Mon Mar 08 20:09:51 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.600522	93.528815	0.000000
-1.743355	73.905706	0.005005
-2.601427	56.563282	0.010010
-4.758685	22.876075	0.015014
-9.447141	25.495577	0.020019
-14.294775	28.984086	0.025024
-18.776395	32.929846	0.030029
-22.975742	29.156136	0.035034
-26.840495	15.664653	0.040038
-30.303689	25.942953	0.045043
-34.579051	28.687406	0.050048
-38.073416	20.239489	0.055053
-41.857755	20.570336	0.060058
-45.671358	31.048049	0.065062
-48.960154	15.889469	0.070067
-52.968120	42.641163	0.075072
-56.807045	28.174269	0.080077
-60.784250	23.404899	0.085082
-64.735641	12.833408	0.090086
-68.070078	35.661730	0.095091
-71.633915	20.966495	0.100096
-75.678848	26.264993	0.105101
-79.013215	29.780272	0.110106
-83.055680	24.325967	0.115110
-86.959856	32.791962	0.120115
-90.907798	28.013242	0.125120
-94.192441	19.336425	0.130125
-98.351355	29.126617	0.135130
-101.978826	29.929233	0.140134
-105.566093	27.614350	0.145139
-109.724965	30.532721	0.150144
-113.548272	24.379656	0.155149
-117.200465	26.488702	0.160154
-121.104327	26.217471	0.165158
-124.279859	22.614878	0.170163
-128.103508	34.797295	0.175168
-131.699528	27.217227	0.180173
-135.736619	22.235206	0.185178
-139.823636	24.423127	0.190182
-143.593169	22.741311	0.195187
-147.375185	24.200963	0.200192
-151.019512	31.770949	0.205197
-155.098698	37.533903	0.210202
-159.039566	33.758609	0.215206
-162.168346	28.153913	0.220211
-166.332921	33.875320	0.225216
-169.712537	33.463747	0.230221
-173.250016	21.068223	0.235226
-177.507951	19.231027	0.240230
-180.714040	32.149113	0.245235
-184.751550	30.112762	0.250240
-188.538033	22.998385	0.255245
-192.364184	27.125264	0.260250
-196.393711	23.349992	0.265254
-199.805812	19.419431	0.270259
-203.351440	25.521478	0.275264
-207.326494	19.391210	0.280269
-211.098779	29.755345	0.285274
-215.227704	16.929197	0.290278
-218.810179	19.453011	0.295283
-222.705907	39.674713	0.300288
-226.176846	26.688376	0.305293
-229.703568	34.644952	0.310298
-233.587448	28.832885	0.315302
-237.134078	17.023932	0.320307
-241.305844	29.938528	0.325312
-244.839659	21.087250	0.330317
-248.626961	11.752934	0.335322
-252.694162	32.188101	0.340326
-255.930896	15.944553	0.345331
-260.460555	33.016060	0.350336
-264.182409	20.763643	0.355341
-267.537082	7.255824	0.360346
-271.556903	21.724613	0.365350
-274.881128	15.044338	0.370355
-278.749247	35.182863	0.375360
-282.539890	17.722153	0.380365
-286.012739	10.070643	0.385370
-290.307769	19.846599	0.390374
-294.302325	19.151768	0.395379
-297.942747	20.940685	0.400384
-301.635442	26.158092	0.405389
-305.141029	32.151399	0.410394
-308.760170	31.549616	0.415398
-312.535240	5.303553	0.420403
-316.694714	42.461618	0.425408
-319.983797	12.463962	0.430413
-324.007694	14.761952	0.435418
-327.894949	36.732721	0.440422
-331.231721	29.228267	0.445427
-335.345229	20.912762	0.450432
-338.978945	22.866236	0.455437
-342.652202	21.224554	0.460442
-347.053278	36.607401	0.465446
-350.186681	-2.834999	0.470451
-354.055475	44.997550	0.475456
-357.617855	11.889931	0.480461
-361.632505	32.561276	0.485466
-365.362285	24.512540	0.490470
-369.083424	17.000134	0.495475
-373.204954	32.466111	0.500480
-377.038278	34.938752	0.505485
-380.323978	24.196874	0.510490
-384.259281	22.401569	0.515494
-387.923147	20.728498	0.520499
-392.021942	41.823310	0.525504
-395.551600	25.599929	0.530509
-399.023827	10.616248	0.535514
-403.323774	23.756551	0.540518
-406.681339	37.266753	0.545523
-410.287314	34.502768	0.550528
-414.163496	24.055482	0.555533
-417.759476	27.267664	0.560538
-421.782687	19.701082	0.565542
-426.010888	37.847438	0.570547
-429.440666	19.747515	0.575552
-433.334930	22.895395	0.580557
-436.655791	26.019522	0.585562
-440.663609	42.516045	0.590566
-444.190805	14.809907	0.595571
-448.236653	28.121005	0.600576
-452.064901	37.305506	0.605581
-455.619132	9.450764	0.610586
-459.675480	36.770500	0.615590
-463.034106	18.646656	0.620595
-467.041928	27.834621	0.625600
-470.587705	23.272997	0.630605
-474.471966	40.063625	0.635610
-478.402395	23.030825	0.640614
-481.986104	22.609713	0.645619
-485.747114	25.607096	0.650624
-489.615480	28.793505	0.655629
-493.169383	25.262880	0.660634
-497.067833	20.566827	0.665638
-500.674598	17.967100	0.670643
-504.649815	37.005078	0.675648
-508.337767	34.246452	0.680653
-512.183768	29.034306	0.685658
-516.390273	24.929913	0.690662
-519.333642	24.192136	0.695667
-523.249155	25.776190	0.700672
-527.043347	28.320081	0.705677
-531.003775	7.853134	0.710682
-534.658404	43.775043	0.715686
-538.194390	23.554081	0.720691
-542.297256	27.515983	0.725696
-545.851564	25.600171	0.730701
-549.521948	16.362793	0.735706
-553.987836	27.008513	0.740710
-557.269492	18.251481	0.745715
-560.852255	23.415446	0.750720
-564.639153	33.713053	0.755725
-568.510447	13.176742	0.760730
-572.746060	25.439797	0.765734
-576.104652	17.891892	0.770739
-579.787372	22.556230	0.775744
-583.516880	29.844001	0.780749
-587.090645	21.269281	0.785754
-591.330271	29.548379	0.790758
-594.701349	30.665563	0.795763
-598.697016	36.239296	0.800768
-602.481477	10.334285	0.805773
-606.413854	27.897535	0.810778
-610.027192	25.280104	0.815782
-613.310285	11.118040	0.820787
-617.498178	22.965147	0.825792
-621.489403	39.993830	0.830797
-624.971198	17.066422	0.835802
-628.921020	23.022350	0.840806
-632.325557	29.927141	0.845811
-636.197503	20.838790	0.850816
-639.674381	28.937766	0.855821
-643.641452	27.521676	0.860826
-647.797705	18.587571	0.865830
-651.354108	25.529265	0.870835
-655.260405	36.391666	0.875840
-658.973402	34.222282	0.880845
-662.582429	16.345335	0.885850
-666.359129	32.865178	0.890854
-670.054373	34.817944	0.895859
-673.685245	27.318416	0.900864
-677.780851	17.124258	0.905869
-681.599396	15.919447	0.910874
-685.113793	22.919126	0.915878
-689.173804	19.179539	0.920883
-692.895694	23.441909	0.925888
-696.534328	18.928587	0.930893
-699.938138	18.928452	0.935898
-703.973491	21.276210	0.940902
-707.605113	9.062173	0.945907
-711.304696	20.631144	0.950912
-715.677847	20.207239	0.955917
-718.852776	25.749348	0.960922
-722.800214	21.529821	0.965926
-726.486815	32.407678	0.970931
-730.105438	28.329564	0.975936
-734.128348	23.043571	0.980941
-737.510050	22.811319	0.985946
-741.798199	34.099119	0.990950
-745.206964	28.804875	0.995955
-749.046285	20.665483	1.000960
-752.768104	20.162783	1.005965
-756.126966	23.908378	1.010970
-760.380463	26.357321	1.015974
-764.338752	23.459398	1.020979
-767.978137	23.195838	1.025984
-771.755894	13.119777	1.030989
-775.442884	38.946022	1.035994
-779.507609	28.438050	1.040998
-782.893608	23.133919	1.046003
-786.566466	32.916929	1.051008
-790.263993	20.461263	1.056013
-794.215041	16.551494	1.061018
-798.336458	24.543989	1.066022
-801.511658	17.779173	1.071027
-805.301384	15.160282	1.076032
-809.549816	36.839396	1.081037
-812.697983	22.476305	1.086042
-816.950188	28.293229	1.091046
-821.017839	5.951791	1.096051
-824.860669	38.337340	1.101056
-828.149115	33.424499	1.106061
-831.497786	19.885053	1.111066
-835.478659	18.000027	1.116070
-839.291857	23.224885	1.121075
-843.241551	19.592503	1.126080
-847.102530	20.744205	1.131085
-850.504362	25.110182	1.136090
-854.218964	3.571743	1.141094
-857.866337	25.438658	1.146099
-861.804258	28.017091	1.151104
-865.619758	19.647030	1.156109
-869.239501	25.750833	1.161114
-873.559285	29.561909	1.166118
-877.305462	5.694864	1.171123
-880.570073	30.138638	1.176128
-884.586426	24.627954	1.181133
-887.979436	4.971340	1.186138
-892.229152	38.901079	1.191142
-895.940316	24.997096	1.196147
-899.674017	5.182099	1.201152
-903.477438	25.355293	1.206157
-906.683120	16.384803	1.211162
-910.799506	19.885904	1.216166
-914.700607	31.343905	1.221171
-918.320468	11.734639	1.226176
-922.453930	25.842584	1.231181
-925.705516	26.225256	1.236186
-929.623019	10.835862	1.241190
-933.256715	25.027903	1.246195
-936.954835	27.322134	1.251200
-941.134810	26.317451	1.256205
-944.507810	4.253086	1.261210
-948.901113	38.084449	1.266214
-952.164751	1.719800	1.271219
-956.112386	28.366881	1.276224
-959.725448	25.857175	1.281229
-962.975507	-2.630258	1.286234
-967.458026	38.218031	1.291238
-971.055629	9.127052	1.296243
-974.519418	16.208923	1.301248
-978.752677	25.966715	1.306253
-982.301026	23.845631	1.311258
-986.796430	32.879029	1.316262
-989.758508	3.967139	1.321267
-993.180685	35.263851	1.326272
-997.619450	15.098186	1.331277
-1001.073698	16.145675	1.336282
-1005.363014	23.288655	1.341286
-1008.586957	17.930566	1.346291
-1012.197171	13.400590	1.351296
-1016.122776	18.047664	1.356301
-1019.685743	23.850898	1.361306
-1023.856650	24.249856	1.366310
-1027.403425	10.723490	1.371315
-1031.352895	19.376361	1.376320
-1035.317137	34.770918	1.381325
-1038.578237	19.915344	1.386330
-1042.791423	15.929669	1.391334
-1046.267942	20.955936	1.396339
-1049.923043	16.693373	1.401344
-1053.796873	9.209681	1.406349
-1057.297833	18.863090	1.411354
-1061.141787	13.936954	1.416358
-1065.270311	14.299248	1.421363
-1069.229336	29.503799	1.426368
-1072.563066	20.140906	1.431373
-1075.751628	22.230856	1.436378
-1080.052696	16.980510	1.441382
-1083.845467	19.548706	1.446387
-1087.606161	40.629896	1.451392
-1091.695906	10.339065	1.456397
-1095.435540	46.115961	1.461402
-1099.085180	10.205929	1.466406
-1102.281135	35.477841	1.471411
-1106.287696	21.042791	1.476416
-1109.867959	21.659629	1.481421
-1113.629922	0.826197	1.486426
-1117.913068	37.328653	1.491430
-1121.745970	1.455889	1.496435
-1125.529887	36.334792	1.501440
-1129.211561	10.155743	1.506445
-1132.850984	30.840722	1.511450
-1136.643704	19.950890	1.516454
-1140.275669	27.231775	1.521459
-1143.875381	10.136284	1.526464
-1148.086559	29.184566	1.531469
-1151.340746	22.935889	1.536474
-1155.533562	26.709815	1.541478
-1158.644235	-2.066066	1.546483
-1162.666558	34.467252	1.551488
-1166.699632	3.558876	1.556493
-1170.392869	21.081535	1.561498
-1174.555632	26.511070	1.566502
-1178.497102	10.637159	1.571507
-1181.393652	15.864112	1.576512
-1185.134021	13.032966	1.581517
-1189.112933	11.837303	1.586522
-1192.856702	20.591550	1.591526
-1196.780135	24.481703	1.596531
-1200.363544	7.058882	1.601536
-1204.354427	28.389916	1.606541
-1207.780983	5.883597	1.611546
-1211.826803	11.111569	1.616550
-1215.640178	23.019573	1.621555
-1219.419936	21.859897	1.626560
-1223.048502	31.302173	1.631565
-1226.837530	-1.668169	1.636570
-1230.531789	29.833168	1.641574
-1234.089918	21.786803	1.646579
-1237.704832	8.760507	1.651584
-1241.941908	43.899728	1.656589
-1245.491452	16.050396	1.661594
-1249.545738	32.322203	1.666598
-1253.096014	29.006623	1.671603
-1256.985375	10.899639	1.676608
-1260.800177	20.994607	1.681613
-1264.429684	9.388244	1.686618
-1268.161688	21.988139	1.691622
-1271.991306	38.039545	1.696627
-1275.391395	18.383119	1.701632
-1279.467361	13.084517	1.706637
-1282.906183	24.478558	1.711642
-1287.444816	4.854590	1.716646
-1291.084598	44.026374	1.721651
-1294.565509	32.196006	1.726656
-1297.966648	28.438772	1.731661
-1301.741802	24.113835	1.736666
-1305.481231	2.283760	1.741670
-1309.515810	30.547291	1.746675
-1313.074376	20.534841	1.751680
-1317.560941	25.749969	1.756685
-1320.982089	30.190659	1.761690
-1324.791494	9.585953	1.766694
-1328.594798	37.009909	1.771699
-1331.623805	-9.273454	1.776704
-1336.036945	27.828787	1.781709
-1339.577908	14.171137	1.786714
-1343.221951	22.031367	1.791718
-1347.124833	9.289450	1.796723
-1350.916671	20.379000	1.801728
-1355.084417	29.190326	1.806733
-1358.148402	5.325362	1.811738
-1362.393926	27.913110	1.816742
-1366.183839	13.724551	1.821747
-1369.480558	15.040653	1.826752
-1373.463747	15.954187	1.831757
-1377.141383	9.445660	1.836762
-1381.180357	13.906495	1.841766
-1384.790322	9.634099	1.846771
-1388.272792	16.323765	1.851776
-1392.619001	23.060260	1.856781
-1395.824624	17.329249	1.861786
-1399.828258	17.733639	1.866790
-1403.702255	28.292429	1.871795
-1407.401850	10.295685	1.876800
-1410.837782	28.774039	1.881805
-1414.686336	18.302030	1.886810
-1418.450038	8.116044	1.891814
-1422.406053	26.094256	1.896819
-1426.192716	23.140042	1.901824
-1430.072117	26.151557	1.906829
-1433.893548	8.268980	1.911834
-1437.245521	13.523426	1.916838
-1440.992066	29.364672	1.921843
-1444.657028	3.074756	1.926848
-1448.883747	19.883780	1.931853
-1452.479767	30.262534	1.936858
-1456.479049	6.241580	1.941862
-1460.190425	21.859616	1.946867
-1463.748464	14.020177	1.951872
-1467.956413	31.291398	1.956877
-1471.268129	6.078690	1.961882
-1474.907142	37.699222	1.966886
-1478.634359	0.514137	1.971891
-1482.228437	34.748127	1.976896
-1486.597201	39.443290	1.981901
-1490.192406	6.587490	1.986906
-1493.523846	29.158373	1.991910
-1497.614767	35.633430	1.996915
-1501.426978	26.944358	2.006912
-1502.741776	20.391140	2.016909
-1499.932421	21.358969	2.026906
-1497.388191	24.524355	2.036902
-1494.990651	20.460107	2.046899
-1493.011628	25.037484	2.056896
-1491.092407	19.453642	2.066893
-1489.651629	16.088883	2.076890
-1487.532916	27.792820	2.086886
-1485.360551	17.782467	2.096883
-1483.790388	24.989336	2.106880
-1481.796168	18.962472	2.116877
-1480.001242	22.183131	2.126874
-1477.741394	15.883228	2.136870
-1475.989657	25.105608	2.146867
-1474.140886	25.835734	2.156864
-1472.067725	23.140192	2.166861
-1470.563456	23.535514	2.176858
-1468.563183	22.027871	2.186854
-1466.588495	26.531762	2.196851
-1464.553507	19.904745	2.206848
-1462.716577	21.828790	2.216845
-1460.873883	22.351496	2.226842
-1459.215031	26.875967	2.236838
-1457.153615	21.703560	2.246835
-1455.561920	23.565833	2.256832
-1453.273324	19.346979	2.266829
-1451.266092	23.517276	2.276826
-1449.764306	24.416655	2.286822
-1447.794539	31.976384	2.296819
-1445.594642	22.629496	2.306816
-1444.090931	19.502563	2.316813
-1441.997389	26.796179	2.326810
-1440.004773	27.874327	2.336806
-1438.616224	15.845464	2.346803
-1437.004306	26.318591	2.356800
-1434.446584	19.528963	2.366797
-1432.423870	15.292704	2.376794
-1430.733908	21.875741	2.386790
-1428.837003	26.058987	2.396787
-1427.024357	25.482930	2.406784
-1425.200832	20.617038	2.416781
-1423.141349	19.237313	2.426778
-1421.542107	11.549658	2.436774
-1419.496094	22.164860	2.446771
-1417.571622	29.812388	2.456768
-1415.940770	21.742331	2.466765
-1414.112524	18.479780	2.476762
-1411.970131	29.107984	2.486758
-1410.217960	26.945426	2.496755
-1408.202148	22.831860	2.506752
-1406.138089	30.752292	2.516749
-1404.331307	34.706851	2.526746
-1402.497576	25.827537	2.536742
-1400.804810	36.082510	2.546739
-1398.845048	17.447969	2.556736
-1396.836916	24.036936	2.566733
-1394.845784	28.475107	2.576730
-1393.447743	25.930341	2.586726
-1391.561445	25.176744	2.596723
-1389.481131	18.618316	2.606720
-1387.624718	37.707486	2.616717
-1385.367390	20.779393	2.626714
-1384.004914	33.381290	2.636710
-1381.859644	3.974730	2.646707
-1379.988451	49.475341	2.656704
-1378.510618	23.552710	2.666701
-1375.922056	-0.157341	2.676698
-1374.639259	32.415266	2.686694
-1372.291924	14.432333	2.696691
-1370.430672	7.130632	2.706688
-1369.036232	44.507137	2.716685
-1366.779455	10.690417	2.726682
-1364.952876	22.003907	2.736678
-1363.088813	19.122475	2.746675
-1361.405449	10.401469	2.756672
-1359.302270	27.120804	2.766669
-1357.568498	16.277676	2.776666
-1355.774459	16.301450	2.786662
-1353.962656	25.931131	2.796659
-1351.911303	22.869738	2.806656
-1350.015350	21.828861	2.816653
-1348.049931	14.082636	2.826650
-1346.422768	15.426189	2.836646
-1344.676092	21.788655	2.846643
-1342.486035	20.411781	2.856640
-1340.515688	26.056396	2.866637
-1338.600127	17.462431	2.876634
-1336.728916	35.976168	2.886630
-1335.116808	38.465215	2.896627
-1332.951421	16.344902	2.906624
-1331.086793	21.856456	2.916621
-1329.340743	30.713589	2.926618
-1327.573978	30.114955	2.936614
-1325.441483	26.405907	2.946611
-1323.826701	22.634473	2.956608
-1321.978157	15.017492	2.966605
-1320.061783	27.522881	2.976602
-1318.012912	27.859555	2.986598
-1316.469632	25.528412	2.996595
-1314.442307	22.107765	3.006592
-1312.097600	20.783531	3.016589
-1310.574070	20.509609	3.026586
-1308.823010	21.001317	3.036582
-1306.951404	27.441709	3.046579
-1304.783190	29.761250	3.056576
-1303.120381	16.891243	3.066573
-1300.954138	27.166823	3.076570
-1299.193953	27.421833	3.086566
-1297.538549	23.451298	3.096563
-1295.825362	17.125377	3.106560
-1293.714790	30.431756	3.116557
-1291.872764	28.505939	3.126554
-1289.632129	17.616466	3.136550
-1288.035943	22.045315	3.146547
-1286.191754	25.487178	3.156544
-1284.260643	34.759964	3.166541
-1282.337726	28.509421	3.176538
-1280.574294	29.112847	3.186534
-1278.675002	29.541384	3.196531
-1276.780751	26.700972	3.206528
-1274.748498	21.667585	3.216525
-1273.237822	22.099904	3.226522
-1271.145415	30.661673	3.236518
-1269.300647	26.307193	3.246515
-1267.144304	23.279593	3.256512
-1265.828443	18.452434	3.266509
-1263.623651	35.810838	3.276506
-1261.628219	36.999210	3.286502
-1259.977266	22.280731	3.296499
-1258.050934	32.114789	3.306496
-1256.189524	39.351014	3.316493
-1254.208302	25.741702	3.326490
-1252.466313	32.670220	3.336486
-1250.490770	22.887331	3.346483
-1248.591167	19.892939	3.356480
-1246.763598	33.587265	3.366477
-1245.065838	24.925594	3.376474
-1243.032901	33.032734	3.386470
-1241.049868	26.734711	3.396467
-1239.430906	20.734935	3.406464
-1237.187661	30.451987	3.416461
-1235.477449	18.944858	3.426458
-1233.582839	28.735069	3.436454
-1231.713801	21.320118	3.446451
-1229.825141	24.388623	3.456448
-1228.136393	21.210109	3.466445
-1225.953070	20.994862	3.476442
-1224.114696	22.479957	3.486438
-1222.808216	30.123930	3.496435
-1220.823741	29.433702	3.506432
-1218.516571	28.023994	3.516429
-1216.861370	28.430066	3.526426
-1214.824876	35.504110	3.536422
-1212.943393	30.359116	3.546419
-1211.204676	21.212529	3.556416
-1209.080607	28.441497	3.566413
-1207.183408	25.182277	3.576410
-1205.340207	31.949387	3.586406
-1203.562835	22.837669	3.596403
-1201.492510	22.815776	3.606400
-1199.881852	26.525588	3.616397
-1198.340900	40.913148	3.626394
-1196.067758	27.162436	3.636390
-1194.104645	36.354403	3.646387
-1192.406647	27.204867	3.656384
-1190.338460	33.140261	3.666381
-1188.563201	38.511519	3.676378
-1186.742783	25.425316	3.686374
-1184.709945	32.702062	3.696371
-1182.695462	19.131692	3.706368
-1181.208035	27.266174	3.716365
-1179.330855	28.194084	3.726362
-1177.345588	28.577372	3.736358
-1175.300527	24.874551	3.746355
-1173.561242	30.278415	3.756352
-1171.978687	24.753417	3.766349
-1170.031445	23.254513	3.776346
-1167.923889	17.602895	3.786342
-1165.943766	28.492564	3.796339
-1164.028793	37.057571	3.806336
-1162.186176	28.633282	3.816333
-1160.754723	24.517103	3.826330
-1158.500758	32.336349	3.836326
-1156.464356	36.132806	3.846323
-1154.879615	26.407773	3.856320
-1152.956966	29.690364	3.866317
-1151.333576	30.900462	3.876314
-1148.892896	25.266610	3.886310
-1147.632593	39.523861	3.896307
-1145.461076	30.110715	3.906304
-1143.467728	30.033300	3.916301
-1141.487218	26.312414	3.926298
-1139.804522	34.125186	3.936294
-1138.048398	26.952558	3.946291
-1136.189919	34.058313	3.956288
-1134.206074	33.987162	3.966285
-1132.010555	26.325853	3.976282
-1130.719762	20.231814	3.986278
-1128.601422	32.141439	3.996275
-1126.548880	23.192578	4.006272
-1124.756391	23.335192	4.016269
-1123.005317	22.916053	4.026266
-1120.914949	23.802012	4.036262
-1119.257815	32.998789	4.046259
-1117.270272	22.860420	4.056256
-1115.412260	32.364514	4.066253
-1113.253164	18.253202	4.076250
-1111.468730	34.547000	4.086246
-1109.943098	33.611342	4.096243
-1108.086496	27.142609	4.106240
-1105.872739	21.788242	4.116237
-1104.249748	22.098501	4.126234
-1102.472418	28.637832	4.136230
-1100.033350	28.114971	4.146227
-1098.454637	32.264148	4.156224
-1096.871878	21.783206	4.166221
-1094.914995	19.644972	4.176218
-1093.033582	30.757330	4.186214
-1090.890012	33.444152	4.196211
-1089.026579	21.928388	4.206208
-1087.229504	22.035563	4.216205
-1085.600595	24.716297	4.226202
-1083.124616	23.608117	4.236198
-1081.890212	28.158144	4.246195
-1079.608137	35.775624	4.256192
-1077.694704	25.537039	4.266189
-1075.916433	27.570251	4.276186
-1074.025381	15.983773	4.286182
-1072.345722	31.002878	4.296179
-1070.420762	25.407387	4.306176
-1068.465057	35.434281	4.316173
-1066.595452	28.480375	4.326170
-1064.913422	24.215231	4.336166
-1062.770558	27.486359	4.346163
-1060.671256	29.776107	4.356160
-1059.233932	28.283068	4.366157
-1057.335870	29.616657	4.376154
-1055.421009	27.483597	4.386150
-1053.454658	21.736246	4.396147
-1051.503816	37.097238	4.406144
-1049.905663	26.135470	4.416141
-1047.880753	25.659958	4.426138
-1045.916280	30.252700	4.436134
-1044.192593	24.245768	4.446131
-1042.286067	24.074965	4.456128
-1040.219773	20.820408	4.466125
-1038.398496	19.460171	4.476122
-1036.538263	28.607162	4.486118
-1034.928046	22.817318	4.496115
-1032.709062	16.386995	4.506112
-1030.764793	32.446898	4.516109
-1029.120520	23.939172	4.526106
-1027.171241	20.300738	4.536102
-1025.509435	31.631427	4.546099
-1023.485051	22.799247	4.556096
-1021.640527	21.945268	4.566093
-1019.711835	21.632000	4.576090
-1017.965273	25.408625	4.586086
-1015.865680	25.961649	4.596083
-1014.084139	35.351760	4.606080
-1012.145324	36.948850	4.616077
-1010.207434	25.361233	4.626074
-1008.549344	32.909643	4.636070
-1006.599620	26.643971	4.646067
-1004.654384	21.127388	4.656064
-1002.655871	26.395201	4.666061
-1000.972251	18.585363	4.676058
-998.984434	21.854506	4.686054
-997.164736	32.334238	4.696051
-995.546181	28.093500	4.706048
-993.582284	25.052712	4.716045
-991.510172	11.763774	4.726042
-989.666360	30.995871	4.736038
-987.890066	20.851910	4.746035
-985.708464	18.658883	4.756032
-984.071408	29.298876	4.766029
-982.315571	27.096574	4.776026
-980.369801	26.221700	4.786022
-978.360956	24.960978	4.796019
-976.524758	34.070821	4.806016
-974.697851	23.146722	4.816013
-972.743896	29.564766	4.826010
-970.809295	31.200457	4.836006
-968.987684	18.668378	4.846003
-967.163540	34.052869	4.856000
-965.418809	30.737696	4.865997
-963.084063	17.897794	4.875994
-961.632989	26.546634	4.885990
-959.714415	22.229528	4.895987
-957.741419	29.430801	4.905984
-955.666379	27.239052	4.915981
-954.184936	18.065881	4.925978
-952.163340	31.061609	4.935974
-950.246060	25.262188	4.945971
-948.477336	24.991925	4.955968
-946.384551	29.087430	4.965965
-944.451735	24.284934	4.975962
-943.079592	25.969533	4.985958
-941.231942	20.954883	4.995955
-939.097267	37.410726	5.005952
-937.218089	26.198837	5.015949
-935.244821	20.104708	5.025946
-933.288054	30.518373	5.035942
-931.148351	27.359530	5.045939
-929.707037	25.736467	5.055936
-927.761758	21.961392	5.065933
-926.008561	28.615248	5.075930
-923.931935	32.137083	5.085926
-922.358120	28.782958	5.095923
-920.392089	25.465591	5.105920
-918.031130	22.986598	5.115917
-916.456980	27.777642	5.125914
-914.745080	30.124729	5.135910
-912.540149	23.800958	5.145907
-910.861727	28.137997	5.155904
-909.015641	37.194219	5.165901
-906.923905	29.233927	5.175898
-905.386935	24.666842	5.185894
-903.737810	32.043096	5.195891
-901.529455	30.589500	5.205888
-899.397419	27.662421	5.215885
-897.271167	26.231429	5.225882
-895.808722	28.575783	5.235878
-893.974096	28.479748	5.245875
-892.223159	39.273710	5.255872
-890.402733	27.817052	5.265869
-888.361705	31.243566	5.275866
-886.640372	33.304975	5.285862
-884.702594	28.479626	5.295859
-882.644792	26.161231	5.305856
-880.624256	18.103409	5.315853
-878.928702	22.764551	5.325850
-877.498309	27.610182	5.335846
-875.213942	33.756036	5.345843
-873.235571	31.169314	5.355840
-871.482215	25.310901	5.365837
-869.490387	20.735854	5.375834
-867.789299	29.447419	5.385830
-865.778872	27.300811	5.395827
-863.609826	26.595588	5.405824
-862.079417	26.666624	5.415821
-860.187368	25.773596	5.425818
-858.599057	22.418774	5.435814
-856.516059	21.640477	5.445811
-854.484558	18.360063	5.455808
-852.779303	23.507536	5.465805
-850.836162	21.112768	5.475802
-848.983930	20.976062	5.485798
-847.166552	24.850440	5.495795
-845.098873	8.497797	5.505792
-843.323374	8.753861	5.515789
-841.264965	24.855697	5.525786
-839.704757	25.368796	5.535782
-837.907593	17.337240	5.545779
-836.019845	24.730659	5.555776
-833.635267	27.941263	5.565773
-832.133513	17.031346	5.575770
-830.455490	30.928374	5.585766
-828.019235	25.606575	5.595763
-826.091459	22.647480	5.605760
-824.878457	12.183172	5.615757
-822.682201	43.370912	5.625754
-820.870476	16.086255	5.635750
-818.873508	25.696286	5.645747
-817.092079	29.740636	5.655744
-814.916874	25.859428	5.665741
-813.509466	25.111793	5.675738
-811.732347	17.481327	5.685734
-809.307100	19.615002	5.695731
-807.707483	28.192845	5.705728
-805.934940	27.618941	5.715725
-803.689637	30.190306	5.725722
-802.020329	26.112095	5.735718
-800.146687	34.931918	5.745715
-798.258813	23.451911	5.755712
-796.378669	27.390505	5.765709
-794.549880	22.456340	5.775706
-792.953481	27.643363	5.785702
-790.818058	37.027629	5.795699
-788.542419	27.025018	5.805696
-787.139636	23.958824	5.815693
-785.414675	22.622068	5.825690
-783.297758	21.148461	5.835686
-781.483656	31.424031	5.845683
-779.329308	14.872850	5.855680
-777.626086	22.202660	5.865677
-775.815349	18.153966	5.875674
-773.797244	28.586397	5.885670
-772.120216	26.848391	5.895667
-770.173040	39.770948	5.905664
-768.210307	24.281372	5.915661
-766.003393	21.280869	5.925658
-764.499068	32.125402	5.935654
-762.653459	25.619204	5.945651
-760.941080	19.416915	5.955648
-759.009151	21.490548	5.965645
-756.956659	21.775036	5.975642
-755.296626	24.132109	5.985638
-753.479960	28.690316	5.995635
-751.246050	26.721230	6.005632
-749.239384	24.535849	6.015629
-747.629723	26.384699	6.025626
-745.759647	22.282335	6.035622
-743.809475	25.174062	6.045619
-742.255428	28.294875	6.055616
-740.031283	30.424450	6.065613
-737.939401	24.041534	6.075610
-736.156104	19.656224	6.085606
-734.912035	29.416657	6.095603
-732.832849	28.954845	6.105600
-730.503779	22.677705	6.115597
-728.890332	26.485303	6.125594
-726.868070	32.981070	6.135590
-725.084302	26.896858	6.145587
-723.075546	18.506325	6.155584
-721.721040	34.686051	6.165581
-719.777796	31.525631	6.175578
-717.240227	17.710958	6.185574
-715.509390	22.361852	6.195571
-714.065410	20.436933	6.205568
-711.972912	34.548868	6.215565
-709.934927	28.634028	6.225562
-708.562279	22.430801	6.235558
-706.588193	27.851199	6.245555
-704.596699	24.054704	6.255552
-702.468153	27.792642	6.265549
-700.668842	25.570966	6.275546
-698.601292	24.032695	6.285542
-697.001792	19.027880	6.295539
-695.353964	20.289653	6.305536
-693.065953	28.367612	6.315533
-691.248760	24.925799	6.325530
-689.235804	25.652424	6.335526
-687.614787	22.456684	6.345523
-685.747964	27.070085	6.355520
-683.661553	20.552308	6.365517
-682.286379	23.177568	6.375514
-680.101464	17.877130	6.385510
-678.402168	29.517885	6.395507
-676.256526	19.024602	6.405504
-674.277306	18.653020	6.415501
-672.841993	18.344664	6.425498
-670.727866	25.174725	6.435494
-668.845333	17.368047	6.445491
-666.663067	31.104129	6.455488
-665.007351	27.126068	6.465485
-663.163746	25.849384	6.475482
-661.326484	17.105798	6.485478
-659.353050	33.189836	6.495475
-657.325032	21.646483	6.505472
-655.864899	25.598622	6.515469
-654.053698	22.260419	6.525466
-651.947108	28.758569	6.535462
-650.159522	28.266056	6.545459
-648.208760	30.051004	6.555456
-646.451695	28.189778	6.565453
-644.480257	26.861108	6.575450
-642.433281	32.200450	6.585446
-640.532813	27.204419	6.595443
-638.965998	31.248466	6.605440
-636.870605	22.068942	6.615437
-634.837056	28.370371	6.625434
-633.298479	27.605043	6.635430
-630.986279	21.526467	6.645427
-629.431139	15.306758	6.655424
-627.905346	30.341365	6.665421
-625.734370	19.446205	6.675418
-623.662455	25.375222	6.685414
-621.959111	27.139724	6.695411
-620.005237	24.866574	6.705408
-618.136464	20.696624	6.715405
-616.463558	23.432242	6.725402
-614.436251	29.902045	6.735398
-612.359843	32.972654	6.745395
-610.352989	17.929267	6.755392
-608.586242	25.433790	6.765389
-606.994334	23.861066	6.775386
-605.180606	32.428545	6.785382
-603.142928	21.009997	6.795379
-601.635956	22.224870	6.805376
-599.472027	22.684311	6.815373
-597.463184	22.061762	6.825370
-595.491229	23.548124	6.835366
-593.871729	23.237232	6.845363
-591.771107	25.609298	6.855360
-590.099451	17.309031	6.865357
-588.164579	21.319575	6.875354
-586.291979	18.176864	6.885350
-584.420477	24.079515	6.895347
-582.533927	23.130747	6.905344
-580.245630	16.732374	6.915341
-578.942103	34.173951	6.925338
-577.103521	25.269165	6.935334
-575.593140	25.457263	6.945331
-572.872987	28.131408	6.955328
-570.974067	23.383556	6.965325
-569.333808	17.789716	6.975322
-567.503519	22.882704	6.985318
-565.523262	18.611305	6.995315
-563.845309	24.540155	7.005312
-561.909771	22.029997	7.015309
-559.792978	17.833103	7.025306
-557.962040	27.046775	7.035302
-556.559011	29.917121	7.045299
-554.297307	18.012855	7.055296
-552.098286	16.698431	7.065293
-550.037406	16.689673	7.075290
-549.028422	26.827223	7.085286
-547.355624	18.866250	7.095283
-544.894393	26.780915	7.105280
-543.202860	13.770971	7.115277
-541.313690	20.791814	7.125274
-539.210543	27.996364	7.135270
-537.469351	30.433786	7.145267
-535.684007	14.967969	7.155264
-533.653489	43.005921	7.165261
-531.866589	28.935542	7.175258
-529.929884	25.391079	7.185254
-528.099669	19.215907	7.195251
-526.092590	25.419039	7.205248
-524.293245	19.581936	7.215245
-522.675828	29.920725	7.225242
-520.899142	31.558332	7.235238
-518.861661	28.594584	7.245235
-516.574178	23.934702	7.255232
-515.090520	22.852980	7.265229
-513.214564	26.042529	7.275226
-511.008318	28.320437	7.285222
-509.237043	27.385401	7.295219
-507.619020	18.730614	7.305216
-505.558527	31.415862	7.315213
-503.633840	34.442911	7.325210
-501.874536	21.191648	7.335206
-499.706945	18.668161	7.345203
-497.949112	23.644892	7.355200
-496.115027	14.747199	7.365197
-494.466393	22.406460	7.375194
-492.552187	19.527156	7.385190
-490.555663	19.306111	7.395187
-488.783985	26.761002	7.405184
-486.966635	25.051306	7.415181
-484.889430	20.268730	7.425178
-483.193183	23.355959	7.435174
-481.049606	27.083809	7.445171
-479.382727	22.090470	7.455168
-477.574008	23.863511	7.465165
-475.528054	27.475913	7.475162
-473.294800	35.128669	7.485158
-471.600516	29.177333	7.495155
-470.015115	26.584225	7.505152
-468.083952	23.058062	7.515149
-466.483364	25.686928	7.525146
-464.409454	25.175669	7.535142
-462.457514	23.365555	7.545139
-460.446170	19.772914	7.555136
-458.465695	23.807866	7.565133
-456.861467	23.553186	7.575130
-454.921405	17.868912	7.585126
-453.060175	27.564123	7.595123
-451.237100	26.521390	7.605120
-449.260694	23.464828	7.615117
-447.333007	22.005945	7.625114
-445.324274	15.380774	7.635110
-443.961799	30.128999	7.645107
-441.874864	7.985512	7.655104
-440.075961	29.110465	7.665101
-437.829681	22.865758	7.675098
-436.024293	34.251375	7.685094
-434.479180	27.218692	7.695091
-432.395549	21.339414	7.705088
-430.242250	17.754128	7.715085
-428.579346	25.908499	7.725082
-427.035965	17.960371	7.735078
-424.698143	26.493259	7.745075
-422.952117	21.522052	7.755072
-421.209694	33.070884	7.765069
-419.288001	14.379883	7.775066
-417.451137	33.602612	7.785062
-415.751192	27.541469	7.795059
-413.853063	23.850108	7.805056
-411.712498	29.002623	7.815053
-409.789644	19.793988	7.825050
-407.911899	28.742967	7.835046
-406.148300	23.221106	7.845043
-404.091961	16.504686	7.855040
-402.546850	17.408881	7.865037
-400.469425	31.518806	7.875034
-398.519417	26.759767	7.885030
-396.686330	25.200772	7.895027
-395.021017	26.690478	7.905024
-392.888686	30.091808	7.915021
-391.052615	27.810808	7.925018
-389.289666	26.075135	7.935014
-387.442151	24.913292	7.945011
-385.582131	28.127595	7.955008
-383.575437	27.279792	7.965005
-381.957548	21.227037	7.975002
-379.667777	21.704479	7.984998
-377.713517	24.461664	7.994995
-376.028595	22.350062	8.004992
-374.656789	27.761133	8.014989
-372.416886	20.655451	8.024986
-370.512419	35.293520	8.034982
-368.610080	29.912152	8.044979
-366.590945	31.451172	8.054976
-364.675784	18.986637	8.064973
-362.835261	31.405587	8.074970
-361.433211	20.622345	8.084966
-359.348832	15.404545	8.094963
-357.285470	20.018418	8.104960
-355.458111	23.127439	8.114957
-353.560753	20.726164	8.124954
-351.719822	20.512707	8.134950
-349.831959	25.227233	8.144947
-347.900159	24.702449	8.154944
-346.265689	18.721276	8.164941
-344.253401	31.166502	8.174938
-342.417746	24.439572	8.184934
-340.497695	23.496696	8.194931
-338.304640	14.720212	8.204928
-336.326261	18.664030	8.214925
-335.321436	24.187390	8.224922
-333.213612	19.636877	8.234918
-331.087716	23.310851	8.244915
-329.002913	28.001851	8.254912
-327.356570	25.236482	8.264909
-325.580244	21.719359	8.274906
-323.509658	27.243106	8.284902
-321.436682	19.388903	8.294899
-319.764298	21.452233	8.304896
-318.093237	25.552489	8.314893
-316.105214	23.937245	8.324890
-314.189590	29.070502	8.334886
-312.125858	20.736232	8.344883
-310.458089	17.713262	8.354880
-308.754628	18.273313	8.364877
-306.739988	24.368075	8.374874
-304.939633	20.433473	8.384870
-303.072045	18.897461	8.394867
-300.793464	21.290328	8.404864
-299.181015	18.923522	8.414861
-297.019082	21.576576	8.424858
-295.597176	25.936081	8.434854
-293.665090	26.211770	8.444851
-291.702572	28.247756	8.454848
-289.702648	19.028482	8.464845
-288.020107	29.627045	8.474842
-286.025907	16.902067	8.484838
-284.137693	18.867818	8.494835
-282.133706	19.613588	8.504832
-280.534218	27.424537	8.514829
-278.791798	23.519725	8.524826
-276.517511	23.259258	8.534822
-274.849369	19.142110	8.544819
-272.835417	18.498490	8.554816
-270.952528	28.825102	8.564813
-269.254201	19.557673	8.574810
-267.209965	18.544511	8.584807
-265.366967	29.335361	8.594803
-263.704587	26.807460	8.604800
-261.323318	20.634512	8.614797
-259.646852	17.695445	8.624794
-258.117021	22.301414	8.634791
-256.076445	17.286466	8.644787
-254.191631	27.521212	8.654784
-252.651646	25.428090	8.664781
-250.512296	27.906383	8.674778
-248.495682	23.804680	8.684775
-246.374287	21.696130	8.694771
-244.758496	17.748400	8.704768
-242.722302	17.240194	8.714765
-241.140233	23.969282	8.724762
-239.306128	31.624405	8.734759
-237.206242	30.436607	8.744755
-235.242845	23.855142	8.754752
-233.511886	24.743996	8.764749
-231.694492	24.758584	8.774746
-229.648942	36.150263	8.784743
-227.933560	19.039569	8.794739
-225.571153	28.947083	8.804736
-224.218228	10.185933	8.814733
-222.153897	20.295743	8.824730
-220.548748	15.752922	8.834727
-218.324924	19.883446	8.844723
-216.656557	19.015570	8.854720
-214.881981	21.684733	8.864717
-212.762973	10.529793	8.874714
-211.208030	18.423683	8.884711
-209.061403	24.415370	8.894707
-207.066940	20.494066	8.904704
-205.495488	16.978147	8.914701
-203.442753	23.022715	8.924698
-201.604754	21.908318	8.934695
-199.754349	14.309190	8.944691
-198.120116	6.616678	8.954688
-196.053929	20.682810	8.964685
-193.990528	21.840725	8.974682
-192.405250	17.250569	8.984679
-190.170516	4.357817	8.994675
-188.532832	10.028128	9.004672
-186.794353	12.744122	9.014669
-184.507401	16.611988	9.024666
-183.028212	20.747698	9.034663
-180.767276	15.037687	9.044659
-179.063539	16.546675	9.054656
-177.336177	9.297179	9.064653
-175.410766	15.000531	9.074650
-173.413009	19.148227	9.084647
-171.705874	14.426540	9.094643
-170.050706	13.601853	9.104640
-167.455150	11.875574	9.114637
-166.037974	10.836250	9.124634
-164.448104	23.129591	9.134631
-162.142802	12.068112	9.144627
-160.207980	11.220910	9.154624
-158.524196	22.501438	9.164621
-156.635711	13.377410	9.174618
-154.979121	19.283140	9.184615
-152.794462	15.715192	9.194611
-150.632634	13.647639	9.204608
-149.214441	22.395450	9.214605
-147.268642	21.169162	9.224602
-145.491349	28.528710	9.234599
-143.647328	15.853055	9.244595
-141.559244	12.797865	9.254592
-139.543688	6.729175	9.264589
-137.857389	10.925018	9.274586
-136.054066	17.102593	9.284583
-133.944004	18.993596	9.294579
-132.119661	17.963530	9.304576
-130.313538	24.931670	9.314573
-128.473531	18.662061	9.324570
-126.458000	21.534410	9.334567
-124.723292	28.771304	9.344563
-122.715503	25.043718	9.354560
-120.910501	16.717721	9.364557
-119.128251	19.570458	9.374554
-117.477922	18.497119	9.384551
-115.303187	14.957628	9.394547
-113.379566	19.859265	9.404544
-111.532748	26.966183	9.414541
-109.784967	18.382496	9.424538
-108.217819	25.627190	9.434535
-105.711142	19.210181	9.444531
-104.008662	19.205306	9.454528
-102.192811	18.167145	9.464525
-100.034479	22.674527	9.474522
-98.277696	21.562112	9.484519
-96.729311	15.689558	9.494515
-94.874099	17.805981	9.504512
-92.614002	21.832951	9.514509
-91.161149	18.332865	9.524506
-89.295910	17.661021	9.534503
-86.903051	22.115210	9.544499
-85.428557	23.998714	9.554496
-83.316219	15.091639	9.564493
-81.775154	24.261973	9.574490
-79.649655	17.613714	9.584487
-77.538174	13.830151	9.594483
-76.045975	22.214123	9.604480
-73.956716	19.024597	9.614477
-72.121839	21.733194	9.624474
-70.284713	25.988709	9.634471
-68.492435	20.844582	9.644467
-66.419751	19.609167	9.654464
-64.732910	10.910506	9.664461
-62.810681	16.600253	9.674458
-60.782302	24.890806	9.684455
-59.139061	28.308892	9.694451
-57.288668	21.339821	9.704448
-55.406515	25.261342	9.714445
-53.187962	23.244820	9.724442
-51.403696	25.680472	9.734439
-49.808043	22.748118	9.744435
-47.895603	19.031066	9.754432
-46.070504	29.741287	9.764429
-43.931032	21.232516	9.774426
-41.779576	25.336865	9.784423
-40.187210	25.106458	9.794419
-38.327222	17.523277	9.804416
-36.489976	19.862072	9.814413
-35.193613	20.953020	9.824410
-32.974502	21.069456	9.834407
-30.951676	28.650441	9.844403
-28.916125	19.455671	9.854400
-26.858562	23.652374	9.864397
-25.254670	24.667432	9.874394
-23.320079	22.342569	9.884391
-21.521525	27.098457	9.894387
-19.638305	31.414552	9.904384
-17.606090	22.626086	9.914381
-15.591747	27.445447	9.924378
-14.310785	25.149066	9.934375
-12.216148	27.598395	9.944371
-10.196759	22.440185	9.954368
-8.426354	20.960947	9.964365
-6.492517	26.299968	9.974362
-4.817544	25.693272	9.984359
-3.511870	54.941624	9.994355
-2.349287	96.990575	10.004352
-1.021824	164.549942	10.014349
0.000000	224.309747	10.019354
0.307373	261.515522	10.024359
0.801585	296.734703	10.029363
1.403613	335.543069	10.034368
2.117495	376.735275	10.039373
2.101758	405.130937	10.044378
2.411734	415.078851	10.049383
2.197755	436.955852	10.054387
2.653726	445.428194	10.059392
3.277067	466.689161	10.064397
3.309698	464.764853	10.069402
3.302171	486.858147	10.074407
3.603940	495.741452	10.079411
3.638813	513.743892	10.084416
3.698186	508.126975	10.089421
3.836411	513.157235	10.094426
4.080419	519.947777	10.099431
4.170063	526.160573	10.104435
3.923084	525.610172	10.109440
4.167917	526.239684	10.114445
4.026966	530.759415	10.119450
4.157486	536.416937	10.124455
4.247940	538.949149	10.129459
4.524288	556.891051	10.134464
4.368401	544.758046	10.139469
4.179496	558.101832	10.144474
4.709295	561.522722	10.149479
4.648324	581.117426	10.154483
4.715454	567.431858	10.159488
4.808368	552.732980	10.164493
4.151826	567.543758	10.169498
4.480763	578.231477	10.174503
4.585090	585.522128	10.179507
4.645269	581.139763	10.184512
4.429670	589.509580	10.189517
4.566038	592.444471	10.194522
4.721769	588.138322	10.199527
4.622057	587.868771	10.204531
4.997978	601.024738	10.209536
5.159822	627.966998	10.214541
5.237872	616.148269	10.219546
5.071645	603.721984	10.224551
5.164777	618.156205	10.229555
5.402068	622.852170	10.234560
5.405080	628.977905	10.239565
4.992623	629.951949	10.244570
5.444614	638.332004	10.249575
5.379402	632.436876	10.254579
5.322948	639.049901	10.259584
5.459302	633.414349	10.264589
5.285014	641.794953	10.269594
5.534933	634.723653	10.274599
5.378267	634.817987	10.279603
5.363349	642.331107	10.284608
5.299854	643.654756	10.289613
5.366114	653.383095	10.294618
5.711014	655.847936	10.299623
6.079235	673.310142	10.304627
5.737329	693.823412	10.309632
6.058388	689.448288	10.314637
5.818143	693.417797	10.319642
6.061099	689.532933	10.324647
5.964510	686.985829	10.329651
6.310231	689.436352	10.334656
6.140838	681.804301	10.339661
5.609157	681.737684	10.344666
6.052666	694.379923	10.349671
6.117086	689.709851	10.354675
5.995360	694.559294	10.359680
6.096005	697.610287	10.364685
5.923980	707.471284	10.369690
6.529763	712.395500	10.374695
6.191752	722.095330	10.379699
6.449048	714.898238	10.384704
6.653525	731.262296	10.389709
6.280675	728.686710	10.394714
6.544646	728.562569	10.399719
6.702431	737.106299	10.404723
6.833215	735.002301	10.409728
6.571912	740.187827	10.414733
6.790982	731.986024	10.419738
6.781822	738.140555	10.424743
6.680354	746.667295	10.429747
6.871590	740.127262	10.434752
6.906906	747.638732	10.439757
6.537591	766.713602	10.444762
7.206964	769.817397	10.449767
7.295382	772.982318	10.454771
7.092414	791.667997	10.459776
7.385573	785.376609	10.464781
7.524243	786.057759	10.469786
7.354980	789.274821	10.474791
7.558924	788.034336	10.479795
7.467762	789.537448	10.484800
7.731605	785.928341	10.489805
7.479622	792.947930	10.494810
7.787979	788.182150	10.499815
7.702981	795.077337	10.504819
7.608706	792.703306	10.509824
7.753522	796.348081	10.514829
7.498096	802.445726	10.519834
7.925589	803.765192	10.524839
7.731842	796.203195	10.529843
7.676248	791.692579	10.534848
7.780593	784.228119	10.539853
7.629741	800.060739	10.544858
7.924774	792.159016	10.549863
7.855809	789.492372	10.554867
7.564004	804.062292	10.559872
7.638095	792.106859	10.564877
8.304143	819.899437	10.569882
8.174767	816.693656	10.574887
8.309774	827.836683	10.579891
8.450432	830.416131	10.584896
8.649527	826.705380	10.589901
8.223670	840.599718	10.594906
8.380879	841.426144	10.599911
8.649323	825.937339	10.604915
8.195955	833.640337	10.609920
8.197179	838.791908	10.614925
8.519243	848.861194	10.619930
8.368293	826.786242	10.624935
8.518492	840.689622	10.629939
8.494330	840.111554	10.634944
8.639169	833.902148	10.639949
8.493870	842.546321	10.644954
8.426958	858.865501	10.649959
8.940835	872.934830	10.654963
8.979805	879.821323	10.659968
9.005289	882.587881	10.664973
8.647863	884.868320	10.669978
9.067219	876.424759	10.674983
9.077773	887.083066	10.679987
8.762450	883.266695	10.684992
9.229440	868.943064	10.689997
8.763546	887.027417	10.695002
8.866626	883.935930	10.700007
9.204794	892.933521	10.705011
9.364715	916.659691	10.710016
9.662997	911.207936	10.715021
9.600857	919.067771	10.720026
9.887637	901.581143	10.725031
10.134196	895.932643	10.730035
9.819086	913.885748	10.735040
10.135390	889.722432	10.740045
9.842421	886.407113	10.745050
9.425039	888.681346	10.750055
9.775744	883.594972	10.755059
9.465032	888.749007	10.760064
9.926157	890.681273	10.765069
9.728873	887.245037	10.770074
9.954730	915.417087	10.775079
10.467127	914.551588	10.780083
9.953088	909.822324	10.785088
10.218113	898.292083	10.790093
10.032988	909.577696	10.795098
9.837033	923.771330	10.800103
10.096597	914.375536	10.805107
10.059500	914.982226	10.810112
10.334912	913.493792	10.815117
9.924149	922.924664	10.820122
10.080425	928.851042	10.825127
10.351393	931.639956	10.830131
10.313062	929.206518	10.835136
10.406610	931.966960	10.840141
10.214054	942.235085	10.845146
10.518746	951.625978	10.850151
11.019393	951.380510	10.855155
11.078989	950.341228	10.860160
10.998436	928.401548	10.865165
10.950865	920.324168	10.870170
10.745808	940.940537	10.875175
10.903824	917.223464	10.880179
10.923820	939.355635	10.885184
10.783503	926.945439	10.890189
10.777568	949.081761	10.895194
10.826960	967.186527	10.900199
11.099310	971.567935	10.905203
10.790569	963.909075	10.910208
11.187557	962.360244	10.915213
11.353336	971.077878	10.920218
11.530232	971.544783	10.925223
11.583907	968.428042	10.930227
11.124920	974.807383	10.935232
11.579387	968.420803	10.940237
11.484731	960.483373	10.945242
11.417233	969.094712	10.950247
11.399933	970.395252	10.955251
11.163357	977.384087	10.960256
11.520369	970.115773	10.965261
11.593990	973.606370	10.970266
11.638966	970.167743	10.975271
11.879570	963.723814	10.980275
11.587224	982.781959	10.985280
11.698649	978.099567	10.990285
11.887809	996.814429	10.995290
11.891389	992.259619	11.000295
12.211591	1001.482492	11.005299
12.117441	1005.051895	11.010304
12.610275	997.011280	11.015309
12.205285	978.042187	11.020314
12.168597	970.661626	11.025319
12.183114	970.405386	11.030323
11.774558	981.393958	11.035328
12.178758	993.475034	11.040333
12.323455	1002.218126	11.045338
12.790330	1004.046989	11.050343
12.677881	989.919737	11.055347
12.374906	1004.210943	11.060352
12.375885	992.547702	11.065357
12.265840	1014.063645	11.070362
12.495600	1011.776666	11.075367
12.795194	1003.118746	11.080371
12.442831	1005.076700	11.085376
12.143003	999.868542	11.090381
12.214166	1005.857412	11.095386
12.137352	1015.078962	11.100391
12.757336	1020.630222	11.105395
12.551278	1032.936397	11.110400
13.106955	1030.348275	11.115405
12.958769	1038.448979	11.120410
13.154369	1030.222366	11.125415
13.362652	1023.649525	11.130419
13.235898	1034.878617	11.135424
13.328589	1037.713333	11.140429
13.424289	1038.445503	11.145434
13.368201	1042.043537	11.150439
13.223375	1024.182480	11.155443
13.023422	1029.694211	11.160448
13.271003	1034.781329	11.165453
13.378276	1032.709423	11.170458
13.505169	1030.374193	11.175463
13.601945	1035.613096	11.180467
13.562187	1043.933051	11.185472
13.790090	1021.138213	11.190477
13.696930	1041.621761	11.195482
13.787718	1037.518225	11.200487
13.933666	1039.458205	11.205491
13.657635	1039.927968	11.210496
14.120519	1025.713648	11.215501
13.748730	1036.229622	11.220506
13.775553	1029.603719	11.225511
13.811710	1033.388887	11.230515
13.621683	1047.185883	11.235520
13.558953	1042.433477	11.240525
13.723995	1052.270908	11.245530
13.732335	1065.056999	11.250535
14.396914	1069.344338	11.255539
13.972168	1081.527740	11.260544
14.237674	1071.735083	11.265549
14.589336	1073.812567	11.270554
14.668815	1077.024711	11.275559
14.626478	1058.560641	11.280563
14.570579	1079.058798	11.285568
14.949148	1071.061600	11.290573
14.701042	1064.818575	11.295578
14.516796	1067.397848	11.300583
14.286725	1057.157543	11.305587
14.608479	1062.810002	11.310592
14.721405	1069.361516	11.315597
14.649613	1083.248497	11.320602
14.410449	1081.873659	11.325607
14.780298	1072.356095	11.330611
14.501143	1078.784068	11.335616
14.449780	1067.856088	11.340621
14.499220	1080.979412	11.345626
14.872280	1094.833299	11.350631
15.320863	1093.698849	11.355635
15.098365	1098.990276	11.360640
15.498413	1090.369899	11.365645
15.461735	1075.607582	11.370650
15.155097	1065.973993	11.375655
15.336821	1060.361001	11.380659
15.167384	1074.876981	11.385664
15.576429	1074.721816	11.390669
15.584493	1071.967141	11.395674
15.640836	1062.356084	11.400679
15.605299	1066.734589	11.405683
15.343449	1069.037658	11.410688
15.735972	1055.861123	11.415693
15.763856	1074.636503	11.420698
15.393324	1064.825448	11.425703
15.634790	1059.543549	11.430707
16.075398	1088.911704	11.435712
15.950299	1079.214458	11.440717
15.624244	1085.495374	11.445722
15.882131	1088.478793	11.450727
16.319035	1093.997782	11.455731
15.643059	1090.286187	11.460736
15.756082	1085.642929	11.465741
15.914422	1097.047370	11.470746
15.950797	1100.502938	11.475751
16.381488	1093.337929	11.480755
16.026312	1110.591193	11.485760
16.315299	1093.465104	11.490765
16.276569	1110.046578	11.495770
16.261949	1106.059184	11.500775
16.415085	1106.933584	11.505779
16.178099	1107.165309	11.510784
16.579275	1104.206002	11.515789
16.548490	1105.067159	11.520794
16.379421	1116.567992	11.525799
16.802612	1099.896730	11.530803
16.450032	1099.711654	11.535808
16.277131	1103.512837	11.540813
16.405729	1105.963372	11.545818
16.641584	1114.095905	11.550823
16.749871	1114.174790	11.555827
16.760087	1127.801153	11.560832
16.896670	1118.155183	11.565837
17.085785	1119.763437	11.570842
17.167362	1117.343958	11.575847
17.156429	1121.273854	11.580851
17.145157	1118.350366	11.585856
17.281875	1119.549084	11.590861
17.391867	1120.728410	11.595866
17.093537	1118.142443	11.600871
17.368496	1113.679929	11.605875
17.056195	1127.353001	11.610880
17.241113	1132.864887	11.615885
17.547119	1110.827004	11.620890
17.186109	1122.183413	11.625895
17.224133	1115.774881	11.630899
17.307461	1126.661454	11.635904
17.354577	1121.210258	11.640909
17.348812	1118.538204	11.645914
17.447067	1120.312337	11.650919
17.740905	1116.710981	11.655923
17.197358	1116.133740	11.660928
17.630886	1145.189326	11.665933
17.955160	1154.402187	11.670938
17.647311	1156.416138	11.675943
18.289051	1137.637854	11.680947
18.206221	1143.692344	11.685952
18.229770	1149.395554	11.690957
18.121945	1124.570941	11.695962
17.894304	1115.549192	11.700967
18.168438	1123.388620	11.705971
18.132202	1146.012624	11.710976
18.410832	1148.268925	11.715981
18.583110	1142.242669	11.720986
18.421209	1134.284330	11.725991
18.326693	1121.215379	11.730995
18.066123	1112.976322	11.736000
18.345765	1128.431556	11.741005
18.529303	1149.541330	11.746010
18.588332	1140.773464	11.751015
19.155960	1125.026887	11.756019
18.656765	1130.901775	11.761024
18.577084	1122.364202	11.766029
18.717040	1123.570288	11.771034
18.425323	1131.831132	11.776039
18.849641	1139.244491	11.781043
18.542075	1145.736950	11.786048
18.782259	1142.405920	11.791053
18.485735	1143.216423	11.796058
18.729677	1141.557944	11.801063
18.576676	1142.211515	11.806067
18.577140	1149.744522	11.811072
18.478565	1153.874486	11.816077
18.751655	1165.752691	11.821082
19.032721	1171.686074	11.826087
19.395251	1173.276136	11.831091
19.045747	1183.151570	11.836096
19.355084	1180.626367	11.841101
19.494606	1176.352593	11.846106
19.237963	1181.804037	11.851111
19.346476	1155.762146	11.856115
19.625354	1171.151316	11.861120
19.481610	1173.738340	11.866125
19.748844	1178.533791	11.871130
19.684908	1173.147596	11.876135
19.962899	1178.832313	11.881139
19.706134	1179.556052	11.886144
19.682373	1177.140748	11.891149
20.035987	1172.599438	11.896154
19.379729	1179.497611	11.901159
20.021870	1171.172890	11.906163
19.863118	1182.993829	11.911168
19.608112	1184.737580	11.916173
19.837353	1184.483359	11.921178
19.877113	1198.773708	11.926183
20.418526	1212.933597	11.931187
20.354332	1207.938518	11.936192
19.986954	1189.645971	11.941197
20.121146	1210.635970	11.946202
20.179441	1211.574390	11.951207
20.372957	1196.699541	11.956211
20.240177	1202.317318	11.961216
20.391559	1205.857071	11.966221
20.657492	1212.625521	11.971226
20.585976	1213.813304	11.976231
20.726085	1193.919618	11.981235
20.600065	1201.570597	11.986240
20.926696	1208.452367	11.991245
20.824451	1209.545703	11.996250
20.610767	1196.557192	12.001255
21.314364	1192.117753	12.006259
21.089925	1172.096158	12.011264
20.478896	1163.249068	12.016269
20.537298	1179.985441	12.021274
20.843229	1193.675088	12.026279
21.125301	1193.180628	12.031283
20.949259	1198.048363	12.036288
21.142733	1206.566179	12.041293
21.069400	1177.358326	12.046298
20.674538	1179.832438	12.051303
20.848019	1167.078671	12.056307
21.030608	1178.583389	12.061312
20.863918	1175.419749	12.066317
20.894750	1171.316277	12.071322
20.793121	1170.249078	12.076327
20.724537	1160.855000	12.081331
20.750965	1178.156291	12.086336
21.000820	1195.783092	12.091341
21.483643	1191.911878	12.096346
20.894466	1194.148900	12.101351
20.939439	1173.530820	12.106355
20.956692	1177.724319	12.111360
20.808883	1171.734911	12.116365
20.942271	1169.390738	12.121370
20.956153	1170.098118	12.126375
20.708240	1163.545935	12.131379
20.711184	1177.141966	12.136384
20.963303	1168.010548	12.141389
21.153037	1174.828981	12.146394
20.645444	1181.138892	12.151399
20.866939	1170.525284	12.156403
20.756352	1170.754197	12.161408
20.947684	1162.873544	12.166413
20.700653	1179.538783	12.171418
21.007410	1185.840237	12.176423
21.324598	1173.881987	12.181427
20.781615	1173.653160	12.186432
20.848770	1179.584394	12.191437
21.019290	1179.910398	12.196442
20.782057	1181.730163	12.201447
21.018580	1175.357754	12.206451
20.900664	1184.234306	12.211456
20.717199	1178.250582	12.216461
21.265950	1175.160491	12.221466
20.859206	1191.955297	12.226471
21.377226	1178.952601	12.231475
20.970378	1197.130423	12.236480
20.833492	1188.097307	12.241485
21.151340	1173.910706	12.246490
20.701483	1184.820862	12.251495
21.036040	1185.831913	12.256499
21.047963	1180.913012	12.261504
20.937766	1189.143359	12.266509
21.016246	1181.597665	12.271514
20.742670	1188.147799	12.276519
21.319612	1182.858081	12.281523
21.252778	1181.862602	12.286528
20.850375	1166.297504	12.291533
20.694308	1162.999707	12.296538
20.341435	1171.834878	12.301543
20.606589	1181.011454	12.306547
20.848644	1183.445483	12.311552
20.842590	1191.031591	12.316557
21.038233	1181.530702	12.321562
20.930675	1186.989909	12.326567
21.343923	1184.180049	12.331571
21.289338	1186.722893	12.336576
20.843328	1184.438012	12.341581
21.128894	1163.915614	12.346586
20.731618	1161.454230	12.351591
20.798359	1159.417157	12.356595
20.726869	1171.615254	12.361600
20.938583	1168.455917	12.366605
20.988145	1178.944214	12.371610
20.908280	1184.187691	12.376615
20.864754	1158.926984	12.381619
20.672720	1165.926151	12.386624
20.844774	1178.661000	12.391629
20.985999	1177.947730	12.396634
20.995175	1194.378156	12.401639
21.146517	1174.653015	12.406643
20.894378	1170.820181	12.411648
20.714145	1162.394816	12.416653
20.979886	1158.406846	12.421658
20.779312	1155.018379	12.426663
20.939930	1144.565887	12.431667
20.932637	1168.762267	12.436672
20.807033	1163.505760	12.441677
20.724738	1160.153620	12.446682
20.992244	1163.312141	12.451687
20.906173	1155.860514	12.456691
20.704787	1164.751944	12.461696
20.983465	1180.448663	12.466701
21.029248	1180.701522	12.471706
20.838822	1176.671185	12.476711
20.966503	1160.874889	12.481715
20.816260	1172.079449	12.486720
20.509523	1169.942669	12.491725
20.682253	1164.463537	12.496730
20.750336	1191.087486	12.501735
21.143403	1195.525404	12.506739
21.204742	1196.762959	12.511744
20.938663	1191.953050	12.516749
21.077766	1171.127571	12.521754
20.619512	1180.028440	12.526759
21.000725	1161.913000	12.531763
20.896466	1169.740265	12.536768
20.823021	1171.395132	12.541773
20.949000	1161.861212	12.546778
20.820862	1167.810974	12.551783
20.813638	1171.032238	12.556787
20.710334	1183.550811	12.561792
20.818273	1200.123188	12.566797
21.357459	1195.564889	12.571802
20.599615	1186.946206	12.576807
20.897715	1175.670668	12.581811
21.071749	1186.632707	12.586816
20.977387	1183.148444	12.591821
21.236522	1174.436952	12.596826
20.969542	1173.446588	12.601831
21.021514	1180.282265	12.606835
20.950556	1191.672890	12.611840
20.913968	1187.821442	12.616845
21.181548	1181.046684	12.621850
21.149982	1184.317565	12.626855
21.100139	1173.537496	12.631859
21.384347	1175.945877	12.636864
21.177130	1180.167294	12.641869
21.349626	1171.360811	12.646874
20.872735	1159.388875	12.651879
20.808498	1156.913797	12.656883
20.609627	1161.996474	12.661888
21.009740	1163.124800	12.666893
21.174918	1153.128893	12.671898
20.844767	1141.042104	12.676903
21.127878	1141.427420	12.681907
21.133354	1147.504097	12.686912
20.952155	1135.631676	12.691917
20.732007	1139.803104	12.696922
20.662878	1142.285181	12.701927
20.943655	1136.385126	12.706931
20.869346	1143.032768	12.711936
20.643032	1150.407980	12.716941
21.025369	1141.639010	12.721946
20.677674	1158.588363	12.726951
20.952827	1141.566926	12.731955
20.946414	1148.468670	12.736960
20.977627	1149.927070	12.741965
21.142811	1152.199889	12.746970
20.900279	1141.176186	12.751975
21.107687	1145.769857	12.756979
20.836794	1142.115063	12.761984
20.759497	1153.289050	12.766989
21.128010	1138.455736	12.771994
20.864548	1149.323520	12.776999
21.019476	1149.946902	12.782003
20.849803	1154.987071	12.787008
20.629553	1151.947096	12.792013
20.912248	1151.734813	12.797018
20.747440	1156.769476	12.802023
21.263545	1151.579359	12.807027
20.663005	1158.757218	12.812032
20.723270	1153.027945	12.817037
20.889082	1145.755347	12.822042
20.735317	1157.384658	12.827047
21.180461	1156.581914	12.832051
20.956824	1153.761675	12.837056
20.951419	1157.909897	12.842061
20.928883	1149.952975	12.847066
20.841712	1147.850565	12.852071
21.055658	1142.538333	12.857075
20.997734	1147.686833	12.862080
20.794705	1151.700992	12.867085
21.190974	1150.060795	12.872090
20.767261	1154.507546	12.877095
20.827363	1155.163398	12.882099
21.157130	1146.245115	12.887104
20.763549	1156.600647	12.892109
21.090387	1150.890359	12.897114
20.888580	1153.054554	12.902119
21.091733	1140.767588	12.907123
20.625564	1155.521788	12.912128
20.531142	1164.407196	12.917133
20.824560	1151.631160	12.922138
20.792650	1171.382877	12.927143
21.181779	1154.778486	12.932147
20.945990	1156.866100	12.937152
20.700862	1160.827052	12.942157
20.733560	1164.943967	12.947162
20.924118	1163.147343	12.952167
21.004274	1155.517816	12.957171
20.897621	1163.290266	12.962176
20.445054	1167.257497	12.967181
21.023092	1159.078625	12.972186
20.850396	1174.836291	12.977191
21.062067	1158.238123	12.982195
20.866194	1157.550233	12.987200
20.700330	1170.323201	12.992205
21.167494	1152.116794	12.997210
20.623859	1162.699691	13.002215
20.721450	1175.306064	13.007219
20.864699	1153.111149	13.012224
20.532208	1181.401158	13.017229
20.855590	1163.739642	13.022234
20.751082	1170.716967	13.027239
20.846718	1175.237010	13.032243
20.986201	1173.480070	13.037248
21.072648	1167.368145	13.042253
21.201597	1158.245340	13.047258
20.912066	1170.552330	13.052263
20.959213	1179.788908	13.057267
20.950234	1169.707225	13.062272
20.944362	1169.651353	13.067277
21.580506	1169.198192	13.072282
21.107067	1179.005080	13.077287
21.104395	1171.645800	13.082291
21.052652	1155.151150	13.087296
20.934274	1183.143661	13.092301
21.148271	1176.525685	13.097306
21.003680	1153.384771	13.102311
20.948408	1164.336056	13.107315
21.227573	1130.186661	13.112320
20.692096	1168.923232	13.117325
21.122208	1139.330805	13.122330
20.694444	1151.142585	13.127335
21.014690	1150.511150	13.132339
20.821766	1141.671504	13.137344
20.683608	1162.802645	13.142349
21.349374	1130.969640	13.147354
20.740333	1146.117202	13.152359
20.819804	1155.485804	13.157363
21.098190	1153.209971	13.162368
20.645493	1164.740309	13.167373
21.180416	1150.679958	13.172378
20.961627	1141.741936	13.177383
20.788363	1158.360692	13.182387
21.019426	1124.657376	13.187392
20.866058	1170.061869	13.192397
21.172451	1140.083895	13.197402
20.840081	1171.873131	13.202407
20.936096	1152.491161	13.207411
21.118430	1138.600598	13.212416
21.044936	1157.518412	13.217421
21.168095	1153.483798	13.222426
21.075902	1154.080361	13.227431
21.036314	1158.456386	13.232435
21.137531	1149.609246	13.237440
20.738258	1164.904720	13.242445
20.878744	1156.718366	13.247450
20.593216	1146.999352	13.252455
20.945902	1156.146182	13.257459
21.085019	1146.349979	13.262464
20.817009	1155.515381	13.267469
20.882929	1151.038888	13.272474
20.663370	1158.001441	13.277479
20.681688	1153.213993	13.282483
20.426935	1157.026669	13.287488
20.623482	1158.431891	13.292493
21.081705	1154.999850	13.297498
20.942542	1164.147861	13.302503
21.064248	1161.089615	13.307507
21.130423	1151.316080	13.312512
21.045450	1158.160973	13.317517
21.055927	1145.611420	13.322522
20.773765	1173.762500	13.327527
20.945400	1147.844596	13.332531
20.949790	1176.438834	13.337536
20.929895	1148.520354	13.342541
21.024611	1154.434566	13.347546
21.184516	1168.388755	13.352551
21.000525	1149.696424	13.357555
20.851589	1129.454687	13.362560
20.653818	1136.554103	13.367565
20.667516	1148.588784	13.372570
20.567483	1162.291111	13.377575
20.917094	1158.909509	13.382579
20.812772	1150.872590	13.387584
20.833248	1173.508093	13.392589
21.225903	1145.424471	13.397594
21.010154	1155.206012	13.402599
20.957195	1176.158003	13.407603
21.032135	1169.065467	13.412608
20.941305	1159.001577	13.417613
20.898556	1166.940456	13.422618
20.923765	1159.078416	13.427623
20.808517	1135.675806	13.432627
21.140463	1156.604226	13.437632
21.052553	1149.482479	13.442637
20.966767	1134.231194	13.447642
20.882671	1140.975013	13.452647
20.835044	1128.065735	13.457651
20.901576	1130.029432	13.462656
20.694139	1127.219231	13.467661
20.829069	1128.676856	13.472666
20.456769	1130.116033	13.477671
20.848216	1143.147019	13.482675
21.138454	1151.151052	13.487680
20.992526	1163.182818	13.492685
21.018962	1141.186325	13.497690
20.865415	1134.068748	13.502695
20.716639	1138.140482	13.507699
20.952731	1141.015426	13.512704
20.911223	1138.478379	13.517709
20.879969	1124.088886	13.522714
20.842139	1145.443696	13.527719
21.043062	1130.397422	13.532723
21.138437	1143.907717	13.537728
21.088937	1135.064124	13.542733
21.012934	1124.633616	13.547738
20.718310	1117.648934	13.552743
20.454266	1139.221165	13.557747
20.575246	1136.032152	13.562752
20.849760	1149.444494	13.567757
21.083908	1150.353285	13.572762
20.759295	1171.616679	13.577767
21.021501	1138.608534	13.582771
20.759094	1157.699980	13.587776
20.732494	1160.812368	13.592781
21.104116	1158.457009	13.597786
20.861884	1156.801954	13.602791
20.932981	1151.848393	13.607795
20.963008	1139.142762	13.612800
20.648334	1166.218799	13.617805
21.112275	1156.578940	13.622810
20.735164	1141.979662	13.627815
20.841461	1153.673148	13.632819
20.925316	1173.587754	13.637824
20.767005	1160.183588	13.642829
20.778935	1157.710555	13.647834
20.843322	1183.794185	13.652839
20.710346	1167.608945	13.657843
21.220806	1159.921824	13.662848
20.961815	1183.658477	13.667853
20.873056	1171.684550	13.672858
20.302185	1159.694486	13.677863
21.099295	1149.843797	13.682867
21.219992	1159.361945	13.687872
20.929952	1171.211699	13.692877
20.837390	1167.455916	13.697882
20.981847	1169.211647	13.702887
20.794378	1164.384478	13.707891
20.859671	1158.403665	13.712896
20.767058	1168.230231	13.717901
21.158778	1164.887642	13.722906
20.899655	1176.547965	13.727911
20.806247	1149.517997	13.732915
20.830072	1147.437308	13.737920
20.797159	1173.620017	13.742925
21.059732	1156.017095	13.747930
21.016790	1153.196422	13.752935
20.973198	1143.995489	13.757939
20.806366	1137.365731	13.762944
20.670363	1136.814950	13.767949
20.579165	1142.042872	13.772954
21.133460	1160.016888	13.777959
21.340203	1165.618347	13.782963
21.270506	1138.267649	13.787968
20.925774	1140.905647	13.792973
21.120158	1135.766848	13.797978
20.876291	1130.448791	13.802983
21.031400	1135.709966	13.807987
20.917783	1136.846111	13.812992
20.963661	1134.498555	13.817997
20.881517	1121.096470	13.823002
20.776639	1134.774313	13.828007
21.015308	1139.883391	13.833011
20.884394	1138.988022	13.838016
20.450382	1136.940933	13.843021
20.790152	1130.053759	13.848026
20.608156	1132.892881	13.853031
20.593450	1132.716993	13.858035
21.102890	1133.941421	13.863040
20.741126	1161.157423	13.868045
21.102177	1134.304159	13.873050
20.451432	1145.117015	13.878055
20.619032	1160.916585	13.883059
21.039303	1156.057143	13.888064
21.149743	1162.700559	13.893069
21.019237	1141.544384	13.898074
20.865299	1159.574589	13.903079
20.740465	1140.874410	13.908083
21.022050	1130.068321	13.913088
20.740104	1135.793443	13.918093
20.678987	1137.186142	13.923098
20.795296	1158.264075	13.928103
20.952559	1170.081909	13.933107
21.065004	1162.638041	13.938112
21.140800	1178.803934	13.943117
20.986523	1135.960495	13.948122
21.001846	1162.722118	13.953127
20.977483	1139.118925	13.958131
20.913727	1149.420271	13.963136
20.577089	1160.667166	13.968141
21.128467	1141.318238	13.973146
20.716211	1141.910656	13.978151
20.525282	1148.463361	13.983155
21.116228	1134.231664	13.988160
20.814154	1150.811031	13.993165
20.816745	1146.525990	13.998170
20.968992	1135.251669	14.003175
20.563289	1145.558664	14.008179
21.097647	1161.820135	14.013184
21.013829	1154.636232	14.018189
20.732929	1161.410863	14.023207
21.244502	1141.510266	14.028224
20.771489	1137.780747	14.033242
21.106316	1138.309291	14.038259
21.052945	1147.789968	14.043277
21.007494	1148.942275	14.048295
20.849142	1143.592780	14.053312
20.477805	1169.498426	14.058330
21.116149	1159.575168	14.063347
21.035510	1168.734610	14.068365
21.381756	1185.028451	14.073383
21.294699	1165.948423	14.078400
21.094742	1151.385017	14.083418
21.220147	1154.502981	14.088435
21.373866	1162.479944	14.093453
20.803055	1151.406259	14.098471
20.938164	1143.494838	14.103488
20.793364	1181.290356	14.108506
21.472147	1171.327609	14.113523
21.321052	1186.821503	14.118541
21.323979	1190.599195	14.123559
21.115693	1169.062694	14.128576
21.206416	1197.788896	14.133594
21.579085	1180.170714	14.138611
21.171175	1174.540132	14.143629
21.576217	1175.224210	14.148647
21.331820	1174.113336	14.153664
21.268413	1165.734944	14.158682
21.322246	1159.735011	14.163699
21.196013	1192.665657	14.168717
21.437281	1194.124575	14.173735
21.511879	1186.052905	14.178752
21.248567	1195.230488	14.183770
21.551377	1175.696604	14.188787
21.417830	1195.216000	14.193805
21.272921	1186.642967	14.198823
21.379627	1202.172834	14.203840
21.126083	1206.348493	14.208858
21.522607	1190.547958	14.213875
21.373890	1199.990396	14.218893
21.217128	1193.454634	14.223911
21.565645	1192.837470	14.228928
21.230470	1189.664795	14.233946
21.687923	1192.987769	14.238963
21.530057	1186.900473	14.243981
21.525027	1226.001374	14.248999
21.702995	1197.238478	14.254016
21.744247	1218.872368	14.259034
22.076507	1215.947147	14.264051
21.664978	1231.718568	14.269069
21.657828	1207.903767	14.274087
21.942726	1222.856280	14.279104
21.789139	1221.307797	14.284122
21.930228	1220.256552	14.289139
21.964776	1215.310397	14.294157
22.055864	1209.194395	14.299175
22.212989	1202.215330	14.304192
21.964614	1201.005993	14.309210
21.961504	1196.786256	14.314227
21.699530	1183.118274	14.319245
21.791216	1185.894004	14.324263
22.051603	1189.001457	14.329280
21.981648	1221.158744	14.334298
22.323614	1209.651583	14.339315
22.111738	1205.798603	14.344333
22.012709	1204.858013	14.349351
21.962570	1200.867560	14.354368
22.183814	1202.054409	14.359386
21.996054	1215.543965	14.364403
22.008632	1219.394054	14.369421
21.928729	1226.211305	14.374439
22.153670	1220.572572	14.379456
22.218953	1220.491340	14.384474
22.293112	1222.881356	14.389491
22.278952	1212.137244	14.394509
22.514146	1219.129166	14.399527
22.368092	1217.186247	14.404544
22.207174	1221.845759	14.409562
22.583341	1217.301270	14.414579
22.361193	1214.315044	14.419597
22.115584	1218.711225	14.424615
22.361665	1220.227578	14.429632
22.315654	1213.656839	14.434650
22.469153	1231.766762	14.439667
22.572486	1207.099109	14.444685
22.657421	1216.428791	14.449703
22.453173	1208.365405	14.454720
22.423068	1218.105097	14.459738
22.450793	1218.599260	14.464755
22.479215	1222.936007	14.469773
22.367019	1219.902357	14.474791
22.943234	1206.158866	14.479808
22.228468	1230.722625	14.484826
22.272042	1218.224907	14.489843
21.969056	1216.486333	14.494861
22.032632	1211.644081	14.499879
22.174531	1202.018614	14.504896
22.000528	1238.749340	14.509914
22.666697	1235.663899	14.514931
22.481301	1249.244340	14.519949
22.567016	1251.270740	14.524967
22.764646	1253.947793	14.529984
22.742387	1254.250164	14.535002
22.781194	1251.423647	14.540019
23.014417	1249.157549	14.545037
22.907714	1248.820617	14.550055
22.968760	1236.791980	14.555072
22.666804	1245.736671	14.560090
22.875017	1251.973181	14.565107
22.900761	1261.592316	14.570125
22.623485	1245.387981	14.575143
22.978805	1247.940787	14.580160
22.822456	1251.798951	14.585178
22.635973	1252.330425	14.590195
22.967500	1244.397060	14.595213
22.826440	1250.805674	14.600231
22.965684	1245.204194	14.605248
22.944241	1262.638952	14.610266
23.135566	1268.747608	14.615283
23.580559	1256.670301	14.620301
23.250876	1263.536846	14.625319
23.273520	1247.237485	14.630336
23.192036	1244.203651	14.635354
23.227208	1246.886165	14.640371
23.365056	1244.624269	14.645389
23.442696	1244.190299	14.650407
23.552030	1238.596738	14.655424
23.286468	1235.258801	14.660442
23.232964	1248.612150	14.665459
23.466115	1251.355892	14.670477
23.183315	1248.418656	14.675495
23.513266	1237.976700	14.680512
23.475565	1256.776213	14.685530
23.289950	1248.643769	14.690547
23.412988	1254.127840	14.695565
23.088658	1243.087127	14.700583
23.423176	1244.095473	14.705600
23.263127	1246.209832	14.710618
23.337907	1242.762557	14.715635
23.617024	1234.640939	14.720653
23.529103	1247.483851	14.725671
23.500752	1244.768715	14.730688
23.407780	1251.794118	14.735706
23.440586	1242.140408	14.740723
23.500804	1244.836229	14.745741
23.321883	1252.278015	14.750759
23.652370	1271.640137	14.755776
23.858680	1274.639836	14.760794
23.854161	1266.431309	14.765811
24.042089	1271.566855	14.770829
23.780441	1265.969535	14.775847
23.984323	1251.830804	14.780864
23.862696	1249.613438	14.785882
23.682971	1246.025866	14.790899
23.673141	1237.292840	14.795917
23.661681	1246.949358	14.800935
24.376760	1256.718082	14.805952
23.863414	1254.075578	14.810970
23.851394	1248.660236	14.815987
24.382127	1240.160300	14.821005
23.903284	1242.795814	14.826023
23.990587	1244.867575	14.831040
24.280159	1239.276726	14.836058
23.970016	1239.802756	14.841075
23.855190	1240.750641	14.846093
23.955354	1241.705134	14.851111
24.297158	1251.269134	14.856128
24.075161	1243.151934	14.861146
24.105913	1246.407704	14.866163
23.914280	1241.269537	14.871181
24.045512	1246.583994	14.876199
24.179540	1235.416702	14.881216
24.328998	1235.160031	14.886234
23.944295	1243.337738	14.891251
24.224756	1242.979953	14.896269
24.035941	1239.694265	14.901287
24.303857	1232.626732	14.906304
24.304483	1242.339519	14.911322
24.377243	1244.402589	14.916339
24.471211	1244.947532	14.921357
23.835560	1250.046120	14.926375
24.141969	1256.907159	14.931392
24.410295	1268.812422	14.936410
24.394665	1271.315862	14.941427
24.435012	1277.178055	14.946445
24.559377	1263.508150	14.951463
24.907225	1270.040133	14.956480
24.623038	1261.852620	14.961498
24.545449	1250.467396	14.966515
24.709452	1239.194651	14.971533
24.613344	1235.049508	14.976551
24.395259	1235.699273	14.981568
24.457501	1251.248869	14.986586
24.660218	1254.796521	14.991603
24.776304	1248.770893	14.996621
24.628119	1248.829094	15.001639
24.725080	1255.860384	15.006656
24.898696	1266.763056	15.011674
24.461856	1270.659670	15.016691
24.985601	1256.831696	15.021709
24.629580	1250.941136	15.026727
24.802983	1262.164719	15.031744
24.452442	1273.688943	15.036762
24.393133	1263.996430	15.041779
24.775224	1265.181225	15.046797
24.809894	1269.848881	15.051815
24.845628	1271.680346	15.056832
24.840524	1257.010254	15.061850
24.920306	1281.499281	15.066867
24.995965	1262.025104	15.071885
24.487924	1269.709717	15.076903
24.908886	1272.006678	15.081920
25.263733	1256.914253	15.086938
24.819011	1275.203009	15.091955
24.992560	1271.510324	15.096973
24.906965	1275.928190	15.101991
24.878158	1298.397598	15.107008
25.080513	1292.696376	15.112026
24.922302	1303.046414	15.117043
25.254375	1290.620591	15.122061
25.488412	1296.923785	15.127079
25.240288	1318.592967	15.132096
25.337497	1306.880959	15.137114
25.465101	1298.100809	15.142131
25.268459	1290.751856	15.147149
25.468723	1309.038453	15.152167
25.424594	1292.266795	15.157184
25.516133	1264.653219	15.162202
25.230266	1266.355087	15.167219
25.160813	1259.786493	15.172237
25.170047	1288.297795	15.177255
25.252873	1305.726986	15.182272
25.459329	1299.937022	15.187290
25.754802	1296.430942	15.192307
25.779957	1291.023811	15.197325
25.733522	1292.440542	15.202343
25.571140	1289.513977	15.207360
25.852625	1285.159166	15.212378
25.351223	1282.780580	15.217395
25.655462	1280.688759	15.222413
25.655494	1290.077644	15.227431
25.547016	1292.427591	15.232448
25.310612	1290.214368	15.237466
25.585034	1299.010537	15.242483
25.659257	1287.837014	15.247501
25.506865	1299.164495	15.252519
25.417171	1297.547613	15.257536
25.462501	1297.085763	15.262554
25.557180	1290.431206	15.267571
25.701885	1310.848574	15.272589
25.566438	1296.502811	15.277607
25.489701	1311.992844	15.282624
26.075350	1310.919451	15.287642
25.831287	1305.615025	15.292659
25.670217	1330.090641	15.297677
25.803976	1318.108538	15.302695
26.183792	1334.993343	15.307712
26.389204	1323.440235	15.312730
26.169605	1320.255388	15.317747
26.108378	1311.019306	15.322765
26.257399	1331.022328	15.327783
26.238851	1330.598978	15.332800
26.565475	1317.862557	15.337818
26.486488	1323.289218	15.342835
26.328540	1308.744120	15.347853
26.199555	1299.301785	15.352871
26.100569	1299.515726	15.357888
26.441782	1290.391641	15.362906
26.154492	1296.696189	15.367923
26.314015	1290.990789	15.372941
26.634006	1295.650698	15.377959
26.487715	1306.307135	15.382976
26.712478	1289.926728	15.387994
26.503445	1287.877445	15.393011
26.701922	1283.158366	15.398029
26.287366	1298.593730	15.403047
26.450084	1291.720691	15.408064
26.465514	1290.027273	15.413082
25.854255	1291.217925	15.418099
26.140965	1293.643263	15.423117
26.351403	1314.886962	15.428135
26.165199	1319.887150	15.433152
26.617423	1314.013940	15.438170
26.573623	1318.785358	15.443187
26.765571	1312.936358	15.448205
26.664636	1319.777456	15.453223
26.319539	1330.393263	15.458240
26.883756	1316.486422	15.463258
26.704908	1316.463002	15.468275
26.743809	1320.843722	15.473293
26.962500	1312.439129	15.478311
26.593877	1318.286345	15.483328
26.969134	1318.814741	15.488346
26.851715	1320.013145	15.493363
26.833963	1311.035957	15.498381
26.691393	1314.829022	15.503399
26.768975	1313.262535	15.508416
26.844482	1312.390050	15.513434
26.572569	1322.336685	15.518451
26.213482	1323.534309	15.523469
26.505586	1342.281331	15.528487
26.748018	1356.688649	15.533504
26.780926	1348.106036	15.538522
27.187383	1341.774519	15.543539
26.953040	1345.008101	15.548557
27.335259	1344.785088	15.553575
27.337397	1342.411121	15.558592
27.387116	1335.299692	15.563610
27.398421	1343.529121	15.568627
27.561117	1331.794064	15.573645
27.620809	1335.289047	15.578663
27.444631	1353.262949	15.583680
27.521809	1324.141512	15.588698
27.350437	1369.122288	15.593715
27.296090	1331.092138	15.598733
27.765308	1338.664965	15.603751
27.377667	1350.055173	15.608768
27.697070	1347.039172	15.613786
27.462277	1344.828829	15.618803
27.751618	1344.497939	15.623821
28.070645	1333.480382	15.628839
27.609600	1322.599832	15.633856
27.547397	1300.146399	15.638874
27.241923	1314.405119	15.643891
27.374269	1314.363525	15.648909
27.628814	1328.789332	15.653927
27.503332	1334.857313	15.658944
27.825450	1341.198385	15.663962
27.725725	1337.631063	15.668979
27.594752	1347.119528	15.673997
27.962892	1342.514935	15.679015
27.582552	1341.617629	15.684032
27.957080	1343.253502	15.689050
28.028096	1333.266463	15.694067
27.920497	1339.180591	15.699085
28.309138	1342.703331	15.704103
27.983365	1326.483045	15.709120
27.772610	1307.444580	15.714138
27.644300	1305.550725	15.719155
27.589306	1334.630760	15.724173
27.736243	1332.076405	15.729191
27.732677	1334.670736	15.734208
27.685584	1338.308587	15.739226
27.796380	1347.649958	15.744243
27.530340	1343.797715	15.749261
27.874446	1347.440812	15.754279
27.967989	1358.430253	15.759296
28.016859	1370.976190	15.764314
28.023437	1375.346353	15.769331
27.855254	1376.305904	15.774349
28.270915	1375.629264	15.779367
28.344624	1372.583234	15.784384
28.152991	1360.086729	15.789402
28.251275	1374.916586	15.794419
28.353093	1370.919153	15.799437
28.535331	1368.764984	15.804455
28.199515	1371.434335	15.809472
28.568297	1364.635357	15.814490
28.461049	1367.567114	15.819507
28.412647	1375.636204	15.824525
28.627091	1372.446611	15.829543
28.317996	1375.044063	15.834560
28.401136	1372.403925	15.839578
28.563395	1372.354414	15.844595
28.400765	1366.124662	15.849613
28.701540	1363.168256	15.854631
28.375531	1374.246645	15.859648
28.608303	1361.657283	15.864666
28.683253	1376.325703	15.869683
28.323745	1384.276110	15.874701
28.537661	1391.683626	15.879719
29.048133	1404.113501	15.884736
29.289747	1396.499548	15.889754
29.179491	1394.190687	15.894771
28.801712	1373.486269	15.899789
28.920534	1368.219893	15.904807
28.668118	1374.338022	15.909824
29.007806	1384.679490	15.914842
29.014821	1381.038506	15.919859
28.824691	1379.734924	15.924877
29.074791	1386.205474	15.929895
29.368426	1396.519691	15.934912
29.140803	1379.766187	15.939930
28.870504	1360.318742	15.944947
29.317257	1379.895264	15.949965
29.445237	1380.348275	15.954983
29.346947	1369.705550	15.960000
28.743974	1369.343950	15.965018
28.886658	1367.111150	15.970035
28.943937	1387.736045	15.975053
29.191768	1396.418543	15.980071
29.462462	1398.629384	15.985088
29.232471	1394.036805	15.990106
29.521470	1391.782239	15.995123
29.109782	1401.634822	16.000141
29.436342	1393.903507	16.005159
29.354167	1404.158122	16.010176
29.301262	1404.353705	16.015194
29.774980	1389.199714	16.020211
29.547595	1392.904085	16.025229
29.838279	1388.097909	16.030247
29.741362	1396.193624	16.035264
29.652012	1395.275071	16.040282
29.764711	1393.163449	16.045299
29.725512	1386.064604	16.050317
29.959194	1370.874987	16.055335
29.804017	1359.473738	16.060352
29.319392	1363.491250	16.065370
29.591324	1372.399542	16.070387
29.705911	1390.696761	16.075405
29.745937	1379.902985	16.080423
29.618146	1379.668509	16.085440
29.551612	1391.941873	16.090458
29.649034	1389.708424	16.095475
29.561467	1397.110546	16.100493
29.495343	1391.617267	16.105511
29.719072	1392.732953	16.110528
29.371224	1386.683737	16.115546
30.190582	1400.160697	16.120563
29.908121	1407.708734	16.125581
30.187625	1408.820245	16.130599
30.334789	1408.376755	16.135616
30.603331	1407.726724	16.140634
30.497457	1386.530627	16.145651
30.275620	1383.051979	16.150669
30.433226	1376.583966	16.155687
30.394118	1384.042844	16.160704
30.415397	1383.284392	16.165722
30.424382	1371.761000	16.170739
30.250105	1385.622928	16.175757
30.319696	1381.470190	16.180775
30.489345	1380.024286	16.185792
30.361883	1381.740227	16.190810
30.635347	1379.757116	16.195827
30.308921	1384.111182	16.200845
30.376574	1376.771940	16.205863
30.592288	1376.561326	16.210880
30.381200	1383.740907	16.215898
30.373263	1378.260373	16.220915
30.301730	1380.963076	16.225933
30.596290	1387.429683	16.230951
30.498669	1378.222956	16.235968
30.385012	1382.289841	16.240986
30.523159	1383.261880	16.246003
30.497410	1407.218989	16.251021
30.700218	1411.867740	16.256039
30.790851	1411.349899	16.261056
30.427822	1416.052718	16.266074
31.203001	1414.422149	16.271091
30.696548	1413.540232	16.276109
30.948657	1410.849544	16.281127
30.839504	1403.192436	16.286144
30.905764	1407.762294	16.291162
31.266393	1405.979200	16.296179
31.010779	1407.138306	16.301197
31.232580	1402.605797	16.306215
31.095155	1405.943479	16.311232
30.980109	1419.462525	16.316250
31.051823	1394.949026	16.321267
30.950974	1415.124146	16.326285
31.030940	1416.072434	16.331303
31.086909	1408.066530	16.336320
31.338591	1408.471500	16.341338
31.654775	1416.471454	16.346355
31.353925	1407.789459	16.351373
31.098083	1412.967519	16.356391
31.200708	1406.527137	16.361408
30.856196	1408.889580	16.366426
31.468936	1409.671102	16.371443
31.099145	1409.920371	16.376461
31.445279	1405.605548	16.381479
31.409137	1408.570015	16.386496
30.946515	1422.105174	16.391514
31.232562	1412.082212	16.396531
31.306019	1420.443339	16.401549
31.632844	1427.014924	16.406567
31.669725	1441.807455	16.411584
31.428358	1440.974490	16.416602
31.769806	1431.513665	16.421619
31.628441	1440.821385	16.426637
31.813542	1440.459929	16.431655
32.136081	1431.483448	16.436672
32.209834	1438.172477	16.441690
32.062171	1404.358406	16.446707
31.884044	1408.130426	16.451725
31.632116	1406.152458	16.456743
31.909162	1398.746776	16.461760
31.616917	1403.968390	16.466778
31.897452	1419.444027	16.471795
31.819960	1436.071566	16.476813
32.075408	1434.448384	16.481831
32.251487	1434.284989	16.486848
32.105187	1437.597353	16.491866
32.284635	1438.452702	16.496883
32.171721	1440.167902	16.501901
32.198227	1422.916083	16.506919
32.317769	1414.115128	16.511936
31.337767	1410.607962	16.516954
32.220182	1422.863706	16.521971
32.140824	1433.747079	16.526989
32.174629	1432.379462	16.532007
32.274835	1429.606037	16.537024
31.976415	1445.406837	16.542042
32.354985	1448.286295	16.547059
32.392715	1454.444695	16.552077
32.232425	1447.111885	16.557095
32.271314	1433.142432	16.562112
32.287695	1434.906221	16.567130
32.099678	1438.966106	16.572147
32.345101	1454.982189	16.577165
32.448136	1461.392862	16.582183
32.750239	1462.563692	16.587200
32.465898	1466.829276	16.592218
32.825185	1465.861187	16.597235
32.718783	1468.729911	16.602253
32.781545	1461.455897	16.607271
33.023435	1462.005570	16.612288
33.052974	1464.652845	16.617306
32.732042	1445.977822	16.622323
32.968973	1446.693447	16.627341
32.613830	1449.236910	16.632359
32.824325	1463.062712	16.637376
32.988735	1452.414206	16.642394
33.119602	1452.173080	16.647411
33.141798	1462.272670	16.652429
32.763555	1463.072253	16.657447
33.115248	1458.915397	16.662464
32.981426	1470.263644	16.667482
33.089910	1462.296524	16.672499
33.211788	1456.079557	16.677517
32.991317	1452.973467	16.682535
33.377331	1450.703419	16.687552
33.062885	1456.490141	16.692570
33.296116	1460.364875	16.697587
33.256566	1453.794570	16.702605
32.893499	1463.442818	16.707623
33.373168	1450.313798	16.712640
33.007061	1452.321056	16.717658
33.050107	1457.772347	16.722675
33.262439	1457.795072	16.727693
33.246178	1456.355217	16.732711
33.416550	1466.066248	16.737728
33.154712	1488.895576	16.742746
33.469602	1482.941960	16.747763
33.751980	1488.282735	16.752781
33.648691	1496.231663	16.757799
34.021277	1477.568682	16.762816
33.938204	1481.830484	16.767834
34.089719	1478.474732	16.772851
33.952046	1463.812990	16.777869
33.653822	1451.143076	16.782887
34.005305	1454.656042	16.787904
33.857029	1447.488050	16.792922
33.873634	1444.013829	16.797939
33.768484	1447.434459	16.802957
33.473228	1447.413874	16.807975
33.898010	1467.237830	16.812992
33.999297	1476.299240	16.818010
33.931444	1481.994735	16.823027
34.221744	1479.008517	16.828045
33.639657	1483.706971	16.833063
34.009242	1476.939274	16.838080
34.093331	1483.889361	16.843098
34.254404	1478.298467	16.848115
34.143624	1479.226846	16.853133
33.904279	1485.121148	16.858151
34.278274	1485.143256	16.863168
34.121668	1480.796912	16.868186
34.014051	1478.157293	16.873203
34.007023	1478.649142	16.878221
33.835047	1486.569695	16.883239
34.291024	1499.544728	16.888256
34.200878	1503.500935	16.893274
34.456035	1502.324517	16.898291
34.696239	1507.884377	16.903309
34.464274	1502.593678	16.908327
34.786080	1498.413265	16.913344
34.809460	1496.921467	16.918362
34.843585	1506.092705	16.923379
34.893499	1504.813745	16.928397
34.858618	1503.416179	16.933415
35.065748	1500.303227	16.938432
34.674641	1486.293768	16.943450
34.611348	1492.428972	16.948467
35.000890	1492.168612	16.953485
34.477416	1512.153303	16.958503
34.997798	1509.605422	16.963520
35.105446	1499.233340	16.968538
35.070522	1501.574735	16.973555
35.389435	1498.105767	16.978573
35.022705	1493.698553	16.983591
35.067942	1475.012281	16.988608
34.767141	1485.838205	16.993626
35.302244	1500.178541	16.998643
35.436055	1493.031602	17.003661
34.988834	1497.906745	17.008679
35.267172	1498.351509	17.013696
35.315910	1500.080259	17.018714
35.046007	1489.809296	17.023731
35.246572	1492.968828	17.028749
35.103812	1505.608364	17.033767
35.389957	1500.348287	17.038784
35.205361	1499.218410	17.043802
35.153402	1495.528603	17.048819
35.353389	1493.439223	17.053837
35.179220	1508.353569	17.058855
35.302250	1502.844236	17.063872
35.300654	1495.105432	17.068890
35.378742	1490.329984	17.073907
35.553716	1513.893473	17.078925
35.495712	1532.833431	17.083943
35.799531	1527.740407	17.088960
35.800230	1534.895722	17.093978
35.562745	1528.168194	17.098995
35.956185	1528.129001	17.104013
35.891879	1527.225321	17.109031
35.894793	1524.899962	17.114048
36.132815	1517.848072	17.119066
36.064434	1525.566513	17.124083
36.054719	1517.882473	17.129101
36.021726	1516.072485	17.134119
36.180306	1510.588939	17.139136
35.993607	1502.845048	17.144154
35.598492	1507.151905	17.149171
36.108654	1516.421827	17.154189
36.014485	1522.796341	17.159207
35.921996	1513.156142	17.164224
36.139820	1517.110424	17.169242
36.065075	1523.450381	17.174259
35.934490	1512.741917	17.179277
36.176833	1526.087662	17.184295
36.369109	1519.763489	17.189312
36.450317	1522.509496	17.194330
36.417163	1530.741403	17.199347
36.353323	1511.984394	17.204365
36.085438	1513.349951	17.209383
36.211630	1518.972042	17.214400
36.166734	1532.748984	17.219418
36.440336	1550.171638	17.224435
36.722984	1546.540134	17.229453
36.427668	1553.948728	17.234471
36.705065	1549.701453	17.239488
36.929602	1545.937649	17.244506
36.836329	1550.954554	17.249523
37.445311	1536.651841	17.254541
36.902608	1546.566313	17.259559
37.129000	1546.116475	17.264576
36.824373	1534.562750	17.269594
36.951973	1538.053243	17.274611
36.930087	1542.685965	17.279629
36.793145	1542.833606	17.284647
37.147017	1543.964727	17.289664
37.368726	1543.260814	17.294682
37.099672	1537.821865	17.299699
37.007588	1541.037520	17.304717
37.224855	1542.165260	17.309735
37.268493	1547.946816	17.314752
37.278662	1546.877105	17.319770
36.938410	1548.884971	17.324787
37.184695	1550.135495	17.329805
37.116182	1549.481014	17.334823
37.263605	1551.105945	17.339840
37.389328	1540.293662	17.344858
37.188233	1559.259622	17.349875
37.312511	1537.164605	17.354893
37.161821	1550.793274	17.359911
36.867327	1543.483392	17.364928
37.320454	1552.219757	17.369946
37.760450	1561.258660	17.374963
37.644018	1571.970302	17.379981
37.407536	1582.089996	17.384999
37.477333	1575.182095	17.390016
37.725481	1579.735582	17.395034
37.641498	1587.822263	17.400051
37.577308	1574.494374	17.405069
37.821540	1578.858155	17.410087
37.668249	1587.854061	17.415104
38.060666	1578.352767	17.420122
37.586160	1581.688409	17.425139
38.000028	1565.405730	17.430157
37.719660	1573.431704	17.435175
37.814198	1574.352511	17.440192
38.156522	1575.839398	17.445210
38.026930	1573.421909	17.450227
38.167662	1561.915106	17.455245
38.137472	1568.106409	17.460263
38.116348	1576.482710	17.465280
38.440254	1567.908610	17.470298
37.952687	1561.637791	17.475315
38.204047	1573.574327	17.480333
38.542841	1588.985014	17.485351
38.517758	1592.336281	17.490368
38.816952	1575.889414	17.495386
38.579349	1573.007820	17.500403
38.938922	1570.406927	17.505421
38.611980	1564.489577	17.510439
38.383922	1563.066187	17.515456
38.673921	1555.653642	17.520474
38.408330	1568.232600	17.525491
38.925316	1559.830626	17.530509
38.861332	1565.785078	17.535527
38.615703	1567.713363	17.540544
38.937057	1564.232979	17.545562
38.527176	1570.077437	17.550579
38.645640	1570.266139	17.555597
38.897979	1573.373389	17.560615
38.638951	1585.805815	17.565632
38.967999	1592.713741	17.570650
38.925580	1586.813923	17.575667
38.957221	1580.154344	17.580685
39.030623	1582.482408	17.585703
39.069800	1581.552782	17.590720
38.882573	1578.276986	17.595738
39.020631	1585.521314	17.600755
38.722404	1588.758845	17.605773
39.069332	1585.722678	17.610791
39.144102	1584.752769	17.615808
39.367805	1574.910308	17.620826
38.848747	1575.932122	17.625843
38.894211	1605.892492	17.630861
39.282221	1607.972975	17.635879
39.340631	1623.218423	17.640896
39.600690	1608.507257	17.645914
39.360200	1613.670356	17.650931
39.613297	1605.832672	17.655949
39.901539	1625.581098	17.660967
39.806609	1614.733167	17.665984
39.780747	1610.691539	17.671002
39.965422	1607.319458	17.676019
40.184869	1611.275081	17.681037
39.894218	1606.706264	17.686055
39.760199	1612.217313	17.691072
40.029791	1611.233635	17.696090
39.934688	1606.772054	17.701107
39.845386	1608.219246	17.706125
40.007832	1600.558040	17.711143
40.063201	1611.838473	17.716160
40.103151	1608.513068	17.721178
40.175625	1607.348475	17.726195
39.937122	1614.398836	17.731213
40.121080	1608.439311	17.736231
40.043797	1618.619367	17.741248
40.176475	1608.296697	17.746266
40.155374	1610.514785	17.751283
39.935812	1609.687769	17.756301
40.262385	1598.303878	17.761319
40.091982	1607.503080	17.766336
40.074691	1597.822517	17.771354
40.123916	1611.063865	17.776371
40.392740	1622.266219	17.781389
40.616823	1630.222782	17.786407
40.268731	1622.049974	17.791424
40.472984	1636.781405	17.796442
40.296686	1641.438784	17.801459
40.518724	1637.794902	17.806477
40.665080	1626.345352	17.811495
40.500669	1631.364192	17.816512
40.678398	1627.493005	17.821530
40.866941	1637.858762	17.826547
40.775302	1634.271200	17.831565
40.916474	1628.227257	17.836583
40.681643	1634.611670	17.841600
40.922968	1632.366245	17.846618
40.714747	1630.275884	17.851635
41.049257	1661.984262	17.856653
41.562350	1666.846299	17.861671
41.422287	1659.467684	17.866688
41.304517	1636.682825	17.871706
41.082428	1626.209087	17.876723
41.296980	1620.438155	17.881741
41.459044	1613.360581	17.886759
41.044199	1626.713707	17.891776
41.239937	1629.852018	17.896794
40.989246	1641.893849	17.901811
41.117504	1649.293138	17.906829
41.658634	1658.216875	17.911847
41.526969	1656.485526	17.916864
41.529275	1652.631299	17.921882
42.006018	1653.782158	17.926899
41.647769	1665.891498	17.931917
42.210393	1648.376160	17.936935
41.643202	1642.696863	17.941952
41.962979	1630.595175	17.946970
41.855461	1620.446080	17.951987
41.658020	1622.841728	17.957005
41.979568	1615.403672	17.962023
41.794243	1623.938319	17.967040
41.845311	1634.387346	17.972058
41.808339	1644.727728	17.977075
41.831259	1656.183253	17.982093
42.115063	1650.819679	17.987111
42.122464	1656.393132	17.992128
41.896126	1646.231509	17.997146
42.428799	1654.500658	18.002163
42.035063	1654.237806	18.007181
42.384354	1645.184570	18.012199
42.199816	1646.401569	18.017216
42.261997	1655.934933	18.022234
42.342017	1645.788944	18.027251
42.225891	1651.131991	18.032269
42.510700	1634.447471	18.037287
42.377649	1645.838202	18.042304
41.906118	1637.294970	18.047322
42.275514	1649.220610	18.052339
42.111113	1656.669723	18.057357
42.471681	1663.599398	18.062375
42.435108	1668.437417	18.067392
42.438593	1668.921304	18.072410
42.767640	1673.395855	18.077427
42.738828	1672.598187	18.082445
43.267912	1671.614017	18.087463
43.141059	1673.611460	18.092480
43.011778	1663.366707	18.097498
43.390144	1660.481237	18.102515
42.977222	1672.136843	18.107533
43.116216	1670.620297	18.112551
43.000138	1659.967609	18.117568
42.984595	1674.584700	18.122586
43.169861	1669.098411	18.127603
43.358199	1668.756884	18.132621
43.448405	1670.123545	18.137639
43.285382	1669.359866	18.142656
43.097859	1664.073029	18.147674
43.120068	1665.582666	18.152691
43.405289	1672.772894	18.157709
43.228827	1669.099753	18.162727
43.362420	1659.844960	18.167744
43.065769	1670.478454	18.172762
43.610983	1653.629688	18.177779
43.417844	1664.201053	18.182797
43.502490	1654.395658	18.187815
43.373164	1666.264000	18.192832
43.453144	1689.249909	18.197850
43.927037	1687.379508	18.202867
43.551747	1702.030405	18.207885
43.658566	1691.699215	18.212903
43.686783	1703.702907	18.217920
43.540112	1701.432837	18.222938
43.811663	1686.469654	18.227955
43.588329	1696.246777	18.232973
43.730247	1693.976299	18.237991
43.769574	1701.394517	18.243008
43.886475	1706.407842	18.248026
44.471817	1705.927495	18.253043
44.376988	1719.418427	18.258061
44.386354	1708.542782	18.263079
44.475004	1687.771386	18.268096
44.312969	1685.508487	18.273114
44.230725	1688.505532	18.278131
44.471551	1687.026225	18.283149
44.386531	1695.453684	18.288167
44.382641	1697.313544	18.293184
44.195484	1720.865914	18.298202
44.795812	1720.952600	18.303219
44.557140	1719.672457	18.308237
44.643785	1721.536757	18.313255
44.828333	1709.793192	18.318272
44.836093	1711.149411	18.323290
45.056604	1703.708548	18.328307
44.970274	1709.219893	18.333325
44.823469	1703.476671	18.338343
45.170672	1701.274124	18.343360
45.004876	1707.156784	18.348378
45.591190	1696.637436	18.353395
44.996626	1696.891094	18.358413
45.102488	1684.337423	18.363431
44.978081	1680.177788	18.368448
44.922408	1687.007121	18.373466
45.290352	1699.920873	18.378483
44.784716	1717.313853	18.383501
45.027962	1698.697958	18.388519
45.198197	1706.191253	18.393536
45.000269	1717.891257	18.398554
45.245386	1711.137011	18.403571
45.237358	1702.118705	18.408589
45.318024	1700.795498	18.413607
45.000719	1704.747090	18.418624
45.213467	1734.790372	18.423642
45.272419	1722.272463	18.428659
45.300977	1734.985548	18.433677
45.641154	1732.405024	18.438695
45.942356	1731.314052	18.443712
45.794066	1746.191481	18.448730
46.074015	1731.981952	18.453747
46.221050	1724.412800	18.458765
46.062538	1740.078351	18.463783
46.206492	1733.502247	18.468800
46.034988	1743.132712	18.473818
45.780612	1735.021969	18.478835
45.658114	1738.992837	18.483853
46.023657	1735.950525	18.488871
45.949122	1730.939794	18.493888
45.753926	1737.273887	18.498906
46.156505	1740.582151	18.503923
46.001585	1743.458666	18.508941
45.975278	1752.337682	18.513959
45.965971	1759.955592	18.518976
46.058705	1767.292969	18.523994
46.747242	1755.001808	18.529011
46.297806	1764.399764	18.534029
46.256938	1758.595582	18.539047
46.880088	1751.065312	18.544064
46.601121	1758.164667	18.549082
46.599571	1747.905776	18.554099
46.580549	1765.343899	18.559117
46.536139	1760.005889	18.564135
46.584477	1768.471896	18.569152
46.666793	1785.470744	18.574170
47.561317	1777.091805	18.579187
47.215937	1777.028874	18.584205
47.222821	1767.463890	18.589223
47.434984	1750.630377	18.594240
47.005971	1760.924830	18.599258
47.170656	1758.460378	18.604275
47.196277	1748.676917	18.609293
46.854588	1755.271903	18.614311
47.176553	1754.570869	18.619328
47.165586	1763.478905	18.624346
47.171204	1766.855203	18.629363
47.308531	1785.020310	18.634381
47.223336	1786.359900	18.639399
47.632833	1774.295694	18.644416
47.429827	1777.760322	18.649434
47.599084	1773.269112	18.654451
47.509181	1779.292279	18.659469
47.696223	1776.025173	18.664487
47.981728	1777.900237	18.669504
47.768477	1774.840115	18.674522
48.097126	1766.464914	18.679539
47.778651	1779.529108	18.684557
47.628950	1779.392499	18.689575
48.004554	1773.364590	18.694592
47.725169	1778.644059	18.699610
47.952521	1776.767350	18.704627
47.971396	1777.206315	18.709645
48.053226	1770.446624	18.714663
48.058759	1784.975522	18.719680
47.947002	1784.916230	18.724698
48.051377	1773.394609	18.729715
47.898837	1787.358844	18.734733
48.092654	1797.097820	18.739751
48.462338	1789.018079	18.744768
48.462100	1804.941599	18.749786
48.300151	1807.440153	18.754803
48.651655	1803.632439	18.759821
48.535322	1806.831571	18.764839
48.882058	1791.876738	18.769856
49.052248	1801.897907	18.774874
48.881464	1787.159321	18.779891
48.950697	1773.765138	18.784909
48.508292	1777.396932	18.789927
48.896894	1770.050349	18.794944
48.756971	1785.719277	18.799962
48.825173	1781.236316	18.804979
48.889942	1795.428593	18.809997
48.942413	1791.508127	18.815015
49.529989	1779.104062	18.820032
49.270562	1784.761016	18.825050
49.418572	1785.517583	18.830067
49.351736	1766.387919	18.835085
49.167400	1763.609474	18.840103
49.274155	1748.482176	18.845120
49.165501	1781.689779	18.850138
49.025631	1786.254879	18.855155
49.181064	1784.337730	18.860173
49.106131	1793.400703	18.865191
49.367799	1783.628336	18.870208
49.427718	1783.121674	18.875226
49.321811	1786.446551	18.880243
49.386164	1789.020694	18.885261
49.074159	1802.074438	18.890279
49.548702	1809.050500	18.895296
49.525263	1825.831885	18.900314
49.634032	1822.352312	18.905331
49.874996	1817.004948	18.910349
49.926923	1820.034103	18.915367
50.146259	1824.184856	18.920384
49.621961	1812.256959	18.925402
49.918697	1816.720978	18.930419
49.937637	1820.735377	18.935437
49.991375	1829.593810	18.940455
50.100518	1836.573105	18.945472
50.084510	1848.219032	18.950490
50.274863	1848.514249	18.955507
50.318252	1833.857861	18.960525
50.345523	1839.948881	18.965543
50.357426	1830.128228	18.970560
50.426467	1834.173967	18.975578
50.461323	1825.098408	18.980595
50.871668	1824.012046	18.985613
50.799618	1837.279235	18.990631
51.137447	1835.830061	18.995648
51.167486	1837.727000	19.000666
51.179043	1830.880961	19.005683
50.938765	1820.991994	19.010701
50.617568	1812.446703	19.015719
51.144173	1817.717194	19.020736
50.834620	1822.150493	19.025754
51.163169	1829.862421	19.030771
51.227964	1831.767973	19.035789
50.960940	1824.433116	19.040807
51.512006	1817.139250	19.045824
51.138036	1813.834193	19.050842
51.286233	1819.210651	19.055859
51.393128	1819.797600	19.060877
51.166345	1826.207553	19.065895
51.637601	1832.051586	19.070912
51.258696	1827.647781	19.075930
51.672413	1820.232675	19.080947
51.734591	1824.878821	19.085965
51.500935	1836.803266	19.090983
51.924801	1834.833862	19.096000
51.932785	1832.177314	19.101018
51.687100	1814.554736	19.106035
51.757629	1807.773235	19.111053
51.543150	1817.588352	19.116071
51.599874	1810.900284	19.121088
51.532623	1831.594437	19.126106
51.423208	1826.757547	19.131123
51.507469	1823.667269	19.136141
51.690039	1833.307392	19.141159
52.024945	1844.864319	19.146176
52.188431	1845.450109	19.151194
52.544472	1860.508343	19.156211
52.711500	1842.253628	19.161229
52.417384	1860.039329	19.166247
52.507880	1846.278324	19.171264
52.410422	1838.021374	19.176282
52.128897	1833.056203	19.181299
52.638230	1836.331736	19.186317
52.497545	1847.025427	19.191335
52.704736	1851.211158	19.196352
52.866612	1844.438666	19.201370
52.217247	1850.505469	19.206387
52.552527	1851.697784	19.211405
52.617740	1856.645474	19.216423
52.767653	1845.951802	19.221440
52.723170	1850.520586	19.226458
52.698167	1843.947783	19.231475
52.916952	1839.141917	19.236493
52.576896	1862.838450	19.241511
52.564463	1875.191684	19.246528
53.005848	1876.082364	19.251546
52.882385	1887.629057	19.256563
53.015912	1882.163525	19.261581
53.224151	1884.761928	19.266599
53.218140	1889.835818	19.271616
53.320867	1879.591664	19.276634
53.277454	1891.113009	19.281651
53.796264	1903.310758	19.286669
53.476467	1904.882828	19.291687
53.314909	1911.678816	19.296704
53.372575	1910.912961	19.301722
53.466875	1913.438306	19.306739
53.587727	1913.703710	19.311757
53.636026	1921.007353	19.316775
53.786024	1910.184633	19.321792
53.901590	1909.886167	19.326810
53.901012	1917.751305	19.331827
54.005420	1903.736344	19.336845
54.271638	1911.584098	19.341863
54.217671	1904.800383	19.346880
54.467222	1897.479059	19.351898
54.095885	1907.319252	19.356915
54.169069	1901.416599	19.361933
54.343899	1900.742170	19.366951
54.594381	1903.034967	19.371968
54.670365	1897.789389	19.376986
54.293207	1906.650522	19.382003
54.270005	1901.022789	19.387021
54.534422	1901.801696	19.392039
54.447811	1899.155502	19.397056
54.961923	1908.679880	19.402074
54.513192	1913.291131	19.407091
54.934583	1911.411774	19.412109
54.962939	1921.985754	19.417127
54.962411	1911.400969	19.422144
54.981849	1906.088901	19.427162
55.283661	1913.904239	19.432179
55.303461	1910.493890	19.437197
55.090659	1894.484604	19.442215
55.031409	1898.154421	19.447232
55.335576	1902.403353	19.452250
55.377680	1914.194221	19.457267
55.563028	1908.610303	19.462285
55.331982	1893.296056	19.467303
55.263280	1910.061161	19.472320
55.467897	1910.803988	19.477338
55.189096	1915.174209	19.482355
55.505876	1902.762890	19.487373
55.661997	1907.164420	19.492391
55.631561	1918.622370	19.497408
55.729569	1906.956941	19.502426
55.524750	1907.025747	19.507443
55.690667	1916.184092	19.512461
55.504945	1914.264705	19.517479
55.643894	1916.512371	19.522496
55.828773	1912.864910	19.527514
55.839667	1933.971460	19.532531
56.117776	1939.731511	19.537549
55.917560	1929.150244	19.542567
55.832171	1946.699844	19.547584
55.998336	1937.109346	19.552602
55.671821	1950.075874	19.557619
55.923308	1932.477684	19.562637
55.862006	1955.178235	19.567655
55.912680	1963.785555	19.572672
56.348017	1961.606667	19.577690
56.178731	1972.756469	19.582707
56.501910	1973.927130	19.587725
56.412281	1977.076422	19.592743
56.324811	1968.380505	19.597760
56.724592	1974.755093	19.602778
56.656417	1990.721112	19.607795
57.057736	1993.542000	19.612813
57.193020	1996.446214	19.617831
57.389679	1995.776165	19.622848
57.762089	1975.031464	19.627866
57.383217	1972.999727	19.632883
57.417084	1970.324869	19.637901
57.487535	1962.440618	19.642919
57.013895	1955.782010	19.647936
57.249408	1951.365123	19.652954
57.085220	1958.463572	19.657971
57.459908	1945.289505	19.662989
57.468665	1954.935406	19.668007
57.385175	1956.133168	19.673024
57.680703	1968.578940	19.678042
57.907731	1984.370459	19.683059
57.728949	1971.931147	19.688077
58.037116	1959.104303	19.693095
57.839392	1958.217153	19.698112
57.848206	1956.751227	19.703130
57.611292	1976.045912	19.708147
57.487826	1974.115016	19.713165
57.628275	1987.567102	19.718183
57.919253	1976.284549	19.723200
58.041926	1975.023832	19.728218
57.915430	1982.583470	19.733235
57.773581	1975.433066	19.738253
58.224106	1988.225370	19.743271
58.206752	2005.584865	19.748288
58.555838	2009.158128	19.753306
58.513846	2006.275137	19.758323
58.468824	2011.658886	19.763341
58.762985	1998.006828	19.768359
58.308669	1996.361500	19.773376
58.872829	1999.900462	19.778394
58.563155	2002.038789	19.783411
58.804063	2005.376046	19.788429
58.834660	2003.980573	19.793447
58.971989	2014.812521	19.798464
59.008410	2002.143808	19.803482
58.663121	1994.546065	19.808499
59.094961	1996.456024	19.813517
58.984061	1997.533892	19.818535
58.989388	2003.801514	19.823552
59.357649	2016.298649	19.828570
59.321922	2023.522935	19.833587
59.072785	2040.507303	19.838605
59.401795	2020.604738	19.843623
59.424906	2025.652009	19.848640
59.535024	2025.039805	19.853658
59.717371	2025.237203	19.858675
60.174033	2018.943010	19.863693
60.025637	2014.357666	19.868711
59.613182	2016.652386	19.873728
59.677328	2010.972927	19.878746
59.694809	2006.177088	19.883763
59.807628	2014.947561	19.888781
60.424349	2008.681330	19.893799
59.867599	2020.135206	19.898816
60.088937	2012.703493	19.903834
60.221651	2012.155326	19.908851
60.164932	2009.537378	19.913869
60.083516	2014.939516	19.918887
59.858343	2026.236698	19.923904
60.135534	2016.252488	19.928922
60.223753	2013.298392	19.933939
60.051710	2009.018843	19.938957
60.369030	2021.530399	19.943975
60.381043	2042.168165	19.948992
60.630197	2039.141208	19.954010
60.908091	2042.793474	19.959027
60.540907	2049.988836	19.964045
60.754563	2040.724179	19.969063
60.598184	2049.458952	19.974080
60.762495	2040.236772	19.979098
60.871980	2046.711172	19.984115
60.676157	2041.710237	19.989133
61.406800	2036.788071	19.994151
61.164218	2059.759943	19.999168
61.565950	2070.551339	20.004186
61.338051	2060.251245	20.009203
61.425933	2063.933819	20.014221
61.638352	2051.645984	20.019239
61.150713	2052.700566	20.024256
61.486581	2065.287853	20.029274
61.753680	2066.923646	20.034291
61.458961	2069.668361	20.039309
61.901841	2072.013874	20.044327
61.915826	2067.614977	20.049344
61.977234	2062.410990	20.054362
61.941696	2054.648986	20.059379
61.579340	2061.873471	20.064397
61.951063	2064.236623	20.069415
62.003104	2068.326037	20.074432
62.200781	2066.125261	20.079450
61.867006	2064.344296	20.084467
62.101717	2059.930650	20.089485
62.234351	2053.382950	20.094503
61.876530	2063.535698	20.099520
62.009446	2076.158507	20.104538
62.314458	2087.726690	20.109555
62.152696	2087.464584	20.114573
62.656675	2090.339907	20.119591
62.251382	2090.344729	20.124608
62.195945	2074.756890	20.129626
62.520233	2076.720193	20.134643
62.462331	2090.590974	20.139661
62.949686	2097.830980	20.144679
62.809340	2104.318506	20.149696
63.282006	2111.766928	20.154714
63.404116	2099.115926	20.159731
63.327089	2108.888868	20.164749
63.475553	2094.283100	20.169767
63.400226	2086.780683	20.174784
63.326862	2081.204924	20.179802
63.669810	2074.499404	20.184819
63.235170	2069.964411	20.189837
63.585733	2081.119482	20.194855
63.649224	2097.261250	20.199872
63.619215	2099.494990	20.204890
64.008852	2094.323592	20.209907
63.970358	2078.789676	20.214925
63.961190	2060.469977	20.219943
63.769677	2058.733965	20.224960
63.892501	2056.026028	20.229978
64.247673	2054.075418	20.234995
63.998939	2061.862232	20.240013
64.047113	2070.586419	20.245031
63.982098	2075.633604	20.250048
64.088021	2086.284997	20.255066
64.234048	2102.322372	20.260083
64.180726	2090.879131	20.265101
64.361232	2092.649860	20.270119
64.020727	2101.056949	20.275136
64.093474	2099.500588	20.280154
64.408959	2087.856960	20.285171
63.926848	2116.045554	20.290189
64.502389	2120.753073	20.295207
64.671624	2123.677068	20.300224
64.758273	2126.782549	20.305242
64.953171	2118.997919	20.310259
64.792749	2117.927056	20.315277
64.866902	2117.915193	20.320295
64.782284	2112.238969	20.325312
65.066964	2127.672236	20.330330
65.463104	2137.155806	20.335347
64.994650	2145.869619	20.340365
65.263590	2138.603285	20.345383
65.565779	2139.760005	20.350400
65.507721	2140.392150	20.355418
65.825709	2144.561871	20.360435
65.245136	2139.400462	20.365453
65.460252	2140.185673	20.370471
65.587533	2139.301737	20.375488
65.475041	2147.683502	20.380506
65.640016	2135.014621	20.385523
65.412436	2145.044407	20.390541
65.641966	2143.590454	20.395559
65.633741	2150.793115	20.400576
65.920843	2161.335443	20.405594
66.327489	2163.479109	20.410611
66.194740	2173.152441	20.415629
66.481038	2160.413852	20.420647
66.451805	2166.370874	20.425664
66.417512	2166.519452	20.430682
66.610284	2160.736051	20.435699
66.425334	2162.524171	20.440717
66.402592	2169.672526	20.445735
66.490691	2164.456381	20.450752
66.613991	2161.032614	20.455770
66.547441	2151.254142	20.460787
66.454316	2162.140256	20.465805
66.755935	2158.039957	20.470823
67.117582	2160.991478	20.475840
66.650777	2158.624521	20.480858
67.173712	2165.879336	20.485875
66.937356	2179.402704	20.490893
67.220967	2186.664236	20.495911
67.525455	2183.120331	20.500928
67.375798	2191.457710	20.505946
67.364763	2193.117424	20.510963
67.350165	2189.150917	20.515981
67.781258	2181.212180	20.520999
67.501984	2178.908123	20.526016
67.499686	2197.956471	20.531034
67.771582	2181.317431	20.536051
67.443014	2191.226499	20.541069
67.562421	2192.476868	20.546087
67.795573	2187.991072	20.551104
67.976350	2194.259111	20.556122
68.136809	2199.462294	20.561139
68.187665	2217.600835	20.566157
68.292864	2208.527977	20.571175
68.433012	2210.206055	20.576192
68.151755	2219.479951	20.581210
68.740931	2198.657891	20.586227
68.358343	2204.658696	20.591245
68.516546	2208.380430	20.596263
68.933967	2207.686178	20.601280
68.974007	2200.561711	20.606298
68.776876	2201.200307	20.611315
69.020980	2203.398215	20.616333
69.027613	2194.213667	20.621351
68.973427	2198.776243	20.626368
68.651053	2201.745619	20.631386
69.059695	2202.103563	20.636403
69.023721	2196.222918	20.641421
69.010220	2193.044332	20.646439
69.185617	2201.340890	20.651456
69.058793	2198.356556	20.656474
69.510556	2198.309642	20.661491
68.756574	2198.604454	20.666509
68.719514	2201.720241	20.671527
68.970342	2212.106368	20.676544
68.700703	2223.376187	20.681562
69.141650	2223.790329	20.686579
69.556871	2237.456810	20.691597
69.486452	2235.989333	20.696615
69.519359	2248.247563	20.701632
69.379372	2261.532266	20.706650
69.988820	2250.429952	20.711667
70.239426	2251.355804	20.716685
70.389792	2244.904292	20.721703
70.411341	2241.296955	20.726720
70.508527	2240.691524	20.731738
70.687170	2234.274833	20.736755
70.778888	2235.830074	20.741773
70.731668	2240.863468	20.746791
70.525067	2237.470270	20.751808
70.471500	2241.093648	20.756826
70.600692	2227.522742	20.761843
70.365344	2233.383671	20.766861
70.321148	2258.336152	20.771879
70.863733	2255.443258	20.776896
71.000353	2267.370354	20.781914
70.822792	2270.203390	20.786931
71.146047	2270.088879	20.791949
71.155129	2274.344081	20.796967
71.511956	2257.666241	20.801984
71.225146	2266.769590	20.807002
71.624622	2254.075793	20.812019
71.493762	2251.077934	20.817037
71.326536	2267.653095	20.822055
71.693524	2264.981688	20.827072
71.309059	2254.212483	20.832090
71.636825	2258.291015	20.837107
71.805307	2264.820600	20.842125
71.410646	2262.147958	20.847143
71.504616	2272.543413	20.852160
71.305966	2285.277484	20.857178
72.067225	2284.286145	20.862195
72.217214	2284.534327	20.867213
72.131394	2285.572035	20.872231
72.274966	2275.942445	20.877248
71.976269	2284.676459	20.882266
72.325486	2315.059414	20.887283
72.414608	2318.100047	20.892301
72.545181	2320.816312	20.897319
72.315659	2311.719688	20.902336
72.514112	2316.943597	20.907354
72.882254	2313.752887	20.912371
73.001346	2308.138484	20.917389
72.819153	2313.086459	20.922407
72.784240	2311.721853	20.927424
72.364323	2313.009475	20.932442
72.696987	2309.670265	20.937459
72.966830	2323.109895	20.942477
73.188374	2335.001481	20.947495
73.762341	2332.356831	20.952512
73.249015	2335.509272	20.957530
73.589095	2330.737387	20.962547
73.911397	2330.852696	20.967565
73.866766	2336.861008	20.972583
74.244083	2316.100882	20.977600
73.636484	2307.726812	20.982618
73.747247	2309.831168	20.987635
73.797436	2320.409822	20.992653
73.391463	2320.166206	20.997671
73.695253	2321.377743	21.002688
73.930090	2332.730794	21.007706
74.072860	2324.318850	21.012723
74.079277	2328.937871	21.017741
74.004936	2328.507658	21.022759
74.215681	2333.487361	21.027776
74.208748	2348.533203	21.032794
74.176189	2348.500604	21.037811
74.383046	2371.623097	21.042829
74.727748	2354.953371	21.047847
74.766655	2366.699499	21.052864
74.639499	2360.534445	21.057882
74.863119	2355.807867	21.062899
75.030480	2354.242683	21.067917
74.404603	2357.630160	21.072935
74.978290	2362.769076	21.077952
75.238975	2385.190858	21.082970
75.242535	2380.662964	21.087987
75.492950	2383.119450	21.093005
75.098777	2389.491847	21.098023
75.392791	2393.269052	21.103040
75.075054	2397.763604	21.108058
75.393859	2382.356432	21.113075
75.329506	2382.719024	21.118093
75.481107	2402.581544	21.123111
75.954469	2406.596000	21.128128
75.924750	2405.936866	21.133146
75.943387	2416.542644	21.138163
76.449773	2403.600428	21.143181
76.494028	2408.469850	21.148199
76.546703	2409.158282	21.153216
76.851581	2405.055823	21.158234
76.524286	2381.148570	21.163251
76.571073	2368.704405	21.168269
76.151705	2367.917070	21.173287
76.254634	2375.769096	21.178304
76.638366	2391.853831	21.183322
76.593924	2401.250529	21.188339
76.704323	2399.010139	21.193357
76.654419	2397.080038	21.198375
76.554666	2404.523942	21.203392
76.589189	2395.960901	21.208410
76.289078	2404.372732	21.213427
76.864932	2412.366444	21.218445
77.023338	2419.471877	21.223463
77.227515	2418.482851	21.228480
77.494865	2428.364689	21.233498
76.907444	2433.499240	21.238515
77.170469	2435.230897	21.243533
77.174424	2430.105157	21.248551
77.446730	2437.378057	21.253568
77.435090	2448.529038	21.258586
77.474751	2449.333595	21.263603
77.948294	2456.759250	21.268621
77.622856	2455.761082	21.273639
77.877858	2448.824805	21.278656
78.144851	2445.773684	21.283674
77.973360	2449.196476	21.288691
78.172183	2448.972030	21.293709
78.166544	2454.706750	21.298727
78.414662	2468.002110	21.303744
78.383288	2473.524643	21.308762
78.693865	2463.245359	21.313779
78.806741	2467.056189	21.318797
78.651560	2480.069011	21.323815
79.006430	2477.413657	21.328832
79.153401	2472.445999	21.333850
79.009473	2468.408015	21.338867
78.947459	2475.024005	21.343885
78.957282	2462.231712	21.348903
79.448186	2466.639017	21.353920
79.155886	2474.233216	21.358938
79.056339	2469.109810	21.363955
79.572861	2467.781526	21.368973
79.475135	2468.474282	21.373991
79.418432	2460.918362	21.379008
79.537020	2457.301002	21.384026
79.697374	2468.809974	21.389043
79.725433	2459.016207	21.394061
79.429968	2473.854927	21.399079
79.729917	2485.808069	21.404096
79.936724	2488.192874	21.409114
79.929359	2491.641413	21.414131
80.042784	2494.621577	21.419149
79.835881	2499.013538	21.424167
80.093461	2493.078881	21.429184
80.347411	2486.517933	21.434202
80.143618	2497.223737	21.439219
80.207794	2517.241933	21.444237
79.992961	2528.748647	21.449255
80.782875	2524.849602	21.454272
80.715219	2519.184671	21.459290
80.879817	2519.366031	21.464307
81.288247	2502.951826	21.469325
81.091984	2504.696957	21.474343
80.987451	2507.125909	21.479360
80.972656	2504.679730	21.484378
80.970474	2502.726274	21.489395
81.192596	2521.113959	21.494413
81.269682	2530.148429	21.499431
81.259115	2534.774156	21.504448
81.832957	2543.399856	21.509466
81.953274	2542.065532	21.514483
82.001782	2528.242148	21.519501
81.562508	2547.787732	21.524519
81.994820	2542.971969	21.529536
81.998067	2524.217107	21.534554
82.089392	2525.155007	21.539571
82.108064	2525.909431	21.544589
81.612483	2526.627095	21.549607
82.083008	2536.198959	21.554624
82.246521	2535.576647	21.559642
82.037778	2541.527841	21.564659
82.489685	2526.628635	21.569677
82.733646	2552.361537	21.574695
82.242859	2565.416942	21.579712
82.336293	2563.160355	21.584730
82.218931	2571.547859	21.589747
82.471368	2563.609879	21.594765
82.646497	2576.017959	21.599783
82.746149	2585.169206	21.604800
83.219369	2578.412795	21.609818
83.164453	2585.298274	21.614835
83.652922	2581.167276	21.619853
83.271563	2587.690304	21.624871
83.116102	2585.192608	21.629888
83.927417	2589.327051	21.634906
83.840851	2573.105752	21.639923
83.965116	2573.144889	21.644941
83.892201	2575.446108	21.649959
83.906071	2566.323882	21.654976
84.271537	2572.138687	21.659994
84.025477	2585.615999	21.665011
83.979974	2562.312409	21.670029
84.285832	2560.427017	21.675047
84.157070	2578.733872	21.680064
84.321172	2562.522164	21.685082
84.410899	2572.010052	21.690099
84.179697	2565.425758	21.695117
84.034102	2577.382383	21.700135
84.151841	2583.634689	21.705152
84.268044	2587.312881	21.710170
84.507127	2591.038335	21.715187
84.867811	2602.876492	21.720205
84.552691	2614.396906	21.725223
84.941525	2625.240330	21.730240
84.983148	2620.626064	21.735258
85.206454	2616.402055	21.740275
85.063991	2621.162106	21.745293
85.277724	2616.740627	21.750311
85.183749	2622.770298	21.755328
85.782156	2624.833904	21.760346
85.585857	2645.000784	21.765363
86.294203	2638.543493	21.770381
86.182640	2617.311891	21.775399
86.053401	2616.736260	21.780416
86.326198	2604.916552	21.785434
86.378210	2602.938709	21.790451
86.177171	2595.980700	21.795469
86.051694	2604.407271	21.800487
86.060020	2606.134733	21.805504
86.481396	2594.633486	21.810522
86.513414	2604.571851	21.815539
86.849481	2618.186035	21.820557
86.767310	2619.806802	21.825575
86.239200	2615.874874	21.830592
86.627053	2618.410949	21.835610
86.723320	2630.245675	21.840627
86.566522	2630.992691	21.845645
86.920743	2630.577501	21.850663
86.761361	2627.887719	21.855680
86.944917	2631.213034	21.860698
87.012147	2661.312907	21.865715
87.052370	2662.494931	21.870733
87.312129	2653.279953	21.875751
87.184944	2660.617459	21.880768
87.828335	2658.248774	21.885786
87.265213	2663.251320	21.890803
87.873801	2669.505617	21.895821
87.855772	2678.084990	21.900839
87.911851	2674.846436	21.905856
88.165283	2665.419305	21.910874
87.851123	2680.374478	21.915891
88.185025	2680.121410	21.920909
88.562466	2672.711663	21.925927
88.634271	2682.403839	21.930944
88.703271	2668.166475	21.935962
88.859008	2653.608539	21.940979
88.740420	2660.169924	21.945997
88.690620	2665.426468	21.951015
88.702944	2654.971231	21.956032
88.861349	2657.199395	21.961050
88.883340	2672.529624	21.966067
88.963792	2680.147862	21.971085
89.151156	2688.735389	21.976103
89.426847	2683.567800	21.981120
89.315859	2696.990640	21.986138
89.207226	2692.144683	21.991155
89.335646	2694.472020	21.996173
89.604431	2682.614347	22.001191
89.596248	2695.880000	22.006208
89.511588	2687.790419	22.011226
89.871176	2693.960159	22.016243
90.100229	2711.672121	22.021261
90.427158	2719.542886	22.026279
90.135120	2716.900984	22.031296
90.216352	2712.311047	22.036314
90.634336	2710.871037	22.041331
90.783848	2695.945945	22.046349
90.977129	2690.671153	22.051367
90.321431	2683.989320	22.056384
90.799484	2668.725561	22.061402
90.873251	2672.996522	22.066419
90.701431	2670.766486	22.071437
91.101387	2673.364353	22.076455
90.886161	2696.467366	22.081472
90.948575	2699.561105	22.086490
90.917719	2692.042629	22.091507
90.953061	2710.424159	22.096525
91.070523	2693.825680	22.101543
90.795229	2702.568008	22.106560
91.258691	2708.191055	22.111578
91.506825	2715.375925	22.116595
91.503607	2722.342891	22.121613
91.657276	2732.978494	22.126631
91.407993	2728.039330	22.131648
91.568956	2738.650177	22.136666
91.795048	2740.025162	22.141683
91.920163	2758.391650	22.146701
92.514103	2752.567641	22.151719
92.305139	2746.573565	22.156736
92.799796	2739.247345	22.161754
92.888069	2758.299290	22.166771
92.650773	2753.574508	22.171789
92.857867	2738.401078	22.176807
92.960744	2750.029558	22.181824
92.797751	2746.674904	22.186842
92.684989	2745.628641	22.191859
92.847322	2739.462096	22.196877
93.095534	2739.183365	22.201895
92.600636	2757.182296	22.206912
93.347520	2757.332158	22.211930
93.275862	2777.325967	22.216947
93.483185	2781.411272	22.221965
93.574174	2774.294918	22.226983
93.331389	2771.757628	22.232000
93.626540	2777.552268	22.237018
93.667909	2780.676910	22.242035
93.749200	2784.579382	22.247053
93.892782	2799.473481	22.252071
94.035297	2797.607030	22.257088
94.266794	2798.151341	22.262106
94.305157	2785.001050	22.267123
94.276366	2798.857640	22.272141
94.473524	2788.940726	22.277159
94.382727	2785.245771	22.282176
94.723870	2809.579296	22.287194
95.096081	2818.700599	22.292211
94.879541	2819.278602	22.297229
95.066352	2811.562538	22.302247
95.101025	2833.411473	22.307264
95.093987	2817.984227	22.312282
94.978210	2811.700756	22.317299
94.783132	2817.745842	22.322317
94.842891	2805.259907	22.327335
95.166970	2819.917594	22.332352
95.639888	2841.869701	22.337370
95.517965	2837.545730	22.342387
95.559989	2836.003629	22.347405
95.632675	2837.015312	22.352423
95.591498	2845.132833	22.357440
95.752425	2841.101976	22.362458
96.015035	2853.324875	22.367475
95.873292	2855.750379	22.372493
96.086396	2873.140232	22.377511
96.577157	2869.287234	22.382528
96.636645	2864.565429	22.387546
96.925725	2863.640706	22.392563
96.853818	2876.657907	22.397581
97.213942	2858.765194	22.402599
96.769588	2855.297283	22.407616
96.642230	2856.756958	22.412634
97.298648	2858.001982	22.417651
97.419922	2862.591845	22.422669
97.321436	2854.613708	22.427687
97.264327	2851.334959	22.432704
97.425825	2853.794695	22.437722
97.329458	2870.787916	22.442739
97.323410	2875.915643	22.447757
97.826611	2875.276906	22.452775
97.908540	2888.018673	22.457792
97.886199	2883.523855	22.462810
98.061356	2884.894392	22.467827
98.079023	2876.146555	22.472845
98.137942	2885.766985	22.477863
97.883406	2889.994401	22.482880
98.325055	2894.396324	22.487898
98.613522	2915.236655	22.492915
98.322763	2917.980893	22.497933
98.552950	2907.041606	22.502951
98.531293	2914.990089	22.507968
98.437982	2915.097745	22.512986
98.943584	2921.856246	22.518003
98.895808	2924.041033	22.523021
99.350217	2925.044553	22.528039
99.590684	2923.039762	22.533056
99.415124	2919.105802	22.538074
99.658990	2915.628024	22.543091
99.989825	2917.617148	22.548109
100.014375	2911.919269	22.553127
100.008905	2916.172260	22.558144
99.853351	2924.813037	22.563162
100.022609	2911.844692	22.568179
99.787460	2924.675595	22.573197
99.961653	2905.454866	22.578215
99.870155	2906.491162	22.583232
99.993215	2907.154237	22.588250
100.483906	2930.386528	22.593267
100.013784	2940.213273	22.598285
100.553072	2946.180637	22.603303
100.473350	2945.302135	22.608320
100.065824	2949.734873	22.613338
100.424895	2955.506808	22.618355
100.252932	2963.277137	22.623373
100.842062	2969.699850	22.628391
100.908247	2978.114951	22.633408
101.049485	2978.195431	22.638426
101.353892	2987.147530	22.643443
101.409347	2999.567978	22.648461
101.647291	2992.814289	22.653479
101.605810	3007.516300	22.658496
101.711700	3009.689968	22.663514
101.971766	2997.602967	22.668531
101.748082	3002.861404	22.673549
102.211057	2994.577353	22.678567
102.411841	2995.113985	22.683584
102.008913	2992.571516	22.688602
102.576552	3003.385142	22.693619
102.509568	3023.642043	22.698637
103.003719	3013.464459	22.703655
102.737453	3017.067673	22.708672
102.777455	3019.818965	22.713690
103.122560	3021.030271	22.718707
103.119625	3023.893024	22.723725
103.078904	3016.610351	22.728743
102.907309	3020.141050	22.733760
102.978400	3017.450625	22.738778
103.302466	3022.355865	22.743795
103.224288	3020.361758	22.748813
103.378846	3043.151505	22.753831
103.706213	3047.958692	22.758848
103.467607	3042.736125	22.763866
103.963365	3042.384094	22.768883
104.001507	3040.600327	22.773901
104.007687	3034.553733	22.778919
104.042626	3042.525509	22.783936
103.998103	3049.580235	22.788954
104.477565	3062.892740	22.793971
104.549289	3065.369975	22.798989
104.305336	3073.149482	22.804007
105.044956	3059.900492	22.809024
105.029576	3064.462656	22.814042
105.182611	3068.732106	22.819059
104.774475	3059.363021	22.824077
104.876657	3067.158122	22.829095
105.200806	3078.071983	22.834112
105.251383	3088.083230	22.839130
105.767656	3079.940867	22.844147
105.651836	3098.215634	22.849165
105.812791	3085.583539	22.854183
106.072397	3069.303338	22.859200
105.693980	3084.748191	22.864218
106.059916	3082.594375	22.869235
105.714864	3074.443845	22.874253
105.868071	3091.933182	22.879271
106.204797	3083.795064	22.884288
105.994897	3080.411630	22.889306
106.039343	3076.431532	22.894323
106.119866	3099.888388	22.899341
106.022574	3115.823315	22.904359
106.347612	3118.043071	22.909376
106.164024	3125.035059	22.914394
106.559543	3134.428147	22.919411
106.611870	3135.661766	22.924429
106.761071	3138.390161	22.929447
107.031914	3143.074250	22.934464
107.321228	3172.466460	22.939482
107.680757	3157.969129	22.944499
107.893035	3164.386737	22.949517
107.769225	3160.453110	22.954535
108.197927	3144.085297	22.959552
107.956277	3156.942610	22.964570
108.296451	3158.293940	22.969587
108.037069	3157.577790	22.974605
108.172691	3156.375476	22.979623
108.332159	3148.452793	22.984640
108.274853	3163.845738	22.989658
108.308811	3148.797027	22.994675
108.221035	3157.665466	22.999693
108.515095	3181.094694	23.004711
108.512763	3178.142219	23.009728
108.821767	3185.058047	23.014746
108.640906	3184.236559	23.019763
108.928062	3187.493570	23.024781
109.110837	3200.626977	23.029799
109.316869	3210.385412	23.034816
109.078074	3210.336142	23.039834
109.672834	3207.064275	23.044851
109.586467	3210.118135	23.049869
109.413018	3221.348210	23.054887
109.660405	3239.522762	23.059904
109.818038	3258.891520	23.064922
110.061439	3240.216215	23.069939
110.044232	3231.616097	23.074957
110.138555	3240.296659	23.079975
110.371232	3256.253062	23.084992
110.523141	3262.238281	23.090010
110.528221	3260.309523	23.095027
110.758446	3257.924043	23.100045
110.256678	3270.300643	23.105063
111.107114	3261.987695	23.110080
111.008096	3296.463614	23.115098
111.183051	3290.814756	23.120115
111.421201	3302.158602	23.125133
111.491236	3303.523918	23.130151
111.640002	3292.215835	23.135168
111.632742	3305.307274	23.140186
111.508769	3286.909160	23.145203
111.686197	3299.573134	23.150221
111.634378	3299.298975	23.155239
111.914629	3304.449633	23.160256
111.997553	3315.698681	23.165274
112.180721	3324.568065	23.170291
112.096303	3318.539733	23.175309
112.450057	3310.361806	23.180327
112.661855	3318.744446	23.185344
112.428694	3315.050031	23.190362
112.808859	3323.227272	23.195379
112.850940	3327.735520	23.200397
112.851399	3346.287811	23.205415
113.158525	3349.938901	23.210432
113.187756	3350.631117	23.215450
113.042821	3346.836102	23.220467
113.115672	3347.613393	23.225485
113.059340	3365.204116	23.230503
113.226284	3360.669530	23.235520
113.222646	3392.781719	23.240538
113.446514	3381.654307	23.245555
113.852826	3396.787150	23.250573
113.719311	3411.225004	23.255591
114.115872	3403.144816	23.260608
114.355019	3401.957438	23.265626
114.408172	3404.394430	23.270643
114.762985	3410.551869	23.275661
114.934193	3411.813751	23.280679
115.177663	3410.205645	23.285696
115.046111	3425.344838	23.290714
115.212739	3413.939423	23.295731
115.204007	3408.427572	23.300749
115.087878	3424.708006	23.305767
115.536728	3418.290189	23.310784
115.589949	3419.400196	23.315802
115.724240	3411.648142	23.320819
115.930643	3411.056714	23.325837
115.558621	3416.769216	23.330855
115.834840	3423.139773	23.335872
115.928840	3439.669890	23.340890
116.102555	3443.264404	23.345907
116.316334	3444.977297	23.350925
115.961139	3438.673522	23.355943
116.459316	3442.081791	23.360960
116.436860	3446.334499	23.365978
116.563283	3462.758788	23.370995
116.792647	3465.370633	23.376013
116.685689	3481.234347	23.381031
116.487648	3473.337818	23.386048
116.707585	3482.879479	23.391066
116.829385	3497.730571	23.396083
117.275249	3506.875963	23.401101
117.161352	3516.094886	23.406119
117.497661	3506.182044	23.411136
117.830384	3517.636047	23.416154
117.842421	3537.029177	23.421171
117.754035	3530.880253	23.426189
117.781632	3536.502336	23.431207
117.911015	3512.904255	23.436224
118.065788	3526.818792	23.441242
118.445521	3547.931799	23.446259
118.694788	3551.031322	23.451277
118.600086	3558.127331	23.456295
118.677111	3552.584447	23.461312
118.660517	3557.758931	23.466330
118.818458	3558.297700	23.471347
119.105757	3552.793654	23.476365
118.934046	3560.145002	23.481383
119.561887	3566.870946	23.486400
119.496850	3578.039171	23.491418
119.237322	3582.412314	23.496435
119.850189	3572.611862	23.501453
119.679161	3582.602936	23.506471
119.709188	3579.641287	23.511488
119.883173	3579.156493	23.516506
120.104412	3602.667233	23.521523
120.399159	3600.589983	23.526541
120.348975	3608.861964	23.531559
120.754634	3601.733577	23.536576
121.024610	3604.100632	23.541594
120.847946	3595.667313	23.546611
120.983619	3587.054407	23.551629
120.792396	3599.454918	23.556647
120.901964	3602.207813	23.561664
120.850344	3615.107593	23.566682
121.296448	3628.811374	23.571699
121.529628	3617.075829	23.576717
121.507198	3621.287680	23.581735
121.486234	3611.023490	23.586752
121.644171	3631.180868	23.591770
121.909740	3648.807918	23.596787
122.545685	3644.501303	23.601805
122.405478	3655.586395	23.606823
122.483403	3640.105402	23.611840
122.584422	3643.558170	23.616858
122.386015	3644.779111	23.621875
122.456777	3641.376749	23.626893
122.796774	3650.407751	23.631911
122.787797	3658.747917	23.636928
122.911029	3665.310522	23.641946
122.720082	3676.063121	23.646963
123.096358	3674.247386	23.651981
123.060672	3686.289650	23.656999
123.086050	3703.854380	23.662016
123.440829	3700.295807	23.667034
123.240743	3715.089894	23.672051
123.680733	3700.078132	23.677069
123.610390	3719.283269	23.682087
123.735734	3720.196946	23.687104
123.806377	3728.006083	23.692122
124.162426	3731.105137	23.697139
124.583116	3726.957892	23.702157
124.315677	3745.753205	23.707175
124.378984	3754.873227	23.712192
124.897703	3739.461860	23.717210
124.850771	3750.158512	23.722227
124.752238	3745.895041	23.727245
124.852705	3753.863050	23.732263
125.079802	3770.963062	23.737280
125.272358	3768.088731	23.742298
125.230709	3779.359573	23.747315
125.667368	3773.081991	23.752333
125.722899	3787.856632	23.757351
125.862259	3805.529954	23.762368
126.159383	3801.096400	23.767386
126.110130	3806.730053	23.772403
126.253376	3809.937785	23.777421
126.159141	3805.287385	23.782439
126.573213	3813.627046	23.787456
126.806330	3797.098547	23.792474
126.653000	3812.127554	23.797491
127.095870	3825.861141	23.802509
127.333029	3838.752043	23.807527
127.095367	3830.805788	23.812544
127.519109	3824.500353	23.817562
127.430657	3823.342368	23.822579
127.553076	3823.790844	23.827597
127.168089	3825.810068	23.832615
127.383091	3844.083359	23.837632
127.751005	3842.702362	23.842650
127.798819	3855.689545	23.847667
128.009865	3852.995531	23.852685
128.533344	3858.584293	23.857703
128.124035	3859.456584	23.862720
128.901753	3868.353425	23.867738
128.914371	3885.644307	23.872755
128.838034	3867.355071	23.877773
128.829590	3865.082279	23.882791
129.042670	3876.467542	23.887808
129.169246	3869.394539	23.892826
128.803031	3888.311190	23.897843
129.410596	3893.966006	23.902861
129.566663	3893.686220	23.907879
129.762218	3907.113995	23.912896
129.975289	3897.679139	23.917914
129.835837	3889.223983	23.922931
130.154585	3905.968149	23.927949
130.127029	3905.688537	23.932967
129.925795	3929.561361	23.937984
130.927556	3925.034295	23.943002
130.928739	3925.334557	23.948019
130.866481	3924.930685	23.953037
130.866966	3922.611623	23.958055
130.849803	3918.840135	23.963072
130.886328	3921.971301	23.968090
131.140868	3923.245900	23.973107
131.294675	3931.295963	23.978125
131.352804	3940.912496	23.983143
131.509485	3948.286405	23.988160
131.656902	3942.731363	23.993178
131.455570	3953.267141	23.998195
131.547583	3947.087703	24.003213
131.972319	3961.359999	24.008231
131.757429	3970.375056	24.013248
132.340840	3969.750239	24.018266
132.263490	3967.698446	24.023283
132.422961	3979.426651	24.028301
132.513854	3998.232800	24.033319
132.387037	4012.300466	24.038336
133.046175	4004.800302	24.043354
132.865255	4011.369082	24.048371
132.769674	4025.910046	24.053389
133.279340	4029.168742	24.058407
133.112399	4039.070586	24.063424
133.264783	4039.475747	24.068442
133.556542	4049.324912	24.073459
133.664591	4050.718062	24.078477
133.961766	4058.491255	24.083495
134.172474	4062.452885	24.088512
134.416457	4052.769147	24.093530
134.397898	4074.400307	24.098547
134.376024	4080.218490	24.103565
134.549652	4083.982302	24.108583
134.741792	4087.887903	24.113600
135.046146	4083.561667	24.118618
135.060437	4087.287956	24.123635
135.576050	4084.001779	24.128653
135.212090	4106.830240	24.133671
135.432556	4118.072135	24.138688
135.643216	4115.981478	24.143706
135.620255	4118.544000	24.148723
135.573095	4121.000253	24.153741
136.105504	4114.331253	24.158759
136.232288	4132.692128	24.163776
136.444530	4131.883421	24.168794
136.463221	4136.298107	24.173811
136.503068	4125.817763	24.178829
136.675662	4127.475162	24.183847
136.541706	4136.419992	24.188864
137.011727	4136.034293	24.193882
137.147799	4161.161875	24.198899
136.983242	4152.734955	24.203917
137.448815	4137.028010	24.208935
137.049067	4161.367082	24.213952
137.302766	4168.838121	24.218970
137.336409	4178.789100	24.223987
137.699578	4190.768182	24.229005
137.926837	4181.920069	24.234023
138.221100	4206.376681	24.239040
138.191291	4204.605181	24.244058
138.561266	4211.180608	24.249075
138.615683	4215.396110	24.254093
138.828924	4198.371605	24.259111
138.869355	4212.746328	24.264128
139.090716	4204.256272	24.269146
139.090714	4208.802968	24.274163
139.191486	4211.423654	24.279181
139.387485	4225.427466	24.284199
139.292083	4237.238995	24.289216
139.408233	4228.817618	24.294234
139.560506	4229.402942	24.299251
139.177018	4243.805169	24.304269
139.818358	4254.742500	24.309287
139.752835	4251.926531	24.314304
139.842686	4279.675673	24.319322
139.685330	4297.104270	24.324339
140.263781	4299.146147	24.329357
140.646079	4296.863691	24.334375
140.831787	4315.431726	24.339392
141.322078	4322.356166	24.344410
141.422157	4314.997691	24.349427
141.413917	4324.672257	24.354445
141.884401	4305.224671	24.359463
141.967434	4320.017491	24.364480
142.131019	4309.596737	24.369498
141.879078	4318.341018	24.374515
141.832171	4319.184655	24.379533
141.958228	4310.465876	24.384551
141.832719	4324.990670	24.389568
141.982475	4335.521086	24.394586
142.138013	4327.485119	24.399603
142.363401	4357.029932	24.404621
143.057738	4357.561085	24.409639
142.966987	4362.322104	24.414656
143.287074	4358.702043	24.419674
143.444000	4365.726857	24.424691
143.425779	4364.782609	24.429709
143.887374	4374.750443	24.434727
143.821303	4388.695508	24.439744
144.228145	4378.659919	24.444762
144.238870	4389.015882	24.449779
144.114482	4394.485533	24.454797
144.365499	4390.105568	24.459815
144.067293	4395.396833	24.464832
144.329305	4391.517779	24.469850
144.498062	4400.231216	24.474867
144.687935	4418.627230	24.479885
145.011830	4408.018011	24.484903
144.940083	4420.756514	24.489920
145.258316	4413.824180	24.494938
145.497120	4420.597612	24.499955
145.158771	4443.805607	24.504973
145.518823	4437.252050	24.509991
145.533901	4437.337712	24.515008
145.627067	4441.683977	24.520026
145.442548	4462.261321	24.525043
145.733418	4475.952108	24.530061
146.184053	4469.441520	24.535079
146.433936	4493.753867	24.540096
146.606044	4496.167355	24.545114
146.979699	4492.301154	24.550131
146.597468	4502.314726	24.555149
146.906520	4499.492478	24.560167
146.939671	4507.742240	24.565184
146.891217	4524.411147	24.570202
147.571561	4521.665786	24.575219
147.479526	4533.270913	24.580237
147.827207	4524.633096	24.585255
147.684803	4525.522651	24.590272
148.013161	4551.066273	24.595290
148.622388	4538.406295	24.600307
148.171953	4554.912774	24.605325
148.746971	4547.505204	24.610343
148.602087	4547.248220	24.615360
148.850779	4553.759756	24.620378
148.822518	4560.671019	24.625395
149.043357	4570.158185	24.630413
149.124157	4563.826093	24.635431
149.424759	4568.914961	24.640448
149.304237	4574.647591	24.645466
149.871776	4583.481632	24.650483
149.813514	4595.396871	24.655501
150.224914	4583.387492	24.660519
150.614800	4596.620508	24.665536
150.191664	4596.271795	24.670554
150.363242	4579.883601	24.675571
150.648062	4605.210851	24.680589
150.641461	4611.174700	24.685607
150.650921	4616.095248	24.690624
150.922678	4621.989547	24.695642
151.208589	4622.373437	24.700659
151.140403	4627.260742	24.705677
151.088351	4640.798684	24.710695
151.369208	4636.583806	24.715712
151.529800	4645.422983	24.720730
152.001522	4654.801765	24.725747
151.882786	4673.760991	24.730765
152.157750	4661.315468	24.735783
152.506100	4665.166426	24.740800
152.609940	4693.801470	24.745818
152.781285	4678.997532	24.750835
153.047774	4692.879636	24.755853
152.795095	4694.128979	24.760871
153.160180	4689.788952	24.765888
153.348926	4687.848028	24.770906
153.532103	4696.796914	24.775923
153.644858	4707.021195	24.780941
153.882329	4714.613889	24.785959
154.011424	4722.146773	24.790976
153.685795	4713.790836	24.795994
154.221278	4718.513484	24.801011
154.270520	4719.547919	24.806029
154.358614	4723.007725	24.811047
154.432589	4727.022018	24.816064
154.482924	4730.078783	24.821082
154.721155	4737.746887	24.826099
154.796753	4742.979463	24.831117
155.133419	4760.867920	24.836135
155.148192	4765.093834	24.841152
155.247728	4770.833147	24.846170
155.276794	4758.305602	24.851187
155.469920	4777.927955	24.856205
155.599923	4798.798607	24.861223
155.797360	4795.953981	24.866240
156.255136	4820.357231	24.871258
156.321121	4813.185663	24.876275
156.351675	4831.504544	24.881293
156.717373	4825.024650	24.886311
156.759564	4822.034064	24.891328
156.813291	4839.565743	24.896346
157.303798	4845.030350	24.901363
157.247690	4853.676856	24.906381
157.359824	4848.912980	24.911399
157.777761	4862.584658	24.916416
157.909387	4874.871836	24.921434
158.247317	4871.243301	24.926451
158.517737	4873.057471	24.931469
158.839933	4873.655850	24.936487
158.923277	4875.737421	24.941504
158.699976	4859.426821	24.946522
158.898262	4871.239234	24.951539
159.103165	4868.122003	24.956557
158.897460	4887.671998	24.961575
159.181029	4887.954789	24.966592
159.363941	4887.510228	24.971610
159.313968	4897.894320	24.976627
159.486996	4906.295858	24.981645
159.976168	4919.927126	24.986663
160.362052	4929.464519	24.991680
160.238373	4919.124535	24.996698
160.326980	4923.039789	25.001715
160.494849	4918.421191	25.006733
160.712307	4933.062611	25.011751
161.055105	4935.553586	25.016768
161.044378	4939.188894	25.021786
161.356106	4933.589976	25.026803
161.434243	4933.756055	25.031821
161.378310	4927.425154	25.036839
162.017143	4947.234700	25.041856
161.649431	4964.606372	25.046874
162.016448	4953.699606	25.051891
161.983987	4969.422462	25.056909
161.831274	4973.649966	25.061927
161.949771	4978.864774	25.066944
162.073422	4992.207464	25.071962
162.534969	4982.735445	25.076979
162.540695	4998.219388	25.081997
162.740288	5022.770341	25.087015
163.235671	5011.072911	25.092032
163.012610	5018.907537	25.097050
163.348373	5025.937196	25.102067
163.503365	5042.059768	25.107085
163.590137	5056.115619	25.112103
163.777424	5052.729754	25.117120
163.850927	5058.693601	25.122138
164.396142	5080.609244	25.127155
164.530153	5095.423039	25.132173
164.527060	5083.811319	25.137191
165.192770	5064.149101	25.142208
164.705731	5074.734377	25.147226
165.154656	5081.948198	25.152243
165.439942	5099.266265	25.157261
165.326595	5106.365207	25.162279
165.800572	5100.144055	25.167296
165.769862	5096.051098	25.172314
165.653017	5096.189265	25.177331
166.416990	5120.130405	25.182349
166.415403	5129.530675	25.187367
166.501742	5122.178708	25.192384
166.448964	5133.131398	25.197402
166.707160	5120.390796	25.202419
166.803785	5134.232747	25.207437
166.839666	5154.293682	25.212455
167.253403	5160.890886	25.217472
167.164617	5166.327613	25.222490
167.241183	5176.234664	25.227507
167.456716	5184.004171	25.232525
167.695159	5175.451047	25.237543
168.119048	5194.868030	25.242560
168.322486	5197.670770	25.247578
168.344262	5199.871553	25.252595
168.871549	5199.940852	25.257613
168.783122	5203.605133	25.262631
169.178948	5218.960245	25.267648
169.124769	5238.164005	25.272666
169.358828	5231.354060	25.277683
169.642510	5235.179295	25.282701
169.305811	5236.178536	25.287719
169.566631	5230.505808	25.292736
169.684838	5250.882585	25.297754
169.776495	5251.414683	25.302771
170.038908	5260.492885	25.307789
170.200744	5273.615764	25.312807
170.542086	5275.900133	25.317824
170.843770	5295.363480	25.322842
171.127422	5280.847843	25.327859
171.435007	5284.015540	25.332877
171.172709	5304.689850	25.337895
171.726244	5291.979897	25.342912
171.470326	5309.115450	25.347930
171.771398	5319.700333	25.352947
172.226601	5303.954471	25.357965
172.574037	5305.596720	25.362983
172.389022	5303.574489	25.368000
172.434325	5303.232098	25.373018
172.597894	5311.281367	25.378035
172.820972	5319.893077	25.383053
172.778833	5333.113038	25.388071
173.167388	5330.078141	25.393088
173.396739	5340.221340	25.398106
173.368426	5333.718294	25.403123
173.531318	5336.665198	25.408141
173.613683	5354.956804	25.413159
173.979974	5346.426467	25.418176
173.545039	5349.125687	25.423194
174.136050	5358.116161	25.428211
174.419926	5369.018500	25.433229
173.938852	5380.321293	25.438247
174.304428	5380.231503	25.443264
174.312932	5404.994502	25.448282
174.797180	5416.365269	25.453299
174.965092	5431.326618	25.458317
175.226085	5437.669023	25.463335
175.601884	5435.583325	25.468352
175.924904	5455.841196	25.473370
175.801619	5464.497984	25.478387
176.383418	5453.131004	25.483405
176.151208	5456.401320	25.488423
176.572790	5475.680586	25.493440
176.940092	5481.570229	25.498458
177.084983	5473.789441	25.503475
177.312182	5478.621282	25.508493
177.508863	5480.649468	25.513511
177.561427	5474.212136	25.518528
177.666196	5486.762147	25.523546
178.007414	5491.716633	25.528563
178.530386	5488.575312	25.533581
178.332125	5495.577053	25.538599
178.727753	5500.242802	25.543616
178.913892	5491.272230	25.548634
178.790527	5487.785534	25.553651
179.036431	5487.576365	25.558669
179.122012	5503.454046	25.563687
179.156274	5511.259708	25.568704
179.497546	5529.625900	25.573722
179.276957	5533.671643	25.578739
179.604481	5536.085703	25.583757
179.610325	5550.167516	25.588775
179.473179	5558.976831	25.593792
180.036534	5565.773005	25.598810
180.006610	5586.230505	25.603827
180.101976	5583.604187	25.608845
180.311264	5603.320259	25.613863
180.683937	5618.254661	25.618880
180.664917	5614.833904	25.623898
180.805863	5624.071733	25.628915
181.435023	5634.165555	25.633933
181.581501	5646.058444	25.638951
181.872947	5639.386278	25.643968
182.299094	5641.968723	25.648986
182.227623	5639.546789	25.654003
182.521976	5648.090686	25.659021
182.592049	5661.721023	25.664039
182.818995	5666.950254	25.669056
182.899887	5665.414249	25.674074
182.653423	5665.741440	25.679092
183.228133	5668.840675	25.684109
183.050431	5686.368564	25.689127
183.555368	5687.287936	25.694144
183.892178	5709.980406	25.699162
184.053881	5715.974514	25.704180
184.320830	5719.453245	25.709197
184.144104	5719.560840	25.714215
184.277150	5713.799733	25.719232
184.754610	5728.155829	25.724250
184.733082	5751.831454	25.729268
185.037014	5740.964850	25.734285
184.884832	5743.120283	25.739303
185.105447	5765.305837	25.744320
185.516267	5770.282364	25.749338
185.567642	5777.913149	25.754356
186.002103	5792.439800	25.759373
185.998236	5805.296913	25.764391
185.829315	5794.800673	25.769408
186.358055	5817.300646	25.774426
186.314723	5831.097122	25.779444
186.766770	5827.566600	25.784461
187.090873	5862.168325	25.789479
187.130962	5873.411219	25.794496
187.114466	5869.844457	25.799514
187.605985	5882.534548	25.804532
188.088346	5879.674188	25.809549
188.572016	5892.000500	25.814567
188.789684	5879.422266	25.819584
188.780372	5877.231906	25.824602
188.771901	5872.541213	25.829620
189.193169	5869.062791	25.834637
188.831625	5888.008791	25.839655
188.982522	5901.803476	25.844672
189.503768	5906.248717	25.849690
189.583864	5908.377370	25.854708
189.614042	5910.114326	25.859725
189.423265	5932.727611	25.864743
189.837011	5936.970503	25.869760
190.103534	5948.470018	25.874778
190.086160	5960.946285	25.879796
190.585667	5964.002504	25.884813
190.901039	5962.801208	25.889831
191.098894	5971.665142	25.894848
191.390676	5982.909691	25.899866
191.298814	5994.209116	25.904884
191.498480	5983.163849	25.909901
191.480062	5993.542896	25.914919
191.837076	6011.407610	25.919936
192.265218	6012.243268	25.924954
191.950041	6028.366353	25.929972
192.248035	6020.392509	25.934989
192.255268	6040.954859	25.940007
192.455374	6053.769443	25.945024
192.456009	6038.959889	25.950042
193.012765	6064.424108	25.955060
192.958331	6072.966427	25.960077
193.243799	6082.747164	25.965095
193.568103	6097.451387	25.970112
193.869477	6097.850954	25.975130
193.993596	6122.797344	25.980148
194.429202	6122.144890	25.985165
194.798713	6124.765562	25.990183
194.489225	6140.843018	25.995200
194.955014	6142.286337	26.000218
195.120668	6153.352867	26.005236
195.276846	6154.251559	26.010253
195.598837	6154.074311	26.015271
196.036106	6180.341370	26.020288
196.434252	6178.823181	26.025306
196.231342	6191.599859	26.030324
196.593973	6177.674968	26.035341
196.525219	6180.935117	26.040359
196.716458	6191.254130	26.045376
197.178179	6203.776955	26.050394
197.186792	6196.498998	26.055412
197.365716	6199.726747	26.060429
197.489971	6208.530964	26.065447
197.879193	6219.314080	26.070464
197.885957	6216.064516	26.075482
197.788934	6224.140094	26.080500
198.167469	6237.628166	26.085517
198.542233	6251.927195	26.090535
198.368056	6245.690890	26.095552
198.860313	6261.007335	26.100570
199.310139	6284.206645	26.105588
199.428425	6281.211501	26.110605
199.533170	6280.339575	26.115623
199.511026	6279.194422	26.120640
199.920529	6292.368418	26.125658
200.174813	6311.407961	26.130676
200.140823	6309.817824	26.135693
200.460242	6316.008897	26.140711
200.290332	6330.281543	26.145728
200.737564	6337.799158	26.150746
201.115551	6343.546622	26.155764
201.121540	6362.317409	26.160781
201.186486	6367.791434	26.165799
201.214166	6370.864741	26.170816
201.611749	6376.356548	26.175834
201.653679	6398.307982	26.180852
201.877553	6400.885835	26.185869
202.169126	6416.164415	26.190887
202.474246	6426.860387	26.195904
202.679665	6429.197295	26.200922
202.972837	6437.150205	26.205940
202.971107	6450.448120	26.210957
203.205210	6457.152442	26.215975
203.327238	6459.530185	26.220992
203.695316	6471.719637	26.226010
203.652819	6478.111664	26.231028
203.990541	6472.526124	26.236045
204.541911	6497.644996	26.241063
204.473173	6507.005710	26.246080
204.510744	6508.584208	26.251098
204.990475	6515.937809	26.256116
205.026858	6524.222017	26.261133
205.291252	6534.089811	26.266151
205.254651	6548.718272	26.271168
206.012301	6550.718549	26.276186
205.981630	6573.528367	26.281204
206.095080	6574.191577	26.286221
206.434997	6583.685456	26.291239
206.595871	6588.528238	26.296256
206.778970	6587.902648	26.301274
207.396077	6612.772848	26.306292
207.489349	6621.935507	26.311309
207.558964	6617.887501	26.316327
207.636464	6625.192773	26.321344
208.187381	6624.041996	26.326362
208.098557	6644.211382	26.331380
208.134483	6642.152954	26.336397
208.373818	6644.623747	26.341415
208.342680	6669.368437	26.346432
208.485750	6679.114839	26.351450
209.037356	6686.736370	26.356468
209.371907	6708.052329	26.361485
209.461330	6707.105718	26.366503
209.325152	6714.401826	26.371520
209.715236	6742.330406	26.376538
210.030202	6745.494890	26.381556
210.179837	6752.656549	26.386573
210.505366	6755.760344	26.391591
210.583827	6762.838943	26.396608
210.733294	6781.293924	26.401626
210.754581	6802.642649	26.406644
211.129411	6804.633969	26.411661
211.366289	6824.326822	26.416679
211.493871	6841.602849	26.421696
211.936254	6849.167921	26.426714
212.249753	6863.147653	26.431732
212.477494	6863.573933	26.436749
212.715289	6863.484847	26.441767
213.078776	6883.898737	26.446784
213.180930	6882.063391	26.451802
213.162367	6893.886037	26.456820
213.422013	6881.540230	26.461837
213.758429	6889.009706	26.466855
213.761011	6917.852469	26.471872
214.181139	6922.357418	26.476890
214.435720	6912.783421	26.481908
213.887350	6925.258604	26.486925
214.610383	6929.502051	26.491943
214.427440	6943.873351	26.496960
214.590786	6958.475849	26.501978
214.768834	6969.199554	26.506996
214.719255	6986.317525	26.512013
215.500050	6993.808268	26.517031
215.373933	7014.058846	26.522048
215.998516	7026.440756	26.527066
216.249663	7046.605274	26.532084
216.514844	7061.448917	26.537101
216.888840	7065.956544	26.542119
217.065383	7072.833975	26.547136
217.264759	7096.627599	26.552154
217.301374	7103.340094	26.557172
217.924912	7097.696172	26.562189
218.118935	7113.659794	26.567207
217.872480	7122.455202	26.572224
218.333370	7117.959160	26.577242
218.828628	7123.941584	26.582260
218.565915	7142.652338	26.587277
218.938635	7149.101989	26.592295
219.263620	7155.516766	26.597312
219.282523	7173.122861	26.602330
219.549824	7170.046349	26.607348
219.451400	7186.354862	26.612365
220.186109	7187.674384	26.617383
220.127281	7199.179534	26.622400
220.221336	7221.887854	26.627418
220.782423	7231.166720	26.632436
221.035628	7246.999098	26.637453
221.298803	7248.954779	26.642471
221.354404	7263.697493	26.647488
221.518142	7269.135648	26.652506
221.745045	7279.441869	26.657524
221.782070	7290.442423	26.662541
222.000826	7298.376192	26.667559
222.225059	7323.767351	26.672576
222.236447	7336.816915	26.677594
223.146123	7342.891513	26.682612
222.857185	7354.716714	26.687629
223.291445	7367.290545	26.692647
223.473337	7383.248524	26.697664
223.825795	7387.304913	26.702682
224.237161	7411.268245	26.707700
224.131017	7423.323218	26.712717
224.814012	7415.954469	26.717735
224.552360	7417.093732	26.722752
224.943090	7433.078270	26.727770
225.079584	7438.100677	26.732788
225.037332	7446.564737	26.737805
225.353135	7450.970821	26.742823
225.875969	7466.728195	26.747840
225.793327	7471.382700	26.752858
226.027810	7477.576003	26.757876
226.114260	7495.870397	26.762893
226.456237	7508.458274	26.767911
226.761345	7521.714531	26.772928
226.438646	7525.806985	26.777946
227.156477	7544.173102	26.782964
227.176408	7562.677245	26.787981
227.636675	7575.119645	26.792999
227.961415	7589.300485	26.798016
227.917631	7591.497912	26.803034
228.296493	7609.535755	26.808052
228.172668	7633.656360	26.813069
228.760624	7626.809367	26.818087
229.379544	7649.098704	26.823104
229.029328	7655.622119	26.828122
229.466241	7683.836134	26.833140
229.901850	7691.947987	26.838157
229.900049	7693.090695	26.843175
230.245982	7710.738927	26.848192
230.519078	7711.184758	26.853210
230.657300	7719.729573	26.858228
230.919169	7739.639970	26.863245
231.348992	7736.900160	26.868263
231.640404	7756.207100	26.873280
231.479418	7771.619809	26.878298
231.935819	7766.638823	26.883316
231.895736	7776.719644	26.888333
232.175185	7800.662933	26.893351
232.670618	7819.954744	26.898368
232.702629	7822.610644	26.903386
232.912548	7812.071463	26.908404
232.536287	7850.682694	26.913421
233.136959	7856.491251	26.918439
233.757559	7867.681678	26.923456
233.880918	7888.939371	26.928474
234.411989	7892.270300	26.933492
234.208182	7917.359324	26.938509
234.825095	7930.464743	26.943527
235.239027	7928.517411	26.948544
235.294496	7938.565014	26.953562
235.536584	7951.660960	26.958580
235.516397	7948.769387	26.963597
236.090064	7950.130395	26.968615
236.522725	7972.556920	26.973632
236.676341	7974.960561	26.978650
236.817321	7970.751313	26.983668
236.984181	7982.530318	26.988685
236.909865	8001.544949	26.993703
237.110597	8009.841556	26.998720
237.311453	8015.498317	27.003738
237.853264	8023.431337	27.008756
237.599656	8040.555505	27.013773
237.886716	8032.133052	27.018791
238.095998	8063.049875	27.023808
238.570460	8065.086865	27.028826
238.686909	8063.701528	27.033844
238.716276	8088.766260	27.038861
238.913476	8107.326228	27.043879
239.176256	8120.976109	27.048896
239.134354	8132.583932	27.053914
239.745979	8145.151400	27.058932
239.896191	8167.438728	27.063949
240.197431	8168.206628	27.068967
240.537914	8195.382619	27.073984
240.872859	8213.778344	27.079002
241.112006	8230.121530	27.084020
241.757087	8226.359829	27.089037
242.010703	8228.143274	27.094055
242.145568	8246.701550	27.099072
242.319111	8253.271564	27.104090
242.708899	8246.234778	27.109108
242.556105	8270.068324	27.114125
243.078665	8267.948625	27.119143
243.396640	8291.213023	27.124160
243.417528	8288.645313	27.129178
243.758227	8300.787925	27.134196
243.635870	8315.305897	27.139213
244.077631	8322.756951	27.144231
244.460544	8329.824750	27.149248
244.398385	8351.269260	27.154266
244.899340	8354.907249	27.159284
244.689951	8367.576664	27.164301
244.959928	8382.607353	27.169319
245.396246	8389.726469	27.174336
245.439986	8418.778820	27.179354
245.665396	8430.187681	27.184372
246.268613	8459.223321	27.189389
246.557726	8469.799790	27.194407
246.914662	8463.487329	27.199424
246.890959	8485.548308	27.204442
247.482948	8494.801017	27.209460
247.564024	8507.768109	27.214477
248.044161	8525.793285	27.219495
248.356177	8512.716231	27.224512
248.289229	8527.920377	27.229530
248.658960	8531.671390	27.234548
248.729915	8545.253881	27.239565
249.041633	8568.206537	27.244583
249.352262	8544.965756	27.249600
249.557487	8590.648239	27.254618
249.916188	8565.727674	27.259636
249.755638	8620.929022	27.264653
249.920106	8592.194743	27.269671
250.343267	8615.593173	27.274688
250.403653	8646.418485	27.279706
250.808010	8638.198893	27.284724
251.239826	8648.489143	27.289741
251.405161	8671.195396	27.294759
251.938696	8654.955103	27.299776
252.177123	8682.236381	27.304794
252.406585	8682.616022	27.309812
252.550167	8692.893232	27.314829
252.558237	8706.068064	27.319847
252.999364	8708.394522	27.324864
252.829527	8727.364714	27.329882
253.132231	8743.134146	27.334900
253.145608	8774.033313	27.339917
253.712956	8769.138970	27.344935
254.056881	8778.890148	27.349952
254.224756	8802.661626	27.354970
254.595343	8816.182439	27.359988
254.859279	8831.811786	27.365005
255.070477	8842.696808	27.370023
255.289357	8827.221757	27.375040
255.352062	8879.072570	27.380058
255.315339	8875.466604	27.385076
255.991225	8877.892588	27.390093
256.128921	8914.268589	27.395111
256.714179	8923.971166	27.400128
256.797929	8948.846119	27.405146
257.484993	8942.934870	27.410164
257.821960	8958.335529	27.415181
257.583004	8976.514431	27.420199
258.415169	8978.954079	27.425216
258.301729	8992.208335	27.430234
258.823340	9001.439140	27.435252
259.037710	8990.353502	27.440269
258.805972	9015.994134	27.445287
259.427428	9008.902363	27.450304
259.555634	9042.487921	27.455322
259.920250	9047.904547	27.460340
260.213643	9056.951434	27.465357
260.353252	9073.261840	27.470375
261.000411	9076.312900	27.475392
260.991021	9109.810770	27.480410
261.348252	9110.472225	27.485428
261.457596	9107.615256	27.490445
261.476121	9127.037115	27.495463
261.722663	9139.596345	27.500480
261.982138	9155.874357	27.505498
262.450501	9164.831650	27.510516
262.867705	9167.874924	27.515533
262.762240	9191.125599	27.520551
262.935776	9190.389694	27.525568
263.356213	9226.571485	27.530586
263.518363	9230.818857	27.535604
263.775166	9251.149930	27.540621
264.169971	9259.919132	27.545639
264.341309	9272.331114	27.550656
264.357843	9288.634617	27.555674
264.500364	9298.086167	27.560692
264.978394	9331.671698	27.565709
265.106859	9326.841232	27.570727
265.570195	9348.340333	27.575744
266.048630	9354.327143	27.580762
266.198085	9372.906135	27.585780
266.475064	9379.852435	27.590797
266.669754	9396.149298	27.595815
267.186210	9402.199315	27.600832
267.165390	9437.066992	27.605850
267.745461	9435.073715	27.610868
268.010046	9436.266166	27.615885
267.837115	9447.626772	27.620903
268.285826	9479.031271	27.625920
268.567530	9491.095734	27.630938
269.032012	9476.523195	27.635956
269.317163	9518.948587	27.640973
269.418059	9523.995080	27.645991
269.681012	9536.252608	27.651008
269.894351	9536.570317	27.656026
270.262811	9554.612183	27.661044
270.771201	9559.410780	27.666061
270.430486	9590.631690	27.671079
270.880674	9600.181939	27.676096
271.402735	9603.900687	27.681114
271.523094	9627.311199	27.686132
271.505554	9644.938612	27.691149
272.007811	9655.355654	27.696167
272.523938	9668.072632	27.701184
272.763213	9687.996321	27.706202
273.026368	9693.825180	27.711220
273.447448	9699.638706	27.716237
273.456519	9723.572313	27.721255
273.782451	9726.310367	27.726272
274.044342	9748.782137	27.731290
274.055311	9767.384873	27.736308
274.703088	9775.739877	27.741325
274.722967	9796.796051	27.746343
275.248574	9813.571409	27.751360
275.114260	9822.849829	27.756378
275.561236	9845.879688	27.761396
275.707173	9859.991257	27.766413
275.795016	9873.779620	27.771431
276.385577	9889.082196	27.776448
276.914401	9908.356056	27.781466
276.881198	9927.628237	27.786484
277.236948	9944.099516	27.791501
277.501246	9961.707955	27.796519
278.172235	9966.823875	27.801536
278.407484	9985.500912	27.806554
278.470295	9990.591407	27.811572
279.050542	9994.545326	27.816589
278.948818	10013.336701	27.821607
279.170182	10026.060440	27.826624
279.318753	10032.506164	27.831642
279.734612	10045.036023	27.836660
280.162091	10055.911461	27.841677
280.570023	10073.093437	27.846695
280.542875	10058.649061	27.851712
280.913401	10080.970628	27.856730
281.257610	10095.312476	27.861748
281.659351	10098.564591	27.866765
281.907556	10122.165221	27.871783
281.894440	10117.136724	27.876800
282.549002	10149.630041	27.881818
282.471860	10147.124067	27.886836
282.895693	10162.313029	27.891853
282.724450	10174.767772	27.896871
283.224924	10195.315870	27.901888
283.542742	10215.294634	27.906906
283.558120	10225.993892	27.911924
284.230517	10241.295592	27.916941
284.248312	10265.512368	27.921959
284.393182	10282.483508	27.926976
284.891450	10285.522754	27.931994
285.223955	10304.116222	27.937012
285.419598	10333.739871	27.942029
285.544342	10355.438797	27.947047
286.162079	10359.085436	27.952064
286.196878	10374.719082	27.957082
286.709948	10421.606994	27.962100
286.864312	10413.154391	27.967117
287.279297	10442.997484	27.972135
287.372197	10456.499516	27.977152
287.954343	10449.047408	27.982170
288.320193	10477.261518	27.987188
288.595265	10493.307135	27.992205
289.102124	10509.124987	27.997223
289.268493	10525.437826	28.002240
289.687645	10530.572048	28.007258
289.419364	10553.827173	28.012276
290.269080	10550.851537	28.017293
290.416814	10568.402146	28.022311
290.449799	10594.150047	28.027328
290.954136	10608.892224	28.032346
291.363672	10632.287334	28.037364
291.445367	10627.182958	28.042381
291.960854	10645.898786	28.047399
292.000965	10662.077256	28.052416
292.295568	10674.314148	28.057434
292.708371	10689.083979	28.062452
292.938067	10700.265279	28.067469
293.280046	10714.355458	28.072487
293.433850	10736.214781	28.077504
293.776558	10736.929000	28.082522
293.953809	10753.944304	28.087540
294.245214	10782.078383	28.092557
294.184958	10793.247728	28.097575
294.519886	10810.662149	28.102592
295.073031	10826.338386	28.107610
295.259857	10853.392606	28.112628
295.548130	10854.368129	28.117645
295.793823	10875.681402	28.122663
295.668999	10890.186123	28.127680
296.307637	10908.873208	28.132698
296.371983	10928.833511	28.137716
296.948057	10935.551074	28.142733
297.156751	10968.748396	28.147751
297.510327	10982.465520	28.152768
298.210706	10995.981790	28.157786
297.960243	11015.531203	28.162804
298.411148	11025.370689	28.167821
298.827410	11047.202406	28.172839
299.241277	11068.984563	28.177856
299.284010	11078.739608	28.182874
299.312065	11099.688878	28.187892
299.965877	11116.277246	28.192909
300.190651	11138.618110	28.197927
300.417341	11159.284359	28.202944
300.980373	11157.564316	28.207962
300.821867	11193.640478	28.212980
301.169603	11216.222358	28.217997
301.714688	11236.790748	28.223015
301.741003	11268.967936	28.228032
302.085138	11289.646732	28.233050
302.718939	11293.621984	28.238068
302.987368	11329.600128	28.243085
303.173934	11343.566529	28.248103
303.258488	11366.050885	28.253120
304.190783	11368.187741	28.258138
304.352857	11397.175846	28.263156
304.640560	11419.912803	28.268173
305.042747	11438.556190	28.273191
304.951208	11463.979923	28.278208
305.837130	11472.577325	28.283226
305.774078	11485.521169	28.288244
306.319905	11500.088012	28.293261
306.809451	11506.654352	28.298279
307.296802	11522.687307	28.303296
308.147427	11517.286151	28.308314
307.965272	11524.133089	28.313332
308.325655	11532.492787	28.318349
309.176848	11537.287376	28.323367
308.478795	11551.346554	28.328384
308.801485	11566.497971	28.333402
309.257558	11582.066516	28.338420
309.267920	11588.098927	28.343437
309.576294	11608.988882	28.348455
309.719949	11624.166530	28.353472
310.571890	11632.751340	28.358490
310.637894	11662.486020	28.363508
310.749847	11680.285245	28.368525
311.130280	11680.370964	28.373543
311.171449	11710.912858	28.378560
311.479298	11727.695952	28.383578
311.451153	11739.296893	28.388596
311.827497	11759.082252	28.393613
312.429494	11773.270111	28.398631
312.627954	11793.784717	28.403648
313.139745	11812.096877	28.408666
313.299277	11836.364421	28.413684
313.235366	11849.377579	28.418701
313.892683	11873.038929	28.423719
314.319061	11889.441670	28.428736
314.487997	11906.827543	28.433754
314.986854	11939.839094	28.438772
315.003505	11944.935246	28.443789
315.662303	11960.229467	28.448807
315.876553	11985.059922	28.453824
315.970296	12004.682469	28.458842
316.574206	12019.684848	28.463860
316.598826	12044.620785	28.468877
317.176035	12053.441271	28.473895
317.163800	12087.575073	28.478912
317.491855	12094.632950	28.483930
317.631067	12115.329406	28.488948
318.037486	12136.216272	28.493965
318.678036	12157.089072	28.498983
318.589910	12185.923378	28.504000
319.105458	12202.262664	28.509018
319.433622	12237.392879	28.514036
319.969476	12253.657757	28.519053
320.585212	12276.547575	28.524071
320.865652	12285.797218	28.529088
321.225970	12306.585021	28.534106
321.539375	12337.082038	28.539124
321.730025	12337.540775	28.544141
322.415865	12346.285092	28.549159
322.395774	12366.546259	28.554176
323.001705	12383.442943	28.559194
323.520435	12388.851974	28.564212
323.317867	12410.638686	28.569229
323.751205	12428.818886	28.574247
323.999929	12437.034749	28.579264
324.636430	12457.952295	28.584282
324.833550	12476.845502	28.589300
325.290385	12491.348785	28.594317
325.556434	12513.825797	28.599335
325.692630	12518.239001	28.604352
326.340921	12532.352907	28.609370
326.468148	12542.992103	28.614388
326.492922	12565.243974	28.619405
326.820876	12578.627804	28.624423
327.547347	12608.095768	28.629440
327.618347	12613.091790	28.634458
327.936222	12635.613655	28.639476
328.153493	12647.307426	28.644493
328.663345	12664.971004	28.649511
328.528317	12681.388124	28.654528
328.839995	12708.392912	28.659546
329.383197	12714.812513	28.664564
329.313601	12735.201894	28.669581
329.630772	12758.798618	28.674599
329.620849	12786.976785	28.679616
330.298146	12805.046346	28.684634
330.867356	12827.308648	28.689652
330.911595	12853.214842	28.694669
331.612949	12871.672422	28.699687
331.720188	12905.238849	28.704704
331.671576	12920.838640	28.709722
332.363612	12930.097661	28.714740
332.399628	12970.917818	28.719757
333.068699	12999.020245	28.724775
333.362775	13006.065273	28.729792
333.825425	13032.674086	28.734810
333.999390	13062.122365	28.739828
334.498405	13074.146422	28.744845
334.900134	13104.680104	28.749863
334.908358	13129.914815	28.754880
335.610508	13142.290660	28.759898
336.136279	13172.709275	28.764916
336.299059	13183.508942	28.769933
337.023272	13207.890195	28.774951
336.865347	13224.612815	28.779968
337.079051	13241.735310	28.784986
337.377210	13257.339216	28.790004
337.874350	13289.411819	28.795021
338.328591	13318.965482	28.800039
338.395931	13338.109889	28.805056
339.057901	13356.150873	28.810074
339.488725	13365.947477	28.815092
339.803443	13394.528019	28.820109
340.275036	13416.217196	28.825127
340.716099	13431.377991	28.830144
340.676498	13439.458130	28.835162
340.865054	13465.229811	28.840180
341.047944	13497.132145	28.845197
341.978093	13501.711527	28.850215
342.104588	13529.443891	28.855232
342.187467	13549.600690	28.860250
343.061650	13562.874731	28.865268
343.160712	13586.750724	28.870285
343.717091	13599.078351	28.875303
344.109060	13610.070262	28.880320
344.292811	13634.537938	28.885338
344.774337	13651.024130	28.890356
345.114749	13677.525057	28.895373
345.514958	13689.542918	28.900391
345.859366	13714.904885	28.905408
346.132437	13725.584444	28.910426
346.541408	13743.974765	28.915444
346.647637	13764.361906	28.920461
347.148489	13783.499581	28.925479
347.395412	13790.831924	28.930496
348.053788	13803.340642	28.935514
348.150580	13820.839388	28.940532
348.075975	13829.162044	28.945549
348.769146	13849.115131	28.950567
348.901470	13861.887787	28.955584
349.046410	13886.238865	28.960602
349.755111	13899.858173	28.965620
349.492232	13925.797424	28.970637
349.902433	13943.569588	28.975655
349.970596	13971.299360	28.980672
350.781235	13996.219804	28.985690
351.513371	14014.861220	28.990708
351.587117	14037.816858	28.995725
352.296869	14059.687340	29.000743
352.553268	14088.282024	29.005760
352.410610	14108.856977	29.010778
352.970638	14124.312698	29.015796
352.799236	14152.834380	29.020813
353.198531	14172.414187	29.025831
354.039287	14205.755605	29.030848
354.220057	14217.573395	29.035866
355.141784	14233.830675	29.040884
355.364602	14258.064950	29.045901
355.657784	14277.594795	29.050919
355.999704	14299.401343	29.055936
356.386585	14320.616412	29.060954
357.211858	14327.110030	29.065972
357.745030	14336.632078	29.070989
357.632492	14361.903029	29.076007
357.802927	14379.566319	29.081024
358.353663	14395.632081	29.086042
358.864809	14402.927142	29.091060
359.355642	14431.181265	29.096077
359.455595	14446.362307	29.101095
359.578119	14474.002070	29.106112
359.709813	14495.114462	29.111130
360.694913	14496.449926	29.116148
361.038256	14514.895033	29.121165
361.292199	14528.821758	29.126183
361.809789	14552.157215	29.131200
361.701553	14563.537707	29.136218
362.246973	14587.684004	29.141236
362.296086	14624.645201	29.146253
362.617224	14647.272061	29.151271
363.054898	14662.775873	29.156288
363.041592	14688.715218	29.161306
363.596134	14707.644967	29.166324
363.745277	14730.567396	29.171341
364.227938	14756.497293	29.176359
364.844791	14795.216156	29.181376
365.242525	14814.763878	29.186394
365.440359	14827.766407	29.191412
365.846715	14867.405470	29.196429
366.116597	14879.299019	29.201447
366.791827	14899.572310	29.206464
366.993820	14932.061948	29.211482
367.776677	14937.848313	29.216500
368.039763	14952.677570	29.221517
368.566489	14975.719482	29.226535
368.716234	14994.055898	29.231552
369.057656	15010.534210	29.236570
369.391621	15007.613779	29.241588
369.565289	15032.682298	29.246605
369.652678	15044.809532	29.251623
370.645125	15060.916708	29.256640
370.562217	15091.624693	29.261658
371.235403	15105.207649	29.266676
371.409957	15127.709110	29.271693
371.687761	15154.633679	29.276711
372.099897	15174.496320	29.281728
372.505147	15204.793855	29.286746
372.709444	15219.072246	29.291764
372.616049	15252.161173	29.296781
373.392246	15276.685174	29.301799
373.741639	15299.524196	29.306816
373.952316	15336.066479	29.311834
374.530706	15355.774450	29.316852
375.056047	15373.588981	29.321869
375.433239	15407.118982	29.326887
375.877251	15430.279068	29.331904
376.241758	15459.701027	29.336922
376.740258	15480.126946	29.341940
376.889973	15507.120983	29.346957
377.538217	15527.845572	29.351975
378.224588	15542.383397	29.356992
378.136224	15583.809464	29.362010
378.498411	15587.283813	29.367028
379.000280	15613.671454	29.372045
379.201805	15655.499357	29.377063
379.470859	15663.778974	29.382080
379.647451	15690.581002	29.387098
380.421393	15719.814918	29.392116
380.877961	15752.223123	29.397133
381.213290	15768.159637	29.402151
381.636962	15789.012078	29.407168
382.194063	15823.836985	29.412186
382.461102	15838.864759	29.417204
382.874286	15852.281491	29.422221
383.431447	15880.883662	29.427239
383.690959	15902.407956	29.432256
383.865383	15926.363176	29.437274
384.361856	15933.942758	29.442292
384.591697	15969.722329	29.447309
384.907565	16006.563659	29.452327
385.614456	16019.545722	29.457344
385.794915	16052.783448	29.462362
386.233367	16078.283445	29.467380
386.862114	16096.692958	29.472397
386.873513	16114.676057	29.477415
387.417210	16140.372242	29.482432
387.611569	16159.922111	29.487450
387.930538	16173.655756	29.492468
388.202894	16205.206834	29.497485
388.589790	16231.465757	29.502503
389.191757	16248.711916	29.507520
389.466204	16267.275119	29.512538
389.653725	16278.768683	29.517556
390.103927	16309.821346	29.522573
390.563637	16346.119794	29.527591
390.739839	16368.625667	29.532608
391.047079	16392.773901	29.537626
391.768445	16414.580085	29.542644
392.276165	16449.378265	29.547661
392.189190	16467.808976	29.552679
392.859760	16501.496855	29.557696
393.389140	16528.047017	29.562714
393.725322	16553.795855	29.567732
394.050546	16577.726685	29.572749
394.508358	16618.151228	29.577767
394.974242	16626.698090	29.582784
395.232102	16660.588278	29.587802
395.676809	16679.118946	29.592820
396.248024	16707.394386	29.597837
396.332189	16741.632264	29.602855
397.229035	16769.033806	29.607872
397.736539	16782.086868	29.612890
397.800911	16804.556284	29.617908
398.323221	16830.797116	29.622925
398.703081	16849.341078	29.627943
399.660635	16868.305543	29.632960
399.555095	16887.838777	29.637978
400.018757	16905.922271	29.642996
400.443831	16929.661975	29.648013
400.499419	16967.900446	29.653031
401.117709	16971.554950	29.658048
401.483117	17004.639689	29.663066
401.932715	17030.533242	29.668084
402.531312	17050.526070	29.673101
402.912924	17075.033657	29.678119
403.335530	17106.211898	29.683136
403.674379	17123.047380	29.688154
404.296302	17137.189272	29.693172
404.324640	17157.762413	29.698189
404.629374	17191.901391	29.703207
405.046624	17209.095102	29.708224
405.616767	17245.201129	29.713242
405.980492	17258.747927	29.718260
406.421018	17283.671805	29.723277
406.688044	17313.537212	29.728295
406.859707	17331.900975	29.733312
407.293966	17374.922914	29.738330
407.504141	17400.037211	29.743348
408.342272	17423.172155	29.748365
408.674243	17445.537274	29.753383
409.316536	17460.788512	29.758400
409.719340	17483.926774	29.763418
409.737520	17499.012359	29.768436
409.858233	17534.392717	29.773453
410.580087	17560.537259	29.778471
410.731796	17580.892309	29.783488
411.313138	17609.896668	29.788506
411.505042	17641.823318	29.793524
412.116353	17661.048052	29.798541
411.988645	17690.817056	29.803559
412.778127	17734.889608	29.808576
413.278670	17759.813158	29.813594
413.848006	17781.231961	29.818612
414.550456	17808.558076	29.823629
414.985850	17822.878342	29.828647
415.131350	17842.823536	29.833664
415.457624	17860.336583	29.838682
415.769500	17894.751744	29.843700
416.479270	17911.003829	29.848717
416.426995	17960.368073	29.853735
417.079145	17977.942710	29.858752
417.319162	17987.347528	29.863770
417.832128	18054.895274	29.868788
418.031573	18061.899658	29.873805
418.483866	18116.968119	29.878823
418.854753	18120.948924	29.883840
419.615608	18169.153429	29.888858
419.827024	18213.302914	29.893876
420.579882	18230.638773	29.898893
420.686162	18258.425616	29.903911
421.153502	18288.252132	29.908928
421.649038	18328.184026	29.913946
422.223934	18365.806225	29.918964
422.799521	18385.186172	29.923981
423.300008	18399.199567	29.928999
423.552853	18435.867379	29.934016
423.518553	18473.964841	29.939034
424.566942	18498.087557	29.944052
425.144955	18513.808337	29.949069
424.981001	18566.540037	29.954087
425.487240	18560.794925	29.959104
426.176956	18609.973136	29.964122
426.499087	18638.721521	29.969140
427.324450	18643.312323	29.974157
427.120163	18706.782983	29.979175
427.910909	18703.633784	29.984192
428.407786	18747.717262	29.989210
428.908186	18776.639072	29.994228
429.556640	18780.255752	29.999245
429.727855	18817.776832	30.004263
430.158515	18847.950032	30.009280
430.588709	18870.231683	30.014298
430.873684	18897.554981	30.019316
431.515238	18925.154192	30.024333
431.691535	18953.752380	30.029351
432.069052	18966.173286	30.034368
432.489056	18995.303983	30.039386
432.825079	19022.685903	30.044404
433.401818	19028.110138	30.049421
433.333416	19061.363669	30.054439
433.753113	19106.937244	30.059456
434.488382	19120.337112	30.064474
434.772349	19144.286564	30.069492
435.551250	19191.099235	30.074509
436.145523	19212.974524	30.079527
436.402407	19227.594421	30.084544
436.667331	19253.375845	30.089562
437.018082	19301.461020	30.094580
437.429239	19318.222217	30.099597
438.053962	19359.090142	30.104615
438.267102	19371.193460	30.109632
438.588122	19406.588102	30.114650
438.935960	19449.266962	30.119668
439.563865	19479.180823	30.124685
439.709273	19507.912120	30.129703
440.450576	19534.337036	30.134720
440.774999	19564.584068	30.139738
441.153425	19614.986362	30.144756
442.267892	19630.130666	30.149773
442.640448	19663.632564	30.154791
442.873543	19684.829808	30.159808
443.358250	19710.587999	30.164826
443.625380	19745.335667	30.169844
444.150553	19772.447423	30.174861
444.943858	19812.268370	30.179879
445.128920	19832.530897	30.184896
445.647317	19862.546018	30.189914
445.867019	19907.730942	30.194932
446.365293	19927.695253	30.199949
446.696177	19971.522409	30.204967
447.085495	19989.476469	30.209984
447.926394	20026.021270	30.215002
448.056910	20060.130337	30.220020
448.782675	20073.311667	30.225037
449.139915	20121.448342	30.230055
449.667273	20151.427550	30.235072
450.108901	20181.062573	30.240090
450.614041	20199.250018	30.245108
451.101209	20221.324909	30.250125
451.682636	20277.520304	30.255143
452.360811	20294.031337	30.260160
452.477890	20306.731837	30.265178
452.709158	20349.157299	30.270196
453.269301	20379.862891	30.275213
453.506198	20406.388943	30.280231
453.909084	20452.967650	30.285248
454.531452	20485.244395	30.290266
454.637494	20524.499422	30.295284
455.319757	20555.728872	30.300301
455.869398	20570.417970	30.305319
456.179346	20623.889862	30.310336
456.845897	20633.474818	30.315354
457.124051	20662.626115	30.320372
457.535833	20680.999487	30.325389
457.981032	20713.868377	30.330407
458.376254	20748.735288	30.335424
458.883424	20770.041147	30.340442
459.103910	20789.501543	30.345460
459.710646	20831.985834	30.350477
460.287879	20856.506231	30.355495
460.552930	20893.234581	30.360512
460.933257	20931.022346	30.365530
461.688556	20943.804783	30.370548
462.008149	20993.746429	30.375565
462.301010	21042.412403	30.380583
462.786827	21075.205888	30.385600
463.480569	21100.170373	30.390618
463.732187	21138.830834	30.395636
464.173614	21168.847343	30.400653
464.894133	21203.635095	30.405671
465.232744	21230.918892	30.410688
465.712487	21268.018307	30.415706
466.094053	21313.784347	30.420724
466.776314	21337.740260	30.425741
467.174474	21394.005875	30.430759
467.661786	21408.587959	30.435776
468.097479	21426.424457	30.440794
468.335097	21501.057499	30.445812
468.994904	21513.584315	30.450829
469.734423	21554.036093	30.455847
470.334509	21573.495661	30.460864
470.571360	21633.324639	30.465882
471.160201	21632.960671	30.470900
471.943505	21688.199678	30.475917
472.399318	21725.958039	30.480935
472.553740	21743.553043	30.485952
473.584788	21756.472963	30.490970
473.702671	21790.105830	30.495988
473.591309	21834.355958	30.501005
474.330209	21862.268550	30.506023
474.793321	21896.356191	30.511040
475.596903	21927.049667	30.516058
475.950884	21971.646601	30.521076
476.598042	21992.338799	30.526093
477.011210	22017.312431	30.531111
477.367683	22048.308125	30.536128
477.964634	22091.008059	30.541146
478.676032	22116.387186	30.546164
478.699554	22139.379368	30.551181
479.779665	22182.499533	30.556199
479.633978	22186.577077	30.561216
480.494755	22219.147441	30.566234
480.978950	22259.423557	30.571252
481.687179	22273.653867	30.576269
482.345190	22297.609208	30.581287
482.359995	22327.665969	30.586304
483.089762	22327.708768	30.591322
483.465323	22380.200389	30.596340
483.790630	22382.245048	30.601357
483.869313	22397.862653	30.606375
484.380855	22448.343429	30.611392
485.239321	22463.569891	30.616410
485.280677	22496.413917	30.621428
485.792929	22533.539103	30.626445
486.108347	22546.889504	30.631463
486.230021	22593.235831	30.636480
487.079208	22618.853725	30.641498
487.175345	22652.273736	30.646516
487.894500	22705.309483	30.651533
488.832562	22727.795333	30.656551
489.044410	22769.029743	30.661568
489.582450	22803.977704	30.666586
490.058936	22831.408500	30.671604
490.682696	22866.768247	30.676621
491.330108	22906.856200	30.681639
491.209846	22946.137174	30.686656
491.815109	22981.260694	30.691674
492.336193	23008.732738	30.696692
492.519137	23050.752214	30.701709
493.335034	23096.147478	30.706727
493.862307	23143.749265	30.711744
494.375132	23173.914966	30.716762
494.862270	23209.817070	30.721780
495.375448	23255.432714	30.726797
495.870935	23293.439764	30.731815
496.532402	23324.565810	30.736832
497.417659	23354.637874	30.741850
497.791249	23400.351784	30.746868
498.301051	23422.831239	30.751885
498.790385	23455.428680	30.756903
499.015719	23497.154318	30.761920
499.933850	23540.132308	30.766938
500.244816	23563.970008	30.771956
500.864461	23593.350766	30.776973
501.249095	23617.432005	30.781991
501.334611	23662.046551	30.787008
502.057823	23707.834041	30.792026
502.828096	23753.614954	30.797044
503.152415	23776.900286	30.802061
503.802012	23792.880433	30.807079
504.002913	23863.036986	30.812096
504.793177	23876.089183	30.817114
505.237764	23906.460126	30.822132
505.819635	23959.922080	30.827149
506.655677	23983.531844	30.832167
506.802934	24013.280062	30.837184
507.323089	24025.045062	30.842202
507.831275	24091.825839	30.847220
507.937756	24120.666283	30.852237
508.648750	24141.999389	30.857255
509.191999	24175.332488	30.862272
509.595678	24206.244557	30.867290
509.927212	24241.981600	30.872308
510.394776	24280.591732	30.877325
510.885945	24316.629609	30.882343
511.079329	24360.086813	30.887360
511.923459	24386.247158	30.892378
512.557814	24411.868323	30.897396
513.117375	24462.308495	30.902413
513.435911	24487.021486	30.907431
514.146279	24526.560808	30.912448
514.730649	24562.779742	30.917466
515.100723	24606.528486	30.922484
515.331558	24639.967464	30.927501
515.866151	24659.415294	30.932519
516.320448	24715.702701	30.937536
516.917168	24757.811237	30.942554
517.407086	24799.472947	30.947572
517.974650	24845.197143	30.952589
518.417311	24869.953974	30.957607
519.201048	24921.306705	30.962624
519.688198	24968.405995	30.967642
520.095735	25009.507930	30.972660
520.843826	25049.730211	30.977677
521.539986	25076.439091	30.982695
521.552483	25114.926021	30.987712
522.060884	25158.117030	30.992730
522.802908	25200.173660	30.997748
523.307374	25238.269014	31.002765
523.844004	25273.124186	31.007783
524.441061	25317.237312	31.012800
524.989484	25357.589853	31.017818
525.693837	25397.738058	31.022836
526.183552	25434.843702	31.027853
526.679601	25478.337669	31.032871
527.247638	25530.787791	31.037888
527.734318	25561.435626	31.042906
528.702142	25592.145523	31.047924
529.249012	25629.962505	31.052941
529.618976	25680.094070	31.057959
530.242592	25698.763315	31.062976
530.456844	25752.456061	31.067994
531.101324	25777.632746	31.073012
531.468794	25809.421789	31.078029
532.225627	25838.962099	31.083047
532.485932	25902.799675	31.088064
532.617816	25926.384278	31.093082
533.826038	25954.386118	31.098100
533.756961	26018.114341	31.103117
534.189946	26053.929093	31.108135
534.841647	26098.932142	31.113152
535.317539	26138.595531	31.118170
536.259616	26178.896113	31.123188
536.850368	26244.949595	31.128205
537.506694	26258.377233	31.133223
537.992942	26283.593313	31.138240
538.579523	26322.782625	31.143258
539.478845	26351.669401	31.148276
539.441260	26382.436190	31.153293
539.968655	26399.420787	31.158311
540.333225	26435.643540	31.163328
540.958153	26458.553265	31.168346
541.377839	26504.720928	31.173364
541.769453	26570.060657	31.178381
542.826348	26592.626837	31.183399
542.783808	26625.981955	31.188416
543.182820	26670.283192	31.193434
543.955929	26701.092417	31.198452
544.292457	26746.622523	31.203469
544.944230	26801.435507	31.208487
545.633327	26839.049928	31.213504
545.689310	26874.370381	31.218522
546.410456	26938.438829	31.223540
546.989600	26976.661934	31.228557
547.865403	27016.681337	31.233575
548.797949	27050.664317	31.238592
548.901868	27093.283706	31.243610
549.795840	27135.308628	31.248628
549.999358	27183.189128	31.253645
550.849629	27225.035322	31.258663
551.295995	27288.625038	31.263680
551.754337	27313.168087	31.268698
552.569200	27358.265285	31.273716
552.652683	27396.194121	31.278733
553.329970	27448.078496	31.283751
554.089316	27474.013991	31.288768
554.467602	27514.113876	31.293786
555.370325	27572.452861	31.298804
556.121369	27599.917482	31.303821
556.237725	27636.002063	31.308839
557.368912	27688.837530	31.313856
557.897841	27717.139744	31.318874
558.499528	27754.491341	31.323892
558.872325	27789.403299	31.328909
559.339122	27817.163310	31.333927
559.912940	27873.386058	31.338944
560.298906	27898.189700	31.343962
560.827628	27951.420577	31.348980
561.462207	27993.065985	31.353997
561.882512	28033.485065	31.359015
562.285023	28065.204454	31.364032
562.751366	28131.795248	31.369050
563.771094	28161.750996	31.374068
563.773702	28206.631706	31.379085
564.461328	28267.542014	31.384103
564.983241	28290.533796	31.389120
565.395315	28345.902331	31.394138
566.456529	28402.809590	31.399156
566.764666	28436.112599	31.404173
567.632617	28482.093211	31.409191
568.247387	28525.520592	31.414208
568.410365	28557.397279	31.419226
569.652015	28583.235692	31.424244
569.976817	28633.116571	31.429261
570.559724	28667.036539	31.434279
570.970040	28696.811433	31.439296
571.301474	28728.039199	31.444314
572.015103	28771.752470	31.449332
572.207379	28813.361710	31.454349
572.894589	28846.687133	31.459367
573.845387	28897.575328	31.464384
574.077805	28943.551319	31.469402
574.618843	28975.753112	31.474420
575.130375	29026.837736	31.479437
575.815725	29064.235771	31.484455
576.467733	29110.340810	31.489472
576.869262	29166.988663	31.494490
577.316206	29216.323988	31.499508
578.206477	29249.507595	31.504525
578.929580	29294.916355	31.509543
579.461496	29339.742693	31.514560
579.694045	29387.998573	31.519578
580.680562	29426.663728	31.524596
581.147337	29475.493991	31.529613
581.446651	29520.992939	31.534631
582.234935	29558.689317	31.539648
582.812748	29620.094962	31.544666
583.599623	29656.250603	31.549684
583.981684	29701.842463	31.554701
584.337956	29766.831216	31.559719
585.324393	29809.364487	31.564736
585.833116	29846.324424	31.569754
586.535603	29882.448309	31.574772
587.174954	29940.436731	31.579789
587.569530	29981.844976	31.584807
588.346767	30020.349469	31.589824
588.641236	30073.216473	31.594842
589.162645	30121.726372	31.599860
589.531015	30170.870667	31.604877
590.373130	30227.946888	31.609895
591.100794	30275.165241	31.614912
591.318261	30335.237860	31.619930
592.225603	30378.380920	31.624948
592.832577	30439.958368	31.629965
592.976671	30478.359906	31.634983
593.996964	30523.824059	31.640000
594.387369	30571.587102	31.645018
595.218780	30626.482161	31.650036
596.155527	30675.548492	31.655053
596.943457	30722.534760	31.660071
597.301118	30764.568652	31.665088
597.740258	30804.933330	31.670106
598.608115	30852.616431	31.675124
599.062179	30901.128345	31.680141
599.373163	30948.698685	31.685159
600.470655	30974.455152	31.690176
600.635811	31025.245043	31.695194
601.228776	31068.748894	31.700212
601.915423	31110.553197	31.705229
602.329462	31153.300920	31.710247
603.358453	31182.012604	31.715264
603.621785	31220.606507	31.720282
604.024826	31251.731582	31.725300
604.962999	31287.666607	31.730317
605.053815	31346.538547	31.735335
606.240141	31385.397195	31.740352
606.438969	31433.160169	31.745370
606.977284	31484.467310	31.750388
607.736494	31527.096425	31.755405
608.025456	31590.843904	31.760423
608.577220	31639.008327	31.765440
608.917338	31701.523497	31.770458
609.840029	31742.519561	31.775476
610.402854	31791.160216	31.780493
610.968243	31854.374543	31.785511
611.879798	31897.502042	31.790528
612.428265	31954.378894	31.795546
613.000335	32005.023489	31.800564
613.704422	32062.332999	31.805581
614.404052	32119.019284	31.810599
615.160567	32157.188538	31.815616
615.554977	32219.905083	31.820634
616.255178	32265.899475	31.825652
617.021638	32311.163161	31.830669
617.090957	32364.484789	31.835687
618.012468	32422.125016	31.840704
618.687730	32472.708914	31.845722
619.293717	32522.452885	31.850740
620.203466	32567.180639	31.855757
620.999037	32628.660636	31.860775
621.469348	32680.984779	31.865792
622.105550	32723.110160	31.870810
622.583528	32758.902619	31.875828
623.622343	32804.970694	31.880845
623.729019	32881.672024	31.885863
624.628742	32915.802580	31.890880
625.002484	32952.053387	31.895898
625.401709	33028.440862	31.900916
626.451234	33075.543544	31.905933
626.883991	33110.976718	31.910951
627.463006	33167.197206	31.915968
627.948690	33241.792375	31.920986
628.619211	33289.800869	31.926004
629.395845	33336.993466	31.931021
630.209487	33397.023339	31.936039
630.779098	33442.909418	31.941056
631.226357	33495.766278	31.946074
631.811724	33554.701342	31.951092
632.909284	33599.241223	31.956109
633.385365	33639.203474	31.961127
634.066001	33674.391899	31.966144
634.834988	33724.608488	31.971162
635.196675	33764.407989	31.976180
636.177130	33806.772932	31.981197
636.495529	33861.716382	31.986215
636.993293	33900.838817	31.991232
637.769358	33931.745640	31.996250
638.404596	33979.151743	32.001268
638.978634	34025.771706	32.006285
639.474056	34077.071697	32.011303
640.150166	34120.398577	32.016320
640.865411	34180.729125	32.021338
641.259947	34222.468069	32.026356
641.944920	34260.995656	32.031373
642.347726	34324.663069	32.036391
643.077926	34372.200198	32.041408
643.857456	34431.138996	32.046426
644.234445	34488.403417	32.051444
645.095624	34538.087611	32.056461
645.574808	34599.262776	32.061479
646.525446	34642.629280	32.066496
647.345964	34699.798585	32.071514
647.822842	34759.557575	32.076532
648.766744	34789.774061	32.081549
649.134547	34842.521765	32.086567
649.905036	34893.067969	32.091584
650.410596	34949.996661	32.096602
651.025535	35003.646616	32.101620
651.827184	35057.454604	32.106637
652.268890	35117.614577	32.111655
652.913922	35167.525819	32.116672
653.205479	35231.211269	32.121690
654.074242	35285.499567	32.126708
655.335877	35338.949896	32.131725
655.677696	35402.793521	32.136743
656.200095	35466.242909	32.141760
657.125373	35516.159443	32.146778
657.469694	35567.604756	32.151796
658.589754	35631.317458	32.156813
658.908424	35682.253292	32.161831
659.590588	35733.799814	32.166848
660.174515	35792.664239	32.171866
661.087314	35852.918961	32.176884
661.797635	35890.129959	32.181901
662.145889	35959.020926	32.186919
662.708135	36021.215947	32.191936
663.575113	36073.386751	32.196954
664.012642	36142.404566	32.201972
664.825361	36185.722969	32.206989
665.512898	36246.412255	32.212007
666.360149	36292.809052	32.217024
667.155670	36360.977793	32.222042
667.489991	36405.465454	32.227060
668.693440	36458.666949	32.232077
669.326601	36518.079448	32.237095
669.912377	36563.137603	32.242112
670.549210	36610.844194	32.247130
670.900178	36646.124523	32.252148
671.991603	36683.251387	32.257165
672.544610	36737.359790	32.262183
673.126083	36772.959983	32.267200
673.921436	36814.370442	32.272218
674.248930	36876.617060	32.277236
674.781796	36923.101927	32.282253
675.381280	36968.352908	32.287271
676.125660	37029.168416	32.292288
676.765838	37084.162701	32.297306
677.379284	37151.356226	32.302324
678.402600	37190.831549	32.307341
679.038546	37228.870889	32.312359
680.059545	37280.492787	32.317376
680.606728	37341.019201	32.322394
681.177163	37393.400580	32.327412
682.276235	37427.693162	32.332429
682.562246	37480.203656	32.337447
683.273855	37551.346742	32.342464
684.110683	37590.333995	32.347482
684.564759	37655.324001	32.352500
685.360883	37694.447261	32.357517
686.140396	37757.515969	32.362535
686.635323	37801.245476	32.367552
687.246815	37857.935443	32.372570
687.380475	37923.414229	32.377588
688.181489	37977.315290	32.382605
688.868557	38041.375729	32.387623
689.799282	38098.182804	32.392640
690.424102	38167.940662	32.397658
691.015404	38225.705640	32.402676
691.610441	38281.510408	32.407693
692.052697	38363.222580	32.412711
692.969987	38419.495229	32.417728
693.688429	38486.533893	32.422746
694.270113	38562.591284	32.427764
694.924312	38613.723833	32.432781
695.715079	38684.455465	32.437799
696.537643	38747.644011	32.442816
697.526504	38807.553523	32.447834
697.818390	38879.535333	32.452852
698.544631	38936.034061	32.457869
699.501587	39008.607454	32.462887
700.105251	39057.559290	32.467904
701.172551	39129.164851	32.472922
701.733974	39194.118466	32.477940
702.568092	39242.324603	32.482957
703.398305	39307.535445	32.487975
704.012026	39357.284397	32.492992
705.083445	39406.694149	32.498010
705.778662	39474.560360	32.503028
706.356584	39520.704640	32.508045
707.080634	39573.211823	32.513063
707.715240	39631.974408	32.518080
708.582620	39669.242896	32.523098
708.847972	39737.148636	32.528116
709.520992	39764.807627	32.533133
710.398990	39810.632133	32.538151
710.752240	39863.561920	32.543168
711.511134	39922.414525	32.548186
712.569763	39974.063923	32.553204
713.047617	40033.975565	32.558221
713.796595	40085.710868	32.563239
714.029301	40148.926021	32.568256
715.008672	40188.953089	32.573274
715.329167	40265.676261	32.578292
715.956284	40329.694993	32.583309
717.020918	40389.541278	32.588327
717.511741	40459.381949	32.593344
718.270150	40519.033025	32.598362
719.042751	40576.889123	32.603380
719.789696	40646.535251	32.608397
720.477413	40713.581312	32.613415
720.716180	40773.790658	32.618432
722.077348	40843.688305	32.623450
722.570913	40929.107272	32.628468
723.264004	41001.579816	32.633485
724.073775	41074.582867	32.638503
724.697998	41129.512432	32.643520
725.567073	41196.406942	32.648538
726.059759	41268.404745	32.653556
726.856312	41338.067877	32.658573
727.871269	41400.675853	32.663591
728.303744	41475.257727	32.668608
729.278686	41544.331898	32.673626
730.090357	41620.673878	32.678644
730.674501	41688.350552	32.683661
731.939244	41757.975557	32.688679
732.292356	41821.065764	32.693696
733.042007	41887.969378	32.698714
733.918789	41945.740991	32.703732
734.691630	42020.624308	32.708749
735.397879	42083.119919	32.713767
736.102756	42157.551007	32.718784
737.107188	42207.897408	32.723802
738.182084	42270.946912	32.728820
738.682328	42326.647582	32.733837
739.713707	42379.299007	32.738855
740.520213	42441.407779	32.743872
741.254675	42499.383703	32.748890
741.880740	42560.275744	32.753908
742.526982	42612.768407	32.758925
743.100156	42660.213572	32.763943
743.856549	42728.087723	32.768960
744.894869	42799.844236	32.773978
745.440802	42851.634441	32.778996
746.227601	42910.407743	32.784013
747.085996	42956.770585	32.789031
747.657572	43014.058168	32.794048
748.499285	43054.922944	32.799066
748.972267	43111.352820	32.804084
750.029529	43169.254385	32.809101
750.623329	43221.217877	32.814119
750.615915	43276.428361	32.819136
751.590190	43340.623893	32.824154
752.020243	43393.147046	32.829172
752.470009	43487.237984	32.834189
753.646109	43531.397399	32.839207
754.062904	43604.019555	32.844224
755.141667	43683.602399	32.849242
755.576619	43737.343402	32.854260
756.304646	43829.839962	32.859277
757.368711	43876.298718	32.864295
757.850947	43954.479434	32.869312
758.752404	44028.095564	32.874330
759.429273	44106.990430	32.879348
759.878992	44172.868707	32.884365
760.870462	44250.537539	32.889383
761.654190	44326.432275	32.894400
762.358607	44395.636681	32.899418
763.173883	44482.867467	32.904436
763.818267	44562.984066	32.909453
764.493269	44632.433843	32.914471
765.147550	44719.735613	32.919488
766.498566	44804.526292	32.924506
767.078788	44879.648277	32.929524
767.540285	44960.985100	32.934541
768.749041	45031.020283	32.939559
769.776640	45109.488484	32.944576
770.566604	45187.108416	32.949594
771.413337	45257.558614	32.954612
771.862654	45326.580206	32.959629
772.839271	45404.729773	32.964647
773.350107	45485.253599	32.969664
774.237416	45562.004789	32.974682
775.289588	45631.644591	32.979700
775.585465	45704.051872	32.984717
777.133548	45772.524920	32.989735
777.609239	45863.211189	32.994752
777.858040	45929.348940	32.999770
778.839444	46010.175704	33.004788
779.680599	46083.005682	33.009805
780.472762	46164.784485	33.014823
780.925217	46243.888823	33.019840
781.731930	46338.127675	33.024858
782.798091	46390.366199	33.029876
783.267859	46488.833361	33.034893
784.372419	46550.666515	33.039911
785.236957	46648.491241	33.044928
785.862447	46720.459060	33.049946
786.905771	46798.730453	33.054964
787.506636	46888.310511	33.059981
788.268359	46962.084347	33.064999
788.960291	47025.805269	33.070016
789.824608	47089.521068	33.075034
790.822710	47164.905031	33.080052
791.406719	47235.704758	33.085069
791.850333	47314.717535	33.090087
792.885974	47384.994811	33.095104
793.703648	47434.414400	33.100122
794.172507	47540.488097	33.105140
795.203096	47598.736811	33.110157
796.079513	47677.452011	33.115175
796.416233	47752.126604	33.120192
797.312201	47838.193935	33.125210
798.388450	47902.456339	33.130228
798.736478	48003.131561	33.135245
799.689499	48075.472436	33.140263
800.794518	48149.155602	33.145280
801.030968	48250.105562	33.150298
802.229752	48318.502204	33.155316
802.864329	48415.032415	33.160333
803.839911	48486.506860	33.165351
804.156323	48575.970408	33.170368
805.152343	48676.868169	33.175386
806.110234	48757.925897	33.180404
806.788747	48847.061829	33.185421
807.774925	48932.100985	33.190439
808.704636	49033.708661	33.195456
809.496622	49098.800039	33.200474
810.397207	49195.270086	33.205492
811.069246	49264.681910	33.210509
812.211248	49330.541982	33.215527
812.855106	49446.365163	33.220544
813.667143	49534.101240	33.225562
814.819554	49594.085262	33.230580
815.454572	49699.911977	33.235597
816.191146	49767.699915	33.240615
816.944244	49858.517233	33.245632
817.723178	49947.163085	33.250650
818.934406	50024.062074	33.255668
820.121864	50111.116463	33.260685
820.811049	50200.225946	33.265703
821.565351	50262.153134	33.270720
822.183482	50343.098639	33.275738
823.282282	50446.230561	33.280756
823.954402	50488.518721	33.285773
824.624546	50591.726021	33.290791
825.790416	50653.655336	33.295808
826.296029	50764.630536	33.300826
827.302002	50811.293676	33.305844
827.913507	50919.577006	33.310861
828.839476	51002.445641	33.315879
829.472866	51070.188696	33.320896
829.977299	51164.491947	33.325914
831.184664	51258.519723	33.330932
831.889208	51330.619953	33.335949
832.821905	51418.128369	33.340967
833.817020	51503.506610	33.345984
834.322946	51538.887355	33.351002
835.265329	51653.651751	33.356020
836.142420	51747.810405	33.361037
837.300943	51781.598230	33.366055
837.957154	51867.827411	33.371072
839.171074	51910.140013	33.376090
839.824246	52007.150670	33.381108
840.703834	52049.510500	33.386125
841.221916	52150.324146	33.391143
842.074826	52225.724349	33.396160
842.894390	52302.357821	33.401178
843.442079	52389.140127	33.406196
844.348966	52443.173433	33.411213
844.820967	52546.044828	33.416231
845.662372	52621.659973	33.421248
846.158610	52744.512168	33.426266
847.536398	52792.563595	33.431284
848.225243	52924.339897	33.436301
848.812487	52994.366739	33.441319
849.193386	53103.416370	33.446336
850.665458	53199.712955	33.451354
851.744625	53283.685000	33.456372
851.890553	53387.623034	33.461389
852.855889	53488.776972	33.466407
854.056687	53583.240896	33.471424
854.738027	53688.237966	33.476442
855.854302	53772.742926	33.481460
856.521046	53880.148425	33.486477
857.829530	53972.981288	33.491495
858.675577	54087.928035	33.496512
859.434321	54179.230307	33.501530
860.260200	54267.432393	33.506548
861.133766	54367.829419	33.511565
862.242813	54455.362417	33.516583
863.460566	54542.768068	33.521600
863.984342	54651.138307	33.526618
864.937158	54727.034919	33.531636
865.707330	54821.422334	33.536653
866.433517	54914.662012	33.541671
867.128600	55021.754126	33.546688
868.447402	55108.988605	33.551706
869.610576	55182.413757	33.556724
870.543589	55277.904463	33.561741
871.456381	55370.141447	33.566759
872.586578	55451.659721	33.571776
873.369753	55554.776453	33.576794
874.266105	55628.807720	33.581812
875.026155	55714.584193	33.586829
875.863427	55801.715548	33.591847
876.791763	55876.626555	33.596864
877.802239	55949.760295	33.601882
878.644334	56062.283307	33.606900
879.534791	56131.128178	33.611917
880.122402	56219.945830	33.616935
880.794309	56292.620300	33.621952
881.355379	56365.565224	33.626970
882.269577	56449.016293	33.631988
882.993933	56557.514300	33.637005
883.888559	56626.256204	33.642023
884.769207	56705.089287	33.647040
885.477721	56810.491468	33.652058
886.615025	56894.385723	33.657076
887.251989	56981.838679	33.662093
888.003456	57073.964726	33.667111
889.346939	57169.766181	33.672128
889.769390	57264.161574	33.677146
890.978799	57356.613919	33.682164
891.743640	57452.556280	33.687181
892.662474	57543.281686	33.692199
894.179512	57628.959293	33.697216
894.736321	57720.788092	33.702234
895.637964	57817.869149	33.707252
896.144280	57917.163454	33.712269
897.163278	57996.125280	33.717287
898.439003	58100.415451	33.722304
899.044797	58195.736669	33.727322
899.671161	58293.804798	33.732340
900.776976	58394.168026	33.737357
901.626595	58493.076163	33.742375
902.851200	58586.728759	33.747392
903.642453	58689.009422	33.752410
904.518124	58782.387049	33.757428
905.448540	58886.540872	33.762445
906.080016	58986.780745	33.767463
907.294089	59082.278090	33.772480
907.836357	59187.603501	33.777498
908.889862	59292.734504	33.782516
909.841807	59385.285341	33.787533
910.541645	59493.583524	33.792551
911.732530	59603.935284	33.797568
912.394727	59712.556448	33.802586
913.553699	59812.098035	33.807604
914.535364	59908.384869	33.812621
915.257707	60012.224510	33.817639
916.341621	60108.376134	33.822656
917.106312	60227.611283	33.827674
917.957553	60338.422417	33.832692
918.949592	60440.011429	33.837709
920.527610	60539.231329	33.842727
921.254182	60652.135364	33.847744
922.077177	60745.976421	33.852762
923.164732	60841.638702	33.857780
924.270120	60928.795800	33.862797
924.508680	61053.509591	33.867815
925.999870	61140.101103	33.872832
926.839950	61248.803942	33.877850
927.891131	61342.911644	33.882868
928.826386	61443.713155	33.887885
929.617389	61539.239898	33.892903
930.912963	61619.527682	33.897920
931.420977	61701.690384	33.902938
932.172983	61802.061982	33.907956
933.077892	61889.691191	33.912973
933.714593	61977.928688	33.917991
934.896261	62091.495224	33.923008
936.061907	62166.450770	33.928026
936.625996	62284.559467	33.933044
937.499536	62383.383389	33.938061
937.895246	62477.872629	33.943079
939.136775	62570.491051	33.948096
939.703406	62678.604666	33.953114
940.561468	62797.831829	33.958132
941.848349	62891.467707	33.963149
942.306137	63010.333607	33.968167
943.382078	63109.069131	33.973184
944.197915	63236.809602	33.978202
945.209883	63360.957741	33.983220
946.405302	63469.897913	33.988237
947.208940	63597.033298	33.993255
948.289318	63709.466766	33.998272
949.167657	63816.570987	34.003290
950.057674	63939.911805	34.008308
951.442585	64047.381994	34.013325
951.936644	64155.761907	34.018343
953.322411	64286.020898	34.023360
954.364185	64381.781078	34.028378
955.278362	64500.034215	34.033396
956.606153	64622.589793	34.038413
957.267850	64705.840081	34.043431
958.401586	64848.591921	34.048448
959.318495	64934.379562	34.053466
960.325567	65077.863832	34.058484
961.437953	65149.381583	34.063501
962.275039	65308.653496	34.068519
963.433234	65392.213077	34.073536
964.151409	65524.418466	34.078554
965.360681	65626.844058	34.083572
966.619569	65715.795817	34.088589
967.243921	65852.629344	34.093607
968.767284	65935.678424	34.098624
969.262199	66044.728993	34.103642
970.207750	66167.437417	34.108660
971.896712	66269.205854	34.113677
972.608534	66362.384991	34.118695
973.606929	66484.644877	34.123712
974.935786	66557.159906	34.128730
975.495024	66682.917698	34.133748
976.571273	66786.573980	34.138765
977.648237	66873.737687	34.143783
978.889912	66976.623301	34.148800
979.537405	67090.838445	34.153818
980.381713	67195.569789	34.158836
981.579170	67274.191557	34.163853
982.216607	67393.795230	34.168871
983.159602	67487.836882	34.173888
984.340587	67554.441275	34.178906
985.276286	67675.603753	34.183924
986.491803	67740.507180	34.188941
987.304773	67839.119488	34.193959
988.292799	67935.941982	34.198976
989.195927	68028.148018	34.203994
989.775271	68119.231014	34.209012
990.859631	68224.365630	34.214029
990.982579	68312.268790	34.219047
992.213775	68436.174911	34.224064
993.359124	68525.438844	34.229082
993.781632	68669.709369	34.234100
995.254064	68755.150881	34.239117
996.364639	68900.848778	34.244135
997.234026	69006.634621	34.249152
998.378601	69103.930803	34.254170
998.702676	69253.610117	34.259188
1000.469495	69332.411851	34.264205
1001.016149	69484.218127	34.269223
1002.143030	69575.675710	34.274240
1003.195273	69713.599341	34.279258
1004.587635	69839.699948	34.284276
1005.508972	69941.527717	34.289293
1006.294892	70068.983508	34.294311
1007.321351	70170.751523	34.299328
1008.355835	70281.970293	34.304346
1009.341260	70430.510966	34.309364
1010.622414	70532.695236	34.314381
1011.304790	70648.015573	34.319399
1012.280356	70770.189210	34.324416
1013.745792	70902.975816	34.329434
1014.765949	70993.408213	34.334452
1015.880342	71147.177801	34.339469
1016.949511	71245.450679	34.344487
1017.915979	71375.925275	34.349504
1019.185302	71473.339767	34.354522
1020.063452	71603.747786	34.359540
1021.358523	71713.404190	34.364557
1022.182122	71817.260145	34.369575
1022.793382	71967.615813	34.374592
1024.207037	72057.478715	34.379610
1025.067623	72193.573685	34.384628
1026.609565	72297.077794	34.389645
1027.217275	72442.357566	34.394663
1028.062252	72526.228309	34.399680
1029.216714	72659.594346	34.404698
1029.968515	72784.065483	34.409716
1031.280445	72893.643616	34.414733
1032.177668	73026.149466	34.419751
1032.902282	73142.469700	34.424768
1034.172329	73272.971713	34.429786
1035.266762	73393.695669	34.434804
1036.378867	73512.964204	34.439821
1037.279978	73629.764725	34.444839
1038.184049	73732.215115	34.449856
1039.043983	73864.517638	34.454874
1039.842428	73972.110768	34.459892
1041.193695	74067.307015	34.464909
1042.087397	74198.475270	34.469927
1043.044155	74313.735405	34.474944
1044.144292	74437.668582	34.479962
1044.829551	74560.651125	34.484980
1045.978352	74663.958381	34.489997
1046.911312	74806.682285	34.495015
1047.935323	74921.947867	34.500032
1049.098053	75031.972252	34.505050
1049.919874	75199.924585	34.510068
1051.305502	75297.547883	34.515085
1052.278436	75432.237867	34.520103
1053.579428	75570.485025	34.525120
1054.549808	75689.321441	34.530138
1055.325396	75813.188351	34.535156
1056.322104	75945.242713	34.540173
1057.296530	76092.550902	34.545191
1059.029835	76213.525193	34.550208
1060.094407	76340.951629	34.555226
1060.709499	76493.230362	34.560244
1062.024459	76591.319888	34.565261
1063.045108	76739.655582	34.570279
1064.066572	76871.339191	34.575296
1065.509314	76994.405719	34.580314
1066.490682	77130.078974	34.585332
1067.961834	77257.060993	34.590349
1068.261363	77388.723751	34.595367
1069.513749	77512.601076	34.600384
1071.255804	77642.190557	34.605402
1071.938912	77781.644512	34.610420
1073.257494	77910.234941	34.615437
1074.111833	78033.508806	34.620455
1075.204800	78161.953421	34.625472
1076.256688	78292.769202	34.630490
1077.251363	78434.345959	34.635508
1078.504615	78563.229000	34.640525
1079.342714	78690.794695	34.645543
1080.673324	78827.833193	34.650560
1081.712936	78968.679644	34.655578
1082.315184	79118.995406	34.660596
1083.706905	79231.408032	34.665613
1085.230752	79367.161596	34.670631
1085.868927	79497.646361	34.675648
1087.363102	79647.527063	34.680666
1088.263897	79779.602616	34.685684
1089.765181	79897.146631	34.690701
1090.680572	80029.979976	34.695719
1091.587730	80161.715641	34.700736
1093.225136	80280.542317	34.705754
1094.276051	80418.015182	34.710772
1095.254324	80535.898872	34.715789
1096.469571	80655.964254	34.720807
1097.354161	80780.589899	34.725824
1098.483850	80880.891347	34.730842
1098.975753	81000.321554	34.735860
1100.456372	81138.261856	34.740877
1101.621820	81236.296333	34.745895
1102.488959	81371.984245	34.750912
1103.434233	81486.863334	34.755930
1104.492570	81616.934360	34.760948
1105.434749	81735.292088	34.765965
1106.743063	81867.651217	34.770983
1107.631293	81999.230917	34.776000
1108.656879	82140.695485	34.781018
1109.768697	82266.381232	34.786036
1110.560526	82387.819917	34.791053
1112.111516	82541.012460	34.796071
1112.795032	82689.489005	34.801088
1114.054594	82803.819648	34.806106
1114.967763	82984.774600	34.811124
1116.343496	83097.280337	34.816141
1117.541448	83247.581910	34.821159
1118.214623	83400.661165	34.826176
1119.519111	83522.973209	34.831194
1120.593692	83672.500881	34.836212
1121.651511	83825.825525	34.841229
1123.088490	83966.699652	34.846247
1123.963070	84115.446733	34.851264
1125.263168	84259.328648	34.856282
1126.459171	84399.750869	34.861300
1127.494669	84542.507185	34.866317
1128.881622	84688.875525	34.871335
1130.003907	84837.284840	34.876352
1131.210479	84986.472097	34.881370
1132.316658	85120.407638	34.886388
1133.653371	85283.068417	34.891405
1134.701365	85405.135034	34.896423
1135.761970	85575.435340	34.901440
1137.200177	85719.646667	34.906458
1138.360301	85855.936626	34.911476
1139.325428	85991.822203	34.916493
1140.376626	86151.114460	34.921511
1141.663650	86291.604318	34.926528
1142.890087	86415.817095	34.931546
1144.018657	86596.294553	34.936564
1145.152156	86717.431975	34.941581
1146.444099	86869.698165	34.946599
1147.051094	87031.894016	34.951616
1149.000497	87154.168778	34.956634
1149.897484	87302.005163	34.961652
1150.579147	87456.731101	34.966669
1152.334104	87589.542029	34.971687
1153.269021	87733.075592	34.976704
1154.456011	87901.793578	34.981722
1155.078151	88028.754960	34.986740
1156.523810	88180.563402	34.991757
1157.954569	88308.023863	34.996775
1158.558397	88480.057732	35.001792
1160.067926	88589.523455	35.006810
1160.916194	88736.555412	35.011828
1162.113251	88879.637592	35.016845
1163.127027	88997.095002	35.021863
1164.118085	89157.019915	35.026880
1165.467611	89278.573781	35.031898
1166.642315	89450.651081	35.036916
1167.842882	89590.973943	35.041933
1169.033088	89717.975089	35.046951
1169.709416	89894.555507	35.051968
1171.245767	90007.458014	35.056986
1172.173274	90177.278491	35.062004
1173.409787	90328.098158	35.067021
1174.537326	90482.787535	35.072039
1175.783534	90602.271999	35.077056
1177.170435	90807.034412	35.082074
1178.050915	90929.551165	35.087092
1179.477726	91097.984003	35.092109
1180.834997	91235.870392	35.097127
1181.661984	91407.348093	35.102144
1183.341100	91543.914067	35.107162
1184.351216	91703.032505	35.112180
1185.348022	91861.939183	35.117197
1186.815719	92009.957284	35.122215
1187.944208	92175.144471	35.127232
1189.329698	92319.237553	35.132250
1190.398909	92487.149747	35.137268
1191.426323	92630.656695	35.142285
1192.812314	92772.817325	35.147303
1193.813132	92953.564107	35.152320
1195.554553	93075.083137	35.157338
1196.651393	93248.802889	35.162356
1197.686739	93406.949286	35.167373
1199.385439	93552.493302	35.172391
1200.551199	93707.743276	35.177408
1202.021971	93870.542175	35.182426
1203.328303	94005.038518	35.187444
1204.499599	94137.128316	35.192461
1206.221930	94284.710064	35.197479
1207.018202	94441.826584	35.202496
1208.286324	94578.679115	35.207514
1209.674489	94706.714985	35.212532
1210.504512	94847.958971	35.217549
1211.604685	95017.460418	35.222567
1213.032868	95161.558890	35.227584
1214.260768	95304.444029	35.232602
1215.522060	95459.178677	35.237620
1216.702722	95590.238226	35.242637
1218.008964	95736.238462	35.247655
1219.152023	95887.224849	35.252672
1220.144129	96030.221691	35.257690
1221.575009	96162.971701	35.262708
1222.665957	96310.142197	35.267725
1223.792334	96455.568444	35.272743
1224.993643	96612.952095	35.277760
1226.245733	96731.734939	35.282778
1226.992511	96877.521577	35.287796
1228.320982	97009.793125	35.292813
1229.381677	97141.703162	35.297831
1230.233856	97308.933392	35.302848
1231.187586	97438.515230	35.307866
1232.815304	97618.763583	35.312884
1233.518654	97745.730040	35.317901
1234.793458	97931.610284	35.322919
1236.110276	98065.597918	35.327936
1237.120208	98243.621420	35.332954
1238.457739	98410.554864	35.337972
1239.386831	98563.351862	35.342989
1241.006994	98722.454955	35.348007
1241.852380	98895.163927	35.353024
1243.080817	99090.854307	35.358042
1244.539069	99228.293207	35.363060
1245.619369	99411.704826	35.368077
1247.113668	99579.887214	35.373095
1248.686526	99757.655884	35.378112
1250.002967	99926.451145	35.383130
1251.213168	100093.024868	35.388148
1252.515461	100264.134124	35.393165
1253.698978	100430.992917	35.398183
1254.786633	100608.339159	35.403200
1256.051722	100788.891624	35.408218
1257.679615	100953.317278	35.413236
1258.807111	101117.342801	35.418253
1259.984223	101303.278595	35.423271
1261.409816	101470.726474	35.428288
1262.709865	101641.080714	35.433306
1264.106079	101796.210289	35.438324
1265.354375	102003.595978	35.443341
1266.867149	102146.016860	35.448359
1268.210030	102352.966699	35.453376
1269.084882	102514.112691	35.458394
1270.920220	102663.148225	35.463412
1271.959184	102842.170757	35.468429
1273.385539	102998.790521	35.473447
1274.729884	103173.337767	35.478464
1276.053992	103349.509407	35.483482
1277.329183	103490.989162	35.488500
1278.173202	103705.142587	35.493517
1279.741777	103833.137672	35.498535
1280.760865	104038.685859	35.503552
1282.201083	104183.737759	35.508570
1283.292002	104373.242659	35.513588
1284.907528	104547.693736	35.518605
1286.130265	104692.732721	35.523623
1287.262345	104895.992344	35.528640
1288.821124	105051.377102	35.533658
1290.002215	105237.311886	35.538676
1291.327152	105395.792571	35.543693
1292.251107	105566.298407	35.548711
1293.969587	105723.472064	35.553728
1294.956336	105875.554877	35.558746
1296.433209	106046.343309	35.563764
1297.661272	106167.412343	35.568781
1298.909035	106366.881800	35.573799
1299.923598	106494.821155	35.578816
1301.067055	106692.183544	35.583834
1302.536204	106832.734823	35.588852
1303.691556	107005.929134	35.593869
1305.309211	107176.336219	35.598887
1306.450361	107323.467366	35.603904
1307.301141	107515.965673	35.608922
1309.306074	107678.587373	35.613940
1310.067745	107834.186601	35.618957
1311.421148	108024.716768	35.623975
1312.841165	108203.409089	35.628992
1313.903093	108363.679060	35.634010
1315.706002	108556.692558	35.639028
1316.629419	108738.828487	35.644045
1318.223484	108903.802233	35.649063
1319.219025	109083.701447	35.654080
1320.452272	109272.735228	35.659098
1322.100204	109439.058507	35.664116
1323.626918	109643.713427	35.669133
1324.574522	109816.517883	35.674151
1326.041183	109999.627597	35.679168
1327.518096	110177.129172	35.684186
1328.865574	110355.912180	35.689204
1330.242056	110542.736724	35.694221
1331.818099	110735.911197	35.699239
1333.548946	110903.041477	35.704256
1334.378851	111096.552595	35.709274
1335.857098	111277.758477	35.714292
1337.110082	111445.816591	35.719309
1338.241931	111652.051235	35.724327
1339.560737	111818.784832	35.729344
1340.664193	112018.583255	35.734362
1342.390806	112215.214218	35.739380
1343.475406	112384.850008	35.744397
1344.579709	112601.364234	35.749415
1346.765738	112775.132084	35.754432
1347.609707	112958.622347	35.759450
1349.205934	113159.307510	35.764468
1350.424664	113360.921537	35.769485
1351.603191	113536.848880	35.774503
1353.335364	113729.629482	35.779520
1354.034900	113924.759685	35.784538
1355.839890	114113.068746	35.789556
1357.026419	114304.180642	35.794573
1358.458074	114493.919293	35.799591
1360.078002	114693.568488	35.804608
1361.385330	114900.340285	35.809626
1362.936545	115079.169322	35.814644
1364.821305	115272.431347	35.819661
1366.014363	115430.276434	35.824679
1367.542117	115596.476644	35.829696
1368.494529	115785.446546	35.834714
1370.200247	115933.906934	35.839732
1371.305336	116093.314888	35.844749
1372.802297	116275.332832	35.849767
1374.121425	116444.021864	35.854784
1375.374291	116607.309482	35.859802
1376.578638	116784.103797	35.864820
1377.613755	116962.983864	35.869837
1379.168935	117132.412354	35.874855
1380.335181	117328.007519	35.879872
1381.583468	117502.666207	35.884890
1382.926631	117676.551250	35.889908
1384.169186	117871.695256	35.894925
1385.376922	118071.962081	35.899943
1387.272043	118246.966254	35.904960
1388.702262	118444.389454	35.909978
1389.935196	118639.350882	35.914996
1391.557999	118815.491237	35.920013
1392.936279	119011.230167	35.925031
1394.304725	119200.849377	35.930048
1395.682630	119399.681189	35.935066
1397.234823	119595.656512	35.940084
1398.714891	119775.295931	35.945101
1399.663455	119977.303015	35.950119
1401.417246	120169.337524	35.955136
1402.345880	120365.677368	35.960154
1404.010684	120579.948037	35.965172
1405.246949	120776.299076	35.970189
1406.900421	120966.949686	35.975207
1408.402444	121150.647684	35.980224
1409.903989	121366.666778	35.985242
1411.538827	121562.745091	35.990260
1413.126943	121772.079541	35.995277
1414.161494	121974.601324	36.000295
1416.142283	122158.534259	36.005312
1416.896937	122368.575819	36.010330
1418.840374	122560.268452	36.015348
1420.057005	122758.131913	36.020365
1421.059463	122968.518819	36.025383
1422.822643	123156.710821	36.030400
1424.132845	123366.393386	36.035418
1425.735968	123569.343657	36.040436
1426.847016	123771.284428	36.045453
1428.663729	123983.120522	36.050471
1430.078194	124169.893223	36.055488
1431.371215	124391.492466	36.060506
1432.409063	124589.891939	36.065524
1434.176665	124788.354250	36.070541
1435.462161	124996.660284	36.075559
1436.915883	125195.276813	36.080576
1438.431207	125418.837835	36.085594
1439.962470	125617.660491	36.090612
1441.490576	125820.057097	36.095629
1442.589223	126037.926163	36.100647
1444.221075	126215.685198	36.105664
1445.955175	126407.590715	36.110682
1446.852846	126595.678406	36.115700
1448.246870	126785.271913	36.120717
1449.554269	126992.209155	36.125735
1451.188296	127176.105040	36.130752
1452.389075	127362.591805	36.135770
1454.023428	127564.629865	36.140788
1455.723815	127751.483263	36.145805
1456.937621	127967.221352	36.150823
1458.366434	128146.393367	36.155840
1460.208214	128353.800731	36.160858
1461.493423	128556.788335	36.165876
1463.025173	128754.088355	36.170893
1464.317437	128961.296253	36.175911
1465.733764	129171.906397	36.180928
1466.727451	129378.860834	36.185946
1468.480819	129564.983389	36.190964
1470.320467	129785.766962	36.195981
1471.574949	130009.470351	36.200999
1472.963970	130220.713569	36.206016
1474.437883	130437.747179	36.211034
1475.771333	130648.394373	36.216052
1477.305082	130854.095793	36.221069
1478.569296	131094.757364	36.226087
1480.445933	131290.703048	36.231104
1481.955794	131502.342177	36.236122
1483.531068	131735.675037	36.241140
1485.380853	131938.356919	36.246157
1486.814434	132143.032153	36.251175
1488.492984	132378.545758	36.256192
1490.216389	132580.200761	36.261210
1491.671698	132777.440034	36.266228
1493.651022	132992.778697	36.271245
1494.686690	133210.828255	36.276263
1496.602340	133398.217493	36.281280
1497.996478	133617.644937	36.286298
1499.239432	133821.488343	36.291316
1500.783693	134027.211227	36.296333
1502.181480	134243.044527	36.301351
1503.743585	134442.850476	36.306368
1505.435361	134664.886817	36.311386
1506.976098	134867.397963	36.316404
1508.857894	135074.164425	36.321421
1510.087890	135289.145295	36.326439
1511.356387	135492.274279	36.331456
1513.000792	135701.997287	36.336474
1514.123949	135914.757008	36.341492
1515.838547	136125.979807	36.346509
1517.406371	136344.652877	36.351527
1518.987177	136551.122926	36.356544
1520.652526	136758.391989	36.361562
1522.012048	136979.903337	36.366580
1523.777313	137180.202802	36.371597
1525.417865	137368.764022	36.376615
1526.998627	137560.592629	36.381632
1528.295124	137751.935430	36.386650
1529.598878	137944.697595	36.391668
1531.501190	138132.068988	36.396685
1532.838784	138315.742295	36.401703
1534.189744	138502.113822	36.406720
1535.959966	138695.174296	36.411738
1536.981732	138899.557381	36.416756
1538.337966	139100.936042	36.421773
1539.691189	139310.617123	36.426791
1541.352955	139502.686282	36.431808
1542.484371	139713.888153	36.436826
1543.989871	139937.679647	36.441844
1545.814894	140145.834284	36.446861
1547.068022	140362.306048	36.451879
1548.269295	140588.583978	36.456896
1549.916746	140820.495713	36.461914
1550.988028	141033.085166	36.466932
1553.029503	141269.766329	36.471949
1554.625653	141502.046327	36.476967
1556.109744	141740.543332	36.481984
1557.711875	141974.359526	36.487002
1559.305955	142213.590541	36.492020
1560.918318	142431.350862	36.497037
1562.607359	142665.589493	36.502055
1564.056358	142909.690520	36.507072
1565.767091	143130.963635	36.512090
1567.152679	143374.520785	36.517108
1568.858148	143611.273585	36.522125
1570.212908	143852.634081	36.527143
1571.844810	144087.501061	36.532160
1573.622703	144326.808150	36.537178
1574.824696	144571.633402	36.542196
1576.860093	144814.426974	36.547213
1578.469202	145051.738502	36.552231
1580.484717	145290.660411	36.557248
1582.042435	145525.334624	36.562266
1583.421079	145766.693593	36.567284
1585.425588	146003.822833	36.572301
1586.988439	146237.018566	36.577319
1588.766075	146462.183615	36.582336
1590.369818	146701.054979	36.587354
1591.958708	146940.767122	36.592372
1594.086435	147155.690205	36.597389
1595.207351	147391.651996	36.602407
1596.509512	147625.152956	36.607424
1598.355891	147846.184591	36.612442
1600.063713	148088.117561	36.617460
1601.577244	148329.386035	36.622477
1602.874260	148577.612069	36.627495
1604.633245	148806.599727	36.632512
1606.162785	149033.622564	36.637530
1607.567077	149277.476239	36.642548
1609.595138	149498.756700	36.647565
1611.195099	149746.271816	36.652583
1612.839723	149964.586605	36.657600
1614.197180	150169.789676	36.662618
1615.630223	150391.310229	36.667636
1617.600949	150595.505847	36.672653
1619.010185	150818.440281	36.677671
1620.214350	151042.106075	36.682688
1621.819556	151267.015496	36.687706
1622.829684	151503.849178	36.692724
1624.972376	151727.928438	36.697741
1626.256521	151961.336976	36.702759
1627.639234	152206.636041	36.707776
1629.449754	152444.908793	36.712794
1631.184300	152687.962287	36.717812
1632.637989	152929.984538	36.722829
1634.326891	153185.219972	36.727847
1635.794649	153428.308611	36.732864
1637.776717	153670.391827	36.737882
1639.018240	153922.090634	36.742900
1640.853394	154173.532245	36.747917
1642.293113	154430.705940	36.752935
1644.445725	154692.992070	36.757952
1645.961829	154938.061944	36.762970
1647.405051	155186.923525	36.767988
1649.224768	155437.147214	36.773005
1650.853423	155706.510656	36.778023
1652.553508	155964.428173	36.783040
1654.381010	156216.621694	36.788058
1655.746749	156475.750026	36.793076
1657.798799	156730.143292	36.798093
1659.500800	156997.096214	36.803111
1660.876768	157266.245882	36.808128
1662.687427	157516.866732	36.813146
1664.519330	157778.758534	36.818164
1666.532326	158030.530241	36.823181
1668.198882	158288.115598	36.828199
1669.469525	158555.123775	36.833216
1671.621179	158797.280106	36.838234
1673.270635	159067.858658	36.843252
1674.866942	159335.886288	36.848269
1676.614706	159583.501468	36.853287
1677.991927	159848.587880	36.858304
1680.035791	160101.701191	36.863322
1681.876254	160373.984126	36.868340
1683.389664	160625.739827	36.873357
1685.129937	160887.999295	36.878375
1686.558676	161141.560158	36.883392
1688.225083	161409.731980	36.888410
1689.792831	161676.678721	36.893428
1691.738048	161936.262997	36.898445
1693.496336	162180.102981	36.903463
1695.036963	162449.786357	36.908480
1697.205296	162717.622008	36.913498
1698.879050	162979.856727	36.918516
1700.483214	163238.997335	36.923533
1702.164533	163494.804863	36.928551
1703.495595	163726.687949	36.933568
1705.832039	163964.639832	36.938586
1707.088166	164200.925889	36.943604
1708.877332	164443.000771	36.948621
1710.259163	164685.560462	36.953639
1712.061911	164930.705576	36.958656
1713.933020	165177.794599	36.963674
1715.260126	165431.389112	36.968692
1716.812284	165679.077508	36.973709
1718.774928	165930.304327	36.978727
1720.038076	166176.646839	36.983744
1722.211196	166425.509941	36.988762
1723.468313	166694.699011	36.993780
1725.157070	166965.800076	36.998797
1727.204662	167221.321762	37.003815
1728.466289	167495.551169	37.008832
1730.037033	167758.787647	37.013850
1731.654667	168029.818927	37.018868
1733.734559	168302.973037	37.023885
1735.236658	168579.100077	37.028903
1736.649501	168882.513609	37.033920
1738.848687	169156.885276	37.038938
1740.574849	169438.056572	37.043956
1742.420899	169714.492404	37.048973
1744.056188	169993.792281	37.053991
1745.827495	170274.328343	37.059008
1747.731748	170565.107042	37.064026
1749.560569	170846.716318	37.069044
1751.370263	171136.867425	37.074061
1753.347445	171415.349552	37.079079
1755.001159	171701.724232	37.084096
1757.047509	171973.565224	37.089114
1758.865153	172268.607182	37.094132
1760.649599	172550.679802	37.099149
1762.648452	172829.460319	37.104167
1764.172465	173105.857257	37.109184
1766.172289	173382.637259	37.114202
1767.917376	173663.062297	37.119220
1769.895339	173945.126831	37.124237
1771.564405	174232.189789	37.129255
1772.958113	174521.214063	37.134272
1775.601503	174776.614981	37.139290
1777.030897	175056.338768	37.144308
1778.926161	175337.918801	37.149325
1781.301441	175618.574627	37.154343
1782.955216	175888.081657	37.159360
1784.740618	176158.089714	37.164378
1786.478074	176430.631744	37.169396
1788.459380	176693.203446	37.174413
1790.359291	176959.329276	37.179431
1791.622032	177236.049754	37.184448
1793.528531	177504.068357	37.189466
1795.512600	177778.153321	37.194484
1797.199553	178058.541856	37.199501
1798.971225	178322.984114	37.204519
1800.563761	178577.624097	37.209536
1802.206362	178828.464263	37.214554
1803.686815	179079.141365	37.219572
1805.454263	179336.473237	37.224589
1807.615392	179594.061370	37.229607
1809.027262	179878.591060	37.234624
1810.712900	180144.504806	37.239642
1812.637447	180409.240417	37.244660
1813.798211	180680.645713	37.249677
1815.483735	180941.870051	37.254695
1817.085060	181240.043377	37.259712
1818.991818	181521.955233	37.264730
1820.872711	181809.569915	37.269748
1822.522584	182108.820021	37.274765
1824.315048	182378.981144	37.279783
1826.080870	182680.855908	37.284800
1828.295213	182975.137428	37.289818
1830.184028	183264.016614	37.294836
1831.754420	183572.729505	37.299853
1833.838245	183869.296280	37.304871
1835.965581	184158.371866	37.309888
1837.676360	184453.238056	37.314906
1839.708911	184745.047889	37.319924
1841.455231	185044.531063	37.324941
1843.652835	185336.039403	37.329959
1844.675257	185643.635511	37.334976
1847.051570	185944.585440	37.339994
1849.240320	186237.864809	37.345012
1850.720516	186540.775495	37.350029
1852.955489	186828.721850	37.355047
1854.610311	187139.184337	37.360064
1856.382870	187435.278392	37.365082
1858.357731	187748.523965	37.370100
1860.287658	188056.601404	37.375117
1862.501549	188347.568081	37.380135
1864.423673	188660.117568	37.385152
1866.385983	188952.206597	37.390170
1868.523521	189245.348289	37.395188
1869.979974	189544.856129	37.400205
1871.800074	189852.518699	37.405223
1873.970553	190160.508368	37.410240
1875.598875	190443.865311	37.415258
1877.582435	190753.119453	37.420276
1879.639852	191044.952515	37.425293
1881.807203	191358.521549	37.430311
1883.208136	191660.399267	37.435328
1885.143251	191958.133055	37.440346
1887.004699	192249.484197	37.445364
1888.759385	192562.225485	37.450381
1890.744766	192857.253642	37.455399
1892.540660	193172.263974	37.460416
1894.881216	193464.218943	37.465434
1896.765613	193771.363257	37.470452
1898.605815	194072.196233	37.475469
1900.531059	194347.990186	37.480487
1902.665276	194639.642159	37.485504
1904.663829	194908.853419	37.490522
1906.824673	195178.294199	37.495540
1908.212536	195455.702520	37.500557
1910.179824	195718.983391	37.505575
1912.093764	195995.410069	37.510592
1913.582465	196278.594330	37.515610
1915.672216	196566.507698	37.520628
1917.463267	196840.343920	37.525645
1919.552023	197124.275295	37.530663
1921.340578	197412.545808	37.535680
1922.766624	197693.272836	37.540698
1924.826532	197986.872268	37.545716
1926.386846	198288.586876	37.550733
1928.104953	198590.532028	37.555751
1929.946289	198895.987864	37.560768
1932.138368	199208.294551	37.565786
1934.100817	199508.721148	37.570804
1935.535297	199823.525195	37.575821
1937.794015	200135.712512	37.580839
1939.533987	200458.239782	37.585856
1941.268677	200778.865881	37.590874
1943.256163	201088.207771	37.595892
1945.335020	201433.204439	37.600909
1947.437670	201752.153171	37.605927
1949.535301	202063.222067	37.610944
1951.344440	202390.002018	37.615962
1953.851810	202720.011455	37.620980
1955.646185	203045.020536	37.625997
1957.616037	203375.855374	37.631015
1959.297751	203702.561694	37.636032
1961.180019	204031.294456	37.641050
1963.845441	204359.003602	37.646068
1965.427870	204688.320886	37.651085
1967.262941	205019.707163	37.656103
1969.487600	205355.819156	37.661120
1971.867043	205666.990171	37.666138
1974.326303	205985.373134	37.671156
1976.127491	206311.110628	37.676173
1978.583410	206629.091424	37.681191
1980.676823	206959.203746	37.686208
1982.431172	207272.742084	37.691226
1984.893805	207573.906870	37.696244
1986.700310	207901.784968	37.701261
1988.684286	208206.418328	37.706279
1990.617012	208520.975875	37.711296
1992.638484	208834.188037	37.716314
1994.788006	209144.956797	37.721332
1996.554773	209461.145093	37.726349
1998.624745	209768.184671	37.731367
2000.792164	210086.826210	37.736384
2002.510567	210404.296521	37.741402
2004.592526	210716.962808	37.746420
2006.011239	211041.466215	37.751437
2008.059324	211342.740755	37.756455
2009.682967	211655.319398	37.761472
2011.276191	211958.052826	37.766490
2013.359441	212266.511744	37.771508
2015.013878	212579.813679	37.776525
2016.830105	212897.407950	37.781543
2018.696241	213218.410977	37.786560
2020.501798	213549.150071	37.791578
2022.745065	213858.594162	37.796596
2024.840607	214194.140272	37.801613
2026.911762	214533.729236	37.806631
2028.640981	214854.685816	37.811648
2030.768607	215195.894279	37.816666
2032.934126	215534.483084	37.821684
2034.624033	215869.733798	37.826701
2036.839319	216208.914802	37.831719
2038.822563	216556.996271	37.836736
2040.718593	216908.508644	37.841754
2043.000239	217258.044481	37.846772
2044.849770	217614.176591	37.851789
2046.881808	217970.027633	37.856807
2048.906382	218317.959018	37.861824
2050.928995	218678.868359	37.866842
2053.062059	219037.336944	37.871860
2055.017222	219402.882236	37.876877
2057.260890	219761.857459	37.881895
2059.377994	220122.911430	37.886912
2061.383402	220492.123635	37.891930
2063.875021	220858.848136	37.896948
2065.588141	221228.059608	37.901965
2067.816368	221596.429369	37.906983
2069.886547	221957.321982	37.912000
2072.175267	222342.420678	37.917018
2074.387531	222692.857129	37.922036
2076.303308	223080.050280	37.927053
2078.400356	223439.041041	37.932071
2080.946189	223812.526281	37.937088
2082.638704	224175.393854	37.942106
2084.883317	224553.031710	37.947124
2086.761963	224930.170722	37.952141
2088.991732	225298.684855	37.957159
2091.039007	225725.969561	37.962176
2093.245511	226098.744794	37.967194
2095.709697	226468.230191	37.972212
2097.588810	226847.422407	37.977229
2099.691816	227208.549660	37.982247
2102.014455	227581.732196	37.987264
2103.541486	227967.410563	37.992282
2106.048280	228332.415005	37.997300
2107.988867	228702.742490	38.002317
2110.339780	229082.504801	38.007335
2112.593701	229457.433389	38.012352
2114.583370	229838.830888	38.017370
2116.714547	230206.290079	38.022388
2118.633620	230582.724179	38.027405
2120.843612	230955.989867	38.032423
2123.361174	231297.766552	38.037440
2125.314830	231656.827941	38.042458
2127.381350	231994.945364	38.047476
2129.320142	232334.303360	38.052493
2131.493278	232685.282915	38.057511
2133.538717	233031.229893	38.062528
2135.742046	233394.474376	38.067546
2137.645269	233736.890783	38.072564
2139.859537	234083.678316	38.077581
2141.917887	234446.390999	38.082599
2144.130568	234802.553221	38.087616
2145.845095	235182.060525	38.092634
2148.070749	235543.582372	38.097652
2150.566081	235910.574204	38.102669
2152.115903	236284.524125	38.107687
2154.334091	236643.841395	38.112704
2156.431762	237037.645066	38.117722
2158.787440	237406.061297	38.122740
2160.736572	237786.582361	38.127757
2162.831119	238179.070038	38.132775
2165.254988	238549.587516	38.137792
2167.506543	238950.256983	38.142810
2169.912903	239328.145631	38.147828
2172.215489	239715.144982	38.152845
2174.068288	240094.393977	38.157863
2176.445717	240495.150615	38.162880
2178.443859	240887.180542	38.167898
2180.593378	241274.082450	38.172916
2183.188116	241668.357156	38.177933
2184.710581	242066.384598	38.182951
2187.489052	242460.785181	38.187968
2189.718130	242865.027774	38.192986
2191.852734	243264.257457	38.198004
2194.229257	243656.973011	38.203021
2196.411476	244051.447819	38.208039
2198.938147	244444.751606	38.213056
2200.877951	244849.783044	38.218074
2203.312627	245239.369963	38.223092
2205.680818	245628.866969	38.228109
2207.536061	246035.134662	38.233127
2210.097423	246420.463012	38.238144
2212.202899	246824.534304	38.243162
2214.232150	247213.352939	38.248180
2216.810061	247616.183148	38.253197
2219.100831	248008.162995	38.258215
2221.552101	248399.966039	38.263232
2223.581853	248795.748737	38.268250
2226.144275	249188.095055	38.273268
2228.561905	249568.171140	38.278285
2230.818286	249972.735197	38.283303
2233.164435	250352.240303	38.288320
2235.566287	250732.143906	38.293338
2238.334745	251105.512890	38.298356
2240.691677	251488.219548	38.303373
2242.500915	251856.026979	38.308391
2245.236417	252197.956453	38.313408
2247.142160	252544.260266	38.318426
2249.154446	252888.058502	38.323444
2251.181178	253233.074404	38.328461
2252.920750	253580.829100	38.333479
2255.774124	253920.228443	38.338496
2257.456324	254285.851114	38.343514
2259.308602	254650.533057	38.348532
2261.655211	255020.852779	38.353549
2263.856527	255382.076888	38.358567
2266.005235	255740.820589	38.363584
2268.172625	256129.892186	38.368602
2270.579586	256490.044187	38.373620
2272.754002	256868.599532	38.378637
2274.876783	257270.610086	38.383655
2277.302574	257649.177751	38.388672
2279.205431	258038.040744	38.393690
2281.486224	258422.678477	38.398708
2283.825371	258813.073965	38.403725
2285.886236	259223.201189	38.408743
2288.404868	259618.497623	38.413760
2290.392166	260034.886900	38.418778
2292.714368	260440.630844	38.423796
2294.885801	260838.041829	38.428813
2297.007349	261266.224034	38.433831
2299.201710	261665.791822	38.438848
2301.592653	262089.817322	38.443866
2303.872165	262506.976928	38.448884
2306.402172	262936.112964	38.453901
2308.465377	263361.386141	38.458919
2311.165085	263783.510615	38.463936
2313.385359	264217.778050	38.468954
2315.994862	264636.488482	38.473972
2318.586544	265054.236912	38.478989
2320.548378	265491.925465	38.484007
2323.164362	265925.370101	38.489024
2325.779620	266333.818637	38.494042
2328.278261	266764.437606	38.499060
2330.980159	267181.434074	38.504077
2333.312548	267612.867707	38.509095
2335.809173	268021.844642	38.514112
2338.053922	268435.332803	38.519130
2340.500548	268850.389685	38.524148
2342.912899	269260.092211	38.529165
2345.110856	269685.452028	38.534183
2347.382456	270095.939513	38.539200
2350.143125	270514.961443	38.544218
2352.284276	270924.962016	38.549236
2354.728266	271346.955982	38.554253
2357.292095	271747.084263	38.559271
2359.712646	272171.698872	38.564288
2361.807030	272586.102386	38.569306
2364.046675	273012.448014	38.574324
2366.784520	273411.761800	38.579341
2368.859233	273821.240550	38.584359
2370.905905	274214.643478	38.589376
2373.923547	274599.992103	38.594394
2376.082117	274981.768054	38.599412
2378.353655	275362.078140	38.604429
2380.287353	275762.256465	38.609447
2382.807110	276135.820738	38.614464
2385.231121	276525.429739	38.619482
2387.259484	276934.535046	38.624500
2390.029740	277307.373666	38.629517
2392.179402	277715.570540	38.634535
2394.160985	278130.246449	38.639552
2396.564738	278527.199993	38.644570
2398.527122	278942.386821	38.649588
2400.984489	279356.174094	38.654605
2403.273375	279795.137270	38.659623
2405.686181	280209.845819	38.664640
2408.058583	280634.696532	38.669658
2410.186805	281079.628973	38.674676
2412.880492	281507.527531	38.679693
2415.173605	281946.057105	38.684711
2417.666420	282389.635406	38.689728
2420.049912	282818.014167	38.694746
2422.282491	283267.374223	38.699764
2425.006095	283710.254484	38.704781
2427.443505	284166.973675	38.709799
2430.243479	284607.249934	38.714816
2433.003574	285060.005057	38.719834
2434.926434	285505.449296	38.724852
2437.698707	285941.791158	38.729869
2440.292404	286400.464762	38.734887
2442.347930	286844.133709	38.739904
2445.345860	287287.017706	38.744922
2447.499455	287746.343688	38.749940
2450.650773	288186.026881	38.754957
2452.888308	288644.373040	38.759975
2455.770869	289083.360943	38.764992
2458.385926	289533.364650	38.770010
2460.402888	289976.044851	38.775028
2463.201310	290418.600539	38.780045
2465.551918	290857.644718	38.785063
2468.060248	291306.798873	38.790080
2470.903303	291741.292709	38.795098
2473.215152	292195.607817	38.800116
2475.985704	292629.044725	38.805133
2478.657319	293079.541630	38.810151
2480.999121	293520.538626	38.815168
2483.941443	293952.396368	38.820186
2486.152204	294390.491186	38.825204
2488.807508	294826.101476	38.830221
2491.238414	295260.984383	38.835239
2493.016744	295707.807233	38.840256
2495.805220	296133.512277	38.845274
2498.303876	296586.442595	38.850292
2500.800481	297021.336757	38.855309
2503.204356	297462.595135	38.860327
2505.688403	297881.714712	38.865344
2508.286615	298290.248081	38.870362
2510.738601	298696.923976	38.875380
2513.092261	299115.934381	38.880397
2515.247732	299517.524234	38.885415
2517.480441	299946.991909	38.890432
2519.954793	300366.894628	38.895450
2522.291563	300796.165846	38.900468
2525.114159	301216.163648	38.905485
2527.714138	301645.136915	38.910503
2529.898746	302091.650931	38.915520
2532.387989	302512.485571	38.920538
2534.693018	302966.496752	38.925556
2537.208695	303411.125601	38.930573
2539.691862	303862.006919	38.935591
2542.045977	304308.055721	38.940608
2544.538359	304762.615918	38.945626
2547.330519	305229.522730	38.950644
2549.850431	305691.873595	38.955661
2552.351735	306155.648287	38.960679
2554.603940	306612.856726	38.965696
2557.567045	307083.413182	38.970714
2560.144153	307548.745842	38.975732
2562.981262	308027.421552	38.980749
2565.606291	308491.523993	38.985767
2568.179509	308976.130751	38.990784
2570.916665	309442.904290	38.995802
2573.517076	309923.337417	39.000820
2576.255549	310382.055383	39.005837
2578.775143	310871.438208	39.010855
2581.542970	311343.330188	39.015872
2584.407340	311807.712116	39.020890
2586.873217	312283.178586	39.025908
2589.624488	312757.327873	39.030925
2592.355403	313225.560370	39.035943
2594.815521	313705.009323	39.040960
2597.691166	314169.658976	39.045978
2600.400643	314644.416244	39.050996
2603.166249	315116.063851	39.056013
2605.676233	315581.527179	39.061031
2608.241262	316056.758077	39.066048
2611.089550	316528.360726	39.071066
2613.629048	317000.594241	39.076084
2615.980387	317467.470933	39.081101
2618.996634	317939.167282	39.086119
2621.407084	318402.245858	39.091136
2623.868282	318893.480204	39.096154
2626.457373	319362.849855	39.101172
2629.026882	319843.852290	39.106189
2631.750956	320316.954594	39.111207
2634.117710	320794.149216	39.116224
2637.410847	321270.686657	39.121242
2639.678793	321763.409411	39.126260
2642.701886	322230.638468	39.131277
2645.451695	322700.219432	39.136295
2647.536607	323154.284350	39.141312
2650.301162	323586.068209	39.146330
2652.888922	324035.833034	39.151348
2655.353006	324476.828018	39.156365
2658.045977	324918.597108	39.161383
2660.359238	325376.397975	39.166400
2663.435127	325819.422202	39.171418
2665.792172	326277.922196	39.176436
2668.267755	326738.153107	39.181453
2670.976765	327197.938087	39.186471
2673.221603	327654.162433	39.191488
2676.218301	328114.531412	39.196506
2678.538370	328598.190308	39.201524
2680.940202	329065.555271	39.206541
2683.642217	329546.379717	39.211559
2686.309762	330040.767157	39.216576
2689.119287	330523.295194	39.221594
2691.322834	331013.229565	39.226612
2693.956655	331512.716810	39.231629
2697.722635	332003.006605	39.236647
2699.904876	332511.090819	39.241664
2702.749828	333006.699964	39.246682
2705.406449	333497.663170	39.251700
2708.212206	334014.093869	39.256717
2711.288764	334517.349836	39.261735
2713.674472	335017.664472	39.266752
2716.783404	335508.973613	39.271770
2719.335917	336028.095635	39.276788
2722.211462	336540.586004	39.281805
2725.312703	337041.381889	39.286823
2728.006716	337550.871663	39.291840
2730.882935	338043.900411	39.296858
2733.766922	338570.288310	39.301876
2736.379893	339060.278752	39.306893
2739.491205	339564.506997	39.311911
2742.066778	340076.331745	39.316928
2744.935471	340581.275934	39.321946
2747.725407	341084.324289	39.326964
2750.490778	341597.173043	39.331981
2753.386141	342091.411639	39.336999
2755.774326	342601.163470	39.342016
2759.173397	343101.103011	39.347034
2761.633921	343612.764526	39.352052
2764.551209	344119.855525	39.357069
2767.681639	344619.368016	39.362087
2770.217947	345139.078107	39.367104
2773.264319	345634.812448	39.372122
2776.258480	346134.079805	39.377140
2778.534502	346638.077181	39.382157
2781.781553	347137.854374	39.387175
2784.329222	347644.567171	39.392192
2787.225127	348147.361459	39.397210
2789.832239	348655.528267	39.402228
2792.336244	349156.090773	39.407245
2795.403479	349645.465689	39.412263
2797.699482	350137.903204	39.417280
2800.503462	350597.152427	39.422298
2803.294162	351072.240677	39.427316
2805.789953	351561.282795	39.432333
2808.708047	352029.996055	39.437351
2811.043559	352517.404803	39.442368
2813.552886	353004.959266	39.447386
2816.426154	353493.695465	39.452404
2819.260382	353984.743292	39.457421
2821.758609	354491.882540	39.462439
2824.300975	355009.823423	39.467456
2827.114904	355516.268049	39.472474
2829.965719	356031.382979	39.477492
2832.262979	356557.368203	39.482509
2835.098181	357081.308304	39.487527
2837.757963	357618.926596	39.492544
2840.625174	358149.018449	39.497562
2843.174340	358692.328315	39.502580
2846.338597	359247.591185	39.507597
2849.495301	359794.396895	39.512615
2852.308316	360353.205441	39.517632
2855.063848	360904.072380	39.522650
2858.426460	361457.222670	39.527668
2861.175633	362007.925618	39.532685
2864.553248	362561.136823	39.537703
2867.477179	363107.053209	39.542720
2870.313800	363664.550091	39.547738
2873.220098	364216.115905	39.552756
2876.274185	364775.493808	39.557773
2879.472637	365327.228467	39.562791
2882.131533	365882.112633	39.567808
2885.054149	366426.923967	39.572826
2888.458657	366989.239133	39.577844
2891.034030	367545.765571	39.582861
2894.450055	368110.297991	39.587879
2897.074054	368653.454530	39.592896
2900.097882	369200.753544	39.597914
2903.242636	369746.529374	39.602932
2906.050063	370310.114750	39.607949
2909.003465	370871.791886	39.612967
2912.173210	371414.497629	39.617984
2915.351388	371977.114306	39.623002
2918.610162	372519.817232	39.628020
2921.531130	373074.746204	39.633037
2924.425105	373614.320993	39.638055
2927.704266	374144.668028	39.643072
2930.597563	374701.152893	39.648090
2933.363251	375251.307264	39.653108
2936.151614	375771.587341	39.658125
2939.213436	376326.704116	39.663143
2941.964450	376885.617506	39.668160
2944.960380	377413.023877	39.673178
2948.123836	377949.784093	39.678196
2950.847316	378499.368193	39.683213
2953.818684	379041.776385	39.688231
2956.693221	379546.847791	39.693248
2959.260844	380052.874592	39.698266
2962.322534	380561.480434	39.703284
2965.141595	381083.259189	39.708301
2968.317557	381583.081245	39.713319
2970.933929	382095.187569	39.718336
2973.726268	382612.028393	39.723354
2976.763107	383136.915812	39.728372
2978.935021	383660.512292	39.733389
2982.388487	384181.488835	39.738407
2985.178461	384719.863196	39.743424
2988.018968	385255.076400	39.748442
2990.693700	385814.126699	39.753460
2993.406689	386361.671945	39.758477
2996.538699	386902.268801	39.763495
2999.390270	387471.259836	39.768512
3002.118015	388048.758644	39.773530
3005.401671	388601.810927	39.778548
3008.329119	389172.716314	39.783565
3011.294945	389737.595499	39.788583
3014.291531	390336.193303	39.793600
3017.278901	390917.536143	39.798618
3020.635535	391492.876321	39.803636
3023.170224	392102.296143	39.808653
3026.541510	392678.248619	39.813671
3029.741009	393259.544486	39.818688
3032.722387	393874.999891	39.823706
3035.889121	394471.090898	39.828724
3038.975655	395044.665213	39.833741
3042.239366	395653.907102	39.838759
3045.482857	396268.846899	39.843776
3048.745592	396845.989170	39.848794
3051.553762	397439.396903	39.853812
3054.711950	398037.911567	39.858829
3057.810441	398646.136489	39.863847
3061.410641	399255.361176	39.868864
3063.929973	399836.119117	39.873882
3067.431943	400450.890095	39.878900
3071.003050	401033.159179	39.883917
3073.801818	401642.871923	39.888935
3077.182707	402239.652061	39.893952
3080.236154	402832.999542	39.898970
3083.326226	403421.132908	39.903988
3086.193709	404032.513412	39.909005
3089.385958	404628.467521	39.914023
3092.709134	405219.927824	39.919040
3095.715030	405826.358892	39.924058
3098.910564	406425.244480	39.929076
3101.679111	407012.778636	39.934093
3105.101100	407621.846713	39.939111
3108.206851	408218.557165	39.944128
3111.492500	408818.751003	39.949146
3114.493078	409424.554713	39.954164
3117.692243	410003.649419	39.959181
3120.733592	410610.006030	39.964199
3123.806024	411170.012180	39.969216
3126.417045	411717.382529	39.974234
3129.645525	412288.292589	39.979252
3132.697063	412850.196858	39.984269
3135.325027	413419.862250	39.989287
3138.534343	413980.655634	39.994304
3140.984638	414556.891290	39.999322
3144.509338	415123.061836	40.004340
3147.201633	415716.723097	40.009357
3150.583341	416321.667102	40.014375
3153.863197	416897.269053	40.019392
3156.418297	417517.827791	40.024410
3159.860234	418083.978822	40.029428
3163.044755	418724.734913	40.034445
3166.143155	419323.578834	40.039463
3169.364811	419939.697041	40.044480
3172.096683	420560.212111	40.049498
3175.471169	421176.532440	40.054516
3178.473468	421833.006787	40.059533
3181.710464	422439.566149	40.064551
3184.735147	423081.818938	40.069568
3187.683117	423726.222420	40.074586
3190.944531	424351.382739	40.079604
3194.027931	425034.926988	40.084621
3197.176431	425673.299328	40.089639
3200.296537	426337.247451	40.094656
3203.600836	427001.504757	40.099674
3207.104178	427681.242500	40.104692
3210.360355	428345.271458	40.109709
3213.584415	429007.262497	40.114727
3216.953544	429698.748615	40.119744
3219.962588	430356.661788	40.124762
3223.161249	431017.365289	40.129780
3226.471067	431713.772141	40.134797
3229.874378	432386.667284	40.139815
3233.263317	433073.324865	40.144832
3236.478309	433737.451678	40.149850
3239.971885	434434.085471	40.154868
3243.556642	435117.643760	40.159885
3246.555959	435783.169757	40.164903
3250.085790	436464.244109	40.169920
3253.007458	437172.339377	40.174938
3256.828980	437827.982958	40.179956
3260.353557	438507.432855	40.184973
3263.350129	439194.721105	40.189991
3266.865801	439869.121786	40.195008
3269.677248	440547.084149	40.200026
3273.282088	441218.522157	40.205044
3276.640106	441926.286264	40.210061
3279.950166	442571.859159	40.215079
3283.715314	443270.253846	40.220096
3286.845970	443935.514819	40.225114
3289.970100	444630.883064	40.230132
3293.360994	445282.648817	40.235149
3296.598896	445982.364512	40.240167
3299.740348	446596.619445	40.245184
3302.504506	447253.239814	40.250202
3305.933227	447885.286153	40.255220
3309.121095	448501.812888	40.260237
3311.875285	449170.732972	40.265255
3315.520513	449796.720444	40.270272
3318.297416	450455.324559	40.275290
3321.552745	451115.858954	40.280308
3324.665158	451775.739085	40.285325
3327.805698	452434.583602	40.290343
3331.088777	453115.655595	40.295360
3334.117682	453813.246227	40.300378
3337.633753	454474.503018	40.305396
3340.722190	455181.404727	40.310413
3344.444618	455879.581207	40.315431
3347.331789	456581.359717	40.320448
3350.624483	457325.962463	40.325466
3353.943322	457997.165994	40.330484
3357.463853	458734.854566	40.335501
3360.856290	459434.945297	40.340519
3363.984039	460178.719385	40.345536
3367.510341	460886.129675	40.350554
3371.168027	461611.405859	40.355572
3374.545602	462339.636413	40.360589
3377.978167	463061.358496	40.365607
3381.639073	463803.609217	40.370624
3385.142063	464515.710585	40.375642
3388.279338	465264.266177	40.380660
3392.047476	466008.548102	40.385677
3395.241698	466733.320309	40.390695
3398.930856	467490.764089	40.395712
3402.179726	468207.182331	40.400730
3405.823667	468981.927304	40.405748
3409.003971	469695.675677	40.410765
3412.414142	470469.188716	40.415783
3416.224193	471186.326371	40.420800
3419.915858	471960.447234	40.425818
3422.981709	472689.786455	40.430836
3426.725873	473426.172573	40.435853
3430.449391	474204.703938	40.440871
3433.880398	474911.760161	40.445888
3437.175026	475697.987258	40.450906
3440.832179	476416.634086	40.455924
3444.216140	477184.740570	40.460941
3447.778378	477913.611388	40.465959
3450.919833	478684.175761	40.470976
3454.529080	479410.659128	40.475994
3457.603712	480184.663743	40.481012
3461.552636	480933.126412	40.486029
3465.116002	481677.426514	40.491047
3468.727879	482451.509801	40.496064
3471.679403	483207.624439	40.501082
3475.636552	483929.236182	40.506100
3479.182793	484720.876995	40.511117
3482.242330	485466.094269	40.516122
3485.359625	486124.908019	40.521127
3489.112548	486758.319963	40.526132
3492.039752	487383.229730	40.531136
3494.885985	487888.179295	40.536141
3498.163158	488344.976216	40.541146
3500.483243	488796.088275	40.546151
3502.630648	489150.116449	40.551156
3504.758051	489422.896024	40.556160
3507.128854	489712.854502	40.561165
3508.594562	489884.784452	40.566170
3510.799679	490034.917762	40.571175
3512.248920	490166.277016	40.576180
3513.518838	490286.216941	40.581184
3514.534938	490331.032889	40.586189
3515.623841	490343.117863	40.591194
3516.666818	490308.764734	40.596199
3517.081493	490254.605624	40.601204
3517.535708	490183.421839	40.606208
3518.781567	490071.238208	40.611213
3519.539579	489946.519103	40.616218
3519.589412	489856.150883	40.621223
3520.258461	489694.064052	40.626228
3520.070580	489494.679858	40.631232
3520.871652	489314.182406	40.636237
3520.814517	489169.579472	40.641242
3521.083251	488929.797838	40.646247
3521.110522	488721.000682	40.651252
3521.166089	488548.161142	40.656256
3521.244059	488303.538957	40.661261
3521.415128	488051.553888	40.666266
3521.119452	487818.736558	40.671271
3521.280670	487634.018516	40.676276
3520.806401	487366.574845	40.681280
3520.999728	487112.395587	40.686285
3520.506778	486890.286907	40.691290
3520.729321	486633.462429	40.696295
3520.156932	486395.504259	40.701300
3519.752917	486162.886521	40.706304
3520.186800	485902.421970	40.711309
3519.444075	485688.596596	40.716314
3519.312095	485444.882943	40.721319
3519.070058	485208.377731	40.726324
3519.366466	484948.732621	40.731328
3518.957936	484758.909278	40.736333
3518.286436	484517.903724	40.741338
3518.407150	484243.837485	40.746343
3517.665671	484082.382058	40.751348
3517.240828	483843.507758	40.756352
3517.708886	483589.897278	40.761357
3516.831707	483416.500323	40.766362
3516.746416	483215.565258	40.771367
3516.707358	482987.462433	40.776372
3516.344952	482776.331569	40.781376
3516.504956	482612.998711	40.786381
3515.353416	482403.812650	40.791386
3515.556842	482177.840862	40.796391
3515.460611	482004.206583	40.801396
3514.701799	481855.808613	40.806400
3514.526940	481646.814795	40.811405
3514.733341	481469.935611	40.816410
3514.331889	481312.305309	40.821415
3514.467375	481120.536326	40.826420
3514.092613	480980.482838	40.831424
3514.195514	480779.442369	40.836429
3513.474834	480629.407532	40.841434
3513.435814	480464.314645	40.846439
3513.328739	480280.633183	40.851444
3513.086024	480164.370568	40.856448
3513.069028	479973.476031	40.861453
3512.831947	479833.544675	40.866458
3512.620044	479670.600914	40.871463
3512.160850	479559.487359	40.876468
3512.441513	479399.352134	40.881472
3512.032974	479247.433078	40.886477
3511.276549	479138.340596	40.891482
3511.694477	478974.531396	40.896487
3511.130584	478880.813474	40.901492
3510.909337	478744.014049	40.906496
3510.842489	478607.848119	40.911501
3510.795421	478514.857665	40.916506
3510.967088	478382.402828	40.921511
3510.339813	478269.332093	40.926516
3510.128047	478164.202648	40.931520
3510.475442	478030.957490	40.936525
3509.953205	477945.388286	40.941530
3510.153424	477818.854947	40.946535
3510.068330	477716.642679	40.951540
3509.242761	477625.950469	40.956544
3509.715740	477518.073916	40.961549
3509.187067	477421.454663	40.966554
3509.294477	477336.543580	40.971559
3509.278149	477232.290648	40.976564
3508.918453	477169.702687	40.981568
3509.261042	477029.862772	40.986573
3508.731693	476953.819029	40.991578
3508.569966	476890.793435	40.996583
3508.537039	476829.977401	41.001588
3508.377941	476725.136190	41.006592
3508.473234	476633.989839	41.011597
3508.374556	476570.649168	41.016602
3508.515599	476463.782440	41.021607
3508.164499	476422.225195	41.026612
3507.810740	476326.688111	41.031616
3508.096673	476224.764411	41.036621
3507.963304	476202.635688	41.041626
3507.441200	476123.191699	41.046631
3507.764527	476031.449035	41.051636
3507.462786	476007.167194	41.056640
3507.706119	475904.843121	41.061645
3507.660282	475826.387109	41.066650
3507.339143	475808.798769	41.071655
3507.146328	475717.845879	41.076660
3506.766123	475684.452353	41.081664
3507.348406	475598.850644	41.086669
3506.724191	475576.393317	41.091674
3507.191880	475492.279210	41.096679
3506.881120	475467.795396	41.101684
3506.612229	475386.179598	41.106688
3506.832257	475361.409007	41.111693
3506.662989	475284.592423	41.116698
3506.878933	475245.832364	41.121703
3506.692885	475195.071907	41.126708
3506.600784	475138.163147	41.131712
3506.735525	475097.590848	41.136717
3506.375791	475009.854553	41.141722
3506.231552	475004.200148	41.146727
3506.156384	474926.049419	41.151732
3506.147466	474886.868014	41.156736
3505.843666	474863.193396	41.161741
3506.270423	474787.497268	41.166746
3506.154124	474743.922570	41.171751
3506.034388	474754.738348	41.176756
3505.958742	474701.272656	41.181760
3506.011347	474638.865132	41.186765
3506.106770	474581.570344	41.191770
3505.908305	474582.412716	41.196775
3505.835694	474522.457748	41.201780
3505.840095	474483.273460	41.206784
3505.493231	474458.642062	41.211789
3505.589092	474415.185197	41.216794
3505.682474	474386.834415	41.221799
3505.770251	474377.696206	41.226804
3505.413658	474319.255552	41.231808
3505.889760	474304.986863	41.236813
3505.488884	474256.893935	41.241818
3505.092267	474235.767799	41.246823
3505.255390	474185.608613	41.251828
3505.449677	474192.269082	41.256832
3505.492568	474132.598856	41.261837
3505.252035	474133.498587	41.266842
3505.785943	474081.455658	41.271847
3505.039792	474044.518191	41.276852
3505.026404	474044.266813	41.281856
3505.425068	474001.673651	41.286861
3505.241351	473962.518096	41.291866
3505.190448	473944.074359	41.296871
3505.174398	473928.311756	41.301876
3505.390585	473891.069831	41.306880
3505.024996	473876.528345	41.311885
3504.867208	473855.465450	41.316890
3505.225962	473809.025614	41.321895
3505.197242	473788.499860	41.326900
3504.847720	473778.619431	41.331904
3505.231271	473755.139034	41.336909
3504.857036	473727.216091	41.341914
3504.969260	473704.995134	41.346919
3504.836925	473699.591945	41.351924
3505.132103	473663.097503	41.356928
3504.974975	473633.467269	41.361933
3504.664503	473620.539046	41.366938
3504.674614	473612.426620	41.371943
3504.816808	473588.933489	41.376948
3504.649994	473568.936267	41.381952
3504.840712	473541.278621	41.386957
3504.495610	473539.204040	41.391962
3504.681110	473503.689809	41.396967
3504.808636	473506.204251	41.401972
3504.591597	473496.099973	41.406976
3504.623684	473467.301367	41.411981
3504.562155	473481.352959	41.416986
3504.649757	473413.207871	41.421991
3504.771101	473432.654735	41.426996
3504.390110	473409.294785	41.432000
3504.881280	473392.995362	41.437005
3504.486253	473375.771444	41.442010
3504.619395	473360.947990	41.447015
3504.371830	473328.999727	41.452020
3504.680685	473350.596838	41.457024
3504.629030	473318.161356	41.462029
3504.678327	473285.355013	41.467034
3504.381391	473267.050940	41.472039
3504.474818	473290.963362	41.477044
3504.164037	473260.849942	41.482048
3505.142631	473224.196005	41.487053
3504.708022	473255.593166	41.492058
3504.253358	473214.603350	41.497063
3504.852898	473204.978182	41.502068
3504.467115	473181.314568	41.507072
3504.724836	473175.089185	41.512077
3504.502274	473158.851695	41.517082
3504.678530	473119.688322	41.522087
3504.609679	473147.986216	41.527092
3504.482943	473095.639654	41.532096
3504.445479	473106.646074	41.537101
3504.481496	473062.435387	41.542106
3504.458419	473067.406990	41.547111
3504.453567	473058.637691	41.552116
3504.503452	473044.486187	41.557120
3504.617927	473026.421035	41.562125
3504.426962	473010.229126	41.567130
3504.380411	473005.369828	41.572135
3504.886929	472974.011538	41.577140
3504.175104	472991.005116	41.582144
3504.801641	472937.322433	41.587149
3504.455384	472947.718722	41.592154
3504.601402	472910.232634	41.597159
3504.909194	472910.741584	41.602164
3504.723401	472886.082829	41.607168
3504.888749	472873.535174	41.612173
3504.276146	472854.317434	41.617178
3504.398701	472849.228593	41.622183
3504.624348	472805.849184	41.627188
3504.261917	472834.447385	41.632192
3504.588661	472786.692240	41.637197
3504.664978	472794.284313	41.642202
3504.515227	472759.784979	41.647207
3504.607936	472743.801496	41.652212
3504.228226	472762.010133	41.657216
3504.708648	472692.634588	41.662221
3504.263597	472720.941838	41.667226
3504.681095	472685.744385	41.672231
3504.337895	472703.491050	41.677236
3504.623999	472661.825402	41.682240
3504.480186	472669.401619	41.687245
3504.569478	472629.592026	41.692250
3504.660635	472650.007607	41.697255
3504.650360	472604.687965	41.702260
3504.530173	472611.145181	41.707264
3504.439728	472579.475086	41.712269
3504.217193	472585.897792	41.717274
3504.256329	472560.290584	41.722279
3504.278223	472543.152151	41.727284
3504.146839	472542.615234	41.732288
3504.207598	472527.751925	41.737293
3504.653590	472514.956912	41.742298
3504.328315	472493.564222	41.747303
3504.400840	472494.921492	41.752308
3504.291735	472477.651625	41.757312
3504.571532	472470.763503	41.762317
3504.393353	472439.614012	41.767322
3504.009710	472464.413928	41.772327
3504.112082	472406.047351	41.777332
3504.287892	472426.196297	41.782336
3503.792897	472419.836184	41.787341
3504.115809	472413.194704	41.792346
3504.051348	472417.818138	41.797351
3504.287579	472370.380506	41.802356
3503.901807	472404.711586	41.807360
3504.261576	472373.122099	41.812365
3503.955651	472370.331466	41.817370
3504.188914	472369.635518	41.822375
3504.403616	472338.423776	41.827380
3504.092582	472355.354527	41.832384
3504.181853	472311.792851	41.837389
3504.075079	472314.952821	41.842394
3504.180997	472342.007505	41.847399
3503.980317	472293.878320	41.852404
3504.075933	472294.927780	41.857408
3504.104760	472290.614050	41.862413
3504.012705	472302.998314	41.867418
3503.985490	472275.778977	41.872423
3504.278882	472270.358816	41.877428
3504.232729	472256.069863	41.882432
3504.160348	472274.585225	41.887437
3504.157175	472236.158270	41.892442
3503.986194	472228.783663	41.897447
3504.155656	472240.264799	41.902452
3504.042916	472220.308411	41.907456
3504.319293	472195.271601	41.912461
3504.392689	472219.898180	41.917466
3504.186041	472184.595740	41.922471
3504.196391	472184.948938	41.927476
3504.206335	472197.266447	41.932480
3504.498247	472176.434923	41.937485
3504.162117	472150.683735	41.942490
3503.886308	472152.704438	41.947495
3504.417448	472155.915692	41.952500
3503.875236	472146.064929	41.957504
3504.187572	472110.680332	41.962509
3503.991527	472111.015458	41.967514
3503.766048	472131.988562	41.972519
3504.461397	472110.231370	41.977524
3504.422978	472082.962853	41.982528
3504.412056	472097.260873	41.987533
3504.269555	472065.648911	41.992538
3503.941722	472063.267270	41.997543
3504.412177	472032.318818	42.002548
3504.129092	472074.999112	42.007552
3504.112498	472017.816252	42.012557
3504.300484	472020.777588	42.017562
3503.696753	472018.388853	42.022567
3504.533136	472017.496172	42.027572
3504.292521	472019.156451	42.032576
3503.964778	471974.392564	42.037581
3504.098210	471997.590418	42.042586
3503.874710	471963.861852	42.047591
3504.246974	471954.322723	42.052596
3503.646970	471982.858263	42.057600
3504.441594	471938.677346	42.062605
3504.460560	471961.284974	42.067610
3504.052853	471918.510769	42.072615
3504.217332	471931.868641	42.077620
3504.195962	471903.988833	42.082624
3504.169010	471897.808062	42.087629
3504.392475	471884.845046	42.092634
3504.346151	471872.076755	42.097639
3504.206113	471870.780736	42.102644
3504.061981	471869.383971	42.107648
3504.212303	471849.334947	42.112653
3504.000094	471839.482573	42.117658
3503.674598	471830.408553	42.122663
3503.811681	471826.635281	42.127668
3504.203920	471832.859656	42.132672
3504.365654	471795.521146	42.137677
3504.156309	471825.465366	42.142682
3504.065159	471786.037542	42.147687
3504.733424	471799.011690	42.152692
3504.067218	471770.219685	42.157696
3504.142926	471785.670259	42.162701
3504.291930	471736.724049	42.167706
3504.198323	471745.154520	42.172711
3504.250712	471724.056215	42.177716
3504.141822	471732.945381	42.182720
3504.195844	471706.219423	42.187725
3504.263022	471698.654891	42.192730
3503.894833	471696.887951	42.197735
3504.304002	471683.134998	42.202740
3503.862843	471692.938552	42.207744
3504.434128	471658.019222	42.212749
3504.295209	471685.924622	42.217754
3504.187200	471655.016340	42.222759
3504.253380	471631.938568	42.227764
3504.193620	471634.482843	42.232768
3504.256047	471603.851730	42.237773
3504.345616	471615.954211	42.242778
3504.085066	471615.032106	42.247783
3504.695090	471555.467541	42.252788
3504.177357	471598.692882	42.257792
3504.383610	471555.060421	42.262797
3504.354602	471561.452855	42.267802
3504.105366	471557.892689	42.272807
3503.775129	471527.627711	42.277812
3504.166840	471511.950897	42.282816
3504.331331	471531.595531	42.287821
3504.109932	471487.117964	42.292826
3503.869551	471518.689860	42.297831
3504.026030	471474.811608	42.302836
3503.598193	471493.434552	42.307840
3503.694312	471463.456975	42.312845
3503.652276	471477.608248	42.317850
3504.108924	471478.296499	42.322855
3504.019104	471459.552497	42.327860
3503.840754	471470.277873	42.332864
3504.174697	471430.528692	42.337869
3504.075433	471443.117401	42.342874
3504.238429	471426.564112	42.347879
3504.319446	471442.166198	42.352884
3503.938998	471397.814974	42.357888
3504.010300	471426.245173	42.362893
3504.123683	471395.960583	42.367898
3503.856791	471405.280446	42.372903
3503.786371	471379.841183	42.377908
3503.870367	471370.752934	42.382912
3504.001732	471364.293489	42.387917
3503.976680	471402.523661	42.392922
3504.014610	471364.240681	42.397927
3504.275118	471335.504385	42.402932
3503.814467	471369.798320	42.407936
3504.114225	471332.031574	42.412941
3504.061588	471365.399159	42.417946
3504.040426	471340.357646	42.422951
3504.212610	471299.163536	42.427956
3503.511880	471335.928986	42.432960
3504.216042	471291.355402	42.437965
3503.780657	471311.956930	42.442970
3503.530832	471305.507019	42.447975
3503.978235	471267.868914	42.452980
3503.740855	471313.179864	42.457984
3503.819387	471290.302551	42.462989
3504.248071	471294.898987	42.467994
3503.883225	471299.418054	42.472999
3503.659539	471262.190199	42.478004
3504.113133	471235.349779	42.483008
3504.344785	471273.032632	42.488013
3504.203869	471230.823213	42.493018
3503.839969	471255.976345	42.498023
3504.350698	471213.815987	42.503028
3503.983779	471225.889452	42.508032
3504.087227	471229.574041	42.513037
3504.159189	471180.081010	42.518042
3503.937183	471212.816532	42.523047
3504.152992	471174.251593	42.528052
3503.883114	471205.118851	42.533056
3503.851616	471159.799390	42.538061
3504.093886	471173.196156	42.543066
3503.352962	471172.502053	42.548071
3503.910877	471177.382280	42.553076
3503.973692	471170.122435	42.558080
3503.974056	471144.620996	42.563085
3503.947606	471157.857451	42.568090
3504.603977	471107.511398	42.573095
3504.064562	471143.237718	42.578100
3503.880690	471103.062769	42.583104
3504.166586	471113.410759	42.588109
3504.156096	471108.139725	42.593114
3504.047541	471106.433092	42.598119
3503.910193	471072.689454	42.603124
3504.005701	471070.747770	42.608128
3503.718375	471072.567602	42.613133
3503.780217	471062.367348	42.618138
3503.796209	471078.132082	42.623143
3504.104064	471068.450631	42.628148
3503.716659	471063.644750	42.633152
3504.084077	471044.422511	42.638157
3504.077090	471042.040736	42.643162
3503.836807	471044.461520	42.648167
3504.281501	471025.429844	42.653172
3504.272085	471027.357850	42.658176
3504.173373	470999.387650	42.663181
3504.147457	470997.313055	42.668186
3504.094177	470983.734132	42.673191
3504.489105	470982.100006	42.678196
3504.351200	470965.593910	42.683200
3504.298866	470972.649299	42.688205
3503.896269	470936.006825	42.693210
3503.793735	470930.851691	42.698215
3503.909963	470941.023790	42.703220
3503.833946	470916.497424	42.708224
3503.830264	470901.541733	42.713229
3503.598739	470923.480300	42.718234
3503.513135	470918.525284	42.723239
3503.677847	470911.350640	42.728244
3503.545305	470928.964132	42.733248
3503.527746	470916.748394	42.738253
3504.117607	470921.775730	42.743258
3503.498347	470919.592115	42.748263
3503.948312	470912.118889	42.753268
3504.134113	470886.232929	42.758272
3503.982453	470886.155464	42.763277
3503.575650	470902.544849	42.768282
3503.564597	470901.279081	42.773287
3503.773185	470881.219911	42.778292
3503.648248	470909.377642	42.783296
3503.776713	470874.526986	42.788301
3503.416304	470881.783198	42.793306
3504.069040	470837.571664	42.798311
3503.940069	470897.062181	42.803316
3503.433204	470872.755961	42.808321
3504.074965	470849.586341	42.813325
3503.932186	470891.537108	42.818330
3503.730085	470841.782393	42.823335
3504.320707	470858.267656	42.828340
3503.943018	470830.544120	42.833345
3503.978149	470812.895167	42.838349
3504.044121	470851.923157	42.843354
3503.696468	470808.325975	42.848359
3503.917062	470831.866255	42.853364
3503.565353	470821.528451	42.858369
3503.923209	470818.683388	42.863373
3503.731837	470825.811503	42.868378
3503.785889	470820.479494	42.873383
3503.584672	470814.782237	42.878388
3504.326788	470770.708532	42.883393
3504.076357	470815.617035	42.888397
3503.780368	470784.534368	42.893402
3504.228516	470753.334036	42.898407
3504.140382	470762.930130	42.903412
3503.749832	470772.979614	42.908417
3503.785320	470738.396922	42.913421
3504.129452	470747.519103	42.918426
3503.794246	470750.005624	42.923431
3504.310030	470704.598666	42.928436
3504.000092	470742.570886	42.933441
3503.852170	470724.849393	42.938445
3504.321814	470712.150931	42.943450
3503.584835	470696.651902	42.948455
3503.980121	470696.994983	42.953460
3503.845993	470676.026491	42.958465
3504.472322	470683.177509	42.963469
3504.196663	470695.693153	42.968474
3504.105999	470660.572576	42.973479
3504.116598	470661.179260	42.978484
3504.295963	470643.152468	42.983489
3504.177680	470658.076848	42.988493
3504.238364	470611.169928	42.993498
3503.884007	470596.015945	42.998503
3503.907244	470620.348157	43.003508
3503.885036	470574.823151	43.008513
3503.750934	470591.017578	43.013517
3503.887752	470581.971335	43.018522
3503.853852	470592.623633	43.023527
3503.664765	470583.679602	43.028532
3503.803118	470573.568414	43.033537
3503.764645	470597.454108	43.038541
3504.009007	470557.869514	43.043546
3503.783884	470547.410165	43.048551
3503.925545	470568.225421	43.053556
3503.897060	470553.019900	43.058561
3504.172045	470565.397888	43.063565
3504.160472	470510.694369	43.068570
3503.462258	470532.301512	43.073575
3503.983334	470516.704901	43.078580
3503.887079	470540.498393	43.083585
3503.542883	470513.732440	43.088589
3503.690216	470530.997831	43.093594
3503.579382	470489.238448	43.098599
3503.522810	470529.199016	43.103604
3503.175379	470499.138052	43.108609
3503.876261	470488.532309	43.113613
3503.598924	470525.029470	43.118618
3503.806595	470495.641263	43.123623
3503.574105	470522.194115	43.128628
3503.299336	470508.142889	43.133633
3503.568971	470482.598076	43.138637
3503.786149	470506.899767	43.143642
3503.589501	470538.415541	43.148647
3503.877483	470537.406686	43.153652
3503.255680	470524.576423	43.158657
3504.099051	470502.996953	43.163661
3504.442008	470480.482554	43.168666
3503.853181	470522.352468	43.173671
3503.859669	470497.660467	43.178676
3503.513386	470477.840711	43.183681
3503.865857	470491.981001	43.188685
3503.745014	470491.239562	43.193690
3503.722593	470439.731679	43.198695
3503.684107	470442.830439	43.203700
3503.657969	470471.987152	43.208705
3503.606653	470473.719032	43.213709
3503.605891	470451.816631	43.218714
3503.711579	470437.603822	43.223719
3503.660845	470473.761054	43.228724
3503.625411	470475.389022	43.233729
3503.185862	470472.669951	43.238733
3504.037813	470448.807561	43.243738
3503.931531	470459.420668	43.248743
3503.573405	470446.193778	43.253748
3503.790625	470418.730563	43.258753
3503.659227	470462.353507	43.263757
3503.642088	470434.369652	43.268762
3503.862548	470413.344850	43.273767
3503.961242	470434.319132	43.278772
3503.844596	470462.526859	43.283777
3503.445835	470404.943649	43.288781
3504.079633	470422.842045	43.293786
3503.787469	470383.443323	43.298791
3503.724812	470391.007545	43.303796
3503.561165	470416.028640	43.308801
3503.591598	470384.690979	43.313805
3504.109815	470432.064538	43.318810
3503.205752	470401.128108	43.323815
3503.808412	470381.715975	43.328820
3503.847356	470398.643706	43.333825
3503.508068	470372.637300	43.338829
3503.726977	470357.747435	43.343834
3503.602970	470391.432070	43.348839
3503.395314	470370.272090	43.353844
3503.830863	470372.028425	43.358849
3503.482072	470409.601790	43.363853
3503.835730	470363.307108	43.368858
3503.714706	470391.211420	43.373863
3503.686154	470400.696862	43.378868
3504.000600	470356.436376	43.383873
3503.723106	470360.384134	43.388877
3504.082034	470370.416750	43.393882
3503.588444	470393.462006	43.398887
3504.199950	470387.129169	43.403892
3503.852507	470350.781145	43.408897
3504.093605	470306.684248	43.413901
3504.102724	470351.147125	43.418906
3503.807136	470325.133752	43.423911
3503.750628	470325.903154	43.428916
3503.531743	470336.889025	43.433921
3503.968046	470307.870020	43.438925
3504.217958	470330.493624	43.443930
3503.620565	470291.396475	43.448935
3503.776002	470319.713492	43.453940
3503.378596	470314.300609	43.458945
3503.960332	470294.435396	43.463949
3504.174599	470323.148714	43.468954
3503.820009	470288.170625	43.473959
3503.903123	470249.523543	43.478964
3504.025194	470269.125378	43.483969
3504.058656	470297.512405	43.488973
3503.994739	470239.520907	43.493978
3504.004719	470260.610788	43.498983
3503.512686	470227.073939	43.503988
3503.613118	470265.590576	43.508993
3503.682529	470257.163254	43.513997
3504.362078	470224.658038	43.519002
3503.803628	470257.701746	43.524007
3503.736319	470243.313345	43.529012
3503.509596	470213.841299	43.534017
3504.051268	470182.169022	43.539021
3503.792096	470198.079318	43.544026
3503.612843	470244.853734	43.549031
3503.769392	470234.283199	43.554036
3503.310550	470216.661116	43.559041
3503.754488	470189.313866	43.564045
3503.683106	470207.577412	43.569050
3503.491188	470199.140672	43.574055
3503.937436	470158.205186	43.579060
3503.894565	470212.715360	43.584065
3503.713393	470211.324336	43.589069
3503.977641	470169.352922	43.594074
3503.543589	470180.372884	43.599079
3503.859146	470186.761981	43.604084
3503.974687	470192.929186	43.609089
3503.781045	470192.148542	43.614093
3503.848420	470189.957719	43.619098
3503.925062	470189.489259	43.624103
3503.949867	470163.526445	43.629108
3504.272317	470130.469115	43.634113
3504.345231	470100.341135	43.639117
3504.004008	470139.688328	43.644122
3503.494428	470130.845460	43.649127
3503.980478	470105.265978	43.654132
3504.064784	470117.775775	43.659137
3503.627966	470090.111296	43.664141
3504.240387	470088.696231	43.669146
3503.805145	470102.150075	43.674151
3503.552232	470073.898796	43.679156
3503.905439	470037.743687	43.684161
3504.146931	470059.253491	43.689165
3504.035762	470077.269934	43.694170
3503.707243	470062.060776	43.699175
3504.265122	470037.990894	43.704180
3504.358003	470069.664419	43.709185
3503.797372	470029.090632	43.714189
3504.525442	469993.687416	43.719194
3504.294089	470028.606436	43.724199
3504.256166	469993.020084	43.729204
3504.292862	469985.611850	43.734209
3503.979832	469982.872716	43.739213
3504.224538	469940.244812	43.744218
3503.488419	469961.909237	43.749223
3503.881855	469922.806889	43.754228
3504.023610	469964.917356	43.759233
3503.223625	469949.681233	43.764237
3503.820878	469929.001998	43.769242
3503.740677	469916.491364	43.774247
3503.536251	469949.073991	43.779252
3503.555514	469927.725590	43.784257
3503.708974	469930.033565	43.789261
3503.936805	469905.407280	43.794266
3503.371509	469930.543144	43.799271
3503.639150	469908.648449	43.804276
3503.957287	469919.955270	43.809281
3503.760138	469942.142944	43.814285
3503.834265	469907.654168	43.819290
3503.492438	469904.412559	43.824295
3503.889736	469904.856740	43.829300
3503.743893	469892.812782	43.834305
3503.574562	469890.507236	43.839309
3503.684084	469908.945257	43.844314
3503.743506	469886.018718	43.849319
3503.660551	469914.880982	43.854324
3503.986078	469897.337457	43.859329
3503.635631	469883.196367	43.864333
3503.801081	469869.227232	43.869338
3503.660464	469887.096390	43.874343
3504.037006	469862.243742	43.879348
3503.987506	469873.203083	43.884353
3503.595197	469882.137837	43.889357
3503.740089	469872.836502	43.894362
3503.791990	469848.694271	43.899367
3503.440449	469838.102441	43.904372
3503.996154	469850.740695	43.909377
3504.222501	469846.648747	43.914381
3503.879880	469831.999368	43.919386
3503.792978	469861.166540	43.924391
3503.386598	469827.108491	43.929396
3504.168088	469786.423499	43.934401
3503.587814	469824.795033	43.939405
3504.089524	469795.663575	43.944410
3504.083052	469803.219130	43.949415
3503.736147	469819.650599	43.954420
3504.279791	469776.163882	43.959425
3503.944417	469799.083382	43.964429
3503.690729	469768.854441	43.969434
3504.067416	469735.585105	43.974439
3503.956195	469768.812406	43.979444
3503.958214	469776.113120	43.984449
3503.507281	469748.399716	43.989453
3503.539493	469737.696477	43.994458
3504.124211	469712.050217	43.999463
3503.658076	469748.984193	44.004468
3504.021166	469763.427512	44.009473
3503.534649	469728.469335	44.014477
3504.054140	469698.878613	44.019482
3503.976829	469712.884557	44.024487
3503.691274	469688.694076	44.029492
3503.893626	469725.370326	44.034497
3503.889097	469709.805488	44.039501
3504.036879	469712.520002	44.044506
3503.474726	469699.476991	44.049511
3503.715572	469660.803887	44.054516
3504.026127	469684.229843	44.059521
3504.072225	469658.161630	44.064525
3504.043937	469658.419575	44.069530
3503.876322	469679.994433	44.074535
3503.987187	469631.454908	44.079540
3503.828140	469654.549505	44.084545
3503.765969	469627.332217	44.089549
3504.101033	469659.018789	44.094554
3504.110440	469618.556911	44.099559
3503.728590	469635.602474	44.104564
3503.839372	469582.144733	44.109569
3503.650252	469622.432204	44.114573
3503.737466	469597.117949	44.119578
3503.489153	469636.299299	44.124583
3503.891306	469599.121650	44.129588
3503.996155	469616.445218	44.134593
3503.795407	469570.946239	44.139597
3503.935735	469586.844557	44.144602
3503.900675	469551.966833	44.149607
3503.706538	469584.092081	44.154612
3503.696437	469582.014844	44.159617
3503.902143	469557.493050	44.164621
3503.659870	469567.975997	44.169626
3503.845894	469549.947208	44.174631
3503.382306	469552.758375	44.179636
3503.683614	469529.032676	44.184641
3503.330309	469582.275299	44.189645
3503.423383	469556.909367	44.194650
3503.941704	469523.414498	44.199655
3503.773395	469568.109899	44.204660
3503.795047	469539.358176	44.209665
3504.117559	469532.056712	44.214669
3503.950541	469524.984728	44.219674
3503.792893	469528.305269	44.224679
3503.850355	469508.978501	44.229684
3503.901544	469498.525652	44.234689
3503.709920	469521.169223	44.239693
3503.477006	469496.665983	44.244698
3503.581878	469526.563849	44.249703
3503.314875	469476.156995	44.254708
3503.536453	469503.247804	44.259713
3503.302177	469497.200492	44.264717
3503.876292	469466.181137	44.269722
3503.606795	469517.281169	44.274727
3503.682024	469472.296081	44.279732
3503.889663	469500.960878	44.284737
3503.740925	469483.846887	44.289741
3503.817809	469505.079065	44.294746
3503.894385	469494.622201	44.299751
3504.325896	469479.799513	44.304756
3503.846837	469459.391342	44.309761
3503.948758	469451.516285	44.314765
3504.075267	469443.586636	44.319770
3503.790114	469457.879116	44.324775
3503.424859	469432.129152	44.329780
3503.828396	469399.159254	44.334785
3503.656078	469393.811958	44.339789
3503.603610	469450.252345	44.344794
3503.731680	469419.151314	44.349799
3503.496811	469425.982565	44.354804
3503.741675	469424.726959	44.359809
3504.022411	469419.561574	44.364813
3503.899528	469426.324421	44.369818
3503.886631	469379.933388	44.374823
3503.370400	469413.326676	44.379828
3503.811057	469376.446763	44.384833
3503.566876	469399.910017	44.389837
3503.975249	469379.158689	44.394842
3503.728422	469402.216736	44.399847
3503.973393	469379.361718	44.404852
3503.439682	469398.256780	44.409857
3503.466470	469376.855923	44.414861
3503.706075	469370.328050	44.419866
3503.512882	469389.676326	44.424871
3503.621373	469363.648586	44.429876
3503.837824	469366.352291	44.434881
3503.540860	469363.864049	44.439885
3503.686586	469387.975528	44.444890
3503.564113	469362.592727	44.449895
3503.666310	469351.776823	44.454900
3503.902950	469399.552157	44.459905
3503.550682	469373.039526	44.464909
3503.881481	469361.376248	44.469914
3503.325442	469357.357165	44.474919
3503.592943	469318.020077	44.479924
3503.668955	469336.159683	44.484929
3503.432163	469355.362772	44.489933
3503.506564	469323.610944	44.494938
3503.453402	469353.990362	44.499943
3503.738168	469328.847370	44.504948
3503.759930	469351.001070	44.509953
3503.827051	469335.323223	44.514957
3503.541794	469351.035474	44.519962
3503.885299	469338.406820	44.524967
3503.696755	469346.295536	44.529972
3503.989139	469313.393774	44.534977
3503.448531	469309.321540	44.539981
3503.853676	469302.919590	44.544986
3503.974665	469322.268971	44.549991
3503.752000	469294.214666	44.554996
3504.008483	469327.688767	44.560001
3503.544570	469293.791050	44.565005
3503.723662	469248.434143	44.570010
3503.529221	469296.784880	44.575015
3503.185473	469281.324043	44.580020
3503.617469	469265.132144	44.585025
3503.175505	469297.601222	44.590029
3503.764227	469263.993404	44.595034
3503.641955	469281.809476	44.600039
3503.383871	469301.117387	44.605044
3504.207215	469254.391087	44.610049
3503.693561	469298.381102	44.615053
3503.900849	469268.940526	44.620058
3503.920246	469286.480687	44.625063
3503.731291	469293.101911	44.630068
3503.567482	469257.838422	44.635073
3503.690715	469263.700468	44.640077
3503.740103	469288.131508	44.645082
3503.970114	469258.940842	44.650087
3503.968130	469268.524005	44.655092
3504.231111	469256.212248	44.660097
3504.028240	469262.480760	44.665101
3503.926704	469223.658153	44.670106
3503.620300	469245.559615	44.675111
3503.683177	469224.964150	44.680116
3503.880993	469248.966149	44.685121
3503.595060	469219.045727	44.690125
3503.763973	469190.371655	44.695130
3503.517764	469203.035647	44.700135
3504.130575	469174.544907	44.705140
3504.069009	469194.328888	44.710145
3503.576574	469181.578752	44.715149
3503.546944	469214.134895	44.720154
3504.235953	469179.902653	44.725159
3503.537233	469184.627056	44.730164
3504.245797	469151.659259	44.735169
3503.738023	469170.347612	44.740173
3504.096532	469126.787403	44.745178
3503.802859	469179.210371	44.750183
3503.072071	469142.363094	44.755188
3503.658363	469123.155197	44.760193
3503.322733	469162.858268	44.765197
3503.618172	469112.716561	44.770202
3503.711272	469147.839286	44.775207
3503.266746	469131.228089	44.780212
3503.809648	469119.125525	44.785217
3503.350929	469144.194782	44.790221
3503.815746	469115.473837	44.795226
3503.480710	469156.799336	44.800231
3503.352258	469122.189174	44.805236
3503.914654	469149.277276	44.810241
3503.316758	469132.386101	44.815245
3503.867511	469122.259731	44.820250
3504.079538	469167.605720	44.825255
3503.517399	469136.258439	44.830260
3503.950111	469100.697586	44.835265
3503.786396	469125.821644	44.840269
3503.787571	469087.743101	44.845274
3503.848575	469113.490801	44.850279
3503.731163	469102.506665	44.855284
3503.933181	469119.511065	44.860289
3503.625534	469086.551678	44.865293
3503.678282	469077.518072	44.870298
3503.872244	469089.706931	44.875303
3503.575255	469060.142953	44.880308
3503.599657	469094.059741	44.885313
3503.460351	469084.093126	44.890317
3504.058053	469053.272247	44.895322
3503.717817	469096.170500	44.900327
3503.516152	469076.022329	44.905332
3503.548938	469077.690327	44.910337
3503.338100	469091.616385	44.915341
3503.179844	469078.204923	44.920346
3503.716842	469103.421068	44.925351
3502.987216	469077.424039	44.930356
3503.507202	469062.840589	44.935361
3503.474288	469101.633968	44.940365
3503.541221	469067.956200	44.945370
3503.543700	469062.581190	44.950375
3503.541499	469096.451475	44.955380
3503.506582	469044.333680	44.960385
3503.475703	469076.890234	44.965389
3503.141146	469065.788291	44.970394
3503.349335	469055.158295	44.975399
3503.631961	469066.674006	44.980404
3503.777641	469094.639303	44.985409
3503.600111	469065.664894	44.990413
3503.945866	469032.602145	44.995418
3503.667415	469087.811637	45.000423
3503.372985	469079.593459	45.005428
3504.045534	469038.772125	45.010433
3503.851502	469083.979662	45.015437
3503.477741	469067.965672	45.020442
3503.903914	469075.098181	45.025447
3503.300537	469059.576810	45.030452
3503.803239	469012.545727	45.035457
3503.362749	469061.696453	45.040461
3503.599878	469019.828426	45.045466
3503.764899	469048.754097	45.050471
3503.252412	469048.733656	45.055476
3504.056338	469028.274385	45.060481
3503.610776	469046.648793	45.065485
3503.579171	469043.104496	45.070490
3503.637961	469044.464165	45.075495
3503.552092	469058.826825	45.080500
3503.480292	469033.587726	45.085505
3503.762633	469050.579486	45.090509
3503.869044	469039.052904	45.095514
3503.821060	469006.103051	45.100519
3503.443948	469025.430029	45.105524
3503.978584	469011.351265	45.110529
3503.952545	469001.265301	45.115533
3503.586990	469033.976229	45.120538
3504.257839	468984.383322	45.125543
3503.904959	469000.410747	45.130548
3504.176570	468971.872254	45.135553
3503.638125	468982.807937	45.140557
3503.845202	468980.797721	45.145562
3503.894131	468964.311211	45.150567
3503.522145	468964.522081	45.155572
3503.750563	468933.962211	45.160577
3503.207368	468956.509849	45.165581
3503.698690	468936.809753	45.170586
3503.785140	468930.305952	45.175591
3503.718535	468943.854383	45.180596
3503.599943	468937.180176	45.185601
3503.375687	468951.260560	45.190605
3503.898509	468915.989374	45.195610
3503.717734	468964.440126	45.200615
3503.593582	468938.448630	45.205620
3504.034720	468950.649205	45.210625
3503.868645	468916.298168	45.215629
3503.685125	468910.901815	45.220634
3503.462788	468913.877750	45.225639
3503.414321	468910.031872	45.230644
3503.846738	468907.073361	45.235649
3503.503943	468924.214737	45.240653
3503.628851	468907.361245	45.245658
3503.891880	468910.108351	45.250663
3503.424162	468933.049716	45.255668
3503.616827	468920.089726	45.260673
3503.839594	468886.741963	45.265677
3503.802320	468881.068966	45.270682
3503.696706	468886.257433	45.275687
3503.875887	468877.964317	45.280692
3504.017851	468878.144657	45.285697
3503.920846	468882.266979	45.290701
3503.679244	468867.144618	45.295706
3503.888044	468853.066547	45.300711
3503.552824	468860.623700	45.305716
3503.289052	468839.369628	45.310721
3503.576043	468844.901683	45.315725
3503.401666	468857.808051	45.320730
3503.456924	468840.559881	45.325735
3503.480694	468874.172900	45.330740
3503.594740	468849.816877	45.335745
3503.397255	468853.600158	45.340749
3503.314830	468868.418741	45.345754
3503.603478	468851.894252	45.350759
3503.360141	468867.143903	45.355764
3503.655337	468863.395809	45.360769
3503.678986	468849.904745	45.365773
3503.778222	468882.035403	45.370778
3503.521334	468858.549286	45.375783
3503.731710	468879.913111	45.380788
3503.918500	468861.985017	45.385793
3503.677667	468860.197698	45.390797
3503.510469	468828.179082	45.395802
3503.914948	468821.523571	45.400807
3503.274909	468846.419026	45.405812
3503.547674	468825.587177	45.410817
3503.434589	468849.030327	45.415821
3503.635070	468833.685954	45.420826
3503.364825	468850.613106	45.425831
3503.519223	468816.819702	45.430836
3503.757996	468853.795949	45.435841
3503.799051	468822.758491	45.440845
3503.571009	468858.338094	45.445850
3503.914645	468841.095048	45.450855
3503.417568	468818.356708	45.455860
3503.555604	468832.684132	45.460865
3503.611453	468798.145712	45.465869
3503.319630	468830.743893	45.470874
3503.944196	468796.419804	45.475879
3503.475373	468835.536096	45.480884
3503.578139	468809.356461	45.485889
3503.517032	468841.056187	45.490893
3503.515954	468814.588747	45.495898
3503.616083	468843.474255	45.500903
3503.664086	468830.283553	45.505908
3503.568727	468820.563388	45.510913
3503.803260	468836.853020	45.515917
3503.826498	468826.505662	45.520922
3503.792669	468796.696901	45.525927
3503.782259	468787.521040	45.530932
3503.755808	468800.758991	45.535937
3503.508950	468789.186701	45.540941
3503.203026	468797.753331	45.545946
3503.666201	468796.108253	45.550951
3503.416347	468794.119538	45.555956
3503.442673	468791.073084	45.560961
3503.648902	468798.544678	45.565965
3503.149044	468795.784211	45.570970
3503.539026	468812.353517	45.575975
3503.338116	468815.021854	45.580980
3503.830342	468783.862322	45.585985
3503.401173	468813.338574	45.590989
3503.480924	468799.331568	45.595994
3503.556273	468821.629471	45.600999
3503.611430	468804.533401	45.606004
3503.803600	468799.888904	45.611009
3503.339986	468791.393129	45.616013
3503.527351	468794.659253	45.621018
3503.843329	468765.099382	45.626023
3503.397101	468793.310751	45.631028
3504.029649	468766.438874	45.636033
3503.664219	468772.479704	45.641037
3503.609326	468763.868611	45.646042
3503.550163	468786.948376	45.651047
3503.600696	468763.616378	45.656052
3503.769141	468789.246086	45.661057
3503.732450	468754.316586	45.666061
3504.022405	468779.318648	45.671066
3503.943278	468745.004292	45.676071
3503.445135	468751.623852	45.681076
3504.012406	468740.429897	45.686081
3503.871256	468724.429582	45.691085
3503.553624	468743.798121	45.696090
3504.116167	468742.289446	45.701095
3503.981556	468712.597904	45.706100
3503.754598	468728.250702	45.711105
3503.926995	468688.623239	45.716109
3503.912396	468726.146805	45.721114
3503.953387	468689.531673	45.726119
3503.661881	468726.693370	45.731124
3504.026103	468658.083293	45.736129
3503.881334	468692.331697	45.741133
3503.625885	468681.166340	45.746138
3504.074981	468644.740149	45.751143
3503.892296	468677.169204	45.756148
3503.855568	468643.557844	45.761153
3504.061315	468612.037701	45.766157
3503.499536	468665.264900	45.771162
3503.786921	468648.131996	45.776167
3503.688159	468616.457172	45.781172
3503.846666	468651.468981	45.786177
3503.807678	468640.827140	45.791181
3503.670378	468608.904872	45.796186
3503.821791	468630.075453	45.801191
3503.530774	468587.681587	45.806196
3503.736875	468598.499785	45.811201
3503.593719	468604.454826	45.816205
3503.526162	468604.313353	45.821210
3503.935099	468598.468342	45.826215
3503.728325	468606.867264	45.831220
3503.740884	468618.375204	45.836225
3504.065363	468561.433164	45.841229
3503.785415	468572.885954	45.846234
3503.712467	468561.995916	45.851239
3503.510027	468568.873024	45.856244
3503.563418	468576.520969	45.861249
3503.699663	468559.513292	45.866253
3503.140678	468594.638603	45.871258
3503.733583	468554.690898	45.876263
3503.371781	468565.953810	45.881268
3503.816580	468583.325910	45.886273
3503.853709	468556.345058	45.891277
3503.170888	468576.075703	45.896282
3503.698098	468547.394824	45.901287
3503.553296	468567.192553	45.906292
3503.594860	468513.945846	45.911297
3503.292320	468555.216689	45.916301
3503.297174	468531.739538	45.921306
3503.636582	468543.601497	45.926311
3503.584084	468516.229121	45.931316
3503.608048	468560.896279	45.936321
3503.540993	468545.492573	45.941325
3503.771785	468535.923544	45.946330
3503.724212	468557.835517	45.951335
3503.612852	468534.528853	45.956340
3504.043984	468537.300144	45.961345
3503.692643	468575.587072	45.966349
3503.780133	468528.417715	45.971354
3503.957553	468543.601095	45.976359
3503.732938	468502.109248	45.981364
3503.650709	468527.981716	45.986369
3503.853724	468496.816766	45.991373
3503.541685	468545.542757	45.996378
3503.457491	468518.276803	46.001383
3503.654253	468524.330254	46.006388
3503.746100	468507.126732	46.011393
3503.836527	468516.036469	46.016397
3503.895919	468472.978527	46.021402
3503.870510	468487.788366	46.026407
3503.949249	468477.837704	46.031412
3503.891296	468473.232670	46.036417
3503.911011	468485.246603	46.041421
3503.869500	468438.705894	46.046426
3503.849052	468468.067323	46.051431
3503.829274	468423.906282	46.056436
3503.893605	468459.744579	46.061441
3503.762414	468428.023891	46.066445
3503.305746	468461.967033	46.071450
3504.006979	468425.602019	46.076455
3503.738158	468439.740494	46.081460
3503.729519	468390.050766	46.086465
3503.634332	468407.812593	46.091469
3503.689079	468408.361659	46.096474
3503.851101	468384.453861	46.101479
3503.874645	468415.887324	46.106484
3503.878435	468397.176476	46.111489
3503.946492	468361.164957	46.116493
3503.669789	468392.290974	46.121498
3504.026260	468360.645221	46.126503
3503.725760	468369.819631	46.131508
3503.443819	468370.421915	46.136513
3503.831624	468371.374686	46.141517
3503.440244	468395.927139	46.146522
3503.910121	468362.691602	46.151527
3503.614720	468355.943746	46.156532
3503.742099	468361.196926	46.161537
3503.747145	468321.037464	46.166541
3503.642243	468356.040694	46.171546
3503.918635	468321.517337	46.176551
3503.858087	468340.389265	46.181556
3503.789399	468335.025317	46.186561
3503.795632	468341.615990	46.191565
3503.634589	468316.035196	46.196570
3503.554686	468318.836585	46.201575
3503.538055	468288.821563	46.206580
3503.558617	468330.447420	46.211585
3503.519494	468301.095140	46.216589
3503.284228	468331.859760	46.221594
3503.873271	468301.546202	46.226599
3503.629101	468331.298121	46.231604
3503.477465	468329.293837	46.236609
3503.621590	468315.479155	46.241613
3503.558881	468338.255741	46.246618
3503.914031	468318.069537	46.251623
3503.871207	468309.456350	46.256628
3503.784189	468275.750939	46.261633
3503.549661	468285.219191	46.266637
3503.636773	468284.647625	46.271642
3503.710094	468281.644375	46.276647
3503.843621	468275.690690	46.281652
3503.749834	468288.179025	46.286657
3504.171233	468250.843831	46.291661
3503.552539	468279.336676	46.296666
3503.533631	468277.362113	46.301671
3503.163915	468247.656369	46.306676
3503.928931	468223.095317	46.311681
3503.789772	468238.126134	46.316685
3503.402572	468286.611076	46.321690
3503.701975	468274.597221	46.326695
3503.748583	468284.325270	46.331700
3503.366854	468281.647473	46.336705
3503.801772	468267.330447	46.341709
3503.864480	468271.579761	46.346714
3503.459258	468240.814803	46.351719
3503.524275	468222.651884	46.356724
3503.815340	468195.529021	46.361729
3503.689105	468237.634615	46.366733
3503.629691	468241.548299	46.371738
3503.178008	468215.607677	46.376743
3503.094127	468208.674224	46.381748
3503.288676	468194.750081	46.386753
3503.448794	468230.472217	46.391757
3503.618160	468196.066982	46.396762
3503.587755	468245.560443	46.401767
3503.286942	468229.990631	46.406772
3503.875049	468205.508227	46.411777
3503.783852	468239.292550	46.416781
3503.754642	468212.575270	46.421786
3503.990646	468241.135896	46.426791
3504.204808	468207.585594	46.431796
3503.461135	468233.765794	46.436801
3503.286395	468202.457294	46.441805
3503.667740	468184.193637	46.446810
3503.759994	468223.120972	46.451815
3503.638470	468217.106172	46.456820
3503.551015	468179.648459	46.461825
3503.391097	468214.153565	46.466829
3503.314710	468187.038064	46.471834
3503.620946	468211.328349	46.476839
3503.505783	468200.089857	46.481844
3503.519172	468173.771440	46.486849
3503.773950	468198.475520	46.491853
3503.395720	468218.868234	46.496858
3503.830002	468186.601453	46.501863
3504.004429	468166.595786	46.506868
3503.746900	468140.928618	46.511873
3503.889725	468132.235309	46.516877
3503.322142	468193.628256	46.521882
3503.465786	468169.824531	46.526887
3503.721957	468138.194297	46.531892
3503.747721	468172.568710	46.536897
3503.457718	468169.622871	46.541901
3503.638595	468152.455693	46.546906
3503.669094	468184.699694	46.551911
3503.630188	468189.066498	46.556916
3503.494412	468178.794660	46.561921
3503.495544	468148.979454	46.566925
3503.326263	468151.642875	46.571930
3503.635733	468116.809719	46.576935
3503.593360	468141.560833	46.581940
3503.604887	468157.784829	46.586945
3503.680437	468126.183126	46.591949
3503.881323	468119.052516	46.596954
3503.804613	468161.150435	46.601959
3504.002670	468134.346429	46.606964
3503.779116	468128.449143	46.611969
3503.810719	468144.517858	46.616973
3503.339166	468107.070021	46.621978
3504.016172	468081.559304	46.626983
3503.895105	468112.052664	46.631988
3503.789065	468086.361485	46.636993
3503.530157	468132.139090	46.641997
3503.451204	468115.215774	46.647002
3504.142821	468077.026267	46.652007
3503.793739	468116.936263	46.657012
3503.435855	468097.673845	46.662017
3504.032603	468044.338197	46.667021
3503.732774	468085.913767	46.672026
3503.582246	468062.055005	46.677031
3503.766180	468061.062481	46.682036
3503.665350	468083.591838	46.687041
3503.807586	468057.506440	46.692045
3503.494459	468054.919182	46.697050
3503.533605	468051.363535	46.702055
3503.511959	468013.185239	46.707060
3503.538506	468042.590540	46.712065
3503.853204	468007.401434	46.717069
3503.530826	468037.115424	46.722074
3503.396215	468046.517284	46.727079
3503.718079	468023.800757	46.732084
3504.016398	468017.212479	46.737089
3503.826316	468060.849703	46.742093
3503.578456	468069.711686	46.747098
3503.707602	468035.718194	46.752103
3503.809434	467990.776432	46.757108
3503.569594	467976.768687	46.762113
3503.792498	467999.956851	46.767117
3503.469734	468016.385913	46.772122
3503.825064	467977.640907	46.777127
3503.670642	468015.796315	46.782132
3503.916635	467986.347825	46.787137
3503.913641	468008.811092	46.792141
3503.696254	467991.047553	46.797146
3503.635837	468000.894062	46.802151
3503.610698	467976.204085	46.807156
3503.429553	467958.384083	46.812161
3503.604933	467941.978197	46.817165
3503.192213	467990.670679	46.822170
3503.121941	467966.900536	46.827175
3503.857162	467950.913231	46.832180
3503.773250	467938.351296	46.837185
3503.949505	467933.861244	46.842189
3503.428731	467938.202850	46.847194
3503.771297	467955.997280	46.852199
3503.763323	467993.571812	46.857204
3503.402516	467972.433612	46.862209
3503.806132	467950.059028	46.867213
3503.811748	467956.954156	46.872218
3503.803572	467961.417561	46.877223
3503.877835	467926.722681	46.882228
3503.859298	467904.009122	46.887233
3503.888908	467923.729182	46.892237
3503.587128	467951.868139	46.897242
3503.407649	467923.957294	46.902247
3503.857086	467880.075893	46.907252
3503.862047	467874.091709	46.912257
3504.004640	467899.168818	46.917261
3503.757858	467913.963345	46.922266
3503.915601	467914.191906	46.927271
3503.673236	467917.881035	46.932276
3503.133357	467906.405278	46.937281
3503.125052	467895.301852	46.942285
3502.949835	467910.744253	46.947290
3503.054370	467897.645444	46.952295
3503.518587	467868.567948	46.957300
3503.517768	467887.735080	46.962305
3503.793517	467909.038853	46.967309
3503.382010	467938.868482	46.972314
3503.657508	467941.005270	46.977319
3503.565963	467945.684682	46.982324
3503.950862	467925.189162	46.987329
3503.605672	467898.673547	46.992333
3503.758960	467892.412392	46.997338
3503.856410	467906.442625	47.002343
3503.804874	467880.134103	47.007348
3503.346561	467884.415142	47.012353
3503.847416	467851.528848	47.017357
3503.888527	467872.109149	47.022362
3503.560587	467892.595642	47.027367
3504.053327	467866.961672	47.032372
3503.461847	467873.139901	47.037377
3503.985490	467821.488558	47.042381
3503.558013	467857.861974	47.047386
3503.624771	467826.971103	47.052391
3503.673020	467838.625948	47.057396
3503.790596	467824.054543	47.062401
3503.824716	467872.879495	47.067405
3503.451027	467865.586084	47.072410
3503.633600	467843.956216	47.077415
3503.894187	467811.310663	47.082420
3503.890506	467825.356935	47.087425
3504.136033	467805.441101	47.092429
3503.664380	467787.058393	47.097434
3503.702504	467819.098922	47.102439
3504.242773	467802.787373	47.107444
3503.755863	467810.673116	47.112449
3503.724961	467772.647968	47.117453
3503.625118	467784.224838	47.122458
3503.645747	467753.239736	47.127463
3503.775824	467772.690523	47.132468
3503.538061	467778.863577	47.137473
3503.820297	467772.683419	47.142477
3503.598977	467765.923663	47.147482
3503.678246	467770.931062	47.152487
3503.842397	467728.666346	47.157492
3503.638999	467762.215634	47.162497
3503.736121	467721.888356	47.167501
3503.299898	467721.703734	47.172506
3503.464299	467750.935531	47.177511
3503.445710	467743.433830	47.182516
3503.660533	467730.317485	47.187521
3503.677158	467745.121203	47.192525
3503.899389	467727.085128	47.197530
3503.607015	467759.887881	47.202535
3503.474356	467739.220452	47.207540
3503.388956	467738.371898	47.212545
3503.872172	467746.712809	47.217549
3503.715031	467714.589493	47.222554
3503.864438	467704.120227	47.227559
3503.904901	467704.874398	47.232564
3503.553768	467702.495930	47.237569
3503.832717	467693.730218	47.242573
3503.602111	467714.911395	47.247578
3503.800718	467702.406078	47.252583
3504.094318	467673.963765	47.257588
3503.732968	467689.587869	47.262593
3503.655539	467665.311448	47.267597
3503.445862	467656.673659	47.272602
3503.390131	467673.922799	47.277607
3503.937436	467658.928407	47.282612
3503.944554	467664.809254	47.287617
3504.039372	467674.631379	47.292621
3503.791681	467644.144890	47.297626
3503.765725	467634.565327	47.302631
3504.011985	467633.715053	47.307636
3503.876075	467638.148010	47.312641
3503.849018	467643.476486	47.317645
3503.683163	467632.752774	47.322650
3503.792237	467631.062164	47.327655
3503.750983	467606.830665	47.332660
3503.755186	467593.798233	47.337665
3503.758331	467607.590035	47.342669
3503.892686	467588.401468	47.347674
3503.806800	467593.333598	47.352679
3503.574514	467594.992905	47.357684
3503.792481	467587.200222	47.362689
3503.760279	467554.296308	47.367693
3503.282967	467560.253752	47.372698
3503.638262	467550.563183	47.377703
3503.652475	467545.693004	47.382708
3503.236455	467566.599393	47.387713
3503.523965	467537.295836	47.392717
3503.682927	467565.311776	47.397722
3503.571883	467552.246827	47.402727
3503.850334	467542.974059	47.407732
3503.545179	467564.877071	47.412737
3503.835479	467552.154344	47.417741
3503.491941	467543.943325	47.422746
3503.750242	467560.787970	47.427751
3503.941784	467535.657571	47.432756
3503.433032	467524.937294	47.437761
3503.745338	467517.332504	47.442765
3503.918458	467523.897054	47.447770
3503.673386	467530.426287	47.452775
3503.706906	467526.567197	47.457780
3503.624618	467516.590826	47.462785
3503.933620	467515.882752	47.467789
3503.376142	467519.723172	47.472794
3503.445006	467524.732273	47.477799
3503.801011	467488.115969	47.482804
3503.463394	467491.110324	47.487809
3503.570675	467492.766673	47.492813
3503.569820	467488.659473	47.497818
3503.627159	467471.409853	47.502823
3503.602277	467502.446673	47.507828
3503.375965	467500.099161	47.512833
3503.700882	467484.734138	47.517837
3503.421485	467481.482281	47.522842
3503.368187	467493.153368	47.527847
3503.564663	467475.678930	47.532852
3503.536867	467521.218500	47.537857
3503.590867	467473.088635	47.542861
3503.617117	467520.597253	47.547866
3503.490698	467505.607828	47.552871
3503.492047	467480.507425	47.557876
3503.228102	467509.959384	47.562881
3503.669357	467477.842540	47.567885
3503.491950	467500.384623	47.572890
3503.365176	467515.566119	47.577895
3503.826989	467488.871725	47.582900
3503.648035	467520.693482	47.587905
3503.573023	467481.407098	47.592909
3503.684729	467436.006227	47.597914
3503.795038	467486.037012	47.602919
3503.497435	467452.363569	47.607924
3503.646040	467447.522833	47.612929
3503.643742	467480.280170	47.617933
3503.564787	467469.035564	47.622938
3503.195152	467483.342736	47.627943
3503.685956	467449.291136	47.632948
3503.531466	467449.721177	47.637953
3503.561282	467486.783564	47.642957
3503.485308	467479.848621	47.647962
3503.906068	467439.063989	47.652967
3503.663382	467439.457263	47.657972
3503.545197	467464.322569	47.662977
3503.780146	467437.106187	47.667981
3503.610755	467423.543306	47.672986
3503.800435	467426.454325	47.677991
3503.529934	467435.573690	47.682996
3503.857157	467417.977124	47.688001
3503.880295	467422.283572	47.693005
3503.580977	467446.061963	47.698010
3503.821089	467427.414316	47.703015
3503.681844	467409.790058	47.708020
3503.661396	467410.148206	47.713025
3503.641575	467393.164256	47.718029
3503.625430	467381.960384	47.723034
3503.489952	467405.915755	47.728039
3503.758789	467399.230531	47.733044
3503.411846	467393.656786	47.738049
3503.873314	467399.009523	47.743053
3503.840576	467377.007549	47.748058
3503.557589	467415.133656	47.753063
3503.591532	467385.413600	47.758068
3503.427596	467392.589250	47.763073
3504.126380	467361.192138	47.768077
3503.613787	467363.859214	47.773082
3503.491978	467363.320645	47.778087
3503.731962	467362.522060	47.783092
3503.735860	467370.127559	47.788097
3503.908849	467352.301778	47.793101
3503.461151	467358.153183	47.798106
3503.556081	467359.608664	47.803111
3503.839612	467349.574393	47.808116
3503.482694	467354.701541	47.813121
3503.491334	467334.315629	47.818125
3503.377214	467320.236868	47.823130
3503.437520	467340.104744	47.828135
3503.647623	467334.138690	47.833140
3503.503813	467327.214420	47.838145
3503.652441	467320.446755	47.843149
3503.634950	467337.132339	47.848154
3503.476801	467336.802344	47.853159
3503.865700	467338.617024	47.858164
3503.613417	467336.527137	47.863169
3503.688383	467334.182694	47.868173
3503.619026	467344.335168	47.873178
3503.104735	467361.555627	47.878183
3503.385248	467338.439239	47.883188
3503.575538	467337.902047	47.888193
3503.458612	467345.729483	47.893197
3503.772485	467351.511223	47.898202
3503.510829	467340.295426	47.903207
3503.715664	467331.591987	47.908212
3503.550615	467324.062579	47.913217
3503.742264	467306.335225	47.918221
3503.700897	467304.972615	47.923226
3503.660659	467304.421151	47.928231
3503.692148	467291.029265	47.933236
3503.757041	467322.863485	47.938241
3503.670793	467316.994976	47.943245
3503.399286	467304.310191	47.948250
3503.598197	467319.085395	47.953255
3503.602989	467308.943039	47.958260
3503.157884	467326.000467	47.963265
3503.335660	467324.248266	47.968269
3503.410854	467313.993369	47.973274
3503.278624	467318.527226	47.978279
3503.554327	467319.092105	47.983284
3503.770310	467316.826786	47.988289
3503.768533	467285.743124	47.993293
3503.497594	467330.205964	47.998298
3503.350279	467278.152269	48.003303
3503.803047	467291.011175	48.008308
3503.616960	467286.983922	48.013313
3503.867666	467280.656480	48.018317
3503.481102	467294.763624	48.023322
3503.542459	467294.753888	48.028327
3503.453905	467272.202840	48.033332
3503.780073	467294.665548	48.038337
3503.765334	467300.245703	48.043341
3503.712888	467282.252665	48.048346
3503.683269	467311.008659	48.053351
3503.581785	467258.237761	48.058356
3503.458876	467253.693436	48.063361
3503.471569	467254.908383	48.068365
3503.734343	467239.755837	48.073370
3503.580785	467254.536090	48.078375
3503.938029	467268.373560	48.083380
3503.685686	467255.026514	48.088385
3503.566368	467232.429578	48.093389
3503.471199	467278.538108	48.098394
3503.419164	467242.898617	48.103399
3503.549667	467268.637589	48.108404
3503.418529	467260.798551	48.113409
3503.451820	467260.438296	48.118413
3503.583649	467254.535300	48.123418
3503.316519	467271.158979	48.128423
3503.293756	467257.369983	48.133428
3503.394452	467266.481458	48.138433
3503.271521	467268.275628	48.143437
3503.402840	467255.577851	48.148442
3503.451045	467279.909995	48.153447
3503.726607	467273.122252	48.158452
3503.804091	467274.529789	48.163457
3503.716604	467256.035187	48.168461
3503.907052	467234.454159	48.173466
3503.533163	467246.378887	48.178471
3503.892708	467240.338479	48.183476
3503.238522	467236.233079	48.188481
3503.825124	467222.854824	48.193485
3503.689043	467228.809134	48.198490
3503.453389	467246.289893	48.203495
3503.903853	467227.963778	48.208500
3503.427181	467250.604138	48.213505
3503.685800	467228.505249	48.218509
3503.862007	467208.954766	48.223514
3503.706340	467208.015881	48.228519
3503.764241	467196.850915	48.233524
3503.744348	467195.738444	48.238529
3503.388149	467204.820746	48.243533
3503.884372	467201.649083	48.248538
3503.826885	467187.510573	48.253543
3503.872883	467205.098973	48.258548
3503.462738	467164.140896	48.263553
3503.346198	467185.253865	48.268557
3503.440759	467153.850534	48.273562
3503.755325	467171.193679	48.278567
3503.505313	467181.425494	48.283572
3503.505625	467176.810968	48.288577
3503.733350	467149.189692	48.293581
3503.514992	467176.403747	48.298586
3503.639699	467178.767281	48.303591
3503.764332	467169.265121	48.308596
3503.996681	467152.291828	48.313601
3503.955260	467176.232593	48.318605
3504.191178	467128.630979	48.323610
3503.496996	467127.118000	48.328615
3503.829875	467100.950580	48.333620
3503.888785	467139.327393	48.338625
3503.893526	467115.392310	48.343629
3503.933507	467120.659614	48.348634
3503.630705	467088.558370	48.353639
3503.760519	467097.056814	48.358644
3503.516223	467086.649473	48.363649
3503.432659	467084.279350	48.368653
3503.616457	467093.580598	48.373658
3503.632726	467086.225279	48.378663
3504.014942	467085.556328	48.383668
3503.660973	467084.953030	48.388673
3503.606163	467095.762534	48.393677
3503.901444	467072.339271	48.398682
3503.374619	467089.004139	48.403687
3503.631796	467026.845636	48.408692
3502.976377	467071.268373	48.413697
3503.248562	467049.420696	48.418701
3503.344978	467063.755903	48.423706
3503.676278	467103.661687	48.428711
3503.755884	467069.065971	48.433716
3503.325388	467083.535157	48.438721
3503.817075	467044.361221	48.443725
3503.694708	467065.475232	48.448730
3503.785025	467062.570539	48.453735
3503.834118	467032.594051	48.458740
3503.604562	467062.903239	48.463745
3503.796921	467066.168844	48.468749
3503.589929	467061.029266	48.473754
3503.550500	467062.404588	48.478759
3503.953819	467039.217754	48.483764
3503.633291	467030.191562	48.488769
3503.642225	467030.798614	48.493773
3504.177691	467016.718394	48.498778
3503.792906	467016.779176	48.503783
3503.939860	467027.049738	48.508788
3503.824554	467014.137255	48.513793
3503.782980	466972.106379	48.518797
3503.930258	466994.496264	48.523802
3503.717518	466981.041368	48.528807
3503.890963	466970.720066	48.533812
3503.785728	466996.141671	48.538817
3503.607789	466980.399388	48.543821
3503.626213	466961.583537	48.548826
3503.487832	466953.999073	48.553831
3503.945572	466939.778961	48.558836
3503.892437	466952.464494	48.563841
3503.424148	466929.618142	48.568845
3503.485748	466960.135000	48.573850
3503.728068	466933.728145	48.578855
3503.795879	466935.289359	48.583860
3503.415086	466955.785112	48.588865
3503.604401	466939.071994	48.593869
3503.767991	466928.549395	48.598874
3503.472353	466952.429176	48.603879
3503.562788	466896.381686	48.608884
3503.290755	466929.892433	48.613889
3503.826127	466909.017186	48.618893
3503.615063	466882.935473	48.623898
3503.592767	466926.447100	48.628903
3503.742614	466899.547730	48.633908
3503.408042	466908.018234	48.638913
3503.595732	466913.312952	48.643917
3503.815603	466889.394319	48.648922
3503.096573	466924.902661	48.653927
3503.346303	466883.484779	48.658932
3503.775640	466931.843767	48.663937
3503.645031	466901.134865	48.668941
3503.836885	466877.423482	48.673946
3503.637374	466922.737937	48.678951
3503.742419	466883.016311	48.683956
3503.624028	466905.042612	48.688961
3503.816819	466865.408502	48.693965
3503.709423	466880.232428	48.698970
3503.864545	466863.626073	48.703975
3503.601636	466853.677938	48.708980
3503.659869	466885.513868	48.713985
3503.808965	466873.624394	48.718989
3503.349644	466861.780371	48.723994
3503.350225	466894.588868	48.728999
3504.078785	466859.687401	48.734004
3503.431661	466840.469550	48.739009
3503.537092	466847.450681	48.744013
3503.886214	466846.482701	48.749018
3503.207232	466830.768792	48.754023
3503.874788	466822.093423	48.759028
3503.285131	466855.147403	48.764033
3503.471442	466821.548594	48.769037
3503.290496	466846.931635	48.774042
3503.119444	466823.277552	48.779047
3503.541858	466832.946871	48.784052
3503.326315	466850.221941	48.789057
3503.310524	466842.263098	48.794061
3503.800656	466833.818614	48.799066
3503.300815	466865.083568	48.804071
3503.611270	466829.386085	48.809076
3503.392588	466844.481171	48.814081
3503.533827	466860.888497	48.819085
3503.692430	466839.007846	48.824090
3503.367758	466858.328517	48.829095
3503.343266	466849.052620	48.834100
3503.644881	466846.925844	48.839105
3503.534107	466842.278093	48.844109
3503.462817	466867.339525	48.849114
3503.450897	466861.712685	48.854119
3503.267159	466838.364878	48.859124
3503.708848	466872.422121	48.864129
3503.513690	466844.309491	48.869133
3503.457399	466864.297661	48.874138
3503.732044	466862.682238	48.879143
3503.858938	466849.122866	48.884148
3503.860476	466846.435012	48.889153
3503.449784	466847.919739	48.894157
3503.612140	466819.091351	48.899162
3503.280613	466818.535207	48.904167
3503.487210	466834.273006	48.909172
3503.561588	466833.449869	48.914177
3503.118992	466837.880759	48.919181
3503.652737	466801.184465	48.924186
3503.107894	466838.845908	48.929191
3503.249264	466808.398136	48.934196
3503.530157	466828.840134	48.939201
3503.443415	466835.699517	48.944205
3503.399076	466812.988865	48.949210
3503.403793	466838.900369	48.954215
3503.654296	466824.053720	48.959220
3503.507457	466831.176148	48.964225
3503.328759	466837.390848	48.969229
3503.779923	466828.090469	48.974234
3503.399871	466831.700130	48.979239
3503.341510	466834.650437	48.984244
3503.604257	466831.515623	48.989249
3503.429161	466836.056359	48.994253
3503.558283	466837.405054	48.999258
3503.901858	466827.817426	49.004263
3503.477711	466830.774841	49.009268
3503.719706	466840.168419	49.014273
3503.695119	466853.103044	49.019277
3503.799711	466852.528677	49.024282
3503.754992	466805.173530	49.029287
3503.576700	466824.014714	49.034292
3503.174256	466790.306079	49.039297
3503.618373	466801.138290	49.044301
3503.296407	466794.292712	49.049306
3503.519714	466811.194196	49.054311
3503.612996	466788.664601	49.059316
3503.589841	466806.365680	49.064321
3503.812838	466807.344576	49.069325
3504.035265	466790.271144	49.074330
3503.608863	466804.841290	49.079335
3503.543341	466812.965052	49.084340
3503.956533	466803.822791	49.089345
3503.672664	466784.648891	49.094349
3503.690585	466781.096386	49.099354
3503.283160	466795.917084	49.104359
3503.761663	466771.044675	49.109364
3503.787740	466767.744424	49.114369
3503.453191	466793.202517	49.119373
3503.652470	466755.088447	49.124378
3503.583017	466801.954587	49.129383
3503.625885	466781.410605	49.134388
3503.625105	466789.169179	49.139393
3503.747233	466786.614385	49.144397
3503.999963	466777.852439	49.149402
3503.856021	466761.039728	49.154407
3503.837415	466744.105774	49.159412
3503.561186	466744.250816	49.164417
3503.480822	466736.403558	49.169421
3503.994253	466739.314210	49.174426
3503.425221	466753.095589	49.179431
3503.536069	466748.717043	49.184436
3503.562539	466728.429148	49.189441
3503.292090	466732.427176	49.194445
3503.426740	466743.054785	49.199450
3503.379334	466750.212233	49.204455
3503.426039	466732.050927	49.209460
3503.410951	466756.444386	49.214465
3502.837767	466725.450219	49.219469
3503.265877	466752.968310	49.224474
3503.243841	466731.775320	49.229479
3503.282204	466752.103600	49.234484
3503.426805	466749.545249	49.239489
3503.294710	466739.373547	49.244493
3503.243246	466740.700082	49.249498
3503.424490	466756.391238	49.254503
3503.683162	466737.993597	49.259508
3503.337871	466769.639936	49.264513
3503.209148	466737.967026	49.269517
3503.616268	466765.133455	49.274522
3503.219076	466748.056508	49.279527
3503.276024	466766.708433	49.284532
3503.279875	466759.253546	49.289537
3503.424519	466739.606201	49.294541
3503.860809	466723.208840	49.299546
3503.407556	466737.479021	49.304551
3503.931977	466763.460601	49.309556
3503.732584	466770.134974	49.314561
3503.158677	466755.367874	49.319565
3503.963138	466722.736096	49.324570
3503.933534	466771.015863	49.329575
3503.268002	466746.273543	49.334580
3502.918348	466735.984099	49.339585
3502.945354	466738.210997	49.344589
3503.290405	466744.038686	49.349594
3503.589448	466748.960880	49.354599
3503.792723	466753.340409	49.359604
3503.538458	466794.607060	49.364609
3503.078939	466787.478968	49.369613
3503.279622	466747.234881	49.374618
3503.373735	466772.625244	49.379623
3503.197945	466775.695538	49.384628
3503.218875	466754.343652	49.389633
3503.793385	466785.134656	49.394637
3503.948383	466751.692814	49.399642
3503.702741	466769.175544	49.404647
3503.771529	466791.324505	49.409652
3503.532204	466749.425861	49.414657
3503.443938	466763.638335	49.419661
3503.469009	466719.618768	49.424666
3503.334787	466736.627532	49.429671
3503.081459	466738.645194	49.434676
3503.570537	466726.752609	49.439681
3503.484331	466737.212293	49.444685
3503.772616	466757.805319	49.449690
3503.448058	466739.753411	49.454695
3503.864890	466732.030401	49.459700
3503.519213	466750.391015	49.464705
3503.558416	466730.354654	49.469709
3503.562675	466744.349680	49.474714
3503.727703	466722.822858	49.479719
3503.744793	466742.596707	49.484724
3503.442702	466769.317428	49.489729
3503.664039	466754.526049	49.494733
3503.640699	466744.134323	49.499738
3502.880463	466757.590957	49.504743
3503.433245	466732.402508	49.509748
3503.489619	466719.766965	49.514753
3503.228307	466776.754620	49.519757
3503.385107	466756.344733	49.524762
3502.757774	466748.127551	49.529767
3503.694494	466725.058901	49.534772
3503.799881	466730.214546	49.539777
3503.695097	466778.911852	49.544781
3503.726659	466749.647662	49.549786
3503.723724	466731.037819	49.554791
3503.452497	466757.652257	49.559796
3503.379577	466720.240367	49.564801
3503.568989	466690.139797	49.569805
3503.654415	466733.736211	49.574810
3503.340586	466727.802092	49.579815
3503.467910	466695.936521	49.584820
3503.674574	466726.075823	49.589825
3503.960767	466706.963876	49.594829
3503.674531	466726.684265	49.599834
3503.640718	466707.572190	49.604839
3503.729859	466745.539264	49.609844
3503.766861	466702.988343	49.614849
3503.411334	466734.382807	49.619853
3503.941214	466698.498294	49.624858
3503.342299	466708.379810	49.629863
3503.127359	466691.324720	49.634868
3503.527397	466673.107515	49.639873
3503.361736	466702.443642	49.644877
3503.452841	466678.798670	49.649882
3503.416984	466691.785885	49.654887
3503.434055	466674.389853	49.659892
3503.896952	466680.097514	49.664897
3503.157176	466683.358383	49.669901
3504.020435	466655.585303	49.674906
3503.694707	466696.052090	49.679911
3503.285793	466689.169513	49.684916
3503.591662	466674.922520	49.689921
3503.632002	466682.167540	49.694925
3503.775721	466708.057233	49.699930
3503.395617	466693.462295	49.704935
3503.699380	466657.816290	49.709940
3503.763864	466687.116061	49.714945
3503.382283	466709.437711	49.719949
3503.691384	466675.160042	49.724954
3503.896547	466672.896366	49.729959
3503.448764	466675.096898	49.734964
3503.917742	466631.869043	49.739969
3503.481184	466680.111922	49.744973
3503.244312	466650.890024	49.749978
3503.403331	466629.009091	49.754983
3503.295522	466671.571278	49.759988
3503.554907	466635.070191	49.764993
3503.450623	466659.680698	49.769997
3503.393347	466661.616669	49.775002
3503.113976	466660.849439	49.780007
3503.570130	466638.313039	49.785012
3503.242558	466668.334027	49.790017
3503.356365	466641.186479	49.795021
3503.654741	466674.861017	49.800026
3503.792520	466666.877835	49.805031
3503.790362	466659.068896	49.810036
3503.828116	466672.754418	49.815041
3503.429462	466659.785087	49.820045
3503.828022	466659.569925	49.825050
3503.601271	466678.063932	49.830055
3503.717620	466638.238643	49.835060
3503.446811	466654.761967	49.840065
3503.316152	466648.088941	49.845069
3503.612170	466646.875799	49.850074
3503.549126	466655.658451	49.855079
3503.169393	466649.329051	49.860084
3503.722325	466610.043216	49.865089
3503.660720	466650.062668	49.870093
3503.270608	466631.716772	49.875098
3503.758072	466614.702726	49.880103
3503.438804	466626.467039	49.885108
3503.636396	466618.017999	49.890113
3503.439240	466628.241726	49.895117
3503.488518	466626.357650	49.900122
3503.569317	466612.653285	49.905127
3503.484517	466654.400517	49.910132
3503.178628	466629.499796	49.915137
3503.847218	466606.017013	49.920141
3503.496678	466648.769740	49.925146
3503.145817	466635.894259	49.930151
3504.167797	466605.966230	49.935156
3503.934701	466601.287052	49.940161
3503.125701	466620.532363	49.945165
3503.465571	466660.691176	49.950170
3502.990552	466649.305899	49.955175
3502.943267	466641.149120	49.960180
3503.842639	466606.575205	49.965185
3503.716281	466640.671897	49.970189
3503.658443	466617.608203	49.975194
3503.546942	466644.958179	49.980199
3503.739970	466647.209554	49.985204
3503.100548	466606.235927	49.990209
3503.428640	466587.320089	49.995213
3503.567605	466615.999670	50.000218
3503.486474	466589.136416	50.005223
3503.517005	466621.332088	50.010228
3503.580565	466577.001885	50.015233
3503.689598	466620.138415	50.020237
3503.699282	466615.826542	50.025242
3503.372684	466605.279843	50.030247
3503.846579	466579.190910	50.035252
3503.689629	466607.308761	50.040257
3503.707030	466590.673251	50.045261
3503.597809	466632.221549	50.050266
3503.747250	466607.198123	50.055271
3503.871248	466565.241689	50.060276
3503.564433	466600.381160	50.065281
3503.218947	466564.229105	50.070285
3503.676946	466571.053181	50.075290
3503.343720	466551.633324	50.080295
3503.676702	466571.965918	50.085300
3503.365144	466578.353822	50.090305
3503.065467	466562.326212	50.095309
3503.292921	466578.618711	50.100314
3503.952161	466544.082649	50.105319
3503.676862	466587.584251	50.110324
3503.976705	466559.139456	50.115329
3503.525548	466592.932595	50.120333
3503.863818	466548.508202	50.125338
3503.850492	466597.343598	50.130343
3503.896158	466538.513214	50.135348
3503.736657	466548.426770	50.140353
3503.180180	466528.687211	50.145357
3503.540540	466536.540925	50.150362
3503.600886	466530.496897	50.155367
3503.338111	466515.934001	50.160372
3503.335565	466557.262745	50.165377
3503.155218	466568.498036	50.170381
3503.582809	466564.018679	50.175386
3503.398922	466559.179584	50.180391
3503.446294	466531.180334	50.185396
3504.048901	466496.703856	50.190401
3503.338371	466548.337182	50.195405
3503.390862	466556.087422	50.200410
3503.619189	466527.552469	50.205415
3503.501264	466558.960345	50.210420
3503.546276	466543.993851	50.215425
3503.560006	466520.310224	50.220429
3503.841952	466539.788850	50.225434
3503.562732	466552.662487	50.230439
3503.094460	466530.424216	50.235444
3503.638855	466518.573481	50.240449
3503.263546	466579.940718	50.245453
3503.413178	466571.651369	50.250458
3503.345075	466551.530381	50.255463
3503.601128	466539.623815	50.260468
3503.636298	466535.155767	50.265473
3503.470805	466583.153183	50.270477
3503.608463	466571.569605	50.275482
3503.566968	466521.221449	50.280487
3503.660760	466509.898320	50.285492
3503.323795	466531.452459	50.290497
3502.549174	466517.528272	50.295501
3503.474170	466519.156869	50.300506
3504.367187	466517.545100	50.305511
3503.707025	466508.623077	50.310516
3503.290527	466528.364239	50.315521
3503.230195	466533.039029	50.320525
3503.752656	466481.283187	50.325530
3503.779762	466478.946215	50.330535
3503.708816	466486.462441	50.335540
3503.476253	466467.736533	50.340545
3503.476794	466497.452351	50.345549
3503.142337	466539.797077	50.350554
3503.426150	466553.291655	50.355559
3503.539154	466527.361120	50.360564
3503.547664	466516.000764	50.365569
3503.006740	466518.723131	50.370573
3503.129164	466516.979613	50.375578
3503.005895	466524.960483	50.380583
3502.871479	466526.502982	50.385588
3503.796819	466501.762470	50.390593
3503.502390	466526.960992	50.395597
3503.325869	466548.794012	50.400602
3503.503498	466536.544871	50.405607
3503.171408	466521.080160	50.410612
3503.644662	466497.222455	50.415617
3503.565341	466509.861682	50.420621
3503.902960	466532.627648	50.425626
3503.834505	466555.914159	50.430631
3503.461044	466536.297809	50.435636
3504.099696	466500.801448	50.440641
3503.560644	466534.101475	50.445645
3503.297992	466555.288876	50.450650
3504.038837	466506.186188	50.455655
3503.808538	466511.141396	50.460660
3503.851439	466509.461156	50.465665
3503.734922	466471.903591	50.470669
3503.818046	466512.052556	50.475674
3503.715920	466486.105265	50.480679
3503.638510	466471.259489	50.485684
3503.968465	466510.050989	50.490689
3503.861554	466495.767701	50.495693
3503.433746	466460.135578	50.500698
3503.680333	466432.307549	50.505703
3503.654862	466483.782041	50.510708
3503.844073	466472.900198	50.515713
3503.394009	466475.405369	50.520717
3503.723750	466451.468876	50.525722
3504.364306	466433.264161	50.530727
3504.072484	466403.442088	50.535732
3503.686489	466364.354916	50.540737
3503.631690	466381.452830	50.545741
3503.216805	466330.656140	50.550746
3503.576778	466249.564215	50.555751
3503.215882	466217.217281	50.560756
3503.266877	466157.877897	50.565761
3502.890478	466070.207883	50.570765
3502.502159	465955.206151	50.575770
3503.184809	465837.904643	50.580775
3502.715641	465754.609167	50.585780
3502.514695	465655.195345	50.590785
3501.927234	465516.591024	50.595789
3501.995798	465361.907689	50.600794
3501.954856	465222.454388	50.605799
3501.418429	465096.061051	50.610804
3501.297410	464963.819979	50.615809
3500.618958	464777.098163	50.620813
3500.849554	464578.668171	50.625818
3500.356384	464428.986173	50.630823
3499.980330	464277.763167	50.635828
3499.756058	464044.102442	50.640833
3499.443932	463878.615441	50.645837
3498.931244	463683.489776	50.650842
3498.618595	463475.296480	50.655847
3498.061259	463260.191565	50.660852
3497.831405	463036.258541	50.665857
3496.855123	462836.177415	50.670861
3496.994626	462609.949987	50.675866
3497.386102	462370.138266	50.680871
3496.841138	462117.386133	50.685876
3496.331528	461870.965558	50.690881
3495.635443	461628.426482	50.695885
3495.083681	461417.512277	50.700890
3494.406409	461145.850567	50.705895
3494.297578	460899.964338	50.710900
3493.960718	460623.829439	50.715905
3493.494051	460372.262083	50.720909
3492.969924	460108.780610	50.725914
3492.616651	459791.956544	50.730919
3492.023978	459513.819107	50.735924
3491.672728	459250.046399	50.740929
3491.058604	458982.355359	50.745933
3490.281141	458672.785556	50.750938
3490.297543	458361.361164	50.755943
3489.269231	458101.537178	50.760948
3488.838676	457811.684970	50.765953
3487.606950	457496.336614	50.770957
3487.961704	457175.964266	50.775962
3487.419754	456905.497302	50.780967
3486.810631	456613.882139	50.785972
3486.355147	456283.021937	50.790977
3485.372937	455962.234762	50.795981
3485.002706	455639.012468	50.800986
3484.117157	455341.995853	50.805991
3483.321554	455038.568338	50.810996
3483.096843	454690.296449	50.816001
3482.510580	454392.458995	50.821005
3481.596851	454095.937856	50.826010
3481.331833	453734.364204	50.831015
3480.721251	453438.091008	50.836020
3480.108486	453135.674705	50.841025
3479.323861	452786.041446	50.846029
3479.213197	452449.692224	50.851034
3478.360117	452112.389830	50.856039
3477.535486	451812.678932	50.861044
3477.364917	451449.227517	50.866049
3476.631986	451121.533031	50.871053
3475.827293	450783.442371	50.876058
3475.345700	450448.746464	50.881063
3474.711786	450097.120241	50.886068
3474.325807	449773.259396	50.891073
3472.929891	449430.878190	50.896077
3472.879086	449071.938013	50.901082
3472.063041	448766.857738	50.906087
3470.843713	448399.007692	50.911092
3470.720113	448032.501227	50.916097
3469.777533	447750.875035	50.921101
3469.024181	447418.919372	50.926106
3468.398177	447049.076595	50.931111
3468.157723	446682.516901	50.936116
3467.298861	446383.756893	50.941121
3466.432502	446046.572083	50.946125
3465.624612	445679.426800	50.951130
3465.600626	445315.806494	50.956135
3464.568963	445001.575442	50.961140
3464.064335	444680.455271	50.966145
3462.971397	444322.318558	50.971149
3462.186650	443974.990513	50.976154
3461.952323	443635.742988	50.981159
3461.125372	443334.097304	50.986164
3460.639284	442979.245769	50.991169
3459.676193	442629.896111	50.996173
3459.014625	442268.665779	51.001178
3458.575597	441930.137474	51.006183
3457.223200	441596.520806	51.011188
3457.331819	441216.674584	51.016193
3456.347084	440899.540046	51.021197
3455.687988	440586.284411	51.026202
3455.371837	440209.713511	51.031207
3454.221650	439899.395184	51.036212
3453.561121	439519.009769	51.041217
3452.770268	439203.117407	51.046221
3452.326426	438875.717334	51.051226
3451.402340	438512.772589	51.056231
3451.148766	438178.174470	51.061236
3450.363736	437858.532376	51.066241
3449.462512	437473.584221	51.071245
3448.673932	437148.627781	51.076250
3447.938014	436836.530295	51.081255
3447.112904	436471.153925	51.086260
3446.771747	436136.313981	51.091265
3446.060439	435843.038386	51.096269
3445.160743	435482.305634	51.101274
3444.757962	435111.663572	51.106279
3443.725339	434822.540059	51.111284
3442.904279	434432.810542	51.116289
3442.474872	434134.037268	51.121293
3441.524247	433794.438764	51.126298
3441.022383	433459.893786	51.131303
3440.095214	433159.765988	51.136308
3438.961454	432807.183129	51.141313
3438.280380	432465.036129	51.146317
3438.114391	432150.937721	51.151322
3437.620409	431858.674104	51.156327
3436.251252	431561.593979	51.161332
3436.000867	431215.324999	51.166337
3435.233784	430880.026893	51.171341
3434.673807	430517.647416	51.176346
3433.764943	430240.286636	51.181351
3432.790153	429916.639518	51.186356
3432.348677	429566.290508	51.191361
3431.453760	429226.242727	51.196365
3430.882495	428954.097213	51.201370
3430.307695	428611.070474	51.206375
3429.724073	428273.856368	51.211380
3429.192636	427981.708016	51.216385
3428.497913	427628.224353	51.221389
3427.421746	427292.548723	51.226394
3426.812140	427023.716559	51.231399
3425.848661	426712.651032	51.236404
3425.317641	426358.159661	51.241409
3424.404711	426071.968505	51.246413
3424.152471	425765.757622	51.251418
3422.968678	425428.145519	51.256423
3422.439696	425110.287635	51.261428
3421.798190	424826.834309	51.266433
3421.062003	424485.228270	51.271437
3420.547856	424181.453921	51.276442
3419.916926	423857.425430	51.281447
3419.286447	423547.210832	51.286452
3418.684027	423245.522910	51.291457
3417.843587	422905.666340	51.296461
3417.202970	422620.285017	51.301466
3416.631599	422311.266439	51.306471
3415.902283	421971.914269	51.311476
3415.268770	421702.881134	51.316481
3414.288042	421351.342766	51.321485
3413.758815	421071.110012	51.326490
3412.874873	420737.381247	51.331495
3412.339468	420448.252220	51.336500
3411.516455	420095.936471	51.341505
3410.894417	419816.493379	51.346509
3410.022108	419485.339106	51.351514
3409.634387	419204.938375	51.356519
3408.616072	418895.317714	51.361524
3407.938868	418582.311712	51.366529
3407.644843	418292.258724	51.371533
3406.821181	417957.369806	51.376538
3406.216405	417677.648897	51.381543
3405.174965	417362.171955	51.386548
3404.680680	417060.578452	51.391553
3403.775312	416773.299807	51.396557
3403.169236	416437.621982	51.401562
3402.582212	416163.168153	51.406567
3401.533227	415858.550148	51.411572
3401.424300	415531.243835	51.416577
3400.417701	415265.105306	51.421581
3400.016685	414929.326811	51.426586
3399.233941	414665.459555	51.431591
3398.323980	414351.199486	51.436596
3397.914397	414034.087374	51.441601
3397.258101	413735.508682	51.446605
3396.234127	413471.821304	51.451610
3395.530581	413142.803702	51.456615
3394.906531	412842.635495	51.461620
3394.308680	412584.666290	51.466625
3393.854074	412258.953661	51.471629
3393.160203	411977.667659	51.476634
3392.344179	411667.302896	51.481639
3391.518714	411372.513425	51.486644
3391.371421	411058.656948	51.491649
3390.100933	410786.853150	51.496653
3389.515021	410471.789327	51.501658
3388.828084	410168.707307	51.506663
3388.055965	409905.253602	51.511668
3387.525082	409584.936905	51.516673
3386.748377	409302.622531	51.521677
3386.063827	409011.701345	51.526682
3385.330992	408714.584168	51.531687
3384.759791	408423.258262	51.536692
3384.412168	408117.560838	51.541697
3383.458550	407836.277468	51.546701
3382.714401	407568.300915	51.551706
3382.047457	407238.781239	51.556711
3381.082461	406957.135858	51.561716
3380.723507	406668.631698	51.566721
3379.942794	406372.948199	51.571725
3379.391463	406096.287251	51.576730
3378.606331	405796.608757	51.581735
3377.798232	405504.657482	51.586740
3377.239529	405223.440528	51.591745
3376.946857	404928.377872	51.596749
3376.031191	404627.488876	51.601754
3375.295615	404362.355546	51.606759
3374.872087	404053.326115	51.611764
3373.929703	403770.276027	51.616769
3372.977108	403480.667293	51.621773
3372.448527	403196.682477	51.626778
3371.631548	402896.219001	51.631783
3370.821897	402612.375114	51.636788
3369.990850	402320.652360	51.641793
3369.982248	402056.223734	51.646797
3368.734706	401780.906186	51.651802
3368.359796	401469.429337	51.656807
3367.675322	401188.044201	51.661812
3367.532625	400915.823703	51.666817
3366.487496	400603.402320	51.671821
3365.934893	400350.205128	51.676826
3365.410281	400038.229854	51.681831
3364.194507	399763.983289	51.686836
3363.615957	399476.440312	51.691841
3363.648782	399153.666361	51.696845
3362.036089	398914.708956	51.701850
3362.054674	398599.659882	51.706855
3360.849714	398343.093097	51.711860
3360.551822	398024.555006	51.716865
3359.760691	397766.316759	51.721869
3359.075282	397463.774213	51.726874
3358.333124	397179.211616	51.731879
3357.439594	396908.017463	51.736884
3356.966145	396609.908096	51.741889
3356.335576	396354.023344	51.746893
3355.539753	396029.901123	51.751898
3355.125257	395781.020141	51.756903
3354.140439	395501.464784	51.761908
3353.808239	395213.541142	51.766913
3352.738299	394915.002720	51.771917
3352.253867	394654.353163	51.776922
3351.394521	394366.709143	51.781927
3350.516474	394063.963328	51.786932
3349.876748	393811.315328	51.791937
3349.525219	393516.185223	51.796941
3348.723439	393247.769658	51.801946
3347.940266	392990.841453	51.806951
3347.511594	392679.749142	51.811956
3346.396572	392430.725863	51.816961
3345.916948	392147.732610	51.821965
3345.646354	391855.931895	51.826970
3344.694722	391599.274359	51.831975
3343.887368	391302.214335	51.836980
3343.230434	391053.668236	51.841985
3342.862099	390731.157812	51.846989
3341.852879	390493.164938	51.851994
3341.405992	390222.941056	51.856999
3340.832595	389919.628110	51.862004
3340.161477	389639.086134	51.867009
3339.298639	389372.634086	51.872013
3338.487378	389095.415684	51.877018
3337.896655	388825.305709	51.882023
3337.013332	388534.515508	51.887028
3335.854163	388287.072174	51.892033
3335.690012	387998.376258	51.897037
3335.085299	387736.270560	51.902042
3334.587923	387474.603733	51.907047
3333.939811	387195.158049	51.912052
3333.217108	386914.781118	51.917057
3332.577601	386656.309658	51.922061
3331.769607	386378.001957	51.927066
3331.329068	386101.388750	51.932071
3330.392870	385837.287462	51.937076
3329.784907	385560.010056	51.942081
3329.019308	385289.901635	51.947085
3328.413080	385018.825097	51.952090
3327.752477	384743.889611	51.957095
3326.936834	384470.934857	51.962100
3326.484654	384213.256011	51.967105
3325.891756	383927.673346	51.972109
3325.108822	383655.546757	51.977114
3324.524571	383381.428497	51.982119
3323.730200	383111.537851	51.987124
3322.918066	382844.649157	51.992129
3322.393569	382578.221762	51.997133
3321.393427	382311.664264	52.002138
3321.086967	382039.094695	52.007143
3320.517620	381773.279189	52.012148
3319.928193	381490.678843	52.017153
3319.354683	381217.331811	52.022157
3318.552945	380958.668903	52.027162
3318.026908	380676.357790	52.032167
3317.250525	380405.733140	52.037172
3316.828078	380138.331686	52.042177
3315.959049	379860.163859	52.047181
3315.071820	379600.767853	52.052186
3314.345851	379303.522752	52.057191
3313.481382	379058.134270	52.062196
3312.897897	378765.339174	52.067201
3312.167204	378519.341179	52.072205
3311.230814	378240.689306	52.077210
3310.933539	377958.042715	52.082215
3309.984922	377718.077103	52.087220
3309.461565	377439.964784	52.092225
3309.042896	377174.450435	52.097229
3308.392688	376911.667227	52.102234
3307.671532	376634.903326	52.107239
3306.548028	376378.601558	52.112244
3306.162391	376102.086196	52.117249
3305.524055	375839.599399	52.122253
3304.732740	375585.453134	52.127258
3303.948350	375318.305603	52.132263
3303.588715	375052.768045	52.137268
3302.357078	374780.981771	52.142273
3301.822890	374542.636184	52.147277
3301.259753	374255.630527	52.152282
3300.699134	374022.093944	52.157287
3299.844851	373760.187678	52.162292
3299.034894	373484.001654	52.167297
3298.677589	373229.441551	52.172301
3297.730606	372983.393466	52.177306
3297.517388	372721.379306	52.182311
3296.820122	372457.633878	52.187316
3296.138129	372192.154502	52.192321
3295.333760	371937.759052	52.197325
3294.430602	371674.448340	52.202330
3294.006618	371410.805814	52.207335
3293.139709	371148.605476	52.212340
3292.306516	370902.043947	52.217345
3292.228521	370627.758738	52.222349
3291.128607	370363.656983	52.227354
3290.699630	370113.897820	52.232359
3290.229507	369852.847984	52.237364
3289.701037	369590.839047	52.242369
3288.820790	369346.387684	52.247373
3288.540465	369067.774162	52.252378
3287.626809	368783.331170	52.257383
3286.665656	368541.915643	52.262388
3286.331752	368270.861695	52.267393
3285.706440	367998.910821	52.272397
3284.628227	367736.647014	52.277402
3283.908771	367485.265074	52.282407
3283.230332	367223.978145	52.287412
3282.658694	366952.546668	52.292417
3281.962139	366696.068156	52.297421
3281.083947	366465.594019	52.302426
3280.850095	366185.835570	52.307431
3279.806762	365935.615655	52.312436
3278.941345	365680.150352	52.317441
3278.619700	365415.743306	52.322445
3277.877032	365162.469255	52.327450
3277.281347	364899.832722	52.332455
3276.406315	364649.528233	52.337460
3275.924801	364398.931144	52.342465
3275.388866	364119.411351	52.347469
3274.364086	363892.764010	52.352474
3273.980052	363603.980819	52.357479
3273.230376	363360.748508	52.362484
3272.333994	363104.459572	52.367489
3272.001769	362861.158631	52.372493
3271.178224	362583.252681	52.377498
3270.684924	362329.160355	52.382503
3269.898457	362079.413273	52.387508
3269.394916	361811.274016	52.392513
3268.707110	361550.490696	52.397517
3267.836583	361297.877454	52.402522
3267.349590	361059.426399	52.407527
3266.553644	360771.225380	52.412532
3265.840080	360542.578825	52.417537
3265.233602	360250.476920	52.422541
3264.374928	360031.545895	52.427546
3264.152557	359760.907857	52.432551
3263.213023	359497.761258	52.437556
3262.524244	359245.439329	52.442561
3262.141198	358986.706028	52.447565
3261.525270	358749.230983	52.452570
3260.903108	358464.576829	52.457575
3259.924340	358212.473595	52.462580
3259.123569	357962.503952	52.467585
3258.725134	357698.167910	52.472589
3257.863176	357450.317516	52.477594
3257.205297	357197.165926	52.482599
3256.808951	356937.227996	52.487604
3256.018553	356672.210548	52.492609
3255.134951	356416.291448	52.497613
3254.293176	356173.139483	52.502618
3253.682021	355906.486434	52.507623
3253.242867	355656.066410	52.512628
3252.543920	355408.561952	52.517633
3252.005167	355140.442882	52.522637
3251.062341	354906.360649	52.527642
3250.539964	354635.462431	52.532647
3250.312856	354396.607505	52.537652
3249.319281	354138.149516	52.542657
3248.428877	353878.783197	52.547661
3247.717600	353614.780889	52.552666
3247.500035	353369.659168	52.557671
3246.578159	353123.400671	52.562676
3245.629398	352868.186910	52.567681
3245.455291	352601.269621	52.572685
3244.829373	352350.150659	52.577690
3243.896400	352082.994507	52.582695
3243.501564	351827.153683	52.587700
3242.466316	351575.943135	52.592705
3242.123188	351327.955971	52.597709
3241.240169	351072.595996	52.602714
3240.766685	350807.600507	52.607719
3240.503051	350549.900425	52.612724
3239.387041	350297.169671	52.617729
3238.714062	350033.118223	52.622733
3237.872792	349778.712744	52.627738
3237.103667	349517.550038	52.632743
3236.346017	349272.978730	52.637748
3235.841483	349024.243131	52.642753
3235.534263	348763.411046	52.647757
3234.658584	348519.033265	52.652762
3233.917665	348252.286200	52.657767
3233.135734	347997.990475	52.662772
3232.392256	347755.268315	52.667777
3232.246259	347496.771930	52.672781
3231.264000	347243.446252	52.677786
3230.881839	346986.104823	52.682791
3229.906615	346729.059674	52.687796
3229.359170	346465.506138	52.692801
3228.488497	346210.478370	52.697805
3227.637644	345960.027899	52.702810
3226.945199	345717.416328	52.707815
3226.537047	345467.402778	52.712820
3225.831989	345222.525808	52.717825
3225.237383	344961.900079	52.722829
3224.455343	344710.389793	52.727834
3223.903951	344455.380247	52.732839
3223.230676	344213.955784	52.737844
3222.441892	343967.025112	52.742849
3222.080816	343697.295301	52.747853
3221.231577	343445.739411	52.752858
3220.847096	343190.723538	52.757863
3220.231828	342941.953967	52.762868
3219.297457	342686.692057	52.767873
3218.932721	342428.818966	52.772877
3218.492832	342167.825754	52.777882
3217.628214	341910.055017	52.782887
3216.687954	341642.367758	52.787892
3216.222914	341394.968180	52.792897
3215.539722	341127.136217	52.797901
3214.500322	340890.185729	52.802906
3213.788042	340631.851045	52.807911
3213.436429	340381.807626	52.812916
3212.669787	340125.974104	52.817921
3211.849918	339860.856667	52.822925
3211.090964	339624.213453	52.827930
3210.598930	339373.730085	52.832935
3209.862463	339129.444741	52.837940
3209.282241	338862.274251	52.842945
3208.764775	338603.798727	52.847949
3207.536294	338355.948075	52.852954
3206.897348	338112.992659	52.857959
3206.487730	337863.457768	52.862964
3205.704950	337621.465177	52.867969
3205.053644	337362.038585	52.872973
3204.346638	337120.974073	52.877978
3204.010279	336862.972201	52.882983
3203.102095	336624.228833	52.887988
3202.651414	336370.901763	52.892993
3201.770159	336115.274349	52.897997
3201.135096	335863.349229	52.903002
3200.309824	335614.737254	52.908007
3199.755454	335366.972527	52.913012
3199.022286	335128.501701	52.918017
3198.632054	334879.207260	52.923021
3197.912690	334630.524057	52.928026
3197.290877	334382.460975	52.933031
3196.796528	334129.310742	52.938036
3195.997980	333886.798206	52.943041
3195.764979	333623.803514	52.948045
3194.610243	333374.497364	52.953050
3194.020833	333122.020465	52.958055
3193.786680	332865.184024	52.963060
3192.566574	332623.141194	52.968065
3191.857618	332366.301707	52.973069
3191.221933	332118.563870	52.978074
3190.633128	331857.655666	52.983079
3190.096779	331615.374004	52.988084
3189.265344	331363.031084	52.993089
3188.766747	331101.291233	52.998093
3188.232111	330847.626651	53.003098
3187.459443	330596.188340	53.008103
3187.005291	330350.758066	53.013108
3186.114221	330091.342618	53.018113
3185.266163	329845.998472	53.023117
3184.570337	329590.725742	53.028122
3183.960157	329340.886934	53.033127
3183.413550	329093.455910	53.038132
3182.364146	328831.897150	53.043137
3182.435971	328583.119122	53.048141
3181.426774	328331.710740	53.053146
3180.557307	328080.508579	53.058151
3180.045602	327818.581281	53.063156
3179.322193	327581.892062	53.068161
3178.726279	327329.982263	53.073165
3177.864722	327070.602926	53.078170
3177.185520	326827.946773	53.083175
3176.486275	326586.744298	53.088180
3175.903795	326326.452748	53.093185
3175.261434	326083.330235	53.098189
3174.619289	325836.744318	53.103194
3173.946418	325588.303889	53.108199
3173.829474	325345.121516	53.113204
3172.922316	325085.106526	53.118209
3172.223690	324831.066508	53.123213
3171.403212	324586.236413	53.128218
3170.920762	324322.816464	53.133223
3170.195847	324074.048753	53.138228
3169.503717	323824.027525	53.143233
3168.950605	323561.431148	53.148237
3168.347097	323323.641319	53.153242
3167.591291	323058.834873	53.158247
3166.818539	322804.622292	53.163252
3166.119398	322548.284010	53.168257
3165.865750	322292.205496	53.173261
3164.850628	322043.732465	53.178266
3164.344688	321789.551115	53.183271
3163.419666	321530.954051	53.188276
3162.440541	321288.329450	53.193281
3162.087642	321030.506131	53.198285
3161.454316	320778.862813	53.203290
3160.794523	320539.037434	53.208295
3160.295237	320294.297282	53.213300
3159.480256	320043.801020	53.218305
3159.232350	319779.057276	53.223309
3158.483726	319540.567399	53.228314
3157.514448	319279.322875	53.233319
3156.980142	319018.518057	53.238324
3156.208273	318758.692226	53.243329
3155.773488	318497.360978	53.248333
3154.935531	318262.243094	53.253338
3154.211020	317996.067466	53.258343
3153.724594	317732.527047	53.263348
3152.937925	317497.679287	53.268353
3152.283274	317235.691925	53.273357
3151.058569	316984.361257	53.278362
3151.088843	316733.824456	53.283367
3150.050352	316485.773282	53.288372
3149.420737	316237.427634	53.293377
3148.776891	315988.650751	53.298381
3148.059874	315729.419365	53.303386
3147.543477	315498.139966	53.308391
3147.065972	315242.510736	53.313396
3146.099468	314984.768374	53.318401
3145.406900	314730.012213	53.323405
3144.788869	314479.878042	53.328410
3144.059784	314230.804866	53.333415
3143.873285	313969.906418	53.338420
3142.994050	313737.763856	53.343425
3142.239381	313473.414615	53.348429
3141.385950	313215.395441	53.353434
3140.583022	312978.299158	53.358439
3140.202184	312728.378038	53.363444
3139.219965	312480.715966	53.368449
3138.774535	312225.583773	53.373453
3137.982137	311992.048719	53.378458
3137.349778	311732.896160	53.383463
3136.734939	311486.803496	53.388468
3135.926632	311244.713376	53.393473
3135.481757	310986.879085	53.398477
3134.898014	310750.889357	53.403482
3134.367175	310493.831516	53.408487
3133.637639	310254.986356	53.413492
3132.793931	310002.458740	53.418497
3132.420065	309733.227726	53.423501
3131.189145	309503.602268	53.428506
3130.561764	309248.288639	53.433511
3130.341882	309000.320305	53.438516
3129.587806	308750.933562	53.443521
3128.778873	308503.592204	53.448525
3128.118773	308257.652854	53.453530
3127.365710	308004.240973	53.458535
3126.656426	307761.186006	53.463540
3126.122610	307514.996051	53.468545
3125.632662	307260.165941	53.473549
3124.680088	307026.875839	53.478554
3123.969815	306767.750519	53.483559
3123.903741	306513.030147	53.488564
3123.017196	306281.536329	53.493569
3121.984343	306007.766976	53.498573
3121.536567	305774.547600	53.503578
3120.964830	305526.781090	53.508583
3120.462516	305266.219371	53.513588
3119.578415	305024.154772	53.518593
3119.007250	304773.025350	53.523597
3118.289888	304523.446565	53.528602
3117.766653	304280.152162	53.533607
3117.003907	304018.279660	53.538612
3116.330610	303765.432950	53.543617
3115.368886	303531.680015	53.548621
3114.794815	303276.193764	53.553626
3113.912975	303023.862638	53.558631
3113.778689	302791.454646	53.563636
3113.217340	302529.904175	53.568641
3112.092301	302277.814021	53.573645
3111.581586	302031.941880	53.578650
3110.838011	301792.625571	53.583655
3110.527732	301520.210496	53.588660
3109.405277	301283.729203	53.593665
3109.033415	301046.186532	53.598669
3108.214331	300797.509041	53.603674
3107.444562	300541.361688	53.608679
3107.224203	300298.624262	53.613684
3105.976123	300053.960850	53.618689
3105.276997	299796.375049	53.623693
3104.815236	299561.849544	53.628698
3103.837407	299305.529507	53.633703
3103.562467	299063.817630	53.638708
3102.968174	298818.972611	53.643713
3102.663233	298574.336136	53.648717
3101.768238	298328.901361	53.653722
3101.064023	298076.560015	53.658727
3100.289752	297831.716674	53.663732
3099.355031	297574.241340	53.668737
3099.001818	297330.502192	53.673741
3098.267521	297084.811144	53.678746
3097.507749	296836.882716	53.683751
3097.067280	296579.582504	53.688756
3096.267900	296348.951855	53.693761
3095.681824	296086.071285	53.698765
3095.006908	295844.698705	53.703770
3094.354784	295596.446096	53.708775
3094.019316	295350.358727	53.713780
3093.104302	295107.724455	53.718785
3092.513471	294846.422033	53.723789
3091.822319	294601.408772	53.728794
3090.712731	294343.218443	53.733799
3090.248894	294091.216061	53.738804
3089.524624	293848.652074	53.743809
3089.288820	293611.180413	53.748813
3088.318564	293346.752847	53.753818
3087.352944	293113.012544	53.758823
3086.825072	292863.183687	53.763828
3086.158150	292623.614516	53.768833
3085.775921	292373.660236	53.773837
3084.928731	292127.013664	53.778842
3084.279913	291888.306814	53.783847
3084.149723	291636.605587	53.788852
3082.905595	291398.298100	53.793857
3082.479057	291136.965586	53.798861
3081.613846	290894.420987	53.803866
3081.076823	290636.518141	53.808871
3080.427028	290393.047639	53.813876
3079.735588	290139.803899	53.818881
3079.436806	289894.138129	53.823885
3078.903632	289645.504045	53.828890
3077.979693	289390.208086	53.833895
3077.356224	289132.011964	53.838900
3076.709644	288884.337510	53.843905
3075.701247	288628.876010	53.848909
3075.268790	288384.732784	53.853914
3074.552692	288129.326505	53.858919
3074.030305	287879.466854	53.863924
3073.044194	287650.589600	53.868929
3072.755436	287386.634304	53.873933
3071.656170	287145.779210	53.878938
3070.962210	286895.818671	53.883943
3070.626059	286635.206638	53.888948
3069.701210	286392.082265	53.893953
3069.318740	286142.606763	53.898957
3068.434613	285891.198516	53.903962
3068.272143	285640.720100	53.908967
3067.349833	285394.411212	53.913972
3066.415909	285136.184939	53.918977
3065.759497	284890.954283	53.923981
3065.280863	284635.813717	53.928986
3064.463558	284388.749080	53.933991
3063.961195	284146.957323	53.938996
3063.071367	283896.720392	53.944001
3062.221464	283648.820094	53.949005
3061.756593	283401.750132	53.954010
3060.827825	283155.262837	53.959015
3060.557823	282904.417983	53.964020
3059.684055	282660.672340	53.969025
3059.448774	282424.440560	53.974029
3058.896226	282159.479760	53.979034
3057.972628	281920.275065	53.984039
3057.477457	281664.499034	53.989044
3056.774518	281419.503411	53.994049
3056.156549	281155.698652	53.999053
3055.229385	280900.576493	54.004058
3054.299522	280662.747671	54.009063
3053.657963	280408.955451	54.014068
3052.876785	280168.225043	54.019073
3052.098778	279923.953973	54.024077
3052.165895	279673.665903	54.029082
3051.300447	279431.242277	54.034087
3050.920819	279173.817254	54.039092
3050.051147	278928.388927	54.044097
3049.534210	278671.112876	54.049101
3048.565781	278425.216191	54.054106
3047.720455	278176.218312	54.059111
3047.491564	277917.801412	54.064116
3046.594283	277679.075446	54.069121
3046.092587	277425.744400	54.074125
3045.496217	277170.772868	54.079130
3044.550757	276923.420676	54.084135
3044.050158	276676.609303	54.089140
3043.351047	276431.612122	54.094145
3042.778602	276169.938559	54.099149
3042.375561	275922.296731	54.104154
3041.184077	275676.562475	54.109159
3040.726800	275408.732798	54.114164
3039.746161	275170.783978	54.119169
3039.272854	274925.369040	54.124173
3038.728907	274676.450658	54.129178
3037.963501	274424.562075	54.134183
3037.621702	274177.114374	54.139188
3036.375262	273945.014498	54.144193
3036.214957	273683.224897	54.149197
3035.439700	273422.424052	54.154202
3034.973776	273184.699570	54.159207
3034.290692	272929.334450	54.164212
3033.483250	272677.758375	54.169217
3032.951617	272424.050293	54.174221
3031.996628	272166.818232	54.179226
3031.035571	271930.725917	54.184231
3030.804809	271668.947859	54.189236
3029.905488	271433.533535	54.194241
3029.273421	271178.797450	54.199245
3028.629933	270935.091029	54.204250
3028.133930	270692.125386	54.209255
3027.462137	270432.913395	54.214260
3026.871704	270185.454968	54.219265
3026.055296	269936.249612	54.224269
3025.619130	269674.861265	54.229274
3024.614100	269432.638788	54.234279
3024.670573	269182.811663	54.239284
3023.604833	268940.904605	54.244289
3022.867952	268671.720055	54.249293
3022.248822	268426.966487	54.254298
3021.453389	268181.833441	54.259303
3021.121599	267918.697514	54.264308
3019.900678	267674.599842	54.269313
3019.077560	267423.715730	54.274317
3018.924933	267168.574314	54.279322
3017.776591	266935.111217	54.284327
3017.327605	266673.115114	54.289332
3016.744260	266438.875208	54.294337
3016.189415	266192.227953	54.299341
3015.587731	265928.015275	54.304346
3014.514624	265694.897493	54.309351
3014.320881	265435.510436	54.314356
3013.580657	265189.708108	54.319361
3012.881888	264936.360841	54.324365
3011.991742	264693.562323	54.329370
3011.562102	264438.721123	54.334375
3011.268347	264179.554510	54.339380
3010.290583	263925.742752	54.344385
3009.368394	263670.623521	54.349389
3008.602485	263433.027139	54.354394
3007.823005	263178.955351	54.359399
3007.628769	262926.624815	54.364404
3006.784147	262683.362110	54.369409
3005.994519	262436.525394	54.374413
3005.317477	262182.361797	54.379418
3004.438059	261939.105194	54.384423
3004.150410	261689.566458	54.389428
3003.277841	261459.807089	54.394433
3002.923018	261210.967032	54.399437
3002.131799	260954.657832	54.404442
3001.106005	260719.753383	54.409447
3000.996073	260457.759392	54.414452
3000.436256	260211.881476	54.419457
2999.253449	259967.528588	54.424461
2998.749538	259721.718691	54.429466
2998.115927	259476.540784	54.434471
2997.263626	259216.779370	54.439476
2996.558037	258978.336777	54.444481
2995.963881	258738.068590	54.449485
2995.539423	258483.028128	54.454490
2994.621708	258245.816815	54.459495
2994.426849	257993.236352	54.464500
2993.331805	257760.408534	54.469505
2993.019507	257504.332706	54.474509
2992.283313	257260.828722	54.479514
2991.917462	257001.145595	54.484519
2991.147309	256750.720454	54.489524
2990.102001	256495.322118	54.494529
2989.791279	256249.434413	54.499533
2989.287799	256003.679378	54.504538
2988.299184	255751.558244	54.509543
2987.695641	255501.108233	54.514548
2987.004476	255249.704655	54.519553
2986.213475	255008.325745	54.524557
2985.684392	254756.820738	54.529562
2984.904427	254513.174132	54.534567
2984.247796	254252.165326	54.539572
2983.341838	254014.243897	54.544577
2982.791866	253766.792743	54.549581
2982.442966	253515.388199	54.554586
2981.806647	253273.223012	54.559591
2981.023223	253017.915116	54.564596
2980.526410	252765.898358	54.569601
2979.525217	252524.173944	54.574605
2979.093014	252269.066199	54.579610
2978.606337	252026.191432	54.584615
2977.988459	251769.305687	54.589620
2977.340335	251518.078693	54.594625
2976.505179	251265.251824	54.599629
2975.993489	251004.428599	54.604634
2975.055848	250755.616969	54.609639
2974.399432	250506.939467	54.614644
2973.888616	250256.736786	54.619649
2973.346823	250005.138754	54.624653
2972.512506	249749.207229	54.629658
2971.659486	249500.282297	54.634663
2971.472134	249248.985899	54.639668
2970.384923	249000.888297	54.644673
2969.617670	248746.322992	54.649677
2969.419302	248500.428388	54.654682
2968.630356	248244.848726	54.659687
2967.884249	247997.182642	54.664692
2967.421912	247739.489410	54.669697
2966.583681	247488.935655	54.674701
2965.903414	247228.782174	54.679706
2964.864175	246985.289692	54.684711
2964.623160	246732.478132	54.689716
2963.862117	246495.563553	54.694721
2963.138351	246231.675340	54.699725
2962.570217	245974.893366	54.704730
2961.603093	245728.259400	54.709735
2961.196750	245479.296143	54.714740
2960.508629	245231.727623	54.719745
2959.780690	244975.456691	54.724749
2959.221768	244719.184965	54.729754
2958.353650	244478.241881	54.734759
2957.973960	244226.577437	54.739764
2957.576642	243974.636155	54.744769
2956.732548	243726.815059	54.749773
2956.472834	243470.371118	54.754778
2955.324637	243215.749044	54.759783
2954.558645	242958.826062	54.764788
2953.657226	242712.543943	54.769793
2953.489909	242451.682029	54.774797
2952.786859	242204.223605	54.779802
2951.933173	241949.659385	54.784807
2951.598198	241698.069358	54.789812
2950.764283	241442.433563	54.794817
2949.986601	241195.116358	54.799821
2949.485898	240936.704189	54.804826
2949.095353	240680.210456	54.809831
2948.141436	240418.153361	54.814836
2947.230466	240169.484351	54.819841
2946.645110	239908.821544	54.824845
2945.987324	239663.143817	54.829850
2945.040531	239412.928810	54.834855
2944.769347	239158.864170	54.839860
2943.984350	238899.483052	54.844865
2943.095027	238660.744966	54.849869
2942.552115	238408.609409	54.854874
2942.026310	238159.425545	54.859879
2941.602485	237910.735388	54.864884
2940.784609	237659.790978	54.869889
2940.238828	237405.748426	54.874893
2939.457296	237146.192712	54.879898
2938.658554	236900.798158	54.884903
2938.416240	236646.327435	54.889908
2937.799355	236383.946545	54.894913
2936.997307	236137.306600	54.899917
2936.190977	235865.790167	54.904922
2935.621937	235626.320708	54.909927
2935.120317	235354.986567	54.914932
2934.208291	235110.607289	54.919937
2933.625334	234856.475046	54.924941
2933.204727	234586.657947	54.929946
2932.359455	234336.540805	54.934951
2931.517422	234073.997863	54.939956
2931.069163	233820.992794	54.944961
2930.166720	233567.169090	54.949965
2929.671956	233304.318620	54.954970
2929.102519	233059.864752	54.959975
2928.732512	232788.084007	54.964980
2927.889899	232540.899296	54.969985
2927.097459	232282.962121	54.974989
2926.789589	232007.405342	54.979994
2925.919281	231759.539591	54.984999
2925.223963	231498.788354	54.990004
2924.370227	231235.873188	54.995009
2923.732297	230982.931224	55.000013
2923.188005	230721.139806	55.005018
2922.031891	230455.855872	55.010023
2921.904986	230203.548115	55.015028
2921.227492	229950.971774	55.020033
2920.515549	229680.323757	55.025037
2919.910521	229422.746943	55.030042
2918.828473	229164.508020	55.035047
2918.308084	228907.326705	55.040052
2917.684790	228650.467980	55.045057
2917.150117	228387.332487	55.050061
2916.186127	228134.093832	55.055066
2915.569336	227879.324205	55.060071
2915.045445	227628.105194	55.065076
2914.023734	227377.653193	55.070081
2913.401063	227120.518900	55.075085
2912.914404	226869.372639	55.080090
2911.965310	226623.112449	55.085095
2911.488048	226363.385923	55.090100
2911.056044	226109.750884	55.095105
2910.439625	225856.349510	55.100109
2909.821429	225601.256078	55.105114
2909.183816	225344.218797	55.110119
2908.513709	225090.624628	55.115124
2907.862582	224840.274439	55.120129
2907.072651	224576.898654	55.125133
2906.737236	224314.342882	55.130138
2905.560503	224062.385258	55.135143
2905.049939	223799.846196	55.140148
2904.569150	223535.482916	55.145153
2903.849936	223287.961739	55.150157
2903.395115	223028.178832	55.155162
2902.404383	222778.016275	55.160167
2902.142599	222511.203150	55.165172
2901.587736	222255.588594	55.170177
2900.480616	222006.147122	55.175181
2900.036758	221734.171835	55.180186
2899.173372	221474.917166	55.185191
2898.791296	221212.850333	55.190196
2897.978897	220961.672629	55.195201
2897.041655	220698.295259	55.200205
2896.630865	220436.464837	55.205210
2895.470792	220182.022451	55.210215
2895.057898	219925.273201	55.215220
2894.446704	219670.389267	55.220225
2893.713530	219420.922737	55.225229
2893.485592	219153.059765	55.230234
2892.409725	218904.069344	55.235239
2892.009693	218644.165775	55.240244
2891.407269	218393.587406	55.245249
2890.566947	218126.474420	55.250253
2889.939101	217863.618459	55.255258
2889.058677	217614.003354	55.260263
2888.636405	217350.811268	55.265268
2887.593006	217097.239678	55.270273
2886.968021	216844.506507	55.275277
2886.716722	216586.356296	55.280282
2885.940388	216334.629066	55.285287
2885.486639	216067.093638	55.290292
2884.663353	215811.251692	55.295297
2884.183164	215555.560040	55.300301
2883.652198	215295.893377	55.305306
2882.629792	215035.681834	55.310311
2882.083035	214767.338919	55.315316
2881.407795	214511.147528	55.320321
2880.483460	214261.691644	55.325325
2879.889811	213997.305027	55.330330
2879.595617	213748.362258	55.335335
2878.527993	213483.339974	55.340340
2878.065269	213229.461886	55.345345
2877.170031	212961.054211	55.350349
2876.796620	212701.067313	55.355354
2875.851730	212455.223589	55.360359
2875.531905	212194.962958	55.365364
2875.058943	211929.025562	55.370369
2873.947309	211674.938143	55.375373
2873.392958	211415.672406	55.380378
2872.703543	211154.710880	55.385383
2872.201592	210891.951609	55.390388
2871.455099	210633.444985	55.395393
2870.763575	210367.548764	55.400397
2870.323118	210113.234096	55.405402
2869.312095	209855.421686	55.410407
2869.121685	209590.404000	55.415412
2868.549169	209335.502527	55.420417
2867.351650	209078.066539	55.425421
2867.486034	208807.617174	55.430426
2866.369714	208538.805220	55.435431
2865.404505	208285.013944	55.440436
2864.924609	208017.121699	55.445441
2864.151569	207746.871667	55.450445
2863.621639	207485.187753	55.455450
2862.614713	207236.320105	55.460455
2862.379812	206973.522664	55.465460
2861.863628	206702.943976	55.470465
2861.118532	206451.849163	55.475469
2860.181077	206182.421343	55.480474
2859.502529	205925.209460	55.485479
2858.960276	205653.392534	55.490484
2858.674066	205409.407291	55.495489
2857.704926	205132.837068	55.500493
2857.295950	204865.418797	55.505498
2856.320716	204610.015970	55.510503
2855.407589	204345.810621	55.515508
2854.843659	204077.402466	55.520513
2854.194105	203828.365557	55.525517
2853.731725	203559.740152	55.530522
2852.647078	203303.991463	55.535527
2851.950437	203046.057263	55.540532
2851.752190	202792.995697	55.545537
2851.045848	202525.940974	55.550541
2850.275523	202251.745787	55.555546
2849.185605	202007.800649	55.560551
2848.474321	201740.737765	55.565556
2848.238818	201488.960610	55.570561
2847.458830	201232.575113	55.575565
2847.211125	200962.922950	55.580570
2846.210172	200712.148640	55.585575
2845.547062	200449.881907	55.590580
2844.894441	200186.151378	55.595585
2844.153319	199931.114750	55.600589
2843.932178	199666.376773	55.605594
2843.016759	199420.239609	55.610599
2842.161379	199147.727800	55.615604
2841.844404	198881.481886	55.620609
2841.188175	198634.543815	55.625613
2840.654746	198356.424306	55.630618
2839.887029	198101.604259	55.635623
2839.234608	197837.630845	55.640628
2838.137818	197572.927480	55.645633
2837.554644	197310.014638	55.650637
2837.183826	197056.409299	55.655642
2836.097431	196799.813751	55.660647
2835.512943	196532.642370	55.665652
2835.192407	196273.714116	55.670657
2834.392580	196009.302566	55.675661
2833.736954	195749.615675	55.680666
2833.173134	195493.160224	55.685671
2832.490308	195230.184742	55.690676
2832.040079	194959.628457	55.695681
2831.055324	194709.618363	55.700685
2830.618635	194437.993926	55.705690
2829.473054	194174.002990	55.710695
2828.892457	193904.134678	55.715700
2828.711415	193642.042332	55.720705
2827.870317	193384.445542	55.725709
2827.232744	193127.568550	55.730714
2826.491568	192861.535683	55.735719
2825.771338	192603.898382	55.740724
2825.335546	192340.988102	55.745729
2824.699863	192077.512898	55.750733
2824.262857	191809.554539	55.755738
2823.251702	191557.656105	55.760743
2822.685014	191290.599048	55.765748
2822.024576	191013.252697	55.770753
2821.236214	190751.068471	55.775757
2820.574861	190488.916457	55.780762
2819.817981	190219.172790	55.785767
2819.468235	189957.585040	55.790772
2818.503167	189684.200517	55.795777
2817.902489	189436.090482	55.800781
2817.663913	189174.082332	55.805786
2816.819476	188898.494988	55.810791
2815.990861	188643.453346	55.815796
2815.369408	188371.052547	55.820801
2814.463299	188108.698070	55.825805
2813.955445	187842.223643	55.830810
2813.222124	187588.266794	55.835815
2812.734029	187320.074767	55.840820
2812.204202	187062.462819	55.845825
2811.124136	186796.682983	55.850829
2810.659482	186526.214668	55.855834
2810.086861	186275.788999	55.860839
2809.345298	186003.650210	55.865844
2808.803661	185740.768118	55.870849
2807.862035	185469.007705	55.875853
2807.481689	185204.970975	55.880858
2806.743911	184949.693785	55.885863
2805.997061	184676.202658	55.890868
2805.462222	184418.721021	55.895873
2804.842558	184160.643692	55.900877
2803.921078	183884.742625	55.905882
2803.331928	183621.816887	55.910887
2802.623162	183366.506016	55.915892
2802.285730	183092.018460	55.920897
2801.409492	182836.609977	55.925901
2800.700154	182567.145684	55.930906
2800.102896	182304.000140	55.935911
2799.644253	182030.785050	55.940916
2799.153521	181767.333308	55.945921
2797.978278	181509.334116	55.950925
2797.755167	181235.908648	55.955930
2797.163560	180971.752679	55.960935
2796.314333	180706.201763	55.965940
2796.022249	180429.485125	55.970945
2795.201039	180160.358838	55.975949
2794.621966	179880.371312	55.980954
2793.415905	179619.004910	55.985959
2792.842805	179346.906215	55.990964
2792.292808	179081.801397	55.995969
2791.191559	178830.891510	56.000973
2790.636993	178556.429152	56.005978
2790.334953	178291.697070	56.010983
2789.500130	178020.080878	56.015988
2788.704941	177750.469814	56.020993
2788.269799	177489.999398	56.025997
2787.775426	177218.372684	56.031002
2787.019570	176956.875300	56.036007
2786.191520	176677.546430	56.041012
2785.711375	176408.822699	56.046017
2784.890969	176148.637998	56.051021
2784.524532	175884.999898	56.056026
2783.629107	175617.542692	56.061031
2782.864527	175346.123801	56.066036
2782.194087	175084.993698	56.071041
2781.171429	174821.708084	56.076045
2780.904298	174548.638688	56.081050
2779.977150	174299.840115	56.086055
2779.131449	174039.825586	56.091060
2779.311621	173763.345840	56.096065
2778.184234	173500.238102	56.101069
2777.682727	173233.243071	56.106074
2777.065488	172967.387323	56.111079
2776.326624	172699.072689	56.116084
2776.021376	172441.170442	56.121089
2775.022549	172179.475481	56.126093
2774.462488	171897.199665	56.131098
2773.537207	171644.411491	56.136103
2772.983591	171368.052003	56.141108
2772.723612	171100.486346	56.146113
2771.830801	170834.243594	56.151117
2771.484072	170566.530032	56.156122
2770.706933	170291.103792	56.161127
2769.725721	170028.492167	56.166132
2769.428265	169753.184544	56.171137
2768.581875	169485.583062	56.176141
2767.888062	169213.025290	56.181146
2767.173511	168933.046379	56.186151
2766.345754	168673.586119	56.191156
2766.077389	168394.952003	56.196161
2765.129737	168133.568846	56.201165
2764.970597	167858.634480	56.206170
2764.179890	167578.156280	56.211175
2763.440394	167264.585479	56.216180
2762.898072	166981.236764	56.221185
2761.616014	166696.481489	56.226189
2761.156424	166435.045561	56.231194
2760.499747	166166.458457	56.236199
2759.952161	165887.353134	56.241204
2759.358078	165644.241469	56.246209
2758.538001	165368.234887	56.251213
2757.825313	165093.688311	56.256218
2757.490759	164813.260428	56.261223
2756.594794	164565.168573	56.266228
2756.210485	164270.537473	56.271233
2755.446533	164004.144649	56.276237
2754.617323	163743.905266	56.281242
2754.124271	163443.004354	56.286247
2753.375542	163190.537469	56.291252
2752.660109	162914.571007	56.296257
2752.088677	162652.874634	56.301261
2751.411721	162365.616053	56.306266
2750.665038	162091.911251	56.311271
2750.013203	161835.522609	56.316276
2749.116911	161551.064230	56.321281
2748.480789	161274.017161	56.326285
2747.810689	161025.278198	56.331290
2747.360437	160745.421522	56.336295
2746.623187	160473.761840	56.341300
2746.334295	160227.599785	56.346305
2745.129620	159930.540767	56.351309
2744.859050	159694.842545	56.356314
2744.321620	159390.474042	56.361319
2743.342748	159146.640934	56.366324
2742.920753	158847.814441	56.371329
2741.781942	158605.764830	56.376333
2741.596058	158303.168063	56.381338
2740.894615	158049.370123	56.386343
2740.149734	157760.532658	56.391348
2739.342172	157500.895117	56.396353
2738.718584	157229.395275	56.401357
2738.484165	156950.234062	56.406362
2737.304056	156684.381906	56.411367
2736.764291	156421.837193	56.416372
2736.112501	156122.930907	56.421377
2735.281934	155873.771220	56.426381
2734.628648	155592.183261	56.431386
2734.279433	155310.320670	56.436391
2733.071977	155070.315358	56.441396
2732.767533	154768.238993	56.446401
2731.833256	154522.156429	56.451405
2731.266968	154250.989122	56.456410
2730.532581	153968.919144	56.461415
2729.814356	153728.769668	56.466420
2729.683433	153428.152376	56.471425
2728.490869	153202.623033	56.476429
2727.954305	152900.231716	56.481434
2727.317618	152647.442778	56.486439
2726.706481	152382.259054	56.491444
2726.109470	152101.314419	56.496449
2725.079994	151846.102626	56.501453
2724.781773	151572.232912	56.506458
2723.716442	151304.969112	56.511463
2723.100161	151031.955035	56.516468
2722.401397	150774.932536	56.521473
2721.793572	150498.515362	56.526477
2721.278486	150278.897779	56.531482
2720.384404	149992.121095	56.536487
2719.910233	149711.774935	56.541492
2719.471182	149477.814557	56.546497
2718.631477	149189.473150	56.551501
2717.995155	148936.230006	56.556506
2717.329787	148648.081901	56.561511
2716.467593	148417.017680	56.566516
2716.623684	148110.634141	56.571521
2715.324950	147882.095740	56.576525
2714.606516	147596.087894	56.581530
2714.120529	147344.968608	56.586535
2713.589077	147058.770780	56.591540
2712.656385	146779.870085	56.596545
2712.106484	146539.175365	56.601549
2711.929534	146236.344743	56.606554
2711.085618	145998.953986	56.611559
2710.200666	145700.993450	56.616564
2709.726390	145463.484661	56.621569
2709.034957	145170.454530	56.626573
2708.365275	144885.810631	56.631578
2707.732942	144647.926464	56.636583
2706.653320	144356.871609	56.641588
2706.431812	144087.133174	56.646593
2705.368120	143826.450840	56.651597
2704.752562	143557.541884	56.656602
2704.072593	143286.027883	56.661607
2703.436933	143031.307506	56.666612
2703.126929	142759.142348	56.671617
2702.127663	142484.191732	56.676621
2701.454039	142226.891956	56.681626
2700.994051	141957.159215	56.686631
2699.995053	141677.451006	56.691636
2699.855053	141422.652850	56.696641
2698.749305	141153.779215	56.701645
2698.328481	140876.083295	56.706650
2698.072533	140599.075332	56.711655
2697.049246	140336.802877	56.716660
2696.463487	140067.920094	56.721665
2695.388454	139800.159076	56.726669
2694.785363	139508.706695	56.731674
2694.000814	139256.735228	56.736679
2693.173346	138995.282064	56.741684
2692.909710	138702.398955	56.746689
2692.048435	138461.499625	56.751693
2691.254098	138193.708605	56.756698
2690.765967	137941.028014	56.761703
2690.060865	137659.532216	56.766708
2689.910788	137400.628357	56.771713
2688.855064	137131.897468	56.776717
2688.140055	136859.799304	56.781722
2687.738370	136596.394353	56.786727
2686.757381	136312.147631	56.791732
2686.001484	136058.191792	56.796737
2685.499306	135800.539336	56.801741
2685.064968	135526.516319	56.806746
2684.322176	135271.510898	56.811751
2683.584726	134994.644568	56.816756
2682.734701	134724.925189	56.821761
2682.140770	134462.929310	56.826765
2681.793274	134207.006873	56.831770
2680.965320	133950.832565	56.836775
2680.259358	133663.240210	56.841780
2679.426457	133392.666862	56.846785
2678.869873	133141.741073	56.851789
2678.363984	132875.998557	56.856794
2677.848713	132600.682556	56.861799
2676.923688	132330.095804	56.866804
2676.551722	132064.949366	56.871809
2675.950360	131794.240251	56.876813
2675.226177	131527.427213	56.881818
2674.576302	131253.847686	56.886823
2673.846262	130988.412461	56.891828
2673.162590	130723.480456	56.896833
2672.315355	130445.291392	56.901837
2671.504462	130174.034138	56.906842
2671.331687	129910.781645	56.911847
2670.108583	129670.559605	56.916852
2670.299084	129357.772248	56.921857
2669.228784	129131.476064	56.926861
2668.367446	128829.631445	56.931866
2667.691674	128578.460547	56.936871
2667.137671	128291.178548	56.941876
2666.479238	128042.549835	56.946881
2665.798200	127781.849248	56.951885
2665.356597	127500.209210	56.956890
2664.783742	127239.636339	56.961895
2663.767994	126945.799620	56.966900
2663.368550	126698.589831	56.971905
2662.535506	126410.927287	56.976909
2661.475367	126155.585228	56.981914
2661.238784	125876.367737	56.986919
2660.707429	125607.422510	56.991924
2659.873210	125359.138202	56.996929
2659.395997	125068.271523	57.001933
2658.676371	124797.878442	57.006938
2658.232948	124537.209450	57.011943
2657.358963	124269.703301	57.016948
2656.691156	123981.545240	57.021953
2655.742883	123719.567389	57.026957
2654.984258	123457.600156	57.031962
2654.768750	123192.184517	57.036967
2653.795064	122900.505810	57.041972
2653.622382	122644.078834	57.046977
2652.826850	122366.065773	57.051981
2652.116505	122113.614542	57.056986
2651.160269	121811.812599	57.061991
2650.282315	121562.935709	57.066996
2650.010970	121293.256355	57.072001
2649.166809	121014.478046	57.077005
2648.535427	120768.248642	57.082010
2648.372852	120494.027557	57.087015
2647.321611	120213.538467	57.092020
2646.737141	119933.181576	57.097025
2645.739731	119681.326143	57.102029
2645.594882	119402.168585	57.107034
2645.013294	119124.974913	57.112039
2644.234152	118857.292883	57.117044
2643.469446	118588.405253	57.122049
2642.498326	118321.178153	57.127053
2641.899252	118043.592601	57.132058
2641.247359	117765.294786	57.137063
2640.121350	117512.452570	57.142068
2639.490469	117238.016453	57.147073
2639.092875	116981.922059	57.152077
2638.688173	116718.449395	57.157082
2637.872380	116465.066946	57.162087
2637.055492	116183.308796	57.167092
2636.681459	115921.578655	57.172097
2636.181439	115649.823749	57.177101
2635.293336	115383.356840	57.182106
2634.890067	115118.992918	57.187111
2634.268739	114842.658026	57.192116
2633.577356	114570.449994	57.197121
2632.861017	114313.531811	57.202125
2631.983522	114038.547423	57.207130
2631.398350	113753.149387	57.212135
2630.648514	113493.807818	57.217140
2629.817714	113236.353978	57.222145
2629.223894	112956.570341	57.227149
2628.733795	112689.250292	57.232154
2628.325683	112420.384330	57.237159
2627.418686	112158.244794	57.242164
2626.694046	111902.082573	57.247169
2626.220447	111616.044059	57.252173
2625.699502	111357.310439	57.257178
2624.986466	111081.082542	57.262183
2624.331177	110803.109833	57.267188
2623.901848	110532.002319	57.272193
2623.045364	110257.227867	57.277197
2622.254056	109983.220337	57.282202
2621.167995	109716.483835	57.287207
2620.623201	109451.999623	57.292212
2620.007211	109170.853788	57.297217
2619.405570	108919.290960	57.302221
2618.817672	108652.544284	57.307226
2618.173678	108370.041572	57.312231
2617.364881	108097.561866	57.317236
2616.547628	107849.794285	57.322241
2615.910248	107576.068701	57.327245
2615.430729	107317.866299	57.332250
2614.883638	107050.033178	57.337255
2613.948538	106779.974056	57.342260
2613.682521	106511.823230	57.347265
2613.092967	106234.501552	57.352269
2611.994135	105973.499568	57.357274
2611.777946	105704.956531	57.362279
2610.693319	105433.090071	57.367284
2609.992937	105166.025615	57.372289
2609.697152	104898.570145	57.377293
2608.813669	104631.102967	57.382298
2608.414644	104360.510507	57.387303
2607.704115	104090.700074	57.392308
2606.948016	103836.753620	57.397313
2606.298149	103559.523507	57.402317
2605.393831	103286.752310	57.407322
2605.061840	103016.615071	57.412327
2604.091139	102749.328986	57.417332
2603.293079	102475.154775	57.422337
2602.630911	102210.344383	57.427341
2602.088072	101945.575177	57.432346
2602.169350	101679.403331	57.437351
2600.893259	101415.593679	57.442356
2600.431970	101143.665374	57.447361
2599.791044	100861.093112	57.452365
2598.623423	100604.424291	57.457370
2598.316224	100328.053639	57.462375
2597.439194	100064.107348	57.467380
2596.737722	99801.347757	57.472385
2596.284366	99536.204996	57.477389
2595.699681	99267.324848	57.482394
2595.059503	99001.190343	57.487399
2593.954573	98737.212957	57.492404
2593.620549	98458.344676	57.497409
2592.797235	98200.043496	57.502413
2592.106327	97936.973807	57.507418
2591.782423	97667.811109	57.512423
2591.086246	97402.725233	57.517428
2590.434612	97127.094708	57.522433
2589.425721	96867.214488	57.527437
2588.927543	96599.969338	57.532442
2588.343852	96323.399216	57.537447
2587.352398	96064.660674	57.542452
2586.918452	95803.344428	57.547457
2586.437965	95548.107621	57.552461
2585.574077	95277.549632	57.557466
2585.178856	94993.235529	57.562471
2584.483016	94743.356242	57.567476
2583.871370	94469.147053	57.572481
2583.064515	94194.794609	57.577485
2582.459071	93928.720679	57.582490
2582.029678	93650.535726	57.587495
2580.745302	93392.153529	57.592500
2580.302593	93124.148425	57.597505
2579.699838	92855.277851	57.602509
2578.737642	92589.251155	57.607514
2578.482447	92321.796732	57.612519
2577.524389	92043.886946	57.617524
2576.860938	91794.441540	57.622529
2576.203369	91530.459081	57.627533
2575.492636	91245.691387	57.632538
2575.276794	90986.819307	57.637543
2574.302747	90730.682668	57.642548
2573.729547	90462.134659	57.647553
2572.797709	90197.742553	57.652557
2572.093532	89940.615047	57.657562
2571.903698	89668.002769	57.662567
2570.875290	89406.076498	57.667572
2570.153426	89131.355304	57.672577
2569.519561	88875.319724	57.677581
2568.643419	88611.673517	57.682586
2568.322442	88347.612880	57.687591
2567.296044	88093.956400	57.692596
2566.824283	87826.914736	57.697601
2566.459490	87566.699666	57.702605
2565.610800	87312.796011	57.707610
2565.240021	87025.379991	57.712615
2564.429436	86792.573529	57.717620
2563.623104	86495.160679	57.722625
2562.829666	86254.534906	57.727629
2562.140287	85984.482595	57.732634
2561.720387	85708.964923	57.737639
2560.914180	85466.442075	57.742644
2560.326609	85202.912511	57.747649
2559.866108	84939.511868	57.752653
2559.004511	84675.227284	57.757658
2558.651890	84395.374089	57.762663
2557.741748	84145.238634	57.767668
2557.237965	83868.002454	57.772673
2556.364461	83603.657112	57.777677
2555.783414	83359.683965	57.782682
2555.668870	83081.908412	57.787687
2554.421588	82818.487830	57.792692
2553.943631	82535.301080	57.797697
2553.261358	82300.242067	57.802701
2552.757771	81993.977948	57.807706
2552.364557	81749.404384	57.812711
2551.232027	81475.423986	57.817716
2550.665003	81225.890094	57.822721
2549.727168	80930.889826	57.827725
2548.957281	80691.654809	57.832730
2548.453619	80408.684839	57.837735
2547.499928	80145.245226	57.842740
2546.870641	79884.387458	57.847745
2546.649730	79624.583580	57.852749
2545.694830	79371.134869	57.857754
2545.136999	79102.722027	57.862759
2544.650608	78851.157226	57.867764
2544.086915	78583.506177	57.872769
2543.437018	78315.137238	57.877773
2542.241283	78048.892362	57.882778
2541.876530	77785.662134	57.887783
2541.115871	77528.162774	57.892788
2540.461882	77257.894790	57.897793
2539.912662	76986.492281	57.902797
2539.325817	76718.945388	57.907802
2538.453242	76455.939567	57.912807
2537.749193	76198.384722	57.917812
2537.022422	75933.366749	57.922817
2536.305796	75665.493196	57.927821
2535.651417	75424.635177	57.932826
2535.202540	75158.835710	57.937831
2534.569859	74901.374801	57.942836
2533.694461	74630.828551	57.947841
2533.391081	74365.345955	57.952845
2532.460585	74117.014586	57.957850
2531.834029	73842.796724	57.962855
2530.786774	73585.665490	57.967860
2530.547566	73332.406917	57.972865
2529.907083	73066.177769	57.977869
2529.089240	72804.167657	57.982874
2528.593492	72536.275582	57.987879
2527.867913	72287.693789	57.992884
2527.301274	72021.542941	57.997889
2526.565750	71761.155213	58.002893
2525.739764	71499.645045	58.007898
2525.365009	71227.298347	58.012903
2524.508192	70973.122595	58.017908
2524.050207	70695.576958	58.022913
2523.295088	70451.786273	58.027917
2522.602382	70189.100549	58.032922
2522.390001	69918.374069	58.037927
2521.375578	69659.173111	58.042932
2520.337744	69411.696835	58.047937
2519.780923	69125.739768	58.052941
2518.787064	68870.434908	58.057946
2518.072397	68608.559250	58.062951
2517.642344	68356.275195	58.067956
2517.266610	68095.473737	58.072961
2516.375877	67840.273709	58.077965
2515.490092	67598.844662	58.082970
2515.184477	67329.359543	58.087975
2514.406201	67072.616014	58.092980
2513.799857	66818.609813	58.097985
2513.166279	66559.605129	58.102989
2512.532051	66297.215984	58.107994
2511.809624	66036.541557	58.112999
2510.857932	65783.116692	58.118004
2510.489649	65527.332480	58.123009
2509.851322	65278.683663	58.128013
2508.948084	65015.021686	58.133018
2508.499166	64755.128689	58.138023
2507.535479	64505.547321	58.143028
2507.023826	64260.690976	58.148033
2506.499837	64005.771794	58.153037
2505.663701	63744.896483	58.158042
2504.974159	63490.118091	58.163047
2504.224960	63240.085576	58.168052
2503.874537	62989.796862	58.173057
2503.576885	62725.199980	58.178061
2502.614465	62474.397752	58.183066
2501.885243	62210.379835	58.188071
2501.249122	61937.847856	58.193076
2500.419074	61702.828438	58.198081
2499.977184	61443.609629	58.203085
2499.242115	61189.106877	58.208090
2498.738372	60926.087358	58.213095
2497.920102	60683.256865	58.218100
2496.840868	60423.855606	58.223105
2496.624068	60166.831374	58.228109
2495.644804	59919.145812	58.233114
2495.127861	59659.903419	58.238119
2494.099944	59407.813616	58.243124
2493.934238	59149.655798	58.248129
2493.376459	58896.039241	58.253133
2492.618178	58644.277867	58.258138
2491.884618	58389.452201	58.263143
2491.342867	58136.574608	58.268148
2490.669384	57882.005928	58.273153
2489.864925	57624.603572	58.278157
2489.211790	57369.851987	58.283162
2488.346731	57118.644171	58.288167
2487.842881	56862.758732	58.293172
2486.862629	56621.076725	58.298177
2486.314842	56359.888434	58.303181
2485.487735	56117.476711	58.308186
2485.144609	55864.383602	58.313191
2484.294477	55603.741358	58.318196
2483.530724	55370.380214	58.323201
2483.396631	55110.001750	58.328205
2482.446728	54869.284228	58.333210
2481.895013	54614.713043	58.338215
2481.254518	54358.396931	58.343220
2480.547328	54097.503555	58.348225
2479.641612	53854.257822	58.353229
2479.168836	53609.497493	58.358234
2478.356124	53359.744286	58.363239
2477.301127	53113.940669	58.368244
2476.610495	52873.632495	58.373249
2476.568327	52630.263144	58.378253
2475.517989	52386.180455	58.383258
2474.852755	52123.660415	58.388263
2474.394832	51878.936987	58.393268
2473.590320	51631.819807	58.398273
2473.017607	51379.145188	58.403277
2471.888243	51144.849208	58.408282
2471.644832	50890.768824	58.413287
2471.061436	50654.924712	58.418292
2470.396747	50407.251758	58.423297
2469.843784	50157.185469	58.428301
2469.238386	49911.569520	58.433306
2468.525887	49666.356723	58.438311
2467.742309	49428.845900	58.443316
2466.993317	49177.065529	58.448321
2466.429613	48923.930717	58.453325
2465.557348	48683.944810	58.458330
2464.835844	48433.666907	58.463335
2463.958390	48202.814559	58.468340
2463.183555	47956.486995	58.473345
2462.787063	47716.274297	58.478349
2461.906085	47487.038770	58.483354
2461.646415	47240.772376	58.488359
2460.833325	47003.061551	58.493364
2460.257203	46762.548715	58.498369
2459.497547	46515.141320	58.503373
2458.694963	46281.537823	58.508378
2458.108329	46042.599013	58.513383
2457.454651	45795.254557	58.518388
2456.412259	45561.303327	58.523393
2456.322278	45318.563542	58.528397
2455.489919	45091.366295	58.533402
2454.684114	44856.444510	58.538407
2453.919865	44614.811332	58.543412
2453.356846	44378.257209	58.548417
2452.417307	44143.511728	58.553421
2451.699363	43924.233794	58.558426
2451.405808	43696.241969	58.563431
2450.767803	43453.343105	58.568436
2449.716262	43213.985512	58.573441
2449.483726	42989.162035	58.578445
2448.758217	42768.881654	58.583450
2447.807683	42528.363304	58.588455
2447.085847	42293.162532	58.593460
2446.705146	42056.010417	58.598465
2446.303094	41818.716334	58.603469
2445.200682	41602.140758	58.608474
2444.452575	41350.533127	58.613479
2443.714194	41135.439321	58.618484
2442.740488	40909.479895	58.623489
2442.240229	40685.415110	58.628493
2441.778967	40464.755588	58.633498
2440.728888	40239.566489	58.638503
2440.028964	40018.733981	58.643508
2439.556446	39795.149164	58.648513
2438.801317	39566.120180	58.653517
2437.836134	39344.187604	58.658522
2437.513657	39120.730132	58.663527
2436.579223	38922.208540	58.668532
2435.662869	38723.798640	58.673537
2435.063468	38500.671452	58.678541
2434.329443	38285.954370	58.683546
2433.465424	38078.882855	58.688551
2432.171085	37874.008146	58.693556
2431.633813	37689.863526	58.698561
2430.521798	37498.684813	58.703565
2429.456441	37313.053689	58.708570
2428.519177	37120.172915	58.713575
2427.782927	36944.508558	58.718580
2426.410509	36780.557974	58.723585
2425.597283	36621.578201	58.728589
2424.931883	36471.672674	58.733594
2424.176097	36286.281987	58.738599
2423.143711	36153.246676	58.743604
2422.473069	36002.559064	58.748609
2421.685793	35844.914923	58.753613
2420.780797	35700.703026	58.758618
2420.201728	35572.477874	58.763623
2419.820764	35413.369908	58.768628
2418.582021	35273.180017	58.773633
2418.275487	35159.371270	58.778637
2417.435843	35016.765391	58.783642
2416.674608	34888.440037	58.788647
2415.625959	34753.280145	58.793652
2415.065473	34615.057006	58.798657
2414.765800	34493.365549	58.803661
2413.575929	34366.668856	58.808666
2413.089506	34234.941939	58.813671
2412.458673	34110.865714	58.818676
2411.508721	33993.021704	58.823681
2410.812176	33869.191594	58.828685
2410.315670	33755.884017	58.833690
2409.872142	33630.405233	58.838695
2408.936899	33524.664169	58.843700
2408.302085	33398.531624	58.848705
2407.706345	33279.421292	58.853709
2406.773237	33170.471050	58.858714
2406.501392	33052.255991	58.863719
2405.759953	32934.024580	58.868724
2404.972443	32822.509370	58.873729
2404.287042	32708.715857	58.878733
2403.619799	32596.151227	58.883738
2403.089058	32479.166469	58.888743
2402.428647	32383.121536	58.893748
2401.571596	32265.813947	58.898753
2401.110734	32139.789844	58.903757
2400.536807	32035.160869	58.908762
2399.755399	31933.817381	58.913767
2399.690416	31810.163284	58.918772
2398.866364	31685.988945	58.923777
2397.867540	31598.005537	58.928781
2397.416831	31451.625433	58.933786
2396.612225	31345.484191	58.938791
2396.231016	31239.350766	58.943796
2395.301140	31133.758501	58.948801
2394.807370	30999.544677	58.953805
2393.898713	30904.919227	58.958810
2393.259412	30801.326024	58.963815
2392.775834	30671.671655	58.968820
2392.327411	30589.943840	58.973825
2391.760318	30461.283986	58.978829
2390.912455	30347.036471	58.983834
2390.327339	30225.706146	58.988839
2389.592155	30121.261887	58.993844
2388.973714	30012.333256	58.998849
2388.598798	29891.084263	59.003853
2387.794039	29783.392199	59.008858
2387.118072	29672.945582	59.013863
2386.609414	29553.848456	59.018868
2386.032596	29433.720275	59.023873
2385.299045	29314.350900	59.028877
2384.554174	29207.766967	59.033882
2384.017411	29070.686214	59.038887
2383.790307	28957.850876	59.043892
2382.492038	28855.324012	59.048897
2382.426375	28725.233365	59.053901
2381.653824	28623.766820	59.058906
2380.966892	28480.022750	59.063911
2379.967618	28378.576311	59.068916
2379.195480	28258.396163	59.073921
2378.775744	28137.655500	59.078925
2378.115314	28029.353445	59.083930
2377.325865	27899.820200	59.088935
2377.089452	27795.491891	59.093940
2375.910892	27689.065697	59.098945
2375.525865	27560.721394	59.103949
2374.880374	27443.553163	59.108954
2374.216312	27332.668796	59.113959
2373.631964	27222.795394	59.118964
2372.800646	27095.541293	59.123969
2372.014263	26972.658302	59.128973
2371.270856	26862.108843	59.133978
2370.912072	26763.975916	59.138983
2370.510295	26641.677376	59.143988
2369.473009	26538.003887	59.148993
2368.954631	26408.149776	59.153997
2368.389192	26303.391244	59.159002
2367.710633	26178.305537	59.164007
2367.187737	26053.437005	59.169012
2366.052891	25939.625442	59.174017
2365.434647	25823.718058	59.179021
2364.323635	25718.780542	59.184026
2364.082339	25601.913863	59.189031
2363.537505	25501.568118	59.194036
2362.529640	25386.502011	59.199041
2362.112191	25272.385572	59.204045
2361.429163	25151.629282	59.209050
2360.751045	25055.287758	59.214055
2360.296420	24941.305143	59.219060
2359.368345	24818.416105	59.224065
2358.789317	24700.596347	59.229069
2358.210589	24619.168935	59.234074
2357.715852	24498.536980	59.239079
2357.036900	24379.137073	59.244084
2356.494800	24272.824520	59.249089
2356.087054	24152.158487	59.254093
2355.247820	24037.085634	59.259098
2354.240865	23908.258743	59.264103
2353.716247	23804.201867	59.269108
2353.054449	23686.322976	59.274113
2352.726954	23570.843844	59.279117
2351.528919	23466.179746	59.284122
2351.284894	23346.002403	59.289127
2350.362004	23230.974712	59.294132
2349.269975	23130.576683	59.299137
2348.841463	23009.570436	59.304141
2348.500338	22904.147192	59.309146
2347.431943	22800.435018	59.314151
2346.987625	22683.407150	59.319156
2346.464810	22561.683353	59.324161
2345.741724	22453.056273	59.329165
2344.531609	22360.555016	59.334170
2343.958527	22245.077109	59.339175
2343.758108	22125.669590	59.344180
2342.565572	22032.160745	59.349185
2341.867110	21931.216798	59.354189
2341.390797	21818.992362	59.359194
2340.773105	21706.194230	59.364199
2340.392631	21608.607329	59.369204
2339.375573	21509.635245	59.374209
2338.629843	21402.290967	59.379213
2337.943859	21314.942732	59.384218
2337.274766	21207.626316	59.389223
2336.650754	21113.177696	59.394228
2335.532026	21011.584653	59.399233
2335.131522	20903.789131	59.404237
2334.804119	20808.858692	59.409242
2333.862440	20698.137976	59.414247
2333.302362	20604.869707	59.419252
2332.347084	20505.407023	59.424257
2332.179044	20395.663564	59.429261
2330.816311	20314.834636	59.434266
2330.397359	20219.407528	59.439271
2329.825651	20112.568692	59.444276
2328.990627	20025.732460	59.449281
2328.267971	19928.475526	59.454285
2327.254341	19833.200343	59.459290
2326.794688	19742.648915	59.464295
2326.276301	19673.666451	59.469300
2325.562019	19565.618840	59.474305
2325.010043	19463.878854	59.479309
2324.140291	19395.998184	59.484314
2323.597895	19287.868394	59.489319
2323.043107	19189.154225	59.494324
2321.876838	19115.453487	59.499329
2321.828554	19022.815294	59.504333
2321.048265	18931.788128	59.509338
2320.374573	18832.832587	59.514343
2319.833175	18741.946659	59.519348
2318.750796	18666.038976	59.524353
2318.381886	18572.267817	59.529357
2317.727580	18482.665945	59.534362
2316.983344	18384.496876	59.539367
2316.660554	18290.774171	59.544372
2315.765851	18198.982410	59.549377
2314.977794	18119.783163	59.554381
2314.448562	18031.725069	59.559386
2313.767243	17925.654301	59.564391
2313.097870	17852.052048	59.569396
2312.249661	17762.265244	59.574401
2311.699543	17664.671241	59.579405
2311.018716	17585.969222	59.584410
2309.899896	17499.844496	59.589415
2309.465458	17387.421631	59.594420
2308.768518	17328.780488	59.599425
2308.509650	17230.002227	59.604429
2307.604012	17148.002131	59.609434
2306.913697	17061.236460	59.614439
2306.184768	16981.173678	59.619444
2305.212301	16911.815703	59.624449
2305.000417	16816.767325	59.629453
2304.256886	16735.750684	59.634458
2303.381817	16654.918521	59.639463
2303.048430	16565.449894	59.644468
2302.206055	16480.660799	59.649473
2301.562846	16394.351174	59.654477
2300.829476	16309.829484	59.659482
2300.400535	16226.582038	59.664487
2299.570387	16142.642535	59.669492
2298.385586	16066.760797	59.674497
2298.452255	15980.368726	59.679501
2297.626354	15911.238265	59.684506
2296.703385	15822.532520	59.689511
2295.872116	15751.565614	59.694516
2295.507744	15671.627624	59.699521
2294.903302	15593.419112	59.704525
2294.024884	15515.263132	59.709530
2293.703636	15429.913854	59.714535
2293.068524	15356.992975	59.719540
2292.068762	15267.352067	59.724545
2291.507420	15188.777799	59.729549
2291.036635	15119.049515	59.734554
2289.837544	15042.468152	59.739559
2289.330767	14958.003193	59.744564
2288.725363	14880.673716	59.749569
2288.218385	14805.259176	59.754573
2287.202338	14745.966909	59.759578
2286.528344	14660.858881	59.764583
2286.279697	14583.499379	59.769588
2285.464829	14520.863085	59.774593
2284.818742	14436.550749	59.779597
2284.404041	14358.650891	59.784602
2283.637341	14283.590638	59.789607
2283.024212	14199.909382	59.794612
2282.270645	14129.927207	59.799617
2281.522408	14046.258950	59.804621
2280.558160	13976.589844	59.809626
2280.061069	13896.230160	59.814631
2279.672417	13835.680752	59.819636
2279.040552	13754.829637	59.824641
2278.257036	13671.596658	59.829645
2277.621235	13601.087940	59.834650
2276.678423	13523.322861	59.839655
2276.462039	13455.777452	59.844660
2275.453509	13380.243009	59.849665
2275.063965	13293.608959	59.854669
2274.011927	13227.847197	59.859674
2273.330649	13154.507656	59.864679
2272.943202	13072.818646	59.869684
2272.048529	13009.537367	59.874689
2271.536130	12929.959535	59.879693
2270.791775	12864.845363	59.884698
2270.156373	12786.300625	59.889703
2269.755421	12711.360850	59.894708
2268.784357	12651.528374	59.899713
2268.251431	12574.366973	59.904718
2267.743539	12506.705709	59.909722
2266.676156	12428.713675	59.914727
2266.317146	12346.406394	59.919732
2265.451668	12288.881293	59.924737
2264.731464	12212.189382	59.929742
2264.408812	12136.580547	59.934746
2263.224562	12071.586111	59.939751
2262.765074	12003.626468	59.944756
2261.810907	11934.496891	59.949761
2261.224994	11874.015384	59.954766
2260.526985	11806.162715	59.959770
2259.894411	11744.004874	59.964775
2259.807369	11669.606923	59.969780
2258.964837	11594.231203	59.974785
2258.343488	11535.044800	59.979790
2257.536051	11455.803782	59.984794
2256.770157	11390.377041	59.989799
2256.401714	11314.294313	59.994804
2255.515487	11252.118367	59.999809
2254.929895	11173.099686	60.004814
2253.853472	11115.829692	60.009818
2253.487721	11055.025784	60.014823
2253.051239	10972.854442	60.019828
2252.398100	10914.457827	60.024833
2251.586263	10833.205233	60.029838
2250.938320	10778.802302	60.034842
2250.408631	10703.716737	60.039847
2249.381880	10632.390294	60.044852
2248.663885	10574.327988	60.049857
2248.358801	10502.118418	60.054862
2247.832845	10435.120802	60.059866
2247.073163	10369.729066	60.064871
2246.676449	10285.364536	60.069876
2245.417096	10223.969603	60.074881
2244.783396	10161.137574	60.079886
2244.426156	10089.975364	60.084890
2243.852374	10029.329701	60.089895
2243.229240	9950.498538	60.094900
2242.089356	9887.206716	60.099905
2241.469935	9813.993098	60.104910
2240.957777	9757.330103	60.109914
2240.087608	9689.700467	60.114919
2239.669891	9623.468390	60.119924
2239.325603	9562.653693	60.124929
2238.394682	9495.999843	60.129934
2237.905818	9434.007041	60.134938
2236.853539	9362.205486	60.139943
2236.444131	9290.263643	60.144948
2235.144886	9225.823994	60.149953
2234.976348	9160.772145	60.154958
2234.337556	9102.613820	60.159962
2233.391689	9034.329357	60.164967
2233.192563	8968.212633	60.169972
2232.521222	8909.474848	60.174977
2231.844725	8839.213741	60.179982
2230.778611	8768.483836	60.184986
2230.352285	8709.728875	60.189991
2229.687026	8629.944542	60.194996
2228.957011	8582.777059	60.200001
2228.215395	8514.511878	60.205006
2227.749654	8449.362741	60.210010
2226.860317	8389.076708	60.215015
2226.535817	8330.773710	60.220020
2225.603586	8266.869278	60.225025
2225.303007	8194.786063	60.230030
2224.670244	8138.795993	60.235034
2224.213790	8065.210087	60.240039
2223.578084	7972.512802	60.245044
2222.273487	7930.724695	60.250049
2222.164338	7859.936437	60.255054
2221.319612	7787.013420	60.260058
2220.426863	7723.231275	60.265063
2219.578376	7664.133648	60.270068
2219.346586	7604.501409	60.275073
2218.715126	7537.847453	60.280078
2218.069930	7474.544583	60.285082
2216.977388	7410.345049	60.290087
2216.456468	7341.530392	60.295092
2215.534435	7289.107584	60.300097
2215.047391	7223.246199	60.305102
2214.311182	7148.783121	60.310106
2213.474995	7101.675828	60.315111
2213.127972	7036.383092	60.320116
2212.613322	6975.560598	60.325121
2211.632207	6911.644505	60.330126
2211.230750	6847.122434	60.335130
2210.564431	6785.939052	60.340135
2210.341475	6713.574612	60.345140
2208.940075	6663.960082	60.350145
2208.597549	6594.994377	60.355150
2207.900816	6540.616986	60.360154
2207.363308	6476.410749	60.365159
2206.563384	6399.999046	60.370164
2205.816969	6342.946048	60.375169
2205.001664	6276.756015	60.380174
2204.522088	6215.859294	60.385178
2203.736498	6165.786703	60.390183
2203.159655	6085.732627	60.395188
2202.532105	6041.968357	60.400193
2201.735664	5974.048514	60.405198
2201.526632	5903.067721	60.410202
2200.298253	5856.525102	60.415207
2199.997897	5791.064809	60.420212
2199.095985	5737.022647	60.425217
2198.679757	5669.994320	60.430222
2198.162570	5606.243739	60.435226
2197.234089	5555.054586	60.440231
2196.907822	5480.837735	60.445236
2195.761191	5426.510577	60.450241
2195.253388	5369.142700	60.455246
2194.760575	5301.539018	60.460250
2193.839633	5245.200981	60.465255
2193.102464	5174.249896	60.470260
2192.343830	5120.236166	60.475265
2192.132951	5060.188092	60.480270
2191.345730	4993.987525	60.485274
2190.579137	4939.575059	60.490279
2190.011467	4867.544857	60.495284
2189.136752	4821.045631	60.500289
2188.611893	4760.872709	60.505294
2187.706937	4698.464462	60.510298
2187.314785	4643.037800	60.515303
2186.984076	4584.949261	60.520308
2185.777274	4527.122973	60.525313
2185.358652	4463.790738	60.530318
2184.741414	4402.663077	60.535322
2183.800311	4348.290738	60.540327
2183.463441	4289.572619	60.545332
2182.752041	4227.689309	60.550337
2181.941607	4169.307847	60.555342
2181.468211	4102.923491	60.560346
2180.988123	4044.810310	60.565351
2180.208374	3985.478328	60.570356
2179.354273	3933.414722	60.575361
2179.157335	3864.129529	60.580366
2178.244226	3806.067064	60.585370
2177.038925	3742.970786	60.590375
2176.672656	3693.903167	60.595380
2176.261219	3629.709046	60.600385
2175.173903	3573.087581	60.605390
2174.744612	3506.019131	60.610394
2173.940334	3453.352341	60.615399
2173.466979	3396.929887	60.620404
2172.446177	3338.716021	60.625409
2171.791034	3277.744169	60.630414
2171.337101	3226.826956	60.635418
2170.308304	3183.870629	60.640423
2170.268350	3120.578748	60.645428
2169.269892	3070.328882	60.650433
2168.532447	3016.847900	60.655438
2168.069319	2956.184445	60.660442
2167.435408	2896.750150	60.665447
2166.931077	2831.175306	60.670452
2166.141184	2781.730037	60.675457
2165.243643	2735.137757	60.680462
2164.865079	2668.584774	60.685466
2163.743268	2622.593058	60.690471
2163.548424	2563.895595	60.695476
2162.440452	2513.788830	60.700481
2161.844858	2452.459272	60.705486
2161.669323	2398.181698	60.710490
2160.760512	2350.005059	60.715495
2160.099200	2287.869670	60.720500
2159.496113	2227.309516	60.725505
2159.026077	2168.434142	60.730510
2157.961854	2111.957417	60.735514
2157.091196	2062.754506	60.740519
2156.759020	2004.517935	60.745524
2156.032473	1950.845155	60.750529
2155.451654	1896.479195	60.755534
2154.786025	1844.667552	60.760538
2153.839936	1787.576425	60.765543
2153.259200	1724.996174	60.770548
2152.740648	1688.536483	60.775553
2152.118508	1637.568710	60.780558
2151.490937	1582.364468	60.785562
2150.495760	1531.099843	60.790567
2149.889796	1479.332079	60.795572
2149.332215	1422.221752	60.800577
2148.305703	1371.074634	60.805582
2147.782750	1312.010052	60.810586
2147.013380	1265.935179	60.815591
2146.632414	1219.317842	60.820596
2145.717411	1172.574857	60.825601
2145.323280	1127.205733	60.830606
2144.471813	1070.249078	60.835610
2144.097667	1032.012941	60.840615
2143.452437	974.320607	60.845620
2142.596356	923.750432	60.850625
2141.960396	878.209142	60.855630
2141.542316	824.255042	60.860634
2140.650038	774.930621	60.865639
2140.418353	731.588576	60.870644
2139.487488	680.266299	60.875649
2138.840298	624.330807	60.880654
2138.419566	571.294270	60.885658
2137.018776	540.608669	60.890663
2136.363630	485.524942	60.895668
2135.631615	430.958233	60.900673
2135.084780	399.429407	60.905678
2134.380989	341.384621	60.910682
2133.410190	314.474200	60.915687
2133.231305	268.455467	60.920692
2132.334277	228.282834	60.925697
2131.475719	190.925264	60.930702
2131.307977	141.745079	60.935706
2130.282449	114.253963	60.940711
2129.372901	56.924181	60.945716
2128.661622	35.206756	60.950721
2127.657578	-1.116455	60.955726
2126.044592	-14.338055	60.960730
2120.793362	89.051781	60.965735
2120.757701	96.596460	60.970740
2121.341875	105.654365	60.975745
2121.924631	100.657765	60.980750
2122.368921	97.255285	60.985754
2122.095057	88.573830	60.990759
2121.611224	88.213767	60.995764
2119.956146	92.118931	61.000769
2119.352969	95.560738	61.005774
2118.904187	89.482082	61.010778
2117.848869	99.161227	61.015783
2117.149402	102.646698	61.020788
2116.882129	115.160618	61.025793
2116.108882	105.148661	61.030798
2115.770704	102.300824	61.035802
2114.502218	107.120742	61.040807
2114.112991	110.564873	61.045812
2114.044129	103.588605	61.050817
2113.295117	118.590017	61.055822
2112.653996	101.025914	61.060826
2111.691136	104.701407	61.065831
2111.128927	103.467575	61.070836
2110.438110	105.116187	61.075841
2108.948566	123.314755	61.080846
2108.629987	110.119465	61.085850
2108.475354	114.051475	61.090855
2107.921879	97.110532	61.095860
2107.390336	111.766785	61.100865
2106.264395	110.150917	61.105870
2105.805480	105.776896	61.110874
2104.713270	109.791446	61.115879
2104.674592	107.577298	61.120884
2104.135484	111.898306	61.125889
2103.818510	119.971736	61.130894
2102.951491	101.311281	61.135898
2101.231902	102.314199	61.140903
2101.053924	114.829718	61.145908
2100.721073	112.689055	61.150913
2099.366209	113.960516	61.155918
2098.755714	109.298325	61.160922
2097.996323	106.488943	61.165927
2097.995100	95.518750	61.170932
2097.582614	99.991542	61.175937
2096.947339	104.840294	61.180942
2096.742966	108.740773	61.185946
2095.667952	114.230137	61.190951
2095.035861	113.644456	61.195956
2094.279503	110.008308	61.200961
2093.401477	118.085614	61.205966
2092.907393	98.503437	61.210970
2091.975830	99.833880	61.215975
2090.808491	108.773914	61.220980
2090.317639	101.758961	61.225985
2089.735427	104.785883	61.230990
2089.090778	98.960650	61.235994
2088.924425	108.218063	61.240999
2088.779435	106.919607	61.246004
2087.844177	97.683969	61.251009
2086.172085	114.247894	61.256014
2086.340695	103.966650	61.261018
2086.115466	105.211819	61.266023
2085.063361	105.402387	61.271028
2083.969999	106.416325	61.276033
2083.861214	110.721087	61.281038
2082.994360	104.459627	61.286042
2081.899728	113.031754	61.291047
2081.712496	109.065613	61.296052
2081.206088	101.985325	61.301057
2080.266946	114.914927	61.306062
2080.156674	102.156507	61.311066
2078.768863	105.658182	61.316071
2077.776870	107.704662	61.321076
2077.807070	107.702986	61.326081
2077.393459	100.880774	61.331086
2076.881412	93.020831	61.336090
2075.400425	105.635883	61.341095
2074.590571	109.055307	61.346100
2074.746325	98.292005	61.351105
2073.952610	109.046087	61.356110
2073.068794	106.142923	61.361114
2072.018222	115.371929	61.366119
2071.855345	105.058136	61.371124
2071.344188	106.474831	61.376129
2070.534335	97.465294	61.381134
2069.646187	112.998116	61.386138
2068.674825	98.212868	61.391143
2068.514459	106.534240	61.396148
2068.534481	105.126026	61.401153
2067.174133	97.097940	61.406158
2066.338030	92.378530	61.411162
2065.438315	109.898474	61.416167
2065.205187	105.091258	61.421172
2064.638176	103.311022	61.426177
2063.688243	104.089328	61.431182
2063.537709	100.637738	61.436186
2062.955032	103.909155	61.441191
2061.934976	107.516474	61.446196
2061.299272	102.038319	61.451201
2060.829184	107.335505	61.456206
2060.313136	113.728034	61.461210
2059.494922	108.136922	61.466215
2058.965631	102.824799	61.471220
2058.385925	96.016336	61.476225
2057.092127	111.295003	61.481230
2056.436265	96.514887	61.486234
2055.673378	101.836461	61.491239
2055.561011	117.829623	61.496244
2054.961618	100.993750	61.501249
2053.354604	111.749177	61.506254
2053.498250	106.211996	61.511258
2052.862132	105.157055	61.516263
2052.090526	105.025591	61.521268
2051.278437	110.162598	61.526273
2050.651176	108.787723	61.531278
2050.236455	103.768065	61.536282
2049.616599	114.855670	61.541287
2049.252498	102.924400	61.546292
2048.622006	98.358436	61.551297
2047.824720	103.526207	61.556302
2046.266043	114.059513	61.561306
2045.969496	111.935173	61.566311
2045.980683	104.594564	61.571316
2044.684867	106.902151	61.576321
2043.494875	117.104150	61.581326
2043.652357	101.181023	61.586330
2042.756369	114.512196	61.591335
2041.630550	112.861645	61.596340
2042.303237	101.950076	61.601345
2041.340943	107.353762	61.606350
2040.473825	113.723164	61.611354
2039.830192	113.550894	61.616359
2039.310287	104.720845	61.621364
2037.998943	106.349687	61.626369
2036.901238	113.242940	61.631374
2037.199164	93.219723	61.636378
2036.635753	107.335432	61.641383
2035.396067	111.321377	61.646388
2034.847932	101.678987	61.651393
2034.109263	113.466660	61.656398
2033.747788	104.471126	61.661402
2033.009948	107.535373	61.666407
2032.268404	106.872466	61.671412
2032.077304	111.981885	61.676417
2031.636784	107.508770	61.681422
2030.778476	105.602892	61.686426
2029.183415	110.493599	61.691431
2028.240925	99.105119	61.696436
2028.428996	102.222682	61.701441
2027.997810	112.903471	61.706446
2027.420580	103.781339	61.711450
2026.324679	106.195972	61.716455
2025.768439	107.019039	61.721460
2025.495969	95.264041	61.726465
2024.877424	102.658385	61.731470
2024.018517	106.080877	61.736474
2022.838282	104.875767	61.741479
2022.021082	112.400987	61.746484
2021.696048	104.303225	61.751489
2020.636098	105.885870	61.756494
2020.604315	101.980219	61.761498
2020.064999	102.111505	61.766503
2019.281048	102.888714	61.771508
2019.044026	102.229314	61.776513
2018.469536	97.731738	61.781518
2017.179200	97.096013	61.786522
2015.971398	100.993329	61.791527
2015.434956	105.515765	61.796532
2014.808472	105.694001	61.801537
2014.521217	107.031017	61.806542
2014.367163	99.648833	61.811546
2013.368768	95.876095	61.816551
2012.819838	96.910882	61.821556
2012.369749	96.438256	61.826561
2011.327672	96.584686	61.831566
2010.224561	93.293749	61.836570
2009.651687	98.235108	61.841575
2009.071960	99.238516	61.846580
2008.585615	94.544036	61.851585
2008.022075	99.681024	61.856590
2007.688102	94.587065	61.861594
2006.814670	101.488880	61.866599
2006.647560	97.705629	61.871604
2005.896653	95.866289	61.876609
2004.309188	102.748974	61.881614
2003.978246	93.698148	61.886618
2003.317594	99.008238	61.891623
2002.710606	97.133442	61.896628
2002.346241	92.638790	61.901633
2001.340663	97.387065	61.906638
2001.200652	98.645522	61.911642
1999.830542	104.516049	61.916647
1998.928388	98.329611	61.921652
1998.614811	95.998258	61.926657
1998.050517	106.074150	61.931662
1997.425393	99.947816	61.936666
1997.010326	101.915371	61.941671
1996.195831	98.715819	61.946676
1995.961482	96.554810	61.951681
1994.925694	104.169917	61.956686
1994.034504	92.629820	61.961690
1993.175355	94.208988	61.966695
1992.288679	93.285290	61.971700
1992.154220	95.487415	61.976705
1991.305795	103.255702	61.981710
1991.124379	85.054186	61.986714
1990.630680	93.464722	61.991719
1989.771670	107.942727	61.996724
1988.686977	90.699819	62.001729
1987.743766	107.594348	62.006734
1987.653952	90.113113	62.011738
1987.019504	99.429043	62.016743
1986.293551	98.549220	62.021748
1986.044700	94.097735	62.026753
1985.129946	107.758305	62.031758
1984.397854	100.625559	62.036762
1983.458097	91.777022	62.041767
1982.383704	107.577522	62.046772
1982.601103	101.039935	62.051777
1981.869158	98.685107	62.056782
1981.397155	99.181013	62.061786
1979.759250	115.643371	62.066791
1978.912024	106.761218	62.071796
1978.813545	95.566790	62.076801
1978.455178	109.479656	62.081806
1977.603435	113.057136	62.086810
1977.022441	101.855717	62.091815
1976.300026	106.278374	62.096820
1976.263471	97.787923	62.101825
1975.029323	111.612730	62.106830
1974.391632	100.395081	62.111834
1973.553344	106.663732	62.116839
1972.774136	96.905085	62.121844
1972.260045	95.207930	62.126849
1971.617334	94.106751	62.131854
1971.358692	91.452886	62.136858
1970.557783	92.176033	62.141863
1969.959112	103.441616	62.146868
1968.999309	97.713751	62.151873
1967.828720	98.773108	62.156878
1967.568044	92.984735	62.161882
1966.997763	92.389276	62.166887
1966.533979	111.640835	62.171892
1966.242842	101.571338	62.176897
1965.786238	90.643486	62.181902
1964.730275	98.646559	62.186906
1963.648057	96.626443	62.191911
1962.799507	101.103814	62.196916
1962.469688	95.482527	62.201921
1961.847380	104.630965	62.206926
1961.500757	102.680159	62.211930
1960.576897	98.618082	62.216935
1959.667395	101.454139	62.221940
1959.335631	94.432894	62.226945
1958.376761	109.191672	62.231950
1958.081388	93.113375	62.236954
1957.520403	106.509647	62.241959
1956.446339	107.783913	62.246964
1956.020868	85.847677	62.251969
1955.080937	102.454694	62.256974
1954.668100	101.853168	62.261978
1954.006274	108.041777	62.266983
1953.006958	111.912335	62.271988
1952.911108	94.274373	62.276993
1951.640062	100.179656	62.281998
1950.609977	99.016975	62.287002
1950.391667	98.196923	62.292007
1949.874312	102.812529	62.297012
1949.600727	98.577852	62.302017
1948.651525	103.768184	62.307022
1948.474983	99.439260	62.312026
1947.725719	106.158964	62.317031
1946.611431	123.041252	62.322036
1945.957311	101.421976	62.327041
1945.070458	101.835514	62.332046
1944.761148	105.049368	62.337050
1944.335458	95.329229	62.342055
1943.387439	105.628456	62.347060
1942.609167	105.288357	62.352065
1941.677378	110.313512	62.357070
1941.428374	101.233920	62.362074
1940.925302	98.577858	62.367079
1940.271855	104.618489	62.372084
1939.946436	96.768379	62.377089
1938.570473	104.927911	62.382094
1937.877111	109.826913	62.387098
1937.167781	90.990149	62.392103
1936.782815	106.760063	62.397108
1936.660282	109.646240	62.402113
1935.896382	108.753531	62.407118
1934.685461	99.120196	62.412122
1933.652237	101.654219	62.417127
1933.370032	113.640670	62.422132
1933.046973	104.106078	62.427137
1932.348820	110.704139	62.432142
1931.470698	103.619821	62.437146
1930.654500	102.323852	62.442151
1929.939377	106.636558	62.447156
1929.605409	98.704232	62.452161
1928.851661	105.520841	62.457166
1928.523116	98.711968	62.462170
1927.690244	99.050714	62.467175
1926.211005	106.370402	62.472180
1926.029293	103.068847	62.477185
1925.261298	104.110043	62.482190
1925.113044	96.182929	62.487194
1924.488342	102.356187	62.492199
1924.170483	105.517785	62.497204
1923.273403	97.976036	62.502209
1922.303313	100.220933	62.507214
1921.627532	102.258269	62.512218
1921.213044	96.213635	62.517223
1920.091594	106.828967	62.522228
1919.210127	99.325739	62.527233
1918.383008	108.459392	62.532238
1917.857251	94.857107	62.537242
1917.358138	96.289262	62.542247
1916.879558	107.696631	62.547252
1916.943440	99.560808	62.552257
1916.010532	97.200057	62.557262
1915.271903	84.951421	62.562266
1914.344292	102.592495	62.567271
1913.567206	111.901127	62.572276
1913.537870	91.877841	62.577281
1912.697538	92.447999	62.582286
1911.733874	119.300618	62.587290
1911.096995	92.970078	62.592295
1910.421495	100.885964	62.597300
1910.291213	92.517630	62.602305
1909.045101	116.617707	62.607310
1908.167644	97.541146	62.612314
1907.440559	83.426815	62.617319
1906.857881	111.316442	62.622324
1906.758648	71.470334	62.627329
1906.261299	106.388722	62.632334
1905.483168	89.338461	62.637338
1904.361317	85.187998	62.642343
1903.234237	118.228985	62.647348
1903.334573	90.950403	62.652353
1902.581841	113.865185	62.657358
1901.782124	102.165529	62.662362
1900.702186	86.837829	62.667367
1899.936351	100.373847	62.672372
1899.503805	109.960503	62.677377
1899.207464	91.184344	62.682382
1898.661282	96.190865	62.687386
1898.669154	108.801433	62.692391
1897.563998	96.241993	62.697396
1896.644935	92.390482	62.702401
1895.774662	112.337321	62.707406
1895.373816	98.186957	62.712410
1894.521541	79.672528	62.717415
1893.283336	120.006857	62.722420
1892.759709	97.095934	62.727425
1892.180277	105.220490	62.732430
1891.820965	91.635946	62.737434
1891.436844	117.508776	62.742439
1891.018465	96.334634	62.747444
1890.599731	92.503038	62.752449
1889.629684	111.823929	62.757454
1888.736452	106.254252	62.762458
1888.291613	91.576320	62.767463
1886.945354	105.893586	62.772468
1886.136557	106.841928	62.777473
1885.390903	101.742387	62.782478
1884.911001	95.399078	62.787482
1884.456475	99.151628	62.792487
1884.361643	101.208700	62.797492
1884.331902	91.146613	62.802497
1883.175827	107.366937	62.807502
1882.368625	90.373338	62.812506
1881.633670	89.630586	62.817511
1880.489941	102.113330	62.822516
1879.524559	86.464695	62.827521
1879.022272	100.376746	62.832526
1878.492606	99.768551	62.837530
1878.141421	100.060800	62.842535
1877.775863	100.973466	62.847540
1877.191104	92.368223	62.852545
1875.660201	91.641458	62.857550
1874.976873	97.981717	62.862554
1874.811085	92.433747	62.867559
1874.036427	102.744887	62.872564
1873.929437	91.498217	62.877569
1872.923757	97.150100	62.882574
1871.824622	96.309058	62.887578
1871.578921	98.593499	62.892583
1870.746721	100.909558	62.897588
1870.273421	97.083475	62.902593
1869.475723	93.805611	62.907598
1868.542204	104.044208	62.912602
1867.925733	103.098153	62.917607
1867.097996	105.528617	62.922612
1867.264464	95.003315	62.927617
1866.794756	101.930950	62.932622
1865.581337	96.979796	62.937626
1864.897126	97.886287	62.942631
1864.203699	99.694637	62.947636
1863.705987	98.045365	62.952641
1863.006997	95.846183	62.957646
1861.527463	103.386710	62.962650
1861.196102	97.350967	62.967655
1860.726070	113.512842	62.972660
1860.433510	87.890879	62.977665
1859.905315	89.513732	62.982670
1859.105545	91.329505	62.987674
1858.241704	95.030355	62.992679
1857.290677	97.064100	62.997684
1856.902688	97.201353	63.002689
1856.455200	100.380384	63.007694
1855.903495	102.180427	63.012698
1855.151629	98.024856	63.017703
1854.230366	101.034693	63.022708
1854.059982	91.911104	63.027713
1853.029608	92.882020	63.032718
1851.548033	110.518032	63.037722
1851.296987	100.421697	63.042727
1850.882136	102.086478	63.047732
1850.694433	99.921232	63.052737
1849.901537	101.355891	63.057742
1849.449820	102.264894	63.062746
1848.659250	93.342271	63.067751
1847.859601	95.071301	63.072756
1847.383726	96.507662	63.077761
1846.477993	102.817012	63.082766
1845.179986	98.751310	63.087770
1844.617682	96.147251	63.092775
1844.139769	101.310091	63.097780
1843.794284	96.205374	63.102785
1843.713315	94.720162	63.107790
1842.748854	90.502162	63.112794
1841.703776	92.724301	63.117799
1840.564276	97.418203	63.122804
1840.450045	85.983467	63.127809
1840.143733	99.929055	63.132814
1838.457760	93.378306	63.137818
1837.912176	95.965817	63.142823
1837.266287	93.758212	63.147828
1836.870982	87.021461	63.152833
1836.322783	90.468782	63.157838
1836.000827	97.024469	63.162842
1835.854492	85.713098	63.167847
1835.133896	97.174659	63.172852
1833.961202	88.787357	63.177857
1833.287533	91.371552	63.182862
1832.691931	98.230873	63.187866
1831.640662	94.392495	63.192871
1830.747371	87.602358	63.197876
1830.251064	93.955504	63.202881
1829.548992	91.078766	63.207886
1829.302575	90.824556	63.212890
1829.252394	88.736821	63.217895
1827.984384	91.095282	63.222900
1827.214892	79.034505	63.227905
1826.731575	85.630000	63.232910
1826.134852	88.632466	63.237914
1825.103567	83.204586	63.242919
1824.089621	103.770292	63.247924
1823.583854	104.586962	63.252929
1823.217047	92.675114	63.257934
1822.449032	97.699525	63.262938
1822.537617	94.998428	63.267943
1821.552413	95.681501	63.272948
1820.772708	89.195013	63.277953
1819.952333	97.061380	63.282958
1819.330021	100.310751	63.287962
1819.016218	94.570258	63.292967
1817.686593	90.897505	63.297972
1816.766373	90.207842	63.302977
1816.355336	96.198962	63.307982
1815.842856	85.456640	63.312986
1815.522784	90.471422	63.317991
1815.119640	96.327255	63.322996
1814.544947	92.771161	63.328001
1813.477238	96.007681	63.333006
1812.497951	94.042246	63.338010
1812.306110	81.430880	63.343015
1810.931621	96.068020	63.348020
1810.566801	89.282281	63.353025
1810.038027	95.173831	63.358030
1809.386445	103.652035	63.363034
1809.187568	99.219446	63.368039
1807.736544	96.758090	63.373044
1806.949456	91.622583	63.378049
1806.707267	98.706474	63.383054
1805.963531	94.448709	63.388058
1805.842691	93.695191	63.393063
1805.284001	90.205942	63.398068
1804.340053	97.601528	63.403073
1803.700874	90.436753	63.408078
1802.595194	99.083251	63.413082
1802.179632	95.199132	63.418087
1801.056630	89.060463	63.423092
1800.660308	82.153581	63.428097
1800.614862	81.615163	63.433102
1800.099811	96.623589	63.438106
1799.087430	97.050801	63.443111
1797.927770	102.955808	63.448116
1797.307035	92.143949	63.453121
1796.699513	93.036702	63.458126
1796.189662	90.859543	63.463130
1795.970492	87.349498	63.468135
1794.439536	94.254855	63.473140
1794.000331	90.156885	63.478145
1793.718980	94.418083	63.483150
1793.085839	94.346705	63.488154
1792.367857	81.028878	63.493159
1791.696040	88.568897	63.498164
1790.777304	89.619875	63.503169
1790.348048	91.610210	63.508174
1789.774766	99.752722	63.513178
1788.914262	90.951611	63.518183
1788.101676	99.732913	63.523188
1787.296242	88.357485	63.528193
1787.196352	83.871339	63.533198
1786.517817	95.408224	63.538202
1785.598433	95.003853	63.543207
1784.458013	104.262973	63.548212
1784.182277	90.715649	63.553217
1783.652287	84.918039	63.558222
1783.464568	97.217458	63.563226
1782.820376	89.706573	63.568231
1781.353206	92.840966	63.573236
1781.007892	82.114688	63.578241
1780.612086	88.194848	63.583246
1779.616797	88.431705	63.588250
1778.770505	96.127163	63.593255
1778.205107	92.392994	63.598260
1777.694909	84.003017	63.603265
1777.204514	88.518173	63.608270
1776.658542	94.538608	63.613274
1776.181227	87.947350	63.618279
1774.863851	98.040352	63.623284
1774.434803	88.596751	63.628289
1774.166334	89.564971	63.633294
1772.679394	94.807633	63.638298
1772.080295	87.452010	63.643303
1771.558067	91.726231	63.648308
1771.141060	94.521982	63.653313
1770.952880	88.267990	63.658318
1770.112011	96.530264	63.663322
1769.558156	89.661018	63.668327
1768.538802	99.120100	63.673332
1767.880272	91.051706	63.678337
1766.605115	92.635509	63.683342
1765.857118	101.371869	63.688346
1765.685092	92.415704	63.693351
1765.179997	94.394432	63.698356
1764.866353	94.195057	63.703361
1764.257015	88.723849	63.708366
1762.814672	91.841693	63.713370
1762.629016	84.888749	63.718375
1761.779457	92.091168	63.723380
1761.422738	94.366439	63.728385
1760.695227	88.893499	63.733390
1759.765125	104.983354	63.738394
1759.199932	84.889101	63.743399
1758.458551	94.852791	63.748404
1757.996699	94.771565	63.753409
1756.866082	94.487478	63.758414
1756.054035	96.513378	63.763418
1755.910519	92.876210	63.768423
1755.528293	90.920054	63.773428
1755.044168	93.513588	63.778433
1754.273742	88.449568	63.783438
1753.235589	88.630167	63.788442
1752.830869	90.301236	63.793447
1752.371785	99.111556	63.798452
1751.333310	94.828081	63.803457
1750.559917	89.316701	63.808462
1750.139918	94.875610	63.813466
1749.552235	88.398076	63.818471
1748.160764	91.760149	63.823476
1747.772868	94.696352	63.828481
1747.220854	95.119854	63.833486
1746.412788	85.600844	63.838490
1746.271637	95.182221	63.843495
1745.796218	98.310512	63.848500
1744.975039	95.616708	63.853505
1744.346729	80.475989	63.858510
1743.349127	90.201262	63.863514
1742.428792	94.150802	63.868519
1741.454663	86.982476	63.873524
1740.846595	97.148914	63.878529
1740.951790	74.798939	63.883534
1739.859247	88.528773	63.888538
1739.955663	73.884791	63.893543
1738.987028	110.640943	63.898548
1738.170911	81.686680	63.903553
1737.791100	91.685983	63.908558
1737.012493	97.918404	63.913562
1735.930408	87.768014	63.918567
1735.028810	94.485144	63.923572
1734.443142	83.808086	63.928577
1734.053943	96.856976	63.933582
1733.646779	92.367596	63.938586
1733.138176	85.538481	63.943591
1731.987187	109.584054	63.948596
1731.655456	90.898720	63.953601
1731.135856	90.173846	63.958606
1730.185761	94.575948	63.963610
1729.632373	89.103748	63.968615
1728.322425	97.923053	63.973620
1727.995117	99.280649	63.978625
1727.670872	91.023567	63.983630
1727.075774	96.547214	63.988634
1726.494773	86.930650	63.993639
1725.231163	95.208036	63.998644
1724.632892	89.391323	64.003649
1724.528483	86.848606	64.008654
1723.699280	102.094582	64.013658
1722.928309	91.902668	64.018663
1721.984245	97.817613	64.023668
1721.343648	100.207358	64.028673
1721.290097	83.393757	64.033678
1720.228288	90.569974	64.038682
1719.595394	86.895424	64.043687
1718.769503	89.707237	64.048692
1718.390000	96.831859	64.053697
1718.166627	90.551927	64.058702
1716.884685	95.016199	64.063706
1716.309356	83.085469	64.068711
1715.392103	91.336231	64.073716
1714.943831	93.271252	64.078721
1714.529348	91.252420	64.083726
1713.288486	97.547225	64.088730
1712.715494	90.800877	64.093735
1712.203934	100.997722	64.098740
1711.916794	96.248020	64.103745
1711.696552	91.456158	64.108750
1710.176957	86.880129	64.113754
1709.921745	82.864914	64.118759
1708.992675	93.542783	64.123764
1708.468819	93.178116	64.128769
1707.184060	93.341134	64.133774
1706.414170	94.079932	64.138778
1706.371543	95.531080	64.143783
1705.717167	89.072036	64.148788
1705.448052	92.460862	64.153793
1705.024357	83.931018	64.158798
1704.060025	92.146685	64.163802
1703.393216	83.409462	64.168807
1702.765417	86.426348	64.173812
1701.720124	88.055670	64.178817
1701.112175	85.246019	64.183822
1700.072476	90.226880	64.188826
1699.772362	85.906577	64.193831
1699.415195	86.612939	64.198836
1698.292891	87.497595	64.203841
1697.817479	79.672947	64.208846
1697.064671	90.032676	64.213850
1696.834585	88.381931	64.218855
1695.680309	83.669045	64.223860
1694.793062	81.461970	64.228865
1694.306240	84.106400	64.233870
1693.918015	87.143580	64.238874
1693.503372	87.947376	64.243879
1692.909051	93.131876	64.248884
1691.680332	93.123583	64.253889
1691.345652	90.242146	64.258894
1690.296364	97.432156	64.263898
1690.269709	88.363034	64.268903
1689.018220	93.059012	64.273908
1688.342106	99.771880	64.278913
1687.985624	82.082356	64.283918
1687.712048	91.038245	64.288922
1686.615081	98.420323	64.293927
1685.568886	102.840859	64.298932
1684.691415	100.832495	64.303937
1684.776092	92.116253	64.308942
1683.772165	89.688029	64.313946
1683.668753	87.545681	64.318951
1682.328576	94.338795	64.323956
1681.821212	92.129728	64.328961
1681.554785	84.678720	64.333966
1680.880944	86.758378	64.338970
1680.183307	86.369283	64.343975
1678.983003	97.541229	64.348980
1678.625065	97.009872	64.353985
1678.175215	83.490238	64.358990
1677.670855	91.044678	64.363994
1677.139786	95.571041	64.368999
1675.897878	91.520175	64.374004
1675.604279	87.971507	64.379009
1674.860277	85.788992	64.384014
1673.491546	84.396379	64.389018
1673.017409	86.575198	64.394023
1672.734020	98.013067	64.399028
1672.253781	87.693000	64.404033
1671.857362	77.137288	64.409038
1670.551908	87.416077	64.414042
1670.222665	86.936932	64.419047
1669.577530	88.480628	64.424052
1668.721659	85.587370	64.429057
1668.123182	81.691338	64.434062
1667.071449	95.954005	64.439066
1666.890069	80.232997	64.444071
1666.514813	93.560352	64.449076
1665.261454	87.738909	64.454081
1664.682211	85.791987	64.459086
1664.002794	95.821541	64.464090
1663.784118	85.043637	64.469095
1663.235601	94.338075	64.474100
1662.064706	89.127975	64.479105
1661.381858	85.114465	64.484110
1660.554249	86.696609	64.489114
1660.356630	85.031250	64.494119
1659.681637	90.253799	64.499124
1658.532458	95.058111	64.504129
1658.038908	91.310984	64.509134
1657.687984	99.493882	64.514138
1657.269101	85.758033	64.519143
1656.135029	82.615674	64.524148
1655.480881	88.594963	64.529153
1655.161057	68.305693	64.534158
1654.395173	93.849603	64.539162
1653.594300	85.430144	64.544167
1652.949548	90.237904	64.549172
1652.430008	86.133804	64.554177
1652.122537	91.873533	64.559182
1650.782977	92.595611	64.564186
1649.967732	86.102219	64.569191
1649.390139	81.750313	64.574196
1648.738875	93.347534	64.579201
1648.659890	78.464930	64.584206
1647.438495	94.039699	64.589210
1646.780702	97.524963	64.594215
1646.400625	95.869665	64.599220
1645.884427	85.496976	64.604225
1645.405245	87.383303	64.609230
1644.016058	103.131386	64.614234
1643.755529	87.474985	64.619239
1643.304157	82.027605	64.624244
1641.926648	96.887626	64.629249
1641.618400	95.140498	64.634254
1640.534090	91.965009	64.639258
1640.245345	90.492313	64.644263
1640.153580	89.390429	64.649268
1639.320256	89.259430	64.654273
1638.154792	91.035592	64.659278
1637.825019	98.928141	64.664282
1637.445257	88.136407	64.669287
1636.811176	89.310944	64.674292
1635.615675	72.640932	64.679297
1635.109690	97.796652	64.684302
1634.470260	99.017769	64.689306
1633.476238	75.293945	64.694311
1632.527030	93.637037	64.699316
1631.672228	91.330217	64.704321
1631.598946	83.353399	64.709326
1630.939889	85.138999	64.714330
1630.725507	85.329128	64.719335
1630.480539	74.088662	64.724340
1629.250589	94.788042	64.729345
1628.753838	81.759975	64.734350
1627.922287	98.923808	64.739354
1627.531012	76.420922	64.744359
1626.386447	93.268640	64.749364
1625.782911	94.206527	64.754369
1625.303182	67.209437	64.759374
1624.394871	101.317879	64.764378
1623.690085	80.506315	64.769383
1622.674160	80.148877	64.774388
1621.900679	82.681170	64.779393
1622.196763	87.787305	64.784398
1621.464010	87.004857	64.789402
1620.961588	85.715911	64.794407
1619.834191	87.192736	64.799412
1619.207606	94.523763	64.804417
1618.866761	93.171304	64.809422
1617.661993	82.701442	64.814426
1616.973507	81.345867	64.819431
1616.530958	85.643719	64.824436
1616.429235	84.123971	64.829441
1616.033107	75.234980	64.834446
1614.325924	86.880103	64.839450
1613.516457	91.830727	64.844455
1613.439144	86.871102	64.849460
1612.744595	89.143290	64.854465
1611.981600	64.690550	64.859470
1611.038206	80.033504	64.864474
1610.642372	84.387010	64.869479
1610.392405	81.397518	64.874484
1609.376966	90.386111	64.879489
1608.571143	73.089691	64.884494
1607.775321	79.154567	64.889498
1607.399791	82.571341	64.894503
1606.953918	83.255539	64.899508
1605.944422	83.899974	64.904513
1605.669482	78.389884	64.909518
1605.119460	82.230173	64.914522
1604.366091	83.005798	64.919527
1603.491082	74.932440	64.924532
1602.389857	88.517041	64.929537
1602.178048	74.937546	64.934542
1601.308983	83.964381	64.939546
1600.375830	87.002992	64.944551
1599.616524	83.149875	64.949556
1599.085590	89.779769	64.954561
1599.099460	80.827220	64.959566
1598.561969	95.531727	64.964570
1597.746276	85.831073	64.969575
1596.628724	86.336569	64.974580
1596.100853	90.826166	64.979585
1595.605585	81.320602	64.984590
1594.887959	81.429843	64.989594
1593.973740	80.687271	64.994599
1593.437964	88.475356	64.999604
1592.910364	91.950984	65.004609
1592.470964	77.929855	65.009614
1590.860174	83.069287	65.014618
1590.550179	71.099612	65.019623
1590.355825	74.572753	65.024628
1589.550283	85.585814	65.029633
1589.321966	69.102782	65.034638
1588.059622	65.523546	65.039642
1587.605471	85.673917	65.044647
1587.251126	85.020584	65.049652
1586.124374	87.791929	65.054657
1585.220210	70.659374	65.059662
1584.515252	88.295070	65.064666
1584.298857	81.704986	65.069671
1583.958332	78.755116	65.074676
1583.077173	91.992543	65.079681
1582.311805	82.563008	65.084686
1581.338711	82.348584	65.089690
1580.717185	92.208109	65.094695
1580.785270	83.702662	65.099700
1579.091370	88.289210	65.104705
1578.825205	72.048721	65.109710
1577.994481	79.088922	65.114714
1577.614929	74.437506	65.119719
1577.304574	79.824473	65.124724
1576.345495	82.023586	65.129729
1575.774922	86.748615	65.134734
1575.360008	81.661292	65.139738
1574.229363	85.508685	65.144743
1573.528371	81.693617	65.149748
1572.568081	70.243558	65.154753
1572.434101	77.283443	65.159758
1571.605677	100.145588	65.164762
1571.171809	79.708880	65.169767
1570.354120	85.073958	65.174772
1569.846154	83.150426	65.179777
1569.201979	80.212533	65.184782
1568.786323	73.796033	65.189786
1567.383187	88.226506	65.194791
1566.911929	90.308696	65.199796
1566.383973	93.234058	65.204801
1566.128382	72.806881	65.209806
1564.796432	83.113571	65.214810
1563.864593	82.045821	65.219815
1563.616067	75.137591	65.224820
1562.681115	78.178075	65.229825
1562.907873	68.296052	65.234830
1562.048692	76.373625	65.239834
1561.004817	84.272400	65.244839
1560.660084	76.606791	65.249844
1559.833074	92.462680	65.254849
1559.718541	84.957600	65.259854
1558.570188	84.162359	65.264858
1557.711921	89.032445	65.269863
1557.403518	85.319000	65.274868
1556.382933	85.921063	65.279873
1555.643725	82.402217	65.284878
1554.887525	99.046336	65.289882
1554.561232	84.575179	65.294887
1554.271315	80.182323	65.299892
1552.824952	85.201039	65.304897
1552.518208	86.441851	65.309902
1551.607313	87.911112	65.314906
1551.333306	91.084694	65.319911
1550.909495	72.270581	65.324916
1549.630799	92.130944	65.329921
1549.326870	83.528498	65.334926
1548.878108	82.040241	65.339930
1548.198881	85.174133	65.344935
1547.010168	86.693845	65.349940
1546.400207	93.539720	65.354945
1545.833124	80.743619	65.359950
1545.506065	87.333241	65.364954
1545.001404	81.159531	65.369959
1544.265918	81.405657	65.374964
1543.468247	88.960986	65.379969
1542.280393	84.893719	65.384974
1541.229476	85.059085	65.389978
1541.086254	74.486833	65.394983
1540.714837	77.527665	65.399988
1540.020986	87.980549	65.404993
1539.656636	85.906478	65.409998
1538.662238	82.412416	65.415002
1537.786518	81.630632	65.420007
1537.728794	89.270230	65.425012
1536.630417	78.209534	65.430017
1536.108621	77.560739	65.435022
1535.030583	95.299879	65.440026
1534.420190	87.979239	65.445031
1534.370704	85.623340	65.450036
1533.670722	92.374717	65.455041
1532.744309	81.538995	65.460046
1531.863485	86.062607	65.465050
1531.157746	84.175239	65.470055
1531.140322	77.315444	65.475060
1529.791444	87.080821	65.480065
1529.131512	89.673941	65.485070
1528.326262	81.531183	65.490074
1527.989010	94.934498	65.495079
1527.570285	86.526904	65.500084
1527.089210	91.892122	65.505089
1526.428005	85.882053	65.510094
1525.574743	82.225230	65.515098
1525.080042	85.279347	65.520103
1524.019736	74.417605	65.525108
1523.005663	76.694855	65.530113
1522.373181	82.438924	65.535118
1521.823552	86.178247	65.540122
1521.569528	80.267476	65.545127
1521.384939	79.640792	65.550132
1520.429002	88.213123	65.555137
1519.499648	82.587847	65.560142
1519.073210	73.490820	65.565146
1517.952309	83.746649	65.570151
1517.154212	77.277394	65.575156
1516.662132	76.406274	65.580161
1516.373314	74.812189	65.585166
1516.003320	88.211238	65.590170
1514.799578	81.260843	65.595175
1514.202435	67.034593	65.600180
1513.395826	82.185532	65.605185
1513.110110	83.350470	65.610190
1512.697853	73.279842	65.615194
1511.768646	79.924147	65.620199
1511.417080	87.763390	65.625204
1510.230592	78.317230	65.630209
1509.441724	82.138721	65.635214
1508.667346	84.493002	65.640218
1508.162998	87.979140	65.645223
1508.024302	86.739648	65.650228
1506.997537	84.217362	65.655233
1506.278467	69.204708	65.660238
1505.582535	79.342548	65.665242
1505.151288	86.286178	65.670247
1504.759525	78.716357	65.675252
1503.232638	76.801796	65.680257
1502.698485	81.412245	65.685262
1502.198878	92.021918	65.690266
1501.922815	87.904394	65.695271
1500.782155	77.414956	65.700276
1500.038593	84.043958	65.705281
1499.680522	80.062464	65.710286
1499.198556	94.991528	65.715290
1498.664434	69.786576	65.720295
1498.008140	88.813226	65.725300
1497.193257	94.297722	65.730305
1496.408717	83.603466	65.735310
1495.980434	61.894970	65.740314
1494.437843	89.508150	65.745319
1494.244069	80.511341	65.750324
1493.783318	81.320917	65.755329
1493.297729	70.118721	65.760334
1492.692529	90.583240	65.765338
1491.498658	81.395291	65.770343
1491.249848	72.634302	65.775348
1490.408695	78.883018	65.780353
1490.228264	97.465074	65.785358
1489.064253	80.921023	65.790362
1487.896389	78.919458	65.795367
1487.946759	89.123206	65.800372
1487.790475	70.501559	65.805377
1486.316227	95.230843	65.810382
1485.591838	62.376800	65.815386
1484.933385	94.073912	65.820391
1484.807324	58.832031	65.825396
1483.831580	88.483899	65.830401
1483.274951	73.270406	65.835406
1482.318090	71.224275	65.840410
1481.866495	51.395975	65.845415
1481.645832	94.337514	65.850420
1480.322731	66.388057	65.855425
1479.308380	90.046095	65.860430
1479.275608	71.702849	65.865434
1478.379293	85.314839	65.870439
1478.268107	71.602697	65.875444
1477.202532	79.815588	65.880449
1476.548238	88.515027	65.885454
1476.111205	88.228069	65.890458
1475.504938	81.874992	65.895463
1474.708523	65.160595	65.900468
1473.759501	71.804902	65.905473
1473.323090	81.135149	65.910478
1473.116740	89.998358	65.915482
1471.599338	77.961978	65.920487
1470.966169	73.929598	65.925492
1470.648137	87.580572	65.930497
1470.069542	64.156686	65.935502
1469.634545	73.224945	65.940506
1468.610894	76.962338	65.945511
1467.987696	79.560671	65.950516
1467.570675	71.329439	65.955521
1466.678291	76.616530	65.960526
1465.978626	74.092741	65.965530
1465.546805	72.783147	65.970535
1465.198041	63.520842	65.975540
1463.874989	86.616112	65.980545
1463.198148	78.074527	65.985550
1462.868925	71.478745	65.990554
1461.865051	63.939991	65.995559
1461.825666	87.889338	66.000564
1460.568842	78.936905	66.005569
1460.257981	66.245200	66.010574
1459.712273	69.996520	66.015578
1458.159775	81.577717	66.020583
1457.755494	60.914040	66.025588
1457.134287	94.071713	66.030593
1456.807464	43.534645	66.035598
1456.100107	85.003438	66.040602
1455.748653	66.204675	66.045607
1454.988754	79.336117	66.050612
1454.169239	83.531480	66.055617
1453.563892	79.034236	66.060622
1452.976084	68.439624	66.065626
1451.778294	88.662446	66.070631
1451.599431	50.341487	66.075636
1450.721772	98.616316	66.080641
1450.348641	71.115110	66.085646
1449.528148	79.937151	66.090650
1448.354972	69.735175	66.095655
1448.198645	81.649545	66.100660
1447.738738	71.485589	66.105665
1447.042042	72.673274	66.110670
1446.112157	69.217884	66.115674
1445.351512	56.879933	66.120679
1445.114170	72.437111	66.125684
1444.376854	86.799657	66.130689
1443.406725	81.067359	66.135694
1442.969380	60.317485	66.140698
1442.285245	87.176112	66.145703
1442.055216	55.678493	66.150708
1440.410172	89.907145	66.155713
1439.971101	76.128853	66.160718
1439.529164	74.760951	66.165722
1439.026343	72.589064	66.170727
1438.670011	83.581219	66.175732
1437.278498	70.583474	66.180737
1436.693450	86.930746	66.185742
1436.584455	55.685115	66.190746
1436.016748	97.871295	66.195751
1434.730542	79.202162	66.200756
1433.996947	76.843037	66.205761
1433.602946	94.061921	66.210766
1433.129499	54.860581	66.215770
1432.505049	87.511001	66.220775
1432.096640	63.911861	66.225780
1430.760428	70.199849	66.230785
1430.215986	79.030056	66.235790
1430.369656	61.710547	66.240794
1428.777464	89.885109	66.245799
1428.438899	64.071987	66.250804
1427.402063	64.053822	66.255809
1427.119599	85.369006	66.260814
1426.466803	76.025720	66.265818
1425.391312	70.086265	66.270823
1425.037207	72.173509	66.275828
1424.628025	72.732063	66.280833
1423.815863	76.603007	66.285838
1423.072591	85.272443	66.290842
1422.187812	76.986260	66.295847
1422.048182	63.644491	66.300852
1421.308756	84.489860	66.305857
1420.680792	65.474876	66.310862
1419.907792	72.692007	66.315866
1419.540048	79.958267	66.320871
1418.482722	68.908464	66.325876
1417.288559	88.422704	66.330881
1417.228459	63.755863	66.335886
1416.531129	89.705164	66.340890
1415.939221	74.397960	66.345895
1415.300977	74.098841	66.350900
1414.271053	86.084256	66.355905
1414.010047	76.787507	66.360910
1413.665060	53.939936	66.365914
1411.960826	91.520955	66.370919
1411.705786	72.571265	66.375924
1411.193694	63.509964	66.380929
1410.719792	77.840099	66.385934
1409.909096	84.572825	66.390938
1408.949084	75.041845	66.395943
1408.276991	65.296386	66.400948
1408.001826	74.369206	66.405953
1407.461705	72.444514	66.410958
1406.767952	73.820965	66.415962
1405.798745	62.129576	66.420967
1405.360127	85.046439	66.425972
1405.236882	71.094969	66.430977
1403.786677	67.528344	66.435982
1403.201524	75.562400	66.440986
1402.838878	56.565186	66.445991
1402.066554	67.248155	66.450996
1400.884721	72.013599	66.456001
1400.421540	82.555985	66.461006
1400.018802	69.738555	66.466010
1399.523195	80.420127	66.471015
1398.849152	76.799517	66.476020
1397.987198	68.894477	66.481025
1397.098467	78.003325	66.486030
1397.123474	82.546991	66.491034
1395.686602	81.854450	66.496039
1395.181320	73.728722	66.501044
1394.255358	76.018822	66.506049
1394.012558	75.784579	66.511054
1393.764270	72.083685	66.516058
1392.312164	85.842377	66.521063
1391.943640	71.455260	66.526068
1391.647979	80.624377	66.531073
1390.649227	82.230651	66.536078
1390.547437	78.583736	66.541082
1389.260002	75.443806	66.546087
1388.632839	75.283272	66.551092
1388.192959	65.464642	66.556097
1387.328887	79.473619	66.561102
1386.802203	75.917895	66.566106
1385.775315	84.241356	66.571111
1385.618114	69.055873	66.576116
1385.164783	74.670568	66.581121
1384.440784	71.193516	66.586126
1383.525063	75.437302	66.591130
1382.529374	84.894301	66.596135
1382.371598	70.587222	66.601140
1381.229730	72.722421	66.606145
1380.463206	71.078137	66.611150
1379.875282	69.815449	66.616154
1379.352166	78.257517	66.621159
1379.581430	69.100457	66.626164
1378.100593	76.387538	66.631169
1377.372192	74.054412	66.636174
1377.024982	80.142647	66.641178
1376.587988	78.408138	66.646183
1375.809136	71.298828	66.651188
1374.981561	71.050313	66.656193
1374.277343	80.465711	66.661198
1373.226912	76.234771	66.666202
1372.132363	90.498004	66.671207
1371.942933	72.085071	66.676212
1371.077848	82.199362	66.681217
1370.745394	77.114746	66.686222
1371.134930	71.260969	66.691226
1369.723708	82.956940	66.696231
1368.998208	78.155562	66.701236
1368.439193	82.147123	66.706241
1367.609127	80.159725	66.711246
1367.063109	79.968953	66.716250
1366.070279	85.272042	66.721255
1365.927720	78.320194	66.726260
1365.209631	77.201195	66.731265
1364.266670	86.947846	66.736270
1363.587837	84.644689	66.741274
1363.039571	80.444309	66.746279
1362.535831	73.264464	66.751284
1361.371685	88.320885	66.756289
1360.229496	90.585449	66.761294
1360.556247	80.614992	66.766298
1359.594955	79.744377	66.771303
1359.545222	100.178957	66.776308
1358.601885	83.273497	66.781313
1357.479833	78.620310	66.786318
1357.324495	78.025258	66.791322
1356.597908	83.648706	66.796327
1355.727363	72.421017	66.801332
1354.590667	92.471738	66.806337
1354.050547	69.782911	66.811342
1354.052965	71.340430	66.816346
1353.247959	81.732163	66.821351
1352.427291	84.240493	66.826356
1351.817142	83.353483	66.831361
1351.217169	68.913292	66.836366
1350.647915	76.128013	66.841370
1349.318638	91.690057	66.846375
1349.128307	77.172124	66.851380
1348.555196	74.125233	66.856385
1348.060070	85.592014	66.861390
1347.060381	69.875029	66.866394
1346.129396	103.819925	66.871399
1345.685384	76.290603	66.876404
1345.494794	82.011764	66.881409
1344.214738	73.285434	66.886414
1343.540357	73.684320	66.891418
1343.147669	87.432308	66.896423
1342.633268	56.221199	66.901428
1342.151424	89.131200	66.906433
1341.139130	87.619031	66.911438
1340.665028	65.411704	66.916442
1339.834658	77.154109	66.921447
1339.392418	96.566194	66.926452
1338.256327	70.646504	66.931457
1337.357458	78.334649	66.936462
1337.194124	79.968977	66.941466
1336.662530	86.001378	66.946471
1336.264546	71.227898	66.951476
1335.322047	78.711680	66.956481
1334.296912	71.316703	66.961486
1334.019511	87.093132	66.966490
1333.302599	71.424235	66.971495
1332.623650	73.865887	66.976500
1331.839728	81.013820	66.981505
1331.263567	77.737195	66.986510
1331.168297	67.378122	66.991514
1329.889675	77.755268	66.996519
1329.450950	66.473141	67.001524
1328.803120	78.822007	67.006529
1328.282167	81.796754	67.011534
1327.787887	58.618149	67.016538
1326.725367	76.339076	67.021543
1326.185408	76.510028	67.026548
1324.946392	70.957720	67.031553
1324.227703	70.449075	67.036558
1323.895356	82.109161	67.041562
1323.326219	80.018799	67.046567
1323.203999	78.888658	67.051572
1322.209031	58.153371	67.056577
1321.298969	87.296515	67.061582
1320.940675	88.693772	67.066586
1320.076518	79.907641	67.071591
1318.948718	72.041742	67.076596
1318.529770	74.853625	67.081601
1317.952086	79.548289	67.086606
1317.649616	73.235272	67.091610
1316.931053	67.015214	67.096615
1315.792258	82.045535	67.101620
1315.599804	72.056706	67.106625
1314.844020	67.086710	67.111630
1314.582209	63.017416	67.116634
1313.270460	76.714397	67.121639
1312.884112	73.546366	67.126644
1312.430423	68.905213	67.131649
1311.241926	84.302965	67.136654
1310.718059	71.958953	67.141658
1310.058764	65.861932	67.146663
1309.680274	66.295783	67.151668
1309.078853	75.401550	67.156673
1307.764629	91.068441	67.161678
1307.200214	54.032487	67.166682
1306.647910	91.616466	67.171687
1306.248965	57.980723	67.176692
1306.008978	76.029753	67.181697
1304.684710	80.308556	67.186702
1304.003303	67.475540	67.191706
1303.502229	76.417130	67.196711
1303.285620	75.784517	67.201716
1302.236786	65.614894	67.206721
1301.103195	67.983762	67.211726
1300.779076	77.174748	67.216730
1300.699863	62.352187	67.221735
1299.932503	58.932517	67.226740
1299.018136	64.447061	67.231745
1298.180841	79.002121	67.236750
1297.818445	61.916055	67.241754
1296.456437	73.918020	67.246759
1295.900846	75.643097	67.251764
1295.613384	70.212319	67.256769
1294.899356	74.028274	67.261774
1294.905780	71.373356	67.266778
1293.395867	72.026511	67.271783
1292.932994	69.624390	67.276788
1292.512788	72.603624	67.281793
1291.646111	77.200743	67.286798
1290.811108	69.138508	67.291802
1289.988711	71.109418	67.296807
1289.371762	66.689759	67.301812
1289.133052	71.691634	67.306817
1288.593330	77.302731	67.311822
1287.791160	67.237393	67.316826
1286.916129	72.763035	67.321831
1286.769470	80.207030	67.326836
1286.136494	72.207286	67.331841
1285.351587	63.272971	67.336846
1284.635216	65.761582	67.341850
1283.572107	69.998870	67.346855
1282.676677	73.630792	67.351860
1282.256677	79.443617	67.356865
1281.775985	59.479671	67.361870
1281.370744	66.480674	67.366874
1280.427153	73.084754	67.371879
1279.424289	77.180011	67.376884
1279.103172	62.689211	67.381889
1278.260555	78.052472	67.386894
1278.114761	68.707478	67.391898
1276.882618	76.942183	67.396903
1276.433176	74.720846	67.401908
1275.902529	75.951556	67.406913
1275.161040	83.731386	67.411918
1275.018256	69.212226	67.416922
1273.939081	71.879942	67.421927
1273.114042	66.853167	67.426932
1272.770029	63.530189	67.431937
1271.447898	75.587323	67.436942
1270.951977	73.179423	67.441946
1270.148382	75.342882	67.446951
1269.816653	68.291826	67.451956
1269.794813	65.706055	67.456961
1268.481853	65.148418	67.461966
1268.227467	74.129631	67.466970
1267.427886	72.093269	67.471975
1266.503387	64.165118	67.476980
1265.726819	65.070675	67.481985
1264.762631	78.261431	67.486990
1264.676295	63.113598	67.491994
1263.895041	70.514992	67.496999
1263.227793	69.993454	67.502004
1262.344190	64.580203	67.507009
1261.889746	73.107551	67.512014
1261.475813	69.202791	67.517018
1260.877694	74.239738	67.522023
1259.864056	78.764045	67.527028
1259.370568	77.691362	67.532033
1258.483129	73.169646	67.537038
1258.259004	69.783455	67.542042
1257.225199	65.862146	67.547047
1256.377123	77.924332	67.552052
1255.978017	77.599845	67.557057
1255.477353	81.843906	67.562062
1254.882231	67.511786	67.567066
1253.606011	72.216608	67.572071
1252.962515	74.192199	67.577076
1252.568350	62.679098	67.582081
1252.216699	69.149643	67.587086
1251.554457	69.802074	67.592090
1250.635577	78.302353	67.597095
1250.140954	82.097627	67.602100
1249.892638	72.018349	67.607105
1248.633525	86.804489	67.612110
1247.796042	74.843081	67.617114
1247.295232	81.211200	67.622119
1246.716152	71.123019	67.627124
1246.545399	74.248665	67.632129
1245.555921	81.353612	67.637134
1245.181874	69.127721	67.642138
1244.321767	82.803379	67.647143
1242.969225	78.160091	67.652148
1242.542978	73.795271	67.657153
1241.819248	77.239066	67.662158
1241.765672	75.665955	67.667162
1240.928861	78.854933	67.672167
1239.780577	80.708955	67.677172
1239.604847	69.087007	67.682177
1239.180155	79.107647	67.687182
1238.638288	74.633487	67.692186
1237.356602	83.511564	67.697191
1236.589350	83.559413	67.702196
1236.646307	68.139652	67.707201
1235.366640	70.888145	67.712206
1234.459917	69.803910	67.717210
1233.919479	73.724733	67.722215
1233.404405	75.765059	67.727220
1233.367951	71.792397	67.732225
1232.139173	69.956750	67.737230
1231.566783	64.695864	67.742234
1230.664580	72.286799	67.747239
1230.348465	74.552517	67.752244
1229.643460	68.923232	67.757249
1228.479358	80.018602	67.762254
1228.557094	77.090587	67.767258
1227.969240	75.460515	67.772263
1227.013062	70.716368	67.777268
1226.207050	70.115986	67.782273
1225.185502	67.809024	67.787278
1224.912990	68.446796	67.792282
1224.460920	72.941737	67.797287
1223.702351	69.851833	67.802292
1222.957623	67.477201	67.807297
1222.252502	71.991882	67.812302
1221.945569	67.806781	67.817306
1220.850980	72.159479	67.822311
1219.833373	70.135727	67.827316
1219.527386	63.287159	67.832321
1219.144998	72.477948	67.837326
1218.751406	57.150344	67.842330
1217.603468	76.100636	67.847335
1217.061089	72.533258	67.852340
1216.866427	69.202308	67.857345
1215.361856	74.823347	67.862350
1214.841314	56.762733	67.867354
1214.005933	69.802132	67.872359
1213.673715	71.129026	67.877364
1213.473968	66.840155	67.882369
1212.346828	70.447446	67.887374
1211.509815	71.736348	67.892378
1211.101776	71.518938	67.897383
1210.578828	79.424866	67.902388
1209.824035	73.827156	67.907393
1209.015292	63.272496	67.912398
1208.144792	68.261305	67.917402
1207.638970	65.099679	67.922407
1207.198902	72.552480	67.927412
1207.211304	67.028306	67.932417
1205.976736	69.364388	67.937422
1205.503903	67.014330	67.942426
1204.259356	84.494597	67.947431
1203.466683	64.503021	67.952436
1202.741204	88.247611	67.957441
1202.261540	73.969681	67.962446
1201.764723	69.582979	67.967450
1201.727847	76.791905	67.972455
1200.464230	85.440057	67.977460
1199.959988	79.927077	67.982465
1199.148938	77.909907	67.987470
1198.627792	72.006980	67.992474
1197.498629	74.528144	67.997479
1197.134759	72.474554	68.002484
1196.845426	68.337117	68.007489
1196.048497	76.535758	68.012494
1195.166122	63.723711	68.017498
1194.545382	60.119920	68.022503
1193.737551	89.811331	68.027508
1193.615872	73.174257	68.032513
1192.687786	64.622272	68.037518
1191.679544	91.453597	68.042522
1191.213336	73.567247	68.047527
1190.588086	71.870596	68.052532
1189.921032	79.643334	68.057537
1188.862033	73.803867	68.062542
1188.247813	70.271574	68.067546
1187.837850	76.169538	68.072551
1187.557110	63.376929	68.077556
1187.373926	74.300547	68.082561
1185.931812	65.656855	68.087566
1185.485757	73.616783	68.092570
1185.029164	80.204945	68.097575
1183.625458	69.134662	68.102580
1183.115318	76.368390	68.107585
1182.861202	72.168586	68.112590
1182.205405	62.322856	68.117594
1181.060723	87.323062	68.122599
1180.229131	79.447971	68.127604
1180.314513	64.274423	68.132609
1179.723764	84.063317	68.137614
1178.808326	65.158812	68.142618
1177.742774	83.619810	68.147623
1176.968255	103.849517	68.152628
1176.948225	72.540921	68.157633
1176.287845	83.303906	68.162638
1175.697548	81.999068	68.167642
1174.425100	61.664367	68.172647
1173.748070	90.861920	68.177652
1173.820385	67.620070	68.182657
1173.100616	95.946119	68.187662
1172.345464	59.626505	68.192666
1171.587274	98.503127	68.197671
1170.726577	69.182626	68.202676
1170.036479	90.964712	68.207681
1168.966914	66.693432	68.212686
1168.860486	80.231895	68.217690
1168.382619	88.800829	68.222695
1167.759525	80.898891	68.227700
1166.551662	71.789048	68.232705
1165.950932	83.879725	68.237710
1165.668967	79.203409	68.242714
1165.157474	81.776157	68.247719
1163.791351	84.650393	68.252724
1163.708525	68.625282	68.257729
1163.066988	70.745653	68.262734
1162.267114	75.652287	68.267738
1161.429140	77.001278	68.272743
1160.434558	80.999072	68.277748
1160.206381	80.281584	68.282753
1159.537556	84.148728	68.287758
1159.040565	80.260349	68.292762
1157.889070	82.439749	68.297767
1157.295212	90.986135	68.302772
1157.253741	76.074011	68.307777
1156.533755	82.570034	68.312782
1155.537351	91.858491	68.317786
1154.769594	66.123201	68.322791
1154.427552	83.171381	68.327796
1154.147431	81.309469	68.332801
1152.969691	57.075921	68.337806
1152.035288	90.705955	68.342810
1152.007065	60.677531	68.347815
1150.726588	94.321616	68.352820
1150.257038	68.713928	68.357825
1149.597744	78.642582	68.362830
1149.012617	81.441497	68.367834
1148.511061	86.385843	68.372839
1147.632007	72.103649	68.377844
1146.956442	82.561565	68.382849
1146.402405	91.508449	68.387854
1146.054519	73.489764	68.392858
1144.937724	90.733707	68.397863
1144.185704	67.246100	68.402868
1143.860747	95.588198	68.407873
1142.881509	82.720606	68.412878
1142.904041	46.983791	68.417882
1141.554943	101.156880	68.422887
1140.800024	75.898905	68.427892
1140.822409	83.718111	68.432897
1139.360871	69.344072	68.437902
1138.903456	91.027654	68.442906
1137.924262	85.576036	68.447911
1138.089939	65.082010	68.452916
1137.616018	99.400449	68.457921
1136.326326	85.924682	68.462926
1135.967494	50.485046	68.467930
1135.385889	51.749116	68.472935
1134.278048	96.411638	68.477940
1133.540092	91.319020	68.482945
1132.564452	79.920498	68.487950
1132.572554	77.189627	68.492954
1132.189736	94.203306	68.497959
1131.414751	83.953937	68.502964
1130.423770	82.205090	68.507969
1129.696498	77.049282	68.512974
1129.235761	77.816343	68.517978
1128.799014	96.087474	68.522983
1127.661491	79.957311	68.527988
1127.461998	84.759005	68.532993
1126.620934	99.776734	68.537998
1125.763237	78.726410	68.543002
1124.924258	80.696855	68.548007
1124.059086	95.128668	68.553012
1124.105684	91.631625	68.558017
1123.368164	72.345627	68.563022
1122.739609	97.167581	68.568026
1121.818800	79.558548	68.573031
1120.934332	81.786950	68.578036
1120.756593	87.064551	68.583041
1120.205311	92.616020	68.588046
1119.424440	75.915083	68.593050
1118.576510	74.794732	68.598055
1117.683027	73.383601	68.603060
1117.553821	93.638384	68.608065
1116.412944	90.159914	68.613070
1115.870713	86.356006	68.618074
1115.377059	80.746752	68.623079
1114.947372	87.147729	68.628084
1114.243580	85.532971	68.633089
1113.036177	78.917674	68.638094
1112.734426	81.488608	68.643098
1112.023581	76.960937	68.648103
1110.926623	90.559188	68.653108
1110.342678	83.770612	68.658113
1109.455257	88.727457	68.663118
1109.318538	88.194111	68.668122
1109.057092	78.601044	68.673127
1108.338755	77.408047	68.678132
1107.397879	83.543423	68.683137
1106.779551	93.598034	68.688142
1106.140322	85.197239	68.693146
1105.872685	82.516534	68.698151
1104.651218	85.564899	68.703156
1104.710647	76.233014	68.708161
1103.216468	92.098900	68.713166
1102.262183	80.854683	68.718170
1101.972643	79.192961	68.723175
1101.140034	84.727680	68.728180
1101.171464	74.496709	68.733185
1100.340304	74.130590	68.738190
1099.134089	91.275234	68.743194
1099.040375	85.006315	68.748199
1098.270525	88.302950	68.753204
1097.516352	74.041914	68.758209
1096.419123	74.609042	68.763214
1095.724929	72.828772	68.768218
1095.501234	82.809567	68.773223
1094.769171	74.675846	68.778228
1094.551821	88.039575	68.783233
1093.611057	76.821597	68.788238
1092.845951	77.309092	68.793242
1092.604909	90.684476	68.798247
1091.261032	80.746377	68.803252
1091.015862	84.292273	68.808257
1090.226596	68.190325	68.813262
1089.382637	84.842130	68.818266
1088.965673	78.276146	68.823271
1087.702143	80.930686	68.828276
1087.463056	87.645104	68.833281
1086.903441	86.841579	68.838286
1086.593622	76.970800	68.843290
1085.782044	71.200830	68.848295
1084.635684	96.851002	68.853300
1084.698773	67.110820	68.858305
1083.930095	84.223708	68.863310
1083.086043	84.367393	68.868314
1082.122587	93.418833	68.873319
1081.501969	65.039441	68.878324
1081.106506	91.521004	68.883329
1080.102910	74.168007	68.888334
1079.287781	101.681382	68.893338
1078.808499	78.210330	68.898343
1078.032039	76.843672	68.903348
1077.906028	76.840027	68.908353
1076.831752	74.423249	68.913358
1076.306735	75.713024	68.918362
1076.037428	68.846032	68.923367
1075.134124	79.642940	68.928372
1074.543455	82.037498	68.933377
1073.735273	75.562134	68.938382
1073.204663	74.206830	68.943386
1072.707044	85.357077	68.948391
1071.488532	71.382794	68.953396
1071.073095	89.809788	68.958401
1070.689417	78.061683	68.963406
1069.567724	64.669637	68.968410
1068.667249	89.804474	68.973415
1067.862210	58.821082	68.978420
1067.635283	101.607366	68.983425
1067.175454	67.286018	68.988430
1066.720650	69.900223	68.993434
1066.065404	87.908073	68.998439
1065.215179	79.630741	69.003444
1064.970398	81.418378	69.008449
1064.309048	78.992687	69.013454
1063.069767	73.090500	69.018458
1062.904782	72.146940	69.023463
1061.745138	72.429139	69.028468
1061.370103	71.753945	69.033473
1060.550487	85.196130	69.038478
1059.615153	71.675096	69.043482
1059.122932	77.195097	69.048487
1058.141212	70.250637	69.053492
1057.769166	78.671863	69.058497
1057.262756	99.514896	69.063502
1056.751609	65.673203	69.068506
1055.480723	88.583674	69.073511
1054.951363	66.883547	69.078516
1054.848244	79.241980	69.083521
1054.114816	95.160325	69.088526
1052.499704	79.189759	69.093530
1052.157700	65.003524	69.098535
1051.287318	86.161467	69.103540
1051.099709	61.368376	69.108545
1050.838504	96.122854	69.113550
1050.426993	69.100998	69.118554
1049.530126	67.925382	69.123559
1048.643426	89.087502	69.128564
1048.078880	60.735485	69.133569
1047.197676	81.625500	69.138574
1046.142770	92.292009	69.143578
1045.954906	79.032088	69.148583
1045.115652	82.776568	69.153588
1045.111532	77.526247	69.158593
1044.369629	72.341260	69.163598
1043.384457	81.303123	69.168602
1043.099452	74.815501	69.173607
1041.189517	98.105181	69.178612
1041.059600	66.956044	69.183617
1040.000989	108.050221	69.188622
1039.802182	64.990981	69.193626
1039.502734	86.583191	69.198631
1039.320163	80.164422	69.203636
1038.520270	71.962672	69.208641
1037.526362	84.327211	69.213646
1036.976004	77.230560	69.218650
1036.036941	71.461968	69.223655
1034.690428	80.590121	69.228660
1034.635053	78.774467	69.233665
1034.043665	72.625732	69.238670
1033.595928	80.779897	69.243674
1032.941084	78.004694	69.248679
1032.270601	76.042485	69.253684
1031.839714	84.652838	69.258689
1030.819636	73.654081	69.263694
1030.003579	70.844606	69.268698
1029.488567	91.882950	69.273703
1029.069583	81.852940	69.278708
1027.997899	66.194899	69.283713
1027.337132	86.042243	69.288718
1026.625526	70.353721	69.293722
1026.840844	67.851647	69.298727
1025.258047	91.857209	69.303732
1024.247879	72.720287	69.308737
1023.834283	79.290587	69.313742
1023.383944	95.767835	69.318746
1023.169884	67.202373	69.323751
1022.213888	87.852002	69.328756
1021.640830	73.186895	69.333761
1021.023291	76.441972	69.338766
1020.097737	75.728219	69.343770
1019.800806	75.015375	69.348775
1018.492243	80.692064	69.353780
1018.278701	78.568858	69.358785
1017.971153	75.393075	69.363790
1017.126325	79.803883	69.368794
1016.845668	66.192912	69.373799
1015.879993	84.258033	69.378804
1015.073757	76.598161	69.383809
1014.265888	70.802398	69.388814
1013.558097	80.980049	69.393818
1012.686635	62.085992	69.398823
1011.442418	82.308413	69.403828
1010.970177	75.752820	69.408833
1010.569468	75.844917	69.413838
1009.960210	71.575493	69.418842
1010.092996	67.924405	69.423847
1009.975412	65.141001	69.428852
1009.065987	69.789152	69.433857
1008.004759	70.068333	69.438862
1007.056938	85.293851	69.443866
1006.078154	69.521698	69.448871
1005.146536	71.349232	69.453876
1004.817760	65.751625	69.458881
1004.116629	75.187091	69.463886
1003.655127	69.094967	69.468890
1002.737930	69.504190	69.473895
1001.989275	75.517555	69.478900
1001.633516	68.145545	69.483905
1001.536452	73.243160	69.488910
1000.657433	69.626902	69.493914
999.748357	62.090632	69.498919
999.200172	72.958778	69.503924
998.670060	76.852769	69.508929
997.426260	63.243666	69.513934
996.364458	60.200508	69.518938
996.483234	70.954653	69.523943
995.668441	85.091476	69.528948
995.788671	63.341643	69.533953
995.182415	57.097526	69.538958
994.014413	72.151496	69.543962
993.368422	71.090517	69.548967
992.041979	76.415269	69.553972
991.310960	70.017543	69.558977
990.832342	80.650714	69.563982
990.338195	75.240257	69.568986
990.318343	64.768320	69.573991
989.291674	62.990521	69.578996
988.412051	64.120702	69.584001
987.735761	78.710116	69.589006
987.159715	68.175293	69.594010
986.325556	69.692455	69.599015
985.290281	72.345416	69.604020
985.626322	58.106516	69.609025
984.785741	78.025035	69.614030
984.143021	49.816391	69.619034
983.350224	90.712115	69.624039
982.674158	57.390281	69.629044
981.754631	70.816826	69.634049
980.889835	71.813771	69.639054
980.278984	72.633125	69.644058
979.691691	57.547717	69.649063
979.433194	72.311911	69.654068
979.207727	66.090782	69.659073
978.065263	75.423018	69.664078
977.241962	71.703292	69.669082
976.958635	69.067679	69.674087
975.595446	59.826558	69.679092
974.780129	74.944262	69.684097
974.391479	68.055279	69.689102
973.864371	73.107785	69.694106
973.926814	71.497302	69.699111
972.609126	63.843143	69.704116
972.019367	85.930940	69.709121
972.005791	61.009268	69.714126
970.597543	65.708416	69.719130
970.186629	73.405743	69.724135
969.189628	65.856669	69.729140
968.884434	89.578545	69.734145
967.656866	51.170814	69.739150
966.700905	90.277538	69.744154
966.767466	61.402547	69.749159
966.336605	67.191897	69.754164
965.754154	69.591476	69.759169
964.904575	69.942648	69.764174
963.984480	68.337124	69.769178
963.713147	72.298747	69.774183
962.480263	71.692260	69.779188
961.347277	76.768638	69.784193
961.169167	80.442633	69.789198
960.402294	82.256585	69.794202
960.324701	72.732064	69.799207
960.238942	70.014558	69.804212
959.305079	67.061438	69.809217
958.469103	73.445075	69.814222
957.564633	76.048850	69.819226
956.907568	66.064639	69.824231
955.883889	68.794608	69.829236
955.223357	69.639218	69.834241
955.176722	67.612457	69.839246
953.797477	82.411497	69.844250
953.170336	66.679612	69.849255
952.246071	71.511482	69.854260
952.071241	62.197971	69.859265
952.042881	74.519265	69.864270
950.680374	66.478036	69.869274
950.140590	72.330450	69.874279
949.754694	73.121901	69.879284
949.313785	60.835782	69.884289
948.174207	66.173391	69.889294
946.993754	72.261782	69.894298
946.779488	66.459896	69.899303
946.396696	67.507881	69.904308
945.712915	72.741429	69.909313
945.040733	70.913548	69.914318
944.209391	83.389428	69.919322
943.781284	69.658442	69.924327
942.684315	70.466853	69.929332
941.942348	69.315511	69.934337
941.628796	70.555893	69.939342
941.216124	72.393908	69.944346
940.781663	72.013599	69.949351
939.408808	77.968619	69.954356
939.008709	60.767256	69.959361
938.432419	60.808461	69.964366
937.103021	77.599023	69.969370
936.513010	73.099489	69.974375
935.929760	69.486651	69.979380
935.378917	82.911316	69.984385
935.194326	64.316407	69.989390
934.743112	75.750990	69.994394
934.153132	66.274897	69.999399
933.227400	75.380285	70.004404
932.550679	71.252497	70.009409
931.585358	69.277314	70.014414
930.365190	81.985369	70.019418
930.140973	78.321705	70.024423
929.786868	70.586771	70.029428
929.281878	68.344383	70.034433
928.525961	61.247369	70.039438
927.659628	75.591079	70.044442
927.392467	70.250169	70.049447
926.697570	62.186294	70.054452
925.503886	86.748091	70.059457
924.989369	60.647816	70.064462
924.362111	87.323921	70.069466
923.772610	75.955521	70.074471
923.036131	57.375911	70.079476
922.078226	67.134503	70.084481
921.859449	66.991095	70.089486
921.162542	74.375991	70.094490
921.006320	57.943179	70.099495
919.773236	60.698599	70.104500
918.967433	73.026917	70.109505
918.741188	71.229000	70.114510
917.621594	72.012639	70.119514
916.662665	71.638529	70.124519
915.750635	68.812831	70.129524
915.714862	73.216336	70.134529
915.322414	68.631758	70.139534
914.938918	76.442992	70.144538
914.947022	61.332239	70.149543
913.717402	52.743225	70.154548
912.513380	70.892005	70.159553
911.646874	62.784486	70.164558
910.816708	74.402369	70.169562
910.502854	69.409493	70.174567
910.307673	74.948472	70.179572
909.302727	72.689461	70.184577
908.748902	69.163405	70.189582
907.824908	82.075056	70.194586
907.130905	72.807898	70.199591
906.206733	79.207164	70.204596
905.805293	79.020290	70.209601
905.507093	63.922014	70.214606
904.888360	75.960386	70.219610
904.032091	67.247303	70.224615
903.334115	66.502108	70.229620
902.205444	67.019133	70.234625
902.121734	66.816388	70.239630
901.119549	68.499079	70.244634
900.139498	65.081854	70.249639
899.502747	68.615962	70.254644
899.117331	75.694264	70.259649
899.050919	69.059928	70.264654
898.551680	70.017648	70.269658
897.527779	62.625845	70.274663
896.657092	64.088927	70.279668
896.152209	76.703657	70.284673
895.215971	60.096957	70.289678
894.408845	61.671342	70.294682
893.941159	66.135695	70.299687
893.558773	66.792562	70.304692
893.129793	69.461026	70.309697
891.934795	55.673931	70.314702
890.958535	74.418793	70.319706
890.880689	62.251520	70.324711
890.328967	58.125932	70.329716
889.210513	61.244722	70.334721
888.579276	74.420420	70.339726
888.131090	74.701430	70.344730
887.646966	54.055422	70.349735
886.809689	54.423585	70.354740
885.810005	71.642624	70.359745
885.390103	68.008535	70.364750
884.906628	72.962652	70.369754
884.622531	52.015172	70.374759
883.787804	70.789543	70.379764
883.229572	68.539870	70.384769
882.638385	64.324376	70.389774
881.122071	61.161228	70.394778
880.545926	59.500999	70.399783
880.338422	57.824676	70.404788
879.560270	69.385400	70.409793
878.567298	69.100297	70.414798
878.108295	62.342377	70.419802
877.807059	50.704223	70.424807
877.208046	67.033222	70.429812
876.089800	81.738717	70.434817
875.472188	50.884904	70.439822
874.879433	83.076069	70.444826
874.241870	59.600370	70.449831
873.482998	75.981628	70.454836
872.331566	56.375324	70.459841
872.053639	64.425203	70.464846
871.602170	69.763710	70.469850
871.518040	64.664901	70.474855
870.652495	58.589813	70.479860
869.579429	71.643452	70.484865
869.237986	59.794086	70.489870
868.063591	65.769586	70.494874
867.205314	61.071512	70.499879
867.017600	48.593755	70.504884
866.295022	66.878795	70.509889
865.877814	56.165787	70.514894
864.459557	70.895370	70.519898
863.699400	69.535649	70.524903
863.990276	60.892310	70.529908
863.237506	56.992681	70.534913
863.004109	68.025188	70.539918
861.455773	76.031277	70.544922
861.259325	65.678920	70.549927
860.648510	64.167706	70.554932
859.437286	56.868813	70.559937
858.976249	52.057063	70.564942
858.133630	84.261189	70.569946
857.867199	39.107789	70.574951
857.202519	68.579261	70.579956
856.515275	63.056082	70.584961
855.934060	56.264009	70.589966
855.015727	83.375913	70.594970
854.286874	53.197361	70.599975
853.330951	66.859943	70.604980
852.646316	73.474971	70.609985
852.871968	63.550568	70.614990
851.968492	75.594844	70.619994
851.007062	75.386727	70.624999
850.081214	69.460004	70.630004
849.606655	69.123939	70.635009
849.418605	59.664327	70.640014
848.744811	64.708658	70.645018
847.617211	72.937929	70.650023
846.988774	67.336010	70.655028
846.411263	64.876541	70.660033
846.166994	52.891879	70.665038
845.177640	66.643357	70.670042
844.338915	72.073465	70.675047
843.896107	52.073720	70.680052
843.318840	60.382539	70.685057
842.565636	65.963026	70.690062
841.617901	63.636596	70.695066
841.164696	53.227353	70.700071
840.849126	64.052176	70.705076
839.840842	62.072831	70.710081
838.965659	46.202312	70.715086
838.510435	85.806444	70.720090
838.269422	60.265039	70.725095
837.662256	76.852376	70.730100
836.550623	69.676401	70.735105
836.065828	58.980465	70.740110
834.979410	72.911393	70.745114
834.059797	66.349791	70.750119
833.611510	68.292831	70.755124
832.671998	64.719381	70.760129
832.581773	72.600627	70.765134
832.027740	66.777149	70.770138
831.925725	59.170842	70.775143
830.913018	73.875312	70.780148
830.234382	70.336028	70.785153
829.857826	57.490961	70.790158
828.221799	79.117691	70.795162
827.810756	67.889650	70.800167
827.139223	61.023656	70.805172
826.963972	72.981984	70.810177
826.045494	56.137549	70.815182
824.951115	88.427485	70.820186
824.470782	68.564577	70.825191
824.304008	56.567583	70.830196
823.389449	70.866947	70.835201
822.961164	53.673274	70.840206
821.862660	61.371247	70.845210
821.581868	85.032444	70.850215
820.961318	56.547555	70.855220
819.716331	87.358722	70.860225
819.290484	45.491636	70.865230
818.318124	89.369356	70.870234
818.529986	63.200816	70.875239
817.490156	82.097736	70.880244
816.730514	75.416063	70.885249
816.096775	70.655459	70.890254
815.741927	64.502256	70.895258
814.474375	81.406014	70.900263
814.153030	52.905048	70.905268
813.266823	71.283948	70.910273
813.349782	66.265773	70.915278
812.328014	56.620353	70.920282
811.473498	82.577305	70.925287
810.842535	62.531820	70.930292
810.235808	63.817305	70.935297
809.378694	67.794913	70.940302
808.392865	60.553203	70.945306
807.902161	78.725665	70.950311
807.526068	54.159781	70.955316
807.010302	89.314216	70.960321
806.627363	56.600232	70.965326
805.345208	101.932275	70.970330
804.983473	54.389324	70.975335
804.549602	82.799128	70.980340
803.241193	59.259950	70.985345
803.088844	94.607268	70.990350
802.229376	102.218338	70.995354
801.648409	71.942128	71.000359
800.801514	40.757471	71.005364
799.722709	92.977913	71.010369
799.680281	63.048056	71.015374
799.078957	72.276869	71.020378
798.037212	59.720610	71.025383
797.529838	83.447827	71.030388
796.677819	78.591094	71.035393
796.514744	54.868037	71.040398
795.685314	94.831350	71.045402
795.558317	62.138116	71.050407
794.530104	73.576248	71.055412
793.666835	73.445562	71.060417
793.014884	79.155019	71.065422
792.297181	69.648844	71.070426
791.505676	71.944550	71.075431
791.183535	91.662318	71.080436
789.674455	85.882069	71.085441
789.782307	51.771728	71.090446
788.922598	91.982688	71.095450
788.243826	63.037170	71.100455
788.067847	79.875976	71.105460
787.254845	78.969363	71.110465
786.414553	60.149316	71.115470
785.454579	88.076786	71.120474
785.456770	69.579905	71.125479
784.503569	60.090728	71.130484
783.623250	98.237733	71.135489
783.315057	51.162494	71.140494
782.552062	100.480165	71.145498
781.347564	79.114684	71.150503
780.913762	55.668100	71.155508
779.969163	87.524213	71.160513
780.178133	54.540993	71.165518
779.478378	84.622010	71.170522
778.408271	56.000566	71.175527
777.765242	76.701313	71.180532
777.295756	53.011273	71.185537
776.606822	85.239817	71.190542
775.694001	68.992122	71.195546
775.003051	49.959099	71.200551
774.917370	83.111828	71.205556
773.982391	62.178106	71.210561
773.378006	83.623293	71.215566
772.542587	56.317433	71.220570
771.639617	89.388983	71.225575
771.208330	49.834451	71.230580
770.108093	97.832360	71.235585
769.496746	66.884543	71.240590
769.232277	57.326734	71.245594
768.725736	92.296785	71.250599
768.116507	64.322587	71.255604
767.218872	48.610208	71.260609
766.575037	75.550680	71.265614
766.270973	69.198602	71.270618
765.184161	69.753175	71.275623
764.626223	73.973312	71.280628
763.911230	67.998869	71.285633
763.453565	78.327540	71.290638
762.408316	72.733656	71.295642
761.883467	74.985344	71.300647
761.281152	67.447649	71.305652
760.744648	96.007844	71.310657
760.188193	62.203504	71.315662
758.969377	86.294702	71.320666
758.282517	56.257743	71.325671
758.067752	86.239478	71.330676
757.465825	60.856479	71.335681
756.951197	69.872811	71.340686
755.890153	71.003568	71.345690
755.547590	64.998223	71.350695
755.135659	65.333405	71.355700
753.927202	79.969721	71.360705
753.399201	64.824498	71.365710
752.764386	59.676184	71.370714
752.144435	80.157234	71.375719
751.316949	50.909028	71.380724
750.498746	92.786417	71.385729
750.230423	70.606499	71.390734
749.051025	72.142430	71.395738
748.088934	65.403137	71.400743
748.334528	73.150497	71.405748
747.160401	70.428088	71.410753
747.264149	58.542572	71.415758
746.216631	93.611360	71.420762
745.264261	59.830644	71.425767
744.754189	87.935634	71.430772
744.574845	66.747593	71.435777
743.547216	69.243319	71.440782
742.461131	80.083597	71.445786
742.117375	64.827050	71.450791
741.743913	67.425199	71.455796
740.819825	79.718774	71.460801
740.335864	69.521013	71.465806
739.497053	67.420118	71.470810
738.752543	75.511174	71.475815
737.669446	72.007927	71.480820
736.487592	49.038413	71.485825
736.176119	82.408413	71.490830
736.148142	66.423545	71.495834
736.045903	46.927836	71.500839
735.575647	69.069114	71.505844
734.025714	105.146683	71.510849
733.660470	75.577282	71.515854
733.273930	79.509957	71.520858
732.277819	83.754134	71.525863
731.452887	54.529181	71.530868
730.680643	88.663212	71.535873
730.132102	78.858905	71.540878
729.824166	41.471878	71.545882
728.875567	73.744886	71.550887
728.086622	78.895884	71.555892
727.659621	47.882516	71.560897
727.174682	79.971341	71.565902
726.114444	69.127366	71.570906
725.465794	43.171571	71.575911
725.019487	84.622317	71.580916
724.257280	69.042910	71.585921
724.078852	39.104821	71.590926
722.733453	88.852608	71.595930
721.792447	70.199997	71.600935
722.154689	35.666040	71.605940
720.806376	86.155401	71.610945
720.119164	47.081596	71.615950
719.665896	86.762653	71.620954
719.457624	68.729776	71.625959
718.904815	72.867107	71.630964
717.603908	72.556982	71.635969
717.087505	63.509193	71.640974
716.682804	86.390639	71.645978
715.420571	89.224911	71.650983
714.725451	67.112964	71.655988
714.153579	52.031521	71.660993
713.606697	86.714677	71.665998
713.569300	65.265942	71.671002
712.763474	66.509037	71.676007
711.863055	79.029069	71.681012
711.045592	74.471202	71.686017
710.101317	60.896594	71.691022
709.312552	62.237892	71.696026
708.485991	76.425509	71.701031
708.122472	61.629410	71.706036
707.586086	69.338848	71.711041
707.303579	57.680404	71.716046
707.156188	67.141284	71.721050
706.351938	84.565787	71.726055
705.839423	61.054495	71.731060
704.390704	73.865237	71.736065
703.804558	75.541683	71.741070
703.814861	69.445474	71.746074
702.383468	67.145647	71.751079
701.553246	80.772494	71.756084
700.826753	58.178316	71.761089
700.669755	59.993000	71.766094
700.132963	57.255868	71.771098
698.656525	75.137447	71.776103
698.405743	56.162095	71.781108
697.912092	57.178882	71.786113
697.544249	67.490094	71.791118
696.474801	58.615520	71.796122
695.268566	84.248461	71.801127
695.004833	55.290545	71.806132
694.117525	75.270145	71.811137
694.354928	68.130168	71.816142
693.715269	62.105913	71.821146
692.651191	89.565876	71.826151
692.613205	59.149687	71.831156
691.066290	92.626529	71.836161
689.963994	58.328869	71.841166
689.643243	89.866475	71.846170
688.801632	56.702068	71.851175
688.986845	69.394569	71.856180
688.542408	44.019673	71.861185
687.551116	77.245597	71.866190
687.162653	39.869842	71.871194
686.047490	90.516046	71.876199
684.859296	66.743356	71.881204
684.355310	47.710570	71.886209
683.817293	69.137284	71.891214
683.464434	45.698371	71.896218
682.738140	79.711528	71.901223
682.199097	55.814996	71.906228
681.279933	67.431322	71.911233
680.775346	75.241352	71.916238
680.475948	57.182012	71.921242
679.174820	68.873349	71.926247
678.808844	66.561579	71.931252
677.812288	56.048100	71.936257
677.787585	64.740439	71.941262
676.596381	71.551271	71.946266
675.883780	75.001317	71.951271
675.393887	44.537281	71.956276
675.110574	77.388718	71.961281
673.929101	58.386533	71.966286
673.259397	80.761420	71.971290
672.705672	54.494071	71.976295
672.292989	69.922994	71.981300
671.266254	64.496509	71.986305
670.602074	57.545827	71.991310
670.151229	75.286186	71.996314
669.444546	63.652714	72.001319
669.186090	79.832900	72.006324
668.104889	70.603837	72.011329
667.523968	67.069544	72.016334
667.289208	68.325793	72.021338
665.844970	62.636230	72.026343
665.367135	54.673500	72.031348
664.432419	71.519565	72.036353
664.303278	68.201898	72.041358
664.141447	60.132081	72.046362
662.881274	63.057502	72.051367
662.446949	82.947641	72.056372
661.854457	63.673487	72.061377
660.597916	61.128239	72.066382
659.762726	66.631945	72.071386
658.957327	66.481052	72.076391
658.737799	54.550837	72.081396
658.335493	67.890358	72.086401
658.052286	74.723760	72.091406
657.096529	66.778785	72.096410
656.081639	67.019198	72.101415
655.951654	71.161746	72.106420
655.138733	72.574712	72.111425
654.251853	54.055458	72.116430
653.415269	77.767275	72.121434
653.084542	59.162609	72.126439
652.706136	54.818688	72.131444
651.573791	77.639377	72.136449
651.155304	73.585667	72.141454
650.651435	60.740424	72.146458
649.250441	58.880462	72.151463
648.542355	60.642564	72.156468
647.915409	57.892994	72.161473
647.394009	72.861448	72.166478
647.411114	66.324219	72.171482
646.391574	62.618520	72.176487
645.645678	60.015618	72.181492
644.795013	66.901535	72.186497
644.539472	71.332141	72.191502
644.177960	59.932280	72.196506
643.065151	64.362211	72.201511
642.466091	62.571657	72.206516
641.883914	66.043515	72.211521
641.215885	65.146980	72.216526
640.185619	74.065678	72.221530
639.593103	69.781080	72.226535
639.485610	65.770885	72.231540
638.436567	57.519102	72.236545
637.493600	62.478617	72.241550
637.080680	56.224323	72.246554
636.232531	70.481613	72.251559
635.936762	64.347423	72.256564
635.018556	71.286675	72.261569
634.326226	65.324438	72.266574
634.012947	56.126069	72.271578
633.209815	70.041898	72.276583
632.554924	56.705084	72.281588
631.547019	55.277666	72.286593
630.887248	75.247846	72.291598
631.214012	64.520497	72.296602
629.838028	71.942631	72.301607
629.444651	62.015894	72.306612
628.630141	67.311324	72.311617
627.829872	59.671168	72.316622
626.957584	69.889263	72.321626
626.292459	74.571165	72.326631
626.027170	50.657881	72.331636
625.284423	89.088850	72.336641
624.707007	53.392574	72.341646
623.742109	73.225275	72.346650
622.902039	80.300315	72.351655
622.924210	59.915961	72.356660
621.949604	59.944982	72.361665
620.597745	51.922773	72.366670
620.160937	70.843527	72.371674
619.240386	56.831559	72.376679
619.422450	61.809022	72.381684
618.783778	65.933236	72.386689
618.601786	60.129416	72.391694
617.706394	61.046204	72.396698
617.033545	62.701785	72.401703
616.225878	60.209648	72.406708
615.204204	67.496519	72.411713
614.599106	68.877978	72.416718
614.149302	55.721387	72.421722
613.083827	70.202512	72.426727
612.430376	77.031806	72.431732
611.670527	72.425380	72.436737
611.487839	60.292197	72.441742
611.074489	58.511498	72.446746
609.959155	79.512959	72.451751
609.707062	46.756187	72.456756
608.731507	70.564239	72.461761
608.118037	56.310997	72.466766
607.320197	76.006720	72.471770
606.634300	65.448527	72.476775
606.416310	57.487006	72.481780
605.610247	55.128650	72.486785
604.344958	69.102316	72.491790
604.202397	62.776588	72.496794
603.471938	70.434951	72.501799
603.031898	59.804495	72.506804
601.811015	66.957528	72.511809
601.205297	59.505581	72.516814
600.695864	59.077353	72.521818
600.308332	68.786195	72.526823
599.402102	65.346304	72.531828
598.461747	53.196610	72.536833
597.593011	79.281980	72.541838
597.723455	50.215610	72.546842
597.304036	70.026088	72.551847
596.447688	66.255000	72.556852
595.749192	58.839907	72.561857
595.135670	65.719606	72.566862
593.948864	54.641999	72.571866
593.107841	56.043689	72.576871
593.067032	53.397893	72.581876
592.400281	64.497830	72.586881
591.094906	54.315836	72.591886
590.397572	63.678226	72.596890
589.884442	61.516056	72.601895
589.467243	43.473946	72.606900
589.300120	63.291539	72.611905
588.807984	66.317011	72.616910
587.783516	60.891783	72.621914
586.754817	61.886579	72.626919
586.529933	57.023091	72.631924
585.280455	53.477038	72.636929
584.402916	75.765179	72.641934
584.605612	59.273708	72.646938
583.940301	73.186521	72.651943
582.892802	38.598013	72.656948
581.803544	63.594186	72.661953
581.183149	69.886819	72.666958
581.086222	51.172416	72.671962
580.568631	54.591422	72.676967
579.848674	67.491136	72.681972
578.811460	48.191682	72.686977
578.072170	86.697776	72.691982
578.067684	37.655317	72.696986
577.333403	62.415192	72.701991
576.328442	57.155586	72.706996
576.022284	60.801100	72.712001
574.908115	58.282105	72.717006
574.264747	80.936631	72.722010
573.728991	49.040281	72.727015
573.306601	82.093614	72.732020
572.437241	45.256521	72.737025
571.255910	66.873993	72.742030
571.224772	63.146514	72.747034
570.212264	54.598809	72.752039
570.125706	60.871066	72.757044
569.079410	61.611646	72.762049
568.136507	62.277416	72.767054
567.822999	47.500215	72.772058
567.134840	71.499027	72.777063
566.802171	56.169819	72.782068
565.907563	50.257175	72.787073
565.265948	75.251455	72.792078
564.605160	46.702182	72.797082
563.022005	76.882875	72.802087
562.655875	50.629863	72.807092
562.181571	56.370981	72.812097
561.605817	71.594082	72.817102
561.354381	56.482157	72.822106
561.240762	54.453468	72.827111
559.859608	59.698827	72.832116
559.481888	32.528393	72.837121
558.568251	65.383980	72.842126
557.843221	76.285069	72.847130
556.738924	81.226160	72.852135
556.480832	49.093218	72.857140
556.165635	60.338999	72.862145
554.888689	51.998991	72.867150
554.282134	48.602848	72.872154
553.811475	67.357111	72.877159
553.532002	62.697849	72.882164
552.825598	57.745491	72.887169
551.400772	50.400379	72.892174
551.111493	74.166939	72.897178
550.761835	41.496704	72.902183
550.364691	62.287574	72.907188
549.200449	63.234593	72.912193
548.203075	59.126467	72.917198
548.139736	54.891645	72.922202
547.365572	55.271943	72.927207
546.623948	67.985891	72.932212
545.942491	68.431842	72.937217
545.299403	55.123146	72.942222
545.069889	67.241472	72.947226
543.664010	48.570005	72.952231
543.400597	83.706256	72.957236
542.862710	49.069698	72.962241
542.048806	85.055252	72.967246
541.288686	44.488881	72.972250
540.315326	81.737650	72.977255
540.171243	61.800811	72.982260
539.532686	61.390009	72.987265
538.562724	65.160183	72.992270
537.713404	50.078853	72.997274
536.903389	80.218408	73.002279
536.968611	47.595616	73.007284
536.378081	71.810674	73.012289
535.556490	92.385360	73.017294
534.667620	57.143993	73.022298
534.348126	66.348446	73.027303
533.222982	67.426431	73.032308
532.763670	35.820712	73.037313
531.887084	79.363017	73.042318
531.571609	49.210289	73.047322
530.780629	71.516178	73.052327
529.870960	57.978731	73.057332
529.367824	75.535042	73.062337
528.627909	64.857760	73.067342
528.937186	40.816740	73.072346
527.744273	95.346481	73.077351
526.922645	55.666616	73.082356
526.298950	68.573080	73.087361
524.834227	82.670012	73.092366
524.481194	57.689012	73.097370
523.470591	75.138513	73.102375
523.542249	56.173351	73.107380
523.229442	77.469588	73.112385
522.586014	54.983698	73.117390
521.945239	86.405090	73.122394
520.456542	64.186285	73.127399
520.720250	35.218579	73.132404
519.131148	87.510783	73.137409
518.211893	62.738235	73.142414
517.851374	36.804474	73.147418
517.158921	89.871581	73.152423
516.874483	59.579862	73.157428
516.884407	58.972735	73.162433
516.058165	67.056352	73.167438
515.194906	44.969751	73.172442
514.558401	79.832701	73.177447
513.838043	38.416419	73.182452
513.213669	84.484087	73.187457
512.481919	43.086953	73.192462
511.619170	76.949949	73.197466
510.549105	41.691772	73.202471
510.431154	47.525929	73.207476
509.545995	72.232590	73.212481
508.927519	47.779567	73.217486
508.315732	68.647209	73.222490
507.482725	43.931920	73.227495
507.119044	80.750852	73.232500
506.202098	60.000491	73.237505
505.662279	39.617411	73.242510
504.775857	67.517377	73.247514
504.276673	42.260093	73.252519
503.968203	74.300257	73.257524
502.950561	58.287027	73.262529
502.050347	49.196381	73.267534
501.582581	71.230026	73.272538
500.938918	56.655230	73.277543
500.913308	42.114448	73.282548
499.686103	83.664293	73.287553
498.809092	46.842663	73.292558
498.579441	67.911186	73.297562
498.045462	53.514451	73.302567
496.562013	74.271815	73.307572
496.615067	29.261725	73.312577
495.490378	84.346639	73.317582
495.447790	49.941845	73.322586
494.320751	60.549029	73.327591
493.602422	55.658512	73.332596
493.053365	66.602530	73.337601
492.395902	55.749720	73.342606
492.375183	62.140788	73.347610
491.231326	48.982852	73.352615
490.730481	70.676436	73.357620
490.319830	64.141133	73.362625
489.060265	56.296678	73.367630
488.428402	53.505363	73.372634
487.869062	71.436451	73.377639
486.733121	72.218153	73.382644
486.394046	53.353124	73.387649
485.300184	79.105381	73.392654
485.027141	58.763357	73.397658
484.878384	69.416542	73.402663
484.314553	57.213229	73.407668
483.199286	52.587787	73.412673
482.311544	76.549021	73.417678
482.326632	65.650563	73.422682
481.144379	52.894535	73.427687
480.453478	74.315647	73.432692
479.741913	70.378045	73.437697
479.462268	51.432595	73.442702
478.970587	74.089753	73.447706
477.822836	47.295873	73.452711
476.796926	79.842972	73.457716
476.765167	51.220338	73.462721
476.102458	57.062440	73.467726
475.340504	64.213370	73.472730
474.045098	57.913635	73.477735
473.946268	55.767486	73.482740
473.548527	76.564772	73.487745
472.752679	61.173768	73.492750
471.759956	65.669787	73.497754
471.260534	56.980470	73.502759
470.926066	80.475126	73.507764
470.379048	53.975018	73.512769
468.867903	66.649155	73.517774
468.490293	66.821231	73.522778
467.969543	64.595652	73.527783
467.553517	49.063734	73.532788
466.775644	68.089273	73.537793
465.854745	61.146445	73.542798
465.510879	54.551630	73.547802
465.135811	54.582963	73.552807
463.846114	70.580507	73.557812
463.114599	53.890983	73.562817
462.698778	56.549525	73.567822
462.389785	63.650370	73.572826
460.931522	50.536233	73.577831
460.440609	68.435918	73.582836
460.038031	65.824108	73.587841
459.196926	57.537713	73.592846
458.984434	66.255221	73.597850
458.151224	57.103457	73.602855
457.355791	53.545057	73.607860
457.265918	64.945741	73.612865
456.157509	57.663810	73.617870
455.307831	55.014431	73.622874
454.535345	61.056943	73.627879
454.179884	62.220482	73.632884
453.306163	62.761740	73.637889
453.072687	72.491776	73.642894
452.231155	47.675377	73.647898
451.131177	63.404589	73.652903
450.836682	52.273212	73.657908
450.261254	73.874609	73.662913
449.546962	47.216683	73.667918
448.805425	80.319256	73.672922
448.017930	64.818127	73.677927
447.878746	63.488907	73.682932
446.993909	50.141506	73.687937
446.433913	38.532081	73.692942
446.028614	75.827514	73.697946
444.841484	70.951778	73.702951
444.146591	43.273705	73.707956
443.274224	84.972012	73.712961
442.769640	52.242918	73.717966
442.558329	66.599036	73.722970
442.070496	57.761234	73.727975
440.720665	66.675714	73.732980
440.677558	56.499274	73.737985
439.595601	53.688226	73.742990
438.746127	69.364922	73.747994
438.369171	63.748296	73.752999
437.954520	53.667322	73.758004
436.894305	52.432810	73.763009
435.879486	78.494157	73.768014
435.545053	54.032174	73.773018
435.158974	56.094665	73.778023
434.683111	58.720203	73.783028
433.660112	72.568603	73.788033
432.589066	65.627634	73.793038
432.314656	63.539421	73.798042
431.714340	68.778702	73.803047
430.908192	47.209714	73.808052
430.304723	79.404099	73.813057
429.124288	58.440320	73.818062
429.135223	64.913068	73.823066
428.331296	65.865809	73.828071
428.312050	45.406120	73.833076
427.353043	75.671898	73.838081
426.373536	50.801805	73.843086
426.226872	69.460294	73.848090
424.924506	46.108118	73.853095
424.365317	66.667777	73.858100
423.530428	64.085434	73.863105
422.951864	69.677618	73.868110
421.993160	78.605484	73.873114
421.583586	49.827041	73.878119
421.025532	67.456744	73.883124
420.615609	67.534635	73.888129
420.014257	65.804424	73.893134
419.527381	64.262540	73.898138
418.610549	49.192029	73.903143
417.784870	68.420720	73.908148
416.981152	35.912793	73.913153
415.871282	70.761251	73.918158
415.531084	32.947502	73.923162
415.197938	69.417763	73.928167
414.388658	62.600665	73.933172
414.810846	27.183680	73.938177
413.025066	87.501816	73.943182
412.693930	61.829862	73.948186
412.179031	41.218938	73.953191
410.836500	77.701826	73.958196
410.362785	50.113090	73.963201
409.889180	38.370073	73.968206
409.487715	78.634088	73.973210
408.551378	48.892559	73.978215
407.784825	77.137699	73.983220
407.193911	47.366365	73.988225
406.469293	73.651107	73.993230
406.290966	51.660416	73.998234
405.264268	62.820884	74.003239
404.488828	65.158294	74.008244
404.162530	51.889063	74.013249
403.145636	66.690483	74.018254
402.732638	80.131064	74.023258
401.940303	53.911337	74.028263
401.286928	65.871705	74.033268
401.003096	68.307391	74.038273
400.031172	40.864289	74.043278
399.510996	66.495166	74.048282
399.000204	53.285292	74.053287
397.935813	52.691662	74.058292
397.304254	67.333921	74.063297
396.313095	67.846606	74.068302
396.245971	55.917393	74.073306
395.615600	61.383802	74.078311
394.557947	76.478715	74.083316
394.263435	60.643614	74.088321
393.681277	38.628990	74.093326
392.497156	59.453786	74.098330
391.721578	68.267325	74.103335
391.111966	66.937379	74.108340
391.070123	58.567808	74.113345
390.081917	65.756386	74.118350
389.214856	51.918935	74.123354
388.403059	67.622748	74.128359
388.275777	38.506069	74.133364
387.789498	78.097664	74.138369
386.775618	60.202723	74.143374
386.148004	51.712045	74.148378
385.500287	67.526898	74.153383
384.781323	55.873430	74.158388
383.739898	44.047444	74.163393
382.759276	80.455329	74.168398
382.522472	59.707045	74.173402
382.138143	72.893909	74.178407
381.753210	64.836031	74.183412
381.602121	57.029458	74.188417
380.291767	80.919289	74.193422
379.755122	68.829935	74.198426
378.810235	62.217374	74.203431
377.801870	64.386918	74.208436
377.151605	66.888880	74.213441
376.926131	46.225538	74.218446
376.654490	83.203228	74.223450
375.855318	72.507063	74.228455
374.665850	61.046834	74.233460
374.401496	79.602666	74.238465
373.854676	52.191162	74.243470
372.795999	69.098029	74.248474
372.172200	70.928771	74.253479
371.524636	49.684602	74.258484
371.209351	62.940874	74.263489
369.907778	78.604485	74.268494
369.320614	43.414540	74.273498
368.758128	82.855873	74.278503
368.133727	56.085889	74.283508
368.054806	65.747139	74.288513
367.312010	48.494954	74.293518
366.409281	77.848239	74.298522
365.500348	50.138080	74.303527
365.028221	73.329818	74.308532
364.107624	41.151179	74.313537
363.500918	71.307197	74.318542
363.459973	54.206498	74.323546
362.353251	56.636131	74.328551
361.361852	59.138845	74.333556
361.295363	68.433864	74.338561
360.406134	61.391425	74.343566
359.603989	60.271929	74.348570
358.814183	60.159648	74.353575
358.003412	57.355882	74.358580
357.945466	66.017224	74.363585
357.274738	60.283439	74.368590
356.128584	57.301323	74.373594
355.404058	61.702606	74.378599
354.822897	80.291577	74.383604
354.745744	44.206712	74.388609
353.846523	73.294521	74.393614
353.618979	48.446566	74.398618
352.953193	61.105878	74.403623
351.642684	61.037157	74.408628
351.347345	63.834201	74.413633
350.086487	69.795307	74.418638
349.906070	64.633047	74.423642
349.327755	71.560792	74.428647
348.056317	66.503016	74.433652
347.657457	61.236807	74.438657
347.115333	57.652270	74.443662
346.940758	73.183589	74.448666
345.989953	48.815147	74.453671
344.697816	54.245107	74.458676
344.347014	73.409174	74.463681
344.091925	62.016086	74.468686
343.215428	59.241721	74.473690
342.511580	60.727282	74.478695
341.701750	76.339340	74.483700
341.547588	62.183304	74.488705
340.502346	50.504591	74.493710
339.630508	66.552269	74.498714
339.299271	48.707844	74.503719
338.485826	71.058324	74.508724
338.414503	59.386812	74.513729
336.921662	47.815702	74.518734
336.022992	70.094613	74.523738
336.398909	51.509905	74.528743
335.557411	49.934676	74.533748
334.828960	57.991710	74.538753
333.575703	73.594015	74.543758
333.117344	56.400579	74.548762
332.789509	75.269272	74.553767
331.891516	58.413961	74.558772
331.343094	53.393928	74.563777
330.552847	59.127085	74.568782
329.813213	66.941497	74.573786
329.234923	66.579489	74.578791
328.572224	55.054264	74.583796
328.015297	54.327756	74.588801
327.206036	66.749762	74.593806
326.809389	66.839744	74.598810
325.810237	64.263116	74.603815
325.004665	60.039373	74.608820
324.722355	48.108205	74.613825
324.287593	53.045168	74.618830
324.071250	58.070317	74.623834
323.044002	50.102214	74.628839
321.864712	64.549514	74.633844
321.189795	53.135044	74.638849
320.433691	56.450191	74.643854
319.754511	57.657455	74.648858
319.341340	61.900324	74.653863
318.772707	69.124553	74.658868
318.491072	45.116235	74.663873
317.193923	81.924627	74.668878
316.794346	50.815639	74.673882
316.784376	52.028205	74.678887
315.507111	74.730137	74.683892
314.443761	57.577937	74.688897
313.835662	48.341483	74.693902
313.670474	60.786986	74.698906
312.934285	56.140635	74.703911
311.946780	56.991792	74.708916
311.494583	45.343153	74.713921
310.778945	51.412903	74.718926
310.343559	58.595393	74.723930
309.365697	71.935195	74.728935
308.747193	66.194678	74.733940
308.534311	52.478495	74.738945
307.507905	61.874459	74.743950
306.411182	48.630282	74.748954
306.101077	70.261921	74.753959
305.458382	60.594190	74.758964
305.321275	58.807365	74.763969
304.051555	43.175042	74.768974
303.344403	81.970834	74.773978
302.655582	49.935041	74.778983
302.283869	68.954208	74.783988
301.889037	65.179061	74.788993
300.925921	58.730280	74.793998
300.343240	62.751027	74.799002
300.133591	65.073980	74.804007
298.879442	62.836028	74.809012
298.150543	68.184130	74.814017
297.760230	58.808893	74.819022
297.165091	57.121876	74.824026
295.917387	45.160093	74.829031
294.958940	64.922428	74.834036
294.820271	50.754483	74.839041
294.262422	54.099536	74.844046
294.009386	64.351462	74.849050
293.315406	37.747175	74.854055
291.820612	75.429087	74.859060
291.996280	54.960428	74.864065
291.239701	54.325669	74.869070
290.370512	57.002882	74.874074
289.678478	72.999842	74.879079
289.285008	47.533429	74.884084
288.586398	63.659151	74.889089
287.543636	50.091014	74.894094
286.771522	54.578739	74.899098
286.462659	67.012455	74.904103
285.747940	41.136818	74.909108
284.909978	67.907937	74.914113
284.534134	45.281770	74.919118
283.712637	58.189819	74.924122
283.300207	44.254737	74.929127
282.186852	57.747007	74.934132
281.577884	53.745818	74.939137
281.000700	49.566111	74.944142
280.548238	47.093168	74.949146
279.765091	54.827793	74.954151
279.003667	65.329474	74.959156
278.211042	33.311855	74.964161
277.593695	65.405909	74.969166
277.473922	57.080309	74.974170
276.634523	46.740678	74.979175
275.624526	55.019205	74.984180
275.194890	53.662182	74.989185
274.801893	58.300780	74.994190
273.537600	63.185482	74.999194
272.830700	55.093805	75.004199
272.225404	62.814280	75.009204
271.983919	56.856000	75.014209
271.533290	55.343062	75.019214
270.700969	52.788751	75.024218
269.812080	47.386220	75.029223
269.191435	53.783014	75.034228
268.940664	52.063192	75.039233
267.824182	61.864581	75.044238
266.900126	60.573751	75.049242
266.961577	55.670977	75.054247
265.816979	61.356561	75.059252
265.267791	59.143447	75.064257
264.448624	63.779019	75.069262
264.259106	67.666148	75.074266
263.473743	60.452665	75.079271
262.314988	61.804191	75.084276
262.148918	55.997884	75.089281
261.442930	65.068420	75.094286
260.583393	60.796537	75.099290
259.669390	52.961790	75.104295
259.025452	59.053239	75.109300
258.996327	53.624046	75.114305
258.279604	53.154820	75.119310
257.336493	53.778164	75.124314
256.922362	47.468968	75.129319
256.042398	59.432353	75.134324
254.933416	59.265334	75.139329
253.906141	63.222925	75.144334
253.546061	56.209722	75.149338
253.448818	54.369242	75.154343
252.925960	62.767236	75.159348
252.726303	50.062871	75.164353
251.480575	67.724929	75.169358
250.577606	66.634156	75.174362
250.433738	70.258561	75.179367
249.056909	59.063225	75.184372
248.685460	56.996814	75.189377
247.915838	50.671749	75.194382
247.227823	62.139374	75.199386
247.279624	44.787399	75.204391
245.888777	57.341540	75.209396
245.484373	54.796292	75.214401
244.924326	54.407744	75.219406
243.813436	60.961533	75.224410
243.325662	56.843272	75.229415
242.540201	62.266628	75.234420
242.560832	58.934588	75.239425
242.120865	57.407342	75.244430
240.456176	64.366357	75.249434
239.915503	62.940312	75.254439
239.544885	73.181028	75.259444
239.148111	54.186520	75.264449
238.200555	61.750260	75.269454
237.169973	54.930670	75.274458
236.891992	55.176780	75.279463
236.059432	64.384183	75.284468
235.717367	55.974184	75.289473
234.856265	51.868131	75.294478
234.222606	54.865760	75.299482
233.734279	54.098378	75.304487
232.681718	67.104774	75.309492
231.754075	59.324246	75.314497
231.233494	71.780676	75.319502
231.009707	71.094118	75.324506
230.591182	66.649449	75.329511
229.329066	68.875269	75.334516
228.929638	58.867612	75.339521
228.118446	57.908864	75.344526
227.516521	71.896761	75.349530
227.219551	33.313034	75.354535
225.827474	80.021770	75.359540
225.782531	53.074350	75.364545
225.061501	52.027120	75.369550
224.451294	63.827674	75.374554
223.618130	65.460029	75.379559
222.764130	60.551810	75.384564
222.393192	59.052985	75.389569
222.029447	72.477825	75.394574
221.037699	58.654022	75.399578
220.595726	60.274476	75.404583
220.029156	66.240070	75.409588
218.945212	58.104446	75.414593
218.289908	52.205838	75.419598
217.754256	70.360221	75.424602
217.324723	60.526087	75.429607
215.911080	61.372679	75.434612
215.220349	57.532765	75.439617
215.073384	60.987363	75.444622
214.386879	64.277255	75.449626
214.157261	36.812144	75.454631
212.730798	65.741160	75.459636
212.391520	49.511168	75.464641
211.702883	48.674805	75.469646
211.218383	61.909167	75.474650
210.540545	64.390334	75.479655
209.454721	56.762759	75.484660
209.078355	56.168331	75.489665
208.831886	54.250725	75.494670
207.685867	65.308858	75.499674
206.778733	61.147078	75.504679
206.170893	62.112781	75.509684
205.985014	59.381326	75.514689
205.482000	51.517353	75.519694
204.474741	56.466757	75.524698
204.216791	57.204805	75.529703
203.313205	61.227845	75.534708
202.657479	63.464233	75.539713
201.583772	52.329414	75.544718
200.723938	56.476357	75.549722
200.653969	46.565994	75.554727
199.656018	59.598377	75.559732
199.045564	47.361610	75.564737
198.297084	57.389762	75.569742
197.663373	69.335986	75.574746
197.500276	60.381835	75.579751
196.591242	55.517093	75.584756
195.782437	62.306574	75.589761
195.337333	58.963634	75.594766
194.758215	47.224886	75.599770
194.093174	69.785089	75.604775
192.874886	46.700369	75.609780
192.517143	67.134879	75.614785
191.715938	55.070435	75.619790
191.273412	58.906443	75.624794
191.184701	55.273315	75.629799
190.195083	61.933939	75.634804
189.446379	58.855429	75.639809
188.610917	49.552771	75.644814
187.569665	77.926854	75.649818
187.377733	41.381008	75.654823
186.830639	61.077776	75.659828
185.959950	63.379975	75.664833
185.188597	57.775824	75.669838
184.250104	53.421950	75.674842
184.099251	70.195171	75.679847
183.571388	48.481039	75.684852
182.890073	66.280198	75.689857
182.290350	64.947154	75.694862
181.221279	70.396823	75.699866
180.923526	46.693878	75.704871
179.995925	38.175418	75.709876
179.342937	74.543666	75.714881
178.944401	42.521609	75.719886
178.173605	76.701070	75.724890
177.516057	63.448435	75.729895
176.891363	43.443279	75.734900
176.397339	65.151522	75.739905
175.098290	54.057374	75.744910
174.299592	54.336050	75.749914
173.897268	56.349130	75.754919
173.373659	54.065734	75.759924
172.872431	43.688007	75.764929
172.595822	62.956905	75.769934
171.452015	51.470606	75.774938
171.122457	69.847579	75.779943
169.567145	64.849356	75.784948
168.975924	38.435323	75.789953
168.365727	51.839517	75.794958
167.795005	73.036489	75.799962
167.669092	54.506566	75.804967
167.375375	61.609718	75.809972
166.572998	54.014242	75.814977
165.556450	80.861167	75.819982
164.745854	59.925335	75.824986
164.676779	57.295102	75.829991
163.173392	57.315576	75.834996
162.909340	64.962741	75.840001
162.585676	46.171066	75.845006
160.980454	66.558479	75.850010
160.473209	54.306843	75.855015
159.634443	47.833577	75.860020
159.438545	68.984975	75.865025
158.954606	32.493606	75.870030
158.559277	66.993197	75.875034
158.429904	48.804433	75.880039
157.285741	56.481538	75.885044
156.419882	50.531372	75.890049
155.251943	63.534107	75.895054
154.872847	52.561359	75.900058
154.530595	52.133377	75.905063
153.661470	67.135211	75.910068
153.253407	59.503674	75.915073
152.238819	58.954246	75.920078
151.508878	60.956492	75.925082
151.246713	58.405928	75.930087
149.985647	63.876757	75.935092
149.448669	61.101946	75.940097
148.879982	52.302356	75.945102
148.496143	54.689356	75.950106
148.024017	49.520027	75.955111
146.850522	57.534526	75.960116
146.225033	58.622896	75.965121
145.828599	50.611070	75.970126
144.874410	56.947536	75.975130
144.272511	48.113824	75.980135
143.369629	57.837046	75.985140
142.960761	56.388433	75.990145
142.635936	59.095585	75.995150
141.667049	69.302391	76.000154
141.017192	54.507980	76.005159
140.234771	59.930877	76.010164
139.740348	56.639965	76.015169
139.427050	59.097716	76.020174
138.270684	62.164520	76.025178
137.601188	57.490251	76.030183
137.261415	54.602005	76.035188
136.312251	49.732652	76.040193
135.966602	63.126215	76.045198
135.099201	56.037823	76.050202
134.771699	64.059355	76.055207
133.869137	66.021325	76.060212
132.990483	51.428970	76.065217
132.528866	64.828411	76.070222
131.912992	67.424289	76.075226
131.337901	54.926455	76.080231
130.242807	69.710455	76.085236
129.717941	60.995336	76.090241
129.383185	57.909186	76.095246
128.557945	57.045746	76.100250
127.833586	49.560841	76.105255
126.925616	65.932838	76.110260
126.644021	70.779182	76.115265
126.260340	57.050852	76.120270
125.196964	58.245316	76.125274
124.413805	53.869854	76.130279
123.295353	67.269959	76.135284
123.247162	60.063560	76.140289
122.925828	39.123881	76.145294
122.076022	57.112314	76.150298
121.176692	49.395133	76.155303
120.746587	63.029228	76.160308
120.169093	50.560168	76.165313
118.923840	46.037635	76.170318
118.476909	53.231443	76.175322
118.271177	53.738839	76.180327
117.539024	55.692563	76.185332
116.159507	71.572097	76.190337
116.007696	53.046318	76.195342
115.282185	63.384619	76.200346
114.897015	48.278380	76.205351
113.807440	57.364375	76.210356
113.036615	51.604062	76.215361
112.448362	64.090208	76.220366
112.079889	54.413517	76.225370
111.732153	46.490123	76.230375
110.620097	60.191959	76.235380
109.943300	55.736468	76.240385
109.551271	48.589634	76.245390
108.918192	61.447175	76.250394
107.922979	49.260757	76.255399
106.985424	51.693483	76.260404
106.488392	51.316994	76.265409
106.298978	49.243658	76.270414
105.648035	56.019024	76.275418
104.738370	53.075012	76.280423
103.947183	57.363992	76.285428
103.609577	37.811381	76.290433
103.048510	60.766546	76.295438
102.088497	41.997528	76.300442
101.685552	60.026667	76.305447
100.689742	59.884245	76.310452
99.820260	53.847953	76.315457
99.443019	55.054433	76.320462
98.426111	56.192616	76.325466
98.255038	57.058737	76.330471
97.289134	60.782689	76.335476
96.582862	53.181377	76.340481
96.375933	62.926090	76.345486
95.728033	54.109188	76.350490
95.489029	54.716502	76.355495
94.078052	57.190035	76.360500
93.388569	49.973952	76.365505
93.059158	56.128809	76.370510
91.924167	60.594034	76.375514
91.462320	53.672787	76.380519
91.086304	62.886262	76.385524
90.505297	62.083230	76.390529
89.739070	56.935581	76.395534
88.787531	59.871979	76.400538
88.527255	65.705179	76.405543
87.482571	53.780529	76.410548
86.384804	51.052588	76.415553
86.190938	54.539896	76.420558
85.164591	66.450980	76.425562
85.364687	63.859822	76.430567
84.394164	48.930510	76.435572
83.612037	58.101519	76.440577
83.010652	59.972904	76.445582
82.391778	60.096787	76.450586
81.827647	46.066121	76.455591
80.824994	60.204648	76.460596
80.253498	57.343904	76.465601
80.005630	51.771425	76.470606
78.657133	58.091951	76.475610
77.975900	54.468172	76.480615
77.316107	58.897043	76.485620
76.926774	50.272289	76.490625
77.067706	43.956617	76.495630
75.511808	51.363543	76.500634
74.948967	50.161832	76.505639
74.684463	51.388181	76.510644
73.755615	52.042433	76.515649
72.620037	51.509181	76.520654
71.923260	55.516627	76.525658
71.754695	55.090918	76.530663
71.073807	52.227123	76.535668
70.875063	45.943544	76.540673
70.136415	42.171243	76.545678
68.828008	52.996710	76.550682
68.549285	46.309600	76.555687
67.483243	54.705933	76.560692
66.678936	54.649671	76.565697
66.085906	48.892561	76.570702
65.655018	48.013560	76.575706
65.543441	63.191041	76.580711
64.804813	37.327238	76.585716
63.822850	70.666785	76.590721
63.413614	41.905825	76.595726
62.426086	45.622196	76.600730
61.289437	67.737252	76.605735
60.795942	41.386528	76.610740
60.440273	54.289707	76.615745
60.214114	51.498466	76.620750
59.574468	46.414218	76.625754
58.519188	34.931227	76.630759
57.677127	59.001872	76.635764
57.336285	54.363520	76.640769
56.684339	51.972896	76.645774
55.495680	54.721633	76.650778
55.192817	50.266446	76.655783
54.684499	47.638468	76.660788
54.009461	55.694925	76.665793
52.877756	61.832668	76.670798
52.185362	65.498826	76.675802
51.772095	52.726076	76.680807
51.408345	58.260408	76.685812
50.909921	61.540843	76.690817
50.271721	56.790653	76.695822
49.297591	71.055528	76.700826
48.931852	57.510428	76.705831
47.919925	54.150694	76.710836
47.063136	49.063236	76.715841
46.611761	54.761342	76.720846
46.062447	63.952000	76.725850
45.302456	47.295610	76.730855
44.625435	71.936001	76.735860
44.024121	55.550741	76.740865
43.661467	49.632326	76.745870
42.481411	61.627852	76.750874
41.651437	61.399087	76.755879
41.457772	62.224663	76.760884
40.851546	52.076591	76.765889
40.445837	64.746504	76.770894
39.141655	63.476966	76.775898
38.947381	57.864407	76.780903
38.041214	45.411535	76.785908
36.517018	73.017463	76.790913
36.542211	61.500904	76.795918
35.888271	52.465807	76.800922
35.644541	54.259662	76.805927
35.420183	54.943487	76.810932
34.004243	74.509204	76.815937
33.830994	56.698017	76.820942
33.114873	66.996993	76.825946
31.749809	43.894812	76.830951
31.169227	46.530809	76.835956
30.670406	56.667397	76.840961
30.495308	60.080757	76.845966
28.947693	60.683914	76.850970
28.494230	53.677773	76.855975
28.277026	58.274169	76.860980
27.385114	55.030912	76.865985
27.210858	52.264510	76.870990
26.295371	67.562323	76.875994
25.562116	52.317675	76.880999
25.228469	55.322691	76.886004
23.598583	60.352542	76.891009
22.982530	51.715079	76.896014
22.269063	49.488808	76.901018
22.172670	52.760313	76.906023
22.023752	64.406900	76.911028
20.938357	76.915590	76.916033
20.028388	38.492807	76.921038
19.419129	56.419236	76.926042
18.982239	46.450734	76.931047
18.726711	58.801821	76.936052
17.361492	64.402854	76.941057
16.778912	61.567546	76.946062
16.303846	56.665201	76.951066
15.708325	48.890151	76.956071
14.545502	44.975804	76.961076
13.603861	63.204395	76.966081
13.604846	71.175121	76.971086
13.026286	47.542257	76.976090
12.607897	61.138216	76.981095
11.667681	57.585725	76.986100
11.180046	54.568131	76.991105
10.773058	43.530499	76.996110
9.370987	57.215545	77.001114
8.638159	53.745087	77.006119
8.024329	59.035481	77.011124
7.786748	55.273158	77.016129
7.518537	47.589398	77.021134
5.995909	74.580123	77.026139
6.020399	51.846055	77.031143
5.199680	61.269225	77.036148
4.325803	64.082888	77.041153
3.477840	44.829310	77.046158