Mon Mar 08 20:13:02 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
0.257936	99.129110	0.000000
0.029869	94.483806	0.005005
-0.995641	42.110176	0.010010
-3.687585	19.932394	0.015014
-8.328920	29.599096	0.020019
-13.463870	17.700898	0.025024
-18.554485	21.180818	0.030029
-22.533712	14.158370	0.035034
-26.672075	16.437826	0.040038
-30.252777	23.374611	0.045043
-34.078467	22.379581	0.050048
-37.769105	21.903869	0.055053
-41.095957	12.886770	0.060058
-45.224868	6.645120	0.065062
-48.601069	12.551171	0.070067
-52.364113	14.406554	0.075072
-56.373350	33.553360	0.080077
-59.933192	19.932823	0.085082
-64.124308	22.946101	0.090086
-67.670328	24.292262	0.095091
-71.435403	19.014402	0.100096
-75.421288	25.750979	0.105101
-79.050562	19.961072	0.110106
-82.952556	21.412923	0.115110
-86.286692	26.407216	0.120115
-90.217054	23.319169	0.125120
-94.137614	16.601273	0.130125
-97.462602	14.302845	0.135130
-101.440252	29.396942	0.140134
-104.996329	18.076481	0.145139
-108.835375	13.652513	0.150144
-112.957311	13.591051	0.155149
-116.339730	18.079037	0.160154
-120.767942	38.399721	0.165158
-123.713347	16.418652	0.170163
-127.647836	9.031308	0.175168
-131.655984	17.763060	0.180173
-135.367555	23.755851	0.185178
-139.137954	8.663172	0.190182
-142.891710	23.707411	0.195187
-146.601862	29.261635	0.200192
-150.220420	21.283061	0.205197
-153.970604	20.362900	0.210202
-158.096206	15.759247	0.215206
-161.278429	9.313139	0.220211
-165.612868	18.615784	0.225216
-169.584408	16.565689	0.230221
-173.325431	13.647828	0.235226
-177.154475	15.520241	0.240230
-180.877852	20.524731	0.245235
-184.472871	10.207175	0.250240
-188.202358	14.979278	0.255245
-191.863237	26.298484	0.260250
-195.861032	32.147820	0.265254
-199.193127	15.140403	0.270259
-203.040659	20.439107	0.275264
-206.898326	11.847554	0.280269
-210.248884	15.890646	0.285274
-214.240794	19.810603	0.290278
-218.147164	7.073472	0.295283
-222.477393	25.128529	0.300288
-226.170873	21.121457	0.305293
-229.395389	8.980373	0.310298
-233.176035	13.563604	0.315302
-236.940686	25.941718	0.320307
-240.881699	22.615943	0.325312
-244.909651	16.401105	0.330317
-248.455496	20.051249	0.335322
-252.154743	18.553876	0.340326
-255.560196	-0.283463	0.345331
-259.275599	23.006359	0.350336
-263.222196	26.723638	0.355341
-267.067740	4.933765	0.360346
-271.306093	36.954418	0.365350
-274.185751	16.122048	0.370355
-278.125076	3.383978	0.375360
-282.182043	36.766459	0.380365
-285.824570	13.269608	0.385370
-289.739186	12.632929	0.390374
-293.424001	27.808291	0.395379
-297.042828	15.433795	0.400384
-301.156239	15.191535	0.405389
-304.451682	-0.558508	0.410394
-308.563822	35.601720	0.415398
-312.235783	11.292820	0.420403
-315.922592	4.739829	0.425408
-320.084511	34.816732	0.430413
-323.465149	5.596837	0.435418
-327.236402	28.280707	0.440422
-330.758661	21.657314	0.445427
-334.759978	12.399834	0.450432
-338.513929	43.654197	0.455437
-341.951913	0.423898	0.460442
-346.074889	33.987290	0.465446
-349.922268	26.078673	0.470451
-353.443646	8.042095	0.475456
-357.266062	6.722233	0.480461
-361.060324	31.480199	0.485466
-364.973879	6.984483	0.490470
-368.837607	10.013817	0.495475
-372.719077	30.305953	0.500480
-376.334517	30.868923	0.505485
-379.683621	22.223273	0.510490
-383.458847	35.047957	0.515494
-387.484413	19.723643	0.520499
-390.800871	11.017615	0.525504
-395.377797	22.369821	0.530509
-398.762422	16.889837	0.535514
-402.821378	13.718773	0.540518
-405.852195	6.085136	0.545523
-410.201870	27.623657	0.550528
-413.939872	20.894500	0.555533
-417.474634	8.667623	0.560538
-421.411519	18.462269	0.565542
-425.467384	28.826239	0.570547
-428.670498	27.308266	0.575552
-432.474339	1.232534	0.580557
-435.985403	30.962838	0.585562
-440.144586	7.685952	0.590566
-443.914387	22.318464	0.595571
-448.140914	24.388802	0.600576
-451.798204	-1.407538	0.605581
-454.946716	23.003016	0.610586
-458.961502	6.983324	0.615590
-462.711986	26.215537	0.620595
-466.117947	-9.081858	0.625600
-470.277144	36.430356	0.630605
-474.033865	15.457654	0.635610
-477.940562	23.727510	0.640614
-481.715651	24.809680	0.645619
-484.828368	3.431422	0.650624
-489.134920	10.155205	0.655629
-492.727295	10.090244	0.660634
-496.664226	16.111670	0.665638
-500.381954	13.061310	0.670643
-503.988032	28.121893	0.675648
-507.681281	10.318006	0.680653
-511.278103	34.901151	0.685658
-515.273704	2.277676	0.690662
-519.166065	22.524441	0.695667
-522.895532	-9.436654	0.700672
-526.864270	16.836314	0.705677
-530.161227	13.397127	0.710682
-534.228947	29.810287	0.715686
-537.946265	-3.994465	0.720691
-541.879300	23.904845	0.725696
-545.326683	20.349366	0.730701
-549.136155	8.078276	0.735706
-553.181467	12.235950	0.740710
-556.774686	-8.272289	0.745715
-560.467928	33.685558	0.750720
-564.451789	17.399358	0.755725
-567.582451	-21.395038	0.760730
-571.905374	19.241066	0.765734
-575.321447	11.033732	0.770739
-579.254273	14.684667	0.775744
-583.296542	9.565452	0.780749
-586.569913	-11.512597	0.785754
-590.788374	39.249018	0.790758
-594.633750	8.889669	0.795763
-598.088663	29.903971	0.800768
-602.446444	-2.180529	0.805773
-605.703566	20.080975	0.810778
-609.671432	13.478742	0.815782
-612.523956	-14.924604	0.820787
-616.814082	19.857899	0.825792
-620.854380	39.218635	0.830797
-624.286673	5.038940	0.835802
-628.036245	17.995470	0.840806
-632.023974	20.551486	0.845811
-635.553342	-22.463323	0.850816
-639.583129	16.077747	0.855821
-643.488663	16.808880	0.860826
-647.016397	12.116888	0.865830
-650.872661	37.487496	0.870835
-654.058639	5.127582	0.875840
-658.395890	15.700856	0.880845
-662.178832	16.000883	0.885850
-666.049400	16.103622	0.890854
-669.817332	6.219724	0.895859
-673.164566	-9.482039	0.900864
-677.157553	16.621559	0.905869
-680.390384	1.297300	0.910874
-684.718732	4.626853	0.915878
-688.519641	15.018297	0.920883
-691.954387	9.322851	0.925888
-696.017826	11.179922	0.930893
-699.737451	12.488519	0.935898
-703.493938	9.980797	0.940902
-707.287769	3.172751	0.945907
-710.784347	21.115882	0.950912
-714.596428	1.998941	0.955917
-718.178209	1.610958	0.960922
-722.354542	8.531938	0.965926
-726.163358	13.076273	0.970931
-729.851646	18.296735	0.975936
-733.873807	18.045371	0.980941
-737.473226	3.703794	0.985946
-741.234950	24.253247	0.990950
-744.789050	-2.287538	0.995955
-748.270094	1.006068	1.000960
-752.449853	26.825848	1.005965
-755.980757	1.014594	1.010970
-760.000287	12.682037	1.015974
-763.810434	16.075566	1.020979
-766.993663	4.622489	1.025984
-771.277056	21.201344	1.030989
-774.828959	8.481088	1.035994
-778.388212	10.710270	1.040998
-782.571307	16.238527	1.046003
-786.093649	5.580779	1.051008
-790.163619	10.925402	1.056013
-793.437207	3.167104	1.061018
-797.488032	12.805512	1.066022
-801.494921	14.634802	1.071027
-805.220626	12.765667	1.076032
-809.351591	16.295691	1.081037
-812.857236	2.213622	1.086042
-816.399542	26.745845	1.091046
-820.044541	21.595082	1.096051
-823.403828	2.130026	1.101056
-827.499586	12.991391	1.106061
-830.921216	2.899466	1.111066
-834.964662	19.033251	1.116070
-839.155935	22.713304	1.121075
-842.234723	-0.175679	1.126080
-846.888835	12.367552	1.131085
-850.595679	7.125813	1.136090
-853.938940	-2.453517	1.141094
-857.299416	16.623847	1.146099
-860.982019	8.044855	1.151104
-865.247820	8.884400	1.156109
-868.879151	-1.421501	1.161114
-872.938101	13.216838	1.166118
-877.018340	17.629773	1.171123
-880.027530	2.878721	1.176128
-883.990440	12.764966	1.181133
-887.720966	12.139266	1.186138
-891.438175	0.040097	1.191142
-895.240674	14.919726	1.196147
-899.203383	14.253898	1.201152
-902.964382	17.813240	1.206157
-906.479241	-0.297547	1.211162
-910.189514	19.382962	1.216166
-913.917464	18.469911	1.221171
-917.688683	7.705519	1.226176
-921.689696	14.952017	1.231181
-925.353916	2.100175	1.236186
-929.216557	12.145486	1.241190
-933.028916	19.316115	1.246195
-936.277929	0.672483	1.251200
-940.460609	17.158243	1.256205
-944.302589	11.225541	1.261210
-948.044657	8.864132	1.266214
-951.807478	17.397122	1.271219
-955.500750	7.246329	1.276224
-959.294257	21.180106	1.281229
-962.830722	12.612605	1.286234
-966.575187	4.970850	1.291238
-970.673334	-1.527916	1.296243
-974.051569	22.360148	1.301248
-978.148084	13.759229	1.306253
-982.311730	15.699038	1.311258
-985.681453	14.979535	1.316262
-989.183600	0.619679	1.321267
-992.586168	26.799621	1.326272
-996.512802	15.110967	1.331277
-1000.641880	10.670212	1.336282
-1004.343921	25.734201	1.341286
-1008.416875	10.954756	1.346291
-1011.942451	-2.264428	1.351296
-1015.716644	25.182806	1.356301
-1019.475274	8.516127	1.361306
-1023.021634	-0.752947	1.366310
-1027.354824	21.619624	1.371315
-1030.687619	17.936173	1.376320
-1034.526630	11.698824	1.381325
-1038.100591	-2.595851	1.386330
-1041.924044	31.264326	1.391334
-1045.717314	3.737395	1.396339
-1049.598620	3.834598	1.401344
-1053.622236	27.345050	1.406349
-1056.839792	-12.289244	1.411354
-1060.593374	26.154603	1.416358
-1064.356847	-0.605987	1.421363
-1068.226307	16.509489	1.426368
-1072.384345	15.708054	1.431373
-1076.003989	12.620858	1.436378
-1079.961280	1.443427	1.441382
-1083.313245	13.108679	1.446387
-1086.604904	13.879541	1.451392
-1091.124281	13.705165	1.456397
-1094.771268	10.264435	1.461402
-1098.367755	9.590828	1.466406
-1102.212213	12.328118	1.471411
-1105.881646	23.914889	1.476416
-1109.576426	2.258583	1.481421
-1113.157330	27.305081	1.486426
-1117.045168	14.916641	1.491430
-1121.153974	19.875406	1.496435
-1124.739722	0.432884	1.501440
-1128.552752	20.065480	1.506445
-1132.253509	8.487589	1.511450
-1136.235289	20.089675	1.516454
-1139.879037	0.358440	1.521459
-1143.501009	23.235537	1.526464
-1147.289133	-12.253326	1.531469
-1151.001978	18.448258	1.536474
-1154.514066	-1.792823	1.541478
-1158.381570	11.721028	1.546483
-1161.953774	9.886254	1.551488
-1166.372785	7.770679	1.556493
-1169.982222	11.602632	1.561498
-1173.514673	3.566220	1.566502
-1177.619148	-8.595060	1.571507
-1181.379398	29.610329	1.576512
-1185.117252	10.941221	1.581517
-1188.366255	24.138575	1.586522
-1191.866309	10.379478	1.591526
-1196.201574	2.182990	1.596531
-1200.200133	20.410472	1.601536
-1204.039923	12.325514	1.606541
-1207.622457	45.157146	1.611546
-1211.167396	-1.925426	1.616550
-1214.838415	27.867629	1.621555
-1218.417384	-11.117241	1.626560
-1222.572470	36.202280	1.631565
-1226.541828	-9.202399	1.636570
-1230.284638	26.694954	1.641574
-1233.909449	-2.946255	1.646579
-1237.331205	6.437678	1.651584
-1240.989420	8.270262	1.656589
-1245.105393	-11.046193	1.661594
-1249.098688	18.607661	1.666598
-1252.826552	8.570131	1.671603
-1256.203673	17.978491	1.676608
-1260.014431	7.435468	1.681613
-1264.091305	-5.736072	1.686618
-1267.591784	18.432067	1.691622
-1271.279531	1.938994	1.696627
-1274.929623	16.077341	1.701632
-1279.200218	27.336404	1.706637
-1282.945186	-10.103304	1.711642
-1286.425466	31.663573	1.716646
-1290.213555	5.200633	1.721651
-1293.328028	13.176261	1.726656
-1298.038138	24.144603	1.731661
-1301.362032	-14.849377	1.736666
-1305.309649	21.244818	1.741670
-1309.479483	4.154089	1.746675
-1312.065635	-26.950865	1.751680
-1316.549071	-25.413410	1.756685
-1320.532213	26.356815	1.761690
-1323.861456	-2.393326	1.766694
-1328.034814	28.115722	1.771699
-1331.570620	-21.460938	1.776704
-1335.193864	23.938160	1.781709
-1339.138879	7.907386	1.786714
-1342.722394	-21.133116	1.791718
-1347.034407	41.847318	1.796723
-1350.417917	6.516390	1.801728
-1353.834854	-16.896323	1.806733
-1357.797538	31.191997	1.811738
-1361.402345	6.084298	1.816742
-1365.600578	13.038267	1.821747
-1369.537619	14.338570	1.826752
-1373.032190	19.484850	1.831757
-1376.846096	16.749320	1.836762
-1380.336765	-26.208690	1.841766
-1384.181297	0.800853	1.846771
-1387.846849	36.118402	1.851776
-1391.587422	40.760095	1.856781
-1395.744569	42.876200	1.861786
-1399.304315	38.611506	1.866790
-1403.242946	29.380599	1.871795
-1407.013552	3.741338	1.876800
-1410.636708	-10.798685	1.881805
-1414.547787	20.122607	1.886810
-1417.610696	-19.786474	1.891814
-1421.976100	39.397753	1.896819
-1425.515881	13.317895	1.901824
-1429.020051	5.062921	1.906829
-1433.182984	27.572886	1.911834
-1436.794290	7.174721	1.916838
-1440.974509	21.071781	1.921843
-1444.184720	-16.778017	1.926848
-1448.116460	36.133649	1.931853
-1451.811575	-4.692815	1.936858
-1455.411543	31.386938	1.941862
-1460.203584	16.868551	1.946867
-1463.342231	-1.211635	1.951872
-1467.337262	22.299571	1.956877
-1470.837932	5.698057	1.961882
-1474.623384	20.269911	1.966886
-1478.367505	-4.547190	1.971891
-1482.084110	23.768139	1.976896
-1485.780852	6.382833	1.981901
-1489.549745	17.191371	1.986906
-1492.821937	8.457848	1.991910
-1497.152164	-2.271204	1.996915
-1501.416523	5.669621	2.006912
-1501.841843	14.154384	2.016909
-1499.242417	11.077767	2.026906
-1496.965575	10.902589	2.036902
-1494.453522	17.661847	2.046899
-1492.756155	1.443857	2.056896
-1490.531171	10.773625	2.066893
-1488.507204	7.634438	2.076890
-1487.373165	11.603529	2.086886
-1484.893282	5.440519	2.096883
-1482.891509	11.769954	2.106880
-1481.209499	10.554857	2.116877
-1479.576807	3.907024	2.126874
-1477.537638	13.244455	2.136870
-1475.452643	7.878836	2.146867
-1473.680821	-0.460088	2.156864
-1471.638842	9.629997	2.166861
-1469.841378	6.266586	2.176858
-1468.016756	17.692435	2.186854
-1466.214369	8.166076	2.196851
-1464.048863	6.270468	2.206848
-1462.601869	4.260971	2.216845
-1460.391271	10.699087	2.226842
-1458.653877	14.750000	2.236838
-1456.495824	8.550130	2.246835
-1454.839819	8.395451	2.256832
-1452.816568	12.094308	2.266829
-1451.054792	2.456053	2.276826
-1449.173788	11.522015	2.286822
-1447.112367	0.065926	2.296819
-1445.350236	13.104304	2.306816
-1443.509024	6.025244	2.316813
-1441.597429	-1.912909	2.326810
-1439.650663	13.475206	2.336806
-1437.914046	4.562511	2.346803
-1436.090553	9.913240	2.356800
-1433.790070	7.296629	2.366797
-1432.112693	9.258910	2.376794
-1430.599599	14.635656	2.386790
-1428.229581	2.845985	2.396787
-1426.409681	10.211881	2.406784
-1424.371711	4.474915	2.416781
-1422.641062	3.716250	2.426778
-1420.933566	5.252169	2.436774
-1419.339193	16.542830	2.446771
-1416.924392	4.090785	2.456768
-1415.174640	8.584982	2.466765
-1413.763580	4.756143	2.476762
-1411.385591	0.832510	2.486758
-1409.705893	7.036743	2.496755
-1407.664695	2.906521	2.506752
-1405.784158	2.747510	2.516749
-1404.024804	16.032670	2.526746
-1401.840917	7.400475	2.536742
-1400.468769	4.402021	2.546739
-1398.541562	0.569509	2.556736
-1396.251249	3.483616	2.566733
-1394.224340	9.182315	2.576730
-1392.741666	10.290070	2.586726
-1391.152747	2.435182	2.596723
-1388.796167	13.371766	2.606720
-1387.117063	0.271787	2.616717
-1385.169000	1.635024	2.626714
-1383.488791	1.528623	2.636710
-1381.383476	7.917361	2.646707
-1379.272756	-4.771735	2.656704
-1377.495784	7.934351	2.666701
-1375.937651	2.027937	2.676698
-1373.841244	7.518177	2.686694
-1371.730366	8.160680	2.696691
-1370.237471	-0.941886	2.706688
-1368.397070	-3.877915	2.716685
-1366.813615	-2.978892	2.726682
-1364.536138	2.035563	2.736678
-1362.632167	-3.441497	2.746675
-1360.581368	-0.261665	2.756672
-1358.859320	1.207240	2.766669
-1357.014458	12.446802	2.776666
-1355.378380	4.377560	2.786662
-1353.228273	8.094095	2.796659
-1351.195478	1.083904	2.806656
-1349.423020	10.299953	2.816653
-1347.489679	-1.618681	2.826650
-1345.550816	32.877799	2.836646
-1344.144290	7.934451	2.846643
-1342.088634	-7.942928	2.856640
-1340.069716	7.567934	2.866637
-1338.339471	4.349581	2.876634
-1336.562333	5.538127	2.886630
-1334.149335	5.568668	2.896627
-1332.625975	2.085033	2.906624
-1330.895590	8.544881	2.916621
-1328.577383	7.599094	2.926618
-1326.727303	6.755074	2.936614
-1325.118738	10.566204	2.946611
-1323.593120	-2.253400	2.956608
-1321.257301	1.954455	2.966605
-1319.506364	4.282386	2.976602
-1317.732778	6.398288	2.986598
-1315.736081	1.433750	2.996595
-1313.597993	-3.575516	3.006592
-1311.727963	3.411428	3.016589
-1309.911513	6.451985	3.026586
-1308.419797	1.481436	3.036582
-1306.390693	13.346774	3.046579
-1304.475690	14.413816	3.056576
-1302.288235	6.690541	3.066573
-1300.701013	9.253094	3.076570
-1298.943909	12.413677	3.086566
-1296.826854	10.508609	3.096563
-1295.097804	19.753761	3.106560
-1293.389839	9.873182	3.116557
-1291.428327	18.658008	3.126554
-1289.794278	19.845810	3.136550
-1287.245352	12.451510	3.146547
-1285.373621	8.948466	3.156544
-1283.665735	15.211445	3.166541
-1281.888648	20.103980	3.176538
-1280.244103	14.098535	3.186534
-1278.055193	15.772244	3.196531
-1276.319658	7.071389	3.206528
-1274.474839	12.950910	3.216525
-1272.529834	15.557274	3.226522
-1270.916227	9.149449	3.236518
-1268.776313	12.283531	3.246515
-1266.848808	-4.710048	3.256512
-1265.267733	10.289951	3.266509
-1263.053538	21.525766	3.276506
-1261.323599	11.883250	3.286502
-1259.145416	2.322161	3.296499
-1257.478741	9.498001	3.306496
-1255.800346	17.208774	3.316493
-1253.568052	18.319817	3.326490
-1251.743623	9.352138	3.336486
-1250.137129	16.564459	3.346483
-1248.108272	7.131473	3.356480
-1246.624655	8.254961	3.366477
-1244.327446	14.736280	3.376474
-1242.466739	16.743572	3.386470
-1240.529019	18.976948	3.396467
-1238.350970	-8.088592	3.406464
-1237.048255	14.079653	3.416461
-1235.042541	18.122546	3.426458
-1233.151272	23.952046	3.436454
-1231.266048	10.981787	3.446451
-1229.280040	15.803043	3.456448
-1227.477360	26.934232	3.466445
-1225.560124	10.641727	3.476442
-1223.783278	11.077307	3.486438
-1221.711600	14.122886	3.496435
-1219.940642	13.823676	3.506432
-1218.326317	4.927532	3.516429
-1216.398082	19.669947	3.526426
-1214.266987	14.459789	3.536422
-1212.376870	5.468999	3.546419
-1210.579850	13.372389	3.556416
-1208.932280	9.085855	3.566413
-1206.891842	5.044337	3.576410
-1204.907791	17.074872	3.586406
-1203.150513	11.076702	3.596403
-1201.156231	15.004620	3.606400
-1199.173360	13.132159	3.616397
-1197.454553	11.960321	3.626394
-1195.533252	17.000367	3.636390
-1193.807768	8.223810	3.646387
-1191.708288	6.441639	3.656384
-1190.018641	0.893216	3.666381
-1188.380945	15.633194	3.676378
-1186.281505	12.831108	3.686374
-1184.209321	7.534095	3.696371
-1182.375529	34.639714	3.706368
-1180.360230	8.448052	3.716365
-1178.736034	-1.228007	3.726362
-1176.946377	38.060632	3.736358
-1175.035298	15.220134	3.746355
-1172.695909	8.527321	3.756352
-1171.323927	8.413547	3.766349
-1169.586110	9.475893	3.776346
-1167.457324	23.597372	3.786342
-1165.257188	3.974103	3.796339
-1163.942339	7.715507	3.806336
-1161.651444	15.124698	3.816333
-1159.857151	28.276618	3.826330
-1158.154682	2.738139	3.836326
-1156.286525	16.127689	3.846323
-1154.297181	-9.085634	3.856320
-1152.277800	17.698213	3.866317
-1150.696979	18.255202	3.876314
-1148.731161	25.165403	3.886310
-1146.573193	11.453723	3.896307
-1144.780629	4.407921	3.906304
-1143.152998	8.503483	3.916301
-1141.276922	11.457278	3.926298
-1139.300083	9.205334	3.936294
-1137.563968	17.180107	3.946291
-1135.327422	5.326789	3.956288
-1133.311891	15.263563	3.966285
-1132.001013	13.351823	3.976282
-1130.111980	3.019258	3.986278
-1128.206382	17.590129	3.996275
-1125.823926	15.214894	4.006272
-1124.035941	5.811061	4.016269
-1122.457380	5.460602	4.026266
-1120.829284	14.169456	4.036262
-1118.720809	18.903334	4.046259
-1116.660441	6.402471	4.056256
-1114.813466	12.619654	4.066253
-1112.910156	11.516253	4.076250
-1111.463735	12.952073	4.086246
-1108.984848	18.506120	4.096243
-1107.128389	15.401941	4.106240
-1105.547324	10.365115	4.116237
-1104.076236	17.210814	4.126234
-1101.442540	17.555218	4.136230
-1099.867222	7.928067	4.146227
-1098.104024	12.267223	4.156224
-1095.918029	14.697835	4.166221
-1094.263724	12.255955	4.176218
-1092.591321	12.897801	4.186214
-1090.434918	13.994300	4.196211
-1088.516744	-0.534697	4.206208
-1086.730332	7.878878	4.216205
-1085.131033	3.641198	4.226202
-1082.798648	6.458903	4.236198
-1081.201844	10.952571	4.246195
-1079.246638	16.105709	4.256192
-1077.395782	7.533369	4.266189
-1075.126610	-0.924305	4.276186
-1073.792178	16.038330	4.286182
-1071.661608	0.692270	4.296179
-1069.770516	10.565327	4.306176
-1068.226382	-1.192974	4.316173
-1066.335948	4.879938	4.326170
-1064.189742	5.046581	4.336166
-1062.171953	10.873357	4.346163
-1060.346523	4.632299	4.356160
-1058.550614	2.928795	4.366157
-1056.852120	9.873934	4.376154
-1054.854733	5.340516	4.386150
-1053.201880	19.334560	4.396147
-1050.916608	6.655682	4.406144
-1049.019657	9.347286	4.416141
-1047.253177	7.365886	4.426138
-1045.335569	10.546786	4.436134
-1043.743098	4.043018	4.446131
-1041.926124	13.460622	4.456128
-1039.964577	11.157524	4.466125
-1038.090816	0.464336	4.476122
-1036.066519	21.457959	4.486118
-1033.883948	-9.515790	4.496115
-1032.377227	-4.159851	4.506112
-1030.623638	16.185534	4.516109
-1028.441809	7.208218	4.526106
-1026.676559	13.628008	4.536102
-1024.786939	9.694437	4.546099
-1022.695111	5.528020	4.556096
-1021.230554	7.898823	4.566093
-1019.273608	5.741732	4.576090
-1017.443628	6.971020	4.586086
-1015.677030	9.143537	4.596083
-1013.344269	4.823344	4.606080
-1011.537808	11.326548	4.616077
-1009.829020	6.084634	4.626074
-1007.944253	8.669282	4.636070
-1006.064057	-4.952069	4.646067
-1004.359783	2.857385	4.656064
-1002.266379	4.137712	4.666061
-1000.425458	12.340557	4.676058
-998.507326	7.278317	4.686054
-996.712499	3.680430	4.696051
-994.647757	7.109405	4.706048
-993.039901	0.227447	4.716045
-991.321769	5.606450	4.726042
-989.112593	2.584899	4.736038
-987.210944	4.459546	4.746035
-985.420801	-3.995655	4.756032
-983.493141	11.010740	4.766029
-981.500300	-4.381115	4.776026
-979.979300	9.577229	4.786022
-978.068493	1.446922	4.796019
-976.077005	7.754791	4.806016
-973.968418	1.387998	4.816013
-972.302731	7.324838	4.826010
-970.298350	5.217039	4.836006
-968.198764	11.414481	4.846003
-966.839986	5.435986	4.856000
-964.896311	-4.608375	4.865997
-963.076199	6.674974	4.875994
-961.082983	7.066686	4.885990
-959.247621	12.411185	4.895987
-957.135425	4.663925	4.905984
-955.384532	6.299038	4.915981
-953.563974	13.456834	4.925978
-951.415648	9.684045	4.935974
-950.009168	8.576534	4.945971
-947.794029	3.724196	4.955968
-945.925534	11.633752	4.965965
-943.983916	11.297991	4.975962
-942.280996	7.798516	4.985958
-940.350383	14.458761	4.995955
-938.789798	5.811358	5.005952
-936.652598	0.973071	5.015949
-934.947661	5.550602	5.025946
-932.609539	7.586021	5.035942
-930.783398	4.346308	5.045939
-929.091067	7.397547	5.055936
-927.345628	8.127302	5.065933
-925.317351	14.838257	5.075930
-923.316164	10.163820	5.085926
-921.602963	11.039250	5.095923
-919.844430	12.835789	5.105920
-917.915742	9.510221	5.115917
-915.956719	9.091180	5.125914
-914.396882	6.917140	5.135910
-912.314541	2.824960	5.145907
-910.429996	11.631918	5.155904
-908.397142	4.498919	5.165901
-906.788084	3.569032	5.175898
-904.528234	6.587977	5.185894
-902.904232	1.400741	5.195891
-901.010703	10.237847	5.205888
-899.148070	4.892471	5.215885
-897.241146	4.505457	5.225882
-895.085830	5.027615	5.235878
-893.502260	12.455437	5.245875
-891.436316	1.990553	5.255872
-889.700763	-4.704927	5.265869
-888.112388	1.650096	5.275866
-886.195273	11.713359	5.285862
-883.600988	1.808186	5.295859
-882.124205	0.327923	5.305856
-880.366385	-5.725366	5.315853
-878.547607	4.560447	5.325850
-876.509078	7.922673	5.335846
-874.593162	6.640618	5.345843
-873.081730	5.325335	5.355840
-871.069689	0.115560	5.365837
-868.924168	0.284070	5.375834
-867.130383	2.289735	5.385830
-865.412396	1.959789	5.395827
-863.489066	3.131648	5.405824
-862.048074	11.059093	5.415821
-859.948194	13.453174	5.425818
-857.744098	15.522726	5.435814
-855.602313	-0.282830	5.445811
-854.022205	13.145155	5.455808
-852.255034	3.285388	5.465805
-850.127578	5.667175	5.475802
-848.642866	14.751245	5.485798
-846.595684	15.507035	5.495795
-844.451187	6.867395	5.505792
-842.865341	17.921484	5.515789
-840.922451	5.856416	5.525786
-838.977913	12.102449	5.535782
-837.532020	19.137089	5.545779
-835.330718	10.156818	5.555776
-833.133336	9.617647	5.565773
-831.480661	-5.863408	5.575770
-829.603073	14.102377	5.585766
-827.902528	10.437581	5.595763
-825.983689	2.182951	5.605760
-824.161626	7.464955	5.615757
-822.184479	6.225256	5.625754
-820.119098	5.708774	5.635750
-818.507471	-2.289919	5.645747
-816.343911	7.328256	5.655744
-814.468581	9.071474	5.665741
-812.750279	14.235873	5.675738
-811.063962	9.264506	5.685734
-809.080738	6.457640	5.695731
-807.106617	13.826264	5.705728
-805.329729	6.118508	5.715725
-803.432725	4.588497	5.725722
-801.406312	12.270851	5.735718
-799.638454	12.256644	5.745715
-797.898707	6.005782	5.755712
-795.887633	7.741529	5.765709
-794.260414	16.903911	5.775706
-792.474530	6.834361	5.785702
-790.143662	9.212114	5.795699
-788.234305	16.191661	5.805696
-786.269165	2.230050	5.815693
-784.748116	7.495462	5.825690
-783.103937	8.285716	5.835686
-780.942674	7.643426	5.845683
-778.906177	4.259688	5.855680
-777.064999	8.491907	5.865677
-775.426075	12.506996	5.875674
-773.459303	14.702971	5.885670
-771.272405	4.796701	5.895667
-769.423998	9.242494	5.905664
-767.944793	7.340362	5.915661
-765.836274	16.129028	5.925658
-763.978661	12.857566	5.935654
-762.129496	4.097835	5.945651
-760.212886	15.394372	5.955648
-758.336725	8.586508	5.965645
-756.787315	16.610380	5.975642
-754.707317	20.010300	5.985638
-752.703722	18.232784	5.995635
-751.037128	5.245682	6.005632
-748.757355	11.645051	6.015629
-746.892572	2.778632	6.025626
-745.396882	14.186653	6.035622
-743.253700	17.472282	6.045619
-741.284145	8.874890	6.055616
-739.691003	8.402365	6.065613
-737.873251	13.549352	6.075610
-735.868791	8.418256	6.085606
-733.896245	6.465730	6.095603
-732.095205	7.723552	6.105600
-730.588552	13.788619	6.115597
-728.397431	4.715337	6.125594
-726.277136	10.109231	6.135590
-724.423892	10.668764	6.145587
-722.852451	6.724691	6.155584
-721.102917	20.247290	6.165581
-719.078916	7.915150	6.175578
-717.062441	15.592858	6.185574
-715.147066	5.349520	6.195571
-713.133434	8.872177	6.205568
-711.511444	9.238162	6.215565
-709.640064	4.652527	6.225562
-707.793774	14.894632	6.235558
-705.612032	1.065824	6.245555
-704.084669	11.687288	6.255552
-702.216618	6.199094	6.265549
-700.221124	11.838729	6.275546
-698.353018	3.906484	6.285542
-696.380975	9.712489	6.295539
-694.499137	3.069545	6.305536
-692.688344	-4.709859	6.315533
-690.795457	13.561107	6.325530
-689.070860	5.626537	6.335526
-686.919166	19.468567	6.345523
-685.174908	-7.170502	6.355520
-683.364823	21.785087	6.365517
-681.606081	17.294829	6.375514
-679.588613	7.253083	6.385510
-677.685069	8.453520	6.395507
-675.874904	4.433442	6.405504
-673.962591	4.659915	6.415501
-671.948165	18.977019	6.425498
-670.149785	-6.197633	6.435494
-668.340609	3.673087	6.445491
-666.407128	14.804395	6.455488
-664.523448	9.710019	6.465485
-662.841799	5.014215	6.475482
-660.838963	10.253265	6.485478
-658.764529	-10.996270	6.495475
-657.039126	30.650975	6.505472
-655.393016	17.574037	6.515469
-653.289294	-10.001857	6.525466
-651.723425	27.630625	6.535462
-649.524909	16.750023	6.545459
-647.323418	-7.142266	6.555456
-645.848286	11.517567	6.565453
-643.808284	-4.898369	6.575450
-642.104339	18.197774	6.585446
-640.112222	2.253662	6.595443
-638.431736	10.817167	6.605440
-636.423080	1.706802	6.615437
-634.648613	8.625931	6.625434
-632.595257	0.383106	6.635430
-630.593307	1.572596	6.645427
-628.812500	5.126207	6.655424
-627.097126	6.318853	6.665421
-625.453296	21.748298	6.675418
-623.369187	1.389268	6.685414
-621.250367	4.341029	6.695411
-619.457449	6.871202	6.705408
-617.676125	9.876882	6.715405
-615.663837	25.121171	6.725402
-613.966211	13.100170	6.735398
-612.138722	13.569176	6.745395
-610.003183	6.154760	6.755392
-608.262112	16.516388	6.765389
-606.347116	3.207075	6.775386
-604.571828	13.190632	6.785382
-602.603665	12.402518	6.795379
-600.825406	6.950845	6.805376
-599.120858	7.988936	6.815373
-597.299883	-5.821625	6.825370
-595.050472	9.168489	6.835366
-593.180897	9.913399	6.845363
-591.345733	7.771368	6.855360
-589.308781	3.411989	6.865357
-587.705193	15.699679	6.875354
-585.832961	2.791921	6.885350
-583.893113	11.078794	6.895347
-581.835393	4.802546	6.905344
-579.909860	3.051852	6.915341
-578.102037	4.686053	6.925338
-576.272065	5.844643	6.935334
-574.455472	8.955242	6.945331
-572.806974	7.332483	6.955328
-570.854700	6.884806	6.965325
-568.926693	7.756182	6.975322
-567.141139	4.201136	6.985318
-564.977408	-0.726330	6.995315
-563.410882	4.536710	7.005312
-561.221558	-1.129003	7.015309
-559.487845	9.154895	7.025306
-557.578604	19.134468	7.035302
-555.779613	-6.985954	7.045299
-553.961926	3.478729	7.055296
-551.968341	4.525948	7.065293
-550.131923	3.829968	7.075290
-547.943760	0.269050	7.085286
-546.429866	-0.095959	7.095283
-544.488389	7.857551	7.105280
-542.780193	6.957861	7.115277
-540.839960	0.965658	7.125274
-538.706209	-0.709319	7.135270
-537.060739	5.403179	7.145267
-535.087595	2.318688	7.155264
-533.364136	6.642536	7.165261
-531.281126	1.233812	7.175258
-529.529189	11.457988	7.185254
-527.404322	1.492356	7.195251
-525.523781	1.817175	7.205248
-524.124735	6.908057	7.215245
-521.902869	6.827863	7.225242
-520.242651	-0.504249	7.235238
-518.298207	4.782145	7.245235
-516.314309	0.535503	7.255232
-514.420667	11.867512	7.265229
-512.618022	6.836713	7.275226
-510.853185	0.353105	7.285222
-508.442123	2.942529	7.295219
-506.894180	6.801829	7.305216
-505.308741	10.205172	7.315213
-503.161518	4.934626	7.325210
-501.238244	1.056075	7.335206
-499.364062	-3.095669	7.345203
-497.574418	8.218227	7.355200
-495.758314	1.522770	7.365197
-493.850846	10.738518	7.375194
-492.082206	8.682970	7.385190
-490.087066	-0.960355	7.395187
-487.919659	6.439265	7.405184
-486.386348	13.248619	7.415181
-484.497092	6.181509	7.425178
-482.325287	-0.288127	7.435174
-480.723400	5.600862	7.445171
-478.944703	9.402807	7.455168
-477.114210	10.700331	7.465165
-474.986866	6.869731	7.475162
-473.186470	10.985564	7.485158
-471.318414	8.162625	7.495155
-469.337233	9.136111	7.505152
-467.561832	4.697025	7.515149
-465.490137	5.804471	7.525146
-464.071203	13.609410	7.535142
-461.940001	5.485327	7.545139
-460.069934	14.563406	7.555136
-457.926999	5.913276	7.565133
-456.234763	5.223023	7.575130
-454.362011	14.033853	7.585126
-452.623822	17.291273	7.595123
-450.663415	8.526618	7.605120
-448.798055	16.410274	7.615117
-446.781866	21.222680	7.625114
-444.878650	11.038304	7.635110
-443.378216	4.739053	7.645107
-441.081151	14.134206	7.655104
-439.573010	12.151867	7.665101
-437.474679	12.794063	7.675098
-435.810608	13.529282	7.685094
-433.742329	8.339289	7.695091
-431.663488	14.150584	7.705088
-430.067163	13.500925	7.715085
-428.043938	6.873487	7.725082
-426.375897	7.906481	7.735078
-424.545196	12.478537	7.745075
-422.460984	11.602573	7.755072
-420.309184	2.725284	7.765069
-418.671261	12.783034	7.775066
-417.080151	12.926797	7.785062
-415.065250	0.841054	7.795059
-413.193112	11.496107	7.805056
-411.284289	-1.529476	7.815053
-409.422196	15.851487	7.825050
-407.584433	13.766016	7.835046
-405.406019	6.605430	7.845043
-403.847120	6.784343	7.855040
-401.849096	5.876370	7.865037
-399.955941	7.039220	7.875034
-398.319916	5.661712	7.885030
-396.378067	16.463539	7.895027
-394.129915	10.553325	7.905024
-392.304107	8.529771	7.915021
-390.576283	11.607324	7.925018
-388.672115	3.690062	7.935014
-386.995778	2.733993	7.945011
-385.193943	5.318185	7.955008
-383.254350	12.485880	7.965005
-381.202752	4.432988	7.975002
-379.351129	8.924376	7.984998
-377.649758	5.768142	7.994995
-375.361238	10.284515	8.004992
-373.600875	12.210644	8.014989
-371.911895	7.104938	8.024986
-370.273989	9.547955	8.034982
-367.873875	11.894554	8.044979
-366.141014	6.611330	8.054976
-364.391902	2.485967	8.064973
-362.645082	6.771482	8.074970
-360.617802	10.317535	8.084966
-358.820132	11.190944	8.094963
-356.734558	9.868005	8.104960
-354.657075	12.272437	8.114957
-353.233726	18.927349	8.124954
-351.376124	1.486050	8.134950
-349.084244	17.557491	8.144947
-347.367735	17.817063	8.154944
-345.751262	12.748208	8.164941
-344.033249	21.831721	8.174938
-341.571733	21.391353	8.184934
-339.842856	11.645379	8.194931
-338.133243	15.183745	8.204928
-335.885753	5.686549	8.214925
-334.229282	19.931669	8.224922
-332.526036	12.384389	8.234918
-330.898037	18.335638	8.244915
-328.676129	13.454341	8.254912
-326.748890	9.979472	8.264909
-325.150883	6.302965	8.274906
-322.885714	14.504990	8.284902
-321.342133	8.751515	8.294899
-319.111774	19.519994	8.304896
-317.352936	11.434936	8.314893
-315.566479	11.817567	8.324890
-313.440898	14.708539	8.334886
-311.767527	16.051796	8.344883
-309.929891	4.007050	8.354880
-307.990596	10.895403	8.364877
-306.392469	15.973597	8.374874
-304.417580	13.165307	8.384870
-302.186553	14.781116	8.394867
-300.926005	21.239432	8.404864
-298.822078	9.471111	8.414861
-296.721138	18.226715	8.424858
-294.838128	11.348617	8.434854
-293.096763	15.518225	8.444851
-291.066405	14.834115	8.454848
-289.112095	15.349439	8.464845
-287.269125	21.468502	8.474842
-285.860574	16.104468	8.484838
-283.534614	11.752885	8.494835
-281.767001	18.090808	8.504832
-279.880384	20.797334	8.514829
-278.195224	17.204832	8.524826
-276.402636	16.481321	8.534822
-274.026771	21.418042	8.544819
-272.320043	11.023580	8.554816
-270.681290	17.783105	8.564813
-268.856341	14.801417	8.574810
-266.777149	8.177802	8.584807
-264.802176	19.654950	8.594803
-262.911494	12.897221	8.604800
-261.225081	24.916190	8.614797
-259.381613	13.708906	8.624794
-257.638045	10.359713	8.634791
-255.563580	20.985782	8.644787
-252.901528	10.042574	8.654784
-251.418202	8.509545	8.664781
-249.729507	6.256942	8.674778
-248.032888	11.662069	8.684775
-246.277196	4.899058	8.694771
-244.370677	-0.904397	8.704768
-242.550647	1.677002	8.714765
-240.527823	9.928838	8.724762
-238.339141	7.435406	8.734759
-236.947172	8.367338	8.744755
-234.846006	2.357573	8.754752
-233.142818	11.604578	8.764749
-231.131708	-5.120662	8.774746
-229.212793	12.355607	8.784743
-227.296260	8.940940	8.794739
-225.307924	12.131771	8.804736
-223.792427	13.876051	8.814733
-222.090473	5.580676	8.824730
-219.767987	5.773633	8.834727
-217.980400	2.808999	8.844723
-216.321231	16.499609	8.854720
-214.273852	4.124628	8.864717
-212.269363	5.236706	8.874714
-210.368031	6.823113	8.884711
-208.774941	10.320173	8.894707
-206.874945	9.099603	8.904704
-204.841179	6.529876	8.914701
-202.902622	15.704615	8.924698
-200.940094	5.788821	8.934695
-199.305857	-1.330541	8.944691
-197.500231	6.851788	8.954688
-195.688733	0.037279	8.964685
-193.598358	12.615478	8.974682
-191.809403	17.944340	8.984679
-189.668433	7.971659	8.994675
-187.906036	13.113720	9.004672
-186.010392	0.535620	9.014669
-184.342721	8.105278	9.024666
-182.273373	2.490607	9.034663
-180.542176	7.181363	9.044659
-178.284933	3.006622	9.054656
-176.937337	7.084422	9.064653
-174.886899	6.975064	9.074650
-173.092024	2.498340	9.084647
-171.071499	1.149625	9.094643
-169.230413	2.854618	9.104640
-167.547902	5.456440	9.114637
-165.779938	3.846469	9.124634
-163.626007	-1.787997	9.134631
-161.671097	-4.176168	9.144627
-159.673763	10.237321	9.154624
-157.877240	7.266565	9.164621
-156.145441	4.170358	9.174618
-154.269849	12.853111	9.184615
-152.439929	8.508168	9.194611
-150.226424	9.948505	9.204608
-148.593037	7.539015	9.214605
-146.799233	11.375125	9.224602
-144.666566	10.191685	9.234599
-142.985200	7.643500	9.244595
-141.254878	18.138282	9.254592
-139.169275	8.581817	9.264589
-137.565745	14.780255	9.274586
-135.361938	7.966344	9.284583
-133.642610	0.888704	9.294579
-131.690291	14.161583	9.304576
-129.641179	6.090332	9.314573
-128.012853	15.425154	9.324570
-125.990184	8.207545	9.334567
-124.069182	4.013871	9.344563
-122.227168	6.552386	9.354560
-120.276342	8.839873	9.364557
-118.663924	8.066280	9.374554
-116.790854	7.881065	9.384551
-115.154063	10.775992	9.394547
-112.797674	7.948039	9.404544
-110.993900	12.166246	9.414541
-109.504140	4.572647	9.424538
-107.507590	9.112185	9.434535
-105.106404	7.405971	9.444531
-103.181765	7.995649	9.454528
-101.570088	12.351872	9.464525
-100.074413	13.155241	9.474522
-97.980336	13.867884	9.484519
-96.011523	14.022652	9.494515
-93.875580	5.452869	9.504512
-92.449325	12.066437	9.514509
-90.607408	17.887427	9.524506
-88.289124	14.500346	9.534503
-86.660200	10.203302	9.544499
-84.774706	7.862576	9.554496
-83.118146	8.442934	9.564493
-81.070926	11.766592	9.574490
-79.101699	5.538012	9.584487
-77.306441	9.853914	9.594483
-75.633346	8.868577	9.604480
-73.679535	13.834938	9.614477
-71.683905	15.689030	9.624474
-69.508839	9.877592	9.634471
-67.772481	15.170735	9.644467
-65.945356	9.530061	9.654464
-63.962852	0.732164	9.664461
-62.536204	9.707649	9.674458
-60.544327	7.675215	9.684455
-58.579604	6.281813	9.694451
-56.618783	14.532661	9.704448
-54.580844	4.286013	9.714445
-53.032985	14.086858	9.724442
-50.839898	25.680992	9.734439
-48.850803	-0.130083	9.744435
-47.532985	9.322218	9.754432
-45.580840	16.222964	9.764429
-43.616629	6.115970	9.774426
-41.791060	18.092394	9.784423
-39.756119	6.594203	9.794419
-37.780508	11.299764	9.804416
-35.727667	15.789338	9.814413
-34.217186	6.365740	9.824410
-32.362278	12.187861	9.834407
-30.389568	12.855188	9.844403
-28.557322	7.621067	9.854400
-26.572499	8.460139	9.864397
-24.758793	12.961024	9.874394
-22.806533	16.519341	9.884391
-20.840982	8.586229	9.894387
-19.226537	12.752607	9.904384
-17.382025	13.753005	9.914381
-15.372893	7.516528	9.924378
-13.365601	12.719133	9.934375
-11.614201	19.711925	9.944371
-9.768421	16.496589	9.954368
-7.581531	10.312286	9.964365
-6.396920	13.254150	9.974362
-4.276419	13.089554	9.984359
-2.633899	24.198425	9.994355
-1.754995	60.144522	10.004352
-0.887985	125.184750	10.014349
0.000000	189.773653	10.019354
0.582689	236.022905	10.024359
1.559236	280.985842	10.029363
1.969699	322.997427	10.034368
2.371646	352.130604	10.039373
2.698676	385.504966	10.044378
3.106274	406.079654	10.049383
3.630430	423.171379	10.054387
3.561168	446.785135	10.059392
3.542475	441.663222	10.064397
3.796066	442.661910	10.069402
4.031905	468.105106	10.074407
4.097962	472.084056	10.079411
4.020177	480.371921	10.084416
3.892444	488.216768	10.089421
4.063557	495.088323	10.094426
4.511019	521.571721	10.099431
4.342962	509.476949	10.104435
4.322192	530.829735	10.109440
4.364345	526.827141	10.114445
4.397027	533.492144	10.119450
4.539467	538.381411	10.124455
4.662283	537.398311	10.129459
4.554708	544.166110	10.134464
5.273713	554.574009	10.139469
5.114657	571.812721	10.144474
4.931406	566.776931	10.149479
5.314570	569.134745	10.154483
4.682212	569.276568	10.159488
4.827858	559.486026	10.164493
4.975828	595.286308	10.169498
5.162691	562.335622	10.174503
5.206563	576.602645	10.179507
5.083352	594.781805	10.184512
5.482897	577.231845	10.189517
5.380459	587.264596	10.194522
5.094467	593.016967	10.199527
5.166293	587.029041	10.204531
5.301573	597.856487	10.209536
5.325350	581.180133	10.214541
5.629330	597.923995	10.219546
6.043095	622.676789	10.224551
5.676157	612.329318	10.229555
5.430934	614.016257	10.234560
5.853853	617.531491	10.239565
5.871192	622.887002	10.244570
5.593073	643.719622	10.249575
5.704201	642.030351	10.254579
5.623318	640.277089	10.259584
5.818576	647.403478	10.264589
5.789887	645.148320	10.269594
5.629478	642.335448	10.274599
5.911870	636.537838	10.279603
5.936865	672.040967	10.284608
6.373246	668.666143	10.289613
6.667769	673.958542	10.294618
6.332845	661.760950	10.299623
6.464356	656.200279	10.304627
6.337961	664.469194	10.309632
6.357825	668.455565	10.314637
6.490570	675.759091	10.319642
6.244900	694.080904	10.324647
6.905025	683.213195	10.329651
6.497307	689.221555	10.334656
6.669587	682.052233	10.339661
6.805385	687.187031	10.344666
6.299284	693.695194	10.349671
6.610163	692.623745	10.354675
6.704693	686.616387	10.359680
6.747469	690.266383	10.364685
6.825681	699.160256	10.369690
6.950471	698.872248	10.374695
7.116715	702.078366	10.379699
6.656106	705.960033	10.384704
6.653402	708.533950	10.389709
6.759962	717.450121	10.394714
7.041299	731.673115	10.399719
7.591716	733.556439	10.404723
7.023906	739.017933	10.409728
6.944621	745.891698	10.414733
7.149887	762.414957	10.419738
7.082177	750.523171	10.424743
7.153025	742.335541	10.429747
7.314326	748.120712	10.434752
7.372677	752.728580	10.439757
7.715793	767.891060	10.444762
7.569642	768.027876	10.449767
7.797908	776.716520	10.454771
7.875474	785.362973	10.459776
7.837496	773.851193	10.464781
7.817321	772.200194	10.469786
8.304220	769.648326	10.474791
8.188842	762.449151	10.479795
8.093263	758.403806	10.484800
7.964233	744.877081	10.489805
7.645027	773.933741	10.494810
7.521704	776.317178	10.499815
7.853314	775.762799	10.504819
8.036980	790.635350	10.509824
8.337471	781.980574	10.514829
8.046211	800.615715	10.519834
8.045529	792.758003	10.524839
8.138973	803.131815	10.529843
8.088428	816.800710	10.534848
8.045124	804.764641	10.539853
8.334230	799.853702	10.544858
8.270388	815.251444	10.549863
8.665943	819.723554	10.554867
8.992452	829.356906	10.559872
8.959875	813.345272	10.564877
8.667580	795.484352	10.569882
8.466432	813.873331	10.574887
8.751925	809.525927	10.579891
8.729142	832.700823	10.584896
9.039837	836.826933	10.589901
8.870410	839.077386	10.594906
8.788266	838.003955	10.599911
9.208584	834.426656	10.604915
9.194000	831.670912	10.609920
9.238375	824.304305	10.614925
9.245710	821.491452	10.619930
9.132602	819.446846	10.624935
9.170594	821.750946	10.629939
8.926083	839.538182	10.634944
9.327672	832.414214	10.639949
9.569736	826.340693	10.644954
9.025246	835.745540	10.649959
9.405107	830.848502	10.654963
9.458930	837.407773	10.659968
9.686181	835.359343	10.664973
9.307422	825.716912	10.669978
9.349591	847.478011	10.674983
9.489833	837.289181	10.679987
9.513240	834.680339	10.684992
9.468336	831.207200	10.689997
9.773740	840.897542	10.695002
9.730258	853.686999	10.700007
9.848882	838.188955	10.705011
9.663461	848.708198	10.710016
10.125306	860.797337	10.715021
9.998181	882.445143	10.720026
10.088566	870.444466	10.725031
10.117521	865.568688	10.730035
10.189120	867.296589	10.735040
10.136253	869.747650	10.740045
10.482368	868.099721	10.745050
10.113838	863.828224	10.750055
10.338404	858.484443	10.755059
10.341903	871.304269	10.760064
10.844584	878.006434	10.765069
10.143696	872.660438	10.770074
10.058484	878.689978	10.775079
10.378594	871.012870	10.780083
10.390378	876.191167	10.785088
10.549591	876.550514	10.790093
10.648026	883.049075	10.795098
10.263838	884.083282	10.800103
10.831645	873.146580	10.805107
10.626257	880.765907	10.810112
10.554220	875.428424	10.815117
10.771136	873.080445	10.820122
10.694766	884.129515	10.825127
10.917327	886.736922	10.830131
10.967615	904.792606	10.835136
11.287199	904.054063	10.840141
11.659976	912.355470	10.845146
11.502742	894.898658	10.850151
11.508198	870.373360	10.855155
11.116357	890.368199	10.860160
11.351459	869.062638	10.865165
11.470205	874.255414	10.870170
11.383347	879.093059	10.875175
11.747996	875.154051	10.880179
11.508968	883.398477	10.885184
11.214930	874.307041	10.890189
11.636307	869.136868	10.895194
11.644223	885.089358	10.900199
11.873250	874.216147	10.905203
11.441973	879.061414	10.910208
11.755204	876.899920	10.915213
11.858148	881.478640	10.920218
11.841243	888.378793	10.925223
11.872967	880.536365	10.930227
11.590415	888.421889	10.935232
11.518098	882.278637	10.940237
11.415120	886.983239	10.945242
11.826129	901.207798	10.950247
12.116822	912.322926	10.955251
11.916603	921.929962	10.960256
12.276634	907.798389	10.965261
12.263844	909.691139	10.970266
11.794101	913.878664	10.975271
12.343427	908.852072	10.980275
12.353443	916.709873	10.985280
12.399363	910.688099	10.990285
12.634076	896.114484	10.995290
12.676212	897.053891	11.000295
12.840026	903.953613	11.005299
12.496934	924.978346	11.010304
12.503580	902.335663	11.015309
12.702732	902.351178	11.020314
12.634958	906.514016	11.025319
13.074038	908.908701	11.030323
12.756333	903.746004	11.035328
12.646844	917.086933	11.040333
12.751344	907.031486	11.045338
12.874091	913.530914	11.050343
12.771825	914.699931	11.055347
12.788329	926.235686	11.060352
13.108687	920.647949	11.065357
13.296338	913.532832	11.070362
13.093177	909.176601	11.075367
13.020599	920.617751	11.080371
13.236622	915.947085	11.085376
13.003979	915.739733	11.090381
13.076735	915.717059	11.095386
12.994290	926.145820	11.100391
13.316615	934.769096	11.105395
13.286609	948.013799	11.110400
13.635476	949.574488	11.115405
13.669232	938.653525	11.120410
13.779912	945.020853	11.125415
13.791184	943.609244	11.130419
13.778568	945.238622	11.135424
13.973128	931.341573	11.140429
13.921644	926.782953	11.145434
13.768562	915.309917	11.150439
13.923668	907.163949	11.155443
13.975400	919.350084	11.160448
13.758399	910.176954	11.165453
14.081596	915.024905	11.170458
13.842810	921.668729	11.175463
13.957797	919.054727	11.180467
14.135182	932.406687	11.185472
14.248768	934.372324	11.190477
14.399408	935.448968	11.195482
13.877753	933.554658	11.200487
14.023453	926.152915	11.205491
14.089358	938.967580	11.210496
14.277165	936.529617	11.215501
14.539113	937.178506	11.220506
14.277351	947.935498	11.225511
14.164237	944.665596	11.230515
14.255180	942.873854	11.235520
14.234928	942.564820	11.240525
14.531087	951.547091	11.245530
14.369169	949.776753	11.250535
14.407965	947.181205	11.255539
14.131352	973.072869	11.260544
14.422987	981.541797	11.265549
14.979485	971.805299	11.270554
14.493056	974.245101	11.275559
14.808163	977.847006	11.280563
14.764847	976.876181	11.285568
14.973260	973.916112	11.290573
15.139841	987.678273	11.295578
14.855847	984.230612	11.300583
15.109593	970.295702	11.305587
15.031563	977.716574	11.310592
15.091011	994.175047	11.315597
15.318714	993.914775	11.320602
15.423594	1010.299789	11.325607
15.655387	995.247149	11.330611
15.910639	985.170759	11.335616
15.783370	977.560215	11.340621
15.965518	972.648931	11.345626
15.500669	976.767885	11.350631
15.973314	961.473443	11.355635
15.824837	967.577764	11.360640
15.547957	979.135120	11.365645
15.656021	962.454346	11.370650
15.590013	970.078299	11.375655
15.957384	963.259344	11.380659
15.751356	965.697002	11.385664
16.158133	971.619730	11.390669
16.089858	964.259979	11.395674
16.039143	968.358613	11.400679
16.221523	965.552507	11.405683
16.127643	966.291263	11.410688
15.922644	972.079751	11.415693
16.403614	971.189312	11.420698
16.113125	972.667470	11.425703
15.801284	964.748904	11.430707
15.959713	972.445872	11.435712
16.175317	975.782951	11.440717
16.495993	980.777982	11.445722
16.255625	972.620934	11.450727
16.398689	967.990272	11.455731
16.154170	983.312931	11.460736
16.553347	999.524842	11.465741
16.735869	992.820509	11.470746
16.597243	999.959323	11.475751
16.701094	1001.942291	11.480755
16.607992	1005.185109	11.485760
16.496666	1002.886305	11.490765
16.936684	998.968359	11.495770
16.553183	1009.984508	11.500775
17.216801	1002.500127	11.505779
17.062923	1003.276838	11.510784
17.167574	1002.820150	11.515789
17.289943	998.848787	11.520794
17.010633	999.349038	11.525799
17.065861	1011.151496	11.530803
16.961249	1019.554333	11.535808
17.072150	1002.259629	11.540813
17.060779	997.090620	11.545818
17.036289	1005.660443	11.550823
17.192675	994.352453	11.555827
16.965625	1007.764253	11.560832
16.820318	1006.606266	11.565837
16.942223	1007.020452	11.570842
17.167484	1033.795695	11.575847
17.570841	1026.486850	11.580851
17.475336	1024.775296	11.585856
17.702841	1022.364103	11.590861
17.960675	1014.521812	11.595866
17.496028	1025.691261	11.600871
18.150877	1022.904410	11.605875
18.079370	1016.756240	11.610880
17.897806	1028.782557	11.615885
18.412688	1014.586761	11.620890
17.968497	1020.545879	11.625895
18.055051	1021.722636	11.630899
18.134464	1026.354041	11.635904
17.821280	1037.652308	11.640909
18.157283	1020.659148	11.645914
18.046823	1029.324696	11.650919
18.092695	1027.062319	11.655923
18.138436	1020.086476	11.660928
18.033641	1031.220616	11.665933
18.353336	1030.341703	11.670938
18.383502	1029.773892	11.675943
18.606454	1015.843848	11.680947
18.363527	1021.381363	11.685952
18.384198	1016.781244	11.690957
18.960521	1023.694083	11.695962
18.537041	1035.107709	11.700967
18.393174	1037.906047	11.705971
18.445635	1034.254904	11.710976
18.329071	1032.523054	11.715981
18.522350	1025.487409	11.720986
18.460071	1043.422449	11.725991
18.464551	1060.897434	11.730995
18.564185	1070.500900	11.736000
18.618124	1065.838690	11.741005
19.054787	1048.596056	11.746010
18.821128	1060.965020	11.751015
19.181540	1046.284475	11.756019
19.516209	1060.787872	11.761024
19.721516	1040.442441	11.766029
19.386776	1047.558939	11.771034
19.448873	1060.006889	11.776039
19.674897	1040.199048	11.781043
19.438185	1035.089618	11.786048
19.539680	1045.556937	11.791053
19.780700	1052.144799	11.796058
19.701821	1036.290112	11.801063
19.408610	1055.387936	11.806067
19.926668	1043.757300	11.811072
19.675311	1037.505341	11.816077
19.517631	1017.023869	11.821082
19.685552	1028.765792	11.826087
19.740847	1035.556730	11.831091
19.511081	1035.885077	11.836096
19.921092	1055.345409	11.841101
20.244708	1044.848069	11.846106
20.232309	1052.286897	11.851111
20.017209	1040.216528	11.856115
19.738569	1024.956682	11.861120
20.039993	1035.803692	11.866125
20.093132	1044.633969	11.871130
20.015704	1054.823903	11.876135
20.033201	1051.348643	11.881139
19.882194	1063.734390	11.886144
19.972241	1068.217456	11.891149
20.293326	1052.959705	11.896154
19.703517	1054.829381	11.901159
20.032227	1058.716142	11.906163
20.002295	1070.617386	11.911168
20.162619	1084.046324	11.916173
20.386334	1082.474664	11.921178
20.163664	1092.924331	11.926183
20.180413	1089.354564	11.931187
20.324327	1087.125426	11.936192
20.348543	1086.978030	11.941197
20.855680	1078.392624	11.946202
20.921614	1096.080201	11.951207
20.777923	1099.835732	11.956211
20.611665	1093.578062	11.961216
20.943380	1107.649893	11.966221
21.323649	1105.870336	11.971226
21.054294	1103.552564	11.976231
21.503196	1093.565064	11.981235
21.218778	1089.510318	11.986240
21.262817	1086.343053	11.991245
21.730617	1079.649954	11.996250
21.621032	1074.707892	12.001255
21.785518	1078.149341	12.006259
21.987364	1070.421604	12.011264
21.672525	1067.022996	12.016269
21.838212	1057.594774	12.021274
21.873717	1051.394831	12.026279
21.478239	1025.277416	12.031283
21.766217	1034.399815	12.036288
21.340753	1038.982434	12.041293
21.591079	1035.159387	12.046298
21.684716	1048.941126	12.051303
21.497332	1037.851930	12.056307
21.506252	1046.143637	12.061312
21.596692	1048.805261	12.066317
21.636150	1032.931705	12.071322
21.186892	1036.728068	12.076327
21.479940	1043.078971	12.081331
21.663572	1042.071947	12.086336
21.216144	1046.777919	12.091341
21.606389	1033.568651	12.096346
21.501454	1030.175999	12.101351
21.614041	1021.385470	12.106355
21.456956	1017.190590	12.111360
21.304608	1014.414204	12.116365
21.354385	1008.691393	12.121370
20.976677	1014.595751	12.126375
21.289697	1034.893112	12.131379
21.223909	1032.355229	12.136384
20.818084	1048.935277	12.141389
21.603521	1038.644985	12.146394
21.290829	1043.047195	12.151399
21.620207	1034.876516	12.156403
21.722244	1043.298449	12.161408
21.402341	1046.345636	12.166413
21.548957	1040.025475	12.171418
21.439729	1056.643384	12.176423
21.635205	1053.653824	12.181427
21.690465	1026.117810	12.186432
21.332666	1025.186098	12.191437
21.283295	1010.055282	12.196442
21.470045	1032.564728	12.201447
21.282230	1011.077248	12.206451
21.649864	1013.708851	12.211456
21.035508	1002.414966	12.216461
21.238001	1014.580292	12.221466
21.107464	1032.787978	12.226471
21.487527	1047.284122	12.231475
21.695046	1050.606738	12.236480
21.411349	1036.863132	12.241485
21.438227	1033.909926	12.246490
21.415275	1018.044763	12.251495
21.346542	1016.286363	12.256499
21.233302	1018.109992	12.261504
21.222769	1037.457599	12.266509
21.530354	1042.658166	12.271514
21.571768	1043.468389	12.276519
21.522996	1044.620999	12.281523
21.584620	1033.228744	12.286528
21.425325	1026.243021	12.291533
21.520708	1026.325548	12.296538
21.451979	1015.966495	12.301543
21.234571	1031.948774	12.306547
21.328467	1020.776885	12.311552
21.011928	1037.148716	12.316557
21.425847	1031.047702	12.321562
21.304301	1036.859176	12.326567
21.529352	1038.177849	12.331571
21.401973	1035.635596	12.336576
21.517020	1037.851749	12.341581
21.468603	1036.011260	12.346586
21.437704	1027.273572	12.351591
21.588531	1023.168355	12.356595
21.528137	1029.651313	12.361600
21.025649	1034.282484	12.366605
21.732959	1015.889709	12.371610
21.486890	1020.038437	12.376615
21.423586	1033.386299	12.381619
21.743646	1031.966436	12.386624
21.602674	1032.827822	12.391629
21.349333	1028.348670	12.396634
21.416539	1039.198344	12.401639
21.562839	1018.621081	12.406643
21.369890	1031.926540	12.411648
21.246958	1031.242797	12.416653
21.687393	1021.805473	12.421658
21.662939	1030.318535	12.426663
21.160570	1037.225220	12.431667
21.517082	1029.692033	12.436672
21.323442	1032.993469	12.441677
21.450386	1030.691353	12.446682
21.726145	1036.224998	12.451687
21.727605	1026.349904	12.456691
21.561047	1031.594547	12.461696
21.346507	1039.548152	12.466701
21.638401	1025.545603	12.471706
21.282824	1011.423980	12.476711
21.236330	1017.720213	12.481715
21.457336	1027.622838	12.486720
21.625962	1034.616473	12.491725
21.365224	1014.329636	12.496730
21.407463	1005.293294	12.501735
21.259968	995.164435	12.506739
21.535568	1010.760561	12.511744
21.412011	1011.024662	12.516749
21.350031	1003.946159	12.521754
21.386668	994.801908	12.526759
20.864769	1007.970574	12.531763
21.410212	1022.393010	12.536768
21.288384	1031.087181	12.541773
21.388754	1029.754393	12.546778
21.262099	1042.079468	12.551783
21.327634	1037.041681	12.556787
21.634745	1038.049225	12.561792
21.206714	1045.294140	12.566797
21.389210	1039.867117	12.571802
21.731602	1032.853419	12.576807
21.467200	1041.448909	12.581811
21.684067	1037.976549	12.586816
21.364351	1027.233317	12.591821
21.581299	1017.497326	12.596826
21.303036	1012.711495	12.601831
21.472737	1013.163791	12.606835
21.583397	995.012853	12.611840
21.599816	1004.222697	12.616845
21.402959	1005.031494	12.621850
21.283879	1002.194612	12.626855
20.994099	1013.632629	12.631859
21.440856	1014.263087	12.636864
21.470034	1016.420392	12.641869
21.349498	1009.650844	12.646874
21.294920	1019.600568	12.651879
21.359815	1013.075834	12.656883
21.742890	1020.554076	12.661888
21.300744	1029.537449	12.666893
21.635365	1008.510700	12.671898
21.326278	1011.133533	12.676903
21.378342	1005.631131	12.681907
21.795254	1006.048731	12.686912
21.687132	1014.851092	12.691917
21.617283	1007.415876	12.696922
21.559501	1014.852461	12.701927
21.076161	1017.485740	12.706931
21.475367	1007.890999	12.711936
21.239059	1018.126746	12.716941
21.580345	1010.332648	12.721946
21.368132	1011.076085	12.726951
21.193976	1030.290506	12.731955
21.551248	1014.238552	12.736960
20.936799	1012.910959	12.741965
21.296649	1035.928964	12.746970
21.162601	1017.705062	12.751975
21.310353	1021.942370	12.756979
21.410948	1019.040488	12.761984
21.194813	1023.271175	12.766989
21.412011	1024.207902	12.771994
21.611333	1022.758410	12.776999
21.403185	1021.026974	12.782003
21.497774	1032.137202	12.787008
21.511067	1028.891275	12.792013
21.560356	1018.997519	12.797018
21.501624	1019.278089	12.802023
21.579400	1022.708123	12.807027
21.471908	1012.137636	12.812032
21.121610	1020.716851	12.817037
21.349848	1017.204835	12.822042
21.275214	1012.107411	12.827047
21.263690	1020.678329	12.832051
21.649809	1014.947606	12.837056
21.416762	1016.558531	12.842061
21.526357	1019.668101	12.847066
20.976363	1026.285911	12.852071
20.887042	1022.565920	12.857075
21.227418	1029.656741	12.862080
21.498043	1051.563063	12.867085
21.763679	1040.507271	12.872090
21.216369	1036.917089	12.877095
21.352843	1041.050545	12.882099
21.267619	1029.896177	12.887104
21.131870	1030.212685	12.892109
21.614143	1055.620770	12.897114
21.514567	1049.019748	12.902119
21.231058	1048.498808	12.907123
21.619758	1043.770600	12.912128
21.415095	1026.934623	12.917133
21.472236	1043.210595	12.922138
21.800991	1034.756165	12.927143
21.490762	1034.198486	12.932147
21.294110	1028.555969	12.937152
21.231107	1034.078986	12.942157
21.644621	1018.768684	12.947162
21.358832	1022.930055	12.952167
21.543429	1035.196023	12.957171
21.545208	1027.293636	12.962176
21.437984	1028.595915	12.967181
21.323244	1035.147467	12.972186
21.705424	1026.791754	12.977191
21.529633	1026.379791	12.982195
21.452431	1026.401534	12.987200
21.349281	1044.863486	12.992205
21.547091	1029.740536	12.997210
21.638131	1022.897816	13.002215
21.280814	1024.919644	13.007219
21.538250	1026.286767	13.012224
21.350875	1037.287427	13.017229
21.537673	1036.395015	13.022234
21.188657	1024.610943	13.027239
21.163618	1041.379411	13.032243
21.484896	1024.604636	13.037248
21.161922	1027.395267	13.042253
21.311500	1031.321628	13.047258
21.535698	1042.526310	13.052263
21.257415	1048.824831	13.057267
21.609981	1031.307048	13.062272
21.481552	1029.127660	13.067277
21.179539	1045.593378	13.072282
21.306154	1037.648999	13.077287
21.444051	1037.171238	13.082291
21.463658	1032.956059	13.087296
21.289171	1040.392346	13.092301
21.523889	1033.203433	13.097306
21.791108	1032.028538	13.102311
21.604582	1039.285396	13.107315
21.766133	1033.667751	13.112320
21.447600	1035.867898	13.117325
21.447007	1034.015050	13.122330
21.556801	1022.086845	13.127335
21.100797	1027.508534	13.132339
21.454344	1022.011660	13.137344
21.195201	1030.008643	13.142349
21.602840	1037.106086	13.147354
21.423585	1034.575261	13.152359
21.304089	1040.965148	13.157363
21.750616	1034.578236	13.162368
21.588542	1017.066853	13.167373
21.352583	1014.494612	13.172378
21.255850	1002.358088	13.177383
21.558225	1008.086173	13.182387
21.552683	1018.643083	13.187392
21.166964	1007.213383	13.192397
21.096095	1013.603388	13.197402
21.328126	1011.711867	13.202407
21.145976	1040.583202	13.207411
21.257242	1043.616817	13.212416
21.385124	1038.665280	13.217421
21.283225	1040.496565	13.222426
21.352728	1047.865559	13.227431
21.176280	1050.905637	13.232435
21.559759	1036.896356	13.237440
21.317748	1044.721882	13.242445
21.450458	1039.823191	13.247450
21.825998	1047.666923	13.252455
21.671836	1045.182556	13.257459
21.406379	1046.781307	13.262464
21.466614	1044.861987	13.267469
21.278252	1036.482143	13.272474
21.125914	1033.691559	13.277479
21.575235	1048.856323	13.282483
21.567314	1047.055105	13.287488
21.223157	1041.417184	13.292493
21.383550	1048.604527	13.297498
21.379989	1035.286176	13.302503
21.486309	1040.902039	13.307507
21.657248	1049.301949	13.312512
21.551372	1033.826883	13.317517
21.269544	1020.936122	13.322522
21.438048	1026.885836	13.327527
21.126260	1020.094746	13.332531
21.443978	1011.170583	13.337536
21.456617	1013.828839	13.342541
21.132515	1017.100616	13.347546
21.713997	1027.265870	13.352551
21.340596	1036.466941	13.357555
21.586243	1027.453338	13.362560
21.403227	1019.569389	13.367565
21.365734	1028.191761	13.372570
21.320547	1028.823406	13.377575
21.420738	1020.394398	13.382579
21.184168	1026.115403	13.387584
21.223755	1022.325969	13.392589
21.447950	1034.763816	13.397594
21.540014	1039.877330	13.402599
21.223350	1031.877494	13.407603
21.547505	1041.443558	13.412608
21.447451	1041.707064	13.417613
21.539758	1036.627161	13.422618
21.699784	1037.003730	13.427623
21.229132	1031.464834	13.432627
21.336054	1023.887878	13.437632
21.493579	1013.317701	13.442637
21.388096	1042.683012	13.447642
21.839957	1023.301221	13.452647
21.340610	1034.223900	13.457651
21.517382	1021.506003	13.462656
21.371287	1014.168098	13.467661
21.432667	1024.020485	13.472666
21.491476	1030.400854	13.477671
21.169368	1033.106193	13.482675
21.562751	1020.054131	13.487680
21.563786	1025.559047	13.492685
21.535473	1028.867231	13.497690
21.633973	1026.684768	13.502695
21.330470	1020.846408	13.507699
21.632504	1022.179610	13.512704
21.570486	1026.210678	13.517709
21.652954	1022.531099	13.522714
21.843348	1032.153182	13.527719
21.382784	1037.115134	13.532723
21.582429	1019.213325	13.537728
21.217818	1010.183519	13.542733
21.349164	1011.036167	13.547738
21.377091	1010.176978	13.552743
21.538070	1027.529194	13.557747
21.450642	1020.940440	13.562752
21.246278	1011.020912	13.567757
21.357280	1023.049450	13.572762
21.516365	1018.711105	13.577767
21.268632	1022.926331	13.582771
21.575160	1018.678012	13.587776
21.637603	1004.817732	13.592781
21.326205	1007.258009	13.597786
21.600487	991.697128	13.602791
21.112710	993.686142	13.607795
21.091203	996.505958	13.612800
21.109739	1016.016056	13.617805
21.336489	1027.038970	13.622810
21.741420	1029.645704	13.627815
21.281319	1036.362722	13.632819
21.583537	1027.592408	13.637824
21.569012	1032.112641	13.642829
21.024362	1015.897022	13.647834
21.438450	1015.679564	13.652839
21.381368	1028.195381	13.657843
21.524749	1030.459053	13.662848
21.466011	1036.888134	13.667853
21.487984	1021.719119	13.672858
21.397201	1012.847490	13.677863
21.210608	1007.928770	13.682867
21.512891	1018.706245	13.687872
21.554833	1017.488432	13.692877
21.300077	1021.293195	13.697882
21.350902	1007.844771	13.702887
21.542334	1013.437588	13.707891
21.549196	1008.885405	13.712896
21.216249	1008.366043	13.717901
21.200410	1002.598506	13.722906
21.758720	999.983173	13.727911
21.190325	1011.148658	13.732915
21.523342	1007.287199	13.737920
21.687478	1010.031679	13.742925
21.786756	1006.669543	13.747930
21.768845	1000.358292	13.752935
21.485172	1002.541835	13.757939
21.693973	1007.605181	13.762944
21.493300	1003.142869	13.767949
21.339942	1008.036894	13.772954
21.477748	1006.469481	13.777959
21.003934	1027.824292	13.782963
21.490241	993.088653	13.787968
21.578009	1014.535230	13.792973
21.557328	1011.190647	13.797978
21.624908	1009.194467	13.802983
21.495017	1015.369960	13.807987
21.532569	1007.296300	13.812992
21.371877	1012.251420	13.817997
21.410257	1011.518297	13.823002
22.046635	993.769216	13.828007
21.388290	986.497252	13.833011
21.210576	976.720152	13.838016
21.160823	980.586826	13.843021
21.312798	999.299766	13.848026
21.685334	1008.011274	13.853031
21.169604	998.322760	13.858035
21.523592	997.069375	13.863040
21.441850	990.462382	13.868045
21.110675	992.170956	13.873050
21.326957	993.267098	13.878055
21.204469	1007.874890	13.883059
21.339706	1020.022562	13.888064
21.571164	1012.860986	13.893069
21.327118	1015.173829	13.898074
21.716896	1008.811747	13.903079
21.460190	1014.343572	13.908083
21.490227	998.007935	13.913088
21.159216	987.187687	13.918093
21.446035	1001.749119	13.923098
21.676694	1005.621541	13.928103
21.162787	996.855249	13.933107
21.613076	992.134582	13.938112
21.319394	986.152744	13.943117
21.251680	993.901560	13.948122
21.398048	995.324241	13.953127
21.150087	1007.252320	13.958131
21.380374	1012.916210	13.963136
21.215382	1021.929494	13.968141
21.378854	1013.400512	13.973146
21.481004	1015.511486	13.978151
21.254422	1019.606644	13.983155
21.011626	1016.343215	13.988160
21.354141	1012.825591	13.993165
21.491453	1013.234166	13.998170
21.490338	1008.487715	14.003175
21.444356	1014.008010	14.008179
21.642063	1007.638714	14.013184
21.498669	1014.626909	14.018189
21.287666	1012.413932	14.023207
21.485452	1012.523920	14.028224
21.567078	1015.933546	14.033242
21.321374	1013.120996	14.038259
21.143858	1011.102906	14.043277
21.420316	1014.494042	14.048295
21.505195	1006.851812	14.053312
21.229857	1019.543545	14.058330
21.373089	1005.549993	14.063347
21.389196	1015.143778	14.068365
21.114956	1013.924429	14.073383
21.566517	1003.096756	14.078400
21.185501	1006.880590	14.083418
21.215127	1019.262582	14.088435
21.495689	1032.359567	14.093453
21.285708	1041.561591	14.098471
21.678245	1045.450141	14.103488
21.719896	1057.985968	14.108506
21.930910	1039.278527	14.113523
22.036081	1052.334294	14.118541
21.452483	1064.200682	14.123559
22.005495	1046.641978	14.128576
21.688800	1047.279154	14.133594
21.755775	1048.391510	14.138611
21.589801	1054.605834	14.143629
21.723956	1047.017068	14.148647
21.868303	1035.008340	14.153664
21.709036	1048.208515	14.158682
21.593758	1042.526593	14.163699
21.646513	1050.486581	14.168717
21.552340	1058.145983	14.173735
21.924435	1053.814545	14.178752
21.800891	1061.882875	14.183770
21.909108	1050.724558	14.188787
22.035929	1051.797483	14.193805
21.929211	1068.666795	14.198823
22.044851	1084.231311	14.203840
22.246126	1072.932301	14.208858
22.439396	1061.513460	14.213875
22.668701	1045.716153	14.218893
21.705594	1059.373279	14.223911
22.011087	1044.496567	14.228928
22.317656	1052.485286	14.233946
21.747774	1063.166647	14.238963
22.095838	1053.602772	14.243981
22.074039	1050.815849	14.248999
22.359525	1061.352927	14.254016
22.001919	1090.905458	14.259034
22.400030	1083.903748	14.264051
22.616760	1084.709096	14.269069
22.096787	1087.134082	14.274087
22.329986	1070.334172	14.279104
22.223009	1077.795865	14.284122
21.946913	1083.060413	14.289139
22.271406	1081.039325	14.294157
22.451008	1092.779300	14.299175
22.782870	1077.146490	14.304192
22.481610	1077.666382	14.309210
22.452275	1075.273889	14.314227
22.790921	1084.882344	14.319245
22.521016	1085.663061	14.324263
22.630678	1072.316553	14.329280
22.126958	1062.364733	14.334298
22.251358	1076.905443	14.339315
22.262951	1067.617003	14.344333
21.959593	1081.117024	14.349351
22.648216	1088.357462	14.354368
22.486974	1082.501968	14.359386
22.308569	1085.503223	14.364403
22.566455	1070.494087	14.369421
21.883777	1092.848848	14.374439
22.521031	1079.934112	14.379456
22.646198	1104.336986	14.384474
22.868616	1113.673004	14.389491
22.812733	1104.959985	14.394509
22.928645	1093.168089	14.399527
23.157698	1102.249800	14.404544
22.937252	1086.884377	14.409562
22.547048	1084.986708	14.414579
22.612124	1077.953176	14.419597
22.690692	1103.143651	14.424615
22.769445	1110.909202	14.429632
23.070038	1115.707433	14.434650
22.910100	1104.200180	14.439667
22.806712	1100.098707	14.444685
22.900489	1114.494909	14.449703
23.033121	1120.240093	14.454720
22.952616	1116.987495	14.459738
22.969931	1103.929376	14.464755
23.526629	1105.290803	14.469773
23.234626	1126.078015	14.474791
23.256273	1104.007877	14.479808
23.159524	1094.746136	14.484826
22.724910	1116.040540	14.489843
23.051892	1094.329111	14.494861
23.186121	1123.375432	14.499879
23.254442	1094.277870	14.504896
23.194049	1124.243937	14.509914
23.290454	1095.464345	14.514931
23.770105	1118.028580	14.519949
23.284267	1087.098861	14.524967
22.929631	1112.147668	14.529984
23.528350	1087.811732	14.535002
23.198399	1113.427577	14.540019
23.047354	1085.996147	14.545037
23.352240	1102.664583	14.550055
23.117347	1104.287526	14.555072
23.500734	1102.452087	14.560090
23.313724	1130.738023	14.565107
23.660614	1103.360847	14.570125
23.389018	1115.275039	14.575143
23.032336	1123.827297	14.580160
23.692899	1108.675255	14.585178
23.358308	1107.025101	14.590195
23.315555	1106.589895	14.595213
23.143708	1130.274164	14.600231
23.606642	1092.426366	14.605248
23.342515	1133.443314	14.610266
23.318256	1120.910879	14.615283
23.502899	1094.394822	14.620301
23.323785	1125.414813	14.625319
23.598559	1111.766673	14.630336
23.637532	1108.763993	14.635354
23.537750	1137.168156	14.640371
23.851764	1125.310037	14.645389
24.282819	1128.418584	14.650407
24.000564	1111.161316	14.655424
24.079880	1102.149900	14.660442
23.428140	1118.038171	14.665459
24.052725	1108.406567	14.670477
23.724666	1104.207224	14.675495
23.562322	1111.042301	14.680512
23.900474	1087.108122	14.685530
23.584850	1125.311428	14.690547
23.876210	1090.209026	14.695565
23.352207	1120.779100	14.700583
24.047407	1119.291881	14.705600
23.862839	1113.254489	14.710618
23.743925	1148.599927	14.715635
24.189600	1123.432662	14.720653
24.568233	1130.028897	14.725671
24.362751	1128.732508	14.730688
24.357011	1133.458483	14.735706
24.192155	1123.276409	14.740723
24.179897	1097.458673	14.745741
23.821616	1121.902500	14.750759
24.077918	1099.499235	14.755776
24.266081	1144.816829	14.760794
24.066040	1126.701765	14.765811
23.919673	1148.524367	14.770829
24.266944	1125.472661	14.775847
23.982481	1127.484162	14.780864
24.727168	1133.086125	14.785882
24.467893	1117.755173	14.790899
24.620589	1151.894907	14.795917
24.204689	1121.554822	14.800935
24.225819	1154.161486	14.805952
24.714574	1126.190666	14.810970
24.236975	1136.665464	14.815987
24.300318	1142.058360	14.821005
24.491200	1118.339515	14.826023
24.200337	1147.195718	14.831040
24.805746	1127.429597	14.836058
24.509593	1142.251362	14.841075
24.752396	1115.806210	14.846093
24.432578	1140.763003	14.851111
24.709614	1131.042102	14.856128
24.881666	1119.930176	14.861146
24.447142	1137.405518	14.866163
24.550489	1117.706898	14.871181
24.500936	1136.147968	14.876199
24.457798	1113.023272	14.881216
24.492795	1157.690546	14.886234
24.358120	1143.423450	14.891251
24.883224	1124.071239	14.896269
24.416918	1159.080446	14.901287
24.451528	1129.616976	14.906304
24.757835	1150.261616	14.911322
24.457045	1132.914475	14.916339
24.760905	1149.916591	14.921357
24.824056	1123.754892	14.926375
24.473044	1144.531093	14.931392
24.897432	1161.419625	14.936410
25.066169	1150.432466	14.941427
24.893784	1172.477891	14.946445
25.297669	1149.391951	14.951463
25.011307	1138.354693	14.956480
25.168497	1142.412930	14.961498
24.966704	1141.650749	14.966515
24.754926	1138.867368	14.971533
24.968819	1142.752977	14.976551
24.988894	1167.158560	14.981568
25.264102	1158.984129	14.986586
24.991183	1181.471867	14.991603
25.088829	1171.636411	14.996621
25.195189	1162.070117	15.001639
24.786022	1168.071604	15.006656
25.202398	1171.379119	15.011674
25.060714	1167.730448	15.016691
24.998249	1159.189895	15.021709
25.494769	1181.927709	15.026727
25.085695	1153.489724	15.031744
25.314450	1177.726772	15.036762
25.436877	1151.167054	15.041779
25.207295	1169.235779	15.046797
25.356214	1172.353154	15.051815
25.457752	1166.419539	15.056832
25.766985	1154.463063	15.061850
25.246801	1162.088220	15.066867
25.449451	1168.309867	15.071885
25.545689	1171.632261	15.076903
25.326514	1167.807196	15.081920
25.433183	1162.673389	15.086938
25.291469	1170.095055	15.091955
25.253091	1169.154236	15.096973
25.754773	1168.147736	15.101991
25.692692	1183.522063	15.107008
25.845123	1182.544522	15.112026
25.503303	1185.714996	15.117043
25.689696	1168.801321	15.122061
26.076138	1173.371960	15.127079
25.970386	1180.198044	15.132096
25.609873	1147.997721	15.137114
25.983751	1154.456308	15.142131
26.208568	1167.515118	15.147149
26.244008	1150.268481	15.152167
25.635742	1156.613157	15.157184
25.920332	1173.420184	15.162202
26.110999	1147.581006	15.167219
25.451872	1163.621506	15.172237
25.842761	1163.902035	15.177255
25.753167	1158.495954	15.182272
25.931403	1166.189043	15.187290
25.910179	1161.305282	15.192307
25.793686	1156.233808	15.197325
25.861050	1170.233180	15.202343
26.043387	1183.960987	15.207360
26.413842	1180.910146	15.212378
26.303961	1164.594254	15.217395
26.140286	1170.992294	15.222413
26.518887	1155.598897	15.227431
26.238782	1169.372127	15.232448
26.283016	1152.275088	15.237466
26.146634	1165.089497	15.242483
26.233369	1161.987958	15.247501
26.297845	1157.090531	15.252519
26.086591	1170.659312	15.257536
25.949909	1163.105814	15.262554
26.028927	1160.672432	15.267571
26.358548	1186.419157	15.272589
26.669765	1182.482761	15.277607
26.215059	1160.710290	15.282624
26.276446	1188.665731	15.287642
26.689685	1174.685581	15.292659
26.769856	1177.856391	15.297677
27.076435	1168.700157	15.302695
26.661104	1168.107302	15.307712
26.808605	1177.051065	15.312730
26.980920	1153.297373	15.317747
26.294512	1153.096943	15.322765
26.616830	1158.063173	15.327783
26.679186	1160.052399	15.332800
26.226676	1153.326306	15.337818
26.486797	1159.439689	15.342835
26.370142	1165.636756	15.347853
26.643104	1170.667488	15.352871
26.936576	1172.796027	15.357888
26.987381	1167.790671	15.362906
26.899303	1164.984411	15.367923
26.948497	1178.343357	15.372941
27.006242	1173.846525	15.377959
26.993630	1158.362941	15.382976
26.735794	1155.542859	15.387994
26.947925	1149.854294	15.393011
26.794536	1156.588868	15.398029
27.113802	1178.430059	15.403047
26.910805	1180.710131	15.408064
27.220213	1162.369064	15.413082
26.950495	1167.752169	15.418099
26.644171	1157.558027	15.423117
26.625172	1154.201235	15.428135
26.836715	1171.450894	15.433152
26.756279	1176.663824	15.438170
26.836709	1172.092591	15.443187
26.763132	1166.913601	15.448205
27.128681	1162.724740	15.453223
26.887376	1175.277481	15.458240
27.141917	1180.048474	15.463258
27.224362	1211.619933	15.468275
27.250648	1193.545765	15.473293
27.535923	1221.569378	15.478311
27.676534	1193.183642	15.483328
27.716868	1181.995153	15.488346
27.127605	1176.684481	15.493363
26.960135	1196.179426	15.498381
27.416230	1182.187716	15.503399
27.376431	1202.997734	15.508416
27.674450	1210.487710	15.513434
27.727453	1211.951499	15.518451
27.429055	1198.319187	15.523469
27.589215	1194.207115	15.528487
27.782209	1180.770143	15.533504
27.293618	1185.834249	15.538522
27.400132	1199.311482	15.543539
27.701375	1200.691638	15.548557
27.542938	1193.025196	15.553575
27.457773	1204.179885	15.558592
27.677342	1208.045731	15.563610
27.700662	1207.938167	15.568627
27.554669	1192.441213	15.573645
27.756569	1204.704659	15.578663
28.027408	1197.034245	15.583680
28.082718	1202.351369	15.588698
28.032947	1195.399014	15.593715
28.120901	1202.700702	15.598733
28.277905	1196.023666	15.603751
27.866825	1203.683352	15.608768
28.086983	1196.859398	15.613786
27.952831	1197.717566	15.618803
28.149658	1188.272099	15.623821
28.029231	1196.506738	15.628839
28.161643	1205.042388	15.633856
27.933271	1197.997398	15.638874
28.001600	1195.837833	15.643891
27.976013	1190.213904	15.648909
28.112101	1194.404502	15.653927
28.245229	1198.180317	15.658944
27.920113	1212.778696	15.663962
28.595011	1196.767024	15.668979
28.494508	1191.963533	15.673997
28.172633	1195.525636	15.679015
28.356202	1197.593059	15.684032
27.879695	1206.394124	15.689050
28.070832	1203.120206	15.694067
28.409211	1210.705986	15.699085
28.388072	1190.992514	15.704103
28.188718	1211.024218	15.709120
28.420183	1198.092301	15.714138
28.380620	1173.222547	15.719155
28.451788	1199.834735	15.724173
28.382122	1197.302370	15.729191
28.427691	1194.106721	15.734208
28.049741	1196.889725	15.739226
28.722298	1189.326699	15.744243
28.603203	1199.217433	15.749261
28.388101	1187.987883	15.754279
28.363674	1197.754986	15.759296
28.464755	1215.791483	15.764314
29.203980	1212.559134	15.769331
28.756221	1213.319460	15.774349
28.826145	1218.543030	15.779367
28.817157	1204.918036	15.784384
28.846898	1193.857062	15.789402
28.940604	1192.445316	15.794419
28.668979	1201.937257	15.799437
28.785401	1215.101482	15.804455
29.074076	1208.582757	15.809472
28.903652	1208.051511	15.814490
28.895502	1213.979624	15.819507
28.881563	1228.679395	15.824525
29.261973	1230.155462	15.829543
29.315344	1224.937330	15.834560
28.946739	1211.107001	15.839578
29.014172	1201.732496	15.844595
28.923289	1221.547151	15.849613
29.106112	1217.398426	15.854631
29.286398	1230.568210	15.859648
29.013776	1232.994667	15.864666
29.206344	1221.431103	15.869683
29.643487	1219.017671	15.874701
29.344654	1240.333072	15.879719
29.434833	1222.217219	15.884736
29.127707	1219.353078	15.889754
29.548002	1219.193215	15.894771
29.270268	1229.365658	15.899789
29.408112	1225.997993	15.904807
29.735841	1219.103393	15.909824
29.455524	1233.188160	15.914842
29.555426	1219.939023	15.919859
29.273624	1226.475470	15.924877
29.338434	1224.749021	15.929895
29.530667	1213.693577	15.934912
29.614422	1226.134750	15.939930
29.483771	1218.010856	15.944947
29.349352	1226.620531	15.949965
29.463425	1217.623949	15.954983
29.393719	1216.376680	15.960000
29.341381	1220.661827	15.965018
29.702304	1214.918048	15.970035
29.536986	1221.349405	15.975053
29.531329	1225.949562	15.980071
29.878145	1221.982310	15.985088
29.451602	1228.565436	15.990106
29.750874	1235.389870	15.995123
29.558652	1251.961588	16.000141
29.751265	1251.353568	16.005159
29.994416	1250.117747	16.010176
29.791713	1255.620750	16.015194
30.301628	1258.092291	16.020211
30.295874	1251.815547	16.025229
30.279848	1250.078393	16.030247
30.049747	1230.947150	16.035264
30.230978	1245.137637	16.040282
30.416740	1237.762327	16.045299
30.215980	1230.522591	16.050317
29.883443	1219.610604	16.055335
30.149521	1221.608246	16.060352
30.183262	1246.134474	16.065370
30.418301	1246.166169	16.070387
30.437473	1229.071462	16.075405
30.104314	1237.473751	16.080423
30.337288	1245.534087	16.085440
30.857014	1241.716998	16.090458
30.454898	1229.658413	16.095475
30.576550	1217.753821	16.100493
30.109265	1215.019037	16.105511
30.536116	1209.829433	16.110528
30.298016	1211.393127	16.115546
30.406101	1237.192577	16.120563
30.635194	1242.560650	16.125581
30.121952	1228.613378	16.130599
30.349838	1252.956079	16.135616
30.641797	1248.816681	16.140634
30.657180	1247.260126	16.145651
30.855916	1245.952741	16.150669
30.592225	1243.418279	16.155687
30.793904	1241.325526	16.160704
30.523219	1244.487814	16.165722
30.310655	1250.231475	16.170739
30.686702	1241.175796	16.175757
30.361872	1238.183920	16.180775
30.625593	1247.430073	16.185792
30.561607	1255.888541	16.190810
30.771726	1261.832199	16.195827
31.114936	1259.658673	16.200845
30.905849	1269.933450	16.205863
31.258047	1265.166271	16.210880
31.217433	1266.387033	16.215898
31.380429	1259.210388	16.220915
31.303170	1251.032344	16.225933
30.956521	1244.349096	16.230951
31.006568	1247.842461	16.235968
30.932814	1242.929299	16.240986
31.216301	1251.626491	16.246003
31.512209	1268.453846	16.251021
31.503485	1260.552717	16.256039
31.256934	1239.394984	16.261056
31.203362	1244.323669	16.266074
31.124856	1251.508791	16.271091
31.572899	1242.389722	16.276109
31.332636	1242.327339	16.281127
31.699932	1235.511361	16.286144
31.126800	1259.627907	16.291162
31.741933	1219.053183	16.296179
31.333590	1249.496549	16.301197
31.435764	1241.382699	16.306215
31.671912	1258.111040	16.311232
31.729152	1265.406648	16.316250
31.673099	1242.246053	16.321267
31.618631	1253.432062	16.326285
31.583193	1241.909562	16.331303
31.684540	1258.321218	16.336320
31.414542	1231.042182	16.341338
31.688541	1254.117604	16.346355
31.954520	1259.946965	16.351373
31.587223	1252.697599	16.356391
31.798553	1255.583254	16.361408
31.991343	1263.286658	16.366426
31.713199	1258.148124	16.371443
31.877744	1248.625973	16.376461
31.866230	1258.425662	16.381479
31.688338	1264.305365	16.386496
31.771718	1256.493364	16.391514
31.914017	1254.954319	16.396531
32.061053	1254.812868	16.401549
31.390272	1256.617021	16.406567
32.092693	1261.403126	16.411584
31.870144	1260.222699	16.416602
31.968480	1277.521998	16.421619
32.449483	1282.164105	16.426637
32.482345	1300.674035	16.431655
32.514693	1281.988484	16.436672
32.100683	1269.568410	16.441690
32.438115	1273.706473	16.446707
32.485197	1279.243579	16.451725
32.018277	1271.045873	16.456743
32.086789	1279.637373	16.461760
32.590756	1261.735465	16.466778
32.485482	1291.101878	16.471795
32.822774	1284.429082	16.476813
32.443718	1299.891835	16.481831
32.692259	1285.598087	16.486848
32.552572	1296.060006	16.491866
32.529000	1288.606375	16.496883
32.872767	1275.798045	16.501901
32.517149	1279.022646	16.506919
32.569018	1283.432758	16.511936
32.858916	1286.096687	16.516954
32.695267	1291.217541	16.521971
32.983446	1279.338249	16.526989
32.923618	1294.968727	16.532007
32.885147	1288.041265	16.537024
32.842997	1274.438796	16.542042
32.681679	1280.926167	16.547059
32.879395	1278.719215	16.552077
32.705423	1298.256232	16.557095
32.630446	1290.293296	16.562112
32.815635	1285.016370	16.567130
32.442559	1285.294476	16.572147
32.451164	1297.684778	16.577165
32.433521	1295.947876	16.582183
32.779131	1302.393736	16.587200
33.328662	1308.555405	16.592218
33.216674	1319.920517	16.597235
33.237535	1313.740171	16.602253
33.254488	1312.257288	16.607271
33.237601	1297.125005	16.612288
33.391493	1322.119815	16.617306
33.438508	1317.961262	16.622323
33.417349	1311.751440	16.627341
33.538278	1327.894222	16.632359
33.559232	1303.198630	16.637376
33.630449	1334.641594	16.642394
33.461498	1330.644888	16.647411
33.594756	1310.958537	16.652429
33.565243	1319.856690	16.657447
33.456102	1328.133646	16.662464
33.460228	1322.810080	16.667482
33.610883	1319.638542	16.672499
33.519900	1316.327797	16.677517
33.797030	1311.391685	16.682535
33.581266	1317.076111	16.687552
33.627946	1315.874764	16.692570
33.156766	1317.799669	16.697587
33.636042	1320.164428	16.702605
33.356939	1320.149135	16.707623
33.412784	1314.859793	16.712640
33.776651	1320.598067	16.717658
33.736694	1342.869586	16.722675
33.899059	1353.802451	16.727693
33.983978	1349.785701	16.732711
33.927239	1341.137166	16.737728
33.970101	1351.845280	16.742746
34.308911	1350.227697	16.747763
34.398725	1335.119255	16.752781
34.496248	1338.954266	16.757799
34.483793	1348.955504	16.762816
34.501856	1331.090105	16.767834
34.199675	1306.016624	16.772851
34.062840	1310.930297	16.777869
34.252534	1317.205983	16.782887
34.258561	1320.026869	16.787904
34.541987	1337.403684	16.792922
34.266331	1333.386243	16.797939
34.631133	1337.710288	16.802957
34.633905	1327.089222	16.807975
34.213006	1326.322649	16.812992
34.493203	1320.417106	16.818010
34.151531	1329.453132	16.823027
34.362182	1339.499004	16.828045
34.441549	1336.544889	16.833063
34.415445	1350.076444	16.838080
34.701101	1343.249842	16.843098
34.614125	1346.117024	16.848115
34.464472	1322.678658	16.853133
34.861342	1348.237206	16.858151
34.372413	1342.750028	16.863168
34.818130	1329.821577	16.868186
34.412804	1334.856724	16.873203
34.443359	1348.288011	16.878221
34.530911	1334.156736	16.883239
34.646455	1368.260437	16.888256
34.984705	1340.544433	16.893274
34.878998	1382.815637	16.898291
35.311571	1353.057020	16.903309
35.338217	1372.411138	16.908327
34.939168	1367.932040	16.913344
34.904527	1367.449916	16.918362
35.283483	1376.056456	16.923379
35.592560	1363.145048	16.928397
35.479478	1361.465829	16.933415
35.318566	1361.209900	16.938432
35.236196	1371.796434	16.943450
35.417306	1353.107515	16.948467
35.410438	1365.667076	16.953485
35.680885	1373.312538	16.958503
35.518653	1364.031181	16.963520
35.520493	1352.373666	16.968538
35.450954	1349.643060	16.973555
35.465787	1345.247395	16.978573
35.303307	1344.916215	16.983591
35.443343	1359.061477	16.988608
35.812155	1352.416655	16.993626
35.434863	1367.643255	16.998643
35.359576	1358.923738	17.003661
35.725823	1351.263195	17.008679
35.669762	1370.985990	17.013696
35.861035	1360.172823	17.018714
36.059453	1363.033819	17.023731
35.687292	1354.561415	17.028749
36.005513	1360.871677	17.033767
35.912494	1356.968241	17.038784
36.077928	1351.007059	17.043802
35.496984	1377.132138	17.048819
35.722390	1359.925740	17.053837
35.908946	1341.559997	17.058855
35.739856	1356.143074	17.063872
35.936741	1372.352441	17.068890
35.930906	1360.071679	17.073907
35.475545	1356.391190	17.078925
35.822715	1360.486829	17.083943
35.724613	1402.258249	17.088960
35.970243	1378.909331	17.093978
35.778161	1383.006035	17.098995
35.723454	1398.226838	17.104013
36.173049	1389.230122	17.109031
36.162648	1408.366835	17.114048
36.556884	1402.402175	17.119066
36.505077	1427.928602	17.124083
36.875070	1407.248004	17.129101
36.817053	1387.058818	17.134119
36.694385	1379.078272	17.139136
36.718376	1365.707406	17.144154
36.721268	1394.103565	17.149171
36.551094	1376.029040	17.154189
36.939520	1377.643839	17.159207
36.763595	1387.881951	17.164224
36.674895	1381.108739	17.169242
37.077831	1379.112854	17.174259
36.913962	1361.284296	17.179277
36.642883	1388.299036	17.184295
36.739023	1383.207728	17.189312
37.195065	1363.222874	17.194330
36.925248	1378.525150	17.199347
37.179498	1373.967031	17.204365
37.132512	1386.064266	17.209383
36.739901	1382.847224	17.214400
36.601817	1366.375159	17.219418
36.738105	1373.952359	17.224435
36.679846	1371.279723	17.229453
37.195669	1390.563718	17.234471
37.196372	1402.676955	17.239488
37.146366	1407.100206	17.244506
37.202262	1401.735322	17.249523
37.250921	1407.336717	17.254541
37.531390	1402.255330	17.259559
37.422890	1403.430303	17.264576
37.702543	1399.585396	17.269594
37.537529	1404.314839	17.274611
37.325868	1403.774431	17.279629
37.720716	1405.462139	17.284647
37.429417	1406.760641	17.289664
37.905871	1395.052569	17.294682
37.691663	1400.818573	17.299699
37.503306	1398.042416	17.304717
37.874228	1393.108622	17.309735
37.715648	1404.014061	17.314752
37.606593	1395.005763	17.319770
37.380575	1389.269008	17.324787
37.712961	1403.522059	17.329805
37.812497	1393.286618	17.334823
37.604331	1396.023706	17.339840
38.047153	1386.274623	17.344858
37.930154	1396.652775	17.349875
37.852362	1407.649148	17.354893
38.225110	1395.050015	17.359911
37.762702	1397.133972	17.364928
38.092020	1393.987407	17.369946
37.992037	1399.408018	17.374963
37.705012	1391.780852	17.379981
37.904331	1399.406213	17.384999
37.609797	1403.157480	17.390016
37.973558	1411.522656	17.395034
38.241052	1424.876903	17.400051
37.894817	1427.337152	17.405069
38.431489	1426.065519	17.410087
38.337741	1428.163044	17.415104
38.772423	1427.075983	17.420122
38.719334	1420.243594	17.425139
38.579017	1425.525935	17.430157
38.862762	1404.459561	17.435175
38.758422	1420.155473	17.440192
38.668674	1414.967961	17.445210
38.778145	1397.029703	17.450227
38.802276	1409.170670	17.455245
38.849704	1378.664919	17.460263
38.630791	1379.308535	17.465280
38.282632	1395.707092	17.470298
39.283483	1377.129649	17.475315
38.915112	1393.526709	17.480333
39.016457	1384.225325	17.485351
39.039573	1383.205475	17.490368
38.835202	1369.164764	17.495386
38.832920	1363.750973	17.500403
38.616756	1406.779153	17.505421
39.221786	1417.087790	17.510439
38.967243	1398.216615	17.515456
39.313444	1428.294642	17.520474
39.251729	1427.181355	17.525491
38.917058	1405.991814	17.530509
39.155042	1423.635519	17.535527
38.857529	1423.321152	17.540544
39.069389	1419.296723	17.545562
39.349610	1407.247143	17.550579
39.075894	1405.173554	17.555597
39.290208	1420.708542	17.560615
39.407066	1400.153262	17.565632
39.059856	1407.761970	17.570650
39.161306	1425.251279	17.575667
39.648852	1428.596269	17.580685
39.589984	1429.294585	17.585703
39.759408	1420.970143	17.590720
39.888867	1438.898578	17.595738
39.948657	1408.036876	17.600755
39.554369	1412.247629	17.605773
39.857647	1413.037622	17.610791
39.736882	1409.519255	17.615808
39.671131	1418.196741	17.620826
39.784185	1437.707047	17.625843
39.752719	1429.960457	17.630861
39.940782	1433.820379	17.635879
39.769274	1430.011235	17.640896
39.840738	1435.360475	17.645914
39.997818	1432.264964	17.650931
40.145085	1448.936918	17.655949
40.049058	1433.661389	17.660967
39.990960	1444.217364	17.665984
40.393577	1423.120996	17.671002
40.014667	1429.754814	17.676019
40.155762	1441.079660	17.681037
40.397520	1427.283913	17.686055
39.800222	1430.385073	17.691072
40.001116	1425.827582	17.696090
40.118389	1430.370449	17.701107
40.050008	1456.506734	17.706125
40.654531	1457.794509	17.711143
40.533301	1466.004262	17.716160
40.517137	1469.374537	17.721178
40.648723	1460.806004	17.726195
40.773888	1454.616829	17.731213
40.740769	1450.601573	17.736231
40.927731	1465.931766	17.741248
40.694362	1452.947915	17.746266
41.055019	1453.780668	17.751283
40.852716	1456.202238	17.756301
41.025755	1454.651978	17.761319
41.409069	1433.407668	17.766336
40.958891	1418.168185	17.771354
40.956131	1408.578233	17.776371
40.678820	1418.074367	17.781389
40.990553	1425.658220	17.786407
41.010087	1439.865249	17.791424
40.869452	1455.425420	17.796442
41.441177	1442.712719	17.801459
41.350251	1447.881803	17.806477
41.097670	1466.456341	17.811495
41.392313	1446.034660	17.816512
41.424927	1445.324739	17.821530
41.657632	1439.124712	17.826547
41.255665	1432.912649	17.831565
41.396770	1434.422184	17.836583
41.264019	1444.162685	17.841600
41.326123	1447.770574	17.846618
41.711662	1436.630653	17.851635
41.360889	1444.727568	17.856653
41.258760	1453.396719	17.861671
41.666557	1444.057437	17.866688
41.268995	1449.547545	17.871706
41.431381	1455.564961	17.876723
41.111047	1444.493559	17.881741
41.453042	1465.027572	17.886759
41.602610	1475.765950	17.891776
41.535197	1479.609999	17.896794
42.027964	1479.957659	17.901811
41.668526	1484.032318	17.906829
41.858736	1474.842543	17.911847
41.768453	1475.361833	17.916864
41.954192	1474.172902	17.921882
41.921317	1468.561037	17.926899
42.113813	1474.284233	17.931917
42.006298	1478.862963	17.936935
42.183285	1487.257969	17.941952
41.893460	1478.959544	17.946970
42.248179	1487.568444	17.951987
42.419103	1495.352536	17.957005
42.579005	1499.009334	17.962023
42.897607	1482.719128	17.967040
42.767357	1475.191180	17.972058
42.758131	1465.599075	17.977075
42.852323	1469.590377	17.982093
42.340067	1472.449903	17.987111
42.497835	1467.090770	17.992128
42.312538	1478.042996	17.997146
42.522902	1462.819244	18.002163
42.585447	1466.983900	18.007181
42.563501	1458.288848	18.012199
43.011714	1482.047836	18.017216
42.913471	1483.601838	18.022234
43.133790	1469.221178	18.027251
42.590364	1478.879335	18.032269
42.820357	1480.467505	18.037287
42.872254	1493.415767	18.042304
42.943283	1501.878015	18.047322
43.170052	1512.025254	18.052339
43.118971	1503.372573	18.057357
43.150283	1494.835742	18.062375
43.365398	1503.040639	18.067392
43.377098	1496.043730	18.072410
43.353072	1485.598275	18.077427
43.155622	1494.137939	18.082445
43.087177	1506.893053	18.087463
43.409876	1489.296618	18.092480
43.276290	1503.973279	18.097498
43.222726	1492.958394	18.102515
43.208749	1497.913883	18.107533
43.323133	1487.237149	18.112551
43.249483	1487.055388	18.117568
43.141753	1495.632652	18.122586
43.300432	1497.469716	18.127603
43.529741	1518.470073	18.132621
43.263465	1523.487828	18.137639
44.014762	1513.118477	18.142656
43.537311	1513.461992	18.147674
44.145574	1507.883143	18.152691
44.087169	1510.327391	18.157709
43.932559	1515.206215	18.162727
44.147637	1494.068868	18.167744
43.807396	1504.573931	18.172762
44.002774	1512.059986	18.177779
43.804783	1507.940449	18.182797
43.941608	1497.565286	18.187815
44.197314	1515.324251	18.192832
43.762316	1494.219789	18.197850
43.866236	1520.224896	18.202867
44.335691	1520.381227	18.207885
44.207757	1527.717509	18.212903
44.274082	1538.407862	18.217920
44.348302	1540.810516	18.222938
44.744172	1539.757951	18.227955
44.914331	1530.329099	18.232973
44.686558	1524.781326	18.237991
44.949252	1524.604126	18.243008
44.735805	1519.400125	18.248026
44.754324	1500.845480	18.253043
44.590580	1499.962383	18.258061
44.502845	1513.769753	18.263079
44.552317	1502.217775	18.268096
44.839978	1530.362729	18.273114
44.453256	1530.438527	18.278131
44.952758	1514.473356	18.283149
44.888471	1527.053225	18.288167
45.397311	1528.793554	18.293184
45.234221	1508.542306	18.298202
45.014702	1557.864941	18.303219
45.215933	1509.934096	18.308237
44.947905	1537.200302	18.313255
45.000474	1518.506502	18.318272
45.173397	1544.093247	18.323290
45.152840	1516.141554	18.328307
45.518234	1524.515974	18.333325
45.029479	1528.502732	18.338343
45.217985	1525.578363	18.343360
44.991116	1526.009328	18.348378
45.529738	1540.202886	18.353395
45.628773	1549.110567	18.358413
45.652162	1559.928903	18.363431
45.953748	1553.505491	18.368448
45.637640	1549.488147	18.373466
45.558018	1554.677487	18.378483
45.935281	1556.095893	18.383501
45.741624	1547.856022	18.388519
46.140314	1543.762440	18.393536
45.884344	1536.830219	18.398554
45.838121	1546.541259	18.403571
46.008379	1541.865926	18.408589
46.077910	1553.825174	18.413607
45.997098	1547.340054	18.418624
45.616708	1536.591181	18.423642
45.592590	1561.812990	18.428659
46.191974	1541.525043	18.433677
45.860865	1545.535427	18.438695
46.020856	1549.064813	18.443712
45.922218	1548.764343	18.448730
45.923751	1547.370409	18.453747
46.456683	1556.715398	18.458765
46.224746	1570.947715	18.463783
46.494624	1567.241174	18.468800
46.508120	1578.347384	18.473818
46.509564	1574.638032	18.478835
46.514290	1584.333108	18.483853
46.538790	1577.541751	18.488871
46.751523	1583.239742	18.493888
46.887394	1574.314966	18.498906
46.626862	1577.968048	18.503923
46.831591	1571.292667	18.508941
47.093399	1577.365064	18.513959
47.145343	1584.120572	18.518976
47.048095	1589.062631	18.523994
47.153385	1557.866960	18.529011
47.368225	1586.101499	18.534029
47.103263	1564.613537	18.539047
47.287593	1580.272239	18.544064
47.271406	1555.497983	18.549082
47.007292	1552.328047	18.554099
47.226000	1575.926381	18.559117
47.292514	1575.306999	18.564135
47.422831	1566.221096	18.569152
47.519968	1565.756488	18.574170
47.165896	1577.603202	18.579187
47.310982	1585.342700	18.584205
47.259806	1574.380854	18.589223
47.282299	1563.280642	18.594240
47.278744	1580.622509	18.599258
47.306619	1585.868648	18.604275
47.282352	1559.862455	18.609293
47.197320	1587.948196	18.614311
47.340116	1600.381850	18.619328
47.584842	1593.135379	18.624346
47.520025	1607.741405	18.629363
47.612382	1610.844303	18.634381
47.717630	1599.314812	18.639399
47.775506	1599.533634	18.644416
47.779383	1626.440476	18.649434
48.031827	1622.201885	18.654451
48.034411	1620.439697	18.659469
48.155837	1648.103316	18.664487
48.395684	1612.724726	18.669504
48.508142	1635.600011	18.674522
48.649825	1621.546339	18.679539
48.742209	1623.384554	18.684557
48.466901	1611.442272	18.689575
48.611429	1621.255074	18.694592
48.851273	1594.457173	18.699610
48.559496	1591.541744	18.704627
49.041508	1582.498844	18.709645
48.894193	1589.792631	18.714663
48.649905	1584.753968	18.719680
48.601923	1586.103343	18.724698
48.488254	1588.971684	18.729715
48.609050	1582.064298	18.734733
48.692792	1588.419919	18.739751
48.773995	1577.797172	18.744768
48.577691	1576.010079	18.749786
48.752036	1603.125641	18.754803
49.354157	1604.438983	18.759821
49.251068	1618.228452	18.764839
49.279959	1596.208316	18.769856
49.116242	1597.727154	18.774874
48.899486	1602.425588	18.779891
49.063593	1613.201075	18.784909
48.818026	1615.000375	18.789927
48.883475	1625.796324	18.794944
49.331034	1613.828424	18.799962
48.869480	1617.007072	18.804979
49.242200	1611.847982	18.809997
49.289983	1632.260843	18.815015
49.434406	1629.982116	18.820032
49.714750	1645.955118	18.825050
49.766107	1659.727862	18.830067
49.990162	1645.829340	18.835085
49.971184	1652.235976	18.840103
49.616166	1634.879573	18.845120
49.823714	1633.740633	18.850138
49.697670	1645.556543	18.855155
50.143042	1652.831349	18.860173
49.876204	1639.078756	18.865191
49.698731	1662.662547	18.870208
50.080783	1651.943007	18.875226
49.977623	1648.687608	18.880243
50.249710	1645.320461	18.885261
50.023778	1652.894225	18.890279
50.201787	1642.608343	18.895296
50.091706	1647.388877	18.900314
50.066100	1639.336080	18.905331
50.267339	1646.531841	18.910349
50.062046	1666.937919	18.915367
50.309329	1657.049958	18.920384
50.371720	1688.407012	18.925402
50.573996	1687.907545	18.930419
50.774184	1672.194423	18.935437
50.743560	1682.771359	18.940455
50.778969	1686.404015	18.945472
50.775897	1666.260732	18.950490
50.830478	1686.175519	18.955507
51.231843	1663.350283	18.960525
51.256619	1665.943310	18.965543
50.941019	1657.463278	18.970560
51.213118	1672.457651	18.975578
50.888865	1678.312098	18.980595
50.987305	1667.301154	18.985613
51.070710	1650.892540	18.990631
50.936710	1675.987356	18.995648
51.606428	1665.555406	19.000666
51.321653	1669.173052	19.005683
51.430040	1662.693888	19.010701
51.240733	1667.450884	19.015719
51.122555	1669.797727	19.020736
51.398577	1654.346232	19.025754
51.133595	1684.330355	19.030771
51.559197	1643.161768	19.035789
51.462091	1665.033919	19.040807
51.024806	1671.859621	19.045824
51.369119	1658.295833	19.050842
51.340454	1689.181357	19.055859
51.680536	1699.181673	19.060877
51.704561	1690.661618	19.065895
51.528895	1680.875694	19.070912
51.775195	1682.281966	19.075930
51.656022	1706.962346	19.080947
52.293844	1678.705577	19.085965
52.231854	1693.926279	19.090983
52.110140	1697.953648	19.096000
52.483498	1668.565618	19.101018
52.059646	1691.784489	19.106035
52.009819	1681.226606	19.111053
52.289028	1719.755035	19.116071
52.362827	1706.876124	19.121088
53.014367	1710.522214	19.126106
52.378425	1721.854794	19.131123
52.748810	1710.448098	19.136141
52.391852	1708.269764	19.141159
52.687019	1731.196286	19.146176
52.811339	1700.578496	19.151194
52.531712	1720.894260	19.156211
52.676425	1705.930830	19.161229
52.552942	1726.114737	19.166247
52.744905	1725.319616	19.171264
52.864896	1692.682804	19.176282
52.822244	1725.157786	19.181299
52.997122	1704.920006	19.186317
52.830788	1712.846086	19.191335
52.898720	1716.207726	19.196352
52.959058	1707.799845	19.201370
53.041836	1719.296229	19.206387
53.376531	1759.517899	19.211405
53.282835	1727.217103	19.216423
53.618325	1745.407213	19.221440
53.662918	1730.226921	19.226458
53.202892	1754.345123	19.231475
53.210091	1721.089169	19.236493
53.545684	1744.023422	19.241511
53.633922	1722.745523	19.246528
53.371720	1744.836028	19.251546
54.075267	1737.072733	19.256563
53.832793	1725.595448	19.261581
53.574107	1743.583012	19.266599
53.644921	1738.904599	19.271616
53.768230	1718.393457	19.276634
53.630399	1741.938022	19.281651
53.914595	1739.838333	19.286669
53.714294	1729.394072	19.291687
53.927174	1767.967813	19.296704
54.026795	1744.144523	19.301722
54.173389	1764.312155	19.306739
54.399307	1765.979658	19.311757
54.286268	1760.534618	19.316775
54.286258	1768.830601	19.321792
54.830592	1773.204801	19.326810
54.704762	1757.735484	19.331827
54.724309	1760.901933	19.336845
54.784243	1769.034204	19.341863
54.518302	1769.833196	19.346880
54.806258	1749.786530	19.351898
54.692854	1779.199273	19.356915
54.676213	1747.760732	19.361933
54.775845	1759.449512	19.366951
54.655988	1764.335462	19.371968
54.956957	1749.076514	19.376986
54.809282	1756.905263	19.382003
55.221869	1766.101271	19.387021
55.051011	1740.447674	19.392039
54.881144	1769.649182	19.397056
54.899494	1741.550852	19.402074
55.058994	1767.893601	19.407091
55.072596	1737.187999	19.412109
54.936269	1768.252878	19.417127
55.184927	1769.770466	19.422144
55.425993	1758.289976	19.427162
55.308243	1790.611915	19.432179
55.315515	1773.170829	19.437197
55.484189	1779.489395	19.442215
55.532459	1782.017349	19.447232
55.720751	1772.088381	19.452250
55.692578	1774.048085	19.457267
55.466992	1770.057140	19.462285
55.692803	1790.267231	19.467303
56.037061	1789.057716	19.472320
56.225723	1783.470174	19.477338
56.068164	1797.696357	19.482355
56.160056	1794.162859	19.487373
56.673639	1792.459159	19.492391
56.548434	1784.617216	19.497408
56.263791	1765.967433	19.502426
56.409419	1763.100191	19.507443
56.216374	1757.582968	19.512461
56.379184	1755.636339	19.517479
56.347870	1768.481716	19.522496
56.309416	1767.641541	19.527514
56.373635	1787.658750	19.532531
56.118570	1800.152876	19.537549
56.745903	1779.246671	19.542567
56.860048	1776.301077	19.547584
56.713508	1809.360669	19.552602
56.939316	1800.174450	19.557619
57.084403	1796.903025	19.562637
56.950439	1781.504191	19.567655
56.818704	1797.031849	19.572672
56.791228	1788.134563	19.577690
56.961615	1782.059159	19.582707
56.740576	1792.004305	19.587725
56.912478	1786.084385	19.592743
56.898268	1796.290703	19.597760
56.942925	1811.643958	19.602778
57.353605	1822.515559	19.607795
57.323489	1821.293384	19.612813
57.564744	1810.756627	19.617831
57.370603	1822.825784	19.622848
57.413695	1822.172374	19.627866
58.046860	1804.691215	19.632883
57.544700	1806.863361	19.637901
57.876980	1805.432388	19.642919
57.760993	1798.323562	19.647936
57.861434	1812.467719	19.652954
57.779997	1813.043811	19.657971
57.705334	1810.707186	19.662989
57.846881	1798.098959	19.668007
57.581405	1809.210508	19.673024
57.865198	1817.535193	19.678042
58.049879	1815.533160	19.683059
58.307764	1842.286641	19.688077
58.261471	1825.143468	19.693095
58.257407	1849.382596	19.698112
58.473288	1839.315476	19.703130
58.826085	1836.204400	19.708147
58.298881	1834.661948	19.713165
58.547498	1830.128183	19.718183
58.194640	1838.864288	19.723200
58.762623	1839.286484	19.728218
58.712008	1832.368562	19.733235
58.511447	1833.333308	19.738253
58.750845	1820.714176	19.743271
58.733294	1842.109871	19.748288
58.593580	1819.493370	19.753306
58.760133	1835.157543	19.758323
58.428185	1853.867927	19.763341
59.165431	1846.544364	19.768359
59.343424	1835.075444	19.773376
59.133659	1863.462392	19.778394
59.402544	1856.400701	19.783411
59.298354	1849.793333	19.788429
59.252689	1857.426545	19.793447
59.704829	1844.696389	19.798464
59.379082	1855.233997	19.803482
59.681379	1858.806833	19.808499
59.729134	1842.513799	19.813517
59.530748	1840.181170	19.818535
59.428343	1860.273813	19.823552
59.356895	1837.138315	19.828570
59.826664	1836.904498	19.833587
59.646724	1848.279286	19.838605
60.067866	1848.212097	19.843623
59.952896	1851.812146	19.848640
59.852392	1856.772118	19.853658
59.862473	1854.678374	19.858675
59.847530	1868.447732	19.863693
60.051797	1874.754372	19.868711
60.231967	1880.817894	19.873728
59.996660	1880.517189	19.878746
60.266727	1877.792101	19.883763
60.134044	1870.248604	19.888781
60.323249	1888.350540	19.893799
60.388214	1877.837128	19.898816
60.449305	1886.669271	19.903834
60.517896	1885.363711	19.908851
60.157285	1896.039041	19.913869
60.584095	1894.737703	19.918887
60.732161	1927.390363	19.923904
60.315685	1913.666088	19.928922
60.431968	1922.189006	19.933939
60.424781	1902.151443	19.938957
60.671098	1950.115971	19.943975
61.160634	1917.488937	19.948992
61.377290	1957.711106	19.954010
61.312138	1937.286337	19.959027
61.448897	1938.063591	19.964045
61.702897	1929.058413	19.969063
62.121833	1929.892916	19.974080
61.571630	1944.800053	19.979098
62.070296	1925.298416	19.984115
61.809913	1907.852660	19.989133
61.454523	1905.710223	19.994151
61.764591	1896.291858	19.999168
61.544372	1900.080161	20.004186
61.689245	1937.571954	20.009203
61.753054	1933.712566	20.014221
61.812260	1915.997186	20.019239
62.087760	1935.675741	20.024256
62.085016	1933.412571	20.029274
62.398529	1916.325171	20.034291
62.196888	1932.395801	20.039309
62.238253	1934.361741	20.044327
62.237534	1930.254669	20.049344
62.179866	1920.542573	20.054362
62.286758	1916.341266	20.059379
62.294150	1910.971345	20.064397
61.958782	1940.976660	20.069415
62.540396	1903.617483	20.074432
62.360091	1955.972715	20.079450
62.632726	1924.860467	20.084467
62.514507	1955.432077	20.089485
62.686414	1950.740621	20.094503
62.881122	1947.034961	20.099520
62.618863	1964.284048	20.104538
62.805435	1942.274421	20.109555
62.900722	1943.404354	20.114573
62.951405	1952.080895	20.119591
63.574000	1943.303219	20.124608
63.036355	1941.623994	20.129626
63.484131	1947.777004	20.134643
63.427877	1939.598367	20.139661
63.189543	1941.423294	20.144679
63.353101	1949.383412	20.149696
63.232135	1926.532520	20.154714
63.256153	1968.259357	20.159731
63.679709	1951.075717	20.164749
63.580954	1977.886321	20.169767
63.826134	1956.520132	20.174784
63.651026	1966.692453	20.179802
64.351443	1966.206350	20.184819
63.833502	1979.999395	20.189837
63.931727	1975.454961	20.194855
64.323494	1947.628593	20.199872
64.181566	1971.238678	20.204890
64.287224	1966.458680	20.209907
64.154492	1966.335097	20.214925
64.299330	1969.579140	20.219943
64.323228	1960.028617	20.224960
64.103009	1965.036030	20.229978
64.225417	1953.256558	20.234995
64.169615	1971.345758	20.240013
64.098778	1981.586405	20.245031
64.476691	1975.976476	20.250048
64.556412	1977.414062	20.255066
64.580514	2006.762866	20.260083
64.673477	1982.010588	20.265101
64.614911	1990.811539	20.270119
64.897655	1989.721931	20.275136
64.844036	1997.151991	20.280154
64.888834	1981.666236	20.285171
65.358529	2025.683280	20.290189
65.183019	2014.407444	20.295207
65.675448	2016.630230	20.300224
65.538612	2020.269988	20.305242
65.871809	2007.678208	20.310259
65.593540	1969.535762	20.315277
65.502806	1995.218834	20.320295
65.902449	1967.718360	20.325312
65.286879	1981.171472	20.330330
65.764268	1984.126535	20.335347
65.768314	2002.206230	20.340365
65.769043	2010.607627	20.345383
66.260178	2000.090661	20.350400
65.924294	1992.879952	20.355418
66.242758	2003.837183	20.360435
66.178468	1995.579571	20.365453
66.232029	2020.726871	20.370471
66.678982	1988.937027	20.375488
66.178568	1985.963550	20.380506
66.158961	1998.220524	20.385523
66.391458	1991.177155	20.390541
66.452783	1994.760138	20.395559
66.540228	2009.000941	20.400576
66.706838	2003.767618	20.405594
66.778005	1994.887509	20.410611
66.720417	1991.178025	20.415629
66.626244	2000.014547	20.420647
66.756392	1987.538535	20.425664
66.729481	2005.961372	20.430682
66.504478	2008.410246	20.435699
66.833555	1998.387887	20.440717
66.554075	2000.058934	20.445735
67.240866	2000.638370	20.450752
66.887888	2007.071682	20.455770
66.990325	2010.851034	20.460787
67.013141	2013.968254	20.465805
67.228894	2021.268855	20.470823
67.225576	2030.901018	20.475840
67.720289	2023.548405	20.480858
67.093002	2022.885484	20.485875
67.092426	2030.813618	20.490893
67.516662	2051.826140	20.495911
67.731558	2049.399257	20.500928
67.692713	2061.399802	20.505946
67.545132	2067.839713	20.510963
67.711600	2053.020323	20.515981
67.770606	2046.640099	20.520999
68.036544	2051.420579	20.526016
68.094295	2060.418530	20.531034
68.265262	2075.542709	20.536051
68.394783	2087.297775	20.541069
68.480490	2074.768999	20.546087
68.592258	2072.989345	20.551104
68.576269	2074.863775	20.556122
68.954289	2072.788405	20.561139
68.679630	2069.598011	20.566157
68.539256	2073.694527	20.571175
69.243982	2061.818962	20.576192
69.021357	2068.008143	20.581210
68.930112	2052.801983	20.586227
68.925561	2058.176161	20.591245
68.968330	2060.469085	20.596263
69.218294	2057.599306	20.601280
69.120083	2067.652468	20.606298
69.044308	2058.413505	20.611315
69.385904	2056.389563	20.616333
69.231850	2066.508259	20.621351
69.569452	2049.706300	20.626368
69.338326	2065.100655	20.631386
69.121565	2068.531372	20.636403
69.404462	2059.873864	20.641421
69.070594	2065.525503	20.646439
69.403085	2080.973144	20.651456
69.655128	2087.207765	20.656474
69.671036	2086.088341	20.661491
69.887741	2088.278028	20.666509
69.794883	2086.543587	20.671527
70.058434	2083.920175	20.676544
70.338971	2086.192492	20.681562
69.912557	2089.928781	20.686579
70.215165	2082.040479	20.691597
70.109596	2086.085829	20.696615
70.324782	2086.902497	20.701632
70.476933	2090.104503	20.706650
70.326996	2102.560101	20.711667
70.674943	2103.171554	20.716685
70.610876	2112.951886	20.721703
70.509803	2108.959868	20.726720
70.654523	2127.097511	20.731738
70.642910	2121.115483	20.736755
70.851225	2106.613412	20.741773
71.098319	2114.223670	20.746791
70.660334	2126.910841	20.751808
70.960947	2111.020782	20.756826
70.849105	2111.092068	20.761843
71.355115	2135.654608	20.766861
71.511107	2141.616703	20.771879
71.511465	2143.228984	20.776896
72.071278	2129.161629	20.781914
71.806250	2130.973531	20.786931
71.605629	2113.620243	20.791949
71.577836	2113.774083	20.796967
71.706053	2126.286021	20.801984
71.969081	2124.461791	20.807002
71.760394	2138.932416	20.812019
72.012536	2133.996870	20.817037
71.792295	2135.342303	20.822055
71.988124	2126.281785	20.827072
71.598643	2131.638719	20.832090
71.785123	2136.743361	20.837107
72.000249	2125.402001	20.842125
72.012270	2162.031510	20.847143
72.796538	2159.548424	20.852160
72.558181	2147.904974	20.857178
72.525663	2160.120099	20.862195
73.002345	2161.736652	20.867213
72.906254	2163.672632	20.872231
72.771387	2158.191595	20.877248
73.039561	2153.473712	20.882266
72.832747	2170.006330	20.887283
73.199523	2147.000235	20.892301
72.891359	2152.901067	20.897319
72.867454	2155.742620	20.902336
73.312958	2154.362775	20.907354
72.971685	2163.866444	20.912371
73.030995	2161.929975	20.917389
73.001920	2157.899720	20.922407
73.132695	2181.241715	20.927424
73.373862	2175.784080	20.932442
73.455144	2185.892073	20.937459
73.591974	2186.582814	20.942477
73.685211	2168.775181	20.947495
73.451314	2187.132152	20.952512
73.570959	2188.127658	20.957530
73.444958	2170.438356	20.962547
74.209391	2189.444680	20.967565
74.179818	2206.998301	20.972583
73.938097	2194.321857	20.977600
74.384543	2189.070586	20.982618
74.128373	2212.988722	20.987635
74.487483	2183.224394	20.992653
74.433724	2205.565508	20.997671
74.680693	2170.489596	21.002688
74.803789	2193.216201	21.007706
74.684841	2195.472013	21.012723
74.861073	2179.350025	21.017741
74.780311	2176.437005	21.022759
74.780644	2201.368161	21.027776
75.219028	2188.731138	21.032794
75.098995	2185.276957	21.037811
75.201372	2183.031593	21.042829
75.277678	2184.752892	21.047847
75.079030	2184.005879	21.052864
75.261506	2179.256035	21.057882
75.014227	2198.277407	21.062899
75.325252	2185.006307	21.067917
75.073799	2188.297863	21.072935
75.117688	2213.402994	21.077952
75.279112	2225.845228	21.082970
75.367133	2211.041333	21.087987
75.297231	2213.729780	21.093005
75.811961	2223.881942	21.098023
75.906150	2241.395420	21.103040
76.380518	2229.383418	21.108058
75.990900	2236.154586	21.113075
76.213945	2241.006466	21.118093
76.130644	2245.616182	21.123111
76.439959	2241.066319	21.128128
76.672082	2238.292160	21.133146
76.382214	2238.516107	21.138163
76.616008	2229.534415	21.143181
76.580523	2242.568070	21.148199
76.325477	2226.791659	21.153216
76.614594	2238.140720	21.158234
76.493697	2251.924192	21.163251
76.904139	2254.674480	21.168269
77.080577	2259.076038	21.173287
76.895584	2267.044721	21.178304
77.252356	2269.015469	21.183322
77.328463	2266.138765	21.188339
77.227185	2263.674174	21.193357
77.389226	2258.030921	21.198375
77.342637	2263.380417	21.203392
77.569046	2252.112666	21.208410
77.362734	2253.169592	21.213427
77.504365	2258.846156	21.218445
77.604761	2254.702418	21.223463
77.433769	2261.061202	21.228480
77.764187	2247.824707	21.233498
77.268448	2268.336146	21.238515
77.740613	2286.626272	21.243533
77.839836	2279.360193	21.248551
77.821097	2278.048074	21.253568
77.799526	2278.575310	21.258586
78.023499	2286.928685	21.263603
78.212986	2298.520201	21.268621
78.495333	2302.978818	21.273639
78.242053	2315.155341	21.278656
78.762991	2309.793047	21.283674
78.500461	2322.504320	21.288691
78.932762	2295.820732	21.293709
78.503666	2336.662890	21.298727
78.787646	2298.211265	21.303744
79.131221	2316.510923	21.308762
78.695636	2304.688007	21.313779
78.624692	2328.557919	21.318797
79.201928	2322.450450	21.323815
79.083717	2329.710077	21.328832
79.337555	2341.830927	21.333850
79.545088	2319.955816	21.338867
79.368925	2346.400336	21.343885
79.852681	2323.858239	21.348903
79.703556	2314.237542	21.353920
79.827163	2325.169461	21.358938
79.618874	2335.342610	21.363955
79.955295	2331.400320	21.368973
80.344585	2319.650355	21.373991
79.985356	2317.119919	21.379008
80.037479	2313.823877	21.384026
80.023270	2326.478252	21.389043
80.056358	2331.192135	21.394061
80.114949	2330.349037	21.399079
80.396045	2368.570575	21.404096
80.545856	2336.124195	21.409114
80.113329	2362.549847	21.414131
80.265474	2344.948115	21.419149
80.321148	2348.524222	21.424167
80.298318	2368.114082	21.429184
80.551409	2385.048675	21.434202
80.951104	2362.438123	21.439219
81.052142	2370.806430	21.444237
81.015227	2392.130516	21.449255
81.226663	2381.500573	21.454272
81.247855	2374.828925	21.459290
81.278582	2379.444096	21.464307
81.594747	2370.661548	21.469325
81.911452	2359.835505	21.474343
81.331745	2389.910594	21.479360
81.470106	2374.813779	21.484378
81.634320	2385.492296	21.489395
81.544025	2399.467661	21.494413
81.840254	2411.089439	21.499431
81.681607	2417.116763	21.504448
82.125653	2399.610783	21.509466
82.275593	2407.411300	21.514483
82.260551	2405.396989	21.519501
82.428162	2391.324282	21.524519
82.461370	2399.531957	21.529536
82.356476	2397.638944	21.534554
82.620516	2394.313811	21.539571
82.740331	2402.416439	21.544589
83.096745	2389.024656	21.549607
83.106821	2390.618111	21.554624
83.331026	2383.929817	21.559642
83.101658	2385.594487	21.564659
82.835008	2395.957888	21.569677
83.049555	2385.520934	21.574695
82.754563	2388.585089	21.579712
82.917649	2388.721079	21.584730
82.900408	2385.137198	21.589747
82.728512	2411.236652	21.594765
83.530384	2401.786734	21.599783
83.376863	2408.622583	21.604800
83.829994	2414.124478	21.609818
83.654617	2407.508542	21.614835
83.640055	2410.894510	21.619853
84.022332	2399.984048	21.624871
83.816668	2411.073931	21.629888
83.850357	2422.229480	21.634906
84.232742	2408.706119	21.639923
83.747377	2435.519438	21.644941
84.637599	2414.758391	21.649959
84.317534	2464.383291	21.654976
84.203675	2431.955145	21.659994
84.852133	2408.654389	21.665011
84.768956	2448.604040	21.670029
84.894306	2434.845566	21.675047
84.944998	2430.042720	21.680064
84.884480	2423.406888	21.685082
84.892900	2445.890259	21.690099
85.147340	2431.383656	21.695117
85.170289	2431.855034	21.700135
85.032272	2436.028355	21.705152
85.159719	2420.318160	21.710170
85.145528	2419.465427	21.715187
84.555816	2457.325031	21.720205
85.190985	2448.033804	21.725223
85.206803	2450.729863	21.730240
85.438158	2465.074800	21.735258
85.557006	2458.717101	21.740275
85.587591	2459.872337	21.745293
85.632023	2480.486709	21.750311
85.463070	2498.446738	21.755328
85.704018	2487.227613	21.760346
85.863049	2470.230268	21.765363
85.718301	2496.856461	21.770381
86.185670	2480.796260	21.775399
85.895186	2519.910036	21.780416
86.453649	2499.403912	21.785434
86.649151	2498.224357	21.790451
87.020981	2503.156424	21.795469
87.193845	2500.740891	21.800487
87.198574	2501.857780	21.805504
87.041192	2501.056976	21.810522
87.033026	2507.005285	21.815539
87.311424	2505.223392	21.820557
87.180969	2500.387271	21.825575
87.075823	2503.771975	21.830592
86.933101	2504.041676	21.835610
87.370477	2497.895087	21.840627
87.526141	2495.806351	21.845645
87.661088	2480.990766	21.850663
87.673600	2508.303722	21.855680
87.904109	2483.496409	21.860698
87.996768	2484.961085	21.865715
87.416421	2492.682248	21.870733
87.950084	2486.477837	21.875751
87.850841	2511.553609	21.880768
88.078621	2516.615621	21.885786
88.077839	2528.534187	21.890803
87.992182	2517.094188	21.895821
88.306034	2520.419163	21.900839
88.203008	2525.490666	21.905856
87.906111	2524.071075	21.910874
88.533311	2546.485035	21.915891
88.388097	2555.432284	21.920909
88.659792	2549.103659	21.925927
88.718438	2549.408893	21.930944
88.643194	2550.377297	21.935962
89.021801	2546.274848	21.940979
88.702043	2561.108109	21.945997
89.102004	2567.542731	21.951015
89.592260	2575.647739	21.956032
89.488216	2570.005894	21.961050
89.894488	2561.980464	21.966067
89.764427	2560.220436	21.971085
89.654633	2562.065054	21.976103
90.149362	2564.621060	21.981120
89.962595	2566.670655	21.986138
89.947708	2566.872780	21.991155
89.600465	2571.877058	21.996173
90.049928	2551.106659	22.001191
89.767844	2559.097274	22.006208
90.149805	2584.231727	22.011226
90.415941	2581.431631	22.016243
90.129323	2582.811283	22.021261
90.602956	2580.569584	22.026279
90.476689	2587.764554	22.031296
90.512746	2592.884692	22.036314
90.625443	2584.825048	22.041331
90.697751	2591.392942	22.046349
91.058982	2597.695322	22.051367
91.032093	2617.307402	22.056384
91.199462	2620.773739	22.061402
91.311664	2615.914618	22.066419
91.202816	2622.452421	22.071437
91.188858	2620.020251	22.076455
91.496485	2618.082668	22.081472
91.081047	2612.436188	22.086490
91.785197	2610.195481	22.091507
91.903538	2620.547204	22.096525
92.056633	2606.427052	22.101543
91.975884	2610.830401	22.106560
91.669284	2606.941018	22.111578
92.155623	2623.446998	22.116595
91.698420	2633.282502	22.121613
91.936333	2627.904660	22.126631
92.236851	2633.065231	22.131648
92.402960	2633.541318	22.136666
92.576232	2630.516910	22.141683
92.701132	2632.156579	22.146701
92.886714	2628.865928	22.151719
93.016698	2633.831885	22.156736
93.276854	2647.452719	22.161754
93.260445	2627.900926	22.166771
93.210396	2626.230382	22.171789
92.959006	2626.920911	22.176807
93.445808	2635.380450	22.181824
93.195679	2643.963792	22.186842
93.359507	2663.829468	22.191859
93.235746	2662.322478	22.196877
93.126630	2641.077063	22.201895
93.433419	2645.317164	22.206912
92.968074	2673.611158	22.211930
93.658036	2684.305169	22.216947
93.675031	2677.866870	22.221965
93.670838	2687.600287	22.226983
94.151072	2697.435801	22.232000
94.144297	2717.208410	22.237018
94.561554	2701.140228	22.242035
94.572437	2716.218240	22.247053
94.637237	2713.331454	22.252071
94.949740	2712.596506	22.257088
94.620386	2711.309493	22.262106
95.093690	2702.238196	22.267123
95.099734	2701.363342	22.272141
94.842761	2706.831494	22.277159
94.906973	2701.158837	22.282176
94.694279	2699.588155	22.287194
95.193531	2712.477973	22.292211
94.994477	2733.134674	22.297229
95.275116	2732.884604	22.302247
95.354559	2727.420304	22.307264
95.234284	2737.784202	22.312282
95.479990	2725.512514	22.317299
95.728732	2731.924130	22.322317
96.045804	2758.585707	22.327335
96.451300	2751.768447	22.332352
96.463349	2740.568322	22.337370
96.206971	2727.973974	22.342387
96.241447	2720.787216	22.347405
96.319469	2727.279538	22.352423
96.630134	2742.817890	22.357440
96.740463	2749.383726	22.362458
96.552495	2745.885971	22.367475
96.852162	2749.900710	22.372493
96.418648	2749.554503	22.377511
96.533489	2750.508341	22.382528
96.639019	2752.089762	22.387546
96.997765	2741.349548	22.392563
96.909691	2766.651292	22.397581
96.814541	2772.036247	22.402599
97.221369	2769.330093	22.407616
97.234615	2774.700911	22.412634
97.225866	2791.337939	22.417651
97.449161	2792.191899	22.422669
97.559419	2801.318012	22.427687
97.749124	2802.819159	22.432704
97.785373	2808.877706	22.437722
98.076401	2805.151754	22.442739
97.994500	2802.716229	22.447757
98.188130	2810.527301	22.452775
98.402848	2810.898110	22.457792
98.616670	2823.658138	22.462810
98.826156	2808.672237	22.467827
98.974611	2818.751084	22.472845
98.824722	2831.087739	22.477863
98.960385	2811.525609	22.482880
99.021719	2837.179627	22.487898
99.163860	2812.705974	22.492915
99.367795	2815.936068	22.497933
99.398451	2816.989069	22.502951
99.599655	2818.228820	22.507968
99.200606	2815.898922	22.512986
99.357799	2812.739393	22.518003
99.536935	2811.874687	22.523021
99.529689	2816.429982	22.528039
99.430635	2814.244955	22.533056
99.308818	2820.813231	22.538074
99.619867	2827.201583	22.543091
99.643286	2846.573129	22.548109
99.763969	2850.936566	22.553127
99.888208	2843.783415	22.558144
99.829218	2869.135759	22.563162
100.228335	2870.774993	22.568179
100.162388	2871.128417	22.573197
100.311815	2877.286144	22.578215
100.653507	2889.949545	22.583232
100.646862	2903.397643	22.588250
100.996259	2901.937100	22.593267
100.932852	2910.696118	22.598285
100.990862	2909.521937	22.603303
101.326695	2897.975103	22.608320
101.144792	2908.562894	22.613338
101.049350	2909.482628	22.618355
101.432925	2905.262878	22.623373
101.338757	2926.312926	22.628391
101.825105	2922.026444	22.633408
101.934425	2932.578829	22.638426
102.192189	2925.339849	22.643443
102.376104	2918.466602	22.648461
102.154801	2929.921978	22.653479
102.674567	2917.902178	22.658496
102.220700	2912.822526	22.663514
102.066602	2909.469563	22.668531
102.420052	2916.581125	22.673549
102.986735	2914.365443	22.678567
102.724788	2907.737910	22.683584
102.524739	2906.597798	22.688602
102.729904	2912.876435	22.693619
103.111342	2906.997377	22.698637
103.043014	2920.760513	22.703655
103.412109	2927.456641	22.708672
103.317809	2942.577615	22.713690
103.269276	2947.182008	22.718707
103.431642	2941.095605	22.723725
103.144596	2932.049444	22.728743
103.846627	2930.669534	22.733760
103.438013	2946.486398	22.738778
103.879877	2933.624011	22.743795
103.885715	2947.770202	22.748813
103.847956	2955.659936	22.753831
104.226386	2967.826731	22.758848
104.251194	2966.710540	22.763866
104.031571	2956.005757	22.768883
104.361863	2950.414854	22.773901
104.246438	2968.126237	22.778919
104.654917	2988.691934	22.783936
104.877241	2982.459092	22.788954
104.962709	2977.678051	22.793971
105.169974	2988.133056	22.798989
104.784292	2996.164023	22.804007
105.009518	2969.599535	22.809024
105.363311	2976.203737	22.814042
104.857457	2988.597283	22.819059
105.471938	2996.094370	22.824077
105.364539	3006.546074	22.829095
105.605175	3004.435067	22.834112
105.630331	3000.340871	22.839130
105.697773	3005.714931	22.844147
106.327413	3027.018616	22.849165
106.236347	3029.882846	22.854183
106.665084	3027.118881	22.859200
106.645188	3027.553062	22.864218
106.267114	3022.823107	22.869235
106.834594	3015.749433	22.874253
106.561149	3041.237738	22.879271
106.819582	3031.774966	22.884288
106.527000	3038.459449	22.889306
106.573781	3026.113040	22.894323
107.014647	3018.456255	22.899341
106.532947	3031.011164	22.904359
106.835622	3037.857943	22.909376
106.892298	3059.544851	22.914394
106.923960	3051.722043	22.919411
107.426774	3054.386185	22.924429
107.119264	3053.046101	22.929447
107.337179	3079.235618	22.934464
107.635929	3092.032681	22.939482
107.456956	3100.620676	22.944499
107.781553	3092.640231	22.949517
108.239897	3109.985000	22.954535
108.654662	3118.594748	22.959552
108.856447	3111.623386	22.964570
108.896721	3107.912170	22.969587
109.025537	3104.868010	22.974605
108.961584	3097.290103	22.979623
109.122687	3102.932432	22.984640
109.151879	3092.724318	22.989658
109.237097	3090.779663	22.994675
109.470988	3095.221085	22.999693
109.418994	3094.035326	23.004711
109.486566	3094.313980	23.009728
109.505596	3108.082242	23.014746
109.318754	3106.526269	23.019763
109.449189	3101.030102	23.024781
109.505726	3100.869248	23.029799
109.672940	3097.252635	23.034816
110.107274	3109.313887	23.039834
109.824073	3129.963328	23.044851
109.893455	3126.274210	23.049869
109.960614	3125.951987	23.054887
109.748640	3141.637813	23.059904
110.303354	3144.124584	23.064922
110.497391	3152.572902	23.069939
110.935567	3153.914910	23.074957
110.830733	3151.895149	23.079975
110.783513	3159.408945	23.084992
110.801815	3150.993562	23.090010
110.977895	3158.461527	23.095027
111.552606	3169.879053	23.100045
111.347516	3183.709864	23.105063
111.243841	3186.062500	23.110080
111.584273	3174.940254	23.115098
111.409487	3190.657959	23.120115
111.566493	3184.127893	23.125133
111.936001	3187.784740	23.130151
112.144007	3187.329938	23.135168
112.545365	3183.180426	23.140186
111.921515	3185.557794	23.145203
112.429921	3183.455195	23.150221
112.639248	3196.933628	23.155239
112.541351	3197.883662	23.160256
112.917649	3187.579235	23.165274
112.768943	3198.099016	23.170291
112.968698	3190.536433	23.175309
112.741773	3192.098546	23.180327
112.994354	3193.971200	23.185344
113.146646	3186.006380	23.190362
113.156443	3192.929035	23.195379
113.268093	3198.739748	23.200397
113.219002	3215.216938	23.205415
113.236467	3221.552381	23.210432
113.443810	3225.781767	23.215450
113.591622	3223.380337	23.220467
113.799800	3242.278532	23.225485
114.093155	3252.241760	23.230503
114.303050	3247.703511	23.235520
114.502412	3241.965046	23.240538
114.393172	3252.744438	23.245555
114.568377	3243.160295	23.250573
114.612477	3243.459999	23.255591
114.418868	3242.340069	23.260608
114.681575	3261.970555	23.265626
114.845609	3276.666834	23.270643
114.949412	3263.727488	23.275661
115.345275	3267.916603	23.280679
115.212231	3274.312250	23.285696
115.512559	3274.941581	23.290714
115.308490	3271.281868	23.295731
115.619898	3272.283846	23.300749
115.835883	3279.358513	23.305767
115.845390	3281.818184	23.310784
116.040975	3276.903074	23.315802
116.013802	3277.329771	23.320819
116.132641	3279.606827	23.325837
116.215224	3282.887052	23.330855
115.904370	3280.451768	23.335872
116.395975	3317.312915	23.340890
116.390565	3315.407851	23.345907
116.421792	3316.827346	23.350925
116.555415	3316.316754	23.355943
116.497002	3329.755408	23.360960
116.866432	3348.261481	23.365978
116.814010	3341.591689	23.370995
117.088442	3341.013023	23.376013
116.955942	3374.774777	23.381031
117.489988	3364.496990	23.386048
118.029443	3360.736010	23.391066
117.608100	3363.905460	23.396083
117.826577	3357.404846	23.401101
118.017887	3377.357573	23.406119
118.117737	3386.346487	23.411136
118.409448	3381.655139	23.416154
118.915167	3387.339383	23.421171
118.736031	3392.473663	23.426189
118.824502	3378.253733	23.431207
118.741577	3383.478859	23.436224
118.688983	3374.616070	23.441242
118.873344	3384.261681	23.446259
118.650601	3395.406161	23.451277
119.208400	3372.438475	23.456295
118.950613	3380.294301	23.461312
119.088209	3397.058138	23.466330
119.593385	3412.150090	23.471347
119.590377	3399.251252	23.476365
119.379134	3408.903321	23.481383
119.508702	3414.542147	23.486400
119.921799	3391.415015	23.491418
119.844441	3422.524363	23.496435
120.022061	3433.806404	23.501453
120.636513	3431.651467	23.506471
120.397734	3443.799084	23.511488
120.485715	3435.226908	23.516506
120.409719	3439.757175	23.521523
120.468859	3441.786561	23.526541
120.926554	3461.411398	23.531559
120.896425	3462.636962	23.536576
121.092201	3457.444095	23.541594
121.127367	3455.348480	23.546611
120.854764	3477.067272	23.551629
121.459666	3474.677874	23.556647
121.403237	3482.657395	23.561664
121.566142	3478.239050	23.566682
121.722942	3481.845722	23.571699
121.876970	3487.200649	23.576717
122.282287	3500.386965	23.581735
122.115364	3506.622930	23.586752
122.668231	3507.085366	23.591770
122.848739	3516.449292	23.596787
122.681372	3502.518597	23.601805
122.749074	3513.641241	23.606823
122.555002	3515.656734	23.611840
122.960141	3505.827311	23.616858
122.869198	3509.712616	23.621875
122.715344	3526.789727	23.626893
123.256616	3535.018507	23.631911
123.326812	3538.686197	23.636928
123.477106	3536.218247	23.641946
123.504816	3534.388106	23.646963
123.504421	3544.497483	23.651981
124.193004	3552.628059	23.656999
123.961209	3563.989637	23.662016
124.316157	3557.891153	23.667034
124.319515	3562.314414	23.672051
124.307761	3562.666293	23.677069
124.500650	3554.499724	23.682087
124.688951	3558.189492	23.687104
124.885022	3548.881065	23.692122
124.928084	3550.758856	23.697139
124.740390	3559.040162	23.702157
125.254401	3574.263810	23.707175
124.973265	3584.382579	23.712192
125.313483	3580.993909	23.717210
125.439676	3573.367344	23.722227
125.686555	3577.788754	23.727245
125.634781	3578.712579	23.732263
125.826586	3574.643567	23.737280
125.965612	3574.542710	23.742298
126.116664	3579.510352	23.747315
125.915319	3598.667022	23.752333
126.407511	3594.246483	23.757351
126.550587	3599.042352	23.762368
126.421007	3601.399971	23.767386
126.339088	3607.544552	23.772403
126.556746	3607.210123	23.777421
126.786389	3630.394734	23.782439
126.845461	3633.758234	23.787456
126.880164	3627.463787	23.792474
127.082794	3630.286814	23.797491
127.300403	3655.771049	23.802509
127.682691	3654.844016	23.807527
127.914643	3665.952388	23.812544
127.683662	3658.909751	23.817562
128.243294	3668.772603	23.822579
128.426100	3658.730747	23.827597
128.217851	3657.697285	23.832615
128.316039	3674.119259	23.837632
128.063794	3651.485595	23.842650
128.606192	3656.817207	23.847667
128.311247	3674.362990	23.852685
128.679299	3670.492393	23.857703
128.510839	3680.269968	23.862720
128.815314	3682.017997	23.867738
129.095729	3695.702662	23.872755
129.233054	3705.540052	23.877773
129.596578	3707.309347	23.882791
129.480213	3711.703759	23.887808
129.518914	3696.901500	23.892826
129.891570	3708.125127	23.897843
129.571660	3723.039818	23.902861
129.845612	3726.907119	23.907879
129.615217	3728.777403	23.912896
130.000703	3735.273856	23.917914
130.227641	3745.404548	23.922931
130.416223	3748.682138	23.927949
130.530425	3758.004875	23.932967
130.616054	3759.135707	23.937984
130.757370	3770.282994	23.943002
131.226930	3781.793286	23.948019
131.362802	3782.803624	23.953037
131.947883	3773.745317	23.958055
131.806490	3779.282750	23.963072
131.971484	3775.395732	23.968090
131.862908	3771.664817	23.973107
131.620516	3776.995742	23.978125
132.288312	3773.783704	23.983143
131.999281	3771.322830	23.988160
131.955219	3765.461719	23.993178
132.442220	3753.004391	23.998195
132.145411	3770.909280	24.003213
132.413772	3775.901550	24.008231
132.546594	3792.566705	24.013248
132.552584	3796.678906	24.018266
132.750193	3793.638582	24.023283
132.804745	3801.403143	24.028301
133.124846	3812.588820	24.033319
132.975163	3824.554998	24.038336
133.403392	3827.600103	24.043354
133.601762	3830.763665	24.048371
133.536081	3836.816866	24.053389
134.090765	3840.730685	24.058407
133.897498	3847.629390	24.063424
134.289235	3848.351942	24.068442
134.788214	3838.599371	24.073459
134.337133	3851.193358	24.078477
134.744945	3854.531198	24.083495
134.527659	3852.463191	24.088512
134.877875	3848.674054	24.093530
135.146388	3857.121136	24.098547
135.115058	3868.744395	24.103565
135.041566	3870.694300	24.108583
135.257555	3874.135884	24.113600
135.383711	3866.581543	24.118618
135.404882	3870.984752	24.123635
135.140821	3891.975963	24.128653
135.694083	3895.602910	24.133671
135.418196	3897.734545	24.138688
135.734695	3909.484088	24.143706
136.189123	3924.335309	24.148723
136.095883	3926.783152	24.153741
136.495099	3932.121178	24.158759
136.657063	3942.641517	24.163776
136.805491	3957.735854	24.168794
137.146050	3955.102987	24.173811
136.636937	3974.700166	24.178829
136.830438	3965.634165	24.183847
136.992560	3968.560471	24.188864
137.252257	3978.113443	24.193882
137.850453	3984.775898	24.198899
137.752944	3990.013004	24.203917
137.871323	3978.308059	24.208935
138.348241	3977.483127	24.213952
138.004117	3987.373082	24.218970
138.178745	4015.487393	24.223987
138.199094	4015.008211	24.229005
138.662991	4009.395610	24.234023
139.093390	4014.084451	24.239040
138.967300	4014.813270	24.244058
139.259826	4001.601690	24.249075
139.059417	4013.181225	24.254093
139.144419	4007.914577	24.259111
139.262148	4009.454075	24.264128
139.161736	4030.122049	24.269146
139.457563	4033.977292	24.274163
139.631855	4041.763008	24.279181
139.586318	4041.808781	24.284199
139.679339	4039.103665	24.289216
139.567258	4056.609736	24.294234
140.217323	4059.482651	24.299251
139.711819	4066.238516	24.304269
139.836391	4077.026860	24.309287
140.493494	4075.368478	24.314304
140.604185	4083.895918	24.319322
140.926404	4091.903503	24.324339
141.010166	4115.488938	24.329357
141.533522	4104.393466	24.334375
141.477521	4109.259788	24.339392
141.568080	4117.642571	24.344410
142.054016	4114.209311	24.349427
142.021907	4102.491287	24.354445
142.255178	4112.868228	24.359463
142.162406	4106.019661	24.364480
142.296034	4094.508849	24.369498
142.721740	4112.456286	24.374515
142.614975	4129.259137	24.379533
142.546917	4124.195416	24.384551
142.779962	4121.430989	24.389568
142.594137	4140.327877	24.394586
142.966853	4114.741536	24.399603
143.045413	4141.306803	24.404621
142.940957	4147.255399	24.409639
143.050953	4147.032521	24.414656
143.318030	4156.457000	24.419674
143.975151	4162.153601	24.424691
143.416457	4183.274799	24.429709
144.012111	4187.702934	24.434727
144.366948	4173.273787	24.439744
143.846583	4193.938935	24.444762
144.811027	4198.651249	24.449779
145.021168	4195.041684	24.454797
144.752494	4205.829888	24.459815
144.985230	4212.122001	24.464832
145.052940	4202.410417	24.469850
145.197884	4198.278696	24.474867
144.911452	4211.452446	24.479885
145.512800	4228.106330	24.484903
145.785393	4218.145747	24.489920
145.481800	4235.251489	24.494938
145.556542	4228.372224	24.499955
145.789544	4251.425920	24.504973
146.097090	4258.391285	24.509991
146.496662	4266.915253	24.515008
146.153451	4264.353589	24.520026
146.536935	4260.474088	24.525043
146.588729	4268.749076	24.530061
146.737690	4281.826728	24.535079
146.912579	4278.915790	24.540096
146.945001	4278.536151	24.545114
147.492390	4286.234195	24.550131
147.424285	4291.045870	24.555149
147.286132	4295.326720	24.560167
147.810553	4303.498844	24.565184
147.722729	4313.667530	24.570202
147.599778	4310.852842	24.575219
147.974549	4318.954437	24.580237
147.749141	4321.802577	24.585255
148.367417	4328.766421	24.590272
148.259231	4339.135031	24.595290
148.580107	4343.075254	24.600307
149.049882	4360.490495	24.605325
149.006178	4358.981574	24.610343
149.486665	4356.489951	24.615360
149.317084	4363.022478	24.620378
149.594861	4359.931500	24.625395
149.531498	4368.591479	24.630413
149.775857	4371.998767	24.635431
150.392134	4372.197834	24.640448
150.062952	4385.146495	24.645466
150.134134	4378.761739	24.650483
150.575009	4372.539879	24.655501
150.183136	4371.355497	24.660519
150.516145	4394.928391	24.665536
150.762258	4406.715518	24.670554
151.078782	4408.676472	24.675571
151.162423	4416.517745	24.680589
150.950697	4419.470706	24.685607
151.603537	4414.548398	24.690624
151.614654	4439.095416	24.695642
151.565197	4434.039634	24.700659
152.205260	4428.864485	24.705677
151.996342	4442.271516	24.710695
152.347844	4429.249173	24.715712
152.426956	4429.241249	24.720730
152.425669	4433.347709	24.725747
152.592663	4457.123380	24.730765
152.588621	4466.629831	24.735783
152.907555	4450.233227	24.740800
153.000824	4472.914653	24.745818
153.199141	4467.623482	24.750835
153.875257	4480.173600	24.755853
153.763878	4483.112148	24.760871
153.753722	4488.395290	24.765888
153.770331	4486.230116	24.770906
154.085334	4484.377654	24.775923
154.037283	4477.189818	24.780941
153.857624	4480.592361	24.785959
154.310664	4489.062311	24.790976
154.301991	4505.585641	24.795994
154.647084	4505.961676	24.801011
154.572549	4504.570146	24.806029
154.551290	4520.545632	24.811047
155.054260	4537.969954	24.816064
154.956977	4542.845361	24.821082
155.159832	4546.620380	24.826099
155.602926	4538.289873	24.831117
155.399574	4583.716796	24.836135
155.828133	4544.687924	24.841152
155.679998	4582.471594	24.846170
156.183203	4560.309217	24.851187
156.249655	4568.452240	24.856205
156.792139	4579.965702	24.861223
156.735093	4586.405655	24.866240
156.807385	4589.378661	24.871258
156.933016	4583.875628	24.876275
157.447930	4581.989710	24.881293
157.182093	4592.119316	24.886311
157.702748	4591.346383	24.891328
157.749225	4602.780036	24.896346
157.683752	4608.499980	24.901363
157.900961	4612.604696	24.906381
157.695610	4613.237621	24.911399
158.132531	4615.498791	24.916416
158.155129	4639.816971	24.921434
158.162956	4641.149861	24.926451
158.878766	4641.416453	24.931469
158.530921	4638.470784	24.936487
158.717247	4642.775523	24.941504
158.922591	4666.086012	24.946522
158.941473	4667.834857	24.951539
159.628777	4674.514895	24.956557
159.293586	4680.594104	24.961575
159.782889	4691.777870	24.966592
159.748381	4689.817480	24.971610
159.885166	4695.619278	24.976627
160.330121	4713.919958	24.981645
160.001700	4724.452175	24.986663
160.456450	4711.973225	24.991680
160.381587	4719.657426	24.996698
160.917807	4733.330605	25.001715
161.004339	4728.219215	25.006733
161.341848	4732.756330	25.011751
161.952325	4720.983354	25.016768
161.888547	4724.131480	25.021786
161.976707	4721.460054	25.026803
162.393180	4719.165018	25.031821
162.144059	4714.988204	25.036839
162.293774	4711.013698	25.041856
162.692529	4730.661447	25.046874
162.599527	4744.982467	25.051891
162.910343	4744.601699	25.056909
163.024711	4750.040509	25.061927
163.199698	4749.465850	25.066944
163.433524	4749.252329	25.071962
163.241441	4742.030685	25.076979
163.384184	4738.811692	25.081997
163.325924	4748.313595	25.087015
163.300979	4733.087774	25.092032
163.851937	4753.877908	25.097050
163.817104	4763.442953	25.102067
164.071466	4767.673950	25.107085
163.828596	4768.736087	25.112103
164.328523	4778.564380	25.117120
164.214988	4795.791511	25.122138
164.387705	4794.979640	25.127155
164.706474	4809.531649	25.132173
164.739820	4831.056559	25.137191
164.825687	4831.860971	25.142208
165.378717	4847.069511	25.147226
165.369260	4861.101991	25.152243
165.850787	4864.484959	25.157261
165.782480	4869.587922	25.162279
165.842358	4876.663869	25.167296
165.876642	4896.768001	25.172314
166.023840	4885.576942	25.177331
166.455154	4891.471104	25.182349
166.352230	4924.500895	25.187367
166.243206	4912.818872	25.192384
167.158824	4915.741674	25.197402
166.965981	4930.508313	25.202419
167.382022	4939.928433	25.207437
167.400092	4946.587849	25.212455
167.732021	4953.474142	25.217472
168.090700	4963.975657	25.222490
168.114635	4967.879218	25.227507
168.423284	4965.897911	25.232525
168.193809	4966.269586	25.237543
168.706113	4974.539212	25.242560
169.113307	4971.621785	25.247578
169.213738	4983.472724	25.252595
169.272112	4981.792490	25.257613
169.318411	4987.372827	25.262631
169.340464	4985.545769	25.267648
169.759663	5000.002502	25.272666
169.694732	5011.024709	25.277683
170.310024	5018.991592	25.282701
170.530523	5014.466061	25.287719
170.421277	5019.055608	25.292736
170.707764	5007.743129	25.297754
170.309777	5012.051449	25.302771
170.253371	5023.644220	25.307789
170.643817	5036.300151	25.312807
170.819110	5037.730674	25.317824
170.848065	5068.363999	25.322842
170.767174	5082.721177	25.327859
171.237789	5085.499408	25.332877
171.316080	5107.600486	25.337895
171.654181	5107.602409	25.342912
171.817083	5110.641318	25.347930
171.960892	5130.346769	25.352947
172.397267	5135.960952	25.357965
172.571294	5136.860676	25.362983
172.510753	5135.097114	25.368000
173.100807	5142.083161	25.373018
172.640388	5162.494661	25.378035
173.569150	5163.963989	25.383053
173.332088	5169.687118	25.388071
173.334767	5172.688648	25.393088
173.989583	5172.301806	25.398106
174.070202	5182.294768	25.403123
174.190114	5192.839233	25.408141
174.564917	5191.199786	25.413159
174.666287	5186.919759	25.418176
174.590257	5187.775962	25.423194
174.270181	5207.683698	25.428211
174.575887	5212.636685	25.433229
174.806700	5213.339344	25.438247
175.142486	5230.353749	25.443264
175.486557	5243.400370	25.448282
175.579029	5242.790860	25.453299
175.733555	5243.812490	25.458317
175.735819	5257.255037	25.463335
175.882899	5264.653186	25.468352
176.501507	5262.737284	25.473370
176.181052	5273.400784	25.478387
176.673380	5288.685545	25.483405
176.969504	5293.448134	25.488423
177.157697	5297.419213	25.493440
177.811481	5290.041211	25.498458
177.899830	5293.230501	25.503475
178.076433	5286.558712	25.508493
178.197940	5282.429638	25.513511
178.092684	5285.870064	25.518528
178.257253	5290.075408	25.523546
178.160152	5309.364010	25.528563
178.641986	5296.412958	25.533581
178.706588	5297.566931	25.538599
178.616735	5310.779551	25.543616
178.999608	5309.196234	25.548634
178.909308	5332.897912	25.553651
179.208244	5339.539479	25.558669
179.261972	5344.905574	25.563687
179.261249	5367.779587	25.568704
179.504234	5363.543802	25.573722
179.409130	5383.485926	25.578739
179.780273	5399.679089	25.583757
180.083287	5398.919578	25.588775
180.170829	5421.727681	25.593792
180.599217	5424.769962	25.598810
180.921984	5434.553779	25.603827
181.269031	5449.245883	25.608845
181.359004	5459.789806	25.613863
181.958194	5462.807226	25.618880
182.137508	5448.356042	25.623898
181.927035	5448.107139	25.628915
182.115705	5450.141330	25.633933
182.179691	5453.456478	25.638951
182.144545	5462.264435	25.643968
182.557906	5466.010070	25.648986
182.510737	5480.768983	25.654003
182.428409	5491.161028	25.659021
182.442760	5501.007431	25.664039
182.745067	5511.138350	25.669056
183.072360	5525.109913	25.674074
182.797957	5534.651500	25.679092
183.039979	5545.373428	25.684109
183.356953	5552.906700	25.689127
183.453520	5574.310119	25.694144
183.851147	5576.148169	25.699162
184.316171	5591.149664	25.704180
184.446093	5596.354230	25.709197
184.736152	5587.033470	25.714215
184.960481	5628.248705	25.719232
185.513210	5629.331184	25.724250
185.310545	5629.507428	25.729268
185.312309	5628.991035	25.734285
185.786776	5638.278780	25.739303
185.748722	5655.169972	25.744320
186.163990	5640.101181	25.749338
186.241340	5656.284032	25.754356
186.479798	5672.417617	25.759373
186.630844	5678.732828	25.764391
187.021894	5677.060059	25.769408
187.522745	5668.457741	25.774426
187.102427	5685.672667	25.779444
187.103547	5691.038621	25.784461
187.560749	5704.420066	25.789479
187.832887	5713.678750	25.794496
188.081130	5716.217206	25.799514
188.207280	5729.595592	25.804532
188.538485	5736.434382	25.809549
188.437899	5734.013143	25.814567
188.733927	5737.736645	25.819584
189.093406	5749.569721	25.824602
189.081342	5755.287888	25.829620
188.695160	5767.379882	25.834637
189.444035	5763.182920	25.839655
189.579158	5778.911415	25.844672
189.389855	5777.228091	25.849690
189.706388	5789.132556	25.854708
190.225367	5799.683071	25.859725
190.591930	5805.694923	25.864743
190.585023	5812.185635	25.869760
190.930273	5812.471216	25.874778
191.046576	5823.602815	25.879796
190.791261	5828.726479	25.884813
191.522292	5836.868111	25.889831
191.644939	5837.162430	25.894848
191.765766	5838.987996	25.899866
191.996371	5858.450078	25.904884
192.185660	5853.436780	25.909901
192.136687	5862.339226	25.914919
191.877051	5872.780259	25.919936
192.173547	5868.448475	25.924954
192.812179	5884.142447	25.929972
192.514761	5895.409284	25.934989
193.162505	5897.300338	25.940007
193.193236	5922.803361	25.945024
193.257690	5922.966134	25.950042
193.744568	5925.759248	25.955060
193.936586	5943.596713	25.960077
194.086249	5943.434360	25.965095
194.149672	5958.651304	25.970112
194.806047	5962.196264	25.975130
194.732749	5965.026760	25.980148
194.741902	5974.165466	25.985165
195.036545	5982.463286	25.990183
195.072925	5983.464467	25.995200
195.155279	5984.717153	26.000218
195.338716	6006.972754	26.005236
195.445378	6016.775677	26.010253
196.000004	6026.090229	26.015271
196.066637	6040.124290	26.020288
196.169538	6038.454147	26.025306
196.306292	6067.667263	26.030324
196.396151	6071.042151	26.035341
196.891154	6081.166350	26.040359
196.880560	6093.242006	26.045376
197.223894	6100.135678	26.050394
197.524745	6113.754053	26.055412
197.603772	6116.370692	26.060429
197.831800	6121.357615	26.065447
197.832082	6161.108178	26.070464
198.325842	6155.954195	26.075482
198.757569	6156.482476	26.080500
198.912594	6172.736120	26.085517
199.136805	6198.227657	26.090535
199.157422	6181.411729	26.095552
199.334384	6195.090052	26.100570
199.684658	6201.291909	26.105588
199.503323	6192.419616	26.110605
200.084629	6205.490643	26.115623
200.150484	6210.896818	26.120640
200.309941	6225.341885	26.125658
200.331987	6249.290682	26.130676
200.556867	6245.562623	26.135693
200.854019	6253.758707	26.140711
201.011935	6259.502686	26.145728
200.871209	6276.182011	26.150746
201.429343	6292.482459	26.155764
201.717240	6295.079996	26.160781
201.967430	6281.218561	26.165799
202.171167	6309.528524	26.170816
202.607593	6312.769548	26.175834
203.182533	6302.391961	26.180852
202.693960	6313.786355	26.185869
202.877938	6321.747972	26.190887
202.880486	6326.177702	26.195904
203.561641	6330.267168	26.200922
203.612643	6343.460617	26.205940
203.508134	6343.286066	26.210957
203.690396	6346.490512	26.215975
203.746342	6368.138370	26.220992
203.896741	6373.011874	26.226010
204.479196	6373.334398	26.231028
204.390113	6397.622145	26.236045
204.737757	6416.415664	26.241063
204.889733	6405.408368	26.246080
205.034352	6426.400188	26.251098
205.021151	6432.614452	26.256116
205.071810	6454.913923	26.261133
205.490199	6463.420448	26.266151
205.579204	6471.778075	26.271168
205.957490	6479.720606	26.276186
206.515044	6489.573915	26.281204
206.398964	6526.553390	26.286221
206.765414	6519.313430	26.291239
207.172578	6519.078555	26.296256
207.367533	6536.177505	26.301274
207.735005	6550.699090	26.306292
207.821763	6548.970884	26.311309
208.173690	6549.024113	26.316327
208.400426	6560.903394	26.321344
208.487408	6574.782875	26.326362
208.847350	6568.827133	26.331380
208.455430	6595.656717	26.336397
209.070530	6590.705898	26.341415
209.194421	6608.766666	26.346432
209.546331	6603.945127	26.351450
209.802644	6599.226945	26.356468
209.285427	6638.037706	26.361485
210.004193	6640.391175	26.366503
210.304951	6628.437124	26.371520
210.659550	6658.797615	26.376538
211.111027	6652.770602	26.381556
210.962033	6653.749452	26.386573
211.080673	6649.103553	26.391591
211.031589	6679.019398	26.396608
211.120660	6667.656089	26.401626
211.578841	6677.233476	26.406644
211.290027	6707.292231	26.411661
212.041547	6717.687542	26.416679
211.997726	6708.962959	26.421696
212.206398	6735.955906	26.426714
213.068137	6741.278681	26.431732
213.309229	6751.046501	26.436749
213.562445	6765.750947	26.441767
213.823661	6764.655793	26.446784
213.850308	6759.558756	26.451802
213.858412	6761.704527	26.456820
213.815626	6772.262683	26.461837
213.934240	6771.339746	26.466855
214.163723	6793.792967	26.471872
214.345484	6803.914099	26.476890
214.478760	6790.590096	26.481908
214.501274	6828.555299	26.486925
214.658687	6843.673988	26.491943
214.821769	6857.563634	26.496960
215.209568	6863.401022	26.501978
215.248171	6876.988737	26.506996
215.544542	6899.914537	26.512013
215.969246	6898.905036	26.517031
216.266496	6927.862170	26.522048
216.632575	6929.813217	26.527066
217.179232	6942.756675	26.532084
217.191078	6949.045841	26.537101
217.202384	6947.566436	26.542119
217.506268	6960.341685	26.547136
217.640049	6978.152705	26.552154
218.023419	6978.445615	26.557172
218.359988	6991.996168	26.562189
218.410061	6998.021197	26.567207
218.663952	7003.133331	26.572224
218.334231	7025.228362	26.577242
218.920154	7026.528328	26.582260
219.315761	7038.954641	26.587277
219.642992	7051.939466	26.592295
219.954255	7059.678204	26.597312
220.000455	7064.211346	26.602330
220.204605	7067.409314	26.607348
220.047722	7097.500543	26.612365
220.572849	7098.924291	26.617383
220.871183	7099.266952	26.622400
220.871562	7120.478659	26.627418
221.329633	7113.101857	26.632436
221.258998	7121.689863	26.637453
221.659071	7134.721373	26.642471
222.144894	7140.503908	26.647488
222.098926	7144.839333	26.652506
222.489034	7157.025079	26.657524
222.392838	7173.672351	26.662541
222.938380	7171.167551	26.667559
222.950028	7192.479848	26.672576
223.184974	7212.815578	26.677594
223.300007	7196.476767	26.682612
223.701819	7208.109934	26.687629
223.873934	7247.588184	26.692647
224.326335	7226.736010	26.697664
224.457522	7236.221116	26.702682
224.833986	7273.997286	26.707700
224.676104	7262.657150	26.712717
224.848102	7271.646386	26.717735
225.353334	7270.121264	26.722752
225.464067	7303.237184	26.727770
225.746316	7296.073216	26.732788
225.771368	7293.395654	26.737805
225.668922	7313.376166	26.742823
226.044880	7322.483201	26.747840
226.050204	7337.429151	26.752858
226.571758	7346.757688	26.757876
226.366856	7351.451324	26.762893
226.795143	7378.190919	26.767911
227.185155	7389.317836	26.772928
227.400207	7385.829463	26.777946
227.806677	7417.414590	26.782964
228.271212	7418.682801	26.787981
228.479455	7434.101631	26.792999
228.586643	7443.151658	26.798016
228.575456	7441.404342	26.803034
228.681671	7434.753039	26.808052
229.352692	7464.219719	26.813069
229.702356	7454.295828	26.818087
230.381523	7454.253632	26.823104
230.712196	7457.159284	26.828122
230.744279	7464.685449	26.833140
230.902988	7485.234341	26.838157
230.937193	7478.504801	26.843175
231.284917	7472.753647	26.848192
231.095025	7490.271467	26.853210
231.729262	7476.118744	26.858228
231.725374	7486.620066	26.863245
231.820447	7493.174727	26.868263
232.117751	7502.478524	26.873280
232.006513	7528.412149	26.878298
232.324357	7518.865448	26.883316
232.745893	7547.276036	26.888333
232.597346	7529.137735	26.893351
233.152825	7554.581958	26.898368
233.103583	7572.459846	26.903386
233.669312	7575.015691	26.908404
233.537542	7600.159606	26.913421
233.598045	7592.844367	26.918439
234.363496	7593.373022	26.923456
234.199065	7626.288037	26.928474
234.392793	7642.858150	26.933492
234.679686	7638.502212	26.938509
234.912253	7657.569798	26.943527
235.423385	7680.289477	26.948544
235.581130	7692.493820	26.953562
235.923330	7717.213824	26.958580
236.237254	7690.308827	26.963597
235.970347	7747.214038	26.968615
236.359425	7727.900840	26.973632
236.367736	7766.540291	26.978650
237.020922	7775.245414	26.983668
237.103298	7772.824575	26.988685
237.228987	7802.928842	26.993703
237.799792	7805.183353	26.998720
237.898531	7793.920716	27.003738
238.056595	7811.780012	27.008756
238.340524	7836.463867	27.013773
238.467568	7842.434482	27.018791
239.192360	7843.266264	27.023808
238.923262	7855.633983	27.028826
239.028873	7871.993363	27.033844
239.481184	7861.173169	27.038861
239.784114	7903.694647	27.043879
239.830070	7897.568116	27.048896
239.986826	7913.732125	27.053914
240.052358	7927.021449	27.058932
240.647413	7942.855187	27.063949
240.431358	7953.371771	27.068967
241.017663	7957.928469	27.073984
241.504313	7984.654350	27.079002
241.368783	7986.037931	27.084020
241.755472	8014.536012	27.089037
241.849483	8015.350322	27.094055
242.520412	8025.432876	27.099072
242.807313	8037.041739	27.104090
243.313774	8034.988383	27.109108
243.671569	8050.835663	27.114125
243.657497	8064.500529	27.119143
244.107975	8050.345084	27.124160
244.257098	8048.636664	27.129178
244.042197	8061.077745	27.134196
244.650683	8078.675155	27.139213
244.515866	8082.653626	27.144231
244.768630	8098.140802	27.149248
245.092969	8116.834765	27.154266
245.118012	8112.950042	27.159284
245.598902	8134.931283	27.164301
245.877039	8154.920718	27.169319
246.105604	8164.134387	27.174336
246.274006	8181.069511	27.179354
246.214677	8181.097821	27.184372
247.016348	8196.798971	27.189389
246.814468	8204.227465	27.194407
247.370109	8225.840879	27.199424
247.466839	8250.760627	27.204442
247.749600	8244.120954	27.209460
248.312448	8264.636410	27.214477
248.214848	8280.931848	27.219495
248.543968	8277.672159	27.224512
249.042799	8294.574418	27.229530
249.073343	8306.896323	27.234548
249.314725	8317.557424	27.239565
249.622857	8322.787269	27.244583
250.015975	8332.996936	27.249600
250.061524	8344.669688	27.254618
250.084457	8363.614224	27.259636
250.550866	8353.577496	27.264653
250.698975	8373.048169	27.269671
251.198368	8387.885738	27.274688
251.238968	8391.106131	27.279706
251.559690	8399.354735	27.284724
251.628886	8412.010489	27.289741
251.738248	8425.158719	27.294759
252.040819	8425.327634	27.299776
252.316987	8445.868576	27.304794
252.400491	8452.797689	27.309812
253.007426	8467.899107	27.314829
253.046682	8490.334859	27.319847
253.113002	8486.489098	27.324864
253.468454	8507.157549	27.329882
253.695869	8505.862292	27.334900
254.216318	8525.626333	27.339917
254.208384	8538.578545	27.344935
254.611293	8548.699458	27.349952
254.901029	8559.735443	27.354970
254.952013	8571.765530	27.359988
255.147479	8584.525629	27.365005
255.418555	8594.387462	27.370023
255.744243	8614.761797	27.375040
256.263627	8626.335642	27.380058
256.273586	8639.173354	27.385076
256.689260	8649.595246	27.390093
256.897989	8661.896914	27.395111
257.249841	8685.582259	27.400128
257.170487	8693.855451	27.405146
257.217424	8708.338185	27.410164
257.854715	8720.426810	27.415181
258.407470	8748.941537	27.420199
258.859793	8746.795212	27.425216
259.087732	8750.856893	27.430234
259.329951	8766.414118	27.435252
259.633583	8765.002825	27.440269
260.155208	8768.296924	27.445287
260.419548	8773.655089	27.450304
260.890224	8787.887022	27.455322
261.119727	8803.082775	27.460340
261.259203	8782.888927	27.465357
261.229718	8791.679858	27.470375
261.240130	8787.879127	27.475392
261.681707	8803.255110	27.480410
261.522137	8816.489827	27.485428
261.798079	8815.317433	27.490445
261.767458	8839.329161	27.495463
261.950365	8849.046267	27.500480
262.292370	8863.130387	27.505498
262.657619	8895.990536	27.510516
263.180804	8905.529117	27.515533
263.087917	8914.668585	27.520551
263.106726	8943.549705	27.525568
264.002926	8957.307160	27.530586
263.766845	8967.431844	27.535604
264.397963	8981.561276	27.540621
264.304828	9014.390087	27.545639
264.575288	9011.717169	27.550656
265.274342	9023.545182	27.555674
265.281731	9032.915823	27.560692
266.166019	9041.429065	27.565709
266.272815	9057.259196	27.570727
266.535735	9067.243038	27.575744
266.952083	9059.514691	27.580762
266.995194	9068.757300	27.585780
267.332501	9080.162224	27.590797
267.535319	9083.039401	27.595815
267.643779	9086.532409	27.600832
268.066485	9097.400846	27.605850
267.980925	9119.977439	27.610868
268.426881	9115.256182	27.615885
268.414237	9140.253867	27.620903
268.504861	9159.727254	27.625920
268.835032	9175.814635	27.630938
268.937635	9184.501727	27.635956
269.508212	9205.724281	27.640973
269.589006	9227.820877	27.645991
270.047332	9241.180968	27.651008
270.464150	9248.710849	27.656026
270.634460	9272.626330	27.661044
270.962938	9279.015527	27.666061
271.457773	9298.426640	27.671079
271.504602	9304.490893	27.676096
272.115271	9316.527987	27.681114
272.234604	9334.233574	27.686132
272.672372	9339.485613	27.691149
272.599358	9360.229834	27.696167
272.696710	9370.741527	27.701184
273.371225	9381.774635	27.706202
273.056908	9401.188938	27.711220
273.634392	9411.973919	27.716237
274.036691	9421.885424	27.721255
274.202368	9447.918317	27.726272
274.764047	9451.976576	27.731290
274.883605	9464.436337	27.736308
275.102855	9479.251582	27.741325
275.299225	9487.008726	27.746343
275.686357	9496.591801	27.751360
276.220515	9516.585543	27.756378
276.055582	9539.147482	27.761396
276.265980	9550.197241	27.766413
276.914717	9547.544207	27.771431
276.960799	9564.562566	27.776448
277.632392	9575.146562	27.781466
277.333378	9600.814288	27.786484
277.619917	9609.410933	27.791501
278.039966	9631.720035	27.796519
278.216544	9633.880682	27.801536
278.798399	9662.623878	27.806554
278.558271	9687.430130	27.811572
279.070799	9683.761222	27.816589
279.667747	9700.688794	27.821607
279.805591	9727.177517	27.826624
279.874792	9734.940893	27.831642
280.032204	9745.282745	27.836660
280.440412	9758.544661	27.841677
280.672714	9773.236930	27.846695
281.036732	9790.864321	27.851712
281.468264	9797.020126	27.856730
281.412716	9807.249199	27.861748
281.725939	9825.749169	27.866765
282.532469	9836.883159	27.871783
282.363900	9857.579161	27.876800
282.959361	9852.235389	27.881818
283.221790	9874.063189	27.886836
283.536757	9889.927521	27.891853
283.689595	9898.613711	27.896871
283.726849	9914.284674	27.901888
284.292308	9910.224827	27.906906
284.100908	9934.825807	27.911924
284.662484	9944.016231	27.916941
285.045518	9961.077738	27.921959
284.941349	9973.787627	27.926976
285.275175	9991.768681	27.931994
285.819710	10012.058505	27.937012
286.071383	10024.417015	27.942029
286.411169	10046.872522	27.947047
286.517346	10071.032041	27.952064
287.099617	10077.112002	27.957082
286.996023	10095.084985	27.962100
287.536022	10101.394398	27.967117
287.913067	10138.590291	27.972135
288.131802	10134.584070	27.977152
288.756670	10155.913435	27.982170
288.946530	10172.339032	27.987188
289.441512	10171.997667	27.992205
289.524021	10191.518152	27.997223
289.524745	10195.035281	28.002240
290.421306	10202.392396	28.007258
290.320609	10225.792282	28.012276
290.527832	10225.733649	28.017293
291.332757	10241.838592	28.022311
291.083400	10257.274649	28.027328
291.380940	10265.206517	28.032346
291.986519	10281.418034	28.037364
292.067563	10289.661033	28.042381
292.545893	10302.294499	28.047399
292.337844	10332.464924	28.052416
293.020362	10337.666904	28.057434
293.064121	10342.260062	28.062452
293.464818	10354.692286	28.067469
293.587867	10370.482655	28.072487
293.843673	10395.014296	28.077504
294.323473	10388.246273	28.082522
294.579335	10410.241164	28.087540
294.910015	10433.028439	28.092557
295.297890	10434.210781	28.097575
295.329548	10451.001864	28.102592
295.444019	10462.607837	28.107610
295.953548	10474.631302	28.112628
295.946227	10497.702336	28.117645
296.518932	10499.929043	28.122663
296.226088	10522.322396	28.127680
296.749074	10544.648723	28.132698
296.947109	10556.071859	28.137716
297.341844	10570.191687	28.142733
297.729823	10579.820577	28.147751
297.844621	10614.256256	28.152768
298.434140	10627.844189	28.157786
298.766133	10642.519850	28.162804
299.015179	10663.808710	28.167821
299.499442	10667.492850	28.172839
299.694599	10694.329467	28.177856
299.841283	10707.461558	28.182874
300.440011	10729.205925	28.187892
300.581372	10744.266207	28.192909
300.893208	10751.438196	28.197927
301.169290	10775.960933	28.202944
301.899252	10781.772505	28.207962
301.878459	10803.160835	28.212980
301.885210	10819.641112	28.217997
302.532840	10842.183720	28.223015
302.556600	10863.580381	28.228032
303.205259	10880.886284	28.233050
303.605118	10890.955768	28.238068
303.879856	10907.703507	28.243085
304.328319	10906.735234	28.248103
304.589364	10930.729798	28.253120
304.939152	10924.605552	28.258138
305.121273	10935.610475	28.263156
305.057074	10954.024035	28.268173
305.357272	10959.205713	28.273191
305.752749	10983.289902	28.278208
306.093122	10991.435296	28.283226
306.443362	11019.003684	28.288244
306.403142	11029.318107	28.293261
306.853249	11050.423583	28.298279
306.988390	11076.147403	28.303296
307.496347	11090.623503	28.308314
307.957286	11106.372997	28.313332
308.304669	11127.229733	28.318349
308.681594	11140.153946	28.323367
309.120850	11154.390003	28.328384
309.458382	11169.310056	28.333402
309.563498	11185.289872	28.338420
310.055331	11198.432316	28.343437
310.692330	11205.230427	28.348455
310.918710	11214.250762	28.353472
310.895891	11225.204348	28.358490
311.139968	11241.784992	28.363508
310.870279	11258.507736	28.368525
311.224152	11275.682424	28.373543
311.702781	11300.248898	28.378560
311.741069	11320.505879	28.383578
312.314889	11330.972923	28.388596
312.279656	11355.824820	28.393613
313.056383	11369.444196	28.398631
313.134975	11393.697988	28.403648
313.660703	11408.294732	28.408666
314.210998	11411.450683	28.413684
314.064339	11439.402618	28.418701
314.365002	11437.774740	28.423719
315.211369	11468.660073	28.428736
315.175861	11487.790619	28.433754
315.386176	11495.383672	28.438772
315.630217	11516.942124	28.443789
315.972947	11525.240115	28.448807
316.031182	11544.740253	28.453824
316.197067	11580.370599	28.458842
317.071822	11598.953270	28.463860
317.181908	11618.463342	28.468877
317.455266	11623.843925	28.473895
317.654427	11652.025062	28.478912
318.053143	11672.488732	28.483930
318.342648	11700.058602	28.488948
318.633484	11724.384564	28.493965
319.364738	11734.528125	28.498983
319.982224	11746.407913	28.504000
320.390294	11769.897541	28.509018
320.739305	11778.518930	28.514036
320.802636	11791.530275	28.519053
321.437520	11797.930757	28.524071
321.901156	11810.898790	28.529088
321.819097	11836.719516	28.534106
322.325972	11835.738341	28.539124
322.099636	11860.402332	28.544141
322.734744	11878.750440	28.549159
322.958546	11897.848839	28.554176
322.777790	11906.242662	28.559194
323.504252	11933.504854	28.564212
323.853348	11946.921375	28.569229
324.227757	11964.958144	28.574247
324.411599	11979.537126	28.579264
324.828197	11992.582858	28.584282
324.975441	12012.277983	28.589300
325.187608	12037.962442	28.594317
325.758575	12061.436798	28.599335
325.951521	12078.186282	28.604352
326.118688	12108.212310	28.609370
326.658406	12126.248901	28.614388
326.890148	12144.376700	28.619405
327.523673	12172.526583	28.624423
327.797582	12184.472882	28.629440
328.152720	12209.624838	28.634458
328.283938	12229.053626	28.639476
328.451838	12239.558446	28.644493
329.134478	12254.691788	28.649511
329.525754	12259.472961	28.654528
329.552833	12293.041009	28.659546
330.370555	12295.046358	28.664564
330.373300	12301.640666	28.669581
330.618716	12333.438937	28.674599
330.975845	12350.676512	28.679616
330.952429	12364.987842	28.684634
331.267096	12371.667849	28.689652
331.491136	12401.479579	28.694669
331.945208	12425.310781	28.699687
332.248503	12439.402866	28.704704
332.412957	12457.592529	28.709722
332.979977	12476.048240	28.714740
332.860817	12506.506939	28.719757
333.459754	12519.579561	28.724775
333.949437	12545.944176	28.729792
334.138436	12576.060527	28.734810
334.822982	12593.263126	28.739828
335.021044	12623.155778	28.744845
335.566280	12629.206884	28.749863
336.105954	12651.053567	28.754880
336.133284	12679.335626	28.759898
336.460223	12695.681922	28.764916
336.668895	12711.957748	28.769933
337.154484	12731.039490	28.774951
337.532350	12754.949078	28.779968
338.011565	12773.870734	28.784986
338.590880	12774.963935	28.790004
338.369016	12806.317791	28.795021
339.076844	12823.888056	28.800039
339.529293	12837.941792	28.805056
339.578685	12861.038880	28.810074
340.305320	12888.187858	28.815092
340.024831	12899.083754	28.820109
340.492608	12910.792731	28.825127
341.085089	12934.929522	28.830144
341.126064	12940.083145	28.835162
341.962084	12956.224241	28.840180
342.190537	12987.976019	28.845197
342.365798	12992.267840	28.850215
342.742631	12999.346921	28.855232
343.052850	13037.369559	28.860250
343.456154	13055.917594	28.865268
343.872346	13074.585796	28.870285
344.363096	13092.030004	28.875303
344.492244	13102.344037	28.880320
344.800895	13124.329754	28.885338
345.134421	13135.642741	28.890356
345.453859	13160.933809	28.895373
345.590737	13181.639798	28.900391
346.163886	13203.178123	28.905408
346.119432	13230.943516	28.910426
346.769933	13235.976893	28.915444
346.862336	13267.585839	28.920461
347.222144	13305.394040	28.925479
347.820761	13303.091362	28.930496
347.847343	13321.461257	28.935514
348.594106	13340.288058	28.940532
348.804693	13373.341440	28.945549
348.515001	13384.647857	28.950567
349.180887	13403.227285	28.955584
349.116025	13438.580382	28.960602
349.569682	13463.139208	28.965620
349.949623	13483.962924	28.970637
350.511365	13501.940587	28.975655
350.901934	13531.224637	28.980672
350.792646	13560.211754	28.985690
351.390908	13589.171387	28.990708
351.960235	13603.035224	28.995725
352.083831	13640.192374	29.000743
352.625028	13659.842017	29.005760
352.943957	13679.793940	29.010778
353.264519	13705.869917	29.015796
353.987243	13728.014469	29.020813
354.000502	13757.976782	29.025831
354.428415	13774.903425	29.030848
354.886278	13804.170981	29.035866
355.369143	13817.663882	29.040884
355.944946	13846.301317	29.045901
356.007586	13865.301738	29.050919
356.591699	13876.441930	29.055936
356.724788	13901.680488	29.060954
357.387035	13928.296596	29.065972
357.716665	13938.194043	29.070989
357.889635	13955.814056	29.076007
358.525568	13980.555630	29.081024
358.644016	14003.419801	29.086042
359.202636	14024.957774	29.091060
359.560808	14038.284284	29.096077
359.598258	14068.437681	29.101095
360.052684	14071.012333	29.106112
360.492031	14102.577078	29.111130
360.728115	14114.224432	29.116148
361.204814	14128.496596	29.121165
361.328421	14165.654239	29.126183
361.967096	14178.898197	29.131200
362.410038	14200.113914	29.136218
362.671749	14225.746363	29.141236
363.531742	14237.710313	29.146253
363.253466	14268.512261	29.151271
363.851872	14277.695457	29.156288
363.932573	14307.409814	29.161306
364.176508	14330.505586	29.166324
364.611909	14344.737698	29.171341
364.959288	14360.930119	29.176359
365.224573	14387.296304	29.181376
365.545498	14427.609305	29.186394
366.288292	14440.328981	29.191412
366.677673	14457.980230	29.196429
367.078460	14481.686191	29.201447
367.364816	14499.468536	29.206464
367.906784	14509.452272	29.211482
367.780731	14544.173181	29.216500
368.428695	14543.392047	29.221517
368.612200	14567.180387	29.226535
368.775481	14582.310366	29.231552
368.925503	14613.846505	29.236570
369.229317	14630.975027	29.241588
369.945029	14663.882338	29.246605
369.921709	14686.638170	29.251623
370.661320	14720.185414	29.256640
370.843782	14738.190244	29.261658
370.840747	14765.827652	29.266676
371.480197	14795.164513	29.271693
371.713775	14822.923038	29.276711
372.424913	14855.413099	29.281728
372.631607	14882.149910	29.286746
373.096004	14916.358205	29.291764
373.698837	14938.556692	29.296781
373.940864	14960.889354	29.301799
374.119417	14979.911364	29.306816
374.899368	15008.873585	29.311834
375.396580	15026.536652	29.316852
376.096199	15055.632105	29.321869
376.552666	15071.170562	29.326887
376.723530	15084.654280	29.331904
376.847240	15105.715484	29.336922
377.303284	15139.093509	29.341940
377.638381	15150.615179	29.346957
378.298292	15168.654947	29.351975
378.681459	15184.724658	29.356992
379.125493	15208.061069	29.362010
379.269022	15239.630529	29.367028
379.613476	15250.492380	29.372045
379.690953	15264.228579	29.377063
380.198255	15287.513111	29.382080
380.511403	15320.019065	29.387098
381.064297	15339.327072	29.392116
381.418513	15356.286015	29.397133
381.839875	15389.422755	29.402151
382.026766	15403.200589	29.407168
382.684617	15432.994893	29.412186
382.845307	15455.765255	29.417204
382.946401	15476.711013	29.422221
383.386707	15510.632417	29.427239
383.829517	15535.848632	29.432256
384.175817	15569.727284	29.437274
384.480832	15592.461569	29.442292
385.545400	15620.188821	29.447309
385.392275	15650.459244	29.452327
385.791619	15675.215096	29.457344
386.449750	15691.105535	29.462362
386.669569	15711.504462	29.467380
387.333923	15731.482956	29.472397
387.509774	15755.858099	29.477415
387.866520	15772.696753	29.482432
388.218325	15794.565792	29.487450
388.638500	15822.168669	29.492468
389.310200	15828.576340	29.497485
389.268103	15856.440985	29.502503
389.800405	15867.702492	29.507520
390.064969	15890.330892	29.512538
390.332711	15906.916014	29.517556
390.966763	15923.702188	29.522573
391.071763	15957.167969	29.527591
391.567913	15986.363843	29.532608
391.970263	16002.910992	29.537626
392.339617	16019.092128	29.542644
393.052773	16054.845122	29.547661
392.862891	16081.833595	29.552679
393.118908	16098.996572	29.557696
394.099706	16132.148817	29.562714
394.128238	16162.325272	29.567732
394.766036	16180.835722	29.572749
394.751949	16200.655946	29.577767
395.211380	16226.546908	29.582784
395.841985	16255.964745	29.587802
395.822253	16299.078008	29.592820
396.532995	16307.809479	29.597837
396.763087	16350.751609	29.602855
397.217069	16370.169872	29.607872
397.798132	16392.360954	29.612890
398.116777	16433.805890	29.617908
398.633914	16458.274008	29.622925
398.957916	16487.919753	29.627943
399.739648	16518.102570	29.632960
400.264962	16543.703399	29.637978
400.271569	16562.879848	29.642996
401.076122	16584.297132	29.648013
400.840715	16622.508919	29.653031
401.436194	16642.539337	29.658048
402.011711	16659.652135	29.663066
402.185876	16686.614467	29.668084
402.525614	16719.459256	29.673101
403.150225	16746.957713	29.678119
403.745702	16759.637564	29.683136
403.800778	16786.455879	29.688154
403.941334	16823.806998	29.693172
404.901587	16835.390553	29.698189
405.558386	16864.506508	29.703207
405.807040	16891.637621	29.708224
406.193839	16912.161224	29.713242
406.635027	16941.187677	29.718260
407.315530	16949.144320	29.723277
407.304182	16983.241123	29.728295
407.535472	17003.517020	29.733312
408.420709	17025.608006	29.738330
408.395424	17051.336572	29.743348
408.686729	17076.507913	29.748365
408.738600	17108.187337	29.753383
408.822633	17124.305268	29.758400
409.371700	17158.203144	29.763418
409.996687	17186.412876	29.768436
410.307712	17225.939920	29.773453
410.747477	17247.316656	29.778471
411.394140	17269.724122	29.783488
411.889876	17299.671986	29.788506
411.877639	17330.202755	29.793524
412.543282	17360.718094	29.798541
413.238593	17384.372375	29.803559
413.341291	17410.301401	29.808576
413.970243	17437.449060	29.813594
414.384431	17469.340766	29.818612
414.550289	17488.032603	29.823629
414.685432	17528.690308	29.828647
415.265035	17554.447148	29.833664
415.929531	17581.813197	29.838682
416.276077	17619.144051	29.843700
416.828840	17642.578745	29.848717
417.488641	17673.385177	29.853735
417.536141	17690.806853	29.858752
418.007847	17726.486664	29.863770
418.500882	17760.569778	29.868788
418.811837	17784.262682	29.873805
419.382646	17806.171834	29.878823
420.403863	17815.255469	29.883840
421.214905	17831.950585	29.888858
421.380028	17854.227369	29.893876
421.472472	17868.674579	29.898893
422.046012	17881.549395	29.903911
422.050049	17932.882054	29.908928
422.890483	17927.176451	29.913946
422.874828	17970.257803	29.918964
423.458571	17995.943271	29.923981
423.672836	18016.258446	29.928999
423.958058	18043.331431	29.934016
424.525754	18065.077874	29.939034
424.892899	18124.068426	29.944052
425.203053	18126.885365	29.949069
425.740578	18172.237093	29.954087
425.979905	18204.963844	29.959104
426.356406	18222.755337	29.964122
426.870984	18256.193033	29.969140
427.564579	18280.110174	29.974157
428.023029	18324.876155	29.979175
428.343497	18344.023510	29.984192
429.026025	18358.917700	29.989210
429.190454	18394.549979	29.994228
429.394931	18412.510035	29.999245
430.071348	18457.560955	30.004263
430.356145	18490.214137	30.009280
430.685397	18519.408041	30.014298
430.916066	18549.293671	30.019316
431.682425	18577.270440	30.024333
431.899318	18603.456099	30.029351
432.495850	18646.691597	30.034368
433.257235	18657.644066	30.039386
432.995893	18682.234031	30.044404
433.787314	18701.747737	30.049421
434.234697	18728.911832	30.054439
434.517526	18767.021342	30.059456
435.086582	18788.008754	30.064474
435.332990	18822.321489	30.069492
435.757526	18842.333188	30.074509
436.122267	18870.614232	30.079527
436.313231	18909.067070	30.084544
437.340644	18923.713557	30.089562
437.400002	18958.819383	30.094580
437.691509	18986.248131	30.099597
438.226119	19010.296062	30.104615
438.364709	19054.379670	30.109632
438.956502	19090.096643	30.114650
439.480581	19123.964623	30.119668
440.179846	19151.686583	30.124685
440.784429	19180.326050	30.129703
440.885632	19211.017054	30.134720
441.651053	19249.110316	30.139738
441.924348	19280.801620	30.144756
442.465756	19313.009345	30.149773
443.526885	19340.548795	30.154791
443.256566	19375.024597	30.159808
443.596408	19396.828111	30.164826
444.137964	19446.027518	30.169844
444.621875	19465.829770	30.174861
444.964700	19491.720870	30.179879
445.181431	19539.080915	30.184896
446.368287	19551.890724	30.189914
446.044245	19594.023498	30.194932
446.571813	19630.025183	30.199949
447.433772	19673.056682	30.204967
447.829183	19711.452159	30.209984
448.433720	19729.157871	30.215002
448.860497	19761.817486	30.220020
449.278736	19775.463349	30.225037
449.835898	19814.575084	30.230055
450.106745	19851.231204	30.235072
450.816213	19880.789955	30.240090
451.187509	19902.896273	30.245108
450.987928	19944.460916	30.250125
451.560473	19967.650297	30.255143
452.155624	20013.123426	30.260160
452.771565	20051.680687	30.265178
453.117017	20069.939515	30.270196
453.710546	20100.677471	30.275213
454.078579	20135.113103	30.280231
454.237946	20171.097524	30.285248
454.963103	20187.982121	30.290266
455.473871	20231.062053	30.295284
455.711195	20265.684951	30.300301
456.572218	20305.314913	30.305319
456.604007	20328.135030	30.310336
457.127679	20346.758740	30.315354
457.658097	20380.972178	30.320372
458.099121	20415.444837	30.325389
458.618694	20439.060327	30.330407
458.905558	20472.373699	30.335424
459.361686	20490.113765	30.340442
459.756873	20531.366300	30.345460
459.844832	20566.174303	30.350477
460.427223	20605.233209	30.355495
460.676440	20641.516637	30.360512
461.429763	20673.544976	30.365530
461.504808	20716.860243	30.370548
462.140610	20751.205359	30.375565
463.187466	20780.958952	30.380583
463.359020	20821.849012	30.385600
463.919563	20837.500941	30.390618
464.668655	20868.594416	30.395636
465.116796	20908.300739	30.400653
465.781329	20943.389039	30.405671
466.143605	20965.710925	30.410688
466.654172	20985.815236	30.415706
467.113202	21033.614500	30.420724
467.530832	21066.713005	30.425741
468.094447	21076.508385	30.430759
468.624979	21110.620634	30.435776
469.256351	21135.756590	30.440794
469.393188	21176.411339	30.445812
469.967202	21197.502807	30.450829
470.306410	21220.379992	30.455847
470.799684	21243.357489	30.460864
471.058041	21283.032780	30.465882
471.627640	21314.514058	30.470900
471.688708	21345.832667	30.475917
472.541094	21369.218570	30.480935
472.779946	21434.765529	30.485952
473.115831	21466.376875	30.490970
473.950642	21506.571633	30.495988
474.337537	21537.107894	30.501005
475.027037	21567.629874	30.506023
475.408275	21611.658411	30.511040
476.195506	21637.925660	30.516058
476.283134	21674.486474	30.521076
476.834777	21709.854363	30.526093
477.538150	21732.899129	30.531111
478.029279	21770.233046	30.536128
478.261334	21794.472079	30.541146
478.728019	21819.678683	30.546164
478.683278	21876.110355	30.551181
479.430936	21886.157691	30.556199
479.900958	21925.981632	30.561216
480.439533	21981.175665	30.566234
480.864356	22009.590647	30.571252
481.330168	22057.032035	30.576269
482.154251	22079.147667	30.581287
482.141718	22123.655405	30.586304
482.719848	22158.267177	30.591322
483.103602	22187.458470	30.596340
483.558662	22227.848667	30.601357
484.200754	22261.441606	30.606375
484.527589	22288.373960	30.611392
485.416639	22320.260404	30.616410
485.532412	22357.213678	30.621428
485.701726	22397.864047	30.626445
486.555545	22426.598147	30.631463
487.019920	22470.103919	30.636480
487.512798	22499.930524	30.641498
487.950112	22530.355148	30.646516
488.238314	22575.270689	30.651533
488.596202	22620.322535	30.656551
489.217160	22655.243614	30.661568
489.997867	22695.216121	30.666586
490.377612	22730.516027	30.671604
490.741003	22769.698299	30.676621
491.295829	22812.635354	30.681639
491.798151	22855.223322	30.686656
491.965613	22902.382412	30.691674
492.748902	22928.634338	30.696692
493.363159	22967.593630	30.701709
493.790726	23007.901205	30.706727
494.336949	23050.372442	30.711744
495.171118	23073.318797	30.716762
495.887343	23112.698540	30.721780
496.018249	23161.162206	30.726797
496.656357	23175.072950	30.731815
497.210371	23237.723681	30.736832
497.315598	23269.776284	30.741850
497.911940	23307.638180	30.746868
498.226269	23346.198024	30.751885
498.619214	23384.895877	30.756903
499.328711	23432.043457	30.761920
499.734292	23474.959616	30.766938
500.582893	23517.892753	30.771956
500.922862	23549.580090	30.776973
501.756305	23565.086526	30.781991
502.199201	23608.031758	30.787008
502.769290	23645.135427	30.792026
503.640193	23670.292424	30.797044
504.014944	23714.453885	30.802061
504.193922	23751.568904	30.807079
504.755239	23773.701212	30.812096
505.358131	23805.381839	30.817114
506.188415	23838.012443	30.822132
506.246139	23883.038509	30.827149
506.828972	23911.927969	30.832167
507.362086	23948.530205	30.837184
507.473452	23995.886583	30.842202
508.238615	24015.323705	30.847220
508.512300	24057.722121	30.852237
509.284759	24102.999652	30.857255
509.843152	24122.219365	30.862272
509.904934	24145.117023	30.867290
510.530859	24196.035760	30.872308
510.850340	24225.612049	30.877325
511.514462	24249.401650	30.882343
511.977885	24296.955691	30.887360
511.867481	24338.527543	30.892378
512.927245	24362.878921	30.897396
513.252134	24411.319445	30.902413
513.580594	24454.352150	30.907431
514.111655	24500.258447	30.912448
514.705782	24541.601249	30.917466
515.077471	24585.537194	30.922484
515.537172	24644.899451	30.927501
516.186865	24670.917197	30.932519
517.091019	24709.771590	30.937536
517.269306	24751.655361	30.942554
517.979752	24799.986822	30.947572
518.352876	24842.993771	30.952589
519.343443	24877.593072	30.957607
519.612676	24915.710199	30.962624
520.011108	24948.659214	30.967642
520.754981	24995.552331	30.972660
520.914531	25040.013270	30.977677
521.679743	25090.240774	30.982695
522.372494	25118.696654	30.987712
522.543322	25170.664606	30.992730
523.389019	25213.318437	30.997748
523.784175	25247.561231	31.002765
524.204040	25283.716678	31.007783
524.834849	25327.347938	31.012800
525.290031	25373.941554	31.017818
526.168634	25412.262146	31.022836
526.738155	25457.774369	31.027853
527.557168	25490.484218	31.032871
527.979719	25525.049364	31.037888
528.498818	25574.421159	31.042906
529.020400	25600.358428	31.047924
529.254005	25640.843798	31.052941
529.820766	25680.723217	31.057959
530.888656	25711.435569	31.062976
531.213947	25760.574915	31.067994
531.760739	25785.223665	31.073012
532.454809	25825.291921	31.078029
532.699052	25858.279190	31.083047
533.334751	25894.567861	31.088064
533.517201	25933.872622	31.093082
533.976059	25961.418024	31.098100
534.610825	25994.211821	31.103117
535.332208	26033.502678	31.108135
535.805189	26076.552979	31.113152
536.121473	26122.143665	31.118170
536.877331	26153.484783	31.123188
536.896451	26193.085607	31.128205
537.475914	26250.665450	31.133223
538.290201	26269.737511	31.138240
538.437081	26322.365289	31.143258
538.852011	26352.548721	31.148276
539.550988	26400.000618	31.153293
539.808650	26436.044285	31.158311
540.481167	26481.782504	31.163328
540.780333	26531.192281	31.168346
541.521971	26568.134433	31.173364
542.114565	26612.002959	31.178381
542.444260	26659.435661	31.183399
543.106135	26695.494312	31.188416
543.431743	26738.054649	31.193434
543.859411	26799.386881	31.198452
544.471459	26858.069775	31.203469
545.179672	26894.037987	31.208487
545.953419	26929.105630	31.213504
546.283509	27000.552957	31.218522
547.310278	27021.222827	31.223540
547.545515	27080.199736	31.228557
547.828134	27142.409571	31.233575
548.935540	27166.369280	31.238592
549.258869	27223.476605	31.243610
550.252521	27263.612620	31.248628
550.449816	27306.294163	31.253645
551.150484	27359.895179	31.258663
551.999846	27394.832838	31.263680
551.973591	27444.156229	31.268698
552.743642	27476.278412	31.273716
553.328022	27527.754836	31.278733
553.654354	27570.492159	31.283751
554.335776	27617.614052	31.288768
555.144510	27663.714470	31.293786
555.596759	27705.086476	31.298804
556.103074	27759.249989	31.303821
556.755867	27815.330022	31.308839
557.230860	27851.770048	31.313856
557.813787	27895.641255	31.318874
558.404094	27927.105965	31.323892
558.822150	27984.634216	31.328909
559.129021	28029.822130	31.333927
560.127080	28080.621491	31.338944
560.586871	28140.114862	31.343962
561.424590	28178.030241	31.348980
562.082808	28214.864989	31.353997
562.343304	28254.070023	31.359015
563.231249	28290.936115	31.364032
563.366475	28334.215646	31.369050
564.196148	28395.420600	31.374068
564.847606	28415.459510	31.379085
564.886443	28464.562923	31.384103
566.073787	28506.625912	31.389120
566.265779	28553.694548	31.394138
566.858175	28591.895789	31.399156
567.529044	28644.047458	31.404173
567.892715	28695.463486	31.409191
568.546775	28722.659506	31.414208
568.800475	28759.882953	31.419226
569.556737	28800.756319	31.424244
569.978837	28846.068408	31.429261
570.154279	28888.701672	31.434279
571.263970	28924.257513	31.439296
571.743803	28963.290666	31.444314
572.120352	29002.595641	31.449332
572.768991	29060.180819	31.454349
573.237559	29113.831718	31.459367
574.035698	29152.802031	31.464384
574.046390	29219.953706	31.469402
574.555769	29253.601431	31.474420
575.441125	29295.752392	31.479437
575.606154	29351.715304	31.484455
576.115578	29407.447069	31.489472
576.795122	29464.986216	31.494490
577.425239	29519.920680	31.499508
577.980923	29568.311634	31.504525
578.655373	29631.124986	31.509543
579.230693	29691.598450	31.514560
579.600574	29745.962110	31.519578
580.521884	29791.510940	31.524596
581.380470	29852.144755	31.529613
581.432212	29907.542968	31.534631
582.609959	29968.077537	31.539648
582.966856	30016.296616	31.544666
584.071214	30063.797963	31.549684
584.532972	30119.223004	31.554701
584.928479	30166.771347	31.559719
585.868401	30210.015982	31.564736
586.206258	30255.112184	31.569754
586.757892	30306.010116	31.574772
587.358702	30353.757972	31.579789
587.797307	30409.835396	31.584807
588.367640	30450.867030	31.589824
589.302244	30497.287218	31.594842
589.991633	30556.015344	31.599860
590.677247	30604.475367	31.604877
590.949924	30654.849892	31.609895
591.920379	30691.270200	31.614912
592.446851	30737.272246	31.619930
593.046626	30775.557829	31.624948
593.670931	30819.741619	31.629965
593.917091	30872.163499	31.634983
594.659073	30927.524601	31.640000
595.024188	30976.881496	31.645018
595.527904	31018.013423	31.650036
595.842822	31075.761320	31.655053
596.368787	31136.091981	31.660071
597.147821	31183.320596	31.665088
597.961391	31252.050145	31.670106
598.523524	31296.965365	31.675124
599.243093	31334.654785	31.680141
599.517018	31388.088856	31.685159
600.286702	31455.667868	31.690176
601.132239	31485.837228	31.695194
601.368697	31529.607159	31.700212
601.591120	31579.877484	31.705229
602.181853	31643.005064	31.710247
603.134766	31681.531260	31.715264
603.625822	31745.586069	31.720282
604.147393	31791.708491	31.725300
605.135714	31840.590496	31.730317
605.873908	31880.877153	31.735335
606.142269	31921.850245	31.740352
607.043190	31966.601454	31.745370
607.868545	32006.501010	31.750388
608.357134	32055.868289	31.755405
608.903071	32126.626853	31.760423
609.455964	32153.627228	31.765440
609.789843	32201.162931	31.770458
610.233799	32273.869099	31.775476
611.187371	32312.719782	31.780493
611.381273	32363.167267	31.785511
612.174657	32426.943328	31.790528
612.691944	32486.996639	31.795546
612.973075	32536.945318	31.800564
614.247816	32592.485703	31.805581
614.305767	32656.969241	31.810599
615.349826	32701.505798	31.815616
616.019376	32765.908136	31.820634
616.280933	32834.453237	31.825652
617.249045	32866.110866	31.830669
617.778086	32946.535998	31.835687
618.564639	32997.344995	31.840704
619.562067	33043.677297	31.845722
619.954145	33095.369028	31.850740
620.716767	33145.542359	31.855757
621.072048	33202.539460	31.860775
621.554692	33247.458490	31.865792
622.730759	33297.583789	31.870810
622.720257	33355.040019	31.875828
623.386188	33404.069438	31.880845
624.048239	33470.056672	31.885863
624.554888	33525.386779	31.890880
625.422728	33586.007737	31.895898
625.802210	33650.659902	31.900916
626.612808	33688.499437	31.905933
627.073023	33752.667847	31.910951
627.950472	33808.601887	31.915968
628.835341	33864.377309	31.920986
629.382395	33911.436341	31.926004
630.186331	33969.250511	31.931021
630.718067	34024.759567	31.936039
631.274687	34078.258235	31.941056
631.938666	34122.931670	31.946074
631.909033	34172.457161	31.951092
632.891142	34242.163861	31.956109
633.097488	34303.353059	31.961127
633.958281	34355.051334	31.966144
634.988776	34405.622482	31.971162
635.205292	34460.023018	31.976180
635.529696	34506.028377	31.981197
636.173414	34562.974779	31.986215
636.597613	34620.235341	31.991232
637.320092	34660.006383	31.996250
638.053878	34731.881167	32.001268
638.842877	34776.720892	32.006285
639.394149	34846.996864	32.011303
640.155517	34898.023797	32.016320
640.954600	34950.990121	32.021338
640.968570	35025.526623	32.026356
641.642146	35082.816857	32.031373
642.393872	35141.089545	32.036391
643.524707	35192.356492	32.041408
643.866819	35268.181766	32.046426
644.383388	35327.072663	32.051444
645.379952	35379.953737	32.056461
645.697644	35446.017855	32.061479
646.574419	35516.716177	32.066496
647.639053	35562.493096	32.071514
647.958084	35628.999126	32.076532
648.491141	35686.321695	32.081549
649.455722	35747.094374	32.086567
650.109435	35796.396083	32.091584
650.692510	35854.259869	32.096602
651.771041	35919.652965	32.101620
652.446002	35973.704843	32.106637
652.882335	36027.440185	32.111655
653.515724	36076.791677	32.116672
654.409530	36129.155493	32.121690
655.033357	36194.235826	32.126708
655.741012	36249.246625	32.131725
656.565481	36302.063441	32.136743
656.692768	36355.092325	32.141760
657.612990	36409.317816	32.146778
658.104631	36472.832738	32.151796
658.651537	36527.704514	32.156813
659.290032	36580.441464	32.161831
659.901114	36637.791136	32.166848
660.873883	36693.681881	32.171866
661.394547	36755.096464	32.176884
662.290092	36812.297392	32.181901
663.198270	36871.295347	32.186919
663.549721	36929.370001	32.191936
664.406790	36978.418952	32.196954
664.752196	37034.579413	32.201972
665.578937	37087.738889	32.206989
665.877427	37148.515516	32.212007
666.436973	37206.446060	32.217024
667.325057	37262.699037	32.222042
667.915251	37325.906680	32.227060
668.220773	37389.579259	32.232077
669.390215	37452.878042	32.237095
669.492068	37502.613192	32.242112
670.179712	37559.756752	32.247130
670.751198	37615.632479	32.252148
671.657932	37668.295461	32.257165
671.992720	37735.653993	32.262183
672.842162	37788.961857	32.267200
673.738249	37850.394779	32.272218
674.350665	37920.607717	32.277236
674.920426	37975.433290	32.282253
675.916084	38027.600786	32.287271
676.335198	38096.476693	32.292288
677.253182	38146.930478	32.297306
677.729224	38203.427218	32.302324
678.312445	38274.817749	32.307341
678.887780	38312.609079	32.312359
679.396330	38398.653123	32.317376
680.720256	38421.337482	32.322394
681.199502	38513.628913	32.327412
681.575749	38585.927207	32.332429
682.419903	38638.730905	32.337447
682.938708	38698.180411	32.342464
683.803453	38778.897131	32.347482
684.614493	38840.035011	32.352500
685.430144	38890.502586	32.357517
685.962403	38957.905512	32.362535
686.161402	39034.074890	32.367552
687.183937	39093.675796	32.372570
687.815594	39155.772088	32.377588
688.539273	39220.037783	32.382605
689.437231	39289.892449	32.387623
689.799628	39365.978965	32.392640
690.630778	39432.415354	32.397658
690.995404	39500.206633	32.402676
692.037241	39570.022205	32.407693
692.494188	39635.842518	32.412711
693.456170	39710.930038	32.417728
694.334960	39774.175017	32.422746
695.028663	39837.129603	32.427764
695.628453	39908.171180	32.432781
696.497802	39967.274466	32.437799
697.115182	40043.689252	32.442816
697.890736	40113.172588	32.447834
698.084274	40177.950485	32.452852
699.085223	40240.856077	32.457869
699.838630	40298.354804	32.462887
700.380116	40386.354282	32.467904
701.152260	40446.258418	32.472922
702.164372	40516.916791	32.477940
702.714500	40585.682615	32.482957
703.419993	40650.549534	32.487975
704.064272	40709.659696	32.492992
704.727186	40784.870535	32.498010
705.450309	40837.820203	32.503028
706.038240	40914.596817	32.508045
706.657221	40975.116968	32.513063
707.082391	41062.078752	32.518080
708.246811	41101.531351	32.523098
708.945478	41169.402255	32.528116
709.616192	41227.910765	32.533133
710.257491	41286.660701	32.538151
710.486295	41358.382400	32.543168
711.595379	41420.152337	32.548186
711.761574	41484.529532	32.553204
712.876873	41551.679607	32.558221
713.521872	41629.480120	32.563239
713.966416	41700.673732	32.568256
714.731330	41772.895311	32.573274
715.880157	41838.546176	32.578292
716.051697	41902.223896	32.583309
716.865303	41965.960498	32.588327
717.748962	42060.261644	32.593344
718.564942	42125.345245	32.598362
719.176811	42200.434812	32.603380
720.045943	42271.206792	32.608397
720.934266	42342.468050	32.613415
721.515419	42418.547545	32.618432
722.264741	42486.141198	32.623450
723.038695	42555.831862	32.628468
723.575510	42635.064066	32.633485
724.517759	42705.942903	32.638503
724.945468	42778.077302	32.643520
725.605866	42851.121224	32.648538
726.120860	42936.338668	32.653556
727.042456	43024.993012	32.658573
727.873573	43084.479066	32.663591
728.202323	43173.556591	32.668608
729.217677	43247.034600	32.673626
730.297121	43330.571229	32.678644
730.952034	43414.434496	32.683661
732.003747	43484.586242	32.688679
732.485133	43546.870672	32.693696
733.227527	43616.444482	32.698714
733.913638	43691.244844	32.703732
734.722663	43773.189551	32.708749
735.843288	43848.599618	32.713767
736.159044	43925.377817	32.718784
737.057388	43995.183835	32.723802
737.737585	44072.819457	32.728820
738.034966	44147.885558	32.733837
739.188891	44213.535223	32.738855
740.077620	44299.176223	32.743872
741.092468	44368.643447	32.748890
741.694273	44449.305770	32.753908
741.939649	44520.656300	32.758925
743.093623	44585.055028	32.763943
743.666894	44663.391695	32.768960
744.045044	44751.598827	32.773978
745.444289	44815.170730	32.778996
745.927085	44885.257841	32.784013
746.787831	44944.392272	32.789031
747.446743	45022.335222	32.794048
748.357323	45083.585243	32.799066
748.668161	45149.391588	32.804084
749.389430	45221.562004	32.809101
750.499701	45289.459339	32.814119
750.781167	45362.823404	32.819136
751.796725	45431.351530	32.824154
752.513906	45494.961939	32.829172
752.773257	45569.813100	32.834189
753.650667	45633.338571	32.839207
754.359909	45720.081444	32.844224
755.323902	45796.565982	32.849242
756.115337	45865.964347	32.854260
756.499250	45955.359694	32.859277
757.680167	46019.797316	32.864295
758.269316	46114.836268	32.869312
758.921004	46192.735129	32.874330
759.773456	46267.040579	32.879348
760.263601	46329.778428	32.884365
761.112225	46418.521685	32.889383
761.670273	46512.665461	32.894400
762.639182	46589.184240	32.899418
763.230632	46672.152109	32.904436
764.185393	46759.037736	32.909453
765.171658	46827.768464	32.914471
766.054660	46914.988091	32.919488
766.857190	46993.554287	32.924506
767.610344	47080.413656	32.929524
768.076995	47152.925998	32.934541
769.094203	47229.029739	32.939559
769.967567	47322.272670	32.944576
770.652699	47401.342097	32.949594
771.753346	47476.723750	32.954612
772.075284	47564.004358	32.959629
773.167694	47633.406000	32.964647
774.071297	47723.999145	32.969664
774.579189	47803.060729	32.974682
775.455670	47887.945143	32.979700
775.842609	47974.091060	32.984717
776.912987	48043.658742	32.989735
777.959648	48125.765928	32.994752
778.394155	48202.689166	32.999770
779.423995	48294.284276	33.004788
780.061053	48377.278179	33.009805
781.070230	48450.917963	33.014823
781.571051	48521.026227	33.019840
782.314881	48613.529896	33.024858
783.288352	48685.851141	33.029876
783.884271	48781.922593	33.034893
784.640242	48863.445271	33.039911
785.493698	48942.668366	33.044928
786.218968	49025.133803	33.049946
787.123556	49093.438335	33.054964
787.762273	49194.929239	33.059981
788.953168	49273.046219	33.064999
789.657736	49347.479737	33.070016
790.376338	49416.673382	33.075034
791.269542	49489.951000	33.080052
791.658932	49561.377993	33.085069
792.733881	49621.765752	33.090087
793.547129	49700.383330	33.095104
793.897785	49772.593577	33.100122
794.723290	49844.974667	33.105140
795.279912	49934.135525	33.110157
796.144766	50012.222461	33.115175
797.051317	50101.079179	33.120192
797.323478	50183.795673	33.125210
798.567691	50261.368930	33.130228
799.369685	50350.937757	33.135245
799.633872	50424.795836	33.140263
800.578227	50516.797874	33.145280
801.415872	50612.755564	33.150298
802.692390	50698.132552	33.155316
803.127217	50798.128275	33.160333
803.782775	50876.703571	33.165351
805.265935	50950.953620	33.170368
805.705613	51058.403708	33.175386
806.647123	51148.626499	33.180404
807.818442	51239.431691	33.185421
808.723061	51317.792571	33.190439
809.347871	51402.333090	33.195456
809.970978	51500.551341	33.200474
810.813587	51575.530776	33.205492
811.241891	51660.810684	33.210509
812.435231	51755.291487	33.215527
813.486876	51835.243851	33.220544
814.397387	51919.533059	33.225562
815.527162	51999.448476	33.230580
816.259523	52087.471793	33.235597
817.073620	52167.510784	33.240615
817.907557	52259.403665	33.245632
818.642076	52338.016994	33.250650
819.815841	52401.873110	33.255668
820.032597	52490.977733	33.260685
820.623136	52569.608678	33.265703
821.715061	52662.589237	33.270720
822.407190	52758.628929	33.275738
823.398553	52843.771193	33.280756
824.128004	52923.953265	33.285773
825.277619	53009.689708	33.290791
825.835504	53084.834380	33.295808
826.588489	53179.916667	33.300826
827.663670	53269.999458	33.305844
828.211925	53352.358402	33.310861
828.884076	53430.655040	33.315879
830.260132	53529.591448	33.320896
830.892353	53606.774784	33.325914
831.782181	53679.460979	33.330932
832.285260	53788.388057	33.335949
833.484947	53859.390773	33.340967
834.159282	53939.971185	33.345984
834.586668	54023.078343	33.351002
835.665678	54099.457284	33.356020
836.157643	54195.050415	33.361037
837.107836	54279.877759	33.366055
838.083636	54344.406675	33.371072
838.635990	54425.561005	33.376090
839.679118	54515.064882	33.381108
839.844645	54606.043978	33.386125
841.148323	54677.383707	33.391143
842.235163	54767.257475	33.396160
842.461350	54871.115550	33.401178
843.699304	54956.405281	33.406196
844.624677	55048.727068	33.411213
845.324678	55135.510995	33.416231
846.185376	55221.676357	33.421248
847.029163	55326.076339	33.426266
847.804660	55418.073487	33.431284
848.703404	55509.492794	33.436301
849.412996	55605.822573	33.441319
850.515374	55714.798399	33.446336
851.317154	55802.143786	33.451354
852.271819	55891.472812	33.456372
853.059956	55988.410790	33.461389
853.972393	56070.237998	33.466407
855.077893	56158.521604	33.471424
855.643127	56258.501542	33.476442
856.492864	56356.454404	33.481460
857.347738	56454.031334	33.486477
858.223878	56543.439176	33.491495
859.352364	56634.556084	33.496512
859.834984	56734.602273	33.501530
861.054196	56824.515624	33.506548
861.855230	56913.716257	33.511565
862.997828	57017.409128	33.516583
863.553792	57111.766765	33.521600
864.155584	57211.285196	33.526618
865.036970	57297.750630	33.531636
866.234471	57405.843807	33.536653
867.192607	57494.409844	33.541671
868.325334	57584.160743	33.546688
868.736507	57687.714929	33.551706
870.095418	57777.557053	33.556724
870.862866	57860.403416	33.561741
871.905450	57957.936370	33.566759
872.810104	58033.895466	33.571776
873.329121	58125.119908	33.576794
874.313214	58224.380938	33.581812
875.527449	58315.890313	33.586829
876.385956	58397.073517	33.591847
877.226421	58477.859013	33.596864
877.785576	58591.531753	33.601882
878.706229	58674.758330	33.606900
879.660200	58759.921547	33.611917
880.483853	58844.635495	33.616935
881.432500	58932.335449	33.621952
881.848023	59020.126965	33.626970
882.755958	59096.159363	33.631988
883.536773	59197.102796	33.637005
884.539502	59279.968598	33.642023
885.150008	59359.051810	33.647040
885.612409	59462.156307	33.652058
886.643895	59553.887156	33.657076
888.057857	59643.243395	33.662093
888.110665	59742.360817	33.667111
889.260243	59844.489865	33.672128
890.268708	59950.184328	33.677146
891.264156	60021.969606	33.682164
892.141296	60141.069560	33.687181
892.933330	60250.389961	33.692199
893.858980	60327.457008	33.697216
894.371159	60452.619020	33.702234
895.673143	60550.837893	33.707252
896.999428	60631.372335	33.712269
897.174266	60748.478814	33.717287
898.781489	60845.501394	33.722304
899.469139	60939.156626	33.727322
900.396190	61045.624867	33.732340
901.250673	61147.975352	33.737357
902.162646	61240.311327	33.742375
903.488926	61338.843067	33.747392
904.060691	61433.608532	33.752410
905.331991	61538.392389	33.757428
905.988992	61644.010274	33.762445
906.836755	61732.554098	33.767463
907.919811	61830.909256	33.772480
908.936760	61928.921803	33.777498
909.787887	62033.367955	33.782516
910.333545	62135.668766	33.787533
911.454644	62244.269569	33.792551
912.358861	62330.590590	33.797568
913.101861	62435.476141	33.802586
913.955147	62563.215641	33.807604
915.072442	62636.927211	33.812621
915.540750	62763.339945	33.817639
916.609589	62872.871575	33.822656
917.733777	62961.462458	33.827674
918.468775	63067.423265	33.832692
919.135934	63183.667659	33.837709
920.213987	63298.407443	33.842727
921.199187	63402.129343	33.847744
922.036783	63513.643526	33.852762
922.715524	63627.173077	33.857780
924.069643	63742.458987	33.862797
925.045017	63850.015383	33.867815
925.997354	63947.464488	33.872832
926.998315	64060.067471	33.877850
927.789377	64165.671815	33.882868
929.017757	64280.971531	33.887885
929.758895	64384.522896	33.892903
930.779751	64460.862241	33.897920
931.653651	64564.968217	33.902938
932.822122	64665.626720	33.907956
933.535944	64747.687851	33.912973
934.497658	64858.789116	33.917991
935.383971	64944.745941	33.923008
936.261852	65052.122534	33.928026
937.110678	65151.103834	33.933044
938.298619	65245.165055	33.938061
939.054427	65349.401480	33.943079
939.818663	65429.155251	33.948096
940.872823	65548.921227	33.953114
941.630385	65636.954453	33.958132
943.031866	65749.889000	33.963149
943.636100	65843.256485	33.968167
944.759144	65951.233924	33.973184
945.671636	66053.775401	33.978202
946.656550	66163.184586	33.983220
947.731404	66254.773744	33.988237
948.084256	66361.401114	33.993255
949.496463	66466.218220	33.998272
950.349433	66584.355090	34.003290
951.191908	66690.028373	34.008308
952.418748	66790.751946	34.013325
953.259797	66905.393223	34.018343
954.335380	67013.238902	34.023360
954.783745	67122.009316	34.028378
955.931377	67231.755596	34.033396
957.022214	67341.821065	34.038413
957.509913	67476.145406	34.043431
959.047597	67565.601535	34.048448
960.054603	67671.320352	34.053466
960.745204	67796.218093	34.058484
961.552251	67902.007885	34.063501
962.781752	68007.497315	34.068519
963.576351	68131.553132	34.073536
964.802440	68253.349032	34.078554
965.883216	68358.421831	34.083572
966.780102	68460.176305	34.088589
967.620157	68586.969497	34.093607
968.785730	68677.740800	34.098624
969.924393	68787.089865	34.103642
970.832792	68904.764615	34.108660
971.631139	69011.503137	34.113677
972.478963	69131.513714	34.118695
973.571187	69237.240149	34.123712
974.577495	69357.776532	34.128730
975.471497	69474.490430	34.133748
976.743906	69579.968945	34.138765
977.490431	69699.266289	34.143783
978.578269	69806.152641	34.148800
979.689452	69913.471788	34.153818
980.061465	70027.018396	34.158836
981.663480	70142.840255	34.163853
982.454502	70247.830356	34.168871
983.364491	70349.668429	34.173888
984.340651	70457.391114	34.178906
985.169243	70557.935411	34.183924
986.359802	70654.916168	34.188941
987.120567	70766.307651	34.193959
988.122402	70867.261918	34.198976
989.224767	70976.351029	34.203994
989.932480	71081.144030	34.209012
991.004718	71183.453435	34.214029
991.886233	71297.678204	34.219047
992.912866	71409.871358	34.224064
994.126257	71522.976864	34.229082
995.082453	71620.353493	34.234100
996.237870	71720.125145	34.239117
996.586665	71837.464259	34.244135
997.803216	71953.244395	34.249152
998.992145	72061.523316	34.254170
999.769937	72189.821932	34.259188
1001.064262	72304.448114	34.264205
1002.135755	72414.826440	34.269223
1003.015186	72528.016105	34.274240
1004.043059	72637.859217	34.279258
1005.039201	72756.295022	34.284276
1006.143974	72857.034589	34.289293
1006.925885	72990.891857	34.294311
1008.103508	73092.985878	34.299328
1009.299022	73217.363945	34.304346
1010.000499	73331.174148	34.309364
1010.953505	73461.348769	34.314381
1012.191840	73567.795595	34.319399
1013.152601	73689.951792	34.324416
1014.412074	73798.968302	34.329434
1015.357884	73918.499586	34.334452
1016.412179	74029.205574	34.339469
1017.358773	74159.916581	34.344487
1018.234884	74268.434239	34.349504
1019.322073	74387.977442	34.354522
1020.157484	74525.470030	34.359540
1021.002354	74640.617206	34.364557
1022.162012	74767.671051	34.369575
1023.130696	74902.636275	34.374592
1024.245832	75010.766058	34.379610
1025.070342	75142.608790	34.384628
1026.426532	75254.651172	34.389645
1027.276346	75396.324588	34.394663
1028.196857	75521.013524	34.399680
1029.461409	75641.092109	34.404698
1029.994378	75765.964277	34.409716
1031.346097	75897.209894	34.414733
1032.482488	76023.251605	34.419751
1033.423728	76146.841497	34.424768
1034.559540	76270.085210	34.429786
1035.542610	76407.485030	34.434804
1036.775852	76541.787191	34.439821
1037.764008	76663.483152	34.444839
1038.548208	76777.533592	34.449856
1040.030369	76878.580971	34.454874
1040.770194	77015.442178	34.459892
1041.769544	77112.819770	34.464909
1043.052045	77235.553077	34.469927
1043.466649	77352.812928	34.474944
1044.695453	77468.035276	34.479962
1045.895766	77588.786633	34.484980
1046.712289	77699.013416	34.489997
1047.559261	77827.318147	34.495015
1048.435535	77951.365479	34.500032
1049.849487	78083.708789	34.505050
1050.769839	78216.934152	34.510068
1051.588097	78331.992841	34.515085
1052.560523	78459.807571	34.520103
1053.329050	78595.903752	34.525120
1054.968193	78724.852915	34.530138
1055.789577	78870.410651	34.535156
1056.923434	78998.177792	34.540173
1058.468437	79121.658153	34.545191
1058.815898	79262.945457	34.550208
1059.931380	79390.812781	34.555226
1061.183169	79536.913587	34.560244
1062.473009	79675.392806	34.565261
1063.354291	79811.163085	34.570279
1064.547203	79945.266549	34.575296
1065.763006	80070.638041	34.580314
1066.675269	80220.015057	34.585332
1067.978734	80351.524628	34.590349
1069.394417	80472.334609	34.595367
1070.225271	80616.670606	34.600384
1071.207983	80743.954312	34.605402
1072.211903	80884.193841	34.610420
1073.432339	81013.160758	34.615437
1074.568274	81150.384841	34.620455
1075.369047	81286.632765	34.625472
1076.574040	81418.670497	34.630490
1077.657891	81565.077879	34.635508
1078.707221	81688.469146	34.640525
1079.888072	81825.026803	34.645543
1080.974370	81970.861404	34.650560
1082.453079	82100.154336	34.655578
1083.471976	82248.106677	34.660596
1084.256218	82371.209112	34.665613
1085.583167	82503.246987	34.670631
1086.662050	82644.339912	34.675648
1087.906092	82772.966312	34.680666
1088.750555	82912.941453	34.685684
1089.829444	83036.778536	34.690701
1091.495123	83171.971944	34.695719
1092.452102	83315.048567	34.700736
1093.361683	83439.167835	34.705754
1094.645313	83563.500199	34.710772
1095.639620	83688.966701	34.715789
1096.934448	83816.750615	34.720807
1097.561126	83940.329888	34.725824
1098.785103	84060.002647	34.730842
1099.808126	84180.921905	34.735860
1100.618971	84305.264306	34.740877
1101.471275	84423.620000	34.745895
1102.345979	84545.721912	34.750912
1103.677480	84679.195294	34.755930
1104.638431	84815.788475	34.760948
1105.557482	84962.144681	34.765965
1106.532080	85096.613178	34.770983
1107.801791	85233.602531	34.776000
1108.621190	85361.130006	34.781018
1109.716165	85518.311547	34.786036
1110.710092	85656.283234	34.791053
1112.327191	85793.252579	34.796071
1112.943741	85957.632772	34.801088
1114.548689	86085.880605	34.806106
1115.786315	86246.288423	34.811124
1117.041012	86372.203668	34.816141
1118.374294	86505.081286	34.821159
1119.125470	86649.610583	34.826176
1120.582092	86787.136658	34.831194
1121.614552	86928.019029	34.836212
1122.540532	87078.290004	34.841229
1124.280826	87199.333731	34.846247
1125.334411	87328.024496	34.851264
1126.612943	87487.164197	34.856282
1127.439774	87620.312667	34.861300
1128.300278	87745.691674	34.866317
1129.719650	87903.376696	34.871335
1130.826211	88047.011601	34.876352
1132.261384	88181.420008	34.881370
1133.093943	88329.425554	34.886388
1134.366143	88468.016148	34.891405
1135.619290	88602.753337	34.896423
1136.503532	88754.655180	34.901440
1137.509582	88901.170007	34.906458
1138.668768	89046.112191	34.911476
1139.831623	89193.546287	34.916493
1141.035288	89331.059334	34.921511
1141.942907	89485.909446	34.926528
1143.144571	89635.136326	34.931546
1144.487769	89770.732843	34.936564
1145.552875	89919.313068	34.941581
1146.604635	90078.862105	34.946599
1147.615104	90228.698947	34.951616
1149.260273	90364.048790	34.956634
1150.455825	90515.236810	34.961652
1151.611774	90662.188714	34.966669
1152.643426	90815.833332	34.971687
1153.630345	90948.913607	34.976704
1155.367557	91096.927016	34.981722
1156.100212	91253.208860	34.986740
1157.439970	91378.172219	34.991757
1158.643591	91512.315573	34.996775
1159.530923	91657.950835	35.001792
1160.276704	91806.126689	35.006810
1161.665165	91936.461249	35.011828
1162.518645	92061.746160	35.016845
1163.880424	92196.089909	35.021863
1164.617677	92352.903796	35.026880
1165.999070	92482.901197	35.031898
1167.241850	92638.795568	35.036916
1167.903781	92785.561983	35.041933
1169.658830	92917.368326	35.046951
1170.613334	93061.465292	35.051968
1172.083456	93214.709130	35.056986
1173.332806	93356.420956	35.062004
1174.445652	93498.572839	35.067021
1175.374909	93648.230910	35.072039
1176.583068	93810.381779	35.077056
1177.802916	93942.481736	35.082074
1178.918007	94104.162524	35.087092
1179.702748	94270.134845	35.092109
1181.198935	94408.158228	35.097127
1182.133987	94572.603519	35.102144
1183.091401	94727.900149	35.107162
1184.481175	94880.130927	35.112180
1185.662510	95044.749277	35.117197
1187.262289	95201.452503	35.122215
1188.205738	95363.138091	35.127232
1189.482256	95528.839174	35.132250
1190.965798	95681.262920	35.137268
1191.766836	95840.596200	35.142285
1193.474479	95992.834622	35.147303
1194.536936	96159.086773	35.152320
1196.080096	96308.424710	35.157338
1197.216960	96462.724360	35.162356
1198.314872	96622.901591	35.167373
1199.721820	96782.758817	35.172391
1200.689897	96932.008875	35.177408
1202.256543	97087.914507	35.182426
1203.357643	97243.952167	35.187444
1204.102168	97397.561473	35.192461
1205.833967	97546.226043	35.197479
1207.109348	97704.668373	35.202496
1208.000379	97859.484782	35.207514
1209.518484	98019.231862	35.212532
1210.374374	98164.269341	35.217549
1211.846864	98323.323603	35.222567
1212.926322	98488.799401	35.227584
1214.244529	98639.959869	35.232602
1215.327863	98798.978102	35.237620
1216.620835	98945.760420	35.242637
1218.193634	99108.112942	35.247655
1219.361061	99267.121067	35.252672
1220.058024	99423.718752	35.257690
1221.705356	99575.832691	35.262708
1222.736358	99751.808536	35.267725
1224.047641	99887.661528	35.272743
1225.054088	100041.525385	35.277760
1226.731842	100167.433086	35.282778
1227.928078	100310.740830	35.287796
1228.673667	100467.312595	35.292813
1230.049757	100600.280780	35.297831
1231.070496	100746.168871	35.302848
1232.253862	100902.243763	35.307866
1233.542897	101036.721471	35.312884
1234.347887	101199.179205	35.317901
1235.404537	101347.596207	35.322919
1236.503498	101511.059694	35.327936
1237.368477	101687.766366	35.332954
1239.043689	101846.844453	35.337972
1239.691813	102030.636744	35.342989
1241.185860	102186.639264	35.348007
1242.655990	102367.778943	35.353024
1243.681731	102542.739184	35.358042
1245.079827	102705.695290	35.363060
1245.900047	102881.684156	35.368077
1247.581955	103051.203480	35.373095
1248.874009	103235.156000	35.378112
1249.975279	103412.009025	35.383130
1251.386321	103587.618206	35.388148
1252.483009	103757.229347	35.393165
1254.193210	103933.489614	35.398183
1255.470262	104116.166886	35.403200
1256.768221	104293.159806	35.408218
1258.129815	104465.277756	35.413236
1259.529054	104642.839373	35.418253
1260.770640	104812.555316	35.423271
1261.863021	104980.169963	35.428288
1263.157764	105152.866751	35.433306
1265.103424	105324.480464	35.438324
1266.202144	105506.051439	35.443341
1267.557968	105660.485324	35.448359
1269.031587	105821.995512	35.453376
1269.888286	106016.575552	35.458394
1271.691107	106154.304363	35.463412
1272.808295	106332.727181	35.468429
1274.113608	106492.066377	35.473447
1275.210967	106657.894783	35.478464
1276.896904	106812.036854	35.483482
1278.400890	106993.269964	35.488500
1279.276768	107155.187973	35.493517
1280.559937	107319.118147	35.498535
1281.828199	107481.532913	35.503552
1283.154329	107646.591341	35.508570
1284.601780	107814.023915	35.513588
1285.846775	107985.780810	35.518605
1287.250283	108142.526865	35.523623
1288.635957	108308.384141	35.528640
1289.119345	108470.075928	35.533658
1290.760006	108628.167166	35.538676
1292.461370	108806.275010	35.543693
1293.305694	108984.001404	35.548711
1294.926109	109118.421793	35.553728
1296.028148	109277.457326	35.558746
1297.370119	109415.043920	35.563764
1298.404381	109571.649065	35.568781
1299.591114	109717.464802	35.573799
1300.925554	109859.099545	35.578816
1302.360163	110016.624972	35.583834
1303.577201	110177.825429	35.588852
1304.772080	110339.834317	35.593869
1306.007765	110492.615675	35.598887
1307.660448	110656.965451	35.603904
1308.714432	110823.417977	35.608922
1309.665242	110979.798567	35.613940
1310.887960	111147.973461	35.618957
1312.085490	111306.696885	35.623975
1313.767275	111497.607251	35.628992
1314.546130	111664.033247	35.634010
1315.807301	111830.940735	35.639028
1317.413878	112018.335026	35.644045
1318.279091	112209.241434	35.649063
1319.862854	112378.664990	35.654080
1321.196160	112548.965083	35.659098
1322.722346	112734.535537	35.664116
1323.524254	112933.566449	35.669133
1325.129760	113109.131794	35.674151
1326.703699	113291.103270	35.679168
1327.840804	113486.559390	35.684186
1329.346676	113674.577257	35.689204
1330.952083	113859.073690	35.694221
1331.750432	114043.788380	35.699239
1333.511458	114226.433299	35.704256
1335.127013	114410.489057	35.709274
1336.458772	114577.207530	35.714292
1337.441338	114789.771944	35.719309
1338.888820	114954.448733	35.724327
1340.531134	115133.960132	35.729344
1341.286098	115346.768008	35.734362
1342.647633	115498.180084	35.739380
1344.494867	115718.762659	35.744397
1345.357745	115886.298701	35.749415
1346.927432	116077.597498	35.754432
1348.174598	116292.861161	35.759450
1349.939425	116462.688777	35.764468
1351.109364	116660.107975	35.769485
1352.449084	116851.550455	35.774503
1354.028719	117029.774727	35.779520
1355.321461	117228.704634	35.784538
1357.101056	117396.738075	35.789556
1358.231919	117584.160906	35.794573
1359.518146	117767.039828	35.799591
1360.863359	117931.119070	35.804608
1362.304009	118145.569875	35.809626
1363.953588	118308.374861	35.814644
1365.241178	118501.661457	35.819661
1366.634870	118674.082723	35.824679
1368.147337	118827.485059	35.829696
1369.581006	118999.420948	35.834714
1370.669214	119163.770513	35.839732
1372.297282	119329.630931	35.844749
1373.326178	119487.330984	35.849767
1374.921606	119650.710259	35.854784
1375.935233	119827.245662	35.859802
1377.285620	120005.432036	35.864820
1378.697429	120169.185682	35.869837
1379.676539	120341.126736	35.874855
1381.009186	120526.449325	35.879872
1381.882691	120712.966975	35.884890
1383.309458	120901.183698	35.889908
1384.513662	121087.436179	35.894925
1385.614869	121280.583143	35.899943
1387.200908	121480.721299	35.904960
1388.742415	121675.941517	35.909978
1389.957533	121879.168503	35.914996
1391.402622	122087.439112	35.920013
1392.470547	122299.545452	35.925031
1394.379041	122489.774072	35.930048
1395.465371	122701.893387	35.935066
1396.606241	122898.250200	35.940084
1398.398301	123102.800773	35.945101
1399.726086	123316.862436	35.950119
1401.303908	123522.311538	35.955136
1402.707617	123740.252862	35.960154
1404.376965	123938.331911	35.965172
1405.623018	124132.705286	35.970189
1406.942333	124362.203659	35.975207
1408.781933	124559.348320	35.980224
1410.107936	124769.482807	35.985242
1411.516076	124975.299379	35.990260
1413.064309	125178.764670	35.995277
1414.100168	125387.759469	36.000295
1416.002278	125583.850419	36.005312
1417.273865	125797.307543	36.010330
1418.578255	126003.186464	36.015348
1420.236951	126215.888719	36.020365
1421.693743	126415.045830	36.025383
1423.491553	126619.508350	36.030400
1424.851442	126820.659887	36.035418
1426.289718	127022.573155	36.040436
1428.173006	127248.713021	36.045453
1429.241671	127438.552863	36.050471
1430.902978	127624.613634	36.055488
1432.033760	127830.597324	36.060506
1434.053195	128030.170890	36.065524
1435.064269	128226.232490	36.070541
1436.659241	128425.610356	36.075559
1438.239608	128621.761677	36.080576
1439.534743	128838.304519	36.085594
1440.953261	129028.935873	36.090612
1442.240295	129221.261635	36.095629
1443.802231	129416.965490	36.100647
1445.334225	129603.566942	36.105664
1446.764584	129802.993593	36.110682
1448.027663	129972.259156	36.115700
1449.267617	130149.954045	36.120717
1450.439711	130336.351568	36.125735
1451.986061	130512.479849	36.130752
1453.716833	130720.733493	36.135770
1454.839124	130915.770299	36.140788
1456.694126	131093.791562	36.145805
1457.579335	131287.627065	36.150823
1458.869933	131483.502587	36.155840
1460.547883	131694.521090	36.160858
1462.035179	131882.285131	36.165876
1463.630582	132075.367097	36.170893
1464.794533	132290.424609	36.175911
1466.304331	132501.159136	36.180928
1467.928120	132697.154871	36.185946
1469.398594	132898.776391	36.190964
1471.222578	133090.067871	36.195981
1472.184071	133319.013595	36.200999
1473.187498	133527.175495	36.206016
1475.213754	133733.567299	36.211034
1476.328491	133944.083890	36.216052
1477.851744	134162.532153	36.221069
1479.200731	134409.657782	36.226087
1480.952035	134600.413446	36.231104
1482.372761	134809.519365	36.236122
1483.873197	135045.311486	36.241140
1485.611559	135263.835330	36.246157
1487.064831	135496.813033	36.251175
1488.599824	135704.500818	36.256192
1490.132178	135925.507918	36.261210
1491.561090	136138.486881	36.266228
1493.066506	136361.959815	36.271245
1494.319106	136578.834786	36.276263
1495.918339	136804.564409	36.281280
1497.601718	137024.884289	36.286298
1499.142362	137247.141941	36.291316
1500.834987	137457.858432	36.296333
1502.116531	137683.670662	36.301351
1503.655570	137923.319608	36.306368
1505.365389	138141.540131	36.311386
1506.617512	138348.189204	36.316404
1508.268865	138576.990880	36.321421
1509.406139	138822.007992	36.326439
1511.119897	139026.953738	36.331456
1512.651118	139261.900622	36.336474
1514.387326	139499.820238	36.341492
1516.269412	139708.216276	36.346509
1517.476322	139943.891730	36.351527
1519.530310	140150.299255	36.356544
1520.482095	140367.325917	36.361562
1521.838856	140614.591404	36.366580
1523.900713	140814.146067	36.371597
1525.463606	141030.484811	36.376615
1526.584556	141232.954516	36.381632
1528.388542	141441.615829	36.386650
1529.622869	141641.522887	36.391668
1530.923263	141836.782197	36.396685
1532.413419	142057.499619	36.401703
1533.888008	142271.465938	36.406720
1535.709749	142478.800831	36.411738
1537.282736	142687.520103	36.416756
1539.053366	142883.750729	36.421773
1539.806342	143114.694217	36.426791
1541.607157	143322.266312	36.431808
1543.664250	143532.029806	36.436826
1544.605382	143747.536103	36.441844
1546.031444	143966.465071	36.446861
1547.832776	144185.792278	36.451879
1549.118147	144401.641395	36.456896
1550.376838	144631.286504	36.461914
1551.613104	144881.913939	36.466932
1553.439098	145094.373855	36.471949
1555.065992	145338.301207	36.476967
1556.391763	145576.739222	36.481984
1558.258302	145817.133898	36.487002
1559.714183	146059.319516	36.492020
1561.373041	146283.462832	36.497037
1562.967341	146527.353962	36.502055
1564.812378	146768.253717	36.507072
1566.192785	147003.423592	36.512090
1567.678913	147233.406657	36.517108
1569.874004	147478.997047	36.522125
1571.196231	147715.005410	36.527143
1572.779916	147955.347294	36.532160
1574.622119	148175.355189	36.537178
1576.160235	148416.620498	36.542196
1577.975351	148653.571665	36.547213
1579.293246	148896.903826	36.552231
1580.741262	149111.732696	36.557248
1581.953672	149359.952972	36.562266
1583.720633	149612.346516	36.567284
1585.673013	149852.289174	36.572301
1587.351773	150093.329275	36.577319
1588.928912	150331.522282	36.582336
1590.791922	150561.304667	36.587354
1592.004520	150806.303358	36.592372
1593.828929	151045.045500	36.597389
1595.537995	151291.186031	36.602407
1597.190466	151523.911820	36.607424
1598.989293	151748.831919	36.612442
1600.359286	151997.922148	36.617460
1602.185000	152225.579659	36.622477
1603.527107	152466.754204	36.627495
1604.874207	152714.649100	36.632512
1606.856391	152945.925355	36.637530
1608.350032	153191.974911	36.642548
1610.252027	153427.020034	36.647565
1611.333795	153663.452254	36.652583
1612.825395	153881.056861	36.657600
1614.400087	154106.117391	36.662618
1615.567944	154346.116153	36.667636
1617.371252	154561.571038	36.672653
1619.043123	154798.855823	36.677671
1620.377353	155034.281387	36.682688
1621.799362	155263.241029	36.687706
1623.528179	155504.262071	36.692724
1625.035129	155745.979390	36.697741
1626.406445	155984.854454	36.702759
1628.072326	156227.691113	36.707776
1629.686397	156472.160714	36.712794
1630.923281	156728.750256	36.717812
1632.995410	156973.252151	36.722829
1634.613317	157228.757892	36.727847
1636.329488	157486.126557	36.732864
1638.163808	157739.420804	36.737882
1639.613445	157996.937065	36.742900
1641.259549	158257.619450	36.747917
1642.731726	158512.676034	36.752935
1644.710981	158772.916314	36.757952
1646.318935	159020.182029	36.762970
1647.504722	159296.783193	36.767988
1649.239914	159554.151560	36.773005
1651.007980	159824.400216	36.778023
1652.732088	160092.438797	36.783040
1654.717114	160350.394711	36.788058
1656.134946	160621.681558	36.793076
1657.635743	160888.252629	36.798093
1659.525563	161159.075545	36.803111
1660.958420	161428.159672	36.808128
1663.104414	161695.534741	36.813146
1664.945285	161955.668419	36.818164
1666.561550	162234.811306	36.823181
1668.560177	162492.983569	36.828199
1669.923910	162763.369599	36.833216
1671.876975	163032.966582	36.838234
1673.755176	163291.962673	36.843252
1675.243701	163553.901326	36.848269
1677.054845	163811.592860	36.853287
1679.035453	164080.584551	36.858304
1681.202225	164334.964002	36.863322
1682.151965	164589.449702	36.868340
1684.289740	164851.865332	36.873357
1686.150430	165109.152347	36.878375
1687.624886	165365.969822	36.883392
1689.239589	165611.973791	36.888410
1691.111137	165876.506313	36.893428
1692.568148	166128.208000	36.898445
1694.509479	166395.675601	36.903463
1695.939945	166652.293396	36.908480
1698.140849	166906.926201	36.913498
1699.755761	167173.309737	36.918516
1701.517932	167422.003838	36.923533
1703.038551	167660.058469	36.928551
1704.443549	167905.781143	36.933568
1706.264061	168128.241104	36.938586
1708.096471	168374.913667	36.943604
1709.620237	168607.710054	36.948621
1710.992548	168854.674423	36.953639
1712.649155	169094.149785	36.958656
1714.127248	169319.905522	36.963674
1715.527801	169591.806975	36.968692
1717.193965	169849.170155	36.973709
1718.760340	170097.646547	36.978727
1720.080087	170352.429777	36.983744
1721.541804	170634.793504	36.988762
1723.730628	170909.686821	36.993780
1725.358487	171176.857423	36.998797
1727.068955	171442.405790	37.003815
1728.821322	171721.471318	37.008832
1730.991656	171987.343620	37.013850
1732.358181	172260.842169	37.018868
1734.061460	172540.542899	37.023885
1736.165227	172818.659817	37.028903
1737.345533	173095.085948	37.033920
1739.356684	173383.889848	37.038938
1740.966985	173676.133816	37.043956
1742.772821	173940.922790	37.048973
1744.527865	174256.020031	37.053991
1746.211315	174523.826107	37.059008
1748.185315	174815.145359	37.064026
1749.989287	175104.032653	37.069044
1751.737708	175395.810553	37.074061
1754.078198	175675.787324	37.079079
1755.297877	175971.687482	37.084096
1757.073096	176260.232376	37.089114
1758.799304	176536.164189	37.094132
1760.541715	176834.765926	37.099149
1762.732964	177118.874014	37.104167
1764.266266	177413.428096	37.109184
1766.144145	177705.569852	37.114202
1767.939754	178002.585767	37.119220
1769.689209	178296.312547	37.124237
1771.995608	178576.327191	37.129255
1773.441257	178872.872017	37.134272
1774.920126	179161.331961	37.139290
1777.321666	179456.917193	37.144308
1778.908786	179757.772146	37.149325
1780.835140	180055.682660	37.154343
1782.258694	180345.517026	37.159360
1784.621356	180620.753144	37.164378
1786.486325	180913.084189	37.169396
1788.024480	181217.535156	37.174413
1790.099829	181492.974747	37.179431
1791.559280	181780.757703	37.184448
1793.343804	182078.400300	37.189466
1794.978377	182363.583669	37.194484
1796.816529	182642.773155	37.199501
1798.625289	182929.899249	37.204519
1800.076799	183212.490761	37.209536
1802.487835	183481.418627	37.214554
1804.404522	183746.125213	37.219572
1806.181558	184005.729379	37.224589
1807.748100	184275.646273	37.229607
1809.339778	184544.774118	37.234624
1811.073901	184826.658591	37.239642
1812.742052	185090.537123	37.244660
1814.449468	185371.972474	37.249677
1815.933161	185657.036094	37.254695
1817.469160	185946.724738	37.259712
1820.078327	186224.050587	37.264730
1821.794390	186503.727827	37.269748
1823.261339	186801.262166	37.274765
1825.295257	187087.617891	37.279783
1827.189761	187374.073674	37.284800
1829.128480	187676.817653	37.289818
1831.181315	187973.797087	37.294836
1832.461513	188260.660437	37.299853
1834.514517	188553.126009	37.304871
1836.442913	188849.953145	37.309888
1838.297612	189155.994107	37.314906
1840.205045	189443.678854	37.319924
1841.711857	189757.583345	37.324941
1844.043074	190028.821419	37.329959
1845.777571	190331.424662	37.334976
1847.582885	190641.696276	37.339994
1849.845469	190945.653621	37.345012
1851.653792	191252.083508	37.350029
1853.112819	191540.461262	37.355047
1855.086529	191847.376314	37.360064
1857.075558	192159.088000	37.365082
1859.466628	192447.577048	37.370100
1861.123294	192746.679770	37.375117
1863.052548	193041.629169	37.380135
1864.931655	193339.913365	37.385152
1866.997367	193656.229290	37.390170
1868.391085	193961.840940	37.395188
1870.326537	194260.629397	37.400205
1872.396549	194551.935746	37.405223
1874.320527	194887.471401	37.410240
1875.934346	195162.342076	37.415258
1878.012616	195495.344372	37.420276
1879.683854	195806.329861	37.425293
1881.877455	196075.922575	37.430311
1883.679106	196418.074833	37.435328
1885.746541	196691.891833	37.440346
1887.768734	196992.053392	37.445364
1889.243741	197322.168023	37.450381
1891.351563	197626.914220	37.455399
1892.891392	197926.624678	37.460416
1894.933651	198233.237895	37.465434
1897.043931	198554.920673	37.470452
1898.727812	198873.271504	37.475469
1900.645120	199154.321911	37.480487
1902.403362	199437.772567	37.485504
1904.131001	199747.122647	37.490522
1906.074651	200005.796186	37.495540
1907.589474	200332.509011	37.500557
1909.450163	200614.413812	37.505575
1911.208588	200907.734580	37.510592
1912.928500	201215.939266	37.515610
1915.035974	201510.045633	37.520628
1916.673707	201842.155296	37.525645
1918.800213	202133.012536	37.530663
1920.549878	202434.225379	37.535680
1922.315778	202779.876796	37.540698
1924.362025	203079.979835	37.545716
1925.869375	203392.901601	37.550733
1927.983064	203722.700229	37.555751
1929.695733	204067.124063	37.560768
1931.702118	204393.008593	37.565786
1933.515998	204700.417952	37.570804
1935.123114	205069.376358	37.575821
1937.559253	205398.257653	37.580839
1939.664064	205713.851963	37.585856
1941.553669	206073.949610	37.590874
1943.540214	206389.794852	37.595892
1945.399256	206740.964755	37.600909
1947.521129	207083.767565	37.605927
1949.722161	207424.198643	37.610944
1951.687967	207746.807866	37.615962
1953.866744	208091.854386	37.620980
1955.538762	208441.261386	37.625997
1957.814285	208771.024823	37.631015
1959.963314	209112.197326	37.636032
1961.979025	209460.806676	37.641050
1963.752336	209794.958890	37.646068
1965.993904	210128.530821	37.651085
1968.245741	210463.397816	37.656103
1970.095837	210809.451273	37.661120
1971.978050	211135.493948	37.666138
1974.385380	211463.778227	37.671156
1976.414704	211804.578287	37.676173
1978.104864	212130.732744	37.681191
1980.262940	212476.175174	37.686208
1982.035133	212806.852334	37.691226
1984.517816	213130.105812	37.696244
1986.231735	213482.632059	37.701261
1988.326502	213795.489186	37.706279
1990.727792	214148.354316	37.711296
1992.742215	214465.518552	37.716314
1994.799079	214796.795405	37.721332
1996.728593	215144.446504	37.726349
1998.697195	215457.179147	37.731367
2000.741259	215783.130583	37.736384
2002.607001	216114.977498	37.741402
2004.757240	216435.659021	37.746420
2006.687905	216778.709608	37.751437
2009.045531	217081.357948	37.756455
2011.144740	217381.255407	37.761472
2012.663971	217687.873710	37.766490
2015.090399	217981.005427	37.771508
2016.638507	218286.250545	37.776525
2018.469128	218585.852965	37.781543
2020.375732	218876.125258	37.786560
2022.058823	219198.417173	37.791578
2024.368820	219504.016420	37.796596
2026.280535	219828.991995	37.801613
2028.259892	220135.509747	37.806631
2030.395241	220455.818288	37.811648
2032.283083	220776.675371	37.816666
2034.421930	221086.193673	37.821684
2036.137821	221417.581254	37.826701
2038.110643	221744.206210	37.831719
2040.486232	222074.704823	37.836736
2042.316084	222396.568444	37.841754
2044.573243	222736.776732	37.846772
2046.121987	223075.257795	37.851789
2048.568632	223402.246416	37.856807
2050.320391	223749.294375	37.861824
2051.938411	224083.731052	37.866842
2054.251818	224450.374189	37.871860
2056.254028	224842.450985	37.876877
2058.183998	225187.229516	37.881895
2060.578893	225543.224084	37.886912
2062.511608	225899.509398	37.891930
2064.583178	226250.187183	37.896948
2066.268946	226614.209694	37.901965
2068.781487	226967.068118	37.906983
2070.746711	227323.468722	37.912000
2072.767557	227694.591800	37.917018
2075.027602	228040.028321	37.922036
2077.007081	228402.373949	37.927053
2079.128939	228769.980996	37.932071
2081.482037	229124.600661	37.937088
2083.535939	229491.358062	37.942106
2085.777794	229857.198296	37.947124
2087.560477	230219.252545	37.952141
2089.847021	230590.320478	37.957159
2092.292541	230945.897880	37.962176
2094.319440	231320.870365	37.967194
2096.353112	231680.655715	37.972212
2098.833267	232034.377862	37.977229
2100.656822	232395.189820	37.982247
2103.564925	232755.475583	37.987264
2105.672248	233102.886107	37.992282
2108.241148	233447.557922	37.997300
2110.397777	233800.068122	38.002317
2112.336086	234141.667704	38.007335
2114.826743	234482.469731	38.012352
2116.423611	234841.625183	38.017370
2118.876655	235175.425679	38.022388
2120.930382	235525.393168	38.027405
2122.823447	235855.500390	38.032423
2124.920968	236175.950225	38.037440
2126.726447	236505.006703	38.042458
2128.854111	236823.472687	38.047476
2130.763899	237152.717866	38.052493
2132.716292	237462.908210	38.057511
2134.898633	237798.309489	38.062528
2136.694395	238132.985764	38.067546
2138.872270	238467.170694	38.072564
2140.967136	238810.132516	38.077581
2142.783467	239155.501710	38.082599
2144.992076	239487.500543	38.087616
2146.842389	239848.106069	38.092634
2148.598871	240193.386364	38.097652
2150.613354	240553.790301	38.102669
2152.416928	240923.702867	38.107687
2154.954768	241292.052380	38.112704
2157.232904	241670.375541	38.117722
2159.199781	242037.751137	38.122740
2161.226604	242422.085496	38.127757
2163.522838	242801.196746	38.132775
2165.781865	243171.983840	38.137792
2168.124414	243557.033682	38.142810
2170.569369	243942.068464	38.147828
2172.411121	244326.234856	38.152845
2174.566238	244706.491842	38.157863
2177.320024	245079.085663	38.162880
2179.449473	245475.325835	38.167898
2181.577846	245859.552866	38.172916
2183.959565	246236.806428	38.177933
2186.027155	246619.826010	38.182951
2188.283168	247006.423684	38.187968
2190.357201	247387.894899	38.192986
2192.746331	247767.894714	38.198004
2195.488911	248158.101492	38.203021
2197.520925	248545.500862	38.208039
2200.041758	248913.671264	38.213056
2201.861505	249303.239950	38.218074
2204.369297	249685.080144	38.223092
2206.353368	250067.486949	38.228109
2208.916977	250452.114315	38.233127
2211.153108	250825.897310	38.238144
2213.405148	251221.117524	38.243162
2215.437195	251608.321269	38.248180
2217.658708	251990.110721	38.253197
2219.592311	252381.421513	38.258215
2222.094371	252760.678833	38.263232
2224.330181	253159.005139	38.268250
2226.238553	253545.724798	38.273268
2228.666757	253935.538095	38.278285
2230.934746	254323.929705	38.283303
2233.401843	254727.861983	38.288320
2235.292743	255110.751950	38.293338
2237.746131	255503.815937	38.298356
2240.149725	255896.380552	38.303373
2241.723061	256278.916680	38.308391
2244.441174	256629.392173	38.313408
2246.828423	257008.295078	38.318426
2248.594053	257353.867725	38.323444
2250.976647	257719.385578	38.328461
2252.783234	258088.373879	38.333479
2255.207416	258443.979368	38.338496
2257.262407	258828.069339	38.343514
2259.674907	259190.917526	38.348532
2262.335044	259563.786417	38.353549
2263.975766	259956.250497	38.358567
2266.605947	260317.313038	38.363584
2268.473070	260717.109154	38.368602
2270.567992	261095.277429	38.373620
2272.797462	261479.064309	38.378637
2274.939733	261867.260223	38.383655
2277.319997	262273.886788	38.388672
2279.444329	262667.573618	38.393690
2281.749487	263069.081784	38.398708
2284.160019	263462.470219	38.403725
2286.399121	263875.065545	38.408743
2289.015614	264271.953303	38.413760
2291.129457	264679.361843	38.418778
2293.619495	265090.343840	38.423796
2295.590128	265482.965997	38.428813
2297.930332	265904.794338	38.433831
2300.440022	266316.765238	38.438848
2302.463155	266737.247522	38.443866
2305.017142	267148.958165	38.448884
2307.730394	267557.595545	38.453901
2309.508474	267995.442803	38.458919
2312.071606	268398.515965	38.463936
2314.336989	268821.984640	38.468954
2316.520563	269254.129118	38.473972
2319.289479	269670.481878	38.478989
2321.663785	270104.959215	38.484007
2323.953590	270517.273117	38.489024
2326.126213	270940.097401	38.494042
2328.391087	271361.637116	38.499060
2331.062687	271781.816988	38.504077
2332.953191	272219.496767	38.509095
2335.486482	272629.893211	38.514112
2338.117699	273072.841420	38.519130
2340.659625	273501.501809	38.524148
2342.787442	273917.856495	38.529165
2345.414093	274355.496466	38.534183
2347.782933	274776.614354	38.539200
2349.913993	275195.737712	38.544218
2352.290095	275625.948960	38.549236
2354.902837	276051.931153	38.554253
2356.901292	276481.948240	38.559271
2359.703478	276903.581801	38.564288
2361.973562	277332.565039	38.569306
2364.353572	277745.374226	38.574324
2366.974639	278170.999254	38.579341
2369.514133	278583.706787	38.584359
2371.998558	278988.243049	38.589376
2374.135647	279375.204299	38.594394
2376.687780	279764.004894	38.599412
2379.074376	280127.987098	38.604429
2381.176232	280530.474976	38.609447
2383.281731	280916.272101	38.614464
2385.665430	281309.798372	38.619482
2387.850750	281700.790149	38.624500
2390.251661	282117.658909	38.629517
2392.182195	282522.382980	38.634535
2394.184693	282928.543369	38.639552
2397.043204	283342.900074	38.644570
2399.062168	283755.433481	38.649588
2401.636441	284173.264035	38.654605
2403.730936	284603.744854	38.659623
2406.202907	285025.121933	38.664640
2408.914274	285457.587252	38.669658
2411.012723	285885.398895	38.674676
2413.474334	286312.720686	38.679693
2416.041506	286753.641324	38.684711
2418.383239	287198.026586	38.689728
2420.703121	287635.657573	38.694746
2423.433654	288079.522869	38.699764
2426.241715	288520.835003	38.704781
2428.267742	288962.753129	38.709799
2430.683987	289403.821306	38.714816
2433.432626	289853.676348	38.719834
2435.609861	290298.210464	38.724852
2438.235078	290737.414529	38.729869
2440.869008	291197.827767	38.734887
2443.467747	291648.618188	38.739904
2445.998637	292080.595250	38.744922
2448.312570	292529.320844	38.749940
2451.101452	292976.242988	38.754957
2453.640566	293428.462192	38.759975
2455.807175	293874.693777	38.764992
2458.425108	294313.130651	38.770010
2460.789696	294769.744062	38.775028
2463.115741	295218.665737	38.780045
2465.785352	295667.684434	38.785063
2468.582130	296113.252718	38.790080
2470.870776	296577.875907	38.795098
2473.220455	297036.239436	38.800116
2476.162036	297467.429585	38.805133
2478.672362	297925.384506	38.810151
2481.016663	298377.776201	38.815168
2484.444689	298816.989337	38.820186
2486.817498	299265.691031	38.825204
2489.448669	299706.958756	38.830221
2491.730397	300146.477206	38.835239
2493.971575	300570.709216	38.840256
2496.810399	301002.897711	38.845274
2499.218616	301453.899522	38.850292
2502.006368	301885.611125	38.855309
2504.237312	302315.657084	38.860327
2506.567092	302728.387982	38.865344
2509.288934	303123.478070	38.870362
2511.376354	303538.912280	38.875380
2513.845664	303932.770186	38.880397
2516.165479	304351.518209	38.885415
2518.179602	304753.929909	38.890432
2520.864857	305178.002588	38.895450
2523.242140	305599.811313	38.900468
2525.584894	306023.427662	38.905485
2527.974183	306458.414753	38.910503
2530.414051	306901.774562	38.915520
2532.849536	307326.870723	38.920538
2535.272136	307778.434619	38.925556
2537.734017	308222.396051	38.930573
2539.952267	308675.208356	38.935591
2542.404549	309130.115540	38.940608
2545.340080	309588.652869	38.945626
2547.985551	310049.571203	38.950644
2550.323654	310509.088677	38.955661
2553.012969	310970.580692	38.960679
2555.186492	311446.630311	38.965696
2557.925431	311908.059932	38.970714
2560.568454	312378.113235	38.975732
2562.856057	312860.183889	38.980749
2565.708644	313345.210827	38.985767
2568.287485	313820.322587	38.990784
2571.192116	314281.665267	38.995802
2573.801097	314786.256030	39.000820
2576.430402	315248.273083	39.005837
2578.955519	315735.169717	39.010855
2581.645016	316223.612702	39.015872
2584.248761	316697.132746	39.020890
2586.841962	317196.710706	39.025908
2589.602746	317669.261523	39.030925
2592.053862	318149.376886	39.035943
2594.864707	318653.103587	39.040960
2597.460108	319129.711711	39.045978
2599.957552	319633.609853	39.050996
2603.325703	320101.150732	39.056013
2606.088831	320579.477318	39.061031
2608.537567	321071.845000	39.066048
2611.517452	321529.382838	39.071066
2614.330487	322002.995562	39.076084
2617.254059	322469.832730	39.081101
2619.864780	322943.345469	39.086119
2622.732239	323413.538825	39.091136
2625.489402	323873.461591	39.096154
2627.757696	324357.357071	39.101172
2630.946311	324803.721105	39.106189
2633.412227	325267.720367	39.111207
2635.993296	325725.451444	39.116224
2638.748764	326194.656536	39.121242
2640.977832	326651.498539	39.126260
2643.866385	327101.122817	39.131277
2646.523559	327577.649260	39.136295
2648.723790	328001.525221	39.141312
2651.212334	328423.677165	39.146330
2653.638030	328864.247941	39.151348
2656.242696	329298.769342	39.156365
2659.122646	329733.854143	39.161383
2660.983330	330182.455270	39.166400
2663.721309	330628.400759	39.171418
2666.240020	331076.587587	39.176436
2668.723423	331518.962111	39.181453
2671.226591	331988.984532	39.186471
2673.752900	332459.660486	39.191488
2676.607094	332921.901647	39.196506
2678.632743	333404.204674	39.201524
2680.893754	333880.702945	39.206541
2683.886164	334359.494476	39.211559
2686.317233	334862.342268	39.216576
2689.406120	335353.350923	39.221594
2692.134002	335849.974147	39.226612
2694.864701	336343.673216	39.231629
2697.341490	336835.123619	39.236647
2700.286772	337352.802023	39.241664
2703.278451	337845.940860	39.246682
2705.891620	338369.275431	39.251700
2708.314810	338869.123739	39.256717
2711.317538	339361.462273	39.261735
2713.780199	339907.990159	39.266752
2716.641622	340397.626303	39.271770
2719.613305	340907.299536	39.276788
2722.651897	341423.280169	39.281805
2725.194062	341945.403321	39.286823
2728.100014	342461.802563	39.291840
2731.021349	342957.502621	39.296858
2733.835783	343482.057747	39.301876
2736.205094	344016.885186	39.306893
2739.535478	344505.475013	39.311911
2742.213528	345029.936638	39.316928
2744.926647	345543.267954	39.321946
2747.850050	346078.369876	39.326964
2750.576386	346581.255456	39.331981
2753.594497	347101.937992	39.336999
2756.349724	347629.435870	39.342016
2759.267249	348134.460870	39.347034
2762.052638	348652.119607	39.352052
2764.502605	349167.592646	39.357069
2767.574971	349687.938120	39.362087
2770.338386	350208.530707	39.367104
2773.135474	350723.248856	39.372122
2775.964920	351244.100384	39.377140
2778.845321	351757.297788	39.382157
2781.821140	352264.306559	39.387175
2784.383686	352785.033116	39.392192
2787.194369	353294.672884	39.397210
2790.102117	353802.515438	39.402228
2792.847218	354341.017682	39.407245
2796.020453	354821.647077	39.412263
2798.779505	355306.678214	39.417280
2801.375932	355782.262440	39.422298
2804.047481	356256.129659	39.427316
2806.627029	356720.539117	39.432333
2809.577123	357184.961785	39.437351
2812.015621	357681.773259	39.442368
2814.714161	358149.526542	39.447386
2817.389787	358638.320846	39.452404
2819.830354	359135.371251	39.457421
2823.144675	359622.988606	39.462439
2825.535250	360125.240091	39.467456
2827.952283	360635.045749	39.472474
2830.897185	361138.797942	39.477492
2833.576258	361649.211244	39.482509
2836.277025	362169.412427	39.487527
2839.046680	362694.876022	39.492544
2841.915563	363217.196326	39.497562
2844.744080	363755.709259	39.502580
2847.543590	364287.571202	39.507597
2850.496477	364824.402365	39.512615
2853.095283	365360.699589	39.517632
2855.783147	365909.893931	39.522650
2859.197865	366459.118820	39.527668
2861.891317	367008.197408	39.532685
2865.061193	367560.518269	39.537703
2867.662531	368117.261735	39.542720
2870.575205	368666.944946	39.547738
2873.780745	369214.417930	39.552756
2876.702110	369779.336994	39.557773
2879.800993	370317.093982	39.562791
2882.486058	370888.988916	39.567808
2885.322386	371433.421862	39.572826
2888.405054	371996.713036	39.577844
2891.143606	372560.507936	39.582861
2894.383620	373124.215923	39.587879
2897.185580	373696.105248	39.592896
2899.982971	374255.605256	39.597914
2903.369505	374809.980601	39.602932
2905.767743	375390.790989	39.607949
2908.952486	375960.558567	39.612967
2911.855237	376527.445033	39.617984
2915.051835	377086.386489	39.623002
2918.064144	377668.513287	39.628020
2920.713580	378239.982554	39.633037
2924.145170	378786.482100	39.638055
2926.933026	379358.268548	39.643072
2930.174017	379920.715007	39.648090
2933.393633	380473.085111	39.653108
2936.521919	381038.679114	39.658125
2939.286873	381595.494062	39.663143
2942.205677	382149.207049	39.668160
2945.501028	382707.596250	39.673178
2948.268256	383252.514567	39.678196
2951.174030	383812.521992	39.683213
2954.285893	384351.078876	39.688231
2957.222196	384875.704250	39.693248
2959.802554	385384.017428	39.698266
2962.934692	385905.350452	39.703284
2965.757434	386430.682104	39.708301
2968.084469	386947.156208	39.713319
2971.117780	387459.402181	39.718336
2974.104133	387982.757984	39.723354
2976.737963	388513.999506	39.728372
2979.676452	389046.174189	39.733389
2982.495810	389589.139226	39.738407
2984.983520	390137.144993	39.743424
2987.738450	390689.563835	39.748442
2991.184409	391245.998731	39.753460
2993.583680	391816.108241	39.758477
2996.565317	392383.808468	39.763495
2999.324332	392955.516346	39.768512
3002.521744	393526.790405	39.773530
3005.286519	394111.919314	39.778548
3008.078833	394706.188708	39.783565
3011.359057	395288.984357	39.788583
3013.988160	395891.957121	39.793600
3017.063865	396483.386592	39.798618
3020.738528	397082.571822	39.803636
3023.462570	397693.713274	39.808653
3026.558580	398296.746576	39.813671
3029.511377	398916.298587	39.818688
3032.574662	399520.886895	39.823706
3035.799063	400134.744040	39.828724
3038.647400	400753.060938	39.833741
3042.083818	401366.912085	39.838759
3045.169479	401991.379711	39.843776
3047.983961	402608.677768	39.848794
3051.704509	403236.950554	39.853812
3054.647994	403848.373112	39.858829
3057.710639	404466.204465	39.863847
3060.891063	405088.162760	39.868864
3063.973883	405715.802831	39.873882
3067.218297	406347.029877	39.878900
3070.103741	406964.840098	39.883917
3073.400216	407576.387712	39.888935
3076.637920	408203.750266	39.893952
3080.048613	408828.132222	39.898970
3083.566572	409433.118636	39.903988
3086.495933	410058.996385	39.909005
3089.603062	410670.258613	39.914023
3092.650242	411288.437500	39.919040
3095.736204	411916.963979	39.924058
3099.131927	412519.069083	39.929076
3102.202315	413139.461740	39.934093
3105.563934	413737.695101	39.939111
3108.434699	414366.001004	39.944128
3111.251986	414979.476128	39.949146
3114.832535	415581.337379	39.954164
3117.745118	416208.101831	39.959181
3121.040780	416791.508609	39.964199
3123.997893	417376.756360	39.969216
3127.255178	417950.820162	39.974234
3130.409537	418511.585156	39.979252
3133.091569	419081.105317	39.984269
3136.302421	419653.748458	39.989287
3139.146341	420232.899375	39.994304
3141.832657	420812.544726	39.999322
3144.993185	421402.187414	40.004340
3147.698134	421990.192130	40.009357
3150.743486	422593.332433	40.014375
3153.685990	423200.580277	40.019392
3156.850518	423810.363826	40.024410
3159.962288	424418.014053	40.029428
3162.498083	425048.238641	40.034445
3165.734723	425667.089662	40.039463
3169.239180	426294.446751	40.044480
3171.769540	426933.216262	40.049498
3175.243387	427567.058976	40.054516
3178.348632	428219.842058	40.059533
3181.344013	428878.553880	40.064551
3184.582993	429537.312135	40.069568
3187.946122	430192.614866	40.074586
3191.379735	430856.121939	40.079604
3194.273463	431520.609399	40.084621
3197.348307	432184.443420	40.089639
3200.701120	432862.830023	40.094656
3203.524868	433550.222593	40.099674
3207.230202	434222.642024	40.104692
3210.433784	434905.354345	40.109709
3213.666609	435589.715155	40.114727
3216.735139	436277.071662	40.119744
3220.068461	436963.228089	40.124762
3223.252262	437650.706206	40.129780
3226.729840	438356.502237	40.134797
3229.858733	439047.090493	40.139815
3233.808270	439731.199812	40.144832
3236.646436	440432.505756	40.149850
3239.874189	441118.741628	40.154868
3243.389264	441819.951582	40.159885
3246.418610	442515.749759	40.164903
3250.099413	443218.564190	40.169920
3253.178208	443918.820618	40.174938
3256.763550	444612.749176	40.179956
3259.714855	445319.313713	40.184973
3263.414029	445993.034329	40.189991
3266.576789	446710.408970	40.195008
3269.554121	447419.995206	40.200026
3273.180529	448094.528234	40.205044
3276.899185	448805.929781	40.210061
3279.985099	449512.803444	40.215079
3283.335550	450208.376761	40.220096
3286.839492	450888.214003	40.225114
3290.038262	451597.840889	40.230132
3293.127293	452299.263978	40.235149
3296.311734	452971.194673	40.240167
3300.075889	453626.059594	40.245184
3302.909970	454285.152047	40.250202
3305.665522	454954.662839	40.255220
3309.299783	455594.461181	40.260237
3312.671821	456264.240485	40.265255
3315.719638	456931.014903	40.270272
3318.319735	457592.780113	40.275290
3321.663603	458267.310966	40.280308
3324.955960	458945.270126	40.285325
3328.152211	459620.086703	40.290343
3331.329488	460290.483841	40.295360
3334.198471	461014.082861	40.300378
3337.600968	461684.654671	40.305396
3340.710606	462410.800082	40.310413
3344.019979	463122.218972	40.315431
3347.357200	463813.577678	40.320448
3350.683625	464550.341292	40.325466
3354.032770	465284.243327	40.330484
3357.310888	466009.026682	40.335501
3360.456230	466742.202584	40.340519
3364.357079	467488.990903	40.345536
3367.533305	468214.625309	40.350554
3370.727994	468997.886667	40.355572
3374.281279	469707.428298	40.360589
3377.515960	470492.599634	40.365607
3381.102099	471221.807033	40.370624
3384.305155	472000.503987	40.375642
3387.909793	472760.449461	40.380660
3391.226472	473508.074851	40.385677
3394.579010	474302.082682	40.390695
3398.786006	475052.493850	40.395712
3401.811165	475831.174134	40.400730
3405.365022	476598.466911	40.405748
3408.892550	477380.041303	40.410765
3412.314489	478118.076794	40.415783
3415.821209	478917.034809	40.420800
3419.433446	479665.042334	40.425818
3423.097683	480464.570280	40.430836
3426.371859	481207.063402	40.435853
3429.685308	482011.537312	40.440871
3432.720900	482772.507240	40.445888
3436.967944	483522.744090	40.450906
3440.210325	484347.954529	40.455924
3443.914018	485088.058999	40.460941
3447.262563	485891.052884	40.465959
3450.786618	486655.279673	40.470976
3454.356636	487438.062895	40.475994
3457.966900	488209.085660	40.481012
3461.544843	488970.129077	40.486029
3464.488925	489764.737887	40.491047
3468.418412	490529.906701	40.496064
3472.012708	491291.813688	40.501082
3475.349286	492068.884997	40.506100
3479.073801	492841.366931	40.511117
3482.808380	493584.571508	40.516122
3486.228690	494288.628005	40.521127
3489.191527	494969.589026	40.526132
3492.801276	495547.076831	40.531136
3495.724824	496109.971204	40.536141
3498.081427	496574.002869	40.541146
3500.831874	496980.595612	40.546151
3503.088889	497374.296000	40.551156
3505.587849	497675.197338	40.556160
3507.740056	497939.594841	40.561165
3509.425037	498163.307039	40.566170
3511.249744	498287.613082	40.571175
3512.466674	498436.568426	40.576180
3513.773643	498516.605428	40.581184
3514.982000	498553.068163	40.586189
3516.300939	498568.958957	40.591194
3517.240515	498550.989861	40.596199
3517.773056	498516.479507	40.601204
3518.576237	498434.590148	40.606208
3519.179096	498337.695791	40.611213
3519.746612	498220.555481	40.616218
3520.607382	498066.561544	40.621223
3520.865384	497968.656532	40.626228
3520.952913	497766.989096	40.631232
3521.612090	497577.835800	40.636237
3521.430285	497388.762816	40.641242
3521.828221	497175.344258	40.646247
3521.857785	496980.765541	40.651252
3521.947391	496769.011150	40.656256
3521.674225	496522.831071	40.661261
3521.567242	496309.330290	40.666266
3521.498851	496057.541966	40.671271
3521.430127	495865.549225	40.676276
3521.356043	495585.805266	40.681280
3521.619453	495361.753486	40.686285
3521.175623	495135.734666	40.691290
3521.208137	494874.242663	40.696295
3521.371189	494632.576235	40.701300
3520.792852	494409.152268	40.706304
3520.712257	494143.059703	40.711309
3520.616555	493901.120762	40.716314
3519.868181	493649.609528	40.721319
3519.949412	493420.904077	40.726324
3519.357252	493185.009858	40.731328
3519.725420	492922.069887	40.736333
3519.401524	492718.082537	40.741338
3519.381226	492476.062455	40.746343
3518.967153	492253.548770	40.751348
3518.618934	492001.901347	40.756352
3518.544259	491792.445495	40.761357
3517.933777	491562.256529	40.766362
3518.053515	491345.218704	40.771367
3517.667109	491119.901590	40.776372
3517.288399	490915.092854	40.781376
3517.380451	490717.298227	40.786381
3516.839293	490488.047426	40.791386
3516.856905	490298.971750	40.796391
3516.472283	490098.713486	40.801396
3516.416359	489883.560581	40.806400
3516.074230	489713.529778	40.811405
3515.974127	489506.027829	40.816410
3515.531780	489332.058618	40.821415
3514.971632	489140.428743	40.826420
3514.624009	488961.071994	40.831424
3515.157629	488764.048201	40.836429
3514.286611	488628.434208	40.841434
3514.532587	488428.261200	40.846439
3513.901402	488292.556248	40.851444
3513.816877	488094.255523	40.856448
3513.789026	487970.914095	40.861453
3513.790237	487782.727676	40.866458
3513.683540	487652.710052	40.871463
3513.332129	487507.482540	40.876468
3513.179356	487346.366837	40.881472
3513.327053	487174.006952	40.886477
3512.763138	487026.580429	40.891482
3512.689236	486864.536353	40.896487
3512.335352	486776.041060	40.901492
3511.975193	486624.526539	40.906496
3512.563603	486452.951713	40.911501
3511.656806	486365.909716	40.916506
3511.686848	486236.215468	40.921511
3511.061673	486099.632752	40.926516
3511.322131	485980.944346	40.931520
3511.153697	485877.622639	40.936525
3511.030344	485735.638613	40.941530
3510.818933	485650.763235	40.946535
3510.673729	485504.677363	40.951540
3510.723750	485408.411296	40.956544
3510.617169	485290.840553	40.961549
3510.074475	485212.196436	40.966554
3509.917948	485092.099234	40.971559
3510.507293	484968.286297	40.976564
3509.669655	484888.116907	40.981568
3509.962030	484814.405556	40.986573
3509.459217	484706.874656	40.991578
3509.805546	484589.886698	40.996583
3509.256765	484541.284804	41.001588
3509.449903	484423.053435	41.006592
3509.332578	484339.424043	41.011597
3509.238394	484251.636075	41.016602
3509.154106	484198.045370	41.021607
3508.787757	484091.249463	41.026612
3508.975295	483993.485312	41.031616
3508.841670	483957.888165	41.036621
3508.413248	483874.508599	41.041626
3508.163635	483777.521778	41.046631
3508.181799	483696.097527	41.051636
3508.382058	483658.521724	41.056640
3508.336574	483561.906901	41.061645
3507.542309	483520.738644	41.066650
3508.105371	483421.594918	41.071655
3507.819749	483406.287771	41.076660
3507.897522	483308.334852	41.081664
3507.633622	483272.098356	41.086669
3507.535126	483192.109135	41.091674
3507.615164	483153.791337	41.096679
3507.333235	483092.527253	41.101684
3507.392348	483028.523644	41.106688
3507.260254	482983.044106	41.111693
3507.364678	482912.192687	41.116698
3507.237907	482880.088632	41.121703
3507.490599	482789.553789	41.126708
3507.358993	482783.696937	41.131712
3507.311113	482699.542825	41.136717
3507.138318	482667.800380	41.141722
3507.021776	482593.081178	41.146727
3506.609598	482581.593606	41.151732
3506.550069	482513.198796	41.156736
3506.862518	482488.523818	41.161741
3506.454347	482432.496614	41.166746
3506.724041	482394.400702	41.171751
3506.901847	482335.341738	41.176756
3506.567517	482322.574953	41.181760
3506.584725	482251.430900	41.186765
3506.728248	482191.971558	41.191770
3506.786418	482155.884770	41.196775
3506.722829	482145.355264	41.201780
3506.542796	482077.282000	41.206784
3506.897587	482047.735360	41.211789
3506.741583	482025.870074	41.216794
3506.892769	481953.538330	41.221799
3506.452497	481926.600058	41.226804
3506.488144	481853.374120	41.231808
3506.521200	481859.753481	41.236813
3506.703619	481794.966274	41.241818
3506.297298	481744.966743	41.246823
3506.532171	481719.897684	41.251828
3506.374182	481682.121342	41.256832
3506.803430	481602.194226	41.261837
3506.221066	481613.332775	41.266842
3506.301286	481546.990065	41.271847
3506.464281	481531.813233	41.276852
3505.955387	481477.674095	41.281856
3505.879705	481480.422342	41.286861
3505.754692	481434.938087	41.291866
3506.331379	481368.110927	41.296871
3506.113201	481375.492936	41.301876
3505.800408	481332.622435	41.306880
3506.327374	481295.091804	41.311885
3505.882463	481266.987880	41.316890
3505.898876	481229.841854	41.321895
3505.557941	481205.015164	41.326900
3505.606545	481160.718993	41.331904
3505.509678	481165.294873	41.336909
3505.905238	481114.964309	41.341914
3505.481908	481109.659795	41.346919
3505.645217	481060.581962	41.351924
3505.405669	481065.028395	41.356928
3505.612225	481008.443903	41.361933
3505.487216	481019.713197	41.366938
3505.089979	480997.580850	41.371943
3505.764909	480963.522693	41.376948
3505.644094	480929.336873	41.381952
3505.425694	480927.597771	41.386957
3505.144250	480892.727839	41.391962
3505.741891	480845.861158	41.396967
3505.037569	480861.428056	41.401972
3505.658628	480811.871865	41.406976
3505.369883	480825.903557	41.411981
3505.003940	480772.753368	41.416986
3505.007927	480806.147075	41.421991
3505.166018	480764.974514	41.426996
3505.524600	480735.982725	41.432000
3505.048904	480742.544204	41.437005
3505.348932	480682.447468	41.442010
3505.332495	480702.010414	41.447015
3505.437170	480661.048776	41.452020
3504.840452	480663.676787	41.457024
3505.348979	480609.931880	41.462029
3505.029951	480628.225178	41.467034
3505.225123	480581.320130	41.472039
3505.094040	480574.043638	41.477044
3505.151480	480560.504337	41.482048
3505.457564	480553.665494	41.487053
3504.784653	480532.995090	41.492058
3504.991570	480495.412173	41.497063
3505.064554	480513.187545	41.502068
3505.143089	480477.145134	41.507072
3505.384706	480462.664505	41.512077
3505.210145	480456.306994	41.517082
3505.338235	480430.949122	41.522087
3505.257302	480401.924957	41.527092
3505.327739	480396.440860	41.532096
3505.671726	480364.967744	41.537101
3504.906039	480366.304937	41.542106
3505.396053	480317.274972	41.547111
3505.395074	480312.156868	41.552116
3505.345149	480309.935004	41.557120
3505.273883	480254.912528	41.562125
3505.206078	480274.737394	41.567130
3505.082952	480228.287218	41.572135
3505.133733	480260.154180	41.577140
3504.919039	480209.917759	41.582144
3505.174311	480189.252325	41.587149
3504.424360	480191.347180	41.592154
3504.990208	480156.696765	41.597159
3505.440176	480176.541248	41.602164
3505.149829	480129.306455	41.607168
3505.172592	480124.792662	41.612173
3505.486194	480092.057014	41.617178
3505.120090	480088.972927	41.622183
3504.924624	480068.885366	41.627188
3505.050570	480042.361784	41.632192
3505.100673	480049.397828	41.637197
3504.851883	480026.227403	41.642202
3504.826474	480016.501543	41.647207
3505.254613	479962.210144	41.652212
3504.757556	479980.329471	41.657216
3504.997091	479965.848809	41.662221
3505.192974	479932.371355	41.667226
3504.947946	479955.214464	41.672231
3504.860171	479908.808628	41.677236
3504.885996	479910.375489	41.682240
3505.023133	479888.968264	41.687245
3505.080688	479881.560350	41.692250
3504.929755	479835.620414	41.697255
3504.946375	479847.982880	41.702260
3504.874633	479801.878320	41.707264
3504.998985	479830.744412	41.712269
3505.044832	479789.992976	41.717274
3504.942506	479799.688396	41.722279
3505.012739	479767.396091	41.727284
3504.703253	479763.036081	41.732288
3504.982976	479750.728018	41.737293
3504.718447	479729.333426	41.742298
3504.751747	479731.557921	41.747303
3505.088013	479697.905854	41.752308
3504.680105	479715.909978	41.757312
3504.883332	479670.673842	41.762317
3504.716752	479702.677409	41.767322
3504.835748	479655.782207	41.772327
3504.809681	479677.324098	41.777332
3504.951092	479663.314818	41.782336
3504.806415	479641.951867	41.787341
3504.555846	479624.001008	41.792346
3504.478749	479632.678977	41.797351
3504.739718	479599.596093	41.802356
3504.670099	479596.313037	41.807360
3504.906177	479579.501481	41.812365
3504.493324	479598.063945	41.817370
3504.448986	479553.322764	41.822375
3504.586003	479595.160626	41.827380
3503.962717	479580.664018	41.832384
3504.887174	479533.033096	41.837389
3504.421629	479548.816669	41.842394
3504.414930	479569.392745	41.847399
3504.361877	479549.839601	41.852404
3504.594215	479519.142950	41.857408
3504.843335	479512.211397	41.862413
3504.750729	479534.929544	41.867418
3504.471326	479509.584219	41.872423
3505.022311	479484.208976	41.877428
3504.622384	479495.167844	41.882432
3504.592999	479444.798839	41.887437
3504.494873	479498.583336	41.892442
3504.566700	479456.306779	41.897447
3504.933047	479475.455695	41.902452
3504.765937	479438.892763	41.907456
3504.729355	479457.446567	41.912461
3504.592830	479416.165732	41.917466
3504.936201	479389.404202	41.922471
3504.740007	479430.332194	41.927476
3504.335647	479391.880917	41.932480
3505.010118	479347.785835	41.937485
3504.711897	479374.286834	41.942490
3504.654696	479366.694153	41.947495
3504.567911	479340.862068	41.952500
3504.583337	479334.220778	41.957504
3504.985197	479314.696861	41.962509
3504.452726	479338.548992	41.967514
3504.898760	479279.843910	41.972519
3504.780400	479317.617787	41.977524
3504.582170	479292.259355	41.982528
3504.827439	479298.099223	41.987533
3504.878479	479258.308759	41.992538
3504.718511	479284.078532	41.997543
3504.664537	479238.172566	42.002548
3504.839925	479266.017848	42.007552
3504.962047	479226.368121	42.012557
3504.641471	479228.091140	42.017562
3504.980973	479209.083758	42.022567
3504.622896	479206.454368	42.027572
3504.772033	479192.088786	42.032576
3504.899570	479168.199060	42.037581
3504.527831	479174.288517	42.042586
3504.387544	479138.075541	42.047591
3504.544735	479142.409020	42.052596
3504.766983	479145.921360	42.057600
3504.456428	479131.831102	42.062605
3504.325953	479122.374802	42.067610
3504.349527	479108.434433	42.072615
3504.420539	479110.906430	42.077620
3504.192380	479099.995879	42.082624
3504.410940	479111.617386	42.087629
3504.317066	479123.643016	42.092634
3504.491782	479074.305064	42.097639
3504.357374	479105.493649	42.102644
3504.414569	479079.081003	42.107648
3504.377642	479101.942880	42.112653
3504.230390	479078.805978	42.117658
3504.079023	479112.987273	42.122663
3504.586696	479065.573141	42.127668
3504.239368	479088.281378	42.132672
3504.388889	479039.910217	42.137677
3504.548365	479065.376392	42.142682
3504.224636	479047.284537	42.147687
3504.376332	479079.492198	42.152692
3504.399000	479022.779060	42.157696
3504.566672	479041.503686	42.162701
3504.300383	479024.669701	42.167706
3504.275167	479051.229340	42.172711
3504.933837	479017.829239	42.177716
3504.119748	479026.928026	42.182720
3504.691757	478974.739701	42.187725
3504.711226	479019.992841	42.192730
3504.658965	478980.319505	42.197735
3504.818516	479003.150443	42.202740
3504.697702	478958.876121	42.207744
3504.725270	478979.244676	42.212749
3504.706069	478936.778686	42.217754
3504.368783	478958.775976	42.222759
3504.667970	478929.588220	42.227764
3504.628720	478943.987241	42.232768
3504.578682	478924.280968	42.237773
3504.529543	478910.149237	42.242778
3504.310801	478912.717733	42.247783
3504.785673	478909.956657	42.252788
3504.909895	478892.351333	42.257792
3504.683601	478858.432004	42.262797
3504.507232	478878.782214	42.267802
3504.863789	478874.924890	42.272807
3505.072781	478828.520306	42.277812
3504.637151	478851.952278	42.282816
3504.444791	478829.683762	42.287821
3504.655391	478813.635776	42.292826
3504.638186	478794.633696	42.297831
3504.446411	478810.577302	42.302836
3504.325563	478794.733723	42.307840
3504.239748	478784.459334	42.312845
3504.388145	478789.503792	42.317850
3504.214004	478766.117378	42.322855
3504.565078	478769.305347	42.327860
3504.261071	478793.223380	42.332864
3504.808282	478771.040629	42.337869
3504.629847	478752.266709	42.342874
3504.237015	478729.776368	42.347879
3504.446635	478746.112702	42.352884
3504.361501	478731.023621	42.357888
3504.252749	478751.718031	42.362893
3504.390718	478730.309428	42.367898
3504.249157	478719.993135	42.372903
3504.617525	478702.653135	42.377908
3504.066243	478708.973828	42.382912
3504.163148	478722.033820	42.387917
3504.600624	478713.501154	42.392922
3503.955533	478725.107347	42.397927
3504.496421	478695.475611	42.402932
3503.909247	478705.096156	42.407936
3504.257173	478680.258779	42.412941
3504.329706	478686.734285	42.417946
3504.194380	478701.655463	42.422951
3504.675005	478701.528790	42.427956
3504.987215	478699.908347	42.432960
3504.549030	478686.851537	42.437965
3504.924914	478678.936747	42.442970
3504.829472	478669.373335	42.447975
3504.671086	478644.818655	42.452980
3504.508819	478648.847973	42.457984
3504.690023	478635.085079	42.462989
3504.385379	478627.176465	42.467994
3504.170637	478606.026193	42.472999
3504.461363	478611.098881	42.478004
3504.306794	478602.203620	42.483008
3504.202960	478598.419007	42.488013
3504.225295	478614.734369	42.493018
3504.517601	478603.538567	42.498023
3504.369143	478572.140442	42.503028
3504.073381	478578.522151	42.508032
3504.415148	478569.953871	42.513037
3504.312545	478566.827897	42.518042
3504.382732	478578.118407	42.523047
3504.429096	478571.269253	42.528052
3504.504233	478586.410653	42.533056
3504.814125	478541.003051	42.538061
3504.535581	478563.548974	42.543066
3504.495504	478542.624429	42.548071
3504.461090	478526.361535	42.553076
3504.336815	478526.431826	42.558080
3504.373683	478515.681787	42.563085
3504.483215	478515.917845	42.568090
3504.196786	478519.510692	42.573095
3504.345053	478512.138611	42.578100
3504.529502	478487.782954	42.583104
3504.402320	478496.672055	42.588109
3504.435620	478493.220509	42.593114
3504.449501	478474.415932	42.598119
3504.834782	478486.315537	42.603124
3504.481126	478475.728558	42.608128
3505.092744	478441.726769	42.613133
3504.885221	478461.980967	42.618138
3504.393359	478414.216459	42.623143
3504.602133	478429.945022	42.628148
3504.336116	478422.790426	42.633152
3504.615267	478439.724186	42.638157
3504.886435	478398.123402	42.643162
3504.778187	478384.000640	42.648167
3504.850131	478403.349160	42.653172
3504.689439	478353.910395	42.658176
3504.532427	478348.715085	42.663181
3504.577249	478339.788193	42.668186
3504.390967	478367.590532	42.673191
3504.966374	478309.622355	42.678196
3504.787392	478318.164957	42.683200
3504.670997	478294.312738	42.688205
3504.806233	478301.640030	42.693210
3504.487623	478281.468762	42.698215
3504.775150	478270.577613	42.703220
3504.179120	478274.067393	42.708224
3504.594773	478268.325426	42.713229
3504.500709	478232.711668	42.718234
3504.313372	478262.744277	42.723239
3504.546767	478218.463008	42.728244
3504.320587	478253.113728	42.733248
3504.705242	478223.708710	42.738253
3504.157135	478215.128878	42.743258
3504.636555	478211.150647	42.748263
3504.376708	478212.306665	42.753268
3504.353514	478219.405622	42.758272
3504.512393	478193.431860	42.763277
3504.630203	478181.756592	42.768282
3504.504393	478171.538888	42.773287
3504.361623	478187.019117	42.778292
3504.702431	478187.472032	42.783296
3504.924398	478139.695409	42.788301
3504.768175	478182.494846	42.793306
3504.803392	478139.562429	42.798311
3504.688156	478129.089627	42.803316
3504.663577	478114.953450	42.808321
3504.728260	478118.186789	42.813325
3504.762196	478096.743268	42.818330
3504.558983	478090.288162	42.823335
3504.668118	478072.836544	42.828340
3504.632076	478077.961015	42.833345
3504.786633	478049.707094	42.838349
3504.819398	478047.066457	42.843354
3504.455409	478056.550674	42.848359
3504.449204	478006.377094	42.853364
3504.433413	478021.178524	42.858369
3504.600235	477989.476246	42.863373
3504.713192	478024.884665	42.868378
3504.548448	477982.845099	42.873383
3504.490969	477985.134818	42.878388
3504.523820	477959.028626	42.883393
3504.575351	477994.801577	42.888397
3504.480328	477968.208792	42.893402
3504.746812	477939.379529	42.898407
3504.808020	477940.940954	42.903412
3504.617809	477918.569718	42.908417
3504.498625	477931.106882	42.913421
3504.768311	477867.154631	42.918426
3504.403753	477900.206016	42.923431
3504.752570	477900.505627	42.928436
3504.689131	477868.940915	42.933441
3504.671281	477881.816867	42.938445
3504.714807	477849.627037	42.943450
3504.440028	477882.866988	42.948455
3504.371614	477833.615078	42.953460
3504.408010	477819.164964	42.958465
3504.120979	477829.346671	42.963469
3504.519634	477844.944321	42.968474
3504.355797	477822.974264	42.973479
3504.157179	477811.450155	42.978484
3504.265172	477819.694204	42.983489
3504.308352	477797.488673	42.988493
3504.360525	477791.297199	42.993498
3504.157793	477824.475179	42.998503
3504.321444	477800.730155	43.003508
3504.389708	477814.302087	43.008513
3504.043881	477814.559441	43.013517
3504.923487	477758.568866	43.018522
3504.587974	477783.557408	43.023527
3504.949872	477758.361906	43.028532
3504.717829	477748.921007	43.033537
3504.772351	477753.676472	43.038541
3504.166625	477753.569447	43.043546
3504.298537	477719.895660	43.048551
3504.400214	477740.861951	43.053556
3504.275649	477743.263665	43.058561
3504.265508	477695.269256	43.063565
3504.618114	477720.098439	43.068570
3504.183801	477704.962405	43.073575
3504.600931	477690.046566	43.078580
3504.411466	477729.608563	43.083585
3504.278473	477672.257323	43.088589
3504.558275	477666.131199	43.093594
3503.844676	477670.551943	43.098599
3504.596353	477658.928236	43.103604
3504.360010	477667.987003	43.108609
3504.382939	477685.924862	43.113613
3504.310480	477658.567867	43.118618
3504.381933	477625.055523	43.123623
3504.494751	477656.257978	43.128628
3503.559374	477653.010068	43.133633
3504.415355	477628.395184	43.138637
3504.179620	477656.713150	43.143642
3503.727919	477638.285465	43.148647
3504.470377	477646.936132	43.153652
3504.414177	477639.089223	43.158657
3504.332531	477654.661568	43.163661
3504.615019	477624.917042	43.168666
3504.082894	477640.053772	43.173671
3504.438891	477621.903874	43.178676
3504.168111	477621.338451	43.183681
3504.290927	477644.328798	43.188685
3504.235811	477602.676565	43.193690
3503.938901	477625.935999	43.198695
3503.713198	477601.846817	43.203700
3504.467392	477578.210925	43.208705
3504.722755	477559.924830	43.213709
3504.217602	477608.609132	43.218714
3504.050202	477625.462113	43.223719
3504.199120	477600.705533	43.228724
3504.649146	477576.306793	43.233729
3504.186633	477598.224006	43.238733
3504.469454	477585.001837	43.243738
3503.974454	477569.115054	43.248743
3504.662828	477529.169731	43.253748
3504.506128	477592.243540	43.258753
3504.038780	477572.297793	43.263757
3504.498868	477523.823195	43.268762
3504.536446	477515.150493	43.273767
3504.748825	477549.378339	43.278772
3504.176517	477555.398619	43.283777
3504.454777	477503.050152	43.288781
3504.891433	477495.125291	43.293786
3504.165527	477538.370920	43.298791
3504.278126	477515.039088	43.303796
3503.812651	477509.284119	43.308801
3504.060028	477504.987646	43.313805
3503.753980	477516.236854	43.318810
3504.039108	477505.193621	43.323815
3505.104465	477483.079602	43.328820
3504.534353	477466.849831	43.333825
3504.500557	477455.958342	43.338829
3504.783652	477451.149385	43.343834
3504.303174	477500.286195	43.348839
3504.223715	477497.409809	43.353844
3504.131298	477468.129765	43.358849
3504.341672	477432.871930	43.363853
3504.469344	477441.569170	43.368858
3504.019060	477455.679447	43.373863
3504.766302	477424.290003	43.378868
3504.453570	477426.113300	43.383873
3504.100608	477462.407277	43.388877
3504.313659	477417.417894	43.393882
3504.113276	477406.045879	43.398887
3504.705462	477393.281518	43.403892
3504.541289	477394.523826	43.408897
3504.533305	477388.037638	43.413901
3504.395851	477423.841477	43.418906
3504.311449	477414.579816	43.423911
3504.299854	477385.185512	43.428916
3504.343567	477357.759062	43.433921
3504.300057	477371.044862	43.438925
3504.602954	477408.755769	43.443930
3504.166009	477378.060242	43.448935
3504.080736	477343.001024	43.453940
3504.329433	477343.012370	43.458945
3504.048101	477384.920988	43.463949
3504.101213	477354.604118	43.468954
3503.839894	477363.666970	43.473959
3504.655767	477332.976100	43.478964
3504.213842	477374.149875	43.483969
3503.861921	477369.137163	43.488973
3504.974045	477325.982117	43.493978
3504.818467	477331.227036	43.498983
3504.669757	477350.662132	43.503988
3504.525946	477330.512960	43.508993
3504.869906	477273.845446	43.513997
3504.802848	477277.403841	43.519002
3504.433549	477298.090250	43.524007
3504.762893	477262.306480	43.529012
3504.520249	477240.550973	43.534017
3504.198985	477283.682513	43.539021
3504.546363	477274.808695	43.544026
3504.216072	477269.184341	43.549031
3504.257424	477240.288288	43.554036
3504.769662	477219.376434	43.559041
3504.705085	477245.032392	43.564045
3504.465360	477216.332779	43.569050
3504.750285	477189.830962	43.574055
3504.922995	477199.028024	43.579060
3504.402104	477188.314742	43.584065
3504.614560	477185.848326	43.589069
3504.940545	477148.848481	43.594074
3504.400599	477140.520313	43.599079
3504.488400	477130.166949	43.604084
3504.897377	477167.962910	43.609089
3504.318160	477129.585590	43.614093
3503.883999	477109.177983	43.619098
3503.545347	477110.549251	43.624103
3504.700850	477086.798673	43.629108
3504.483368	477102.595650	43.634113
3504.184509	477137.006367	43.639117
3504.548496	477092.245819	43.644122
3504.350767	477117.213413	43.649127
3504.307215	477067.499538	43.654132
3504.209238	477087.636443	43.659137
3503.943808	477107.343641	43.664141
3504.113721	477088.614469	43.669146
3503.768482	477087.351225	43.674151
3504.610871	477070.086948	43.679156
3504.697260	477091.512488	43.684161
3504.467548	477093.677479	43.689165
3504.582982	477047.131501	43.694170
3504.468364	477036.353926	43.699175
3504.418378	477071.434995	43.704180
3503.584267	477064.217646	43.709185
3503.814756	477055.869044	43.714189
3504.294162	477044.338699	43.719194
3504.071300	477049.999797	43.724199
3504.315912	477084.578128	43.729204
3504.347051	477057.913512	43.734209
3503.812725	477030.983445	43.739213
3503.716047	477028.971339	43.744218
3503.847411	477038.377745	43.749223
3504.028221	477028.364416	43.754228
3503.970928	477024.065310	43.759233
3504.681545	476995.823388	43.764237
3504.560112	477008.614904	43.769242
3504.297673	477068.564666	43.774247
3504.378536	477045.389355	43.779252
3504.514293	477001.475618	43.784257
3504.394776	477030.282938	43.789261
3504.512794	476977.299536	43.794266
3504.385550	477017.816098	43.799271
3504.427839	477025.969490	43.804276
3504.368420	477019.846099	43.809281
3504.196624	476987.232762	43.814285
3504.351210	476971.546942	43.819290
3504.515823	476954.541740	43.824295
3504.642234	476934.248094	43.829300
3504.461515	476934.073889	43.834305
3504.032932	476919.088406	43.839309
3504.225828	476948.150573	43.844314
3503.850702	476963.161628	43.849319
3504.218428	476953.726929	43.854324
3504.104685	476967.480253	43.859329
3504.082938	476964.189196	43.864333
3504.319098	476963.645000	43.869338
3503.888568	476948.457112	43.874343
3504.444201	476920.442316	43.879348
3504.355202	476938.956058	43.884353
3503.834005	476969.702262	43.889357
3504.067532	476942.245245	43.894362
3504.339071	476942.962559	43.899367
3504.076184	476914.671648	43.904372
3504.085792	476899.819633	43.909377
3504.099980	476939.198947	43.914381
3504.480820	476909.893976	43.919386
3504.194855	476892.605145	43.924391
3504.361020	476935.052185	43.929396
3504.301641	476904.904468	43.934401
3504.292242	476920.111174	43.939405
3504.026266	476900.284983	43.944410
3504.138308	476879.689447	43.949415
3503.713253	476898.459077	43.954420
3504.301170	476881.437594	43.959425
3504.007889	476894.154975	43.964429
3504.198744	476887.839936	43.969434
3503.750766	476899.720130	43.974439
3504.043953	476866.374212	43.979444
3504.073133	476914.570269	43.984449
3504.037659	476918.833314	43.989453
3503.864477	476899.043140	43.994458
3504.474882	476868.130615	43.999463
3504.149095	476909.286986	44.004468
3504.190749	476907.050268	44.009473
3504.190219	476880.441106	44.014477
3504.185753	476921.597352	44.019482
3503.961324	476884.227856	44.024487
3504.083829	476883.093410	44.029492
3504.358865	476889.233387	44.034497
3504.089329	476862.818770	44.039501
3504.252810	476862.032637	44.044506
3504.459179	476851.761759	44.049511
3504.481714	476894.890480	44.054516
3504.090427	476891.505765	44.059521
3504.061122	476871.287350	44.064525
3504.516019	476843.288368	44.069530
3504.444759	476810.962962	44.074535
3504.354527	476857.201336	44.079540
3504.525359	476870.504275	44.084545
3504.099509	476849.486879	44.089549
3504.411537	476807.774970	44.094554
3504.453052	476824.038075	44.099559
3504.125664	476822.214465	44.104564
3503.986131	476781.080713	44.109569
3504.190884	476819.923297	44.114573
3504.234468	476812.871244	44.119578
3504.238308	476794.776260	44.124583
3504.161959	476831.331764	44.129588
3504.214395	476804.562077	44.134593
3503.919022	476836.844010	44.139597
3504.215000	476816.928921	44.144602
3504.232390	476799.744118	44.149607
3504.433730	476795.201349	44.154612
3504.467358	476809.539702	44.159617
3504.363595	476782.946727	44.164621
3504.459203	476751.304434	44.169626
3504.184278	476767.110753	44.174631
3504.509910	476747.038854	44.179636
3504.677072	476773.469741	44.184641
3503.957123	476780.577960	44.189645
3503.977960	476779.611630	44.194650
3504.056048	476782.082798	44.199655
3504.073283	476755.673401	44.204660
3504.224554	476740.596141	44.209665
3504.290728	476729.587089	44.214669
3504.178679	476717.440452	44.219674
3504.360893	476738.090954	44.224679
3504.115408	476747.759796	44.229684
3504.208542	476708.515137	44.234689
3504.311738	476689.339976	44.239693
3504.410855	476686.435250	44.244698
3504.318596	476682.141597	44.249703
3504.593486	476692.285753	44.254708
3504.296757	476721.577685	44.259713
3504.258251	476720.975524	44.264717
3504.555763	476711.349071	44.269722
3504.209081	476719.209271	44.274727
3504.287735	476710.732469	44.279732
3504.442290	476705.183381	44.284737
3504.436090	476697.885733	44.289741
3504.331282	476675.398242	44.294746
3503.762207	476675.893631	44.299751
3503.793491	476656.577750	44.304756
3504.498391	476651.499198	44.309761
3504.247946	476671.204454	44.314765
3504.869282	476643.280259	44.319770
3504.380697	476670.017661	44.324775
3504.437840	476622.871696	44.329780
3504.251453	476657.772305	44.334785
3504.371371	476637.225962	44.339789
3504.168031	476618.352605	44.344794
3504.365139	476598.148817	44.349799
3504.167869	476614.855310	44.354804
3504.389847	476640.213325	44.359809
3504.079505	476628.959617	44.364813
3504.427096	476604.626576	44.369818
3503.854661	476598.229343	44.374823
3504.291679	476591.013661	44.379828
3504.038012	476613.709896	44.384833
3504.212674	476572.019209	44.389837
3504.342719	476609.910991	44.394842
3504.416007	476630.376080	44.399847
3504.258787	476585.139247	44.404852
3504.655062	476561.457364	44.409857
3504.425711	476592.715551	44.414861
3504.231523	476559.344784	44.419866
3504.353885	476583.654229	44.424871
3504.186893	476575.925784	44.429876
3504.654995	476526.028336	44.434881
3504.287014	476556.700267	44.439885
3504.305853	476512.094351	44.444890
3504.233776	476540.286652	44.449895
3503.837246	476558.089072	44.454900
3504.032069	476528.103355	44.459905
3504.397714	476518.668781	44.464909
3504.428501	476541.725620	44.469914
3504.218049	476551.287649	44.474919
3504.172772	476516.169982	44.479924
3504.341070	476486.644562	44.484929
3504.287507	476525.883337	44.489933
3504.420408	476490.078557	44.494938
3504.198935	476510.032818	44.499943
3504.378009	476495.711257	44.504948
3504.593525	476483.563393	44.509953
3504.367058	476513.604801	44.514957
3504.146208	476482.164157	44.519962
3503.709416	476473.312554	44.524967
3504.477148	476448.710180	44.529972
3504.366683	476490.289543	44.534977
3503.980613	476501.704020	44.539981
3504.352685	476469.916219	44.544986
3504.302593	476484.977630	44.549991
3504.235923	476448.849522	44.554996
3504.458517	476425.346985	44.560001
3504.483301	476456.869330	44.565005
3503.952869	476441.696847	44.570010
3503.961873	476444.787199	44.575015
3504.514391	476411.399542	44.580020
3504.335285	476450.404879	44.585025
3504.192582	476405.874944	44.590029
3504.373336	476392.161270	44.595034
3504.197209	476436.741564	44.600039
3504.023704	476446.449859	44.605044
3504.330489	476420.247686	44.610049
3503.606508	476412.657896	44.615053
3504.272392	476392.278441	44.620058
3504.246418	476426.292444	44.625063
3504.263126	476392.482585	44.630068
3504.150947	476417.741638	44.635073
3503.752085	476425.204716	44.640077
3504.328578	476397.743438	44.645082
3504.492383	476367.458271	44.650087
3504.040061	476400.424620	44.655092
3504.095313	476378.215613	44.660097
3504.328932	476370.170346	44.665101
3504.329991	476390.342981	44.670106
3504.525157	476357.315826	44.675111
3504.074603	476394.539492	44.680116
3504.212380	476398.014984	44.685121
3503.929711	476370.689458	44.690125
3503.948533	476348.182062	44.695130
3504.399770	476346.539461	44.700135
3504.114980	476364.679190	44.705140
3504.619022	476339.155334	44.710145
3504.130887	476365.842382	44.715149
3504.355641	476332.759825	44.720154
3504.294266	476367.438436	44.725159
3504.448394	476360.013955	44.730164
3503.678296	476323.287200	44.735169
3504.310515	476302.203376	44.740173
3504.405827	476323.983123	44.745178
3504.497906	476346.878442	44.750183
3504.184760	476321.585090	44.755188
3504.321879	476322.272987	44.760193
3504.170195	476323.513385	44.765197
3504.091830	476311.411865	44.770202
3503.886518	476316.969022	44.775207
3504.410528	476300.920180	44.780212
3504.694236	476258.603383	44.785217
3504.162412	476263.198443	44.790221
3504.473278	476269.282262	44.795226
3504.505996	476308.963994	44.800231
3504.180283	476293.252186	44.805236
3504.132028	476241.205471	44.810241
3504.427773	476210.290985	44.815245
3504.039792	476252.979103	44.820250
3504.139582	476274.910253	44.825255
3503.777245	476246.583435	44.830260
3504.504934	476215.803433	44.835265
3504.067274	476278.266850	44.840269
3504.301394	476275.137985	44.845274
3504.081310	476265.238324	44.850279
3503.801359	476264.066080	44.855284
3504.085417	476270.407564	44.860289
3504.000503	476265.707175	44.865293
3504.078295	476256.013859	44.870298
3504.025499	476251.207019	44.875303
3504.238499	476261.158431	44.880308
3504.282957	476251.521068	44.885313
3504.281739	476259.377532	44.890317
3504.295617	476241.838008	44.895322
3504.221464	476251.733437	44.900327
3504.272813	476237.330509	44.905332
3504.804413	476195.278516	44.910337
3504.739223	476181.502198	44.915341
3504.631671	476201.641502	44.920346
3504.381744	476182.724414	44.925351
3504.146280	476209.371734	44.930356
3504.017346	476176.142076	44.935361
3504.302334	476156.481503	44.940365
3504.083477	476175.624703	44.945370
3504.339059	476150.697424	44.950375
3504.390853	476143.187665	44.955380
3504.255531	476183.960610	44.960385
3504.088945	476174.356565	44.965389
3504.341763	476138.481523	44.970394
3504.356425	476180.295179	44.975399
3504.090003	476143.488490	44.980404
3504.420756	476131.423574	44.985409
3503.915659	476135.254147	44.990413
3504.435821	476097.917568	44.995418
3504.343151	476140.914052	45.000423
3504.545476	476129.832469	45.005428
3504.496304	476127.103158	45.010433
3504.117388	476134.613876	45.015437
3504.447819	476086.460428	45.020442
3504.503432	476087.668078	45.025447
3504.320828	476126.928024	45.030452
3504.486601	476079.155385	45.035457
3504.189736	476104.241274	45.040461
3503.989497	476084.454575	45.045466
3503.848304	476069.169605	45.050471
3504.698632	476024.735313	45.055476
3504.544402	476073.976096	45.060481
3504.422186	476081.649008	45.065485
3504.486516	476053.254484	45.070490
3504.039838	476042.985036	45.075495
3504.477352	476014.835595	45.080500
3504.465135	476036.835393	45.085505
3504.210356	476063.739389	45.090509
3503.942483	476038.590586	45.095514
3504.163679	476014.682302	45.100519
3504.311532	476011.719090	45.105524
3504.469160	476062.684637	45.110529
3503.993323	476015.874921	45.115533
3504.283333	475981.666375	45.120538
3504.440032	475977.282538	45.125543
3504.476979	475962.628257	45.130548
3504.543753	475946.296594	45.135553
3504.376556	475967.256544	45.140557
3504.310067	475948.512990	45.145562
3504.582403	475927.840462	45.150567
3504.148944	475956.192068	45.155572
3504.265137	475966.513732	45.160577
3503.844355	475944.126051	45.165581
3504.151333	475952.947657	45.170586
3504.230190	475981.370316	45.175591
3503.692949	475961.383327	45.180596
3504.287564	475926.011439	45.185601
3504.047911	475988.647203	45.190605
3504.217921	475965.355188	45.195610
3503.859794	475943.261723	45.200615
3504.084621	475918.896572	45.205620
3504.205775	475929.268157	45.210625
3503.861827	475958.213853	45.215629
3503.752998	475922.902452	45.220634
3504.124124	475927.861744	45.225639
3503.948554	475926.825042	45.230644
3504.338087	475945.517498	45.235649
3503.704389	475926.001897	45.240653
3503.801293	475960.504131	45.245658
3504.191991	475941.485567	45.250663
3504.432811	475914.330119	45.255668
3504.172569	475963.385180	45.260673
3504.133332	475929.836821	45.265677
3504.121958	475953.711982	45.270682
3504.422835	475921.326333	45.275687
3503.966515	475949.630875	45.280692
3504.119166	475924.263406	45.285697
3503.973953	475949.122772	45.290701
3504.035012	475917.484631	45.295706
3504.233403	475891.552339	45.300711
3504.191933	475934.541170	45.305716
3504.521240	475894.395929	45.310721
3503.890807	475933.625655	45.315725
3504.563045	475893.527586	45.320730
3504.542526	475880.808424	45.325735
3504.121925	475918.687160	45.330740
3504.231445	475862.813032	45.335745
3504.170108	475884.820759	45.340749
3503.754806	475862.330748	45.345754
3504.401079	475845.806041	45.350759
3504.104754	475884.577562	45.355764
3504.212732	475853.742895	45.360769
3504.019069	475904.713674	45.365773
3503.992356	475881.199221	45.370778
3504.439032	475851.780936	45.375783
3504.236747	475901.942096	45.380788
3504.211671	475887.297564	45.385793
3504.093770	475845.550243	45.390797
3504.124528	475861.714451	45.395802
3504.347554	475827.465544	45.400807
3504.040161	475843.277715	45.405812
3504.012204	475861.377303	45.410817
3503.927341	475861.644119	45.415821
3504.178335	475823.487900	45.420826
3504.020638	475874.199638	45.425831
3503.639727	475859.509951	45.430836
3504.232304	475864.434258	45.435841
3504.019732	475859.551203	45.440845
3504.278109	475856.874622	45.445850
3504.041659	475868.620615	45.450855
3504.302606	475853.221237	45.455860
3504.250829	475874.619222	45.460865
3503.760144	475843.372289	45.465869
3504.433650	475818.378548	45.470874
3504.611614	475851.144802	45.475879
3504.332772	475835.678663	45.480884
3504.759178	475830.035682	45.485889
3504.322721	475820.676868	45.490893
3504.462154	475805.245972	45.495898
3504.287715	475766.548641	45.500903
3503.975290	475805.120111	45.505908
3504.057044	475774.289468	45.510913
3503.728201	475796.745065	45.515917
3504.182105	475793.581390	45.520922
3504.315456	475790.519064	45.525927
3504.153827	475787.908855	45.530932
3504.017182	475804.200940	45.535937
3504.183720	475783.646360	45.540941
3504.107472	475814.374684	45.545946
3504.357902	475791.576628	45.550951
3504.054647	475793.550632	45.555956
3504.414375	475774.790241	45.560961
3504.037897	475769.781008	45.565965
3503.913995	475746.585881	45.570970
3504.387650	475758.270394	45.575975
3504.176376	475775.385291	45.580980
3504.190798	475754.499914	45.585985
3504.047596	475747.933194	45.590989
3504.090345	475785.029328	45.595994
3504.016451	475754.172567	45.600999
3503.954587	475774.457137	45.606004
3504.428184	475756.591099	45.611009
3504.309338	475767.355508	45.616013
3504.092578	475732.871826	45.621018
3504.435857	475708.132891	45.626023
3504.037830	475752.800452	45.631028
3504.425168	475711.125063	45.636033
3504.444037	475754.763673	45.641037
3504.574425	475729.703602	45.646042
3503.870628	475704.775341	45.651047
3504.009133	475682.552411	45.656052
3504.416960	475718.932032	45.661057
3504.111140	475726.684784	45.666061
3504.098321	475716.802782	45.671066
3503.837648	475695.251202	45.676071
3504.117208	475674.982773	45.681076
3504.271288	475688.441202	45.686081
3504.217967	475719.115359	45.691085
3504.056294	475709.003444	45.696090
3504.643429	475675.507728	45.701095
3504.104925	475692.116853	45.706100
3504.000604	475685.290532	45.711105
3503.825248	475668.794165	45.716109
3503.995477	475650.215671	45.721114
3504.189752	475684.753673	45.726119
3504.056851	475690.958491	45.731124
3504.400426	475651.266698	45.736129
3504.247621	475692.043398	45.741133
3504.017551	475686.554820	45.746138
3504.366730	475670.533111	45.751143
3503.709576	475709.260622	45.756148
3504.435814	475657.343431	45.761153
3504.389105	475660.341334	45.766157
3504.034738	475671.649892	45.771162
3503.705445	475651.274918	45.776167
3503.663483	475654.018635	45.781172
3503.842346	475653.888961	45.786177
3503.618036	475681.295523	45.791181
3503.899783	475675.371239	45.796186
3504.647025	475669.829568	45.801191
3504.161337	475691.549762	45.806196
3504.198518	475655.099697	45.811201
3503.868030	475649.779042	45.816205
3504.300970	475636.126373	45.821210
3504.402266	475671.540778	45.826215
3504.357652	475637.942098	45.831220
3504.288514	475690.059547	45.836225
3503.986994	475669.224016	45.841229
3504.238205	475647.135297	45.846234
3504.069271	475632.259879	45.851239
3504.272108	475600.852273	45.856244
3504.038652	475597.341017	45.861249
3504.284534	475618.641541	45.866253
3504.148686	475646.338293	45.871258
3503.993860	475635.312887	45.876263
3503.910625	475615.456549	45.881268
3504.337648	475603.832290	45.886273
3504.182890	475651.350812	45.891277
3504.318487	475616.507118	45.896282
3504.444709	475614.155516	45.901287
3504.013068	475641.645588	45.906292
3504.017231	475605.403402	45.911297
3504.667485	475567.082222	45.916301
3504.684113	475559.881930	45.921306
3504.452257	475566.558614	45.926311
3504.235711	475586.614381	45.931316
3504.599821	475594.007864	45.936321
3504.188456	475585.101163	45.941325
3504.087552	475560.482937	45.946330
3504.657028	475535.454603	45.951335
3504.336532	475583.100854	45.956340
3504.283922	475555.940615	45.961345
3504.762155	475508.978936	45.966349
3504.551693	475532.429870	45.971354
3503.901775	475513.524685	45.976359
3504.480973	475488.900259	45.981364
3504.421938	475504.267939	45.986369
3504.343893	475539.609545	45.991373
3504.356903	475496.269497	45.996378
3504.919150	475450.662973	46.001383
3504.518338	475469.278032	46.006388
3504.582414	475496.132387	46.011393
3504.172467	475454.176978	46.016397
3504.477783	475413.172882	46.021402
3504.098028	475450.336406	46.026407
3504.210976	475459.898524	46.031412
3504.271840	475443.060511	46.036417
3503.972926	475452.332912	46.041421
3503.622829	475450.867578	46.046426
3504.580216	475428.362883	46.051431
3504.377156	475410.958301	46.056436
3504.288953	475403.673146	46.061441
3504.582991	475423.901816	46.066445
3504.214244	475438.710242	46.071450
3503.952775	475421.517652	46.076455
3504.454191	475399.338430	46.081460
3504.637921	475392.466484	46.086465
3504.294516	475418.067457	46.091469
3503.818859	475384.232355	46.096474
3504.359091	475360.627691	46.101479
3504.210229	475375.249346	46.106484
3504.087342	475395.290499	46.111489
3504.552226	475362.878037	46.116493
3504.515814	475401.355963	46.121498
3504.612530	475356.684500	46.126503
3504.234120	475346.403906	46.131508
3504.554512	475346.251862	46.136513
3504.196263	475326.235953	46.141517
3504.529213	475346.154422	46.146522
3504.820381	475331.003313	46.151527
3504.536579	475309.809794	46.156532
3504.157073	475320.108756	46.161537
3504.573342	475275.589363	46.166541
3504.432088	475312.107185	46.171546
3504.420687	475274.853104	46.176551
3504.123121	475283.973303	46.181556
3504.539830	475253.291681	46.186561
3504.393325	475264.973118	46.191565
3504.438965	475276.877623	46.196570
3504.454128	475253.609263	46.201575
3504.385626	475229.086891	46.206580
3504.406232	475232.885232	46.211585
3504.650262	475212.216449	46.216589
3504.288203	475218.153499	46.221594
3504.321640	475218.908510	46.226599
3504.352418	475201.618856	46.231604
3504.649462	475181.347170	46.236609
3504.725756	475198.518481	46.241613
3504.435890	475167.593583	46.246618
3504.174784	475199.669957	46.251623
3504.197807	475154.401434	46.256628
3504.417443	475144.837234	46.261633
3504.002821	475150.326414	46.266637
3504.325849	475115.908434	46.271642
3504.766370	475160.140637	46.276647
3504.430638	475127.448827	46.281652
3504.545517	475142.282408	46.286657
3504.303602	475101.769681	46.291661
3504.555001	475131.737614	46.296666
3504.743433	475095.668147	46.301671
3504.626790	475115.708590	46.306676
3504.574508	475063.456727	46.311681
3504.433814	475091.560513	46.316685
3504.575983	475068.829445	46.321690
3504.188434	475063.568342	46.326695
3504.174921	475052.216150	46.331700
3504.184203	475035.335263	46.336705
3504.412163	475031.446848	46.341709
3503.722024	475027.450092	46.346714
3504.478499	475002.239481	46.351719
3504.271358	475033.902076	46.356724
3504.467504	475012.632391	46.361729
3504.422674	475021.611385	46.366733
3504.279621	474999.685653	46.371738
3504.762662	475002.194415	46.376743
3504.426428	474975.939937	46.381748
3504.228198	474995.993392	46.386753
3504.316185	474963.285038	46.391757
3504.192399	474999.192394	46.396762
3504.103752	474963.571997	46.401767
3504.290603	474938.096511	46.406772
3503.787162	474967.170206	46.411777
3504.014892	474935.250745	46.416781
3504.005243	474950.205527	46.421786
3504.022612	474956.386819	46.426791
3504.357137	474935.450007	46.431796
3504.163529	474968.681928	46.436801
3504.140173	474963.413927	46.441805
3504.099913	474943.398071	46.446810
3504.344885	474957.248134	46.451815
3504.134388	474964.986110	46.456820
3504.435191	474935.234729	46.461825
3504.254795	474944.032427	46.466829
3504.562420	474948.089594	46.471834
3504.383018	474904.930761	46.476839
3504.224635	474940.286107	46.481844
3504.052271	474925.562780	46.486849
3504.629768	474890.901444	46.491853
3503.828690	474902.382410	46.496858
3504.005664	474904.483355	46.501863
3503.882898	474875.153656	46.506868
3503.915382	474898.161411	46.511873
3503.681154	474881.318882	46.516877
3503.755934	474854.745840	46.521882
3503.963853	474918.429336	46.526887
3503.750444	474926.167787	46.531892
3503.961878	474930.290849	46.536897
3503.754385	474941.677977	46.541901
3503.325147	474925.170440	46.546906
3503.396513	474915.122675	46.551911
3504.099438	474906.090250	46.556916
3504.319199	474904.534810	46.561921
3503.286929	474933.337310	46.566925
3503.519491	474921.844775	46.571930
3504.191320	474910.739011	46.576935
3503.718559	474920.444643	46.581940
3503.619981	474930.141821	46.586945
3503.552055	474929.341500	46.591949
3504.061066	474905.741244	46.596954
3503.994684	474938.547592	46.601959
3503.761773	474968.896445	46.606964
3503.943539	474966.890813	46.611969
3504.052377	474970.066991	46.616973
3503.972779	474958.573124	46.621978
3504.013045	474926.277765	46.626983
3504.174744	474914.948494	46.631988
3504.032014	474954.964745	46.636993
3504.317447	474930.842275	46.641997
3503.988520	474969.823453	46.647002
3504.207307	474949.563905	46.652007
3503.926521	474943.981762	46.657012
3503.748603	474943.350892	46.662017
3504.088603	474939.343374	46.667021
3503.621108	474931.611105	46.672026
3504.159165	474905.623868	46.677031
3503.887719	474927.513774	46.682036
3503.236001	474942.874175	46.687041
3503.716157	474935.245577	46.692045
3504.137322	474916.728130	46.697050
3504.063572	474936.103011	46.702055
3503.904775	474981.545485	46.707060
3504.267330	474963.544234	46.712065
3504.006823	474953.092738	46.717069
3503.439668	474948.164125	46.722074
3504.371840	474943.049234	46.727079
3504.316612	474928.053950	46.732084
3504.151962	474928.130631	46.737089
3504.396226	474928.548197	46.742093
3504.062517	474936.305657	46.747098
3504.355221	474930.176668	46.752103
3504.411171	474935.287397	46.757108
3504.307563	474907.830215	46.762113
3503.878190	474912.966965	46.767117
3503.883543	474944.291981	46.772122
3504.260231	474932.624606	46.777127
3504.169332	474957.172469	46.782132
3504.052423	474923.381274	46.787137
3504.215995	474909.213111	46.792141
3503.820374	474967.263963	46.797146
3504.020412	474957.753462	46.802151
3503.837225	474948.709037	46.807156
3503.614558	474935.159517	46.812161
3503.726752	474940.818936	46.817165
3503.960892	474914.322163	46.822170
3504.198425	474937.550912	46.827175
3503.542453	474982.058181	46.832180
3503.835829	474973.648093	46.837185
3503.838731	474946.883776	46.842189
3504.220713	474924.672225	46.847194
3504.315637	474926.228555	46.852199
3504.045622	474942.795857	46.857204
3504.418097	474920.484425	46.862209
3504.220153	474923.709096	46.867213
3504.337987	474963.075879	46.872218
3504.251375	474952.748967	46.877223
3504.234507	474896.030436	46.882228
3503.960851	474905.501850	46.887233
3504.397502	474897.575979	46.892237
3504.449821	474887.379143	46.897242
3504.205863	474919.960141	46.902247
3503.964665	474943.315235	46.907252
3504.185197	474913.475131	46.912257
3504.491518	474886.713469	46.917261
3503.882200	474925.485602	46.922266
3504.382209	474911.112198	46.927271
3504.143726	474901.975114	46.932276
3504.136002	474897.617031	46.937281
3504.279574	474911.229706	46.942285
3504.291130	474875.137114	46.947290
3504.311982	474853.337386	46.952295
3503.846128	474874.649802	46.957300
3504.430983	474904.514679	46.962305
3504.477397	474886.867461	46.967309
3503.920373	474879.200010	46.972314
3504.469644	474872.168737	46.977319
3504.307620	474857.545104	46.982324
3504.238154	474821.870738	46.987329
3503.769916	474833.552584	46.992333
3503.700241	474843.600060	46.997338
3503.986718	474842.490276	47.002343
3503.653589	474856.938669	47.007348
3504.628458	474828.753345	47.012353
3504.573211	474841.535769	47.017357
3504.034473	474864.177640	47.022362
3504.181280	474806.672651	47.027367
3504.214397	474787.101249	47.032372
3504.557402	474834.036118	47.037377
3504.030031	474810.447482	47.042381
3504.265099	474796.420009	47.047386
3504.120722	474820.013389	47.052391
3504.468999	474799.682537	47.057396
3504.261897	474824.350304	47.062401
3504.369553	474768.777594	47.067405
3504.362278	474764.368722	47.072410
3504.422289	474802.427027	47.077415
3504.317582	474769.698127	47.082420
3504.104004	474783.367334	47.087425
3504.199107	474759.426811	47.092429
3503.968149	474798.798349	47.097434
3504.034441	474755.448298	47.102439
3504.044319	474793.159717	47.107444
3503.988085	474791.039615	47.112449
3504.343784	474729.192786	47.117453
3504.006871	474760.724248	47.122458
3504.028232	474725.542253	47.127463
3504.145124	474746.154425	47.132468
3504.144926	474741.744430	47.137473
3503.923019	474740.917748	47.142477
3504.118726	474753.102979	47.147482
3504.315336	474732.390513	47.152487
3503.837844	474764.400395	47.157492
3504.326163	474755.756649	47.162497
3504.284459	474744.864948	47.167501
3504.001796	474764.830596	47.172506
3504.229289	474734.532924	47.177511
3504.112919	474741.546453	47.182516
3504.299107	474725.904589	47.187521
3504.433982	474719.901861	47.192525
3504.180347	474726.785021	47.197530
3504.666357	474711.551966	47.202535
3504.611279	474749.932697	47.207540
3504.238566	474728.499175	47.212545
3504.519091	474682.175109	47.217549
3504.397260	474715.750927	47.222554
3504.345395	474669.175227	47.227559
3504.096788	474703.125932	47.232564
3504.226804	474679.889452	47.237569
3504.318374	474710.491545	47.242573
3504.133786	474659.425416	47.247578
3504.529510	474673.150468	47.252583
3504.669583	474634.046438	47.257588
3504.315475	474674.603548	47.262593
3504.130522	474649.946811	47.267597
3504.237145	474653.326148	47.272602
3504.300139	474637.044718	47.277607
3504.304010	474614.487070	47.282612
3504.148693	474627.538894	47.287617
3504.379795	474620.152302	47.292621
3503.806207	474648.933397	47.297626
3504.372510	474604.743651	47.302631
3503.971741	474642.216113	47.307636
3503.731007	474634.599959	47.312641
3504.494323	474609.742611	47.317645
3503.906166	474654.290567	47.322650
3504.057586	474612.498142	47.327655
3503.661104	474626.449812	47.332660
3503.752255	474646.964774	47.337665
3503.774838	474614.975855	47.342669
3503.876086	474638.479934	47.347674
3503.792636	474639.760340	47.352679
3504.313368	474605.969219	47.357684
3504.137652	474651.820623	47.362689
3504.239011	474645.519032	47.367693
3504.077166	474626.840017	47.372698
3504.077860	474624.862970	47.377703
3504.283813	474587.471896	47.382708
3504.068073	474594.957390	47.387713
3504.186864	474578.008125	47.392717
3504.089044	474606.105806	47.397722
3503.993652	474571.246137	47.402727
3504.077615	474611.480685	47.407732
3504.106598	474598.803586	47.412737
3504.296434	474566.281256	47.417741
3504.162229	474611.669979	47.422746
3504.361723	474573.975761	47.427751
3504.246030	474598.882805	47.432756
3504.135533	474586.278432	47.437761
3504.399369	474541.274623	47.442765
3504.182872	474561.888984	47.447770
3504.024648	474562.319481	47.452775
3504.251969	474554.984153	47.457780
3503.746548	474599.671222	47.462785
3503.749072	474571.588532	47.467789
3504.075926	474549.030454	47.472794
3504.168221	474592.406509	47.477799
3503.843674	474561.688928	47.482804
3504.027059	474569.212732	47.487809
3504.148100	474583.538847	47.492813
3503.421315	474574.529481	47.497818
3504.035151	474557.958168	47.502823
3504.038220	474589.588231	47.507828
3503.428375	474579.343825	47.512833
3504.087470	474566.719187	47.517837
3503.900152	474568.979123	47.522842
3504.494589	474547.747384	47.527847
3504.025927	474599.170426	47.532852
3503.982219	474574.288514	47.537857
3504.195085	474594.530841	47.542861
3503.631324	474585.090194	47.547866
3504.040732	474578.080926	47.552871
3504.147393	474574.465045	47.557876
3504.225770	474596.046568	47.562881
3504.228070	474591.636145	47.567885
3504.037499	474558.464266	47.572890
3503.966829	474567.498235	47.577895
3504.132932	474547.601444	47.582900
3503.842086	474527.624783	47.587905
3504.231158	474548.903800	47.592909
3504.298998	474537.893294	47.597914
3504.081905	474525.356421	47.602919
3504.064283	474544.824184	47.607924
3504.221695	474541.250967	47.612929
3504.448880	474545.472999	47.617933
3504.284189	474542.457591	47.622938
3504.518451	474546.678504	47.627943
3504.560136	474502.774213	47.632948
3504.152703	474520.073240	47.637953
3504.248812	474504.698894	47.642957
3504.002957	474510.516402	47.647962
3504.151451	474509.732549	47.652967
3504.334903	474517.154981	47.657972
3504.042298	474516.238082	47.662977
3504.241187	474512.252783	47.667981
3504.129309	474488.496725	47.672986
3504.074650	474456.874597	47.677991
3503.766577	474477.503517	47.682996
3504.130479	474470.704165	47.688001
3504.418759	474446.682051	47.693005
3504.035468	474491.096605	47.698010
3504.290697	474467.333191	47.703015
3504.271971	474467.031978	47.708020
3504.033618	474480.401162	47.713025
3504.266288	474487.663754	47.718029
3504.033789	474466.309175	47.723034
3504.010019	474486.893152	47.728039
3504.116850	474450.227155	47.733044
3503.862922	474460.709464	47.738049
3504.111653	474443.638170	47.743053
3504.015863	474445.326060	47.748058
3504.069143	474441.870664	47.753063
3504.132953	474452.099998	47.758068
3504.295793	474437.779552	47.763073
3504.489816	474440.536826	47.768077
3504.124827	474457.220913	47.773082
3504.538887	474437.487587	47.778087
3503.883525	474451.429602	47.783092
3504.498466	474433.185232	47.788097
3504.381324	474399.748037	47.793101
3503.950796	474423.032270	47.798106
3503.757941	474385.754547	47.803111
3504.110368	474406.431218	47.808116
3503.580543	474401.699333	47.813121
3504.021511	474391.643585	47.818125
3503.780030	474420.473894	47.823130
3504.026971	474411.158487	47.828135
3504.060404	474391.738726	47.833140
3503.990011	474429.362125	47.838145
3503.916327	474395.664603	47.843149
3503.807323	474427.464702	47.848154
3503.990037	474404.473032	47.853159
3503.815344	474405.260968	47.858164
3503.646456	474413.651552	47.863169
3503.976432	474409.696206	47.868173
3503.514796	474418.944103	47.873178
3504.041054	474401.372697	47.878183
3503.701393	474444.006291	47.883188
3503.934473	474442.448711	47.888193
3504.116981	474448.147845	47.893197
3503.712722	474436.046021	47.898202
3504.001626	474446.391853	47.903207
3503.698431	474440.711732	47.908212
3504.108823	474470.047227	47.913217
3504.072619	474447.039515	47.918221
3503.801656	474468.828456	47.923226
3503.881845	474459.285974	47.928231
3504.308082	474448.218776	47.933236
3503.784665	474454.587072	47.938241
3504.046203	474436.398560	47.943245
3503.674466	474433.669311	47.948250
3504.246477	474411.731310	47.953255
3504.137641	474437.600585	47.958260
3503.885011	474442.962970	47.963265
3504.281796	474404.628973	47.968269
3504.100794	474452.813421	47.973274
3504.185131	474405.455236	47.978279
3504.183847	474466.385238	47.983284
3503.777860	474447.440502	47.988289
3504.323013	474420.792552	47.993293
3504.167957	474430.296133	47.998298
3504.049256	474442.734004	48.003303
3504.187362	474409.763387	48.008308
3504.376165	474436.193908	48.013313
3504.514089	474440.075236	48.018317
3504.040895	474423.320786	48.023322
3504.098506	474392.491860	48.028327
3504.377337	474397.922332	48.033332
3504.282283	474398.494919	48.038337
3504.090644	474414.239215	48.043341
3504.020822	474396.762015	48.048346
3503.863842	474404.136912	48.053351
3504.083336	474375.867588	48.058356
3503.753607	474431.831241	48.063361
3504.062515	474418.805645	48.068365
3504.210992	474397.238709	48.073370
3504.270627	474411.270509	48.078375
3504.216288	474399.975096	48.083380
3503.906752	474355.973927	48.088385
3504.321571	474348.963725	48.093389
3504.234461	474381.013889	48.098394
3504.133164	474360.145368	48.103399
3503.710963	474393.515737	48.108404
3503.917684	474360.635577	48.113409
3504.324670	474366.755470	48.118413
3503.779881	474381.541796	48.123418
3504.034540	474358.640084	48.128423
3503.895275	474392.776786	48.133428
3503.460268	474368.615444	48.138433
3503.943385	474382.985856	48.143437
3504.055306	474374.553510	48.148442
3504.030120	474379.626512	48.153447
3503.988911	474370.508700	48.158452
3504.031604	474376.787547	48.163457
3504.276649	474393.679414	48.168461
3503.946851	474359.566096	48.173466
3504.242147	474381.671158	48.178471
3504.283119	474368.485115	48.183476
3504.243431	474389.223778	48.188481
3504.701400	474347.737194	48.193485
3504.244239	474347.049058	48.198490
3504.155052	474340.625416	48.203495
3504.179235	474356.031503	48.208500
3504.061880	474348.142290	48.213505
3504.328870	474333.044950	48.218509
3503.926970	474359.619621	48.223514
3504.174737	474347.161239	48.228519
3504.217597	474337.421838	48.233524
3504.269380	474328.035856	48.238529
3504.475626	474314.164678	48.243533
3504.291066	474297.111052	48.248538
3504.233145	474312.682220	48.253543
3504.034277	474292.082503	48.258548
3504.027857	474291.424507	48.263553
3504.254779	474326.314497	48.268557
3504.110850	474302.563287	48.273562
3504.123018	474278.787378	48.278567
3504.218877	474300.366451	48.283572
3503.958898	474275.873191	48.288577
3504.035505	474267.345001	48.293581
3504.209413	474286.073069	48.298586
3504.179476	474261.137908	48.303591
3504.045351	474275.504569	48.308596
3504.168107	474279.033490	48.313601
3504.383466	474263.335970	48.318605
3504.039871	474275.353270	48.323610
3504.124089	474287.455020	48.328615
3504.380708	474276.718681	48.333620
3504.172196	474273.253942	48.338625
3504.465648	474240.765408	48.343629
3504.512345	474239.085198	48.348634
3504.526168	474229.198262	48.353639
3504.233574	474245.921770	48.358644
3504.323683	474216.304022	48.363649
3504.396725	474229.573464	48.368653
3504.041005	474195.007749	48.373658
3504.276762	474189.394450	48.378663
3504.446423	474187.441346	48.383668
3504.102545	474204.933359	48.388673
3503.982610	474217.979853	48.393677
3503.517438	474202.947444	48.398682
3503.921716	474190.464230	48.403687
3504.107840	474195.098352	48.408692
3503.999407	474230.447037	48.413697
3503.903502	474200.148992	48.418701
3503.956665	474186.149849	48.423706
3504.097283	474206.758818	48.428711
3503.813631	474213.089294	48.433716
3504.240099	474197.256976	48.438721
3503.849087	474219.318612	48.443725
3504.235458	474215.050170	48.448730
3504.307838	474211.034116	48.453735
3504.301913	474206.472837	48.458740
3504.153059	474181.353609	48.463745
3504.196597	474168.065649	48.468749
3504.156253	474180.339222	48.473754
3504.119007	474160.170046	48.478759
3504.181543	474167.915862	48.483764
3504.053144	474172.346245	48.488769
3504.285411	474148.687471	48.493773
3504.067936	474157.542060	48.498778
3504.181907	474175.012426	48.503783
3503.701563	474160.894822	48.508788
3503.885543	474142.921071	48.513793
3503.936120	474162.479803	48.518797
3504.198313	474158.433739	48.523802
3503.555632	474180.281738	48.528807
3504.174210	474164.723178	48.533812
3503.703047	474180.207686	48.538817
3504.135382	474151.701649	48.543821
3503.987769	474187.766275	48.548826
3504.195351	474146.014708	48.553831
3504.237952	474181.440988	48.558836
3503.942239	474136.676796	48.563841
3504.186039	474146.624380	48.568845
3504.055793	474150.700222	48.573850
3504.138262	474115.000603	48.578855
3504.232404	474158.732127	48.583860
3503.973827	474127.699319	48.588865
3504.386860	474132.855196	48.593869
3503.952039	474176.518211	48.598874
3504.089091	474150.187863	48.603879
3504.128144	474127.928262	48.608884
3504.250642	474145.093160	48.613889
3504.041564	474162.665285	48.618893
3504.203930	474118.791785	48.623898
3504.142547	474128.888994	48.628903
3503.994725	474130.585134	48.633908
3503.577251	474117.065856	48.638913
3504.037232	474097.122179	48.643917
3504.064508	474124.237620	48.648922
3504.140575	474117.787790	48.653927
3504.291616	474096.118748	48.658932
3504.163370	474131.217280	48.663937
3504.289721	474098.400091	48.668941
3504.594406	474094.296608	48.673946
3504.128274	474129.904765	48.678951
3504.351430	474112.482398	48.683956
3504.320750	474069.754508	48.688961
3504.352431	474093.979890	48.693965
3503.973980	474060.431364	48.698970
3503.985729	474085.217510	48.703975
3504.190209	474055.733526	48.708980
3503.923397	474091.411631	48.713985
3504.073076	474063.609131	48.718989
3504.238668	474089.891695	48.723994
3504.228910	474054.561386	48.728999
3504.201895	474080.063344	48.734004
3503.804266	474088.186067	48.739009
3504.259343	474060.538059	48.744013
3503.652735	474085.117789	48.749018
3504.116046	474049.408555	48.754023
3504.308790	474082.479476	48.759028
3504.073886	474047.742342	48.764033
3504.629783	474040.760429	48.769037
3503.856748	474051.375684	48.774042
3503.973108	474018.559946	48.779047
3503.997372	474055.915616	48.784052
3503.685384	474029.504009	48.789057
3504.030749	474045.113026	48.794061
3503.609312	474036.967603	48.799066
3503.787829	474035.469308	48.804071
3504.265894	474036.052707	48.809076
3504.159861	474060.198512	48.814081
3504.449731	474038.811615	48.819085
3503.946074	474051.817480	48.824090
3504.210470	474035.605121	48.829095
3504.309180	474056.018101	48.834100
3503.989145	474031.077816	48.839105
3504.243138	474050.807271	48.844109
3504.423604	474028.068989	48.849114
3503.870314	474014.114886	48.854119
3504.415315	473982.650704	48.859124
3503.905167	474037.021826	48.864129
3503.881952	474003.163604	48.869133
3504.005885	474029.503522	48.874138
3504.003413	474007.098278	48.879143
3504.093656	474030.249959	48.884148
3503.870468	474023.796705	48.889153
3504.149194	474009.204185	48.894157
3504.019431	474028.943622	48.899162
3504.005948	474018.807443	48.904167
3504.196153	474001.491572	48.909172
3504.118943	474041.245805	48.914177
3504.320899	474009.278276	48.919181
3504.204825	474028.457944	48.924186
3504.295711	474000.816725	48.929191
3504.104925	473967.339768	48.934196
3504.191004	474001.847041	48.939201
3504.313671	473970.196132	48.944205
3503.914297	474003.664913	48.949210
3503.512357	473979.852723	48.954215
3504.282174	473957.122598	48.959220
3503.707423	473990.821885	48.964225
3503.789041	473955.781112	48.969229
3503.837411	473988.773620	48.974234
3503.512270	473967.788000	48.979239
3504.083024	473995.679472	48.984244
3504.005437	473985.553407	48.989249
3504.135751	473978.892194	48.994253
3503.954413	474001.731990	48.999258
3503.992189	473972.578382	49.004263
3503.993137	473995.440067	49.009268
3503.384775	473990.517731	49.014273
3503.999188	473980.637135	49.019277
3503.990613	473992.703034	49.024282
3504.032095	473997.664211	49.029287
3504.069036	473979.865630	49.034292
3503.742582	474016.364356	49.039297
3503.886982	473988.359822	49.044301
3504.050311	473998.522964	49.049306
3503.641655	474008.218896	49.054311
3504.096361	473992.483339	49.059316
3504.068031	473996.644486	49.064321
3503.930345	473994.334409	49.069325
3503.636746	474008.168857	49.074330
3503.863654	473999.566109	49.079335
3503.843826	473995.260437	49.084340
3503.514888	474016.602801	49.089345
3503.934421	474013.799127	49.094349
3504.137437	474036.983668	49.099354
3503.688832	474042.884045	49.104359
3504.338945	474006.030002	49.109364
3504.086154	474036.231310	49.114369
3504.301386	474008.114225	49.119373
3503.995492	474018.503591	49.124378
3504.226005	473996.872576	49.129383
3504.184104	474043.667336	49.134388
3503.796038	474018.382948	49.139393
3504.068816	474026.044898	49.144397
3504.413438	474008.096331	49.149402
3504.274509	474014.606760	49.154407
3503.997777	474038.830260	49.159412
3504.492884	474005.397036	49.164417
3504.372302	474017.531314	49.169421
3504.214995	473985.671222	49.174426
3504.348065	473992.493510	49.179431
3504.319355	473963.806621	49.184436
3503.893380	474006.049239	49.189441
3504.432099	473975.904016	49.194445
3504.221538	473993.831362	49.199450
3504.069232	473955.025698	49.204455
3504.274743	473952.357225	49.209460
3503.953134	473951.242118	49.214465
3504.593748	473938.873473	49.219469
3504.093638	473962.270611	49.224474
3504.062725	473945.750014	49.229479
3504.156410	473933.417115	49.234484
3504.063670	473944.989429	49.239489
3504.283221	473946.272679	49.244493
3504.290791	473944.598630	49.249498
3504.199104	473928.087623	49.254503
3504.121770	473916.947652	49.259508
3504.071256	473901.748100	49.264513
3504.445397	473895.200398	49.269517
3504.092416	473916.394591	49.274522
3503.848954	473892.101025	49.279527
3504.122806	473902.550897	49.284532
3503.802488	473920.292888	49.289537
3504.200699	473899.344947	49.294541
3504.171272	473908.321998	49.299546
3504.147330	473898.897095	49.304551
3504.103502	473901.945494	49.309556
3504.402146	473901.948954	49.314561
3504.367187	473895.972827	49.319565
3504.444986	473873.656133	49.324570
3504.109223	473862.455593	49.329575
3504.516653	473859.704503	49.334580
3504.069102	473884.816944	49.339585
3504.193250	473848.400587	49.344589
3504.292656	473880.371367	49.349594
3503.986750	473831.502084	49.354599
3504.300521	473844.530961	49.359604
3503.618185	473833.131721	49.364609
3504.245692	473805.304041	49.369613
3504.096431	473846.388031	49.374618
3503.876693	473817.680437	49.379623
3504.131128	473834.216441	49.384628
3504.092281	473815.213090	49.389633
3503.968761	473840.629216	49.394637
3504.213242	473829.995945	49.399642
3504.353855	473841.784895	49.404647
3503.919332	473827.609125	49.409652
3504.179866	473848.148812	49.414657
3503.844062	473839.533549	49.419661
3504.180640	473827.466350	49.424666
3503.969944	473835.508935	49.429671
3504.365115	473833.672233	49.434676
3503.673539	473827.445020	49.439681
3503.897323	473843.124099	49.444685
3503.638890	473840.883780	49.449690
3503.941025	473831.812845	49.454695
3503.954208	473839.921429	49.459700
3503.992347	473854.362544	49.464705
3504.065565	473837.724018	49.469709
3503.833548	473843.387453	49.474714
3504.160776	473844.856460	49.479719
3504.318176	473823.642351	49.484724
3503.879058	473835.979157	49.489729
3504.026837	473792.766256	49.494733
3504.104672	473806.339367	49.499738
3503.862913	473780.727409	49.504743
3504.137247	473812.518572	49.509748
3503.973217	473800.936013	49.514753
3504.002576	473816.696533	49.519757
3504.293858	473780.557792	49.524762
3504.023327	473828.808555	49.529767
3504.154802	473802.732101	49.534772
3503.592822	473815.189721	49.539777
3503.488718	473802.989389	49.544781
3503.988389	473810.564868	49.549786
3503.653292	473805.295146	49.554791
3504.034322	473815.423971	49.559796
3503.779168	473823.980507	49.564801
3504.087862	473804.972910	49.569805
3504.370850	473811.670180	49.574810
3504.020638	473815.426011	49.579815
3504.116813	473805.627237	49.584820
3503.969096	473805.904013	49.589825
3504.190434	473826.551300	49.594829
3504.159187	473810.537565	49.599834
3503.794078	473817.945568	49.604839
3504.031582	473812.838808	49.609844
3504.145968	473798.779032	49.614849
3504.256725	473832.471619	49.619853
3504.273835	473809.404069	49.624858
3503.925872	473812.906084	49.629863
3504.572468	473788.319647	49.634868
3503.988793	473784.457890	49.639873
3503.853007	473797.557850	49.644877
3504.009920	473777.712453	49.649882
3504.244150	473802.159628	49.654887
3504.604874	473778.733584	49.659892
3503.705078	473796.009656	49.664897
3504.024584	473769.447213	49.669901
3504.209273	473812.202021	49.674906
3503.892760	473779.403622	49.679911
3503.744176	473816.939124	49.684916
3503.671357	473778.779557	49.689921
3503.826991	473810.690867	49.694925
3504.030039	473780.851870	49.699930
3504.029129	473791.395917	49.704935
3504.100225	473793.108176	49.709940
3504.415426	473796.403998	49.714945
3504.136732	473798.374309	49.719949
3504.286789	473771.889343	49.724954
3504.169398	473796.848326	49.729959
3504.259213	473770.829107	49.734964
3503.743001	473758.085577	49.739969
3504.503956	473726.079948	49.744973
3504.222417	473775.245036	49.749978
3503.482136	473764.615296	49.754983
3504.034663	473743.186578	49.759988
3504.249388	473732.862112	49.764993
3504.121209	473752.094645	49.769997
3504.044489	473789.213303	49.775002
3503.821130	473752.750315	49.780007
3503.856269	473783.717562	49.785012
3504.057806	473747.339487	49.790017
3504.098465	473759.853971	49.795021
3503.812442	473784.282009	49.800026
3503.782913	473746.115539	49.805031
3504.287145	473770.114542	49.810036
3503.908825	473753.395236	49.815041
3503.977740	473771.025146	49.820045
3504.361918	473749.268198	49.825050
3503.789687	473781.041133	49.830055
3503.835636	473752.747684	49.835060
3503.947192	473780.813409	49.840065
3504.212586	473770.024726	49.845069
3504.392490	473767.056124	49.850074
3504.102782	473745.354987	49.855079
3503.968135	473735.288508	49.860084
3504.094755	473743.683355	49.865089
3504.103861	473735.266995	49.870093
3504.362732	473728.686767	49.875098
3504.303107	473735.488904	49.880103
3504.299459	473737.567826	49.885108
3504.179721	473735.812496	49.890113
3504.234255	473725.411960	49.895117
3504.046430	473719.612018	49.900122
3504.137717	473707.127286	49.905127
3504.107716	473686.703037	49.910132
3503.711444	473713.581811	49.915137
3504.092223	473703.281778	49.920141
3504.095940	473692.939949	49.925146
3503.870880	473699.413400	49.930151
3504.097273	473701.050431	49.935156
3504.138171	473690.499956	49.940161
3504.129774	473688.422871	49.945165
3503.993238	473712.117677	49.950170
3503.913923	473690.738074	49.955175
3504.432784	473711.490532	49.960180
3504.363371	473680.781992	49.965185
3504.344417	473705.421375	49.970189
3504.211940	473693.326845	49.975194
3504.296810	473662.188355	49.980199
3504.452575	473689.486835	49.985204
3504.228461	473686.328615	49.990209
3504.596955	473648.605978	49.995213
3504.525490	473687.853067	50.000218
3503.813744	473662.365934	50.005223
3504.077394	473618.272582	50.010228
3503.989371	473644.139573	50.015233
3504.217019	473617.388682	50.020237
3504.321733	473629.335505	50.025242
3504.171299	473646.341190	50.030247
3504.348378	473609.814658	50.035252
3504.447450	473658.058101	50.040257
3504.238640	473622.251581	50.045261
3504.355133	473647.883474	50.050266
3504.099042	473626.328974	50.055271
3504.194141	473587.889049	50.060276
3504.510669	473587.281374	50.065281
3503.957208	473612.056041	50.070285
3504.581117	473574.546362	50.075290
3504.472311	473580.190396	50.080295
3504.500564	473593.213868	50.085300
3504.186042	473578.207879	50.090305
3504.062954	473551.258872	50.095309
3504.583114	473529.682970	50.100314
3504.029182	473582.287978	50.105319
3504.032051	473561.250098	50.110324
3504.185418	473556.866268	50.115329
3504.003893	473586.296589	50.120333
3504.191903	473562.846903	50.125338
3504.129826	473565.796850	50.130343
3504.010938	473569.059931	50.135348
3503.955883	473536.777437	50.140353
3504.145879	473490.769132	50.145357
3503.961641	473535.661228	50.150362
3503.596248	473522.690943	50.155367
3504.066610	473526.114364	50.160372
3504.013252	473515.223847	50.165377
3504.090036	473529.760469	50.170381
3503.990221	473514.213572	50.175386
3504.167284	473535.729927	50.180391
3504.248534	473517.011474	50.185396
3503.968969	473547.420506	50.190401
3504.012264	473537.021651	50.195405
3504.340862	473526.324235	50.200410
3503.911091	473542.157532	50.205415
3504.175477	473534.156976	50.210420
3504.286725	473528.005556	50.215425
3504.042843	473536.509737	50.220429
3504.337766	473507.466903	50.225434
3504.039996	473523.836970	50.230439
3504.435004	473489.455564	50.235444
3504.080765	473518.862586	50.240449
3503.694477	473489.623235	50.245453
3504.709660	473480.439448	50.250458
3503.855198	473514.792039	50.255463
3503.992775	473491.451627	50.260468
3504.217183	473478.438789	50.265473
3503.853733	473514.234559	50.270477
3504.206253	473478.643226	50.275482
3503.946475	473522.584127	50.280487
3504.232153	473484.215273	50.285492
3503.817649	473516.014382	50.290497
3504.342364	473470.510749	50.295501
3504.321473	473481.058113	50.300506
3504.476509	473443.875764	50.305511
3504.416052	473466.443588	50.310516
3504.385231	473457.982732	50.315521
3504.297519	473453.738369	50.320525
3504.495081	473463.744288	50.325530
3504.230940	473423.485199	50.330535
3504.364445	473439.736478	50.335540
3504.117481	473422.641290	50.340545
3504.749741	473403.379410	50.345549
3504.329999	473406.537988	50.350554
3504.324064	473400.100893	50.355559
3503.871912	473395.609959	50.360564
3504.485065	473358.000198	50.365569
3503.937432	473398.539733	50.370573
3504.090828	473363.841452	50.375578
3504.094218	473388.680457	50.380583
3504.211330	473386.887663	50.385588
3503.697546	473385.600124	50.390593
3503.634196	473370.300820	50.395597
3504.466255	473356.684936	50.400602
3503.951790	473407.509898	50.405607
3503.837708	473391.508927	50.410612
3504.197237	473356.017659	50.415617
3504.091035	473386.095372	50.420621
3504.341202	473378.198389	50.425626
3504.279585	473367.207713	50.430631
3504.305904	473386.314784	50.435636
3503.891269	473359.665069	50.440641
3504.075821	473313.707920	50.445645
3504.237813	473346.075189	50.450650
3503.855422	473343.094010	50.455655
3504.339758	473319.039587	50.460660
3504.194548	473358.400349	50.465665
3504.209586	473317.032373	50.470669
3504.263238	473343.282897	50.475674
3503.711938	473364.154153	50.480679
3503.794648	473336.918873	50.485684
3504.105269	473340.215493	50.490689
3504.094212	473331.447303	50.495693
3504.344545	473344.739992	50.500698
3503.905557	473373.907151	50.505703
3504.290098	473327.005950	50.510708
3504.075205	473356.543260	50.515713
3503.692416	473305.606455	50.520717
3503.996822	473325.886267	50.525722
3503.620780	473321.484674	50.530727
3504.330968	473278.739424	50.535732
3503.868967	473298.633461	50.540737
3503.918195	473249.605271	50.545741
3503.710459	473238.029300	50.550746
3503.525014	473154.211613	50.555751
3503.656047	473119.972696	50.560756
3503.469280	473048.878886	50.565761
3503.231597	472962.229817	50.570765
3502.692360	472887.896045	50.575770
3502.703000	472795.174411	50.580775
3502.908278	472676.820772	50.585780
3502.559783	472587.804983	50.590785
3502.423729	472456.272635	50.595789
3502.537322	472336.207887	50.600794
3502.308292	472195.461971	50.605799
3501.470710	472054.811275	50.610804
3501.878400	471900.933769	50.615809
3501.397099	471748.919321	50.620813
3501.335790	471566.571010	50.625818
3500.816576	471385.611608	50.630823
3500.651426	471197.902479	50.635828
3500.224134	471023.972457	50.640833
3500.115244	470827.328089	50.645837
3500.012140	470623.177378	50.650842
3499.184775	470421.674144	50.655847
3498.736588	470210.678684	50.660852
3498.266050	469983.105288	50.665857
3497.869385	469776.660406	50.670861
3497.716425	469548.423649	50.675866
3497.027523	469326.961893	50.680871
3497.084242	469085.605583	50.685876
3496.722278	468851.816870	50.690881
3496.000994	468594.301852	50.695885
3495.916275	468366.092127	50.700890
3495.493709	468091.081112	50.705895
3494.862357	467825.328098	50.710900
3494.116732	467584.537716	50.715905
3493.977261	467304.350269	50.720909
3493.588370	467026.886080	50.725914
3492.815961	466770.573859	50.730919
3492.679939	466458.681475	50.735924
3492.096635	466212.221031	50.740929
3491.208888	465893.593258	50.745933
3490.884801	465625.786346	50.750938
3490.821201	465308.845193	50.755943
3489.916925	465048.070354	50.760948
3489.233267	464738.673588	50.765953
3488.873580	464440.327654	50.770957
3488.279249	464145.666162	50.775962
3487.967863	463820.171268	50.780967
3487.350213	463541.937198	50.785972
3487.370979	463192.391295	50.790977
3486.160604	462894.817734	50.795981
3485.673648	462563.600483	50.800986
3484.988212	462236.771445	50.805991
3484.565878	461933.125908	50.810996
3484.169692	461595.539483	50.816001
3483.066996	461279.261317	50.821005
3482.954384	460938.880920	50.826010
3481.796654	460619.000576	50.831015
3481.446874	460294.980635	50.836020
3480.846708	459955.017091	50.841025
3480.277270	459648.573212	50.846029
3480.027650	459303.319439	50.851034
3478.828728	458963.942508	50.856039
3478.267325	458642.823182	50.861044
3478.038158	458281.723055	50.866049
3477.328071	457959.552029	50.871053
3476.769144	457605.696651	50.876058
3476.090335	457266.414474	50.881063
3475.342239	456909.178953	50.886068
3474.630235	456592.467544	50.891073
3473.787558	456244.266794	50.896077
3473.461737	455884.005640	50.901082
3472.629089	455551.520222	50.906087
3472.028460	455218.029245	50.911092
3471.552688	454852.346569	50.916097
3470.695776	454508.738298	50.921101
3470.317834	454175.146017	50.926106
3469.154659	453792.506861	50.931111
3468.902602	453483.797407	50.936116
3468.193465	453103.561162	50.941121
3467.325201	452772.156953	50.946125
3467.060324	452402.190059	50.951130
3466.106195	452074.189056	50.956135
3465.502884	451678.638845	50.961140
3464.531206	451365.904384	50.966145
3464.017452	451009.300226	50.971149
3463.961448	450646.274968	50.976154
3462.581710	450314.510289	50.981159
3461.851938	449958.685320	50.986164
3461.282399	449608.462642	50.991169
3460.342254	449263.774182	50.996173
3459.919844	448921.993037	51.001178
3459.222514	448558.021632	51.006183
3458.288618	448234.784511	51.011188
3457.540653	447864.973979	51.016193
3456.813059	447533.016011	51.021197
3456.178572	447178.504107	51.026202
3455.397978	446844.920740	51.031207
3454.783666	446501.459934	51.036212
3454.192692	446154.792865	51.041217
3452.899859	445837.162848	51.046221
3453.115137	445472.238369	51.051226
3452.393641	445132.987628	51.056231
3451.153529	444796.656543	51.061236
3450.543197	444437.125699	51.066241
3449.864917	444128.867875	51.071245
3449.302938	443748.405976	51.076250
3448.337416	443439.829428	51.081255
3447.746566	443096.823757	51.086260
3447.334005	442743.378659	51.091265
3446.321752	442426.217666	51.096269
3445.980460	442085.188810	51.101274
3444.979313	441744.919441	51.106279
3444.475003	441398.779507	51.111284
3443.800936	441068.449870	51.116289
3443.147738	440736.132574	51.121293
3442.490166	440382.717470	51.126298
3441.662206	440071.918990	51.131303
3441.229936	439718.763374	51.136308
3440.488538	439375.780178	51.141313
3439.668281	439048.924355	51.146317
3438.945349	438707.604440	51.151322
3438.062363	438361.735676	51.156327
3437.429330	438026.662563	51.161332
3436.783238	437703.188721	51.166337
3435.675035	437368.968909	51.171341
3435.234821	437048.068936	51.176346
3434.733401	436707.727626	51.181351
3433.974426	436379.481727	51.186356
3433.662380	436039.609236	51.191361
3432.820961	435709.615889	51.196365
3432.270974	435381.120908	51.201370
3431.343690	435052.681331	51.206375
3430.690153	434717.237489	51.211380
3429.847684	434388.877520	51.216385
3429.247655	434061.236720	51.221389
3428.567034	433708.874018	51.226394
3427.866283	433392.691784	51.231399
3426.964705	433059.398318	51.236404
3426.097617	432739.400288	51.241409
3425.065587	432418.510268	51.246413
3424.850146	432083.572249	51.251418
3424.023540	431775.998116	51.256423
3423.363840	431448.714518	51.261428
3422.963388	431128.800634	51.266433
3421.959778	430810.273254	51.271437
3421.193298	430476.544429	51.276442
3420.885205	430167.320380	51.281447
3419.889462	429835.016328	51.286452
3419.221658	429510.604791	51.291457
3418.728366	429198.427479	51.296461
3417.942135	428870.090582	51.301466
3417.372171	428554.997351	51.306471
3416.470670	428241.273388	51.311476
3415.819431	427915.747711	51.316481
3414.727354	427608.497079	51.321485
3414.210648	427292.136082	51.326490
3414.018248	426970.869232	51.331495
3412.976698	426672.158716	51.336500
3412.110345	426347.460727	51.341505
3411.480886	426040.652383	51.346509
3411.385771	425724.485701	51.351514
3410.252079	425408.530322	51.356519
3409.811273	425080.549640	51.361524
3409.064131	424771.866034	51.366529
3408.189142	424464.088130	51.371533
3407.756775	424142.241506	51.376538
3407.281569	423838.050926	51.381543
3406.076829	423526.479208	51.386548
3405.835426	423198.850856	51.391553
3404.924647	422887.377837	51.396557
3404.433509	422570.805520	51.401562
3403.537636	422282.133624	51.406567
3402.544816	421958.902235	51.411572
3401.805766	421644.974935	51.416577
3400.917689	421343.895849	51.421581
3400.729030	421037.190571	51.426586
3399.738030	420723.216534	51.431591
3399.301973	420427.822592	51.436596
3398.852334	420125.289323	51.441601
3398.078898	419813.734865	51.446605
3397.247970	419507.393880	51.451610
3396.690944	419191.174814	51.456615
3395.676482	418885.719867	51.461620
3395.579130	418566.702882	51.466625
3394.490221	418287.750531	51.471629
3393.637064	417965.365811	51.476634
3393.323968	417654.451652	51.481639
3392.550602	417357.351500	51.486644
3391.954230	417051.023250	51.491649
3391.123572	416748.133247	51.496653
3390.269912	416446.717292	51.501658
3389.585924	416154.722768	51.506663
3388.739573	415833.431001	51.511668
3388.361715	415536.884772	51.516673
3387.396743	415241.622512	51.521677
3387.165920	414944.691301	51.526682
3386.663490	414648.536856	51.531687
3386.029564	414324.831914	51.536692
3385.377095	414029.228518	51.541697
3384.227922	413733.395775	51.546701
3383.785640	413422.990379	51.551706
3382.997361	413107.656142	51.556711
3382.372156	412816.762485	51.561716
3381.660776	412512.183543	51.566721
3381.065925	412208.701117	51.571725
3380.240813	411912.671917	51.576730
3379.637764	411608.396955	51.581735
3378.854209	411307.374658	51.586740
3377.928517	411001.873996	51.591745
3377.162173	410707.551583	51.596749
3376.621120	410400.713426	51.601754
3376.003817	410117.441294	51.606759
3375.530328	409832.339493	51.611764
3374.683304	409510.369487	51.616769
3374.156196	409247.938777	51.621773
3373.402692	408937.358312	51.626778
3372.836986	408640.824022	51.631783
3372.047156	408348.134343	51.636788
3371.001728	408038.327914	51.641793
3370.269417	407750.477502	51.646797
3369.903432	407455.602945	51.651802
3369.179349	407164.746876	51.656807
3368.435965	406894.324660	51.661812
3367.897807	406574.994451	51.666817
3367.099654	406293.088038	51.671821
3366.498108	405994.856617	51.676826
3366.002327	405710.228499	51.681831
3365.282061	405416.153109	51.686836
3364.405940	405125.810383	51.691841
3363.495627	404840.045356	51.696845
3362.975120	404538.737312	51.701850
3362.355499	404243.999649	51.706855
3361.541317	403971.962158	51.711860
3361.087471	403663.518436	51.716865
3360.379370	403393.899300	51.721869
3359.820867	403094.134036	51.726874
3358.953798	402802.116447	51.731879
3358.306707	402519.440788	51.736884
3357.689217	402234.749894	51.741889
3356.890400	401945.789376	51.746893
3356.398823	401658.023223	51.751898
3355.713999	401362.633868	51.756903
3354.988791	401078.686979	51.761908
3354.415694	400791.637773	51.766913
3353.483460	400509.625130	51.771917
3352.846843	400216.175078	51.776922
3352.086972	399935.655438	51.781927
3351.007980	399640.490752	51.786932
3350.468443	399361.202395	51.791937
3349.964576	399093.370917	51.796941
3349.578113	398802.588744	51.801946
3348.958612	398525.441350	51.806951
3347.852052	398239.979502	51.811956
3347.465393	397948.249271	51.816961
3346.597369	397672.328894	51.821965
3345.829758	397389.755134	51.826970
3344.841891	397115.323607	51.831975
3344.469611	396841.504335	51.836980
3344.231371	396556.043350	51.841985
3343.100150	396278.424371	51.846989
3342.457677	395995.844541	51.851994
3341.843817	395728.486558	51.856999
3340.948101	395447.365922	51.862004
3340.490154	395162.309294	51.867009
3339.807013	394889.108153	51.872013
3339.003260	394611.627175	51.877018
3338.341141	394336.816565	51.882023
3337.961390	394063.026950	51.887028
3337.429137	393782.267392	51.892033
3336.444541	393514.340542	51.897037
3335.666390	393223.928321	51.902042
3335.239849	392942.967261	51.907047
3334.293679	392659.670643	51.912052
3333.589863	392397.081054	51.917057
3333.018147	392110.033986	51.922061
3332.433238	391836.055849	51.927066
3331.984400	391570.012596	51.932071
3331.177905	391284.190955	51.937076
3330.755315	391004.205366	51.942081
3329.717442	390731.459911	51.947085
3329.271589	390456.508264	51.952090
3328.796611	390170.904914	51.957095
3327.830861	389901.625271	51.962100
3327.580471	389612.625463	51.967105
3326.635026	389331.488847	51.972109
3325.958515	389052.799488	51.977114
3325.538374	388775.440576	51.982119
3324.660244	388492.455897	51.987124
3324.019657	388219.806482	51.992129
3322.987749	387950.090399	51.997133
3322.523847	387660.981572	52.002138
3321.763604	387387.683670	52.007143
3320.616209	387100.941722	52.012148
3320.584561	386833.780197	52.017153
3319.867640	386563.495461	52.022157
3318.965771	386287.592445	52.027162
3318.302840	386012.336206	52.032167
3317.419858	385741.207065	52.037172
3317.222093	385470.120170	52.042177
3316.298877	385196.374026	52.047181
3315.826421	384913.984240	52.052186
3315.255832	384651.215518	52.057191
3314.289478	384381.157786	52.062196
3313.742078	384099.638387	52.067201
3313.227192	383831.819613	52.072205
3312.755430	383540.848791	52.077210
3311.862087	383272.272067	52.082215
3310.854369	382996.310642	52.087220
3310.440235	382716.260398	52.092225
3309.110805	382463.133754	52.097229
3308.831669	382196.385215	52.102234
3308.441483	381914.061758	52.107239
3307.484626	381647.340277	52.112244
3307.113154	381376.963660	52.117249
3306.048343	381101.328253	52.122253
3305.606663	380816.461519	52.127258
3305.011794	380550.285642	52.132263
3304.018172	380283.916659	52.137268
3303.364336	380005.741352	52.142273
3302.825188	379746.443949	52.147277
3302.129209	379478.623502	52.152282
3301.654202	379213.436971	52.157287
3300.987654	378940.699240	52.162292
3300.329161	378669.611656	52.167297
3299.728144	378394.545174	52.172301
3298.757291	378125.232892	52.177306
3298.138833	377860.238044	52.182311
3297.351814	377587.510078	52.187316
3297.152895	377294.974113	52.192321
3296.033038	377029.875012	52.197325
3295.233854	376759.865054	52.202330
3294.776385	376499.007377	52.207335
3294.146940	376234.334234	52.212340
3293.643387	375969.028965	52.217345
3292.908161	375704.750661	52.222349
3292.429666	375436.741610	52.227354
3291.810227	375157.560531	52.232359
3290.845754	374896.950849	52.237364
3290.590606	374629.842407	52.242369
3289.355119	374358.130343	52.247373
3288.667774	374079.893913	52.252378
3288.073450	373809.908414	52.257383
3287.407513	373555.271988	52.262388
3287.047560	373276.393321	52.267393
3286.258114	373012.513395	52.272397
3285.491539	372744.201784	52.277402
3284.733836	372470.010583	52.282407
3283.706834	372204.789438	52.287412
3283.486173	371940.227735	52.292417
3282.434116	371690.957969	52.297421
3281.818082	371419.306978	52.302426
3281.230606	371154.747524	52.307431
3280.331422	370887.259222	52.312436
3279.919972	370636.101171	52.317441
3279.370946	370376.873319	52.322445
3278.937245	370107.194986	52.327450
3278.314702	369839.147612	52.332455
3277.308188	369585.151862	52.337460
3276.911205	369306.431187	52.342465
3276.050212	369033.379208	52.347469
3275.411553	368777.819542	52.352474
3275.115328	368522.051581	52.357479
3274.145578	368250.792846	52.362484
3274.017846	367966.322118	52.367489
3272.995189	367708.527208	52.372493
3272.488793	367434.493327	52.377498
3271.734040	367167.315602	52.382503
3270.974114	366906.726718	52.387508
3270.411076	366617.202266	52.392513
3269.427699	366358.477412	52.397517
3268.700450	366101.898662	52.402522
3268.195088	365826.964291	52.407527
3267.243282	365555.050286	52.412532
3267.149981	365288.927202	52.417537
3266.137445	365037.298142	52.422541
3265.407570	364758.932501	52.427546
3265.065043	364485.898018	52.432551
3264.082357	364222.428349	52.437556
3263.525684	363952.274306	52.442561
3262.988055	363696.695284	52.447565
3262.117762	363419.666879	52.452570
3261.372162	363163.914266	52.457575
3260.345160	362901.563674	52.462580
3260.067251	362625.683663	52.467585
3259.255189	362372.481734	52.472589
3258.724217	362105.595360	52.477594
3257.921920	361850.200798	52.482599
3257.102898	361592.466522	52.487604
3256.647837	361321.339780	52.492609
3255.935990	361066.740966	52.497613
3255.238433	360808.118087	52.502618
3254.589686	360544.142427	52.507623
3254.049748	360285.848054	52.512628
3253.531371	360012.510120	52.517633
3252.645756	359756.303300	52.522637
3251.849621	359492.905039	52.527642
3251.351905	359229.814411	52.532647
3250.478215	358972.558271	52.537652
3249.923922	358708.990305	52.542657
3249.423554	358456.227428	52.547661
3248.769880	358197.889110	52.552666
3248.055297	357924.239746	52.557671
3247.256726	357675.286266	52.562676
3246.866531	357414.815507	52.567681
3246.028057	357150.826156	52.572685
3245.329648	356881.647333	52.577690
3244.907562	356610.362072	52.582695
3243.838935	356356.584184	52.587700
3243.355211	356086.832758	52.592705
3242.785435	355832.947901	52.597709
3242.114211	355569.178328	52.602714
3241.467542	355312.885434	52.607719
3240.839421	355051.778496	52.612724
3240.403240	354778.602511	52.617729
3239.447725	354514.592558	52.622733
3238.300172	354250.866127	52.627738
3237.945844	353990.855750	52.632743
3237.304794	353738.676972	52.637748
3236.570044	353485.646514	52.642753
3236.047022	353223.902990	52.647757
3235.492279	352954.859074	52.652762
3234.810612	352696.293812	52.657767
3233.955059	352443.862822	52.662772
3233.352523	352165.456825	52.667777
3232.659251	351910.656223	52.672781
3231.860211	351647.497930	52.677786
3231.463999	351377.377518	52.682791
3230.372350	351128.489868	52.687796
3230.057206	350872.708325	52.692801
3229.156009	350614.625888	52.697805
3228.399102	350343.666603	52.702810
3227.976987	350095.202803	52.707815
3227.067904	349845.949561	52.712820
3226.741957	349577.616174	52.717825
3225.944093	349329.106552	52.722829
3225.429921	349077.954873	52.727834
3224.836940	348805.918601	52.732839
3224.305792	348544.637390	52.737844
3223.483738	348273.041995	52.742849
3222.781868	348023.824186	52.747853
3222.188710	347747.048719	52.752858
3221.502232	347488.994179	52.757863
3220.680417	347233.428772	52.762868
3220.295639	346960.536210	52.767873
3219.125367	346707.645197	52.772877
3218.560078	346445.927047	52.777882
3218.262467	346188.186942	52.782887
3217.217118	345938.556237	52.787892
3216.547089	345680.796432	52.792897
3215.852599	345418.585031	52.797901
3215.202114	345165.197834	52.802906
3214.811665	344904.081448	52.807911
3214.058745	344656.817119	52.812916
3213.431208	344386.292653	52.817921
3212.495538	344131.597096	52.822925
3211.643425	343883.047097	52.827930
3211.193260	343618.701868	52.832935
3210.766460	343351.042739	52.837940
3209.861507	343098.908821	52.842945
3209.288783	342840.994063	52.847949
3208.656950	342592.123915	52.852954
3208.130727	342329.185100	52.857959
3207.365785	342082.599400	52.862964
3206.624960	341817.095961	52.867969
3205.858207	341556.915567	52.872973
3205.361768	341302.342344	52.877978
3204.709649	341045.247194	52.882983
3203.945072	340806.954749	52.887988
3203.305545	340535.829679	52.892993
3202.884256	340281.265881	52.897997
3201.645045	340025.557666	52.903002
3201.470489	339764.512511	52.908007
3200.599288	339512.944209	52.913012
3200.327240	339246.770301	52.918017
3199.633399	338986.898727	52.923021
3198.863425	338730.423810	52.928026
3198.347343	338464.158003	52.933031
3197.542487	338205.828235	52.938036
3196.792815	337935.600590	52.943041
3196.129707	337684.552328	52.948045
3195.434127	337419.812611	52.953050
3194.966849	337152.591880	52.958055
3193.846618	336908.588122	52.963060
3193.490026	336657.334752	52.968065
3192.751333	336395.678072	52.973069
3191.886812	336143.535768	52.978074
3191.529765	335887.951902	52.983079
3190.549929	335616.198407	52.988084
3190.320857	335360.439576	52.993089
3189.371550	335106.601205	52.998093
3188.646906	334845.089096	53.003098
3187.933403	334576.140605	53.008103
3187.393784	334345.630206	53.013108
3186.730820	334076.849996	53.018113
3186.121236	333813.992009	53.023117
3185.386696	333568.769753	53.028122
3184.508064	333312.316962	53.033127
3183.747123	333053.655222	53.038132
3183.278344	332794.462619	53.043137
3182.514886	332544.658921	53.048141
3181.934746	332300.120716	53.053146
3181.275733	332028.557180	53.058151
3180.534026	331779.154735	53.063156
3180.014669	331522.409607	53.068161
3179.488106	331274.702602	53.073165
3178.784011	331009.838087	53.078170
3177.980735	330758.787092	53.083175
3177.240075	330502.175263	53.088180
3176.713569	330243.084595	53.093185
3176.096913	329987.266079	53.098189
3175.535609	329735.002247	53.103194
3175.107960	329475.816926	53.108199
3173.857040	329227.021149	53.113204
3173.266133	328968.063608	53.118209
3172.807954	328703.584905	53.123213
3171.673988	328454.335310	53.128218
3171.445395	328213.037917	53.133223
3170.563805	327954.963149	53.138228
3170.007203	327694.366497	53.143233
3169.482495	327440.790925	53.148237
3168.615180	327187.523343	53.153242
3168.353223	326923.847780	53.158247
3167.598454	326662.311600	53.163252
3167.036576	326418.540891	53.168257
3166.013729	326165.778434	53.173261
3165.507297	325903.411234	53.178266
3164.902705	325648.289549	53.183271
3164.233955	325377.824390	53.188276
3163.374280	325126.255023	53.193281
3162.951059	324859.823059	53.198285
3162.025274	324609.713859	53.203290
3161.596233	324343.306630	53.208295
3160.934970	324103.032965	53.213300
3160.017474	323840.393289	53.218305
3159.533506	323580.510421	53.223309
3158.848821	323333.618354	53.228314
3158.189095	323067.778316	53.233319
3157.179198	322809.987779	53.238324
3156.825072	322558.381745	53.243329
3156.103399	322307.826141	53.248333
3155.206403	322059.461807	53.253338
3154.933054	321791.112435	53.258343
3154.234577	321548.189552	53.263348
3153.831072	321274.588607	53.268353
3153.040003	321025.466238	53.273357
3152.051104	320754.171525	53.278362
3151.404074	320513.809389	53.283367
3150.805816	320253.629279	53.288372
3150.206785	319997.140591	53.293377
3149.659019	319732.775204	53.298381
3148.675809	319486.861854	53.303386
3148.385880	319221.664891	53.308391
3147.524808	318976.189206	53.313396
3147.015485	318724.648046	53.318401
3146.358633	318467.782389	53.323405
3145.437168	318212.612990	53.328410
3145.029438	317946.107050	53.333415
3144.323507	317704.524845	53.338420
3143.826489	317424.307081	53.343425
3143.198872	317165.931036	53.348429
3142.311320	316916.634855	53.353434
3141.839114	316654.795367	53.358439
3141.095320	316393.914841	53.363444
3140.051023	316142.604470	53.368449
3139.877448	315870.912314	53.373453
3138.912731	315624.782607	53.378458
3138.403734	315360.246471	53.383463
3137.258037	315106.072220	53.388468
3136.909682	314848.995659	53.393473
3136.226482	314600.094370	53.398477
3135.150044	314349.777810	53.403482
3134.808848	314083.123871	53.408487
3134.299976	313834.778874	53.413492
3133.435726	313573.553840	53.418497
3132.844571	313314.729515	53.423501
3132.171326	313074.047985	53.428506
3131.572882	312820.622027	53.433511
3130.499467	312572.083368	53.438516
3129.940814	312319.362967	53.443521
3129.681190	312058.649820	53.448525
3128.690615	311818.525068	53.453530
3128.235530	311565.430090	53.458535
3127.180934	311313.575308	53.463540
3126.572816	311067.939071	53.468545
3126.017519	310815.825954	53.473549
3125.226693	310557.867227	53.478554
3124.730157	310305.998363	53.483559
3124.080745	310062.607448	53.488564
3123.738779	309805.365473	53.493569
3122.862466	309561.296426	53.498573
3121.968576	309302.383630	53.503578
3121.762197	309043.386972	53.508583
3121.042006	308785.948035	53.513588
3120.543152	308534.483299	53.518593
3119.733508	308279.960488	53.523597
3118.830358	308022.548928	53.528602
3118.366793	307766.034972	53.533607
3117.481849	307518.143504	53.538612
3117.043433	307261.879215	53.543617
3116.358159	307005.016847	53.548621
3115.424164	306760.442193	53.553626
3115.133256	306493.152005	53.558631
3114.144529	306247.922965	53.563636
3113.712569	305993.845232	53.568641
3112.949266	305737.705804	53.573645
3112.519209	305475.095822	53.578650
3112.032693	305215.066310	53.583655
3111.413775	304965.829275	53.588660
3111.091710	304707.428071	53.593665
3110.256698	304444.319980	53.598669
3109.150129	304183.495371	53.603674
3108.686119	303923.332597	53.608679
3107.790950	303662.779192	53.613684
3107.151748	303397.804668	53.618689
3106.418821	303149.142785	53.623693
3105.750725	302889.621667	53.628698
3105.310361	302630.115003	53.633703
3104.193744	302370.765832	53.638708
3103.833319	302107.680366	53.643713
3103.508052	301843.493843	53.648717
3102.332750	301603.328791	53.653722
3101.725707	301344.992341	53.658727
3101.176674	301083.615793	53.663732
3100.462789	300825.651946	53.668737
3099.843640	300569.964686	53.673741
3099.252039	300318.423715	53.678746
3098.788268	300046.667152	53.683751
3097.728420	299797.567883	53.688756
3096.946929	299547.176340	53.693761
3096.554749	299285.746694	53.698765
3095.740264	299025.656813	53.703770
3095.115990	298767.726593	53.708775
3094.410329	298523.764679	53.713780
3093.691965	298258.208577	53.718785
3093.085691	298010.104619	53.723789
3092.383129	297748.900112	53.728794
3092.050258	297489.393960	53.733799
3091.089039	297242.414757	53.738804
3090.540484	296985.437808	53.743809
3089.872056	296720.304568	53.748813
3089.113516	296467.282084	53.753818
3088.683814	296207.458463	53.758823
3087.687018	295943.420294	53.763828
3087.071675	295693.404766	53.768833
3086.673738	295455.222244	53.773837
3085.592384	295199.931750	53.778842
3084.952651	294928.450293	53.783847
3084.350225	294683.397633	53.788852
3083.595328	294430.575824	53.793857
3082.952687	294178.601852	53.798861
3082.040121	293921.500430	53.803866
3081.853239	293670.854475	53.808871
3081.290603	293425.870539	53.813876
3080.545546	293175.770785	53.818881
3079.917621	292914.726681	53.823885
3079.043575	292665.283488	53.828890
3078.456204	292389.308437	53.833895
3077.764793	292148.443846	53.838900
3076.822441	291890.046096	53.843905
3076.510210	291636.438156	53.848909
3075.665946	291392.184377	53.853914
3075.392191	291133.068849	53.858919
3074.464027	290888.394932	53.863924
3073.877171	290625.508309	53.868929
3073.134369	290376.475093	53.873933
3072.323560	290134.354180	53.878938
3071.771460	289861.554386	53.883943
3071.411915	289614.319007	53.888948
3070.589170	289357.631756	53.893953
3069.755867	289104.384116	53.898957
3068.964067	288846.698292	53.903962
3068.485567	288592.477248	53.908967
3067.991618	288342.817201	53.913972
3067.408386	288083.926236	53.918977
3066.791941	287823.843333	53.923981
3065.840284	287580.953217	53.928986
3065.536455	287314.682680	53.933991
3064.862668	287057.307886	53.938996
3063.665768	286814.074036	53.944001
3063.339133	286546.558615	53.949005
3062.959093	286297.133774	53.954010
3062.150748	286025.644801	53.959015
3061.163336	285775.424365	53.964020
3060.549527	285525.857761	53.969025
3060.195586	285262.038678	53.974029
3059.162945	285016.918574	53.979034
3058.491887	284748.565103	53.984039
3058.037738	284493.344188	53.989044
3057.374018	284228.962290	53.994049
3056.893196	283980.239707	53.999053
3055.907773	283726.452278	54.004058
3055.290161	283466.366808	54.009063
3054.579287	283211.262273	54.014068
3053.712739	282962.727593	54.019073
3053.418834	282699.712626	54.024077
3052.589152	282455.017602	54.029082
3052.143536	282196.967266	54.034087
3051.240013	281943.548114	54.039092
3050.553063	281683.651117	54.044097
3049.919337	281436.097723	54.049101
3049.369423	281181.552667	54.054106
3048.784781	280917.436937	54.059111
3048.017046	280671.916501	54.064116
3047.267080	280415.187117	54.069121
3046.908514	280152.181446	54.074125
3045.956719	279910.408306	54.079130
3045.592915	279642.156849	54.084135
3044.959727	279388.184765	54.089140
3044.135204	279132.638399	54.094145
3043.774596	278871.491928	54.099149
3042.883560	278608.060792	54.104154
3042.175704	278346.638090	54.109159
3041.328511	278091.553554	54.114164
3040.730461	277835.894718	54.119169
3040.116615	277572.139404	54.124173
3039.082024	277328.392393	54.129178
3038.528001	277073.261343	54.134183
3038.211794	276814.603467	54.139188
3037.492200	276560.339042	54.144193
3036.766044	276311.627753	54.149197
3035.865337	276055.405437	54.154202
3035.463724	275793.628428	54.159207
3034.767721	275550.133378	54.164212
3033.847130	275293.914212	54.169217
3033.415176	275032.269361	54.174221
3032.638765	274779.974999	54.179226
3031.975553	274528.910690	54.184231
3031.581886	274276.479387	54.189236
3030.769408	274016.040913	54.194241
3030.370788	273763.584979	54.199245
3029.254714	273518.450173	54.204250
3028.651341	273248.988371	54.209255
3027.860265	273001.382712	54.214260
3027.143054	272758.069560	54.219265
3027.103460	272489.893966	54.224269
3026.133642	272242.418611	54.229274
3025.357474	271984.190490	54.234279
3025.037672	271729.175621	54.239284
3024.000634	271469.893777	54.244289
3023.645123	271216.234516	54.249293
3022.780854	270959.625118	54.254298
3022.398726	270699.195650	54.259303
3021.488164	270448.680665	54.264308
3020.547649	270190.173460	54.269313
3020.428199	269933.726672	54.274317
3019.546409	269688.632142	54.279322
3018.762271	269422.459992	54.284327
3017.978798	269169.735087	54.289332
3017.455672	268926.392331	54.294337
3016.594829	268663.416182	54.299341
3016.127417	268419.198901	54.304346
3015.516934	268164.409598	54.309351
3015.077272	267908.931208	54.314356
3014.251504	267658.785967	54.319361
3013.982801	267389.222344	54.324365
3012.864403	267139.709450	54.329370
3012.063326	266878.558462	54.334375
3011.662764	266630.434852	54.339380
3010.923211	266364.002523	54.344385
3010.322684	266102.973060	54.349389
3009.754628	265839.850237	54.354394
3009.169761	265569.548250	54.359399
3008.369536	265314.688701	54.364404
3007.304481	265060.431530	54.369409
3006.903575	264794.023045	54.374413
3006.182343	264544.474326	54.379418
3005.497065	264283.790583	54.384423
3004.716276	264040.975188	54.389428
3004.113814	263781.679449	54.394433
3003.701646	263519.170300	54.399437
3003.008349	263274.431513	54.404442
3002.809729	263016.804271	54.409447
3002.032670	262747.018750	54.414452
3000.950869	262496.255233	54.419457
3000.455283	262235.823240	54.424461
2999.654546	261977.451726	54.429466
2999.212326	261710.899476	54.434471
2998.446980	261459.832069	54.439476
2997.434345	261209.822733	54.444481
2997.239360	260949.853673	54.449485
2996.275231	260703.606338	54.454490
2995.510921	260430.280952	54.459495
2994.914955	260183.211794	54.464500
2994.211835	259929.589188	54.469505
2994.019694	259667.838201	54.474509
2993.252237	259414.379097	54.479514
2992.332534	259159.900180	54.484519
2991.700539	258899.009115	54.489524
2990.910277	258639.314886	54.494529
2990.553540	258377.056514	54.499533
2989.681836	258132.146852	54.504538
2988.968710	257863.604082	54.509543
2988.659509	257603.427390	54.514548
2987.571676	257360.131745	54.519553
2987.074374	257101.156911	54.524557
2986.326569	256836.211759	54.529562
2985.570678	256586.039211	54.534567
2984.735075	256327.933806	54.539572
2984.537338	256079.099677	54.544577
2983.980929	255815.526208	54.549581
2983.040222	255562.862896	54.554586
2982.581845	255304.597201	54.559591
2981.958008	255035.840141	54.564596
2980.893865	254792.543751	54.569601
2980.482128	254532.692733	54.574605
2980.019820	254277.892526	54.579610
2978.997986	254016.356095	54.584615
2978.467343	253750.209177	54.589620
2977.464859	253509.604166	54.594625
2977.144959	253249.383856	54.599629
2976.360791	252990.052343	54.604634
2975.919908	252732.958875	54.609639
2975.197091	252477.998676	54.614644
2974.562024	252218.797494	54.619649
2974.133703	251953.986787	54.624653
2973.349423	251694.860946	54.629658
2972.699870	251449.466108	54.634663
2971.994932	251188.800495	54.639668
2971.049146	250935.838821	54.644673
2970.660567	250655.412936	54.649677
2969.922046	250416.145659	54.654682
2969.340368	250157.092032	54.659687
2968.716983	249891.551523	54.664692
2967.878665	249637.148770	54.669697
2967.279457	249373.286085	54.674701
2966.424729	249114.888592	54.679706
2965.884009	248859.726960	54.684711
2965.207852	248608.890965	54.689716
2964.671890	248347.159199	54.694721
2964.267721	248081.612599	54.699725
2963.123120	247838.084399	54.704730
2962.427763	247573.679848	54.709735
2961.902470	247319.664397	54.714740
2961.260254	247057.620707	54.719745
2960.581424	246801.465889	54.724749
2959.955382	246540.668420	54.729754
2959.319487	246282.877948	54.734759
2958.670441	246029.953972	54.739764
2957.765669	245769.023821	54.744769
2957.351448	245511.225176	54.749773
2956.608412	245248.818892	54.754778
2956.012475	244998.944295	54.759783
2955.487080	244734.467339	54.764788
2954.606233	244473.739655	54.769793
2953.859664	244219.230230	54.774797
2953.252900	243973.230028	54.779802
2952.643059	243719.973209	54.784807
2952.162596	243460.890365	54.789812
2951.134066	243204.899688	54.794817
2950.869575	242934.961083	54.799821
2949.917744	242685.809423	54.804826
2949.315926	242425.449226	54.809831
2948.796797	242166.604387	54.814836
2947.734457	241903.517072	54.819841
2947.847861	241644.776938	54.824845
2947.147441	241390.724372	54.829850
2946.597449	241124.680157	54.834855
2945.666922	240860.886736	54.839860
2944.861435	240604.738940	54.844865
2944.425371	240328.034333	54.849869
2943.519005	240073.482480	54.854874
2942.904918	239817.968211	54.859879
2942.493265	239547.602254	54.864884
2941.605421	239277.566969	54.869889
2941.146079	239019.840091	54.874893
2940.042561	238753.990879	54.879898
2939.599705	238490.125775	54.884903
2938.988853	238227.866670	54.889908
2938.097882	237976.423783	54.894913
2937.901740	237713.463675	54.899917
2937.204060	237442.817148	54.904922
2936.523496	237178.254433	54.909927
2935.961984	236913.444361	54.914932
2935.040749	236656.432840	54.919937
2934.527700	236379.088353	54.924941
2933.898350	236122.312046	54.929946
2933.202907	235854.597575	54.934951
2932.677721	235595.030587	54.939956
2931.527540	235327.847828	54.944961
2931.052794	235049.609671	54.949965
2930.280102	234799.810859	54.954970
2929.752665	234538.031663	54.959975
2929.213670	234256.113749	54.964980
2928.419079	233999.980136	54.969985
2928.024899	233726.469054	54.974989
2927.182817	233473.272575	54.979994
2926.394646	233194.885585	54.984999
2925.893681	232928.803325	54.990004
2925.070123	232663.256668	54.995009
2924.534249	232401.128114	55.000013
2923.591810	232127.453781	55.005018
2923.194639	231874.827695	55.010023
2922.730830	231600.799050	55.015028
2921.644157	231344.871617	55.020033
2921.116638	231078.900675	55.025037
2920.582145	230818.482346	55.030042
2919.788344	230544.941958	55.035047
2919.195132	230286.902421	55.040052
2918.345301	230021.087463	55.045057
2918.033790	229752.921977	55.050061
2917.037109	229484.967619	55.055066
2916.461821	229234.312194	55.060071
2915.867951	228976.047422	55.065076
2915.218191	228695.793550	55.070081
2914.831576	228425.352483	55.075085
2913.736491	228177.277614	55.080090
2913.238765	227897.613340	55.085095
2912.482488	227630.059503	55.090100
2911.598657	227382.590033	55.095105
2911.061429	227115.104992	55.100109
2910.404519	226846.990499	55.105114
2909.780543	226584.829489	55.110119
2908.973804	226324.124045	55.115124
2908.494552	226057.295207	55.120129
2907.892618	225798.150298	55.125133
2907.097220	225535.345066	55.130138
2906.936661	225268.188288	55.135143
2906.183957	224992.787877	55.140148
2905.203275	224735.908650	55.145153
2904.638019	224457.616124	55.150157
2903.887019	224200.995050	55.155162
2903.213722	223945.864648	55.160167
2902.780650	223675.624767	55.165172
2901.755589	223405.097645	55.170177
2901.287246	223137.487574	55.175181
2900.622909	222880.729809	55.180186
2899.825731	222609.418327	55.185191
2899.034527	222342.867781	55.190196
2898.374087	222093.406176	55.195201
2898.083027	221829.515128	55.200205
2897.308652	221555.683319	55.205210
2896.673752	221305.189172	55.210215
2895.940937	221031.772770	55.215220
2895.114398	220760.459843	55.220225
2894.629184	220493.370957	55.225229
2893.963453	220236.915191	55.230234
2893.179705	219972.943239	55.235239
2892.885417	219705.190523	55.240244
2891.650848	219451.106119	55.245249
2891.270868	219181.446786	55.250253
2890.508952	218923.954354	55.255258
2889.885404	218659.465390	55.260263
2889.383407	218395.263657	55.265268
2888.463206	218142.356107	55.270273
2888.192984	217865.772511	55.275277
2887.435138	217599.641267	55.280282
2886.740108	217344.995255	55.285287
2886.593320	217064.589343	55.290292
2885.627977	216811.108217	55.295297
2884.770871	216526.018200	55.300301
2884.202555	216263.222449	55.305306
2883.783400	215987.102684	55.310311
2883.100328	215720.024918	55.315316
2881.958337	215451.315241	55.320321
2881.913323	215182.343850	55.325325
2880.971498	214907.100403	55.330330
2879.957406	214641.619455	55.335335
2879.583422	214372.996149	55.340340
2878.909728	214113.713014	55.345345
2878.326041	213834.115147	55.350349
2877.404131	213570.151282	55.355354
2876.376747	213307.299797	55.360359
2876.287639	213039.285959	55.365364
2875.361720	212778.915239	55.370369
2874.836605	212508.465210	55.375373
2874.232885	212247.969249	55.380378
2873.265944	211979.526039	55.385383
2873.091833	211705.447292	55.390388
2872.047755	211439.729587	55.395393
2871.685094	211170.315899	55.400397
2870.741204	210907.130105	55.405402
2870.137885	210632.894864	55.410407
2869.544008	210376.350583	55.415412
2868.682561	210108.089542	55.420417
2868.238984	209839.610767	55.425421
2867.716365	209574.225692	55.430426
2867.077927	209310.578285	55.435431
2866.523231	209042.998759	55.440436
2865.811245	208772.250784	55.445441
2865.025228	208501.401191	55.450445
2864.471040	208238.088713	55.455450
2863.748197	207957.469884	55.460455
2863.118218	207683.557496	55.465460
2862.253116	207419.037864	55.470465
2861.875381	207140.544519	55.475469
2860.850398	206874.296319	55.480474
2860.151157	206606.254177	55.485479
2859.713510	206328.232302	55.490484
2859.110699	206062.748154	55.495489
2858.418064	205796.006779	55.500493
2857.391994	205533.340994	55.505498
2856.882908	205269.500064	55.510503
2856.336638	204998.030397	55.515508
2855.511028	204731.467695	55.520513
2855.187394	204467.639251	55.525517
2854.429045	204198.904911	55.530522
2853.480712	203933.917956	55.535527
2853.103277	203657.541079	55.540532
2852.242480	203396.042452	55.545537
2851.713810	203123.662655	55.550541
2851.160717	202853.171481	55.555546
2850.411693	202583.527092	55.560551
2849.610354	202309.743689	55.565556
2849.125068	202054.440233	55.570561
2848.480345	201778.560364	55.575565
2847.825876	201513.691055	55.580570
2846.725095	201249.619051	55.585575
2846.236852	200980.004829	55.590580
2845.607117	200709.040001	55.595585
2844.737433	200448.562026	55.600589
2844.335852	200183.748213	55.605594
2843.515899	199920.058140	55.610599
2843.175272	199648.187537	55.615604
2842.081584	199391.631319	55.620609
2841.762498	199120.370793	55.625613
2841.323897	198850.212197	55.630618
2840.384918	198575.006077	55.635623
2840.211728	198307.836748	55.640628
2839.136673	198043.165665	55.645633
2838.830597	197763.498974	55.650637
2837.582352	197497.878272	55.655642
2837.252481	197224.173369	55.660647
2836.808857	196952.256628	55.665652
2836.051090	196693.522679	55.670657
2835.252226	196411.154654	55.675661
2834.736687	196140.984093	55.680666
2833.463462	195883.811866	55.685671
2832.985876	195606.945170	55.690676
2832.522772	195335.103707	55.695681
2831.896272	195061.889933	55.700685
2831.351824	194809.213848	55.705690
2830.410939	194540.175249	55.710695
2830.098018	194257.767699	55.715700
2829.133702	193988.506745	55.720705
2828.485984	193721.767298	55.725709
2828.228804	193448.974613	55.730714
2827.085775	193183.398004	55.735719
2827.060433	192905.469460	55.740724
2825.831503	192632.746102	55.745729
2825.432317	192358.175218	55.750733
2824.631924	192092.054044	55.755738
2823.913200	191813.185469	55.760743
2823.848917	191540.970841	55.765748
2822.561579	191285.949424	55.770753
2822.062430	191004.226220	55.775757
2821.650432	190724.641038	55.780762
2820.908296	190461.216878	55.785767
2820.096704	190187.041708	55.790772
2819.333330	189913.178548	55.795777
2818.749999	189634.886431	55.800781
2817.884969	189374.617518	55.805786
2817.123092	189106.662053	55.810791
2817.214180	188821.639522	55.815796
2816.352737	188553.448532	55.820801
2815.732659	188278.198176	55.825805
2814.972341	188005.401591	55.830810
2814.292579	187724.667982	55.835815
2813.687659	187452.804197	55.840820
2812.867191	187183.393319	55.845825
2812.335454	186905.363751	55.850829
2811.446286	186630.343928	55.855834
2810.958263	186355.058687	55.860839
2810.443970	186080.084588	55.865844
2809.588487	185804.835423	55.870849
2808.777467	185523.042045	55.875853
2808.326415	185248.190195	55.880858
2807.528924	184977.262172	55.885863
2807.065118	184701.054504	55.890868
2806.158517	184421.801975	55.895873
2805.977471	184147.880923	55.900877
2805.175249	183881.018328	55.905882
2804.482024	183600.732203	55.910887
2803.862105	183313.452494	55.915892
2803.146976	183038.159987	55.920897
2802.107406	182766.088040	55.925901
2801.507791	182489.445009	55.930906
2800.853216	182218.345869	55.935911
2800.337244	181934.722255	55.940916
2799.283822	181675.532411	55.945921
2799.090413	181392.166551	55.950925
2798.349411	181125.412833	55.955930
2797.549950	180856.342241	55.960935
2797.094146	180558.064542	55.965940
2796.473414	180293.408477	55.970945
2795.931508	180015.894479	55.975949
2795.424987	179736.176160	55.980954
2794.458588	179457.422896	55.985959
2793.723984	179180.402790	55.990964
2793.127330	178903.120985	55.995969
2792.531350	178609.152958	56.000973
2791.788748	178339.885812	56.005978
2790.704965	178081.702070	56.010983
2790.670628	177791.174093	56.015988
2789.946524	177515.842273	56.020993
2789.302290	177236.722075	56.025997
2788.973621	176957.757288	56.031002
2787.765665	176671.505820	56.036007
2786.991615	176384.755190	56.041012
2786.301643	176124.193771	56.046017
2785.896426	175844.014960	56.051021
2785.210505	175559.151238	56.056026
2784.380843	175292.130813	56.061031
2783.858631	175008.084449	56.066036
2783.154543	174738.860229	56.071041
2782.386129	174452.402140	56.076045
2781.717012	174175.964940	56.081050
2781.275653	173904.199236	56.086055
2780.587499	173618.383014	56.091060
2779.883428	173352.932601	56.096065
2779.323836	173070.406587	56.101069
2778.637365	172788.958244	56.106074
2777.488206	172517.225094	56.111079
2777.031806	172231.929015	56.116084
2776.201884	171972.930121	56.121089
2775.672092	171691.668282	56.126093
2774.896837	171423.189981	56.131098
2774.080698	171150.230859	56.136103
2774.044883	170870.766117	56.141108
2772.946512	170604.264911	56.146113
2772.500158	170323.215933	56.151117
2771.954721	170051.277173	56.156122
2770.853792	169773.019111	56.161127
2770.445581	169494.360872	56.166132
2770.069055	169232.879610	56.171137
2769.043215	168950.559071	56.176141
2768.266769	168673.313077	56.181146
2767.799417	168396.541515	56.186151
2767.126596	168146.559228	56.191156
2766.356163	167798.807840	56.196161
2765.955140	167526.215707	56.201165
2765.485122	167243.476537	56.206170
2764.686372	166964.975035	56.211175
2763.841351	166685.147793	56.216180
2763.429990	166405.050517	56.221185
2762.558303	166134.933584	56.226189
2762.028165	165858.712014	56.231194
2761.191162	165589.331052	56.236199
2760.520564	165306.600211	56.241204
2760.038317	165019.874610	56.246209
2758.971224	164768.883920	56.251213
2758.454180	164469.720172	56.256218
2757.573580	164199.389972	56.261223
2757.233888	163914.150791	56.266228
2756.793547	163648.561093	56.271233
2755.673462	163387.047920	56.276237
2755.378763	163093.810644	56.281242
2754.480146	162823.874973	56.286247
2754.552398	162551.804136	56.291252
2753.150254	162270.268027	56.296257
2752.744366	162000.133358	56.301261
2752.514929	161708.295583	56.306266
2751.413202	161438.466081	56.311271
2750.736893	161150.085526	56.316276
2750.001789	160888.758447	56.321281
2749.396626	160599.748131	56.326285
2748.545563	160333.040287	56.331290
2747.915067	160063.629732	56.336295
2747.703474	159765.461191	56.341300
2746.995898	159489.405533	56.346305
2746.255018	159226.222883	56.351309
2745.801413	158933.197676	56.356314
2744.579672	158662.353295	56.361319
2744.011196	158387.364916	56.366324
2743.451808	158106.758313	56.371329
2742.778144	157804.433738	56.376333
2742.271620	157542.116613	56.381338
2741.266719	157286.783199	56.386343
2740.816730	156973.281819	56.391348
2739.938310	156708.665503	56.396353
2739.740524	156440.371363	56.401357
2738.995568	156170.920238	56.406362
2738.112903	155883.938104	56.411367
2737.291630	155594.800402	56.416372
2736.744735	155339.815799	56.421377
2736.181787	155034.599980	56.426381
2735.550097	154792.191860	56.431386
2734.883179	154486.628848	56.436391
2734.671550	154188.585045	56.441396
2733.837475	153958.989689	56.446401
2732.253017	153648.368140	56.451405
2732.497402	153353.602531	56.456410
2731.660720	153120.467052	56.461415
2730.883913	152813.538593	56.466420
2730.290512	152508.160031	56.471425
2729.580246	152255.805084	56.476429
2729.192859	151970.976990	56.481434
2728.156482	151696.498562	56.486439
2727.525555	151412.921353	56.491444
2726.688782	151146.156351	56.496449
2725.876792	150876.936602	56.501453
2725.480288	150584.648628	56.506458
2724.775356	150308.604206	56.511463
2723.971112	150038.322570	56.516468
2723.127375	149775.891161	56.521473
2723.085948	149481.269203	56.526477
2722.318375	149226.239730	56.531482
2721.419206	148943.196853	56.536487
2720.899159	148662.091732	56.541492
2720.654869	148377.272535	56.546497
2719.354307	148094.758267	56.551501
2719.181167	147809.894741	56.556506
2718.109376	147539.117375	56.561511
2717.371458	147270.538828	56.566516
2716.514826	146990.772630	56.571521
2716.166387	146725.962217	56.576525
2715.652552	146440.504154	56.581530
2714.583419	146181.416753	56.586535
2714.435977	145893.974005	56.591540
2713.767335	145615.067113	56.596545
2712.815209	145339.092252	56.601549
2712.520321	145057.691268	56.606554
2712.011191	144785.183837	56.611559
2710.981132	144498.274989	56.616564
2710.117154	144221.584484	56.621569
2709.608272	143945.589924	56.626573
2709.025451	143670.130531	56.631578
2707.862893	143406.125363	56.636583
2707.636987	143124.845407	56.641588
2706.781874	142854.811410	56.646593
2706.245363	142574.983436	56.651597
2705.438594	142296.865376	56.656602
2705.017295	142032.907119	56.661607
2704.304701	141744.906407	56.666612
2703.532335	141472.940220	56.671617
2702.897805	141190.700957	56.676621
2702.403254	140921.872200	56.681626
2701.585351	140643.135794	56.686631
2700.981978	140364.444221	56.691636
2700.673394	140096.978284	56.696641
2699.899985	139829.143680	56.701645
2699.085365	139532.311959	56.706650
2698.251331	139251.126249	56.711655
2697.802388	138975.243697	56.716660
2697.055770	138710.070251	56.721665
2696.433396	138424.513768	56.726669
2696.209774	138136.076444	56.731674
2695.109524	137869.962883	56.736679
2694.366762	137590.836609	56.741684
2693.763451	137305.237123	56.746689
2692.947393	137040.102395	56.751693
2692.186336	136753.021484	56.756698
2691.332784	136483.336995	56.761703
2690.901976	136205.711677	56.766708
2690.462622	135940.412924	56.771713
2689.733995	135658.088837	56.776717
2689.095245	135374.876724	56.781722
2688.380408	135104.243008	56.786727
2687.656507	134821.672266	56.791732
2687.187559	134550.509366	56.796737
2686.312653	134276.923556	56.801741
2686.017785	133990.647264	56.806746
2684.979016	133708.581947	56.811751
2684.302956	133450.012525	56.816756
2683.656555	133177.823708	56.821761
2682.832694	132902.096250	56.826765
2682.620237	132613.724824	56.831770
2681.600661	132353.987667	56.836775
2681.179695	132071.548558	56.841780
2680.585817	131795.592196	56.846785
2679.861824	131520.141811	56.851789
2679.160559	131239.698796	56.856794
2678.359601	130959.388687	56.861799
2677.572638	130679.803138	56.866804
2677.346646	130410.089260	56.871809
2676.683360	130135.379528	56.876813
2675.884941	129855.638928	56.881818
2674.980522	129585.595968	56.886823
2674.531918	129308.764746	56.891828
2673.901669	129019.099376	56.896833
2673.047832	128752.599979	56.901837
2672.473438	128468.494329	56.906842
2671.500175	128192.595623	56.911847
2671.274828	127914.422184	56.916852
2670.466903	127641.639731	56.921857
2669.645064	127376.799585	56.926861
2669.520309	127102.771283	56.931866
2668.533804	126818.176523	56.936871
2668.040992	126541.380167	56.941876
2667.480895	126258.831804	56.946881
2666.758070	125984.274539	56.951885
2666.293631	125697.691228	56.956890
2665.337865	125436.078650	56.961895
2664.725578	125146.222892	56.966900
2664.335954	124857.757222	56.971905
2663.517411	124598.023138	56.976909
2662.965883	124303.163621	56.981914
2661.683824	124025.045085	56.986919
2661.241173	123737.425248	56.991924
2660.680303	123463.629940	56.996929
2659.531632	123193.206615	57.001933
2659.021754	122919.180264	57.006938
2658.579790	122644.942820	57.011943
2658.199272	122366.521014	57.016948
2657.397410	122093.489070	57.021953
2656.591095	121821.578008	57.026957
2655.896366	121528.371804	57.031962
2655.407198	121254.930790	57.036967
2654.971306	120968.393797	57.041972
2654.072049	120695.836175	57.046977
2653.560187	120418.604833	57.051981
2652.695222	120128.545553	57.056986
2652.076724	119873.276242	57.061991
2651.203243	119586.747555	57.066996
2650.571937	119312.708236	57.072001
2649.822058	119036.767180	57.077005
2649.461359	118752.172414	57.082010
2648.734510	118485.177716	57.087015
2647.863670	118197.197654	57.092020
2647.318640	117924.574927	57.097025
2646.508198	117656.542010	57.102029
2646.219911	117378.704774	57.107034
2645.243174	117101.582634	57.112039
2644.979434	116822.871595	57.117044
2644.286215	116551.302543	57.122049
2643.374801	116270.396086	57.127053
2642.824424	115989.638639	57.132058
2642.062097	115713.246598	57.137063
2641.240818	115442.921977	57.142068
2640.743150	115156.821207	57.147073
2639.742057	114891.018279	57.152077
2639.509299	114596.072411	57.157082
2638.573985	114343.307553	57.162087
2638.089317	114064.452427	57.167092
2637.625885	113793.492223	57.172097
2636.300095	113516.388505	57.177101
2636.113499	113239.786438	57.182106
2635.589802	112963.748559	57.187111
2634.853667	112686.573326	57.192116
2633.937370	112410.070701	57.197121
2633.202523	112135.344726	57.202125
2632.907796	111849.192508	57.207130
2632.128404	111593.771806	57.212135
2631.623988	111304.206868	57.217140
2631.040541	111019.836110	57.222145
2629.952745	110748.462319	57.227149
2629.497755	110464.153784	57.232154
2628.654100	110192.842641	57.237159
2627.992497	109919.252965	57.242164
2627.328122	109650.495752	57.247169
2626.528744	109384.738922	57.252173
2626.407391	109098.216906	57.257178
2625.533542	108835.764789	57.262183
2624.548078	108545.889919	57.267188
2624.309047	108271.801289	57.272193
2623.203899	108008.677770	57.277197
2622.662809	107732.822059	57.282202
2622.176524	107460.939119	57.287207
2621.535890	107187.573616	57.292212
2621.126703	106910.925995	57.297217
2620.347093	106627.189711	57.302221
2619.660599	106336.951425	57.307226
2618.466431	106069.206252	57.312231
2618.219954	105797.044046	57.317236
2617.715346	105516.659011	57.322241
2616.270203	105250.542574	57.327245
2615.924725	104983.810773	57.332250
2615.356108	104712.803238	57.337255
2614.659998	104429.054528	57.342260
2614.032553	104167.705698	57.347265
2613.355604	103901.882375	57.352269
2612.993567	103618.325201	57.357274
2611.905176	103361.296111	57.362279
2611.389210	103085.033506	57.367284
2611.125054	102802.771142	57.372289
2610.183671	102538.959007	57.377293
2609.590669	102253.634290	57.382298
2608.876024	101989.900269	57.387303
2607.944168	101708.556203	57.392308
2607.525749	101430.356610	57.397313
2606.596923	101160.087867	57.402317
2606.163101	100883.330851	57.407322
2605.453310	100626.049901	57.412327
2604.474981	100344.450647	57.417332
2604.425773	100069.494598	57.422337
2603.581275	99801.048816	57.427341
2602.992674	99530.402708	57.432346
2602.175473	99243.146261	57.437351
2601.794946	98969.537095	57.442356
2600.832186	98701.953796	57.447361
2600.128724	98427.634824	57.452365
2599.818700	98146.096169	57.457370
2599.116016	97893.766454	57.462375
2598.593445	97610.733237	57.467380
2597.824417	97323.766021	57.472385
2597.035888	97060.721771	57.477389
2596.472327	96774.731005	57.482394
2595.719151	96503.823456	57.487399
2595.241173	96231.480325	57.492404
2594.649193	95950.394121	57.497409
2593.633864	95682.467911	57.502413
2593.194828	95384.305200	57.507418
2592.526198	95120.503583	57.512423
2591.742166	94845.708119	57.517428
2591.293057	94565.326871	57.522433
2590.409190	94284.745355	57.527437
2589.930644	94005.174819	57.532442
2588.977054	93729.506820	57.537447
2588.523885	93450.294341	57.542452
2587.864202	93178.619565	57.547457
2587.002934	92906.396692	57.552461
2586.751363	92622.730347	57.557466
2585.867454	92352.914734	57.562471
2585.032598	92078.243982	57.567476
2584.447890	91801.260719	57.572481
2583.948400	91526.569069	57.577485
2583.363263	91244.615531	57.582490
2582.462404	90972.372108	57.587495
2581.905326	90687.339851	57.592500
2581.292858	90417.409898	57.597505
2580.421500	90136.162707	57.602509
2580.088010	89854.016039	57.607514
2579.486753	89575.877968	57.612519
2578.631008	89296.027624	57.617524
2577.804920	89020.683826	57.622529
2576.929174	88744.254616	57.627533
2576.408927	88466.041869	57.632538
2575.546794	88201.542404	57.637543
2574.673664	87929.313696	57.642548
2574.495292	87652.439283	57.647553
2573.483674	87387.339564	57.652557
2572.648668	87123.070936	57.657562
2572.269786	86848.438398	57.662567
2571.627795	86575.163277	57.667572
2571.040674	86308.228346	57.672577
2570.660528	86025.511608	57.677581
2570.020364	85750.738076	57.682586
2569.209003	85480.723971	57.687591
2568.138873	85206.760909	57.692596
2567.738207	84925.126953	57.697601
2566.780698	84665.738252	57.702605
2566.341631	84392.871018	57.707610
2565.806813	84118.063915	57.712615
2564.950377	83855.087955	57.717620
2564.588345	83579.379464	57.722625
2563.864931	83310.063672	57.727629
2563.211436	83035.543031	57.732634
2562.527307	82773.034995	57.737639
2561.748067	82490.733010	57.742644
2561.177362	82210.911565	57.747649
2560.382734	81947.563119	57.752653
2560.103484	81667.202091	57.757658
2559.462569	81390.552594	57.762663
2558.618014	81133.433179	57.767668
2557.851360	80849.003025	57.772673
2557.349833	80580.137249	57.777677
2556.586608	80298.033576	57.782682
2556.022755	80041.662703	57.787687
2555.238510	79760.146387	57.792692
2554.934531	79486.631128	57.797697
2553.697495	79213.691944	57.802701
2553.205303	78931.969570	57.807706
2552.603263	78658.423848	57.812711
2551.902718	78395.885143	57.817716
2551.322212	78110.994371	57.822721
2550.338157	77849.534134	57.827725
2549.960121	77567.527298	57.832730
2549.213411	77302.405703	57.837735
2548.349764	77029.937055	57.842740
2548.092544	76748.796811	57.847745
2547.164256	76491.089846	57.852749
2546.458223	76205.029113	57.857754
2545.976553	75941.207508	57.862759
2545.471630	75674.465887	57.867764
2544.457712	75400.794813	57.872769
2543.624178	75127.802123	57.877773
2543.389402	74863.974481	57.882778
2542.473859	74590.153120	57.887783
2541.776182	74314.628425	57.892788
2541.463470	74046.300416	57.897793
2540.191838	73776.613862	57.902797
2539.889037	73510.166692	57.907802
2539.244666	73249.605448	57.912807
2538.390729	72968.815299	57.917812
2537.911969	72701.906353	57.922817
2537.412603	72425.565430	57.927821
2536.733017	72158.967998	57.932826
2535.953528	71894.258694	57.937831
2535.090505	71622.902248	57.942836
2534.830394	71350.598821	57.947841
2534.087906	71084.266544	57.952845
2533.266806	70798.827185	57.957850
2532.661808	70545.604984	57.962855
2531.719666	70267.831529	57.967860
2531.377883	69989.200437	57.972865
2530.420061	69738.331134	57.977869
2530.053808	69463.011368	57.982874
2529.055678	69195.681129	57.987879
2528.282060	68928.426637	57.992884
2527.592794	68646.576233	57.997889
2526.779656	68392.312829	58.002893
2526.214355	68124.662667	58.007898
2525.725111	67865.611101	58.012903
2525.060089	67593.962405	58.017908
2524.432794	67335.829610	58.022913
2523.510197	67073.592579	58.027917
2523.322381	66805.014176	58.032922
2522.434576	66545.112500	58.037927
2521.471074	66287.971590	58.042932
2521.105681	66012.038837	58.047937
2520.226053	65758.539344	58.052941
2519.730972	65495.876063	58.057946
2519.144869	65227.917883	58.062951
2518.326534	64961.624506	58.067956
2517.642451	64705.806127	58.072961
2516.723420	64444.516243	58.077965
2516.466929	64179.965208	58.082970
2515.940029	63920.519978	58.087975
2514.957228	63650.816843	58.092980
2514.588894	63387.516603	58.097985
2513.877028	63140.065839	58.102989
2513.167611	62860.772819	58.107994
2512.610292	62600.546318	58.112999
2512.123128	62335.335730	58.118004
2511.172066	62072.630480	58.123009
2510.323647	61817.630483	58.128013
2509.878668	61542.924217	58.133018
2509.359021	61283.181583	58.138023
2508.558637	61021.708010	58.143028
2507.952411	60756.212474	58.148033
2507.191176	60489.843118	58.153037
2506.560135	60227.568750	58.158042
2505.911765	59962.167117	58.163047
2505.147345	59701.899603	58.168052
2504.691051	59436.876984	58.173057
2503.937393	59175.950402	58.178061
2503.612673	58907.299795	58.183066
2502.542707	58642.293967	58.188071
2501.652393	58374.601624	58.193076
2501.188204	58120.319122	58.198081
2500.205544	57852.503367	58.203085
2499.777787	57601.808137	58.208090
2499.132631	57340.988288	58.213095
2498.377181	57089.722138	58.218100
2497.983625	56814.732464	58.223105
2497.118547	56563.889629	58.228109
2496.205357	56305.297956	58.233114
2495.683856	56036.606339	58.238119
2494.719232	55792.815387	58.243124
2494.527746	55531.810046	58.248129
2493.563900	55273.101725	58.253133
2493.017262	55019.387798	58.258138
2492.072707	54759.607765	58.263143
2491.629022	54496.220569	58.268148
2491.248438	54247.269313	58.273153
2490.226774	53991.183126	58.278157
2489.486888	53747.076955	58.283162
2488.859531	53486.907261	58.288167
2488.260909	53241.975455	58.293172
2487.763662	52976.622187	58.298177
2487.030524	52729.196827	58.303181
2486.470733	52471.714172	58.308186
2485.822223	52216.119182	58.313191
2484.717483	51965.327094	58.318196
2484.271777	51702.559859	58.323201
2483.516972	51459.246316	58.328205
2482.990288	51209.151462	58.333210
2482.487863	50936.058717	58.338215
2481.642350	50689.539776	58.343220
2481.053352	50438.225377	58.348225
2480.569245	50178.656584	58.353229
2479.768102	49923.700568	58.358234
2478.852273	49669.351636	58.363239
2478.218861	49422.218665	58.368244
2477.899996	49157.991345	58.373249
2477.060829	48913.795791	58.378253
2476.165936	48657.145562	58.383258
2475.758669	48407.472817	58.388263
2474.733353	48165.284674	58.393268
2474.133030	47896.815529	58.398273
2473.617290	47653.977907	58.403277
2472.994572	47402.572625	58.408282
2472.208383	47158.810441	58.413287
2471.789695	46902.717529	58.418292
2470.871637	46650.607503	58.423297
2470.040709	46417.771929	58.428301
2469.638899	46147.374898	58.433306
2469.091699	45903.484708	58.438311
2468.265269	45655.106670	58.443316
2467.541065	45401.247489	58.448321
2466.900018	45153.922536	58.453325
2466.060885	44904.190884	58.458330
2465.477571	44659.419253	58.463335
2464.548928	44422.185385	58.468340
2464.210410	44171.572091	58.473345
2463.284109	43931.431825	58.478349
2462.785057	43694.032274	58.483354
2461.981396	43444.363410	58.488359
2461.398074	43208.394317	58.493364
2460.743257	42965.745085	58.498369
2460.068129	42719.497455	58.503373
2459.622103	42469.289495	58.508378
2458.619253	42228.938346	58.513383
2458.042741	42000.185049	58.518388
2457.487869	41743.022821	58.523393
2456.709546	41493.156828	58.528397
2456.104806	41267.187741	58.533402
2455.245299	41015.962920	58.538407
2454.627495	40791.051961	58.543412
2454.246449	40539.310868	58.548417
2453.202039	40306.382606	58.553421
2452.662629	40052.088976	58.558426
2451.739640	39829.593021	58.563431
2450.724796	39601.281144	58.568436
2450.501155	39343.577625	58.573441
2449.530731	39127.981339	58.578445
2448.915552	38882.898587	58.583450
2448.216250	38654.655317	58.588455
2447.579078	38424.157438	58.593460
2446.980024	38182.785956	58.598465
2445.976516	37965.493026	58.603469
2445.347052	37734.589172	58.608474
2445.043347	37503.848641	58.613479
2443.998412	37284.980885	58.618484
2443.575285	37050.200066	58.623489
2442.538254	36833.752118	58.628493
2441.754146	36609.703762	58.633498
2441.454239	36381.355205	58.638503
2440.410960	36166.280873	58.643508
2439.838252	35943.804238	58.648513
2438.951759	35719.930983	58.653517
2438.288043	35494.746796	58.658522
2437.724476	35295.935534	58.663527
2437.035327	35083.676446	58.668532
2436.014234	34856.300652	58.673537
2435.308026	34649.282563	58.678541
2434.346603	34446.508157	58.683546
2433.923951	34234.822913	58.688551
2432.734135	34038.787253	58.693556
2432.080850	33837.229378	58.698561
2431.172827	33643.576345	58.703565
2430.074722	33458.603032	58.708570
2429.099976	33275.457983	58.713575
2428.274005	33106.869198	58.718580
2427.766280	32928.516385	58.723585
2426.430047	32760.079982	58.728589
2425.391958	32595.471111	58.733594
2424.743044	32432.350766	58.738599
2423.843419	32287.298401	58.743604
2423.121838	32125.565783	58.748609
2422.006027	31977.533897	58.753613
2421.396828	31816.755124	58.758618
2420.968594	31676.724580	58.763623
2419.616898	31556.202641	58.768628
2419.034327	31405.711727	58.773633
2418.307118	31275.046637	58.778637
2417.366720	31145.607757	58.783642
2417.029450	31007.742663	58.788647
2415.862427	30891.778481	58.793652
2415.336140	30764.757617	58.798657
2414.752541	30652.723802	58.803661
2414.101703	30519.478781	58.808666
2413.193674	30401.029588	58.813671
2412.446407	30285.191177	58.818676
2412.229627	30164.106137	58.823681
2411.455793	30044.167304	58.828685
2410.376373	29930.510694	58.833690
2409.906428	29815.633332	58.838695
2409.228390	29698.024902	58.843700
2408.823326	29582.318915	58.848705
2407.912490	29471.308834	58.853709
2407.437417	29351.095487	58.858714
2407.097943	29237.236344	58.863719
2405.864125	29137.650151	58.868724
2405.213352	29021.252467	58.873729
2404.753929	28911.707100	58.878733
2404.187525	28795.567810	58.883738
2403.483046	28688.707447	58.888743
2402.813137	28575.709460	58.893748
2402.602752	28458.713587	58.898753
2401.448073	28344.871461	58.903757
2400.602274	28232.241830	58.908762
2400.570811	28114.055775	58.913767
2399.929184	28000.090496	58.918772
2399.465815	27878.439135	58.923777
2398.725901	27775.332838	58.928781
2397.864877	27658.935617	58.933786
2397.156489	27542.437628	58.938791
2396.284150	27440.704330	58.943796
2396.067242	27324.242149	58.948801
2395.041230	27227.328934	58.953805
2394.647348	27113.502023	58.958810
2393.851329	26986.119831	58.963815
2393.138656	26874.275500	58.968820
2392.633293	26764.443128	58.973825
2391.966378	26650.126492	58.978829
2391.575848	26561.223182	58.983834
2390.664341	26449.552334	58.988839
2390.100242	26326.277166	58.993844
2389.735654	26210.572272	58.998849
2388.803623	26093.786927	59.003853
2387.915356	25989.414804	59.008858
2387.502334	25867.769055	59.013863
2386.616063	25766.635356	59.018868
2386.206488	25661.014293	59.023873
2385.530806	25542.544077	59.028877
2384.792200	25431.964089	59.033882
2384.214244	25326.604905	59.038887
2383.670491	25215.652765	59.043892
2383.173995	25094.323065	59.048897
2382.686759	24992.698211	59.053901
2381.494993	24870.368507	59.058906
2381.222428	24752.707341	59.063911
2380.045444	24639.235365	59.068916
2379.818937	24524.254400	59.073921
2379.217533	24418.230511	59.078925
2378.357596	24307.270848	59.083930
2378.040319	24198.648693	59.088935
2376.864255	24089.451148	59.093940
2376.451088	23959.969650	59.098945
2376.024394	23849.110318	59.103949
2374.815369	23737.413196	59.108954
2374.498484	23629.463712	59.113959
2373.365221	23511.058231	59.118964
2373.267965	23407.018992	59.123969
2372.705427	23299.623974	59.128973
2371.732982	23195.550378	59.133978
2371.358806	23086.347081	59.138983
2370.448722	22972.126903	59.143988
2370.071165	22856.810020	59.148993
2369.076010	22754.074236	59.153997
2368.317656	22632.969847	59.159002
2368.170389	22520.392816	59.164007
2367.262785	22404.325497	59.169012
2366.668097	22290.097343	59.174017
2365.803611	22188.040943	59.179021
2365.335667	22069.164115	59.184026
2364.484180	21964.914412	59.189031
2363.228219	21870.790327	59.194036
2362.921316	21767.130669	59.199041
2362.006103	21661.400786	59.204045
2361.278808	21553.889779	59.209050
2360.908913	21441.377844	59.214055
2360.101673	21357.573078	59.219060
2359.866929	21245.149282	59.224065
2358.843078	21139.799373	59.229069
2358.094509	21041.442072	59.234074
2357.398170	20938.902461	59.239079
2356.613238	20838.195055	59.244084
2356.002540	20745.184549	59.249089
2355.314962	20645.626300	59.254093
2354.641012	20561.649899	59.259098
2353.943241	20462.558266	59.264103
2353.104114	20362.808729	59.269108
2352.272638	20261.469357	59.274113
2351.909036	20166.945555	59.279117
2351.427214	20086.047098	59.284122
2350.774100	19974.280196	59.289127
2349.542271	19899.381303	59.294132
2349.246976	19798.801093	59.299137
2348.774855	19696.973392	59.304141
2347.802547	19605.468957	59.309146
2347.310467	19507.038773	59.314151
2346.514852	19418.868929	59.319156
2345.508842	19327.245947	59.324161
2345.164395	19246.199003	59.329165
2344.567041	19147.420292	59.334170
2343.970409	19050.050840	59.339175
2343.074787	18974.803486	59.344180
2342.631829	18868.795335	59.349185
2341.830523	18779.926233	59.354189
2341.250938	18712.327293	59.359194
2340.608169	18603.704526	59.364199
2339.929338	18520.376533	59.369204
2339.157734	18422.751009	59.374209
2338.517779	18342.354782	59.379213
2337.492066	18245.086035	59.384218
2337.410481	18159.210646	59.389223
2336.303573	18083.193171	59.394228
2335.843002	17992.046102	59.399233
2334.959695	17896.354273	59.404237
2334.070210	17826.891326	59.409242
2333.891752	17729.188732	59.414247
2333.258145	17647.957378	59.419252
2332.853598	17561.238606	59.424257
2331.787465	17478.452620	59.429261
2331.025262	17394.758685	59.434266
2330.665102	17303.865946	59.439271
2329.757792	17222.743176	59.444276
2329.210142	17133.693302	59.449281
2328.753600	17047.722497	59.454285
2327.715487	16962.495986	59.459290
2327.080762	16882.382571	59.464295
2326.582195	16800.779842	59.469300
2326.112899	16696.060920	59.474305
2325.167987	16615.763847	59.479309
2324.261275	16545.658207	59.484314
2324.062991	16465.533390	59.489319
2323.005923	16385.982052	59.494324
2322.223598	16299.141622	59.499329
2321.898129	16214.420306	59.504333
2321.204207	16133.508972	59.509338
2320.796071	16052.291687	59.514343
2319.782141	15966.735941	59.519348
2319.155553	15876.228901	59.524353
2318.644254	15801.479939	59.529357
2317.830115	15720.426955	59.534362
2317.565009	15631.677762	59.539367
2316.323530	15551.904559	59.544372
2315.754524	15476.572411	59.549377
2314.939868	15400.701267	59.554381
2314.151889	15320.006935	59.559386
2313.869780	15238.302782	59.564391
2313.111272	15163.537624	59.569396
2312.585037	15086.483424	59.574401
2311.789065	15012.926846	59.579405
2310.744256	14921.198011	59.584410
2310.519627	14839.198799	59.589415
2309.694108	14764.853278	59.594420
2309.014144	14701.604932	59.599425
2308.507361	14616.331040	59.604429
2307.751982	14537.498292	59.609434
2307.307073	14467.741264	59.614439
2306.269048	14387.015735	59.619444
2305.982705	14307.387477	59.624449
2304.993508	14238.851882	59.629453
2304.402203	14169.291772	59.634458
2303.746038	14082.513228	59.639463
2303.077116	14016.316399	59.644468
2302.600970	13941.473541	59.649473
2302.373537	13858.752897	59.654477
2301.328619	13789.781881	59.659482
2300.816639	13693.079333	59.664487
2299.870985	13629.173828	59.669492
2299.628604	13537.896503	59.674497
2298.738025	13465.472816	59.679501
2297.665076	13396.565634	59.684506
2296.948680	13313.701866	59.689511
2296.385313	13243.696962	59.694516
2295.483930	13171.444081	59.699521
2294.700919	13095.892352	59.704525
2294.353575	13041.312415	59.709530
2294.024528	12967.750924	59.714535
2293.194352	12888.764557	59.719540
2292.214220	12812.262059	59.724545
2291.719195	12746.110543	59.729549
2291.008537	12676.452976	59.734554
2290.501798	12590.602908	59.739559
2289.662710	12519.535980	59.744564
2289.036827	12457.532289	59.749569
2288.608213	12383.163627	59.754573
2287.853611	12308.327413	59.759578
2287.432483	12236.981284	59.764583
2286.517514	12184.784573	59.769588
2286.206429	12092.156868	59.774593
2285.651229	12023.582749	59.779597
2284.363997	11963.035880	59.784602
2284.200870	11875.948398	59.789607
2283.485990	11804.637872	59.794612
2282.258858	11730.463757	59.799617
2282.039994	11657.920467	59.804621
2281.283804	11593.040411	59.809626
2280.476310	11519.762239	59.814631
2279.781590	11450.395193	59.819636
2279.405299	11367.957199	59.824641
2278.729896	11304.909557	59.829645
2277.776047	11231.195987	59.834650
2277.131291	11169.165062	59.839655
2276.378353	11098.154073	59.844660
2275.654252	11025.275369	59.849665
2274.807101	10965.325292	59.854669
2273.986020	10907.701288	59.859674
2273.622360	10839.234127	59.864679
2272.919711	10775.071833	59.869684
2272.286182	10706.053559	59.874689
2271.929221	10639.926040	59.879693
2270.785874	10580.028815	59.884698
2270.665181	10499.209954	59.889703
2269.897338	10440.229323	59.894708
2269.104524	10376.023462	59.899713
2268.412069	10307.688579	59.904718
2267.810212	10242.520419	59.909722
2267.168387	10178.621248	59.914727
2266.548670	10117.428579	59.919732
2265.978501	10042.957392	59.924737
2265.507156	9977.909328	59.929742
2264.331142	9915.791493	59.934746
2263.749044	9850.047140	59.939751
2263.386482	9786.828427	59.944756
2262.583934	9716.212698	59.949761
2262.105406	9652.082371	59.954766
2261.098230	9581.964028	59.959770
2260.692153	9509.796855	59.964775
2259.489524	9454.367512	59.969780
2259.423478	9380.642124	59.974785
2258.893843	9319.072356	59.979790
2258.079299	9249.825977	59.984794
2257.245452	9175.508604	59.989799
2256.901575	9113.339825	59.994804
2256.331169	9044.912048	59.999809
2255.620889	8984.967106	60.004814
2254.803470	8904.505576	60.009818
2254.041190	8837.238904	60.014823
2252.998740	8775.729435	60.019828
2252.654281	8714.462151	60.024833
2251.847674	8644.482059	60.029838
2251.336018	8586.922423	60.034842
2250.666749	8511.062837	60.039847
2250.001843	8451.686756	60.044852
2249.336773	8392.565748	60.049857
2248.907015	8323.886635	60.054862
2247.977318	8255.100959	60.059866
2247.545850	8187.148515	60.064871
2246.715546	8132.529241	60.069876
2246.051823	8069.520164	60.074881
2245.357854	8001.796372	60.079886
2244.495096	7938.960623	60.084890
2243.968155	7875.900692	60.089895
2243.302774	7812.305266	60.094900
2242.633467	7747.174446	60.099905
2242.104284	7685.652358	60.104910
2241.311386	7634.314532	60.109914
2240.784691	7557.174243	60.114919
2239.916246	7490.519355	60.119924
2239.200150	7438.900239	60.124929
2238.727846	7367.972268	60.129934
2237.712218	7317.175718	60.134938
2237.594929	7239.998955	60.139943
2236.849137	7185.969260	60.144948
2236.340095	7111.438692	60.149953
2235.267687	7048.734618	60.154958
2234.545107	6994.499213	60.159962
2234.218479	6937.494012	60.164967
2233.571059	6871.720284	60.169972
2232.491812	6811.925042	60.174977
2232.195894	6744.587935	60.179982
2231.359462	6696.906082	60.184986
2230.760245	6626.131933	60.189991
2229.965892	6575.231839	60.194996
2229.677707	6505.547153	60.200001
2228.742073	6442.846035	60.205006
2228.111742	6373.685565	60.210010
2227.825332	6304.437737	60.215015
2226.909887	6257.340118	60.220020
2226.202195	6191.849516	60.225025
2225.624664	6128.188212	60.230030
2224.974381	6061.827748	60.235034
2224.319805	6003.850398	60.240039
2223.792854	5937.190132	60.245044
2222.955093	5882.866644	60.250049
2221.952462	5820.674129	60.255054
2221.122548	5751.984402	60.260058
2220.792717	5691.775885	60.265063
2220.167520	5633.613917	60.270068
2219.243242	5580.639024	60.275073
2218.922126	5505.984186	60.280078
2218.410226	5462.099911	60.285082
2217.792223	5392.431767	60.290087
2216.891001	5328.881251	60.295092
2216.571944	5264.220428	60.300097
2215.830927	5204.387510	60.305102
2214.924892	5138.167200	60.310106
2214.343197	5084.012680	60.315111
2213.577875	5027.959100	60.320116
2212.882918	4965.745050	60.325121
2212.731412	4899.906161	60.330126
2211.383245	4837.314375	60.335130
2210.803037	4774.691737	60.340135
2210.220246	4714.739490	60.345140
2209.529027	4661.861857	60.350145
2208.800571	4595.535374	60.355150
2207.701393	4550.027646	60.360154
2207.206906	4482.946858	60.365159
2207.069732	4424.102605	60.370164
2206.155242	4387.007270	60.375169
2205.931766	4309.825558	60.380174
2205.354495	4249.029670	60.385178
2204.610568	4186.842457	60.390183
2203.966478	4128.105825	60.395188
2203.306268	4071.339679	60.400193
2202.710578	3995.424514	60.405198
2201.497045	3951.704942	60.410202
2201.225687	3873.473960	60.415207
2200.372588	3816.409745	60.420212
2199.605027	3760.754889	60.425217
2198.953023	3705.938372	60.430222
2198.157687	3638.730143	60.435226
2197.867406	3576.706991	60.440231
2196.973931	3536.560852	60.445236
2196.502038	3468.996106	60.450241
2195.753597	3392.516038	60.455246
2195.161202	3341.605346	60.460250
2194.603581	3284.173002	60.465255
2193.656483	3224.253091	60.470260
2192.854258	3166.285904	60.475265
2192.371182	3103.214160	60.480270
2191.886185	3056.778520	60.485274
2191.035551	2997.943545	60.490279
2190.445866	2930.484350	60.495284
2189.548950	2883.777086	60.500289
2189.139931	2827.657259	60.505294
2188.064645	2771.772669	60.510298
2187.640768	2723.200790	60.515303
2186.821790	2652.623344	60.520308
2186.143256	2595.062271	60.525313
2185.419635	2553.423566	60.530318
2184.567705	2499.734675	60.535322
2184.391625	2430.023107	60.540327
2183.441100	2399.734414	60.545332
2182.691849	2338.320026	60.550337
2182.429510	2273.936221	60.555342
2181.293720	2221.234137	60.560346
2181.183861	2170.330626	60.565351
2180.611899	2129.729678	60.570356
2179.293891	2066.847696	60.575361
2179.047148	2017.516718	60.580366
2178.120267	1953.955746	60.585370
2177.616226	1910.259073	60.590375
2176.905400	1852.423761	60.595380
2175.697240	1809.651285	60.600385
2175.870731	1756.683255	60.605390
2174.771078	1717.298714	60.610394
2174.327471	1655.654204	60.615399
2173.891469	1601.823003	60.620404
2172.973077	1551.649984	60.625409
2172.417475	1481.949538	60.630414
2171.510255	1442.309701	60.635418
2171.337896	1382.585140	60.640423
2170.422197	1336.466960	60.645428
2169.585982	1280.322301	60.650433
2168.972752	1219.998118	60.655438
2168.430894	1180.642458	60.660442
2167.495543	1140.008095	60.665447
2166.842661	1073.045360	60.670452
2166.350779	1025.962050	60.675457
2165.666730	981.284308	60.680462
2164.772013	928.381521	60.685466
2164.175337	882.925390	60.690471
2163.185947	832.535889	60.695476
2162.493565	794.896447	60.700481
2162.440589	737.040064	60.705486
2161.261141	695.865357	60.710490
2160.547817	651.305242	60.715495
2159.906302	604.590814	60.720500
2159.345432	562.291768	60.725505
2158.964704	517.089529	60.730510
2157.603418	468.967994	60.735514
2157.374501	422.628658	60.740519
2157.092162	388.009675	60.745524
2155.581914	346.101569	60.750529
2155.344271	307.377303	60.755534
2154.388839	272.362349	60.760538
2153.773398	224.851832	60.765543
2153.300679	192.461713	60.770548
2152.636012	154.688662	60.775553
2151.888893	115.257295	60.780558
2150.980365	80.303173	60.785562
2150.178370	31.113554	60.790567
2149.582180	7.471440	60.795572
2148.411426	-12.408528	60.800577
2146.815068	-15.991819	60.805582
2141.529420	92.231906	60.810586
2141.799795	81.980257	60.815591
2142.751976	81.914312	60.820596
2142.965997	87.834624	60.825601
2143.211289	86.907894	60.830606
2142.634294	88.476941	60.835610
2142.090485	87.782631	60.840615
2141.141604	105.335603	60.845620
2140.148155	93.152512	60.850625
2139.821531	87.650528	60.855630
2139.628578	97.238584	60.860634
2138.687662	85.290005	60.865639
2137.794330	89.796509	60.870644
2136.497489	96.489515	60.875649
2136.390900	93.078256	60.880654
2135.908484	99.788701	60.885658
2135.406079	85.659108	60.890663
2134.881270	91.135271	60.895668
2133.307543	94.642756	60.900673
2133.226925	101.142805	60.905678
2132.771480	105.663416	60.910682
2132.132674	99.938158	60.915687
2132.007420	92.390548	60.920692
2130.709429	103.399664	60.925697
2130.133494	92.837600	60.930702
2129.154806	101.427582	60.935706
2127.930117	89.325341	60.940711
2127.808874	89.421813	60.945716
2127.433693	97.055065	60.950721
2126.952876	85.801434	60.955726
2126.290288	102.432238	60.960730
2125.460335	92.080781	60.965735
2124.923621	98.815611	60.970740
2123.909544	103.718155	60.975745
2123.562263	85.927665	60.980750
2123.083267	100.615006	60.985754
2122.739050	89.409084	60.990759
2121.521698	98.070046	60.995764
2120.761524	89.894656	61.000769
2120.857223	92.987473	61.005774
2119.945882	88.786154	61.010778
2118.964225	96.367403	61.015783
2118.338779	91.691812	61.020788
2117.587264	94.737708	61.025793
2117.468456	96.770204	61.030798
2116.596986	89.549142	61.035802
2115.808422	94.502633	61.040807
2115.178528	90.977295	61.045812
2114.363333	97.639621	61.050817
2113.732718	90.851832	61.055822
2112.784231	97.489577	61.060826
2112.088356	98.569738	61.065831
2111.505913	88.633161	61.070836
2110.655271	99.161315	61.075841
2110.239316	90.089259	61.080846
2109.995580	98.751859	61.085850
2109.699910	95.082033	61.090855
2108.712747	94.279887	61.095860
2107.409088	92.998126	61.100865
2107.526878	93.152863	61.105870
2106.281143	95.141824	61.110874
2106.299157	99.346052	61.115879
2105.861289	89.831217	61.120884
2104.092379	94.060360	61.125889
2103.616345	91.264362	61.130894
2103.263048	90.771633	61.135898
2102.918097	95.088642	61.140903
2102.191576	98.414415	61.145908
2100.859535	100.328767	61.150913
2100.749257	87.586119	61.155918
2100.101379	100.811683	61.160922
2099.567459	91.611696	61.165927
2098.419883	92.096511	61.170932
2097.867150	103.305920	61.175937
2097.684293	83.343217	61.180942
2096.905910	101.703309	61.185946
2095.790254	88.763809	61.190951
2095.418973	86.873666	61.195956
2095.016775	93.804763	61.200961
2093.659638	87.715704	61.205966
2093.680429	87.710798	61.210970
2092.817122	103.249137	61.215975
2091.832267	81.048372	61.220980
2091.697996	92.203991	61.225985
2090.967883	89.837799	61.230990
2089.795347	91.466662	61.235994
2089.333893	91.585580	61.240999
2088.974356	83.770817	61.246004
2088.048701	99.073052	61.251009
2087.475342	92.351876	61.256014
2086.655335	94.076184	61.261018
2086.483669	99.565705	61.266023
2086.070584	93.733687	61.271028
2084.982173	94.494535	61.276033
2084.206144	86.952428	61.281038
2083.702180	96.033192	61.286042
2083.030715	103.973648	61.291047
2082.705339	83.066937	61.296052
2081.659876	101.693325	61.301057
2081.051446	92.677046	61.306062
2080.774035	91.975170	61.311066
2079.351279	87.035039	61.316071
2078.566590	91.413940	61.321076
2078.451754	94.332012	61.326081
2077.883258	85.287326	61.331086
2076.483461	87.365398	61.336090
2076.171214	93.960539	61.341095
2076.046118	87.494653	61.346100
2074.889644	93.643463	61.351105
2074.296223	95.585698	61.356110
2073.304193	96.294989	61.361114
2072.902458	87.659061	61.366119
2072.943451	97.550598	61.371124
2072.066058	100.340526	61.376129
2071.372694	87.319841	61.381134
2070.624578	98.052496	61.386138
2069.721176	88.542160	61.391143
2069.462099	90.010315	61.396148
2068.716516	95.051611	61.401153
2067.872465	78.524213	61.406158
2066.690361	92.443218	61.411162
2065.842284	91.382486	61.416167
2066.290490	78.846108	61.421172
2065.333100	97.579938	61.426177
2064.550352	92.900939	61.431182
2063.872362	97.775400	61.436186
2062.924407	90.396193	61.441191
2062.643468	91.976623	61.446196
2061.932061	96.392784	61.451201
2061.301131	86.695720	61.456206
2060.927794	94.287683	61.461210
2060.214314	83.160876	61.466215
2059.427127	83.381948	61.471220
2058.308607	85.822229	61.476225
2057.755820	91.115193	61.481230
2056.811678	94.223209	61.486234
2056.138743	90.870289	61.491239
2056.426947	83.903604	61.496244
2055.418458	97.273120	61.501249
2054.741417	84.571538	61.506254
2054.058754	86.002836	61.511258
2053.224441	90.998293	61.516263
2052.814494	91.774487	61.521268
2052.358266	95.372756	61.526273
2051.610661	91.148634	61.531278
2050.320073	93.907946	61.536282
2049.640515	93.780797	61.541287
2049.890372	83.825704	61.546292
2048.531918	89.732197	61.551297
2047.903726	87.816602	61.556302
2047.655114	80.343775	61.561306
2046.806002	87.252756	61.566311
2046.345142	94.160052	61.571316
2045.644656	82.151291	61.576321
2045.213942	74.544947	61.581326
2043.826691	88.630544	61.586330
2042.718016	93.787809	61.591335
2042.768508	81.171045	61.596340
2041.917359	94.950813	61.601345
2041.457773	85.619209	61.606350
2040.938086	83.853546	61.611354
2040.222444	89.240162	61.616359
2039.826446	86.385747	61.621364
2039.001635	95.802846	61.626369
2038.729849	92.933449	61.631374
2037.525158	98.444983	61.636378
2036.766446	98.704119	61.641383
2036.231176	81.318793	61.646388
2035.465384	96.056374	61.651393
2035.237383	94.151387	61.656398
2034.939202	87.668821	61.661402
2033.754494	93.481520	61.666407
2032.833164	79.711749	61.671412
2031.731416	91.948099	61.676417
2031.065254	91.596489	61.681422
2030.530652	86.318333	61.686426
2030.085675	88.553971	61.691431
2029.982050	80.151434	61.696436
2029.127925	86.091435	61.701441
2028.857693	76.535835	61.706446
2028.181464	87.096240	61.711450
2027.230767	92.332513	61.716455
2026.203991	86.367678	61.721460
2025.254892	85.463334	61.726465
2024.769259	84.526439	61.731470
2024.170843	100.580964	61.736474
2023.658197	102.573466	61.741479
2023.688287	89.707634	61.746484
2022.653760	91.787687	61.751489
2021.655865	88.218279	61.756494
2020.457671	79.741880	61.761498
2019.817075	85.592806	61.766503
2020.101298	82.056462	61.771508
2018.869761	92.343893	61.776513
2018.477857	88.984231	61.781518
2017.848475	89.071468	61.786522
2017.467822	76.144683	61.791527
2016.959899	83.477317	61.796532
2015.890467	95.528782	61.801537
2014.937964	79.327689	61.806542
2014.741408	89.014073	61.811546
2013.819471	93.173510	61.816551
2013.665615	74.921885	61.821556
2012.507006	98.774663	61.826561
2011.194772	94.993381	61.831566
2010.750727	102.137701	61.836570
2010.549722	98.016070	61.841575
2010.081884	80.159606	61.846580
2009.009189	93.495166	61.851585
2008.635566	80.545189	61.856590
2008.255444	86.163977	61.861594
2007.616901	92.101310	61.866599
2006.802896	89.163436	61.871604
2005.559871	95.849532	61.876609
2005.300870	100.493515	61.881614
2004.678596	96.752542	61.886618
2003.895810	96.998162	61.891623
2003.726487	92.231292	61.896628
2002.271739	84.601401	61.901633
2001.540429	90.348463	61.906638
2000.915658	89.793182	61.911642
2000.422830	89.915518	61.916647
2000.092101	85.516450	61.921652
1999.135290	95.314034	61.926657
1998.634030	82.059477	61.931662
1998.403002	84.205974	61.936666
1997.802575	94.752781	61.941671
1997.067183	88.653408	61.946676
1995.837515	93.295331	61.951681
1995.091535	86.436008	61.956686
1994.821370	93.073357	61.961690
1993.998247	86.618921	61.966695
1993.729275	80.863400	61.971700
1992.748054	88.466689	61.976705
1991.657712	82.018397	61.981710
1991.090890	89.030817	61.986714
1990.262287	96.518430	61.991719
1990.137139	88.381071	61.996724
1989.192052	81.763077	62.001729
1988.857749	90.916263	62.006734
1988.527697	87.400140	62.011738
1988.080064	88.874574	62.016743
1987.137437	89.137684	62.021748
1985.969876	85.142655	62.026753
1985.690784	84.154065	62.031758
1985.179044	84.358249	62.036762
1983.824396	78.576355	62.041767
1983.006266	85.207634	62.046772
1982.124669	83.991409	62.051777
1982.408562	81.464317	62.056782
1981.666924	87.441668	62.061786
1981.000119	79.699351	62.066791
1980.698821	72.507702	62.071796
1979.740387	89.321066	62.076801
1978.484925	82.820143	62.081806
1978.367281	84.505542	62.086810
1977.596909	87.961299	62.091815
1977.117617	89.495950	62.096820
1976.315022	88.219882	62.101825
1975.467044	77.235880	62.106830
1974.445449	86.409842	62.111834
1973.802021	94.371090	62.116839
1973.941502	80.800392	62.121844
1972.797690	90.812154	62.126849
1972.792697	87.493589	62.131854
1972.062240	87.816064	62.136858
1970.985489	89.664729	62.141863
1969.973056	83.760719	62.146868
1969.434921	92.279239	62.151873
1968.943901	80.486411	62.156878
1968.416232	83.118363	62.161882
1967.577350	93.300916	62.166887
1967.519754	88.719736	62.171892
1966.387589	89.258929	62.176897
1965.556643	82.450949	62.181902
1964.930553	79.150545	62.186906
1964.414321	88.766246	62.191911
1963.939102	80.460542	62.196916
1963.091827	89.075434	62.201921
1961.649726	85.956583	62.206926
1961.565616	80.449257	62.211930
1960.824694	92.978424	62.216935
1960.291982	90.218259	62.221940
1959.682389	88.113662	62.226945
1959.075639	92.292471	62.231950
1958.631248	87.126165	62.236954
1958.220978	90.671420	62.241959
1957.302691	83.002140	62.246964
1955.791049	96.907258	62.251969
1955.558597	91.352514	62.256974
1955.465492	84.534653	62.261978
1954.226372	91.584406	62.266983
1954.060524	89.740523	62.271988
1953.347532	94.261033	62.276993
1952.117992	91.805428	62.281998
1951.585151	93.028477	62.287002
1951.043545	87.606380	62.292007
1950.558010	90.017194	62.297012
1949.903692	97.204353	62.302017
1949.836796	94.272486	62.307022
1948.486981	86.036220	62.312026
1947.358727	85.237608	62.317031
1946.939484	88.727522	62.322036
1946.529085	96.878859	62.327041
1945.929865	86.618587	62.332046
1945.718092	84.629037	62.337050
1944.694495	95.290325	62.342055
1944.028691	78.823002	62.347060
1943.114884	90.036112	62.352065
1942.593560	91.916469	62.357070
1942.359881	83.274400	62.362074
1940.792958	88.395632	62.367079
1940.611595	90.157376	62.372084
1939.720356	87.756885	62.377089
1939.266205	90.621589	62.382094
1938.541606	80.461647	62.387098
1938.336996	89.430252	62.392103
1937.853805	87.110065	62.397108
1936.704229	87.611034	62.402113
1935.547981	87.651039	62.407118
1935.015121	92.108268	62.412122
1934.303750	94.939690	62.417127
1934.356081	86.337373	62.422132
1933.791438	87.901348	62.427137
1932.814318	84.932624	62.432142
1931.899411	94.184281	62.437146
1931.495212	93.628697	62.442151
1930.844924	83.010703	62.447156
1930.551715	83.028830	62.452161
1929.290052	89.072969	62.457166
1928.560718	83.674371	62.462170
1928.003774	84.814522	62.467175
1927.790551	93.778189	62.472180
1926.773198	80.853149	62.477185
1925.722088	86.086467	62.482190
1924.993965	93.200192	62.487194
1924.315831	81.236816	62.492199
1924.050714	78.558758	62.497204
1923.625509	78.110583	62.502209
1922.838151	89.693114	62.507214
1922.909739	81.794185	62.512218
1921.698643	87.904414	62.517223
1921.046457	81.476487	62.522228
1920.223542	73.489329	62.527233
1919.337385	89.110151	62.532238
1918.790502	93.738335	62.537242
1917.466256	92.658625	62.542247
1916.794001	83.671461	62.547252
1916.285390	89.471495	62.552257
1916.536085	88.485543	62.557262
1916.063731	85.424086	62.562266
1915.183181	85.115999	62.567271
1914.719018	80.233528	62.572276
1913.512902	82.016021	62.577281
1912.995986	89.834198	62.582286
1912.554427	86.200178	62.587290
1911.406421	80.898007	62.592295
1910.380203	83.449843	62.597300
1909.592509	88.803771	62.602305
1908.917645	94.411014	62.607310
1909.147251	76.800254	62.612314
1908.443896	80.131852	62.617319
1908.135435	71.578935	62.622324
1907.547432	86.281992	62.627329
1906.586757	88.552204	62.632334
1905.716120	77.672749	62.637338
1904.963896	75.390547	62.642343
1904.615348	72.181715	62.647348
1903.205566	75.153968	62.652353
1902.350528	86.114917	62.657358
1902.067987	84.997580	62.662362
1901.534388	95.745091	62.667367
1900.980391	73.282105	62.672372
1900.678731	78.727603	62.677377
1900.049260	85.341568	62.682382
1899.225001	70.861060	62.687386
1898.438268	69.249780	62.692391
1898.191722	76.479434	62.697396
1897.604185	78.088048	62.702401
1895.954581	84.110208	62.707406
1895.612140	79.153229	62.712410
1894.766385	82.964730	62.717415
1894.603728	75.768433	62.722420
1893.830383	83.168445	62.727425
1892.954700	78.185735	62.732430
1892.331960	72.163136	62.737434
1891.546549	84.790826	62.742439
1891.295525	80.771768	62.747444
1890.691497	86.869212	62.752449
1889.860381	80.370358	62.757454
1889.203141	78.711716	62.762458
1888.161703	88.383992	62.767463
1887.745674	79.797690	62.772468
1887.124331	79.784338	62.777473
1887.013324	75.884973	62.782478
1886.034097	88.423593	62.787482
1885.119522	74.596060	62.792487
1884.597599	76.460752	62.797492
1883.981378	86.136485	62.802497
1883.456746	85.265729	62.807502
1882.292596	88.597951	62.812506
1881.134954	93.911274	62.817511
1880.983266	83.811781	62.822516
1880.327950	78.678981	62.827521
1879.810472	83.171619	62.832526
1879.757391	84.878310	62.837530
1878.912308	87.191679	62.842535
1878.341442	83.578193	62.847540
1877.393017	76.300070	62.852545
1876.824715	82.505378	62.857550
1875.782201	83.363097	62.862554
1874.679358	91.618056	62.867559
1874.558724	83.025859	62.872564
1873.806683	87.563621	62.877569
1873.408238	79.785045	62.882574
1873.450841	77.179562	62.887578
1871.928113	82.460961	62.892583
1871.202070	91.195394	62.897588
1870.816713	81.024196	62.902593
1870.457162	89.635793	62.907598
1869.705524	75.547446	62.912602
1868.196497	83.781735	62.917607
1867.495773	77.210154	62.922612
1867.251035	87.380397	62.927617
1866.768908	85.061633	62.932622
1866.408769	72.174215	62.937626
1865.274361	83.554817	62.942631
1864.604757	82.131521	62.947636
1863.755984	82.704610	62.952641
1863.433474	75.049595	62.957646
1863.041151	76.087933	62.962650
1861.763184	82.224568	62.967655
1861.291780	80.490701	62.972660
1860.508908	85.794991	62.977665
1860.221281	90.020920	62.982670
1859.957955	73.609585	62.987674
1858.815187	90.266164	62.992679
1857.731995	89.482514	62.997684
1857.158515	81.247629	63.002689
1856.472867	71.830555	63.007694
1856.216616	78.315890	63.012698
1855.789113	84.768494	63.017703
1855.254837	82.487973	63.022708
1854.367758	84.555717	63.027713
1853.365127	91.821841	63.032718
1853.048137	76.462916	63.037722
1851.973160	78.855365	63.042727
1851.172803	78.993439	63.047732
1850.672181	84.866324	63.052737
1849.525072	79.587695	63.057742
1849.503535	73.341932	63.062746
1848.861788	75.250884	63.067751
1848.714965	74.637106	63.072756
1848.244405	84.135183	63.077761
1847.043532	89.408074	63.082766
1846.501148	78.304652	63.087770
1845.833689	82.477348	63.092775
1844.715662	83.597791	63.097780
1844.187635	89.336265	63.102785
1843.559570	78.640666	63.107790
1843.479737	75.474332	63.112794
1842.060597	83.588712	63.117799
1841.204854	82.481967	63.122804
1840.570267	76.087542	63.127809
1840.120913	85.851899	63.132814
1840.099065	74.479767	63.137818
1839.269940	87.817695	63.142823
1838.231642	77.106809	63.147828
1837.342783	86.387463	63.152833
1837.031307	78.286021	63.157838
1836.795089	66.291951	63.162842
1835.849800	79.575779	63.167847
1835.096782	69.724733	63.172852
1834.169514	81.231719	63.177857
1833.600320	80.959377	63.182862
1833.404511	77.437738	63.187866
1832.167886	82.937072	63.192871
1831.295123	80.954713	63.197876
1830.782378	75.435035	63.202881
1830.194226	80.886602	63.207886
1830.142826	75.717855	63.212890
1829.417905	83.073925	63.217895
1828.445765	76.761481	63.222900
1827.859573	88.591195	63.227905
1827.242903	86.872513	63.232910
1826.657228	78.016711	63.237914
1825.518586	85.712845	63.242919
1824.671999	80.840653	63.247924
1824.194370	82.502791	63.252929
1823.740213	85.310745	63.257934
1823.609152	77.032435	63.262938
1822.812340	78.885593	63.267943
1821.942334	81.523040	63.272948
1821.223189	64.636923	63.277953
1820.303609	80.185791	63.282958
1820.066518	72.668604	63.287962
1818.893499	75.917106	63.292967
1817.923353	75.404092	63.297972
1817.656358	87.072743	63.302977
1817.208071	77.908139	63.307982
1817.084554	69.407875	63.312986
1816.186433	73.013255	63.317991
1815.142099	79.171157	63.322996
1814.341382	78.926119	63.328001
1813.887317	76.665987	63.333006
1813.321218	60.630742	63.338010
1812.269177	77.875279	63.343015
1811.546702	72.332140	63.348020
1810.933123	62.927299	63.353025
1810.384207	72.510348	63.358030
1810.143535	77.911476	63.363034
1809.575592	80.243935	63.368039
1808.987321	69.833758	63.373044
1808.072480	78.943506	63.378049
1807.340459	81.052873	63.383054
1807.018498	64.054815	63.388058
1805.713705	74.276674	63.393063
1804.986661	75.705618	63.398068
1804.650979	80.128402	63.403073
1804.048347	81.554938	63.408078
1803.758772	78.951738	63.413082
1802.498334	86.086931	63.418087
1801.900814	76.050362	63.423092
1801.387194	77.617298	63.428097
1800.478821	84.466366	63.433102
1800.306795	75.459742	63.438106
1798.995775	82.766960	63.443111
1798.092012	78.299653	63.448116
1797.787055	80.981422	63.453121
1797.224192	83.779833	63.458126
1797.115272	78.071469	63.463130
1796.652141	76.569679	63.468135
1795.791406	84.065586	63.473140
1794.768638	76.435046	63.478145
1794.212248	78.153847	63.483150
1793.485663	76.488896	63.488154
1793.065689	80.527694	63.493159
1792.262786	91.869878	63.498164
1791.634300	89.008271	63.503169
1790.528249	80.094765	63.508174
1789.921191	84.587449	63.513178
1789.227613	92.037896	63.518183
1788.732126	74.908121	63.523188
1788.498854	77.860768	63.528193
1787.383469	81.883838	63.533198
1786.727999	81.374483	63.538202
1785.852591	75.737370	63.543207
1785.356424	81.428214	63.548212
1785.183038	80.731930	63.553217
1784.324280	91.556309	63.558222
1783.141388	80.355925	63.563226
1782.467083	76.071375	63.568231
1781.991056	83.607117	63.573236
1781.765756	76.985304	63.578241
1781.264864	87.368098	63.583246
1780.433847	84.185435	63.588250
1779.809014	79.599731	63.593255
1779.114554	84.107872	63.598260
1778.238074	86.386834	63.603265
1777.081307	82.328697	63.608270
1776.565638	74.075199	63.613274
1775.709854	90.424469	63.618279
1775.264706	78.575537	63.623284
1775.039212	71.018672	63.628289
1774.449267	83.889718	63.633294
1774.119228	72.407271	63.638298
1772.831078	85.855942	63.643303
1772.033977	79.873677	63.648308
1772.108223	82.143592	63.653313
1771.026904	81.392795	63.658318
1770.218268	87.305141	63.663322
1769.697052	83.764220	63.668327
1769.052688	89.563754	63.673332
1769.227677	86.588759	63.678337
1767.781621	94.317965	63.683342
1767.093710	85.260802	63.688346
1766.568388	87.335781	63.693351
1765.352772	81.787387	63.698356
1764.751119	78.875799	63.703361
1764.002880	84.751748	63.708366
1763.516388	82.118325	63.713370
1762.845074	84.637511	63.718375
1762.665714	93.034430	63.723380
1762.358317	82.737345	63.728385
1760.966174	84.134728	63.733390
1760.327594	80.609294	63.738394
1759.915064	84.088701	63.743399
1758.712613	84.178696	63.748404
1758.125882	79.843977	63.753409
1757.292556	85.342375	63.758414
1757.103364	85.016014	63.763418
1756.571109	80.239005	63.768423
1756.233818	82.919605	63.773428
1755.779635	76.769358	63.778433
1754.718575	74.118375	63.783438
1753.964531	78.921396	63.788442
1752.417939	90.589831	63.793447
1751.967007	84.506871	63.798452
1751.451263	78.374285	63.803457
1750.778723	86.568834	63.808462
1750.683661	73.601507	63.813466
1750.393343	80.995803	63.818471
1749.569088	86.500647	63.823476
1748.472382	79.476350	63.828481
1747.705135	83.191851	63.833486
1747.479187	78.878687	63.838490
1747.064694	84.146581	63.843495
1745.868387	88.150981	63.848500
1745.015681	77.729199	63.853505
1744.246386	80.844238	63.858510
1744.173367	76.768550	63.863514
1743.191452	74.965975	63.868519
1742.494137	73.499808	63.873524
1742.276377	82.910440	63.878529
1741.554605	81.199010	63.883534
1740.407735	78.146942	63.888538
1739.703431	81.696339	63.893543
1739.466501	80.984919	63.898548
1739.181839	73.003815	63.903553
1738.057998	84.832187	63.908558
1737.401510	67.559282	63.913562
1736.462842	83.622107	63.918567
1736.133667	75.942946	63.923572
1735.733095	79.442532	63.928577
1734.186444	82.174847	63.933582
1733.797542	68.002156	63.938586
1732.956947	79.757160	63.943591
1732.266380	78.714103	63.948596
1732.430056	71.049713	63.953601
1731.545266	86.979412	63.958606
1730.616354	77.749240	63.963610
1730.298528	78.387855	63.968615
1729.671856	73.195364	63.973620
1728.627601	78.334622	63.978625
1727.662638	81.476009	63.983630
1727.291493	75.244777	63.988634
1726.648832	75.025125	63.993639
1726.050914	80.382070	63.998644
1725.771035	72.658817	64.003649
1724.445453	81.313449	64.008654
1723.923302	70.120133	64.013658
1723.946818	75.228584	64.018663
1722.694621	72.196406	64.023668
1722.185982	71.004617	64.028673
1721.190544	80.598672	64.033678
1720.723435	73.067572	64.038682
1720.788697	74.608818	64.043687
1719.407014	71.970924	64.048692
1718.808570	73.198127	64.053697
1718.112923	89.282287	64.058702
1717.727971	76.654300	64.063706
1716.519582	73.851698	64.068711
1715.868018	67.302327	64.073716
1715.312488	73.160292	64.078721
1714.570713	78.962686	64.083726
1714.248429	65.272985	64.088730
1713.926256	71.931207	64.093735
1712.714696	78.957750	64.098740
1712.222304	74.341572	64.103745
1711.422494	72.983150	64.108750
1710.878706	69.158841	64.113754
1710.627072	64.067637	64.118759
1709.446992	77.524389	64.123764
1708.591652	73.295420	64.128769
1708.055827	68.612030	64.133774
1707.544444	65.441709	64.138778
1707.195579	80.860537	64.143783
1705.994712	78.610227	64.148788
1705.646616	70.490980	64.153793
1705.014466	78.117751	64.158798
1704.576834	70.764892	64.163802
1703.558381	69.415967	64.168807
1702.682677	75.580237	64.173812
1702.492795	79.517851	64.178817
1701.737716	77.608307	64.183822
1701.130112	71.692166	64.188826
1699.786775	73.408240	64.193831
1699.575957	73.019090	64.198836
1699.480973	68.693020	64.203841
1698.862385	75.082947	64.208846
1697.512895	74.966099	64.213850
1696.446174	80.315508	64.218855
1695.965899	71.723694	64.223860
1695.889219	75.099307	64.228865
1695.289078	82.156478	64.233870
1694.636223	68.388401	64.238874
1693.722928	72.540249	64.243879
1692.953623	76.093671	64.248884
1692.815034	62.630257	64.253889
1691.535227	86.932805	64.258894
1691.043588	83.775116	64.263898
1690.368271	73.612179	64.268903
1689.867034	81.273352	64.273908
1689.555520	75.595601	64.278913
1688.050753	79.656898	64.283918
1687.420378	70.415603	64.288922
1686.951218	71.757890	64.293927
1686.217468	68.734848	64.298932
1686.363615	66.417259	64.303937
1684.683645	79.907686	64.308942
1684.089220	73.404437	64.313946
1683.599509	76.066676	64.318951
1683.117423	73.393150	64.323956
1683.070981	71.364756	64.328961
1681.811779	84.469832	64.333966
1681.088767	73.920255	64.338970
1680.897123	77.463930	64.343975
1680.093114	81.495930	64.348980
1679.315025	71.745116	64.353985
1678.420300	85.825155	64.358990
1678.021497	75.705031	64.363994
1677.225869	77.007713	64.368999
1676.165987	75.334237	64.374004
1675.659461	70.575242	64.379009
1674.921473	85.250097	64.384014
1674.808604	78.214647	64.389018
1674.353026	74.579752	64.394023
1673.206385	74.496927	64.399028
1672.511874	68.687635	64.404033
1671.550829	72.689387	64.409038
1671.390976	69.724999	64.414042
1670.979815	73.387114	64.419047
1669.981147	73.504704	64.424052
1669.362674	71.213947	64.429057
1668.901821	73.734417	64.434062
1668.071793	70.680943	64.439066
1667.054160	64.139271	64.444071
1666.044543	74.052540	64.449076
1665.954543	75.260495	64.454081
1665.604883	72.769356	64.459086
1664.901829	68.774823	64.464090
1663.809172	67.805112	64.469095
1663.190566	75.700959	64.474100
1662.899321	72.962434	64.479105
1662.129170	73.701286	64.484110
1661.400615	71.082681	64.489114
1660.702854	75.258650	64.494119
1660.059919	75.292934	64.499124
1659.804384	73.766082	64.504129
1658.377697	82.428917	64.509134
1657.893169	73.645410	64.514138
1657.395481	70.509192	64.519143
1656.650039	77.978933	64.524148
1656.177628	76.945398	64.529153
1655.283998	82.130140	64.534158
1654.413728	74.300413	64.539162
1654.012528	72.888157	64.544167
1653.451286	70.369130	64.549172
1653.073223	67.461481	64.554177
1651.639584	70.604797	64.559182
1651.158035	66.042105	64.564186
1650.772060	72.647390	64.569191
1650.477597	63.636593	64.574196
1649.948733	69.250647	64.579201
1648.515957	69.892913	64.584206
1648.157591	66.988444	64.589210
1647.698223	62.392269	64.594215
1647.052035	70.552680	64.599220
1646.469693	63.382089	64.604225
1645.491322	73.400780	64.609230
1645.000040	73.674316	64.614234
1644.258401	64.296180	64.619239
1643.176691	62.518960	64.624244
1642.941036	64.470679	64.629249
1642.019742	65.717642	64.634254
1642.094376	65.429804	64.639258
1640.663186	75.594538	64.644263
1639.521473	67.219765	64.649268
1639.339191	59.769600	64.654273
1639.047620	69.404822	64.659278
1638.708434	62.331221	64.664282
1637.722378	67.920131	64.669287
1636.758636	73.261085	64.674292
1636.313390	70.936514	64.679297
1635.663552	78.491992	64.684302
1635.095669	68.127520	64.689306
1634.030246	79.058862	64.694311
1633.296758	74.195586	64.699316
1633.349432	72.999805	64.704321
1632.635926	75.145696	64.709326
1631.442319	70.316088	64.714330
1630.669947	60.392515	64.719335
1629.985232	72.990050	64.724340
1629.929737	67.307913	64.729345
1629.222769	63.922686	64.734350
1628.267392	68.483339	64.739354
1627.551781	68.265838	64.744359
1627.160446	76.253315	64.749364
1626.421363	65.632206	64.754369
1625.432682	62.280692	64.759374
1624.753340	65.532849	64.764378
1624.496458	68.629595	64.769383
1623.745099	74.143387	64.774388
1623.213362	65.001560	64.779393
1622.545322	71.648499	64.784398
1621.684059	69.741657	64.789402
1621.228139	64.402235	64.794407
1620.581607	66.431839	64.799412
1619.679156	66.685543	64.804417
1618.931984	64.032066	64.809422
1618.284998	69.250171	64.814426
1617.817365	68.007738	64.819431
1617.093532	72.250932	64.824436
1616.302468	64.675135	64.829441
1615.326346	65.389951	64.834446
1615.011722	66.540553	64.839450
1614.737351	59.508699	64.844455
1614.169507	65.367055	64.849460
1613.465605	54.350884	64.854465
1612.788071	64.269752	64.859470
1611.998753	63.404833	64.864474
1610.970921	61.753102	64.869479
1610.249902	74.832622	64.874484
1609.996443	58.493920	64.879489
1609.116300	72.264154	64.884494
1608.748815	70.285185	64.889498
1607.721967	59.722415	64.894503
1606.844510	67.580542	64.899508
1606.734214	63.567557	64.904513
1606.053726	63.722931	64.909518
1605.233528	53.794355	64.914522
1604.197644	59.447955	64.919527
1603.444808	75.440275	64.924532
1603.166928	67.548006	64.929537
1602.584673	66.736925	64.934542
1602.255739	60.415446	64.939546
1601.499230	61.489597	64.944551
1600.465656	73.622188	64.949556
1600.175213	66.760035	64.954561
1599.437771	72.504996	64.959566
1598.781625	71.240477	64.964570
1598.484548	64.496067	64.969575
1597.759688	75.415890	64.974580
1596.526509	63.908242	64.979585
1595.784805	70.549542	64.984590
1595.115038	67.585746	64.989594
1594.754808	68.956473	64.994599
1593.494461	71.323278	64.999604
1592.935529	58.216807	65.004609
1592.310262	66.736581	65.009614
1592.169536	61.017529	65.014618
1591.723382	64.631597	65.019623
1590.731693	72.419573	65.024628
1590.097822	69.144164	65.029633
1589.217105	70.307433	65.034638
1588.653036	70.600427	65.039642
1588.737469	70.951239	65.044647
1587.107672	76.021149	65.049652
1586.544378	77.638591	65.054657
1586.033738	70.909184	65.059662
1585.518635	58.522690	65.064666
1584.385399	70.906069	65.069671
1583.638262	71.589250	65.074676
1583.617011	57.530088	65.079681
1582.962994	64.953776	65.084686
1582.336374	73.104782	65.089690
1581.799062	68.303395	65.094695
1580.903257	69.424911	65.099700
1580.339340	69.538120	65.104705
1579.476585	64.074116	65.109710
1578.566183	66.218185	65.114714
1577.931109	61.121690	65.119719
1577.283432	73.263940	65.124724
1576.900900	63.155458	65.129729
1576.652845	66.673405	65.134734
1575.457640	62.504791	65.139738
1574.940550	58.778774	65.144743
1574.285020	67.934105	65.149748
1573.802684	75.526057	65.154753
1572.656437	72.365166	65.159758
1571.674530	81.063028	65.164762
1571.497864	68.966520	65.169767
1570.706428	77.873805	65.174772
1570.572659	66.617262	65.179777
1569.452374	65.770246	65.184782
1568.626744	76.198332	65.189786
1568.414856	74.002272	65.194791
1567.651109	73.276799	65.199796
1566.842745	68.740817	65.204801
1566.137577	75.532430	65.209806
1565.629187	71.718302	65.214810
1565.340551	60.364951	65.219815
1564.039123	82.526416	65.224820
1563.372075	63.873933	65.229825
1562.767134	75.951054	65.234830
1562.343756	67.552080	65.239834
1561.788308	67.990359	65.244839
1560.887759	87.670806	65.249844
1560.282538	75.347506	65.254849
1559.482934	79.337839	65.259854
1559.314045	68.523670	65.264858
1558.750116	68.166978	65.269863
1557.388134	77.220101	65.274868
1556.884280	63.475717	65.279873
1556.161888	79.672934	65.284878
1555.801622	70.693107	65.289882
1555.462762	68.402109	65.294887
1553.959512	70.476381	65.299892
1553.799067	62.404627	65.304897
1553.232281	71.998425	65.309902
1552.492735	65.780035	65.314906
1551.627955	62.402560	65.319911
1550.726093	71.130280	65.324916
1550.484501	68.651952	65.329921
1549.998603	74.312808	65.334926
1548.869840	73.520761	65.339930
1548.218186	72.638721	65.344935
1547.522314	74.181045	65.349940
1547.306667	62.204275	65.354945
1546.654640	74.318837	65.359950
1545.556961	69.936055	65.364954
1545.143922	67.065520	65.369959
1544.321997	75.821542	65.374964
1544.189168	68.768785	65.379969
1543.163699	71.120373	65.384974
1542.260293	73.577140	65.389978
1541.894024	69.399835	65.394983
1541.285393	72.926191	65.399988
1540.947394	61.932328	65.404993
1539.818884	70.182002	65.409998
1538.992147	80.689117	65.415002
1538.894347	69.620818	65.420007
1537.433942	69.759783	65.425012
1536.568070	79.976664	65.430017
1536.147798	77.548801	65.435022
1535.434010	72.177831	65.440026
1535.294027	66.042373	65.445031
1534.743647	76.969177	65.450036
1534.514894	80.536099	65.455041
1533.680819	75.509075	65.460046
1532.725902	74.148548	65.465050
1532.224837	67.491750	65.470055
1530.925789	70.364599	65.475060
1530.438707	55.570528	65.480065
1529.905620	71.989960	65.485070
1529.358090	68.074833	65.490074
1528.203604	73.603814	65.495079
1527.504900	81.449335	65.500084
1527.027356	63.397508	65.505089
1526.691722	63.154354	65.510094
1526.161058	72.819683	65.515098
1525.982122	66.116436	65.520103
1525.022588	74.935325	65.525108
1524.208083	73.248156	65.530113
1523.328798	61.692209	65.535118
1522.187630	71.329966	65.540122
1521.757568	63.936532	65.545127
1521.155261	77.878673	65.550132
1520.840895	67.783025	65.555137
1520.449326	77.191304	65.560142
1519.432739	75.662394	65.565146
1518.851162	66.902235	65.570151
1518.071829	85.235703	65.575156
1517.191718	75.611543	65.580161
1516.434912	77.830572	65.585166
1515.995524	90.179432	65.590170
1515.948370	70.692070	65.595175
1514.841638	75.426612	65.600180
1513.980115	67.467832	65.605185
1513.336016	69.664221	65.610190
1512.437708	82.691511	65.615194
1512.447721	72.191102	65.620199
1511.517606	78.789824	65.625204
1510.518899	80.686189	65.630209
1510.137283	78.162306	65.635214
1509.811509	81.664226	65.640218
1509.254376	68.830289	65.645223
1508.115930	72.655288	65.650228
1507.454529	72.552203	65.655233
1507.129437	71.927351	65.660238
1506.167403	74.797124	65.665242
1505.666705	71.454848	65.670247
1505.006881	81.394583	65.675252
1504.227829	69.001164	65.680257
1502.924334	67.211938	65.685262
1502.398958	74.585244	65.690266
1501.954296	68.299516	65.695271
1501.635235	67.246375	65.700276
1501.249822	72.375635	65.705281
1500.450672	74.945153	65.710286
1499.407628	81.445136	65.715290
1499.177816	64.356843	65.720295
1498.319717	79.911768	65.725300
1497.507022	64.544998	65.730305
1496.427689	70.196082	65.735310
1496.163080	77.285117	65.740314
1495.742521	58.096793	65.745319
1495.250632	78.708880	65.750324
1494.084539	71.834504	65.755329
1493.436605	73.153193	65.760334
1492.919968	72.926189	65.765338
1492.730199	57.253878	65.770343
1491.207951	78.583168	65.775348
1490.680921	69.287675	65.780353
1490.189195	74.159455	65.785358
1489.648303	68.494538	65.790362
1489.369839	74.869876	65.795367
1488.088087	75.106630	65.800372
1487.321228	72.934112	65.805377
1486.889808	80.795513	65.810382
1486.151634	80.479140	65.815386
1486.297708	63.063056	65.820391
1485.099990	77.530295	65.825396
1483.986873	79.274547	65.830401
1483.580782	71.118836	65.835406
1483.204864	67.521786	65.840410
1482.829759	63.314360	65.845415
1481.867226	78.985225	65.850420
1481.251352	65.949334	65.855425
1480.445041	73.958608	65.860430
1479.081269	73.840989	65.865434
1478.476885	65.757791	65.870439
1478.225427	70.350131	65.875444
1477.616099	69.142856	65.880449
1477.512117	68.132808	65.885454
1476.885937	75.706629	65.890458
1476.123162	57.510929	65.895463
1475.284619	78.402015	65.900468
1474.576194	71.585803	65.905473
1473.962166	75.661780	65.910478
1472.690451	77.661461	65.915482
1472.530560	75.722062	65.920487
1471.918773	80.141441	65.925492
1471.459860	68.909775	65.930497
1470.349290	75.027856	65.935502
1469.253299	90.098656	65.940506
1469.371670	73.052798	65.945511
1468.722452	78.351710	65.950516
1467.833964	75.689197	65.955521
1467.127431	74.129961	65.960526
1466.316617	75.430388	65.965530
1466.179581	59.973615	65.970535
1465.211401	75.065090	65.975540
1464.349553	74.271663	65.980545
1464.124247	75.892187	65.985550
1463.512165	78.331069	65.990554
1462.739118	78.293043	65.995559
1461.701942	75.706197	66.000564
1461.496059	71.484497	66.005569
1460.851793	67.474380	66.010574
1459.360480	72.861381	66.015578
1459.161088	66.878868	66.020583
1458.706033	69.724858	66.025588
1458.377149	66.949770	66.030593
1457.245913	71.648805	66.035598
1456.089727	81.894494	66.040602
1456.079479	64.858049	66.045607
1455.697670	73.402232	66.050612
1454.789283	76.815400	66.055617
1453.848456	74.780919	66.060622
1453.141385	65.457284	66.065626
1452.977854	61.621497	66.070631
1452.012958	66.910653	66.075636
1450.831422	77.158793	66.080641
1450.272594	74.081220	66.085646
1449.593584	63.843276	66.090650
1449.545688	54.829613	66.095655
1449.000059	64.028993	66.100660
1448.542256	68.605242	66.105665
1447.960046	65.600770	66.110670
1446.811662	59.799032	66.115674
1445.875727	65.326424	66.120679
1445.038590	75.051504	66.125684
1444.464950	65.288799	66.130689
1444.211510	60.565334	66.135694
1443.740480	65.351832	66.140698
1442.921903	68.693963	66.145703
1442.012756	67.799257	66.150708
1441.423141	73.572798	66.155713
1441.098431	60.192629	66.160718
1439.820204	74.994354	66.165722
1439.219529	60.932682	66.170727
1438.785682	64.628388	66.175732
1438.403939	66.317925	66.180737
1437.651411	63.321600	66.185742
1436.337675	62.481733	66.190746
1435.995027	66.371092	66.195751
1435.463752	71.274394	66.200756
1435.129355	62.665783	66.205761
1434.124650	65.171796	66.210766
1433.096320	68.739642	66.215770
1432.930963	60.881564	66.220775
1432.328340	69.670561	66.225780
1431.984524	65.417173	66.230785
1430.825521	66.599490	66.235790
1430.023501	68.545044	66.240794
1429.792342	62.364170	66.245799
1428.925301	69.151573	66.250804
1427.431803	68.439621	66.255809
1427.278013	59.198372	66.260814
1426.599648	64.905597	66.265818
1426.604596	52.770807	66.270823
1426.173346	60.036121	66.275828
1424.905166	62.923036	66.280833
1424.479270	68.287380	66.285838
1423.805522	70.742378	66.290842
1422.957685	54.693726	66.295847
1421.788565	58.288679	66.300852
1421.348361	62.392227	66.305857
1420.811472	63.477255	66.310862
1420.216968	68.108347	66.315866
1420.285371	59.090393	66.320871
1419.082862	64.920341	66.325876
1418.307972	61.224295	66.330881
1417.895754	58.922903	66.335886
1416.594714	62.702819	66.340890
1415.817831	63.288278	66.345895
1415.335749	61.390629	66.350900
1415.035633	62.952085	66.355905
1414.863029	61.765300	66.360910
1414.100451	63.023384	66.365914
1413.500832	65.521792	66.370919
1412.802889	68.735956	66.375924
1411.773295	58.328257	66.380929
1410.937059	65.757281	66.385934
1410.258777	73.940177	66.390938
1410.078857	60.275245	66.395943
1408.965978	65.047068	66.400948
1408.190455	58.673611	66.405953
1407.680406	57.628762	66.410958
1407.046518	65.568069	66.415962
1406.781331	58.276188	66.420967
1405.485753	60.762212	66.425972
1404.386121	62.266245	66.430977
1404.476178	61.370434	66.435982
1403.750948	63.194987	66.440986
1403.589519	64.947279	66.445991
1402.355291	63.227517	66.450996
1401.696470	71.140830	66.456001
1401.371303	56.117655	66.461006
1400.656158	68.119265	66.466010
1399.866030	57.892698	66.471015
1398.809909	76.658066	66.476020
1398.480891	73.061460	66.481025
1398.209493	55.356953	66.486030
1396.922070	59.252978	66.491034
1396.228800	59.855114	66.496039
1395.393743	63.777008	66.501044
1395.048109	60.558341	66.506049
1395.034693	61.361489	66.511054
1393.916508	70.013250	66.516058
1393.131664	63.004224	66.521063
1392.578387	71.096294	66.526068
1391.939807	70.740467	66.531073
1391.775397	66.486956	66.536078
1390.475431	67.768960	66.541082
1389.933945	72.897807	66.546087
1389.477488	61.462366	66.551092
1388.707148	62.286476	66.556097
1387.587635	68.065402	66.561102
1386.967149	72.582367	66.566106
1386.868124	60.443603	66.571111
1386.261049	70.695067	66.576116
1385.053640	65.166077	66.581121
1384.495074	64.573619	66.586126
1383.944034	77.391202	66.591130
1383.654599	57.289575	66.596135
1382.705401	69.288968	66.601140
1381.495425	75.760329	66.606145
1381.644467	68.577642	66.611150
1380.796404	74.352850	66.616154
1379.977857	63.943156	66.621159
1379.212789	67.404526	66.626164
1378.531616	72.137707	66.631169
1378.432473	55.845505	66.636174
1377.466909	76.570716	66.641178
1376.769391	65.149938	66.646183
1376.163229	74.705865	66.651188
1375.343130	69.170508	66.656193
1374.685486	54.406756	66.661198
1373.284264	65.468803	66.666202
1372.851793	66.149334	66.671207
1372.614384	71.445882	66.676212
1372.443294	68.666225	66.681217
1372.262169	59.383601	66.686222
1370.879579	66.439032	66.691226
1370.212000	68.621840	66.696231
1369.777544	67.363144	66.701236
1368.474056	73.053057	66.706241
1368.140999	53.360475	66.711246
1367.330201	64.193066	66.716250
1367.205214	59.165361	66.721255
1366.053869	71.266272	66.726260
1364.891788	63.060457	66.731265
1364.707580	60.945171	66.736270
1364.176846	65.438410	66.741274
1364.004189	56.365743	66.746279
1363.024268	64.886730	66.751284
1362.006048	75.635613	66.756289
1361.796698	66.352742	66.761294
1360.616921	71.370172	66.766298
1359.716885	72.990724	66.771303
1359.296838	62.971835	66.776308
1358.819926	72.762670	66.781313
1358.459642	56.532480	66.786318
1358.147312	68.104236	66.791322
1357.202135	56.290778	66.796327
1356.226922	67.673027	66.801332
1355.561085	70.423233	66.806337
1354.665462	64.166649	66.811342
1353.598635	73.623923	66.816346
1353.260294	61.993109	66.821351
1352.999916	65.557179	66.826356
1352.753154	65.853401	66.831361
1351.913755	66.207555	66.836366
1351.023406	59.437656	66.841370
1350.450510	58.442230	66.846375
1349.826969	70.938616	66.851380
1348.612385	73.662516	66.856385
1348.453335	56.405340	66.861390
1347.475104	65.011213	66.866394
1347.135484	58.442341	66.871399
1346.668613	72.303041	66.876404
1345.168406	73.796660	66.881409
1344.836856	68.029125	66.886414
1344.456549	68.553144	66.891418
1343.885801	61.245193	66.896423
1342.778657	73.009522	66.901428
1342.012916	73.459199	66.906433
1341.712698	67.973673	66.911438
1341.105372	67.120909	66.916442
1340.937764	63.465544	66.921447
1339.915989	77.363995	66.926452
1338.621639	64.672539	66.931457
1338.497210	58.219264	66.936462
1337.909450	64.323665	66.941466
1337.058369	58.954091	66.946471
1336.240147	71.386814	66.951476
1335.771249	66.054252	66.956481
1335.322405	63.198910	66.961486
1334.208001	79.247163	66.966490
1333.381751	66.049239	66.971495
1332.952173	69.972925	66.976500
1332.632231	70.843722	66.981505
1332.281075	58.869620	66.986510
1330.940635	70.240552	66.991514
1330.619428	63.115274	66.996519
1330.056632	64.925064	67.001524
1329.039844	65.808867	67.006529
1328.257778	62.588628	67.011534
1327.287432	68.761733	67.016538
1326.982469	74.234592	67.021543
1326.887721	69.325076	67.026548
1326.247364	65.921471	67.031553
1325.355837	56.226689	67.036558
1324.648712	62.242839	67.041562
1324.187579	60.702981	67.046567
1323.037142	62.666106	67.051572
1322.451481	67.549685	67.056577
1322.322212	56.674080	67.061582
1321.182185	59.625821	67.066586
1320.330080	61.543100	67.071591
1319.437640	55.150418	67.076596
1318.866474	65.370949	67.081601
1318.845846	62.854370	67.086606
1318.239982	65.517784	67.091610
1317.557498	61.531132	67.096615
1316.747826	67.380671	67.101620
1315.685888	64.291653	67.106625
1315.886761	54.103119	67.111630
1314.497132	59.655365	67.116634
1314.255222	62.002317	67.121639
1313.375652	61.583900	67.126644
1312.205950	73.036503	67.131649
1311.819718	62.215937	67.136654
1311.120751	63.415055	67.141658
1310.906813	63.682409	67.146663
1310.117511	66.622553	67.151668
1309.207167	73.199266	67.156673
1308.736629	58.091998	67.161678
1307.783633	69.798717	67.166682
1307.345988	69.328971	67.171687
1306.859586	60.291995	67.176692
1305.953767	71.822492	67.181697
1305.250116	64.046851	67.186702
1304.564559	68.531599	67.191706
1304.556868	59.434292	67.196711
1303.265967	71.773438	67.201716
1302.825472	68.205610	67.206721
1302.130422	58.580522	67.211726
1301.704234	61.854005	67.216730
1300.517525	73.809181	67.221735
1299.935591	63.890157	67.226740
1299.265414	67.426343	67.231745
1299.146434	53.393807	67.236750
1298.082317	77.364111	67.241754
1297.392897	64.202797	67.246759
1296.459352	71.967425	67.251764
1296.075121	68.100510	67.256769
1296.015787	63.491280	67.261774
1294.452471	75.279263	67.266778
1294.041906	69.793942	67.271783
1293.359650	66.262973	67.276788
1292.732802	65.558396	67.281793
1292.518143	65.721793	67.286798
1291.403804	80.328795	67.291802
1290.772239	66.332007	67.296807
1290.298040	73.604167	67.301812
1289.650054	69.621498	67.306817
1288.612654	56.939691	67.311822
1288.373552	62.537688	67.316826
1287.525225	70.812288	67.321831
1287.286299	68.089154	67.326836
1285.822810	71.322557	67.331841
1285.735875	52.759332	67.336846
1285.205253	74.891350	67.341850
1284.309025	65.905340	67.346855
1283.561501	61.555321	67.351860
1282.641745	69.021309	67.356865
1282.527030	60.324196	67.361870
1281.629586	64.982975	67.366874
1280.599864	63.689629	67.371879
1280.012086	61.515516	67.376884
1279.624308	67.430447	67.381889
1279.371076	60.994502	67.386894
1278.474505	71.798177	67.391898
1277.542256	72.832554	67.396903
1277.287097	60.646096	67.401908
1276.374084	77.170092	67.406913
1275.624718	65.759174	67.411918
1274.540452	74.049213	67.416922
1274.327159	60.410116	67.421927
1273.812019	62.248608	67.426932
1273.006639	70.658302	67.431937
1272.441523	54.646776	67.436942
1271.879798	69.443442	67.441946
1271.347576	58.754903	67.446951
1270.311312	64.392910	67.451956
1269.460778	61.924702	67.456961
1268.638528	61.229121	67.461966
1268.351289	67.927539	67.466970
1268.290473	62.484387	67.471975
1267.295318	66.600496	67.476980
1266.131510	72.807533	67.481985
1265.822359	58.180795	67.486990
1265.082036	68.478687	67.491994
1264.101734	59.420906	67.496999
1263.473013	61.756824	67.502004
1262.803216	74.900782	67.507009
1262.856747	67.239725	67.512014
1261.985497	74.540323	67.517018
1261.383612	72.791055	67.522023
1260.460051	75.709985	67.527028
1259.864552	69.251189	67.532033
1259.399213	60.160419	67.537038
1258.031662	65.338622	67.542042
1257.450210	61.160893	67.547047
1257.115669	62.726261	67.552052
1256.667616	65.257371	67.557057
1255.991398	62.772491	67.562062
1255.108165	64.748353	67.567066
1254.739468	61.066625	67.572071
1254.202746	57.296502	67.577076
1252.879960	75.281173	67.582081
1252.319109	57.890795	67.587086
1251.655576	67.200403	67.592090
1251.227588	64.141501	67.597095
1250.931968	65.003709	67.602100
1249.690436	62.159306	67.607105
1249.191676	55.428110	67.612110
1248.542886	64.729065	67.617114
1248.218614	68.117231	67.622119
1247.358687	61.500224	67.627124
1246.298672	60.022485	67.632129
1245.899881	59.221740	67.637134
1245.088851	58.467615	67.642138
1244.646845	72.341711	67.647143
1243.869731	62.344936	67.652148
1242.772284	74.252825	67.657153
1242.598167	66.389858	67.662158
1242.222254	66.257219	67.667162
1241.799502	57.788852	67.672167
1240.937216	69.675118	67.677172
1239.920951	67.040893	67.682177
1239.412756	53.593770	67.687182
1237.878678	59.840762	67.692186
1237.292016	65.544482	67.697191
1237.176136	54.335624	67.702196
1236.560928	67.360519	67.707201
1236.210164	54.550647	67.712206
1235.940076	57.048732	67.717210
1235.198913	58.946821	67.722215
1234.640931	57.766135	67.727220
1233.408093	69.231953	67.732225
1232.746051	55.973286	67.737230
1232.266523	64.184526	67.742234
1231.830836	58.012552	67.747239
1230.425563	64.380988	67.752244
1229.510887	61.585545	67.757249
1229.175100	67.000233	67.762254
1228.819372	73.512437	67.767258
1228.727179	60.499032	67.772263
1227.692392	68.098436	67.777268
1226.823489	67.222640	67.782273
1226.609518	62.779920	67.787278
1225.097485	57.523368	67.792282
1224.430042	66.139782	67.797287
1223.609867	60.848912	67.802292
1223.106997	67.922219	67.807297
1223.246171	54.998182	67.812302
1222.517926	57.870296	67.817306
1221.684448	67.796676	67.822311
1220.828017	63.568069	67.827316
1220.189375	68.843267	67.832321
1219.436278	66.030019	67.837326
1218.846811	69.906607	67.842330
1217.973565	63.305921	67.847335
1217.728574	51.989871	67.852340
1216.648007	59.077766	67.857345
1215.918557	55.155382	67.862350
1215.335626	62.780704	67.867354
1214.650932	60.437525	67.872359
1214.694412	66.739602	67.877364
1213.938072	70.745221	67.882369
1213.218881	67.406219	67.887374
1212.455147	56.609442	67.892378
1211.772911	67.289167	67.897383
1211.012230	55.594672	67.902388
1209.775576	65.108949	67.907393
1209.881607	66.454467	67.912398
1209.114235	55.622002	67.917402
1208.103910	65.404626	67.922407
1207.323925	64.407471	67.927412
1206.441412	66.383235	67.932417
1206.020366	59.833645	67.937422
1205.972309	74.126044	67.942426
1205.296076	74.518952	67.947431
1204.420532	68.432691	67.952436
1203.466715	67.597212	67.957441
1203.425615	60.820060	67.962446
1202.083671	66.442046	67.967450
1201.274238	59.943178	67.972455
1201.150312	69.026650	67.977460
1200.437264	62.676448	67.982465
1199.965900	63.021012	67.987470
1198.839862	61.790322	67.992474
1198.213971	62.764973	67.997479
1197.898672	62.644778	68.002484
1197.252048	62.832719	68.007489
1196.162011	51.062880	68.012494
1195.406196	58.762999	68.017498
1194.606557	60.400755	68.022503
1194.682859	48.551103	68.027508
1194.074336	63.498704	68.032513
1193.004551	58.864090	68.037518
1192.616065	53.212871	68.042522
1192.153429	48.424948	68.047527
1191.367871	56.008379	68.052532
1190.133343	68.141492	68.057537
1189.354992	52.435130	68.062542
1189.049868	60.465684	68.067546
1188.669045	64.277561	68.072551
1188.084811	47.417612	68.077556
1187.081107	67.220133	68.082561
1186.743169	59.944591	68.087566
1185.876023	62.372053	68.092570
1184.489028	65.289011	68.097575
1184.026335	56.913739	68.102580
1183.245513	67.300081	68.107585
1183.331213	62.259390	68.112590
1182.904456	65.089881	68.117594
1182.314585	59.286192	68.122599
1181.601928	50.014019	68.127604
1180.588991	69.631943	68.132609
1180.071102	53.250267	68.137614
1178.708718	54.266350	68.142618
1178.206910	63.074038	68.147623
1178.187854	54.492611	68.152628
1177.447956	69.188313	68.157633
1176.723090	62.970878	68.162638
1175.834517	62.659590	68.167642
1175.196109	63.558971	68.172647
1174.916862	58.439129	68.177652
1173.953394	64.486615	68.182657
1173.111779	67.985440	68.187662
1172.409842	68.552746	68.192666
1171.730508	68.939849	68.197671
1171.623198	61.555099	68.202676
1170.469785	62.520611	68.207681
1169.860279	61.777039	68.212686
1169.337985	58.942874	68.217690
1168.936428	76.293826	68.222695
1167.946630	56.656865	68.227700
1167.070953	61.660701	68.232705
1166.491867	57.577234	68.237710
1166.213310	60.727914	68.242714
1165.541641	69.982064	68.247719
1165.073437	60.147498	68.252724
1163.891033	63.631138	68.257729
1163.582454	62.119087	68.262734
1162.327728	67.456002	68.267738
1161.464591	63.422437	68.272743
1161.422739	59.661943	68.277748
1160.688088	62.826812	68.282753
1160.530960	60.965844	68.287758
1159.739018	66.729029	68.292762
1158.595685	64.955513	68.297767
1158.033379	52.840011	68.302772
1157.657877	71.629639	68.307777
1156.813402	46.176202	68.312782
1155.873136	64.937371	68.317786
1155.219926	67.352897	68.322791
1155.103975	62.555575	68.327796
1154.222008	64.829294	68.332801
1153.382940	67.127730	68.337806
1152.459227	76.943909	68.342810
1151.954144	62.373588	68.347815
1151.898897	69.006734	68.352820
1151.029899	69.617959	68.357825
1150.341765	57.494082	68.362830
1149.609967	68.807713	68.367834
1148.573023	79.334144	68.372839
1148.071270	60.978829	68.377844
1147.220490	73.032011	68.382849
1146.761882	57.419885	68.387854
1146.298477	70.750213	68.392858
1145.964465	63.873000	68.397863
1144.980550	57.865500	68.402868
1144.112144	63.837955	68.407873
1143.864730	63.828389	68.412878
1142.737743	65.351072	68.417882
1141.819020	62.141592	68.422887
1142.181975	61.706969	68.427892
1141.428669	65.431442	68.432897
1140.268876	57.871901	68.437902
1139.400856	55.874848	68.442906
1138.601183	69.201887	68.447911
1138.684544	67.045646	68.452916
1137.606143	69.929319	68.457921
1136.891880	59.110512	68.462926
1136.482155	59.878922	68.467930
1135.663177	54.808657	68.472935
1134.787884	60.160927	68.477940
1134.072061	67.826321	68.482945
1133.600164	56.940588	68.487950
1133.287929	62.308960	68.492954
1132.527410	60.320043	68.497959
1131.558900	62.691107	68.502964
1130.789310	60.840820	68.507969
1130.516605	62.043151	68.512974
1129.551161	64.123586	68.517978
1128.528774	60.250972	68.522983
1128.111441	56.487123	68.527988
1127.415094	65.029306	68.532993
1127.146583	55.554056	68.537998
1127.095554	57.049119	68.543002
1125.694232	72.665261	68.548007
1125.096925	55.596108	68.553012
1124.474309	70.069751	68.558017
1124.003312	59.109764	68.563022
1123.012691	69.073773	68.568026
1122.282065	63.973690	68.573031
1122.203996	62.488059	68.578036
1121.182983	62.186816	68.583041
1120.297982	60.720718	68.588046
1119.935855	54.444039	68.593050
1119.213569	73.255707	68.598055
1118.337468	63.276303	68.603060
1117.434474	74.243456	68.608065
1116.898262	61.849437	68.613070
1116.653474	61.030526	68.618074
1116.279440	64.142783	68.623079
1115.329958	63.856972	68.628084
1114.349985	55.305386	68.633089
1113.737086	68.128088	68.638094
1113.677134	65.198326	68.643098
1112.658136	65.653658	68.648103
1111.969485	68.844338	68.653108
1111.243432	68.046782	68.658113
1110.056262	59.644837	68.663118
1109.081034	61.912904	68.668122
1108.338283	70.344210	68.673127
1108.307300	60.047484	68.678132
1107.901641	70.877192	68.683137
1107.750179	60.522361	68.688142
1107.394081	67.446189	68.693146
1106.107637	67.144593	68.698151
1105.439159	57.769229	68.703156
1104.704028	67.065017	68.708161
1103.338968	67.077106	68.713166
1102.693636	57.933014	68.718170
1102.020539	59.914924	68.723175
1102.276110	55.525268	68.728180
1101.694674	58.512827	68.733185
1100.967001	54.681656	68.738190
1100.217686	55.795802	68.743194
1099.488478	69.157369	68.748199
1099.052242	52.081535	68.753204
1097.804007	58.376172	68.758209
1097.083952	64.079056	68.763214
1096.900267	54.289141	68.768218
1095.756977	66.242204	68.773223
1095.329436	50.864845	68.778228
1094.515959	59.495043	68.783233
1094.326105	49.155790	68.788238
1093.840341	58.254226	68.793242
1092.386295	60.190051	68.798247
1092.241400	53.530340	68.803252
1091.307428	60.940294	68.808257
1090.710949	62.034864	68.813262
1089.807768	56.848707	68.818266
1088.972348	66.592508	68.823271
1088.996593	53.699379	68.828276
1088.364418	57.526014	68.833281
1087.416363	55.369834	68.838286
1086.803144	52.146476	68.843290
1085.855025	64.957846	68.848295
1085.474459	58.289890	68.853300
1084.687388	56.705734	68.858305
1083.582537	59.461178	68.863310
1083.137517	48.965406	68.868314
1082.498619	59.305535	68.873319
1082.451460	49.391415	68.878324
1081.800980	59.337595	68.883329
1080.827059	49.406892	68.888334
1080.351386	50.094341	68.893338
1079.761651	58.990133	68.898343
1078.932702	59.640741	68.903348
1077.621886	54.590386	68.908353
1077.109357	59.153308	68.913358
1077.081439	58.459170	68.918362
1076.357709	53.802683	68.923367
1076.030653	65.733148	68.928372
1074.957934	58.276479	68.933377
1074.445257	61.223147	68.938382
1073.775854	54.722557	68.943386
1072.421512	59.383112	68.948391
1071.984609	50.257918	68.953396
1071.697966	57.903935	68.958401
1070.951861	49.444476	68.963406
1069.967190	52.207615	68.968410
1069.084149	50.747533	68.973415
1068.691400	45.902795	68.978420
1068.199577	63.078862	68.983425
1067.850542	62.547759	68.988430
1067.230184	57.898484	68.993434
1066.458002	55.572419	68.998439
1066.072227	58.735431	69.003444
1065.242621	61.125422	69.008449
1064.078916	64.804814	69.013454
1063.605691	55.683820	69.018458
1063.058361	58.601310	69.023463
1062.450381	60.599678	69.028468
1061.128733	63.539418	69.033473
1060.713924	64.308649	69.038478
1060.828556	58.634193	69.043482
1059.811764	63.767734	69.048487
1058.925316	58.906913	69.053492
1058.054103	63.146872	69.058497
1057.783024	60.865671	69.063502
1057.568851	55.278210	69.068506
1056.384736	56.567181	69.073511
1055.549161	56.952360	69.078516
1054.928890	62.774990	69.083521
1054.408752	56.720565	69.088526
1053.916272	53.930569	69.093530
1052.789480	58.750468	69.098535
1052.658011	60.892223	69.103540
1052.274207	55.560391	69.108545
1051.102176	62.122031	69.113550
1050.239001	54.876457	69.118554
1049.853470	65.163677	69.123559
1049.616159	55.672442	69.128564
1047.702911	57.410117	69.133569
1047.131583	55.950918	69.138574
1047.182305	64.804760	69.143578
1046.704260	61.837436	69.148583
1046.459605	53.583628	69.153588
1045.301411	53.484000	69.158593
1044.444649	63.802026	69.163598
1043.883647	54.141524	69.168602
1042.719546	61.788361	69.173607
1042.177293	56.521156	69.178612
1041.481444	66.203344	69.183617
1041.165905	58.949501	69.188622
1041.051758	52.805269	69.193626
1039.864722	62.448903	69.198631
1039.289454	58.965646	69.203636
1038.463438	61.112238	69.208641
1038.107274	55.411757	69.213646
1037.264566	60.586993	69.218650
1035.957453	64.142562	69.223655
1035.950049	63.311128	69.228660
1035.370589	66.823481	69.233665
1034.762375	63.176741	69.238670
1033.953654	62.048603	69.243674
1032.977894	60.373061	69.248679
1032.555469	48.684759	69.253684
1032.014279	53.622807	69.258689
1031.412738	52.259876	69.263694
1030.819294	59.667712	69.268698
1030.016762	58.477094	69.273703
1029.324185	44.734551	69.278708
1028.407191	64.803983	69.283713
1027.398539	53.637840	69.288718
1027.109258	54.283034	69.293722
1026.396161	64.849430	69.298727
1026.239025	50.864020	69.303732
1025.625036	48.604262	69.308737
1024.708820	57.633994	69.313742
1024.157802	62.663490	69.318746
1023.584927	69.263863	69.323751
1022.889198	59.728870	69.328756
1022.010142	57.640581	69.333761
1021.475160	63.752405	69.338766
1020.887829	58.249540	69.343770
1019.443612	56.982822	69.348775
1019.100999	64.849046	69.353780
1018.793165	50.330981	69.358785
1018.019228	52.934465	69.363790
1017.774450	51.131606	69.368794
1016.627857	70.937970	69.373799
1016.085456	52.445691	69.378804
1015.528651	62.583549	69.383809
1014.744348	46.282172	69.388814
1013.966527	54.186089	69.393818
1013.189502	67.077485	69.398823
1013.090929	46.650762	69.403828
1012.332207	62.744991	69.408833
1011.106812	56.657704	69.413838
1010.610551	43.133083	69.418842
1010.005584	66.279784	69.423847
1009.780830	56.427036	69.428852
1009.341070	60.596793	69.433857
1008.326214	60.283579	69.438862
1007.908261	52.449986	69.443866
1006.648810	61.531176	69.448871
1005.852765	68.665341	69.453876
1005.426057	62.976087	69.458881
1004.658566	63.967003	69.463886
1004.565782	50.862284	69.468890
1003.371325	56.763652	69.473895
1002.723863	59.608779	69.478900
1001.533614	51.737213	69.483905
1001.402682	63.653820	69.488910
1001.284970	54.922536	69.493914
1000.524790	59.099118	69.498919
999.456822	57.096082	69.503924
998.956174	57.087395	69.508929
998.476573	66.631115	69.513934
997.991589	54.645284	69.518938
996.753917	60.551954	69.523943
996.469455	55.849263	69.528948
995.761954	61.887617	69.533953
994.555338	60.971019	69.538958
994.151251	66.210521	69.543962
993.397711	63.476261	69.548967
993.129581	68.055507	69.553972
992.734447	67.156455	69.558977
991.693398	70.844749	69.563982
990.861491	56.376948	69.568986
990.366245	76.060777	69.573991
989.774709	67.237723	69.578996
988.458913	61.754574	69.584001
988.105250	57.411378	69.589006
987.773535	58.159515	69.594010
987.353218	62.043925	69.599015
986.602192	58.651719	69.604020
985.869494	60.890706	69.609025
985.099376	64.792924	69.614030
984.559248	49.851383	69.619034
983.022845	58.975066	69.624039
982.681081	51.466806	69.629044
982.174402	67.490984	69.634049
981.985176	60.155559	69.639054
981.484774	51.212369	69.644058
980.244301	51.695105	69.649063
979.659516	58.067154	69.654068
979.018745	58.981149	69.659073
978.573681	62.680275	69.664078
977.889076	55.811574	69.669082
976.761862	54.795624	69.674087
976.524118	56.052328	69.679092
976.125786	58.835749	69.684097
975.013287	60.282086	69.689102
974.379663	54.113284	69.694106
973.700074	55.134376	69.699111
973.432815	45.465013	69.704116
972.782958	58.336175	69.709121
971.348110	55.394949	69.714126
971.155088	53.833004	69.719130
970.426664	65.798943	69.724135
970.172590	55.331163	69.729140
969.319030	53.465905	69.734145
968.614929	65.076336	69.739150
968.125450	47.698385	69.744154
967.028168	62.670151	69.749159
966.259440	55.969370	69.754164
965.617655	58.517153	69.759169
964.930342	51.521164	69.764174
965.191915	56.203775	69.769178
964.326483	60.625757	69.774183
963.452380	59.023950	69.779188
963.172800	58.779837	69.784193
961.758377	66.471264	69.789198
961.079722	49.478206	69.794202
960.555754	57.191945	69.799207
960.172986	56.249935	69.804212
959.191461	64.109014	69.809217
958.091274	64.422793	69.814222
957.788172	48.514783	69.819226
957.270951	60.863406	69.824231
956.889847	67.305550	69.829236
956.006327	59.642230	69.834241
955.359796	63.887469	69.839246
954.951180	53.904725	69.844250
954.135521	50.402974	69.849255
953.149945	57.046940	69.854260
952.451403	64.069415	69.859265
951.769032	49.686650	69.864270
951.849253	55.210194	69.869274
950.591661	60.399430	69.874279
949.884584	59.971040	69.879284
949.302110	55.616953	69.884289
948.726986	68.569271	69.889294
948.442731	55.670054	69.894298
947.146825	63.933950	69.899303
946.439070	57.139901	69.904308
946.279150	57.411305	69.909313
945.454070	66.407639	69.914318
944.609115	50.503850	69.919322
943.927233	59.551508	69.924327
943.455748	57.705886	69.929332
943.118167	58.849176	69.934337
942.043770	53.050120	69.939342
941.493757	63.860223	69.944346
940.692763	56.808215	69.949351
940.318264	60.114518	69.954356
939.384029	58.359872	69.959361
938.505137	66.111170	69.964366
937.930916	59.218610	69.969370
937.222704	53.809118	69.974375
937.013059	55.252153	69.979380
936.939708	56.671926	69.984385
935.277555	69.201156	69.989390
935.099843	51.319473	69.994394
934.034263	65.023145	69.999399
932.995808	55.566374	70.004404
932.515202	62.651940	70.009409
931.556221	59.526215	70.014414
931.779062	62.213957	70.019418
931.241929	60.989026	70.024423
930.853568	58.135183	70.029428
929.714993	59.469001	70.034433
929.045472	58.555277	70.039438
928.408493	52.230916	70.044442
927.272734	56.746381	70.049447
926.570664	61.277989	70.054452
926.232924	59.636579	70.059457
925.634963	64.064895	70.064462
925.084518	62.646553	70.069466
924.330558	55.566569	70.074471
923.596660	66.311324	70.079476
923.051288	54.128559	70.084481
922.225833	62.669245	70.089486
921.682113	50.464145	70.094490
920.990461	57.181193	70.099495
920.539111	45.964278	70.104500
919.932555	56.654073	70.109505
918.670761	63.710990	70.114510
918.562340	56.468368	70.119514
918.020333	59.616835	70.124519
916.699070	52.959843	70.129524
916.297983	58.326598	70.134529
915.580255	59.470461	70.139534
915.309872	55.330057	70.144538
914.225609	58.631039	70.149543
913.416982	46.701472	70.154548
913.143127	49.681121	70.159553
912.496085	63.043824	70.164558
912.156425	48.910877	70.169562
910.821576	60.452956	70.174567
910.327325	53.099855	70.179572
910.112412	58.260378	70.184577
908.648270	59.291219	70.189582
908.128659	54.525042	70.194586
907.308259	61.106473	70.199591
907.101821	57.760091	70.204596
906.975975	61.480965	70.209601
906.065094	63.008782	70.214606
904.993791	48.640623	70.219610
904.336745	63.003068	70.224615
904.172988	55.565839	70.229620
903.364810	51.080536	70.234625
902.229521	58.908907	70.239630
901.961608	51.065658	70.244634
901.361523	63.818533	70.249639
900.226337	59.771594	70.254644
899.713508	62.084420	70.259649
899.053243	63.438326	70.264654
899.066214	49.052161	70.269658
897.477891	54.245165	70.274663
896.831178	65.365533	70.279668
896.533681	53.539124	70.284673
895.872545	61.799794	70.289678
895.721133	54.213956	70.294682
894.358400	54.479661	70.299687
893.715013	54.403829	70.304692
893.396748	50.570652	70.309697
892.741364	64.352553	70.314702
891.857647	55.148707	70.319706
890.800731	56.851146	70.324711
890.673424	57.864792	70.329716
890.329895	50.296913	70.334721
889.337124	55.560720	70.339726
888.549198	50.189161	70.344730
888.064544	54.372383	70.349735
887.317229	49.278196	70.354740
886.606278	53.981524	70.359745
885.466575	50.786815	70.364750
885.029655	58.056231	70.369754
884.635952	59.173768	70.374759
884.352658	62.328377	70.379764
883.449816	56.848956	70.384769
882.518654	64.625932	70.389774
882.276008	46.366695	70.394778
881.666145	57.380277	70.399783
880.478574	50.150133	70.404788
879.848834	59.774518	70.409793
879.569268	61.622898	70.414798
879.133875	59.191263	70.419802
877.853441	58.603417	70.424807
877.185591	57.397723	70.429812
876.924975	57.730884	70.434817
876.023587	63.718124	70.439822
875.441958	59.182583	70.444826
874.709961	63.118185	70.449831
874.398808	51.666094	70.454836
873.532700	56.747333	70.459841
872.402047	62.868823	70.464846
871.862671	62.308118	70.469850
871.342139	62.859251	70.474855
870.908958	50.319629	70.479860
870.248705	57.429057	70.484865
869.399801	61.198772	70.489870
869.002217	54.670762	70.494874
868.382922	58.437050	70.499879
866.857275	51.386864	70.504884
866.528085	51.844472	70.509889
865.707073	56.022884	70.514894
865.654080	53.841036	70.519898
865.531357	63.392621	70.524903
864.238576	58.225983	70.529908
863.488076	54.450560	70.534913
862.609996	62.329472	70.539918
862.658552	55.194331	70.544922
861.597564	59.702654	70.549927
860.584601	52.007944	70.554932
860.147784	59.859205	70.559937
859.502567	60.947392	70.564942
859.004293	51.942402	70.569946
857.710372	62.189701	70.574951
856.989690	57.157511	70.579956
857.285490	49.205637	70.584961
856.259939	64.957599	70.589966
856.013319	45.998880	70.594970
854.603409	52.858631	70.599975
853.982891	51.781021	70.604980
853.976406	62.547206	70.609985
852.881733	59.501453	70.614990
852.379389	47.433288	70.619994
851.744445	53.400202	70.624999
851.177568	63.741518	70.630004
850.014377	59.516146	70.635009
849.194161	59.550464	70.640014
848.715695	57.042116	70.645018
848.325906	64.125853	70.650023
847.759605	54.463105	70.655028
847.544299	57.895460	70.660033
845.975428	62.325357	70.665038
845.613824	53.899401	70.670042
845.410940	63.227214	70.675047
844.245207	53.663022	70.680052
843.658082	59.515104	70.685057
843.160017	61.402993	70.690062
842.501753	58.905916	70.695066
841.371073	54.339506	70.700071
840.654803	71.789410	70.705076
840.536415	54.418669	70.710081
839.838618	61.182441	70.715086
839.544308	60.783001	70.720090
838.358503	61.938307	70.725095
837.401884	56.860101	70.730100
837.479207	64.195904	70.735105
836.772642	68.207888	70.740110
835.813452	53.451360	70.745114
835.251373	65.887554	70.750119
834.480730	70.636668	70.755124
833.526577	64.334429	70.760129
832.749839	56.092809	70.765134
832.382495	51.475873	70.770138
831.945013	56.764855	70.775143
831.291898	56.431983	70.780148
830.540235	59.637488	70.785153
829.544418	67.087323	70.790158
829.451831	52.643853	70.795162
828.713847	56.140475	70.800167
827.659437	64.673472	70.805172
827.139142	58.325839	70.810177
826.386235	58.508714	70.815182
826.516076	54.210014	70.820186
825.042468	55.505743	70.825191
824.235840	58.035643	70.830196
823.944087	58.755364	70.835201
823.435506	56.918824	70.840206
822.317282	42.368965	70.845210
821.722016	60.699981	70.850215
820.908933	58.216514	70.855220
820.641366	54.419431	70.860225
820.228884	67.595015	70.865230
819.321558	62.144716	70.870234
818.222438	55.761488	70.875239
817.902623	60.724259	70.880244
817.558003	58.798550	70.885249
816.652930	63.550140	70.890254
815.856279	53.510931	70.895258
815.290640	57.875778	70.900263
814.534475	54.448180	70.905268
814.509216	54.128915	70.910273
813.027792	63.759566	70.915278
812.870477	60.938353	70.920282
812.008049	48.066552	70.925287
811.177211	61.455365	70.930292
810.598624	53.350940	70.935297
809.345495	51.899399	70.940302
809.369726	55.654729	70.945306
809.335305	50.689936	70.950311
808.137428	60.655479	70.955316
807.678870	52.290693	70.960321
806.926007	77.274328	70.965326
805.946799	57.350491	70.970330
805.225820	68.626188	70.975335
804.286552	62.318440	70.980340
804.342708	63.402230	70.985345
803.628734	62.842524	70.990350
803.020979	50.808496	70.995354
802.052159	63.361467	71.000359
801.641284	58.127030	71.005364
801.048418	51.958104	71.010369
800.079548	59.666990	71.015374
799.823390	53.469701	71.020378
798.827035	62.073885	71.025383
797.711599	65.843471	71.030388
797.116821	56.421800	71.035393
796.604006	58.682605	71.040398
796.290219	68.174720	71.045402
795.609507	59.276049	71.050407
794.775555	65.181620	71.055412
794.136692	52.173320	71.060417
793.305440	60.178828	71.065422
792.974761	61.926549	71.070426
792.210108	48.082044	71.075431
790.934107	56.841119	71.080436
790.784215	52.692595	71.085441
790.496792	59.310636	71.090446
789.904575	50.997091	71.095450
788.987484	44.597524	71.100455
788.152729	61.662607	71.105460
787.791706	47.652938	71.110465
786.676902	60.481444	71.115470
786.156404	53.447926	71.120474
785.563303	51.443511	71.125479
785.070814	51.379955	71.130484
784.634969	49.476658	71.135489
783.404924	46.759974	71.140494
782.894890	52.295459	71.145498
782.700387	56.473511	71.150503
781.567309	48.887841	71.155508
780.921320	52.946958	71.160513
780.082474	47.879994	71.165518
779.994044	53.130765	71.170522
779.008763	47.647168	71.175527
778.077909	58.506867	71.180532
777.516512	52.977872	71.185537
776.947567	61.359496	71.190542
776.365762	53.416434	71.195546
775.612504	55.792782	71.200551
774.807651	64.722860	71.205556
774.559349	52.871306	71.210561
773.986317	66.228554	71.215566
772.896178	56.676020	71.220570
772.022340	59.011643	71.225575
771.470242	61.660304	71.230580
771.431941	50.242073	71.235585
770.371244	55.387430	71.240590
769.818926	57.145205	71.245594
769.153339	53.936579	71.250599
768.332350	60.205921	71.255604
767.543825	45.696644	71.260609
766.627919	57.489038	71.265614
766.237878	64.072959	71.270618
765.817634	53.442454	71.275623
765.542059	68.121062	71.280628
764.813084	58.493696	71.285633
763.684726	62.508187	71.290638
763.380107	55.752526	71.295642
762.299356	51.864139	71.300647
761.528212	66.640555	71.305652
761.116912	51.125115	71.310657
760.577211	57.285031	71.315662
760.167674	60.093915	71.320666
759.071981	61.597589	71.325671
757.793612	58.363517	71.330676
757.800251	59.120895	71.335681
757.233974	54.940891	71.340686
756.917532	53.773904	71.345690
755.794083	54.154548	71.350695
755.000525	67.140075	71.355700
754.634912	56.516643	71.360705
754.059944	67.994595	71.365710
753.260215	53.302609	71.370714
752.464090	57.852381	71.375719
751.787437	61.662516	71.380724
751.766983	60.254457	71.385729
750.162826	59.325574	71.390734
749.719861	60.972910	71.395738
749.385546	60.983524	71.400743
748.717935	58.524230	71.405748
747.923971	49.962136	71.410753
746.741336	52.469917	71.415758
746.757471	49.950662	71.420762
746.335130	49.998942	71.425767
745.579453	52.590134	71.430772
744.796419	52.189663	71.435777
744.234297	55.377631	71.440782
743.406220	52.860311	71.445786
742.393182	62.676614	71.450791
741.553621	60.290424	71.455796
741.415213	58.581042	71.460801
740.704042	57.981487	71.465806
739.613128	56.185634	71.470810
738.819323	54.872305	71.475815
738.437250	59.381398	71.480820
738.430179	57.452425	71.485825
737.855261	62.785375	71.490830
736.624413	61.929527	71.495834
735.989798	50.314513	71.500839
734.907587	71.192413	71.505844
735.164806	51.546428	71.510849
734.295599	73.159925	71.515854
733.535190	62.034831	71.520858
732.904336	68.198229	71.525863
731.713169	60.374261	71.530868
731.005420	57.136090	71.535873
730.108542	60.222822	71.540878
729.579411	60.430022	71.545882
729.585966	56.374860	71.550887
729.262391	68.582298	71.555892
728.485278	53.181870	71.560897
727.544326	57.642749	71.565902
726.885422	63.142026	71.570906
726.312245	54.800238	71.575911
725.176853	66.253877	71.580916
724.828285	54.620132	71.585921
724.164493	62.608459	71.590926
723.489481	50.566247	71.595930
722.673422	53.487159	71.600935
721.837519	54.386553	71.605940
721.656022	56.271371	71.610945
720.899002	59.871970	71.615950
720.190168	57.129107	71.620954
719.331671	51.548086	71.625959
718.386091	58.181029	71.630964
718.220870	46.522834	71.635969
717.520192	66.007552	71.640974
717.328412	58.792416	71.645978
716.476626	55.416342	71.650983
715.602206	60.418532	71.655988
715.014714	61.495987	71.660993
713.982816	60.706242	71.665998
713.287361	52.560535	71.671002
712.659364	52.070741	71.676007
712.076775	54.377359	71.681012
711.937096	50.936801	71.686017
711.120572	49.731171	71.691022
710.293897	56.507601	71.696026
709.867857	47.521119	71.701031
708.863005	56.421551	71.706036
707.936109	57.073679	71.711041
707.510434	61.122969	71.716046
706.904331	54.655000	71.721050
706.979656	50.085877	71.726055
705.623211	49.871320	71.731060
705.232941	55.832423	71.736065
704.182728	56.986702	71.741070
703.551262	55.645963	71.746074
702.875932	47.946461	71.751079
701.912764	60.418135	71.756084
701.409585	51.093873	71.761089
701.267351	49.072888	71.766094
700.739327	49.007122	71.771098
700.021878	43.433617	71.776103
699.021804	58.782610	71.781108
698.854874	52.217917	71.786113
697.817868	59.357400	71.791118
696.863989	60.277163	71.796122
696.782755	59.640402	71.801127
695.660347	61.670294	71.806132
695.110623	52.553704	71.811137
693.990537	64.662461	71.816142
693.585108	52.913208	71.821146
693.357161	52.414916	71.826151
692.170947	56.131160	71.831156
691.974841	51.824434	71.836161
691.414521	60.020205	71.841166
690.714341	54.273649	71.846170
689.644544	47.013823	71.851175
688.596466	53.756127	71.856180
688.567253	43.419763	71.861185
688.045265	49.094349	71.866190
687.279958	54.429234	71.871194
686.393536	47.048757	71.876199
685.301288	56.579659	71.881204
685.633765	43.713206	71.886209
685.007088	57.462169	71.891214
683.770067	50.646835	71.896218
683.024162	57.473486	71.901223
682.495125	59.050964	71.906228
682.167367	55.548895	71.911233
680.966343	53.469422	71.916238
680.362817	53.152347	71.921242
679.967160	50.107339	71.926247
679.330828	62.481254	71.931252
678.560529	47.070311	71.936257
677.800626	57.871278	71.941262
677.305874	55.662010	71.946266
676.920805	56.331953	71.951271
675.489873	53.436011	71.956276
675.010283	61.585817	71.961281
674.436960	57.503144	71.966286
673.982999	56.443214	71.971290
673.616169	45.536172	71.976295
672.619598	55.870229	71.981300
672.037180	56.946886	71.986305
671.149025	49.877330	71.991310
670.802285	62.837454	71.996314
670.094099	52.109330	72.001319
669.054880	59.233407	72.006324
668.403719	47.261534	72.011329
668.060990	57.857317	72.016334
667.664692	52.136498	72.021338
666.619518	48.567323	72.026343
665.882261	58.473767	72.031348
665.362069	59.092692	72.036353
664.849532	51.816684	72.041358
663.835720	58.756955	72.046362
663.360127	49.806758	72.051367
662.639963	62.222406	72.056372
662.382485	42.385597	72.061377
661.110850	53.782097	72.066382
660.306905	53.727160	72.071386
660.012325	51.861314	72.076391
659.896548	56.708033	72.081396
659.359933	46.461923	72.086401
658.178201	47.540973	72.091406
657.549145	49.044500	72.096410
656.940041	52.402380	72.101415
655.770402	63.569775	72.106420
655.513100	57.058897	72.111425
654.725569	55.626334	72.116430
654.287238	51.960539	72.121434
653.427597	48.752887	72.126439
652.764921	60.512873	72.131444
652.365213	52.624430	72.136449
651.869812	44.136256	72.141454
650.836706	52.080901	72.146458
650.417963	45.898490	72.151463
649.438022	49.801088	72.156468
648.392246	37.489969	72.161473
647.231698	55.967761	72.166478
647.004639	40.673754	72.171482
646.914804	45.711868	72.176487
646.133678	46.988892	72.181492
645.741665	41.043487	72.186497
645.462894	48.585762	72.191502
644.187338	45.190469	72.196506
643.908346	45.668495	72.201511
643.107045	55.334420	72.206516
641.975654	35.873310	72.211521
641.378132	46.463928	72.216526
640.933443	41.392601	72.221530
640.562132	48.517556	72.226535
639.682074	41.834633	72.231540
638.834335	44.174024	72.236545
638.288806	43.861917	72.241550
637.849458	52.921463	72.246554
636.796532	40.475877	72.251559
636.177807	52.384968	72.256564
635.680254	39.847795	72.261569
634.998899	54.133710	72.266574
634.306559	50.525712	72.271578
633.840150	46.325111	72.276583
633.082202	64.412402	72.281588
632.657053	44.581800	72.286593
631.305398	55.516424	72.291598
630.625207	48.333351	72.296602
630.523145	42.305510	72.301607
629.827530	57.265437	72.306612
629.232671	42.930381	72.311617
628.259621	51.428404	72.316622
627.525963	48.796750	72.321626
627.147118	40.252182	72.326631
626.617045	47.433955	72.331636
625.698202	39.208750	72.336641
625.161713	48.717396	72.341646
624.253556	52.688992	72.346650
624.063036	46.238449	72.351655
622.595689	56.194931	72.356660
621.941827	41.259034	72.361665
621.380086	54.511990	72.366670
620.964843	48.100385	72.371674
620.829991	41.193155	72.376679
619.885900	54.013443	72.381684
619.221811	53.359120	72.386689
618.688493	47.001010	72.391694
617.886006	43.886767	72.396698
617.072116	50.656452	72.401703
616.166101	47.763685	72.406708
615.861636	43.753329	72.411713
615.099303	35.331331	72.416718
614.723466	44.486409	72.421722
614.021808	44.055676	72.426727
612.950150	45.475163	72.431732
612.624389	39.207000	72.436737
612.053117	43.522317	72.441742
610.801119	45.618608	72.446746
610.215604	41.924227	72.451751
609.654163	51.096251	72.456756
609.710281	49.646043	72.461761
608.708231	57.894821	72.466766
607.850196	46.528313	72.471770
607.934041	47.470500	72.476775
606.931960	57.018607	72.481780
605.744531	43.992097	72.486785
605.253034	43.420674	72.491790
604.530945	48.117955	72.496794
603.575867	38.288568	72.501799
602.720973	56.749235	72.506804
602.186498	41.143096	72.511809
601.950956	51.154141	72.516814
601.391186	51.678462	72.521818
601.405000	46.486822	72.526823
600.241547	42.841904	72.531828
599.577148	44.038857	72.536833
598.628657	50.183474	72.541838
597.666402	51.292251	72.546842
597.081455	48.058222	72.551847
596.676207	53.752077	72.556852
596.259530	49.630291	72.561857
595.285573	42.596512	72.566862
594.270240	58.799456	72.571866
593.772242	37.309021	72.576871
593.379486	57.388051	72.581876
593.303944	44.521926	72.586881
592.123598	48.081168	72.591886
591.209871	52.195578	72.596890
591.033816	39.933629	72.601895
590.017593	50.133649	72.606900
589.328780	39.068191	72.611905
588.621054	43.097757	72.616910
587.871067	51.970250	72.621914
587.980630	43.524516	72.626919
586.978541	44.675908	72.631924
586.070729	43.581048	72.636929
585.853275	45.960420	72.641934
584.589956	49.547072	72.646938
584.112338	36.696105	72.651943
582.807014	45.992904	72.656948
582.822475	40.769467	72.661953
582.394983	39.535041	72.666958
581.539266	58.210294	72.671962
580.644246	46.420786	72.676967
579.907012	49.603558	72.681972
579.762354	46.518596	72.686977
578.882363	50.205042	72.691982
577.654125	47.596980	72.696986
577.506940	45.877972	72.701991
576.845075	48.339160	72.706996
576.680372	44.801682	72.712001
575.674672	46.620661	72.717006
574.432753	52.455650	72.722010
574.236199	39.225630	72.727015
573.682252	52.065789	72.732020
573.010268	46.456703	72.737025
571.994555	49.923508	72.742030
571.382809	45.539501	72.747034
571.202117	41.577246	72.752039
570.417488	51.295718	72.757044
569.253861	38.457821	72.762049
568.877677	40.931855	72.767054
568.608657	40.101095	72.772058
567.814817	40.369408	72.777063
566.601070	40.621024	72.782068
565.955829	47.567274	72.787073
565.991583	36.255553	72.792078
565.296000	47.965591	72.797082
564.529881	42.019865	72.802087
563.520786	49.120252	72.807092
563.042347	42.561044	72.812097
562.157828	38.477511	72.817102
561.279385	39.992394	72.822106
561.098580	39.921818	72.827111
560.429577	45.921014	72.832116
559.945615	44.047500	72.837121
558.996307	37.057120	72.842126
557.909899	42.998223	72.847130
557.725689	41.926890	72.852135
557.297414	46.933755	72.857140
556.352234	39.881220	72.862145
555.557779	44.891215	72.867150
554.814780	45.919360	72.872154
554.721662	38.761082	72.877159
553.777256	51.523090	72.882164
552.719820	35.822082	72.887169
552.297357	45.607444	72.892174
551.981750	42.672707	72.897178
551.549121	39.509043	72.902183
550.173249	41.516289	72.907188
549.640351	50.967607	72.912193
549.275272	40.396193	72.917198
548.597477	43.779225	72.922202
547.929234	46.255626	72.927207
546.574385	48.519706	72.932212
546.351195	33.795935	72.937217
546.069902	47.931410	72.942222
544.837072	44.108348	72.947226
544.300452	35.806537	72.952231
543.782303	42.671050	72.957236
543.351772	42.533023	72.962241
543.077279	38.976770	72.967246
541.758907	47.687501	72.972250
541.292860	37.264627	72.977255
540.610496	43.932961	72.982260
539.863895	41.913638	72.987265
538.708473	31.843403	72.992270
538.011842	44.121274	72.997274
537.806923	39.953161	73.002279
537.438049	35.182001	73.007284
536.703892	35.292594	73.012289
535.925369	38.527680	73.017294
534.992657	43.633812	73.022298
535.270634	35.131301	73.027303
534.089194	48.516075	73.032308
533.307661	44.007745	73.037313
532.844220	35.845660	73.042318
532.049006	52.076625	73.047322
531.051376	36.011314	73.052327
530.619267	49.418655	73.057332
529.896492	40.969888	73.062337
529.644156	39.633462	73.067342
528.211724	48.786538	73.072346
527.584013	33.147981	73.077351
527.097331	45.438143	73.082356
526.922049	50.627052	73.087361
526.525801	34.372925	73.092366
525.261173	44.487955	73.097370
524.762594	35.371168	73.102375
524.271469	44.546190	73.107380
523.536338	37.614746	73.112385
522.644030	40.798578	73.117390
521.451542	46.438069	73.122394
521.198030	37.045721	73.127399
521.085389	36.084410	73.132404
520.261830	39.900645	73.137409
519.950403	43.073951	73.142414
518.925779	39.695526	73.147418
517.549699	36.363621	73.152423
517.013276	42.721727	73.157428
516.519417	36.360519	73.162433
516.543258	35.688108	73.167438
515.668330	36.027697	73.172442
514.913360	35.807320	73.177447
514.042600	45.872234	73.182452
513.660480	42.782529	73.187457
512.687606	35.021693	73.192462
511.699301	39.559561	73.197466
511.388773	43.864900	73.202471
510.792108	40.470347	73.207476
510.463088	45.682166	73.212481
509.496653	44.222959	73.217486
508.578484	48.524170	73.222490
508.193343	41.409257	73.227495
507.603016	54.315138	73.232500
506.534132	45.424801	73.237505
505.932025	39.216446	73.242510
505.381713	46.969123	73.247514
505.016514	37.999817	73.252519
504.730115	53.835949	73.257524
503.702250	44.453411	73.262529
503.094216	39.849654	73.267534
502.090884	50.008225	73.272538
501.434742	38.198058	73.277543
500.602760	53.725306	73.282548
499.776320	44.842083	73.287553
499.774560	37.353890	73.292558
499.167644	45.872469	73.297562
498.169379	42.235981	73.302567
497.108139	47.759966	73.307572
497.027889	35.957410	73.312577
496.952592	40.064441	73.317582
495.698891	50.065790	73.322586
494.980158	39.478189	73.327591
494.287421	44.963973	73.332596
493.756534	51.702801	73.337601
492.824059	34.709410	73.342606
492.037446	45.659727	73.347610
491.342994	41.443451	73.352615
491.094242	49.575420	73.357620
490.383787	47.432091	73.362625
489.884043	30.421812	73.367630
488.574765	47.094185	73.372634
488.461228	37.673239	73.377639
488.119566	43.637651	73.382644
487.259343	41.696365	73.387649
486.730397	39.372748	73.392654
485.604532	38.207012	73.397658
484.295568	35.982419	73.402663
483.923799	49.378573	73.407668
483.227256	37.305208	73.412673
482.681304	39.823640	73.417678
482.302300	45.705699	73.422682
482.421477	37.354630	73.427687
481.690914	41.104027	73.432692
480.768328	43.761299	73.437697
480.097065	37.770535	73.442702
478.970527	46.332470	73.447706
478.472062	36.075620	73.452711
477.471592	34.782687	73.457716
477.222696	39.473998	73.462721
476.442792	37.931478	73.467726
475.089071	33.421288	73.472730
474.951282	43.514518	73.477735
474.855360	44.389148	73.482740
474.100862	41.339848	73.487745
473.364260	33.360056	73.492750
472.501267	46.848651	73.497754
472.060624	43.896000	73.502759
470.901326	51.679468	73.507764
470.178802	38.414997	73.512769
469.551948	52.701708	73.517774
468.954949	51.328735	73.522778
468.990783	41.095572	73.527783
468.156330	47.116413	73.532788
467.065238	52.642012	73.537793
466.671625	40.064686	73.542798
465.908390	49.090688	73.547802
464.982253	54.828115	73.552807
464.261415	41.522377	73.557812
463.750588	45.150048	73.562817
463.371374	56.358732	73.567822
462.824006	50.058092	73.572826
462.059780	49.530145	73.577831
460.884532	47.112385	73.582836
460.463178	55.650297	73.587841
460.328266	46.622236	73.592846
459.144977	47.786777	73.597850
458.357338	44.572461	73.602855
457.917604	47.704717	73.607860
457.456891	48.129717	73.612865
456.916499	44.847630	73.617870
455.709649	54.653890	73.622874
455.149109	44.949364	73.627879
454.604972	46.125618	73.632884
454.310897	44.180879	73.637889
453.589646	40.213296	73.642894
452.699034	52.621430	73.647898
452.403909	39.954306	73.652903
451.045669	47.589712	73.657908
450.275744	55.799982	73.662913
450.098149	38.771501	73.667918
449.371547	54.034405	73.672922
449.349328	47.981247	73.677927
448.102270	47.358347	73.682932
447.323662	47.805609	73.687937
447.064068	45.383901	73.692942
445.973089	46.071726	73.697946
445.292696	45.557234	73.702951
444.940449	46.781763	73.707956
444.287312	50.559834	73.712961
443.584106	46.434847	73.717966
442.570350	50.885340	73.722970
442.301965	51.941978	73.727975
441.764417	38.285376	73.732980
440.542217	49.380788	73.737985
439.822463	53.112708	73.742990
439.432545	46.148370	73.747994
439.150890	41.451637	73.752999
438.033986	49.488541	73.758004
437.158321	52.956738	73.763009
436.769332	47.059777	73.768014
436.132923	50.188679	73.773018
435.894259	43.187632	73.778023
434.879919	52.307260	73.783028
433.900261	50.772925	73.788033
433.963479	45.846217	73.793038
432.635412	46.234374	73.798042
431.797034	42.531446	73.803047
431.526008	51.316625	73.808052
431.035099	50.823986	73.813057
430.798335	44.653634	73.818062
429.539309	41.487622	73.823066
429.065965	39.025860	73.828071
428.440759	47.408602	73.833076
427.032020	40.776885	73.838081
426.585687	35.587610	73.843086
426.054659	45.406044	73.848090
425.727217	49.772430	73.853095
425.440243	50.715344	73.858100
424.314937	43.327314	73.863105
423.616959	46.221616	73.868110
423.174241	51.585590	73.873114
422.307850	44.843815	73.878119
421.508120	50.425505	73.883124
420.667192	54.386456	73.888129
420.416296	43.792151	73.893134
419.546642	54.337855	73.898138
419.156663	46.324929	73.903143
418.074553	52.396280	73.908148
417.445807	46.512293	73.913153
417.287047	44.124983	73.918158
416.313432	63.189608	73.923162
415.320473	54.917955	73.928167
414.748005	54.925559	73.933172
414.194077	45.320911	73.938177
414.076652	51.746312	73.943182
413.446151	51.014160	73.948186
412.370853	48.063295	73.953191
411.809830	60.308554	73.958196
411.218798	56.444804	73.963201
410.083842	39.228266	73.968206
409.454143	52.088391	73.973210
409.149871	48.503786	73.978215
409.039344	56.799805	73.983220
408.007569	52.001828	73.988225
407.143985	51.010366	73.993230
406.127840	61.962592	73.998234
406.108860	46.089901	74.003239
404.908102	54.747266	74.008244
404.217904	48.470977	74.013249
403.961879	43.232461	74.018254
403.300313	49.000286	74.023258
402.246088	51.191315	74.028263
401.696889	44.353283	74.033268
400.711823	53.845124	74.038273
400.824614	45.212817	74.043278
399.965480	42.475083	74.048282
399.007137	45.978538	74.053287
398.432714	46.591966	74.058292
397.719789	48.939914	74.063297
397.315593	36.704896	74.068302
396.730734	42.058403	74.073306
395.860037	42.102490	74.078311
395.403235	40.620473	74.083316
394.611701	47.574294	74.088321
394.099886	42.018592	74.093326
392.697178	47.735783	74.098330
392.415218	51.040016	74.103335
392.158834	47.611776	74.108340
391.289160	47.382907	74.113345
390.283590	35.106526	74.118350
389.668023	45.165499	74.123354
389.243193	40.835338	74.128359
388.824092	45.066530	74.133364
388.130654	45.058723	74.138369
387.533570	38.210983	74.143374
386.845256	48.918595	74.148378
386.145688	42.205445	74.153383
385.133264	41.605113	74.158388
384.277470	42.580321	74.163393
384.321238	36.305361	74.168398
383.429943	45.518929	74.173402
382.487848	43.053022	74.178407
381.882778	38.492980	74.183412
381.055924	48.598237	74.188417
381.013891	36.879490	74.193422
379.838614	45.441343	74.198426
379.052678	35.432164	74.203431
378.365972	36.382009	74.208436
377.718303	43.450095	74.213441
377.894384	47.249009	74.218446
376.877507	47.333740	74.223450
376.074955	39.134272	74.228455
375.389111	40.033521	74.233460
374.767623	49.316058	74.238465
374.743707	33.545091	74.243470
373.192888	47.280489	74.248474
372.889866	46.852534	74.253479
372.148781	45.288094	74.258484
370.985009	42.691946	74.263489
370.632504	50.761607	74.268494
369.875403	48.857544	74.273498
369.782054	41.022857	74.278503
369.131121	37.092980	74.283508
368.046588	42.522957	74.288513
367.671020	42.455045	74.293518
366.780063	46.398752	74.298522
365.806470	49.977185	74.303527
365.450168	42.889247	74.308532
364.441960	58.301109	74.313537
364.271541	47.821715	74.318542
363.992753	51.335165	74.323546
362.667592	47.146893	74.328551
362.011685	42.186554	74.333556
361.134166	56.606255	74.338561
361.254412	36.630523	74.343566
360.251057	49.660570	74.348570
359.469345	40.816012	74.353575
359.274016	44.697758	74.358580
358.009051	55.249701	74.363585
357.318014	45.690573	74.368590
356.719354	45.134700	74.373594
356.009573	39.364566	74.378599
355.833622	49.594752	74.383604
355.175180	52.221016	74.388609
354.636601	34.513701	74.393614
353.320710	45.966247	74.398618
352.860943	44.274991	74.403623
352.349289	44.876849	74.408628
350.989815	49.765637	74.413633
350.714602	31.902827	74.418638
350.070451	48.614332	74.423642
349.894384	31.948316	74.428647
349.544106	29.340815	74.433652
348.239273	38.886770	74.438657
347.973619	37.323845	74.443662
347.155765	47.651586	74.448666
346.010702	41.660678	74.453671
345.515465	39.585595	74.458676
344.933286	35.066069	74.463681
344.624243	42.628942	74.468686
343.708873	48.096624	74.473690
343.101539	43.543260	74.478695
342.662454	35.188125	74.483700
342.083401	50.571019	74.488705
341.008972	37.332723	74.493710
340.159355	45.380680	74.498714
339.798504	47.752959	74.503719
339.728295	38.126448	74.508724
338.729299	44.796397	74.513729
337.876797	38.774642	74.518734
337.025103	48.768757	74.523738
335.624676	40.861685	74.528743
335.311334	41.430368	74.533748
334.410247	36.431845	74.538753
334.428245	35.946432	74.543758
333.831801	44.499633	74.548762
333.752256	51.485082	74.553767
332.784858	36.195607	74.558772
332.128732	52.718228	74.563777
331.212620	47.130780	74.568782
330.458944	44.071935	74.573786
329.252931	39.566675	74.578791
328.956319	43.119234	74.583796
328.537086	41.681702	74.588801
328.333116	34.107486	74.593806
326.976098	44.264124	74.598810
326.173416	44.105022	74.603815
326.064047	39.667838	74.608820
325.384487	49.897858	74.613825
324.936490	45.289147	74.618830
323.808925	47.540777	74.623834
323.631024	38.633126	74.628839
322.600281	41.895850	74.633844
321.573433	41.728320	74.638849
321.293398	32.497928	74.643854
320.944792	47.162900	74.648858
319.858572	33.590631	74.653863
319.186550	38.601674	74.658868
318.303158	43.881352	74.663873
318.072259	29.133643	74.668878
317.521115	41.773108	74.673882
316.448389	45.950788	74.678887
315.938852	32.480572	74.683892
315.247906	42.810168	74.688897
314.718759	33.214228	74.693902
313.844895	32.717991	74.698906
313.048663	46.290588	74.703911
312.694392	44.957816	74.708916
312.141190	36.135207	74.713921
311.194779	47.129948	74.718926
310.488954	51.734828	74.723930
309.923539	36.818089	74.728935
309.852169	36.361110	74.733940
308.558841	53.677516	74.738945
307.701961	42.276278	74.743950
307.093145	40.219305	74.748954
306.853232	36.698575	74.753959
306.590851	49.992146	74.758964
305.346882	51.639482	74.763969
304.913402	46.058703	74.768974
303.985201	50.460920	74.773978
303.064302	37.657040	74.778983
302.371304	43.813065	74.783988
301.636624	46.676979	74.788993
301.430927	35.629257	74.793998
300.952703	38.794473	74.799002
300.505774	33.925423	74.804007
299.706398	40.074748	74.809012
298.989070	41.281789	74.814017
298.398384	42.579026	74.819022
296.875839	35.736890	74.824026
296.527232	43.115273	74.829031
296.149141	34.871847	74.834036
295.470972	41.993690	74.839041
295.057705	40.291882	74.844046
294.158527	43.893170	74.849050
293.505142	35.627391	74.854055
293.104808	42.640305	74.859060
292.151673	44.340637	74.864065
291.218019	37.451957	74.869070
290.665360	34.096182	74.874074
289.969384	49.783121	74.879079
289.384127	34.301891	74.884084
288.973665	40.684106	74.889089
288.179183	45.676831	74.894094
287.714866	37.685250	74.899098
287.191035	37.431260	74.904103
286.232894	35.705914	74.909108
285.195983	42.599526	74.914113
284.624776	45.237132	74.919118
284.492609	49.556639	74.924122
283.734021	40.809345	74.929127
283.278781	48.619435	74.934132
282.272257	37.806573	74.939137
281.983957	44.918320	74.944142
280.917723	43.385232	74.949146
279.849174	46.601963	74.954151
279.378339	46.071465	74.959156
279.093573	39.226018	74.964161
278.609684	35.100825	74.969166
277.639164	44.844250	74.974170
276.480320	32.347951	74.979175
276.309812	45.557494	74.984180
276.002130	43.914548	74.989185
275.208559	42.722756	74.994190
274.224805	39.334774	74.999194
273.399865	43.857727	75.004199
273.234273	33.629885	75.009204
272.462173	44.223141	75.014209
271.507924	39.222079	75.019214
271.094865	39.779856	75.024218
270.845286	46.082821	75.029223
269.661627	34.367863	75.034228
268.736127	41.202725	75.039233
268.248301	44.330057	75.044238
267.802267	46.884643	75.049242
267.053048	38.850173	75.054247
266.322312	37.263620	75.059252
265.396447	42.226831	75.064257
265.405435	44.305222	75.069262
265.006537	40.658459	75.074266
264.049580	38.612834	75.079271
263.557495	38.379018	75.084276
262.081689	40.063325	75.089281
261.256474	32.813626	75.094286
260.647649	42.166692	75.099290
260.360744	33.702176	75.104295
259.971794	28.538487	75.109300
259.374032	44.510946	75.114305
258.835766	39.232291	75.119310
257.773844	42.518931	75.124314
257.394378	46.370111	75.129319
256.764374	37.402076	75.134324
255.859665	37.473709	75.139329
255.423585	42.231134	75.144334
255.010015	32.566332	75.149338
253.884082	40.626814	75.154343
253.096205	40.848548	75.159348
252.573610	43.848970	75.164353
251.669114	38.721723	75.169358
250.647970	35.666118	75.174362
249.874819	49.279201	75.179367
249.745721	34.239331	75.184372
249.277134	43.995794	75.189377
248.895344	41.563630	75.194382
248.217267	42.759698	75.199386
246.996005	34.204432	75.204391
246.731536	39.765499	75.209396
245.984926	45.181082	75.214401
245.469786	45.537530	75.219406
244.424147	46.457896	75.224410
243.705286	49.210502	75.229415
243.635319	44.221457	75.234420
242.484041	41.626535	75.239425
241.643084	43.654333	75.244430
241.144321	33.984192	75.249434
240.519729	52.605300	75.254439
240.336866	47.700476	75.259444
239.299324	42.562903	75.264449
238.642742	45.706101	75.269454
238.341693	43.986416	75.274458
237.520606	41.777228	75.279463
236.697036	43.338665	75.284468
235.462189	39.539746	75.289473
235.409487	45.297280	75.294478
234.940247	49.970115	75.299482
234.158969	44.055311	75.304487
233.383385	43.048309	75.309492
232.491533	50.942192	75.314497
232.477425	40.043702	75.319502
231.664714	41.188700	75.324506
230.272410	50.955222	75.329511
230.006293	41.844042	75.334516
229.237170	48.303934	75.339521
228.571778	40.273462	75.344526
228.552220	46.243317	75.349530
227.244418	49.785192	75.354535
227.006814	46.677234	75.359540
226.390121	47.278516	75.364545
225.539968	40.028073	75.369550
224.547021	41.291683	75.374554
223.806566	51.097796	75.379559
223.296644	36.301547	75.384564
223.118832	49.608441	75.389569
222.339163	45.051046	75.394574
221.477246	44.595512	75.399578
221.070353	53.263590	75.404583
220.585334	40.106439	75.409588
219.097418	52.256623	75.414593
219.084961	48.698068	75.419598
218.340009	49.378140	75.424602
217.179259	51.630375	75.429607
216.919042	40.999759	75.434612
215.889334	46.408441	75.439617
215.400233	45.614381	75.444622
215.138691	44.374068	75.449626
214.129841	46.485404	75.454631
213.742900	48.324154	75.459636
212.494635	45.503450	75.464641
212.529758	44.870237	75.469646
212.007799	39.770332	75.474650
210.678383	34.497965	75.479655
210.588235	40.438071	75.484660
209.718525	48.216473	75.489665
208.853593	47.534359	75.494670
208.219350	47.802576	75.499674
207.661580	34.272282	75.504679
207.403341	36.659754	75.509684
206.042340	41.192489	75.514689
205.282167	50.289016	75.519694
205.047287	38.195787	75.524698
204.143932	46.589790	75.529703
203.936727	29.457303	75.534708
203.064599	45.885059	75.539713
202.315625	40.498091	75.544718
202.042043	42.783939	75.549722
200.839793	40.501494	75.554727
200.298867	45.766038	75.559732
199.620968	42.151149	75.564737
198.828962	40.512886	75.569742
198.762129	30.813327	75.574746
197.477359	41.712232	75.579751
197.034162	41.557364	75.584756
195.948932	48.941225	75.589761
195.956751	30.650173	75.594766
195.207653	35.350277	75.599770
193.975966	32.269918	75.604775
193.468983	30.411193	75.609780
193.000270	39.428141	75.614785
192.943607	30.308816	75.619790
192.100756	40.601149	75.624794
191.014441	41.083352	75.629799
190.543112	34.403273	75.634804
189.933532	41.700270	75.639809
189.122438	35.873813	75.644814
188.310137	41.719320	75.649818
187.982991	37.911336	75.654823
187.400800	39.382273	75.659828
186.315102	31.611198	75.664833
185.402328	32.338531	75.669838
185.217593	43.911997	75.674842
184.667590	38.434975	75.679847
184.100854	28.807228	75.684852
182.947483	46.154967	75.689857
182.414498	43.185562	75.694862
182.106545	44.743660	75.699866
181.053687	41.377773	75.704871
180.472291	26.938272	75.709876
179.631081	28.716988	75.714881
179.039920	40.147099	75.719886
178.981104	41.676518	75.724890
177.883005	45.423089	75.729895
177.228731	44.300579	75.734900
176.656748	31.606714	75.739905
176.104671	39.162608	75.744910
175.041351	39.426701	75.749914
174.144693	37.983314	75.754919
174.192007	20.092809	75.759924
173.467836	43.763051	75.764929
172.998446	36.701072	75.769934
171.997666	41.824478	75.774938
171.480419	37.206347	75.779943
171.006865	35.233495	75.784948
169.551656	41.698705	75.789953
169.023350	46.473998	75.794958
168.351200	25.787338	75.799962
167.950047	44.443775	75.804967
167.797352	39.471080	75.809972
167.037426	48.525000	75.814977
166.441605	38.824623	75.819982
165.533740	38.469469	75.824986
164.268576	48.423893	75.829991
164.084348	42.062298	75.834996
163.686992	46.379930	75.840001
162.650478	41.830392	75.845006
162.049032	38.225403	75.850010
161.142732	40.460749	75.855015
161.111715	49.053136	75.860020
160.232456	41.059938	75.865025
159.169713	38.186035	75.870030
158.799750	45.274539	75.875034
158.358636	49.536076	75.880039
157.445000	39.569425	75.885044
156.406164	52.133710	75.890049
155.979350	40.887893	75.895054
155.613874	46.107127	75.900058
155.006206	58.124895	75.905063
154.001304	31.595473	75.910068
153.042131	48.877573	75.915073
152.640026	34.627095	75.920078
152.287709	44.506945	75.925082
151.642668	44.338536	75.930087
150.925338	49.222811	75.935092
149.929067	52.685097	75.940097
149.515545	40.998802	75.945102
149.133342	53.150918	75.950106
148.062082	51.025798	75.955111
147.475691	39.461676	75.960116
147.025513	50.137668	75.965121
146.341403	41.600889	75.970126
145.356369	37.923030	75.975130
144.473689	53.710713	75.980135
144.045143	42.689086	75.985140
143.338150	47.951733	75.990145
143.165286	42.854531	75.995150
142.297059	45.369222	76.000154
141.169408	46.419392	76.005159
141.324446	41.058616	76.010164
140.627724	54.132871	76.015169
139.497288	47.133714	76.020174
138.737221	40.668403	76.025178
138.143908	45.800970	76.030183
138.063063	40.175049	76.035188
137.013082	42.818060	76.040193
136.141101	52.309294	76.045198
135.570844	54.481612	76.050202
135.085065	44.189728	76.055207
134.547007	41.826651	76.060212
133.454660	58.311619	76.065217
132.729489	40.812321	76.070222
132.563312	32.979819	76.075226
131.584028	47.783184	76.080231
130.644988	38.493908	76.085236
130.048832	44.301817	76.090241
129.562708	41.936768	76.095246
129.509424	30.200935	76.100250
128.796188	53.643964	76.105255
128.059165	43.081503	76.110260
127.287857	45.145538	76.115265
126.076403	49.241340	76.120270
125.390905	40.515571	76.125274
124.803488	41.720870	76.130279
124.524595	40.007129	76.135284
123.908602	40.274034	76.140289
123.327496	44.215720	76.145294
122.339555	34.144252	76.150298
121.768143	47.986944	76.155303
121.132002	33.332277	76.160308
120.102551	45.625431	76.165313
119.195595	44.376081	76.170318
118.902783	33.047419	76.175322
118.423978	54.065737	76.180327
118.190085	39.490422	76.185332
117.406324	39.618510	76.190337
116.661317	41.251031	76.195342
116.280639	41.404730	76.200346
115.029192	47.265089	76.205351
114.259388	43.478813	76.210356
113.342277	47.847788	76.215361
113.179136	50.198031	76.220366
113.138358	45.330489	76.225370
111.806070	39.779537	76.230375
111.055411	40.194064	76.235380
110.475989	39.212592	76.240385
110.116429	45.488946	76.245390
108.962801	51.910836	76.250394
108.202134	56.453552	76.255399
107.953171	41.391820	76.260404
107.604745	55.385033	76.265409
106.701310	51.389846	76.270414
105.886261	38.819907	76.275418
104.899390	45.757639	76.280423
104.755015	52.866947	76.285428
104.272818	48.380426	76.290433
103.245866	38.655782	76.295438
102.778874	40.628726	76.300442
101.975654	54.407470	76.305447
101.166849	39.792951	76.310452
100.300297	43.874766	76.315457
99.684371	55.271003	76.320462
99.322405	49.264160	76.325466
98.528996	42.064642	76.330471
98.580466	48.564021	76.335476
97.316153	55.741527	76.340481
96.625673	51.108458	76.345486
96.408055	48.795212	76.350490
94.716342	48.703832	76.355495
94.584413	41.886085	76.360500
94.153230	53.541425	76.365505
93.631290	55.270840	76.370510
92.678952	44.425781	76.375514
91.895853	56.069433	76.380519
91.580352	54.639056	76.385524
90.958135	47.369667	76.390529
90.092804	46.017503	76.395534
89.353391	49.237018	76.400538
88.585985	48.189339	76.405543
88.164017	45.911832	76.410548
87.278394	37.246374	76.415553
86.281726	53.094817	76.420558
86.070459	52.242290	76.425562
85.312455	56.636364	76.430567
85.013837	41.935768	76.435572
84.358196	38.670579	76.440577
83.502566	53.399055	76.445582
83.266670	49.328971	76.450586
82.056134	40.360534	76.455591
81.189870	51.568046	76.460596
80.668829	45.870406	76.465601
80.045978	50.695481	76.470606
80.005505	45.383225	76.475610
78.784520	53.522008	76.480615
78.372002	45.572681	76.485620
78.138830	48.444989	76.490625
77.025432	54.530918	76.495630
76.224805	47.417707	76.500634
75.461579	42.610181	76.505639
74.640811	43.915775	76.510644
73.193526	53.497187	76.515649
72.829587	51.819089	76.520654
73.168259	46.965154	76.525658
72.298918	50.637446	76.530663
72.265696	47.854860	76.535668
71.172720	50.101084	76.540673
70.047286	42.572928	76.545678
69.884445	56.834570	76.550682
68.612713	63.385693	76.555687
67.855069	50.188487	76.560692
67.327351	53.459400	76.565697
67.066118	48.513483	76.570702
66.674360	48.475005	76.575706
65.677500	51.338217	76.580711
64.778691	44.456696	76.585716
64.457352	43.372583	76.590721
63.633360	42.297668	76.595726
63.446054	46.960258	76.600730
62.182701	53.193099	76.605735
62.067931	48.681110	76.610740
61.519026	43.554004	76.615745
60.387913	49.669569	76.620750
59.761232	50.617812	76.625754
58.905082	57.775976	76.630759
57.823963	39.767393	76.635764
57.137333	45.585012	76.640769
56.231654	51.658323	76.645774
56.172972	45.696160	76.650778
55.453735	48.113009	76.655783
55.342520	40.680151	76.660788
55.188795	38.698896	76.665793
54.036773	40.957696	76.670798
53.231610	42.159890	76.675802
52.759735	46.888359	76.680807
51.782660	43.270767	76.685812
50.949902	44.542013	76.690817
50.316354	46.137858	76.695822
49.907215	40.575336	76.700826
48.846036	42.825959	76.705831
48.453748	49.813962	76.710836
47.931014	46.879222	76.715841
47.283098	59.212481	76.720846
46.112902	39.985022	76.725850
45.287633	48.387116	76.730855
44.847533	50.458278	76.735860
44.553502	44.918397	76.740865
44.135482	49.155767	76.745870
43.455954	40.634065	76.750874
42.555722	52.107183	76.755879
42.115075	40.283330	76.760884
41.255661	48.875360	76.765889
39.999440	53.222751	76.770894
39.958820	37.099718	76.775898
39.105273	52.791317	76.780903
38.707076	41.756998	76.785908
37.926233	51.692582	76.790913
36.732346	47.611290	76.795918
36.789823	41.285279	76.800922
36.242544	39.995947	76.805927
35.625075	48.038498	76.810932
34.866064	38.431997	76.815937
34.007190	47.506455	76.820942
33.233847	36.297020	76.825946
32.328791	49.043415	76.830951
31.688530	41.297567	76.835956
30.977223	36.814493	76.840961
30.591202	49.123324	76.845966
30.275853	41.547995	76.850970
29.175041	57.424103	76.855975
28.603229	43.003617	76.860980
28.259612	45.108275	76.865985
27.270946	40.910690	76.870990
26.345407	45.457642	76.875994
25.618032	50.628957	76.880999
25.397014	41.367136	76.886004
24.972599	38.192813	76.891009
24.038868	49.037386	76.896014
23.617023	41.975746	76.901018
22.677805	43.956212	76.906023
22.034587	39.533238	76.911028
21.120583	43.851287	76.916033
20.338287	43.867217	76.921038
20.218895	43.958761	76.926042
19.727135	50.751335	76.931047
19.025851	50.828456	76.936052
18.057350	43.198035	76.941057
17.536147	39.356378	76.946062
17.237148	45.121646	76.951066
15.674641	43.593714	76.956071
15.175815	32.876634	76.961076
14.803986	45.854932	76.966081
14.192381	42.707311	76.971086
13.160605	29.087125	76.976090
12.271020	51.755669	76.981095
11.873777	35.717902	76.986100
11.479839	46.599381	76.991105
11.046869	50.317206	76.996110
10.441564	37.652366	77.001114
9.324637	48.724841	77.006119
9.060503	47.123871	77.011124
8.389643	40.481968	77.016129
7.182568	50.651104	77.021134
6.403438	39.857310	77.026139
6.077282	34.011927	77.031143
5.337565	45.774815	77.036148
5.017288	45.758061	77.041153
4.357524	51.803204	77.046158