106.172640	1.597599	9.434535
-103.910074	9.823917	9.444531
-101.865435	4.489517	9.454528
-100.652307	9.045093	9.464525
-98.328914	6.299744	9.474522
-96.460517	7.804636	9.484519
-94.663608	9.603549	9.494515
-92.966776	5.889291	9.504512
-91.081441	11.319669	9.514509
-88.777086	8.206336	9.524506
-87.343523	12.982525	9.534503
-85.379137	11.743853	9.544499
-82.942323	9.493549	9.554496
-81.630644	8.685840	9.564493
-79.794263	13.623542	9.574490
-77.906195	15.202674	9.584487
-75.878402	13.903370	9.594483
-73.866743	6.395436	9.604480
-71.994149	6.987101	9.614477
-70.317706	8.819462	9.624474
-68.587320	7.561298	9.634471
-66.631839	5.504638	9.644467
-64.798988	-1.082707	9.654464
-62.749092	1.286884	9.664461
-60.728379	4.932108	9.674458
-59.262635	6.865982	9.684455
-57.009455	-0.153131	9.694451
-55.006710	6.284797	9.704448
-53.430774	10.872514	9.714445
-51.863140	7.186789	9.724442
-49.781906	11.520223	9.734439
-47.664092	4.702701	9.744435
-45.804434	8.267850	9.754432
-43.849479	9.984750	9.764429
-42.249510	6.619116	9.774426
-40.397174	2.968502	9.784423
-38.356433	2.592372	9.794419
-36.490875	6.019226	9.804416
-34.597963	6.126128	9.814413
-32.841048	5.932641	9.824410
-30.913831	14.343579	9.834407
-28.889105	7.744592	9.844403
-27.173171	10.786401	9.854400
-25.273204	7.780265	9.864397
-23.403498	6.435175	9.874394
-21.536932	9.888722	9.884391
-19.574752	14.725884	9.894387
-17.727684	13.401777	9.904384
-15.587004	4.673376	9.914381
-13.754627	4.804161	9.924378
-12.502970	8.753676	9.934375
-10.555921	6.003709	9.944371
-8.252846	2.072809	9.954368
-6.346373	1.915480	9.964365
-4.699802	7.281389	9.974362
-3.641283	32.424693	9.984359
-2.036829	69.707647	9.994355
-0.813207	123.678479	10.004352
0.000000	176.605267	10.009357
1.157754	211.604931	10.014362
1.053563	258.779085	10.019367
1.840767	279.622618	10.024371
2.084280	310.534475	10.029376
2.507604	334.107344	10.034381
3.173379	353.622130	10.039386
2.806633	370.267736	10.044391
2.903082	377.315148	10.049395
3.037835	385.237926	10.054400
3.046691	396.132705	10.059405
3.459484	422.167326	10.064410
3.514011	435.048025	10.069415
3.828622	434.337104	10.074419
3.691530	450.354838	10.079424
3.696179	459.031661	10.084429
3.748529	440.846557	10.089434
3.634661	458.497400	10.094439
4.023968	466.116279	10.099443
4.124407	489.211072	10.104448
4.008241	488.250331	10.109453
4.283642	483.128801	10.114458
4.250258	499.111124	10.119463
4.055451	501.933266	10.124467
3.896328	505.919768	10.129472
4.176786	502.953032	10.134477
4.675343	509.509031	10.139482
4.146676	508.833274	10.144487
4.676469	506.107452	10.149491
4.425898	532.054128	10.154496
5.010942	537.667555	10.159501
4.875586	527.734203	10.164506
4.666836	525.906745	10.169511
4.928624	526.683368	10.174515
4.685783	544.597729	10.179520
4.810047	543.869858	10.184525
4.810501	551.539771	10.189530
5.022370	565.357394	10.194535
4.839940	564.153337	10.199539
5.239179	567.774834	10.204544
4.901005	563.214756	10.209549
4.882709	569.837457	10.214554
4.754586	571.035810	10.219559
5.046355	565.662492	10.224563
5.333994	573.912635	10.229568
5.191075	580.347069	10.234573
5.383791	572.863891	10.239578
5.198219	583.783517	10.244583
5.444135	580.382321	10.249587
5.535385	598.992484	10.254592
5.616729	604.381941	10.259597
5.825442	611.938245	10.264602
5.584764	616.753043	10.269607
5.806039	610.184623	10.274611
5.580844	613.634509	10.279616
5.407668	618.044316	10.284621
5.911675	604.076135	10.289626
5.489229	619.190279	10.294631
5.579847	624.029503	10.299635
5.697113	617.949164	10.304640
5.625730	617.865912	10.309645
5.552227	616.083098	10.314650
5.989648	649.000528	10.319655
6.153918	649.026338	10.324659
6.304727	660.855854	10.329664
6.069915	671.510595	10.334669
6.593663	668.139177	10.339674
6.456724	665.510215	10.344679
6.135612	678.050515	10.349683
6.044427	676.056055	10.354688
6.176352	675.995564	10.359693
6.380067	675.169861	10.364698
6.210524	682.666692	10.369703
6.477450	671.981541	10.374707
6.151829	686.443239	10.379712
6.404936	683.195410	10.384717
6.573582	691.321102	10.389722
6.495254	712.804782	10.394727
6.613983	715.554876	10.399731
6.704149	716.171233	10.404736
6.707761	717.829544	10.409741
6.576414	714.091113	10.414746
6.386504	725.443610	10.419751
6.785823	717.906902	10.424755
6.725879	737.310893	10.429760
6.677765	746.153995	10.434765
7.015577	755.714541	10.439770
6.632946	775.546937	10.444775
7.071286	764.120032	10.449779
6.964376	763.857946	10.454784
7.135680	766.730548	10.459789
7.436397	766.218942	10.464794
7.016570	766.309538	10.469799
7.320246	780.951642	10.474803
7.386607	795.544885	10.479808
7.098607	805.777709	10.484813
7.333345	803.362244	10.489818
7.357429	805.914568	10.494823
7.611073	803.084510	10.499827
7.421734	813.569679	10.504832
7.332766	806.987581	10.509837
7.507356	812.245550	10.514842
7.539142	839.948582	10.519847
7.713462	835.797093	10.524851
8.098579	846.102345	10.529856
7.767906	843.665101	10.534861
8.146099	849.732685	10.539866
8.147489	854.756527	10.544871
8.050761	852.568965	10.549875
8.114612	855.009299	10.554880
8.327873	850.771171	10.559885
8.369762	845.983225	10.564890
8.201461	856.502914	10.569895
8.556906	845.489708	10.574899
8.708396	848.928449	10.579904
8.211090	859.623621	10.584909
8.547274	847.109097	10.589914
8.136095	859.867342	10.594919
8.193839	862.967808	10.599923
8.151775	857.734363	10.604928
8.400965	861.655832	10.609933
8.280936	853.039700	10.614938
8.195360	883.049656	10.619943
8.571193	890.240408	10.624947
8.824170	894.561822	10.629952
8.514759	897.954246	10.634957
8.853497	895.072752	10.639962
8.452895	902.849400	10.644967
8.621956	905.440116	10.649971
8.709214	906.782335	10.654976
8.903732	917.442889	10.659981
9.211461	925.951800	10.664986
8.893160	945.267971	10.669991
9.108789	938.671919	10.674995
9.180450	940.325708	10.680000
9.018778	948.165193	10.685005
9.375759	943.419994	10.690010
8.940614	944.616888	10.695015
9.229411	946.217120	10.700019
9.056216	955.558113	10.705024
9.228441	950.900728	10.710029
9.888964	964.927863	10.715034
9.622983	967.565907	10.720039
9.621888	966.536316	10.725043
9.789967	974.299562	10.730048
9.508514	979.515218	10.735053
9.565046	983.226179	10.740058
9.580653	986.349162	10.745063
9.569115	980.276602	10.750067
9.825032	985.054887	10.755072
9.845110	985.086353	10.760077
10.063107	976.130803	10.765082
9.640721	983.769044	10.770087
9.948440	993.522203	10.775091
9.901143	986.398793	10.780096
9.540858	988.315451	10.785101
9.558940	1004.872013	10.790106
9.838183	1025.859153	10.795111
9.885669	1018.728493	10.800115
10.379375	1035.124068	10.805120
10.361011	1030.802987	10.810125
10.669283	1011.491407	10.815130
10.335957	1026.564950	10.820135
10.256659	1033.558713	10.825139
10.605990	1029.363484	10.830144
10.518290	1024.539379	10.835149
10.759180	1033.678755	10.840154
10.462285	1047.559068	10.845159
10.834418	1043.182002	10.850163
10.659702	1047.461297	10.855168
10.613098	1063.834280	10.860173
10.894426	1054.661999	10.865178
10.801441	1050.482124	10.870183
11.019336	1049.048591	10.875187
10.951710	1049.404705	10.880192
10.892290	1049.600238	10.885197
11.112543	1047.049849	10.890202
11.099070	1051.273463	10.895207
11.135659	1054.517693	10.900211
11.165125	1057.507594	10.905216
10.688404	1059.092751	10.910221
11.381434	1043.515474	10.915226
11.050730	1064.432805	10.920231
11.029366	1068.339139	10.925235
11.403302	1083.326734	10.930240
11.230939	1080.356418	10.935245
11.367037	1087.483007	10.940250
11.149725	1091.247138	10.945255
11.661550	1096.153375	10.950259
11.870935	1096.569383	10.955264
11.491973	1104.684885	10.960269
11.655106	1097.852708	10.965274
11.548146	1101.343772	10.970279
11.782502	1099.519678	10.975283
11.708837	1093.067472	10.980288
11.547503	1096.707558	10.985293
11.835422	1105.782708	10.990298
11.857939	1118.074609	10.995303
12.068519	1130.183557	11.000307
12.379521	1137.427352	11.005312
12.206533	1128.037333	11.010317
12.410901	1126.236942	11.015322
12.328612	1131.624311	11.020327
12.027331	1116.549334	11.025331
12.433326	1133.291750	11.030336
12.233022	1132.148842	11.035341
12.774387	1130.354621	11.040346
12.217140	1143.472305	11.045351
12.684909	1139.035802	11.050355
13.010727	1142.244956	11.055360
12.168360	1128.306528	11.060365
12.564573	1131.640069	11.065370
12.501581	1136.019841	11.070375
12.607717	1140.675412	11.075379
12.712266	1135.462636	11.080384
12.506655	1142.359905	11.085389
12.675216	1137.125879	11.090394
12.563249	1139.610075	11.095399
12.505836	1151.492129	11.100403
12.544337	1144.476382	11.105408
12.611362	1164.204467	11.110413
12.986866	1170.687357	11.115418
13.043739	1182.475512	11.120423
12.815267	1181.051664	11.125427
12.901138	1184.499375	11.130432
13.109564	1180.235114	11.135437
13.371045	1182.732291	11.140442
13.385683	1184.868293	11.145447
13.304580	1192.139966	11.150451
13.281217	1189.254671	11.155456
13.071791	1189.657061	11.160461
13.233438	1189.989223	11.165466
13.338639	1198.517985	11.170471
13.309598	1209.145027	11.175475
13.480149	1211.943721	11.180480
13.779733	1208.262582	11.185485
14.196136	1193.287516	11.190490
14.114246	1210.342810	11.195495
14.221494	1203.495843	11.200499
14.526152	1190.902474	11.205504
13.833771	1175.542886	11.210509
13.959028	1179.460556	11.215514
14.063071	1173.788950	11.220519
13.931674	1182.388558	11.225523
14.017489	1179.785473	11.230528
13.982901	1175.496898	11.235533
14.326194	1174.327204	11.240538
14.069415	1181.420311	11.245543
14.087209	1182.456667	11.250547
14.363892	1206.111121	11.255552
14.465808	1207.345374	11.260557
14.804559	1203.240093	11.265562
14.510909	1193.777813	11.270567
14.236482	1189.559029	11.275571
14.180323	1195.858470	11.280576
14.126806	1203.065824	11.285581
14.389548	1206.110011	11.290586
14.388404	1217.429628	11.295591
14.555993	1203.850430	11.300595
14.798562	1211.685501	11.305600
14.546524	1215.275429	11.310605
14.574077	1219.938830	11.315610
14.472325	1226.581450	11.320615
14.651579	1222.332869	11.325619
14.456438	1231.773735	11.330624
14.587949	1247.084023	11.335629
15.266029	1251.736712	11.340634
15.103787	1248.152882	11.345639
15.130460	1245.556065	11.350643
15.709257	1238.618096	11.355648
15.056778	1249.940705	11.360653
15.373458	1251.047664	11.365658
15.364072	1251.533267	11.370663
15.391584	1247.666855	11.375667
15.784036	1255.485928	11.380672
15.547170	1258.180880	11.385677
15.620608	1238.736144	11.390682
15.335448	1252.002916	11.395687
15.196027	1256.801773	11.400691
15.661330	1258.574162	11.405696
15.397508	1257.922351	11.410701
15.387262	1249.892452	11.415706
15.401364	1255.296031	11.420711
15.468892	1259.535171	11.425715
15.504416	1252.120873	11.430720
15.587796	1271.619413	11.435725
16.041573	1268.763652	11.440730
16.146005	1285.825585	11.445735
15.903856	1279.338669	11.450739
16.409938	1278.247082	11.455744
16.338721	1279.128906	11.460749
16.388436	1272.306853	11.465754
16.405661	1261.932338	11.470759
16.385165	1238.744663	11.475763
16.144511	1238.584326	11.480768
16.049712	1246.965244	11.485773
16.321303	1245.201425	11.490778
16.416457	1255.453874	11.495783
16.170061	1271.357482	11.500787
16.639822	1276.201105	11.505792
16.376289	1281.245274	11.510797
16.786821	1286.226082	11.515802
16.535452	1277.748919	11.520807
16.759381	1280.690502	11.525811
16.640451	1264.260049	11.530816
16.436940	1274.104405	11.535821
16.838616	1267.953199	11.540826
17.066189	1266.601680	11.545831
16.994368	1281.901860	11.550835
17.317353	1268.553285	11.555840
17.205553	1272.005738	11.560845
17.406840	1260.155782	11.565850
17.068527	1260.665464	11.570855
16.974797	1251.469306	11.575859
17.030930	1253.335345	11.580864
16.946430	1268.205443	11.585869
17.296260	1266.963735	11.590874
17.046266	1274.814329	11.595879
17.023545	1278.320385	11.600883
17.214190	1275.229047	11.605888
17.276955	1271.957833	11.610893
17.238757	1279.273169	11.615898
16.988298	1281.691169	11.620903
17.298277	1264.727096	11.625907
17.388892	1286.769734	11.630912
17.511217	1303.727909	11.635917
17.740319	1309.880972	11.640922
18.222418	1300.947753	11.645927
17.712145	1295.637442	11.650931
17.890338	1305.279008	11.655936
18.196646	1302.471995	11.660941
18.168777	1273.270857	11.665946
18.118038	1283.630176	11.670951
17.809403	1280.903907	11.675955
18.169734	1262.528299	11.680960
17.844787	1280.833558	11.685965
17.948974	1274.947422	11.690970
17.941190	1285.280967	11.695975
18.103028	1297.607569	11.700979
18.273390	1303.156556	11.705984
18.102651	1312.440615	11.710989
18.291716	1304.382047	11.715994
18.276771	1313.291169	11.720999
18.542380	1303.411600	11.726003
18.671220	1301.907091	11.731008
18.193869	1310.541455	11.736013
18.452375	1312.652770	11.741018
18.183491	1308.614419	11.746023
18.343761	1318.407088	11.751027
18.487310	1315.484106	11.756032
18.378149	1308.799342	11.761037
18.931852	1311.672561	11.766042
18.527040	1312.278009	11.771047
18.727195	1325.469014	11.776051
18.974093	1334.121913	11.781056
18.817740	1342.474856	11.786061
19.318722	1335.624949	11.791066
19.226143	1341.867184	11.796071
19.400337	1328.110194	11.801075
19.404530	1315.386445	11.806080
18.744142	1311.659702	11.811085
18.874698	1312.465189	11.816090
18.900284	1328.702375	11.821095
19.110454	1327.946571	11.826099
19.616508	1328.143376	11.831104
19.502304	1340.145031	11.836109
19.685990	1326.738196	11.841114
19.571335	1328.376016	11.846119
19.575767	1336.156098	11.851123
19.677035	1337.150764	11.856128
19.403404	1331.708075	11.861133
19.550159	1319.018354	11.866138
19.597730	1342.452530	11.871143
19.993518	1328.053058	11.876147
19.810479	1315.463253	11.881152
19.630981	1341.698087	11.886157
19.726428	1330.643983	11.891162
19.864760	1328.262734	11.896167
19.855644	1324.656038	11.901171
19.712671	1332.376050	11.906176
19.503196	1340.201292	11.911181
19.883424	1322.372800	11.916186
19.898066	1331.868580	11.921191
20.142904	1348.556526	11.926195
20.653274	1355.722900	11.931200
20.469588	1357.614589	11.936205
19.917205	1333.850845	11.941210
20.763883	1351.917275	11.946215
20.574607	1348.776132	11.951219
20.318512	1335.174503	11.956224
20.534270	1330.866451	11.961229
20.833379	1325.474338	11.966234
20.478575	1321.495419	11.971239
20.590079	1327.848601	11.976243
20.951379	1319.062374	11.981248
20.391518	1328.722329	11.986253
20.593468	1335.515257	11.991258
20.616863	1348.934754	11.996263
20.667811	1358.659731	12.001267
20.572283	1365.686205	12.006272
20.302878	1371.023083	12.011277
20.643182	1354.768441	12.016282
20.739075	1363.907500	12.021287
20.743760	1363.939845	12.026291
21.019320	1357.405010	12.031296
21.237972	1357.305453	12.036301
21.000261	1362.492190	12.041306
21.119691	1360.519235	12.046311
20.826292	1359.247652	12.051315
21.274190	1357.961910	12.056320
20.908979	1374.658881	12.061325
21.028205	1374.223516	12.066330
21.199982	1370.269404	12.071335
21.116408	1365.319945	12.076339
21.265974	1360.650275	12.081344
20.871243	1374.202721	12.086349
21.059029	1358.267298	12.091354
21.094686	1360.472514	12.096359
20.867326	1341.384708	12.101363
21.041230	1329.297785	12.106368
20.825946	1334.873603	12.111373
21.174325	1326.026354	12.116378
20.918937	1335.901104	12.121383
20.980467	1335.730414	12.126387
21.045619	1323.935236	12.131392
20.769032	1327.877618	12.136397
20.682512	1315.117875	12.141402
20.874390	1332.262111	12.146407
20.735892	1325.834336	12.151411
20.962515	1335.752053	12.156416
20.876364	1332.252261	12.161421
20.791594	1331.571887	12.166426
21.046491	1329.337628	12.171431
20.925987	1339.835850	12.176435
21.215772	1332.615925	12.181440
20.990742	1330.863500	12.186445
21.325298	1325.774820	12.191450
21.051096	1339.606058	12.196455
20.950532	1339.532186	12.201459
21.153185	1330.531557	12.206464
21.104334	1325.754772	12.211469
21.220524	1328.689895	12.216474
21.273102	1335.946626	12.221479
21.053749	1332.956943	12.226483
21.102677	1328.558806	12.231488
20.893776	1322.008218	12.236493
21.029473	1313.800460	12.241498
20.962269	1308.599247	12.246503
21.167992	1308.449713	12.251507
21.173886	1298.058055	12.256512
20.756403	1316.624128	12.261517
20.703415	1321.798733	12.266522
21.042637	1297.364546	12.271527
21.113156	1306.897130	12.276531
21.613386	1306.109254	12.281536
21.413523	1316.552308	12.286541
21.386678	1298.072828	12.291546
21.040067	1295.180723	12.296551
21.010099	1301.073904	12.301555
21.197428	1289.513159	12.306560
20.887295	1281.680887	12.311565
21.011208	1276.597438	12.316570
21.221561	1275.570368	12.321575
20.895536	1267.265970	12.326579
20.992691	1269.582790	12.331584
20.805355	1279.459263	12.336589
20.903549	1271.609176	12.341594
20.681083	1275.793650	12.346599
20.622940	1278.958422	12.351603
20.894943	1270.446669	12.356608
20.729429	1282.857012	12.361613
20.788592	1275.224463	12.366618
21.021931	1288.470067	12.371623
20.705610	1291.240777	12.376627
20.850443	1301.105284	12.381632
21.043870	1308.538234	12.386637
20.999975	1306.072512	12.391642
21.365809	1299.010787	12.396647
20.855535	1292.456243	12.401651
20.627387	1279.471536	12.406656
20.742735	1283.682555	12.411661
20.704754	1283.303807	12.416666
21.192635	1304.907789	12.421671
20.821764	1308.086178	12.426675
21.088560	1302.554146	12.431680
20.877995	1283.796478	12.436685
20.706594	1285.485922	12.441690
21.168665	1279.910135	12.446695
20.824167	1278.728713	12.451699
21.059451	1271.840790	12.456704
20.813432	1276.114178	12.461709
20.583571	1284.136609	12.466714
21.182050	1287.922057	12.471719
21.099196	1305.204701	12.476723
21.043064	1286.909682	12.481728
20.803342	1290.234308	12.486733
20.571582	1280.266929	12.491738
20.583029	1290.922267	12.496743
20.757791	1311.904412	12.501747
21.113209	1310.805315	12.506752
21.071500	1311.163609	12.511757
21.095981	1305.753805	12.516762
20.865978	1290.668852	12.521767
20.736947	1284.627520	12.526771
20.816133	1296.984652	12.531776
20.726226	1305.314360	12.536781
21.009577	1309.068075	12.541786
21.397945	1318.191994	12.546791
20.909380	1308.204055	12.551795
21.302651	1285.349282	12.556800
21.207814	1280.280222	12.561805
20.971037	1291.416706	12.566810
20.790820	1286.824892	12.571815
20.784278	1289.137755	12.576819
21.006552	1287.233563	12.581824
20.948285	1296.723603	12.586829
20.907512	1293.208697	12.591834
21.008283	1283.910529	12.596839
20.857269	1285.398024	12.601843
21.051667	1285.221910	12.606848
20.863630	1278.975524	12.611853
20.780395	1296.835391	12.616858
20.891278	1293.083404	12.621863
20.969344	1294.862371	12.626867
21.196517	1280.625460	12.631872
21.060746	1289.705228	12.636877
20.949667	1281.013295	12.641882
20.834284	1292.344886	12.646887
20.574496	1294.157241	12.651891
20.986152	1296.226779	12.656896
21.135049	1293.798119	12.661901
20.862459	1289.228923	12.666906
21.012272	1287.866152	12.671911
20.961375	1288.643809	12.676915
21.342282	1286.977668	12.681920
20.917946	1296.286397	12.686925
20.656177	1301.100053	12.691930
21.014287	1283.645725	12.696935
20.970205	1294.965945	12.701939
20.972061	1306.649435	12.706944
20.841279	1297.123261	12.711949
21.116545	1299.624568	12.716954
20.941734	1306.482308	12.721959
20.781630	1291.055041	12.726963
21.277744	1289.137132	12.731968
21.215120	1296.636149	12.736973
21.019635	1288.170566	12.741978
20.857331	1280.986506	12.746983
20.433993	1280.192978	12.751987
20.941463	1281.934991	12.756992
20.966599	1289.033647	12.761997
21.152993	1294.848159	12.767002
20.971124	1286.621683	12.772007
20.643141	1280.056992	12.777011
21.112478	1284.339284	12.782016
21.134610	1291.080447	12.787021
20.918194	1276.277197	12.792026
21.125811	1263.437466	12.797031
20.674733	1275.212100	12.802035
20.691003	1271.194508	12.807040
20.792547	1266.862115	12.812045
20.848598	1272.538134	12.817050
20.836225	1278.775433	12.822055
20.453985	1297.954034	12.827059
21.054672	1300.848143	12.832064
21.013364	1316.558237	12.837069
20.947197	1302.420134	12.842074
21.212258	1305.654787	12.847079
21.014863	1295.174130	12.852083
21.255553	1276.413881	12.857088
20.983218	1288.644146	12.862093
21.112903	1278.497689	12.867098
20.919437	1278.022314	12.872103
20.815397	1275.850046	12.877107
21.022862	1266.922807	12.882112
20.905540	1281.192596	12.887117
20.528766	1283.496702	12.892122
20.840482	1278.643497	12.897127
20.858405	1281.941218	12.902131
20.901051	1266.193052	12.907136
20.799055	1274.425321	12.912141
20.826920	1282.299409	12.917146
21.066628	1280.985378	12.922151
20.939075	1277.613630	12.927155
21.010693	1273.205582	12.932160
20.733712	1270.379647	12.937165
20.867364	1288.594422	12.942170
21.265397	1274.481654	12.947175
20.926055	1276.533780	12.952179
20.837491	1282.827389	12.957184
20.883203	1273.481239	12.962189
20.914928	1271.825064	12.967194
20.938244	1282.909017	12.972199
20.902130	1278.473996	12.977203
21.088100	1272.655242	12.982208
20.661359	1277.015804	12.987213
20.770369	1278.556441	12.992218
20.841341	1277.581565	12.997223
21.163736	1283.554155	13.002227
21.257114	1285.456836	13.007232
20.910074	1295.489683	13.012237
20.841634	1276.203146	13.017242
21.432615	1280.303606	13.022247
20.963119	1284.385557	13.027251
21.083511	1272.362411	13.032256
21.099970	1276.652281	13.037261
21.142165	1277.544400	13.042266
21.477773	1268.407484	13.047271
21.023261	1258.379454	13.052275
20.786684	1248.345055	13.057280
20.934646	1258.379346	13.062285
20.857346	1275.839267	13.067290
20.682755	1246.765665	13.072295
20.757308	1284.555336	13.077299
20.947658	1280.692904	13.082304
20.869632	1284.523178	13.087309
21.050828	1282.254949	13.092314
21.001046	1281.343489	13.097319
20.915316	1291.937057	13.102323
21.119749	1280.239549	13.107328
21.098393	1276.765705	13.112333
21.053067	1267.875632	13.117338
20.983611	1253.810642	13.122343
20.734473	1251.760871	13.127347
21.081937	1254.119766	13.132352
21.092406	1257.664678	13.137357
20.731472	1255.607506	13.142362
21.071460	1253.336032	13.147367
20.810210	1261.044909	13.152371
20.669193	1257.206953	13.157376
21.025250	1261.275491	13.162381
20.937486	1263.902507	13.167386
20.958497	1257.611747	13.172391
20.560368	1262.811421	13.177395
20.800714	1253.164577	13.182400
20.894586	1256.773457	13.187405
20.634481	1261.520602	13.192410
20.979169	1266.858841	13.197415
20.595731	1282.942018	13.202419
21.065853	1281.124451	13.207424
21.183541	1298.975927	13.212429
20.736885	1279.500551	13.217434
21.031107	1270.466430	13.222439
20.640007	1274.837076	13.227443
20.801399	1295.209464	13.232448
20.982087	1304.759167	13.237453
20.712516	1305.436084	13.242458
21.164066	1292.478571	13.247463
21.104490	1308.861785	13.252467
21.100266	1281.886702	13.257472
21.096818	1268.464036	13.262477
20.653916	1266.623367	13.267482
21.076466	1262.007958	13.272487
21.138097	1281.325475	13.277491
21.350735	1255.968518	13.282496
21.267239	1257.038382	13.287501
20.872709	1256.784315	13.292506
21.387548	1265.776064	13.297511
21.423667	1277.102401	13.302515
21.303667	1262.285364	13.307520
21.013425	1243.953622	13.312525
20.754463	1242.059962	13.317530
21.200814	1227.160510	13.322535
20.505896	1241.367847	13.327539
20.552817	1255.966232	13.332544
21.059168	1244.674763	13.337549
21.113717	1261.217917	13.342554
21.447645	1247.262059	13.347559
20.939004	1256.645712	13.352563
20.688749	1245.241532	13.357568
20.692312	1244.518687	13.362573
20.894184	1240.383190	13.367578
20.959328	1235.965147	13.372583
20.579257	1238.354928	13.377587
21.004384	1262.976136	13.382592
20.989566	1250.824762	13.387597
20.476714	1253.087489	13.392602
20.636450	1250.191900	13.397607
20.510415	1271.524743	13.402611
20.797408	1263.624046	13.407616
20.787492	1273.503755	13.412621
20.938776	1280.960759	13.417626
21.458853	1269.741199	13.422631
21.168972	1272.957126	13.427635
21.015133	1263.994476	13.432640
20.896009	1272.401366	13.437645
21.102716	1276.899013	13.442650
21.016746	1259.622781	13.447655
20.842710	1260.394846	13.452659
21.225540	1249.676592	13.457664
20.883986	1253.853247	13.462669
20.832103	1247.533117	13.467674
20.863781	1227.535232	13.472679
20.789322	1248.055561	13.477683
20.694337	1255.487177	13.482688
21.050115	1248.930133	13.487693
20.995188	1252.132234	13.492698
20.721988	1254.624821	13.497703
20.769874	1259.169873	13.502707
21.012143	1266.249654	13.507712
20.960599	1258.188489	13.512717
20.789353	1273.144969	13.517722
21.022713	1269.174754	13.522727
20.879860	1258.297488	13.527731
20.950549	1258.978479	13.532736
21.025838	1268.649050	13.537741
20.883104	1267.411792	13.542746
20.864233	1244.214386	13.547751
21.063688	1249.880139	13.552755
20.811825	1253.186192	13.557760
20.902841	1246.392257	13.562765
20.585175	1247.518394	13.567770
20.760485	1246.804426	13.572775
20.929613	1270.185980	13.577779
20.855452	1264.478107	13.582784
20.695829	1277.781649	13.587789
20.992046	1254.677474	13.592794
20.707185	1271.156504	13.597799
21.167946	1279.841492	13.602803
21.371672	1260.621953	13.607808
21.042565	1263.125035	13.612813
20.684417	1255.618984	13.617818
21.243937	1257.059375	13.622823
20.600976	1249.008970	13.627827
20.620020	1256.745677	13.632832
20.491154	1265.184079	13.637837
20.823269	1273.612036	13.642842
20.850670	1272.369718	13.647847
20.666985	1270.577589	13.652851
21.183969	1268.952825	13.657856
21.209569	1275.348070	13.662861
20.935027	1270.055362	13.667866
21.093897	1258.652148	13.672871
21.275140	1280.863251	13.677875
20.984979	1267.319159	13.682880
20.931748	1253.221619	13.687885
20.805996	1249.576774	13.692890
20.883368	1248.725460	13.697895
20.632218	1255.861861	13.702899
21.089557	1261.137974	13.707904
21.257378	1257.041019	13.712909
20.810259	1252.996419	13.717914
20.989856	1250.696911	13.722919
20.832728	1250.400247	13.727923
20.805963	1248.985219	13.732928
20.788992	1246.232935	13.737933
20.561204	1258.481301	13.742938
21.002887	1265.382616	13.747943
20.952584	1271.398878	13.752947
21.001633	1274.180694	13.757952
21.161687	1281.852345	13.762957
20.763887	1259.547998	13.767962
20.973235	1252.676837	13.772967
20.781251	1263.459222	13.777971
20.640904	1246.330452	13.782976
20.942879	1285.695514	13.787981
21.058072	1258.228336	13.792986
21.030891	1284.448233	13.797991
20.963626	1236.375513	13.802995
20.859321	1260.382566	13.808000
21.069006	1255.457333	13.813005
20.882096	1256.095832	13.818010
20.681936	1248.577200	13.823015
20.998152	1265.138547	13.828019
20.933532	1247.428411	13.833024
20.930287	1252.112505	13.838029
20.767492	1245.672870	13.843034
21.091847	1248.675700	13.848039
20.846253	1257.213141	13.853043
20.902833	1249.812832	13.858048
21.204831	1243.726421	13.863053
20.903799	1247.882418	13.868058
21.254341	1243.122380	13.873063
21.173612	1237.544878	13.878067
20.913078	1247.852478	13.883072
20.716250	1242.649887	13.888077
21.120243	1250.194302	13.893082
21.138773	1242.752757	13.898087
20.988598	1255.244209	13.903091
20.872568	1244.233364	13.908096
20.617771	1236.028011	13.913101
20.705489	1242.823346	13.918106
21.025889	1246.908607	13.923111
21.029852	1239.442578	13.928115
20.854438	1268.079928	13.933120
21.249051	1246.874515	13.938125
20.837543	1245.339503	13.943130
21.059884	1239.650580	13.948135
20.909457	1242.703907	13.953139
20.887761	1242.201136	13.958144
20.876182	1241.099080	13.963149
20.599723	1247.302793	13.968154
20.989570	1246.819536	13.973159
20.760252	1240.516672	13.978163
20.795603	1246.869349	13.983168
20.800145	1244.663996	13.988173
20.639687	1254.323274	13.993178
21.130604	1243.094193	13.998183
20.753640	1250.596016	14.003187
20.758970	1242.286088	14.008192
21.015300	1247.542025	14.013210
20.997542	1247.277432	14.018227
20.903768	1243.424489	14.023245
20.736141	1243.726467	14.028263
21.045390	1248.764025	14.033280
21.046777	1245.204201	14.038298
20.544538	1251.727076	14.043315
21.079978	1247.080100	14.048333
20.694436	1261.667741	14.053351
20.929403	1277.631851	14.058368
21.337029	1290.334449	14.063386
20.896453	1290.355936	14.068403
21.400820	1283.816926	14.073421
21.211001	1284.683988	14.078439
21.060441	1282.387876	14.083456
21.323200	1279.506765	14.088474
21.063875	1293.858812	14.093491
21.255229	1293.870736	14.098509
21.206970	1276.152825	14.103527
20.923324	1301.642103	14.108544
21.153861	1288.812489	14.113562
21.234891	1291.915556	14.118579
21.381280	1287.818238	14.123597
21.170403	1291.206954	14.128615
21.195533	1290.852153	14.133632
21.477022	1285.303473	14.138650
21.323858	1289.403395	14.143667
21.415378	1299.875643	14.148685
21.433696	1295.150694	14.153703
21.384423	1304.679610	14.158720
21.157607	1289.365323	14.163738
21.209595	1297.292548	14.168755
21.170018	1290.906360	14.173773
21.017234	1294.430522	14.178791
21.490594	1294.466674	14.183808
21.529008	1289.902109	14.188826
21.243351	1295.176139	14.193843
21.539274	1310.611488	14.198861
21.574692	1320.380150	14.203879
21.382936	1319.284476	14.208896
21.631852	1326.359224	14.213914
21.802016	1331.541686	14.218931
21.491421	1323.174318	14.223949
21.314469	1335.155408	14.228967
21.522143	1330.030600	14.233984
21.750996	1324.650743	14.239002
21.441648	1331.536125	14.244019
21.532356	1323.648990	14.249037
21.464060	1327.719656	14.254055
21.507656	1327.547517	14.259072
21.739095	1321.921868	14.264090
21.533712	1329.229520	14.269107
22.089291	1338.150771	14.274125
21.989443	1332.482009	14.279143
21.651227	1331.681816	14.284160
21.837364	1338.374917	14.289178
21.822425	1353.428904	14.294195
21.776292	1359.426064	14.299213
21.921136	1355.222012	14.304231
21.696866	1372.778954	14.309248
21.996425	1365.566316	14.314266
22.233789	1370.555611	14.319283
21.981693	1359.257904	14.324301
21.968072	1366.193657	14.329319
21.914975	1375.396053	14.334336
22.162527	1363.724504	14.339354
21.953489	1363.098752	14.344371
21.797198	1353.569504	14.349389
22.209148	1365.846781	14.354407
22.038523	1374.361664	14.359424
22.065104	1365.687244	14.364442
21.969476	1368.315158	14.369459
21.628252	1362.277488	14.374477
21.698694	1371.628484	14.379495
21.856212	1395.973227	14.384512
22.067082	1399.475589	14.389530
22.270379	1405.881277	14.394547
22.532113	1393.537360	14.399565
22.784268	1389.585158	14.404583
22.321045	1393.305146	14.409600
22.272091	1391.330997	14.414618
22.345506	1399.852585	14.419635
22.605086	1398.118649	14.424653
22.639743	1394.348996	14.429671
22.511109	1399.234663	14.434688
22.746954	1389.386452	14.439706
22.527069	1386.829259	14.444723
22.536656	1380.639674	14.449741
22.477400	1359.992989	14.454759
22.255816	1383.273514	14.459776
22.451558	1393.781114	14.464794
22.583071	1399.982754	14.469811
22.860060	1390.238087	14.474829
22.826653	1400.215975	14.479847
22.635713	1397.880669	14.484864
22.788486	1392.682802	14.489882
22.887564	1379.461960	14.494899
22.908769	1383.831386	14.499917
22.938953	1358.678059	14.504935
22.776406	1365.972606	14.509952
22.762286	1361.419543	14.514970
22.850881	1356.735272	14.519987
22.931106	1345.143908	14.525005
22.856445	1352.734302	14.530023
22.924090	1362.652003	14.535040
22.867704	1357.246848	14.540058
22.745530	1363.363099	14.545075
22.529653	1359.631844	14.550093
22.634938	1367.615097	14.555111
22.744303	1368.193780	14.560128
23.075637	1377.732819	14.565146
23.198995	1393.842268	14.570163
23.022369	1369.818264	14.575181
23.024359	1356.773370	14.580199
23.147056	1364.088483	14.585216
22.989149	1352.107251	14.590234
23.012228	1359.759134	14.595251
23.180992	1360.943370	14.600269
23.251086	1347.560446	14.605287
22.856260	1355.390664	14.610304
22.967513	1353.109407	14.615322
22.971685	1373.489551	14.620339
23.071508	1377.506675	14.625357
23.306702	1385.786956	14.630375
23.008386	1400.439471	14.635392
23.364084	1391.429407	14.640410
23.236026	1384.423387	14.645427
23.116252	1397.922753	14.650445
23.281726	1391.848293	14.655463
23.164264	1410.416962	14.660480
23.452095	1394.042093	14.665498
23.656944	1396.875332	14.670515
23.569689	1392.937943	14.675533
23.459537	1393.082898	14.680551
23.612106	1401.665791	14.685568
23.493764	1395.853668	14.690586
23.538227	1399.266173	14.695603
23.174107	1400.975838	14.700621
23.651394	1392.625900	14.705639
23.523055	1401.961433	14.710656
23.157426	1399.836454	14.715674
23.565521	1404.491800	14.720691
23.285806	1393.409249	14.725709
23.335257	1396.610181	14.730727
23.385407	1404.874372	14.735744
23.537164	1392.647093	14.740762
23.709720	1395.435149	14.745779
23.691071	1402.642270	14.750797
23.776695	1384.094370	14.755815
23.640291	1398.302649	14.760832
23.723572	1385.754404	14.765850
23.666402	1387.657344	14.770867
23.559628	1397.377956	14.775885
23.847211	1392.399249	14.780903
23.568862	1391.488834	14.785920
23.745069	1404.661010	14.790938
23.827368	1415.639734	14.795955
23.519438	1424.042844	14.800973
24.096557	1415.035200	14.805991
24.002765	1425.898878	14.811008
23.854340	1416.690793	14.816026
24.063477	1419.150560	14.821043
24.039413	1418.644733	14.826061
23.867538	1414.357479	14.831079
24.000566	1428.060361	14.836096
24.396449	1415.715476	14.841114
24.398635	1415.842513	14.846131
24.174623	1426.881113	14.851149
24.319563	1415.189712	14.856167
24.542786	1399.981271	14.861184
24.098503	1394.584491	14.866202
24.116836	1397.183223	14.871219
23.625843	1396.443572	14.876237
24.059685	1411.067402	14.881255
24.210612	1420.913660	14.886272
24.552069	1413.897228	14.891290
24.702836	1414.192468	14.896307
24.269754	1419.983968	14.901325
24.768241	1401.557375	14.906343
24.379411	1383.155937	14.911360
24.489849	1388.231547	14.916378
24.518839	1375.907465	14.921395
24.451448	1377.381043	14.926413
24.568467	1387.179205	14.931431
24.115730	1395.814601	14.936448
24.033539	1376.857766	14.941466
24.188703	1390.080474	14.946483
24.100731	1410.492670	14.951501
24.558051	1415.258141	14.956519
24.564155	1421.693717	14.961536
24.690090	1420.430962	14.966554
24.495602	1421.018789	14.971571
24.747433	1424.909438	14.976589
24.736316	1413.359329	14.981607
24.462862	1408.702903	14.986624
24.427739	1418.830509	14.991642
24.783344	1416.090286	14.996659
24.489495	1423.968926	15.001677
24.762680	1410.199634	15.006695
24.591283	1410.083807	15.011712
24.579291	1423.120857	15.016730
24.621403	1416.628779	15.021747
24.547934	1424.860791	15.026765
24.756700	1421.761757	15.031783
24.752489	1430.357091	15.036800
25.221325	1440.942285	15.041818
25.195162	1428.924245	15.046835
24.504554	1426.972216	15.051853
25.062886	1441.540042	15.056871
25.163382	1440.864915	15.061888
25.045613	1441.530164	15.066906
25.127094	1423.138599	15.071923
24.743865	1425.634652	15.076941
25.003420	1439.863183	15.081959
24.959310	1445.241879	15.086976
24.822685	1464.680379	15.091994
25.185991	1458.844887	15.097011
25.044954	1453.133885	15.102029
25.331053	1457.755227	15.107047
25.305183	1464.883309	15.112064
25.373039	1458.566425	15.117082
25.374060	1456.784063	15.122099
25.204407	1465.045596	15.127117
25.347314	1453.986821	15.132135
25.638133	1455.131148	15.137152
25.166888	1459.969240	15.142170
25.515873	1439.101603	15.147187
25.382022	1450.662222	15.152205
25.476680	1450.263295	15.157223
25.341556	1450.286396	15.162240
25.431428	1446.119400	15.167258
25.465520	1441.981750	15.172275
24.929199	1451.141724	15.177293
25.117797	1441.870429	15.182311
25.563814	1446.626703	15.187328
25.046919	1460.634619	15.192346
25.407099	1458.312069	15.197363
25.484217	1451.430587	15.202381
25.427619	1445.119402	15.207399
25.645608	1446.415339	15.212416
25.304638	1446.100052	15.217434
25.718463	1467.797627	15.222451
26.050361	1467.923983	15.227469
26.253457	1463.624095	15.232487
26.040313	1448.395546	15.237504
25.922198	1448.359307	15.242522
25.736109	1444.788439	15.247539
25.770952	1434.616767	15.252557
25.677909	1438.222667	15.257575
25.678900	1441.384149	15.262592
25.639087	1443.924526	15.267610
25.763896	1443.146424	15.272627
26.020940	1458.734419	15.277645
26.067725	1469.649637	15.282663
26.091138	1471.898373	15.287680
25.672021	1469.992692	15.292698
26.401293	1466.779168	15.297715
26.132453	1473.491420	15.302733
25.819598	1464.860071	15.307751
26.175111	1463.489911	15.312768
26.190546	1466.806392	15.317786
26.324350	1468.317099	15.322803
26.251728	1459.346997	15.327821
26.361847	1460.012078	15.332839
26.439366	1435.381159	15.337856
26.035383	1446.052091	15.342874
26.344592	1434.027744	15.347891
26.080674	1450.425535	15.352909
25.904551	1456.243702	15.357927
26.221466	1466.827979	15.362944
26.143915	1473.896671	15.367962
26.212009	1469.668650	15.372979
26.294882	1473.657045	15.377997
26.027919	1471.404637	15.383015
26.381091	1469.909012	15.388032
26.120398	1481.420677	15.393050
26.307734	1472.838525	15.398067
26.893226	1474.428193	15.403085
26.484271	1469.365511	15.408103
26.842691	1472.164833	15.413120
26.515050	1476.136912	15.418138
26.724158	1467.628366	15.423155
26.544646	1463.886564	15.428173
26.379935	1472.002599	15.433191
26.659274	1473.403580	15.438208
26.386890	1480.588293	15.443226
26.629976	1468.347956	15.448243
26.600949	1475.361721	15.453261
26.746906	1484.172226	15.458279
26.926303	1494.967215	15.463296
26.486823	1493.300725	15.468314
26.900510	1493.173371	15.473331
26.687517	1505.876052	15.478349
26.736742	1503.299509	15.483367
26.880704	1502.889570	15.488384
26.980028	1505.217435	15.493402
26.955668	1496.588813	15.498419
26.765262	1495.884580	15.503437
26.870721	1509.731931	15.508455
27.201157	1502.283074	15.513472
27.248690	1504.718297	15.518490
26.968350	1495.793889	15.523507
26.785531	1503.184543	15.528525
26.787649	1509.537426	15.533543
27.227407	1499.296405	15.538560
26.792297	1502.025680	15.543578
27.219370	1507.332391	15.548595
26.898242	1497.761702	15.553613
26.942944	1504.488451	15.558631
27.455683	1523.255611	15.563648
27.514650	1519.387669	15.568666
27.325008	1495.485079	15.573683
27.074810	1499.663456	15.578701
27.298988	1509.952680	15.583719
27.679509	1516.001399	15.588736
27.529120	1517.109142	15.593754
27.552011	1507.905132	15.598771
27.386519	1489.040086	15.603789
27.291253	1500.910759	15.608807
27.408724	1524.721004	15.613824
27.493629	1528.081472	15.618842
27.728601	1520.794119	15.623859
27.838819	1531.106254	15.628877
27.578945	1526.678852	15.633895
27.886822	1514.229947	15.638912
27.509041	1506.008464	15.643930
27.555008	1503.471765	15.648947
27.720081	1521.278234	15.653965
27.824811	1523.987473	15.658983
27.690255	1532.940275	15.664000
27.848256	1518.607251	15.669018
28.082905	1519.156520	15.674035
27.738511	1510.549049	15.679053
27.732162	1507.690368	15.684071
27.959073	1504.045746	15.689088
27.656989	1515.820435	15.694106
27.755697	1521.531873	15.699123
28.038170	1526.757838	15.704141
27.679825	1530.719100	15.709159
27.957498	1528.526099	15.714176
28.110891	1522.398457	15.719194
28.043890	1533.073905	15.724211
28.125534	1526.682434	15.729229
28.075571	1525.010439	15.734247
28.099238	1520.751738	15.739264
28.165310	1529.384683	15.744282
28.006406	1532.371920	15.749299
28.359926	1514.440202	15.754317
28.402074	1521.362414	15.759335
28.566543	1530.291114	15.764352
28.273117	1526.495108	15.769370
28.377243	1522.774115	15.774387
28.437929	1528.546674	15.779405
28.223405	1532.546342	15.784423
28.384476	1525.805586	15.789440
28.382064	1528.001822	15.794458
28.205931	1513.014258	15.799475
28.690095	1508.966819	15.804493
28.174417	1517.439298	15.809511
28.251609	1520.242588	15.814528
28.463236	1525.063015	15.819546
28.400286	1510.008639	15.824563
28.653141	1513.584554	15.829581
28.166758	1515.629901	15.834599
28.563673	1517.658626	15.839616
28.234711	1517.503438	15.844634
28.250872	1518.496530	15.849651
28.899800	1523.163838	15.854669
28.455503	1536.131521	15.859687
28.733963	1541.318807	15.864704
28.894010	1544.703473	15.869722
29.061544	1539.193323	15.874739
29.228186	1527.687127	15.879757
28.729043	1523.348224	15.884775
28.880201	1508.365088	15.889792
29.204100	1501.032102	15.894810
29.087725	1516.720617	15.899827
29.445720	1503.032089	15.904845
29.374515	1496.811298	15.909863
29.170942	1501.356606	15.914880
29.006438	1507.931113	15.919898
29.103931	1504.464431	15.924915
29.315281	1503.584436	15.929933
28.870160	1519.023378	15.934951
29.216053	1504.078398	15.939968
29.079010	1503.329474	15.944986
28.769285	1509.535475	15.950003
28.899530	1506.647142	15.955021
28.826069	1506.292332	15.960039
28.974278	1512.919207	15.965056
29.275411	1521.714423	15.970074
29.203365	1538.806852	15.975091
29.280574	1542.810326	15.980109
29.244364	1546.012371	15.985127
29.690648	1543.039017	15.990144
29.601518	1541.936394	15.995162
29.687778	1546.919965	16.000179
29.571229	1522.464566	16.005197
29.458552	1504.387002	16.010215
29.178105	1505.413245	16.015232
29.250983	1534.344360	16.020250
29.162236	1532.661248	16.025267
29.528914	1531.531540	16.030285
29.038576	1548.133864	16.035303
29.580153	1546.487062	16.040320
29.598973	1536.103949	16.045338
29.615871	1550.673306	16.050355
29.703085	1543.192438	16.055373
29.647030	1549.524730	16.060391
29.671537	1551.340734	16.065408
29.814460	1546.388196	16.070426
29.804562	1547.681166	16.075443
29.783030	1534.767275	16.080461
29.837712	1556.984724	16.085479
30.142638	1568.605223	16.090496
30.034334	1551.249688	16.095514
29.457683	1556.590673	16.100531
29.860411	1573.082827	16.105549
29.877375	1576.532793	16.110567
29.999850	1576.846706	16.115584
30.016582	1580.649057	16.120602
30.208907	1573.086917	16.125619
30.393770	1567.037605	16.130637
30.141999	1583.384846	16.135655
29.966070	1575.431567	16.140672
30.360926	1574.467244	16.145690
30.963050	1566.801992	16.150707
30.656341	1558.635208	16.155725
30.451673	1562.387927	16.160743
30.184437	1544.618888	16.165760
30.557976	1528.198738	16.170778
30.102688	1527.200134	16.175795
30.532467	1538.217907	16.180813
30.363724	1546.314178	16.185831
30.349537	1561.452416	16.190848
30.922267	1561.590697	16.195866
30.772715	1565.097105	16.200883
30.517302	1552.677454	16.205901
30.591054	1544.777173	16.210919
30.422254	1539.490550	16.215936
30.468140	1526.057842	16.220954
30.486191	1542.553903	16.225971
30.803939	1544.546497	16.230989
30.939693	1557.803915	16.236007
30.538516	1547.059933	16.241024
30.779582	1540.341017	16.246042
30.473772	1555.303187	16.251059
30.865946	1551.056484	16.256077
30.689138	1566.473915	16.261095
30.591272	1572.484133	16.266112
30.849189	1559.826088	16.271130
30.711805	1570.610313	16.276147
30.861357	1564.185974	16.281165
30.620868	1564.663169	16.286183
30.594176	1565.688266	16.291200
30.784976	1575.133451	16.296218
30.849478	1567.778886	16.301235
30.785461	1567.807948	16.306253
30.856022	1588.007923	16.311271
30.980340	1595.327613	16.316288
30.966103	1595.848944	16.321306
30.932943	1603.000279	16.326323
31.212707	1601.322874	16.331341
31.267757	1596.044569	16.336359
31.450794	1595.213128	16.341376
31.611526	1592.665973	16.346394
31.858355	1594.361581	16.351411
31.374842	1600.611068	16.356429
31.715369	1596.256189	16.361447
31.793831	1592.240404	16.366464
31.300949	1573.502970	16.371482
31.357403	1586.914631	16.376499
31.513501	1586.491744	16.381517
31.503084	1584.898375	16.386535
31.552998	1589.851580	16.391552
31.717490	1596.301295	16.396570
31.546426	1587.096711	16.401587
31.653043	1585.726915	16.406605
31.735787	1589.916705	16.411623
31.427187	1595.633365	16.416640
31.594009	1585.083469	16.421658
31.110147	1588.190187	16.426675
31.533103	1586.287029	16.431693
31.418003	1591.469468	16.436711
31.155042	1602.728340	16.441728
31.792312	1604.265722	16.446746
31.673571	1613.739855	16.451763
31.838626	1608.318161	16.456781
31.735920	1604.516882	16.461799
31.932844	1629.175050	16.466816
32.170481	1604.390893	16.471834
31.687061	1619.068432	16.476851
31.563203	1622.827154	16.481869
31.862840	1598.388614	16.486887
31.947684	1614.090756	16.491904
32.017309	1640.608069	16.496922
32.068136	1646.627634	16.501939
32.309071	1630.316607	16.506957
32.232389	1644.635149	16.511975
32.168885	1647.560004	16.516992
32.308999	1639.518529	16.522010
32.515423	1646.111013	16.527027
32.903130	1633.948142	16.532045
32.511893	1616.706081	16.537063
32.479908	1618.403692	16.542080
32.752616	1599.257828	16.547098
33.044769	1595.958273	16.552115
32.527712	1594.250662	16.557133
32.554504	1601.176935	16.562151
32.424910	1594.032635	16.567168
32.787286	1590.863449	16.572186
32.466918	1604.610501	16.577203
32.336721	1600.829338	16.582221
32.660585	1599.684432	16.587239
32.816754	1597.930788	16.592256
32.776600	1588.741502	16.597274
32.529777	1597.584838	16.602291
32.367495	1609.357753	16.607309
33.213465	1605.711892	16.612327
32.821896	1618.358213	16.617344
33.079254	1627.369683	16.622362
32.983895	1619.782619	16.627379
32.996994	1599.701338	16.632397
33.148694	1597.372694	16.637415
32.854225	1608.611428	16.642432
33.245639	1599.405209	16.647450
33.238412	1586.857068	16.652467
33.151464	1599.586917	16.657485
33.189866	1599.942553	16.662503
32.774838	1597.929239	16.667520
32.941010	1605.509667	16.672538
32.944246	1622.414013	16.677555
33.018957	1628.980307	16.682573
33.008928	1636.595146	16.687591
33.233430	1653.756813	16.692608
33.449981	1637.658875	16.697626
33.545072	1635.389590	16.702643
33.425500	1641.222405	16.707661
33.876285	1629.002288	16.712679
33.545375	1634.227029	16.717696
33.850265	1627.549802	16.722714
33.899144	1636.522172	16.727731
33.727499	1634.314308	16.732749
34.020126	1625.402247	16.737767
33.837942	1610.999125	16.742784
33.575327	1604.583880	16.747802
33.624213	1596.402827	16.752819
33.342257	1597.251569	16.757837
33.787400	1616.846014	16.762855
33.822961	1631.302366	16.767872
33.993078	1626.785899	16.772890
33.920584	1611.492273	16.777907
33.822190	1608.503538	16.782925
34.042119	1598.310095	16.787943
33.731215	1601.386083	16.792960
34.002792	1586.407255	16.797978
33.920324	1593.572742	16.802995
33.539150	1608.833270	16.808013
34.137531	1611.759511	16.813031
33.974720	1624.330026	16.818048
33.827970	1627.260289	16.823066
34.135682	1624.880017	16.828083
34.074362	1637.962880	16.833101
34.417540	1630.826523	16.838119
34.063794	1632.690284	16.843136
33.999078	1636.224077	16.848154
34.436204	1631.232449	16.853171
34.285353	1630.580100	16.858189
34.400868	1625.528089	16.863207
34.067766	1634.072184	16.868224
34.296137	1639.251767	16.873242
34.163216	1629.800404	16.878259
34.741316	1625.500430	16.883277
34.772573	1623.214588	16.888295
34.496593	1627.249252	16.893312
34.304742	1629.941323	16.898330
34.396758	1629.882578	16.903347
34.261436	1635.088708	16.908365
34.375488	1626.131199	16.913383
34.372324	1647.834209	16.918400
34.659227	1656.167745	16.923418
34.867698	1664.560986	16.928435
34.868118	1666.140178	16.933453
35.004878	1666.859220	16.938471
34.838345	1666.700144	16.943488
35.040286	1656.824128	16.948506
34.975471	1662.958097	16.953523
34.603778	1669.969983	16.958541
35.382020	1655.084874	16.963559
35.022028	1663.960458	16.968576
35.242914	1663.340050	16.973594
35.485675	1655.291633	16.978611
34.973946	1652.842285	16.983629
35.006789	1656.725456	16.988647
34.814164	1659.364174	16.993664
34.841136	1662.345386	16.998682
35.025218	1669.732659	17.003699
34.998186	1659.026443	17.008717
35.303686	1658.777922	17.013735
35.109667	1657.405734	17.018752
35.140348	1651.093122	17.023770
35.319597	1658.457566	17.028787
34.951636	1664.712245	17.033805
35.485388	1668.836415	17.038823
35.374618	1680.922061	17.043840
35.813165	1690.928691	17.048858
35.618531	1679.465841	17.053875
35.558491	1684.486952	17.058893
35.799455	1681.610812	17.063911
35.907660	1669.269127	17.068928
36.101749	1654.150009	17.073946
35.796768	1647.019499	17.078963
35.366390	1656.005403	17.083981
35.664330	1650.068580	17.088999
35.460649	1662.110829	17.094016
35.352858	1663.560993	17.099034
35.814188	1673.334320	17.104051
35.655462	1673.589268	17.109069
35.893451	1683.793046	17.114087
35.589517	1690.995478	17.119104
35.882944	1686.998862	17.124122
36.187142	1676.480471	17.129139
36.101345	1691.137133	17.134157
36.496893	1678.131423	17.139175
36.418439	1681.662699	17.144192
36.140347	1693.790773	17.149210
36.311854	1672.479211	17.154227
36.014055	1691.201269	17.159245
36.522971	1677.858159	17.164263
36.454110	1683.997501	17.169280
36.491118	1687.692830	17.174298
36.581942	1680.868827	17.179315
36.217805	1691.121458	17.184333
36.575497	1682.818745	17.189351
36.564637	1680.671743	17.194368
36.534097	1672.832071	17.199386
36.617413	1678.608946	17.204403
36.398171	1679.940037	17.209421
36.527108	1679.044863	17.214439
36.686129	1685.223363	17.219456
36.814545	1670.424582	17.224474
36.912631	1672.191114	17.229491
36.474013	1675.289059	17.234509
36.833120	1675.864101	17.239527
36.833482	1675.082241	17.244544
36.674782	1685.092893	17.249562
36.771234	1674.640671	17.254579
36.694218	1679.666061	17.259597
36.787230	1679.324018	17.264615
36.625407	1689.168434	17.269632
36.453783	1688.148168	17.274650
37.098947	1690.009912	17.279667
36.760051	1703.649903	17.284685
37.028369	1703.415177	17.289703
37.069176	1698.905156	17.294720
36.944110	1704.485620	17.299738
37.072172	1709.814932	17.304755
36.887324	1699.442165	17.309773
36.836379	1699.252068	17.314791
37.333080	1705.645700	17.319808
37.159946	1704.463656	17.324826
37.450123	1698.049861	17.329843
37.262011	1703.641953	17.334861
37.331822	1712.738445	17.339879
37.657543	1724.718330	17.344896
37.341403	1721.020274	17.349914
37.881451	1719.291903	17.354931
37.727956	1722.638533	17.359949
37.723408	1698.682488	17.364967
37.685525	1699.519047	17.369984
37.526731	1705.996780	17.375002
37.845320	1693.270741	17.380019
37.609480	1695.257273	17.385037
37.627560	1699.466847	17.390055
37.513445	1703.148531	17.395072
37.671440	1734.149118	17.400090
37.788873	1729.869108	17.405107
37.839998	1739.114886	17.410125
37.867712	1731.177804	17.415143
38.404987	1725.083229	17.420160
37.932092	1734.799542	17.425178
38.291649	1732.250537	17.430195
38.316399	1736.150750	17.435213
38.162422	1734.105217	17.440231
38.357946	1722.938747	17.445248
38.496647	1737.866384	17.450266
38.689659	1719.486541	17.455283
38.220780	1710.872063	17.460301
38.305284	1695.259156	17.465319
38.621450	1693.555486	17.470336
38.324397	1698.894397	17.475354
38.441158	1688.286345	17.480371
38.106293	1686.016418	17.485389
38.137255	1706.219728	17.490407
38.281609	1710.132317	17.495424
38.375597	1727.906336	17.500442
38.650384	1726.446785	17.505459
38.561422	1733.652702	17.510477
38.688846	1728.930658	17.515495
39.114153	1722.278226	17.520512
38.531810	1720.263266	17.525530
38.873326	1713.213649	17.530547
38.884213	1717.301682	17.535565
38.928406	1717.458201	17.540583
39.127856	1710.141813	17.545600
39.091477	1719.719281	17.550618
39.091746	1710.506167	17.555635
38.894550	1713.938414	17.560653
38.718969	1706.662969	17.565671
38.773755	1725.056705	17.570688
38.667720	1721.394350	17.575706
38.940241	1709.897863	17.580723
38.892048	1714.110147	17.585741
38.841604	1710.711056	17.590759
38.825304	1727.826276	17.595776
38.881040	1748.455123	17.600794
39.298216	1739.428748	17.605811
39.331444	1748.851990	17.610829
39.105019	1742.690456	17.615847
39.573537	1729.347450	17.620864
39.217613	1749.184672	17.625882
39.491887	1749.729204	17.630899
39.372698	1748.851579	17.635917
39.162308	1744.109480	17.640935
39.200054	1744.238713	17.645952
39.213826	1748.853249	17.650970
39.421815	1761.662039	17.655987
39.664356	1788.246423	17.661005
39.825712	1789.667828	17.666023
39.804109	1763.387921	17.671040
39.675390	1790.418483	17.676058
39.833386	1788.359362	17.681075
39.900565	1781.853685	17.686093
40.122699	1772.008976	17.691111
40.044606	1774.989665	17.696128
40.115546	1775.031808	17.701146
40.417502	1761.801855	17.706163
40.178114	1764.257717	17.711181
39.956213	1770.832059	17.716199
40.492379	1773.779269	17.721216
40.157145	1770.834568	17.726234
40.294007	1756.713890	17.731251
40.351463	1767.390108	17.736269
40.458365	1765.600258	17.741287
40.044039	1746.566927	17.746304
40.225755	1762.450406	17.751322
40.478398	1762.708956	17.756339
40.305018	1764.341048	17.761357
40.574511	1778.256874	17.766375
40.851218	1767.772690	17.771392
40.473332	1770.673780	17.776410
40.826502	1770.464845	17.781427
40.879382	1773.380600	17.786445
40.508600	1765.516495	17.791463
40.898413	1756.323018	17.796480
40.876756	1777.881310	17.801498
40.660273	1756.651956	17.806515
40.767801	1764.935515	17.811533
40.452210	1765.290989	17.816551
40.760759	1757.991783	17.821568
40.933076	1769.749212	17.826586
40.749027	1763.053954	17.831603
40.491094	1780.136990	17.836621
40.586920	1769.414243	17.841639
40.807888	1771.132874	17.846656
40.599984	1774.867287	17.851674
41.047078	1796.442078	17.856691
41.110515	1787.034798	17.861709
40.859038	1789.437537	17.866727
41.363510	1786.530361	17.871744
41.105136	1795.707563	17.876762
40.941416	1791.274179	17.881779
41.137353	1772.141906	17.886797
41.204401	1789.102335	17.891815
41.120853	1790.550217	17.896832
41.017351	1809.987043	17.901850
41.401025	1810.095709	17.906867
41.601482	1806.157934	17.911885
41.277335	1832.946041	17.916903
42.092864	1813.057374	17.921920
41.580115	1819.461052	17.926938
41.519687	1822.616683	17.931955
41.880708	1808.068524	17.936973
41.924995	1814.207178	17.941991
42.021077	1812.892524	17.947008
42.103399	1817.733673	17.952026
42.088891	1806.418169	17.957043
42.113504	1805.627715	17.962061
41.679546	1808.986064	17.967079
42.219175	1806.696187	17.972096
42.182229	1813.458124	17.977114
41.980917	1809.650495	17.982131
42.030631	1812.464518	17.987149
42.073539	1813.344826	17.992167
42.202456	1817.387320	17.997184
42.210342	1818.674332	18.002202
42.361656	1819.397353	18.007219
42.516793	1798.407537	18.012237
42.378206	1814.670919	18.017255
42.415170	1798.842116	18.022272
42.321221	1809.924755	18.027290
41.880382	1804.113567	18.032307
42.461822	1799.704474	18.037325
42.380626	1811.058783	18.042343
42.519328	1803.948664	18.047360
42.458144	1814.371709	18.052378
42.542641	1820.815408	18.057395
42.746657	1839.652673	18.062413
42.701127	1831.255314	18.067431
43.019215	1831.553764	18.072448
42.834027	1825.355730	18.077466
42.652323	1843.269816	18.082483
42.904539	1838.060649	18.087501
43.053118	1840.478240	18.092519
43.097769	1832.595029	18.097536
43.023647	1834.455114	18.102554
42.849547	1838.398081	18.107571
43.286591	1829.903306	18.112589
42.933355	1838.304441	18.117607
43.150377	1834.986929	18.122624
43.332001	1825.299655	18.127642
42.933753	1833.325725	18.132659
43.159428	1819.346549	18.137677
42.847916	1834.331936	18.142695
43.284574	1833.768341	18.147712
43.430296	1868.681678	18.152730
43.543326	1864.959178	18.157747
43.494192	1862.020735	18.162765
43.520762	1865.613955	18.167783
43.692245	1863.945927	18.172800
43.773010	1863.799314	18.177818
43.505286	1858.970368	18.182835
43.787931	1855.419017	18.187853
44.034354	1867.562678	18.192871
43.996131	1861.562983	18.197888
44.108371	1859.037674	18.202906
43.914219	1846.824286	18.207923
44.080071	1824.299037	18.212941
43.877182	1831.447669	18.217959
43.886036	1825.144754	18.222976
44.283995	1842.810659	18.227994
43.901587	1839.077523	18.233011
44.276038	1850.725701	18.238029
43.859363	1873.194992	18.243047
44.250584	1870.455299	18.248064
44.536286	1869.620053	18.253082
44.205262	1872.527846	18.258099
44.746614	1857.847057	18.263117
44.298860	1874.746550	18.268135
44.408780	1869.613550	18.273152
44.435154	1858.809007	18.278170
44.288981	1864.520312	18.283187
44.560045	1861.373499	18.288205
44.429844	1867.376412	18.293223
44.644567	1856.526099	18.298240
44.321856	1866.430901	18.303258
44.139728	1867.839458	18.308275
44.537962	1855.699893	18.313293
44.392180	1877.962392	18.318311
44.106514	1881.948333	18.323328
44.596283	1890.315717	18.328346
44.661526	1897.769252	18.333363
44.807034	1876.677040	18.338381
44.758232	1891.604855	18.343399
44.987147	1878.845766	18.348416
44.932659	1874.223476	18.353434
45.016174	1883.380810	18.358451
45.162418	1896.688776	18.363469
45.100940	1910.004716	18.368487
45.537899	1910.221288	18.373504
45.583684	1898.172507	18.378522
45.384857	1884.468613	18.383539
45.056002	1891.432872	18.388557
45.256557	1895.928003	18.393575
45.615001	1917.139590	18.398592
45.335179	1917.165319	18.403610
45.363456	1924.296002	18.408627
45.766740	1911.856711	18.413645
45.781556	1922.239398	18.418663
45.824491	1923.080383	18.423680
45.715593	1910.276046	18.428698
46.193749	1915.430047	18.433715
46.089739	1905.014350	18.438733
45.822426	1898.332310	18.443751
45.868560	1910.246831	18.448768
45.849931	1910.072026	18.453786
45.739437	1905.807868	18.458803
46.272958	1904.226810	18.463821
46.027215	1910.171091	18.468839
45.987462	1916.287013	18.473856
46.268753	1913.569565	18.478874
46.069039	1918.351911	18.483891
46.275736	1904.970282	18.488909
46.308923	1903.437563	18.493927
46.342888	1910.521715	18.498944
46.302985	1902.169036	18.503962
46.201099	1908.129697	18.508979
46.366209	1894.078312	18.513997
46.365824	1901.775123	18.519015
46.264624	1906.697482	18.524032
46.778563	1896.825025	18.529050
46.805642	1892.301403	18.534067
46.525778	1885.037781	18.539085
46.373387	1908.740691	18.544103
46.413864	1907.183214	18.549120
46.470141	1891.483364	18.554138
46.757302	1925.185078	18.559155
46.974951	1928.275932	18.564173
47.004217	1930.234370	18.569191
46.778443	1936.537271	18.574208
47.079019	1926.645341	18.579226
46.608261	1946.548336	18.584243
47.015991	1937.175709	18.589261
46.705794	1930.560268	18.594279
47.175743	1928.561485	18.599296
47.279655	1926.411871	18.604314
46.893933	1930.135359	18.609331
47.305949	1916.719398	18.614349
47.288281	1923.662355	18.619367
47.075524	1916.364418	18.624384
47.155967	1933.852988	18.629402
47.333072	1945.716762	18.634419
47.602578	1944.939151	18.639437
47.689275	1956.627018	18.644455
47.658928	1958.286655	18.649472
47.767157	1943.473513	18.654490
47.474863	1957.490125	18.659507
47.643658	1948.880763	18.664525
47.869131	1951.141391	18.669543
47.774435	1953.553757	18.674560
47.919848	1955.879064	18.679578
47.816682	1951.530354	18.684595
47.514832	1953.083855	18.689613
47.953297	1949.808077	18.694631
47.787478	1952.214484	18.699648
48.035579	1943.458769	18.704666
48.078933	1960.811715	18.709683
48.326008	1973.205473	18.714701
48.518915	1973.374455	18.719719
48.268057	1971.142991	18.724736
48.488423	1967.672333	18.729754
48.278918	1956.667811	18.734771
48.309559	1950.421142	18.739789
48.357037	1957.850800	18.744807
48.402582	1964.536730	18.749824
49.021410	1964.755758	18.754842
48.743321	1967.043220	18.759859
49.053980	1956.577080	18.764877
48.919952	1943.878967	18.769895
48.385663	1947.363459	18.774912
48.701880	1935.823647	18.779930
48.650447	1949.836443	18.784947
48.935842	1953.157169	18.789965
48.931813	1955.353728	18.794983
48.592056	1962.903352	18.800000
49.017335	1962.465838	18.805018
48.887220	1969.557312	18.810035
48.938191	1960.674152	18.815053
49.078068	1957.917902	18.820071
49.001530	1963.432524	18.825088
49.053383	1959.335939	18.830106
49.249165	1963.724887	18.835123
49.251334	1957.754889	18.840141
49.267696	1951.098365	18.845159
49.123519	1975.822540	18.850176
49.558151	1975.912071	18.855194
49.362123	1983.673162	18.860211
49.401197	1989.142612	18.865229
49.322250	1986.061035	18.870247
49.151183	1997.642182	18.875264
49.686192	1982.806549	18.880282
49.939724	1985.419784	18.885299
49.581973	1989.613879	18.890317
49.644595	1985.122313	18.895335
49.515124	1994.909865	18.900352
50.258898	2002.992984	18.905370
50.027762	2022.310451	18.910387
49.942906	2014.708919	18.915405
50.028584	2005.900421	18.920423
50.065592	2015.724356	18.925440
50.491678	2016.521541	18.930458
50.449501	2014.060159	18.935475
50.485305	2009.788367	18.940493
50.634953	2008.150547	18.945511
50.158693	2014.326691	18.950528
50.431069	2004.311791	18.955546
50.248587	2017.264882	18.960563
50.364307	2015.597865	18.965581
50.320396	2003.517685	18.970599
50.295308	2008.231311	18.975616
50.196010	2013.939918	18.980634
50.172110	2014.403030	18.985651
50.202128	2007.874864	18.990669
50.509075	2026.307417	18.995687
50.575284	2039.648728	19.000704
50.839071	2038.975846	19.005722
50.853178	2036.961662	19.010739
50.718339	2047.533476	19.015757
51.130853	2041.954177	19.020775
51.012888	2041.655214	19.025792
51.282779	2030.509682	19.030810
51.208546	2037.428681	19.035827
51.282457	2042.776191	19.040845
51.271661	2033.180816	19.045863
51.547359	2030.384014	19.050880
51.739885	2039.709679	19.055898
51.594545	2033.126099	19.060915
51.625676	2045.732113	19.065933
51.715884	2033.734337	19.070951
51.379697	2034.638942	19.075968
51.715545	2028.881538	19.080986
51.593078	2034.176995	19.086003
51.466235	2027.735186	19.091021
51.764591	2023.673201	19.096039
51.534586	2029.025133	19.101056
51.512155	2032.160592	19.106074
51.773832	2031.012990	19.111091
51.507474	2031.437694	19.116109
51.828824	2043.972251	19.121127
52.021513	2070.198589	19.126144
51.820626	2058.374635	19.131162
52.033073	2058.337581	19.136179
51.727431	2057.049224	19.141197
52.316225	2051.363155	19.146215
51.983045	2063.629311	19.151232
52.456721	2054.788789	19.156250
52.332438	2048.138922	19.161267
52.022278	2069.616246	19.166285
52.776624	2070.276136	19.171303
52.485642	2087.187050	19.176320
52.791587	2097.347249	19.181338
52.606445	2091.057857	19.186355
53.004936	2092.038774	19.191373
53.166614	2072.178535	19.196391
52.804646	2063.153532	19.201408
52.606438	2054.616799	19.206426
53.062857	2059.678365	19.211443
52.793590	2069.404892	19.216461
53.407472	2072.251683	19.221479
53.131602	2062.588453	19.226496
53.230375	2062.110203	19.231514
53.131850	2060.519823	19.236531
53.007352	2055.420999	19.241549
53.235812	2059.293529	19.246567
53.153270	2076.350512	19.251584
53.371059	2076.797101	19.256602
53.715714	2078.521212	19.261619
53.285942	2091.398978	19.266637
53.611630	2076.547872	19.271655
53.423658	2081.891546	19.276672
53.286179	2070.741741	19.281690
53.586367	2074.933172	19.286707
53.467225	2084.986554	19.291725
53.486883	2075.787418	19.296743
53.471047	2078.726779	19.301760
53.524050	2079.014032	19.306778
53.893185	2090.186623	19.311795
53.632186	2081.260337	19.316813
53.687296	2084.479395	19.321831
53.746577	2098.523441	19.326848
53.974649	2114.006653	19.331866
54.132522	2109.712218	19.336883
54.233746	2117.767321	19.341901
54.357164	2103.217438	19.346919
54.323288	2116.345119	19.351936
53.990083	2109.047418	19.356954
54.632016	2104.916456	19.361971
54.643834	2118.617303	19.366989
54.571978	2104.787554	19.372007
54.396576	2107.005176	19.377024
54.455729	2105.323576	19.382042
54.548630	2101.495686	19.387059
54.819712	2100.802761	19.392077
54.530365	2105.432722	19.397095
54.400778	2101.917172	19.402112
54.373203	2092.027130	19.407130
55.057831	2116.285873	19.412147
54.968004	2129.683615	19.417165
55.156888	2131.066057	19.422183
55.461428	2126.219682	19.427200
55.418008	2125.639838	19.432218
55.384935	2111.832212	19.437235
54.816352	2103.552724	19.442253
55.468951	2118.784189	19.447271
55.231819	2120.228283	19.452288
55.095083	2137.342746	19.457306
55.607216	2125.360973	19.462323
55.440095	2119.929147	19.467341
55.449079	2124.453331	19.472359
55.345447	2120.801501	19.477376
55.367638	2121.236816	19.482394
55.451911	2121.909197	19.487411
55.537367	2125.688147	19.492429
55.450389	2124.972103	19.497447
55.460135	2128.341553	19.502464
55.713272	2132.796911	19.507482
56.333608	2145.480502	19.512499
56.071899	2147.419308	19.517517
56.013543	2142.525412	19.522535
56.401588	2140.980118	19.527552
56.265628	2137.320856	19.532570
56.342719	2140.303611	19.537587
56.164388	2150.629176	19.542605
56.561672	2141.209321	19.547623
56.601822	2141.377501	19.552640
56.201308	2141.751243	19.557658
56.416079	2136.980531	19.562675
56.570118	2132.373664	19.567693
56.630354	2147.422779	19.572711
56.534110	2130.126760	19.577728
56.488127	2139.553452	19.582746
56.697452	2140.584993	19.587763
56.393933	2142.185970	19.592781
56.608525	2136.462022	19.597799
56.516955	2135.353449	19.602816
56.292559	2139.543621	19.607834
56.737664	2156.868906	19.612851
56.817152	2168.466857	19.617869
56.998643	2163.909086	19.622887
57.002666	2177.173925	19.627904
56.885379	2167.266679	19.632922
57.143095	2168.461966	19.637939
56.913383	2175.805382	19.642957
57.201071	2190.376239	19.647975
57.323240	2188.745928	19.652992
57.338181	2202.614672	19.658010
57.495565	2192.942031	19.663027
57.642227	2201.965226	19.668045
57.503835	2201.988846	19.673063
57.544922	2198.288747	19.678080
57.340542	2197.866707	19.683098
57.943328	2186.940100	19.688115
57.739557	2197.842345	19.693133
57.836540	2192.731745	19.698151
57.896350	2202.303628	19.703168
57.437595	2212.533960	19.708186
58.018602	2221.133957	19.713203
58.187860	2233.887994	19.718221
58.294898	2230.690183	19.723239
58.103441	2224.157916	19.728256
58.155972	2219.040239	19.733274
58.581011	2221.464141	19.738291
58.576874	2218.924296	19.743309
58.534838	2224.818911	19.748327
58.849630	2217.924330	19.753344
58.759977	2216.357686	19.758362
58.973572	2212.150290	19.763379
58.896444	2212.426839	19.768397
58.974688	2221.014210	19.773415
58.842541	2211.573354	19.778432
58.958332	2217.158072	19.783450
58.819511	2212.931375	19.788467
58.588948	2219.110890	19.793485
58.769658	2213.288494	19.798503
58.896136	2208.805551	19.803520
58.753402	2221.529111	19.808538
58.827781	2220.051139	19.813555
58.891931	2238.969434	19.818573
59.324356	2244.903220	19.823591
59.474034	2245.684727	19.828608
59.427228	2240.435019	19.833626
59.468075	2235.874487	19.838643
59.323204	2248.161102	19.843661
59.092183	2244.010450	19.848679
59.743997	2229.844938	19.853696
59.618061	2234.263256	19.858714
59.673728	2235.416840	19.863731
59.157898	2237.809901	19.868749
59.440285	2262.869233	19.873767
59.694367	2270.804086	19.878784
59.878470	2270.867510	19.883802
60.106761	2259.092923	19.888819
60.299398	2262.148512	19.893837
60.179241	2263.932621	19.898855
60.636434	2254.389879	19.903872
60.695364	2260.398970	19.908890
60.863911	2258.314506	19.913907
61.035248	2250.777386	19.918925
60.789511	2254.222219	19.923943
60.616485	2228.332141	19.928960
60.643932	2225.703887	19.933978
60.720043	2225.276437	19.938995
60.624832	2213.757978	19.944013
60.641761	2220.942528	19.949031
60.738359	2238.463497	19.954048
60.336915	2243.901052	19.959066
61.013229	2259.986200	19.964083
60.931655	2253.526059	19.969101
60.644227	2247.878987	19.974119
60.822524	2257.965276	19.979136
60.535952	2254.694953	19.984154
60.839618	2258.541385	19.989171
60.924199	2274.675305	19.994189
60.946618	2283.339258	19.999207
61.208730	2270.538352	20.004224
61.460205	2276.304378	20.009242
61.503423	2286.523917	20.014259
61.434682	2275.315800	20.019277
61.431037	2289.176580	20.024295
61.603581	2277.363677	20.029312
61.424293	2276.881003	20.034330
61.633299	2296.779882	20.039347
62.051792	2309.138724	20.044365
61.732278	2317.810040	20.049383
62.119453	2313.933589	20.054400
62.153482	2325.828360	20.059418
61.969274	2314.427837	20.064435
62.390404	2308.096714	20.069453
62.001352	2313.123322	20.074471
62.425265	2313.598396	20.079488
62.244765	2312.500846	20.084506
62.427868	2312.860165	20.089523
62.673331	2311.817378	20.094541
62.478790	2307.498864	20.099559
62.690352	2305.155843	20.104576
62.458673	2316.688707	20.109594
62.501033	2317.185306	20.114611
62.660401	2308.191836	20.119629
62.666874	2305.497697	20.124647
62.766064	2301.948757	20.129664
62.180999	2314.917555	20.134682
62.946009	2317.881870	20.139699
62.937521	2329.283191	20.144717
62.958101	2334.610999	20.149735
63.175181	2323.909405	20.154752
63.146348	2320.819763	20.159770
62.908341	2323.568086	20.164787
63.117571	2323.534692	20.169805
63.104235	2334.933644	20.174823
63.630942	2325.414377	20.179840
63.395934	2329.741579	20.184858
63.410342	2329.723525	20.189875
63.563311	2330.425860	20.194893
63.358842	2326.450278	20.199911
63.479674	2351.349908	20.204928
63.634299	2350.768358	20.209946
63.652391	2357.414801	20.214963
64.056093	2351.777015	20.219981
63.796047	2349.948088	20.224999
64.241721	2356.653757	20.230016
64.348329	2349.215001	20.235034
64.192923	2345.612271	20.240051
64.553363	2354.083927	20.245069
63.921320	2367.182961	20.250087
64.401722	2350.666192	20.255104
64.372308	2354.579929	20.260122
64.287727	2355.121945	20.265139
64.521325	2346.341561	20.270157
64.561681	2355.998448	20.275175
64.696620	2347.277844	20.280192
64.506277	2352.516599	20.285210
64.507850	2371.945283	20.290227
64.814224	2361.904267	20.295245
64.585334	2380.229244	20.300263
64.620419	2377.052315	20.305280
65.214178	2383.528307	20.310298
64.847252	2384.412663	20.315315
65.354102	2370.696438	20.320333
64.925873	2367.703518	20.325351
64.991874	2376.475411	20.330368
64.857719	2399.462038	20.335386
64.919460	2409.787252	20.340403
65.149252	2389.627844	20.345421
65.220024	2402.194025	20.350439
65.185350	2394.481254	20.355456
65.458449	2412.812730	20.360474
65.525949	2426.662295	20.365491
65.875051	2431.497284	20.370509
65.692229	2419.213962	20.375527
65.936766	2424.482490	20.380544
66.177413	2427.071120	20.385562
66.016565	2417.013343	20.390579
66.524074	2421.901718	20.395597
66.149510	2420.879943	20.400615
66.586770	2421.973470	20.405632
66.441119	2424.407411	20.410650
66.189870	2415.366100	20.415667
66.411196	2405.587950	20.420685
66.723876	2416.618784	20.425703
66.944554	2413.947880	20.430720
66.910208	2416.760483	20.435738
66.828961	2406.122925	20.440755
66.759032	2388.137328	20.445773
66.199518	2392.985076	20.450791
66.579998	2404.171833	20.455808
66.784915	2415.582446	20.460826
66.518847	2419.194946	20.465843
66.392572	2416.767358	20.470861
66.673719	2422.908608	20.475879
66.731561	2421.997200	20.480896
67.210637	2441.799722	20.485914
66.961308	2448.218288	20.490931
67.437598	2442.848899	20.495949
67.230408	2451.559797	20.500967
67.211908	2446.285835	20.505984
67.554329	2437.979628	20.511002
67.302832	2430.535020	20.516019
67.976906	2450.071280	20.521037
67.652652	2474.475797	20.526055
67.921954	2464.273090	20.531072
67.979463	2472.440760	20.536090
67.717591	2472.140355	20.541107
67.895280	2477.039664	20.546125
67.861273	2467.091402	20.551143
67.755776	2467.474730	20.556160
68.031620	2476.755928	20.561178
68.244006	2463.380745	20.566195
68.547500	2468.739777	20.571213
68.505497	2467.230789	20.576231
68.479590	2452.357508	20.581248
68.749487	2465.753247	20.586266
68.562983	2463.941678	20.591283
68.893199	2458.210176	20.596301
68.647159	2468.214844	20.601319
68.510600	2462.993526	20.606336
68.958619	2474.745313	20.611354
68.815153	2494.687307	20.616371
68.938059	2487.056326	20.621389
69.014969	2490.324696	20.626407
69.081714	2494.297070	20.631424
69.448751	2494.020637	20.636442
69.122928	2486.501334	20.641459
69.517521	2478.768037	20.646477
69.474468	2484.974389	20.651495
69.122158	2490.639374	20.656512
69.316006	2483.306977	20.661530
69.197669	2479.872127	20.666547
69.548633	2481.900461	20.671565
69.419996	2480.597991	20.676583
69.543618	2480.457123	20.681600
69.780610	2498.394118	20.686618
69.888865	2500.714429	20.691635
70.052757	2504.476250	20.696653
69.937908	2499.429215	20.701671
70.450621	2507.480260	20.706688
70.108795	2515.630628	20.711706
69.952011	2516.554625	20.716723
70.347897	2495.842385	20.721741
70.165651	2515.745760	20.726759
70.015962	2507.144389	20.731776
70.264641	2507.374488	20.736794
70.002782	2511.948280	20.741811
70.642095	2524.155682	20.746829
70.715536	2538.807467	20.751847
70.575808	2540.833052	20.756864
70.816782	2538.040908	20.761882
71.023540	2542.998527	20.766899
71.095751	2527.665910	20.771917
71.053501	2543.677993	20.776935
70.890522	2550.312502	20.781952
71.232680	2531.395022	20.786970
70.599085	2543.121942	20.791987
70.960031	2550.854283	20.797005
71.260674	2566.668554	20.802023
71.303667	2566.210196	20.807040
71.611601	2563.629173	20.812058
71.556918	2567.857683	20.817075
71.715835	2564.461182	20.822093
71.681703	2562.048762	20.827111
71.689087	2555.526319	20.832128
71.857123	2560.361127	20.837146
71.917278	2562.072469	20.842163
71.897479	2557.540386	20.847181
72.112547	2554.809001	20.852199
72.081506	2558.735637	20.857216
71.997038	2566.448570	20.862234
72.265700	2582.951466	20.867251
72.635122	2575.400678	20.872269
72.468227	2578.165235	20.877287
72.571472	2578.281671	20.882304
72.571071	2581.105409	20.887322
72.675388	2582.046760	20.892339
72.522238	2578.685082	20.897357
73.043330	2576.505808	20.902375
73.011153	2578.479638	20.907392
72.937609	2573.312728	20.912410
72.942889	2566.303744	20.917427
72.846664	2578.354781	20.922445
72.865201	2574.532335	20.927463
72.787595	2576.744655	20.932480
73.162262	2563.699017	20.937498
72.790362	2586.782848	20.942515
73.099721	2589.395944	20.947533
73.505740	2590.092543	20.952551
73.481855	2601.550018	20.957568
73.701444	2605.444561	20.962586
73.624342	2601.995240	20.967603
73.670541	2605.254377	20.972621
73.635498	2607.895660	20.977639
73.786744	2598.978029	20.982656
74.053058	2599.447574	20.987674
73.559066	2600.512661	20.992691
73.670501	2605.369096	20.997709
73.951152	2612.287615	21.002727
73.993812	2617.234463	21.007744
74.459306	2624.586785	21.012762
74.230898	2634.807416	21.017779
74.509290	2626.777167	21.022797
74.337836	2625.422521	21.027815
74.383260	2635.981743	21.032832
74.608973	2631.825780	21.037850
74.391687	2633.769361	21.042867
74.431013	2651.117483	21.047885
74.899988	2644.623636	21.052903
74.920520	2658.600468	21.057920
74.765151	2654.922145	21.062938
74.775402	2658.754130	21.067955
74.788257	2652.515502	21.072973
75.339830	2649.488176	21.077991
75.239797	2677.106509	21.083008
75.791269	2676.685038	21.088026
75.527805	2671.423319	21.093043
75.666589	2680.166483	21.098061
75.763880	2679.508330	21.103079
75.759259	2675.252229	21.108096
75.947200	2674.434108	21.113114
76.014138	2671.996112	21.118131
75.977912	2670.304489	21.123149
76.131298	2682.646155	21.128167
75.727040	2680.027676	21.133184
76.256999	2669.331776	21.138202
76.118883	2671.357909	21.143219
76.250696	2680.864353	21.148237
76.268058	2666.573079	21.153255
76.203333	2670.089819	21.158272
76.503327	2668.532561	21.163290
76.424835	2668.410554	21.168307
76.534640	2673.290081	21.173325
76.724560	2664.577037	21.178343
76.289149	2685.883324	21.183360
76.617524	2675.621497	21.188378
76.665263	2690.022690	21.193395
76.713199	2699.227116	21.198413
76.937737	2693.182811	21.203431
76.687333	2703.653188	21.208448
76.978820	2689.263116	21.213466
76.909021	2711.491961	21.218483
77.042229	2715.211538	21.223501
77.226301	2719.033908	21.228519
77.097676	2725.050292	21.233536
77.455399	2716.872055	21.238554
77.533431	2722.123200	21.243571
77.477979	2725.063503	21.248589
77.703387	2718.927023	21.253607
77.598810	2744.853547	21.258624
77.873459	2741.278878	21.263642
78.212106	2752.207508	21.268659
77.902674	2743.093470	21.273677
78.424022	2735.659951	21.278695
78.296265	2750.159195	21.283712
78.255087	2741.270592	21.288730
78.365068	2736.086939	21.293747
78.352960	2735.824563	21.298765
78.585924	2742.741312	21.303783
78.253277	2740.626594	21.308800
78.347455	2734.889368	21.313818
78.659391	2760.567014	21.318835
78.970015	2774.759617	21.323853
79.402763	2771.733127	21.328871
78.746817	2768.266748	21.333888
79.183220	2758.476873	21.338906
79.653699	2768.103192	21.343923
79.434850	2756.477384	21.348941
79.805700	2748.018596	21.353959
79.887671	2758.328247	21.358976
79.621904	2747.969990	21.363994
79.855294	2729.745250	21.369011
79.737151	2717.426190	21.374029
79.943241	2708.718407	21.379047
79.581434	2721.380594	21.384064
79.842247	2720.403763	21.389082
80.287892	2746.837176	21.394099
79.894353	2738.981669	21.399117
79.922076	2750.639468	21.404135
79.870560	2753.740393	21.409152
80.139624	2747.611097	21.414170
80.252810	2751.049143	21.419187
79.956444	2760.102439	21.424205
80.059612	2740.746150	21.429223
80.018927	2756.832940	21.434240
80.162904	2787.113598	21.439258
80.431788	2780.034943	21.444275
80.396278	2780.930963	21.449293
80.384505	2785.059879	21.454311
80.755203	2792.760120	21.459328
80.592022	2809.480017	21.464346
80.784443	2816.585749	21.469363
80.966962	2809.294324	21.474381
81.307091	2800.840405	21.479399
80.996953	2817.282496	21.484416
80.912241	2815.556114	21.489434
81.560135	2819.746587	21.494451
81.372004	2843.644706	21.499469
81.401757	2833.853561	21.504487
81.595272	2838.077962	21.509504
81.759756	2832.390837	21.514522
81.641390	2815.507327	21.519539
81.575946	2847.057977	21.524557
82.238298	2825.671954	21.529575
81.813018	2824.250797	21.534592
82.092913	2847.042316	21.539610
82.630330	2842.236438	21.544627
82.571609	2855.025808	21.549645
82.698260	2847.865191	21.554663
82.778853	2841.890975	21.559680
82.716083	2832.641582	21.564698
82.519724	2822.457044	21.569715
82.621074	2832.806131	21.574733
83.220867	2831.492072	21.579751
83.138690	2840.622164	21.584768
82.949268	2845.649363	21.589786
83.187521	2844.564431	21.594803
83.052964	2841.185567	21.599821
83.298123	2845.562192	21.604839
83.497080	2850.120016	21.609856
83.437088	2836.660507	21.614874
83.497104	2831.240956	21.619891
83.333346	2829.231432	21.624909
83.752174	2837.517874	21.629927
83.587361	2830.981868	21.634944
83.357705	2832.045715	21.639962
83.581128	2838.733570	21.644979
83.493916	2850.592260	21.649997
83.500861	2858.208966	21.655015
83.733623	2866.670611	21.660032
83.948687	2870.100305	21.665050
83.898794	2869.512810	21.670067
84.141235	2887.810450	21.675085
84.649940	2882.420790	21.680103
84.691756	2889.877785	21.685120
84.434320	2898.730677	21.690138
84.753551	2897.454278	21.695155
84.658248	2897.071451	21.700173
84.788772	2892.619903	21.705191
85.016127	2887.227917	21.710208
85.220350	2881.360606	21.715226
85.067000	2870.929273	21.720243
85.004130	2894.904246	21.725261
85.082503	2881.271610	21.730279
85.271665	2888.423517	21.735296
85.264078	2910.710390	21.740314
85.611062	2911.487214	21.745331
85.325067	2912.157330	21.750349
85.485133	2915.622548	21.755367
85.776719	2928.061941	21.760384
85.772375	2922.159444	21.765402
85.596634	2912.577209	21.770419
85.193044	2929.724933	21.775437
85.593884	2934.649376	21.780455
85.618032	2952.952022	21.785472
85.628916	2959.502356	21.790490
86.128514	2954.446054	21.795507
86.259324	2948.337936	21.800525
86.377337	2949.371515	21.805543
86.641365	2968.043365	21.810560
86.684158	2987.496187	21.815578
87.040650	2971.423229	21.820595
86.992582	2966.843613	21.825613
87.025446	2970.716121	21.830631
87.226815	2975.302703	21.835648
87.054595	2961.607702	21.840666
87.278498	2963.901779	21.845683
87.075732	2967.089009	21.850701
86.862116	2964.664245	21.855719
87.013201	2976.839776	21.860736
87.318515	2963.584605	21.865754
87.284592	2968.198484	21.870771
87.426062	2991.267153	21.875789
87.775841	2996.392470	21.880807
87.747317	2997.726295	21.885824
87.815107	2998.904750	21.890842
87.870085	2982.746933	21.895859
87.936743	2990.541389	21.900877
88.109322	2993.426503	21.905895
88.299813	2986.322495	21.910912
88.106682	2982.258400	21.915930
88.583264	3010.863007	21.920947
88.685471	3012.572415	21.925965
88.448025	3010.725638	21.930983
88.649395	3018.988658	21.936000
88.761581	3014.153006	21.941018
89.081387	2997.322897	21.946035
89.030139	3004.910419	21.951053
88.914559	3010.744716	21.956071
89.038461	3001.632984	21.961088
88.728801	2989.149167	21.966106
89.095803	3008.609306	21.971123
89.350914	3038.352056	21.976141
89.696956	3041.797871	21.981159
89.559497	3028.105130	21.986176
89.340336	3037.751156	21.991194
89.473169	3040.834541	21.996211
89.549342	3034.213605	22.001229
89.730829	3050.554745	22.006247
90.082759	3041.406624	22.011264
89.928197	3038.926808	22.016282
90.324755	3041.786438	22.021299
90.261080	3036.352714	22.026317
90.425665	3044.004157	22.031335
90.263323	3037.385074	22.036352
90.163318	3050.245697	22.041370
90.360501	3055.057146	22.046387
90.649352	3053.282173	22.051405
90.634895	3052.902967	22.056423
90.857514	3051.027650	22.061440
90.685572	3066.304308	22.066458
90.798359	3055.660500	22.071475
91.016949	3052.539110	22.076493
90.468091	3065.583808	22.081511
90.992912	3075.014463	22.086528
90.784299	3083.376725	22.091546
90.919361	3085.533968	22.096563
90.956961	3099.383436	22.101581
91.071537	3110.530558	22.106599
91.324196	3124.392948	22.111616
91.495110	3121.231165	22.116634
91.968209	3135.534289	22.121651
92.192814	3142.902484	22.126669
92.139401	3143.969709	22.131687
92.325575	3148.314931	22.136704
92.696426	3146.036047	22.141722
92.822603	3143.283335	22.146739
92.892412	3118.131655	22.151757
92.769118	3113.597812	22.156775
92.906733	3094.738968	22.161792
92.502973	3090.060295	22.166810
92.815437	3101.518011	22.171827
92.820824	3099.247076	22.176845
92.567655	3115.085766	22.181863
93.360894	3122.105272	22.186880
93.158486	3146.787233	22.191898
93.407443	3135.638693	22.196915
93.415740	3132.633413	22.201933
93.694858	3134.590712	22.206951
93.496334	3122.758431	22.211968
93.139702	3134.875053	22.216986
93.556397	3140.316966	22.222003
93.766779	3122.688485	22.227021
93.423620	3148.691530	22.232039
93.658029	3153.460105	22.237056
93.838468	3156.698745	22.242074
93.834770	3177.993533	22.247091
93.993128	3150.984723	22.252109
93.826195	3183.167388	22.257127
94.293637	3160.725698	22.262144
94.143422	3215.354693	22.267162
94.321571	3173.061806	22.272179
94.303671	3196.273415	22.277197
94.179571	3217.460822	22.282215
94.813599	3209.684241	22.287232
94.886854	3211.163889	22.292250
94.889577	3217.829694	22.297267
95.271778	3210.615562	22.302285
95.234478	3211.767532	22.307303
95.580861	3223.296233	22.312320
95.505122	3223.885637	22.317338
95.591328	3204.518853	22.322355
95.541374	3208.917481	22.327373
95.528528	3234.272561	22.332391
95.594127	3209.376248	22.337408
95.458365	3249.456856	22.342426
95.857964	3246.511071	22.347443
95.426850	3257.536097	22.352461
95.698004	3232.363123	22.357479
95.948128	3274.583115	22.362496
95.978658	3259.943063	22.367514
96.283710	3280.194523	22.372531
96.709690	3267.907784	22.377549
96.383328	3262.324727	22.382567
96.809121	3261.347511	22.387584
96.710108	3281.274051	22.392602
96.849246	3260.114781	22.397619
96.782067	3289.386363	22.402637
97.153268	3287.819260	22.407655
97.281310	3292.049516	22.412672
97.278476	3293.658508	22.417690
97.184853	3299.291986	22.422707
97.582132	3307.219520	22.427725
97.478658	3299.599832	22.432743
97.720023	3280.365521	22.437760
97.593013	3305.957602	22.442778
97.814785	3272.305186	22.447795
97.905527	3317.123632	22.452813
97.880185	3305.057501	22.457831
98.302677	3291.939091	22.462848
98.067294	3338.393791	22.467866
98.433274	3294.513943	22.472883
98.443221	3325.763357	22.477901
98.477415	3326.398947	22.482919
98.717657	3308.869309	22.487936
98.971472	3314.878435	22.492954
99.027243	3309.775591	22.497971
98.871966	3318.163303	22.502989
98.973102	3298.230032	22.508007
99.173630	3296.768805	22.513024
99.066689	3334.829823	22.518042
99.283643	3317.056901	22.523059
99.883376	3334.329053	22.528077
99.547658	3335.556939	22.533095
100.134090	3326.428667	22.538112
99.942752	3324.520221	22.543130
99.881928	3333.135934	22.548147
99.909007	3333.527244	22.553165
100.111566	3333.892143	22.558183
100.179373	3330.155246	22.563200
100.364618	3329.800820	22.568218
99.968809	3321.614989	22.573235
100.443974	3334.060066	22.578253
100.332401	3333.808035	22.583271
100.182472	3331.640490	22.588288
100.336645	3326.909735	22.593306
99.996503	3338.514973	22.598323
100.424005	3345.993287	22.603341
100.526773	3343.190783	22.608359
100.476193	3363.237139	22.613376
100.774871	3349.058438	22.618394
100.654544	3373.096061	22.623411
101.235758	3384.131221	22.628429
101.131595	3388.577877	22.633447
100.935822	3377.460747	22.638464
101.275070	3388.798791	22.643482
101.214736	3417.497687	22.648499
101.812135	3413.815541	22.653517
101.701340	3403.807304	22.658535
101.734431	3418.368086	22.663552
101.654735	3422.497001	22.668570
102.283100	3431.933404	22.673587
102.271276	3426.335521	22.678605
102.272675	3455.835624	22.683623
102.222453	3438.584196	22.688640
102.588483	3436.301319	22.693658
102.463961	3439.738894	22.698675
102.838269	3442.067272	22.703693
102.606158	3463.950303	22.708711
102.887685	3469.639650	22.713728
103.187999	3459.114310	22.718746
102.938732	3457.985159	22.723763
103.398279	3458.581241	22.728781
103.116622	3444.043491	22.733799
103.063197	3470.850423	22.738816
103.601110	3472.775937	22.743834
103.292727	3484.030124	22.748851
103.697888	3503.322017	22.753869
103.908873	3490.929364	22.758887
103.624410	3480.642783	22.763904
103.928156	3511.476043	22.768922
103.883995	3503.418095	22.773939
104.134521	3521.777385	22.778957
104.079509	3501.980434	22.783975
104.728983	3510.080244	22.788992
104.543577	3517.551771	22.794010
104.933715	3493.453530	22.799027
104.940347	3502.773601	22.804045
105.065592	3530.855540	22.809063
105.294633	3522.963248	22.814080
105.314370	3534.480574	22.819098
105.187458	3545.211098	22.824115
105.505979	3536.512426	22.829133
105.280752	3550.408955	22.834151
105.129265	3548.142515	22.839168
105.431013	3539.128731	22.844186
105.694937	3533.518297	22.849203
105.725175	3529.125026	22.854221
105.664113	3546.672713	22.859239
105.745589	3554.083607	22.864256
106.216907	3560.139956	22.869274
105.915085	3570.019761	22.874291
106.135864	3568.520668	22.879309
106.422681	3558.855590	22.884327
106.637225	3555.778789	22.889344
106.753269	3559.823040	22.894362
106.346877	3561.515295	22.899379
106.631164	3576.511281	22.904397
106.986110	3595.941881	22.909415
107.052356	3589.674673	22.914432
107.294728	3592.219980	22.919450
107.244279	3598.587664	22.924467
107.284972	3583.254246	22.929485
107.316192	3583.499381	22.934503
107.512128	3586.565742	22.939520
107.570559	3598.266517	22.944538
107.443628	3609.023049	22.949555
107.885944	3601.444383	22.954573
107.807933	3609.141104	22.959591
107.762257	3607.052071	22.964608
108.154097	3607.342744	22.969626
107.912478	3628.916830	22.974643
108.455461	3641.570032	22.979661
108.907802	3627.384651	22.984679
108.760178	3635.186092	22.989696
108.785640	3650.282424	22.994714
108.921570	3636.452694	22.999731
108.729278	3628.618883	23.004749
108.882449	3640.123665	23.009767
108.865254	3640.212909	23.014784
109.628111	3649.313368	23.019802
109.179873	3654.359303	23.024819
109.515372	3655.482537	23.029837
109.735601	3660.953619	23.034855
109.809095	3665.759825	23.039872
110.133700	3653.986852	23.044890
109.952196	3650.633376	23.049907
110.252712	3637.376790	23.054925
110.067199	3644.998640	23.059943
109.945082	3649.682646	23.064960
110.239683	3662.542236	23.069978
110.054612	3668.268312	23.074995
110.351655	3679.878400	23.080013
110.378028	3688.694374	23.085031
110.430606	3698.237718	23.090048
110.717229	3693.780701	23.095066
110.798511	3703.942463	23.100083
110.995794	3716.002694	23.105101
111.434945	3692.410752	23.110119
111.321485	3688.876510	23.115136
111.614319	3705.642703	23.120154
111.872752	3707.144789	23.125171
111.537535	3701.441048	23.130189
112.040521	3691.402384	23.135207
111.893014	3695.345538	23.140224
112.007885	3695.049524	23.145242
111.607226	3708.858547	23.150259
112.098569	3712.786357	23.155277
112.439720	3721.286282	23.160295
111.996424	3721.279073	23.165312
112.279857	3726.562329	23.170330
112.184631	3735.832716	23.175347
112.435915	3729.790016	23.180365
112.783986	3740.057928	23.185383
112.485784	3753.008197	23.190400
112.900381	3748.246791	23.195418
112.838263	3747.786280	23.200435
112.902052	3746.472673	23.205453
113.180932	3763.557374	23.210471
113.029153	3786.223338	23.215488
113.904651	3770.499379	23.220506
113.876245	3770.419716	23.225523
113.820081	3764.614816	23.230541
114.085799	3780.815914	23.235559
113.454948	3783.166981	23.240576
113.971013	3791.305531	23.245594
114.197742	3799.192885	23.250611
114.153012	3795.665749	23.255629
114.238319	3791.155852	23.260647
114.314656	3810.038061	23.265664
114.641072	3818.817280	23.270682
114.914088	3844.793309	23.275699
114.911373	3832.744371	23.280717
115.028508	3816.768441	23.285735
114.888505	3843.644925	23.290752
114.806211	3833.318775	23.295770
114.872107	3825.137694	23.300787
115.443197	3843.034872	23.305805
115.601689	3859.969763	23.310823
115.392750	3868.765160	23.315840
115.844730	3833.108208	23.320858
115.835237	3869.313615	23.325875
115.626637	3876.370544	23.330893
116.107044	3874.836313	23.335911
115.909086	3884.147561	23.340928
116.166630	3896.811893	23.345946
116.592734	3911.392302	23.350963
116.843640	3907.160384	23.355981
117.110061	3899.025159	23.360999
117.154853	3908.117577	23.366016
117.290610	3894.562161	23.371034
117.501409	3897.186499	23.376051
117.232672	3898.558710	23.381069
117.758435	3893.253284	23.386087
117.684066	3886.846330	23.391104
117.481466	3886.033000	23.396122
117.526999	3890.326932	23.401139
117.550380	3890.199680	23.406157
117.937648	3890.111942	23.411175
117.443144	3884.345428	23.416192
117.894023	3888.352109	23.421210
117.875923	3913.090925	23.426227
117.851793	3940.841134	23.431245
118.087834	3923.601695	23.436263
118.263688	3922.810608	23.441280
118.229316	3934.220458	23.446298
118.318859	3956.380164	23.451315
118.624208	3961.560897	23.456333
118.904786	3944.234883	23.461351
118.857750	3957.677821	23.466368
119.264486	3974.661360	23.471386
119.242379	3987.092688	23.476403
119.117104	3983.070193	23.481421
119.573068	3969.577706	23.486439
119.505375	3987.362178	23.491456
119.944632	3999.185831	23.496474
119.815928	4004.033044	23.501491
119.643580	4011.293497	23.506509
120.123306	3998.560219	23.511527
119.848403	4012.941799	23.516544
120.370777	4025.040122	23.521562
120.620450	4026.362716	23.526579
120.549826	4033.884637	23.531597
121.061263	4035.601280	23.536615
121.003032	4032.921860	23.541632
121.288339	4023.142658	23.546650
120.851741	4030.095211	23.551667
120.967962	4041.243569	23.556685
121.572680	4048.668819	23.561703
121.395267	4059.921439	23.566720
121.686139	4050.290004	23.571738
121.642556	4064.626095	23.576755
121.439884	4067.589356	23.581773
122.034052	4055.466294	23.586791
121.739299	4066.834385	23.591808
122.110994	4084.234258	23.596826
122.320204	4094.180809	23.601843
122.337850	4089.267058	23.606861
122.417889	4079.266471	23.611879
122.534045	4095.417039	23.616896
122.849308	4101.522102	23.621914
123.215249	4110.490279	23.626931
123.322247	4116.011055	23.631949
123.586495	4114.864467	23.636967
123.491097	4109.680042	23.641984
123.736423	4110.247387	23.647002
124.044986	4105.677408	23.652019
123.716196	4107.341613	23.657037
124.141165	4095.497220	23.662055
124.283973	4094.550136	23.667072
124.268858	4103.737971	23.672090
124.502071	4104.280503	23.677107
124.326922	4103.520993	23.682125
124.674626	4091.112326	23.687143
124.578914	4092.530120	23.692160
124.679322	4094.557742	23.697178
124.667026	4087.222021	23.702195
124.818082	4097.059853	23.707213
124.709443	4087.428383	23.712231
124.490794	4096.211305	23.717248
124.576171	4109.984890	23.722266
125.157384	4112.612345	23.727283
125.058853	4118.299623	23.732301
125.219402	4132.136759	23.737319
125.060950	4140.386212	23.742336
125.384129	4149.211773	23.747354
125.420461	4156.423289	23.752371
125.288124	4185.146971	23.757389
125.950650	4173.636712	23.762407
125.874188	4188.773452	23.767424
125.957586	4209.222809	23.772442
126.065407	4207.372736	23.777459
125.964702	4220.029186	23.782477
126.359190	4223.745246	23.787495
126.820879	4240.829676	23.792512
126.992384	4238.070319	23.797530
127.166076	4244.249936	23.802547
127.289260	4249.759529	23.807565
127.761575	4240.945457	23.812583
127.718640	4254.298336	23.817600
127.769476	4257.915023	23.822618
127.835533	4248.273684	23.827635
128.136260	4259.267712	23.832653
128.465244	4261.759996	23.837671
128.327505	4254.550390	23.842688
128.397134	4243.173952	23.847706
128.653779	4238.859214	23.852723
128.345088	4250.490832	23.857741
128.709319	4235.114579	23.862759
128.782333	4255.372145	23.867776
128.612373	4271.249158	23.872794
128.791795	4273.652803	23.877811
129.097583	4288.010493	23.882829
129.222277	4270.402164	23.887847
129.347349	4297.562092	23.892864
129.189655	4305.881529	23.897882
129.509630	4314.675448	23.902899
129.294586	4319.209290	23.907917
129.938275	4320.338501	23.912935
129.971388	4332.430142	23.917952
129.970239	4341.288656	23.922970
130.557391	4344.757701	23.927987
130.221271	4340.347875	23.933005
130.626347	4341.520643	23.938023
130.476365	4350.407615	23.943040
131.069113	4347.851673	23.948058
131.377682	4345.750098	23.953075
130.688381	4369.135133	23.958093
131.502825	4351.738457	23.963111
131.459484	4355.901956	23.968128
131.388883	4357.252839	23.973146
131.764243	4356.889317	23.978163
131.331393	4359.335544	23.983181
131.425403	4371.065877	23.988199
131.632782	4382.585415	23.993216
131.769543	4382.234766	23.998234
132.244682	4388.773070	24.003251
131.918590	4389.993995	24.008269
132.658167	4405.166029	24.013287
132.692150	4409.812799	24.018304
132.362540	4426.166183	24.023322
132.466431	4426.601913	24.028339
132.613080	4433.328707	24.033357
132.855684	4442.948433	24.038375
132.876844	4448.642712	24.043392
133.256620	4445.270349	24.048410
133.263258	4439.880741	24.053427
133.165616	4474.848574	24.058445
133.722370	4475.378863	24.063463
133.967977	4475.550496	24.068480
133.959005	4486.458776	24.073498
134.152547	4482.186283	24.078515
134.276336	4495.366480	24.083533
134.440922	4498.203613	24.088551
134.532791	4503.376889	24.093568
134.438157	4510.502479	24.098586
135.016254	4499.536419	24.103603
134.811630	4510.327239	24.108621
134.895109	4519.634917	24.113639
135.303834	4520.203758	24.118656
135.211299	4543.755079	24.123674
135.332305	4532.969652	24.128691
135.172567	4535.797149	24.133709
135.656080	4561.530065	24.138727
135.691201	4566.904356	24.143744
135.609552	4571.511403	24.148762
136.332560	4579.958022	24.153779
136.021433	4585.448891	24.158797
136.570871	4598.309579	24.163815
136.571699	4591.918644	24.168832
136.451066	4590.640663	24.173850
136.626972	4595.938236	24.178867
137.047314	4604.647889	24.183885
137.082828	4615.556252	24.188903
137.370791	4612.834109	24.193920
137.475253	4609.960296	24.198938
137.655403	4599.026153	24.203955
137.647408	4607.228277	24.208973
137.524806	4629.765025	24.213991
138.199770	4635.042034	24.219008
138.123611	4638.681426	24.224026
138.581187	4622.847785	24.229043
138.423949	4623.106470	24.234061
138.254709	4632.972923	24.239079
138.571273	4633.490386	24.244096
138.529419	4632.945590	24.249114
138.644250	4627.843097	24.254131
138.794148	4648.040960	24.259149
138.790145	4657.547539	24.264167
139.133361	4659.351659	24.269184
139.199366	4665.727983	24.274202
139.326463	4660.424499	24.279219
139.454718	4665.621138	24.284237
139.839437	4682.977171	24.289255
139.956836	4671.534571	24.294272
139.927663	4686.090022	24.299290
140.077147	4687.308296	24.304307
140.070842	4706.432185	24.309325
139.801260	4710.237742	24.314343
139.916060	4716.214551	24.319360
140.143490	4740.266615	24.324378
140.688436	4745.254453	24.329395
141.087879	4740.305565	24.334413
141.170106	4752.743718	24.339431
141.174810	4771.117819	24.344448
141.316256	4780.842791	24.349466
141.444368	4778.906025	24.354483
141.603738	4776.178398	24.359501
141.349178	4793.985777	24.364519
142.093735	4791.891715	24.369536
142.231254	4790.409712	24.374554
142.343187	4799.506925	24.379571
142.519183	4792.425600	24.384589
142.642579	4792.733152	24.389607
142.791897	4806.464943	24.394624
142.568116	4827.879823	24.399642
143.244340	4825.160240	24.404659
143.453196	4829.569218	24.409677
143.309467	4824.057913	24.414695
143.826267	4815.336315	24.419712
143.672526	4817.640563	24.424730
143.600182	4805.689248	24.429747
144.000815	4829.590336	24.434765
143.833357	4851.452536	24.439783
144.218260	4844.038941	24.444800
143.967610	4847.335687	24.449818
144.389716	4841.155164	24.454835
144.619856	4858.662707	24.459853
144.456512	4882.870143	24.464871
144.738669	4885.293697	24.469888
144.938167	4876.923166	24.474906
144.786337	4877.555446	24.479923
145.064390	4889.875171	24.484941
144.851662	4910.470271	24.489959
145.359193	4907.222183	24.494976
145.015708	4920.039094	24.499994
145.433413	4931.561714	24.505011
145.745963	4936.961918	24.510029
145.838532	4943.539450	24.515047
146.364873	4931.406037	24.520064
146.222073	4953.896155	24.525082
146.367961	4960.575327	24.530099
146.226347	4969.012933	24.535117
146.423905	4964.810462	24.540135
146.593456	4983.433092	24.545152
146.871988	5009.740714	24.550170
147.117355	5002.959751	24.555187
147.190207	5011.224730	24.560205
147.015093	5015.267037	24.565223
147.360864	5027.940312	24.570240
147.426401	5032.582247	24.575258
147.566981	5036.275286	24.580275
147.878855	5053.738562	24.585293
148.042203	5063.379202	24.590311
148.383293	5059.863402	24.595328
148.093108	5072.799388	24.600346
148.811434	5084.771377	24.605363
148.953337	5093.815219	24.610381
148.819075	5098.462287	24.615399
149.288356	5077.206850	24.620416
149.420090	5090.629399	24.625434
149.692214	5086.211254	24.630451
149.611539	5096.682226	24.635469
149.508576	5111.507895	24.640487
149.977605	5113.924505	24.645504
149.850841	5108.435561	24.650522
150.041180	5113.952866	24.655539
150.484488	5116.124199	24.660557
150.382808	5131.456307	24.665575
150.598359	5131.867962	24.670592
150.523423	5132.416404	24.675610
150.565220	5143.615229	24.680627
151.000675	5150.334065	24.685645
151.139276	5163.160066	24.690663
151.125119	5157.412423	24.695680
151.050035	5165.539020	24.700698
151.046779	5188.622433	24.705715
151.470145	5195.274775	24.710733
151.312273	5212.404851	24.715751
151.942472	5220.660534	24.720768
151.879934	5229.386982	24.725786
151.613231	5228.793053	24.730803
151.934843	5258.480157	24.735821
152.142088	5261.675662	24.740839
152.747424	5265.937378	24.745856
152.695703	5290.141058	24.750874
153.161939	5299.258396	24.755891
153.981393	5275.710275	24.760909
153.645040	5286.266990	24.765927
153.736943	5280.379664	24.770944
154.043273	5305.039986	24.775962
154.121870	5309.510789	24.780979
154.385744	5306.576022	24.785997
154.210190	5307.593648	24.791015
154.381981	5311.809650	24.796032
154.478301	5307.810457	24.801050
154.277417	5311.663428	24.806067
154.510129	5310.594944	24.811085
154.436461	5333.733080	24.816103
154.678128	5330.128440	24.821120
155.018404	5343.805899	24.826138
155.089368	5341.456504	24.831155
155.231191	5350.633469	24.836173
155.291100	5352.777862	24.841191
155.871189	5358.545433	24.846208
155.778375	5380.049582	24.851226
155.791832	5398.646492	24.856243
156.531621	5380.617001	24.861261
156.086445	5385.678760	24.866279
156.376757	5395.396925	24.871296
156.845732	5419.995319	24.876314
156.510643	5422.496141	24.881331
156.866910	5410.726951	24.886349
156.918292	5435.597283	24.891367
157.277769	5436.125245	24.896384
157.394864	5447.228119	24.901402
157.382836	5451.736228	24.906419
157.773510	5461.378645	24.911437
157.334208	5466.114587	24.916455
157.222277	5479.812354	24.921472
157.914979	5496.367371	24.926490
158.197283	5505.968881	24.931507
158.633320	5511.844446	24.936525
158.800771	5523.870805	24.941543
159.049038	5518.859228	24.946560
159.307685	5523.859160	24.951578
158.980078	5537.076864	24.956595
159.335679	5536.131951	24.961613
159.961101	5549.234685	24.966631
159.776757	5556.205154	24.971648
160.223755	5563.867174	24.976666
160.234195	5563.748266	24.981683
160.133842	5568.480544	24.986701
160.314344	5559.510827	24.991719
160.733059	5565.903682	24.996736
160.653264	5594.642191	25.001754
160.806178	5596.830007	25.006771
160.980883	5579.484341	25.011789
161.332051	5591.393351	25.016807
161.410218	5587.941379	25.021824
161.580551	5588.252480	25.026842
161.356755	5620.675336	25.031859
161.765536	5613.932549	25.036877
161.254908	5612.726100	25.041895
161.472405	5653.116468	25.046912
162.043422	5635.901076	25.051930
161.444870	5671.079850	25.056947
162.151782	5667.367120	25.061965
162.241883	5677.702708	25.066983
162.377789	5697.082917	25.072000
162.584140	5704.109955	25.077018
163.120168	5710.498329	25.082035
163.060784	5724.244587	25.087053
163.097347	5740.928889	25.092071
163.482329	5729.806268	25.097088
163.562410	5729.584209	25.102106
163.620071	5755.978733	25.107123
163.925967	5761.722527	25.112141
164.079717	5773.682045	25.117159
163.878813	5789.799279	25.122176
164.148673	5801.114864	25.127194
164.368471	5811.060896	25.132211
164.805596	5809.191948	25.137229
164.625739	5830.191396	25.142247
165.009065	5831.389004	25.147264
165.551534	5847.645820	25.152282
165.639613	5857.371361	25.157299
165.997119	5856.020177	25.162317
166.124909	5849.705220	25.167335
166.045928	5857.595229	25.172352
166.577476	5846.278433	25.177370
166.341058	5869.621157	25.182387
166.795677	5874.351586	25.187405
166.625152	5873.853220	25.192423
166.724782	5884.464360	25.197440
167.062095	5884.294905	25.202458
166.995814	5907.263616	25.207475
167.290077	5906.129420	25.212493
167.566777	5908.319575	25.217511
167.376525	5925.450133	25.222528
167.891608	5925.604786	25.227546
167.819306	5936.857023	25.232563
167.895350	5932.950582	25.237581
168.282880	5963.341372	25.242599
168.388033	5954.555723	25.247616
168.815203	5948.178830	25.252634
168.646358	5970.871330	25.257651
169.353950	5991.928553	25.262669
169.346638	5991.741666	25.267687
169.400198	5997.386535	25.272704
169.544514	5988.102917	25.277722
169.895254	5998.244548	25.282739
170.265998	6007.498712	25.287757
170.505676	6030.243391	25.292775
170.498881	6026.820598	25.297792
171.032369	6015.042341	25.302810
170.989484	6022.173783	25.307827
170.975145	6020.374432	25.312845
171.185469	6015.273544	25.317863
171.242969	6005.145435	25.322880
171.474223	6014.912764	25.327898
171.370960	6016.685972	25.332915
171.716803	6029.353022	25.337933
171.584660	6034.431172	25.342951
171.473627	6029.589215	25.347968
171.826986	6027.191540	25.352986
171.741033	6050.543601	25.358003
171.831421	6070.261199	25.363021
172.305896	6067.002403	25.368039
172.053127	6094.265230	25.373056
172.614414	6089.410465	25.378074
172.596875	6109.621298	25.383091
172.992010	6118.705643	25.388109
173.288643	6133.614958	25.393127
173.121954	6133.420438	25.398144
173.380441	6152.190862	25.403162
173.394621	6158.665786	25.408179
173.333720	6179.608213	25.413197
173.917989	6193.878528	25.418215
173.710557	6205.154087	25.423232
174.284912	6205.027084	25.428250
174.572142	6221.931587	25.433267
174.821012	6224.631315	25.438285
175.117969	6250.090112	25.443303
175.038756	6253.420410	25.448320
175.618935	6264.092885	25.453338
175.571079	6265.267231	25.458355
175.691847	6280.639804	25.463373
176.040159	6278.551298	25.468391
176.319702	6277.686130	25.473408
176.848967	6279.699966	25.478426
176.862513	6309.200712	25.483443
177.302373	6308.156565	25.488461
177.358795	6303.342104	25.493479
177.176415	6310.976626	25.498496
177.548718	6305.642113	25.503514
177.555503	6308.611758	25.508531
177.666077	6305.107247	25.513549
177.506429	6305.267997	25.518567
177.548544	6320.905698	25.523584
177.707452	6334.882066	25.528602
177.988832	6356.983335	25.533619
178.426338	6369.318219	25.538637
178.488717	6368.962866	25.543655
178.360130	6388.257127	25.548672
179.025282	6381.760284	25.553690
179.130421	6402.429514	25.558707
179.093314	6406.930899	25.563725
179.167751	6414.050117	25.568743
179.448270	6412.944040	25.573760
179.921830	6424.598976	25.578778
179.743612	6452.890662	25.583795
180.068292	6459.655303	25.588813
180.530954	6457.177980	25.593831
180.368428	6465.371158	25.598848
181.015210	6481.820537	25.603866
180.915036	6486.257260	25.608883
180.885695	6481.442253	25.613901
181.248574	6481.822594	25.618919
181.326083	6480.610411	25.623936
181.548142	6493.307039	25.628954
181.554931	6503.627379	25.633971
181.786444	6503.225388	25.638989
181.882974	6514.875207	25.644007
181.747954	6539.008457	25.649024
182.544321	6533.552753	25.654042
182.583792	6553.197290	25.659059
182.391426	6573.499571	25.664077
182.780273	6562.736836	25.669095
182.949736	6579.120023	25.674112
183.237825	6588.622975	25.679130
183.365443	6605.886953	25.684148
183.303221	6606.759140	25.689165
183.774920	6613.900087	25.694183
183.965741	6635.928882	25.699200
184.147654	6626.096004	25.704218
184.362809	6639.453165	25.709236
184.585788	6649.536154	25.714253
184.716932	6654.105200	25.719271
184.861494	6676.347563	25.724288
185.188837	6692.582182	25.729306
185.581721	6685.522023	25.734324
185.061639	6700.946855	25.739341
185.610343	6716.469588	25.744359
185.763285	6723.565424	25.749376
185.990954	6727.772926	25.754394
186.470578	6740.084884	25.759412
186.882884	6741.608396	25.764429
186.736836	6744.438060	25.769447
187.072867	6748.743160	25.774464
187.245752	6752.595916	25.779482
187.420720	6764.326266	25.784500
187.590549	6776.486233	25.789517
187.758817	6775.076239	25.794535
187.535744	6780.595570	25.799552
187.879827	6791.092071	25.804570
188.155874	6796.789893	25.809588
188.242267	6802.966414	25.814605
188.509473	6815.931492	25.819623
188.647920	6821.700828	25.824640
188.963661	6826.105171	25.829658
189.002614	6844.087727	25.834676
189.092499	6862.137714	25.839693
189.591010	6853.206207	25.844711
189.234518	6867.166118	25.849728
189.810782	6883.868731	25.854746
189.941861	6890.995671	25.859764
189.781543	6901.955043	25.864781
190.137933	6925.691143	25.869799
190.262600	6920.466705	25.874816
190.402361	6929.150886	25.879834
190.589832	6942.786535	25.884852
190.609215	6952.415961	25.889869
191.048533	6965.749481	25.894887
191.060809	6980.017343	25.899904
191.433853	6980.977512	25.904922
191.443291	6976.251361	25.909940
191.544320	7015.425631	25.914957
191.725835	7009.889973	25.919975
192.117121	7027.349228	25.924992
192.289863	7043.689133	25.930010
192.887775	7038.647268	25.935028
192.811941	7069.943486	25.940045
193.184661	7081.210613	25.945063
193.595670	7074.923153	25.950080
193.556841	7066.089778	25.955098
194.067702	7088.740139	25.960116
194.105044	7095.679918	25.965133
194.519343	7079.509099	25.970151
194.470183	7094.910398	25.975168
194.686762	7106.137135	25.980186
195.343338	7123.796540	25.985204
194.985844	7118.407359	25.990221
195.534100	7111.379665	25.995239
195.284170	7129.372431	26.000256
195.292041	7130.698465	26.005274
195.553181	7140.617561	26.010292
195.412916	7155.512593	26.015309
196.043135	7162.845691	26.020327
195.989486	7176.464922	26.025344
196.380146	7181.406610	26.030362
196.858258	7192.391871	26.035380
196.522693	7223.655076	26.040397
196.765404	7216.136306	26.045415
197.104621	7225.462358	26.050432
197.351332	7242.536572	26.055450
197.615690	7248.811580	26.060468
197.626311	7254.553470	26.065485
197.948842	7283.034414	26.070503
197.995162	7267.792256	26.075520
198.341276	7318.168430	26.080538
199.057532	7309.187776	26.085556
198.882077	7301.380785	26.090573
199.622745	7310.590172	26.095591
199.482560	7299.611481	26.100608
199.688606	7341.523663	26.105626
200.206623	7312.908549	26.110644
200.023816	7335.855565	26.115661
200.320879	7306.072674	26.120679
200.309671	7321.594045	26.125696
200.569137	7340.195089	26.130714
201.051755	7324.759787	26.135732
201.072043	7372.255690	26.140749
201.058318	7337.643326	26.145767
201.216908	7360.731865	26.150784
201.524711	7358.819622	26.155802
202.149819	7377.619704	26.160820
202.056574	7387.472724	26.165837
202.218699	7372.102631	26.170855
202.119309	7382.682847	26.175872
202.050393	7387.553890	26.180890
202.650860	7390.969635	26.185908
202.465145	7412.186266	26.190925
202.431386	7416.511179	26.195943
202.969096	7423.058190	26.200960
203.013994	7430.815985	26.205978
203.175213	7467.089557	26.210996
203.626824	7466.769689	26.216013
203.682627	7454.326861	26.221031
203.989570	7491.736226	26.226048
203.851298	7495.017207	26.231066
204.363473	7494.896187	26.236084
204.661015	7512.220681	26.241101
204.666949	7537.328395	26.246119
205.139509	7539.607169	26.251136
204.872522	7542.952742	26.256154
205.097516	7564.754018	26.261172
205.374647	7578.675734	26.266189
205.764786	7579.546671	26.271207
206.153204	7592.835371	26.276224
206.091869	7624.226436	26.281242
206.467053	7615.879073	26.286260
206.790220	7627.492063	26.291277
207.111820	7666.003433	26.296295
207.460194	7645.558292	26.301312
207.294810	7646.995396	26.306330
207.447090	7680.883713	26.311348
207.999559	7645.483245	26.316365
208.365927	7697.095927	26.321383
208.103795	7680.815137	26.326400
208.234687	7726.265334	26.331418
208.991627	7685.155263	26.336436
208.819455	7714.040860	26.341453
208.965992	7744.373025	26.346471
209.397885	7720.007898	26.351488
209.319745	7752.334294	26.356506
209.683801	7758.411084	26.361524
209.553938	7766.107217	26.366541
209.883908	7784.592146	26.371559
210.459065	7779.817252	26.376576
210.665865	7794.867674	26.381594
210.978327	7808.002658	26.386612
211.093174	7827.495238	26.391629
211.300989	7814.034114	26.396647
211.911353	7814.783407	26.401664
211.735938	7811.791512	26.406682
211.791185	7840.660769	26.411700
212.152350	7841.316818	26.416717
212.376374	7846.215271	26.421735
212.515107	7849.138223	26.426752
212.470513	7878.458586	26.431770
212.956591	7878.693440	26.436788
212.949487	7873.281167	26.441805
213.026305	7878.051240	26.446823
213.113492	7895.312939	26.451840
212.887327	7914.034614	26.456858
212.973390	7909.700382	26.461876
213.232047	7930.794977	26.466893
213.960866	7966.669268	26.471911
214.248881	7977.618542	26.476928
214.010736	7974.022097	26.481946
214.618699	7996.822819	26.486964
214.774638	8008.014272	26.491981
214.847350	8021.459912	26.496999
215.328474	8024.308643	26.502016
215.441125	8054.492622	26.507034
215.820641	8053.112567	26.512052
215.974842	8092.690357	26.517069
216.129428	8096.125425	26.522087
216.409140	8097.591541	26.527104
216.408997	8118.420006	26.532122
216.881291	8128.524452	26.537140
217.040571	8146.921378	26.542157
217.353873	8152.676735	26.547175
217.872296	8151.756074	26.552192
218.111231	8165.959828	26.557210
217.848133	8176.860985	26.562228
218.201907	8188.743359	26.567245
218.836037	8198.904278	26.572263
218.693342	8208.862507	26.577280
218.715385	8221.828561	26.582298
219.561852	8221.744736	26.587316
219.688918	8237.451960	26.592333
219.457755	8262.502699	26.597351
219.914540	8253.204838	26.602368
219.893934	8259.665766	26.607386
220.368343	8264.134164	26.612404
220.654115	8287.088988	26.617421
220.722774	8295.643673	26.622439
221.131219	8295.826392	26.627456
221.055505	8314.660709	26.632474
221.580341	8326.117775	26.637492
221.762246	8333.544180	26.642509
221.639403	8330.587075	26.647527
222.331959	8358.938706	26.652544
222.062514	8367.182233	26.657562
222.645014	8361.175348	26.662580
222.778480	8361.058837	26.667597
222.729275	8374.063922	26.672615
222.992004	8393.924736	26.677632
223.330471	8408.172655	26.682650
223.550324	8397.348206	26.687668
223.853350	8419.923580	26.692685
223.798359	8428.204556	26.697703
224.041740	8444.273507	26.702720
224.185109	8462.265768	26.707738
224.370763	8450.527679	26.712756
224.919769	8481.794924	26.717773
224.948281	8499.677281	26.722791
225.525399	8484.677381	26.727808
225.318063	8483.422318	26.732826
225.727634	8521.164134	26.737844
226.193971	8531.763563	26.742861
226.446631	8527.648882	26.747879
226.499767	8518.033579	26.752896
226.668356	8537.061354	26.757914
226.970792	8553.185532	26.762932
227.234783	8555.205794	26.767949
227.199006	8563.804037	26.772967
227.595474	8595.656086	26.777984
226.984309	8604.122609	26.783002
227.608073	8612.888779	26.788020
227.864479	8631.308591	26.793037
227.747188	8661.625668	26.798055
228.661548	8659.325429	26.803072
228.919385	8679.259796	26.808090
228.942471	8688.196523	26.813108
229.009764	8706.186255	26.818125
229.449165	8720.825197	26.823143
229.982179	8727.303513	26.828160
230.287661	8741.277670	26.833178
230.608060	8751.046764	26.838196
230.680111	8755.697487	26.843213
230.622663	8757.884691	26.848231
230.628457	8781.984177	26.853248
230.816893	8789.346032	26.858266
231.643198	8799.083294	26.863284
231.515490	8816.972837	26.868301
231.837543	8818.108085	26.873319
231.943893	8824.752820	26.878336
232.141107	8850.703328	26.883354
232.536673	8855.740015	26.888372
233.316566	8863.457716	26.893389
233.360242	8866.952348	26.898407
233.520569	8872.758341	26.903424
234.102197	8880.415592	26.908442
234.408891	8882.756435	26.913460
234.532639	8894.931783	26.918477
234.020279	8889.775947	26.923495
234.741122	8893.769322	26.928512
234.968325	8912.308235	26.933530
234.636163	8919.876687	26.938548
235.021213	8932.272441	26.943565
234.988100	8952.775262	26.948583
235.182259	8945.343629	26.953600
235.572740	8974.042034	26.958618
235.567873	8992.219090	26.963636
236.139001	8996.177343	26.968653
236.116552	9012.786993	26.973671
236.677515	9028.471127	26.978688
236.712276	9047.928105	26.983706
237.106057	9070.407768	26.988724
237.678433	9070.031644	26.993741
237.877373	9088.476134	26.998759
237.694599	9079.409557	27.003776
238.093756	9103.559772	27.008794
238.273540	9104.424999	27.013812
238.440275	9120.155158	27.018829
238.328084	9129.241977	27.023847
239.096544	9135.939075	27.028864
238.954484	9162.072080	27.033882
239.005930	9173.421923	27.038900
239.629365	9172.963689	27.043917
239.737476	9210.065198	27.048935
240.107008	9209.203235	27.053952
240.315513	9224.199357	27.058970
240.854088	9226.000856	27.063988
241.047170	9244.742346	27.069005
241.117366	9264.478422	27.074023
241.390905	9254.530061	27.079040
241.498181	9273.275823	27.084058
241.579260	9301.052356	27.089076
241.976095	9306.662648	27.094093
242.053062	9316.140027	27.099111
242.438668	9344.899335	27.104128
242.421604	9347.215534	27.109146
242.781558	9367.009819	27.114164
243.331948	9387.721210	27.119181
243.121608	9400.785924	27.124199
243.881790	9395.538793	27.129216
244.018324	9422.698037	27.134234
244.260097	9442.490802	27.139252
244.839914	9449.287758	27.144269
244.686772	9454.181949	27.149287
245.042200	9471.031682	27.154304
245.174120	9479.427056	27.159322
245.564364	9496.267333	27.164340
245.569080	9508.511732	27.169357
245.779877	9526.182515	27.174375
246.385266	9531.039620	27.179392
246.922950	9536.683419	27.184410
246.486964	9565.368736	27.189428
247.004375	9572.292947	27.194445
247.483011	9584.002300	27.199463
247.576992	9602.048662	27.204480
247.621316	9608.249582	27.209498
247.779937	9627.707635	27.214516
248.306299	9619.850500	27.219533
248.470328	9658.100586	27.224551
248.889929	9651.327127	27.229568
249.029837	9672.157466	27.234586
249.189442	9685.220506	27.239604
249.826245	9690.340998	27.244621
249.890457	9708.113269	27.249639
249.944595	9715.391937	27.254656
250.134482	9742.677034	27.259674
250.598258	9752.387340	27.264692
250.867106	9734.857366	27.269709
250.319976	9787.189099	27.274727
251.082016	9764.473694	27.279744
251.035662	9795.222832	27.284762
250.917646	9811.893456	27.289780
251.249723	9817.540235	27.294797
251.738068	9841.547979	27.299815
252.144196	9862.564749	27.304832
252.117782	9885.179512	27.309850
252.580219	9898.157872	27.314868
253.021067	9916.862677	27.319885
252.819198	9936.694945	27.324903
253.054847	9937.581220	27.329920
253.468722	9955.453466	27.334938
253.986480	9982.747723	27.339956
254.355282	9987.960618	27.344973
254.590182	10008.385566	27.349991
254.876109	10028.774078	27.355008
255.033420	10026.926420	27.360026
255.075513	10058.590589	27.365044
255.855910	10039.995430	27.370061
255.593637	10067.933173	27.375079
255.813583	10076.673697	27.380096
256.907129	10109.841443	27.385114
256.884252	10112.377852	27.390132
257.107437	10105.175138	27.395149
257.987548	10124.419673	27.400167
257.973356	10134.649077	27.405184
258.138753	10136.500738	27.410202
257.968846	10136.106387	27.415220
258.604638	10156.319687	27.420237
258.247292	10183.555497	27.425255
258.281219	10179.754997	27.430272
258.819605	10213.851146	27.435290
259.106604	10209.323683	27.440308
259.168541	10236.684769	27.445325
259.435684	10261.017259	27.450343
259.423918	10260.209728	27.455360
259.884602	10300.417355	27.460378
260.103451	10296.112422	27.465396
260.551859	10338.977299	27.470413
261.201229	10341.090624	27.475431
261.440597	10349.859690	27.480448
261.834886	10374.143766	27.485466
261.861815	10385.854141	27.490484
262.310660	10401.081093	27.495501
262.558851	10412.431597	27.500519
263.006705	10429.161833	27.505536
263.007452	10426.569827	27.510554
262.803534	10443.349673	27.515572
263.434150	10456.723132	27.520589
263.635547	10472.735249	27.525607
263.487362	10509.340182	27.530624
264.067459	10510.938881	27.535642
264.239970	10525.333326	27.540660
264.530062	10525.952048	27.545677
264.827385	10557.323967	27.550695
265.077792	10554.283706	27.555712
265.461445	10577.526285	27.560730
265.436274	10598.255554	27.565748
266.075339	10592.713720	27.570765
266.050899	10613.561727	27.575783
266.290275	10632.147657	27.580800
266.636672	10632.105795	27.585818
266.801211	10656.130654	27.590836
266.923234	10658.702294	27.595853
267.215567	10692.736054	27.600871
267.141751	10716.020290	27.605888
267.858340	10725.517012	27.610906
268.039239	10746.838105	27.615924
268.788006	10762.792006	27.620941
268.981115	10777.882249	27.625959
269.109621	10791.489113	27.630976
269.661123	10788.609754	27.635994
269.599350	10812.045287	27.641012
269.754669	10827.964788	27.646029
270.490623	10843.718956	27.651047
270.626257	10850.209217	27.656064
270.714945	10862.810037	27.661082
271.007930	10875.016682	27.666100
270.928289	10893.628210	27.671117
271.412863	10906.292667	27.676135
271.703216	10931.076242	27.681152
272.234879	10939.872253	27.686170
272.165905	10955.815443	27.691188
272.541072	10980.908641	27.696205
272.624651	10997.572447	27.701223
273.098564	11014.131554	27.706240
273.455002	11040.616881	27.711258
273.324690	11058.713338	27.716276
273.940987	11061.966105	27.721293
274.431156	11078.438484	27.726311
274.187259	11114.056720	27.731328
274.839135	11117.386070	27.736346
275.110477	11135.409152	27.741364
275.336804	11145.576115	27.746381
275.574763	11167.562775	27.751399
275.734592	11182.792913	27.756416
276.290321	11198.088636	27.761434
276.182169	11226.771680	27.766452
276.508671	11238.513667	27.771469
277.285522	11246.344473	27.776487
277.340091	11252.988310	27.781504
277.508049	11274.308672	27.786522
278.029775	11289.609122	27.791540
278.180853	11305.835557	27.796557
278.806364	11313.564994	27.801575
279.014017	11329.952431	27.806592
279.182995	11335.009558	27.811610
279.114824	11343.596453	27.816628
279.670515	11361.426524	27.821645
280.161466	11373.068032	27.826663
279.873020	11387.836237	27.831680
280.355107	11374.876365	27.836698
280.379082	11413.154816	27.841716
280.948813	11415.855913	27.846733
281.308943	11424.511721	27.851751
280.976085	11455.039183	27.856768
281.802958	11450.916398	27.861786
281.261515	11477.267795	27.866804
281.983635	11488.320060	27.871821
282.533790	11496.154471	27.876839
282.333078	11541.158327	27.881856
283.147823	11546.837046	27.886874
283.178293	11561.781248	27.891892
283.472154	11588.652924	27.896909
283.814938	11595.384767	27.901927
283.900751	11614.810959	27.906944
284.023838	11641.560808	27.911962
284.068166	11660.046485	27.916980
284.587330	11695.219814	27.921997
285.100498	11700.219841	27.927015
285.364593	11720.670797	27.932032
285.646624	11744.617671	27.937050
285.791728	11779.726075	27.942068
286.173455	11781.447050	27.947085
286.508188	11796.706203	27.952103
286.507334	11825.985987	27.957120
287.377734	11846.760750	27.962138
288.031562	11859.505681	27.967156
287.925293	11864.464798	27.972173
288.199953	11883.639290	27.977191
288.390709	11906.022169	27.982208
288.770080	11911.324174	27.987226
289.089942	11928.268917	27.992244
289.158251	11933.734237	27.997261
289.764501	11951.097713	28.002279
289.774462	11971.351829	28.007296
290.156903	11989.186256	28.012314
290.038718	12017.105817	28.017332
290.479969	12032.949534	28.022349
291.039482	12043.838452	28.027367
291.258326	12073.975816	28.032384
291.374449	12087.975807	28.037402
291.932764	12106.820853	28.042420
292.457186	12129.170555	28.047437
292.770583	12149.790535	28.052455
292.798038	12150.902962	28.057472
293.187422	12163.139365	28.062490
293.227177	12181.197070	28.067508
293.657473	12197.704620	28.072525
294.239401	12211.462445	28.077543
294.204183	12242.502859	28.082560
294.490661	12242.565787	28.087578
295.060120	12250.682434	28.092596
295.261137	12275.940530	28.097613
295.817562	12275.588545	28.102631
295.938855	12298.940930	28.107648
296.494359	12295.081361	28.112666
296.674479	12286.973456	28.117684
296.433134	12313.757592	28.122701
297.164635	12331.588539	28.127719
297.256772	12329.179389	28.132736
297.456390	12349.199146	28.137754
298.008263	12370.484658	28.142772
298.135668	12379.671800	28.147789
298.253396	12392.478234	28.152807
298.234791	12416.752123	28.157824
298.467435	12440.725092	28.162842
298.915448	12445.140931	28.167860
299.090589	12482.619780	28.172877
299.704031	12497.748840	28.177895
299.707023	12515.068824	28.182912
299.840003	12524.400773	28.187930
300.404151	12566.368482	28.192948
300.792799	12580.983880	28.197965
301.214232	12595.008090	28.202983
301.301236	12631.056479	28.208000
301.896220	12641.038581	28.213018
302.073076	12657.519342	28.218036
302.026049	12689.271711	28.223053
302.418880	12696.329598	28.228071
302.836310	12736.061256	28.233088
302.895825	12760.996791	28.238106
303.495158	12774.217928	28.243124
303.814142	12802.367165	28.248141
304.268599	12808.091600	28.253159
304.388080	12840.340372	28.258176
304.726937	12862.924005	28.263194
305.197692	12874.637983	28.268212
305.614891	12891.418549	28.273229
306.229720	12919.220773	28.278247
306.629569	12923.027350	28.283264
306.393466	12932.025224	28.288282
307.010408	12943.133113	28.293300
307.491516	12957.579476	28.298317
307.620238	12963.560139	28.303335
307.815794	12986.080412	28.308352
307.873560	13002.626771	28.313370
308.424572	13013.014794	28.318388
308.410222	13033.296243	28.323405
309.251059	13054.917031	28.328423
309.322718	13066.368121	28.333440
309.161971	13086.351640	28.338458
309.924372	13113.924481	28.343476
310.037002	13123.428876	28.348493
310.523889	13131.591829	28.353511
310.490607	13162.150140	28.358528
311.033519	13177.464880	28.363546
311.830063	13196.274501	28.368564
311.531799	13219.678644	28.373581
312.144736	13216.029890	28.378599
312.665492	13219.520730	28.383616
312.736088	13252.219343	28.388634
312.689084	13253.255169	28.393652
312.957250	13282.354388	28.398669
313.459832	13301.114178	28.403687
313.355291	13327.967435	28.408704
313.975481	13341.568875	28.413722
314.112782	13349.286469	28.418740
314.020110	13388.836078	28.423757
314.816000	13406.211939	28.428775
315.021088	13420.443776	28.433792
315.364983	13439.120012	28.438810
315.624096	13456.174148	28.443828
315.785020	13479.644628	28.448845
316.682793	13502.206252	28.453863
316.965610	13527.527778	28.458880
317.175252	13547.137625	28.463898
317.627805	13539.866232	28.468916
317.910095	13577.034944	28.473933
318.174401	13593.592517	28.478951
318.588982	13605.814662	28.483968
318.901745	13621.360954	28.488986
319.500242	13635.964395	28.494004
319.490927	13662.114916	28.499021
319.968111	13688.716503	28.504039
320.447142	13678.158286	28.509056
320.427214	13713.028467	28.514074
321.280180	13716.392685	28.519092
321.166569	13747.163725	28.524109
321.519536	13753.349233	28.529127
321.669775	13772.157301	28.534144
321.961281	13774.515126	28.539162
322.014808	13801.177152	28.544180
322.396266	13834.152164	28.549197
322.955068	13841.423626	28.554215
323.160231	13878.881655	28.559232
323.264441	13898.707906	28.564250
323.825690	13901.050900	28.569268
324.140580	13941.620490	28.574285
324.494096	13962.942025	28.579303
324.830321	13982.235406	28.584320
324.788705	13999.646152	28.589338
325.649382	14018.373767	28.594356
325.598322	14040.274293	28.599373
325.942822	14067.898652	28.604391
326.344872	14086.874882	28.609408
326.479405	14119.671531	28.614426
327.176727	14135.552409	28.619444
327.134862	14153.340122	28.624461
327.684004	14167.916914	28.629479
328.451932	14189.743409	28.634496
328.558862	14212.818730	28.639514
329.217228	14226.375724	28.644532
329.093582	14244.113603	28.649549
329.633330	14252.070672	28.654567
329.957747	14272.093936	28.659584
329.690932	14289.515222	28.664602
330.411374	14291.258673	28.669620
330.842348	14320.434418	28.674637
330.750570	14341.433181	28.679655
331.150698	14370.708471	28.684672
331.347349	14380.582826	28.689690
331.875268	14389.295861	28.694708
332.389853	14426.805499	28.699725
332.509248	14444.501531	28.704743
332.480160	14467.475919	28.709760
332.876961	14484.617797	28.714778
333.659482	14499.110287	28.719796
333.843995	14538.428005	28.724813
334.000828	14554.634273	28.729831
334.629330	14557.022349	28.734848
334.891619	14590.192351	28.739866
335.232983	14616.470457	28.744884
335.953636	14632.670293	28.749901
336.315616	14646.128484	28.754919
336.599668	14664.739507	28.759936
336.817054	14688.623106	28.764954
337.175764	14694.765578	28.769972
337.653664	14725.295244	28.774989
337.537417	14725.674178	28.780007
338.282413	14752.879752	28.785024
338.502990	14764.569536	28.790042
338.924750	14781.972956	28.795060
338.972930	14817.980165	28.800077
339.374403	14835.438735	28.805095
340.092631	14849.211589	28.810112
340.033206	14867.824071	28.815130
340.446902	14895.000042	28.820148
341.135614	14910.543335	28.825165
341.094443	14933.411518	28.830183
341.751790	14940.018962	28.835200
342.063410	14961.068429	28.840218
342.509735	14990.369035	28.845236
342.584335	15008.442056	28.850253
343.071851	15023.207598	28.855271
343.481616	15033.033062	28.860288
343.635511	15052.482909	28.865306
343.933223	15068.834256	28.870324
344.157534	15079.791489	28.875341
344.381360	15101.304634	28.880359
344.883098	15128.900913	28.885376
344.992101	15148.859488	28.890394
345.204535	15175.360530	28.895412
345.372024	15204.902493	28.900429
345.659463	15225.778859	28.905447
346.316252	15257.819194	28.910464
346.243941	15286.132904	28.915482
346.958518	15310.405845	28.920500
347.128675	15348.185974	28.925517
347.332613	15356.877399	28.930535
347.813822	15386.136108	28.935552
348.007085	15404.866612	28.940570
348.554953	15441.153345	28.945588
348.885710	15455.327696	28.950605
349.137927	15487.849036	28.955623
349.927542	15506.476754	28.960640
349.835253	15530.686551	28.965658
350.185371	15557.268552	28.970676
350.697265	15578.105398	28.975693
351.117331	15598.139662	28.980711
351.474771	15633.273695	28.985728
351.800665	15660.967866	28.990746
352.147247	15684.322895	28.995764
352.287568	15699.804323	29.000781
352.928920	15735.646140	29.005799
353.451193	15746.913576	29.010816
353.422385	15771.914553	29.015834
354.018702	15807.255945	29.020852
354.493266	15822.071166	29.025869
354.710269	15847.813348	29.030887
355.216311	15875.090101	29.035904
355.540254	15888.569425	29.040922
356.069417	15927.467354	29.045940
356.049031	15929.887330	29.050957
356.407104	15965.312912	29.055975
357.339969	15984.249326	29.060992
357.261308	16012.355682	29.066010
357.495196	16033.391852	29.071028
357.828528	16064.570341	29.076045
358.394590	16084.405631	29.081063
359.034692	16109.914224	29.086080
359.201160	16134.896578	29.091098
359.452452	16151.664575	29.096116
359.931317	16168.589204	29.101133
360.235721	16185.911075	29.106151
360.526502	16203.003978	29.111168
360.563624	16227.548122	29.116186
361.363754	16253.679566	29.121204
361.621666	16281.293876	29.126221
361.640244	16303.245186	29.131239
362.096185	16332.816961	29.136256
362.519183	16349.694895	29.141274
363.119882	16391.969336	29.146292
363.125273	16409.347475	29.151309
363.374416	16444.116435	29.156327
364.127012	16471.090532	29.161344
364.271088	16487.044521	29.166362
364.517353	16515.127962	29.171380
365.019543	16537.254072	29.176397
365.551680	16571.709563	29.181415
366.446647	16589.241373	29.186432
366.306629	16610.864512	29.191450
367.267496	16625.544561	29.196468
367.666810	16646.414777	29.201485
367.362596	16650.406739	29.206503
367.869606	16670.158807	29.211520
368.379913	16699.649310	29.216538
368.573618	16709.165849	29.221556
369.019098	16716.569539	29.226573
368.930833	16743.259081	29.231591
369.444273	16756.960708	29.236608
369.531300	16778.331002	29.241626
370.068167	16815.472129	29.246644
370.310181	16840.192935	29.251661
370.756790	16874.132886	29.256679
371.290189	16883.387554	29.261696
371.454472	16911.707981	29.266714
371.950543	16939.464434	29.271732
372.245720	16975.722339	29.276749
372.977978	17000.443025	29.281767
373.504152	17023.113780	29.286784
373.561470	17050.215834	29.291802
373.977932	17073.374168	29.296820
374.427830	17088.843878	29.301837
374.415082	17117.748340	29.306855
374.717429	17152.973752	29.311872
375.495153	17178.812152	29.316890
375.426365	17210.363998	29.321908
376.198624	17235.895920	29.326925
376.437918	17257.390430	29.331943
376.989259	17288.608799	29.336960
377.393337	17305.991140	29.341978
378.098236	17321.871583	29.346996
378.715226	17333.439732	29.352013
378.501235	17371.356903	29.357031
379.287231	17371.191276	29.362048
379.853948	17397.548463	29.367066
379.754001	17423.512374	29.372084
380.729113	17437.636268	29.377101
380.696921	17450.571808	29.382119
380.980616	17480.931729	29.387136
381.120812	17507.705071	29.392154
381.645362	17527.978037	29.397172
382.435392	17541.375488	29.402189
382.290132	17583.196043	29.407207
382.604115	17593.454723	29.412224
382.954460	17625.976165	29.417242
382.921097	17660.328949	29.422260
383.945796	17685.309426	29.427277
383.805887	17711.651810	29.432295
384.151752	17733.776801	29.437312
384.588973	17782.017160	29.442330
385.133508	17805.184530	29.447348
385.515027	17822.407479	29.452365
386.017516	17869.994452	29.457383
386.617877	17895.765871	29.462400
386.876463	17926.127322	29.467418
387.015262	17943.977235	29.472436
387.555944	17960.719494	29.477453
387.935571	17993.100240	29.482471
388.294713	18004.947962	29.487488
388.470410	18040.569770	29.492506
388.850236	18066.513617	29.497524
389.383254	18089.968273	29.502541
389.534770	18120.481017	29.507559
390.038883	18142.304226	29.512576
390.503481	18172.427043	29.517594
390.938856	18206.309906	29.522612
391.682267	18221.666667	29.527629
391.859317	18255.246723	29.532647
392.141717	18275.329939	29.537664
392.108124	18296.523725	29.542682
392.634465	18326.432288	29.547700
393.388876	18348.469044	29.552717
393.489702	18385.800359	29.557735
394.143782	18411.280232	29.562752
394.641625	18443.858825	29.567770
394.873983	18473.462561	29.572788
395.340366	18489.858191	29.577805
395.606732	18518.283400	29.582823
396.138129	18551.606458	29.587840
396.497655	18573.959996	29.592858
396.950955	18608.960542	29.597876
397.609616	18627.525630	29.602893
397.850150	18659.486636	29.607911
398.030874	18676.461437	29.612928
398.727993	18710.447001	29.617946
398.923243	18734.886758	29.622964
399.533612	18764.010741	29.627981
399.706312	18784.550281	29.632999
400.191720	18815.128903	29.638016
400.525509	18858.076151	29.643034
400.810804	18882.398643	29.648052
401.169985	18901.613354	29.653069
401.221595	18936.160143	29.658087
401.532686	18958.242032	29.663104
402.119320	18986.505649	29.668122
402.570161	19037.542239	29.673140
403.250393	19071.364355	29.678157
403.187653	19104.787998	29.683175
404.122572	19117.456058	29.688192
404.590397	19171.018360	29.693210
404.568013	19201.015259	29.698228
405.222647	19212.234728	29.703245
405.564409	19257.860594	29.708263
405.966525	19296.779191	29.713280
406.480217	19304.188817	29.718298
406.686476	19354.951635	29.723316
407.516593	19387.676121	29.728333
407.869502	19418.879029	29.733351
408.285337	19433.339168	29.738368
408.669623	19474.725300	29.743386
408.637909	19491.839569	29.748404
409.351298	19508.632762	29.753421
409.862508	19544.387240	29.758439
410.170988	19558.176780	29.763456
410.653281	19577.571931	29.768474
411.118071	19600.155854	29.773492
411.170522	19638.350674	29.778509
411.686406	19664.577497	29.783527
412.405744	19673.611303	29.788544
412.722805	19708.797067	29.793562
412.643485	19750.144017	29.798580
413.465867	19767.630791	29.803597
413.762048	19795.156687	29.808615
413.847757	19821.034579	29.813632
414.633277	19851.398514	29.818650
414.842386	19884.356864	29.823668
415.410966	19908.138154	29.828685
415.546702	19949.104492	29.833703
416.093632	19978.675143	29.838720
416.780478	19985.393686	29.843738
417.282881	20044.365257	29.848756
417.924888	20056.394891	29.853773
418.196425	20070.921139	29.858791
418.327766	20118.550910	29.863808
418.990053	20137.935406	29.868826
419.226622	20168.600437	29.873844
419.635252	20194.034156	29.878861
419.683232	20248.836050	29.883879
420.543113	20263.617581	29.888896
421.049391	20290.949051	29.893914
420.926343	20333.449096	29.898932
421.801011	20350.402955	29.903949
422.296695	20386.424462	29.908967
422.524278	20420.890194	29.913984
422.863728	20445.530939	29.919002
423.260567	20475.337492	29.924020
424.291408	20507.480332	29.929037
424.444950	20538.679843	29.934055
425.074866	20566.626807	29.939072
425.286789	20590.437226	29.944090
425.812868	20625.872491	29.949108
426.378089	20648.678966	29.954125
426.718942	20676.123700	29.959143
426.778184	20691.760849	29.964160
427.305449	20720.495003	29.969178
427.724262	20758.791289	29.974196
428.115742	20789.373006	29.979213
428.694121	20816.824634	29.984231
428.771396	20850.587222	29.989248
429.529356	20873.720054	29.994266
429.756464	20915.068504	29.999284
430.033010	20942.926758	30.004301
430.978632	20961.789518	30.009319
430.890033	21007.357554	30.014336
431.234652	21037.712940	30.019354
431.706195	21066.150661	30.024372
432.163119	21089.719232	30.029389
432.607388	21127.549309	30.034407
432.973325	21155.092868	30.039424
433.517103	21177.274311	30.044442
433.560362	21219.589605	30.049460
434.258824	21248.158455	30.054477
434.681952	21278.725848	30.059495
435.089265	21313.604343	30.064512
435.582381	21344.999817	30.069530
436.299758	21370.724893	30.074548
436.821292	21404.519479	30.079565
437.172986	21434.009016	30.084583
437.365668	21464.893454	30.089600
437.910182	21495.815612	30.094618
438.504355	21527.660781	30.099636
438.614567	21565.578610	30.104653
439.183505	21585.299127	30.109671
439.115832	21627.409139	30.114688
439.618940	21651.059794	30.119706
440.200818	21701.545928	30.124724
440.758548	21744.402426	30.129741
441.679334	21770.308388	30.134759
441.667025	21798.550858	30.139776
442.253048	21828.029789	30.144794
442.456441	21873.410477	30.149812
442.803865	21908.166346	30.154829
443.333367	21940.986619	30.159847
443.514029	21982.728817	30.164864
444.213106	22027.651373	30.169882
444.729065	22072.401618	30.174900
445.341853	22087.148652	30.179917
445.855596	22120.522314	30.184935
446.316824	22174.503120	30.189952
446.798325	22198.997587	30.194970
447.354129	22230.075331	30.199988
447.607316	22263.904283	30.205005
448.045104	22295.671180	30.210023
448.572073	22340.964645	30.215040
449.217706	22366.170390	30.220058
449.571990	22402.845573	30.225076
449.932885	22429.508119	30.230093
450.604051	22456.578071	30.235111
450.893440	22496.991417	30.240128
451.593844	22528.909901	30.245146
452.062780	22562.646052	30.250164
452.482411	22590.006761	30.255181
452.992904	22607.464909	30.260199
453.297168	22647.463577	30.265216
453.826623	22682.882081	30.270234
454.457047	22710.288173	30.275252
454.610058	22736.210946	30.280269
455.004629	22763.469624	30.285287
455.217336	22805.830306	30.290304
455.690679	22824.309824	30.295322
456.084097	22870.520798	30.300340
456.819600	22898.446044	30.305357
457.323384	22916.268688	30.310375
457.647680	22941.903813	30.315392
457.731165	22974.891027	30.320410
458.109580	22995.929830	30.325428
458.939293	23033.475072	30.330445
459.115312	23060.176015	30.335463
459.473478	23108.215825	30.340480
460.149381	23126.958780	30.345498
460.498965	23170.805333	30.350516
460.793628	23208.180261	30.355533
461.764079	23243.832997	30.360551
462.099336	23270.080462	30.365568
462.267143	23309.231439	30.370586
462.929806	23339.457109	30.375604
463.265747	23381.872949	30.380621
463.622483	23422.269269	30.385639
463.822860	23457.534794	30.390656
464.739226	23491.623816	30.395674
465.186485	23527.563756	30.400692
465.428383	23566.269580	30.405709
466.211676	23600.505273	30.410727
466.695866	23640.700688	30.415744
467.441018	23672.533234	30.420762
467.743336	23705.706857	30.425780
468.071486	23747.660999	30.430797
468.954935	23764.095365	30.435815
469.194685	23817.125428	30.440832
469.572587	23843.909738	30.445850
470.158486	23871.321793	30.450868
470.387248	23917.659726	30.455885
470.981026	23939.282992	30.460903
471.365439	23985.698721	30.465920
471.788008	24019.766734	30.470938
472.124134	24075.456395	30.475956
472.351492	24095.667694	30.480973
473.336744	24136.064947	30.485991
473.516219	24182.137397	30.491008
474.215113	24211.623286	30.496026
474.938835	24253.876496	30.501044
474.751313	24287.104168	30.506061
475.392960	24321.014263	30.511079
475.765449	24376.917371	30.516096
476.359700	24419.980899	30.521114
477.205700	24458.839988	30.526132
477.508344	24490.329572	30.531149
478.150514	24525.925653	30.536167
478.412870	24571.767840	30.541184
478.987103	24610.775360	30.546202
479.351069	24645.204571	30.551220
479.989938	24690.732696	30.556237
480.645289	24718.665267	30.561255
481.066520	24757.268231	30.566272
481.603009	24789.585251	30.571290
481.845260	24811.834426	30.576308
482.066745	24848.345021	30.581325
483.190570	24865.679603	30.586343
483.450756	24908.683460	30.591360
483.997477	24940.259507	30.596378
484.441238	24966.861927	30.601396
484.569645	25004.319559	30.606413
485.244414	25042.192007	30.611431
485.945106	25071.511428	30.616448
486.091197	25099.383225	30.621466
486.707285	25141.386548	30.626484
486.685435	25177.945328	30.631501
487.555382	25203.976114	30.636519
488.077903	25252.584651	30.641536
488.256573	25279.023442	30.646554
488.801142	25315.121286	30.651572
489.102548	25359.590463	30.656589
489.690235	25400.410323	30.661607
490.199585	25448.097555	30.666624
490.526795	25481.739615	30.671642
490.973636	25520.916178	30.676660
491.381397	25577.525260	30.681677
492.266407	25623.794334	30.686695
492.832787	25668.655413	30.691712
493.205523	25698.463067	30.696730
493.689588	25726.724826	30.701748
494.081598	25791.238202	30.706765
494.593107	25833.224560	30.711783
495.447180	25873.558906	30.716800
496.274946	25908.291140	30.721818
496.553793	25934.126609	30.726836
497.241913	25985.049824	30.731853
497.628094	26009.254211	30.736871
498.514435	26038.827857	30.741888
498.749230	26082.257216	30.746906
499.552419	26097.728409	30.751924
499.781001	26146.888295	30.756941
500.486737	26178.522604	30.761959
500.965516	26217.294029	30.766976
501.011485	26237.127305	30.771994
501.898193	26272.325965	30.777012
502.084089	26317.344798	30.782029
502.673275	26353.528477	30.787047
503.128053	26381.977249	30.792064
503.561155	26438.354524	30.797082
504.255225	26466.804716	30.802100
504.709529	26508.269424	30.807117
504.958195	26542.992880	30.812135
505.354200	26585.532940	30.817152
506.023994	26626.200265	30.822170
506.383790	26660.926756	30.827188
506.841590	26711.855100	30.832205
507.514000	26736.280476	30.837223
507.905804	26780.283070	30.842240
508.031150	26827.337602	30.847258
508.943401	26870.616274	30.852276
509.334991	26902.659719	30.857293
510.105925	26931.460092	30.862311
510.516301	26954.710396	30.867328
511.055644	26997.647825	30.872346
511.603282	27024.334026	30.877364
511.869508	27070.575086	30.882381
512.564949	27104.392725	30.887399
513.094951	27152.893975	30.892416
513.295102	27188.633376	30.897434
514.205414	27216.471414	30.902452
514.951105	27247.920278	30.907469
514.843171	27285.852614	30.912487
515.527865	27324.916921	30.917504
516.198890	27367.490874	30.922522
516.429182	27393.215105	30.927540
516.875316	27450.816557	30.932557
517.316092	27480.894003	30.937575
518.091520	27534.918570	30.942592
518.294231	27586.459920	30.947610
519.062297	27622.149997	30.952628
519.401995	27652.970247	30.957645
519.687355	27700.977969	30.962663
520.267277	27753.785694	30.967680
520.732634	27801.950973	30.972698
521.724078	27844.613809	30.977716
522.058256	27897.331944	30.982733
522.579037	27931.595918	30.987751
523.020607	27974.022095	30.992768
523.322853	28025.959463	30.997786
524.504380	28065.827246	31.002804
525.135236	28110.335079	31.007821
525.566328	28153.901062	31.012839
526.272018	28196.892405	31.017856
526.872012	28237.775045	31.022874
527.471208	28266.351482	31.027892
527.825309	28292.595538	31.032909
527.958302	28364.979277	31.037927
529.211500	28374.993559	31.042944
529.380939	28419.202294	31.047962
529.862655	28464.762245	31.052980
530.207346	28511.420389	31.057997
530.924098	28556.131648	31.063015
531.389608	28591.835040	31.068032
531.663923	28634.494443	31.073050
532.282071	28667.581559	31.078068
532.635337	28723.384699	31.083085
532.883162	28763.160272	31.088103
534.032588	28819.842270	31.093120
534.514756	28864.744600	31.098138
534.983735	28905.047850	31.103156
535.460010	28941.675288	31.108173
535.980156	28990.511400	31.113191
536.658822	29033.972561	31.118208
537.380910	29069.426556	31.123226
537.787616	29104.522731	31.128244
538.205316	29157.384523	31.133261
538.584529	29191.114307	31.138279
539.239481	29217.663350	31.143296
539.579850	29257.389151	31.148314
540.105111	29299.731413	31.153332
540.703188	29354.687756	31.158349
541.379630	29389.264106	31.163367
541.851089	29429.538325	31.168384
542.249182	29478.937439	31.173402
542.867824	29506.438248	31.178420
543.188414	29556.477130	31.183437
543.482453	29600.031017	31.188455
544.526976	29637.541819	31.193472
544.560348	29703.536798	31.198490
544.912613	29748.621430	31.203508
545.209880	29803.272635	31.208525
546.080803	29850.574139	31.213543
546.679193	29912.478806	31.218560
547.112548	29968.716294	31.223578
548.087617	30011.923272	31.228596
548.536821	30050.303619	31.233613
549.019141	30108.588766	31.238631
549.854121	30158.754012	31.243648
550.250319	30212.293998	31.248666
551.040225	30254.538288	31.253684
551.687775	30301.009928	31.258701
552.108738	30356.380819	31.263719
552.759528	30393.034166	31.268736
552.971556	30458.835121	31.273754
553.439261	30502.407886	31.278772
554.105356	30555.226777	31.283789
554.391993	30607.578335	31.288807
555.190825	30649.863204	31.293824
555.503871	30718.763209	31.298842
556.415860	30764.201194	31.303860
557.086238	30828.999236	31.308877
557.740814	30880.859672	31.313895
558.299984	30910.060206	31.318912
558.505864	30969.210395	31.323930
559.373032	31014.968264	31.328948
559.941039	31077.514168	31.333965
560.612250	31122.636902	31.338983
561.047356	31152.938771	31.344000
561.645027	31238.179804	31.349018
562.076866	31264.830774	31.354036
562.577681	31316.080371	31.359053
563.193308	31374.126586	31.364071
563.911871	31406.552391	31.369088
564.232381	31461.720809	31.374106
565.114441	31502.191647	31.379124
565.848173	31565.753208	31.384141
566.179884	31617.484585	31.389159
567.040994	31658.977278	31.394176
567.263465	31691.785268	31.399194
567.990818	31737.978784	31.404212
568.352408	31775.190367	31.409229
568.872455	31825.623671	31.414247
569.609778	31869.023170	31.419264
569.790611	31926.806468	31.424282
570.888662	31959.790753	31.429300
571.469858	31993.829873	31.434317
571.513002	32048.733952	31.439335
571.974324	32091.021148	31.444352
572.284611	32143.268250	31.449370
572.949500	32202.991256	31.454388
573.491889	32251.576688	31.459405
573.943458	32319.719013	31.464423
574.839901	32365.556381	31.469440
575.269982	32420.765735	31.474458
575.724438	32472.248564	31.479476
576.443766	32523.300062	31.484493
576.892035	32571.866757	31.489511
577.619836	32624.849573	31.494528
577.912846	32682.390691	31.499546
578.570966	32745.040510	31.504564
579.177293	32813.614164	31.509581
579.913603	32870.940330	31.514599
580.650242	32920.396795	31.519616
581.104324	32983.546566	31.524634
581.726394	33040.584162	31.529652
582.571713	33086.491581	31.534669
582.857077	33145.800870	31.539687
583.688244	33200.865420	31.544704
584.143577	33260.906206	31.549722
584.801843	33306.169412	31.554740
585.467323	33367.562607	31.559757
586.090769	33422.550646	31.564775
586.881430	33472.610164	31.569792
586.939314	33528.563437	31.574810
587.532971	33578.273203	31.579828
588.720955	33633.884494	31.584845
589.169567	33689.380445	31.589863
590.141079	33747.091481	31.594880
590.737614	33788.775135	31.599898
590.777752	33839.644124	31.604916
591.909310	33876.255492	31.609933
592.339856	33923.476553	31.614951
592.975664	33980.696482	31.619968
593.377069	34038.869761	31.624986
593.711329	34095.469768	31.630004
594.504583	34136.755695	31.635021
594.914460	34200.549250	31.640039
595.731722	34254.669023	31.645056
596.242118	34307.608325	31.650074
596.867202	34350.359162	31.655092
597.673814	34402.186003	31.660109
597.751744	34467.135296	31.665127
598.399620	34517.182887	31.670144
599.236049	34575.506300	31.675162
599.561414	34621.008981	31.680180
600.580480	34655.992724	31.685197
601.053900	34708.407967	31.690215
601.636166	34753.345174	31.695232
602.091670	34807.082988	31.700250
602.928356	34851.525951	31.705268
603.369250	34899.118588	31.710285
603.862764	34943.246006	31.715303
604.522751	34997.133151	31.720320
605.180070	35047.688432	31.725338
605.720793	35099.019100	31.730356
606.604812	35124.671088	31.735373
606.827448	35194.245783	31.740391
606.958688	35237.476383	31.745408
607.797019	35302.845389	31.750426
608.415124	35371.022628	31.755444
609.056282	35425.185302	31.760461
609.300020	35481.244820	31.765479
610.083704	35543.335064	31.770496
610.747833	35603.299057	31.775514
611.260930	35665.773359	31.780532
611.945890	35724.936795	31.785549
612.167050	35779.544278	31.790567
612.994719	35836.522498	31.795584
614.367782	35898.693615	31.800602
614.595874	35968.636409	31.805620
615.486268	36016.709265	31.810637
615.789658	36069.745473	31.815655
616.927194	36149.312030	31.820672
617.286789	36191.001616	31.825690
617.799715	36262.390057	31.830708
618.813926	36303.726588	31.835725
619.195686	36362.276866	31.840743
619.540491	36416.546709	31.845760
620.135009	36482.419509	31.850778
620.912738	36541.337742	31.855796
621.767958	36594.798527	31.860813
622.355677	36666.069576	31.865831
623.057851	36722.619918	31.870848
623.600445	36777.390726	31.875866
624.192684	36820.913034	31.880884
625.099551	36884.729158	31.885901
625.532790	36952.658514	31.890919
626.612137	36998.736564	31.895936
627.243253	37046.118998	31.900954
627.739414	37083.924896	31.905972
628.475602	37139.425964	31.910989
628.745966	37204.416740	31.916007
629.599918	37252.500534	31.921024
630.307871	37301.589933	31.926042
630.460703	37367.511325	31.931060
631.548285	37406.098779	31.936077
631.886553	37471.559060	31.941095
632.278225	37521.308038	31.946112
632.910226	37574.775968	31.951130
633.488992	37632.630823	31.956148
634.604049	37671.460466	31.961165
634.540091	37732.453019	31.966183
635.166845	37785.277612	31.971200
635.839129	37852.781535	31.976218
636.290300	37881.297361	31.981236
636.989035	37951.794671	31.986253
637.440676	38012.824380	31.991271
638.143627	38063.411473	31.996288
638.971265	38123.166101	32.001306
639.167125	38196.503683	32.006324
639.969502	38246.559921	32.011341
640.348561	38315.462029	32.016359
641.047479	38385.718316	32.021376
641.867969	38451.413069	32.026394
642.363125	38521.592000	32.031412
642.917056	38579.004699	32.036429
643.750549	38657.005983	32.041447
644.120020	38715.847070	32.046464
644.670432	38800.751264	32.051482
645.713598	38866.222964	32.056500
646.795775	38898.439966	32.061517
647.170720	38999.447967	32.066535
648.292128	39031.304208	32.071552
649.419053	39116.335775	32.076570
649.299613	39177.719221	32.081588
650.321124	39204.697419	32.086605
650.966120	39286.607322	32.091623
651.421935	39348.778048	32.096640
652.376096	39401.538222	32.101658
652.697847	39457.666376	32.106676
653.275948	39525.288168	32.111693
653.932155	39598.850229	32.116711
654.647109	39662.157136	32.121728
655.207197	39723.863242	32.126746
655.666729	39787.810481	32.131764
656.868653	39847.908969	32.136781
657.781853	39906.192983	32.141799
658.316111	39981.215769	32.146816
658.658368	40044.446265	32.151834
659.518225	40087.592221	32.156852
659.926063	40157.287240	32.161869
660.896646	40227.105812	32.166887
661.272787	40264.849646	32.171904
662.228498	40352.294169	32.176922
662.632227	40386.392877	32.181940
663.261914	40475.602437	32.186957
664.118903	40515.760163	32.191975
664.317653	40583.561685	32.196992
665.532137	40646.909411	32.202010
666.011385	40721.655648	32.207028
666.680220	40781.113796	32.212045
667.377639	40840.338947	32.217063
668.000720	40906.371112	32.222080
669.094788	40941.786549	32.227098
669.447922	41015.658460	32.232116
669.918910	41068.488139	32.237133
670.781717	41117.128726	32.242151
671.357582	41171.044307	32.247168
672.277421	41225.586532	32.252186
672.232842	41271.975073	32.257204
673.344546	41353.333333	32.262221
674.045764	41398.247272	32.267239
674.631629	41456.725918	32.272256
675.261841	41508.318909	32.277274
675.607333	41590.109389	32.282292
676.194788	41631.421289	32.287309
677.032264	41697.587960	32.292327
677.368215	41777.841705	32.297344
678.262382	41849.197748	32.302362
678.676015	41904.062448	32.307380
679.677770	41973.645082	32.312397
680.086036	42061.262804	32.317415
680.646110	42112.096038	32.322432
681.804592	42195.311760	32.327450
682.241536	42246.874669	32.332468
683.141052	42337.257423	32.337485
683.922482	42381.337947	32.342503
684.370507	42460.432092	32.347520
684.776791	42537.539824	32.352538
685.576597	42623.949962	32.357556
686.650446	42676.696497	32.362573
687.472951	42745.963847	32.367591
687.830658	42826.534446	32.372608
688.992531	42872.716288	32.377626
689.148874	42966.687163	32.382644
690.004932	43022.068523	32.387661
691.120914	43076.269992	32.392679
691.498740	43178.070301	32.397696
692.552151	43228.629571	32.402714
693.194966	43293.272022	32.407732
693.760744	43351.558448	32.412749
694.525658	43440.460676	32.417767
695.141588	43479.387829	32.422784
695.928927	43574.945958	32.427802
696.583360	43613.397287	32.432820
696.925512	43699.119181	32.437837
697.540724	43785.927292	32.442855
698.635653	43852.436642	32.447872
699.134224	43904.269134	32.452890
699.861536	43997.268319	32.457908
700.522428	44059.201116	32.462925
701.443438	44107.380372	32.467943
701.874403	44213.657622	32.472960
702.921617	44246.660013	32.477978
703.384404	44351.507224	32.482996
703.966755	44390.911798	32.488013
704.997048	44488.969350	32.493031
705.428945	44563.082112	32.498048
706.385610	44608.995299	32.503066
706.911581	44688.298593	32.508084
707.522419	44762.118733	32.513101
708.377811	44823.628977	32.518119
708.678135	44879.224651	32.523136
709.695514	44948.901991	32.528154
710.500115	45006.143345	32.533172
710.991967	45058.384149	32.538189
711.568973	45161.337918	32.543207
712.278491	45198.935407	32.548224
712.690937	45289.019984	32.553242
713.534243	45368.897326	32.558260
714.257236	45421.796449	32.563277
714.895523	45488.555141	32.568295
715.240714	45579.607799	32.573312
716.350429	45659.658580	32.578330
717.014875	45721.268653	32.583348
717.438451	45810.521304	32.588365
718.199869	45898.799433	32.593383
718.860632	45966.007507	32.598400
719.768468	46054.054895	32.603418
720.655284	46140.721114	32.608436
721.304321	46204.786633	32.613453
722.332952	46293.279755	32.618471
723.143131	46365.589030	32.623488
723.824950	46434.177378	32.628506
724.741969	46530.529298	32.633524
725.337795	46580.451896	32.638541
726.104685	46693.757741	32.643559
726.962816	46730.388407	32.648576
727.683619	46822.432015	32.653594
728.484999	46892.123123	32.658612
729.056770	46956.358290	32.663629
730.024438	47048.672969	32.668647
730.702171	47097.656442	32.673664
731.628714	47174.733485	32.678682
732.010330	47264.852081	32.683700
733.009550	47322.940839	32.688717
733.438397	47391.986519	32.693735
733.993164	47485.716433	32.698752
735.181764	47526.536542	32.703770
735.682990	47633.681604	32.708788
736.533683	47687.838754	32.713805
737.374073	47777.315869	32.718823
737.593705	47858.020080	32.723840
738.584686	47931.124206	32.728858
739.171962	48018.730837	32.733876
739.880489	48091.318980	32.738893
741.136216	48164.732151	32.743911
741.617258	48243.396133	32.748928
742.590613	48316.167060	32.753946
742.978867	48398.749485	32.758964
743.462428	48479.764751	32.763981
744.619094	48561.720771	32.768999
745.241188	48644.642592	32.774016
746.210573	48713.623175	32.779034
746.937078	48782.431291	32.784052
747.383982	48851.287343	32.789069
748.615183	48915.184878	32.794087
748.723195	48976.642543	32.799104
749.579077	49041.546880	32.804122
750.343553	49130.433967	32.809140
751.023767	49193.069738	32.814157
751.790637	49261.103385	32.819175
751.980636	49352.272864	32.824192
752.901337	49419.979716	32.829210
753.931854	49492.481338	32.834228
754.700904	49585.563517	32.839245
755.205498	49656.953631	32.844263
755.947805	49742.540422	32.849280
756.674549	49839.401431	32.854298
757.447107	49903.798386	32.859316
758.161989	50000.173060	32.864333
759.520878	50072.735224	32.869351
759.757693	50157.031837	32.874368
760.580393	50229.228758	32.879386
761.404392	50313.012948	32.884404
762.420135	50403.084453	32.889421
763.278639	50490.025863	32.894439
763.694901	50575.848437	32.899456
764.252952	50656.205421	32.904474
765.280667	50736.794096	32.909492
765.928995	50820.779044	32.914509
767.201431	50896.378284	32.919527
767.579640	50990.615578	32.924544
768.461157	51072.305127	32.929562
769.486911	51142.371740	32.934580
770.089652	51252.356324	32.939597
770.966598	51324.987695	32.944615
771.726391	51392.853905	32.949632
772.710914	51472.474500	32.954650
773.546795	51555.625173	32.959668
773.938900	51637.464642	32.964685
774.912428	51728.843433	32.969703
775.336107	51814.579256	32.974720
776.074127	51899.467024	32.979738
776.980351	51970.912920	32.984756
778.241935	52056.970961	32.989773
778.825613	52145.409558	32.994791
779.646359	52234.315795	32.999808
780.393716	52307.558778	33.004826
781.176475	52392.451225	33.009844
781.862327	52482.532074	33.014861
782.707383	52554.343497	33.019879
783.179790	52645.125042	33.024896
784.038143	52732.525520	33.029914
785.133996	52813.598724	33.034932
785.860198	52889.384863	33.039949
786.969182	52965.369182	33.044967
787.769641	53046.913366	33.049984
788.765306	53118.472678	33.055002
789.272285	53191.400891	33.060020
789.882579	53265.464918	33.065037
791.140681	53328.670202	33.070055
791.535027	53409.671549	33.075072
792.113306	53478.060574	33.080090
793.112518	53555.387266	33.085108
793.750497	53625.720987	33.090125
794.613307	53700.324177	33.095143
795.203026	53778.502888	33.100160
795.913201	53842.942880	33.105178
796.687951	53919.183263	33.110196
796.860254	54016.357095	33.115213
797.979127	54098.451867	33.120231
798.998771	54181.850549	33.125248
799.712152	54268.568235	33.130266
800.553146	54354.117145	33.135284
801.196130	54436.639546	33.140301
801.764876	54518.312473	33.145319
802.378631	54609.406482	33.150336
803.426988	54707.258893	33.155354
804.264678	54800.316167	33.160372
804.608891	54900.677363	33.165389
805.748815	54989.177065	33.170407
806.658148	55078.427246	33.175424
807.744857	55181.058030	33.180442
808.903887	55255.437400	33.185460
809.760056	55352.588433	33.190477
810.525521	55427.018523	33.195495
811.544070	55515.934666	33.200512
812.301984	55600.590451	33.205530
813.457049	55663.795043	33.210548
813.855114	55768.849301	33.215565
814.804421	55841.979753	33.220583
815.454815	55936.802420	33.225600
816.471895	56003.366611	33.230618
817.396041	56085.081537	33.235636
817.949845	56172.266144	33.240653
819.003742	56266.859000	33.245671
819.774494	56349.385514	33.250688
820.661212	56418.850794	33.255706
821.570133	56501.504364	33.260724
821.892577	56597.970443	33.265741
822.794020	56690.736804	33.270759
823.712633	56766.123386	33.275776
824.391321	56862.508900	33.280794
825.161710	56943.175698	33.285812
826.323232	57028.815568	33.290829
827.213132	57107.087053	33.295847
827.789802	57196.662542	33.300864
828.507838	57286.449567	33.305882
829.286909	57374.948820	33.310900
830.144854	57462.239519	33.315917
830.704982	57564.579208	33.320935
831.401678	57653.459102	33.325952
832.588612	57746.280061	33.330970
833.646495	57821.475183	33.335988
834.078431	57897.502633	33.341005
834.829951	57984.673846	33.346023
835.665565	58070.124203	33.351040
836.287114	58157.076992	33.356058
837.361662	58241.574609	33.361076
838.043621	58338.055724	33.366093
838.929755	58425.861083	33.371111
839.971501	58500.944739	33.376128
840.732784	58604.186328	33.381146
841.833892	58685.471090	33.386164
842.255841	58785.304463	33.391181
843.459706	58864.957264	33.396199
844.230459	58942.794583	33.401216
844.487604	59039.716343	33.406234
845.682482	59135.485411	33.411252
846.531060	59226.056678	33.416269
847.328975	59323.155891	33.421287
848.302346	59432.935141	33.426304
848.999900	59503.420875	33.431322
850.019713	59597.079645	33.436340
850.872833	59702.999481	33.441357
851.682790	59785.595122	33.446375
852.582560	59880.006893	33.451392
853.328017	59976.543256	33.456410
854.452860	60068.871126	33.461428
855.046873	60179.210845	33.466445
856.146675	60262.671765	33.471463
856.803035	60348.808396	33.476480
858.021090	60454.014551	33.481498
858.955618	60540.205672	33.486516
859.913319	60640.595201	33.491533
860.548071	60742.249090	33.496551
861.510781	60815.349768	33.501568
861.965706	60922.028209	33.506586
863.339647	61014.207450	33.511604
863.916614	61118.398501	33.516621
865.133715	61200.509361	33.521639
865.910147	61298.304287	33.526656
866.630539	61375.016793	33.531674
867.751513	61480.790420	33.536692
868.430826	61587.714798	33.541709
869.224280	61664.682091	33.546727
870.239267	61752.356338	33.551744
870.787821	61854.045765	33.556762
871.975287	61958.974759	33.561780
872.752096	62041.475132	33.566797
873.565616	62149.713846	33.571815
874.613144	62242.374196	33.576832
875.530383	62342.630874	33.581850
876.212682	62428.460332	33.586868
877.048125	62538.649213	33.591885
878.195957	62639.009708	33.596903
879.427085	62711.794031	33.601920
879.831749	62801.054408	33.606938
880.846821	62893.666290	33.611956
881.910073	62943.493230	33.616973
882.457212	63072.064860	33.621991
883.163287	63130.560308	33.627008
884.342761	63224.979151	33.632026
885.007708	63291.565538	33.637044
885.558953	63407.160313	33.642061
886.641722	63482.333256	33.647079
887.378516	63558.423643	33.652096
888.046730	63676.792968	33.657114
889.066959	63753.066396	33.662132
889.592890	63879.925851	33.667149
890.539588	63954.216011	33.672167
891.403738	64079.005080	33.677184
892.337237	64145.576995	33.682202
893.422290	64279.638632	33.687220
893.986633	64353.877517	33.692237
894.856486	64502.735275	33.697255
896.052608	64586.282162	33.702272
896.865855	64669.290324	33.707290
897.934989	64802.878164	33.712308
898.817307	64878.650669	33.717325
899.538091	65001.921163	33.722343
900.612425	65087.599220	33.727360
901.589508	65212.763035	33.732378
902.676887	65299.046322	33.737396
903.266511	65415.187227	33.742413
904.266574	65510.498680	33.747431
905.254248	65610.417185	33.752448
905.903756	65726.465180	33.757466
907.218532	65825.817974	33.762484
908.538807	65932.273243	33.767501
909.118261	66031.813600	33.772519
910.217306	66124.566823	33.777536
911.279059	66226.984410	33.782554
912.357208	66333.549921	33.787572
913.358202	66410.304475	33.792589
914.372189	66503.758419	33.797607
915.296558	66597.994554	33.802624
915.708259	66705.151401	33.807642
916.346243	66809.774571	33.812660
917.731709	66907.002459	33.817677
918.172945	67008.265917	33.822695
919.363109	67112.284889	33.827712
920.071805	67228.174615	33.832730
921.287134	67333.552061	33.837748
922.310727	67411.936777	33.842765
922.882119	67523.181918	33.847783
924.354032	67622.717990	33.852800
924.818528	67732.553705	33.857818
925.859470	67824.774792	33.862836
927.316900	67930.278058	33.867853
927.804691	68020.869851	33.872871
928.748153	68120.246208	33.877888
929.729069	68224.544521	33.882906
930.696678	68315.105561	33.887924
931.386552	68407.208404	33.892941
932.357609	68505.514732	33.897959
933.422804	68574.652209	33.902976
934.012694	68672.135610	33.907994
934.590952	68770.600543	33.913012
935.849694	68860.985142	33.918029
936.317355	68959.317011	33.923047
937.557967	69071.033117	33.928064
938.102856	69181.236969	33.933082
938.945696	69276.573105	33.938100
939.911613	69382.143528	33.943117
940.609439	69486.329404	33.948135
941.790444	69605.797121	33.953152
942.751986	69718.647980	33.958170
943.470210	69827.103176	33.963188
944.830654	69936.815101	33.968205
945.590722	70056.504180	33.973223
946.450891	70169.449586	33.978240
947.466041	70294.867704	33.983258
948.548519	70384.270242	33.988276
949.517419	70510.107760	33.993293
950.293260	70624.446517	33.998311
951.883865	70743.224216	34.003328
952.462487	70836.341838	34.008346
953.220870	70956.194630	34.013364
954.690917	71086.252394	34.018381
955.326940	71168.274172	34.023399
956.685825	71311.385439	34.028416
957.357464	71401.748847	34.033434
958.285809	71517.603861	34.038452
959.603024	71619.061494	34.043469
960.380721	71760.910070	34.048487
961.559785	71841.679359	34.053504
962.276568	71962.979164	34.058522
963.211345	72087.650665	34.063540
964.201298	72171.288370	34.068557
965.157185	72330.608509	34.073575
966.436205	72411.105168	34.078592
967.242169	72535.484061	34.083610
968.253598	72656.943437	34.088628
969.382742	72767.207133	34.093645
970.040988	72879.208180	34.098663
970.990346	72999.150407	34.103680
972.589197	73080.559350	34.108698
973.273217	73233.718673	34.113716
974.336889	73324.211736	34.118733
975.384081	73429.203295	34.123751
976.364961	73545.245068	34.128768
976.962535	73660.413299	34.133786
978.137671	73766.498414	34.138804
978.992680	73888.242964	34.143821
979.699504	73991.490724	34.148839
980.649365	74106.472783	34.153856
981.615231	74239.778389	34.158874
982.949014	74328.855478	34.163892
983.734321	74424.257251	34.168909
984.769630	74556.631323	34.173927
985.616505	74626.621033	34.178944
986.620975	74769.352334	34.183962
987.569414	74834.757772	34.188980
988.522756	74971.703849	34.193997
989.069535	75047.961015	34.199015
990.441490	75158.900768	34.204032
991.224697	75305.677594	34.209050
992.172514	75393.670692	34.214068
993.180722	75501.213453	34.219085
994.361832	75639.821481	34.224103
995.322589	75750.810967	34.229120
996.532254	75856.674166	34.234138
997.046688	75959.785724	34.239156
998.219822	76100.666951	34.244173
998.922585	76208.394799	34.249191
1000.242968	76349.526088	34.254208
1001.671463	76447.173464	34.259226
1002.064659	76592.738791	34.264244
1003.451783	76685.856248	34.269261
1004.289118	76816.153208	34.274279
1005.405817	76935.302386	34.279296
1006.514521	77043.753781	34.284314
1007.423528	77179.628554	34.289332
1008.737839	77266.553994	34.294349
1009.314820	77426.758629	34.299367
1010.746400	77520.511189	34.304384
1011.841939	77671.812341	34.309402
1012.904867	77773.822009	34.314420
1014.439647	77851.948738	34.319437
1015.190714	78011.270731	34.324455
1016.278783	78100.530004	34.329472
1017.067211	78231.646508	34.334490
1017.804378	78323.825709	34.339508
1019.541202	78432.190915	34.344525
1020.265864	78585.295972	34.349543
1021.299140	78658.303832	34.354560
1022.617625	78798.984739	34.359578
1023.187442	78883.153362	34.364596
1024.438804	79028.074983	34.369613
1025.509599	79118.333794	34.374631
1026.436228	79251.798778	34.379648
1027.527677	79346.580918	34.384666
1028.429137	79459.584813	34.389684
1029.674129	79585.239450	34.394701
1030.572954	79686.216567	34.399719
1031.196652	79814.689393	34.404736
1032.635182	79932.856766	34.409754
1033.661051	80046.248635	34.414772
1034.362723	80165.830354	34.419789
1035.432730	80297.528417	34.424807
1036.501801	80393.633718	34.429824
1037.687489	80521.642294	34.434842
1038.609989	80644.232094	34.439860
1039.329838	80733.232718	34.444877
1040.453720	80854.957345	34.449895
1041.411915	80958.055167	34.454912
1042.352112	81055.726427	34.459930
1043.088518	81176.452617	34.464948
1043.986117	81299.189330	34.469965
1045.278645	81428.975461	34.474983
1046.363654	81541.797216	34.480000
1047.467293	81660.350147	34.485018
1048.326977	81788.127634	34.490036
1049.397453	81916.839564	34.495053
1050.375216	82036.685287	34.500071
1050.984120	82162.437826	34.505088
1052.185531	82305.108326	34.510106
1053.285793	82428.243021	34.515124
1054.067372	82545.436179	34.520141
1055.314252	82708.755166	34.525159
1056.614396	82808.672204	34.530176
1057.600893	82949.939941	34.535194
1058.772154	83074.205082	34.540212
1060.184718	83203.205600	34.545229
1061.008341	83358.606133	34.550247
1061.987856	83474.710933	34.555264
1063.250394	83599.002603	34.560282
1063.738097	83763.449460	34.565300
1064.901411	83860.346060	34.570317
1066.130534	84030.992838	34.575335
1067.425363	84153.955012	34.580352
1068.202654	84287.665793	34.585370
1069.178146	84426.005395	34.590388
1070.543094	84579.191930	34.595405
1072.097935	84711.346560	34.600423
1072.903182	84841.636024	34.605440
1074.413533	84970.258824	34.610458
1075.715527	85100.401327	34.615476
1076.704648	85227.445796	34.620493
1077.657530	85362.494793	34.625511
1078.356410	85497.212021	34.630528
1079.858056	85624.929740	34.635546
1080.480967	85756.246489	34.640564
1081.988152	85882.403185	34.645581
1082.730263	86033.144956	34.650599
1083.608848	86176.512702	34.655616
1085.108985	86280.688614	34.660634
1085.748324	86453.832453	34.665652
1087.503170	86565.992958	34.670669
1088.669017	86700.144030	34.675687
1089.433803	86855.491109	34.680704
1090.992215	86961.614888	34.685722
1091.481212	87103.925343	34.690740
1092.542564	87230.388574	34.695757
1093.856983	87366.701669	34.700775
1094.703489	87509.413223	34.705792
1095.866480	87645.530869	34.710810
1097.223146	87759.253258	34.715828
1098.023871	87886.166503	34.720845
1099.002019	88015.923066	34.725863
1099.817885	88142.759541	34.730880
1100.858982	88272.242059	34.735898
1101.556617	88400.420446	34.740916
1102.993600	88533.939158	34.745933
1104.077784	88659.306898	34.750951
1104.703681	88817.795117	34.755968
1106.162734	88940.777806	34.760986
1106.839571	89099.898676	34.766004
1107.806701	89248.932544	34.771021
1108.947572	89397.769065	34.776039
1110.447512	89516.302953	34.781056
1111.516911	89696.284770	34.786074
1112.683095	89830.904325	34.791092
1113.787945	89981.287281	34.796109
1115.107662	90124.750340	34.801127
1115.946350	90269.049728	34.806144
1117.184324	90413.520559	34.811162
1118.451329	90583.802558	34.816180
1119.514638	90720.638439	34.821197
1120.813119	90864.881299	34.826215
1121.700794	91011.593640	34.831232
1122.698852	91172.620129	34.836250
1123.805466	91338.999856	34.841268
1125.139356	91472.274790	34.846285
1126.345131	91623.070428	34.851303
1127.426270	91774.993698	34.856320
1129.023875	91921.283013	34.861338
1130.043120	92078.094381	34.866356
1131.068818	92236.259295	34.871373
1132.602967	92370.077049	34.876391
1133.828525	92519.421047	34.881408
1134.797284	92672.506830	34.886426
1135.956816	92816.936431	34.891444
1136.894928	92955.343079	34.896461
1138.391074	93134.501054	34.901479
1139.214738	93252.416444	34.906496
1140.273225	93422.785267	34.911514
1141.459953	93561.295320	34.916532
1142.683688	93709.838073	34.921549
1143.934774	93870.692266	34.926567
1144.857306	94036.508121	34.931584
1146.182751	94161.318767	34.936602
1147.083074	94329.929710	34.941620
1148.329993	94493.464612	34.946637
1149.604435	94633.845991	34.951655
1150.457916	94784.529487	34.956672
1151.700820	94960.377435	34.961690
1153.044173	95083.495221	34.966708
1153.781478	95279.913924	34.971725
1155.431201	95407.070990	34.976743
1156.201535	95583.119173	34.981760
1157.870942	95721.268611	34.986778
1158.864128	95846.299665	34.991796
1160.104695	96002.970734	34.996813
1161.525886	96111.450659	35.001831
1162.437316	96263.419001	35.006848
1163.629457	96405.804532	35.011866
1164.723610	96535.447475	35.016884
1165.466448	96666.772763	35.021901
1166.861709	96815.871892	35.026919
1167.771826	96973.601753	35.031936
1168.960955	97103.334075	35.036954
1170.208217	97272.879849	35.041972
1171.206076	97411.374196	35.046989
1172.552083	97562.307977	35.052007
1173.599526	97722.077188	35.057024
1174.767357	97862.546313	35.062042
1175.912415	98029.507636	35.067060
1176.978249	98165.781620	35.072077
1178.206378	98337.881543	35.077095
1178.824717	98495.497582	35.082112
1180.546801	98621.649069	35.087130
1181.605011	98833.173946	35.092148
1182.690261	98958.644092	35.097165
1183.976629	99147.006145	35.102183
1185.188843	99294.524760	35.107200
1186.301248	99457.984188	35.112218
1187.704040	99636.822918	35.117236
1189.048761	99780.723746	35.122253
1190.222563	99943.272160	35.127271
1191.126656	100109.793525	35.132288
1192.341278	100268.604963	35.137306
1193.823627	100435.757997	35.142324
1194.508352	100589.309721	35.147341
1196.046381	100788.919751	35.152359
1196.938815	100933.633636	35.157376
1198.495818	101120.608537	35.162394
1199.682229	101297.564833	35.167412
1201.027374	101454.623734	35.172429
1202.420871	101614.447312	35.177447
1203.362503	101794.065769	35.182464
1204.694180	101962.943174	35.187482
1205.983944	102127.994122	35.192500
1206.936776	102295.630756	35.197517
1208.374060	102445.449547	35.202535
1209.626148	102624.392314	35.207552
1210.601866	102801.273342	35.212570
1211.970910	102963.096908	35.217588
1213.052009	103118.146250	35.222605
1214.543209	103318.013253	35.227623
1215.598084	103483.788196	35.232640
1216.808972	103633.195010	35.237658
1217.895859	103822.183653	35.242676
1219.168296	103996.406832	35.247693
1220.356166	104149.845083	35.252711
1221.768038	104353.245472	35.257728
1222.970476	104490.832223	35.262746
1224.219816	104639.568555	35.267764
1225.341501	104821.674839	35.272781
1226.979794	104952.183521	35.277799
1227.848772	105113.025630	35.282816
1229.283280	105268.672094	35.287834
1230.349876	105411.329343	35.292852
1231.582117	105581.147204	35.297869
1232.784062	105722.721663	35.302887
1234.282784	105876.963364	35.307904
1235.142684	106041.755752	35.312922
1236.303421	106185.250683	35.317940
1237.216004	106376.553010	35.322957
1238.843440	106524.374054	35.327975
1239.754648	106684.416362	35.332992
1240.899753	106876.388192	35.338010
1242.516060	107033.112140	35.343028
1243.566579	107187.332318	35.348045
1244.823725	107353.007236	35.353063
1246.021704	107549.007435	35.358080
1247.555219	107715.071269	35.363098
1248.803650	107889.687545	35.368116
1249.946186	108067.764842	35.373133
1251.267615	108221.448604	35.378151
1252.062346	108423.981881	35.383168
1253.446624	108583.854038	35.388186
1254.798477	108752.080455	35.393204
1255.477197	108961.668279	35.398221
1257.048881	109122.014200	35.403239
1258.317499	109294.637404	35.408256
1259.928191	109507.828674	35.413274
1261.742309	109676.184220	35.418292
1262.729777	109847.071181	35.423309
1264.142334	110040.943454	35.428327
1265.743779	110203.355168	35.433344
1266.741666	110382.618090	35.438362
1268.574897	110541.336756	35.443380
1269.696036	110712.562980	35.448397
1270.851610	110889.127131	35.453415
1272.553337	111067.276763	35.458432
1273.301299	111211.076039	35.463450
1274.817007	111411.456046	35.468468
1275.629621	111566.134313	35.473485
1276.908786	111766.978917	35.478503
1278.404158	111914.157562	35.483520
1279.437553	112122.640004	35.488538
1280.808569	112265.377902	35.493556
1281.782390	112485.633983	35.498573
1283.401016	112628.556167	35.503591
1284.420322	112856.600636	35.508608
1285.573653	113004.637743	35.513626
1287.078358	113215.130749	35.518644
1287.983215	113373.015067	35.523661
1289.549699	113558.585255	35.528679
1290.760140	113763.622308	35.533696
1291.977485	113943.996666	35.538714
1293.691650	114097.578849	35.543732
1294.928755	114269.083459	35.548749
1295.845296	114435.949279	35.553767
1296.967072	114606.613581	35.558784
1298.642084	114779.432138	35.563802
1299.536307	114925.122517	35.568820
1300.390796	115129.170112	35.573837
1302.099993	115297.264089	35.578855
1303.108946	115504.772084	35.583872
1304.656835	115640.904481	35.588890
1306.020160	115850.156940	35.593908
1307.436796	116020.093883	35.598925
1308.142337	116219.242168	35.603943
1309.760061	116389.428188	35.608960
1310.652176	116602.142528	35.613978
1312.778959	116771.661402	35.618996
1313.643900	116968.688294	35.624013
1315.681830	117146.745545	35.629031
1316.583667	117327.485479	35.634048
1317.632600	117529.660092	35.639066
1319.294479	117697.460940	35.644084
1320.418850	117888.660511	35.649101
1321.826692	118101.254717	35.654119
1322.678336	118293.178119	35.659136
1324.676471	118461.873918	35.664154
1326.121219	118685.426983	35.669172
1327.185161	118853.862295	35.674189
1328.499568	119047.952834	35.679207
1330.006924	119265.169296	35.684224
1331.199005	119438.058255	35.689242
1332.530637	119643.851654	35.694260
1333.996342	119833.327135	35.699277
1335.437477	120022.326682	35.704295
1337.102615	120241.856400	35.709312
1338.097029	120418.056939	35.714330
1339.358374	120629.637784	35.719348
1340.675793	120806.384821	35.724365
1342.426728	120999.337779	35.729383
1343.737800	121214.208177	35.734400
1344.457839	121408.455143	35.739418
1345.956743	121580.644675	35.744436
1347.648037	121817.065376	35.749453
1348.923268	121982.403499	35.754471
1350.359467	122202.669964	35.759488
1351.548137	122373.622183	35.764506
1353.327788	122597.548196	35.769524
1353.988180	122788.851199	35.774541
1355.929923	122968.920486	35.779559
1357.219089	123211.648909	35.784576
1358.231575	123384.864772	35.789594
1360.132923	123597.165680	35.794612
1361.739229	123760.359819	35.799629
1362.962774	123994.961827	35.804647
1364.345322	124166.236765	35.809664
1366.248574	124361.571270	35.814682
1367.523157	124517.679194	35.819700
1368.321868	124707.428753	35.824717
1369.687097	124883.384824	35.829735
1371.386330	125028.484673	35.834752
1372.283591	125256.436497	35.839770
1373.907631	125399.815017	35.844788
1375.094665	125589.078429	35.849805
1376.292716	125756.719570	35.854823
1377.253953	125947.820040	35.859840
1378.888511	126156.421639	35.864858
1380.210683	126322.311218	35.869876
1381.585883	126521.114719	35.874893
1382.452359	126721.583906	35.879911
1384.206298	126920.203468	35.884928
1384.678893	127127.160473	35.889946
1386.787513	127291.524925	35.894964
1387.745677	127543.110816	35.899981
1388.847595	127752.645370	35.904999
1390.893149	127937.798453	35.910016
1391.469546	128182.458386	35.915034
1393.696743	128357.945324	35.920052
1394.894448	128597.569780	35.925069
1396.587888	128797.783419	35.930087
1398.133693	129014.401805	35.935104
1399.425693	129217.671961	35.940122
1400.888147	129431.912584	35.945140
1402.769198	129632.064458	35.950157
1403.787199	129849.520702	35.955175
1405.517845	130040.590804	35.960192
1406.483361	130275.718693	35.965210
1408.391183	130468.245813	35.970228
1409.759674	130673.389455	35.975245
1411.107725	130880.438194	35.980263
1412.756398	131114.172353	35.985280
1413.781933	131299.928127	35.990298
1415.623267	131516.620401	35.995316
1416.920423	131727.230871	36.000333
1418.231338	131935.585576	36.005351
1419.781669	132134.642372	36.010368
1421.039393	132355.551443	36.015386
1422.667407	132540.332793	36.020404
1423.851968	132782.389863	36.025421
1425.791258	132958.610385	36.030439
1427.579445	133184.306860	36.035456
1428.213821	133411.392139	36.040474
1429.766032	133583.040805	36.045492
1431.325207	133824.020940	36.050509
1432.472597	134043.300876	36.055527
1434.003501	134234.317150	36.060544
1435.552628	134472.656231	36.065562
1436.871885	134683.551206	36.070580
1438.817016	134867.955167	36.075597
1439.845481	135131.343771	36.080615
1441.291747	135310.216663	36.085632
1442.697065	135497.916180	36.090650
1443.914492	135746.214566	36.095668
1445.590037	135938.701697	36.100685
1446.988315	136104.953969	36.105703
1448.251880	136295.798317	36.110720
1449.439625	136530.347066	36.115738
1450.968421	136756.467621	36.120756
1451.697561	136942.345187	36.125773
1453.240423	137123.672213	36.130791
1455.074181	137375.688089	36.135808
1456.069232	137577.874079	36.140826
1457.735713	137776.926170	36.145844
1459.194780	138027.752664	36.150861
1460.698425	138222.829272	36.155879
1462.019738	138460.147461	36.160896
1463.280815	138686.591561	36.165914
1465.223429	138908.278307	36.170932
1466.543880	139106.735397	36.175949
1467.672888	139373.605857	36.180967
1469.332324	139560.670087	36.185984
1470.918915	139814.178089	36.191002
1471.975019	140062.158417	36.196020
1473.822017	140266.077659	36.201037
1474.941132	140529.474950	36.206055
1477.229667	140725.824665	36.211072
1478.513513	140999.148401	36.216090
1480.101176	141228.931034	36.221108
1481.788300	141411.465346	36.226125
1483.450918	141681.325912	36.231143
1484.595093	141888.941808	36.236160
1485.964152	142121.224669	36.241178
1487.742913	142331.632404	36.246196
1489.852636	142609.148611	36.251213
1491.028712	142823.026798	36.256231
1492.550597	143028.866794	36.261248
1494.739931	143235.438635	36.266266
1495.864688	143507.948407	36.271284
1497.183481	143698.920091	36.276301
1498.728231	143943.939448	36.281319
1500.225904	144137.686523	36.286336
1501.963895	144385.416421	36.291354
1503.403815	144596.121715	36.296372
1504.616594	144850.605761	36.301389
1506.241000	145046.315698	36.306407
1507.829334	145310.959934	36.311424
1509.205593	145502.402626	36.316442
1510.916008	145774.154882	36.321460
1512.511255	145986.302600	36.326477
1513.840892	146209.445593	36.331495
1515.263903	146448.470541	36.336512
1516.979680	146643.478837	36.341530
1518.212506	146906.836780	36.346548
1519.777175	147127.679998	36.351565
1521.287950	147371.362744	36.356583
1523.223692	147586.940403	36.361600
1524.323693	147834.837055	36.366618
1525.491305	148016.238007	36.371636
1527.202954	148262.329537	36.376653
1528.605820	148457.170574	36.381671
1530.255092	148691.904604	36.386688
1531.656097	148902.011164	36.391706
1532.867072	149114.469126	36.396724
1534.533369	149358.193103	36.401741
1535.910885	149560.600248	36.406759
1537.405709	149805.229564	36.411776
1538.568184	150013.822039	36.416794
1540.316290	150281.791171	36.421812
1541.783716	150484.379994	36.426829
1543.286652	150717.453327	36.431847
1545.014862	150980.360486	36.436864
1546.712423	151229.025133	36.441882
1548.011060	151441.497161	36.446900
1549.173257	151715.732511	36.451917
1550.585205	151930.674547	36.456935
1552.275251	152206.960024	36.461952
1553.936119	152427.114413	36.466970
1555.419313	152715.126105	36.471988
1557.102621	152953.397416	36.477005
1558.943741	153189.921136	36.482023
1560.123214	153469.759472	36.487040
1562.036108	153696.132722	36.492058
1563.321757	153980.598808	36.497076
1564.711973	154235.547480	36.502093
1566.398282	154468.237907	36.507111
1568.158853	154763.817874	36.512128
1569.907575	155042.691463	36.517146
1571.291728	155278.440427	36.522164
1572.923093	155518.919127	36.527181
1574.659632	155769.881234	36.532199
1576.422193	156050.244434	36.537216
1578.111965	156331.242809	36.542234
1579.949393	156542.254408	36.547252
1581.620498	156841.695991	36.552269
1582.747529	157087.325096	36.557287
1584.987379	157315.306427	36.562304
1586.721203	157605.983002	36.567322
1587.718114	157844.930535	36.572340
1590.033234	158070.571813	36.577357
1591.437985	158370.309976	36.582375
1593.184361	158591.911264	36.587392
1594.508132	158836.519866	36.592410
1596.053165	159117.183631	36.597428
1597.836390	159346.899388	36.602445
1599.359402	159624.425965	36.607463
1600.957986	159852.563939	36.612480
1602.566075	160119.023332	36.617498
1603.637170	160366.662790	36.622516
1605.981113	160607.368205	36.627533
1607.333071	160890.080451	36.632551
1608.858342	161118.504590	36.637568
1610.899688	161367.797697	36.642586
1612.211550	161630.143418	36.647604
1613.958934	161828.367887	36.652621
1615.315652	162099.054330	36.657639
1617.360695	162284.019899	36.662656
1618.832360	162545.509989	36.667674
1619.842149	162785.224634	36.672692
1621.889408	163000.426929	36.677709
1623.129846	163255.871627	36.682727
1624.579558	163500.517850	36.687744
1625.614441	163741.350887	36.692762
1627.177208	164006.324691	36.697780
1628.555665	164249.275188	36.702797
1630.099558	164516.868263	36.707815
1631.882338	164782.763956	36.712832
1633.178179	165053.634392	36.717850
1634.726489	165333.851904	36.722868
1636.428471	165621.212908	36.727885
1638.216392	165873.887567	36.732903
1639.834655	166162.927542	36.737920
1641.562347	166441.831319	36.742938
1642.883783	166720.598784	36.747956
1645.530929	166971.229310	36.752973
1646.869515	167294.770167	36.757991
1648.216341	167569.887142	36.763008
1650.231081	167833.243901	36.768026
1651.625239	168115.460126	36.773044
1653.488856	168412.545317	36.778061
1655.085949	168683.140643	36.783079
1656.804506	168977.475553	36.788096
1658.758712	169259.598679	36.793114
1660.191475	169533.714258	36.798132
1662.156208	169818.579610	36.803149
1663.660591	170113.857876	36.808167
1665.493546	170396.921914	36.813184
1667.172775	170674.799132	36.818202
1668.812761	170959.458133	36.823220
1670.894728	171245.533141	36.828237
1672.788064	171532.794525	36.833255
1674.206104	171808.400037	36.838272
1675.889550	172091.246491	36.843290
1677.230878	172378.322689	36.848308
1679.262298	172653.139062	36.853325
1680.545019	172941.002466	36.858343
1682.342048	173243.551975	36.863360
1684.199682	173509.522203	36.868378
1685.471412	173832.113730	36.873396
1687.642396	174085.492110	36.878413
1689.491083	174389.957661	36.883431
1691.285346	174668.377633	36.888448
1693.125858	174948.098834	36.893466
1694.524232	175243.965258	36.898484
1696.665520	175527.080600	36.903501
1697.950237	175788.031774	36.908519
1699.741976	176109.556787	36.913536
1701.354660	176346.343004	36.918554
1703.102125	176643.838779	36.923572
1704.917087	176886.254122	36.928589
1706.475057	177137.807939	36.933607
1707.832995	177435.637722	36.938624
1709.654130	177664.469313	36.943642
1710.944506	177954.295579	36.948660
1712.882026	178228.340156	36.953677
1714.120334	178482.959690	36.958695
1715.658818	178784.081763	36.963712
1717.917341	179048.362498	36.968730
1719.442122	179344.885358	36.973748
1721.467959	179627.412803	36.978765
1723.153726	179891.662908	36.983783
1724.541372	180204.973578	36.988800
1726.161805	180462.805079	36.993818
1727.728780	180755.753234	36.998836
1729.804145	181076.383363	37.003853
1731.733342	181342.418154	37.008871
1734.255252	181597.766117	37.013888
1735.728164	181916.125540	37.018906
1737.427551	182188.596771	37.023924
1739.654101	182471.542521	37.028941
1741.619084	182780.402885	37.033959
1743.277259	183027.331876	37.038976
1744.777494	183336.739427	37.043994
1746.621152	183588.159184	37.049012
1748.610793	183882.799662	37.054029
1750.203304	184144.349842	37.059047
1751.876615	184454.790905	37.064064
1754.169249	184700.080506	37.069082
1755.528654	185010.219995	37.074100
1757.280192	185284.174001	37.079117
1759.447147	185563.646883	37.084135
1760.763346	185846.872963	37.089152
1762.802738	186141.596580	37.094170
1764.475506	186402.868041	37.099188
1766.224801	186703.389589	37.104205
1767.478493	186987.723993	37.109223
1768.939014	187279.590254	37.114240
1771.354924	187540.318796	37.119258
1772.789589	187881.986806	37.124276
1774.627736	188154.218540	37.129293
1776.511006	188481.023540	37.134311
1778.126151	188736.175544	37.139328
1779.918505	189067.364408	37.144346
1781.749562	189352.370377	37.149364
1783.938127	189637.029445	37.154381
1785.295815	189949.080691	37.159399
1787.107274	190244.666106	37.164416
1789.288551	190536.171804	37.169434
1790.700015	190845.682332	37.174452
1792.093702	191139.943675	37.179469
1794.030799	191445.224826	37.184487
1795.834156	191752.673869	37.189504
1797.626275	192052.359906	37.194522
1799.207266	192329.288572	37.199540
1801.169128	192631.375182	37.204557
1802.971350	192904.083991	37.209575
1804.819274	193165.948906	37.214592
1806.459759	193470.845668	37.219610
1808.153810	193728.765680	37.224628
1810.131908	194054.286403	37.229645
1812.334612	194302.178691	37.234663
1813.704381	194635.566887	37.239680
1815.314532	194879.824830	37.244698
1816.878414	195207.880974	37.249716
1818.875693	195500.841506	37.254733
1820.791039	195796.913521	37.259751
1822.522654	196079.575825	37.264768
1824.667978	196422.206540	37.269786
1826.343371	196688.927462	37.274804
1827.740950	197022.047704	37.279821
1830.270501	197298.066364	37.284839
1831.638018	197626.511894	37.289856
1833.943950	197924.767994	37.294874
1835.583171	198229.109713	37.299892
1837.088596	198540.594867	37.304909
1839.128920	198844.622636	37.309927
1840.738181	199173.356797	37.314944
1842.795226	199491.893207	37.319962
1844.569877	199798.037511	37.324980
1846.021162	200127.767283	37.329997
1848.494597	200435.365519	37.335015
1850.283710	200772.521700	37.340032
1852.298308	201099.730956	37.345050
1853.908901	201412.447359	37.350068
1855.929253	201727.309116	37.355085
1858.038912	202050.383709	37.360103
1859.892240	202371.216091	37.365120
1861.984546	202696.467771	37.370138
1863.833443	203017.279208	37.375156
1865.920196	203331.174852	37.380173
1867.736351	203644.543994	37.385191
1869.442229	203972.238126	37.390208
1871.526939	204285.035065	37.395226
1873.389225	204600.077749	37.400244
1875.438411	204916.488832	37.405261
1877.756003	205231.919709	37.410279
1879.666183	205539.153187	37.415296
1881.586289	205840.712475	37.420314
1883.463013	206159.595010	37.425332
1884.859133	206463.716047	37.430349
1886.840225	206801.601431	37.435367
1888.844100	207102.531910	37.440384
1890.636696	207413.005562	37.445402
1892.452401	207742.556959	37.450420
1894.723846	208045.163500	37.455437
1896.426124	208356.557706	37.460455
1898.033257	208690.996755	37.465472
1900.364299	208991.694392	37.470490
1901.917088	209286.778985	37.475508
1903.905970	209580.996015	37.480525
1905.890037	209865.782895	37.485543
1907.483856	210177.724113	37.490560
1909.087923	210460.504763	37.495578
1910.763533	210766.647021	37.500596
1912.564139	211058.044554	37.505613
1914.451137	211362.124950	37.510631
1916.078889	211686.217638	37.515648
1918.007620	212000.476101	37.520666
1919.636667	212338.841485	37.525684
1921.507681	212651.779293	37.530701
1923.438560	212966.029460	37.535719
1925.212618	213307.893589	37.540736
1927.123846	213641.447471	37.545754
1929.154152	213989.139905	37.550772
1930.941864	214322.259806	37.555789
1933.054511	214659.646415	37.560807
1934.308583	215003.430083	37.565824
1936.666934	215347.738554	37.570842
1938.704157	215699.501555	37.575860
1940.610959	216040.723904	37.580877
1942.574155	216394.127361	37.585895
1944.842093	216753.235688	37.590912
1946.943791	217092.680273	37.595930
1948.543144	217451.809460	37.600948
1950.561344	217808.474401	37.605965
1952.570897	218150.947826	37.610983
1954.601864	218514.483139	37.616000
1956.600425	218868.122075	37.621018
1958.773429	219220.440018	37.626036
1960.548440	219585.938607	37.631053
1962.636623	219927.024129	37.636071
1964.481031	220301.225335	37.641088
1966.735402	220659.784232	37.646106
1968.934133	221010.087947	37.651124
1971.109746	221366.885191	37.656141
1973.399957	221709.876868	37.661159
1975.466134	222075.328905	37.666176
1977.312786	222417.848209	37.671194
1979.439240	222762.330831	37.676212
1981.464355	223103.745622	37.681229
1983.183158	223513.294137	37.686247
1985.006777	223867.898813	37.691264
1987.357164	224224.580093	37.696282
1989.534507	224574.928948	37.701300
1991.416227	224924.970723	37.706317
1993.591855	225249.432296	37.711335
1995.521003	225620.357322	37.716352
1997.510250	225963.072641	37.721370
1999.711061	226320.434578	37.726388
2001.572806	226650.627506	37.731405
2003.674287	226996.313345	37.736423
2005.604508	227359.652668	37.741440
2007.513497	227693.029441	37.746458
2009.396913	228018.564140	37.751476
2011.432527	228352.329757	37.756493
2013.246237	228648.011790	37.761511
2015.336374	228986.952102	37.766528
2017.106512	229310.808104	37.771546
2019.264393	229638.006950	37.776564
2021.061380	229963.562685	37.781581
2023.202699	230301.661865	37.786599
2025.021872	230650.911942	37.791616
2026.934035	230970.637155	37.796634
2028.929664	231318.185607	37.801652
2030.749414	231661.725112	37.806669
2032.756383	232013.337972	37.811687
2034.828405	232353.512965	37.816704
2036.551412	232713.783276	37.821722
2038.497700	233072.902041	37.826740
2040.474677	233433.464969	37.831757
2042.694202	233797.292497	37.836775
2044.502386	234170.507718	37.841792
2046.802669	234537.118986	37.846810
2048.918952	234915.113798	37.851828
2050.652751	235276.153886	37.856845
2053.138248	235642.866846	37.861863
2055.394853	236017.440176	37.866880
2057.447277	236393.520389	37.871898
2060.181617	236742.977613	37.876916
2061.859887	237123.716992	37.881933
2064.105012	237481.102505	37.886951
2066.263783	237859.279228	37.891968
2068.261927	238219.601879	37.896986
2070.445256	238582.461660	37.902004
2072.088586	238959.758841	37.907021
2074.445427	239332.956440	37.912039
2076.684647	239696.547605	37.917056
2078.438620	240081.171440	37.922074
2080.897873	240454.940706	37.927092
2083.147940	240839.615395	37.932109
2084.901184	241204.964829	37.937127
2087.055752	241580.767230	37.942144
2089.173488	241965.771402	37.947162
2091.488608	242325.548794	37.952180
2093.331665	242715.551915	37.957197
2095.565123	243088.425505	37.962215
2097.663992	243475.494843	37.967232
2099.647916	243846.987877	37.972250
2101.872943	244217.884946	37.977268
2103.821765	244597.869429	37.982285
2106.366511	244977.328687	37.987303
2108.160170	245369.735437	37.992320
2110.496125	245737.723565	37.997338
2112.842839	246123.085035	38.002356
2114.729421	246513.016508	38.007373
2116.720074	246879.741648	38.012391
2118.703794	247261.379151	38.017408
2120.999714	247631.842553	38.022426
2123.335905	247998.617379	38.027444
2125.548506	248348.571836	38.032461
2127.379486	248707.300235	38.037479
2129.545755	249054.748996	38.042496
2131.048977	249401.033662	38.047514
2133.154241	249763.836056	38.052532
2135.041006	250107.318131	38.057549
2137.257101	250487.174324	38.062567
2139.275113	250860.966486	38.067584
2140.920479	251232.354667	38.072602
2143.220480	251611.615948	38.077620
2145.218722	251989.376450	38.082637
2147.537357	252371.659279	38.087655
2149.579126	252778.829775	38.092672
2151.734530	253160.174958	38.097690
2154.014097	253549.553650	38.102708
2155.894628	253945.956589	38.107725
2158.103299	254353.231177	38.112743
2160.331212	254741.375873	38.117760
2162.412797	255131.525923	38.122778
2164.743654	255548.106226	38.127796
2166.897205	255950.744324	38.132813
2169.176369	256361.110974	38.137831
2171.738541	256754.922073	38.142848
2173.717382	257172.171150	38.147866
2176.339502	257556.245127	38.152884
2178.427497	257977.593610	38.157901
2180.354569	258370.720865	38.162919
2182.849111	258777.704761	38.167936
2184.892103	259192.076903	38.172954
2187.243301	259593.470956	38.177972
2189.840064	260013.929487	38.182989
2191.891371	260416.515530	38.188007
2194.361735	260815.047508	38.193024
2196.203706	261222.316666	38.198042
2198.874618	261627.879992	38.203060
2200.874481	262024.583124	38.208077
2203.110459	262436.008405	38.213095
2205.521136	262838.769563	38.218112
2207.662340	263245.079581	38.223130
2210.119186	263647.783648	38.228148
2212.044306	264062.740553	38.233165
2214.329303	264473.093753	38.238183
2216.530314	264874.366461	38.243200
2218.711011	265292.154820	38.248218
2221.262057	265684.532624	38.253236
2223.367675	266108.455911	38.258253
2225.381140	266510.115692	38.263271
2227.853317	266925.039769	38.268288
2229.662863	267333.058025	38.273306
2232.151709	267742.797946	38.278324
2234.447533	268154.169219	38.283341
2236.562349	268567.017505	38.288359
2238.970577	268970.801415	38.293376
2240.944737	269379.481060	38.298394
2243.172777	269774.834793	38.303412
2245.250632	270154.843574	38.308429
2247.612052	270545.095946	38.313447
2249.647841	270925.416643	38.318464
2251.755222	271321.298422	38.323482
2253.938574	271713.027586	38.328500
2255.967204	272113.088346	38.333517
2258.313695	272509.466175	38.338535
2260.546069	272914.956646	38.343552
2262.800210	273298.749290	38.348570
2265.194117	273695.145362	38.353588
2267.411836	274113.695825	38.358605
2269.598279	274518.635100	38.363623
2272.064921	274923.428394	38.368640
2274.060967	275335.333093	38.373658
2276.615988	275757.158137	38.378676
2278.874699	276168.767193	38.383693
2281.087695	276566.208384	38.388711
2283.544115	276986.855082	38.393728
2285.283424	277413.534430	38.398746
2287.953134	277832.089530	38.403764
2290.120467	278269.065458	38.408781
2292.055857	278700.438500	38.413799
2294.783518	279122.413571	38.418816
2296.790925	279570.058496	38.423834
2298.949602	280004.825159	38.428852
2301.473013	280452.311697	38.433869
2303.463068	280890.280113	38.438887
2306.264414	281334.394298	38.443904
2308.402554	281774.371017	38.448922
2310.963663	282206.811836	38.453940
2313.389108	282656.649721	38.458957
2315.964392	283098.944156	38.463975
2318.438624	283528.628863	38.468992
2320.517771	283978.546018	38.474010
2322.783253	284419.846958	38.479028
2325.173400	284866.818041	38.484045
2327.348935	285311.765060	38.489063
2329.917414	285750.501777	38.494080
2332.118999	286220.948449	38.499098
2334.469101	286654.079331	38.504116
2336.965390	287108.296466	38.509133
2339.046752	287555.999441	38.514151
2341.767842	288014.523709	38.519168
2344.415359	288459.925707	38.524186
2346.504095	288905.390278	38.529204
2348.966426	289356.586848	38.534221
2350.903475	289812.540141	38.539239
2353.784600	290248.478098	38.544256
2355.867804	290711.316369	38.549274
2358.567474	291154.877108	38.554292
2361.047241	291605.610122	38.559309
2363.270662	292049.498887	38.564327
2365.979005	292492.649543	38.569344
2368.283470	292934.237665	38.574362
2370.333471	293359.861756	38.579380
2372.482914	293769.567393	38.584397
2374.523530	294192.066949	38.589415
2377.182013	294599.531196	38.594432
2378.990341	295034.233686	38.599450
2381.469471	295456.661295	38.604468
2383.910632	295886.181281	38.609485
2386.088177	296329.154476	38.614503
2388.340164	296752.326681	38.619520
2390.793297	297196.981600	38.624538
2392.986621	297635.580203	38.629556
2395.856876	298075.823221	38.634573
2397.984263	298535.259715	38.639591
2400.900050	298960.963539	38.644608
2402.861683	299421.567115	38.649626
2405.443220	299860.505227	38.654644
2407.827698	300309.303855	38.659661
2409.865409	300777.080365	38.664679
2412.824601	301231.653159	38.669696
2414.839221	301689.016128	38.674714
2417.295943	302147.171353	38.679732
2419.575213	302619.755843	38.684749
2421.926210	303086.663055	38.689767
2424.775248	303548.892296	38.694784
2426.919804	304035.540474	38.699802
2429.525711	304501.996407	38.704820
2432.184329	304963.540113	38.709837
2434.649901	305443.782427	38.714855
2437.159086	305903.568662	38.719872
2439.967081	306386.115674	38.724890
2442.242993	306847.002498	38.729908
2444.550847	307326.323314	38.734925
2446.802912	307804.762198	38.739943
2449.480586	308272.971779	38.744960
2451.939516	308756.352737	38.749978
2454.297535	309241.703610	38.754996
2457.146678	309724.307743	38.760013
2459.312935	310209.583552	38.765031
2461.947521	310692.344799	38.770048
2464.106689	311170.404290	38.775066
2466.905648	311658.266207	38.780084
2469.212344	312139.473229	38.785101
2472.042592	312631.288308	38.790119
2474.631146	313114.961002	38.795136
2476.419900	313607.292380	38.800154
2479.379053	314096.286587	38.805172
2482.227181	314582.603885	38.810189
2484.342978	315073.911542	38.815207
2486.875861	315561.214018	38.820224
2489.339574	316049.795075	38.825242
2491.936651	316530.504581	38.830260
2494.682517	317023.049161	38.835277
2496.668584	317507.787512	38.840295
2499.554921	317992.406211	38.845312
2501.950722	318481.925805	38.850330
2504.270839	318940.749118	38.855348
2506.530296	319385.433393	38.860365
2509.189146	319857.405307	38.865383
2511.303368	320319.403797	38.870400
2513.778372	320782.307893	38.875418
2516.273519	321240.990537	38.880436
2518.796422	321703.272811	38.885453
2520.943221	322190.475725	38.890471
2523.620848	322660.093564	38.895488
2525.999488	323148.905210	38.900506
2528.494849	323623.270475	38.905524
2531.062137	324114.230835	38.910541
2533.252101	324606.314772	38.915559
2535.638303	325096.460039	38.920576
2538.353079	325592.721521	38.925594
2541.017411	326078.093289	38.930612
2543.647881	326584.266402	38.935629
2545.648284	327101.049814	38.940647
2548.609610	327606.884706	38.945664
2551.390979	328115.106604	38.950682
2553.918486	328620.902129	38.955700
2556.848222	329120.586705	38.960717
2559.340450	329628.184234	38.965735
2561.862912	330136.890935	38.970752
2564.117191	330650.461572	38.975770
2567.297773	331165.786462	38.980788
2570.047871	331677.722412	38.985805
2572.626387	332191.789636	38.990823
2575.415761	332699.369889	38.995840
2578.092926	333217.172412	39.000858
2580.577202	333731.268956	39.005876
2583.586693	334234.791304	39.010893
2585.955679	334743.236111	39.015911
2588.495659	335254.392493	39.020928
2591.021076	335769.584760	39.025946
2593.537718	336285.663250	39.030964
2596.768461	336799.898024	39.035981
2599.025499	337322.205324	39.040999
2601.550459	337815.951412	39.046016
2604.440013	338335.839887	39.051034
2607.104360	338852.839929	39.056052
2609.796184	339368.282653	39.061069
2612.392076	339889.855606	39.066087
2615.150134	340404.467001	39.071104
2617.851061	340921.393779	39.076122
2620.112680	341431.149722	39.081140
2623.038325	341943.284513	39.086157
2625.591315	342460.958262	39.091175
2628.601506	342964.540242	39.096192
2631.180286	343484.562454	39.101210
2633.522523	344010.660244	39.106228
2636.403627	344522.678835	39.111245
2638.955861	345030.073615	39.116263
2641.402490	345549.464069	39.121280
2644.336230	346050.137872	39.126298
2646.665321	346539.072376	39.131316
2649.782975	347010.004887	39.136333
2651.955575	347488.115569	39.141351
2654.587633	347969.449812	39.146368
2657.447917	348446.301077	39.151386
2659.506312	348933.303123	39.156404
2661.954701	349426.941224	39.161421
2664.752366	349912.065939	39.166439
2667.124187	350410.632352	39.171456
2669.621317	350911.916062	39.176474
2671.798625	351427.842589	39.181492
2674.403584	351936.537756	39.186509
2676.572666	352463.193715	39.191527
2679.329117	352982.542110	39.196544
2682.216194	353512.221683	39.201562
2685.006422	354058.106535	39.206580
2687.577003	354591.836063	39.211597
2690.525690	355131.617735	39.216615
2692.947499	355686.529700	39.221632
2695.562440	356218.331571	39.226650
2698.179808	356783.430120	39.231668
2701.192433	357324.269916	39.236685
2703.404664	357891.983836	39.241703
2705.962899	358441.919671	39.246720
2709.021467	359012.862558	39.251738
2712.130051	359587.547368	39.256756
2714.604835	360147.300013	39.261773
2717.203410	360720.275500	39.266791
2720.138924	361284.282150	39.271808
2723.073446	361854.906600	39.276826
2725.535859	362435.014992	39.281844
2728.652692	362995.368607	39.286861
2731.361195	363589.864898	39.291879
2734.099501	364154.934367	39.296896
2737.131961	364729.035991	39.301914
2739.558296	365317.996755	39.306932
2742.506047	365893.086952	39.311949
2745.338124	366475.953814	39.316967
2748.236392	367048.067923	39.321984
2751.340186	367621.588673	39.327002
2753.830170	368199.005767	39.332020
2756.889159	368772.467963	39.337037
2759.446422	369351.331137	39.342055
2762.455451	369928.161144	39.347072
2765.577511	370505.853724	39.352090
2768.458960	371081.698890	39.357108
2771.697155	371638.169503	39.362125
2774.276643	372207.627443	39.367143
2776.846869	372783.701868	39.372160
2780.052961	373332.238524	39.377178
2782.704276	373900.748716	39.382196
2785.739947	374462.517118	39.387213
2788.923254	375030.927578	39.392231
2791.023139	375597.573417	39.397248
2793.991055	376142.837444	39.402266
2796.608356	376671.404252	39.407284
2799.134556	377209.213809	39.412301
2802.118880	377728.676385	39.417319
2804.392520	378243.906327	39.422336
2807.402706	378778.193098	39.427354
2809.701266	379316.517713	39.432372
2812.472735	379863.563423	39.437389
2815.271340	380397.126012	39.442407
2818.028876	380946.086858	39.447424
2820.789312	381488.874865	39.452442
2823.403397	382057.021434	39.457460
2826.000835	382612.934843	39.462477
2828.702366	383172.045367	39.467495
2831.389359	383746.395688	39.472512
2834.210250	384323.227395	39.477530
2836.830750	384910.279296	39.482548
2839.910509	385496.868771	39.487565
2842.548916	386082.022286	39.492583
2845.215380	386669.191317	39.497600
2848.298536	387263.488622	39.502618
2851.101876	387860.027274	39.507636
2853.718979	388474.720903	39.512653
2856.950480	389067.418037	39.517671
2859.760130	389679.752561	39.522688
2862.898242	390277.745386	39.527706
2865.499084	390896.204517	39.532724
2868.663137	391505.205155	39.537741
2871.583004	392116.237470	39.542759
2874.286581	392725.822429	39.547776
2877.438022	393336.137361	39.552794
2880.362292	393957.737384	39.557812
2883.459404	394575.494896	39.562829
2886.240961	395203.206665	39.567847
2889.232731	395817.408140	39.572864
2892.344173	396422.577377	39.577882
2894.888221	397052.980507	39.582900
2897.767840	397685.930486	39.587917
2901.189197	398305.242179	39.592935
2903.894243	398926.811011	39.597952
2907.144235	399546.811259	39.602970
2910.007923	400179.944353	39.607988
2913.238076	400800.202970	39.613005
2916.339225	401417.554437	39.618023
2919.382390	402040.227647	39.623040
2922.684232	402646.190673	39.628058
2925.133303	403274.993496	39.633076
2928.059533	403879.801035	39.638093
2931.314436	404487.739391	39.643111
2934.242419	405088.872900	39.648128
2937.271017	405739.337403	39.653146
2940.169461	406317.813626	39.658164
2943.030798	406962.017577	39.663181
2946.401537	407552.285223	39.668199
2949.090773	408166.857757	39.673216
2952.153079	408773.729059	39.678234
2954.877810	409331.593345	39.683252
2957.779822	409939.151249	39.688269
2960.842757	410476.510880	39.693287
2963.404302	411050.160613	39.698304
2966.119986	411629.021655	39.703322
2968.939043	412204.205378	39.708340
2971.900897	412813.089754	39.713357
2974.702099	413372.311647	39.718375
2976.919603	413991.579522	39.723392
2980.406529	414585.822110	39.728410
2982.595171	415181.956100	39.733428
2985.776121	415810.257934	39.738445
2988.938331	416408.189448	39.743463
2991.420311	417034.421291	39.748480
2994.524347	417677.494117	39.753498
2997.698376	418292.337660	39.758516
3000.649393	418920.633326	39.763533
3003.656783	419568.898802	39.768551
3006.130505	420205.628784	39.773568
3009.676068	420860.215425	39.778586
3012.609647	421487.823222	39.783604
3015.335385	422166.630263	39.788621
3018.833687	422799.870565	39.793639
3021.395507	423478.468715	39.798656
3024.873115	424130.176755	39.803674
3027.554156	424779.385894	39.808692
3030.699513	425469.116213	39.813709
3033.908144	426132.675166	39.818727
3036.780247	426796.701731	39.823744
3040.113579	427470.265052	39.828762
3043.051499	428165.177599	39.833780
3046.345406	428807.859948	39.838797
3049.761600	429510.488836	39.843815
3052.699433	430168.924403	39.848832
3055.513139	430832.504860	39.853850
3058.978209	431528.562632	39.858868
3062.198047	432197.641653	39.863885
3065.298176	432872.699476	39.868903
3068.426917	433565.969894	39.873920
3071.180152	434242.768914	39.878938
3074.852255	434904.209841	39.883956
3077.409051	435608.658356	39.888973
3081.398565	436261.580885	39.893991
3083.601563	436975.644941	39.899008
3086.735423	437633.073505	39.904026
3090.201462	438318.412317	39.909044
3092.975983	438998.245875	39.914061
3096.095210	439704.566875	39.919079
3099.427248	440362.601008	39.924096
3103.008509	441065.189353	39.929114
3106.128826	441743.930537	39.934132
3109.168265	442426.817670	39.939149
3111.923286	443126.236907	39.944167
3115.046381	443794.236980	39.949184
3118.203869	444494.920014	39.954202
3121.645111	445112.000819	39.959220
3124.539112	445787.576031	39.964237
3127.510499	446389.915058	39.969255
3130.283430	447077.926756	39.974272
3133.442141	447687.695587	39.979290
3136.533673	448341.044543	39.984308
3138.982005	449025.051677	39.989325
3142.323601	449650.382246	39.994343
3145.112674	450347.103311	39.999360
3148.382304	451002.070637	40.004378
3151.432818	451667.986789	40.009396
3154.408231	452381.319844	40.014413
3157.258384	453034.878573	40.019431
3160.186347	453761.993036	40.024448
3163.566440	454434.052233	40.029466
3166.799414	455134.049704	40.034484
3169.093638	455868.737264	40.039501
3172.757224	456557.742314	40.044519
3175.727744	457299.411171	40.049536
3178.831524	458030.661264	40.054554
3181.534688	458756.637822	40.059572
3184.893603	459501.258266	40.064589
3188.109151	460247.394083	40.069607
3191.309813	460977.317006	40.074624
3194.559808	461765.034011	40.079642
3197.908127	462504.950181	40.084660
3200.982352	463253.029138	40.089677
3204.447038	464037.189631	40.094695
3207.597468	464781.156572	40.099712
3210.902260	465564.376016	40.104730
3214.247918	466312.811185	40.109748
3217.576570	467085.905253	40.114765
3221.124344	467866.067785	40.119783
3223.820244	468617.154185	40.124800
3227.461457	469399.773777	40.129818
3230.791656	470170.478341	40.134836
3234.017332	470947.795522	40.139853
3237.147760	471713.265735	40.144871
3240.423839	472509.276910	40.149888
3243.972603	473267.038324	40.154906
3246.961266	474062.529040	40.159924
3250.981535	474846.348425	40.164941
3253.895873	475602.808799	40.169959
3257.356011	476403.189083	40.174976
3260.485250	477178.969983	40.179994
3264.237397	477917.061972	40.185012
3267.128334	478732.099575	40.190029
3270.895297	479527.807470	40.195047
3273.873742	480304.703809	40.200064
3277.436718	481063.837166	40.205082
3280.878884	481829.733022	40.210100
3284.032617	482585.081608	40.215117
3287.909927	483337.506931	40.220135
3291.015250	484133.840380	40.225152
3293.970647	484925.111380	40.230170
3297.439487	485648.201613	40.235188
3300.157089	486359.155052	40.240205
3303.545621	487039.658759	40.245223
3307.053633	487771.656820	40.250240
3309.839479	488490.099190	40.255258
3312.708789	489241.088503	40.260276
3315.733724	490012.029665	40.265293
3318.929548	490761.593286	40.270311
3321.861879	491506.015911	40.275328
3324.546146	492252.670781	40.280346
3328.690721	492991.639437	40.285364
3331.566262	493804.272478	40.290381
3334.629298	494618.759495	40.295399
3337.616258	495399.130835	40.300416
3340.468864	496186.560828	40.305434
3343.807062	496974.637676	40.310452
3347.474677	497781.414253	40.315469
3351.249566	498574.099721	40.320487
3354.408962	499426.230105	40.325504
3357.500102	500282.016956	40.330522
3360.889381	501102.776552	40.335540
3364.125886	501933.367800	40.340557
3367.646746	502774.982210	40.345575
3370.995104	503604.165092	40.350592
3374.710988	504445.315912	40.355610
3378.203133	505287.572454	40.360628
3381.273960	506120.466628	40.365645
3385.147939	506933.105612	40.370663
3388.187843	507799.943753	40.375680
3390.902860	508685.311948	40.380698
3395.143886	509546.270756	40.385716
3398.273892	510419.675253	40.390733
3401.905952	511245.875754	40.395751
3405.463750	512147.685413	40.400768
3408.985980	512990.419569	40.405786
3412.707158	513848.670492	40.410804
3415.947046	514733.591907	40.415821
3419.139342	515611.562933	40.420839
3423.001622	516507.340645	40.425856
3426.333305	517399.471871	40.430874
3430.054664	518259.565117	40.435892
3433.122235	519138.530249	40.440909
3436.926341	519969.772162	40.445927
3440.562373	520833.930923	40.450944
3443.684822	521721.978485	40.455962
3447.255963	522604.309480	40.460980
3450.962524	523507.345916	40.465997
3454.507994	524357.869024	40.471015
3458.205596	525214.474380	40.476032
3460.991921	526111.410070	40.481050
3464.868790	526986.596868	40.486068
3467.959824	527872.345284	40.491085
3471.736754	528751.534268	40.496103
3475.091187	529628.372288	40.501120
3478.847685	530470.037577	40.506125
3482.509674	531269.696343	40.511130
3485.781910	532039.009974	40.516135
3489.713548	532740.025390	40.521140
3492.626908	533371.147548	40.526144
3494.924305	533947.578243	40.531149
3497.770070	534452.418020	40.536154
3500.178005	534908.814743	40.541159
3502.562933	535294.834006	40.546164
3504.821702	535670.912291	40.551168
3506.662938	535952.588130	40.556173
3508.371976	536186.141501	40.561178
3509.918331	536424.061034	40.566183
3511.762253	536528.984848	40.571188
3513.131482	536671.462006	40.576192
3513.761898	536737.682843	40.581197
3515.682681	536735.055755	40.586202
3516.479231	536740.031403	40.591207
3517.820818	536704.360901	40.596212
3518.585110	536663.629458	40.601216
3518.980827	536609.974846	40.606221
3519.493827	536479.524379	40.611226
3520.408021	536329.612847	40.616231
3520.768796	536205.296055	40.621236
3521.301219	536009.475493	40.626240
3521.108289	535865.139310	40.631245
3521.664738	535675.170263	40.636250
3521.888172	535473.885713	40.641255
3521.345697	535232.913448	40.646260
3521.678880	535015.440624	40.651264
3522.276496	534747.961664	40.656269
3522.549140	534510.587592	40.661274
3522.341708	534277.226213	40.666279
3522.210622	534029.097604	40.671284
3522.521227	533784.027478	40.676288
3522.112033	533559.326159	40.681293
3522.026973	533300.114563	40.686298
3521.506683	533010.401239	40.691303
3522.063086	532729.050859	40.696308
3521.526663	532499.099915	40.701312
3520.670932	532214.376227	40.706317
3521.083829	531930.356324	40.711322
3520.757978	531710.566801	40.716327
3520.125278	531451.815335	40.721332
3520.386412	531165.026541	40.726336
3520.178859	530913.576199	40.731341
3520.063021	530646.139770	40.736346
3519.777929	530413.794150	40.741351
3519.490668	530205.549104	40.746356
3519.488101	529951.271765	40.751360
3518.980220	529685.043256	40.756365
3519.253272	529404.789914	40.761370
3518.487404	529194.585822	40.766375
3518.200945	528983.241920	40.771380
3518.321593	528727.055627	40.776384
3517.480605	528494.466463	40.781389
3517.802698	528249.005042	40.786394
3517.711975	528009.113804	40.791399
3517.406652	527809.330639	40.796404
3517.177600	527630.203760	40.801408
3516.611146	527411.757097	40.806413
3516.432164	527192.083754	40.811418
3516.326066	526983.060233	40.816423
3516.173635	526772.979907	40.821428
3515.841886	526547.661080	40.826432
3515.936150	526321.361959	40.831437
3515.675653	526122.409875	40.836442
3515.354320	525950.051757	40.841447
3515.629936	525740.951708	40.846452
3515.221903	525561.223419	40.851456
3514.678713	525392.685372	40.856461
3514.641738	525191.816202	40.861466
3513.822763	525012.955503	40.866471
3513.720484	524818.966558	40.871476
3513.845578	524647.484360	40.876480
3513.495140	524527.434079	40.881485
3513.283455	524337.146766	40.886490
3513.073265	524164.145373	40.891495
3512.631174	523996.941638	40.896500
3513.023202	523835.316703	40.901504
3512.369369	523715.257794	40.906509
3511.955810	523544.556775	40.911514
3511.981608	523402.448214	40.916519
3512.793770	523241.155384	40.921524
3512.807427	523090.957422	40.926528
3511.891886	522937.366109	40.931533
3511.765318	522815.498349	40.936538
3511.702453	522715.661754	40.941543
3511.650751	522563.598705	40.946548
3510.782786	522412.977713	40.951552
3511.021257	522267.084456	40.956557
3511.028011	522175.272066	40.961562
3510.255357	522056.180264	40.966567
3509.626416	521930.593483	40.971572
3510.590255	521797.372495	40.976576
3510.300205	521729.619636	40.981581
3510.144005	521623.016279	40.986586
3509.222652	521492.770385	40.991591
3510.295684	521353.006394	40.996596
3510.052534	521298.693175	41.001600
3509.550053	521192.748463	41.006605
3509.812528	521064.081651	41.011610
3509.249050	520957.234967	41.016615
3509.051892	520877.379864	41.021620
3509.166356	520795.149300	41.026624
3508.949290	520691.229247	41.031629
3508.631076	520581.661586	41.036634
3508.996792	520475.018832	41.041639
3508.993236	520369.192191	41.046644
3508.797098	520288.423936	41.051648
3508.672783	520219.273440	41.056653
3508.990350	520168.558959	41.061658
3508.566067	520081.606471	41.066663
3508.015077	519991.791416	41.071668
3507.659867	519909.276710	41.076672
3507.671426	519839.192989	41.081677
3507.498340	519755.030669	41.086682
3507.257501	519687.767243	41.091687
3507.971813	519609.733945	41.096692
3508.182955	519551.904731	41.101696
3507.517712	519514.136543	41.106701
3507.654579	519416.877675	41.111706
3507.046347	519345.069457	41.116711
3507.004473	519280.908001	41.121716
3507.731671	519191.543917	41.126720
3507.246522	519183.580544	41.131725
3506.817888	519086.206844	41.136730
3507.450948	519011.470389	41.141735
3507.380148	518941.952111	41.146740
3507.135517	518926.466684	41.151744
3506.791411	518890.820691	41.156749
3506.881168	518791.795742	41.161754
3506.981276	518736.357895	41.166759
3506.550608	518684.948041	41.171764
3507.064630	518610.228591	41.176768
3507.110235	518552.877161	41.181773
3506.940371	518528.782953	41.186778
3506.757510	518460.696277	41.191783
3506.432569	518393.491445	41.196788
3507.204783	518314.734932	41.201792
3506.830929	518278.131512	41.206797
3506.869874	518262.398366	41.211802
3506.581197	518203.935476	41.216807
3505.883350	518137.395376	41.221812
3506.421653	518057.410378	41.226816
3506.233830	518061.789032	41.231821
3506.058086	518000.576814	41.236826
3506.363569	517936.001257	41.241831
3506.359053	517865.052025	41.246836
3506.411454	517816.951333	41.251840
3506.082164	517794.802932	41.256845
3506.274752	517772.015740	41.261850
3506.281168	517745.667428	41.266855
3505.840309	517688.895608	41.271860
3505.673094	517665.204294	41.276864
3505.602430	517607.463408	41.281869
3505.239049	517554.370568	41.286874
3504.922357	517527.010984	41.291879
3505.498286	517475.134852	41.296884
3505.224565	517466.530372	41.301888
3504.965069	517463.486503	41.306893
3505.434174	517396.910704	41.311898
3505.138902	517413.393138	41.316903
3505.158833	517369.089155	41.321908
3505.497263	517313.861751	41.326912
3505.358571	517328.296642	41.331917
3505.515682	517285.487912	41.336922
3504.956871	517250.428620	41.341927
3505.298627	517197.728912	41.346932
3505.536164	517215.290490	41.351936
3505.207532	517199.715580	41.356941
3505.258055	517170.223905	41.361946
3505.455598	517131.100170	41.366951
3505.184560	517101.406335	41.371956
3505.206847	517062.360711	41.376960
3505.083895	517013.223386	41.381965
3505.386191	516962.299221	41.386970
3505.420686	516950.156220	41.391975
3505.157979	516916.667761	41.396980
3505.749412	516882.285634	41.401984
3505.288694	516856.869495	41.406989
3505.390513	516844.867496	41.411994
3505.255475	516835.482169	41.416999
3505.180526	516802.520111	41.422004
3505.405792	516790.751429	41.427008
3504.729515	516774.775908	41.432013
3504.957020	516699.081695	41.437018
3505.375209	516694.514504	41.442023
3504.686695	516689.515349	41.447028
3504.762171	516641.761634	41.452032
3505.062335	516591.544711	41.457037
3505.038128	516580.068183	41.462042
3504.927921	516604.310582	41.467047
3504.823853	516582.681284	41.472052
3504.767812	516543.141085	41.477056
3504.397830	516517.710087	41.482061
3504.710318	516493.587266	41.487066
3505.145981	516453.716266	41.492071
3504.438727	516436.126929	41.497076
3504.618453	516437.868609	41.502080
3504.755669	516453.575586	41.507085
3504.682870	516429.968741	41.512090
3504.660219	516403.521754	41.517095
3504.533169	516386.447556	41.522100
3504.818319	516335.018443	41.527104
3504.662808	516342.780956	41.532109
3504.501447	516344.273107	41.537114
3504.476122	516314.943634	41.542119
3504.317372	516269.602901	41.547124
3504.494557	516296.632526	41.552128
3504.395701	516294.220526	41.557133
3504.579661	516282.609741	41.562138
3504.594016	516277.651091	41.567143
3504.579147	516247.611797	41.572148
3504.509450	516220.565054	41.577152
3504.361632	516179.470669	41.582157
3505.157245	516147.836407	41.587162
3504.897032	516127.596738	41.592167
3504.885192	516107.469513	41.597172
3504.714621	516073.105015	41.602176
3504.729743	516066.982940	41.607181
3504.742660	516046.548275	41.612186
3504.229127	516057.654933	41.617191
3503.973407	516039.437476	41.622196
3504.314948	516013.539219	41.627200
3503.787280	516054.892456	41.632205
3504.396063	516044.023571	41.637210
3504.424332	516021.765721	41.642215
3504.389088	516000.529399	41.647220
3504.072017	515983.838856	41.652224
3503.967808	515967.468683	41.657229
3504.298197	515959.728883	41.662234
3504.546680	515970.158820	41.667239
3504.438024	515964.309152	41.672244
3504.747929	515951.666711	41.677248
3504.391099	515946.665480	41.682253
3504.502000	515919.640283	41.687258
3504.356881	515916.072288	41.692263
3504.126634	515897.092007	41.697268
3503.866283	515861.932046	41.702272
3504.482668	515835.130274	41.707277
3504.357066	515847.389589	41.712282
3504.139146	515843.782509	41.717287
3504.049130	515822.301736	41.722292
3504.817810	515787.333008	41.727296
3504.172394	515777.572565	41.732301
3504.320469	515761.061162	41.737306
3504.704530	515783.608174	41.742311
3504.103804	515779.909856	41.747316
3504.179734	515749.754164	41.752320
3504.267783	515720.152847	41.757325
3504.521618	515706.709857	41.762330
3504.531978	515729.872351	41.767335
3503.861561	515718.901985	41.772340
3504.136841	515693.772359	41.777344
3503.991478	515696.880497	41.782349
3504.034484	515682.560427	41.787354
3504.572844	515672.461088	41.792359
3504.675785	515637.951312	41.797364
3504.142765	515673.540554	41.802368
3504.176383	515658.311564	41.807373
3504.432597	515636.219481	41.812378
3504.228260	515633.470018	41.817383
3504.134763	515593.933498	41.822388
3504.449777	515572.287232	41.827392
3504.796514	515555.541919	41.832397
3504.311508	515524.058319	41.837402
3504.456316	515538.348789	41.842407
3503.959362	515561.541124	41.847412
3504.161278	515506.329333	41.852416
3504.298805	515485.621401	41.857421
3504.437823	515526.971718	41.862426
3504.302250	515519.659406	41.867431
3504.065685	515496.380593	41.872436
3504.291679	515467.111069	41.877440
3504.072993	515444.486866	41.882445
3504.316861	515465.690869	41.887450
3504.484289	515473.453319	41.892455
3504.404253	515447.570245	41.897460
3504.281553	515428.319546	41.902464
3504.610692	515431.302157	41.907469
3504.626455	515354.219162	41.912474
3504.625925	515340.917240	41.917479
3504.401060	515309.999055	41.922484
3504.234664	515316.600469	41.927488
3504.332633	515316.736693	41.932493
3504.026423	515316.380444	41.937498
3504.081937	515308.329746	41.942503
3503.853270	515338.662056	41.947508
3504.395408	515281.220901	41.952512
3504.226838	515255.806728	41.957517
3504.779144	515239.079186	41.962522
3504.277083	515230.914267	41.967527
3504.132468	515215.864781	41.972532
3504.699299	515204.243315	41.977536
3504.183613	515200.329111	41.982541
3504.271424	515173.609833	41.987546
3503.829711	515195.074275	41.992551
3504.258981	515210.281052	41.997556
3504.246870	515202.544461	42.002560
3504.085298	515183.552518	42.007565
3503.760237	515167.621099	42.012570
3504.099201	515158.868008	42.017575
3504.133246	515127.857987	42.022580
3504.322892	515120.241205	42.027584
3504.058630	515104.249537	42.032589
3504.550667	515098.759831	42.037594
3504.021567	515101.928730	42.042599
3504.392160	515075.518651	42.047604
3504.553247	515063.253116	42.052608
3504.084597	515056.802508	42.057613
3504.358366	515086.297178	42.062618
3503.947802	515070.025130	42.067623
3504.065379	515034.146176	42.072628
3504.255294	515053.234917	42.077632
3504.041463	515053.521584	42.082637
3503.949843	515016.815819	42.087642
3504.417168	514976.885732	42.092647
3504.367201	514968.497490	42.097652
3504.375033	514999.905769	42.102656
3504.114442	515006.724507	42.107661
3504.154540	514970.958822	42.112666
3504.285945	514967.094023	42.117671
3504.095588	514967.124086	42.122676
3504.113330	514948.204692	42.127680
3504.104540	514954.983653	42.132685
3504.179169	514936.257570	42.137690
3503.903109	514907.875693	42.142695
3504.127010	514884.927886	42.147700
3504.292673	514873.925972	42.152704
3504.121841	514913.101283	42.157709
3503.774206	514868.949940	42.162714
3504.281786	514847.474624	42.167719
3504.524786	514841.619561	42.172724
3504.490547	514873.085306	42.177728
3504.098371	514861.109389	42.182733
3504.007668	514861.477756	42.187738
3504.412367	514847.706759	42.192743
3504.144706	514823.622659	42.197748
3504.068108	514803.251209	42.202752
3503.559423	514786.842657	42.207757
3504.414185	514751.959334	42.212762
3504.248350	514780.411271	42.217767
3503.822901	514793.629179	42.222772
3504.032370	514788.133454	42.227776
3503.852252	514788.414797	42.232781
3503.826083	514747.752894	42.237786
3504.486341	514716.896036	42.242791
3503.974951	514750.612357	42.247796
3504.415752	514740.780781	42.252800
3503.955886	514710.303274	42.257805
3504.570052	514667.314457	42.262810
3504.559081	514664.787170	42.267815
3504.131299	514669.558693	42.272820
3504.329827	514694.513749	42.277824
3504.196296	514681.586386	42.282829
3504.361324	514662.087013	42.287834
3503.839870	514636.019560	42.292839
3504.159410	514615.079470	42.297844
3504.261667	514637.723144	42.302848
3503.907073	514603.485883	42.307853
3504.084076	514618.176688	42.312858
3504.397818	514628.091346	42.317863
3504.196796	514615.275759	42.322868
3504.067835	514579.030163	42.327872
3503.945666	514570.956616	42.332877
3504.634322	514533.013703	42.337882
3504.134621	514509.926855	42.342887
3504.029445	514513.939306	42.347892
3504.013051	514536.652449	42.352896
3503.770199	514530.469430	42.357901
3504.352527	514499.776234	42.362906
3504.200575	514519.172519	42.367911
3504.283043	514482.893297	42.372916
3504.249034	514507.076099	42.377920
3504.248499	514459.732835	42.382925
3504.039546	514478.480628	42.387930
3503.880723	514467.934382	42.392935
3504.265134	514450.220987	42.397940
3503.944000	514445.365404	42.402944
3503.982253	514417.438825	42.407949
3504.377478	514422.434399	42.412954
3504.261057	514430.242195	42.417959
3503.693193	514402.613716	42.422964
3504.284101	514358.919660	42.427968
3504.268371	514373.691723	42.432973
3503.797871	514397.791929	42.437978
3503.577340	514365.353900	42.442983
3503.869909	514344.923547	42.447988
3504.261783	514334.189013	42.452992
3503.905219	514377.340236	42.457997
3504.036531	514341.457637	42.463002
3504.251186	514350.174178	42.468007
3503.569725	514327.571037	42.473012
3504.384447	514293.451812	42.478016
3504.244023	514336.366653	42.483021
3503.901051	514292.718871	42.488026
3504.089132	514284.950217	42.493031
3503.948277	514308.340894	42.498036
3504.526736	514263.333452	42.503040
3503.946265	514293.268018	42.508045
3503.792514	514285.755718	42.513050
3503.790365	514256.621314	42.518055
3504.150145	514234.612188	42.523060
3503.884377	514269.454014	42.528064
3503.935476	514254.220990	42.533069
3503.967479	514230.088676	42.538074
3504.044075	514219.100414	42.543079
3504.141268	514197.082162	42.548084
3503.968306	514170.756581	42.553088
3503.751854	514212.216893	42.558093
3503.829379	514175.229654	42.563098
3504.113756	514201.891639	42.568103
3503.820073	514216.606609	42.573108
3504.100562	514193.041943	42.578112
3504.206793	514162.372805	42.583117
3504.160631	514149.481805	42.588122
3504.255072	514148.657550	42.593127
3504.263133	514144.407407	42.598132
3503.730967	514150.965925	42.603136
3504.121895	514156.164584	42.608141
3503.798163	514152.725607	42.613146
3503.606710	514142.437221	42.618151
3503.618465	514138.894634	42.623156
3504.251402	514108.445637	42.628160
3504.129565	514101.130537	42.633165
3504.153164	514084.687748	42.638170
3504.333520	514077.274291	42.643175
3503.704562	514084.202206	42.648180
3504.016342	514082.584870	42.653184
3504.082205	514087.227949	42.658189
3503.758060	514109.636238	42.663194
3504.032946	514090.776402	42.668199
3503.789187	514061.376359	42.673204
3504.121428	514040.737041	42.678208
3503.764346	514048.734797	42.683213
3503.972796	514045.414010	42.688218
3504.026518	514043.230477	42.693223
3503.900386	514036.118355	42.698228
3504.008161	514026.440166	42.703232
3503.976371	514019.515453	42.708237
3503.770002	514018.586991	42.713242
3504.148214	514040.530285	42.718247
3504.461140	514022.675997	42.723252
3504.352430	513955.115662	42.728256
3504.408308	513939.578107	42.733261
3503.827777	513938.708780	42.738266
3504.359780	513952.737070	42.743271
3503.924888	513968.283888	42.748276
3504.276272	513931.252830	42.753280
3504.218578	513878.454100	42.758285
3503.807446	513892.682092	42.763290
3503.575621	513901.317689	42.768295
3503.330012	513901.204738	42.773300
3504.009519	513902.968855	42.778304
3504.157822	513917.007239	42.783309
3503.916611	513896.357219	42.788314
3504.434077	513893.948623	42.793319
3503.663747	513900.696627	42.798324
3504.337774	513895.633009	42.803329
3504.135509	513816.604736	42.808333
3503.866988	513808.958616	42.813338
3503.683435	513830.839227	42.818343
3504.074868	513832.750049	42.823348
3504.152119	513809.419301	42.828353
3504.035530	513809.285957	42.833357
3503.823904	513806.233849	42.838362
3503.932765	513784.820206	42.843367
3504.096758	513776.346971	42.848372
3503.961862	513791.340709	42.853377
3503.886761	513763.026304	42.858381
3503.560272	513756.198645	42.863386
3504.128538	513739.871762	42.868391
3504.632723	513726.691123	42.873396
3504.614277	513715.312894	42.878401
3503.786370	513735.525076	42.883405
3503.784639	513724.043045	42.888410
3504.472604	513698.491141	42.893415
3504.082500	513665.724491	42.898420
3503.935374	513677.179457	42.903425
3504.006167	513707.770863	42.908429
3503.463694	513689.596182	42.913434
3504.137773	513655.447321	42.918439
3504.003280	513631.998047	42.923444
3504.103887	513645.791281	42.928449
3503.752314	513672.554619	42.933453
3503.798893	513689.391331	42.938458
3504.007053	513689.661902	42.943463
3503.784099	513681.705025	42.948468
3503.730074	513662.441453	42.953473
3503.836061	513665.560818	42.958477
3503.732702	513659.254264	42.963482
3503.915524	513668.279687	42.968487
3503.818245	513669.154948	42.973492
3503.865115	513654.023218	42.978497
3503.613387	513631.654716	42.983501
3503.770070	513623.536641	42.988506
3503.800855	513619.535690	42.993511
3504.133094	513573.047839	42.998516
3503.909979	513588.662698	43.003521
3503.796000	513609.166853	43.008525
3503.677885	513596.843219	43.013530
3504.035134	513601.996790	43.018535
3503.711394	513584.697919	43.023540
3503.904121	513557.908917	43.028545
3504.042060	513549.186770	43.033549
3503.491939	513570.973906	43.038554
3504.138591	513541.179305	43.043559
3503.918165	513552.089526	43.048564
3504.325549	513561.990011	43.053569
3504.211102	513546.630766	43.058573
3503.956976	513533.569834	43.063578
3504.041367	513511.400963	43.068583
3503.957747	513507.974485	43.073588
3504.329958	513497.394281	43.078593
3504.079638	513505.678918	43.083597
3503.824606	513487.053918	43.088602
3503.995845	513458.143650	43.093607
3504.364471	513441.645702	43.098612
3504.223116	513429.224452	43.103617
3504.016509	513421.720121	43.108621
3504.293397	513418.742480	43.113626
3504.041700	513424.700526	43.118631
3503.896559	513406.665072	43.123636
3503.946704	513385.310788	43.128641
3503.733605	513387.013710	43.133645
3503.729353	513397.636943	43.138650
3504.157238	513384.670434	43.143655
3504.417215	513361.917193	43.148660
3504.239372	513383.342225	43.153665
3504.134420	513374.405460	43.158669
3503.859805	513358.970193	43.163674
3504.293891	513323.998674	43.168679
3504.306364	513310.541344	43.173684
3504.221603	513293.710242	43.178689
3504.171482	513333.477143	43.183693
3503.815517	513322.759004	43.188698
3503.938089	513296.334766	43.193703
3503.930829	513285.662656	43.198708
3504.264588	513272.812107	43.203713
3503.860367	513276.568611	43.208717
3503.960581	513223.489959	43.213722
3504.044082	513250.589870	43.218727
3503.755445	513274.055918	43.223732
3503.509992	513243.440702	43.228737
3504.061765	513233.186041	43.233741
3504.253119	513201.540608	43.238746
3504.142853	513185.522779	43.243751
3504.169932	513231.904266	43.248756
3504.061849	513214.469761	43.253761
3504.506935	513172.920235	43.258765
3504.051179	513182.249188	43.263770
3504.136803	513204.239815	43.268775
3503.951847	513183.478864	43.273780
3503.653176	513141.439806	43.278785
3504.332037	513113.915667	43.283789
3503.949770	513147.463015	43.288794
3503.938250	513162.791899	43.293799
3504.027580	513143.859170	43.298804
3504.173536	513129.925338	43.303809
3504.121724	513111.723066	43.308813
3503.779680	513090.632738	43.313818
3504.035832	513101.417336	43.318823
3503.843964	513108.782404	43.323828
3503.612046	513078.468258	43.328833
3504.136411	513062.451174	43.333837
3504.044320	513057.356647	43.338842
3503.802865	513070.496229	43.343847
3503.524175	513062.497285	43.348852
3504.283723	513028.738333	43.353857
3504.185997	513018.940297	43.358861
3503.868148	513066.489621	43.363866
3504.141615	513040.951660	43.368871
3504.045577	513000.853031	43.373876
3503.953952	512986.855464	43.378881
3503.990426	513030.352674	43.383885
3503.871764	513016.966423	43.388890
3504.274205	512971.932791	43.393895
3504.159568	512996.585759	43.398900
3503.923513	512970.015357	43.403905
3503.880143	512978.115785	43.408909
3503.882089	512967.998455	43.413914
3504.252816	512949.577468	43.418919
3503.737631	512939.238347	43.423924
3504.020757	512929.329477	43.428929
3503.762462	512929.522034	43.433933
3504.118493	512935.890045	43.438938
3503.809663	512922.483191	43.443943
3504.024261	512897.864852	43.448948
3503.842285	512904.115571	43.453953
3504.204853	512877.248065	43.458957
3503.731422	512911.467896	43.463962
3504.348935	512866.551746	43.468967
3503.836204	512870.780758	43.473972
3503.996744	512865.646244	43.478977
3504.032335	512846.165238	43.483981
3503.937290	512854.375064	43.488986
3503.970166	512835.855598	43.493991
3504.096611	512813.021558	43.498996
3503.767415	512848.129257	43.504001
3504.040742	512817.127762	43.509005
3503.608414	512833.838677	43.514010
3504.262783	512807.481379	43.519015
3503.691266	512795.481753	43.524020
3503.846197	512789.386977	43.529025
3503.827942	512782.763131	43.534029
3504.111008	512805.734779	43.539034
3503.920297	512782.343801	43.544039
3503.661493	512769.434774	43.549044
3503.724161	512764.416870	43.554049
3503.971722	512748.493827	43.559053
3503.778586	512757.781503	43.564058
3503.768483	512763.398079	43.569063
3503.782439	512767.240355	43.574068
3503.927086	512731.959267	43.579073
3503.707298	512767.758039	43.584077
3503.593759	512748.502836	43.589082
3503.941684	512717.337610	43.594087
3503.442063	512762.235472	43.599092
3503.543448	512715.579419	43.604097
3503.841936	512716.442760	43.609101
3503.719015	512764.366806	43.614106
3503.588547	512753.106808	43.619111
3503.851857	512727.822909	43.624116
3504.003545	512711.510300	43.629121
3504.029981	512744.993843	43.634125
3503.522930	512739.357781	43.639130
3503.680005	512708.576804	43.644135
3503.594874	512703.025799	43.649140
3504.066670	512675.230166	43.654145
3503.719933	512733.762119	43.659149
3503.397191	512709.279023	43.664154
3503.749116	512675.836729	43.669159
3503.793460	512650.030880	43.674164
3504.022422	512689.401077	43.679169
3503.832209	512693.629742	43.684173
3503.703072	512673.415787	43.689178
3503.725043	512655.656637	43.694183
3503.706601	512678.322011	43.699188
3503.632895	512705.902912	43.704193
3503.852311	512668.940543	43.709197
3503.432737	512640.476367	43.714202
3504.094212	512615.331713	43.719207
3504.071337	512649.126755	43.724212
3503.899387	512635.141594	43.729217
3504.035104	512648.070128	43.734221
3503.758172	512626.058383	43.739226
3504.039031	512608.865296	43.744231
3503.444890	512615.383611	43.749236
3503.398355	512606.841897	43.754241
3504.006635	512575.281157	43.759245
3503.583614	512618.245017	43.764250
3503.845681	512608.086358	43.769255
3503.498457	512624.480510	43.774260
3503.463795	512640.825244	43.779265
3503.740172	512616.550834	43.784269
3503.827450	512572.982369	43.789274
3503.885550	512553.446884	43.794279
3503.537150	512557.751171	43.799284
3503.760580	512546.232754	43.804289
3503.888282	512563.108348	43.809293
3503.556463	512612.279910	43.814298
3503.339662	512591.219751	43.819303
3503.579263	512576.006011	43.824308
3503.693293	512560.002725	43.829313
3503.540705	512616.936220	43.834317
3503.915995	512578.987884	43.839322
3503.791357	512601.771318	43.844327
3503.651496	512574.476887	43.849332
3503.774255	512590.645028	43.854337
3504.092654	512556.297249	43.859341
3503.569237	512577.980261	43.864346
3503.758276	512581.997250	43.869351
3503.752193	512548.105431	43.874356
3503.891655	512588.147630	43.879361
3503.670890	512558.589584	43.884365
3503.904127	512519.601258	43.889370
3503.671922	512554.036611	43.894375
3503.836717	512534.888931	43.899380
3503.616219	512549.694950	43.904385
3503.899905	512525.065151	43.909389
3503.529383	512545.864071	43.914394
3503.820831	512545.413291	43.919399
3503.575230	512541.506357	43.924404
3503.544289	512499.878668	43.929409
3503.352423	512489.589341	43.934413
3503.529302	512524.010683	43.939418
3503.797179	512487.394365	43.944423
3503.655729	512517.363841	43.949428
3503.641795	512506.085260	43.954433
3503.491192	512507.677218	43.959437
3503.650916	512493.690102	43.964442
3503.590735	512526.631316	43.969447
3503.506247	512524.520020	43.974452
3504.125719	512491.136248	43.979457
3503.956221	512501.179123	43.984461
3503.831668	512531.398836	43.989466
3503.909690	512470.328701	43.994471
3503.923457	512495.265620	43.999476
3503.686964	512463.686438	44.004481
3503.857695	512492.291367	44.009485
3503.739722	512458.315880	44.014490
3503.760427	512494.178389	44.019495
3503.672774	512457.769961	44.024500
3503.522718	512469.883830	44.029505
3503.857894	512446.055162	44.034509
3503.507755	512454.254914	44.039514
3503.957373	512454.386170	44.044519
3503.888616	512453.031177	44.049524
3503.707059	512458.017329	44.054529
3504.086384	512461.245473	44.059533
3503.597463	512437.597635	44.064538
3503.960157	512414.321026	44.069543
3503.672519	512437.535137	44.074548
3503.917131	512405.272765	44.079553
3504.117073	512428.713341	44.084557
3503.638059	512412.753066	44.089562
3504.073865	512409.851306	44.094567
3503.810769	512413.535106	44.099572
3504.331022	512370.960008	44.104577
3504.022398	512407.684141	44.109581
3503.686693	512380.774460	44.114586
3503.962072	512382.602619	44.119591
3503.947648	512339.909607	44.124596
3504.127186	512350.757379	44.129601
3503.777497	512341.251711	44.134605
3503.723138	512367.261909	44.139610
3504.171333	512345.590470	44.144615
3503.384856	512336.457357	44.149620
3503.723611	512312.880873	44.154625
3503.319887	512319.672724	44.159629
3503.452454	512316.565943	44.164634
3503.661228	512325.992676	44.169639
3503.652491	512330.799789	44.174644
3503.604687	512324.180435	44.179649
3504.247693	512320.082411	44.184653
3503.687892	512319.968520	44.189658
3503.862758	512327.174786	44.194663
3504.148281	512299.762092	44.199668
3503.818653	512281.299318	44.204673
3504.083201	512279.992804	44.209677
3503.971660	512277.885753	44.214682
3504.012163	512285.012100	44.219687
3503.511306	512252.968442	44.224692
3503.815512	512267.236488	44.229697
3503.919598	512244.860503	44.234701
3503.670206	512247.328081	44.239706
3504.295863	512244.295111	44.244711
3503.805051	512252.517194	44.249716
3504.003778	512213.483035	44.254721
3503.952064	512231.702584	44.259725
3503.808953	512215.638444	44.264730
3503.718299	512190.713219	44.269735
3503.310410	512243.540155	44.274740
3503.571293	512225.085160	44.279745
3503.329746	512216.928183	44.284749
3502.947540	512210.665164	44.289754
3503.617906	512183.393803	44.294759
3503.273553	512240.207106	44.299764
3502.880815	512222.158941	44.304769
3503.485339	512203.851956	44.309773
3503.431900	512192.528824	44.314778
3503.659724	512207.770151	44.319783
3503.227468	512266.620751	44.324788
3503.195149	512249.780325	44.329793
3503.023810	512239.285253	44.334797
3503.114694	512243.216663	44.339802
3503.816911	512240.829225	44.344807
3503.656899	512270.549134	44.349812
3503.380582	512276.612645	44.354817
3503.612328	512268.886756	44.359821
3503.560461	512236.266229	44.364826
3504.059886	512202.546757	44.369831
3503.512818	512256.913268	44.374836
3503.790146	512257.678804	44.379841
3503.988873	512236.299591	44.384845
3503.605325	512216.934701	44.389850
3503.967163	512223.959698	44.394855
3503.631999	512245.411028	44.399860
3503.664357	512245.962348	44.404865
3503.715877	512245.853006	44.409869
3503.551253	512232.119291	44.414874
3503.386301	512206.902310	44.419879
3503.796687	512202.790439	44.424884
3503.919067	512190.528945	44.429889
3503.910014	512230.494285	44.434893
3503.392187	512245.600499	44.439898
3503.346017	512220.111828	44.444903
3504.263537	512184.707446	44.449908
3503.969646	512195.326623	44.454913
3503.606348	512216.529501	44.459917
3503.898796	512215.825618	44.464922
3504.002651	512210.193994	44.469927
3503.535842	512202.224377	44.474932
3503.872541	512156.541344	44.479937
3504.070314	512164.351108	44.484941
3503.889195	512140.300094	44.489946
3503.884898	512130.183252	44.494951
3503.732559	512134.406068	44.499956
3503.484029	512165.202489	44.504961
3503.128119	512189.085364	44.509965
3503.192385	512174.708377	44.514970
3503.502309	512149.416252	44.519975
3503.621540	512129.314157	44.524980
3503.744009	512131.419450	44.529985
3504.054878	512134.962002	44.534989
3503.595963	512134.579226	44.539994
3504.189315	512109.242244	44.544999
3503.840936	512093.969247	44.550004
3503.809203	512136.771297	44.555009
3503.866473	512133.625797	44.560013
3503.770550	512130.555097	44.565018
3504.291779	512090.913221	44.570023
3503.910477	512133.719944	44.575028
3503.650347	512127.235248	44.580033
3503.647001	512098.653788	44.585037
3504.141817	512081.375765	44.590042
3503.628064	512116.160030	44.595047
3503.858290	512111.368387	44.600052
3503.300600	512078.422806	44.605057
3503.814181	512050.366613	44.610061
3503.835696	512079.956986	44.615066
3504.404979	512053.257859	44.620071
3504.304980	512039.969064	44.625076
3504.081019	512063.173619	44.630081
3504.009213	512027.975871	44.635085
3503.749569	512020.125187	44.640090
3503.791325	512042.377191	44.645095
3504.099308	512022.548662	44.650100
3503.704502	512032.222723	44.655105
3503.880497	511988.537565	44.660109
3504.074856	512005.302000	44.665114
3504.179906	511983.987866	44.670119
3503.999429	512016.342025	44.675124
3503.509126	511958.850444	44.680129
3503.851682	511967.345647	44.685133
3503.531422	511934.058731	44.690138
3503.550766	511966.937868	44.695143
3503.799474	511942.970402	44.700148
3503.898488	511970.525194	44.705153
3504.175591	511950.195583	44.710157
3504.083258	511950.513680	44.715162
3503.725891	511925.529048	44.720167
3503.999795	511906.262240	44.725172
3503.570127	511925.250090	44.730177
3504.195549	511922.571219	44.735181
3504.102788	511911.557644	44.740186
3503.746755	511885.813920	44.745191
3503.938441	511898.430649	44.750196
3504.026633	511874.286104	44.755201
3503.923241	511885.684776	44.760205
3503.450885	511898.102933	44.765210
3503.936415	511860.843809	44.770215
3503.599036	511874.303004	44.775220
3503.584579	511849.314648	44.780225
3504.032800	511839.581404	44.785229
3503.936855	511865.548353	44.790234
3504.127263	511823.985203	44.795239
3503.962713	511849.861843	44.800244
3503.646464	511817.434066	44.805249
3504.160032	511805.161054	44.810253
3503.472309	511823.582743	44.815258
3504.222586	511796.298135	44.820263
3503.843094	511850.234746	44.825268
3503.211080	511822.713368	44.830273
3503.923659	511798.318261	44.835277
3503.793480	511828.236578	44.840282
3503.873913	511769.187085	44.845287
3504.024528	511800.528137	44.850292
3503.558975	511780.568650	44.855297
3504.266605	511768.720235	44.860301
3503.631157	511786.121930	44.865306
3504.121753	511763.886578	44.870311
3503.787936	511768.795819	44.875316
3503.744977	511718.264530	44.880321
3503.931506	511755.721222	44.885325
3503.631407	511730.980195	44.890330
3503.768338	511761.615241	44.895335
3503.353450	511748.123046	44.900340
3503.265560	511758.102871	44.905345
3503.779351	511732.879084	44.910349
3503.668358	511767.145102	44.915354
3504.135577	511738.083952	44.920359
3503.673131	511721.614522	44.925364
3503.517484	511714.455500	44.930369
3503.704289	511702.942304	44.935373
3503.950427	511708.721083	44.940378
3504.006652	511694.547316	44.945383
3503.675058	511721.310563	44.950388
3504.031330	511686.955047	44.955393
3504.059334	511674.556333	44.960397
3503.674042	511688.731490	44.965402
3503.853914	511671.958132	44.970407
3503.675062	511672.846388	44.975412
3503.658546	511671.786608	44.980417
3503.413911	511685.332470	44.985421
3503.427483	511698.584565	44.990426
3503.771378	511676.675819	44.995431
3503.519325	511695.787617	45.000436
3503.567550	511686.168098	45.005441
3503.886802	511649.895984	45.010445
3503.824719	511649.146939	45.015450
3503.677339	511628.833450	45.020455
3503.670372	511630.959264	45.025460
3503.998077	511648.714754	45.030465
3503.835089	511632.501438	45.035469
3503.914997	511648.019591	45.040474
3503.947617	511624.844667	45.045479
3503.668089	511620.639348	45.050484
3503.976148	511613.305814	45.055489
3504.181350	511618.686381	45.060493
3503.309969	511620.291167	45.065498
3504.297081	511607.437275	45.070503
3504.001725	511583.707066	45.075508
3503.630593	511575.165550	45.080513
3503.560844	511562.073957	45.085517
3503.685852	511576.725030	45.090522
3504.077200	511560.474618	45.095527
3504.047310	511596.701137	45.100532
3503.905386	511578.207932	45.105537
3503.754448	511546.259402	45.110541
3504.171145	511524.389544	45.115546
3504.075096	511561.233667	45.120551
3503.971241	511544.960333	45.125556
3503.831201	511533.701040	45.130561
3504.042528	511522.234436	45.135565
3504.073142	511503.359754	45.140570
3504.141688	511523.483447	45.145575
3504.194223	511497.876916	45.150580
3503.667385	511480.608000	45.155585
3504.221975	511458.513905	45.160589
3503.818122	511462.978998	45.165594
3504.001717	511484.703415	45.170599
3504.267888	511443.734438	45.175604
3504.085977	511433.493488	45.180609
3503.869273	511440.660842	45.185613
3503.675750	511434.772429	45.190618
3503.904559	511413.842739	45.195623
3503.714914	511434.867369	45.200628
3503.926575	511405.238973	45.205633
3504.008027	511396.979960	45.210637
3503.314505	511393.295327	45.215642
3503.787080	511392.057045	45.220647
3503.529962	511404.340360	45.225652
3503.705921	511397.280561	45.230657
3503.826728	511388.661196	45.235661
3503.826194	511413.197241	45.240666
3503.885849	511373.019580	45.245671
3503.939641	511377.665309	45.250676
3503.609817	511358.240360	45.255681
3503.665202	511383.172327	45.260685
3504.013381	511367.383863	45.265690
3503.809419	511353.352118	45.270695
3504.043638	511375.928699	45.275700
3504.050602	511319.115210	45.280705
3503.635589	511344.273354	45.285709
3503.220601	511322.737053	45.290714
3503.653227	511327.171148	45.295719
3503.536980	511314.542023	45.300724
3503.556068	511341.503385	45.305729
3503.684804	511313.304452	45.310733
3503.579589	511329.358054	45.315738
3503.484362	511337.214509	45.320743
3503.870383	511320.205864	45.325748
3503.444579	511356.040161	45.330753
3504.272440	511316.499793	45.335757
3503.782999	511330.843478	45.340762
3503.965637	511287.813146	45.345767
3503.899512	511302.646434	45.350772
3503.918274	511274.616590	45.355777
3504.002238	511310.471589	45.360781
3503.682941	511253.658861	45.365786
3503.638821	511270.461713	45.370791
3503.666546	511238.939680	45.375796
3503.858921	511274.474079	45.380801
3504.057706	511248.591109	45.385805
3503.727676	511275.506575	45.390810
3503.823290	511244.530312	45.395815
3503.976227	511218.755724	45.400820
3503.457696	511237.454840	45.405825
3503.777254	511188.736521	45.410829
3503.473900	511247.114945	45.415834
3503.617194	511232.168182	45.420839
3503.281168	511226.555170	45.425844
3503.967218	511198.217369	45.430849
3503.863028	511217.761641	45.435853
3503.274684	511224.330154	45.440858
3503.681977	511217.334898	45.445863
3503.957695	511224.323330	45.450868
3503.526254	511213.211065	45.455873
3503.477588	511205.377248	45.460877
3503.677582	511165.682821	45.465882
3503.684235	511209.594116	45.470887
3503.630168	511179.046115	45.475892
3503.588658	511189.373073	45.480897
3503.957903	511195.891422	45.485901
3503.624588	511182.385884	45.490906
3503.852172	511174.660160	45.495911
3503.592155	511222.863158	45.500916
3503.594658	511200.552452	45.505921
3503.625378	511187.191740	45.510925
3504.016726	511161.480563	45.515930
3503.960743	511183.647954	45.520935
3503.698669	511167.500448	45.525940
3503.593331	511135.189810	45.530945
3503.771589	511161.215669	45.535949
3503.690230	511168.867648	45.540954
3503.801455	511139.457028	45.545959
3503.935690	511160.936707	45.550964
3504.083154	511124.538861	45.555969
3503.622138	511127.343590	45.560973
3503.476658	511123.066370	45.565978
3503.435885	511131.015493	45.570983
3503.856528	511099.380509	45.575988
3503.794203	511138.092062	45.580993
3504.165261	511102.771819	45.585997
3503.640033	511122.787473	45.591002
3503.727578	511071.879511	45.596007
3503.902435	511100.536713	45.601012
3503.660519	511068.348717	45.606017
3503.848349	511077.981815	45.611021
3503.525502	511100.950352	45.616026
3503.659797	511064.959185	45.621031
3503.852140	511099.279777	45.626036
3503.651506	511086.512051	45.631041
3503.949161	511035.671953	45.636045
3503.585495	511075.088959	45.641050
3503.787624	511033.420854	45.646055
3503.699791	511074.210804	45.651060
3503.243532	511062.242323	45.656065
3503.600757	511034.006815	45.661069
3503.790284	511043.589072	45.666074
3503.310092	511062.838817	45.671079
3503.681067	511043.403923	45.676084
3503.232607	511078.888247	45.681089
3503.736790	511037.324180	45.686093
3503.075212	511062.167575	45.691098
3503.471445	511058.057669	45.696103
3503.800917	511056.740802	45.701108
3503.733564	511035.604508	45.706113
3503.796063	511074.347067	45.711117
3503.485375	511068.173502	45.716122
3503.580655	511045.898520	45.721127
3503.428334	511041.268226	45.726132
3503.601810	511000.768156	45.731137
3504.038186	511046.180265	45.736141
3503.302057	511020.039995	45.741146
3503.668078	511014.417131	45.746151
3503.761043	511044.200369	45.751156
3503.864168	511003.104336	45.756161
3503.802577	511032.507296	45.761165
3504.198735	511007.705762	45.766170
3503.968012	511024.133624	45.771175
3503.801716	510997.802071	45.776180
3503.774699	511020.218049	45.781185
3503.922345	510975.978285	45.786189
3503.787309	511003.166905	45.791194
3503.936450	510986.296551	45.796199
3503.689253	510990.484050	45.801204
3503.879535	510954.787348	45.806209
3503.750293	510972.565175	45.811213
3503.470768	510950.703448	45.816218
3503.475143	510984.193934	45.821223
3503.796124	510949.083653	45.826228
3503.573827	510989.945648	45.831233
3503.737796	510958.806292	45.836237
3503.990222	510966.405603	45.841242
3503.600469	510963.381135	45.846247
3503.958089	510920.676360	45.851252
3503.451107	510950.251042	45.856257
3503.740806	510915.246817	45.861261
3503.517828	510913.005437	45.866266
3503.583704	510944.108499	45.871271
3503.804558	510947.210209	45.876276
3503.474711	510914.580503	45.881281
3503.972182	510934.890049	45.886285
3503.344232	510933.370364	45.891290
3503.741569	510909.934460	45.896295
3503.646516	510947.791569	45.901300
3503.656831	510914.905733	45.906305
3503.861338	510925.750467	45.911309
3503.800075	510880.885794	45.916314
3503.906782	510915.068518	45.921319
3503.898281	510884.209241	45.926324
3503.568281	510904.143701	45.931329
3503.857221	510882.900312	45.936333
3503.619957	510882.128330	45.941338
3503.836994	510896.057164	45.946343
3504.101611	510858.071910	45.951348
3503.760518	510872.746667	45.956353
3503.904642	510850.868441	45.961357
3503.472898	510884.984559	45.966362
3503.673583	510849.285992	45.971367
3503.930802	510840.796565	45.976372
3503.394162	510900.174279	45.981377
3503.432269	510871.837170	45.986381
3504.016360	510839.720551	45.991386
3503.687558	510860.363151	45.996391
3503.555761	510822.744022	46.001396
3503.666141	510851.361241	46.006401
3504.109794	510801.256241	46.011405
3503.892280	510831.088924	46.016410
3503.732188	510859.040602	46.021415
3503.781403	510820.178667	46.026420
3503.671107	510812.405002	46.031425
3503.491751	510798.925418	46.036429
3503.726693	510799.596539	46.041434
3503.431780	510789.069515	46.046439
3503.642830	510799.457971	46.051444
3503.274370	510813.985330	46.056449
3503.812768	510804.439614	46.061453
3503.581383	510801.693633	46.066458
3503.717833	510813.510432	46.071463
3503.960171	510795.410967	46.076468
3503.586936	510807.713062	46.081473
3503.923856	510785.652506	46.086477
3503.779248	510786.990716	46.091482
3504.097181	510743.887042	46.096487
3503.706214	510783.056076	46.101492
3503.072580	510751.688271	46.106497
3504.238389	510727.220005	46.111501
3503.827175	510734.013665	46.116506
3503.522991	510739.424431	46.121511
3503.460179	510788.963453	46.126516
3503.535419	510781.919321	46.131521
3503.596332	510754.337286	46.136525
3503.746798	510758.158438	46.141530
3503.779557	510766.298474	46.146535
3503.659196	510737.834417	46.151540
3503.936287	510714.366661	46.156545
3503.654647	510752.456059	46.161549
3503.601888	510743.256704	46.166554
3503.920803	510708.753357	46.171559
3503.701735	510741.571351	46.176564
3503.444218	510728.609981	46.181569
3503.229483	510708.204861	46.186573
3503.937761	510694.736671	46.191578
3503.681262	510705.452044	46.196583
3503.680943	510704.440235	46.201588
3503.387130	510685.312379	46.206593
3503.681381	510680.611402	46.211597
3503.554280	510727.934723	46.216602
3503.265204	510712.347564	46.221607
3503.660868	510692.706004	46.226612
3503.596333	510695.043401	46.231617
3503.642871	510722.659091	46.236621
3503.710692	510678.937094	46.241626
3503.968100	510701.055575	46.246631
3503.856894	510732.490561	46.251636
3503.263608	510704.303564	46.256641
3503.589559	510706.427464	46.261645
3503.288644	510683.556941	46.266650
3503.720951	510663.251864	46.271655
3504.120516	510667.337215	46.276660
3503.287506	510706.019783	46.281665
3503.206896	510679.117688	46.286669
3503.817649	510667.132054	46.291674
3503.407827	510686.320505	46.296679
3503.998537	510648.586795	46.301684
3503.191106	510700.216850	46.306689
3503.635884	510653.450295	46.311693
3503.502878	510697.739120	46.316698
3503.433548	510683.381995	46.321703
3503.823223	510653.268836	46.326708
3503.483021	510689.293364	46.331713
3504.038732	510697.654326	46.336717
3503.746749	510678.273215	46.341722
3503.818847	510635.005756	46.346727
3503.823000	510654.331179	46.351732
3503.364538	510645.701815	46.356737
3504.183724	510606.060000	46.361741
3503.888592	510664.590883	46.366746
3503.251534	510639.041473	46.371751
3503.736084	510634.158629	46.376756
3503.149331	510670.475125	46.381761
3503.098845	510648.374442	46.386765
3503.751000	510636.078691	46.391770
3503.590232	510660.641140	46.396775
3503.433861	510633.143846	46.401780
3503.593808	510623.860215	46.406785
3503.530969	510661.459904	46.411789
3503.970328	510636.145086	46.416794
3503.674504	510640.239173	46.421799
3503.743078	510611.137939	46.426804
3503.819758	510617.045057	46.431809
3503.950368	510618.795107	46.436813
3503.257179	510615.869129	46.441818
3504.252636	510582.169250	46.446823
3504.020552	510579.220975	46.451828
3503.532806	510561.995541	46.456833
3503.846751	510574.745701	46.461837
3503.696497	510585.899684	46.466842
3503.304496	510566.736623	46.471847
3504.319308	510535.866752	46.476852
3503.874703	510548.483866	46.481857
3504.236152	510540.331961	46.486861
3503.868457	510537.303930	46.491866
3503.928900	510511.694675	46.496871
3504.062227	510528.874945	46.501876
3503.551613	510568.366933	46.506881
3503.573121	510540.588414	46.511885
3503.532473	510527.542022	46.516890
3503.935060	510500.563273	46.521895
3503.797244	510519.354771	46.526900
3503.753871	510528.721168	46.531905
3503.838668	510487.019689	46.536909
3503.591781	510511.545371	46.541914
3503.415443	510513.040395	46.546919
3504.069860	510502.363144	46.551924
3503.468108	510504.026593	46.556929
3503.715749	510506.264081	46.561933
3503.602457	510489.788865	46.566938
3503.581344	510515.240111	46.571943
3503.710140	510498.929009	46.576948
3503.802946	510465.270388	46.581953
3503.519725	510494.405747	46.586957
3503.776020	510472.812864	46.591962
3504.304054	510434.835631	46.596967
3504.009152	510486.081763	46.601972
3503.625470	510477.642864	46.606977
3503.758599	510425.764524	46.611981
3503.821462	510431.167965	46.616986
3503.671219	510453.654753	46.621991
3503.636662	510457.859364	46.626996
3503.260313	510437.681835	46.632001
3504.294058	510412.171555	46.637005
3503.966915	510418.952051	46.642010
3503.931415	510454.220614	46.647015
3504.150107	510405.111273	46.652020
3503.829989	510403.138142	46.657025
3504.079937	510434.668367	46.662029
3503.899732	510404.189514	46.667034
3503.859726	510402.779220	46.672039
3503.583946	510390.377000	46.677044
3503.942586	510353.691176	46.682049
3503.655819	510366.131698	46.687053
3503.800166	510340.761889	46.692058
3503.563611	510377.377802	46.697063
3503.803388	510348.653805	46.702068
3503.579752	510368.217924	46.707073
3503.549413	510360.987937	46.712077
3503.903765	510354.759590	46.717082
3503.406861	510364.653096	46.722087
3503.284810	510324.248733	46.727092
3503.817846	510323.456158	46.732097
3504.006946	510329.902127	46.737101
3503.777833	510340.107469	46.742106
3503.508413	510310.502628	46.747111
3503.872283	510340.294863	46.752116
3503.409543	510331.210681	46.757121
3503.658048	510308.809339	46.762125
3504.047094	510311.176281	46.767130
3503.677702	510350.444076	46.772135
3503.523460	510307.110381	46.777140
3503.549961	510280.595474	46.782145
3503.775008	510309.499031	46.787149
3503.428865	510285.167932	46.792154
3503.754390	510284.155189	46.797159
3503.564663	510312.871335	46.802164
3503.535484	510283.076695	46.807169
3503.553883	510312.974175	46.812173
3503.759621	510282.231732	46.817178
3503.813366	510285.056419	46.822183
3503.946576	510293.585546	46.827188
3503.935801	510259.234593	46.832193
3504.006038	510273.642474	46.837197
3504.044102	510242.218160	46.842202
3503.438576	510275.452279	46.847207
3503.934047	510228.170624	46.852212
3503.325229	510276.482005	46.857217
3503.673878	510249.258423	46.862221
3504.054360	510263.971427	46.867226
3503.732061	510219.905179	46.872231
3503.490212	510231.124462	46.877236
3503.669383	510207.216153	46.882241
3503.523769	510228.994199	46.887245
3503.746804	510197.894719	46.892250
3503.423730	510243.277216	46.897255
3503.696075	510203.670313	46.902260
3503.800009	510225.661886	46.907265
3503.377001	510228.258378	46.912269
3503.880044	510207.334465	46.917274
3503.465179	510234.163786	46.922279
3503.700302	510218.796882	46.927284
3503.251349	510243.051326	46.932289
3503.474820	510210.029262	46.937293
3503.558608	510258.130036	46.942298
3503.459086	510240.336985	46.947303
3503.717700	510215.859607	46.952308
3503.625498	510200.847982	46.957313
3503.485965	510220.348383	46.962317
3503.652120	510178.329736	46.967322
3503.273970	510201.864742	46.972327
3503.567893	510177.482915	46.977332
3503.519532	510217.105019	46.982337
3503.790447	510185.340238	46.987341
3503.484166	510207.801417	46.992346
3503.830750	510181.185172	46.997351
3503.958546	510216.833159	47.002356
3503.345629	510199.475364	47.007361
3503.778297	510164.750572	47.012365
3503.586185	510186.991361	47.017370
3503.715238	510184.795429	47.022375
3503.991420	510208.732934	47.027380
3503.372309	510166.079478	47.032385
3504.071916	510159.442337	47.037389
3504.053267	510193.140380	47.042394
3503.497238	510173.446279	47.047399
3503.759034	510164.955795	47.052404
3503.350180	510166.285227	47.057409
3503.656183	510153.234352	47.062413
3503.850811	510150.673898	47.067418
3503.577416	510161.139313	47.072423
3503.864828	510112.574800	47.077428
3503.984318	510097.124877	47.082433
3503.714200	510134.151360	47.087437
3503.785967	510140.565352	47.092442
3503.601886	510159.465743	47.097447
3503.519854	510128.414357	47.102452
3503.408616	510117.655514	47.107457
3503.759859	510109.201458	47.112461
3503.426505	510141.785694	47.117466
3503.380571	510141.792930	47.122471
3504.071480	510113.654949	47.127476
3503.688522	510126.819155	47.132481
3503.543282	510077.412246	47.137485
3503.801943	510113.393918	47.142490
3503.621956	510099.610323	47.147495
3504.040853	510083.860096	47.152500
3503.622534	510105.833182	47.157505
3503.767658	510100.093155	47.162509
3503.625082	510092.678420	47.167514
3503.753787	510080.920352	47.172519
3504.038050	510092.613098	47.177524
3503.316279	510064.900698	47.182529
3503.536320	510040.226792	47.187533
3503.576765	510076.445408	47.192538
3503.540999	510044.020529	47.197543
3503.444838	510069.686672	47.202548
3503.488989	510049.846972	47.207553
3503.568041	510050.896919	47.212557
3503.618203	510055.998923	47.217562
3503.597443	510070.826106	47.222567
3503.710564	510059.981172	47.227572
3503.536800	510072.707605	47.232577
3503.547133	510065.015722	47.237581
3503.566752	510058.384834	47.242586
3503.491318	510075.345587	47.247591
3503.718935	510041.715422	47.252596
3503.470568	510082.988446	47.257601
3503.807934	510045.748799	47.262605
3503.730541	510051.174528	47.267610
3503.365480	510038.482602	47.272615
3503.984802	510011.620612	47.277620
3503.351556	510029.479077	47.282625
3503.145486	510030.624686	47.287629
3503.508117	510029.504876	47.292634
3503.226322	510036.936072	47.297639
3503.534571	510033.092799	47.302644
3503.459867	510059.666252	47.307649
3503.467824	510024.047027	47.312653
3503.712967	510034.481152	47.317658
3503.236491	510044.321019	47.322663
3503.682813	510016.019163	47.327668
3503.579246	510049.123786	47.332673
3503.349490	510023.104328	47.337677
3503.944701	510032.774811	47.342682
3503.628286	510027.714835	47.347687
3503.649907	510035.705198	47.352692
3503.770135	510042.465723	47.357697
3503.877840	510025.955131	47.362701
3503.870200	510023.426629	47.367706
3503.465584	510027.791023	47.372711
3503.652899	510002.262143	47.377716
3503.883373	510005.919036	47.382721
3503.265884	509994.228258	47.387725
3504.038844	509976.701781	47.392730
3503.654588	510023.359375	47.397735
3503.913032	509992.203333	47.402740
3503.725389	510019.654793	47.407745
3503.854803	509968.989911	47.412749
3504.063692	509969.412215	47.417754
3503.712366	509973.110480	47.422759
3504.249482	509955.418883	47.427764
3503.523645	509971.065911	47.432769
3503.755636	509940.268114	47.437773
3504.038433	509969.314897	47.442778
3503.829336	509960.544585	47.447783
3503.355105	509929.150077	47.452788
3503.302151	509925.920407	47.457793
3504.029148	509908.046967	47.462797
3503.524762	509946.932268	47.467802
3503.430412	509923.825706	47.472807
3504.079985	509904.092521	47.477812
3503.905718	509935.235369	47.482817
3503.288037	509936.446042	47.487821
3503.901193	509912.620510	47.492826
3503.530107	509933.017935	47.497831
3503.704881	509884.875335	47.502836
3503.805483	509874.082857	47.507841
3503.580745	509911.709776	47.512845
3503.755067	509907.128733	47.517850
3503.557972	509890.261435	47.522855
3503.702046	509910.071520	47.527860
3503.199198	509904.383252	47.532865
3503.749007	509864.934091	47.537869
3503.547386	509905.997773	47.542874
3503.201918	509902.713144	47.547879
3503.727461	509869.136741	47.552884
3503.384263	509904.657443	47.557889
3503.494904	509893.155073	47.562893
3503.760265	509917.094696	47.567898
3503.860393	509884.951602	47.572903
3504.012670	509890.442269	47.577908
3503.862829	509852.419112	47.582913
3503.817702	509881.467282	47.587917
3503.755429	509851.373560	47.592922
3503.577187	509889.802686	47.597927
3503.867716	509847.864761	47.602932
3503.591124	509883.982110	47.607937
3503.646265	509854.426370	47.612941
3503.835200	509817.614446	47.617946
3503.681120	509861.048654	47.622951
3503.412915	509815.100832	47.627956
3503.381537	509836.557752	47.632961
3503.609826	509808.846555	47.637965
3503.687151	509841.518231	47.642970
3503.607609	509822.456733	47.647975
3504.118702	509797.534099	47.652980
3503.529606	509856.316576	47.657985
3503.596013	509821.041852	47.662989
3503.619267	509853.671456	47.667994
3503.029240	509837.574532	47.672999
3503.977429	509812.431051	47.678004
3503.621357	509842.236755	47.683009
3503.375614	509794.413340	47.688013
3503.381595	509806.555021	47.693018
3503.246138	509794.029000	47.698023
3503.328732	509806.107978	47.703028
3502.973404	509847.398473	47.708033
3503.479506	509819.946948	47.713037
3503.604458	509844.768968	47.718042
3503.289744	509872.443125	47.723047
3503.688079	509832.360107	47.728052
3503.645030	509854.476575	47.733057
3503.702069	509824.566325	47.738061
3503.797830	509845.699573	47.743066
3503.729681	509806.853895	47.748071
3503.994282	509802.309150	47.753076
3503.513456	509822.521673	47.758081
3503.743775	509795.518454	47.763085
3503.869293	509828.941452	47.768090
3503.721368	509807.563408	47.773095
3503.714809	509813.483960	47.778100
3503.459858	509816.812864	47.783105
3503.577214	509785.678749	47.788109
3503.542583	509793.779304	47.793114
3503.320574	509765.481484	47.798119
3503.533355	509783.965398	47.803124
3503.312870	509792.449491	47.808129
3503.088328	509765.467525	47.813133
3503.153627	509784.834855	47.818138
3503.019395	509809.546109	47.823143
3504.027922	509789.452492	47.828148
3503.886079	509814.974451	47.833153
3503.651282	509821.184046	47.838157
3503.583710	509818.664986	47.843162
3503.202350	509807.341512	47.848167
3503.690945	509802.002447	47.853172
3503.322533	509800.694605	47.858177
3503.200214	509786.547483	47.863181
3503.255084	509784.515009	47.868186
3503.437777	509764.096542	47.873191
3503.393183	509801.796417	47.878196
3503.834879	509772.938355	47.883201
3503.993975	509814.754752	47.888205
3503.763849	509782.360101	47.893210
3503.766264	509771.532483	47.898215
3504.162126	509752.851116	47.903220
3503.681774	509802.610761	47.908225
3503.569916	509785.223944	47.913229
3503.979190	509736.133164	47.918234
3503.363198	509775.137681	47.923239
3503.678481	509758.745807	47.928244
3503.302953	509744.891645	47.933249
3503.676418	509745.642104	47.938253
3503.695658	509770.480939	47.943258
3503.241329	509744.243583	47.948263
3503.863825	509711.309277	47.953268
3503.578370	509767.160170	47.958273
3503.170824	509763.986515	47.963277
3503.047257	509749.839559	47.968282
3503.721070	509736.882018	47.973287
3503.833734	509721.685810	47.978292
3504.092355	509719.266961	47.983297
3504.147891	509725.683674	47.988301
3503.872234	509709.941698	47.993306
3503.508842	509712.377059	47.998311
3503.350950	509713.666857	48.003316
3503.422290	509708.747876	48.008321
3503.082108	509718.262817	48.013325
3503.443338	509718.003319	48.018330
3503.228999	509725.373391	48.023335
3503.201986	509728.868663	48.028340
3503.167810	509742.585169	48.033345
3503.561727	509738.829480	48.038349
3503.717823	509782.670211	48.043354
3503.349923	509741.493826	48.048359
3503.619781	509755.465833	48.053364
3503.543114	509722.591463	48.058369
3503.445966	509708.136730	48.063373
3503.300713	509741.349723	48.068378
3503.458552	509711.929290	48.073383
3503.344041	509697.932645	48.078388
3503.113283	509757.923686	48.083393
3503.551296	509780.672536	48.088397
3503.664503	509751.411008	48.093402
3503.520896	509777.085087	48.098407
3503.121361	509730.247095	48.103412
3503.751790	509743.302013	48.108417
3503.305914	509768.568530	48.113421
3503.553353	509754.717099	48.118426
3503.221976	509739.540496	48.123431
3503.823607	509726.240194	48.128436
3503.713477	509744.066865	48.133441
3503.613348	509755.567625	48.138445
3503.874074	509724.107171	48.143450
3503.842529	509721.228240	48.148455
3504.838031	509707.005560	48.153460
3504.450792	509695.126400	48.158465
3503.701054	509683.304528	48.163469
3503.830044	509686.876340	48.168474
3503.827179	509677.111986	48.173479
3504.093563	509663.561056	48.178484
3504.206900	509644.823039	48.183489
3503.762914	509665.333492	48.188493
3503.944158	509645.218683	48.193498
3503.295344	509664.597831	48.198503
3503.852344	509684.241720	48.203508
3503.961654	509647.644396	48.208513
3503.807257	509607.698815	48.213517
3504.113876	509620.197869	48.218522
3503.893540	509629.086777	48.223527
3504.032458	509646.621211	48.228532
3503.735219	509650.968728	48.233537
3503.914667	509621.595321	48.238541
3504.236603	509608.996871	48.243546
3503.752181	509611.957325	48.248551
3503.720877	509596.733167	48.253556
3503.509083	509588.266660	48.258561
3504.218710	509565.184327	48.263565
3503.897028	509546.666746	48.268570
3503.685659	509583.583937	48.273575
3503.717797	509552.311085	48.278580
3503.480822	509557.408026	48.283585
3503.287086	509551.215426	48.288589
3503.623564	509549.998531	48.293594
3503.117621	509552.152875	48.298599
3503.518721	509552.645999	48.303604
3503.524917	509548.698577	48.308609
3504.295686	509528.186881	48.313613
3504.008008	509555.250131	48.318618
3503.590812	509573.631464	48.323623
3503.810590	509539.900368	48.328628
3503.395983	509520.942092	48.333633
3503.306692	509507.194281	48.338637
3503.744360	509478.133982	48.343642
3503.774702	509520.831564	48.348647
3503.693507	509537.692566	48.353652
3503.672119	509533.294144	48.358657
3503.675422	509502.835282	48.363661
3504.245975	509513.926624	48.368666
3503.891811	509538.318862	48.373671
3503.908842	509469.405415	48.378676
3503.726995	509453.395400	48.383681
3503.793683	509476.962274	48.388685
3503.939771	509480.480832	48.393690
3503.651408	509450.573931	48.398695
3503.327203	509486.952614	48.403700
3503.572995	509456.050579	48.408705
3503.483814	509487.534955	48.413709
3503.646007	509503.851568	48.418714
3503.430986	509493.968858	48.423719
3503.823227	509462.487139	48.428724
3504.110423	509423.078477	48.433729
3503.860306	509414.668538	48.438733
3504.049168	509414.537471	48.443738
3503.759616	509421.110033	48.448743
3503.979348	509410.146648	48.453748
3503.785959	509388.927057	48.458753
3503.431426	509415.140968	48.463757
3503.522080	509384.111539	48.468762
3503.631899	509375.745881	48.473767
3503.655735	509367.140830	48.478772
3503.748605	509385.087574	48.483777
3503.543964	509420.637969	48.488781
3503.974203	509426.793186	48.493786
3503.185269	509411.941592	48.498791
3503.463781	509393.885532	48.503796
3503.535052	509398.529035	48.508801
3503.810339	509385.988391	48.513805
3503.755025	509397.684688	48.518810
3503.657484	509438.682437	48.523815
3503.747855	509399.254235	48.528820
3503.482331	509361.855426	48.533825
3503.492700	509361.044232	48.538829
3503.823372	509382.495088	48.543834
3503.562409	509362.146270	48.548839
3503.472070	509364.487925	48.553844
3503.333737	509375.236042	48.558849
3503.397298	509364.449099	48.563853
3503.811605	509329.168975	48.568858
3503.534029	509390.737162	48.573863
3503.398151	509372.544195	48.578868
3504.112631	509353.457867	48.583873
3503.301937	509364.008689	48.588877
3503.536321	509401.462962	48.593882
3503.457505	509410.936761	48.598887
3503.319030	509417.485445	48.603892
3503.498731	509395.296172	48.608897
3503.408993	509396.727008	48.613901
3503.420102	509392.272817	48.618906
3503.845448	509372.422681	48.623911
3503.766381	509407.497893	48.628916
3503.693751	509395.619395	48.633921
3503.451758	509387.511731	48.638925
3503.684846	509373.965837	48.643930
3503.610767	509362.391118	48.648935
3503.206479	509337.258335	48.653940
3503.493522	509331.495622	48.658945
3503.628899	509362.590562	48.663949
3503.909995	509326.117190	48.668954
3503.557300	509365.941143	48.673959
3503.012983	509344.271008	48.678964
3503.895531	509318.327653	48.683969
3503.472168	509341.010850	48.688973
3503.179843	509369.441210	48.693978
3503.424431	509374.411495	48.698983
3503.426090	509358.422982	48.703988
3503.684261	509372.447744	48.708993
3503.496449	509359.170747	48.713997
3503.369206	509343.657956	48.719002
3503.321912	509357.073267	48.724007
3503.429001	509349.062197	48.729012
3503.789517	509331.600259	48.734017
3503.569361	509333.911841	48.739021
3503.682863	509373.560898	48.744026
3503.525904	509366.502293	48.749031
3503.311675	509360.464650	48.754036
3503.479390	509337.518262	48.759041
3503.711846	509323.668854	48.764045
3503.606755	509360.974489	48.769050
3503.418874	509373.653073	48.774055
3503.587502	509344.280904	48.779060
3503.877218	509342.666620	48.784065
3503.387015	509356.910873	48.789069
3503.367353	509330.351204	48.794074
3503.766981	509293.353071	48.799079
3503.865371	509314.284171	48.804084
3503.458575	509318.800875	48.809089
3503.845854	509313.123504	48.814093
3503.793137	509308.274614	48.819098
3503.303731	509340.227284	48.824103
3503.647263	509316.342356	48.829108
3503.856285	509332.955304	48.834113
3503.543910	509323.037287	48.839117
3503.344324	509320.033062	48.844122
3503.857859	509305.279084	48.849127
3504.034420	509271.453103	48.854132
3503.802048	509255.703869	48.859137
3503.476861	509275.285280	48.864141
3503.825332	509312.013372	48.869146
3503.732807	509300.643910	48.874151
3503.082262	509287.338806	48.879156
3503.926070	509270.913527	48.884161
3503.829442	509263.238192	48.889165
3503.570550	509297.127749	48.894170
3503.604065	509326.822170	48.899175
3503.715155	509298.875699	48.904180
3503.433763	509255.255877	48.909185
3503.588276	509249.159911	48.914189
3503.564831	509274.360381	48.919194
3503.309038	509274.552575	48.924199
3503.289944	509247.132556	48.929204
3503.810844	509220.588469	48.934209
3503.275838	509270.560671	48.939213
3503.546216	509257.261771	48.944218
3503.706204	509260.525197	48.949223
3503.520666	509234.345769	48.954228
3503.821633	509267.387953	48.959233
3503.115968	509253.737363	48.964237
3504.059694	509229.049105	48.969242
3503.704663	509254.757378	48.974247
3503.564857	509268.996916	48.979252
3503.554126	509255.388275	48.984257
3503.320838	509264.987761	48.989261
3503.540754	509244.916969	48.994266
3503.634872	509254.667095	48.999271
3503.490738	509277.356837	49.004276
3503.699810	509252.278771	49.009281
3503.750261	509237.395546	49.014285
3503.779099	509249.584602	49.019290
3503.409855	509231.883737	49.024295
3503.201083	509219.470078	49.029300
3504.007339	509192.476076	49.034305
3503.802477	509205.663430	49.039309
3503.819402	509239.054140	49.044314
3503.676711	509239.380245	49.049319
3503.604888	509215.560829	49.054324
3504.169592	509203.986230	49.059329
3503.640341	509230.733998	49.064333
3503.425035	509180.930823	49.069338
3503.747450	509169.495689	49.074343
3503.597725	509206.960501	49.079348
3503.561840	509184.805033	49.084353
3503.611716	509174.576693	49.089357
3503.500522	509191.493371	49.094362
3503.045085	509187.112870	49.099367
3503.231945	509180.556402	49.104372
3504.028821	509157.054965	49.109377
3503.336429	509198.956845	49.114381
3503.722435	509171.877447	49.119386
3504.019429	509160.496922	49.124391
3503.698404	509155.488012	49.129396
3503.789423	509157.952818	49.134401
3503.623138	509144.216887	49.139405
3503.860281	509167.403069	49.144410
3503.746209	509183.004708	49.149415
3503.790685	509159.521006	49.154420
3503.547404	509145.797246	49.159425
3503.096926	509150.928053	49.164429
3503.015371	509156.354721	49.169434
3503.108448	509153.810171	49.174439
3503.679228	509149.419246	49.179444
3503.643917	509164.856664	49.184449
3503.952754	509174.623494	49.189453
3503.870298	509165.023219	49.194458
3503.774063	509185.125102	49.199463
3504.084134	509186.087992	49.204468
3503.916281	509165.268859	49.209473
3503.588795	509144.829106	49.214477
3503.825508	509141.553503	49.219482
3503.691737	509143.497282	49.224487
3503.632276	509139.408355	49.229492
3503.915957	509125.500095	49.234497
3503.532095	509116.706378	49.239501
3503.596815	509117.404474	49.244506
3503.357192	509123.362100	49.249511
3503.276328	509140.982383	49.254516
3503.637736	509135.410236	49.259521
3503.584247	509100.203584	49.264525
3503.751326	509079.483197	49.269530
3503.518638	509055.385407	49.274535
3503.474815	509056.606627	49.279540
3503.277458	509055.271689	49.284545
3503.435722	509054.841877	49.289549
3503.489222	509038.490698	49.294554
3503.564046	509056.035863	49.299559
3503.285610	509074.142812	49.304564
3502.902461	509083.816682	49.309569
3503.118162	509114.899373	49.314573
3503.511782	509125.462372	49.319578
3503.249929	509142.402912	49.324583
3503.105915	509138.428541	49.329588
3503.125271	509139.133806	49.334593
3503.209554	509154.957101	49.339597
3503.769889	509146.216545	49.344602
3503.764933	509125.118635	49.349607
3503.657841	509113.751352	49.354612
3504.130182	509103.405599	49.359617
3503.834215	509112.762095	49.364621
3503.116559	509102.149063	49.369626
3503.303632	509105.357641	49.374631
3503.530786	509128.545454	49.379636
3503.555372	509127.630809	49.384641
3503.534663	509117.160609	49.389645
3503.790074	509112.667733	49.394650
3503.580086	509116.596821	49.399655
3503.282063	509122.766063	49.404660
3503.715473	509074.934497	49.409665
3503.326635	509065.483786	49.414669
3504.041762	509063.701044	49.419674
3503.706142	509089.001722	49.424679
3503.350541	509108.638726	49.429684
3503.713665	509118.751181	49.434689
3503.471552	509129.111084	49.439693
3503.965423	509115.776750	49.444698
3503.958266	509121.343459	49.449703
3503.877260	509085.584566	49.454708
3503.890334	509072.477983	49.459713
3503.708685	509057.428901	49.464717
3503.837598	509066.161704	49.469722
3503.782210	509081.754159	49.474727
3503.660033	509088.199199	49.479732
3503.623326	509093.770587	49.484737
3503.313035	509082.587191	49.489741
3503.779993	509074.721499	49.494746
3503.698938	509038.405955	49.499751
3503.483297	509047.749789	49.504756
3503.810174	509052.251791	49.509761
3503.883182	509062.460732	49.514765
3503.968875	509047.774159	49.519770
3503.455027	509056.861543	49.524775
3503.602072	509047.579104	49.529780
3503.772002	509032.626221	49.534785
3504.081449	509004.900906	49.539789
3503.987488	509020.297127	49.544794
3503.860265	509019.254681	49.549799
3503.663203	509019.994158	49.554804
3504.119851	509014.508111	49.559809
3503.666732	508966.259805	49.564813
3503.684089	508942.881288	49.569818
3503.943751	508935.098895	49.574823
3503.214874	508949.684788	49.579828
3503.564065	508950.641509	49.584833
3503.544301	508974.678106	49.589837
3503.617527	508942.942284	49.594842
3503.823609	508923.025095	49.599847
3503.136117	508954.352027	49.604852
3503.211377	508961.777844	49.609857
3503.708474	508917.072779	49.614861
3503.518649	508944.678085	49.619866
3503.613473	508967.229270	49.624871
3503.535137	508928.686805	49.629876
3504.023100	508931.240695	49.634881
3503.769420	508964.168739	49.639885
3503.848406	508981.713322	49.644890
3503.801235	508918.019289	49.649895
3503.892257	508886.432341	49.654900
3504.109467	508896.315006	49.659905
3503.856753	508888.057010	49.664909
3503.942840	508884.754570	49.669914
3503.688037	508896.685125	49.674919
3503.772775	508877.141243	49.679924
3503.962757	508866.485799	49.684929
3502.944073	508901.508166	49.689933
3503.635724	508916.375530	49.694938
3503.914598	508900.292179	49.699943
3503.768030	508866.769465	49.704948
3503.368586	508867.085562	49.709953
3503.143560	508882.452025	49.714957
3503.357634	508878.168010	49.719962
3504.065050	508860.954349	49.724967
3503.644980	508876.756422	49.729972
3503.640777	508870.280633	49.734977
3503.557026	508858.858896	49.739981
3503.175601	508888.619656	49.744986
3503.741464	508911.855418	49.749991
3503.497866	508915.638073	49.754996
3503.785508	508902.032590	49.760001
3503.123100	508885.895616	49.765005
3503.200023	508886.389404	49.770010
3503.283245	508883.643984	49.775015
3503.100811	508886.809813	49.780020
3503.497365	508887.253080	49.785025
3503.222998	508901.716577	49.790029
3503.948631	508865.728539	49.795034
3503.739846	508892.426177	49.800039
3503.682933	508904.021867	49.805044
3503.449555	508925.107073	49.810049
3503.629471	508919.614140	49.815053
3503.887279	508857.895559	49.820058
3503.903258	508832.189641	49.825063
3503.631788	508846.045560	49.830068
3503.186440	508849.708326	49.835073
3502.839293	508855.278262	49.840077
3503.387482	508858.632197	49.845082
3503.462102	508885.942813	49.850087
3503.434197	508869.351355	49.855092
3503.688249	508829.086426	49.860097
3503.770865	508837.978454	49.865101
3503.897368	508836.491115	49.870106
3503.792067	508853.305999	49.875111
3503.981854	508824.030796	49.880116
3503.999321	508828.227581	49.885121
3503.451708	508831.096960	49.890125
3503.317948	508811.587538	49.895130
3503.672095	508815.123944	49.900135
3503.690667	508824.582671	49.905140
3503.692917	508788.152239	49.910145
3503.684252	508831.313068	49.915149
3503.843215	508831.085529	49.920154
3503.693976	508850.791402	49.925159
3503.303271	508810.122367	49.930164
3504.123705	508785.604757	49.935169
3503.374722	508830.653509	49.940173
3504.049624	508830.546811	49.945178
3503.956148	508819.986738	49.950183
3503.770112	508793.300747	49.955188
3504.050189	508750.805240	49.960193
3503.350855	508776.113267	49.965197
3503.250760	508779.367296	49.970202
3503.557289	508793.890859	49.975207
3503.495393	508800.427673	49.980212
3503.668712	508789.167647	49.985217
3503.167178	508801.036072	49.990221
3503.346706	508757.038553	49.995226
3503.262128	508784.070908	50.000231
3503.155533	508799.064544	50.005236
3503.948190	508811.588557	50.010241
3503.791040	508783.380067	50.015245
3503.747315	508769.320882	50.020250
3503.383693	508779.042432	50.025255
3503.740050	508817.693031	50.030260
3503.942176	508778.549331	50.035265
3503.788014	508762.837883	50.040269
3503.862889	508779.674957	50.045274
3503.799112	508777.711715	50.050279
3503.446039	508724.791961	50.055284
3503.920963	508737.012067	50.060289
3503.765602	508779.234860	50.065293
3503.872624	508763.127948	50.070298
3503.541359	508726.345321	50.075303
3503.645491	508707.051169	50.080308
3503.794208	508734.957483	50.085313
3503.776564	508740.019997	50.090317
3503.490964	508743.758730	50.095322
3503.797972	508736.120557	50.100327
3503.528342	508721.338076	50.105332
3503.872909	508736.867626	50.110337
3503.617323	508741.158189	50.115341
3503.789376	508730.556092	50.120346
3503.583029	508720.772762	50.125351
3503.654256	508714.133200	50.130356
3503.943790	508671.180625	50.135361
3503.565457	508661.576238	50.140365
3503.300187	508680.541678	50.145370
3503.564589	508707.822579	50.150375
3503.538438	508704.335454	50.155380
3503.457125	508705.613222	50.160385
3503.560650	508706.153408	50.165389
3503.676402	508703.301623	50.170394
3503.553046	508667.396766	50.175399
3503.478164	508641.907317	50.180404
3503.870507	508641.794681	50.185409
3503.152557	508678.287898	50.190413
3503.619063	508695.063154	50.195418
3503.744439	508658.714183	50.200423
3503.431150	508648.289945	50.205428
3503.758378	508659.825081	50.210433
3502.886774	508663.049283	50.215437
3503.651015	508682.054389	50.220442
3503.797246	508704.901377	50.225447
3503.610144	508670.372737	50.230452
3503.534848	508610.831028	50.235457
3503.796560	508618.227522	50.240461
3503.784313	508605.023391	50.245466
3503.397838	508605.236246	50.250471
3503.223440	508602.531501	50.255476
3503.689307	508606.404477	50.260481
3503.590699	508606.774224	50.265485
3503.777464	508606.036309	50.270490
3503.268077	508640.523322	50.275495
3503.130736	508646.616739	50.280500
3503.297624	508670.320670	50.285505
3503.614612	508674.672542	50.290509
3503.448571	508663.719062	50.295514
3503.019617	508645.065674	50.300519
3502.861492	508646.709771	50.305524
3503.379335	508648.753003	50.310529
3503.292095	508674.773994	50.315533
3503.086671	508686.292108	50.320538
3503.056945	508689.484434	50.325543
3503.079689	508702.079622	50.330548
3503.626244	508698.451377	50.335553
3503.186900	508704.997288	50.340557
3503.363238	508691.055049	50.345562
3503.536130	508676.657964	50.350567
3503.203586	508712.432422	50.355572
3503.511117	508725.437957	50.360577
3503.222150	508731.757699	50.365581
3503.689595	508729.457500	50.370586
3503.647372	508729.514747	50.375591
3503.417468	508712.550287	50.380596
3503.746220	508678.901482	50.385601
3503.638217	508690.353597	50.390605
3503.684732	508687.107972	50.395610
3503.418280	508673.185107	50.400615
3503.806791	508675.096985	50.405620
3504.075956	508660.482279	50.410625
3503.851541	508653.484641	50.415629
3503.422909	508655.778666	50.420634
3503.322971	508655.642645	50.425639
3503.413260	508656.690902	50.430644
3503.826079	508673.474664	50.435649
3503.698877	508678.706306	50.440653
3503.905445	508641.028926	50.445658
3503.562250	508642.499884	50.450663
3503.756168	508661.190376	50.455668
3504.054484	508670.503775	50.460673
3503.636141	508639.553461	50.465677
3504.014443	508602.709015	50.470682
3503.922006	508597.512018	50.475687
3503.338360	508620.929863	50.480692
3503.423804	508622.383671	50.485697
3503.344469	508625.077871	50.490701
3503.235793	508623.678285	50.495706
3503.213553	508621.202482	50.500711
3503.590744	508606.216471	50.505716
3504.052568	508592.886801	50.510721
3503.573955	508638.753482	50.515725
3503.497533	508633.250377	50.520730
3503.850512	508597.573673	50.525735
3503.483556	508577.038290	50.530740
3503.336665	508538.961173	50.535745
3503.149197	508496.791932	50.540749
3502.956342	508443.238814	50.545754
3502.900279	508389.866303	50.550759
3503.023163	508334.593192	50.555764
3503.425377	508269.712571	50.560769
3503.071852	508186.583694	50.565773
3502.772902	508078.146099	50.570778
3503.068982	507967.893385	50.575783
3502.565857	507841.574264	50.580788
3501.937116	507690.581025	50.585793
3502.273172	507537.409938	50.590797
3502.051863	507432.396904	50.595802
3501.581580	507263.259630	50.600807
3501.725170	507083.295994	50.605812
3501.936409	506906.760800	50.610817
3501.199752	506733.915877	50.615821
3501.059571	506542.555156	50.620826
3500.457446	506362.600743	50.625831
3499.623450	506190.980333	50.630836
3499.719264	505990.720404	50.635841
3499.719242	505791.283030	50.640845
3499.282590	505569.949107	50.645850
3499.191250	505346.837158	50.650855
3498.389448	505115.737392	50.655860
3498.604823	504871.771024	50.660865
3498.045299	504636.122480	50.665869
3497.766357	504370.667687	50.670874
3497.562983	504117.444790	50.675879
3497.499008	503857.920386	50.680884
3497.123664	503584.067470	50.685889
3496.358256	503314.877769	50.690893
3495.921980	503062.739457	50.695898
3495.654006	502773.116102	50.700903
3494.802740	502468.851091	50.705908
3494.721604	502189.311803	50.710913
3494.266330	501926.885245	50.715917
3493.574531	501611.140891	50.720922
3493.119717	501300.111670	50.725927
3492.818618	500967.387458	50.730932
3492.380209	500650.421825	50.735937
3491.619335	500346.055720	50.740941
3490.709160	500014.473150	50.745946
3490.600647	499713.384919	50.750951
3489.942689	499420.174633	50.755956
3489.655446	499106.195332	50.760961
3488.946533	498753.396440	50.765965
3487.963130	498423.112453	50.770970
3488.235726	498071.005774	50.775975
3487.462232	497727.816426	50.780980
3486.597044	497439.720330	50.785985
3485.914911	497099.339942	50.790989
3485.795896	496725.295381	50.795994
3485.647094	496350.994704	50.800999
3484.268123	496018.704288	50.806004
3484.172868	495700.078798	50.811009
3483.570261	495362.792849	50.816013
3482.588348	494979.278920	50.821018
3482.494183	494589.033781	50.826023
3481.638958	494278.352619	50.831028
3480.959082	493908.137210	50.836033
3480.608901	493525.050226	50.841037
3480.180624	493200.407959	50.846042
3479.687962	492826.444521	50.851047
3478.343082	492448.303579	50.856052
3478.470778	492050.981132	50.861057
3477.647503	491683.124345	50.866061
3476.877824	491335.561096	50.871066
3476.132938	490981.960432	50.876071
3475.514787	490609.694449	50.881076
3474.940077	490222.675228	50.886081
3473.841172	489841.960926	50.891085
3473.940725	489441.903202	50.896090
3473.335581	489090.929458	50.901095
3472.365012	488737.676911	50.906100
3471.571996	488329.733527	50.911105
3471.785404	487914.125254	50.916109
3470.602846	487543.610421	50.921114
3469.873100	487186.694363	50.926119
3468.613488	486782.945529	50.931124
3468.705237	486387.789347	50.936129
3467.570495	486050.774718	50.941133
3466.542450	485652.335486	50.946138
3466.314890	485269.517557	50.951143
3465.946107	484894.567219	50.956148
3465.174226	484528.438302	50.961153
3464.361666	484099.787491	50.966157
3463.946625	483710.483125	50.971162
3463.301539	483337.573000	50.976167
3462.745602	482977.714152	50.981172
3461.938929	482585.561084	50.986177
3461.307337	482207.357567	50.991181
3460.687614	481784.705809	50.996186
3460.172297	481365.220827	51.001191
3459.514841	480987.149891	51.006196
3457.655382	480618.940588	51.011201
3457.478548	480234.951649	51.016205
3457.448376	479825.390996	51.021210
3456.452384	479471.213297	51.026215
3455.521195	479109.619956	51.031220
3454.928661	478728.404199	51.036225
3454.180930	478319.534088	51.041229
3453.705871	477910.967267	51.046234
3452.914614	477565.541918	51.051239
3452.047036	477173.798008	51.056244
3451.824460	476751.381714	51.061249
3450.570548	476413.105511	51.066253
3449.865894	476015.281713	51.071258
3450.081475	475597.029624	51.076263
3448.443146	475237.505747	51.081268
3447.872467	474873.041916	51.086273
3447.402236	474450.920843	51.091277
3446.465422	474099.883278	51.096282
3446.065861	473691.067073	51.101287
3445.276604	473340.195887	51.106292
3444.755320	472953.232888	51.111297
3444.252549	472542.635781	51.116301
3443.170162	472189.763455	51.121306
3442.308265	471786.406851	51.126311
3441.970842	471380.525950	51.131316
3441.415406	470995.559492	51.136321
3440.379949	470680.018977	51.141325
3439.244332	470288.134558	51.146330
3439.147746	469880.969428	51.151335
3438.378368	469532.210580	51.156340
3437.404155	469136.527010	51.161345
3436.914314	468773.210134	51.166349
3435.890945	468399.728871	51.171354
3435.983977	467996.401403	51.176359
3434.902292	467641.981400	51.181364
3434.361799	467238.232512	51.186369
3433.207400	466893.192404	51.191373
3432.822325	466482.710970	51.196378
3432.262502	466149.227997	51.201383
3431.364553	465759.706416	51.206388
3430.678766	465370.093461	51.211393
3430.297752	465022.162250	51.216397
3429.126094	464626.476249	51.221402
3428.491965	464273.298614	51.226407
3427.895780	463868.936825	51.231412
3427.115312	463489.244983	51.236417
3426.301288	463157.885723	51.241421
3425.297133	462784.455117	51.246426
3425.098340	462390.450822	51.251431
3424.238479	462071.863483	51.256436
3423.526547	461693.600203	51.261441
3423.173953	461290.064727	51.266445
3422.201891	460969.500845	51.271450
3421.073704	460581.190268	51.276455
3420.471452	460203.746157	51.281460
3419.965073	459854.940225	51.286465
3419.330417	459517.156611	51.291469
3418.078332	459141.470978	51.296474
3418.031087	458747.224990	51.301479
3417.508717	458418.892940	51.306484
3416.529667	458087.584471	51.311489
3415.980041	457733.780441	51.316493
3415.061875	457341.118360	51.321498
3414.739988	456960.429300	51.326503
3414.048952	456601.657950	51.331508
3413.188627	456277.000545	51.336513
3412.531884	455889.598682	51.341517
3412.117977	455508.493658	51.346522
3411.221587	455202.598471	51.351527
3409.711763	454817.545438	51.356532
3410.079177	454420.012018	51.361537
3408.764940	454124.823232	51.366541
3407.843172	453737.730832	51.371546
3407.614247	453407.757003	51.376551
3406.585704	453034.420054	51.381556
3406.063714	452694.283364	51.386561
3405.691939	452340.113011	51.391565
3404.783407	451976.482364	51.396570
3404.538832	451648.819864	51.401575
3403.364293	451268.068677	51.406580
3403.326461	450891.749328	51.411585
3402.064648	450568.291975	51.416589
3401.161168	450224.779174	51.421594
3401.283273	449825.987104	51.426599
3399.900350	449520.397529	51.431604
3398.880756	449141.819904	51.436609
3398.721365	448768.276653	51.441613
3397.639906	448450.699161	51.446618
3397.201266	448123.575962	51.451623
3396.111321	447743.921119	51.456628
3395.754129	447415.607910	51.461633
3394.982700	447063.602888	51.466637
3394.370757	446718.774557	51.471642
3393.880521	446379.149759	51.476647
3393.326440	446022.882249	51.481652
3392.433391	445692.041365	51.486657
3391.912751	445312.206839	51.491661
3390.880201	445000.006424	51.496666
3390.261788	444665.656365	51.501671
3389.664347	444305.207906	51.506676
3389.009572	443930.854767	51.511681
3388.138573	443602.570370	51.516685
3387.337610	443285.336508	51.521690
3386.791057	442921.509073	51.526695
3386.340511	442558.980850	51.531700
3385.636119	442219.534227	51.536705
3384.708012	441914.841279	51.541709
3383.784614	441587.908591	51.546714
3383.137259	441227.574616	51.551719
3382.529349	440869.209016	51.556724
3382.011034	440519.962179	51.561729
3381.257656	440234.004693	51.566733
3380.691197	439904.810146	51.571738
3379.920840	439538.784810	51.576743
3379.052251	439198.789352	51.581748
3378.654590	438834.928592	51.586753
3378.176177	438519.105270	51.591757
3377.407061	438214.214561	51.596762
3376.676791	437831.580641	51.601767
3375.745644	437534.145508	51.606772
3375.073460	437184.444576	51.611777
3374.291260	436837.066440	51.616781
3373.692278	436486.684168	51.621786
3373.104403	436193.164807	51.626791
3372.237416	435864.066160	51.631796
3370.917697	435525.031635	51.636801
3370.588167	435175.147175	51.641805
3370.210799	434836.030630	51.646810
3369.491120	434555.207947	51.651815
3368.302998	434227.179906	51.656820
3367.935396	433868.244692	51.661825
3367.139501	433588.312132	51.666829
3366.516647	433236.390914	51.671834
3365.990856	432906.184607	51.676839
3365.388793	432622.275242	51.681844
3364.526979	432267.814059	51.686849
3364.417984	431930.191104	51.691853
3363.072861	431629.807156	51.696858
3362.501687	431276.454566	51.701863
3361.868462	430984.381093	51.706868
3361.270542	430648.266282	51.711873
3360.517106	430315.422181	51.716877
3359.705837	430013.538595	51.721882
3359.477318	429666.230140	51.726887
3358.272682	429378.520859	51.731892
3358.025168	429022.217170	51.736897
3357.192813	428723.979091	51.741901
3356.296086	428371.527855	51.746906
3355.651404	428064.135604	51.751911
3354.896864	427766.407810	51.756916
3354.172706	427413.840444	51.761921
3353.769977	427118.945041	51.766925
3352.897264	426801.313958	51.771930
3352.433503	426478.001589	51.776935
3351.547267	426152.542533	51.781940
3350.870424	425837.891478	51.786945
3350.392384	425529.935931	51.791949
3349.363726	425211.879049	51.796954
3348.848676	424892.010090	51.801959
3347.993207	424569.727470	51.806964
3347.611701	424282.392238	51.811969
3346.660268	423940.559639	51.816973
3346.060801	423657.951320	51.821978
3345.543730	423312.841791	51.826983
3344.945871	423030.328374	51.831988
3344.336836	422678.494236	51.836993
3343.525248	422385.491956	51.841997
3342.657138	422055.993299	51.847002
3342.005607	421747.794158	51.852007
3340.864209	421441.396427	51.857012
3340.471656	421133.073330	51.862017
3340.228622	420815.425757	51.867021
3339.139919	420519.882004	51.872026
3338.535286	420208.660922	51.877031
3338.288922	419882.848847	51.882036
3337.591481	419568.078854	51.887041
3336.662965	419274.783067	51.892045
3335.771872	418936.131292	51.897050
3335.441254	418647.332685	51.902055
3334.750279	418317.762213	51.907060
3334.245190	418027.638448	51.912065
3333.992377	417678.886499	51.917069
3332.662022	417386.955919	51.922074
3332.449834	417062.909986	51.927079
3331.357526	416737.703860	51.932084
3330.582519	416442.957388	51.937089
3329.712314	416138.847785	51.942093
3329.433787	415812.714945	51.947098
3328.461329	415516.237170	51.952103
3327.758561	415192.654405	51.957108
3327.051308	414901.057547	51.962113
3326.758999	414584.491986	51.967117
3325.889499	414276.221271	51.972122
3325.408269	413970.172716	51.977127
3324.548118	413666.010363	51.982132
3323.696991	413346.928121	51.987137
3323.116766	413038.547893	51.992141
3322.604269	412737.090660	51.997146
3322.316043	412424.439821	52.002151
3321.030324	412123.022415	52.007156
3320.484475	411801.613763	52.012161
3319.867344	411494.417684	52.017165
3319.067968	411199.597148	52.022170
3318.779711	410882.610287	52.027175
3318.148622	410575.178315	52.032180
3317.111911	410261.657646	52.037185
3316.442093	409957.529080	52.042189
3315.887533	409657.546895	52.047194
3315.171209	409337.028372	52.052199
3314.410938	409032.117055	52.057204
3313.807692	408731.015272	52.062209
3313.232779	408426.017770	52.067213
3312.495687	408120.000919	52.072218
3312.059303	407805.292678	52.077223
3311.048688	407493.874246	52.082228
3310.462324	407182.334751	52.087233
3309.659277	406883.127176	52.092237
3308.890335	406581.979777	52.097242
3308.471064	406275.360697	52.102247
3307.401108	405981.523885	52.107252
3306.769254	405670.967660	52.112257
3306.698431	405366.394073	52.117261
3305.752737	405073.139075	52.122266
3304.794881	404764.963752	52.127271
3304.477585	404454.930353	52.132276
3303.873575	404150.683516	52.137281
3303.269925	403850.932565	52.142285
3302.161490	403553.800374	52.147290
3301.679040	403229.038955	52.152295
3300.697147	402938.464225	52.157300
3300.144659	402641.159363	52.162305
3299.515386	402338.729356	52.167309
3298.638862	402042.105662	52.172314
3298.220534	401733.510696	52.177319
3297.873010	401436.594423	52.182324
3296.853827	401143.416637	52.187329
3296.130024	400829.421616	52.192333
3295.321807	400540.119655	52.197338
3294.882847	400245.189720	52.202343
3293.959241	399958.290350	52.207348
3293.326453	399640.481877	52.212353
3292.920486	399341.522143	52.217357
3292.368789	399051.276750	52.222362
3291.803221	398740.516021	52.227367
3290.993880	398439.756171	52.232372
3290.409331	398137.000569	52.237377
3289.648782	397840.371326	52.242381
3288.767516	397537.225030	52.247386
3288.464730	397239.297785	52.252391
3287.753260	396931.263463	52.257396
3286.368545	396640.162760	52.262401
3286.048883	396346.425050	52.267405
3285.647219	396046.036841	52.272410
3284.847693	395738.666566	52.277415
3283.880907	395451.887813	52.282420
3283.081571	395146.139273	52.287425
3282.590194	394852.695466	52.292429
3281.614338	394562.071609	52.297434
3281.487892	394270.751600	52.302439
3280.622129	393971.918594	52.307444
3280.119944	393677.881686	52.312449
3279.464689	393374.128589	52.317453
3278.939627	393083.929476	52.322458
3278.182644	392786.442004	52.327463
3277.377328	392485.425425	52.332468
3277.065226	392183.438325	52.337473
3276.451009	391891.794099	52.342477
3275.171396	391600.252693	52.347482
3274.887980	391301.380940	52.352487
3273.875855	390992.832498	52.357492
3273.329188	390698.294451	52.362497
3272.410005	390406.889602	52.367501
3271.759790	390118.236867	52.372506
3271.308208	389818.082399	52.377511
3270.491876	389538.249298	52.382516
3269.703973	389236.744603	52.387521
3269.317082	388944.302788	52.392525
3268.386857	388658.988291	52.397530
3267.966176	388350.425197	52.402535
3267.348995	388067.141688	52.407540
3266.482898	387770.265217	52.412545
3265.896519	387478.707714	52.417549
3265.128352	387192.033716	52.422554
3264.676401	386902.561022	52.427559
3264.016251	386612.686663	52.432564
3263.346778	386319.327537	52.437569
3262.963298	386023.021759	52.442573
3261.742325	385734.119269	52.447578
3261.334624	385427.335086	52.452583
3260.439221	385135.935073	52.457588
3259.757052	384850.526283	52.462593
3259.242334	384551.126908	52.467597
3259.012796	384271.389639	52.472602
3258.189632	383965.574718	52.477607
3257.090469	383679.688911	52.482612
3256.457807	383388.513523	52.487617
3255.769818	383097.497243	52.492621
3255.025900	382811.955617	52.497626
3254.618586	382516.592368	52.502631
3253.993521	382232.807912	52.507636
3253.106409	381933.980855	52.512641
3252.515743	381645.277982	52.517645
3251.702876	381361.694830	52.522650
3251.374750	381059.618793	52.527655
3250.014976	380782.425503	52.532660
3249.749063	380488.016261	52.537665
3249.450867	380195.339442	52.542669
3248.722537	379910.791249	52.547674
3248.171139	379620.515601	52.552679
3247.617809	379317.444302	52.557684
3246.879269	379020.707901	52.562689
3246.215950	378735.199816	52.567693
3245.392583	378447.476659	52.572698
3244.736951	378140.902419	52.577703
3244.057595	377847.632581	52.582708
3243.306764	377555.720013	52.587713
3242.794454	377261.630937	52.592717
3242.087858	376968.765958	52.597722
3241.386089	376682.435319	52.602727
3240.861404	376381.321250	52.607732
3240.132663	376084.917644	52.612737
3239.350738	375801.162604	52.617741
3238.793653	375499.462074	52.622746
3237.989164	375202.733352	52.627751
3237.048715	374916.377175	52.632756
3236.569006	374636.483683	52.637761
3236.070263	374336.367975	52.642765
3235.116927	374048.176265	52.647770
3234.616907	373756.298578	52.652775
3233.848231	373469.523642	52.657780
3233.040729	373176.164213	52.662785
3232.611640	372886.914872	52.667789
3231.965603	372599.911069	52.672794
3231.499236	372306.135453	52.677799
3230.787508	372019.290731	52.682804
3229.605135	371716.516921	52.687809
3229.379609	371432.745853	52.692813
3228.448836	371149.466060	52.697818
3228.091613	370852.635769	52.702823
3227.025906	370564.361722	52.707828
3226.138811	370275.319712	52.712833
3225.856030	369983.966825	52.717837
3225.346119	369703.383983	52.722842
3224.770624	369421.537650	52.727847
3224.002829	369125.371039	52.732852
3223.222035	368843.248152	52.737857
3222.999425	368531.192145	52.742861
3221.833810	368261.033067	52.747866
3221.648910	367957.261048	52.752871
3220.721325	367679.326408	52.757876
3220.328760	367371.945009	52.762881
3219.386287	367076.962629	52.767885
3218.092065	366802.973215	52.772890
3217.696480	366502.074176	52.777895
3217.169857	366217.324679	52.782900
3216.165657	365934.150077	52.787905
3216.154206	365643.081908	52.792909
3215.184231	365357.124973	52.797914
3214.759025	365065.278928	52.802919
3214.123817	364772.751817	52.807924
3213.289746	364475.877947	52.812929
3212.779617	364186.304252	52.817933
3212.041763	363912.845516	52.822938
3211.619262	363613.153014	52.827943
3210.668594	363323.796285	52.832948
3209.859913	363020.573380	52.837953
3209.392011	362734.342661	52.842957
3208.609900	362448.109014	52.847962
3207.942520	362161.626471	52.852967
3207.358167	361864.442018	52.857972
3206.826225	361575.898878	52.862977
3206.483658	361283.430847	52.867981
3205.269270	360994.381453	52.872986
3204.764064	360698.678514	52.877991
3204.140529	360402.407215	52.882996
3203.622522	360107.873195	52.888001
3202.808027	359819.211517	52.893005
3201.908758	359539.518725	52.898010
3201.370184	359229.002188	52.903015
3200.883668	358957.841760	52.908020
3200.157827	358654.374542	52.913025
3199.521203	358350.942234	52.918029
3198.739264	358083.437228	52.923034
3198.094214	357778.323224	52.928039
3197.564322	357491.791343	52.933044
3196.669115	357207.275091	52.938049
3196.034758	356911.137159	52.943053
3195.148620	356626.107223	52.948058
3194.624067	356330.253885	52.953063
3193.663816	356055.666222	52.958068
3193.346925	355764.001157	52.963073
3192.909997	355461.792233	52.968077
3192.078682	355181.148142	52.973082
3191.263549	354899.889186	52.978087
3190.749867	354597.661879	52.983092
3189.908959	354317.116405	52.988097
3189.491370	354012.045625	52.993101
3188.912180	353749.982816	52.998106
3188.018983	353443.049801	53.003111
3187.109998	353154.390427	53.008116
3186.512848	352864.229496	53.013121
3186.060580	352579.032263	53.018125
3185.222664	352304.074584	53.023130
3184.773307	352015.107247	53.028135
3183.898593	351721.726367	53.033140
3183.161659	351430.867148	53.038145
3182.861788	351142.405935	53.043149
3182.009519	350860.316944	53.048154
3181.170926	350568.832910	53.053159
3180.435537	350293.899675	53.058164
3179.724488	350002.214287	53.063169
3179.931212	349706.997118	53.068173
3178.729466	349428.824662	53.073178
3177.989255	349126.016948	53.078183
3177.339382	348845.412709	53.083188
3176.265433	348559.758319	53.088193
3175.811071	348275.302505	53.093197
3174.996817	347993.549219	53.098202
3174.466920	347706.608178	53.103207
3173.915343	347433.031640	53.108212
3173.468580	347149.027116	53.113217
3173.164270	346845.349177	53.118221
3172.242550	346562.994962	53.123226
3171.377433	346267.191262	53.128231
3170.982579	345970.573510	53.133236
3170.221436	345687.629659	53.138241
3169.531283	345391.437481	53.143245
3168.576085	345105.161679	53.148250
3168.233425	344822.529249	53.153255
3167.687496	344527.251692	53.158260
3166.660095	344245.412098	53.163265
3166.194072	343945.384605	53.168269
3165.540815	343662.490365	53.173274
3164.854980	343375.527281	53.178279
3163.997832	343074.666435	53.183284
3163.340760	342793.805079	53.188289
3162.676889	342504.390778	53.193293
3162.004866	342222.307342	53.198298
3161.570358	341937.435918	53.203303
3161.001609	341644.107938	53.208308
3160.069912	341351.268732	53.213313
3159.656960	341066.440809	53.218317
3158.977923	340772.387978	53.223322
3158.151486	340486.681000	53.228327
3157.717146	340196.557804	53.233332
3156.943774	339905.901444	53.238337
3155.952825	339620.547517	53.243341
3155.290034	339332.722094	53.248346
3154.866473	339043.890205	53.253351
3154.256846	338746.558684	53.258356
3153.332633	338473.280748	53.263361
3153.040002	338180.325857	53.268365
3152.369915	337894.786277	53.273370
3151.478739	337602.279900	53.278375
3150.933031	337311.855924	53.283380
3149.957300	337026.793717	53.288385
3149.351305	336726.524973	53.293389
3148.717167	336440.617059	53.298394
3148.208997	336144.887033	53.303399
3147.322952	335863.522434	53.308404
3146.790501	335581.337006	53.313409
3146.465431	335279.744534	53.318413
3145.596434	334993.944074	53.323418
3144.598455	334703.071321	53.328423
3144.292476	334418.452280	53.333428
3143.346427	334141.316117	53.338433
3142.992399	333845.908240	53.343437
3142.223174	333570.523900	53.348442
3141.705949	333269.716877	53.353447
3140.923814	332987.509541	53.358452
3139.963170	332695.451508	53.363457
3139.411191	332397.039394	53.368461
3138.970194	332125.950944	53.373466
3138.276943	331828.526264	53.378471
3137.618192	331547.974048	53.383476
3137.066059	331252.332265	53.388481
3136.545423	330959.255664	53.393485
3135.610414	330675.561474	53.398490
3134.996095	330378.627635	53.403495
3134.258578	330092.379527	53.408500
3133.382624	329805.974021	53.413505
3133.143360	329505.820439	53.418509
3132.370756	329220.592964	53.423514
3131.255701	328936.360617	53.428519
3130.808435	328637.127627	53.433524
3130.168784	328357.884407	53.438529
3129.381512	328069.778040	53.443533
3128.955817	327790.040654	53.448538
3128.426585	327488.066548	53.453543
3127.697118	327204.785281	53.458548
3126.678579	326920.199353	53.463553
3126.129998	326612.369123	53.468557
3125.614788	326346.363956	53.473562
3124.842366	326049.642292	53.478567
3124.388973	325767.916294	53.483572
3123.557736	325471.711047	53.488577
3123.027156	325178.741603	53.493581
3122.193858	324906.416887	53.498586
3121.288056	324614.497800	53.503591
3120.979025	324326.480653	53.508596
3120.118406	324047.817663	53.513601
3119.585623	323763.245796	53.518605
3119.093316	323466.368756	53.523610
3118.115528	323189.300102	53.528615
3117.590687	322893.342844	53.533620
3116.900667	322616.405051	53.538625
3116.322228	322314.318066	53.543629
3115.362455	322045.186960	53.548634
3114.845449	321741.153198	53.553639
3114.212967	321465.042924	53.558644
3113.366871	321175.776292	53.563649
3113.158530	320891.092835	53.568653
3112.149567	320607.935592	53.573658
3111.406415	320313.532029	53.578663
3110.747640	320043.990844	53.583668
3109.971686	319757.203923	53.588673
3109.973491	319469.580094	53.593677
3109.012439	319194.940866	53.598682
3108.284352	318895.972639	53.603687
3107.816112	318599.177607	53.608692
3106.774156	318318.335746	53.613697
3106.387601	318027.229678	53.618701
3105.797443	317743.004479	53.623706
3105.104918	317458.056224	53.628711
3104.487422	317164.998013	53.633716
3103.622708	316877.681799	53.638721
3103.335370	316589.585882	53.643725
3102.628654	316290.351654	53.648730
3102.075857	316005.478984	53.653735
3101.425941	315715.706442	53.658740
3100.331318	315429.313711	53.663745
3099.849958	315128.588996	53.668749
3098.999363	314844.447753	53.673754
3098.515599	314556.173495	53.678759
3097.919067	314250.269886	53.683764
3096.782185	313971.417139	53.688769
3096.478632	313680.285500	53.693773
3095.740975	313399.738404	53.698778
3095.065945	313105.990289	53.703783
3094.350960	312806.187246	53.708788
3093.619940	312527.546678	53.713793
3093.209127	312234.340110	53.718797
3092.344927	311953.936690	53.723802
3091.695249	311658.882066	53.728807
3091.199413	311381.423738	53.733812
3090.239043	311092.833865	53.738817
3089.964428	310796.851882	53.743821
3088.977212	310512.517405	53.748826
3088.254475	310228.929793	53.753831
3088.021317	309935.485557	53.758836
3087.220100	309651.450627	53.763841
3086.659616	309360.781527	53.768845
3085.772431	309073.830388	53.773850
3085.093664	308770.777174	53.778855
3084.534070	308484.434914	53.783860
3083.858965	308209.773308	53.788865
3083.581712	307900.237234	53.793869
3082.581878	307615.643377	53.798874
3081.703295	307322.626151	53.803879
3081.333256	307025.529724	53.808884
3080.477273	306732.838647	53.813889
3079.911010	306446.594768	53.818893
3079.339473	306162.693939	53.823898
3078.530780	305864.340128	53.828903
3077.667181	305580.713490	53.833908
3076.856251	305295.193471	53.838913
3076.555756	305007.096442	53.843917
3075.678812	304717.332908	53.848922
3074.991869	304444.371634	53.853927
3074.580279	304140.552531	53.858932
3073.712168	303863.187758	53.863937
3072.844665	303581.773269	53.868941
3072.266211	303282.664530	53.873946
3071.483021	302994.130555	53.878951
3071.319437	302703.409744	53.883956
3070.210428	302434.917187	53.888961
3069.790993	302139.881078	53.893965
3069.418576	301854.641487	53.898970
3068.534171	301568.743882	53.903975
3068.005958	301274.589219	53.908980
3067.287196	300985.226395	53.913985
3066.763211	300695.985028	53.918989
3065.686505	300403.749180	53.923994
3065.113011	300121.696201	53.928999
3064.706694	299833.835374	53.934004
3063.642954	299546.485572	53.939009
3063.371421	299255.419112	53.944013
3062.631183	298966.616484	53.949018
3061.975115	298674.030982	53.954023
3061.202926	298385.920070	53.959028
3060.622034	298109.467708	53.964033
3059.943947	297810.695854	53.969037
3059.422496	297530.871590	53.974042
3058.875369	297229.658724	53.979047
3058.186444	296937.279408	53.984052
3056.907266	296652.989720	53.989057
3056.675740	296373.576294	53.994061
3056.122592	296070.834566	53.999066
3055.120401	295791.491365	54.004071
3054.727087	295500.336513	54.009076
3054.137239	295206.742037	54.014081
3053.632216	294903.965515	54.019085
3052.645513	294629.457092	54.024090
3051.775288	294327.959992	54.029095
3051.530561	294049.105837	54.034100
3050.165168	293765.564429	54.039105
3049.647810	293468.951001	54.044109
3049.475286	293188.734593	54.049114
3048.585181	292892.281298	54.054119
3048.029788	292609.348847	54.059124
3047.465633	292322.113439	54.064129
3046.817677	292025.569830	54.069133
3045.767027	291741.288590	54.074138
3045.539092	291456.494808	54.079143
3044.819700	291146.998468	54.084148
3043.718557	290880.220567	54.089153
3042.965095	290584.685264	54.094157
3043.086492	290284.961810	54.099162
3041.820801	290008.786050	54.104167
3041.465534	289709.697726	54.109172
3040.429931	289432.848309	54.114177
3040.072670	289136.790395	54.119181
3039.423910	288854.734722	54.124186
3038.715942	288560.030626	54.129191
3038.587202	288264.394143	54.134196
3037.528645	287973.386916	54.139201
3037.002362	287677.227070	54.144205
3036.524613	287384.777612	54.149210
3035.577712	287086.646401	54.154215
3034.803615	286799.871799	54.159220
3034.013748	286504.975168	54.164225
3033.210377	286206.056495	54.169229
3032.591996	285932.678263	54.174234
3031.925543	285638.576429	54.179239
3031.419946	285350.688614	54.184244
3030.298842	285067.278545	54.189249
3029.782782	284789.604734	54.194253
3029.411339	284483.714615	54.199258
3028.463151	284210.871400	54.204263
3028.047165	283919.734043	54.209268
3027.518423	283638.063068	54.214273
3026.803744	283348.016861	54.219277
3026.010741	283055.461542	54.224282
3025.466239	282776.339439	54.229287
3024.923092	282474.448370	54.234292
3024.441566	282184.059056	54.239297
3023.590058	281899.178384	54.244301
3022.678835	281613.110034	54.249306
3021.890346	281309.372611	54.254311
3021.398579	281031.387495	54.259316
3020.765273	280733.024563	54.264321
3020.247248	280448.370704	54.269325
3019.413871	280168.096286	54.274330
3018.340925	279879.735303	54.279335
3018.244674	279580.166381	54.284340
3017.327379	279300.236094	54.289345
3016.823856	279003.685814	54.294349
3016.464738	278731.333024	54.299354
3015.579766	278428.195750	54.304359
3015.070394	278138.013307	54.309364
3014.131092	277856.940143	54.314369
3013.471571	277563.215805	54.319373
3012.748317	277271.258837	54.324378
3011.815745	276994.463194	54.329383
3011.578118	276697.539375	54.334388
3010.765484	276414.204800	54.339393
3010.045446	276115.523586	54.344397
3009.401552	275820.141204	54.349402
3008.653798	275537.101964	54.354407
3008.273485	275241.041157	54.359412
3007.392969	274951.986941	54.364417
3006.784345	274662.838770	54.369421
3006.126084	274364.147835	54.374426
3005.273653	274092.840709	54.379431
3005.091508	273794.762123	54.384436
3004.230110	273497.504215	54.389441
3003.482162	273227.377682	54.394445
3002.863466	272929.673965	54.399450
3002.300850	272648.082906	54.404455
3001.561878	272348.055267	54.409460
3000.559001	272071.220208	54.414465
3000.354337	271763.340303	54.419469
2999.736323	271492.887966	54.424474
2998.849337	271207.477439	54.429479
2998.195798	270899.210441	54.434484
2997.542779	270614.017761	54.439489
2996.940162	270325.913821	54.444493
2996.118206	270031.783260	54.449498
2995.860698	269745.611449	54.454503
2995.359564	269453.798901	54.459508
2994.749377	269163.379034	54.464513
2994.152557	268854.594588	54.469517
2993.371507	268561.298680	54.474522
2992.176334	268277.771869	54.479527
2992.203317	267966.724367	54.484532
2991.190361	267680.825958	54.489537
2990.455057	267391.700239	54.494541
2989.748005	267094.929775	54.499546
2989.357479	266805.698899	54.504551
2988.735393	266507.005254	54.509556
2988.032972	266212.654107	54.514561
2987.645862	265906.334187	54.519565
2986.752581	265613.057866	54.524570
2985.836832	265313.036285	54.529575
2985.257068	265019.303289	54.534580
2984.389539	264730.353123	54.539585
2983.535958	264423.420578	54.544589
2983.091109	264129.921614	54.549594
2982.566303	263850.239181	54.554599
2982.105842	263550.274324	54.559604
2981.000699	263271.142661	54.564609
2980.577388	262963.863171	54.569613
2979.923203	262664.311817	54.574618
2979.039725	262377.632835	54.579623
2978.506272	262084.098810	54.584628
2978.090826	261791.284960	54.589633
2977.373601	261493.756707	54.594637
2976.818585	261203.410453	54.599642
2975.952172	260905.982840	54.604647
2975.563603	260598.827659	54.609652
2974.232765	260320.956976	54.614657
2973.746563	260021.152600	54.619661
2973.077362	259718.066754	54.624666
2972.583260	259430.870773	54.629671
2971.868448	259134.770962	54.634676
2971.510758	258836.093692	54.639681
2970.942414	258546.542025	54.644685
2970.320776	258252.389544	54.649690
2969.563706	257953.190863	54.654695
2969.108652	257651.423494	54.659700
2968.128706	257358.551319	54.664705
2967.323106	257048.181369	54.669709
2966.579971	256747.988875	54.674714
2965.597630	256465.687194	54.679719
2965.524719	256174.888683	54.684724
2964.594009	255872.740689	54.689729
2964.153597	255588.367971	54.694733
2963.740262	255291.843569	54.699738
2963.170060	254990.123700	54.704743
2962.732113	254671.906210	54.709748
2961.747671	254380.923535	54.714753
2961.037751	254066.875752	54.719757
2960.282015	253763.888370	54.724762
2959.610841	253467.713209	54.729767
2958.996359	253157.191749	54.734772
2957.936021	252874.576564	54.739777
2957.393935	252569.851081	54.744781
2956.788847	252278.378765	54.749786
2955.885232	251977.353283	54.754791
2955.624621	251673.527077	54.759796
2954.533484	251385.545749	54.764801
2953.969695	251079.221961	54.769805
2953.223869	250787.035967	54.774810
2952.693114	250504.722874	54.779815
2951.783098	250195.883451	54.784820
2951.323385	249907.601038	54.789825
2951.022956	249616.441715	54.794829
2950.105230	249318.683051	54.799834
2949.313138	249026.991484	54.804839
2949.106922	248714.834838	54.809844
2948.188538	248430.651447	54.814849
2947.212904	248118.388659	54.819853
2947.040437	247826.015614	54.824858
2946.397505	247536.773545	54.829863
2945.796352	247234.435995	54.834868
2945.007016	246933.605894	54.839873
2944.478429	246635.536382	54.844877
2944.060566	246335.361790	54.849882
2943.134522	246033.995021	54.854887
2942.703730	245719.537600	54.859892
2941.776226	245417.892302	54.864897
2941.256518	245118.322218	54.869901
2940.591095	244816.789576	54.874906
2939.892186	244512.665462	54.879911
2939.152663	244204.830556	54.884916
2938.169506	243907.246508	54.889921
2937.992779	243601.921396	54.894925
2936.789340	243307.454909	54.899930
2936.323501	243005.996775	54.904935
2935.610730	242689.044831	54.909940
2934.704581	242407.851587	54.914945
2934.188356	242104.952131	54.919949
2933.659430	241801.851726	54.924954
2932.943891	241507.948930	54.929959
2932.365918	241213.923222	54.934964
2931.490413	240906.423652	54.939969
2931.050511	240606.495282	54.944973
2930.257034	240310.876232	54.949978
2929.627323	240015.588516	54.954983
2929.108104	239713.510558	54.959988
2928.327930	239422.857248	54.964993
2927.645809	239123.556804	54.969997
2927.172821	238826.108399	54.975002
2926.491590	238522.964352	54.980007
2926.027068	238220.856321	54.985012
2925.166442	237934.192050	54.990017
2924.677807	237618.440858	54.995021
2923.373604	237319.422104	55.000026
2922.932556	237023.806987	55.005031
2922.514611	236713.267355	55.010036
2921.936040	236418.999825	55.015041
2920.976968	236122.832685	55.020045
2920.339177	235822.948800	55.025050
2919.884978	235518.427865	55.030055
2919.127014	235218.080986	55.035060
2918.459641	234922.889686	55.040065
2917.769689	234626.786162	55.045069
2917.123045	234312.750695	55.050074
2916.263378	234025.384200	55.055079
2915.959972	233722.652753	55.060084
2915.119782	233427.747928	55.065089
2914.242266	233119.150977	55.070093
2913.672111	232827.897333	55.075098
2912.815580	232530.808075	55.080103
2912.507624	232230.602861	55.085108
2911.545399	231940.610770	55.090113
2911.355764	231630.509343	55.095117
2910.519855	231340.473666	55.100122
2909.557880	231046.996014	55.105127
2909.524614	230735.217811	55.110132
2908.580687	230436.366779	55.115137
2907.919244	230139.839969	55.120141
2907.274656	229837.226101	55.125146
2906.503826	229523.913871	55.130151
2906.137757	229223.982404	55.135156
2905.121906	228933.168233	55.140161
2904.641694	228621.773751	55.145165
2904.035442	228326.975692	55.150170
2903.081740	228033.608568	55.155175
2902.374805	227730.171670	55.160180
2901.514674	227426.149046	55.165185
2901.207229	227132.771821	55.170189
2900.383322	226824.060813	55.175194
2899.762615	226532.390254	55.180199
2899.161932	226222.933231	55.185204
2898.318248	225942.961074	55.190209
2897.991300	225637.129248	55.195213
2897.256752	225332.941658	55.200218
2896.523128	225042.414546	55.205223
2895.719998	224746.820167	55.210228
2895.140104	224439.148874	55.215233
2894.509691	224141.543498	55.220237
2893.758511	223841.272338	55.225242
2893.145336	223553.315785	55.230247
2892.880199	223239.794483	55.235252
2891.945832	222950.541648	55.240257
2891.341598	222644.039673	55.245261
2890.869352	222339.516591	55.250266
2889.806845	222043.120621	55.255271
2889.426696	221750.220251	55.260276
2888.809745	221439.180657	55.265281
2888.370137	221131.640351	55.270285
2887.743633	220821.915975	55.275290
2886.865329	220524.312994	55.280295
2886.277336	220210.817164	55.285300
2885.394464	219917.647182	55.290305
2884.830568	219607.166971	55.295309
2884.068117	219292.111550	55.300314
2883.157558	219007.681869	55.305319
2882.727024	218695.847894	55.310324
2882.112516	218390.587146	55.315329
2881.177946	218098.667470	55.320333
2880.534060	217810.967170	55.325338
2879.643585	217507.446883	55.330343
2879.360196	217189.053595	55.335348
2878.513110	216906.353436	55.340353
2878.003080	216600.243830	55.345357
2877.406580	216300.984574	55.350362
2876.652922	215999.040314	55.355367
2876.106287	215706.394646	55.360372
2875.304673	215409.399278	55.365377
2874.495101	215091.862752	55.370381
2874.074462	214805.870741	55.375386
2873.313925	214508.745562	55.380391
2872.982853	214199.932782	55.385396
2871.851405	213904.192783	55.390401
2871.143589	213607.483330	55.395405
2870.760805	213306.803490	55.400410
2870.049369	213009.320906	55.405415
2869.636402	212707.350351	55.410420
2868.744286	212415.881256	55.415425
2868.468591	212114.120842	55.420429
2867.462589	211814.628494	55.425434
2866.565940	211509.990953	55.430439
2866.286141	211195.024130	55.435444
2865.259610	210898.453998	55.440449
2864.797502	210591.970204	55.445453
2864.323036	210282.269808	55.450458
2863.691598	209982.166846	55.455463
2862.995980	209678.359104	55.460468
2862.397819	209379.895626	55.465473
2861.760953	209072.988828	55.470477
2861.164659	208758.542649	55.475482
2860.272333	208471.902837	55.480487
2859.704400	208150.239033	55.485492
2858.932129	207847.877976	55.490497
2858.025610	207550.795924	55.495501
2857.999829	207244.768882	55.500506
2857.185420	206941.693648	55.505511
2856.614438	206624.683818	55.510516
2855.705780	206317.083267	55.515521
2855.249388	206010.176303	55.520525
2854.622409	205704.672430	55.525530
2853.786869	205399.801332	55.530535
2853.056295	205076.347396	55.535540
2852.705884	204778.796785	55.540545
2851.892942	204480.468302	55.545549
2851.351929	204156.976796	55.550554
2850.505507	203862.996474	55.555559
2849.868112	203546.993942	55.560564
2849.096283	203242.836910	55.565569
2848.656760	202931.744176	55.570573
2848.063661	202622.000978	55.575578
2847.057906	202306.789138	55.580583
2846.713555	202005.116302	55.585588
2846.027416	201695.927485	55.590593
2845.246973	201391.705583	55.595597
2844.570206	201069.589633	55.600602
2843.733794	200766.805325	55.605607
2843.078241	200453.941036	55.610612
2842.518452	200150.836400	55.615617
2841.917249	199837.763467	55.620621
2841.433797	199526.213452	55.625626
2840.260520	199230.464489	55.630631
2839.841335	198924.366857	55.635636
2839.466266	198617.882257	55.640641
2838.488703	198312.754608	55.645645
2837.913032	197999.281261	55.650650
2837.145938	197690.611860	55.655655
2836.433176	197384.887788	55.660660
2836.017443	197079.232995	55.665665
2835.452590	196766.948727	55.670669
2834.866348	196456.985572	55.675674
2833.765674	196155.414730	55.680679
2833.671134	195837.043029	55.685684
2832.751598	195524.326248	55.690689
2831.946898	195216.911870	55.695693
2831.494768	194903.755895	55.700698
2830.645771	194592.013452	55.705703
2830.194245	194281.087941	55.710708
2829.065464	193984.573126	55.715713
2828.554201	193666.382912	55.720717
2828.044728	193356.770158	55.725722
2827.087779	193058.197886	55.730727
2826.633280	192745.539336	55.735732
2826.163178	192425.811059	55.740737
2825.382563	192127.750899	55.745741
2824.758544	191817.466211	55.750746
2823.655128	191506.432425	55.755751
2823.358090	191192.791939	55.760756
2822.648342	190893.952039	55.765761
2822.057593	190592.207058	55.770765
2821.878211	190268.922750	55.775770
2820.994298	189967.597105	55.780775
2820.259328	189645.575511	55.785780
2819.532597	189328.631097	55.790785
2818.509213	189016.773888	55.795789
2818.056886	188712.181838	55.800794
2817.744705	188400.839483	55.805799
2817.030874	188088.824928	55.810804
2816.208863	187780.900679	55.815809
2815.364816	187466.888112	55.820813
2815.024258	187144.655896	55.825818
2813.888072	186848.975246	55.830823
2813.290500	186530.083010	55.835828
2812.745286	186218.359738	55.840833
2812.160962	185914.506744	55.845837
2811.619190	185607.608603	55.850842
2810.912207	185297.202155	55.855847
2810.190613	184965.695461	55.860852
2809.685823	184664.204457	55.865857
2808.815441	184357.595874	55.870861
2808.481702	184043.882374	55.875866
2807.505678	183739.419201	55.880871
2806.680845	183422.111514	55.885876
2806.352313	183113.059629	55.890881
2805.532560	182806.873552	55.895885
2805.183787	182486.507846	55.900890
2804.081096	182179.734939	55.905895
2803.712539	181854.886658	55.910900
2803.011055	181551.285633	55.915905
2802.066737	181238.350371	55.920909
2801.845408	180920.443768	55.925914
2801.516396	180622.806925	55.930919
2800.554482	180298.954749	55.935924
2799.982235	179975.679308	55.940929
2798.962923	179664.242935	55.945933
2798.478825	179343.413264	55.950938
2797.548325	179039.065013	55.955943
2796.724262	178710.077143	55.960948
2796.155214	178407.685895	55.965953
2795.275146	178096.518887	55.970957
2794.736295	177785.363753	55.975962
2794.080467	177487.266579	55.980967
2793.416864	177180.905406	55.985972
2792.942160	176867.826424	55.990977
2792.112563	176552.300420	55.995981
2791.251802	176242.645118	56.000986
2790.621812	175936.771201	56.005991
2789.707331	175626.442270	56.010996
2789.086398	175330.046795	56.016001
2788.329529	175030.330087	56.021005
2788.111364	174715.853393	56.026010
2786.976794	174424.467881	56.031015
2786.601624	174120.424173	56.036020
2786.122615	173818.942815	56.041025
2785.162814	173508.421161	56.046029
2784.546595	173206.813547	56.051034
2783.945151	172914.782304	56.056039
2783.708323	172598.532031	56.061044
2782.987431	172311.420436	56.066049
2782.127815	171953.166369	56.071053
2781.567074	171614.529132	56.076058
2780.970154	171309.410296	56.081063
2780.085310	171003.194916	56.086068
2779.823274	170691.325982	56.091073
2778.790017	170381.298492	56.096077
2778.403744	170079.729395	56.101082
2777.443101	169776.244402	56.106087
2776.952762	169462.564924	56.111092
2776.424661	169155.353959	56.116097
2775.621733	168848.519620	56.121101
2775.285128	168536.883441	56.126106
2774.176091	168235.862998	56.131111
2773.711708	167906.068143	56.136116
2772.814500	167601.776604	56.141121
2772.170036	167303.627390	56.146125
2771.562321	166995.543730	56.151130
2770.953230	166691.430101	56.156135
2770.482984	166361.776894	56.161140
2769.715601	166080.110798	56.166145
2768.742169	165762.304383	56.171149
2768.581122	165452.242729	56.176154
2767.294113	165128.413566	56.181159
2766.966760	164830.386541	56.186164
2766.345925	164514.671152	56.191169
2765.682839	164217.872057	56.196173
2765.240420	163902.489708	56.201178
2764.188475	163617.886895	56.206183
2763.820106	163272.390186	56.211188
2762.988197	162998.361239	56.216193
2762.460662	162676.645860	56.221197
2761.932321	162359.917423	56.226202
2761.374436	162052.248841	56.231207
2760.696963	161742.224345	56.236212
2759.808532	161426.705455	56.241217
2759.087122	161118.117291	56.246221
2758.618054	160797.439368	56.251226
2757.691727	160506.166742	56.256231
2757.084914	160184.969513	56.261236
2756.502119	159867.483674	56.266241
2755.781707	159563.689114	56.271245
2755.199130	159255.908895	56.276250
2754.577731	158930.530167	56.281255
2753.692993	158630.176814	56.286260
2753.383854	158319.056230	56.291265
2752.623776	158007.119992	56.296269
2752.206899	157694.496581	56.301274
2751.016684	157382.824809	56.306279
2750.373694	157080.183838	56.311284
2750.104449	156760.007193	56.316289
2748.986355	156447.468080	56.321293
2748.292509	156144.856154	56.326298
2747.828931	155832.244429	56.331303
2747.116020	155522.204695	56.336308
2746.310777	155217.394152	56.341313
2745.533972	154911.475964	56.346317
2745.277744	154600.418998	56.351322
2744.535353	154298.746504	56.356327
2743.620215	153993.862772	56.361332
2743.134680	153681.363469	56.366337
2742.455435	153380.502763	56.371341
2741.615446	153065.764730	56.376346
2741.227064	152758.914971	56.381351
2740.587923	152451.179917	56.386356
2739.891408	152140.813069	56.391361
2739.188757	151837.872895	56.396365
2738.614104	151514.502803	56.401370
2737.604239	151216.065580	56.406375
2737.001243	150899.327966	56.411380
2736.584528	150595.985414	56.416385
2735.802723	150296.516418	56.421389
2735.214046	149982.530750	56.426394
2734.594039	149682.825736	56.431399
2734.091666	149363.354668	56.436404
2733.444740	149056.847576	56.441409
2732.529228	148743.929777	56.446413
2732.477570	148419.872285	56.451418
2731.475935	148116.582190	56.456423
2730.506213	147805.664740	56.461428
2729.903902	147497.360917	56.466433
2729.297882	147184.663573	56.471437
2728.793898	146872.067530	56.476442
2728.112597	146568.855870	56.481447
2727.336723	146254.250308	56.486452
2726.501289	145949.734696	56.491457
2726.232794	145637.342364	56.496461
2725.649166	145325.829074	56.501466
2724.831494	145006.324824	56.506471
2724.097498	144693.443856	56.511476
2723.748560	144382.080742	56.516481
2722.781534	144070.958457	56.521485
2722.150124	143744.829999	56.526490
2721.234502	143449.157557	56.531495
2720.821693	143126.876616	56.536500
2719.937617	142803.466594	56.541505
2719.047781	142505.079962	56.546509
2718.708147	142186.545749	56.551514
2718.158442	141887.590318	56.556519
2717.371197	141574.063449	56.561524
2716.995964	141261.262323	56.566529
2716.136407	140958.998063	56.571533
2715.712465	140632.336399	56.576538
2714.863107	140321.525987	56.581543
2714.529229	140004.322529	56.586548
2713.420255	139686.114455	56.591553
2712.788141	139374.936410	56.596557
2712.423268	139062.753694	56.601562
2711.341188	138755.807955	56.606567
2710.728628	138438.195232	56.611572
2710.074151	138128.367792	56.616577
2709.266758	137823.560696	56.621581
2708.516666	137502.702064	56.626586
2707.814666	137201.035401	56.631591
2707.441961	136889.486700	56.636596
2706.931270	136591.645344	56.641601
2705.937762	136285.219503	56.646605
2705.326351	135969.056133	56.651610
2704.645005	135663.057425	56.656615
2703.954014	135354.776857	56.661620
2703.269548	135047.260736	56.666625
2702.831505	134739.569114	56.671629
2702.243904	134428.690608	56.676634
2701.326591	134123.355346	56.681639
2700.905703	133807.846002	56.686644
2700.168413	133501.510734	56.691649
2699.077937	133193.723115	56.696653
2699.124261	132869.093257	56.701658
2698.116631	132577.304114	56.706663
2697.304337	132270.066723	56.711668
2696.516572	131970.754779	56.716673
2695.882724	131659.888399	56.721677
2695.537584	131345.486753	56.726682
2694.773420	131042.370436	56.731687
2694.365583	130724.048210	56.736692
2694.008921	130411.462443	56.741697
2693.007941	130104.672338	56.746701
2692.574327	129782.846716	56.751706
2691.713044	129477.286080	56.756711
2690.890335	129157.116949	56.761716
2690.483963	128844.747166	56.766721
2689.392087	128543.005421	56.771725
2689.271425	128236.629922	56.776730
2688.237924	127920.966300	56.781735
2687.731123	127603.013069	56.786740
2686.622904	127304.170396	56.791745
2686.064252	126988.416882	56.796749
2685.875321	126672.176658	56.801754
2684.707254	126362.000437	56.806759
2683.994481	126063.172212	56.811764
2683.430502	125752.386577	56.816769
2682.628270	125437.616702	56.821773
2682.236031	125129.566681	56.826778
2681.522294	124820.961583	56.831783
2681.184029	124533.811777	56.836788
2680.827405	124186.211134	56.841793
2679.401385	123885.094685	56.846797
2678.601694	123574.041413	56.851802
2678.287342	123266.330602	56.856807
2677.546564	122954.297491	56.861812
2676.833997	122656.497583	56.866817
2675.869232	122357.712486	56.871821
2675.429335	122041.172945	56.876826
2674.901576	121753.219730	56.881831
2674.139590	121430.796273	56.886836
2673.673685	121119.249154	56.891841
2672.672032	120816.310114	56.896845
2672.152792	120501.706178	56.901850
2671.724532	120200.118132	56.906855
2670.902343	119892.584305	56.911860
2670.439838	119587.809311	56.916865
2669.737209	119276.289943	56.921869
2669.127781	118955.643959	56.926874
2668.231841	118660.990919	56.931879
2667.459465	118355.022654	56.936884
2667.349829	118038.295256	56.941889
2666.256922	117736.016006	56.946893
2665.632348	117425.211202	56.951898
2664.736473	117115.487790	56.956903
2664.224952	116808.043062	56.961908
2663.532668	116502.833190	56.966913
2662.864763	116208.889434	56.971917
2662.338045	115888.186171	56.976922
2661.627458	115583.815361	56.981927
2660.904426	115281.411401	56.986932
2660.367681	114965.278553	56.991937
2659.531788	114659.263147	56.996941
2658.839275	114346.945451	57.001946
2658.311390	114052.458763	57.006951
2657.796465	113744.601178	57.011956
2657.235303	113433.575096	57.016961
2656.251348	113125.367889	57.021965
2655.734243	112812.070541	57.026970
2655.003952	112512.601403	57.031975
2654.500932	112211.773505	57.036980
2653.640926	111892.303762	57.041985
2653.125601	111592.608598	57.046989
2652.067689	111282.614680	57.051994
2651.168237	110984.142740	57.056999
2651.203728	110669.775948	57.062004
2650.624451	110371.869906	57.067009
2649.759962	110065.509489	57.072013
2649.553715	109742.531060	57.077018
2648.475354	109452.317299	57.082023
2647.509802	109138.896596	57.087028
2647.101541	108829.744527	57.092033
2646.489264	108526.809003	57.097037
2645.703362	108219.716957	57.102042
2645.037232	107913.904231	57.107047
2644.460270	107612.554487	57.112052
2643.697759	107303.217906	57.117057
2642.622566	106997.037486	57.122061
2642.435355	106692.192249	57.127066
2641.783492	106370.433422	57.132071
2641.259036	106066.537842	57.137076
2640.571805	105753.948193	57.142081
2640.015138	105449.431123	57.147085
2639.377783	105141.390579	57.152090
2638.501095	104836.151718	57.157095
2638.272807	104522.852068	57.162100
2637.351337	104204.756060	57.167105
2636.391992	103900.880971	57.172109
2635.821665	103582.058903	57.177114
2634.983766	103278.800645	57.182119
2634.320535	102973.101643	57.187124
2633.583565	102660.865269	57.192129
2633.246367	102366.807609	57.197133
2632.692974	102059.282515	57.202138
2631.699114	101753.334673	57.207143
2631.273609	101438.527909	57.212148
2630.492063	101141.308321	57.217153
2629.404266	100832.552040	57.222157
2629.027596	100522.615200	57.227162
2628.738270	100216.753586	57.232167
2627.901333	99919.019320	57.237172
2627.230145	99599.804723	57.242177
2626.777086	99308.639469	57.247181
2626.056153	98992.225678	57.252186
2625.151569	98684.395195	57.257191
2624.395423	98379.431182	57.262196
2623.833368	98065.098073	57.267201
2622.939392	97774.390082	57.272205
2622.306813	97472.443927	57.277210
2621.724724	97160.955136	57.282215
2620.609247	96869.887926	57.287220
2620.410887	96559.526225	57.292225
2619.485138	96261.948892	57.297229
2618.846652	95955.850911	57.302234
2618.348335	95659.501192	57.307239
2617.749071	95362.188416	57.312244
2617.459981	95064.177239	57.317249
2616.322043	94758.415705	57.322253
2615.540544	94453.813079	57.327258
2615.131038	94156.822334	57.332263
2614.405384	93850.208895	57.337268
2614.037064	93542.128972	57.342273
2613.239710	93230.297644	57.347277
2612.572511	92935.868767	57.352282
2611.863890	92637.265372	57.357287
2611.009504	92324.910517	57.362292
2610.856762	92011.174406	57.367297
2609.832654	91723.881816	57.372301
2609.180876	91412.382801	57.377306
2608.582039	91112.020010	57.382311
2607.829600	90814.164765	57.387316
2607.178607	90505.880401	57.392321
2606.549055	90197.647710	57.397325
2606.092349	89884.034591	57.402330
2605.203114	89590.782600	57.407335
2604.619230	89286.575145	57.412340
2603.985628	88985.758971	57.417345
2603.225225	88680.637015	57.422349
2602.607297	88378.609562	57.427354
2602.066653	88070.221828	57.432359
2601.236148	87774.373235	57.437364
2600.815975	87464.884683	57.442369
2599.792165	87156.035093	57.447373
2599.298682	86856.291433	57.452378
2598.101804	86558.837765	57.457383
2597.752045	86262.794372	57.462388
2597.553311	85955.625301	57.467393
2596.775936	85660.038380	57.472397
2595.630275	85358.219528	57.477402
2595.460041	85039.782482	57.482407
2594.538402	84739.483564	57.487412
2594.032847	84445.569221	57.492417
2593.123359	84146.271945	57.497421
2592.664608	83839.631087	57.502426
2591.842088	83539.320851	57.507431
2591.151947	83237.365020	57.512436
2590.515418	82926.747263	57.517441
2589.770630	82626.913108	57.522445
2589.068571	82334.282627	57.527450
2588.605483	82034.247536	57.532455
2587.847499	81730.663691	57.537460
2587.223949	81424.813119	57.542465
2586.362983	81132.788729	57.547469
2585.903812	80832.472471	57.552474
2585.419705	80543.673084	57.557479
2584.744815	80233.697255	57.562484
2584.291767	79927.873421	57.567489
2583.590713	79630.033733	57.572493
2582.719206	79320.882230	57.577498
2582.247122	79017.647718	57.582503
2581.475904	78714.807277	57.587508
2581.027365	78414.689288	57.592513
2579.866051	78106.850325	57.597517
2579.429915	77792.957453	57.602522
2578.427124	77494.518596	57.607527
2577.565359	77201.327215	57.612532
2577.241301	76898.392137	57.617537
2576.830078	76609.319772	57.622541
2575.935136	76307.003557	57.627546
2575.337459	75995.856827	57.632551
2574.590389	75698.423926	57.637556
2574.125304	75402.794411	57.642561
2573.323712	75101.051656	57.647565
2572.633390	74807.722054	57.652570
2572.120240	74501.754781	57.657575
2571.246189	74199.751945	57.662580
2570.570173	73897.278806	57.667585
2569.842924	73595.515226	57.672589
2568.950149	73311.279885	57.677594
2568.540369	73013.833306	57.682599
2567.919954	72709.076095	57.687604
2567.297910	72411.171708	57.692609
2566.311502	72126.879434	57.697613
2565.919405	71822.048968	57.702618
2565.077181	71525.694079	57.707623
2564.172348	71232.907155	57.712628
2563.898871	70938.478934	57.717633
2563.072806	70648.937693	57.722637
2562.402961	70350.343494	57.727642
2561.801152	70068.116505	57.732647
2561.051503	69764.755332	57.737652
2560.724767	69461.616845	57.742657
2559.875563	69172.158063	57.747661
2559.371737	68860.316406	57.752666
2558.646508	68576.268402	57.757671
2557.757442	68287.202746	57.762676
2557.297681	67984.906294	57.767681
2556.724195	67688.585831	57.772685
2555.984702	67397.416566	57.777690
2555.088063	67097.977105	57.782695
2554.811361	66812.870520	57.787700
2554.188785	66501.535209	57.792705
2553.077023	66227.288014	57.797709
2552.793589	65921.129700	57.802714
2552.328801	65606.484522	57.807719
2551.172411	65309.219608	57.812724
2550.763945	65025.559856	57.817729
2550.464671	64710.899971	57.822733
2549.248013	64431.825548	57.827738
2548.779802	64126.776326	57.832743
2547.779903	63823.199797	57.837748
2547.459892	63534.976475	57.842753
2546.684273	63234.881652	57.847757
2546.012869	62951.971925	57.852762
2545.400689	62643.740153	57.857767
2544.302115	62356.541399	57.862772
2543.677138	62067.090775	57.867777
2543.200357	61770.074192	57.872781
2542.647647	61474.308907	57.877786
2541.774922	61183.223861	57.882791
2541.334420	60903.160401	57.887796
2540.581567	60599.913034	57.892801
2539.966582	60315.372073	57.897805
2539.298696	60024.082624	57.902810
2538.858232	59730.852986	57.907815
2537.853739	59444.399213	57.912820
2537.252853	59141.651525	57.917825
2536.316933	58859.487897	57.922829
2535.942649	58561.043675	57.927834
2535.157886	58286.831359	57.932839
2534.096698	57991.929768	57.937844
2533.866814	57707.291665	57.942849
2532.904406	57410.918303	57.947853
2532.507328	57123.904028	57.952858
2531.942588	56838.344960	57.957863
2530.743100	56552.356092	57.962868
2530.593505	56256.745929	57.967873
2529.640627	55975.993022	57.972877
2529.346259	55690.304501	57.977882
2528.649774	55405.582913	57.982887
2527.852523	55114.125492	57.987892
2527.441757	54818.507151	57.992897
2526.424600	54543.295759	57.997901
2525.592697	54248.104675	58.002906
2525.328900	53952.382160	58.007911
2524.377125	53671.914504	58.012916
2523.890567	53384.257960	58.017921
2523.183632	53106.057466	58.022925
2522.577799	52810.961510	58.027930
2521.739427	52530.003131	58.032935
2520.914225	52244.728160	58.037940
2520.162327	51967.172484	58.042945
2519.684623	51688.644270	58.047949
2519.166734	51390.988520	58.052954
2518.789658	51100.655424	58.057959
2517.696385	50835.889871	58.062964
2517.219488	50545.534137	58.067969
2516.433332	50251.793238	58.072973
2516.129353	49969.499443	58.077978
2515.087831	49678.877158	58.082983
2514.251732	49394.576217	58.087988
2513.995944	49114.290834	58.092993
2513.064583	48831.193974	58.097997
2512.267347	48551.170971	58.103002
2511.804575	48273.215628	58.108007
2510.951216	47990.107187	58.113012
2510.532228	47718.957784	58.118017
2509.757736	47420.134313	58.123021
2508.842116	47126.377104	58.128026
2508.687944	46873.430867	58.133031
2507.899470	46567.687489	58.138036
2507.325048	46292.045782	58.143041
2506.642646	46008.122900	58.148045
2505.771224	45723.076979	58.153050
2505.130114	45437.863192	58.158055
2504.075031	45164.842506	58.163060
2503.359860	44888.103474	58.168065
2503.003647	44610.657262	58.173069
2502.327913	44317.930681	58.178074
2501.714044	44052.109329	58.183079
2500.855624	43783.057625	58.188084
2500.665272	43496.210285	58.193089
2499.557904	43228.730951	58.198093
2498.790789	42951.996215	58.203098
2498.352916	42665.805884	58.208103
2497.596575	42399.014238	58.213108
2497.168569	42124.759316	58.218113
2496.020134	41860.811409	58.223117
2495.626551	41583.163514	58.228122
2494.984774	41294.071741	58.233127
2494.347644	41024.196368	58.238132
2493.632768	40747.751242	58.243137
2492.973614	40483.761187	58.248141
2491.969216	40202.265898	58.253146
2491.410583	39931.608020	58.258151
2490.744043	39663.206896	58.263156
2489.983272	39387.595730	58.268161
2489.053300	39121.497615	58.273165
2488.759008	38852.827365	58.278170
2487.862554	38593.458497	58.283175
2486.987363	38323.132490	58.288180
2486.808875	38047.126725	58.293185
2486.099906	37788.069261	58.298189
2485.527207	37525.655786	58.303194
2484.645955	37247.675357	58.308199
2483.684361	36987.070628	58.313204
2483.076568	36718.485570	58.318209
2482.133791	36462.513969	58.323213
2481.559615	36189.879442	58.328218
2480.968706	35936.354184	58.333223
2480.186229	35680.626725	58.338228
2479.898845	35412.168247	58.343233
2479.021808	35159.123686	58.348237
2478.320379	34901.228501	58.353242
2477.790536	34642.696904	58.358247
2477.025076	34381.848749	58.363252
2476.474258	34120.741502	58.368257
2475.913710	33877.505492	58.373261
2474.739521	33604.203921	58.378266
2474.099782	33339.745942	58.383271
2473.341458	33109.371757	58.388276
2472.700018	32845.631470	58.393281
2472.074395	32597.299879	58.398285
2471.277890	32337.944163	58.403290
2470.601036	32091.015707	58.408295
2469.808352	31854.007274	58.413300
2469.363360	31591.962418	58.418305
2468.483891	31356.491813	58.423309
2467.834314	31097.007519	58.428314
2467.229275	30855.652777	58.433319
2466.429282	30623.510808	58.438324
2465.779956	30378.665636	58.443329
2465.152279	30130.392161	58.448333
2464.430713	29884.418782	58.453338
2463.644147	29650.711706	58.458343
2462.615034	29408.990526	58.463348
2462.599378	29167.553039	58.468353
2461.773983	28920.221953	58.473357
2460.584835	28702.946933	58.478362
2460.468697	28451.932207	58.483367
2459.306156	28226.231085	58.488372
2458.791081	27969.238081	58.493377
2457.993348	27750.643634	58.498381
2457.181690	27530.664987	58.503386
2456.645425	27294.550958	58.508391
2455.957909	27067.683317	58.513396
2455.137341	26828.116684	58.518401
2454.372484	26609.735448	58.523405
2453.816192	26386.496045	58.528410
2453.086963	26159.757580	58.533415
2452.076674	25947.152605	58.538420
2451.324418	25710.964925	58.543425
2450.414254	25492.874625	58.548429
2449.931184	25286.176447	58.553434
2449.360368	25079.359013	58.558439
2448.184440	24872.248487	58.563444
2447.372241	24660.703993	58.568449
2446.458252	24467.202716	58.573453
2445.138581	24280.514499	58.578458
2444.588761	24077.533583	58.583463
2443.414224	23902.751080	58.588468
2442.431583	23731.477798	58.593473
2441.448329	23563.019236	58.598477
2440.237174	23400.659984	58.603482
2439.227267	23260.118443	58.608487
2438.061641	23113.768973	58.613492
2437.293716	22973.311632	58.618497
2436.409907	22831.030921	58.623501
2435.574254	22710.125970	58.628506
2434.718417	22583.578610	58.633511
2433.295884	22467.981597	58.638516
2432.596770	22348.871488	58.643521
2431.875141	22250.763598	58.648525
2431.037818	22154.298854	58.653530
2430.276667	22055.494128	58.658535
2429.504663	21965.645612	58.663540
2428.739108	21865.407312	58.668545
2427.333166	21774.119939	58.673549
2426.456991	21704.086426	58.678554
2426.135772	21623.993797	58.683559
2425.132113	21561.611501	58.688564
2424.528540	21479.583362	58.693569
2423.629679	21407.097662	58.698573
2423.373336	21339.280099	58.703578
2422.848906	21266.025871	58.708583
2421.670251	21198.989954	58.713588
2421.407875	21135.323285	58.718593
2421.057107	21065.044295	58.723597
2419.867749	20993.636516	58.728602
2419.366528	20922.715652	58.733607
2418.931923	20867.042170	58.738612
2418.292229	20791.694073	58.743617
2417.716975	20733.017122	58.748621
2417.264578	20664.335871	58.753626
2416.511055	20593.450184	58.758631
2415.949254	20528.143893	58.763636
2415.766491	20448.178593	58.768641
2414.757600	20378.230463	58.773645
2414.039026	20306.256545	58.778650
2414.006348	20221.873059	58.783655
2413.171286	20158.388005	58.788660
2412.637863	20093.827463	58.793665
2411.836866	20022.464774	58.798669
2411.575797	19942.486048	58.803674
2411.198710	19864.037582	58.808679
2410.257640	19796.937234	58.813684
2409.871488	19718.488172	58.818689
2409.068666	19634.301813	58.823693
2408.271227	19560.703715	58.828698
2407.767254	19476.537528	58.833703
2406.751105	19413.934066	58.838708
2406.420378	19327.721388	58.843713
2405.669620	19257.117234	58.848717
2405.051304	19175.087311	58.853722
2404.635076	19099.764425	58.858727
2403.860157	19028.310965	58.863732
2403.321572	18945.402018	58.868737
2402.751555	18865.779355	58.873741
2401.854185	18800.010502	58.878746
2401.249018	18709.952502	58.883751
2400.716631	18635.157484	58.888756
2400.168695	18553.946979	58.893761
2399.239346	18485.448427	58.898765
2398.747460	18408.004351	58.903770
2398.152261	18327.223277	58.908775
2397.066077	18261.558874	58.913780
2396.835457	18163.601200	58.918785
2395.933438	18103.689769	58.923789
2395.346617	18027.721827	58.928794
2394.517428	17949.278512	58.933799
2394.160433	17884.808079	58.938804
2393.374705	17810.469654	58.943809
2392.716419	17732.266355	58.948813
2392.059406	17659.632424	58.953818
2391.133012	17571.132352	58.958823
2390.278119	17507.944835	58.963828
2389.918213	17429.795602	58.968833
2389.201414	17358.468486	58.973837
2388.597056	17295.381627	58.978842
2388.074868	17233.315839	58.983847
2387.137450	17152.195548	58.988852
2386.589090	17078.589052	58.993857
2386.224606	17010.515388	58.998861
2385.673740	16947.579332	59.003866
2385.122887	16864.646741	59.008871
2384.119758	16788.205868	59.013876
2383.542302	16713.742600	59.018881
2383.244659	16633.705187	59.023885
2382.405421	16569.983082	59.028890
2381.645629	16490.802496	59.033895
2380.781913	16417.351375	59.038900
2380.233485	16338.894203	59.043905
2379.493010	16269.803667	59.048909
2378.909750	16189.182022	59.053914
2378.544403	16122.450850	59.058919
2377.537011	16057.542225	59.063924
2376.824686	15975.172592	59.068929
2376.170310	15904.911870	59.073933
2375.344314	15838.680300	59.078938
2374.898099	15778.977320	59.083943
2374.198670	15702.689612	59.088948
2373.643981	15628.144811	59.093953
2372.995583	15564.462017	59.098957
2372.212693	15494.764390	59.103962
2371.920913	15407.135341	59.108967
2370.814786	15339.552189	59.113972
2370.001676	15275.076787	59.118977
2369.815965	15208.442144	59.123981
2368.845737	15133.530967	59.128986
2368.438910	15057.266360	59.133991
2367.867577	14987.997510	59.138996
2367.414969	14906.802702	59.144001
2366.599780	14854.251740	59.149005
2365.743409	14783.563258	59.154010
2365.346102	14699.758327	59.159015
2364.701435	14634.857788	59.164020
2363.885196	14547.710141	59.169025
2363.491292	14492.474728	59.174029
2362.732253	14419.193054	59.179034
2362.189062	14328.551884	59.184039
2361.460466	14270.343391	59.189044
2360.782877	14174.815077	59.194049
2359.853225	14111.576534	59.199053
2359.283763	14038.283491	59.204058
2358.800203	13950.967099	59.209063
2357.882552	13897.660904	59.214068
2357.207075	13827.681570	59.219073
2356.639308	13759.956005	59.224077
2355.830050	13688.530972	59.229082
2355.270310	13604.906656	59.234087
2354.164878	13539.607292	59.239092
2353.822708	13470.961407	59.244097
2353.108359	13406.845379	59.249101
2352.425067	13344.999405	59.254106
2352.111894	13268.635351	59.259111
2351.417351	13204.490400	59.264116
2350.701031	13125.901906	59.269121
2349.955904	13054.132127	59.274125
2349.336289	12983.855142	59.279130
2348.667574	12909.317511	59.284135
2347.579825	12852.270841	59.289140
2347.196415	12781.213391	59.294145
2346.263906	12711.838939	59.299149
2345.633022	12658.664328	59.304154
2345.160527	12589.622886	59.309159
2344.750276	12531.153355	59.314164
2343.985786	12454.439243	59.319169
2343.360574	12390.816020	59.324173
2342.758961	12321.404489	59.329178
2342.338673	12246.317409	59.334183
2341.234293	12191.451579	59.339188
2340.905932	12116.920280	59.344193
2340.150149	12045.777769	59.349197
2339.380458	11969.494813	59.354202
2338.888618	11894.843765	59.359207
2338.005803	11829.544371	59.364212
2337.194121	11751.985361	59.369217
2336.951619	11680.966935	59.374221
2336.105245	11626.019038	59.379226
2335.604926	11561.737200	59.384231
2334.454650	11486.608693	59.389236
2333.712091	11422.328781	59.394241
2333.498620	11359.770164	59.399245
2332.539156	11304.545877	59.404250
2332.325784	11216.247437	59.409255
2331.432602	11156.737008	59.414260
2330.925013	11089.142430	59.419265
2330.221221	11029.199472	59.424269
2329.260362	10958.023792	59.429274
2329.135647	10887.710392	59.434279
2328.107672	10822.736625	59.439284
2327.242716	10759.201688	59.444289
2326.847113	10684.245872	59.449293
2326.188348	10636.009157	59.454298
2325.825905	10561.999045	59.459303
2324.804841	10490.338054	59.464308
2324.313179	10422.371927	59.469313
2323.739686	10359.178664	59.474317
2322.820455	10292.412743	59.479322
2322.244970	10217.266469	59.484327
2321.288773	10153.472812	59.489332
2320.888325	10078.398093	59.494337
2320.508633	10022.432499	59.499341
2319.451013	9954.418996	59.504346
2318.934083	9871.091849	59.509351
2318.358651	9812.122546	59.514356
2317.653952	9734.932888	59.519361
2316.765733	9678.665797	59.524365
2316.429545	9605.487782	59.529370
2315.950092	9535.300863	59.534375
2314.922485	9473.671696	59.539380
2314.275330	9416.674269	59.544385
2313.607718	9335.754619	59.549389
2312.845443	9275.940945	59.554394
2312.153670	9207.300042	59.559399
2311.316330	9148.270357	59.564404
2310.910354	9078.500336	59.569409
2310.730615	9016.073910	59.574413
2309.849777	8945.575522	59.579418
2309.284247	8858.558145	59.584423
2308.318489	8813.139934	59.589428
2307.529077	8745.187603	59.594433
2307.327317	8667.456249	59.599437
2306.197604	8610.231549	59.604442
2305.756055	8545.081947	59.609447
2305.301663	8483.793922	59.614452
2304.669105	8412.865800	59.619457
2303.752366	8348.148215	59.624461
2302.672632	8286.387455	59.629466
2302.382206	8208.213028	59.634471
2301.696597	8147.168165	59.639476
2301.190464	8083.169167	59.644481
2300.766776	8013.451495	59.649485
2299.715737	7953.808824	59.654490
2298.997419	7878.691416	59.659495
2298.483332	7821.766136	59.664500
2297.733378	7750.909875	59.669505
2297.265659	7692.383464	59.674509
2296.591665	7621.895599	59.679514
2296.217925	7547.663932	59.684519
2295.381720	7489.567520	59.689524
2294.514190	7413.417505	59.694529
2293.916537	7353.336945	59.699533
2293.135605	7280.781988	59.704538
2292.446764	7219.718565	59.709543
2291.628987	7153.081526	59.714548
2291.020646	7091.742395	59.719553
2290.395657	7025.056420	59.724557
2289.457568	6957.895060	59.729562
2289.403559	6899.090805	59.734567
2288.687654	6837.253117	59.739572
2287.877493	6767.850265	59.744577
2286.931548	6703.881998	59.749581
2286.327422	6645.551726	59.754586
2285.816239	6579.313513	59.759591
2284.975471	6518.872610	59.764596
2284.480696	6462.101710	59.769601
2283.941896	6393.416380	59.774605
2283.143489	6337.448194	59.779610
2282.513584	6261.421000	59.784615
2281.679335	6206.733652	59.789620
2281.047278	6127.116217	59.794625
2280.616714	6080.402046	59.799629
2279.766584	6011.733951	59.804634
2279.317887	5956.934313	59.809639
2278.605240	5892.742458	59.814644
2277.975158	5827.002089	59.819649
2277.648106	5743.269177	59.824653
2276.650842	5690.407149	59.829658
2275.936213	5627.369115	59.834663
2275.156903	5565.627251	59.839668
2274.397864	5507.495616	59.844673
2273.842277	5434.361847	59.849677
2273.386149	5382.118636	59.854682
2272.640283	5304.667443	59.859687
2272.115829	5247.391667	59.864692
2271.268366	5194.732442	59.869697
2270.819257	5118.142969	59.874701
2270.022554	5062.834765	59.879706
2269.489230	4987.195529	59.884711
2268.731299	4931.178933	59.889716
2268.118380	4865.712226	59.894721
2267.616699	4802.036644	59.899725
2266.773674	4743.321937	59.904730
2266.009559	4665.503158	59.909735
2265.680762	4616.907497	59.914740
2264.745016	4556.449476	59.919745
2264.223493	4484.176259	59.924750
2263.175447	4429.178459	59.929754
2262.634663	4364.886340	59.934759
2262.117829	4301.742948	59.939764
2261.174338	4234.341678	59.944769
2260.788258	4170.241964	59.949774
2260.087119	4112.476538	59.954778
2259.452292	4043.459328	59.959783
2258.552781	3991.802432	59.964788
2258.053116	3927.626369	59.969793
2257.295499	3866.867695	59.974798
2256.381023	3813.577362	59.979802
2255.640851	3726.402518	59.984807
2255.416138	3674.860517	59.989812
2254.609384	3622.448894	59.994817
2254.039716	3583.883680	59.999822
2253.360778	3511.876808	60.004826
2252.688401	3448.648987	60.009831
2252.217640	3393.739364	60.014836
2251.589520	3331.463991	60.019841
2250.742257	3256.247017	60.024846
2249.784678	3202.207105	60.029850
2249.517739	3137.307550	60.034855
2248.688099	3080.324430	60.039860
2248.201306	3015.418495	60.044865
2247.410394	2960.280543	60.049870
2246.637590	2900.793987	60.054874
2246.171211	2840.528042	60.059879
2245.159004	2784.470876	60.064884
2244.351991	2729.427039	60.069889
2244.121493	2661.732224	60.074894
2242.995984	2618.300717	60.079898
2242.438585	2571.826790	60.084903
2241.978464	2507.716918	60.089908
2241.319223	2458.361505	60.094913
2241.064560	2388.614410	60.099918
2239.747868	2337.346550	60.104922
2239.200806	2278.351905	60.109927
2238.390980	2230.121983	60.114932
2237.941933	2166.097809	60.119937
2237.581042	2111.972802	60.124942
2236.497195	2067.254149	60.129946
2235.826354	2001.210138	60.134951
2235.614084	1950.209239	60.139956
2234.485383	1893.633834	60.144961
2233.962874	1823.669347	60.149966
2233.362755	1778.360722	60.154970
2232.954584	1715.428104	60.159975
2231.993072	1658.188384	60.164980
2230.922092	1610.884308	60.169985
2230.731949	1541.341567	60.174990
2229.947463	1495.963716	60.179994
2229.271066	1446.498546	60.184999
2228.462786	1385.414450	60.190004
2227.660644	1326.890714	60.195009
2227.341643	1276.703923	60.200014
2226.544380	1241.984767	60.205018
2226.220347	1169.488441	60.210023
2225.108444	1128.748022	60.215028
2224.185622	1085.325223	60.220033
2223.891079	1023.665976	60.225038
2222.880052	981.050706	60.230042
2222.125578	921.455007	60.235047
2221.686184	878.444999	60.240052
2221.036509	831.590724	60.245057
2220.297614	773.355658	60.250062
2219.032311	741.209856	60.255066
2219.211832	705.353010	60.260071
2218.674082	644.232275	60.265076
2217.711289	599.071602	60.270081
2217.069756	554.878804	60.275086
2216.357707	514.628611	60.280090
2215.618443	465.723958	60.285095
2214.759701	423.224945	60.290100
2213.764548	373.500201	60.295105
2213.473775	330.491897	60.300110
2212.544041	299.533298	60.305114
2211.954123	254.508509	60.310119
2211.180275	221.869600	60.315124
2210.397636	190.706556	60.320129
2209.750086	146.954338	60.325134
2208.846292	134.107292	60.330138
2208.202795	98.570164	60.335143
2207.418661	59.095891	60.340148
2206.774159	30.081067	60.345153
2206.056143	-0.423219	60.350158
2204.171937	9.838369	60.355162
2200.152949	81.727180	60.360167
2200.025759	87.747370	60.365172
2200.695559	79.789787	60.370177
2201.381452	79.881210	60.375182
2200.886034	82.572676	60.380186
2200.283246	78.327129	60.385191
2199.444542	70.468533	60.390196
2198.052739	89.345404	60.395201
2197.954645	89.947542	60.400206
2197.494720	91.884361	60.405210
2196.545068	96.256315	60.410215
2195.832128	89.320734	60.415220
2195.774766	93.062291	60.420225
2195.179164	93.550981	60.425230
2193.905717	95.293606	60.430234
2193.156516	95.926508	60.435239
2192.377651	102.226706	60.440244
2192.036094	90.091564	60.445249
2191.467744	87.351206	60.450254
2190.512309	91.191093	60.455258
2190.190527	89.632123	60.460263
2190.192750	95.384214	60.465268
2189.529606	100.970647	60.470273
2188.954432	95.489170	60.475278
2187.541541	100.951714	60.480282
2186.990164	90.603356	60.485287
2186.535621	95.040259	60.490292
2185.642411	87.581373	60.495297
2185.063283	83.127080	60.500302
2183.949881	96.915352	60.505306
2183.182530	94.573982	60.510311
2182.746156	93.323340	60.515316
2182.222439	89.730694	60.520321
2181.851405	81.766361	60.525326
2180.768133	91.092005	60.530330
2180.581518	90.530258	60.535335
2180.330107	86.509650	60.540340
2179.163407	98.180744	60.545345
2178.918231	93.446394	60.550350
2178.379368	90.376523	60.555354
2177.189062	83.592379	60.560359
2176.130558	89.113809	60.565364
2175.783543	89.673444	60.570369
2175.404943	89.457534	60.575374
2174.875350	99.796002	60.580378
2173.864848	99.325551	60.585383
2173.355272	92.438131	60.590388
2172.575819	96.049839	60.595393
2171.871984	89.839763	60.600398
2171.131648	102.154389	60.605402
2170.232659	88.634888	60.610407
2170.349287	89.382724	60.615412
2169.733529	90.644136	60.620417
2169.372160	90.531143	60.625422
2167.768949	90.995213	60.630426
2167.371375	98.362388	60.635431
2167.049564	101.291235	60.640436
2166.304165	99.493564	60.645441
2165.855383	97.792328	60.650446
2164.465649	95.321065	60.655450
2164.204604	89.108544	60.660455
2163.611673	100.087816	60.665460
2162.839802	102.266515	60.670465
2162.322690	85.660391	60.675470
2161.348856	88.993873	60.680474
2160.878858	92.031382	60.685479
2160.311012	84.350582	60.690484
2159.306232	93.446170	60.695489
2158.923027	92.792619	60.700494
2157.860242	97.521567	60.705498
2157.272906	87.595223	60.710503
2156.813736	85.469881	60.715508
2155.724547	102.176285	60.720513
2155.403281	88.109407	60.725518
2155.669654	93.237713	60.730522
2154.495374	86.148276	60.735527
2153.571785	85.747617	60.740532
2152.551667	93.218299	60.745537
2152.119846	90.820547	60.750542
2152.140523	82.947027	60.755546
2151.168225	90.291855	60.760551
2150.373353	88.771687	60.765556
2149.308816	88.771845	60.770561
2149.476096	90.047783	60.775566
2148.042350	102.761005	60.780570
2147.824178	98.960618	60.785575
2147.172354	88.312837	60.790580
2145.970788	103.969527	60.795585
2146.491970	85.177100	60.800590
2145.176494	92.656803	60.805594
2144.212888	84.409627	60.810599
2143.706983	101.419280	60.815604
2142.901361	103.158659	60.820609
2142.598547	77.386823	60.825614
2141.792329	93.753444	60.830618
2141.456472	84.389574	60.835623
2141.071244	102.457090	60.840628
2139.915029	98.721971	60.845633
2139.466881	90.575923	60.850638
2138.562815	91.909896	60.855642
2137.992884	91.886768	60.860647
2137.683484	81.096357	60.865652
2136.811882	89.358723	60.870657
2136.424788	90.948119	60.875662
2134.779088	92.147469	60.880666
2134.313965	83.567324	60.885671
2134.210926	86.116120	60.890676
2133.098808	82.347205	60.895681
2132.290456	87.067323	60.900686
2132.059644	87.494989	60.905690
2131.416315	95.875674	60.910695
2130.563868	92.000902	60.915700
2129.498696	83.213210	60.920705
2129.728803	91.482106	60.925710
2128.822579	104.280358	60.930714
2127.753026	79.711929	60.935719
2127.586811	99.455603	60.940724
2126.708691	102.726605	60.945729
2126.301558	73.637805	60.950734
2125.488713	109.532010	60.955738
2124.762218	80.042886	60.960743
2124.493616	104.090350	60.965748
2123.842323	90.930516	60.970753
2123.240025	86.437340	60.975758
2121.845391	94.509907	60.980762
2120.868207	74.663787	60.985767
2120.558798	94.485366	60.990772
2120.361972	93.308683	60.995777
2119.466060	82.469423	61.000782
2118.532418	94.527731	61.005786
2117.753518	86.533519	61.010791
2118.215160	90.489172	61.015796
2117.075817	93.878893	61.020801
2116.307127	87.877815	61.025806
2115.495542	92.030775	61.030810
2115.019180	94.343936	61.035815
2114.575200	97.453014	61.040820
2113.748001	94.116688	61.045825
2112.908807	89.019314	61.050830
2111.659987	107.528210	61.055834
2111.301412	92.808123	61.060839
2111.432327	76.822986	61.065844
2110.357741	96.849563	61.070849
2109.700170	95.170431	61.075854
2108.871816	97.365991	61.080858
2108.051164	89.146605	61.085863
2107.815627	84.328741	61.090868
2107.182537	92.315159	61.095873
2106.945657	94.520936	61.100878
2106.279498	89.052346	61.105882
2104.691584	101.061529	61.110887
2103.927739	87.821800	61.115892
2103.020256	96.540860	61.120897
2103.026312	92.116723	61.125902
2102.209510	85.593454	61.130906
2101.206799	101.515052	61.135911
2101.467757	93.505633	61.140916
2100.681302	82.767279	61.145921
2100.167138	97.562721	61.150926
2099.793118	102.549805	61.155930
2098.733701	92.245826	61.160935
2097.817998	71.718217	61.165940
2096.741167	103.401454	61.170945
2096.050573	101.377498	61.175950
2095.457769	100.124888	61.180954
2095.011673	90.330685	61.185959
2094.454012	83.195466	61.190964
2093.750050	93.965289	61.195969
2093.721347	102.325715	61.200974
2093.207308	88.303637	61.205978
2092.088277	87.391568	61.210983
2091.014454	81.554036	61.215988
2089.899545	87.508627	61.220993
2089.492536	78.960273	61.225998
2089.390420	88.883990	61.231002
2088.715318	97.089960	61.236007
2088.100995	87.361879	61.241012
2087.315369	99.158600	61.246017
2086.638253	89.867817	61.251022
2086.345506	90.781534	61.256026
2085.255440	97.159522	61.261031
2084.494579	95.134106	61.266036
2083.378547	104.111765	61.271041
2083.148212	90.229162	61.276046
2082.217976	98.105054	61.281050
2081.618808	99.728113	61.286055
2081.421656	85.419221	61.291060
2080.379701	91.234512	61.296065
2079.957271	85.533297	61.301070
2079.836442	98.271567	61.306074
2079.125467	92.360685	61.311079
2078.717890	87.836619	61.316084
2077.249481	97.437874	61.321089
2076.679162	89.027393	61.326094
2076.013249	95.238728	61.331098
2075.345105	97.358413	61.336103
2074.840537	94.634768	61.341108
2073.952779	99.914684	61.346113
2073.725727	92.294934	61.351118
2072.513497	90.147198	61.356122
2071.591785	95.803068	61.361127
2071.316779	84.214040	61.366132
2070.074919	92.099965	61.371137
2070.152668	89.326484	61.376142
2069.572016	94.746888	61.381146
2069.074066	88.256604	61.386151
2068.692363	85.693227	61.391156
2067.895355	98.073626	61.396161
2067.000681	95.206897	61.401166
2065.968004	92.731060	61.406170
2065.147772	101.694895	61.411175
2064.817282	80.115675	61.416180
2064.306004	91.353215	61.421185
2063.920036	92.155578	61.426190
2063.330541	88.584438	61.431194
2061.898531	90.000643	61.436199
2061.006102	83.166133	61.441204
2060.406821	97.554058	61.446209
2060.426530	89.885689	61.451214
2059.465937	84.796565	61.456218
2058.878139	79.927386	61.461223
2058.934325	75.552068	61.466228
2058.052275	77.940657	61.471233
2056.878910	90.618889	61.476238
2055.827125	96.648628	61.481242
2054.902726	95.948525	61.486247
2054.665895	87.619160	61.491252
2053.855605	95.945933	61.496257
2053.656797	82.960316	61.501262
2053.322229	80.684339	61.506266
2052.296847	83.504090	61.511271
2052.265264	80.662811	61.516276
2051.565976	87.778265	61.521281
2050.305009	77.528386	61.526286
2049.420000	79.496420	61.531290
2048.772655	88.290893	61.536295
2048.564202	68.750156	61.541300
2047.809278	88.550966	61.546305
2047.688774	77.164500	61.551310
2046.643809	79.192613	61.556314
2045.199851	85.883807	61.561319
2044.829269	73.420602	61.566324
2044.202478	84.118256	61.571329
2043.942383	85.525089	61.576334
2043.566892	82.995422	61.581338
2042.463567	75.694524	61.586343
2041.572750	75.947839	61.591348
2040.532497	88.967630	61.596353
2040.356698	81.639365	61.601358
2039.903207	75.839018	61.606362
2039.163336	80.374833	61.611367
2039.169611	78.732282	61.616372
2037.666697	93.265197	61.621377
2036.878246	74.876171	61.626382
2036.245923	66.601706	61.631386
2035.400197	92.025887	61.636391
2035.265304	75.674537	61.641396
2034.593333	87.618791	61.646401
2034.375264	82.058610	61.651406
2033.796206	71.579097	61.656410
2032.432223	82.489943	61.661415
2031.744729	83.715463	61.666420
2030.713878	87.581561	61.671425
2030.556857	80.472657	61.676430
2029.922984	85.177723	61.681434
2029.351944	85.623129	61.686439
2029.250897	78.415460	61.691444
2027.999172	79.378889	61.696449
2026.846731	84.394907	61.701454
2026.697360	87.499812	61.706458
2025.900372	93.973222	61.711463
2025.582137	77.015489	61.716468
2024.430949	80.162708	61.721473
2023.720999	83.706652	61.726478
2023.095052	80.808329	61.731482
2022.241935	83.291681	61.736487
2022.203812	82.274313	61.741492
2021.595805	93.311178	61.746497
2021.308100	78.690265	61.751502
2020.136861	78.015161	61.756506
2018.980448	85.408169	61.761511
2018.559512	86.440005	61.766516
2017.720520	97.456767	61.771521
2017.510374	83.668748	61.776526
2017.040397	76.177456	61.781530
2015.951091	82.826564	61.786535
2015.371180	69.393701	61.791540
2014.288416	79.851506	61.796545
2013.857488	72.376095	61.801550
2013.265515	75.365176	61.806554
2012.567324	73.632598	61.811559
2012.425988	70.815051	61.816564
2012.087043	83.414464	61.821569
2011.088620	67.632254	61.826574
2010.126497	73.461696	61.831578
2009.321553	74.693248	61.836583
2008.956024	69.664235	61.841588
2008.020672	91.002761	61.846593
2006.763406	81.960206	61.851598
2006.767193	85.953814	61.856602
2005.787178	88.422621	61.861607
2005.466306	80.511867	61.866612
2004.641890	83.883181	61.871617
2004.493971	80.464310	61.876622
2004.241544	85.309100	61.881626
2003.096559	88.660338	61.886631
2002.250031	80.717907	61.891636
2001.230115	81.415906	61.896641
2000.993889	75.421819	61.901646
2000.473342	81.739394	61.906650
1999.714348	78.818043	61.911655
1998.658252	78.938342	61.916660
1997.824444	89.750862	61.921665
1997.631586	78.459462	61.926670
1997.080379	71.469903	61.931674
1996.293750	85.537491	61.936679
1996.139640	79.058882	61.941684
1994.665093	79.316561	61.946689
1993.640547	68.431558	61.951694
1993.262134	76.757588	61.956698
1992.509354	86.896534	61.961703
1992.556658	82.241941	61.966708
1991.985404	75.766471	61.971713
1991.446741	74.711866	61.976718
1990.689320	83.178480	61.981722
1989.619596	88.482568	61.986727
1989.229818	73.570380	61.991732
1988.644441	77.928725	61.996737
1987.759052	70.465536	62.001742
1986.545016	80.258245	62.006746
1985.629103	90.421512	62.011751
1985.433519	78.305840	62.016756
1984.901249	86.903867	62.021761
1984.859462	76.509389	62.026766
1984.278406	84.310952	62.031770
1982.761055	76.758849	62.036775
1982.289145	76.731234	62.041780
1981.590863	75.988959	62.046785
1981.030280	74.583038	62.051790
1980.782622	81.603161	62.056794
1979.852067	90.346410	62.061799
1978.980038	65.838211	62.066804
1978.128934	89.954437	62.071809
1977.520814	85.255654	62.076814
1977.201751	77.193240	62.081818
1976.238161	88.083131	62.086823
1976.537903	77.006844	62.091828
1975.407529	83.462221	62.096833
1974.296644	85.928160	62.101838
1973.371454	87.852137	62.106842
1972.937954	90.068633	62.111847
1972.846993	67.021216	62.116852
1972.157883	83.582136	62.121857
1971.218483	79.662883	62.126862
1970.137371	75.048649	62.131866
1969.589660	75.998118	62.136871
1968.948681	77.560028	62.141876
1968.405052	91.631628	62.146881
1968.267551	74.355081	62.151886
1967.642143	75.368921	62.156890
1965.833891	84.866476	62.161895
1965.582752	71.674740	62.166900
1964.717028	91.912598	62.171905
1964.066756	77.081186	62.176910
1963.952299	86.530636	62.181914
1963.760041	83.118805	62.186919
1963.380148	75.130703	62.191924
1962.158829	83.196321	62.196929
1961.265436	81.264520	62.201934
1960.864498	90.231193	62.206938
1960.323325	84.441627	62.211943
1959.232697	76.315624	62.216948
1958.507750	85.019929	62.221953
1957.856284	83.869701	62.226958
1957.947354	75.141397	62.231962
1956.664522	87.457006	62.236967
1955.745186	85.042069	62.241972
1954.873488	92.009879	62.246977
1954.458002	86.315474	62.251982
1954.133770	74.336922	62.256986
1953.604954	81.612979	62.261991
1953.341459	76.593007	62.266996
1952.041839	87.015877	62.272001
1951.287282	87.723809	62.277006
1951.034723	72.988538	62.282010
1949.760276	93.236090	62.287015
1949.004611	83.814335	62.292020
1948.402752	82.891189	62.297025
1947.820514	82.747060	62.302030
1947.391539	77.601978	62.307034
1946.901577	81.448469	62.312039
1946.277504	69.377180	62.317044
1945.646383	90.399348	62.322049
1944.950510	92.504541	62.327054
1944.096995	86.963248	62.332058
1943.445953	88.383267	62.337063
1943.337020	72.679071	62.342068
1942.545531	68.411516	62.347073
1941.290073	84.278638	62.352078
1940.885716	79.834513	62.357082
1940.096807	86.618879	62.362087
1939.573382	74.600993	62.367092
1937.936201	86.873517	62.372097
1937.825245	82.333931	62.377102
1937.928298	79.706239	62.382106
1937.030335	84.308173	62.387111
1936.384165	80.884830	62.392116
1935.926086	89.390666	62.397121
1934.548239	89.109504	62.402126
1933.962054	79.470050	62.407130
1933.251914	76.515736	62.412135
1932.840604	72.060103	62.417140
1932.310278	79.252827	62.422145
1932.009354	86.189950	62.427150
1931.289809	81.314915	62.432154
1929.904175	84.187169	62.437159
1929.505740	75.799914	62.442164
1929.151986	80.630831	62.447169
1928.544054	74.099706	62.452174
1928.039079	82.740710	62.457178
1926.324885	86.174457	62.462183
1926.221149	73.197438	62.467188
1925.473906	74.236936	62.472193
1925.229159	84.459235	62.477198
1924.656818	80.666224	62.482202
1923.547063	86.378793	62.487207
1922.848671	84.373472	62.492212
1921.905894	89.178060	62.497217
1921.525197	80.089432	62.502222
1921.636095	79.251826	62.507226
1920.528924	92.287004	62.512231
1920.096924	74.424894	62.517236
1919.258360	86.289959	62.522241
1918.402299	78.617145	62.527246
1917.335820	68.000600	62.532250
1916.112067	74.751503	62.537255
1916.009946	74.900149	62.542260
1915.477675	81.400936	62.547265
1915.096422	73.802550	62.552270
1914.750824	80.021401	62.557274
1914.128071	85.461125	62.562279
1913.631592	75.083652	62.567284
1912.577561	73.666204	62.572289
1911.906411	82.123866	62.577294
1911.556550	76.143103	62.582298
1910.254218	80.672053	62.587303
1909.455317	77.336041	62.592308
1908.826981	81.311733	62.597313
1908.201722	73.783625	62.602318
1908.208567	73.757284	62.607322
1907.528087	77.712870	62.612327
1906.436349	77.487220	62.617332
1905.600829	74.904463	62.622337
1904.890378	72.636149	62.627342
1904.849549	68.298315	62.632346
1904.200162	76.195883	62.637351
1903.164501	75.057783	62.642356
1902.673417	72.743603	62.647361
1901.860585	65.067094	62.652366
1901.321486	73.902739	62.657370
1900.184568	74.997802	62.662375
1899.866772	70.260838	62.667380
1899.067134	71.865299	62.672385
1898.173438	86.552266	62.677390
1897.974340	69.993539	62.682394
1897.377350	81.314073	62.687399
1897.003973	74.925482	62.692404
1895.956335	83.923868	62.697409
1894.724832	82.159306	62.702414
1894.858256	78.273175	62.707418
1893.866749	92.477385	62.712423
1893.926066	78.908380	62.717428
1892.643897	73.665391	62.722433
1891.585805	74.905631	62.727438
1891.330299	86.581941	62.732442
1891.012463	76.336954	62.737447
1890.280133	72.482626	62.742452
1889.229316	85.127256	62.747457
1888.483517	87.383885	62.752462
1888.044473	87.814671	62.757466
1887.377321	88.521359	62.762471
1886.604355	67.863988	62.767476
1885.599541	84.271622	62.772481
1884.600751	89.695365	62.777486
1884.797110	81.284643	62.782490
1884.407854	74.118022	62.787495
1883.646057	85.095738	62.792500
1883.256325	88.610951	62.797505
1882.148439	77.669847	62.802510
1881.870822	81.184604	62.807514
1880.828936	80.391259	62.812519
1879.535683	75.323493	62.817524
1878.782889	81.411465	62.822529
1878.171562	80.354229	62.827534
1878.162831	77.171878	62.832538
1877.657418	83.635293	62.837543
1877.607645	79.795593	62.842548
1876.594334	79.308358	62.847553
1875.299661	84.539395	62.852558
1874.660339	78.636134	62.857562
1874.385662	79.583271	62.862567
1873.486802	74.952759	62.867572
1872.890803	71.237633	62.872577
1872.001667	86.728087	62.877582
1871.591151	73.875476	62.882586
1870.992916	74.804602	62.887591
1870.150440	72.500492	62.892596
1869.090837	83.750987	62.897601
1868.250350	70.983993	62.902606
1867.929412	69.251481	62.907610
1867.544397	76.261875	62.912615
1867.012562	77.398068	62.917620
1866.713176	64.168295	62.922625
1866.030317	69.538721	62.927630
1864.894230	67.315924	62.932634
1864.531606	71.517501	62.937639
1863.568590	70.867752	62.942644
1862.351781	66.554222	62.947649
1861.542372	83.284054	62.952654
1861.324428	72.343582	62.957658
1860.620475	76.119987	62.962663
1860.519174	62.644309	62.967668
1860.338377	61.368917	62.972673
1859.598014	67.439145	62.977678
1858.524828	70.149864	62.982682
1857.529760	79.554630	62.987687
1857.119744	74.095914	62.992692
1855.838632	71.492467	62.997697
1854.734961	65.066888	63.002702
1855.212881	60.477967	63.007706
1854.213729	78.594033	63.012711
1853.996740	74.935421	63.017716
1853.833340	70.330060	63.022721
1852.453369	75.100009	63.027726
1851.944480	65.194441	63.032730
1851.098932	78.293736	63.037735
1850.324636	71.155148	63.042740
1849.446883	74.588586	63.047745
1848.768448	72.138594	63.052750
1848.723527	67.184856	63.057754
1847.860889	74.480813	63.062759
1847.570276	73.525617	63.067764
1846.324652	67.669757	63.072769
1845.460511	71.667132	63.077774
1845.106811	68.022345	63.082778
1844.443305	80.307455	63.087783
1844.046542	77.219833	63.092788
1842.915865	70.177258	63.097793
1842.086746	76.502848	63.102798
1841.780661	74.127769	63.107802
1841.552755	74.597573	63.112807
1840.606368	73.248213	63.117812
1839.402641	62.476896	63.122817
1838.683532	70.719840	63.127822
1838.580117	55.497333	63.132826
1837.858940	68.747176	63.137831
1837.822697	74.287735	63.142836
1836.660888	74.681915	63.147841
1835.535899	71.550665	63.152846
1835.330229	71.933364	63.157850
1834.608200	76.546812	63.162855
1833.866820	72.542560	63.167860
1833.021637	70.945333	63.172865
1832.363627	76.852691	63.177870
1832.158281	65.555432	63.182874
1831.517356	70.463491	63.187879
1830.596598	72.680109	63.192884
1829.677260	75.241837	63.197889
1829.145480	76.510487	63.202894
1828.827651	79.531762	63.207898
1828.141799	75.408313	63.212903
1827.233837	71.954037	63.217908
1826.745956	77.004945	63.222913
1825.537554	79.716650	63.227918
1825.596304	66.348019	63.232922
1824.811621	78.269190	63.237927
1823.876335	61.515171	63.242932
1822.967648	55.468637	63.247937
1822.122162	70.598932	63.252942
1822.024811	72.952870	63.257946
1821.596515	68.604033	63.262951
1820.994391	65.795020	63.267956
1819.489775	73.323806	63.272961
1818.849115	72.939837	63.277966
1818.770696	66.513890	63.282970
1818.054726	76.378945	63.287975
1817.742903	67.850242	63.292980
1816.835727	70.148282	63.297985
1815.541579	68.570317	63.302990
1815.718825	60.988925	63.307994
1815.084513	59.720900	63.312999
1813.918305	55.869272	63.318004
1813.253094	63.493408	63.323009
1812.452428	76.103058	63.328014
1812.185446	57.489441	63.333018
1811.327939	59.213497	63.338023
1811.247054	75.187428	63.343028
1810.233405	69.091332	63.348033
1809.496251	75.049106	63.353038
1808.888371	69.844162	63.358042
1808.170838	70.959395	63.363047
1807.269954	66.925292	63.368052
1806.363926	63.853899	63.373057
1805.732941	76.264725	63.378062
1805.693934	68.591520	63.383066
1805.007209	72.180707	63.388071
1804.285495	69.087929	63.393076
1803.431921	63.059455	63.398081
1802.658573	81.623776	63.403086
1802.437702	70.284833	63.408090
1801.438944	69.708589	63.413095
1800.784573	64.727063	63.418100
1800.332230	60.222787	63.423105
1799.250652	73.219227	63.428110
1799.172651	63.689929	63.433114
1798.592298	67.216495	63.438119
1797.840544	71.755826	63.443124
1797.473149	72.252515	63.448129
1796.294152	60.015537	63.453134
1795.336116	57.501160	63.458138
1794.024549	75.774073	63.463143
1793.631211	75.797090	63.468148
1793.741325	59.827931	63.473153
1793.092356	63.505735	63.478158
1792.857054	68.461344	63.483162
1791.801987	65.626502	63.488167
1790.890745	68.117574	63.493172
1790.443881	59.091536	63.498177
1789.608854	78.564466	63.503182
1788.877698	59.430086	63.508186
1788.099661	68.428257	63.513191
1787.360321	69.788220	63.518196
1786.996148	73.528027	63.523201
1786.299804	70.688256	63.528206
1785.995505	60.816451	63.533210
1784.832579	76.605841	63.538215
1784.237934	70.164110	63.543220
1783.634291	63.679658	63.548225
1783.187262	61.156671	63.553230
1782.957869	62.777832	63.558234
1781.863401	63.173957	63.563239
1780.930704	70.911540	63.568244
1780.572779	57.749436	63.573249
1779.612929	64.983576	63.578254
1778.682614	69.136551	63.583258
1777.872564	73.874370	63.588263
1777.614029	66.814744	63.593268
1777.316166	62.142444	63.598273
1776.776215	67.386119	63.603278
1775.955085	70.276026	63.608282
1775.144916	71.486399	63.613287
1774.447714	70.657282	63.618292
1774.249872	61.178559	63.623297
1773.040255	62.681016	63.628302
1772.585108	63.803470	63.633306
1771.641953	73.181089	63.638311
1771.030126	65.501094	63.643316
1770.775737	64.614268	63.648321
1769.536256	71.618448	63.653326
1769.046536	54.888317	63.658330
1768.444149	65.873836	63.663335
1768.234873	64.407442	63.668340
1767.192958	63.685109	63.673345
1766.185505	71.686869	63.678350
1765.660575	66.047740	63.683354
1765.073245	66.052687	63.688359
1764.863034	68.497085	63.693364
1764.531547	56.994387	63.698369
1763.296823	64.335261	63.703374
1762.436594	63.172512	63.708378
1762.009822	70.468648	63.713383
1760.973500	69.423746	63.718388
1760.118297	60.667560	63.723393
1759.205580	69.433250	63.728398
1759.037445	63.469390	63.733402
1758.496865	66.661657	63.738407
1758.171892	67.692481	63.743412
1758.148911	71.816475	63.748417
1756.739775	78.052863	63.753422
1756.145299	66.561967	63.758426
1755.476347	61.614309	63.763431
1754.286698	55.484699	63.768436
1753.548609	57.703866	63.773441
1752.830754	68.436505	63.778446
1752.415805	69.052711	63.783450
1752.123155	63.400349	63.788455
1751.463249	64.047575	63.793460
1751.344090	52.271478	63.798465
1750.043756	75.896097	63.803470
1749.412548	64.778450	63.808474
1748.783945	77.070639	63.813479
1748.055317	76.188175	63.818484
1747.370237	73.357664	63.823489
1746.689117	80.692626	63.828494
1746.619006	74.796769	63.833498
1745.537155	72.664755	63.838503
1744.260231	75.819440	63.843508
1744.061359	75.426822	63.848513
1743.502712	72.514735	63.853518
1743.053090	64.790064	63.858522
1741.947299	74.729658	63.863527
1741.114253	74.224884	63.868532
1740.569126	63.899351	63.873537
1739.721480	78.690983	63.878542
1739.905865	74.449846	63.883546
1738.916808	69.791138	63.888551
1737.825504	67.774164	63.893556
1737.456539	65.915264	63.898561
1736.897029	68.700555	63.903566
1736.610794	69.540736	63.908570
1735.554516	76.017542	63.913575
1734.626622	62.644789	63.918580
1734.657464	71.621729	63.923585
1733.497735	68.907608	63.928590
1732.455276	65.048977	63.933594
1731.922965	72.027582	63.938599
1731.213232	71.241465	63.943604
1731.105171	71.889353	63.948609
1730.669436	68.667603	63.953614
1729.618275	68.080787	63.958618
1728.643505	67.368304	63.963623
1728.117882	72.314837	63.968628
1728.039403	62.952774	63.973633
1726.918187	70.958422	63.978638
1725.770589	68.606636	63.983642
1725.332833	70.336586	63.988647
1724.727662	56.609827	63.993652
1724.631889	66.616069	63.998657
1723.637673	71.179736	64.003662
1722.880347	68.606701	64.008666
1721.953561	71.707360	64.013671
1721.889434	69.815813	64.018676
1721.621512	62.221554	64.023681
1720.069506	77.276441	64.028686
1719.514751	67.990023	64.033690
1718.859217	62.865213	64.038695
1718.598654	72.096582	64.043700
1717.924792	77.967058	64.048705
1716.741881	79.512605	64.053710
1716.242743	70.501191	64.058714
1715.712017	79.520022	64.063719
1715.216771	68.967386	64.068724
1714.444039	68.675380	64.073729
1713.135244	68.342370	64.078734
1712.721142	60.394459	64.083738
1712.388394	70.878291	64.088743
1711.997656	71.036518	64.093748
1711.341962	64.964034	64.098753
1710.499130	70.240059	64.103758
1709.784373	61.691809	64.108762
1709.640082	66.923109	64.113767
1708.213469	71.785684	64.118772
1707.494921	59.677462	64.123777
1707.021497	62.713998	64.128782
1706.492331	62.586723	64.133786
1705.896203	63.867193	64.138791
1704.662686	66.426827	64.143796
1704.254332	56.644106	64.148801
1703.461847	72.079800	64.153806
1703.211035	70.307788	64.158810
1702.812251	70.888319	64.163815
1702.079349	61.928237	64.168820
1701.429509	56.999638	64.173825
1700.821021	66.477069	64.178830
1700.081156	61.870259	64.183834
1698.967389	64.518101	64.188839
1698.212799	64.836621	64.193844
1698.026879	62.317904	64.198849
1697.174313	74.385488	64.203854
1696.300246	68.704067	64.208858
1695.616132	66.034260	64.213863
1694.607915	75.344968	64.218868
1694.572724	50.757657	64.223873
1694.129861	72.800093	64.228878
1693.879814	68.651615	64.233882
1692.720755	58.598652	64.238887
1691.815232	72.037062	64.243892
1691.586890	54.891724	64.248897
1690.422412	69.855100	64.253902
1689.423605	65.585875	64.258906
1689.165422	65.078110	64.263911
1688.502044	59.626567	64.268916
1688.225953	60.778937	64.273921
1687.539146	77.162896	64.278926
1686.353928	74.514344	64.283930
1685.750590	62.616474	64.288935
1685.345431	68.581458	64.293940
1685.144347	59.240455	64.298945
1683.840479	76.088264	64.303950
1683.184673	65.416073	64.308954
1682.323020	57.212851	64.313959
1681.797899	66.008448	64.318964
1681.704633	70.394325	64.323969
1680.705076	64.248747	64.328974
1680.173210	62.149242	64.333978
1679.496823	59.697399	64.338983
1678.830168	59.279750	64.343988
1678.228728	52.011281	64.348993
1676.634814	70.396877	64.353998
1676.649345	62.437655	64.359002
1676.319871	60.632413	64.364007
1675.641375	69.480761	64.369012
1674.673398	64.012954	64.374017
1673.673409	72.887142	64.379022
1673.449008	72.186365	64.384026
1673.060672	75.702953	64.389031
1672.078377	78.287349	64.394036
1671.372530	64.616016	64.399041
1670.472242	74.056234	64.404046
1670.032004	71.109587	64.409050
1670.026604	60.419237	64.414055
1668.730456	67.024047	64.419060
1667.737156	60.235696	64.424065
1667.419302	61.358435	64.429070
1667.024126	57.247210	64.434074
1666.392052	71.621423	64.439079
1665.220086	54.755292	64.444084
1664.955484	62.798338	64.449089
1664.191436	70.269479	64.454094
1663.549922	62.311975	64.459098
1662.910384	65.652435	64.464103
1661.820896	75.449123	64.469108
1661.839860	65.119158	64.474113
1660.794879	68.995510	64.479118
1660.395069	68.205910	64.484122
1659.359240	61.337590	64.489127
1658.562461	68.747701	64.494132
1658.431414	59.580071	64.499137
1657.691071	64.112890	64.504142
1656.856595	64.046741	64.509146
1656.232770	62.885896	64.514151
1655.475331	66.626689	64.519156
1655.139140	62.649590	64.524161
1654.520993	60.350920	64.529166
1653.447981	63.916352	64.534170
1652.800491	59.498300	64.539175
1652.153347	68.846269	64.544180
1651.852865	61.094778	64.549185
1650.901506	63.622227	64.554190
1650.049222	61.403328	64.559194
1649.692475	70.577440	64.564199
1648.995436	72.307593	64.569204
1649.124398	59.927572	64.574209
1647.429827	74.782797	64.579214
1647.206911	68.788230	64.584218
1646.516939	67.283099	64.589223
1645.167387	60.092483	64.594228
1644.753632	61.244651	64.599233
1643.949353	69.583157	64.604238
1643.831266	66.268388	64.609242
1643.562140	62.591281	64.614247
1642.485874	56.308106	64.619252
1641.561531	60.236257	64.624257
1640.562480	64.939482	64.629262
1640.414756	61.810762	64.634266
1639.737632	55.796900	64.639271
1639.128053	66.707887	64.644276
1638.476122	75.329685	64.649281
1637.873529	78.768357	64.654286
1637.341049	72.255296	64.659290
1636.631946	63.163730	64.664295
1635.491151	75.847942	64.669300
1635.107393	69.481557	64.674305
1634.377413	67.815637	64.679310
1634.187759	76.673064	64.684314
1632.788725	62.026986	64.689319
1631.971971	77.570623	64.694324
1631.760806	69.338189	64.699329
1631.096194	66.170166	64.704334
1630.549533	73.108489	64.709338
1630.287086	68.667115	64.714343
1629.195289	79.236849	64.719348
1628.846045	59.731232	64.724353
1627.922377	75.816951	64.729358
1626.869724	66.855655	64.734362
1626.659970	68.918385	64.739367
1625.583219	75.366943	64.744372
1625.250601	57.389830	64.749377
1624.673711	71.036227	64.754382
1623.720005	63.114141	64.759386
1622.795104	62.485235	64.764391
1622.199804	76.713273	64.769396
1622.172329	56.002274	64.774401
1621.561073	63.977397	64.779406
1620.769643	65.471830	64.784410
1620.074380	57.896600	64.789415
1619.319468	68.040668	64.794420
1618.803916	68.281813	64.799425
1617.504858	70.694212	64.804430
1616.854517	68.985684	64.809434
1616.678208	55.175065	64.814439
1615.802402	74.627679	64.819444
1615.703627	57.614731	64.824449
1614.443943	72.454492	64.829454
1613.522746	68.789525	64.834458
1613.028400	68.606278	64.839463
1612.372373	72.438199	64.844468
1612.396195	69.025197	64.849473
1611.962497	65.762149	64.854478
1610.839673	70.150754	64.859482
1610.306663	70.186528	64.864487
1609.131372	67.769814	64.869492
1608.293705	60.557815	64.874497
1607.656003	72.676429	64.879502
1607.428341	64.035060	64.884506
1607.167436	66.017612	64.889511
1606.243625	65.145701	64.894516
1605.294722	60.072266	64.899521
1604.699896	68.725992	64.904526
1604.343450	57.744513	64.909530
1603.793728	70.719579	64.914535
1602.368003	64.687473	64.919540
1602.125604	56.032682	64.924545
1601.688058	66.720809	64.929550
1600.853827	63.685394	64.934554
1600.171341	56.772004	64.939559
1598.976679	70.795658	64.944564
1599.102456	60.691571	64.949569
1598.336960	54.130398	64.954574
1597.250890	66.955722	64.959578
1596.475747	59.503572	64.964583
1595.579406	66.792328	64.969588
1595.699429	59.193225	64.974593
1595.236090	66.146695	64.979598
1594.339135	61.959095	64.984602
1593.597328	57.422013	64.989607
1592.898802	60.585788	64.994612
1592.420245	53.975875	64.999617
1591.190911	67.852080	65.004622
1590.345502	51.422948	65.009626
1589.972630	51.103718	65.014631
1589.566236	72.394492	65.019636
1589.299771	67.950610	65.024641
1588.711612	56.670078	65.029646
1587.282658	57.004316	65.034650
1586.997704	56.986491	65.039655
1586.334297	67.216945	65.044660
1585.342046	60.970907	65.049665
1584.176645	64.377588	65.054670
1583.893413	56.792098	65.059674
1583.483475	57.401225	65.064679
1582.964372	63.221902	65.069684
1582.501965	64.481153	65.074689
1582.087559	56.963810	65.079694
1580.781433	60.668803	65.084698
1580.023052	59.002682	65.089703
1579.517998	67.771450	65.094708
1579.460052	60.960674	65.099713
1578.620990	58.616704	65.104718
1577.805455	62.231136	65.109722
1577.525609	60.090035	65.114727
1575.883153	69.930453	65.119732
1575.205994	65.687438	65.124737
1574.633863	70.567270	65.129742
1574.256710	75.558042	65.134746
1573.981369	63.497717	65.139751
1573.149147	65.118486	65.144756
1572.684496	64.238283	65.149761
1571.910152	68.199392	65.154766
1571.269347	64.780035	65.159770
1570.222245	67.303803	65.164775
1569.340075	67.655246	65.169780
1568.916683	65.122237	65.174785
1568.319577	64.423921	65.179790
1567.726526	63.174634	65.184794
1567.556438	55.556979	65.189799
1566.241345	66.844986	65.194804
1566.042173	57.978340	65.199809
1565.134000	63.001446	65.204814
1564.353556	70.681782	65.209818
1563.358780	59.808046	65.214823
1562.658074	70.848635	65.219828
1562.461782	60.108209	65.224833
1562.112052	64.571101	65.229838
1561.356278	62.212326	65.234842
1560.380562	59.118987	65.239847
1559.684608	56.772784	65.244852
1559.691935	59.095899	65.249857
1558.745265	58.569818	65.254862
1557.919434	58.093918	65.259866
1557.331516	54.100069	65.264871
1556.442394	63.866523	65.269876
1555.723044	59.753215	65.274881
1555.025443	49.385752	65.279886
1554.343491	71.182329	65.284890
1554.424613	55.429115	65.289895
1553.423513	67.280637	65.294900
1552.442143	55.457081	65.299905
1551.603237	52.501272	65.304910
1550.746020	69.227685	65.309914
1550.859725	48.177331	65.314919
1549.787763	59.425130	65.319924
1549.307401	48.945884	65.324929
1548.294176	58.739939	65.329934
1547.942804	63.259860	65.334938
1547.758526	54.833952	65.339943
1546.423348	58.970908	65.344948
1545.934459	53.982092	65.349953
1545.152088	49.845690	65.354958
1544.536326	57.706426	65.359962
1544.289285	61.826590	65.364967
1543.441624	65.383062	65.369972
1542.662685	67.241366	65.374977
1542.151148	63.068234	65.379982
1541.328706	62.572879	65.384986
1540.683148	52.291761	65.389991
1539.777608	57.298686	65.394996
1539.603481	53.373124	65.400001
1539.013083	60.701582	65.405006
1537.885845	65.215487	65.410010
1537.291876	55.001861	65.415015
1536.473045	67.078300	65.420020
1536.263572	56.505548	65.425025
1535.215884	64.037552	65.430030
1534.285043	54.055644	65.435034
1533.781370	56.015280	65.440039
1533.344871	64.194447	65.445044
1533.139166	64.056808	65.450049
1532.633574	55.275128	65.455054
1531.384726	57.304293	65.460058
1531.172178	61.333825	65.465063
1529.976855	62.350021	65.470068
1528.831263	57.544405	65.475073
1528.263757	64.393014	65.480078
1527.532070	61.814391	65.485082
1527.807908	51.410518	65.490087
1527.185627	54.987945	65.495092
1526.546532	61.081572	65.500097
1525.499677	59.395080	65.505102
1524.656539	59.994211	65.510106
1524.303529	49.707612	65.515111
1523.258125	61.984048	65.520116
1522.510864	50.150117	65.525121
1522.202707	54.456600	65.530126
1521.435824	57.465683	65.535130
1521.231040	43.547663	65.540135
1520.352903	58.738372	65.545140
1519.739675	54.234496	65.550145
1519.092305	63.609324	65.555150
1518.257618	55.185856	65.560154
1517.580960	58.057607	65.565159
1516.605711	53.478804	65.570164
1516.004770	55.207909	65.575169
1515.650574	56.683350	65.580174
1515.135492	62.996956	65.585178
1514.229524	54.630548	65.590183
1513.202157	65.134878	65.595188
1513.271824	59.259412	65.600193
1512.840373	59.266452	65.605198
1511.506014	58.942338	65.610202
1510.896401	56.468895	65.615207
1510.415482	63.795729	65.620212
1509.735087	62.457840	65.625217
1508.983056	57.961833	65.630222
1508.167007	51.799791	65.635226
1507.765870	59.266901	65.640231
1507.076374	66.152246	65.645236
1506.270091	59.484052	65.650241
1505.740043	56.256839	65.655246
1504.867838	65.708398	65.660250
1504.471772	52.475171	65.665255
1503.394732	60.782936	65.670260
1502.571934	57.450866	65.675265
1502.183655	62.836048	65.680270
1501.993881	63.452777	65.685274
1501.623435	57.333456	65.690279
1500.184041	68.633360	65.695284
1499.543408	53.043738	65.700289
1499.177730	62.670253	65.705294
1498.383605	58.125747	65.710298
1498.082008	55.054610	65.715303
1497.035683	63.437917	65.720308
1496.487031	55.565059	65.725313
1496.052434	47.387090	65.730318
1494.635355	54.746006	65.735322
1493.870582	53.547681	65.740327
1493.232620	66.842686	65.745332
1492.817822	54.741475	65.750337
1492.882426	47.214264	65.755342
1492.249427	66.025933	65.760346
1491.806543	56.152568	65.765351
1490.646764	65.873746	65.770356
1489.842496	56.917205	65.775361
1488.969097	61.501168	65.780366
1487.749088	61.999363	65.785370
1487.844963	55.485835	65.790375
1487.156434	66.638031	65.795380
1487.272433	63.759134	65.800385
1486.008661	61.716068	65.805390
1485.079002	65.334471	65.810394
1484.434790	58.998478	65.815399
1484.011552	56.623149	65.820404
1483.162758	52.522554	65.825409
1482.510241	55.059334	65.830414
1481.750787	70.100319	65.835418
1481.450826	57.780597	65.840423
1480.337836	63.746130	65.845428
1479.549469	54.984176	65.850433
1479.057124	64.276028	65.855438
1478.503783	69.819904	65.860442
1478.361232	51.672299	65.865447
1477.386059	56.702923	65.870452
1476.711207	67.684223	65.875457
1476.097928	62.309935	65.880462
1475.358017	59.579680	65.885466
1474.500956	62.502188	65.890471
1473.440616	57.023920	65.895476
1472.998498	64.694657	65.900481
1472.768993	55.463862	65.905486
1472.065405	66.590070	65.910490
1471.755630	54.902659	65.915495
1470.670255	60.710850	65.920500
1470.200005	63.248626	65.925505
1469.283205	55.609317	65.930510
1468.276657	58.643888	65.935514
1467.650545	51.677435	65.940519
1467.212421	58.286303	65.945524
1466.577410	58.606385	65.950529
1466.310283	50.561070	65.955534
1465.755026	61.567512	65.960538
1464.925331	46.069457	65.965543
1463.987054	59.856863	65.970548
1463.603007	50.928163	65.975553
1462.860980	47.162250	65.980558
1461.693697	56.209726	65.985562
1461.705105	52.338260	65.990567
1461.159300	62.698263	65.995572
1459.953835	50.834684	66.000577
1459.200164	64.121273	66.005582
1458.399401	56.953932	66.010586
1458.611023	49.352896	66.015591
1457.615771	68.266295	66.020596
1456.633134	58.772019	66.025601
1455.998413	59.347510	66.030606
1455.285540	59.235292	66.035610
1455.292501	51.556402	66.040615
1454.028531	54.595623	66.045620
1453.524939	58.111627	66.050625
1453.254917	46.427370	66.055630
1452.024403	62.076199	66.060634
1450.957960	59.281160	66.065639
1450.270937	66.565070	66.070644
1449.793360	64.181038	66.075649
1449.812242	52.706312	66.080654
1449.315520	58.241190	66.085658
1448.860236	48.136437	66.090663
1447.417358	54.993302	66.095668
1446.969835	65.392878	66.100673
1446.239313	58.597555	66.105678
1445.233114	55.152738	66.110682
1444.728624	45.809550	66.115687
1444.045724	67.983146	66.120692
1443.930202	59.801776	66.125697
1443.044418	55.054253	66.130702
1441.810000	64.968649	66.135706
1441.378767	59.398291	66.140711
1440.714895	64.549753	66.145716
1440.285982	52.367229	66.150721
1440.106708	47.125816	66.155726
1438.961836	47.935349	66.160730
1438.203185	47.849335	66.165735
1437.741351	57.648818	66.170740
1437.151747	58.841581	66.175745
1436.301959	48.000063	66.180750
1435.429629	58.914984	66.185754
1434.887634	58.073908	66.190759
1434.555777	52.063582	66.195764
1433.824495	54.581354	66.200769
1432.780394	57.221382	66.205774
1432.095905	51.497327	66.210778
1432.075856	59.313857	66.215783
1431.302974	52.936837	66.220788
1430.066893	53.123818	66.225793
1429.855756	59.587809	66.230798
1429.187084	63.412315	66.235802
1428.529553	55.323407	66.240807
1427.537535	62.215850	66.245812
1426.416176	59.806422	66.250817
1426.288635	59.937050	66.255822
1425.656873	69.881817	66.260826
1425.449485	52.069365	66.265831
1424.868553	58.188455	66.270836
1423.479422	65.229171	66.275841
1422.986656	52.508052	66.280846
1422.240243	72.462063	66.285850
1421.995623	54.015320	66.290855
1421.289873	61.360554	66.295860
1420.132269	69.912955	66.300865
1419.780670	65.339136	66.305870
1419.158893	62.681580	66.310874
1418.823959	58.289608	66.315879
1417.458013	74.324242	66.320884
1417.073771	55.344635	66.325889
1416.889551	51.442768	66.330894
1415.939371	65.146930	66.335898
1415.125070	57.787802	66.340903
1414.817088	69.628534	66.345908
1414.053933	53.000346	66.350913
1413.126430	52.220551	66.355918
1412.018843	62.608356	66.360922
1411.896856	57.442988	66.365927
1411.397292	62.527340	66.370932
1410.878905	53.965338	66.375937
1410.008045	49.869855	66.380942
1408.897222	50.316041	66.385946
1408.890629	55.110733	66.390951
1408.107958	48.878774	66.395956
1406.971558	57.716369	66.400961
1406.641103	49.682709	66.405966
1405.878651	61.824319	66.410970
1405.664487	45.645014	66.415975
1403.952310	64.965671	66.420980
1403.531276	57.143514	66.425985
1403.187557	56.818100	66.430990
1402.533049	67.900250	66.435994
1402.520874	58.209168	66.440999
1401.349929	58.686989	66.446004
1400.266276	60.237396	66.451009
1400.229387	53.267185	66.456014
1399.452526	56.910208	66.461018
1399.096398	55.560229	66.466023
1397.664535	59.528130	66.471028
1397.061037	65.288135	66.476033
1396.898175	58.210220	66.481038
1396.112668	57.619160	66.486042
1395.379862	56.551394	66.491047
1394.685945	59.813825	66.496052
1394.251233	59.118122	66.501057
1393.828063	49.616949	66.506062
1392.198811	68.142310	66.511066
1392.050180	56.870825	66.516071
1391.345061	50.468858	66.521076
1391.023862	63.811283	66.526081
1389.963164	57.363339	66.531086
1389.294083	57.758237	66.536090
1389.196205	52.677345	66.541095
1388.385694	58.415066	66.546100
1387.045549	59.369196	66.551105
1386.415184	64.365541	66.556110
1385.816027	53.082102	66.561114
1385.725341	57.568480	66.566119
1385.292645	51.381816	66.571124
1384.349374	61.142724	66.576129
1383.630714	50.516914	66.581134
1382.681398	51.475148	66.586138
1382.495054	50.241677	66.591143
1381.064291	60.242495	66.596148
1380.771212	60.153448	66.601153
1380.010953	43.146379	66.606158
1379.761393	63.920213	66.611162
1378.922100	43.913895	66.616167
1377.968723	50.453296	66.621172
1377.070389	59.161600	66.626177
1377.002010	50.936483	66.631182
1376.327242	58.801894	66.636186
1375.411785	43.872576	66.641191
1374.835745	62.113826	66.646196
1373.991240	56.248078	66.651201
1373.854309	52.080092	66.656206
1372.934460	59.948196	66.661210
1372.220266	46.366640	66.666215
1371.415021	64.734210	66.671220
1370.959129	53.464270	66.676225
1370.948979	47.530544	66.681230
1370.051590	57.355118	66.686234
1369.391752	56.288375	66.691239
1368.280632	50.857653	66.696244
1367.138918	55.839097	66.701249
1366.806038	57.205518	66.706254
1366.083039	64.452586	66.711258
1365.839593	61.121501	66.716263
1365.106184	58.730850	66.721268
1364.162458	52.650658	66.726273
1363.791907	53.453819	66.731278
1363.153803	54.217516	66.736282
1362.476322	45.838511	66.741287
1361.512903	54.126679	66.746292
1360.673177	50.442558	66.751297
1360.261778	48.060642	66.756302
1359.716563	55.023992	66.761306
1359.128094	45.080781	66.766311
1358.198181	61.527049	66.771316
1357.284203	61.897813	66.776321
1357.322204	53.058154	66.781326
1356.539904	52.906541	66.786330
1355.854402	54.250176	66.791335
1354.892111	62.757356	66.796340
1354.219343	62.796478	66.801345
1353.912766	52.250240	66.806350
1353.246064	72.238889	66.811354
1352.201061	52.989057	66.816359
1351.698467	59.269161	66.821364
1350.869502	53.008313	66.826369
1350.757214	53.686845	66.831374
1349.914579	60.088812	66.836378
1349.523403	51.289000	66.841383
1348.685330	50.789885	66.846388
1347.859546	58.332398	66.851393
1346.902178	51.407607	66.856398
1345.947157	53.951509	66.861402
1345.992549	65.521606	66.866407
1345.276714	57.738444	66.871412
1344.561637	51.290770	66.876417
1344.022294	53.789089	66.881422
1343.163728	57.738413	66.886426
1342.713599	58.953175	66.891431
1341.915804	53.893677	66.896436
1340.898875	65.375628	66.901441
1340.374404	49.081675	66.906446
1339.671075	60.821256	66.911450
1339.602239	52.700289	66.916455
1338.815055	38.408154	66.921460
1337.230752	59.219139	66.926465
1336.954869	45.612068	66.931470
1336.489900	65.004120	66.936474
1336.134174	47.795568	66.941479
1335.864851	57.720563	66.946484
1334.292789	56.316334	66.951489
1334.243692	41.224076	66.956494
1333.448956	52.675426	66.961498
1332.538484	45.501929	66.966503
1331.685916	43.570180	66.971508
1331.269909	40.864169	66.976513
1331.001031	47.031424	66.981518
1329.941868	53.210788	66.986522
1328.980984	64.817866	66.991527
1328.458850	56.207600	66.996532
1327.884078	50.503982	67.001537
1327.723875	45.101866	67.006542
1326.830884	64.796917	67.011546
1325.801603	47.441578	67.016551
1325.580813	56.991447	67.021556
1324.916551	58.612395	67.026561
1324.222966	50.128734	67.031566
1323.185543	54.436063	67.036570
1323.024177	50.182087	67.041575
1322.355783	42.588508	67.046580
1320.994810	53.139614	67.051585
1320.868436	51.647470	67.056590
1319.723435	53.523034	67.061594
1319.335794	60.570145	67.066599
1319.167997	47.475719	67.071604
1317.858417	66.964210	67.076609
1317.339279	45.823717	67.081614
1316.787594	65.322590	67.086618
1316.382179	47.875953	67.091623
1315.244439	58.017858	67.096628
1314.271354	59.137583	67.101633
1314.338394	42.226085	67.106638
1313.486459	61.193980	67.111642
1312.730289	59.010380	67.116647
1311.826870	53.131948	67.121652
1311.030902	56.109442	67.126657
1311.234033	51.743903	67.131662
1310.520748	52.145849	67.136666
1309.495561	54.178977	67.141671
1308.720604	50.749491	67.146676
1308.131197	60.529847	67.151681
1308.103631	59.925536	67.156686
1306.771389	63.715229	67.161690
1305.888418	51.701126	67.166695
1305.422494	57.820872	67.171700
1304.954946	55.872068	67.176705
1304.667187	49.205090	67.181710
1303.349044	57.707361	67.186714
1302.515213	59.262240	67.191719
1302.512460	55.763594	67.196724
1301.631487	58.112822	67.201729
1301.024132	44.943218	67.206734
1299.955712	53.722733	67.211738
1299.819521	48.547024	67.216743
1299.167101	51.000255	67.221748
1298.291749	60.975877	67.226753
1297.640846	54.946921	67.231758
1296.867187	60.183671	67.236762
1296.495863	52.516057	67.241767
1295.219427	47.512180	67.246772
1294.491025	54.214522	67.251777
1294.103689	47.892943	67.256782
1293.578631	60.023632	67.261786
1293.368171	60.813964	67.266791
1292.902589	55.947653	67.271796
1291.623793	56.428480	67.276801
1291.246841	45.538657	67.281806
1290.262822	53.568362	67.286810
1289.620581	61.732952	67.291815
1288.913530	50.379977	67.296820
1288.070297	50.821513	67.301825
1287.658277	53.425748	67.306830
1287.277813	61.504564	67.311834
1286.455929	46.342805	67.316839
1285.637123	45.110561	67.321844
1285.008198	54.818356	67.326849
1284.615019	43.759239	67.331854
1283.627671	53.186573	67.336858
1282.986162	54.094325	67.341863
1282.587330	47.271558	67.346868
1281.850045	49.566408	67.351873
1281.328256	46.282748	67.356878
1280.111244	46.246008	67.361882
1279.415401	58.255626	67.366887
1279.366966	57.063310	67.371892
1278.609836	60.953950	67.376897
1277.893410	52.738849	67.381902
1277.263653	53.846572	67.386906
1276.676179	61.519937	67.391911
1276.074515	60.959604	67.396916
1274.458583	58.291436	67.401921
1273.947953	54.249108	67.406926
1273.615243	60.653589	67.411930
1273.443149	57.255981	67.416935
1273.120739	56.730090	67.421940
1271.775702	72.362502	67.426945
1271.437466	55.553282	67.431950
1270.701066	62.791461	67.436954
1269.815262	57.280807	67.441959
1268.964978	61.768123	67.446964
1268.000801	63.514040	67.451969
1267.927716	63.126690	67.456974
1267.487009	65.305007	67.461978
1266.495372	61.591460	67.466983
1265.814113	49.129013	67.471988
1264.849365	56.108626	67.476993
1264.583987	56.545014	67.481998
1264.296330	62.243782	67.487002
1263.376511	53.201637	67.492007
1263.076725	50.642728	67.497012
1262.072741	57.013605	67.502017
1261.390098	51.636223	67.507022
1260.531355	56.629481	67.512026
1259.727379	55.462692	67.517031
1259.486594	56.439187	67.522036
1258.642723	58.118671	67.527041
1258.202819	54.169174	67.532046
1257.222429	60.772831	67.537050
1256.589756	55.911022	67.542055
1256.360553	47.399275	67.547060
1255.102741	55.623906	67.552065
1254.596000	52.612232	67.557070
1253.944995	50.148594	67.562074
1253.714117	54.092745	67.567079
1252.562085	53.219409	67.572084
1251.102432	54.512715	67.577089
1251.169582	51.023456	67.582094
1250.913332	61.208133	67.587098
1250.284094	60.477158	67.592103
1249.998291	55.978063	67.597108
1248.594981	63.615590	67.602113
1248.407750	50.992595	67.607118
1247.607402	46.914348	67.612122
1246.609869	59.164321	67.617127
1245.778923	49.433158	67.622132
1245.114923	54.333955	67.627137
1244.522356	50.109133	67.632142
1244.292432	57.586881	67.637146
1243.558395	53.411361	67.642151
1243.159857	56.847618	67.647156
1242.262690	60.151866	67.652161
1241.840981	52.869146	67.657166
1240.621594	52.623079	67.662170
1239.457295	73.599133	67.667175
1239.492344	48.751643	67.672180
1238.886315	55.669490	67.677185
1238.410746	55.067039	67.682190
1237.391649	48.685093	67.687194
1236.564948	61.095552	67.692199
1236.255993	53.939974	67.697204
1235.779528	55.945795	67.702209
1235.265683	45.845687	67.707214
1234.158113	56.495300	67.712218
1233.668176	52.913289	67.717223
1233.256945	50.233343	67.722228
1231.754536	54.067475	67.727233
1231.393653	50.668357	67.732238
1230.927099	52.548031	67.737242
1230.460045	52.710581	67.742247
1229.669862	48.870406	67.747252
1228.531410	55.595394	67.752257
1228.245730	49.740183	67.757262
1227.763164	71.560251	67.762266
1227.118540	63.956606	67.767271
1226.138875	54.931878	67.772276
1225.209137	58.827903	67.777281
1225.140592	48.500875	67.782286
1224.289068	68.908400	67.787290
1223.798866	55.253435	67.792295
1223.055687	57.044643	67.797300
1222.313341	60.057788	67.802305
1221.965059	55.562325	67.807310
1221.141119	59.594483	67.812314
1219.910709	54.034578	67.817319
1219.599465	51.023361	67.822324
1218.896166	63.019985	67.827329
1218.725512	60.642384	67.832334
1217.847929	47.518936	67.837338
1216.737831	59.113498	67.842343
1216.673054	51.753524	67.847348
1215.873548	54.110324	67.852353
1214.901227	58.848860	67.857358
1214.128413	60.409832	67.862362
1213.720127	58.309704	67.867367
1213.566159	61.003792	67.872372
1211.870415	64.578541	67.877377
1211.627879	59.664162	67.882382
1211.410005	58.872510	67.887386
1210.816423	55.787929	67.892391
1209.748534	55.528822	67.897396
1208.858742	66.563263	67.902401
1208.146412	50.220391	67.907406
1208.153354	56.187682	67.912410
1206.993194	63.871711	67.917415
1206.125895	49.522987	67.922420
1205.248378	56.236448	67.927425
1205.219032	47.834844	67.932430
1205.059437	57.210986	67.937434
1203.848207	55.006755	67.942439
1203.078059	52.003869	67.947444
1202.409055	59.223458	67.952449
1202.009371	57.147195	67.957454
1201.406213	55.628385	67.962458
1200.204244	54.922278	67.967463
1199.808546	51.768386	67.972468
1199.031648	57.168091	67.977473
1198.960291	48.027314	67.982478
1198.026160	57.619667	67.987482
1196.853668	63.686225	67.992487
1196.806659	43.661235	67.997492
1196.251035	58.078506	68.002497
1194.969318	63.725645	68.007502
1194.168964	48.983103	68.012506
1193.628189	61.349674	68.017511
1193.475773	54.913488	68.022516
1192.482744	52.261424	68.027521
1192.334976	55.503273	68.032526
1191.363042	60.527168	68.037530
1190.815444	49.194604	68.042535
1190.316462	60.171621	68.047540
1189.085459	51.595293	68.052545
1188.451926	57.800052	68.057550
1187.743488	58.012038	68.062554
1187.196890	59.426660	68.067559
1187.005513	53.217432	68.072564
1186.260566	54.893820	68.077569
1185.791686	51.242244	68.082574
1184.431419	60.277937	68.087578
1183.615746	57.695434	68.092583
1183.213509	52.759155	68.097588
1182.438314	58.198015	68.102593
1182.544502	58.658891	68.107598
1181.666077	50.879576	68.112602
1180.575117	53.107707	68.117607
1180.338513	51.052818	68.122612
1179.395423	53.361504	68.127617
1178.616744	55.443782	68.132622
1177.772893	60.939292	68.137626
1177.241702	48.356827	68.142631
1176.577439	54.154913	68.147636
1176.209074	59.216854	68.152641
1175.546361	62.674635	68.157646
1174.394868	52.072018	68.162650
1174.014982	60.360471	68.167655
1173.995924	48.762514	68.172660
1172.819211	65.867778	68.177665
1172.070284	52.023760	68.182670
1171.351147	58.048183	68.187674
1170.725318	52.084663	68.192679
1170.391109	54.943027	68.197684
1169.537788	61.863951	68.202689
1168.575723	62.701296	68.207694
1167.988219	67.402300	68.212698
1167.557104	60.482192	68.217703
1167.302161	59.630212	68.222708
1166.153987	60.817259	68.227713
1165.507606	56.935311	68.232718
1164.901178	60.614364	68.237722
1164.150990	56.794656	68.242727
1163.453252	55.219940	68.247732
1162.603452	66.156572	68.252737
1162.352732	60.776751	68.257742
1161.875048	54.494798	68.262746
1160.582841	54.236699	68.267751
1159.845669	49.300083	68.272756
1159.457711	49.451644	68.277761
1159.195864	49.799176	68.282766
1158.923432	51.327884	68.287770
1157.227803	55.129714	68.292775
1156.768818	53.968009	68.297780
1156.296118	59.352456	68.302785
1155.638472	49.087597	68.307790
1154.735779	44.915281	68.312794
1154.187580	51.429727	68.317799
1153.633137	55.029554	68.322804
1153.247907	56.027456	68.327809
1152.617348	53.642590	68.332814
1152.004159	58.368179	68.337818
1151.286100	59.824272	68.342823
1150.023569	54.365702	68.347828
1148.859642	66.022465	68.352833
1148.666787	48.520003	68.357838
1148.803433	51.070103	68.362842
1147.542234	57.865104	68.367847
1147.065099	55.780670	68.372852
1146.271381	61.121567	68.377857
1145.725676	54.005240	68.382862
1145.256539	52.192332	68.387866
1144.454334	53.694923	68.392871
1143.699636	61.210412	68.397876
1142.745765	53.001591	68.402881
1142.597366	45.519319	68.407886
1142.076193	58.816275	68.412890
1141.145019	53.371235	68.417895
1140.528324	59.153880	68.422900
1139.960052	57.795108	68.427905
1139.340428	55.645035	68.432910
1138.245376	51.585317	68.437914
1137.679612	61.295705	68.442919
1137.225285	58.127496	68.447924
1136.611934	56.394294	68.452929
1135.702208	55.641735	68.457934
1134.813722	46.851698	68.462938
1134.223037	62.160748	68.467943
1134.140678	53.652470	68.472948
1133.542369	60.094474	68.477953
1132.241602	47.836270	68.482958
1131.713538	53.065531	68.487962
1131.166423	50.031925	68.492967
1130.710658	52.168504	68.497972
1129.563605	61.403683	68.502977
1129.052563	58.805859	68.507982
1128.548896	58.650995	68.512986
1127.862461	62.503622	68.517991
1127.556711	50.867697	68.522996
1126.485473	59.138394	68.528001
1125.736148	58.043375	68.533006
1125.447043	57.086453	68.538010
1124.385932	51.277336	68.543015
1123.712868	42.328469	68.548020
1122.890904	57.871410	68.553025
1122.713214	49.009315	68.558030
1122.273426	53.592216	68.563034
1121.168493	57.904049	68.568039
1120.445691	50.700790	68.573044
1119.504638	53.639917	68.578049
1119.539576	51.831984	68.583054
1119.082458	52.365114	68.588058
1117.929266	59.909302	68.593063
1117.560289	45.095031	68.598068
1116.978502	55.695738	68.603073
1115.974621	53.619408	68.608078
1115.231053	51.932156	68.613082
1114.415848	56.691462	68.618087
1114.134577	42.664288	68.623092
1113.044783	59.407249	68.628097
1112.325789	61.970456	68.633102
1111.596810	52.440736	68.638106
1111.305818	54.388691	68.643111
1110.840238	44.889614	68.648116
1110.503186	52.893726	68.653121
1109.287070	52.552591	68.658126
1108.671859	44.545372	68.663130
1107.984881	48.752880	68.668135
1107.755484	45.870579	68.673140
1106.220129	43.536618	68.678145
1105.549276	59.837649	68.683150
1105.211509	52.856982	68.688154
1105.142738	49.777253	68.693159
1104.722886	51.463448	68.698164
1103.681322	66.399552	68.703169
1102.971186	50.046919	68.708174
1102.359785	44.973630	68.713178
1101.191182	59.993010	68.718183
1100.482407	58.303380	68.723188
1100.013907	54.522459	68.728193
1099.534517	54.869912	68.733198
1099.071437	48.450045	68.738202
1097.898901	51.528497	68.743207
1097.698480	58.596300	68.748212
1096.935337	58.876933	68.753217
1096.288342	49.616438	68.758222
1095.534389	56.401730	68.763226
1094.866377	56.720845	68.768231
1094.500181	60.683377	68.773236
1093.618745	51.518518	68.778241
1092.587745	54.287470	68.783246
1092.293640	48.020488	68.788250
1091.766447	55.255381	68.793255
1091.068806	48.525920	68.798260
1089.919196	67.703620	68.803265
1089.211791	59.696873	68.808270
1088.866758	47.701378	68.813274
1088.420663	49.628279	68.818279
1087.388510	41.830888	68.823284
1086.385553	46.725715	68.828289
1086.139486	57.400747	68.833294
1085.651696	54.463364	68.838298
1084.893065	36.254622	68.843303
1084.811961	54.970613	68.848308
1083.432072	53.179603	68.853313
1082.614794	59.509800	68.858318
1083.000437	54.025609	68.863322
1081.180732	56.081142	68.868327
1080.576906	55.764036	68.873332
1079.754723	40.474707	68.878337
1079.695794	63.334316	68.883342
1079.525871	49.596919	68.888346
1078.791522	60.225057	68.893351
1077.929120	50.831687	68.898356
1077.174051	55.750160	68.903361
1075.991004	51.529438	68.908366
1075.372704	42.865173	68.913370
1074.555765	51.227884	68.918375
1074.488589	39.569797	68.923380
1074.189217	49.384454	68.928385
1073.440468	48.469123	68.933390
1072.631630	47.049295	68.938394
1072.111044	56.142256	68.943399
1071.318052	40.622796	68.948404
1070.071000	59.845952	68.953409
1069.396468	61.571092	68.958414
1069.482172	49.634804	68.963418
1068.239271	51.458245	68.968423
1067.312025	51.958947	68.973428
1066.677592	42.434710	68.978433
1065.912854	50.342867	68.983438
1066.038690	40.073249	68.988442
1065.191818	64.182505	68.993447
1065.258917	45.790363	68.998452
1064.007680	51.024300	69.003457
1063.194258	62.201153	69.008462
1062.717863	43.360922	69.013466
1061.439299	50.445707	69.018471
1060.755433	55.245630	69.023476
1060.282785	63.523619	69.028481
1059.831278	39.772248	69.033486
1059.687422	56.475112	69.038490
1058.586425	67.338195	69.043495
1057.728629	50.543900	69.048500
1057.226054	42.327981	69.053505
1056.511024	44.893722	69.058510
1055.863149	48.391742	69.063514
1054.647661	62.060922	69.068519
1054.552512	45.794971	69.073524
1054.219144	47.186734	69.078529
1053.509760	35.656052	69.083534
1052.281901	51.400757	69.088538
1051.660010	51.433441	69.093543
1051.650915	45.187353	69.098548
1050.759063	49.752300	69.103553
1050.218514	49.013575	69.108558
1049.597720	46.780140	69.113562
1048.845543	51.881075	69.118567
1047.811144	58.455544	69.123572
1046.995307	57.355363	69.128577
1046.303796	56.530275	69.133582
1046.206131	45.323290	69.138586
1045.652685	52.401525	69.143591
1044.586675	35.782297	69.148596
1044.135825	50.080404	69.153601
1043.319334	65.467962	69.158606
1042.352136	50.067679	69.163610
1041.426748	57.296549	69.168615
1041.281658	53.013207	69.173620
1040.872440	45.685978	69.178625
1040.090268	47.447170	69.183630
1039.906022	44.977140	69.188634
1038.435108	56.244405	69.193639
1038.057748	47.043530	69.198644
1037.605817	43.222145	69.203649
1036.663911	52.025768	69.208654
1035.953506	41.562784	69.213658
1035.401001	53.462900	69.218663
1034.995993	40.401550	69.223668
1034.219213	50.743144	69.228673
1033.333713	43.381313	69.233678
1032.900285	50.509836	69.238682
1031.911208	67.135883	69.243687
1031.727088	53.359753	69.248692
1030.480942	43.921812	69.253697
1029.774159	55.231502	69.258702
1029.785826	39.175637	69.263706
1028.861421	41.951304	69.268711
1028.061952	34.157926	69.273716
1027.172078	43.997147	69.278721
1026.598985	31.487643	69.283726
1026.201216	54.497324	69.288730
1025.519044	50.811913	69.293735
1025.034054	37.777486	69.298740
1023.992995	47.295432	69.303745
1023.167216	58.382798	69.308750
1023.015667	43.508734	69.313754
1022.463909	33.329585	69.318759
1021.251025	55.868171	69.323764
1020.843628	40.927591	69.328769
1019.728191	46.933098	69.333774
1019.854786	50.910265	69.338778
1019.108029	62.268896	69.343783
1018.205029	46.945143	69.348788
1017.739827	44.779997	69.353793
1016.906115	54.340649	69.358798
1016.239558	62.931751	69.363802
1015.345612	28.353146	69.368807
1015.217734	65.432760	69.373812
1014.825142	36.744357	69.378817
1013.179255	66.195410	69.383822
1012.965902	36.773634	69.388826
1012.037976	80.300618	69.393831
1011.967047	41.609464	69.398836
1011.067045	42.837512	69.403841
1010.170261	51.566158	69.408846
1009.613103	50.885275	69.413850
1009.072248	46.527721	69.418855
1008.312045	30.120046	69.423860
1007.603787	59.910730	69.428865
1006.757035	35.531612	69.433870
1006.779692	52.288391	69.438874
1006.082353	48.852967	69.443879
1004.957927	46.403227	69.448884
1004.622166	47.893142	69.453889
1003.747654	44.580521	69.458894
1002.767088	39.972831	69.463898
1001.743930	51.681345	69.468903
1001.546436	41.538864	69.473908
1000.958006	48.723589	69.478913
1000.607586	55.127747	69.483918
1000.020042	46.136933	69.488922
998.781245	63.720446	69.493927
998.285740	46.980499	69.498932
997.940980	42.345758	69.503937
997.094234	48.962918	69.508942
996.550367	51.719048	69.513946
995.759802	49.269805	69.518951
995.476161	49.726471	69.523956
994.376501	40.796647	69.528961
993.281418	57.094225	69.533966
993.034721	39.294473	69.538970
992.267657	52.584827	69.543975
992.227154	48.185509	69.548980
991.669692	49.313333	69.553985
990.245093	62.905427	69.558990
990.001393	46.756161	69.563994
989.415608	55.570939	69.568999
988.606366	53.663954	69.574004
987.936728	47.966069	69.579009
986.875221	59.217100	69.584014
986.577521	53.182504	69.589018
985.689735	57.174427	69.594023
984.634331	58.586475	69.599028
984.404504	44.924863	69.604033
983.567028	45.042327	69.609038
983.696967	40.809844	69.614042
982.710642	51.946412	69.619047
981.845482	38.385899	69.624052
981.044151	43.724889	69.629057
980.709340	45.102699	69.634062
980.465268	33.871724	69.639066
978.978504	37.974720	69.644071
978.442367	44.581880	69.649076
978.215987	39.933038	69.654081
977.191028	45.375418	69.659086
976.322558	43.684431	69.664090
975.435008	51.129633	69.669095
974.809715	46.955824	69.674100
974.873910	42.181902	69.679105
974.372886	53.719040	69.684110
973.442231	35.006327	69.689114
972.589837	46.700288	69.694119
972.057817	49.580686	69.699124
971.653794	50.154275	69.704129
970.593566	60.894206	69.709134
970.240415	42.501152	69.714138
969.477388	42.449088	69.719143
968.417038	35.473058	69.724148
967.831647	36.414531	69.729153
967.270755	54.014743	69.734158
967.033345	46.944027	69.739162
966.443327	51.196058	69.744167
965.457561	48.074608	69.749172
964.482521	45.402434	69.754177
963.747445	38.899738	69.759182
963.418022	48.865825	69.764186
963.174688	46.454087	69.769191
962.039666	49.469860	69.774196
961.420368	31.362010	69.779201
960.805430	43.738808	69.784206
960.280208	40.096251	69.789210
959.344031	53.386715	69.794215
958.936165	41.915314	69.799220
958.506698	31.033948	69.804225
957.340066	57.898389	69.809230
956.594300	48.489668	69.814234
955.819805	36.261379	69.819239
955.289485	61.387796	69.824244
955.296294	39.094670	69.829249
953.384104	68.897188	69.834254
953.400683	31.182431	69.839258
952.951128	81.049508	69.844263
952.546227	45.338168	69.849268
951.817706	56.813746	69.854273
950.721864	40.782753	69.859278
950.496720	47.310470	69.864282
949.832406	48.663451	69.869287
948.672889	43.844578	69.874292
947.933460	61.372291	69.879297
947.328162	51.816647	69.884302
947.179098	40.729818	69.889306
946.572843	40.663852	69.894311
945.329444	50.499433	69.899316
944.791375	50.963479	69.904321
944.118255	55.813753	69.909326
943.890205	43.894297	69.914330
942.557638	51.668928	69.919335
941.702396	45.721491	69.924340
941.386100	53.181446	69.929345
941.444693	53.782341	69.934350
940.814081	52.961784	69.939354
939.495473	48.284918	69.944359
938.616680	52.712211	69.949364
938.555362	53.302228	69.954369
937.866937	50.489841	69.959374
937.185330	60.833660	69.964378
936.709958	50.397959	69.969383
935.862439	50.725181	69.974388
934.581527	50.186297	69.979393
933.434078	48.908705	69.984398
933.075571	51.758344	69.989402
932.901862	52.700539	69.994407
932.493941	39.581342	69.999412
932.363675	40.205983	70.004417
930.867327	68.895303	70.009422
930.525056	31.089438	70.014426
929.685945	64.464640	70.019431
929.365371	40.753987	70.024436
928.575738	35.015302	70.029441
927.697619	47.795088	70.034446
927.571439	44.708739	70.039450
926.332750	40.254117	70.044455
925.233268	64.655879	70.049460
924.994264	45.284366	70.054465
923.785764	43.322679	70.059470
923.896746	46.718884	70.064474
923.335114	48.408746	70.069479
923.062725	51.818657	70.074484
922.259639	47.980644	70.079489
921.345237	45.354027	70.084494
920.188358	41.849847	70.089498
919.175283	70.110625	70.094503
918.889009	50.081195	70.099508
918.480883	51.549523	70.104513
917.877590	53.987139	70.109518
917.691583	45.785530	70.114522
916.561074	54.895152	70.119527
915.926800	45.586970	70.124532
915.431020	45.795148	70.129537
914.048317	56.428728	70.134542
913.770821	42.270128	70.139546
913.420024	47.110109	70.144551
912.919915	42.151623	70.149556
911.833748	49.631603	70.154561
910.616689	57.108765	70.159566
910.470903	49.769602	70.164570
910.216329	65.149750	70.169575
909.280012	56.309077	70.174580
908.425450	41.616305	70.179585
907.632918	49.722873	70.184590
907.437937	40.929799	70.189594
907.050351	50.253903	70.194599
906.107246	46.170115	70.199604
905.525184	43.090093	70.204609
904.473566	45.267921	70.209614
904.032254	47.656108	70.214618
903.135662	47.887078	70.219623
902.230138	41.272768	70.224628
902.008434	47.032010	70.229633
901.403878	39.138278	70.234638
900.997552	47.844083	70.239642
899.819154	52.494101	70.244647
899.195920	42.641732	70.249652
899.179370	47.713930	70.254657
897.962445	59.483277	70.259662
897.206499	49.934282	70.264666
896.751477	52.125969	70.269671
896.187804	50.898979	70.274676
895.664102	42.244950	70.279681
894.432863	47.950410	70.284686
893.957751	57.119726	70.289690
893.698405	55.681886	70.294695
892.797044	48.415672	70.299700
892.087792	45.385856	70.304705
891.138951	49.532593	70.309710
890.963387	45.952666	70.314714
890.519932	50.417913	70.319719
889.357236	36.357634	70.324724
888.454134	57.719500	70.329729
887.959040	39.125156	70.334734
887.663301	55.779635	70.339738
886.949467	48.612879	70.344743
885.737794	35.911762	70.349748
885.536800	43.692388	70.354753
884.874590	49.751961	70.359758
884.321359	37.720284	70.364762
883.173528	30.870178	70.369767
882.478572	49.497757	70.374772
882.292599	44.410438	70.379777
881.682135	48.689391	70.384782
880.920237	34.089119	70.389786
880.138251	37.578559	70.394791
879.464997	55.469454	70.399796
879.149240	54.299199	70.404801
877.822375	45.746196	70.409806
877.015163	45.477280	70.414810
876.632901	48.717034	70.419815
876.065127	35.300045	70.424820
875.899525	47.542265	70.429825
875.143407	52.648599	70.434830
874.304894	44.237057	70.439834
873.727241	51.979870	70.444839
873.102797	47.850108	70.449844
872.223656	29.362637	70.454849
871.184823	60.122080	70.459854
870.703636	45.262671	70.464858
870.313882	57.409696	70.469863
869.843832	55.328925	70.474868
869.327771	40.194391	70.479873
868.465588	40.523970	70.484878
868.013517	53.213887	70.489882
866.849857	43.379740	70.494887
865.728390	38.810306	70.499892
865.555545	59.573430	70.504897
865.115110	38.587767	70.509902
864.557967	41.256152	70.514906
863.583304	55.170891	70.519911
862.951987	49.172075	70.524916
862.592569	42.565472	70.529921
861.966058	50.293987	70.534926
861.076863	43.443719	70.539930
860.530509	54.496102	70.544935
859.730873	47.846030	70.549940
858.954128	48.518383	70.554945
857.901946	56.420303	70.559950
857.543020	52.795451	70.564954
857.048586	56.846222	70.569959
856.774380	53.326150	70.574964
856.266550	49.267711	70.579969
854.716437	59.385527	70.584974
854.379474	64.492959	70.589978
854.027142	45.950009	70.594983
852.796895	59.369305	70.599988
852.280209	58.869661	70.604993
851.475182	53.051452	70.609998
851.553482	47.819576	70.615002
850.960243	48.443800	70.620007
849.572126	47.888909	70.625012
849.266777	47.111215	70.630017
848.582110	49.173892	70.635022
847.642804	60.331401	70.640026
846.840221	53.322278	70.645031
846.035657	51.791466	70.650036
845.704348	42.189099	70.655041
845.035703	60.762047	70.660046
845.005371	62.020451	70.665050
843.974766	36.158491	70.670055
843.163607	48.352086	70.675060
843.004737	47.981559	70.680065
841.753481	64.975783	70.685070
841.152721	57.299063	70.690074
840.229676	48.836337	70.695079
839.440474	51.260986	70.700084
839.570737	47.569310	70.705089
838.703773	54.194463	70.710094
837.770669	40.001478	70.715098
837.271197	51.793827	70.720103
836.480893	64.561246	70.725108
836.531645	50.418215	70.730113
835.340937	54.806885	70.735118
834.633118	58.707134	70.740122
833.992925	52.779120	70.745127
832.979508	62.754753	70.750132
831.948145	51.767379	70.755137
831.526876	55.019657	70.760142
831.323802	50.013908	70.765146
830.830278	67.650722	70.770151
830.218490	44.645582	70.775156
829.496245	42.038873	70.780161
828.419789	62.365549	70.785166
828.421974	61.291338	70.790170
827.912281	44.162657	70.795175
826.836609	71.965085	70.800180
825.648643	36.512519	70.805185
825.320259	68.250076	70.810190
824.887681	50.383760	70.815194
824.386911	58.040234	70.820199
823.504252	37.959139	70.825204
823.028800	48.014700	70.830209
822.016757	62.206625	70.835214
821.123443	64.468093	70.840218
820.507779	52.343869	70.845223
820.015587	48.262451	70.850228
819.601327	43.419625	70.855233
818.408861	70.455369	70.860238
818.124207	45.838649	70.865242
817.464906	54.160559	70.870247
816.911763	78.232559	70.875252
816.212208	59.877332	70.880257
815.358810	35.059447	70.885262
815.004984	81.918371	70.890266
814.268471	75.121070	70.895271
813.263261	38.308551	70.900276
812.406413	63.201529	70.905281
811.988902	39.857993	70.910286
811.548181	68.972202	70.915290
811.352730	38.880646	70.920295
809.846294	47.807307	70.925300
809.479268	67.762458	70.930305
808.862160	44.324541	70.935310
808.654985	76.455952	70.940314
807.570702	43.443622	70.945319
806.534439	52.524087	70.950324
806.181835	45.701957	70.955329
805.720029	62.338721	70.960334
805.325772	40.837982	70.965338
804.545400	38.836586	70.970343
803.520486	46.808290	70.975348
802.881966	39.803035	70.980353
801.822899	61.263856	70.985358
801.238776	49.640792	70.990362
801.194685	39.656845	70.995367
800.601242	56.976837	71.000372
799.800485	48.860492	71.005377
798.381294	45.558968	71.010382
798.015520	37.734485	71.015386
797.711617	54.697742	71.020391
797.048787	48.762308	71.025396
796.258644	33.239383	71.030401
795.344777	63.195249	71.035406
794.920659	32.660750	71.040410
794.553973	65.739985	71.045415
793.692783	29.480130	71.050420
792.883031	69.626396	71.055425
792.183204	38.295314	71.060430
791.662136	57.131754	71.065434
791.308359	60.789583	71.070439
790.297417	48.977442	71.075444
789.927090	39.441223	71.080449
789.368080	70.097501	71.085454
788.411153	28.321286	71.090458
787.469629	53.344415	71.095463
787.011870	36.781467	71.100468
786.549019	55.099313	71.105473
785.852153	50.197409	71.110478
784.809949	48.776984	71.115482
784.321615	39.046677	71.120487
783.639068	66.789670	71.125492
783.557229	31.293519	71.130497
782.417174	67.047216	71.135502
781.670121	39.452919	71.140506
781.560274	63.679811	71.145511
780.127691	53.801792	71.150516
779.542794	43.493959	71.155521
778.762164	74.207602	71.160526
778.449971	50.710110	71.165530
778.362975	44.020734	71.170535
777.368750	60.113091	71.175540
777.171302	43.005682	71.180545
776.108677	47.936921	71.185550
774.997183	49.151415	71.190554
773.808103	50.657364	71.195559
773.221317	38.317274	71.200564
772.751486	61.106615	71.205569
772.743897	55.088947	71.210574
772.395063	48.860697	71.215578
771.589244	42.497057	71.220583
770.303689	50.729451	71.225588
769.676431	40.480404	71.230593
769.439466	63.513355	71.235598
768.479809	52.016314	71.240602
767.864950	32.868696	71.245607
766.884892	46.128338	71.250612
766.974324	63.461040	71.255617
766.039156	44.512626	71.260622
764.998697	57.961656	71.265626
764.814675	45.227880	71.270631
763.931400	53.836176	71.275636
763.729860	38.020870	71.280641
762.355665	38.715833	71.285646
761.545882	52.027215	71.290650
761.279597	47.911423	71.295655
760.613745	30.779263	71.300660
760.366599	47.042812	71.305665
759.526320	44.860168	71.310670
758.973332	32.014847	71.315674
757.959250	62.360380	71.320679
756.922443	37.041905	71.325684
756.217622	51.833010	71.330689
756.069707	36.252006	71.335694
755.433301	67.119279	71.340698
755.089932	26.760771	71.345703
754.258468	64.348093	71.350708
753.771334	31.986615	71.355713
752.460092	67.051678	71.360718
751.428775	33.480662	71.365722
751.418256	51.652376	71.370727
750.279125	60.490636	71.375732
750.594031	36.106488	71.380737
749.686700	65.257125	71.385742
748.574323	40.985097	71.390746
747.831205	43.514391	71.395751
747.158311	66.776009	71.400756
746.585530	50.672892	71.405761
746.411038	38.350744	71.410766
745.326259	67.341991	71.415770
745.166286	33.023587	71.420775
744.219827	56.100101	71.425780
743.743433	50.721589	71.430785
742.533138	47.762131	71.435790
742.116818	68.619201	71.440794
741.921815	49.124047	71.445799
740.565609	51.284208	71.450804
740.137274	58.266880	71.455809
739.477647	41.737660	71.460814
738.926844	52.860143	71.465818
738.202784	50.042453	71.470823
737.122057	49.542757	71.475828
736.556820	46.758125	71.480833
735.877662	49.975785	71.485838
735.706249	50.288462	71.490842
735.462018	48.624322	71.495847
734.352745	59.323250	71.500852
733.794314	46.243840	71.505857
733.446770	48.088877	71.510862
732.277872	60.296886	71.515866
731.635538	47.245026	71.520871
730.907303	54.515128	71.525876
730.070834	41.901011	71.530881
729.160380	40.201031	71.535886
728.495249	50.605326	71.540890
728.438440	47.591521	71.545895
727.918232	58.086281	71.550900
727.403129	48.506894	71.555905
726.261525	55.226264	71.560910
725.531541	54.084139	71.565914
725.370060	46.772732	71.570919
723.981251	54.159049	71.575924
723.456735	56.396519	71.580929
722.719814	43.575755	71.585934
722.432540	55.335905	71.590938
721.918106	48.478062	71.595943
720.777813	49.578900	71.600948
720.318328	35.982311	71.605953
719.819303	37.873544	71.610958
719.106361	46.749597	71.615962
718.108951	44.875821	71.620967
717.144877	43.097655	71.625972
717.098115	44.612546	71.630977
716.371353	44.833888	71.635982
715.738618	63.010069	71.640986
715.472317	46.717830	71.645991
714.413270	55.600116	71.650996
714.068846	42.921852	71.656001
712.809801	45.131207	71.661006
712.191776	45.980168	71.666010
711.700057	54.122458	71.671015
711.081117	42.791963	71.676020
710.623230	41.631747	71.681025
709.996268	53.568977	71.686030
709.198844	52.328792	71.691034
708.750335	22.162496	71.696039
707.659582	52.018781	71.701044
706.835154	50.997349	71.706049
706.110842	54.991710	71.711054
705.740753	54.088734	71.716058
705.403512	41.667934	71.721063
704.713181	52.180319	71.726068
703.512282	36.749645	71.731073
702.893593	55.943804	71.736078
702.426248	59.285433	71.741082
702.427018	43.079979	71.746087
700.999926	40.967141	71.751092
700.456453	57.257381	71.756097
699.926030	50.077258	71.761102
699.227563	38.412526	71.766106
698.768947	34.716854	71.771111
697.646109	50.383449	71.776116
697.237489	43.738986	71.781121
696.797600	41.290775	71.786126
696.253832	59.287217	71.791130
695.169594	51.045753	71.796135
694.426095	55.831599	71.801140
694.187713	55.290828	71.806145
692.899031	42.231528	71.811150
691.889971	48.434672	71.816154
691.581983	42.327662	71.821159
690.835882	59.720852	71.826164
690.975490	47.824902	71.831169
690.575868	43.615243	71.836174
689.557343	32.108710	71.841178
688.847242	50.491149	71.846183
688.292382	32.292740	71.851188
687.133273	42.594356	71.856193
686.386360	53.853721	71.861198
685.426053	36.842588	71.866202
685.526920	57.729241	71.871207
684.891815	37.768069	71.876212
684.255459	49.314158	71.881217
683.372269	49.951477	71.886222
682.811017	47.640857	71.891226
682.756001	29.604119	71.896231
681.201973	52.359516	71.901236
680.682809	57.844456	71.906241
680.211117	44.450077	71.911246
679.062116	37.075172	71.916250
678.433637	46.596907	71.921255
677.550564	33.545572	71.926260
677.610183	45.370315	71.931265
677.009970	52.782457	71.936270
676.198663	40.799832	71.941274
675.501069	39.103821	71.946279
674.909462	33.491384	71.951284
674.290210	52.499560	71.956289
673.391612	42.043036	71.961294
672.331312	40.986641	71.966298
672.053212	35.305359	71.971303
671.651069	36.235063	71.976308
670.961163	47.597304	71.981313
670.160009	35.089554	71.986318
669.406567	39.112212	71.991322
669.356233	22.627938	71.996327
668.136722	46.982599	72.001332
667.354357	28.235421	72.006337
666.976707	27.849287	72.011342
666.274532	38.100220	72.016346
665.434110	64.162192	72.021351
664.296138	35.335629	72.026356
664.085075	23.085562	72.031361
663.646227	57.462948	72.036366
663.043438	29.402674	72.041370
662.560868	46.153105	72.046375
661.376882	24.175851	72.051380
660.805297	58.629566	72.056385
660.597139	33.352660	72.061390
659.126712	28.499880	72.066394
658.550416	40.503148	72.071399
657.942015	39.482022	72.076404
657.869910	31.322246	72.081409
657.480815	37.215372	72.086414
656.094398	50.669058	72.091418
655.553746	37.053879	72.096423
654.879814	29.270623	72.101428
654.558981	47.688835	72.106433
653.514449	52.568358	72.111438
652.682866	40.689890	72.116442
652.149787	31.654261	72.121447
651.455209	60.111887	72.126452
651.351732	40.289980	72.131457
650.378571	33.271842	72.136462
649.386709	45.967304	72.141466
649.129596	50.492787	72.146471
648.733451	41.206703	72.151476
647.832626	39.317575	72.156481
647.022291	43.398183	72.161486
646.198153	37.567334	72.166490
646.177669	36.302784	72.171495
645.230309	40.815194	72.176500
644.559260	49.709821	72.181505
644.116977	42.517258	72.186510
642.534439	41.309093	72.191514
642.318703	23.860902	72.196519
641.539195	42.948201	72.201524
640.933753	48.661336	72.206529
640.810525	42.745671	72.211534
639.637424	46.500879	72.216538
639.181447	39.116547	72.221543
637.906776	40.164710	72.226548
637.748598	32.945831	72.231553
637.535285	42.669516	72.236558
636.147261	40.370735	72.241562
635.727394	30.087140	72.246567
635.281670	38.020267	72.251572
634.867537	49.884187	72.256577
633.786389	29.082667	72.261582
632.715283	42.407297	72.266586
632.442021	36.920780	72.271591
632.126374	50.025764	72.276596
631.506995	39.923737	72.281601
630.442897	32.792367	72.286606
629.751758	52.504230	72.291610
629.562393	35.827638	72.296615
628.263958	44.658189	72.301620
627.371382	41.577234	72.306625
627.245886	42.817677	72.311630
626.701145	50.373946	72.316634
626.341128	34.542921	72.321639
625.012029	33.155643	72.326644
624.465211	40.174532	72.331649
624.066180	41.537381	72.336654
623.551843	48.670942	72.341658
622.861048	33.389307	72.346663
621.527763	47.030070	72.351668
621.201746	35.192523	72.356673
620.661045	48.995625	72.361678
619.714202	17.237289	72.366682
619.053871	44.609290	72.371687
618.455226	46.341377	72.376692
618.404962	39.649324	72.381697
617.724544	30.880006	72.386702
616.303431	44.501643	72.391706
615.874119	36.294687	72.396711
615.420721	47.321245	72.401716
614.770083	42.774713	72.406721
613.681126	40.220171	72.411726
612.809572	44.892396	72.416730
612.795634	33.717885	72.421735
612.325261	37.189306	72.426740
611.765224	40.886306	72.431745
610.863483	29.665549	72.436750
610.045763	39.107049	72.441754
609.627571	43.673956	72.446759
608.764125	39.799944	72.451764
607.790298	39.193399	72.456769
607.431538	33.865575	72.461774
606.627810	34.468188	72.466778
605.929372	33.366805	72.471783
605.015144	30.029130	72.476788
604.584556	39.839454	72.481793
604.207947	35.676610	72.486798
603.673454	30.312125	72.491802
602.808689	30.960729	72.496807
601.926699	28.127243	72.501812
601.441349	34.620713	72.506817
601.556576	32.408941	72.511822
600.009307	41.402127	72.516826
599.461410	32.947577	72.521831
598.896440	33.103763	72.526836
598.291039	39.043961	72.531841
597.152308	36.901027	72.536846
596.280391	49.683051	72.541850
596.392019	33.190329	72.546855
595.934839	40.182331	72.551860
595.029740	44.074632	72.556865
594.355879	36.647751	72.561870
593.347730	48.752928	72.566874
592.993286	34.478953	72.571879
592.011323	46.373391	72.576884
591.101153	43.194333	72.581889
590.552544	37.108324	72.586894
589.803051	43.219699	72.591898
589.736136	40.816176	72.596903
589.415399	38.358471	72.601908
588.376046	42.322616	72.606913
587.946856	34.068344	72.611918
586.819465	49.395094	72.616922
586.096661	34.825001	72.621927
585.346731	37.937279	72.626932
584.779721	36.343491	72.631937
584.483188	35.447742	72.636942
583.696864	37.009468	72.641946
582.930699	36.388780	72.646951
581.996742	43.456724	72.651956
581.593835	42.254664	72.656961
581.265956	37.089071	72.661966
580.182987	35.735149	72.666970
579.632971	35.546782	72.671975
579.028875	38.407191	72.676980
578.489590	41.689334	72.681985
578.051681	25.738285	72.686990
576.771484	33.574110	72.691994
576.335281	38.468718	72.696999
575.749203	36.239346	72.702004
575.113206	45.550995	72.707009
574.208019	41.160131	72.712014
573.418814	36.085365	72.717018
573.061233	40.205834	72.722023
572.453408	37.667710	72.727028
571.738659	36.896919	72.732033
571.389458	38.187188	72.737038
570.261075	47.831139	72.742042
569.933650	35.856643	72.747047
569.066397	50.465497	72.752052
567.888631	41.283432	72.757057
568.279363	24.657965	72.762062
567.159912	40.529035	72.767066
566.444332	42.292373	72.772071
565.391692	35.843562	72.777076
565.073813	47.632230	72.782081
564.699131	41.952156	72.787086
564.095501	45.441658	72.792090
563.136739	40.989951	72.797095
562.466280	43.443071	72.802100
561.720207	38.448165	72.807105
561.793678	29.196111	72.812110
560.247779	47.899331	72.817114
559.795199	39.480066	72.822119
559.264233	37.669246	72.827124
558.242243	37.865123	72.832129
557.490636	37.592184	72.837134
556.702343	32.517281	72.842138
556.373200	40.452346	72.847143
556.037683	40.789598	72.852148
555.565007	39.423625	72.857153
554.851612	26.878305	72.862158
553.994014	36.865450	72.867162
553.739355	34.249001	72.872167
552.665856	34.907218	72.877172
551.601830	44.641840	72.882177
551.545941	30.493779	72.887182
550.802600	42.402250	72.892186
549.988679	31.850308	72.897191
548.973964	40.848571	72.902196
548.436180	38.341872	72.907201
548.363161	30.431397	72.912206
546.953317	46.572649	72.917210
546.429385	34.181638	72.922215
545.979801	37.315465	72.927220
545.345529	34.366852	72.932225
545.082983	36.332402	72.937230
543.606745	37.278688	72.942234
543.084131	31.537038	72.947239
542.705519	38.068705	72.952244
542.165525	31.554014	72.957249
541.840982	32.572294	72.962254
540.417445	30.127850	72.967258
540.209285	32.272382	72.972263
539.393046	38.887952	72.977268
538.640963	37.031940	72.982273
537.744008	30.402237	72.987278
537.074704	36.228053	72.992282
536.995072	34.649674	72.997287
536.398807	33.330200	73.002292
535.095356	33.870523	73.007297
535.102290	29.291808	73.012302
534.229739	38.712099	73.017306
533.569897	36.388839	73.022311
532.925037	39.714614	73.027316
532.148072	36.180071	73.032321
531.633651	25.488976	73.037326
530.739356	46.939347	73.042330
529.791724	37.077293	73.047335
529.124048	42.961198	73.052340
528.796070	29.515607	73.057345
528.668832	31.070123	73.062350
527.251573	27.952951	73.067354
526.285614	28.646083	73.072359
526.265409	30.684986	73.077364
525.300489	34.744522	73.082369
525.207837	35.653329	73.087374
523.765791	38.109530	73.092378
523.420686	34.616575	73.097383
522.547573	30.215896	73.102388
522.091969	36.431844	73.107393
522.068750	33.180906	73.112398
520.831429	43.398853	73.117402
520.331758	39.996746	73.122407
519.711613	38.007766	73.127412
518.630749	46.541948	73.132417
517.876897	29.061245	73.137422
517.233721	38.574302	73.142426
516.892575	42.662199	73.147431
516.758806	41.806756	73.152436
515.603186	41.664418	73.157441
515.381139	29.176448	73.162446
514.276357	48.129516	73.167450
513.962565	40.353584	73.172455
512.887143	40.712523	73.177460
512.188279	47.158028	73.182465
511.964209	29.119877	73.187470
511.066472	43.661056	73.192474
510.085818	35.996092	73.197479
509.527368	30.540839	73.202484
508.933914	42.397056	73.207489
508.605141	36.394314	73.212494
507.299380	38.380988	73.217498
506.522354	37.631176	73.222503
505.983878	42.592546	73.227508
505.878170	42.358643	73.232513
505.306728	35.672364	73.237518
504.711010	44.826229	73.242522
504.201605	31.623998	73.247527
503.284491	33.715905	73.252532
501.761929	40.253210	73.257537
501.362676	33.883255	73.262542
500.906776	35.726658	73.267546
500.392500	34.856147	73.272551
500.127822	27.865554	73.277556
498.692076	43.362864	73.282561
498.131708	34.727417	73.287566
497.669179	41.704514	73.292570
497.253183	42.240662	73.297575
496.987049	35.001156	73.302580
495.757203	40.403808	73.307585
495.265320	31.505158	73.312590
494.332172	41.967949	73.317594
493.637285	38.838207	73.322599
492.709017	30.836925	73.327604
492.066490	45.708010	73.332609
491.915361	35.468365	73.337614
491.120497	53.258817	73.342618
490.924256	39.923119	73.347623
490.056393	35.281934	73.352628
489.342600	49.746513	73.357633
488.912545	30.971680	73.362638
487.512944	38.695690	73.367642
486.794459	40.579353	73.372647
487.144948	40.230197	73.377652
485.619479	46.525142	73.382657
485.073733	36.759923	73.387662
484.057582	49.908700	73.392666
483.553545	44.709691	73.397671
483.305010	45.339003	73.402676
482.730235	43.848972	73.407681
482.393788	36.021468	73.412686
481.178449	40.587663	73.417690
480.756462	44.120778	73.422695
480.180113	31.482694	73.427700
478.774633	50.717053	73.432705
478.497623	39.073569	73.437710
477.697907	48.321438	73.442714
477.562634	43.645536	73.447719
476.730391	36.901475	73.452724
475.699863	43.600086	73.457729
475.421514	36.458717	73.462734
475.033306	35.645392	73.467738
474.289424	37.925739	73.472743
473.027991	45.930501	73.477748
472.445357	39.171902	73.482753
472.341790	35.733507	73.487758
471.502962	47.638287	73.492762
470.440088	44.284924	73.497767
470.429937	33.565537	73.502772
469.248597	47.136423	73.507777
468.556650	42.214921	73.512782
467.725015	46.951788	73.517786
467.043309	43.769495	73.522791
466.956807	47.737985	73.527796
466.295291	45.992136	73.532801
466.145290	37.786447	73.537806
464.926517	39.156929	73.542810
464.133405	42.216200	73.547815
463.067549	36.080183	73.552820
461.919496	35.029978	73.557825
461.736704	42.028738	73.562830
461.602702	47.769287	73.567834
460.982859	44.506181	73.572839
460.608552	43.630723	73.577844
459.355457	47.818194	73.582849
459.040590	34.479332	73.587854
458.021435	42.625258	73.592858
456.798866	43.703055	73.597863
456.697227	29.973858	73.602868
455.972713	38.780842	73.607873
455.866514	34.425144	73.612878
455.163421	31.717741	73.617882
453.902670	45.119945	73.622887
453.530870	33.086325	73.627892
453.045941	40.984719	73.632897
452.691307	28.808029	73.637902
451.674580	41.969514	73.642906
450.624794	39.962280	73.647911
450.008484	31.422491	73.652916
449.139678	29.846862	73.657921
448.640661	33.251912	73.662926
447.936891	41.481623	73.667930
447.356350	44.033976	73.672935
447.251956	40.649327	73.677940
446.419125	41.240860	73.682945
445.710413	31.115296	73.687950
444.943462	39.042857	73.692954
444.658149	30.237458	73.697959
443.694637	41.674859	73.702964
442.792893	37.116356	73.707969
442.363630	33.384530	73.712974
441.695024	51.187982	73.717978
440.835115	33.752594	73.722983
440.167743	34.920121	73.727988
439.260231	40.369203	73.732993
439.034043	39.280926	73.737998
438.467893	38.559033	73.743002
437.307561	49.047004	73.748007
436.694663	32.969348	73.753012
436.181196	36.173291	73.758017
436.094620	34.126124	73.763022
435.304837	38.558305	73.768026
433.975237	49.429614	73.773031
433.683726	30.350474	73.778036
433.214070	38.610686	73.783041
432.716925	47.889196	73.788046
431.627093	46.448131	73.793050
430.969376	33.056681	73.798055
430.562893	39.197010	73.803060
429.395629	40.590839	73.808065
428.635474	39.592375	73.813070
428.256673	55.515785	73.818074
427.672277	46.800610	73.823079
427.421089	40.525340	73.828084
426.694864	41.080971	73.833089
425.857015	39.621834	73.838094
425.395688	41.461385	73.843098
424.477308	47.520868	73.848103
423.549741	37.961578	73.853108
422.689686	44.320828	73.858113
422.400157	44.439472	73.863118
422.232809	42.893998	73.868122
421.175917	43.385633	73.873127
420.726235	34.992754	73.878132
419.987277	45.046180	73.883137
419.477783	44.791471	73.888142
418.300502	50.428619	73.893146
417.268097	50.802821	73.898151
417.230719	32.099476	73.903156
416.440800	41.831462	73.908161
416.112698	40.086114	73.913166
414.935095	41.331796	73.918170
414.189786	38.896042	73.923175
413.962749	37.927744	73.928180
413.276263	39.943513	73.933185
412.542665	41.938406	73.938190
411.821905	39.262214	73.943194
411.466919	31.483412	73.948199
410.963136	38.629505	73.953204
409.883793	43.727535	73.958209
409.033554	37.809482	73.963214
408.783446	41.031385	73.968218
407.710885	44.497877	73.973223
406.817320	42.691257	73.978228
405.952461	46.645013	73.983233
405.291553	37.052702	73.988238
404.902010	47.189217	73.993242
404.583832	51.379115	73.998247
404.577662	38.334827	74.003252
404.081753	48.362145	74.008257
403.095609	35.440903	74.013262
402.469052	45.225704	74.018266
400.735009	44.008724	74.023271
400.356766	39.505581	74.028276
399.575149	46.658108	74.033281
399.509304	41.550135	74.038286
398.916565	40.745761	74.043290
398.112917	46.821660	74.048295
397.663052	38.824603	74.053300
397.071864	54.147963	74.058305
396.179421	39.671211	74.063310
394.966171	34.875382	74.068314
394.451166	34.498563	74.073319
394.144121	34.167447	74.078324
393.374912	38.577438	74.083329
392.679550	39.430915	74.088334
391.672952	44.090035	74.093338
391.098444	37.872602	74.098343
391.247430	48.248132	74.103348
390.407105	44.723734	74.108353
389.691105	42.404734	74.113358
388.786870	44.638123	74.118362
388.457061	39.428722	74.123367
387.513532	43.358751	74.128372
386.306539	46.436694	74.133377
385.733959	33.640358	74.138382
385.620498	31.758317	74.143386
384.822034	33.793514	74.148391
383.822860	45.756976	74.153396
382.889360	37.002842	74.158401
382.700247	34.044834	74.163406
382.053821	35.921771	74.168410
381.584949	38.344387	74.173415
381.503888	34.150258	74.178420
380.232358	35.393579	74.183425
379.515479	38.180546	74.188430
379.307171	39.695951	74.193434
378.135009	47.962476	74.198439
377.775053	30.620907	74.203444
376.785988	51.964989	74.208449
376.517385	36.529455	74.213454
375.567594	29.151358	74.218458
374.981310	49.499335	74.223463
374.670762	34.851026	74.228468
373.411153	40.285280	74.233473
372.450184	35.108661	74.238478
372.167231	47.583997	74.243482
371.579962	46.061294	74.248487
371.482513	33.474655	74.253492
370.035485	37.385586	74.258497
369.550261	37.570113	74.263502
369.185775	36.973783	74.268506
368.320083	37.636806	74.273511
367.332726	28.189572	74.278516
366.737852	36.991681	74.283521
366.347103	28.201526	74.288526
365.986051	33.492584	74.293530
364.971404	30.961008	74.298535
364.497322	25.369359	74.303540
363.576652	39.226714	74.308545
363.256954	33.561577	74.313550
361.872326	35.363788	74.318554
361.224475	35.861220	74.323559
361.072345	29.835089	74.328564
360.083302	43.947756	74.333569
360.311146	24.626619	74.338574
359.337116	39.381818	74.343578
358.103847	37.124765	74.348583
357.952489	38.550676	74.353588
357.017641	43.192066	74.358593
356.326794	35.031591	74.363598
355.568725	31.506714	74.368602
354.943096	42.683726	74.373607
354.867077	29.645854	74.378612
353.975923	39.493326	74.383617
353.069697	43.881014	74.388622
352.906995	41.582650	74.393626
351.618615	35.545226	74.398631
350.717890	30.392131	74.403636
349.640809	38.955724	74.408641
349.245453	29.839900	74.413646
348.904711	35.192374	74.418650
348.594743	41.911800	74.423655
348.714696	35.903804	74.428660
347.730958	48.268489	74.433665
346.903888	43.538863	74.438670
345.765539	34.229232	74.443674
344.372853	39.903890	74.448679
344.126147	39.384980	74.453684
343.537132	39.466214	74.458689
343.423064	38.558761	74.463694
342.974004	32.087979	74.468698
342.052666	45.951758	74.473703
341.262480	44.455095	74.478708
340.675435	40.338455	74.483713
339.864684	46.634682	74.488718
338.806712	37.451006	74.493722
337.886745	41.899232	74.498727
337.788027	31.275975	74.503732
337.133073	34.100389	74.508737
337.264094	40.837836	74.513742
336.529249	40.436145	74.518746
335.478928	35.697955	74.523751
335.187033	34.768385	74.528756
333.690838	48.558218	74.533761
332.732819	43.040546	74.538766
332.603058	32.702914	74.543770
332.107398	50.138212	74.548775
331.539218	42.109568	74.553780
330.646588	45.817054	74.558785
330.229654	46.104238	74.563790
329.804183	37.182435	74.568794
328.330336	41.811974	74.573799
327.968616	31.044568	74.578804
327.159778	43.171659	74.583809
326.968671	40.896747	74.588814
325.854533	40.687966	74.593818
324.993757	38.021503	74.598823
324.701050	21.131261	74.603828
324.063276	49.698064	74.608833
323.450852	36.168559	74.613838
322.597331	34.836528	74.618842
321.853889	37.741277	74.623847
321.575828	40.502472	74.628852
320.930568	42.292513	74.633857
320.198306	36.883936	74.638862
319.397581	45.401920	74.643866
318.710083	39.849023	74.648871
318.313267	29.396276	74.653876
317.214751	42.537720	74.658881
316.565140	39.880178	74.663886
316.122051	38.034910	74.668890
315.563778	40.935377	74.673895
315.031607	35.048665	74.678900
314.251516	41.874560	74.683905
313.560279	44.488737	74.688910
313.153456	35.688538	74.693914
311.915732	39.603985	74.698919
311.463234	39.736002	74.703924
310.826380	36.245433	74.708929
310.141448	46.555180	74.713934
309.441509	31.631512	74.718938
308.468746	45.028865	74.723943
307.999982	35.377583	74.728948
307.273306	33.916538	74.733953
306.935148	35.517294	74.738958
306.542655	30.869798	74.743962
305.224896	36.817940	74.748967
305.073427	37.270959	74.753972
304.271760	47.353326	74.758977
303.798763	42.909456	74.763982
302.748556	39.623535	74.768986
302.139060	35.340187	74.773991
301.649564	37.453887	74.778996
301.055128	38.653977	74.784001
300.020160	33.222699	74.789006
299.370002	32.752333	74.794010
298.652498	34.687925	74.799015
298.410817	42.676866	74.804020
297.908592	43.185793	74.809025
296.789765	35.692757	74.814030
296.162014	39.428991	74.819034
295.574452	40.091859	74.824039
295.575633	34.378743	74.829044
294.336883	33.945429	74.834049
293.782322	32.590986	74.839054
293.531839	36.708602	74.844058
292.007221	35.232832	74.849063
291.216569	41.044929	74.854068
290.725114	38.808433	74.859073
290.430619	35.816772	74.864078
289.910197	27.042576	74.869082
288.802298	36.304911	74.874087
288.225477	29.353072	74.879092
287.306952	39.526599	74.884097
287.238192	38.924143	74.889102
287.268946	25.303181	74.894106
286.185733	39.016162	74.899111
285.340077	31.052267	74.904116
284.025649	29.811063	74.909121
283.118800	35.867169	74.914126
282.917132	26.319973	74.919130
282.528316	38.351735	74.924135
282.168471	28.626338	74.929140
281.431590	33.004398	74.934145
280.458070	25.718433	74.939150
280.211650	24.948767	74.944154
278.953347	24.841830	74.949159
278.118293	31.632338	74.954164
277.234521	40.910990	74.959169
277.170837	38.776610	74.964174
276.955182	36.907711	74.969178
275.856280	42.540305	74.974183
275.065022	37.117496	74.979188
274.520265	41.939566	74.984193
273.832308	38.666874	74.989198
273.556652	33.016810	74.994202
272.154030	49.973825	74.999207
271.734170	35.297242	75.004212
271.410072	42.786847	75.009217
270.690016	31.600369	75.014222
270.040772	22.586537	75.019226
269.055676	48.955393	75.024231
268.716430	42.512849	75.029236
267.945945	43.805660	75.034241
266.897621	40.558876	75.039246
266.585160	34.124682	75.044250
265.453882	40.979762	75.049255
265.510192	41.514772	75.054260
265.166475	41.859677	75.059265
263.865711	42.355562	75.064270
263.217096	43.507531	75.069274
262.704606	41.324853	75.074279
261.667469	42.097238	75.079284
260.901062	43.422515	75.084289
260.187061	36.677040	75.089294
260.032549	30.750643	75.094298
259.523131	50.988606	75.099303
259.113610	44.073175	75.104308
258.302274	32.332011	75.109313
257.629414	43.205927	75.114318
256.378559	33.370271	75.119322
255.393809	48.300665	75.124327
255.458610	42.110661	75.129332
254.916045	38.814798	75.134337
254.311723	43.014053	75.139342
253.388701	24.694768	75.144346
252.528856	36.090460	75.149351
252.148448	31.824222	75.154356
251.805455	40.963062	75.159361
250.301051	34.182752	75.164366
249.929946	29.358406	75.169370
249.228142	36.193911	75.174375
249.047466	28.122451	75.179380
248.408293	33.522506	75.184385
246.799546	37.341020	75.189390
246.952963	43.204469	75.194394
246.135962	41.390437	75.199399
245.579372	36.040610	75.204404
244.534606	41.197840	75.209409
243.822229	32.126272	75.214414
243.596022	31.572569	75.219418
243.163611	42.200012	75.224423
242.333128	32.570147	75.229428
241.388257	40.106676	75.234433
240.662050	45.867516	75.239438
240.297085	41.617737	75.244442
239.125413	43.621017	75.249447
238.307251	36.262995	75.254452
237.908714	32.479009	75.259457
237.637096	39.268015	75.264462
237.224637	34.448685	75.269466
236.438462	45.039493	75.274471
235.306922	34.238723	75.279476
234.768089	34.020267	75.284481
234.075035	37.555628	75.289486
233.935701	45.566100	75.294490
233.001683	37.978984	75.299495
231.967792	36.644203	75.304500
231.669676	56.552042	75.309505
231.185341	35.256699	75.314510
229.999567	30.470773	75.319514
229.156731	50.749274	75.324519
229.087629	44.564848	75.329524
228.744233	42.107657	75.334529
227.400876	48.670159	75.339534
227.007642	49.194839	75.344538
226.050064	49.103060	75.349543
225.905870	44.818088	75.354548
224.896203	38.829339	75.359553
223.919194	38.694931	75.364558
223.599329	37.489157	75.369562
222.863110	37.667998	75.374567
222.955776	43.329833	75.379572
221.588612	39.336018	75.384577
220.686790	53.174644	75.389582
220.810185	35.633072	75.394586
219.684322	45.940592	75.399591
218.851658	44.758227	75.404596
218.073669	45.568158	75.409601
217.846743	43.712100	75.414606
217.782076	38.193976	75.419610
216.121764	46.945210	75.424615
215.718534	38.081389	75.429620
215.205579	34.426027	75.434625
214.255973	42.053200	75.439630
213.561633	44.011930	75.444634
212.448864	49.325086	75.449639
212.242418	45.956724	75.454644
211.800912	37.327649	75.459649
211.568300	47.790789	75.464654
210.759550	36.268414	75.469658
209.949832	43.428618	75.474663
209.399571	32.409046	75.479668
208.574055	42.621380	75.484673
207.440648	46.077153	75.489678
207.090588	46.429384	75.494682
206.407038	48.075758	75.499687
205.679707	48.455023	75.504692
204.921883	42.184875	75.509697
203.645645	39.609924	75.514702
203.783563	50.441318	75.519706
203.183667	50.746654	75.524711
202.800245	45.118510	75.529716
202.307987	44.599343	75.534721
201.440646	43.267981	75.539726
201.041402	35.808496	75.544730
199.885176	43.206860	75.549735
198.862986	42.975594	75.554740
198.600666	43.171921	75.559745
197.926046	37.501904	75.564750
197.223933	34.160536	75.569754
196.316481	38.341902	75.574759
195.960972	42.077329	75.579764
195.601649	42.987664	75.584769
194.480487	40.351726	75.589774
193.829051	29.084961	75.594778
193.257030	47.451728	75.599783
192.936396	42.606728	75.604788
192.200959	43.089784	75.609793
190.812335	37.680252	75.614798
190.496557	24.258047	75.619802
189.929565	39.941799	75.624807
189.531290	38.441046	75.629812
188.587775	42.035273	75.634817
187.760098	39.740450	75.639822
187.185513	31.304479	75.644826
186.928769	40.293961	75.649831
186.416215	41.118349	75.654836
185.470952	41.250112	75.659841
184.579426	39.859539	75.664846
184.160327	39.208871	75.669850
182.987190	36.813023	75.674855
182.197428	39.804036	75.679860
182.102151	37.676275	75.684865
181.691226	39.400605	75.689870
180.961468	30.145766	75.694874
179.903635	38.668504	75.699879
179.632938	44.240045	75.704884
179.171221	31.989045	75.709889
177.932593	40.403425	75.714894
177.257957	38.604563	75.719898
176.447063	35.567531	75.724903
176.119114	36.953802	75.729908
175.619503	45.267702	75.734913
174.670481	46.295714	75.739918
174.230467	36.827532	75.744922
173.494749	46.497317	75.749927
172.894249	28.263837	75.754932
171.762956	25.295238	75.759937
171.027445	45.731656	75.764942
170.520932	47.327736	75.769946
170.224960	49.442142	75.774951
169.972841	45.328914	75.779956
169.181789	33.187193	75.784961
167.981504	32.802999	75.789966
167.487315	34.177933	75.794970
166.889470	38.999023	75.799975
165.960093	33.705505	75.804980
165.773808	33.082370	75.809985
164.757277	45.569016	75.814990
164.414958	34.363350	75.819994
163.129079	48.220645	75.824999
162.611898	52.508521	75.830004
161.998118	43.413372	75.835009
161.698872	36.999166	75.840014
161.643336	38.580107	75.845018
160.351179	43.557634	75.850023
159.745983	33.761006	75.855028
159.086985	39.131127	75.860033
157.887120	35.791872	75.865038
157.283092	31.616498	75.870042
156.890539	38.800077	75.875047
156.452162	31.857741	75.880052
155.722502	37.412582	75.885057
154.949450	34.993953	75.890062
154.260535	26.748100	75.895066
153.554313	34.900989	75.900071
153.132889	39.151519	75.905076
152.409284	35.561297	75.910081
151.792574	48.179726	75.915086
151.237947	30.632748	75.920090
150.296555	42.484563	75.925095
149.118463	43.139131	75.930100
148.761132	38.768314	75.935105
148.328005	39.885952	75.940110
148.250148	27.375077	75.945114
146.640970	41.069471	75.950119
146.058694	34.731936	75.955124
145.587976	25.241859	75.960129
145.078615	37.444221	75.965134
144.881654	35.840419	75.970138
143.513807	35.341040	75.975143
142.791643	37.018816	75.980148
142.616300	21.093865	75.985153
141.966593	33.403752	75.990158
141.085176	26.973583	75.995162
140.274534	38.637403	76.000167
139.804538	45.286171	76.005172
139.309544	30.839221	76.010177
138.082302	40.997364	76.015182
137.779420	38.946861	76.020186
136.851900	45.897227	76.025191
136.732843	31.934342	76.030196
136.064387	29.694569	76.035201
134.866548	43.261884	76.040206
134.413681	32.586328	76.045210
134.111956	33.711398	76.050215
133.428727	41.589412	76.055220
132.378763	38.765546	76.060225
131.606895	39.675445	76.065230
131.397015	42.933527	76.070234
130.945212	34.350269	76.075239
129.657041	41.116888	76.080244
129.081065	27.803992	76.085249
128.695380	40.678869	76.090254
128.237802	33.488884	76.095258
126.885109	25.033520	76.100263
126.234460	26.600555	76.105268
126.127785	27.063787	76.110273
125.326390	30.998043	76.115278
124.517809	26.170950	76.120282
123.724067	36.952202	76.125287
123.198149	33.828748	76.130292
123.043971	28.875227	76.135297
121.805873	36.053301	76.140302
121.117616	30.762352	76.145306
120.478094	35.169079	76.150311
120.211644	32.034212	76.155316
119.210616	28.931334	76.160321
117.996699	44.978435	76.165326
117.807253	32.050147	76.170330
117.209189	41.229668	76.175335
117.072069	36.237157	76.180340
116.379207	31.818936	76.185345
115.280952	38.495355	76.190350
114.555972	29.933591	76.195354
114.181090	38.785805	76.200359
113.004790	42.130194	76.205364
112.418216	35.161042	76.210369
111.788692	45.365797	76.215374
111.427868	35.388301	76.220378
111.101217	38.735961	76.225383
110.254260	38.140922	76.230388
109.689413	37.579737	76.235393
108.800082	32.413889	76.240398
108.108895	23.067784	76.245402
107.241429	41.294017	76.250407
106.975652	48.233476	76.255412
106.276223	36.649563	76.260417
105.165740	37.413211	76.265422
104.498842	30.600365	76.270426
103.966733	34.516915	76.275431
103.590970	43.522226	76.280436
103.353669	29.436291	76.285441
102.008278	33.644950	76.290446
101.362282	32.033918	76.295450
100.729114	33.099891	76.300455
99.911214	34.026602	76.305460
99.473025	34.460706	76.310465
97.998727	44.894791	76.315470
98.122956	34.529309	76.320474
97.812019	39.911742	76.325479
97.069382	34.914879	76.330484
96.446805	33.476720	76.335489
95.504993	31.815101	76.340494
95.024911	31.879022	76.345498
93.681255	24.991194	76.350503
93.059021	34.109917	76.355508
92.690151	29.032953	76.360513
92.325975	38.952558	76.365518
91.849498	34.799436	76.370522
91.122763	26.640057	76.375527
90.064851	21.635137	76.380532
89.803362	29.497931	76.385537
89.187431	36.464844	76.390542
88.423682	23.000577	76.395546
87.639655	31.672050	76.400551
87.021483	27.311310	76.405556
86.394065	27.138551	76.410561
85.129507	34.404432	76.415566
84.977367	22.747450	76.420570
84.173932	36.292875	76.425575
83.769285	33.881746	76.430580
83.139104	26.865948	76.435585
81.829505	39.790406	76.440590
81.510763	28.809648	76.445594
81.180308	38.034796	76.450599
80.034327	31.501774	76.455604
79.394366	35.648402	76.460609
78.617965	35.302300	76.465614
78.279038	31.584529	76.470618
77.935215	35.286566	76.475623
77.424604	36.266772	76.480628
76.180787	26.972543	76.485633
75.795969	37.535636	76.490638
75.519928	28.192713	76.495642
74.356842	26.776112	76.500647
73.173151	28.350906	76.505652
73.144293	33.773501	76.510657
72.543911	41.859071	76.515662
71.831202	31.029448	76.520666
70.574318	26.879378	76.525671
69.854260	30.885828	76.530676
70.023173	36.281613	76.535681
69.190498	42.693361	76.540686
68.902336	28.405827	76.545690
67.689164	35.428572	76.550695
66.878042	32.538263	76.555700
66.836431	27.814360	76.560705
65.588866	39.087442	76.565710
64.403662	32.022981	76.570714
64.649281	35.383448	76.575719
63.875581	40.899608	76.580724
63.433681	32.404671	76.585729
62.277546	34.124875	76.590734
61.752826	34.473445	76.595738
61.699437	32.862522	76.600743
60.680514	39.133676	76.605748
59.374572	37.031864	76.610753
58.724984	43.638327	76.615758
58.347784	32.912882	76.620762
57.897394	32.398105	76.625767
57.522802	34.912961	76.630772
56.807472	25.725255	76.635777
55.988210	51.231965	76.640782
55.462676	34.432537	76.645786
54.491290	35.054183	76.650791
53.670281	34.989573	76.655796
53.609582	39.548410	76.660801
52.860502	38.556185	76.665806
51.905198	32.029034	76.670810
51.117217	31.058783	76.675815
50.315935	47.792248	76.680820
50.077415	36.932728	76.685825
49.236946	46.750122	76.690830
48.695208	33.673047	76.695834
48.128601	38.634247	76.700839
47.178519	36.526143	76.705844
46.746270	44.187540	76.710849
45.838132	42.384960	76.715854
45.063693	34.457115	76.720858
44.674555	39.423124	76.725863
44.168352	37.603745	76.730868
43.423666	36.174038	76.735873
42.247581	40.152313	76.740878
41.738265	39.380452	76.745882
41.753565	34.380985	76.750887
40.649580	40.861242	76.755892
40.299731	28.059477	76.760897
39.394899	38.503677	76.765902
38.739957	32.501018	76.770906
37.590698	30.273311	76.775911
36.549866	23.371910	76.780916
36.544477	43.581504	76.785921
35.878127	16.827905	76.790926
35.398403	37.549928	76.795930
35.061982	35.116888	76.800935
34.533859	44.468179	76.805940
33.648384	26.871532	76.810945
32.927117	31.788019	76.815950
32.365983	38.381952	76.820954
31.459313	29.596907	76.825959
30.342671	34.514961	76.830964
30.067553	34.971949	76.835969
29.456538	43.505468	76.840974
28.374140	33.392369	76.845978
27.930073	32.045596	76.850983
27.621420	39.127500	76.855988
27.335656	32.398958	76.860993
25.906563	24.667000	76.865998
25.144157	31.830737	76.871002
24.757841	46.113837	76.876007
24.341231	48.603865	76.881012
23.970664	24.299219	76.886017
23.032043	30.869788	76.891022
22.227108	44.801796	76.896026
21.856596	46.201183	76.901031
20.853049	39.462557	76.906036
19.862341	36.607216	76.911041
18.978571	33.764779	76.916046
18.975845	29.069367	76.921050
18.642805	39.990031	76.926055
17.382271	43.373128	76.931060
17.175151	29.220905	76.936065
16.680947	37.614374	76.941070
15.972560	25.612498	76.946074
14.787838	41.823693	76.951079
14.020610	42.888995	76.956084
13.853855	31.414112	76.961089
12.991905	27.484910	76.966094
11.877761	28.857842	76.971098
11.336958	39.150951	76.976103
11.074142	29.619865	76.981108
10.509694	30.327994	76.986113
9.587049	27.567451	76.991118
8.610691	31.329391	76.996122
8.451497	36.638743	77.001127
8.035350	50.779960	77.006132
7.193476	31.221086	77.011137
6.133966	32.123293	77.016142
5.508521	43.049603	77.021147
5.336520	39.540166	77.026151
4.246310	35.431349	77.031156
3.502167	34.752143	77.036161