Mon Mar 08 20:19:37 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.615911	89.033150	0.000000
-0.875639	99.268862	0.005005
-1.521197	34.965595	0.010010
-2.939168	6.851208	0.015014
-7.254080	-28.448677	0.020019
-13.093967	-14.932463	0.025024
-18.440736	-11.807391	0.030029
-22.812369	-7.019766	0.035034
-26.849089	-25.942813	0.040038
-30.721972	-3.302970	0.045043
-33.872204	-11.499878	0.050048
-37.701593	-22.541846	0.055053
-41.292841	-16.298694	0.060058
-44.766511	-7.682232	0.065062
-48.549178	-26.453392	0.070067
-52.566188	-20.041387	0.075072
-56.127091	-8.853370	0.080077
-60.188782	-10.455579	0.085082
-63.781544	-16.930897	0.090086
-67.342237	-11.731715	0.095091
-71.329320	-22.797349	0.100096
-74.868622	-1.852147	0.105101
-79.288310	-23.206977	0.110106
-82.481352	-10.144417	0.115110
-86.538028	-25.459524	0.120115
-90.093627	-9.863484	0.125120
-93.866030	-20.105533	0.130125
-97.815221	5.865823	0.135130
-101.655739	-6.311172	0.140134
-105.149195	-8.207378	0.145139
-108.897740	-17.142862	0.150144
-112.419920	-0.974994	0.155149
-116.888306	-7.922337	0.160154
-119.804275	-30.661781	0.165158
-123.950690	-7.569776	0.170163
-127.932253	-31.722322	0.175168
-131.493095	-2.793269	0.180173
-135.702122	-37.542086	0.185178
-139.708663	-4.908893	0.190182
-143.486763	-25.178607	0.195187
-147.034764	-13.834847	0.200192
-150.386819	-27.056280	0.205197
-154.402883	1.071881	0.210202
-157.874204	-26.080757	0.215206
-161.810040	-16.184118	0.220211
-165.424542	-2.622148	0.225216
-168.882377	-26.467144	0.230221
-173.219760	-16.889580	0.235226
-176.572664	-11.860587	0.240230
-180.608948	-27.869425	0.245235
-184.640168	-12.137443	0.250240
-187.818867	-24.248014	0.255245
-191.909495	-17.440869	0.260250
-195.471262	-8.975714	0.265254
-199.127645	-24.907964	0.270259
-203.214520	-8.539491	0.275264
-207.012452	-19.231405	0.280269
-210.629085	-12.788434	0.285274
-214.567316	5.612538	0.290278
-218.481929	-17.717975	0.295283
-222.052222	2.320952	0.300288
-225.238974	-14.573976	0.305293
-229.298843	-20.723768	0.310298
-233.266295	-18.452257	0.315302
-237.293849	-2.121576	0.320307
-240.624352	-27.297120	0.325312
-243.999648	3.275476	0.330317
-248.364773	-18.488236	0.335322
-251.876093	-14.277462	0.340326
-255.914127	-2.016457	0.345331
-259.485054	-21.106452	0.350336
-263.463406	-22.966025	0.355341
-267.125861	-5.952469	0.360346
-270.836841	-20.600231	0.365350
-274.551690	-4.726233	0.370355
-278.443626	-15.559130	0.375360
-281.935106	-27.923962	0.380365
-286.230842	-8.352597	0.385370
-289.177683	-17.701161	0.390374
-293.502823	-23.021656	0.395379
-297.116209	-5.588573	0.400384
-300.773737	-25.213405	0.405389
-304.907676	-14.725150	0.410394
-308.272474	-7.324104	0.415398
-312.248071	-11.077810	0.420403
-315.982798	-11.038264	0.425408
-319.526644	-15.982006	0.430413
-323.581179	-24.492995	0.435418
-327.266631	-26.377143	0.440422
-330.930911	-5.085275	0.445427
-334.862000	-15.225902	0.450432
-338.443889	-19.280516	0.455437
-342.791315	-10.360172	0.460442
-346.158454	-13.829366	0.465446
-349.993199	-26.014719	0.470451
-353.691030	-3.101213	0.475456
-357.268178	-33.128500	0.480461
-361.315777	-6.280152	0.485466
-364.830790	-19.968792	0.490470
-368.602949	-20.875591	0.495475
-372.600113	-17.277728	0.500480
-376.057319	-4.262519	0.505485
-380.017119	-17.761858	0.510490
-383.514024	-7.933381	0.515494
-387.143699	-17.075025	0.520499
-391.548278	-29.205586	0.525504
-394.693715	-1.985609	0.530509
-398.801599	-31.305233	0.535514
-402.871709	-2.636722	0.540518
-406.168155	-17.836109	0.545523
-410.376423	-21.751173	0.550528
-413.684508	-0.669020	0.555533
-417.818914	-19.466937	0.560538
-421.468821	-5.045906	0.565542
-424.683291	-10.373218	0.570547
-428.730343	-25.189372	0.575552
-432.353321	-8.284397	0.580557
-436.319603	6.578241	0.585562
-440.160778	-21.137699	0.590566
-443.822042	-5.674118	0.595571
-447.653353	-7.626245	0.600576
-451.219317	-18.808914	0.605581
-455.329360	6.824366	0.610586
-459.021342	-34.477642	0.615590
-462.585734	5.031299	0.620595
-466.680383	-22.686682	0.625600
-470.477201	9.744760	0.630605
-474.126235	-20.139983	0.635610
-477.803138	-16.202042	0.640614
-481.460880	-3.224048	0.645619
-485.046717	-18.329790	0.650624
-488.782708	-11.206666	0.655629
-493.112524	-4.146375	0.660634
-496.775373	-26.788060	0.665638
-500.310396	7.708241	0.670643
-504.030711	-4.578711	0.675648
-507.375721	-40.051301	0.680653
-511.299220	-19.255515	0.685658
-515.230133	10.512068	0.690662
-519.347547	-16.823743	0.695667
-523.048181	11.593575	0.700672
-526.330098	-27.031711	0.705677
-530.494025	6.874424	0.710682
-533.859110	-20.349723	0.715686
-538.023164	-18.885184	0.720691
-541.831755	-11.870223	0.725696
-545.526084	-21.357643	0.730701
-549.370201	-2.955466	0.735706
-553.048605	-20.351625	0.740710
-557.075414	0.213194	0.745715
-560.505176	-23.272951	0.750720
-564.388685	1.725097	0.755725
-568.235913	-7.294782	0.760730
-572.047450	-3.005633	0.765734
-575.465817	-29.702404	0.770739
-579.310767	14.544131	0.775744
-582.678743	-41.773459	0.780749
-586.663061	-47.516818	0.785754
-590.719200	-33.446967	0.790758
-594.471033	8.468338	0.795763
-598.126353	-22.377029	0.800768
-601.557204	-3.435299	0.805773
-605.607951	-32.246425	0.810778
-609.210829	-6.457448	0.815782
-613.221869	-11.989943	0.820787
-617.221535	-27.234326	0.825792
-620.796789	10.944117	0.830797
-624.845551	-13.835377	0.835802
-628.296318	-13.709833	0.840806
-631.706565	-6.436704	0.845811
-635.572292	-14.874811	0.850816
-639.045595	-27.797017	0.855821
-643.608380	-4.443769	0.860826
-647.036696	-13.137810	0.865830
-651.197710	-28.993385	0.870835
-654.598440	-25.438324	0.875840
-657.765110	-25.900556	0.880845
-662.066928	-7.390403	0.885850
-665.906503	-18.639382	0.890854
-669.506691	-24.876034	0.895859
-673.561470	-0.323522	0.900864
-677.012837	-27.807989	0.905869
-680.872085	-7.342307	0.910874
-684.514945	-15.431197	0.915878
-688.018844	-26.355331	0.920883
-692.148374	7.356312	0.925888
-696.105580	-34.263930	0.930893
-700.053702	-0.340029	0.935898
-703.468103	-22.920133	0.940902
-707.412836	-19.419979	0.945907
-711.137939	11.590624	0.950912
-714.659329	-26.642842	0.955917
-718.668817	4.701760	0.960922
-722.322887	-14.046185	0.965926
-725.956652	-17.019669	0.970931
-730.089843	-0.308694	0.975936
-733.003160	-19.304294	0.980941
-737.116279	-18.013114	0.985946
-741.223588	-3.352976	0.990950
-744.555437	-37.050167	0.995955
-748.634345	2.060366	1.000960
-752.517624	-24.408852	1.005965
-756.275840	3.864992	1.010970
-759.801562	-30.769372	1.015974
-763.718355	6.265416	1.020979
-767.595159	-23.208659	1.025984
-770.688933	-0.509415	1.030989
-775.018522	-13.431739	1.035994
-778.946077	-2.081636	1.040998
-782.329800	-5.684731	1.046003
-786.111657	-18.331905	1.051008
-789.939663	-4.802763	1.056013
-793.593201	-4.147869	1.061018
-797.477252	-22.463128	1.066022
-801.447916	-11.828291	1.071027
-805.218279	-1.990216	1.076032
-808.682582	-20.262174	1.081037
-812.787944	-9.914844	1.086042
-816.024279	-8.599688	1.091046
-819.633373	-14.377404	1.096051
-823.984353	6.439891	1.101056
-827.700522	-19.691656	1.106061
-831.535405	-12.126470	1.111066
-835.000772	-3.297390	1.116070
-838.747593	-17.854873	1.121075
-842.752903	3.340815	1.126080
-846.110127	-29.279917	1.131085
-850.397619	5.245599	1.136090
-853.909393	-17.249312	1.141094
-857.802179	4.880811	1.146099
-861.576730	-15.400796	1.151104
-864.872872	-8.131400	1.156109
-869.081829	1.020016	1.161114
-872.674137	-12.037330	1.166118
-876.247871	5.434345	1.171123
-880.456000	-19.006940	1.176128
-883.984338	-4.156890	1.181133
-887.753737	-26.172183	1.186138
-891.871847	-2.361376	1.191142
-895.189100	-14.317886	1.196147
-899.041968	-9.301012	1.201152
-902.547236	-0.582143	1.206157
-906.719051	-10.454633	1.211162
-910.367653	-7.271128	1.216166
-913.871520	-8.729264	1.221171
-918.227737	0.570348	1.226176
-921.501996	-8.445921	1.231181
-925.358989	-15.453170	1.236186
-929.324813	-17.018752	1.241190
-932.687645	-14.464330	1.246195
-936.743943	-8.974936	1.251200
-940.241608	-22.368963	1.256205
-944.188594	-9.118592	1.261210
-948.173745	-13.394757	1.266214
-951.431363	-26.943830	1.271219
-955.521087	-4.003143	1.276224
-958.870861	-22.606946	1.281229
-963.202705	-5.233117	1.286234
-966.400874	-37.607835	1.291238
-970.585900	-12.058037	1.296243
-974.399694	-12.794795	1.301248
-978.270772	-14.265067	1.306253
-982.022027	-21.703827	1.311258
-985.869553	8.489397	1.316262
-989.277875	-16.391783	1.321267
-993.075981	-10.804826	1.326272
-996.556116	-20.358859	1.331277
-1000.976654	-12.773861	1.336282
-1004.538176	-15.591316	1.341286
-1008.049046	-8.538104	1.346291
-1011.779787	-4.300608	1.351296
-1015.384576	-10.507594	1.356301
-1019.300231	-16.794153	1.361306
-1023.302275	-2.807936	1.366310
-1026.956466	-9.150494	1.371315
-1030.977300	-4.070278	1.376320
-1034.330366	-3.657016	1.381325
-1038.246464	-16.894084	1.386330
-1042.179530	-15.192817	1.391334
-1045.813056	-3.310639	1.396339
-1049.520614	-4.491584	1.401344
-1053.054257	-27.976026	1.406349
-1057.245592	-16.488703	1.411354
-1060.819640	11.841237	1.416358
-1064.531780	-24.325375	1.421363
-1068.360093	14.668258	1.426368
-1071.981299	-22.611931	1.431373
-1076.032757	-4.231028	1.436378
-1079.509276	-12.104626	1.441382
-1083.297553	-29.428654	1.446387
-1087.374651	13.751819	1.451392
-1090.700903	-22.949518	1.456397
-1094.370714	-16.018982	1.461402
-1098.225592	-8.410761	1.466406
-1102.255579	-31.008381	1.471411
-1106.537642	-10.972738	1.476416
-1110.084144	-24.681917	1.481421
-1113.789960	7.246949	1.486426
-1117.227542	-22.738205	1.491430
-1120.315656	-10.224151	1.496435
-1124.367528	-10.741242	1.501440
-1128.153069	-15.537837	1.506445
-1132.294525	-0.378069	1.511450
-1136.249698	-33.678400	1.516454
-1140.046969	-6.771240	1.521459
-1143.748410	-19.053791	1.526464
-1147.279636	-25.103607	1.531469
-1151.035663	-4.224877	1.536474
-1155.177528	-5.538000	1.541478
-1158.464627	-7.571294	1.546483
-1162.027528	-18.510457	1.551488
-1166.082432	-3.859606	1.556493
-1170.016956	-29.105650	1.561498
-1173.826894	-9.422955	1.566502
-1177.208281	-15.000006	1.571507
-1181.245008	-21.061922	1.576512
-1184.314594	-28.136360	1.581517
-1188.978590	-0.328843	1.586522
-1192.547030	-16.137854	1.591526
-1196.520438	-6.728712	1.596531
-1200.348293	-6.091020	1.601536
-1203.501646	-5.901843	1.606541
-1207.092373	-14.056557	1.611546
-1211.338623	-13.648339	1.616550
-1214.928392	-13.182749	1.621555
-1219.147741	-8.144565	1.626560
-1222.851962	5.601943	1.631565
-1226.706412	-4.506793	1.636570
-1229.444446	-23.540748	1.641574
-1233.374257	13.988698	1.646579
-1237.932649	1.266311	1.651584
-1241.264936	-28.648730	1.656589
-1245.351210	-8.738800	1.661594
-1248.862533	21.429374	1.666598
-1252.245014	-28.003328	1.671603
-1256.319855	6.729999	1.676608
-1259.793787	-27.793449	1.681613
-1263.752496	10.007132	1.686618
-1268.021366	-33.790036	1.691622
-1271.397902	-5.147738	1.696627
-1275.361973	-12.134090	1.701632
-1279.082673	-20.696774	1.706637
-1282.335539	-5.215401	1.711642
-1286.137431	-2.229117	1.716646
-1290.096952	-14.176825	1.721651
-1294.421543	8.401468	1.726656
-1297.740109	-12.039043	1.731661
-1302.002270	-9.538836	1.736666
-1305.138339	-41.333167	1.741670
-1308.524359	-44.170346	1.746675
-1312.883250	15.559989	1.751680
-1317.105160	-9.335474	1.756685
-1320.352478	-37.190448	1.761690
-1324.102903	8.629635	1.766694
-1328.110095	-13.051929	1.771699
-1331.538021	-29.178041	1.776704
-1335.294368	-20.027335	1.781709
-1338.992424	11.501644	1.786714
-1342.551673	-18.946137	1.791718
-1345.911613	-48.812372	1.796723
-1350.534228	10.502929	1.801728
-1354.324068	12.982815	1.806733
-1358.081695	19.049535	1.811738
-1361.986127	3.641479	1.816742
-1365.609980	-14.123075	1.821747
-1369.388405	-28.234617	1.826752
-1372.725300	-2.048905	1.831757
-1376.869554	-11.568550	1.836762
-1380.397237	-34.753755	1.841766
-1384.209264	-21.544817	1.846771
-1387.961749	13.321587	1.851776
-1391.689214	-4.118866	1.856781
-1395.810105	-20.144980	1.861786
-1399.618592	-17.647847	1.866790
-1402.329493	-50.106094	1.871795
-1406.776109	-6.640633	1.876800
-1410.621284	-9.948156	1.881805
-1414.349306	9.701294	1.886810
-1418.418231	-8.654177	1.891814
-1421.967349	-33.958263	1.896819
-1425.690339	-9.274880	1.901824
-1429.462991	-8.697683	1.906829
-1433.098576	-23.869526	1.911834
-1436.749366	3.579094	1.916838
-1440.607341	-15.319410	1.921843
-1444.477469	-39.887711	1.926848
-1448.046119	-11.395796	1.931853
-1452.106439	12.300977	1.936858
-1456.165559	-28.716316	1.941862
-1459.138238	-56.980807	1.946867
-1463.381406	-1.992997	1.951872
-1467.103448	-1.117942	1.956877
-1470.755506	-26.033342	1.961882
-1474.279997	-1.421086	1.966886
-1478.229149	-28.384476	1.971891
-1481.949351	-25.973881	1.976896
-1485.546312	-6.318535	1.981901
-1489.867040	-15.617331	1.986906
-1493.295575	-43.373595	1.991910
-1496.937552	-12.019014	1.996915
-1501.379499	-20.049302	2.006912
-1501.996714	-20.700472	2.016909
-1499.106840	-44.711514	2.026906
-1496.762326	-24.489677	2.036902
-1494.559605	-22.559505	2.046899
-1492.680395	-18.667143	2.056896
-1491.000797	-19.585077	2.066893
-1488.778017	-30.885521	2.076890
-1486.777572	-6.486233	2.086886
-1484.741840	-28.214880	2.096883
-1483.257175	-21.494805	2.106880
-1481.333020	-16.199737	2.116877
-1479.374663	-22.595047	2.126874
-1477.491712	-10.654406	2.136870
-1475.279563	-22.483629	2.146867
-1473.689053	-32.617105	2.156864
-1472.220554	-23.065177	2.166861
-1469.899392	-17.699472	2.176858
-1467.890601	-23.697089	2.186854
-1465.950245	-15.856374	2.196851
-1464.187931	-20.058865	2.206848
-1462.383967	-22.938650	2.216845
-1460.285630	-10.132549	2.226842
-1458.571401	-23.970819	2.236838
-1456.590174	-23.157687	2.246835
-1454.573256	-20.485673	2.256832
-1453.119857	-19.295938	2.266829
-1451.158758	-17.012847	2.276826
-1449.072726	-24.151678	2.286822
-1447.145500	-34.844277	2.296819
-1445.244878	-17.334761	2.306816
-1443.538214	-12.102721	2.316813
-1441.594236	0.557612	2.326810
-1439.392677	-37.991552	2.336806
-1438.035142	-1.858044	2.346803
-1436.176218	-20.594897	2.356800
-1433.723545	-22.669123	2.366797
-1431.915872	-21.984485	2.376794
-1430.616340	-27.868510	2.386790
-1428.608087	-26.001867	2.396787
-1426.464702	-25.884095	2.406784
-1424.820159	-6.341063	2.416781
-1422.689129	-26.292960	2.426778
-1420.740218	2.486445	2.436774
-1418.775484	-23.043677	2.446771
-1417.284915	-13.116316	2.456768
-1415.406167	-16.448534	2.466765
-1413.090659	-17.899244	2.476762
-1411.473849	-16.831953	2.486758
-1409.594871	-21.593042	2.496755
-1407.685637	-18.674815	2.506752
-1406.020071	-6.291960	2.516749
-1403.975910	-19.325719	2.526746
-1401.955184	-23.542696	2.536742
-1400.299656	-17.710376	2.546739
-1398.179899	-11.432939	2.556736
-1396.585525	-13.754950	2.566733
-1394.384359	-18.894427	2.576730
-1392.706404	-25.007952	2.586726
-1390.882967	-26.627738	2.596723
-1388.918182	-23.558927	2.606720
-1386.918715	-15.855486	2.616717
-1385.054027	-25.142350	2.626714
-1383.700881	-13.041021	2.636710
-1381.479863	-18.733097	2.646707
-1379.519925	-38.485465	2.656704
-1378.020945	-12.616415	2.666701
-1375.537838	-11.629365	2.676698
-1373.583575	-40.875899	2.686694
-1372.089331	-4.072689	2.696691
-1370.600053	-5.916841	2.706688
-1368.071161	-12.067111	2.716685
-1366.364160	-39.761541	2.726682
-1364.438614	0.253448	2.736678
-1362.383452	-25.973168	2.746675
-1360.966527	-16.502891	2.756672
-1358.823405	-11.766935	2.766669
-1357.077111	-18.551330	2.776666
-1354.961524	-8.471359	2.786662
-1353.248148	-29.744137	2.796659
-1351.504287	-21.780292	2.806656
-1349.625816	-28.034825	2.816653
-1347.488215	-34.090852	2.826650
-1345.679746	-30.258091	2.836646
-1343.779297	-19.820018	2.846643
-1341.965285	-24.302254	2.856640
-1340.028908	-13.489426	2.866637
-1338.258995	-11.876633	2.876634
-1336.334900	-10.337461	2.886630
-1334.714544	-11.896278	2.896627
-1332.934337	-13.603830	2.906624
-1330.427827	-13.859859	2.916621
-1329.012423	-14.902744	2.926618
-1326.840971	-15.760353	2.936614
-1325.061438	-19.922872	2.946611
-1323.315807	-6.736507	2.956608
-1321.309286	-14.183013	2.966605
-1319.226797	-13.835936	2.976602
-1317.476521	-16.075488	2.986598
-1315.829706	-15.993386	2.996595
-1313.813968	-9.244511	3.006592
-1312.125307	-14.106109	3.016589
-1310.032348	-0.193798	3.026586
-1308.030314	-11.463509	3.036582
-1306.281049	-11.929864	3.046579
-1304.570298	-5.095850	3.056576
-1302.537177	-20.756521	3.066573
-1300.590574	-6.247665	3.076570
-1298.657336	-14.018716	3.086566
-1297.077186	-5.005530	3.096563
-1295.103835	-6.560823	3.106560
-1293.135300	-9.288416	3.116557
-1291.295680	-2.779730	3.126554
-1289.163945	-15.450083	3.136550
-1287.767208	-15.474767	3.146547
-1285.793646	-9.825877	3.156544
-1283.851274	-17.704158	3.166541
-1281.858487	-15.538087	3.176538
-1279.984237	-16.226516	3.186534
-1278.047716	-17.534338	3.196531
-1276.327758	-10.671779	3.206528
-1274.412582	-9.971066	3.216525
-1272.550638	-12.526856	3.226522
-1270.469633	-7.468262	3.236518
-1268.681903	-14.303438	3.246515
-1267.279650	-18.683410	3.256512
-1264.972587	-9.202369	3.266509
-1263.139609	-12.680291	3.276506
-1261.356742	-16.854350	3.286502
-1259.375165	-15.406412	3.296499
-1257.647237	-10.488656	3.306496
-1255.648045	-7.651002	3.316493
-1253.753994	-13.399579	3.326490
-1251.694315	-14.491843	3.336486
-1250.020226	-8.158724	3.346483
-1247.865207	-10.003558	3.356480
-1246.584946	-14.177694	3.366477
-1244.400785	-1.669282	3.376474
-1242.383055	-15.641259	3.386470
-1240.438144	-6.861653	3.396467
-1239.053803	-12.827050	3.406464
-1237.121519	-15.264605	3.416461
-1234.824749	-16.110605	3.426458
-1233.152160	-8.375230	3.436454
-1231.290450	-15.722708	3.446451
-1229.335750	-15.422990	3.456448
-1227.122312	-11.511256	3.466445
-1225.735807	-19.314751	3.476442
-1223.838262	-17.491783	3.486438
-1221.903633	-7.297459	3.496435
-1219.901130	-15.903685	3.506432
-1218.109258	-10.868244	3.516429
-1216.256753	-16.100181	3.526426
-1214.137889	-9.749791	3.536422
-1212.607140	-5.804583	3.546419
-1210.647410	-7.810751	3.556416
-1209.051773	-13.246299	3.566413
-1206.763270	-25.125408	3.576410
-1204.725828	-8.384316	3.586406
-1203.019478	-24.399965	3.596403
-1201.448541	-14.175850	3.606400
-1199.403838	-14.390999	3.616397
-1197.409958	-4.512424	3.626394
-1195.339672	-15.385632	3.636390
-1193.970691	-10.710368	3.646387
-1191.849598	-15.682126	3.656384
-1189.660493	-9.196121	3.666381
-1188.021036	-11.212598	3.676378
-1186.421994	-16.495529	3.686374
-1184.197773	-11.928683	3.696371
-1182.655580	-8.932586	3.706368
-1180.682484	-20.731212	3.716365
-1178.684145	-7.409900	3.726362
-1176.575786	-18.263921	3.736358
-1174.997471	-8.967738	3.746355
-1173.242743	-5.118334	3.756352
-1171.447510	-12.674592	3.766349
-1169.092946	-12.779829	3.776346
-1167.459952	-5.810113	3.786342
-1165.439419	-1.436429	3.796339
-1163.598898	-16.546755	3.806336
-1161.863811	-19.230572	3.816333
-1159.899194	-10.376683	3.826330
-1158.028815	-14.580458	3.836326
-1156.322805	-16.934380	3.846323
-1154.570876	-19.404586	3.856320
-1152.280209	-11.120713	3.866317
-1150.407875	-13.242312	3.876314
-1148.557942	-22.790316	3.886310
-1146.658610	-19.448732	3.896307
-1144.691980	-5.970744	3.906304
-1143.175285	-5.008814	3.916301
-1141.253704	-12.108458	3.926298
-1139.022164	-18.621415	3.936294
-1137.534180	-17.904345	3.946291
-1135.581322	-15.011808	3.956288
-1133.998830	-13.687795	3.966285
-1131.751492	-8.613051	3.976282
-1129.839356	-7.226516	3.986278
-1128.096099	-16.700606	3.996275
-1126.121606	-12.253212	4.006272
-1124.042373	-12.958521	4.016269
-1122.465714	-13.537640	4.026266
-1120.334397	-6.568668	4.036262
-1118.826869	-14.413575	4.046259
-1116.667985	-13.788032	4.056256
-1115.044649	-0.885045	4.066253
-1112.923659	-1.224419	4.076250
-1111.353789	-12.014353	4.086246
-1109.479908	-11.891065	4.096243
-1107.231881	-15.716298	4.106240
-1105.349663	-7.417554	4.116237
-1103.515084	-4.873934	4.126234
-1101.797011	-25.590016	4.136230
-1099.858010	-13.034345	4.146227
-1098.057877	-14.227050	4.156224
-1096.222066	-4.858317	4.166221
-1094.233021	-11.943456	4.176218
-1092.398775	-11.084393	4.186214
-1090.345547	-6.872175	4.196211
-1088.490300	-14.592702	4.206208
-1086.944365	-6.933256	4.216205
-1085.042042	-24.972678	4.226202
-1082.942321	-11.811165	4.236198
-1081.057571	-12.883192	4.246195
-1079.229671	-9.425919	4.256192
-1077.303153	-11.545077	4.266189
-1075.397006	-13.222059	4.276186
-1073.717355	-8.045397	4.286182
-1071.808306	-16.472362	4.296179
-1069.745174	-8.470927	4.306176
-1067.929716	-6.629959	4.316173
-1066.256671	-10.792628	4.326170
-1063.914317	-16.192799	4.336166
-1062.293339	-15.732200	4.346163
-1060.831181	-13.496846	4.356160
-1058.508032	-24.992977	4.366157
-1056.518282	-18.827034	4.376154
-1054.857173	-4.673289	4.386150
-1052.878261	-13.690849	4.396147
-1050.820186	-14.615325	4.406144
-1049.217510	-10.545727	4.416141
-1047.576974	-10.173502	4.426138
-1045.481339	-6.926380	4.436134
-1043.667767	-12.663506	4.446131
-1041.648791	-11.410820	4.456128
-1039.675397	-16.627227	4.466125
-1037.854345	0.563897	4.476122
-1035.993187	-13.712870	4.486118
-1034.680835	-16.879997	4.496115
-1032.522644	-3.241494	4.506112
-1030.480408	-22.327929	4.516109
-1028.495732	-11.454636	4.526106
-1026.574032	-17.278511	4.536102
-1024.498439	-17.266358	4.546099
-1023.046376	-10.037084	4.556096
-1021.058308	-15.096362	4.566093
-1019.090912	-8.293690	4.576090
-1017.422574	-20.183976	4.586086
-1015.551234	-17.726687	4.596083
-1013.604417	-13.753153	4.606080
-1011.555099	-21.157316	4.616077
-1009.858232	-10.277445	4.626074
-1007.923361	-19.772628	4.636070
-1006.114975	-10.729409	4.646067
-1003.973766	-15.726328	4.656064
-1002.761784	-13.858266	4.666061
-1000.504062	-22.143584	4.676058
-998.201470	-26.403726	4.686054
-996.689403	-19.384547	4.696051
-994.789227	-1.613973	4.706048
-993.087224	-9.144149	4.716045
-990.756974	-14.859662	4.726042
-989.114391	-9.107047	4.736038
-987.420576	-10.213198	4.746035
-985.512047	-10.981079	4.756032
-983.752071	-14.688679	4.766029
-981.674751	-12.556385	4.776026
-979.740164	-12.423755	4.786022
-977.714932	-4.449323	4.796019
-976.078170	-11.572765	4.806016
-974.123451	-13.759504	4.816013
-972.228649	1.700539	4.826010
-970.268136	-17.713823	4.836006
-968.789331	-17.112010	4.846003
-966.663219	-12.905019	4.856000
-964.764123	-23.295964	4.865997
-962.813217	-8.460641	4.875994
-960.775736	-5.210455	4.885990
-959.227020	-22.536461	4.895987
-957.552799	-15.298462	4.905984
-955.444810	-4.080100	4.915981
-953.414461	-13.020554	4.925978
-951.568127	-16.359861	4.935974
-950.020990	-14.043294	4.945971
-947.842807	-16.272059	4.955968
-945.979110	-7.976526	4.965965
-944.405988	-5.886724	4.975962
-942.138284	-13.063668	4.985958
-940.121336	-14.794573	4.995955
-938.646573	-8.748260	5.005952
-936.783366	-5.602809	5.015949
-934.592013	-10.356653	5.025946
-932.700601	-33.992785	5.035942
-931.074817	4.469763	5.045939
-929.458866	-4.363368	5.055936
-927.221358	-23.948292	5.065933
-925.202628	9.809667	5.075930
-923.346667	-16.028040	5.085926
-921.559262	-8.724428	5.095923
-919.678640	-16.936752	5.105920
-918.074122	-16.768663	5.115917
-915.873467	-10.715250	5.125914
-913.966351	-17.452434	5.135910
-912.285480	-23.032465	5.145907
-910.344251	-24.018656	5.155904
-908.541670	-15.021791	5.165901
-906.790439	-8.724418	5.175898
-904.824319	-15.565760	5.185894
-902.707515	-27.339795	5.195891
-901.254550	-12.006409	5.205888
-899.075163	-20.879074	5.215885
-897.016814	-17.164833	5.225882
-895.070827	-16.459258	5.235878
-893.430520	-17.558366	5.245875
-891.719388	-19.753457	5.255872
-889.934404	-12.978344	5.265869
-887.745938	-18.222701	5.275866
-885.606002	-21.891510	5.285862
-884.290955	-1.123792	5.295859
-882.346090	-17.947878	5.305856
-880.597140	-8.860311	5.315853
-878.587796	-30.527516	5.325850
-876.360312	-10.366700	5.335846
-874.582698	-11.625106	5.345843
-872.969830	-23.233298	5.355840
-870.884058	-11.592911	5.365837
-868.891581	-27.002056	5.375834
-867.103411	-12.355347	5.385830
-865.520746	1.190626	5.395827
-863.741304	-2.605261	5.405824
-861.447527	-12.901354	5.415821
-859.885213	-6.257972	5.425818
-857.689734	-15.232645	5.435814
-855.747402	-6.845398	5.445811
-854.128604	-19.749179	5.455808
-852.318833	-5.769015	5.465805
-850.156737	-16.460858	5.475802
-848.353700	-16.608648	5.485798
-846.729277	-20.798129	5.495795
-844.694831	-11.312519	5.505792
-842.699886	-17.624774	5.515789
-841.086176	-3.032241	5.525786
-838.868775	-9.315325	5.535782
-837.043762	-24.198768	5.545779
-835.352970	3.143211	5.555776
-833.536854	18.911230	5.565773
-831.585439	12.882228	5.575770
-830.071855	-8.647312	5.585766
-827.807272	-11.638151	5.595763
-825.530663	-40.114939	5.605760
-824.092556	-11.898960	5.615757
-822.332200	-4.208858	5.625754
-820.236218	-28.741265	5.635750
-818.399124	-16.339549	5.645747
-816.577575	-5.987828	5.655744
-814.604302	-27.641337	5.665741
-812.683226	-9.240816	5.675738
-810.721563	-21.760459	5.685734
-809.170397	-27.801235	5.695731
-807.233667	-14.674958	5.705728
-805.333779	-12.853593	5.715725
-803.423962	-10.155979	5.725722
-801.535713	-30.918050	5.735718
-799.857734	-4.196063	5.745715
-797.634103	-13.936188	5.755712
-796.024877	-6.324534	5.765709
-793.888292	-15.990745	5.775706
-792.132865	-9.962352	5.785702
-790.226587	-11.370725	5.795699
-788.552762	-9.881083	5.805696
-786.498836	-16.265876	5.815693
-784.448633	-3.523994	5.825690
-782.724075	-11.600761	5.835686
-780.996188	9.516304	5.845683
-779.163833	-7.899178	5.855680
-777.223832	-12.464298	5.865677
-775.261033	-2.660868	5.875674
-773.173848	-23.683662	5.885670
-771.246069	-18.142244	5.895667
-770.073814	-1.538698	5.905664
-768.032518	-15.210969	5.915661
-765.486753	-23.499491	5.925658
-764.038384	-9.780412	5.935654
-761.974410	-1.464619	5.945651
-760.325660	-26.168657	5.955648
-758.350935	-13.266283	5.965645
-756.508814	-11.994555	5.975642
-754.589793	-12.347113	5.985638
-752.664864	-13.054274	5.995635
-750.865459	-15.361263	6.005632
-749.063218	1.290028	6.015629
-747.097422	-14.776319	6.025626
-745.226847	-12.380259	6.035622
-743.490112	-7.550336	6.045619
-741.626345	-9.420793	6.055616
-739.271560	-6.151648	6.065613
-737.813124	-14.558461	6.075610
-735.816449	1.059205	6.085606
-734.167211	-15.318097	6.095603
-732.077761	-0.867811	6.105600
-730.035477	-41.994661	6.115597
-728.252301	-4.559624	6.125594
-726.611296	5.129505	6.135590
-724.706255	-22.237941	6.145587
-722.608180	-8.396884	6.155584
-721.288540	-15.204244	6.165581
-718.788048	-14.582399	6.175578
-716.961890	4.415999	6.185574
-715.259483	6.848435	6.195571
-713.696887	-7.404105	6.205568
-711.255061	-15.447035	6.215565
-709.439798	-11.553258	6.225562
-707.657729	-28.220163	6.235558
-705.966629	1.311747	6.245555
-703.905946	-5.947164	6.255552
-701.962249	-15.585636	6.265549
-700.223229	-18.206600	6.275546
-698.230961	-21.899015	6.285542
-696.529096	-14.597335	6.295539
-694.692181	-10.184409	6.305536
-692.850802	-11.274461	6.315533
-690.808540	-11.081435	6.325530
-689.085856	-20.501432	6.335526
-687.041302	-0.462718	6.345523
-685.377287	-6.488306	6.355520
-683.086307	-39.432267	6.365517
-681.623390	-4.751599	6.375514
-679.681695	8.719797	6.385510
-677.497029	-23.144647	6.395507
-675.688492	-20.552314	6.405504
-673.775501	-28.250192	6.415501
-672.446753	-10.189063	6.425498
-670.428472	-9.842197	6.435494
-668.136042	-12.788393	6.445491
-666.493265	2.735903	6.455488
-664.683317	-2.684611	6.465485
-662.334359	-10.423731	6.475482
-660.915269	-25.128530	6.485478
-659.081705	-0.183767	6.495475
-657.289447	-10.434288	6.505472
-655.112218	-4.773157	6.515469
-653.236952	-17.204686	6.525466
-651.162341	-14.923249	6.535462
-649.535756	-6.324322	6.545459
-647.600146	-7.342558	6.555456
-645.867901	-16.910891	6.565453
-643.850771	-19.071021	6.575450
-641.916875	-19.807944	6.585446
-640.408458	-12.978962	6.595443
-638.435179	-14.606327	6.605440
-636.234856	-22.654805	6.615437
-634.509821	-33.295581	6.625434
-632.628580	-15.185340	6.635430
-631.004896	-5.498111	6.645427
-628.905901	-17.597499	6.655424
-626.923470	-21.812460	6.665421
-625.157649	-17.006041	6.675418
-623.106220	-20.488388	6.685414
-621.325969	-16.672626	6.695411
-619.510223	-7.889175	6.705408
-617.961347	-8.138279	6.715405
-615.968560	-13.107997	6.725402
-613.624979	-45.586654	6.735398
-612.200830	-2.307665	6.745395
-610.236701	-18.765206	6.755392
-608.017451	-21.724915	6.765389
-606.165458	-24.758571	6.775386
-604.865624	-14.405420	6.785382
-602.719868	-1.285485	6.795379
-600.749318	-12.570177	6.805376
-598.717777	-30.587312	6.815373
-597.061813	-21.440451	6.825370
-594.889937	-47.696279	6.835366
-593.299670	-24.569337	6.845363
-591.689670	-26.416505	6.855360
-589.599374	-15.790175	6.865357
-587.541810	-15.466882	6.875354
-585.710588	-17.163083	6.885350
-583.945034	-24.542101	6.895347
-581.993601	-30.892984	6.905344
-580.226243	-20.126644	6.915341
-578.204952	-28.236465	6.925338
-576.508415	-15.311579	6.935334
-574.338933	-21.506252	6.945331
-572.405193	-22.850949	6.955328
-570.773209	-22.123363	6.965325
-568.642038	-27.633007	6.975322
-567.204537	-16.041906	6.985318
-565.276712	-20.497554	6.995315
-563.497206	-20.442434	7.005312
-561.333933	-30.355856	7.015309
-559.373137	-18.553099	7.025306
-557.595678	-20.166486	7.035302
-555.787203	-19.786008	7.045299
-553.876855	-17.080377	7.055296
-551.817496	-25.943052	7.065293
-549.898710	-12.679456	7.075290
-548.100240	-27.571112	7.085286
-546.583583	0.283677	7.095283
-544.428545	-24.865858	7.105280
-542.428682	-26.576332	7.115277
-540.548433	-11.007774	7.125274
-538.854935	-28.205137	7.135270
-537.009632	-17.130703	7.145267
-535.224689	-30.836054	7.155264
-533.414323	-12.032329	7.165261
-531.487807	-22.299470	7.175258
-529.259660	-28.094552	7.185254
-527.373552	-13.761576	7.195251
-525.607081	-20.084456	7.205248
-524.204811	-15.575127	7.215245
-521.823459	-21.958324	7.225242
-519.819561	-39.039465	7.235238
-518.087748	-7.380862	7.245235
-516.507387	-27.758885	7.255232
-514.379341	-28.386198	7.265229
-512.647876	-24.242055	7.275226
-511.163352	-20.503702	7.285222
-508.908681	-14.534296	7.295219
-506.786542	-17.036327	7.305216
-505.046967	-29.921309	7.315213
-503.221969	-24.064842	7.325210
-501.776400	-21.127051	7.335206
-499.264236	-21.847277	7.345203
-497.329252	-25.801943	7.355200
-496.021900	-23.923582	7.365197
-493.864623	-15.677700	7.375194
-491.663816	-35.374845	7.385190
-490.145252	-13.052598	7.395187
-487.871658	-4.582139	7.405184
-486.334417	-21.509806	7.415181
-484.533361	-5.909594	7.425178
-482.579909	-14.242184	7.435174
-480.627155	-17.800229	7.445171
-478.767409	-24.880030	7.455168
-476.973520	-22.747803	7.465165
-474.869445	-20.344607	7.475162
-473.175326	-21.254666	7.485158
-471.627367	-17.419056	7.495155
-469.272600	-17.552045	7.505152
-467.637399	-20.923584	7.515149
-465.653279	-19.001716	7.525146
-463.651797	-18.847769	7.535142
-461.738959	-19.047534	7.545139
-460.221174	-14.596083	7.555136
-458.385768	-10.067465	7.565133
-456.230946	-19.180565	7.575130
-454.452626	-10.125750	7.585126
-452.480411	-36.395412	7.595123
-450.746054	-5.967059	7.605120
-448.637619	-45.032905	7.615117
-446.843909	-0.347581	7.625114
-445.034120	-16.728270	7.635110
-443.214249	-9.151564	7.645107
-440.992806	-8.584330	7.655104
-439.441676	-12.638699	7.665101
-437.725084	-8.915249	7.675098
-435.263982	-21.006002	7.685094
-433.784716	-16.510490	7.695091
-431.951903	-18.502074	7.705088
-430.048816	-16.684070	7.715085
-428.077456	-17.819937	7.725082
-426.544194	-26.413782	7.735078
-424.445417	-13.500893	7.745075
-422.465849	-4.893420	7.755072
-420.661157	-26.507149	7.765069
-418.608698	-15.547786	7.775066
-416.721300	-17.833847	7.785062
-414.919650	2.033967	7.795059
-413.187888	-25.305651	7.805056
-411.564464	-20.774726	7.815053
-409.233403	-15.169500	7.825050
-407.354389	-18.021020	7.835046
-405.747655	0.883251	7.845043
-403.989229	-11.537359	7.855040
-401.878828	-16.899876	7.865037
-399.883733	-15.360206	7.875034
-398.175105	-14.695262	7.885030
-396.274933	-17.502787	7.895027
-394.438264	-17.172475	7.905024
-392.431780	-11.883275	7.915021
-390.544677	-13.139860	7.925018
-388.461995	-19.055273	7.935014
-386.869400	-11.451705	7.945011
-385.131523	-16.855775	7.955008
-383.386602	-10.838005	7.965005
-380.926616	-18.436710	7.975002
-379.328060	-13.595493	7.984998
-377.730187	-16.266322	7.994995
-375.700663	-19.756021	8.004992
-373.543728	-6.686581	8.014989
-371.818799	-6.903638	8.024986
-370.040412	-10.875836	8.034982
-368.225037	-8.350662	8.044979
-365.871945	-14.097667	8.054976
-364.321568	3.974117	8.064973
-362.652293	-13.456133	8.074970
-360.587514	-9.946100	8.084966
-358.702359	-22.249547	8.094963
-356.679043	-4.846922	8.104960
-355.044681	-5.998396	8.114957
-353.074759	-4.435719	8.124954
-351.566899	-5.057026	8.134950
-349.381198	-4.311906	8.144947
-347.491731	-14.320394	8.154944
-345.482369	-11.054116	8.164941
-343.459133	-20.179273	8.174938
-341.702907	-16.948365	8.184934
-339.776393	-16.725507	8.194931
-338.149401	-8.836884	8.204928
-336.246478	-10.790647	8.214925
-334.485812	-20.265433	8.224922
-332.396429	-7.991958	8.234918
-330.496165	-15.594412	8.244915
-328.447379	-12.814383	8.254912
-326.840047	-3.116407	8.264909
-325.112311	-17.671407	8.274906
-323.249294	-14.037559	8.284902
-321.527670	-11.903146	8.294899
-319.087055	-16.558885	8.304896
-317.191107	-22.229705	8.314893
-315.669020	-14.344847	8.324890
-313.666018	-20.302739	8.334886
-311.654460	-10.978740	8.344883
-309.916407	-7.754377	8.354880
-308.329713	-11.800135	8.364877
-306.120663	-17.119904	8.374874
-304.312234	-10.059117	8.384870
-302.519351	-11.286384	8.394867
-300.347927	-7.265985	8.404864
-298.787018	-14.981603	8.414861
-296.985931	-13.808746	8.424858
-294.929750	-9.160509	8.434854
-292.938395	-19.057335	8.444851
-291.299735	-21.816719	8.454848
-289.485913	-6.669915	8.464845
-287.214495	-1.760782	8.474842
-285.363382	-13.596152	8.484838
-283.688792	-20.368386	8.494835
-281.632079	-8.847493	8.504832
-279.831791	-13.457821	8.514829
-277.831765	-23.877037	8.524826
-276.341528	-16.083377	8.534822
-274.449892	-6.910714	8.544819
-272.240373	-24.326093	8.554816
-270.906211	-17.890589	8.564813
-268.643196	-12.018581	8.574810
-266.418143	-11.120202	8.584807
-264.879489	-20.065328	8.594803
-263.318039	-2.195747	8.604800
-261.260527	-13.468820	8.614797
-259.022924	-14.219178	8.624794
-257.433890	-7.371211	8.634791
-255.631435	-4.940196	8.644787
-253.791473	-1.649955	8.654784
-251.398381	-14.545960	8.664781
-250.007533	-15.162737	8.674778
-247.952073	-23.007781	8.684775
-246.447005	-2.813016	8.694771
-244.414894	-24.262443	8.704768
-242.418188	-19.007865	8.714765
-240.249949	-12.307594	8.724762
-238.616956	-21.416174	8.734759
-236.778751	-21.229661	8.744755
-235.030271	-20.004153	8.754752
-232.844857	-12.147740	8.764749
-231.033193	-21.924267	8.774746
-229.509052	-16.831081	8.784743
-227.453952	-16.274992	8.794739
-225.428818	-7.074648	8.804736
-223.181761	-16.301752	8.814733
-221.780038	-16.986560	8.824730
-220.088157	-20.491715	8.834727
-217.880834	-22.135568	8.844723
-215.967314	-21.506351	8.854720
-214.232070	-16.977339	8.864717
-212.289844	-24.177481	8.874714
-210.387724	-29.463967	8.884711
-208.629804	-19.914672	8.894707
-206.713728	-27.859010	8.904704
-204.940155	-22.316173	8.914701
-202.941110	-13.544253	8.924698
-201.117805	-24.372552	8.934695
-199.222770	-19.903766	8.944691
-197.399119	-10.316001	8.954688
-195.550749	-16.051770	8.964685
-193.611166	-17.596035	8.974682
-191.519009	-25.688455	8.984679
-190.102775	-19.614924	8.994675
-187.908859	-22.260760	9.004672
-186.232757	-15.914504	9.014669
-184.286245	-28.972843	9.024666
-182.540559	-11.393116	9.034663
-180.442986	-15.147713	9.044659
-178.344386	-17.953583	9.054656
-176.674438	-15.596093	9.064653
-174.763111	-19.313070	9.074650
-173.075754	-12.578623	9.084647
-171.231960	-24.357484	9.094643
-169.118288	-14.178123	9.104640
-167.542226	-9.317373	9.114637
-165.000300	-25.593685	9.124634
-163.794664	-35.091885	9.134631
-161.996678	-17.773109	9.144627
-159.941226	-29.628363	9.154624
-157.960925	-11.042432	9.164621
-155.826326	-23.649220	9.174618
-154.314374	-28.203973	9.184615
-152.281267	-15.840822	9.194611
-150.275948	-12.884763	9.204608
-148.580502	-16.693580	9.214605
-146.703640	-31.400150	9.224602
-144.740637	-19.444204	9.234599
-143.183861	-22.968799	9.244595
-141.178675	-18.370707	9.254592
-139.101748	-22.979290	9.264589
-137.167176	-13.196030	9.274586
-135.510491	-24.315050	9.284583
-134.080381	-18.692090	9.294579
-131.729869	-27.574063	9.304576
-129.448314	-28.907595	9.314573
-127.873086	-39.239966	9.324570
-126.076515	-28.841039	9.334567
-124.040136	-26.901959	9.344563
-122.395402	-24.571987	9.354560
-120.490240	-31.243545	9.364557
-118.611445	-20.025670	9.374554
-116.478533	-30.327031	9.384551
-114.826389	-21.888081	9.394547
-113.164505	-6.072700	9.404544
-111.122205	-23.848103	9.414541
-109.062295	-19.137142	9.424538
-107.265991	-30.043171	9.434535
-105.544431	-19.763296	9.444531
-103.460365	-19.589068	9.454528
-101.519970	-27.646152	9.464525
-99.927975	-19.889130	9.474522
-97.787283	-25.549895	9.484519
-96.266541	-19.066687	9.494515
-94.026426	-25.444322	9.504512
-92.517478	-26.815595	9.514509
-90.296517	-27.409994	9.524506
-88.431832	-26.081347	9.534503
-86.658959	-19.477315	9.544499
-84.868355	-21.278761	9.554496
-82.853046	-22.055067	9.564493
-81.136732	-18.073952	9.574490
-79.297286	-26.208068	9.584487
-77.414917	-14.586537	9.594483
-75.304453	-23.018085	9.604480
-73.725738	-32.730499	9.614477
-71.539220	-29.785916	9.624474
-69.507294	-25.945142	9.634471
-67.873889	-32.428052	9.644467
-66.373226	-28.158331	9.654464
-64.314943	-30.962407	9.664461
-62.070497	-25.871924	9.674458
-60.259649	-20.980669	9.684455
-58.563948	-25.855190	9.694451
-56.666876	-21.312405	9.704448
-54.731779	-25.200440	9.714445
-52.882418	-25.680263	9.724442
-51.014099	-26.587821	9.734439
-49.240829	-23.496770	9.744435
-47.289802	-29.239334	9.754432
-45.406180	-22.496631	9.764429
-43.354934	-23.967017	9.774426
-41.747521	-20.058495	9.784423
-39.643510	-22.754591	9.794419
-37.932774	-21.745535	9.804416
-35.969930	-23.020245	9.814413
-34.108904	-26.026501	9.824410
-32.239335	-21.048280	9.834407
-30.576221	-25.145527	9.844403
-28.369937	-25.248084	9.854400
-26.687776	-22.496144	9.864397
-24.760474	-27.417062	9.874394
-22.754081	-28.019801	9.884391
-21.356784	-17.489194	9.894387
-19.087857	-23.790840	9.904384
-17.219643	-21.348029	9.914381
-15.606298	-21.024432	9.924378
-13.321026	-31.048456	9.934375
-11.295457	-27.258719	9.944371
-9.789805	-27.099508	9.954368
-7.676345	-23.667976	9.964365
-6.006203	-33.025485	9.974362
-4.382091	-19.308610	9.984359
-3.322743	4.593570	9.994355
-2.637883	66.217678	10.004352
-0.998255	141.291725	10.014349
0.000000	219.894039	10.019354
0.348405	262.443698	10.024359
1.102575	301.473839	10.029363
1.835600	350.455959	10.034368
2.145009	387.042158	10.039373
2.421034	412.838437	10.044378
2.775505	440.071406	10.049383
2.679648	464.686086	10.054387
3.406606	483.595258	10.059392
3.205696	506.580493	10.064397
3.713203	525.346534	10.069402
3.679429	539.364175	10.074407
3.693313	549.912939	10.079411
4.069635	553.862928	10.084416
4.111088	572.968288	10.089421
4.417736	584.287213	10.094426
4.395521	596.748242	10.099431
4.390904	594.821970	10.104435
4.582688	587.461907	10.109440
4.309089	602.739961	10.114445
4.389924	601.454472	10.119450
4.491504	606.790243	10.124455
4.646529	607.252743	10.129459
4.803112	620.085806	10.134464
4.988075	623.061849	10.139469
4.868290	629.918382	10.144474
5.153359	638.339285	10.149479
4.923963	641.878150	10.154483
5.017765	646.724758	10.159488
4.964226	660.001368	10.164493
4.982361	664.109442	10.169498
5.285504	656.192279	10.174503
5.417636	656.973815	10.179507
5.455778	655.318250	10.184512
5.116224	656.367406	10.189517
5.360478	651.752224	10.194522
5.531079	656.848352	10.199527
5.061323	664.910289	10.204531
5.664881	670.727395	10.209536
5.442155	672.751370	10.214541
5.472690	659.300158	10.219546
5.557074	668.595158	10.224551
5.440685	669.078877	10.229555
5.627084	674.790640	10.234560
5.359544	693.160144	10.239565
5.605709	702.834628	10.244570
5.570519	704.267313	10.249575
5.458275	737.750482	10.254579
5.884287	699.565302	10.259584
5.594144	737.449626	10.264589
5.592245	711.765089	10.269594
6.114541	752.328349	10.274599
6.137017	737.585276	10.279603
6.466216	766.298885	10.284608
6.004658	747.205017	10.289613
6.062374	771.130262	10.294618
6.348249	743.963192	10.299623
6.102845	775.435039	10.304627
6.521384	764.533223	10.309632
6.124723	757.585472	10.314637
6.011533	781.454418	10.319642
6.419729	764.126719	10.324647
6.052748	760.082074	10.329651
6.311410	786.422672	10.334656
6.551467	783.258886	10.339661
6.546578	803.840058	10.344666
6.667695	802.898203	10.349671
6.699669	815.499007	10.354675
6.905173	804.541257	10.359680
7.053569	826.100934	10.364685
7.423916	804.750176	10.369690
7.264893	815.817136	10.374695
7.270626	817.848845	10.379699
7.138867	828.115118	10.384704
6.919494	805.413957	10.389709
7.185375	803.633742	10.394714
6.879190	828.995359	10.399719
6.897617	816.703396	10.404723
7.080413	825.422992	10.409728
6.852457	821.863925	10.414733
6.826563	827.625380	10.419738
7.011541	830.582540	10.424743
7.254625	851.067456	10.429747
7.210483	852.561507	10.434752
7.140497	872.344194	10.439757
7.203236	866.564160	10.444762
7.555263	857.013275	10.449767
7.555458	867.435145	10.454771
7.559496	865.896958	10.459776
7.358966	871.112282	10.464781
7.660797	884.832302	10.469786
7.932299	897.861744	10.474791
7.651628	912.795902	10.479795
7.946226	896.968485	10.484800
7.804657	915.958413	10.489805
8.125453	909.539541	10.494810
8.169840	911.926215	10.499815
8.102167	907.335476	10.504819
8.437694	909.284631	10.509824
8.207153	921.914784	10.514829
8.323477	908.599467	10.519834
8.313815	919.226371	10.524839
8.208834	915.923629	10.529843
8.573810	910.079599	10.534848
8.138097	920.555267	10.539853
8.130862	934.870252	10.544858
8.322748	917.543757	10.549863
8.252135	913.726184	10.554867
8.190662	915.699240	10.559872
8.008876	941.613638	10.564877
8.254803	941.836149	10.569882
8.417454	944.256004	10.574887
8.521563	956.812309	10.579891
8.756881	964.517523	10.584896
8.765554	951.047450	10.589901
8.685866	969.571842	10.594906
9.261350	971.304538	10.599911
8.609818	954.016335	10.604915
8.972097	978.039998	10.609920
8.772738	966.746159	10.614925
9.322268	1013.941582	10.619930
9.175636	990.272899	10.624935
9.050785	1021.986248	10.629939
9.556461	1003.054730	10.634944
9.086000	1008.478738	10.639949
9.268844	1004.855678	10.644954
9.165797	996.165761	10.649959
9.249298	1022.761808	10.654963
9.500026	996.074534	10.659968
8.940433	1018.703054	10.664973
9.654620	1011.600073	10.669978
9.252613	999.234669	10.674983
9.300736	1026.650070	10.679987
9.705158	1000.326203	10.684992
9.381097	1012.253841	10.689997
9.894378	1039.497301	10.695002
9.913343	1036.211031	10.700007
9.865234	1037.574847	10.705011
10.311358	1040.135583	10.710016
9.981358	1045.101962	10.715021
10.224101	1002.280600	10.720026
9.888090	1023.720718	10.725031
9.717521	1027.726531	10.730035
10.025353	1038.501577	10.735040
10.028637	1057.746128	10.740045
9.959343	1043.334350	10.745050
10.028624	1049.741454	10.750055
10.368271	1050.366911	10.755059
10.342858	1056.625120	10.760064
9.720614	1061.239149	10.765069
10.028756	1055.587054	10.770074
10.472423	1055.733872	10.775079
10.420778	1068.592661	10.780083
10.423111	1089.278741	10.785088
11.053598	1087.478184	10.790093
10.940892	1072.552905	10.795098
10.836453	1075.792823	10.800103
10.477481	1064.503865	10.805107
10.794743	1076.950582	10.810112
10.844938	1088.952629	10.815117
10.927007	1088.259837	10.820122
11.086288	1094.561142	10.825127
10.785255	1087.552247	10.830131
11.002484	1096.894142	10.835136
10.932801	1092.891869	10.840141
11.006708	1088.606496	10.845146
11.175938	1112.979720	10.850151
11.016230	1079.657266	10.855155
11.126804	1105.746098	10.860160
11.130263	1091.581288	10.865165
11.144774	1112.230766	10.870170
11.521535	1089.771543	10.875175
11.146900	1076.431879	10.880179
11.478956	1099.612163	10.885184
11.655602	1078.377056	10.890189
11.686423	1093.955576	10.895194
11.550434	1090.982593	10.900199
11.424802	1095.642001	10.905203
11.609052	1093.575151	10.910208
11.467704	1095.040576	10.915213
11.611652	1090.203135	10.920218
11.981546	1112.522695	10.925223
11.215022	1092.674341	10.930227
11.894852	1124.142869	10.935232
11.770658	1126.622700	10.940237
11.760309	1114.967436	10.945242
11.988997	1146.232004	10.950247
11.914027	1130.597321	10.955251
12.433210	1128.044957	10.960256
12.463308	1148.401839	10.965261
11.912687	1124.272246	10.970266
12.419922	1128.775527	10.975271
12.280273	1163.263841	10.980275
12.506699	1124.301975	10.985280
12.311788	1135.723411	10.990285
12.201215	1123.702501	10.995290
12.512422	1149.013508	11.000295
12.149100	1143.080547	11.005299
12.353817	1122.280870	11.010304
12.259859	1142.782112	11.015309
12.186875	1138.870239	11.020314
12.690859	1164.257758	11.025319
13.041515	1165.400285	11.030323
12.673718	1135.556559	11.035328
12.639193	1158.074737	11.040333
12.915461	1177.402063	11.045338
12.993119	1172.346508	11.050343
12.886080	1175.839176	11.055347
13.060006	1184.506787	11.060352
13.044261	1163.839987	11.065357
13.227989	1177.298423	11.070362
13.578540	1173.692727	11.075367
12.976585	1172.093468	11.080371
13.151003	1162.830913	11.085376
13.178460	1181.051477	11.090381
13.198904	1168.159648	11.095386
13.162688	1171.142698	11.100391
13.218743	1173.040273	11.105395
13.720117	1153.286071	11.110400
13.654147	1186.620968	11.115405
13.630848	1182.310071	11.120410
13.611853	1165.338618	11.125415
13.395292	1183.781035	11.130419
13.667933	1170.550931	11.135424
13.540056	1173.698414	11.140429
13.374773	1184.418143	11.145434
13.526104	1183.129245	11.150439
13.552083	1174.126903	11.155443
13.694507	1191.244191	11.160448
14.132416	1174.355970	11.165453
13.267929	1192.433385	11.170458
13.883469	1198.570498	11.175463
14.225259	1186.143066	11.180467
14.084874	1221.744974	11.185472
13.790888	1211.412218	11.190477
14.436724	1214.616076	11.195482
14.493334	1205.851682	11.200487
13.871156	1216.473998	11.205491
14.477960	1216.210018	11.210496
14.239005	1199.835010	11.215501
14.351107	1224.840437	11.220506
14.534099	1198.906348	11.225511
14.402675	1224.612943	11.230515
14.663584	1205.838476	11.235520
14.431073	1207.933471	11.240525
14.356777	1204.778734	11.245530
14.629857	1209.300466	11.250535
14.438946	1214.656306	11.255539
14.325698	1210.367632	11.260544
14.583664	1216.921336	11.265549
14.533337	1206.912422	11.270554
14.986003	1214.316595	11.275559
15.080480	1248.841886	11.280563
15.077369	1207.804842	11.285568
14.994629	1212.533140	11.290573
14.760412	1241.764918	11.295578
15.172694	1225.653442	11.300583
14.950577	1234.095666	11.305587
15.128744	1254.757091	11.310592
15.398209	1245.116619	11.315597
14.891210	1251.855430	11.320602
15.225589	1238.385180	11.325607
15.159260	1253.850056	11.330611
15.570610	1244.063950	11.335616
15.354644	1271.419433	11.340621
15.461492	1229.503760	11.345626
15.210967	1255.207329	11.350631
15.282787	1235.674496	11.355635
15.483700	1251.334867	11.360640
15.508430	1228.266097	11.365645
15.069097	1271.198261	11.370650
15.737452	1243.975559	11.375655
15.509885	1286.452939	11.380659
15.740576	1253.312247	11.385664
15.794957	1249.154522	11.390669
16.010279	1304.364762	11.395674
16.112781	1271.490484	11.400679
16.245495	1279.999143	11.405683
15.859267	1285.431894	11.410688
16.221090	1277.033520	11.415693
15.993703	1270.132638	11.420698
16.153411	1280.709138	11.425703
16.532126	1276.179548	11.430707
16.454080	1259.064437	11.435712
16.243371	1279.680689	11.440717
16.356978	1277.856896	11.445722
16.734648	1272.456983	11.450727
16.416814	1277.380498	11.455731
16.588826	1290.183309	11.460736
16.780166	1260.199679	11.465741
16.619526	1284.747234	11.470746
16.708896	1286.500736	11.475751
16.651532	1278.560312	11.480755
16.550386	1263.298674	11.485760
16.457474	1295.714012	11.490765
16.614636	1280.685549	11.495770
16.678096	1266.454227	11.500775
16.347697	1289.186960	11.505779
16.763729	1267.402454	11.510784
16.954672	1301.855714	11.515789
17.252628	1298.159027	11.520794
17.213586	1278.415158	11.525799
17.060199	1290.746315	11.530803
17.270276	1277.795756	11.535808
17.165654	1284.986075	11.540813
16.995710	1279.436957	11.545818
17.512641	1284.011283	11.550823
17.293898	1305.748507	11.555827
17.319803	1312.818670	11.560832
17.657092	1304.769553	11.565837
17.312954	1301.665719	11.570842
17.471250	1310.701758	11.575847
17.777913	1307.317499	11.580851
17.647625	1307.973768	11.585856
18.089289	1303.828374	11.590861
17.432559	1293.119748	11.595866
17.951843	1290.447490	11.600871
17.617546	1308.033621	11.605875
17.993199	1295.875090	11.610880
17.983151	1296.037509	11.615885
17.753579	1303.490621	11.620890
18.230499	1298.716698	11.625895
17.725053	1303.085087	11.630899
17.821996	1315.463071	11.635904
17.793265	1323.063934	11.640909
17.679509	1321.997080	11.645914
18.339903	1309.310565	11.650919
17.772952	1297.608312	11.655923
18.012485	1312.458330	11.660928
18.159955	1312.117801	11.665933
17.900307	1319.719223	11.670938
18.283605	1314.392515	11.675943
18.398922	1330.850383	11.680947
18.671596	1323.724634	11.685952
18.740786	1332.730743	11.690957
18.243618	1324.554509	11.695962
18.878677	1320.794586	11.700967
18.630201	1328.652856	11.705971
18.836294	1332.791066	11.710976
18.917925	1331.541658	11.715981
18.973411	1314.662231	11.720986
18.769770	1313.515096	11.725991
18.577258	1315.147978	11.730995
19.000025	1317.542178	11.736000
19.037681	1330.133062	11.741005
18.851863	1336.355474	11.746010
19.209697	1340.150933	11.751015
19.194248	1327.627393	11.756019
19.120064	1319.388426	11.761024
19.364956	1337.172376	11.766029
19.091551	1333.694548	11.771034
19.113098	1314.221669	11.776039
19.141805	1335.462145	11.781043
19.410502	1334.364252	11.786048
19.030408	1326.804867	11.791053
19.401556	1333.755318	11.796058
19.188822	1325.513214	11.801063
18.994662	1332.098083	11.806067
18.707879	1339.069897	11.811072
19.151211	1347.136383	11.816077
19.089244	1360.899112	11.821082
19.398383	1350.086851	11.826087
19.631701	1357.171263	11.831091
19.577716	1362.522664	11.836096
19.860089	1359.120190	11.841101
19.898267	1359.872596	11.846106
20.264039	1345.507820	11.851111
19.790615	1370.092793	11.856115
19.845348	1338.396105	11.861120
19.946931	1369.526885	11.866125
19.907891	1358.372751	11.871130
20.369591	1360.711863	11.876135
20.164556	1365.355636	11.881139
20.591343	1386.222027	11.886144
20.988647	1337.587479	11.891149
20.273116	1368.069556	11.896154
20.923221	1345.211519	11.901159
20.537454	1354.835844	11.906163
20.357080	1358.944238	11.911168
20.643212	1348.619782	11.916173
20.454782	1351.430024	11.921178
20.846952	1342.493752	11.926183
20.779925	1344.280091	11.931187
20.855851	1346.765888	11.936192
20.785578	1347.332160	11.941197
20.601406	1355.967103	11.946202
20.957455	1353.880699	11.951207
20.502902	1352.325718	11.956211
20.951382	1351.374194	11.961216
20.879961	1358.589215	11.966221
20.796507	1357.028661	11.971226
20.988363	1349.597238	11.976231
20.581184	1360.970704	11.981235
20.632091	1354.712959	11.986240
20.822230	1363.385977	11.991245
20.954300	1379.018042	11.996250
21.221381	1377.918827	12.001255
21.434415	1382.595274	12.006259
21.505809	1384.581895	12.011264
21.583025	1376.520602	12.016269
21.321833	1377.856933	12.021274
21.367319	1376.129151	12.026279
21.413433	1388.182560	12.031283
21.333187	1380.534319	12.036288
21.345667	1389.530585	12.041293
21.046622	1383.155177	12.046298
21.435713	1372.748048	12.051303
21.176187	1386.293148	12.056307
21.094270	1382.403135	12.061312
21.403221	1386.614843	12.066317
21.376317	1377.940938	12.071322
21.666262	1379.031665	12.076327
21.465729	1389.127950	12.081331
21.698960	1386.529687	12.086336
22.019257	1387.055742	12.091341
21.616343	1382.142999	12.096346
21.890205	1373.227155	12.101351
21.421965	1359.257170	12.106355
21.538238	1358.312900	12.111360
21.448175	1345.894287	12.116365
21.468100	1349.749953	12.121370
21.573956	1358.449027	12.126375
21.370574	1348.309883	12.131379
20.881870	1346.935394	12.136384
21.572753	1355.599504	12.141389
21.471314	1365.328299	12.146394
21.379637	1363.948831	12.151399
21.295559	1347.373907	12.156403
21.374669	1358.540495	12.161408
21.580463	1361.910770	12.166413
21.543276	1355.313832	12.171418
21.727217	1340.232149	12.176423
21.445486	1359.183510	12.181427
21.477518	1359.427530	12.186432
21.742060	1344.989013	12.191437
21.781873	1354.313641	12.196442
21.947300	1361.147105	12.201447
21.681121	1373.720254	12.206451
21.623612	1338.986845	12.211456
21.774085	1329.191828	12.216461
21.437938	1327.468150	12.221466
21.393739	1333.950252	12.226471
21.031182	1328.048631	12.231475
21.446438	1323.420156	12.236480
21.875727	1314.720836	12.241485
21.536696	1325.960401	12.246490
21.777863	1326.068559	12.251495
21.760485	1336.108786	12.256499
21.765560	1319.496018	12.261504
21.709172	1321.121383	12.266509
21.341575	1325.310093	12.271514
21.470423	1323.725141	12.276519
21.385113	1321.292816	12.281523
21.339571	1322.444933	12.286528
21.541374	1319.585185	12.291533
21.439477	1310.366607	12.296538
21.507686	1304.902499	12.301543
21.203309	1305.376796	12.306547
21.348612	1312.008439	12.311552
21.463780	1313.964414	12.316557
21.055020	1325.276601	12.321562
21.537594	1319.320612	12.326567
21.456830	1325.959933	12.331571
21.218570	1328.153634	12.336576
21.653449	1324.487142	12.341581
21.650652	1334.532927	12.346586
21.328563	1313.965237	12.351591
21.422052	1310.711174	12.356595
21.285919	1307.940022	12.361600
21.314798	1294.545255	12.366605
21.170907	1321.946110	12.371610
21.385319	1323.305928	12.376615
21.533783	1327.603142	12.381619
21.275798	1335.130189	12.386624
21.586996	1337.165289	12.391629
21.424955	1328.225957	12.396634
21.461939	1325.876629	12.401639
21.383965	1328.289196	12.406643
21.318166	1329.441391	12.411648
21.673838	1321.791462	12.416653
21.224612	1326.893648	12.421658
21.512999	1315.611628	12.426663
21.526072	1316.344381	12.431667
21.400108	1320.265887	12.436672
21.437963	1321.507206	12.441677
21.382989	1324.673056	12.446682
21.557795	1313.611007	12.451687
21.180047	1323.358614	12.456691
21.244300	1320.205408	12.461696
21.453815	1317.937374	12.466701
21.215705	1316.220139	12.471706
21.468984	1315.164131	12.476711
21.612323	1306.355880	12.481715
21.356474	1324.150295	12.486720
21.386642	1313.713723	12.491725
21.534641	1322.398168	12.496730
21.480728	1310.451645	12.501735
21.626634	1318.625481	12.506739
21.189119	1321.943810	12.511744
21.618672	1307.931604	12.516749
21.606735	1317.094149	12.521754
21.504046	1312.758028	12.526759
21.749921	1316.782654	12.531763
21.597785	1319.844149	12.536768
21.459515	1310.489444	12.541773
21.495734	1324.031471	12.546778
21.422252	1309.817217	12.551783
21.171517	1318.634645	12.556787
21.145394	1321.056288	12.561792
21.491778	1310.291733	12.566797
21.477587	1319.186553	12.571802
21.568439	1315.016684	12.576807
21.929689	1321.014635	12.581811
21.605808	1320.347156	12.586816
21.571279	1319.545214	12.591821
21.465966	1319.185079	12.596826
21.763748	1309.628358	12.601831
21.490367	1299.968776	12.606835
21.579442	1288.669680	12.611840
21.724578	1278.367762	12.616845
21.487902	1279.387933	12.621850
21.658770	1286.569005	12.626855
21.289376	1286.113794	12.631859
21.494966	1286.109353	12.636864
21.496365	1278.749346	12.641869
21.436650	1295.236669	12.646874
21.359781	1291.065173	12.651879
21.197734	1278.451515	12.656883
21.278684	1290.513480	12.661888
21.555654	1291.618886	12.666893
21.313155	1299.007824	12.671898
21.746137	1288.393478	12.676903
21.621377	1276.984993	12.681907
21.479099	1294.575175	12.686912
21.539183	1274.413370	12.691917
21.236417	1295.772892	12.696922
21.177421	1291.527580	12.701927
21.424246	1295.340734	12.706931
21.268332	1307.809506	12.711936
21.599540	1294.257707	12.716941
21.360987	1284.617812	12.721946
21.297628	1311.537440	12.726951
21.643002	1286.345283	12.731955
21.323239	1291.716972	12.736960
21.620073	1299.556059	12.741965
21.413571	1300.281255	12.746970
21.651565	1290.465997	12.751975
21.915555	1297.734726	12.756979
21.204878	1266.838376	12.761984
21.548002	1285.565396	12.766989
21.058709	1289.992706	12.771994
21.223879	1278.798177	12.776999
21.235649	1293.782278	12.782003
21.335283	1311.909492	12.787008
21.726898	1284.174181	12.792013
21.162843	1307.347916	12.797018
21.602764	1304.634698	12.802023
21.196315	1295.258121	12.807027
21.098291	1296.130020	12.812032
21.522159	1294.414437	12.817037
21.551698	1286.157368	12.822042
21.626185	1304.328009	12.827047
21.694989	1286.913470	12.832051
21.649857	1297.265607	12.837056
21.596622	1270.788739	12.842061
21.189454	1264.955760	12.847066
21.279160	1271.116852	12.852071
21.311244	1236.905567	12.857075
21.040333	1292.254821	12.862080
21.364613	1276.922158	12.867085
21.447005	1300.303440	12.872090
21.487411	1312.411314	12.877095
21.069371	1292.360438	12.882099
21.444985	1324.472451	12.887104
21.569730	1286.136659	12.892109
21.420711	1293.069130	12.897114
21.527467	1305.316229	12.902119
21.571046	1307.706252	12.907123
21.253109	1293.124144	12.912128
21.562794	1288.857877	12.917133
21.463514	1310.047767	12.922138
21.163305	1275.971394	12.927143
21.268168	1265.305319	12.932147
21.611753	1304.204965	12.937152
21.351129	1296.087213	12.942157
21.385426	1307.629923	12.947162
21.505141	1291.648618	12.952167
21.668755	1284.040380	12.957171
21.366590	1271.341843	12.962176
21.334084	1283.432937	12.967181
21.323224	1267.638068	12.972186
21.278226	1271.649150	12.977191
21.409071	1289.137414	12.982195
21.068230	1279.794538	12.987200
21.513843	1304.059348	12.992205
21.796573	1300.122234	12.997210
21.390101	1283.412721	13.002215
21.448571	1284.111423	13.007219
21.255700	1285.055220	13.012224
21.666534	1272.397503	13.017229
21.540019	1279.607080	13.022234
21.417368	1280.962307	13.027239
21.197553	1279.762560	13.032243
21.082003	1277.726156	13.037248
21.573255	1285.630422	13.042253
21.494717	1279.074806	13.047258
21.282127	1280.431763	13.052263
21.309031	1294.583961	13.057267
21.156284	1277.701519	13.062272
21.450757	1291.572913	13.067277
21.838891	1308.398834	13.072282
21.375908	1286.464337	13.077287
21.636605	1275.396502	13.082291
21.305725	1287.792237	13.087296
21.547167	1278.889507	13.092301
21.282397	1284.419581	13.097306
21.110874	1272.660584	13.102311
21.011811	1291.067050	13.107315
21.141967	1266.629933	13.112320
21.566703	1318.843695	13.117325
21.214924	1315.025128	13.122330
21.318781	1321.843162	13.127335
21.530004	1313.303205	13.132339
21.563751	1323.224880	13.137344
21.479732	1296.738681	13.142349
21.267120	1328.819943	13.147354
21.565779	1310.569185	13.152359
21.747314	1301.589262	13.157363
21.055789	1293.235882	13.162368
21.600240	1289.285414	13.167373
21.500561	1302.484814	13.172378
21.672300	1276.427799	13.177383
21.461511	1281.193890	13.182387
21.416564	1299.859822	13.187392
21.862507	1281.885234	13.192397
21.422632	1270.363009	13.197402
21.216398	1301.375581	13.202407
21.566217	1268.219006	13.207411
21.541775	1304.922280	13.212416
21.649314	1292.656702	13.217421
21.578919	1294.634386	13.222426
21.552195	1269.728692	13.227431
21.556626	1308.110001	13.232435
21.449469	1283.534085	13.237440
21.603469	1284.354747	13.242445
21.608753	1295.660798	13.247450
21.629050	1275.626765	13.252455
21.534635	1256.298616	13.257459
21.436508	1243.821452	13.262464
21.249881	1265.996624	13.267469
21.451457	1235.243424	13.272474
21.315642	1260.228532	13.277479
21.377027	1250.372083	13.282483
21.433853	1246.195045	13.287488
21.384254	1269.453825	13.292493
21.481584	1244.419576	13.297498
21.122570	1276.117214	13.302503
21.583312	1255.361667	13.307507
21.385196	1281.438552	13.312512
21.224881	1252.696911	13.317517
21.244780	1286.056189	13.322522
21.620833	1257.347262	13.327527
21.618669	1282.393093	13.332531
20.801883	1257.585048	13.337536
21.781409	1247.544311	13.342541
21.443788	1292.248603	13.347546
21.526527	1285.640453	13.352551
21.666571	1284.280805	13.357555
21.014319	1267.985831	13.362560
21.347757	1231.411495	13.367565
21.110568	1273.723216	13.372570
21.421046	1296.490939	13.377575
21.493835	1307.412487	13.382579
21.276034	1281.062775	13.387584
21.722105	1313.228181	13.392589
21.210463	1274.173894	13.397594
21.626204	1255.308434	13.402599
21.597912	1284.341872	13.407603
21.161984	1265.612239	13.412608
21.226417	1231.495157	13.417613
21.521778	1274.712278	13.422618
21.415770	1260.671996	13.427623
21.496098	1271.221726	13.432627
21.165987	1277.539668	13.437632
21.631870	1256.360671	13.442637
21.596793	1239.200881	13.447642
21.384310	1285.820139	13.452647
21.059056	1271.275491	13.457651
21.371908	1243.795673	13.462656
21.316435	1279.636497	13.467661
21.438029	1262.035370	13.472666
21.593371	1275.553621	13.477671
21.430834	1255.089878	13.482675
21.251877	1266.869998	13.487680
21.541351	1272.355822	13.492685
21.358378	1258.302587	13.497690
21.664285	1243.800801	13.502695
21.798493	1247.600365	13.507699
21.480758	1274.453263	13.512704
21.471401	1247.786509	13.517709
22.012583	1238.970037	13.522714
21.789435	1285.786541	13.527719
21.628920	1275.762037	13.532723
21.327751	1250.505906	13.537728
21.466255	1272.350106	13.542733
21.540847	1281.766913	13.547738
21.525394	1255.744523	13.552743
21.480255	1277.155968	13.557747
21.426765	1257.203116	13.562752
21.624003	1250.210861	13.567757
21.405761	1236.806677	13.572762
21.281181	1232.491418	13.577767
21.305127	1222.888544	13.582771
20.634399	1241.955413	13.587776
21.248910	1237.429228	13.592781
21.214780	1269.168073	13.597786
21.368219	1262.244300	13.602791
21.216391	1270.978114	13.607795
21.604584	1245.973166	13.612800
21.280823	1274.590081	13.617805
21.512895	1257.786634	13.622810
21.346578	1257.781587	13.627815
21.419626	1269.538863	13.632819
21.323438	1268.857147	13.637824
21.545036	1264.240656	13.642829
21.496937	1260.673292	13.647834
21.449062	1259.222192	13.652839
21.692723	1276.422784	13.657843
21.172741	1256.142210	13.662848
21.355002	1264.477376	13.667853
21.434035	1267.166093	13.672858
21.432371	1260.763807	13.677863
21.739601	1270.039421	13.682867
21.489972	1261.221335	13.687872
21.456265	1270.221740	13.692877
21.418460	1263.333201	13.697882
21.636186	1264.585251	13.702887
21.461907	1269.277705	13.707891
21.407969	1242.636994	13.712896
21.478462	1252.126977	13.717901
21.435435	1245.786489	13.722906
21.152385	1232.362684	13.727911
21.385056	1230.611371	13.732915
21.240501	1260.243629	13.737920
21.478405	1265.296123	13.742925
21.554933	1269.325669	13.747930
21.432640	1268.911471	13.752935
21.492193	1254.464738	13.757939
21.224107	1257.653525	13.762944
21.526170	1263.708202	13.767949
21.443065	1272.666025	13.772954
21.308851	1249.800769	13.777959
21.464513	1234.599126	13.782963
21.310120	1257.040382	13.787968
21.227925	1258.482196	13.792973
21.453775	1247.423095	13.797978
21.488143	1255.176286	13.802983
21.612919	1264.673389	13.807987
21.031858	1262.050483	13.812992
21.482756	1250.072379	13.817997
21.442682	1256.443400	13.823002
21.172948	1264.584151	13.828007
21.615856	1264.712171	13.833011
21.473916	1265.829196	13.838016
21.431592	1254.738745	13.843021
21.176100	1253.577807	13.848026
21.043334	1264.122096	13.853031
21.443039	1283.056134	13.858035
21.241962	1271.880602	13.863040
21.643548	1287.966329	13.868045
21.764645	1279.712007	13.873050
21.196676	1254.796471	13.878055
21.159107	1268.421179	13.883059
21.352983	1282.482077	13.888064
21.265960	1277.735031	13.893069
21.210797	1268.911154	13.898074
21.070356	1293.539083	13.903079
21.411860	1271.753842	13.908083
21.285547	1273.746750	13.913088
21.129298	1287.951809	13.918093
21.283651	1279.643296	13.923098
21.051526	1283.589610	13.928103
21.307752	1280.524066	13.933107
21.307339	1274.681401	13.938112
21.213589	1282.582777	13.943117
21.158400	1282.391269	13.948122
21.099100	1283.518769	13.953127
21.759739	1296.268883	13.958131
21.520272	1288.012140	13.963136
21.598495	1277.197340	13.968141
21.363166	1289.681917	13.973146
21.677387	1282.226280	13.978151
21.793351	1264.561392	13.983155
21.234760	1278.226633	13.988160
21.519198	1281.522844	13.993165
21.457278	1273.114787	13.998170
21.661914	1279.467289	14.003175
21.531533	1282.712966	14.008179
21.109734	1296.594530	14.013184
21.066017	1274.110623	14.018189
20.995513	1285.739523	14.023207
21.360878	1293.882597	14.028224
21.609142	1283.529103	14.033242
21.384565	1280.598297	14.038259
21.586053	1267.644318	14.043277
21.323294	1267.461261	14.048295
21.269405	1290.003950	14.053312
21.561887	1286.123975	14.058330
21.643123	1287.611582	14.063347
21.340406	1278.171773	14.068365
21.710393	1280.538220	14.073383
21.391632	1295.407829	14.078400
21.582664	1284.827519	14.083418
21.223977	1290.394753	14.088435
21.207035	1307.161980	14.093453
21.670058	1309.384610	14.098471
21.690633	1326.861571	14.103488
21.991235	1318.027047	14.108506
21.418432	1333.305286	14.113523
21.645004	1327.655223	14.118541
21.936307	1329.236738	14.123559
21.518694	1321.223025	14.128576
21.678233	1327.745769	14.133594
21.775528	1322.043972	14.138611
21.720355	1322.040153	14.143629
21.723079	1328.603639	14.148647
21.496926	1315.813776	14.153664
21.994332	1321.047856	14.158682
21.679912	1342.809525	14.163699
21.870509	1316.969982	14.168717
21.884261	1322.742081	14.173735
21.410678	1345.652232	14.178752
21.983553	1328.379387	14.183770
21.953134	1370.464055	14.188787
21.906319	1354.123689	14.193805
21.916313	1349.670580	14.198823
22.155750	1373.509923	14.203840
22.333436	1346.415589	14.208858
21.831631	1360.653816	14.213875
22.043256	1356.833908	14.218893
22.601212	1349.922947	14.223911
22.151157	1370.243436	14.228928
22.074883	1329.962598	14.233946
22.456617	1363.515846	14.238963
22.311101	1338.757018	14.243981
22.009416	1319.179296	14.248999
21.898988	1350.240800	14.254016
22.280082	1345.577498	14.259034
21.950917	1381.106559	14.264051
22.303971	1355.253620	14.269069
22.467340	1369.443962	14.274087
22.258019	1350.743335	14.279104
22.370290	1375.007213	14.284122
22.700962	1368.371585	14.289139
22.244563	1360.342015	14.294157
22.489740	1366.914036	14.299175
22.257020	1361.623496	14.304192
22.533762	1370.575095	14.309210
22.388011	1365.764592	14.314227
22.398982	1375.751124	14.319245
22.588499	1356.447349	14.324263
22.442530	1353.190971	14.329280
22.273671	1371.146494	14.334298
22.498803	1373.801891	14.339315
22.442212	1355.128806	14.344333
22.260032	1377.349187	14.349351
22.468359	1361.383381	14.354368
22.091165	1381.517666	14.359386
22.441193	1345.554215	14.364403
21.779043	1377.424192	14.369421
22.916935	1352.672989	14.374439
22.533122	1414.671227	14.379456
23.014794	1394.770265	14.384474
23.157468	1388.888177	14.389491
22.812730	1375.761685	14.394509
22.724871	1365.279280	14.399527
22.668121	1361.541500	14.404544
22.694558	1352.992920	14.409562
22.532814	1376.086179	14.414579
22.524508	1389.564629	14.419597
22.554000	1391.082521	14.424615
22.412201	1417.019732	14.429632
22.845258	1389.955369	14.434650
22.756584	1417.444489	14.439667
22.712348	1395.971071	14.444685
22.614017	1408.702582	14.449703
22.780742	1373.726235	14.454720
22.588415	1408.870184	14.459738
23.332312	1390.860580	14.464755
22.834627	1428.238128	14.469773
23.423539	1402.596016	14.474791
23.095450	1399.754052	14.479808
22.686561	1417.700727	14.484826
23.427707	1408.758132	14.489843
23.200636	1420.621460	14.494861
23.333069	1416.787427	14.499879
23.293664	1396.565320	14.504896
23.359981	1404.738853	14.509914
23.436246	1412.534864	14.514931
23.250993	1387.977338	14.519949
23.544448	1404.673148	14.524967
23.579874	1394.749909	14.529984
23.242377	1402.489218	14.535002
23.316444	1386.675355	14.540019
23.119083	1398.832791	14.545037
23.469898	1405.763920	14.550055
23.422920	1383.546943	14.555072
23.438831	1412.988726	14.560090
23.392549	1370.123325	14.565107
22.992814	1417.058279	14.570125
23.364722	1396.929438	14.575143
23.620785	1402.928753	14.580160
23.272706	1430.374331	14.585178
23.230943	1402.704582	14.590195
22.991173	1411.768476	14.595213
23.300944	1401.291834	14.600231
23.073291	1432.406816	14.605248
23.656366	1414.385082	14.610266
23.603582	1441.373038	14.615283
23.533383	1422.500696	14.620301
23.500212	1436.917500	14.625319
23.615330	1410.336377	14.630336
23.592107	1421.924957	14.635354
23.923786	1430.913447	14.640371
23.756941	1440.915801	14.645389
24.022124	1418.405172	14.650407
23.844102	1419.627415	14.655424
24.029122	1434.080198	14.660442
24.270572	1423.037158	14.665459
23.947559	1419.848327	14.670477
23.981546	1431.699914	14.675495
23.974596	1419.856529	14.680512
23.425600	1411.295879	14.685530
24.133057	1388.502404	14.690547
24.100055	1446.746785	14.695565
23.820545	1426.627424	14.700583
24.015552	1405.131563	14.705600
23.711083	1422.828791	14.710618
24.119531	1407.342230	14.715635
24.000848	1414.172075	14.720653
23.945142	1417.422812	14.725671
24.112761	1434.975547	14.730688
24.261182	1408.142160	14.735706
23.931015	1439.059583	14.740723
23.942555	1423.694512	14.745741
23.956836	1431.115042	14.750759
24.210364	1428.711969	14.755776
23.930979	1423.096952	14.760794
24.046497	1424.074182	14.765811
24.224465	1429.620365	14.770829
24.048919	1427.090681	14.775847
24.165077	1407.505967	14.780864
23.895178	1436.501044	14.785882
24.516346	1413.424001	14.790899
23.995020	1429.062205	14.795917
24.544734	1408.936446	14.800935
24.129513	1440.144280	14.805952
24.196588	1425.128987	14.810970
24.552632	1413.120749	14.815987
24.378196	1456.666330	14.821005
24.299635	1418.623950	14.826023
24.879198	1458.588746	14.831040
24.658322	1432.896420	14.836058
24.371803	1425.844846	14.841075
24.441207	1425.668579	14.846093
24.248607	1424.486505	14.851111
24.662914	1444.209926	14.856128
24.392142	1456.157330	14.861146
24.750771	1439.009758	14.866163
24.613644	1457.864785	14.871181
24.707856	1466.634779	14.876199
24.455257	1452.271320	14.881216
24.550848	1454.053946	14.886234
24.909946	1441.093550	14.891251
24.841059	1469.215092	14.896269
25.228493	1447.611401	14.901287
24.741938	1421.582384	14.906304
24.822917	1419.787260	14.911322
24.628115	1423.165573	14.916339
24.813529	1435.799944	14.921357
24.760369	1431.518898	14.926375
24.783666	1449.771047	14.931392
24.880162	1451.405669	14.936410
25.080852	1448.241838	14.941427
25.163242	1450.432396	14.946445
25.040185	1439.397146	14.951463
25.363230	1448.003220	14.956480
24.775304	1421.269951	14.961498
24.826709	1429.996415	14.966515
25.059018	1438.928403	14.971533
25.054824	1437.604596	14.976551
25.037413	1450.184816	14.981568
24.923983	1456.400383	14.986586
24.937712	1441.392009	14.991603
25.145303	1453.488047	14.996621
25.356799	1447.421932	15.001639
25.190409	1446.937221	15.006656
25.202221	1428.709292	15.011674
25.399387	1471.295909	15.016691
25.075919	1455.322015	15.021709
25.447705	1443.959306	15.026727
25.294305	1447.058897	15.031744
25.695819	1439.636463	15.036762
25.442086	1456.378710	15.041779
25.349633	1430.810619	15.046797
25.217141	1459.786972	15.051815
25.604919	1446.235279	15.056832
25.014007	1446.068379	15.061850
25.565540	1448.909250	15.066867
25.202855	1458.066706	15.071885
25.247005	1426.354826	15.076903
25.323383	1458.472116	15.081920
25.315440	1434.663278	15.086938
25.162266	1457.014430	15.091955
25.319468	1456.064414	15.096973
25.523267	1446.966837	15.101991
25.933635	1477.561743	15.107008
25.519064	1468.592666	15.112026
25.593287	1466.013700	15.117043
25.570297	1484.597307	15.122061
25.947908	1465.634609	15.127079
25.742594	1488.610732	15.132096
26.309828	1465.218177	15.137114
25.910835	1479.177435	15.142131
25.848777	1436.946688	15.147149
25.331241	1465.202700	15.152167
25.897418	1444.633834	15.157184
25.520358	1466.997116	15.162202
25.964762	1479.086865	15.167219
25.936160	1466.987354	15.172237
25.778393	1488.947617	15.177255
26.021230	1473.359991	15.182272
26.001661	1484.309410	15.187290
26.240770	1473.145586	15.192307
26.163462	1479.736062	15.197325
26.234440	1477.176487	15.202343
26.291553	1449.091343	15.207360
26.020682	1447.714117	15.212378
26.184646	1442.643412	15.217395
26.048891	1437.375129	15.222413
25.867916	1450.414004	15.227431
26.073270	1456.105261	15.232448
26.367734	1465.159482	15.237466
26.267694	1462.108106	15.242483
26.279729	1483.953192	15.247501
26.307443	1474.694925	15.252519
26.684063	1458.461505	15.257536
26.044530	1462.152998	15.262554
26.217172	1463.528520	15.267571
26.450005	1463.098105	15.272589
26.179139	1469.060373	15.277607
26.776470	1461.298393	15.282624
26.924132	1476.030874	15.287642
26.621436	1451.844317	15.292659
26.489302	1452.110741	15.297677
26.367167	1440.900743	15.302695
26.652493	1439.308969	15.307712
26.124630	1437.897232	15.312730
26.143036	1452.538625	15.317747
26.609636	1466.513963	15.322765
26.633181	1474.593686	15.327783
26.702431	1474.653390	15.332800
26.673006	1472.370944	15.337818
26.510755	1459.488966	15.342835
26.536526	1467.870342	15.347853
26.633815	1474.428249	15.352871
26.659093	1483.556875	15.357888
26.358064	1459.296110	15.362906
26.480442	1475.599305	15.367923
26.713767	1459.730075	15.372941
26.532364	1459.946157	15.377959
26.822716	1476.456935	15.382976
26.814017	1467.262680	15.387994
26.849243	1476.013774	15.393011
27.047740	1510.464871	15.398029
27.334769	1491.601528	15.403047
26.955719	1470.440942	15.408064
27.002813	1468.556837	15.413082
26.791153	1481.551872	15.418099
27.256922	1462.502760	15.423117
26.721898	1460.915990	15.428135
26.862031	1479.707947	15.433152
26.984377	1497.285281	15.438170
27.253149	1492.611535	15.443187
27.361410	1488.669657	15.448205
27.427896	1490.467940	15.453223
27.432007	1485.133288	15.458240
27.240452	1468.891382	15.463258
27.327543	1482.329535	15.468275
27.528722	1464.960089	15.473293
27.287224	1464.383539	15.478311
27.228527	1453.797321	15.483328
27.100344	1467.669332	15.488346
27.277081	1471.413100	15.493363
27.384796	1487.891675	15.498381
27.348356	1491.340697	15.503399
27.505254	1481.058262	15.508416
27.349091	1507.933847	15.513434
27.308616	1504.025125	15.518451
27.527634	1486.567867	15.523469
27.190032	1496.899506	15.528487
27.576496	1497.594434	15.533504
27.717515	1499.126008	15.538522
27.492640	1490.507322	15.543539
27.511873	1495.323820	15.548557
27.640018	1493.094887	15.553575
27.538832	1513.820815	15.558592
27.626830	1486.698054	15.563610
27.370121	1490.800388	15.568627
27.628266	1507.129153	15.573645
27.898851	1488.689994	15.578663
28.005858	1485.424697	15.583680
27.550829	1493.659411	15.588698
28.018667	1500.867641	15.593715
27.879325	1483.887528	15.598733
27.729728	1511.834842	15.603751
28.121936	1487.910187	15.608768
27.698426	1499.820641	15.613786
27.806999	1510.101575	15.618803
28.123578	1506.472522	15.623821
28.196841	1516.372139	15.628839
28.259918	1513.538547	15.633856
28.098549	1501.766914	15.638874
28.123697	1482.926475	15.643891
27.998943	1501.397351	15.648909
27.520625	1493.486029	15.653927
27.670688	1529.074293	15.658944
27.777330	1511.666388	15.663962
27.720419	1515.516645	15.668979
27.842651	1522.246769	15.673997
28.128108	1520.461489	15.679015
28.523142	1521.647394	15.684032
28.451255	1523.695834	15.689050
28.193611	1534.109911	15.694067
28.478780	1497.249606	15.699085
27.879479	1522.017323	15.704103
28.340708	1535.568093	15.709120
28.875689	1530.446047	15.714138
28.359618	1541.768847	15.719155
28.745188	1548.722816	15.724173
28.254810	1514.993706	15.729191
28.605821	1549.816176	15.734208
28.702595	1549.810144	15.739226
28.570539	1542.606464	15.744243
28.899535	1523.840988	15.749261
28.540574	1545.709948	15.754279
28.730049	1526.483817	15.759296
28.714612	1522.600983	15.764314
28.752217	1521.624422	15.769331
29.011958	1500.025290	15.774349
28.759499	1525.849788	15.779367
28.180834	1523.022597	15.784384
28.736275	1508.942323	15.789402
28.710192	1555.479153	15.794419
29.049675	1531.845971	15.799437
28.765309	1541.108962	15.804455
28.634133	1564.411570	15.809472
29.308071	1532.441711	15.814490
28.811685	1555.572900	15.819507
29.420609	1538.836737	15.824525
29.237180	1543.341091	15.829543
28.874289	1546.672311	15.834560
29.219222	1550.294894	15.839578
28.965538	1546.133885	15.844595
29.542376	1544.950197	15.849613
29.220527	1546.101011	15.854631
29.099736	1516.929652	15.859648
29.391340	1529.103587	15.864666
29.579131	1495.286020	15.869683
29.265068	1527.500342	15.874701
29.407167	1499.231663	15.879719
29.377183	1519.839281	15.884736
29.599117	1497.969337	15.889754
28.963551	1521.346033	15.894771
29.526593	1511.673607	15.899789
29.390108	1512.404754	15.904807
29.187235	1512.080011	15.909824
29.206566	1494.706500	15.914842
29.211383	1536.061674	15.919859
29.593376	1538.641749	15.924877
29.404175	1527.399123	15.929895
29.433036	1549.468920	15.934912
29.433819	1522.234951	15.939930
29.291890	1564.278980	15.944947
29.677268	1539.686811	15.949965
29.234684	1549.874787	15.954983
29.897966	1538.953137	15.960000
29.666616	1547.485677	15.965018
29.776496	1539.870614	15.970035
29.836627	1565.994528	15.975053
30.000871	1527.442027	15.980071
29.739826	1556.476043	15.985088
29.594284	1532.965835	15.990106
29.592670	1551.000295	15.995123
29.750460	1545.493249	16.000141
29.671018	1549.191382	16.005159
29.708967	1531.775534	16.010176
29.904282	1541.665140	16.015194
29.897809	1536.446985	16.020211
29.846936	1540.944353	16.025229
30.050617	1538.157541	16.030247
30.219698	1555.957149	16.035264
30.489813	1548.034960	16.040282
29.823626	1535.750801	16.045299
30.164930	1532.630590	16.050317
29.833719	1541.839706	16.055335
30.258484	1561.665438	16.060352
30.381403	1557.562333	16.065370
30.472368	1562.685154	16.070387
30.496639	1543.950166	16.075405
30.305424	1549.228098	16.080423
29.977399	1546.261828	16.085440
30.154354	1563.152578	16.090458
30.563448	1535.696947	16.095475
30.696187	1553.452012	16.100493
30.626351	1567.088302	16.105511
30.251153	1559.668570	16.110528
30.579628	1560.067591	16.115546
30.472785	1547.724096	16.120563
30.440374	1587.928426	16.125581
30.312543	1570.647508	16.130599
30.711403	1537.879963	16.135616
30.972280	1569.672353	16.140634
30.652562	1577.386896	16.145651
30.669734	1542.465455	16.150669
30.670577	1586.167508	16.155687
30.660805	1557.781369	16.160704
30.768206	1567.394013	16.165722
30.826316	1551.269491	16.170739
30.778224	1588.291034	16.175757
30.801494	1555.152357	16.180775
30.956052	1574.138760	16.185792
31.117601	1554.367287	16.190810
31.048317	1558.593898	16.195827
31.164905	1546.938340	16.200845
31.205781	1593.665168	16.205863
30.877475	1566.630677	16.210880
31.332628	1528.173343	16.215898
30.695137	1574.046427	16.220915
30.763131	1550.294499	16.225933
31.436815	1562.811780	16.230951
31.261445	1550.203940	16.235968
31.517028	1569.200964	16.240986
30.895645	1539.234035	16.246003
31.156092	1560.657383	16.251021
31.697178	1547.527871	16.256039
31.207737	1542.976613	16.261056
31.137561	1532.634407	16.266074
31.365674	1568.760865	16.271091
31.338022	1546.645945	16.276109
31.215967	1570.821688	16.281127
31.255697	1561.728185	16.286144
31.330500	1558.276104	16.291162
31.634171	1532.580159	16.296179
31.205724	1575.221249	16.301197
31.677864	1582.056037	16.306215
31.162169	1575.646540	16.311232
31.212881	1548.690054	16.316250
31.520702	1554.668594	16.321267
31.407722	1577.339129	16.326285
31.328937	1545.751984	16.331303
31.425644	1586.262897	16.336320
31.614761	1539.417545	16.341338
31.569349	1572.378755	16.346355
31.896333	1599.534518	16.351373
32.178822	1569.195282	16.356391
31.705880	1575.156789	16.361408
31.916231	1557.372074	16.366426
31.610531	1573.232436	16.371443
31.756202	1581.193643	16.376461
31.874643	1583.877108	16.381479
32.038718	1585.996458	16.386496
31.928160	1600.100158	16.391514
32.152647	1585.388347	16.396531
31.826308	1601.904821	16.401549
32.384919	1580.596094	16.406567
31.996141	1586.397894	16.411584
31.723884	1595.674717	16.416602
31.960659	1573.366576	16.421619
32.076009	1588.080731	16.426637
32.448495	1572.013008	16.431655
32.191514	1575.288018	16.436672
32.083785	1591.226933	16.441690
32.645911	1587.862284	16.446707
32.502955	1592.268964	16.451725
32.615945	1581.169217	16.456743
32.303622	1587.468471	16.461760
32.125928	1604.096516	16.466778
32.224423	1591.690346	16.471795
32.405126	1583.312076	16.476813
32.404196	1583.165902	16.481831
32.425758	1597.926486	16.486848
32.486498	1588.840626	16.491866
32.701567	1582.276821	16.496883
32.326873	1587.557290	16.501901
32.505697	1593.048346	16.506919
32.485806	1615.507469	16.511936
32.616473	1594.768759	16.516954
32.689091	1622.794100	16.521971
32.764559	1613.436894	16.526989
32.941872	1597.950818	16.532007
32.829018	1629.002296	16.537024
33.000724	1588.945447	16.542042
33.140402	1618.235776	16.547059
32.803078	1597.508785	16.552077
32.941049	1608.565302	16.557095
33.120831	1600.360198	16.562112
32.835627	1613.329329	16.567130
32.919610	1591.070697	16.572147
33.027226	1616.281089	16.577165
33.363395	1585.437765	16.582183
32.620779	1621.577610	16.587200
33.589436	1592.538285	16.592218
33.165179	1605.554754	16.597235
33.356677	1589.394759	16.602253
33.291560	1593.428811	16.607271
33.419616	1617.059811	16.612288
33.352807	1601.614240	16.617306
33.876330	1588.166604	16.622323
33.233857	1602.381885	16.627341
33.497823	1554.800970	16.632359
33.058401	1584.671219	16.637376
32.980381	1588.660139	16.642394
33.653972	1578.068716	16.647411
33.033571	1615.176889	16.652429
33.410463	1598.561034	16.657447
33.594158	1589.325004	16.662464
33.136570	1616.104150	16.667482
33.468458	1584.399513	16.672499
33.515296	1623.320329	16.677517
33.497786	1583.389627	16.682535
33.244114	1626.959369	16.687552
33.670322	1605.427909	16.692570
34.024818	1636.219250	16.697587
33.866489	1630.850679	16.702605
33.771632	1624.834924	16.707623
34.096426	1635.723243	16.712640
33.788735	1637.449092	16.717658
34.137079	1633.473603	16.722675
33.745072	1630.688976	16.727693
34.008303	1631.984000	16.732711
33.960056	1627.601441	16.737728
33.597963	1623.580392	16.742746
33.985153	1628.102299	16.747763
33.972936	1627.912308	16.752781
34.151583	1634.900895	16.757799
34.198534	1629.562503	16.762816
33.583841	1628.627053	16.767834
33.779098	1611.672072	16.772851
33.986679	1638.502468	16.777869
34.119737	1627.613412	16.782887
34.141109	1665.931229	16.787904
34.495872	1659.579486	16.792922
34.486293	1648.044641	16.797939
34.399652	1669.993834	16.802957
34.758976	1654.285191	16.807975
34.230338	1647.873006	16.812992
34.893763	1635.548152	16.818010
34.725100	1647.061010	16.823027
34.594956	1613.682404	16.828045
34.566182	1637.354181	16.833063
34.272533	1627.599670	16.838080
34.686731	1610.798530	16.843098
34.796165	1657.749006	16.848115
34.333842	1639.034875	16.853133
34.989072	1645.250620	16.858151
34.996991	1656.189494	16.863168
34.879252	1633.407703	16.868186
34.654399	1660.250482	16.873203
34.796881	1622.837686	16.878221
35.214854	1656.654819	16.883239
34.680094	1647.269079	16.888256
34.978129	1647.268699	16.893274
35.041069	1664.243818	16.898291
34.890890	1641.626061	16.903309
35.086171	1646.681939	16.908327
34.954091	1666.447195	16.913344
35.053911	1627.542127	16.918362
35.360817	1663.088403	16.923379
35.102036	1644.588762	16.928397
35.205404	1632.150320	16.933415
35.146358	1628.208348	16.938432
35.376994	1634.806407	16.943450
35.522974	1657.001618	16.948467
35.207180	1633.033919	16.953485
35.280769	1666.940608	16.958503
34.874122	1650.816171	16.963520
35.224686	1623.887224	16.968538
35.091706	1652.365403	16.973555
35.188112	1641.902170	16.978573
35.292508	1648.724859	16.983591
35.253545	1676.812145	16.988608
35.478645	1656.283224	16.993626
35.837939	1693.282531	16.998643
35.124147	1678.380507	17.003661
35.937819	1651.508206	17.008679
35.687936	1693.004336	17.013696
35.676404	1680.754062	17.018714
35.892997	1644.948003	17.023731
35.799191	1697.346839	17.028749
35.766130	1690.773798	17.033767
36.052075	1662.558935	17.038784
35.834622	1691.657840	17.043802
36.017710	1657.629862	17.048819
36.095461	1681.556849	17.053837
36.038763	1677.730891	17.058855
36.268364	1676.102364	17.063872
35.867229	1668.766934	17.068890
36.081763	1674.044689	17.073907
35.976465	1664.252248	17.078925
36.156362	1686.495576	17.083943
36.039233	1661.563357	17.088960
36.074084	1699.053290	17.093978
36.252707	1655.869605	17.098995
36.255541	1686.761185	17.104013
36.215022	1669.444201	17.109031
36.346322	1669.794451	17.114048
36.077671	1680.942619	17.119066
36.361669	1685.070450	17.124083
36.302929	1700.259217	17.129101
36.198561	1700.079203	17.134119
36.786154	1708.366393	17.139136
37.046223	1694.866298	17.144154
37.002110	1697.690539	17.149171
36.949231	1681.954802	17.154189
36.388800	1667.364950	17.159207
36.903558	1668.440540	17.164224
36.446173	1672.850204	17.169242
36.950251	1661.939699	17.174259
36.504006	1664.165840	17.179277
36.954568	1674.332573	17.184295
36.653055	1678.934452	17.189312
36.882102	1674.471474	17.194330
37.087752	1694.437728	17.199347
37.375856	1673.977383	17.204365
37.000912	1699.209829	17.209383
36.932206	1669.489530	17.214400
36.741886	1692.992111	17.219418
37.353082	1669.195822	17.224435
37.063225	1716.144106	17.229453
37.443086	1684.024193	17.234471
37.306582	1682.321924	17.239488
37.015317	1693.439102	17.244506
37.112491	1668.343705	17.249523
36.850570	1697.459152	17.254541
37.314906	1676.959684	17.259559
37.168059	1693.378423	17.264576
37.307323	1692.686079	17.269594
37.443484	1685.673925	17.274611
37.328341	1700.593268	17.279629
37.233451	1700.748364	17.284647
37.559483	1688.953896	17.289664
36.982434	1703.213894	17.294682
37.122553	1709.799684	17.299699
37.512124	1705.831757	17.304717
37.415352	1719.859444	17.309735
37.822305	1739.770059	17.314752
37.793678	1716.679773	17.319770
37.587463	1721.400171	17.324787
37.489867	1734.226231	17.329805
37.718380	1735.474893	17.334823
37.860146	1724.869089	17.339840
37.700793	1724.719866	17.344858
37.722227	1723.755309	17.349875
37.856522	1709.773472	17.354893
37.743222	1721.900468	17.359911
37.785693	1716.004343	17.364928
37.704937	1731.482940	17.369946
38.141363	1736.130734	17.374963
37.995933	1744.276883	17.379981
38.036757	1749.450240	17.384999
38.197748	1740.334139	17.390016
38.158434	1754.256742	17.395034
38.639088	1744.556406	17.400051
38.473154	1748.252655	17.405069
38.402281	1757.329150	17.410087
38.681434	1745.537395	17.415104
38.758229	1742.747187	17.420122
38.473014	1732.445427	17.425139
38.477509	1721.630287	17.430157
38.120787	1725.372689	17.435175
38.612528	1725.816462	17.440192
38.455965	1734.909756	17.445210
38.540750	1749.405584	17.450227
38.745497	1753.599557	17.455245
38.738927	1748.526057	17.460263
39.174166	1737.832539	17.465280
38.693872	1737.748660	17.470298
38.598478	1733.766840	17.475315
38.514932	1748.574228	17.480333
38.678025	1749.745237	17.485351
38.846772	1744.799504	17.490368
38.758119	1741.626704	17.495386
38.714107	1740.622247	17.500403
38.775485	1742.820920	17.505421
38.704002	1750.371695	17.510439
38.773759	1752.122299	17.515456
38.762268	1765.527676	17.520474
38.855271	1770.022618	17.525491
39.098437	1773.567109	17.530509
38.931943	1791.582548	17.535527
39.286347	1771.098909	17.540544
38.817187	1789.661261	17.545562
39.142208	1779.405284	17.550579
39.296538	1765.687610	17.555597
39.426035	1792.044686	17.560615
39.186519	1779.859004	17.565632
39.570026	1778.965682	17.570650
39.554687	1782.280848	17.575667
39.775185	1795.677567	17.580685
39.370381	1785.311473	17.585703
40.246016	1766.246932	17.590720
39.655184	1784.226221	17.595738
40.005682	1761.091128	17.600755
39.778553	1765.651283	17.605773
40.038689	1770.429451	17.610791
39.946381	1769.118093	17.615808
39.911826	1767.256411	17.620826
40.121614	1763.814213	17.625843
40.003545	1772.141629	17.630861
39.941162	1754.883084	17.635879
39.947513	1762.075390	17.640896
40.286806	1774.289119	17.645914
40.076659	1772.713414	17.650931
40.218592	1769.206532	17.655949
40.117683	1773.578247	17.660967
40.176965	1766.707303	17.665984
40.246074	1774.339485	17.671002
40.320333	1774.167160	17.676019
40.559904	1769.691463	17.681037
40.311718	1771.862436	17.686055
40.485351	1766.865581	17.691072
40.239816	1769.920160	17.696090
40.197064	1780.477103	17.701107
40.159544	1773.310138	17.706125
40.206689	1768.906030	17.711143
40.289459	1772.985758	17.716160
40.259438	1772.826919	17.721178
40.484748	1764.240086	17.726195
40.849438	1762.468883	17.731213
40.463914	1763.302681	17.736231
40.498664	1755.633421	17.741248
40.367467	1760.582537	17.746266
40.125833	1777.321651	17.751283
40.663266	1778.355882	17.756301
40.344621	1772.160256	17.761319
40.161834	1794.040029	17.766336
40.284805	1789.870784	17.771354
40.483173	1813.531789	17.776371
41.067594	1813.183717	17.781389
40.725593	1799.508991	17.786407
40.974386	1827.599438	17.791424
41.193868	1809.473188	17.796442
40.879539	1799.185462	17.801459
41.073665	1815.803211	17.806477
41.102934	1795.619930	17.811495
41.516915	1828.168682	17.816512
41.605174	1788.415600	17.821530
41.319986	1819.704181	17.826547
41.899622	1782.521696	17.831565
40.950933	1813.618788	17.836583
41.593106	1796.804670	17.841600
41.660585	1783.637226	17.846618
41.394234	1813.329333	17.851635
41.929465	1796.887771	17.856653
41.415872	1803.151578	17.861671
41.563822	1770.936328	17.866688
41.719053	1824.441053	17.871706
41.721959	1782.966566	17.876723
41.861326	1812.743398	17.881741
41.298176	1803.465901	17.886759
42.194352	1793.713419	17.891776
42.079631	1826.359075	17.896794
42.136693	1784.885382	17.901811
42.251686	1814.853295	17.906829
41.705221	1796.213725	17.911847
42.172355	1760.477533	17.916864
41.873614	1787.805807	17.921882
41.676817	1828.460162	17.926899
42.006653	1814.593329	17.931917
41.803975	1813.944505	17.936935
42.341784	1808.296528	17.941952
42.214086	1836.108841	17.946970
42.561898	1814.603733	17.951987
42.319880	1833.142497	17.957005
42.665595	1822.164323	17.962023
42.258746	1835.703606	17.967040
42.571033	1828.833179	17.972058
42.508516	1822.796454	17.977075
42.839506	1837.803658	17.982093
42.375441	1819.234287	17.987111
42.594049	1847.749581	17.992128
42.406466	1816.880762	17.997146
42.485566	1838.769170	18.002163
42.543126	1824.711373	18.007181
42.524223	1819.952845	18.012199
42.621429	1829.106397	18.017216
42.815904	1807.232503	18.022234
42.490367	1839.639680	18.027251
42.636256	1822.794574	18.032269
42.413556	1821.862655	18.037287
42.419911	1854.769060	18.042304
43.307335	1858.289472	18.047322
42.938486	1853.442028	18.052339
43.118433	1868.276726	18.057357
43.021850	1862.416877	18.062375
42.909089	1856.573767	18.067392
43.253023	1876.464735	18.072410
42.778908	1857.198498	18.077427
42.791046	1854.398132	18.082445
43.193398	1881.306453	18.087463
43.257636	1892.647080	18.092480
43.564253	1880.899599	18.097498
43.686755	1874.996938	18.102515
43.676360	1884.291954	18.107533
43.384819	1898.254923	18.112551
43.815904	1886.530057	18.117568
43.880829	1880.908709	18.122586
43.490816	1873.832520	18.127603
43.835709	1875.125555	18.132621
43.950006	1870.632055	18.137639
43.722334	1877.229389	18.142656
44.121756	1862.041088	18.147674
43.878050	1888.033146	18.152691
43.928722	1850.118457	18.157709
43.838828	1841.471740	18.162727
43.886491	1870.577483	18.167744
44.260815	1860.348192	18.172762
43.904595	1858.407240	18.177779
44.129478	1863.947682	18.182797
44.272752	1873.114364	18.187815
43.990847	1860.227516	18.192832
43.961269	1875.317434	18.197850
44.058103	1878.912032	18.202867
44.117007	1870.166061	18.207885
44.225953	1882.355272	18.212903
44.270329	1877.250006	18.217920
44.473943	1869.701618	18.222938
44.353235	1886.920218	18.227955
44.355662	1865.765847	18.232973
44.380899	1862.714854	18.237991
44.368600	1865.096755	18.243008
44.497818	1860.042458	18.248026
44.081857	1886.154793	18.253043
44.084586	1891.486859	18.258061
44.588444	1890.753662	18.263079
44.383758	1907.837816	18.268096
44.932345	1916.494717	18.273114
44.535207	1899.388491	18.278131
44.935676	1907.112613	18.283149
44.983513	1884.516377	18.288167
44.978592	1918.585614	18.293184
45.128830	1893.931249	18.298202
45.194302	1892.380785	18.303219
44.975983	1906.849608	18.308237
45.208454	1900.896364	18.313255
45.375269	1905.014634	18.318272
45.548179	1887.650765	18.323290
45.179691	1900.617703	18.328307
45.039514	1903.241801	18.333325
45.286033	1891.925466	18.338343
45.184479	1916.866149	18.343360
45.743426	1928.201836	18.348378
45.113017	1931.398055	18.353395
45.455475	1935.164278	18.358413
45.526972	1917.137002	18.363431
45.441081	1947.738122	18.368448
45.677552	1907.555234	18.373466
45.572276	1949.156447	18.378483
45.785282	1906.559563	18.383501
46.016721	1937.690497	18.388519
45.806782	1916.189251	18.393536
46.098677	1919.408258	18.398554
45.953976	1936.234341	18.403571
45.943990	1898.370098	18.408589
46.038554	1931.125756	18.413607
46.039621	1913.256008	18.418624
46.570503	1919.354855	18.423642
45.728803	1916.896720	18.428659
45.913661	1910.825224	18.433677
46.148500	1929.454798	18.438695
46.294428	1901.535510	18.443712
45.888220	1923.883692	18.448730
46.381227	1908.982437	18.453747
46.431417	1898.745041	18.458765
46.371164	1922.343652	18.463783
46.389768	1915.870807	18.468800
46.797647	1891.556026	18.473818
46.406900	1925.995128	18.478835
46.418711	1906.544359	18.483853
46.548899	1900.022264	18.488871
46.567421	1905.921250	18.493888
46.583094	1946.757555	18.498906
46.838534	1935.400437	18.503923
46.892146	1927.325384	18.508941
46.777975	1951.783648	18.513959
46.864011	1946.022054	18.518976
46.979042	1939.197193	18.523994
47.243105	1938.047633	18.529011
46.987379	1967.544877	18.534029
46.892801	1924.348910	18.539047
46.792158	1938.108438	18.544064
47.091962	1948.942778	18.549082
47.082471	1936.047022	18.554099
46.987145	1947.874038	18.559117
47.105639	1932.128000	18.564135
46.928856	1933.873903	18.569152
47.398718	1936.899362	18.574170
46.926784	1927.777122	18.579187
47.566228	1965.358509	18.584205
47.952511	1955.397806	18.589223
47.159814	1959.513393	18.594240
47.623749	1928.655257	18.599258
47.519517	1952.750142	18.604275
47.643265	1978.034097	18.609293
47.567654	1966.113126	18.614311
47.045342	1965.957294	18.619328
47.288909	1964.018195	18.624346
47.930514	1946.887818	18.629363
47.946285	1947.157401	18.634381
47.856407	1978.899667	18.639399
47.803855	1950.411043	18.644416
48.101766	1993.513241	18.649434
48.010475	1986.977667	18.654451
48.595210	1961.709621	18.659469
48.559273	1975.411674	18.664487
48.162835	1946.202400	18.669504
48.703391	1925.410430	18.674522
48.325515	1984.432422	18.679539
48.317846	1985.923270	18.684557
48.234119	1953.228611	18.689575
48.362311	1937.485740	18.694592
48.401821	1963.026922	18.699610
48.493419	1952.513896	18.704627
49.043933	1937.457150	18.709645
48.852869	1952.263017	18.714663
48.254940	1976.037130	18.719680
48.330943	1947.510705	18.724698
48.955728	1931.375608	18.729715
48.838681	1971.212256	18.734733
48.967100	1996.769205	18.739751
48.671808	1996.802109	18.744768
48.516544	1968.389606	18.749786
49.111457	1953.424862	18.754803
48.564019	1997.454700	18.759821
48.643757	1979.190077	18.764839
49.015251	1974.495077	18.769856
48.968467	1994.832342	18.774874
49.292564	1963.969692	18.779891
48.893142	2010.316627	18.784909
49.078371	1975.519924	18.789927
49.022165	1956.241958	18.794944
48.953126	2026.221337	18.799962
49.017148	2019.522551	18.804979
49.274325	1999.417468	18.809997
49.556331	1998.033808	18.815015
49.108827	2049.868979	18.820032
49.607914	2033.123029	18.825050
49.379933	2004.654412	18.830067
49.455976	1988.315759	18.835085
49.816436	2028.512137	18.840103
49.955602	2007.169011	18.845120
50.072066	2037.368384	18.850138
49.728432	2001.635065	18.855155
50.052226	2030.023831	18.860173
50.225144	2022.455091	18.865191
50.294475	1999.139519	18.870208
49.983079	2033.366443	18.875226
50.215457	2031.241930	18.880243
49.881247	2028.995420	18.885261
49.874468	2014.439610	18.890279
50.499157	2005.810963	18.895296
50.393070	2048.636409	18.900314
50.627082	2041.588029	18.905331
49.822369	2040.613637	18.910349
50.861343	2005.661824	18.915367
50.812817	2043.335833	18.920384
50.756214	2045.479436	18.925402
51.268806	1993.583492	18.930419
50.737433	2034.079425	18.935437
50.660709	1993.222654	18.940455
50.548770	2014.293932	18.945472
50.417423	1982.709498	18.950490
50.509691	2016.502342	18.955507
50.647956	2025.920032	18.960525
50.859694	2023.224654	18.965543
50.746348	2055.000716	18.970560
50.715758	2018.956304	18.975578
51.050817	2031.505983	18.980595
50.785514	2027.736797	18.985613
50.966011	2036.856747	18.990631
50.881540	2028.558267	18.995648
50.777399	2054.962522	19.000666
51.085000	2060.121757	19.005683
51.178426	2063.989080	19.010701
51.725749	2026.837869	19.015719
51.273384	2078.678638	19.020736
51.057069	2068.047894	19.025754
51.655873	2044.756345	19.030771
51.625609	2044.962485	19.035789
51.206833	2053.259368	19.040807
51.731740	2054.970454	19.045824
51.795727	2053.225154	19.050842
52.049331	2050.790510	19.055859
51.549403	2085.282007	19.060877
51.640157	2069.927212	19.065895
51.398298	2057.581218	19.070912
51.933078	2038.210463	19.075930
51.946459	2087.420800	19.080947
51.580015	2087.465051	19.085965
51.912925	2075.102880	19.090983
51.983643	2108.477800	19.096000
51.998385	2077.236380	19.101018
51.935562	2097.378144	19.106035
52.255133	2062.358458	19.111053
52.335662	2052.698139	19.116071
52.374572	2096.298131	19.121088
52.159510	2081.317717	19.126106
52.459875	2108.469245	19.131123
52.520329	2094.931402	19.136141
52.542567	2127.046225	19.141159
52.586774	2101.379647	19.146176
52.532903	2126.330388	19.151194
52.813676	2096.205834	19.156211
52.531033	2129.726822	19.161229
52.915595	2105.248661	19.166247
52.878845	2141.001933	19.171264
52.466417	2115.178493	19.176282
53.157857	2080.145074	19.181299
53.039976	2132.264600	19.186317
53.315457	2113.833308	19.191335
53.116297	2098.029212	19.196352
53.380552	2122.329881	19.201370
53.289503	2128.894527	19.206387
52.798955	2111.197324	19.211405
53.717661	2073.554176	19.216423
53.734950	2099.695325	19.221440
53.156045	2115.434678	19.226458
54.057390	2069.803247	19.231475
53.842026	2116.519145	19.236493
53.348926	2103.909583	19.241511
53.182285	2101.299706	19.246528
53.636191	2078.319079	19.251546
53.816477	2082.864692	19.256563
53.363921	2126.411021	19.261581
53.526863	2097.219196	19.266599
53.918775	2105.702997	19.271616
53.628277	2162.146141	19.276634
53.702641	2145.905108	19.281651
54.253759	2114.041655	19.286669
54.003440	2112.057035	19.291687
54.351083	2139.847603	19.296704
53.677622	2123.695973	19.301722
54.461300	2100.799572	19.306739
54.257531	2120.145864	19.311757
54.249780	2153.607336	19.316775
54.244735	2131.524099	19.321792
53.816430	2132.197995	19.326810
54.685655	2113.195377	19.331827
54.504653	2153.163848	19.336845
54.093306	2122.018601	19.341863
54.477023	2113.525852	19.346880
54.696369	2161.780216	19.351898
54.505113	2141.345329	19.356915
54.811140	2131.755961	19.361933
54.814610	2161.687321	19.366951
54.903291	2142.128021	19.371968
54.594955	2143.529981	19.376986
54.998564	2150.218670	19.382003
55.204211	2153.089684	19.387021
55.116725	2139.554944	19.392039
55.154094	2153.646601	19.397056
55.319428	2125.733226	19.402074
55.298295	2165.995563	19.407091
55.140894	2140.807815	19.412109
55.258973	2163.670506	19.417127
55.162439	2141.798475	19.422144
55.117763	2147.915281	19.427162
55.355421	2142.705164	19.432179
55.442285	2147.945253	19.437197
55.399178	2162.708861	19.442215
55.580448	2182.917208	19.447232
55.381195	2168.472166	19.452250
55.754282	2189.563873	19.457267
55.990755	2175.126413	19.462285
55.812892	2171.141893	19.467303
55.859706	2178.271322	19.472320
55.907349	2185.370735	19.477338
56.047569	2163.663836	19.482355
56.131731	2187.697604	19.487373
55.597849	2178.072268	19.492391
56.068820	2156.194652	19.497408
55.863569	2188.806796	19.502426
56.084853	2199.833176	19.507443
56.411322	2203.370783	19.512461
56.568194	2199.304555	19.517479
57.010269	2206.515681	19.522496
56.889774	2203.797750	19.527514
56.471234	2177.415165	19.532531
56.841383	2179.690505	19.537549
56.652179	2185.537789	19.542567
56.675228	2167.432984	19.547584
56.656676	2164.590261	19.552602
56.632448	2192.394619	19.557619
56.846576	2176.293286	19.562637
56.762888	2207.223369	19.567655
57.113869	2169.950521	19.572672
56.839146	2206.157192	19.577690
57.090075	2174.719015	19.582707
56.999838	2205.771265	19.587725
56.976463	2168.589585	19.592743
56.965774	2212.627279	19.597760
56.799295	2188.941589	19.602778
57.312440	2164.412934	19.607795
57.078504	2213.537298	19.612813
57.139809	2195.037813	19.617831
57.560671	2219.694348	19.622848
57.775193	2209.123779	19.627866
57.476123	2218.523252	19.632883
57.775534	2211.620093	19.637901
57.685794	2208.846917	19.642919
57.807425	2205.509914	19.647936
58.027394	2229.556699	19.652954
58.081586	2219.384507	19.657971
57.914303	2205.489618	19.662989
57.939386	2211.249253	19.668007
58.239296	2217.064163	19.673024
57.854575	2220.276314	19.678042
57.950149	2219.672714	19.683059
58.207997	2213.274842	19.688077
58.254220	2211.502468	19.693095
58.264380	2199.452793	19.698112
58.004825	2231.048062	19.703130
58.338583	2206.401651	19.708147
58.316727	2206.114087	19.713165
58.003143	2237.502478	19.718183
58.378348	2214.976217	19.723200
58.966069	2240.373827	19.728218
58.395611	2222.456418	19.733235
58.609319	2249.867429	19.738253
58.826855	2238.407581	19.743271
58.700539	2237.156661	19.748288
58.623170	2241.362736	19.753306
58.739380	2229.090053	19.758323
59.204793	2237.699067	19.763341
58.859296	2234.145540	19.768359
58.837201	2237.894478	19.773376
59.133287	2272.780149	19.778394
59.472855	2265.057288	19.783411
59.504841	2267.709051	19.788429
59.003271	2281.373966	19.793447
59.716196	2249.361714	19.798464
59.530258	2282.101551	19.803482
59.597148	2264.939762	19.808499
59.695202	2263.030125	19.813517
59.548213	2269.828703	19.818535
59.851014	2250.445899	19.823552
60.028896	2264.773237	19.828570
59.885011	2260.743946	19.833587
60.142777	2265.500635	19.838605
59.969679	2261.636456	19.843623
59.683045	2253.410987	19.848640
59.832907	2278.345228	19.853658
59.955837	2266.917749	19.858675
59.951155	2254.082293	19.863693
59.944339	2256.729231	19.868711
60.085105	2252.574320	19.873728
60.063901	2241.500190	19.878746
60.110077	2264.297427	19.883763
60.540826	2266.638624	19.888781
60.053078	2285.078723	19.893799
60.310119	2275.010998	19.898816
60.439373	2287.074612	19.903834
60.483693	2275.938094	19.908851
60.613056	2278.036342	19.913869
60.157952	2277.636970	19.918887
60.416842	2286.816937	19.923904
60.582631	2291.295714	19.928922
60.781756	2315.084837	19.933939
60.915703	2311.464266	19.938957
60.945622	2312.348242	19.943975
61.097727	2310.612454	19.948992
60.992806	2313.690337	19.954010
61.011033	2309.015392	19.959027
61.409506	2294.119385	19.964045
61.288057	2301.415712	19.969063
61.810341	2298.588959	19.974080
61.411992	2297.935136	19.979098
61.058128	2297.250623	19.984115
61.453113	2312.138001	19.989133
61.425878	2328.574561	19.994151
61.687716	2318.592559	19.999168
61.677192	2331.757626	20.004186
61.573013	2334.934499	20.009203
61.462471	2335.502667	20.014221
61.595128	2336.286887	20.019239
61.609100	2320.911038	20.024256
62.100286	2322.333373	20.029274
62.124699	2345.035105	20.034291
62.146411	2347.329861	20.039309
62.183431	2360.728051	20.044327
62.631705	2336.527214	20.049344
62.281518	2344.965910	20.054362
62.278929	2358.357830	20.059379
62.597831	2346.436552	20.064397
62.365362	2350.453457	20.069415
62.527614	2351.720609	20.074432
62.555983	2337.805402	20.079450
62.830727	2351.143647	20.084467
62.705578	2344.444993	20.089485
62.710073	2360.577645	20.094503
63.035482	2353.498808	20.099520
63.077959	2352.504111	20.104538
63.076042	2345.279274	20.109555
63.228373	2344.430658	20.114573
63.176324	2349.466453	20.119591
63.322317	2339.845841	20.124608
63.299782	2362.635314	20.129626
63.308232	2339.701722	20.134643
63.116051	2339.021310	20.139661
63.283302	2359.664734	20.144679
63.471236	2333.045140	20.149696
63.263140	2344.228201	20.154714
63.069678	2355.287810	20.159731
63.505859	2337.165671	20.164749
63.362099	2350.089301	20.169767
63.522672	2363.702177	20.174784
63.661840	2370.549550	20.179802
63.843929	2391.984268	20.184819
64.023660	2365.546040	20.189837
63.627275	2381.505114	20.194855
63.843451	2394.166880	20.199872
64.285433	2372.158281	20.204890
64.089151	2371.563466	20.209907
64.324222	2369.071950	20.214925
64.264859	2381.514946	20.219943
64.274409	2378.963437	20.224960
64.456527	2356.258533	20.229978
64.441210	2371.785579	20.234995
64.461773	2373.372641	20.240013
64.485592	2398.198984	20.245031
64.863479	2388.786758	20.250048
64.734500	2408.712194	20.255066
64.861084	2413.803683	20.260083
64.779003	2384.719573	20.265101
64.920669	2406.156826	20.270119
64.693141	2402.681974	20.275136
64.905601	2386.677418	20.280154
65.001620	2411.132035	20.285171
64.911682	2384.152383	20.290189
64.933563	2411.915986	20.295207
64.982603	2405.878531	20.300224
65.348831	2393.309425	20.305242
65.751664	2420.825883	20.310259
65.607631	2412.110377	20.315277
65.351502	2413.994835	20.320295
65.558054	2422.867834	20.325312
65.977246	2408.448982	20.330330
65.930583	2416.347727	20.335347
65.878183	2412.114248	20.340365
66.122312	2413.052160	20.345383
66.037735	2397.548796	20.350400
65.874255	2403.598137	20.355418
65.918541	2413.339391	20.360435
66.029511	2407.791510	20.365453
66.328501	2419.929629	20.370471
66.321609	2428.817008	20.375488
66.189929	2420.982024	20.380506
66.245333	2407.754592	20.385523
66.443021	2427.610653	20.390541
66.479272	2406.652241	20.395559
66.248177	2404.902834	20.400576
66.264405	2426.532374	20.405594
66.048666	2410.091125	20.410611
66.205324	2401.466888	20.415629
66.466173	2427.296069	20.420647
66.332665	2439.381266	20.425664
66.768228	2433.234964	20.430682
66.417402	2461.000683	20.435699
66.729111	2441.618565	20.440717
66.666812	2441.358682	20.445735
66.768862	2476.275788	20.450752
67.448295	2466.898795	20.455770
67.031729	2471.769387	20.460787
67.377491	2459.592827	20.465805
67.404650	2472.011090	20.470823
67.205277	2461.393085	20.475840
67.180015	2460.139400	20.480858
67.018941	2477.241649	20.485875
67.362264	2449.160836	20.490893
67.205915	2503.203052	20.495911
67.527297	2491.218337	20.500928
67.700363	2499.384903	20.505946
67.794495	2504.650705	20.510963
67.636473	2502.428718	20.515981
68.010885	2493.393733	20.520999
67.893602	2499.268213	20.526016
67.645273	2493.002069	20.531034
68.300117	2503.737733	20.536051
68.182948	2511.890028	20.541069
68.343366	2520.845953	20.546087
68.446522	2516.116496	20.551104
68.850497	2497.817604	20.556122
68.515675	2519.700690	20.561139
68.844868	2517.934276	20.566157
68.879670	2512.647837	20.571175
68.658685	2501.698182	20.576192
69.125628	2512.943610	20.581210
69.108840	2508.649366	20.586227
69.207039	2497.955562	20.591245
69.117485	2516.939659	20.596263
68.889709	2496.677629	20.601280
69.460573	2497.466695	20.606298
69.091829	2497.244671	20.611315
69.042872	2507.391769	20.616333
69.044573	2510.609212	20.621351
69.100891	2489.873218	20.626368
69.185338	2525.739461	20.631386
69.335989	2533.572980	20.636403
69.471319	2520.519109	20.641421
69.671484	2545.205105	20.646439
69.476625	2539.993036	20.651456
69.764818	2519.503963	20.656474
69.656826	2545.597464	20.661491
69.576084	2524.279212	20.666509
69.544883	2545.498052	20.671527
70.078912	2546.978076	20.676544
70.099000	2545.610968	20.681562
70.117271	2556.795845	20.686579
70.178840	2566.079034	20.691597
70.387061	2554.060403	20.696615
70.174402	2553.766293	20.701632
70.582108	2550.648654	20.706650
70.439423	2564.381657	20.711667
70.721360	2547.248950	20.716685
70.799009	2537.068077	20.721703
70.715689	2566.204756	20.726720
70.518735	2555.589442	20.731738
70.849769	2549.816854	20.736755
70.504329	2552.254356	20.741773
70.814546	2557.197841	20.746791
70.457685	2579.390498	20.751808
71.349536	2556.898512	20.756826
71.180748	2591.806390	20.761843
71.194731	2572.739791	20.766861
71.638787	2572.126222	20.771879
71.416597	2598.519614	20.776896
71.716625	2556.428432	20.781914
71.579183	2594.066923	20.786931
71.599941	2568.410339	20.791949
71.376592	2586.759099	20.796967
71.613132	2553.886950	20.801984
71.900297	2583.961921	20.807002
71.454991	2579.680937	20.812019
71.260175	2581.749128	20.817037
71.978753	2591.497802	20.822055
71.717536	2608.421898	20.827072
71.916225	2614.524471	20.832090
72.171168	2599.096528	20.837107
72.084004	2626.706464	20.842125
72.401683	2579.923777	20.847143
72.318958	2617.957889	20.852160
72.640620	2622.717879	20.857178
72.654075	2626.500575	20.862195
72.775873	2632.731042	20.867213
72.692500	2634.995409	20.872231
73.277338	2620.763874	20.877248
72.978616	2632.033183	20.882266
72.884988	2611.859715	20.887283
72.998641	2610.830840	20.892301
73.418350	2633.640662	20.897319
73.488114	2603.558936	20.902336
73.205033	2626.654654	20.907354
73.138591	2615.516664	20.912371
73.144210	2612.797419	20.917389
73.412324	2630.090963	20.922407
73.533021	2620.840733	20.927424
73.132234	2640.975796	20.932442
73.794602	2619.528670	20.937459
73.574338	2619.723431	20.942477
73.936859	2625.057380	20.947495
73.572624	2624.108648	20.952512
73.876935	2609.836914	20.957530
73.828215	2611.047282	20.962547
73.810824	2633.390385	20.967565
74.116447	2622.032598	20.972583
73.884683	2607.799164	20.977600
73.960904	2626.735731	20.982618
73.767205	2654.056742	20.987635
73.908317	2638.373977	20.992653
73.951190	2655.162324	20.997671
74.145587	2659.197758	21.002688
74.189440	2658.574860	21.007706
74.322586	2690.489188	21.012723
74.751197	2692.468198	21.017741
75.214062	2663.375279	21.022759
75.238380	2698.475998	21.027776
75.065476	2663.661614	21.032794
75.147014	2691.693891	21.037811
75.097764	2669.204732	21.042829
75.053554	2689.307379	21.047847
75.200009	2665.531677	21.052864
75.149820	2693.468555	21.057882
75.369331	2659.456022	21.062899
75.095376	2676.069180	21.067917
75.256773	2688.456781	21.072935
75.246323	2680.683338	21.077952
75.452420	2709.872468	21.082970
75.517799	2704.810757	21.087987
75.408984	2703.970732	21.093005
75.519678	2706.203375	21.098023
75.580861	2703.824482	21.103040
75.493957	2720.012223	21.108058
76.112290	2716.300933	21.113075
76.014267	2732.184491	21.118093
76.366842	2726.871680	21.123111
76.148631	2733.749476	21.128128
76.308011	2717.344015	21.133146
76.318252	2735.798076	21.138163
76.273950	2715.611878	21.143181
76.494442	2753.619226	21.148199
76.706270	2744.727212	21.153216
76.695568	2766.736740	21.158234
77.279460	2749.064044	21.163251
76.858620	2755.462903	21.168269
77.095528	2747.773466	21.173287
77.071467	2774.098610	21.178304
77.160455	2754.093248	21.183322
77.699618	2741.716502	21.188339
77.357783	2743.565115	21.193357
77.581342	2763.452906	21.198375
77.565585	2746.568800	21.203392
77.377907	2746.383965	21.208410
77.804906	2750.819656	21.213427
77.735882	2738.689349	21.218445
77.809710	2747.780353	21.223463
77.598774	2725.254754	21.228480
77.556766	2732.219286	21.233498
77.877559	2766.493412	21.238515
77.380535	2738.860681	21.243533
78.484930	2705.572921	21.248551
78.157137	2737.595470	21.253568
78.021211	2770.477874	21.258586
78.179944	2731.779118	21.263603
77.911924	2716.115895	21.268621
78.037222	2769.727986	21.273639
78.253602	2809.070136	21.278656
78.311672	2807.734701	21.283674
78.344684	2784.337928	21.288691
78.152607	2787.140356	21.293709
79.314694	2771.808251	21.298727
78.884363	2806.052022	21.303744
78.809798	2801.092038	21.308762
79.200738	2816.067890	21.313779
79.212306	2788.408229	21.318797
79.320639	2813.825094	21.323815
79.205926	2788.837851	21.328832
79.363612	2790.930085	21.333850
79.155161	2814.864468	21.338867
79.196977	2795.279516	21.343885
79.388404	2790.352626	21.348903
79.580680	2804.966082	21.353920
79.498795	2780.467578	21.358938
79.652999	2814.788048	21.363955
80.035019	2816.331673	21.368973
79.754240	2817.542097	21.373991
79.817902	2829.787307	21.379008
79.910953	2818.329552	21.384026
79.846254	2827.820247	21.389043
80.049110	2827.628977	21.394061
80.345980	2811.178674	21.399079
80.708689	2841.983858	21.404096
80.343747	2820.025400	21.409114
80.577281	2849.310328	21.414131
80.829965	2839.779346	21.419149
80.865664	2853.963976	21.424167
80.790783	2856.831103	21.429184
81.020039	2854.619664	21.434202
81.282108	2844.347027	21.439219
81.026545	2857.577603	21.444237
81.058604	2855.225355	21.449255
81.222820	2825.375875	21.454272
80.926406	2871.099534	21.459290
81.095570	2842.327608	21.464307
81.382719	2836.933165	21.469325
81.139580	2832.564016	21.474343
81.315467	2875.688297	21.479360
81.208575	2864.577017	21.484378
81.781292	2862.641160	21.489395
81.441308	2900.871989	21.494413
81.529717	2865.821168	21.499431
81.814907	2864.621765	21.504448
81.477038	2867.794333	21.509466
81.869760	2891.109119	21.514483
82.157860	2898.978336	21.519501
82.059445	2886.046364	21.524519
82.055880	2903.367828	21.529536
82.313028	2900.554145	21.534554
82.308660	2886.014382	21.539571
82.459148	2910.045847	21.544589
82.168768	2889.041295	21.549607
82.583407	2914.680067	21.554624
82.496932	2927.761824	21.559642
82.791927	2914.159860	21.564659
83.108023	2935.968081	21.569677
83.479821	2906.460524	21.574695
83.421316	2906.564207	21.579712
83.362879	2927.392304	21.584730
83.690219	2903.990876	21.589747
83.376284	2932.148035	21.594765
83.852765	2898.396794	21.599783
83.820097	2918.160480	21.604800
83.716832	2891.747551	21.609818
83.536500	2917.172089	21.614835
83.972287	2896.073747	21.619853
83.715561	2904.932828	21.624871
84.220483	2895.470917	21.629888
83.850322	2925.509840	21.634906
84.176984	2883.533811	21.639923
83.740115	2920.311628	21.644941
83.740323	2898.839122	21.649959
84.403366	2931.580317	21.654976
83.977946	2919.155886	21.659994
84.348673	2951.305838	21.665011
84.432941	2918.856727	21.670029
84.482758	2947.181651	21.675047
84.390452	2936.016864	21.680064
84.773314	2955.907831	21.685082
85.021062	2961.219307	21.690099
85.016386	2967.972703	21.695117
85.025885	2959.375540	21.700135
85.499472	2963.096744	21.705152
85.228012	2966.095921	21.710170
85.258721	2973.143360	21.715187
85.494241	2951.652128	21.720205
85.033440	2973.227984	21.725223
85.646339	2945.966093	21.730240
85.185534	2961.420083	21.735258
85.674555	2972.386265	21.740275
85.763813	2996.084693	21.745293
85.787533	2980.641308	21.750311
86.117662	2993.451392	21.755328
85.911672	2989.139984	21.760346
85.866803	2973.481799	21.765363
86.331291	2989.769111	21.770381
86.553793	2981.879701	21.775399
86.499452	2984.248039	21.780416
86.561484	2985.491116	21.785434
86.533969	2976.619040	21.790451
86.594434	2966.759167	21.795469
86.338557	2997.601976	21.800487
86.680125	2967.354236	21.805504
86.572340	3013.945736	21.810522
86.968152	2997.072789	21.815539
86.803839	2999.444508	21.820557
86.881482	3032.167592	21.825575
86.893720	2999.817884	21.830592
86.749762	3021.580041	21.835610
87.208063	3022.742623	21.840627
87.276073	3036.982059	21.845645
87.538079	3043.975342	21.850663
87.498233	3042.759328	21.855680
87.776135	3035.469075	21.860698
87.420153	3067.288399	21.865715
87.207300	3043.966600	21.870733
87.956684	3028.003930	21.875751
87.744106	3085.124899	21.880768
88.023145	3057.735916	21.885786
88.219251	3075.143729	21.890803
88.084115	3093.338259	21.895821
88.059322	3061.963379	21.900839
88.111141	3083.582714	21.905856
88.347531	3080.385313	21.910874
88.633009	3095.923369	21.915891
88.363097	3122.297787	21.920909
88.721590	3121.546036	21.925927
88.911872	3071.819057	21.930944
89.132356	3096.397348	21.935962
88.952833	3098.532390	21.940979
89.317072	3068.249363	21.945997
89.232692	3105.105150	21.951015
89.341439	3091.927583	21.956032
89.500145	3123.123788	21.961050
89.310064	3126.552863	21.966067
90.032971	3098.042155	21.971085
89.833725	3137.409784	21.976103
89.983578	3092.580906	21.981120
89.847910	3106.678270	21.986138
90.149564	3117.318124	21.991155
90.599802	3103.761234	21.996173
90.311564	3097.860654	22.001191
90.335096	3115.784499	22.006208
90.199493	3108.954226	22.011226
90.403887	3089.305983	22.016243
90.561821	3120.448032	22.021261
90.498773	3095.576302	22.026279
90.584008	3111.899061	22.031296
90.373979	3089.191054	22.036314
90.388500	3125.668510	22.041331
90.592612	3097.870583	22.046349
90.696496	3144.745735	22.051367
90.632500	3122.535103	22.056384
90.770652	3153.021225	22.061402
90.430434	3137.664027	22.066419
90.925970	3153.491931	22.071437
90.661318	3173.114403	22.076455
91.429261	3144.989712	22.081472
91.115912	3194.285786	22.086490
91.153522	3200.680946	22.091507
91.550197	3178.845903	22.096525
91.426845	3204.910783	22.101543
91.670566	3190.614323	22.106560
91.701696	3212.953724	22.111578
91.318044	3208.267852	22.116595
92.068113	3207.231051	22.121613
92.008726	3244.196470	22.126631
92.278166	3217.887911	22.131648
92.375784	3221.576322	22.136666
92.562931	3253.793973	22.141683
92.572732	3222.685389	22.146701
92.562292	3265.127106	22.151719
93.250796	3242.211073	22.156736
92.889738	3275.573361	22.161754
93.366436	3230.516530	22.166771
93.447274	3264.532767	22.171789
93.477363	3224.738630	22.176807
93.521077	3242.713686	22.181824
93.719127	3236.360303	22.186842
93.792985	3251.546060	22.191859
93.747481	3213.567644	22.196877
93.689864	3222.120647	22.201895
93.917841	3232.909987	22.206912
93.938564	3228.135239	22.211930
93.884302	3238.957007	22.216947
93.983376	3260.044417	22.221965
93.850516	3226.999193	22.226983
94.173698	3247.917128	22.232000
94.151426	3233.548990	22.237018
94.241683	3236.140510	22.242035
94.746174	3232.295441	22.247053
94.170149	3220.115797	22.252071
94.210590	3260.205372	22.257088
94.609042	3239.366558	22.262106
94.586905	3272.576470	22.267123
94.879001	3262.183125	22.272141
94.767470	3280.135789	22.277159
94.848922	3255.636395	22.282176
94.713779	3294.660714	22.287194
95.053978	3275.095969	22.292211
95.393433	3292.192505	22.297229
95.185788	3305.066599	22.302247
95.485368	3279.660056	22.307264
95.915892	3287.423395	22.312282
95.392217	3297.612135	22.317299
95.905968	3288.320829	22.322317
95.794966	3309.146841	22.327335
95.732334	3302.017736	22.332352
95.519617	3302.971929	22.337370
96.319050	3292.116165	22.342387
95.917150	3316.283583	22.347405
96.295211	3331.251011	22.352423
95.586016	3321.117981	22.357440
95.702737	3328.948689	22.362458
96.274051	3329.236683	22.367475
96.456148	3369.115974	22.372493
96.456713	3344.648995	22.377511
96.899921	3351.579708	22.382528
96.835312	3391.554249	22.387546
96.953548	3375.036624	22.392563
97.428779	3397.163114	22.397581
97.247883	3367.052925	22.402599
96.736725	3392.575882	22.407616
97.399788	3354.328361	22.412634
97.482795	3394.864594	22.417651
97.664666	3381.176407	22.422669
97.630861	3424.714101	22.427687
97.492300	3401.524615	22.432704
98.234699	3382.757693	22.437722
97.789684	3423.231900	22.442739
98.012218	3382.240915	22.447757
97.997962	3415.763745	22.452775
98.133617	3402.260679	22.457792
98.354904	3448.928517	22.462810
98.276753	3433.454490	22.467827
98.228904	3444.358765	22.472845
98.769600	3434.694158	22.477863
98.487246	3424.750991	22.482880
99.077622	3458.665975	22.487898
98.749759	3442.933638	22.492915
99.033358	3469.933069	22.497933
99.071231	3460.005673	22.502951
98.913304	3442.875990	22.507968
99.070622	3476.194614	22.512986
99.064854	3463.773588	22.518003
99.488872	3455.683458	22.523021
99.462541	3513.628282	22.528039
99.468790	3496.477075	22.533056
99.844436	3480.811855	22.538074
99.403054	3502.294145	22.543091
99.927608	3518.319189	22.548109
99.971309	3505.686510	22.553127
99.954264	3534.858602	22.558144
100.349249	3510.723322	22.563162
100.374225	3532.588301	22.568179
100.442857	3511.590100	22.573197
100.403488	3520.671321	22.578215
100.685500	3534.153445	22.583232
100.994938	3545.291076	22.588250
100.601567	3525.880732	22.593267
101.356258	3531.401834	22.598285
101.493580	3546.011427	22.603303
101.172784	3525.688068	22.608320
101.358033	3558.353482	22.613338
101.126940	3519.745481	22.618355
101.549541	3549.346198	22.623373
101.717588	3529.655179	22.628391
101.193162	3539.720709	22.633408
101.745944	3521.563571	22.638426
101.757380	3556.593682	22.643443
101.972598	3554.879150	22.648461
101.887076	3565.273514	22.653479
101.818614	3558.395352	22.658496
101.982970	3568.803360	22.663514
101.928441	3560.420569	22.668531
102.232769	3597.685213	22.673549
102.869806	3578.082954	22.678567
102.559217	3603.553841	22.683584
102.963009	3566.087307	22.688602
102.813643	3625.425598	22.693619
102.863527	3600.976283	22.698637
103.093906	3573.842662	22.703655
102.646927	3596.439022	22.708672
103.110410	3597.188651	22.713690
103.466111	3609.307712	22.718707
103.590377	3602.041679	22.723725
103.411624	3622.584751	22.728743
103.739499	3614.373784	22.733760
103.848464	3591.081597	22.738778
103.834478	3619.293716	22.743795
104.253492	3607.780218	22.748813
104.051842	3607.875267	22.753831
104.218483	3617.277668	22.758848
104.127315	3636.224147	22.763866
104.557997	3632.765957	22.768883
104.140702	3621.405475	22.773901
104.288473	3642.243398	22.778919
104.897674	3626.846769	22.783936
104.991712	3643.326826	22.788954
105.043540	3641.665084	22.793971
104.994574	3621.174747	22.798989
104.808610	3637.937002	22.804007
105.321863	3647.836347	22.809024
105.429556	3660.782391	22.814042
105.586690	3667.437154	22.819059
105.310930	3659.733814	22.824077
105.456640	3651.837413	22.829095
105.372138	3671.710282	22.834112
105.864638	3648.116143	22.839130
105.795209	3662.305737	22.844147
105.834774	3680.448754	22.849165
106.295672	3688.809221	22.854183
105.917487	3686.800716	22.859200
106.311113	3683.132107	22.864218
106.263684	3686.043788	22.869235
106.353933	3693.563484	22.874253
106.675625	3688.606082	22.879271
106.167635	3684.765031	22.884288
106.639645	3705.699223	22.889306
106.865206	3693.226954	22.894323
106.589206	3712.840945	22.899341
107.508985	3704.773883	22.904359
106.633879	3699.633685	22.909376
107.054960	3709.510012	22.914394
107.185927	3720.279000	22.919411
107.347074	3725.757170	22.924429
107.682017	3742.387710	22.929447
107.497211	3724.305464	22.934464
107.772795	3748.775383	22.939482
107.766641	3741.840003	22.944499
107.595566	3754.417613	22.949517
107.847742	3742.058264	22.954535
107.688538	3763.607637	22.959552
107.838563	3761.432298	22.964570
108.132957	3758.629034	22.969587
108.386105	3802.391115	22.974605
108.589838	3789.912806	22.979623
108.168592	3797.997099	22.984640
109.045291	3784.148969	22.989658
109.148337	3829.874066	22.994675
108.895547	3787.356197	22.999693
109.141382	3828.721929	23.004711
109.388807	3796.608269	23.009728
109.376462	3841.940406	23.014746
109.366517	3807.663667	23.019763
109.513627	3841.766647	23.024781
109.856313	3803.786152	23.029799
109.472257	3863.350045	23.034816
110.011359	3825.536400	23.039834
110.135389	3835.792920	23.044851
109.809011	3853.301497	23.049869
110.430501	3818.099671	23.054887
110.657099	3818.770668	23.059904
110.222937	3864.796284	23.064922
110.370340	3860.469953	23.069939
110.633619	3850.903590	23.074957
110.864603	3874.339353	23.079975
110.902230	3866.012486	23.084992
110.898997	3849.749680	23.090010
110.749911	3876.794477	23.095027
110.488966	3891.965066	23.100045
111.117619	3885.127405	23.105063
111.236688	3902.902469	23.110080
111.470913	3874.864640	23.115098
111.866154	3927.593112	23.120115
111.904766	3930.027802	23.125133
112.287728	3916.810487	23.130151
112.203249	3928.066290	23.135168
112.193582	3928.903187	23.140186
112.605731	3892.296623	23.145203
112.411255	3935.418592	23.150221
112.615221	3939.750989	23.155239
112.627898	3912.859910	23.160256
112.579073	3912.983294	23.165274
112.904566	3932.924078	23.170291
112.630977	3909.653843	23.175309
113.030063	3916.123040	23.180327
112.807609	3914.632437	23.185344
113.154985	3917.349055	23.190362
113.122145	3925.112685	23.195379
113.051341	3953.634212	23.200397
113.411292	3937.299236	23.205415
113.569300	3938.969172	23.210432
113.571964	3940.728382	23.215450
113.708565	3945.423142	23.220467
113.718713	3961.577902	23.225485
114.157132	3958.698931	23.230503
114.114014	3990.612747	23.235520
113.955481	3964.568536	23.240538
114.065642	3986.040671	23.245555
114.159843	3979.001860	23.250573
114.541775	3991.864351	23.255591
114.615468	3991.390030	23.260608
114.561489	4006.673260	23.265626
114.651467	4010.934967	23.270643
115.020395	4014.092610	23.275661
115.112949	4008.325233	23.280679
115.199153	4025.658884	23.285696
114.693336	4036.856096	23.290714
115.194986	4025.183571	23.295731
115.587788	4039.962162	23.300749
115.511841	4046.865082	23.305767
115.865548	4059.607846	23.310784
115.684557	4051.655557	23.315802
115.887512	4061.204273	23.320819
116.233926	4067.842409	23.325837
116.434205	4065.516633	23.330855
116.766760	4073.549313	23.335872
116.412966	4081.105403	23.340890
117.225472	4073.921329	23.345907
116.953901	4069.636574	23.350925
116.989625	4076.450117	23.355943
117.125005	4079.323285	23.360960
117.499176	4064.743228	23.365978
117.714658	4065.120238	23.370995
117.066684	4067.436311	23.376013
117.407362	4068.064745	23.381031
117.451847	4065.280822	23.386048
117.561194	4074.512517	23.391066
117.951227	4091.046568	23.396083
117.771320	4113.308508	23.401101
118.336646	4093.409430	23.406119
118.263239	4094.010285	23.411136
118.220015	4097.897583	23.416154
118.269389	4117.118046	23.421171
118.018999	4096.667027	23.426189
118.543017	4092.788736	23.431207
118.179207	4114.287868	23.436224
118.050944	4117.123634	23.441242
118.541812	4097.299354	23.446259
118.434030	4134.051335	23.451277
118.665900	4127.982443	23.456295
118.654204	4152.726185	23.461312
118.918808	4159.557548	23.466330
119.011522	4164.581896	23.471347
119.163483	4184.001625	23.476365
119.619932	4183.244435	23.481383
119.505450	4167.649561	23.486400
119.475497	4224.956672	23.491418
120.252908	4209.702529	23.496435
119.909178	4216.701719	23.501453
120.480664	4223.021636	23.506471
120.496752	4200.765917	23.511488
120.300801	4221.598118	23.516506
120.632650	4228.264610	23.521523
120.554898	4230.545631	23.526541
120.876212	4224.987909	23.531559
120.964721	4241.287809	23.536576
121.136468	4228.280889	23.541594
121.303585	4216.162831	23.546611
121.637918	4238.677281	23.551629
121.726938	4259.105389	23.556647
121.940686	4251.090834	23.561664
122.079645	4254.676946	23.566682
122.324202	4250.227240	23.571699
122.223191	4260.786613	23.576717
122.437864	4261.174772	23.581735
122.430422	4254.963061	23.586752
122.308588	4259.082408	23.591770
122.344291	4251.223679	23.596787
122.451733	4249.868442	23.601805
122.361570	4256.245893	23.606823
122.374274	4262.400845	23.611840
122.555692	4276.412586	23.616858
122.719607	4272.825302	23.621875
122.486482	4288.701412	23.626893
122.988896	4301.653521	23.631911
123.477353	4310.018607	23.636928
123.369467	4317.512793	23.641946
123.691258	4310.018254	23.646963
123.581612	4307.922787	23.651981
123.658714	4325.576835	23.656999
123.959230	4331.936075	23.662016
123.741758	4327.769265	23.667034
124.095645	4350.079389	23.672051
124.222419	4354.974870	23.677069
124.408685	4365.319381	23.682087
124.850353	4372.281513	23.687104
124.797099	4365.626313	23.692122
125.281767	4378.517602	23.697139
125.117823	4383.933008	23.702157
124.934312	4383.455636	23.707175
125.029146	4361.989493	23.712192
124.998771	4374.592397	23.717210
125.244494	4362.257943	23.722227
125.178275	4380.148089	23.727245
125.517187	4404.319524	23.732263
125.950669	4389.374125	23.737280
125.731124	4401.824715	23.742298
125.824061	4393.037982	23.747315
125.809136	4393.261375	23.752333
125.938441	4433.540589	23.757351
126.106817	4425.651958	23.762368
125.980722	4421.515390	23.767386
126.421802	4439.179188	23.772403
126.378367	4456.862840	23.777421
126.607988	4470.154377	23.782439
126.676746	4451.432160	23.787456
126.929372	4480.115532	23.792474
127.242831	4479.130975	23.797491
127.555228	4484.660046	23.802509
127.424510	4485.074180	23.807527
127.473993	4495.557019	23.812544
127.372291	4494.901401	23.817562
127.396445	4493.514584	23.822579
127.535851	4514.815275	23.827597
127.935737	4515.243134	23.832615
128.573567	4524.043143	23.837632
128.231299	4526.342002	23.842650
128.700144	4538.716767	23.847667
128.832378	4537.797289	23.852685
128.669429	4535.571051	23.857703
128.947377	4525.893354	23.862720
129.215835	4546.529246	23.867738
129.581319	4532.907469	23.872755
129.343477	4536.304364	23.877773
129.335446	4530.984694	23.882791
129.814481	4543.858149	23.887808
130.012859	4546.896002	23.892826
129.955492	4547.694914	23.897843
130.159770	4539.341092	23.902861
130.150577	4548.038184	23.907879
130.642428	4545.174971	23.912896
130.062413	4540.017300	23.917914
130.584616	4545.091294	23.922931
130.488432	4542.199127	23.927949
130.777339	4547.789394	23.932967
130.842763	4561.083596	23.937984
130.867254	4580.021505	23.943002
131.165303	4577.888524	23.948019
130.961773	4564.835734	23.953037
131.226540	4583.715669	23.958055
131.422677	4581.572977	23.963072
131.682989	4576.566070	23.968090
131.571071	4587.707182	23.973107
131.774824	4600.988017	23.978125
131.355626	4602.179742	23.983143
131.918049	4597.796460	23.988160
131.677572	4610.082218	23.993178
131.973964	4630.071862	23.998195
132.178416	4630.039227	24.003213
132.171682	4628.881519	24.008231
132.619518	4622.861374	24.013248
132.791716	4656.992146	24.018266
132.868388	4642.216665	24.023283
133.267026	4673.974209	24.028301
133.045373	4672.441704	24.033319
133.310975	4644.716001	24.038336
133.272044	4658.025358	24.043354
133.066630	4682.136941	24.048371
133.913888	4676.385057	24.053389
133.743031	4675.100117	24.058407
133.882746	4682.463756	24.063424
133.754966	4688.221210	24.068442
134.218367	4697.844453	24.073459
134.471584	4706.046680	24.078477
134.198559	4703.909554	24.083495
134.581340	4711.900753	24.088512
134.699267	4728.989460	24.093530
134.911910	4738.614954	24.098547
135.198952	4747.045450	24.103565
134.903879	4737.864902	24.108583
134.985718	4752.029856	24.113600
135.041952	4755.966762	24.118618
135.422136	4759.317083	24.123635
135.795350	4757.297171	24.128653
135.374191	4782.274036	24.133671
136.119579	4761.756923	24.138688
136.347102	4801.542409	24.143706
136.026665	4808.727750	24.148723
136.630588	4791.747194	24.153741
136.646440	4805.393296	24.158759
137.047276	4795.845295	24.163776
136.868846	4810.929726	24.168794
136.920639	4803.212096	24.173811
137.607831	4792.443158	24.178829
137.043443	4795.427260	24.183847
137.495816	4802.167626	24.188864
137.548719	4817.281258	24.193882
137.483249	4831.578338	24.198899
137.727858	4829.545883	24.203917
137.652963	4825.029729	24.208935
138.109623	4815.474387	24.213952
137.940235	4832.790748	24.218970
138.229153	4840.841038	24.223987
138.389991	4856.653368	24.229005
137.860400	4852.257694	24.234023
138.200716	4849.842601	24.239040
138.206120	4869.513169	24.244058
138.808041	4880.096211	24.249075
138.967682	4881.789598	24.254093
138.974141	4880.252165	24.259111
139.628806	4896.720549	24.264128
139.488903	4918.386537	24.269146
139.641591	4902.427319	24.274163
139.773024	4894.158073	24.279181
139.959125	4896.210684	24.284199
140.181769	4900.500271	24.289216
140.285126	4900.453075	24.294234
140.282557	4900.337809	24.299251
140.581830	4898.834713	24.304269
140.472096	4914.011350	24.309287
140.795298	4920.375885	24.314304
140.963446	4922.666578	24.319322
140.833302	4923.416540	24.324339
141.030967	4920.206829	24.329357
140.832271	4935.348899	24.334375
141.382741	4935.656003	24.339392
141.687485	4934.447820	24.344410
141.472710	4960.467462	24.349427
141.681450	4950.283677	24.354445
141.699302	4953.547070	24.359463
141.919539	4950.458047	24.364480
141.971409	4973.267257	24.369498
142.221210	4979.314691	24.374515
143.127374	4968.974851	24.379533
142.555126	4967.897846	24.384551
142.342103	4987.584520	24.389568
142.587120	4995.979380	24.394586
142.489624	4996.285961	24.399603
142.782010	5002.774234	24.404621
143.427633	5031.748456	24.409639
143.324416	5032.143272	24.414656
143.318484	5030.994058	24.419674
142.939422	5037.503659	24.424691
143.741309	5055.242836	24.429709
143.548542	5068.749376	24.434727
144.035756	5084.022169	24.439744
144.100437	5076.391237	24.444762
144.195155	5099.244158	24.449779
144.327597	5089.453198	24.454797
144.751109	5100.740609	24.459815
144.972670	5106.684823	24.464832
145.350315	5107.799091	24.469850
145.519278	5105.187076	24.474867
145.558951	5099.902074	24.479885
145.868496	5106.142212	24.484903
145.901611	5113.246939	24.489920
145.889528	5105.483482	24.494938
145.880642	5112.487130	24.499955
145.892620	5096.460456	24.504973
146.005815	5125.640120	24.509991
145.992263	5132.359742	24.515008
146.384767	5131.801513	24.520026
146.265069	5141.229311	24.525043
146.611118	5137.515229	24.530061
146.446382	5156.347956	24.535079
147.012322	5158.994564	24.540096
147.223890	5162.924119	24.545114
147.330844	5168.468115	24.550131
147.493548	5159.408622	24.555149
147.498347	5167.741974	24.560167
147.623764	5178.405145	24.565184
147.657557	5190.611467	24.570202
147.457319	5204.397809	24.575219
147.788167	5194.302164	24.580237
148.119519	5209.185356	24.585255
148.143561	5201.845620	24.590272
148.547656	5225.411709	24.595290
148.476301	5231.456173	24.600307
148.688646	5246.470875	24.605325
148.524437	5247.341928	24.610343
148.609858	5251.190924	24.615360
149.023367	5276.429672	24.620378
149.383275	5276.244021	24.625395
149.524732	5263.833397	24.630413
149.909583	5293.274530	24.635431
150.041882	5292.288915	24.640448
150.274265	5301.462431	24.645466
150.279578	5301.662156	24.650483
150.361822	5311.552694	24.655501
150.242280	5313.385836	24.660519
150.365301	5309.298192	24.665536
151.038500	5316.160928	24.670554
150.645671	5333.688936	24.675571
151.081541	5323.832133	24.680589
150.648661	5343.206617	24.685607
150.816757	5351.724870	24.690624
151.389619	5337.783718	24.695642
151.542608	5374.095219	24.700659
151.950314	5361.562604	24.705677
152.245482	5389.610043	24.710695
152.008660	5391.397384	24.715712
152.356867	5385.663444	24.720730
152.295742	5410.528109	24.725747
152.810551	5387.718268	24.730765
152.957294	5386.917578	24.735783
152.692549	5406.495839	24.740800
153.187194	5406.885809	24.745818
153.272231	5426.031496	24.750835
153.346491	5400.216669	24.755853
153.356120	5435.553645	24.760871
153.468823	5423.813807	24.765888
153.851928	5424.047701	24.770906
153.767629	5461.959639	24.775923
153.809217	5437.842938	24.780941
153.840210	5434.681719	24.785959
154.280272	5457.714571	24.790976
154.348155	5477.110084	24.795994
154.317523	5450.869765	24.801011
154.453769	5494.169355	24.806029
154.894255	5476.112693	24.811047
155.103997	5513.475177	24.816064
154.659972	5495.779797	24.821082
155.358961	5481.989115	24.826099
154.956292	5529.116293	24.831117
155.535038	5498.932525	24.836135
155.160256	5541.806311	24.841152
155.661837	5532.926209	24.846170
155.949982	5564.273758	24.851187
155.846257	5556.842504	24.856205
156.102374	5565.620622	24.861223
156.390551	5583.438417	24.866240
156.920000	5586.277375	24.871258
156.965746	5592.636093	24.876275
157.096746	5587.500778	24.881293
157.663693	5600.951970	24.886311
157.884851	5617.347895	24.891328
158.133067	5603.780021	24.896346
157.696586	5628.575094	24.901363
158.038854	5599.990446	24.906381
158.172447	5605.637353	24.911399
158.172087	5605.852147	24.916416
158.192049	5604.697187	24.921434
158.046848	5624.556412	24.926451
158.555282	5629.826518	24.931469
158.836863	5644.161884	24.936487
158.387735	5642.759161	24.941504
158.865488	5645.486006	24.946522
159.101590	5660.081173	24.951539
159.173586	5674.476733	24.956557
159.437856	5669.685175	24.961575
159.400656	5693.847115	24.966592
159.841975	5684.359748	24.971610
159.795730	5716.094503	24.976627
159.955069	5712.156727	24.981645
160.428467	5719.038139	24.986663
160.289954	5741.019800	24.991680
160.545596	5728.466279	24.996698
161.007615	5741.559068	25.001715
160.972371	5756.626354	25.006733
161.294280	5753.997707	25.011751
161.011275	5750.957289	25.016768
161.396340	5760.515056	25.021786
161.611460	5775.036584	25.026803
161.820734	5781.254450	25.031821
162.238227	5784.587264	25.036839
162.526911	5774.687547	25.041856
162.617401	5757.387312	25.046874
162.744505	5755.712545	25.051891
162.474921	5771.559871	25.056909
162.884021	5794.968735	25.061927
163.126853	5796.927464	25.066944
163.512581	5779.746916	25.071962
163.381650	5786.557142	25.076979
163.226908	5808.606002	25.081997
163.617487	5797.560294	25.087015
163.351477	5793.279646	25.092032
163.638271	5809.539445	25.097050
163.539751	5837.117897	25.102067
163.758383	5820.581520	25.107085
164.318385	5824.984377	25.112103
164.311788	5842.005333	25.117120
164.374291	5847.495309	25.122138
164.504784	5851.721197	25.127155
164.168843	5863.903634	25.132173
165.090432	5878.237887	25.137191
164.875785	5888.072302	25.142208
165.424988	5895.361036	25.147226
165.519911	5898.315754	25.152243
165.402056	5906.152200	25.157261
165.567831	5920.669152	25.162279
165.544634	5929.740627	25.167296
165.936753	5933.535396	25.172314
165.983659	5949.175107	25.177331
166.041983	5975.710784	25.182349
166.372767	5971.912392	25.187367
166.801002	6003.126825	25.192384
167.134783	5999.694564	25.197402
167.113162	5994.120057	25.202419
167.457559	6021.190026	25.207437
167.882743	5993.284510	25.212455
167.800179	6032.234546	25.217472
168.151889	6008.997384	25.222490
168.337419	6015.655772	25.227507
168.426710	6025.922512	25.232525
168.809111	6021.160785	25.237543
168.639771	6022.411117	25.242560
168.838558	6018.790318	25.247578
168.879527	6047.104545	25.252595
169.128589	6056.804560	25.257613
169.478244	6044.043034	25.262631
169.039003	6047.219052	25.267648
169.357320	6066.001097	25.272666
170.088313	6065.136331	25.277683
169.675702	6068.416677	25.282701
170.103868	6074.007358	25.287719
170.213746	6086.184196	25.292736
170.454400	6092.690644	25.297754
170.601603	6103.482398	25.302771
170.589990	6103.584130	25.307789
170.484232	6100.439851	25.312807
170.428947	6120.124125	25.317824
170.709141	6136.601691	25.322842
171.612370	6153.079857	25.327859
171.347324	6170.606574	25.332877
171.955753	6161.759417	25.337895
171.807894	6159.879834	25.342912
172.080611	6166.848526	25.347930
172.125860	6161.710163	25.352947
172.330505	6176.193633	25.357965
172.660983	6202.307905	25.362983
172.584952	6173.736917	25.368000
172.483697	6204.225068	25.373018
172.868225	6191.354792	25.378035
172.938399	6219.558483	25.383053
173.167763	6228.465569	25.388071
173.306476	6210.443541	25.393088
173.757017	6240.997993	25.398106
174.085332	6240.972362	25.403123
173.735334	6246.217490	25.408141
174.093344	6249.013110	25.413159
173.900704	6274.520938	25.418176
174.081666	6277.079657	25.423194
174.786649	6298.501248	25.428211
174.901381	6303.330067	25.433229
175.018692	6295.668872	25.438247
175.113421	6295.251707	25.443264
174.846377	6336.637041	25.448282
175.640934	6320.428408	25.453299
175.725662	6331.486769	25.458317
176.104408	6343.329856	25.463335
176.298907	6362.161916	25.468352
176.329310	6356.224154	25.473370
176.735951	6354.004380	25.478387
176.881337	6368.787012	25.483405
176.907313	6364.653184	25.488423
177.135313	6381.768746	25.493440
177.010454	6374.455314	25.498458
177.482658	6383.243529	25.503475
177.557167	6388.943428	25.508493
177.694209	6393.076379	25.513511
178.164792	6406.774984	25.518528
178.003889	6408.708477	25.523546
178.577344	6411.214084	25.528563
177.996623	6410.473465	25.533581
178.660025	6427.498421	25.538599
178.974945	6439.205425	25.543616
178.534779	6431.472543	25.548634
179.311758	6432.122798	25.553651
179.352715	6458.010679	25.558669
180.073797	6452.632290	25.563687
179.874428	6457.672522	25.568704
179.753326	6466.731613	25.573722
180.098248	6445.244596	25.578739
180.092930	6472.589082	25.583757
180.399700	6475.805175	25.588775
180.656340	6493.675521	25.593792
180.598762	6491.082074	25.598810
180.832343	6480.135633	25.603827
180.923280	6527.156608	25.608845
180.945936	6503.532910	25.613863
181.182880	6514.464862	25.618880
181.168018	6545.235762	25.623898
181.806876	6528.361740	25.628915
181.644196	6536.659626	25.633933
182.027413	6551.564236	25.638951
182.252905	6555.329875	25.643968
182.211378	6573.780492	25.648986
182.555770	6583.758332	25.654003
182.315573	6580.766773	25.659021
182.913672	6592.553061	25.664039
182.986073	6613.714842	25.669056
182.837475	6596.995398	25.674074
183.649848	6624.978467	25.679092
183.837034	6637.744523	25.684109
184.015192	6620.051656	25.689127
184.259869	6637.667599	25.694144
184.279454	6627.279153	25.699162
184.339818	6666.679344	25.704180
184.531472	6666.547261	25.709197
184.746345	6659.435223	25.714215
184.911757	6664.733648	25.719232
184.795669	6687.031778	25.724250
185.035192	6680.581404	25.729268
185.204263	6719.571021	25.734285
185.197414	6714.904179	25.739303
185.680372	6720.930899	25.744320
185.986621	6734.767732	25.749338
186.408550	6737.630360	25.754356
186.019694	6758.787209	25.759373
186.503281	6761.412635	25.764391
186.825385	6765.943403	25.769408
186.874681	6796.366284	25.774426
187.071278	6786.298833	25.779444
187.372771	6793.858037	25.784461
187.377625	6807.017584	25.789479
187.863267	6831.059474	25.794496
188.109453	6820.652861	25.799514
188.075495	6850.929412	25.804532
188.366183	6851.567528	25.809549
188.601505	6844.135071	25.814567
188.700711	6844.306473	25.819584
188.673464	6872.996646	25.824602
189.376273	6853.696657	25.829620
189.268272	6894.389432	25.834637
189.325503	6867.426849	25.839655
189.595033	6903.804572	25.844672
189.870233	6892.356310	25.849690
190.180685	6891.256431	25.854708
189.987641	6932.057281	25.859725
190.276262	6910.085257	25.864743
190.711731	6926.786788	25.869760
190.544263	6921.477512	25.874778
190.938721	6961.080925	25.879796
191.353634	6946.397918	25.884813
191.173155	6976.741358	25.889831
191.384273	6967.977528	25.894848
191.490809	6964.403467	25.899866
191.900576	6967.328663	25.904884
191.922964	6996.836497	25.909901
191.946462	6973.165496	25.914919
192.324820	7004.063487	25.919936
192.639536	7005.095106	25.924954
192.771904	7007.750608	25.929972
192.989911	7017.980994	25.934989
192.973015	7004.013509	25.940007
193.535846	7026.396673	25.945024
193.467750	7036.051911	25.950042
193.881786	7015.351640	25.955060
193.828539	7033.164254	25.960077
193.835372	7048.230082	25.965095
194.499307	7051.085662	25.970112
194.034541	7079.318054	25.975130
194.380356	7078.605132	25.980148
194.666907	7074.497228	25.985165
194.737175	7093.998340	25.990183
195.076635	7115.178058	25.995200
195.094523	7119.626042	26.000218
195.192661	7104.256947	26.005236
195.303810	7152.553644	26.010253
195.869223	7157.553225	26.015271
196.080464	7151.067032	26.020288
196.174316	7194.918891	26.025306
196.408559	7167.070725	26.030324
196.755885	7208.222855	26.035341
196.645075	7210.247600	26.040359
197.380834	7186.457985	26.045376
197.337497	7190.478295	26.050394
197.713261	7237.593805	26.055412
197.936040	7234.477947	26.060429
197.681630	7250.524276	26.065447
198.312654	7216.214528	26.070464
198.013142	7283.429535	26.075482
198.102983	7269.598209	26.080500
198.798993	7275.391348	26.085517
198.893320	7320.979181	26.090535
198.765465	7307.135319	26.095552
199.263031	7309.500548	26.100570
199.728547	7344.488518	26.105588
199.807113	7319.538287	26.110605
199.897304	7361.584728	26.115623
200.157533	7348.328856	26.120640
200.578362	7345.571655	26.125658
200.556543	7378.299022	26.130676
200.624303	7345.197611	26.135693
201.101202	7397.281899	26.140711
201.328602	7373.682397	26.145728
201.398992	7397.909433	26.150746
201.761712	7378.971413	26.155764
201.777892	7405.627313	26.160781
201.805141	7421.644660	26.165799
201.985567	7398.098243	26.170816
201.908642	7419.898690	26.175834
202.656491	7417.075178	26.180852
202.871076	7428.839094	26.185869
202.770752	7440.720100	26.190887
202.739786	7456.649988	26.195904
203.109965	7444.809279	26.200922
203.490819	7469.525900	26.205940
203.604820	7452.203417	26.210957
203.218304	7495.490711	26.215975
204.038612	7492.031695	26.220992
203.732379	7490.932525	26.226010
204.560130	7542.419277	26.231028
204.423454	7522.311232	26.236045
204.562588	7550.296385	26.241063
204.560569	7538.309581	26.246080
204.897967	7578.597255	26.251098
205.068539	7588.380820	26.256116
205.671400	7573.495709	26.261133
205.484614	7629.309897	26.266151
206.047901	7611.846362	26.271168
206.361701	7592.244717	26.276186
206.242642	7594.493498	26.281204
206.789152	7655.185585	26.286221
206.950878	7644.038878	26.291239
207.251831	7665.979296	26.296256
207.383985	7650.586903	26.301274
207.384378	7676.639955	26.306292
208.069529	7663.398679	26.311309
207.404093	7679.217511	26.316327
208.302956	7690.445303	26.321344
208.556540	7684.828647	26.326362
208.694764	7698.258846	26.331380
209.004191	7715.949155	26.336397
209.046527	7712.788789	26.341415
209.189710	7712.573944	26.346432
209.488701	7725.231844	26.351450
209.435442	7744.279837	26.356468
210.092289	7749.412971	26.361485
209.923172	7746.564057	26.366503
209.925837	7763.042835	26.371520
210.485511	7786.646447	26.376538
210.547655	7786.586936	26.381556
210.970279	7789.745511	26.386573
210.736879	7818.069881	26.391591
210.903968	7814.747977	26.396608
211.504949	7802.752955	26.401626
211.236993	7865.038452	26.406644
211.941750	7861.365662	26.411661
211.840468	7859.972562	26.416679
212.377542	7876.135729	26.421696
212.718666	7867.888052	26.426714
213.111158	7892.186504	26.431732
213.084113	7883.777985	26.436749
212.937285	7923.185429	26.441767
213.176310	7894.267410	26.446784
213.311649	7920.660533	26.451802
213.716677	7924.740177	26.456820
213.929546	7907.247971	26.461837
213.661363	7957.606312	26.466855
213.908168	7945.108986	26.471872
214.500052	7957.953296	26.476890
214.206970	7994.530396	26.481908
214.753678	7976.489969	26.486925
214.507331	7994.987592	26.491943
215.084721	8024.892896	26.496960
215.384970	8018.496001	26.501978
215.644102	8037.607873	26.506996
216.402152	8050.109464	26.512013
216.014030	8044.267648	26.517031
216.140705	8082.568106	26.522048
216.607717	8070.009605	26.527066
216.577290	8096.157218	26.532084
216.926560	8105.019966	26.537101
217.192309	8116.562250	26.542119
217.456232	8129.647047	26.547136
217.541227	8132.987778	26.552154
217.633341	8158.655662	26.557172
218.257981	8152.557143	26.562189
218.239278	8167.075023	26.567207
218.461797	8190.160204	26.572224
218.966146	8170.100167	26.577242
219.071356	8207.813448	26.582260
219.310729	8205.365139	26.587277
219.328014	8205.825802	26.592295
219.669546	8230.103031	26.597312
219.664595	8238.500252	26.602330
220.015381	8257.342070	26.607348
220.536753	8249.518675	26.612365
220.614017	8278.067430	26.617383
220.586219	8278.156020	26.622400
220.931368	8289.598441	26.627418
220.862360	8307.974545	26.632436
221.016485	8307.144203	26.637453
221.921947	8303.614783	26.642471
222.053635	8358.857677	26.647488
221.965367	8345.092302	26.652506
222.188010	8347.149809	26.657524
223.313059	8340.842399	26.662541
223.686968	8339.382943	26.667559
223.805659	8346.867436	26.672576
224.010009	8384.005119	26.677594
223.941674	8381.735666	26.682612
224.373884	8334.871636	26.687629
224.258267	8379.711690	26.692647
224.615200	8345.107059	26.697664
224.512914	8377.107447	26.702682
224.433635	8385.287625	26.707700
224.764363	8375.669835	26.712717
224.455095	8401.169214	26.717735
225.228617	8397.667101	26.722752
225.391253	8415.838811	26.727770
225.078382	8425.944710	26.732788
225.506550	8452.666641	26.737805
225.686004	8445.356392	26.742823
225.942988	8477.567255	26.747840
225.940096	8482.844378	26.752858
226.177788	8512.398010	26.757876
226.963417	8520.003675	26.762893
226.638007	8525.799625	26.767911
226.795180	8552.251762	26.772928
227.116620	8570.207923	26.777946
227.457305	8571.270930	26.782964
227.695142	8600.609112	26.787981
227.993926	8589.117237	26.792999
228.009963	8638.077578	26.798016
228.155868	8612.920090	26.803034
228.223877	8670.217787	26.808052
228.966417	8653.594749	26.813069
229.129076	8677.872110	26.818087
229.136454	8706.838066	26.823104
230.026818	8710.324373	26.828122
229.884896	8709.158782	26.833140
230.091501	8747.803876	26.838157
230.634121	8731.152032	26.843175
230.705930	8766.750636	26.848192
231.210557	8758.605456	26.853210
231.139394	8774.107230	26.858228
231.477505	8792.577980	26.863245
231.972229	8774.912355	26.868263
231.842410	8819.185505	26.873280
232.285693	8783.791806	26.878298
232.532977	8840.533584	26.883316
232.554440	8827.308171	26.888333
233.131440	8841.986696	26.893351
232.988368	8859.729256	26.898368
233.612681	8845.653893	26.903386
233.322338	8893.963588	26.908404
233.790235	8862.987280	26.913421
233.887852	8888.923084	26.918439
233.982589	8937.622420	26.923456
234.446420	8925.073944	26.928474
234.972723	8902.507921	26.933492
235.077283	8959.630149	26.938509
234.955756	8939.819938	26.943527
235.253634	8968.976160	26.948544
235.216745	8973.021888	26.953562
235.661367	8972.413532	26.958580
235.862501	9024.270102	26.963597
236.265263	8993.868108	26.968615
236.567182	9041.439405	26.973632
236.701667	9027.464382	26.978650
236.683883	9065.118781	26.983668
237.282180	9065.956627	26.988685
237.485536	9078.878800	26.993703
237.640921	9098.249363	26.998720
238.224709	9091.639208	27.003738
238.244589	9095.531524	27.008756
238.177343	9112.453762	27.013773
238.899396	9097.519033	27.018791
238.672095	9145.969395	27.023808
239.298027	9113.536406	27.028826
239.306604	9173.807384	27.033844
239.689703	9168.307631	27.038861
239.821118	9157.763066	27.043879
239.509286	9185.868033	27.048896
240.252651	9176.678915	27.053914
240.215653	9231.179586	27.058932
240.327890	9226.386741	27.063949
240.427157	9226.527476	27.068967
241.145587	9233.047286	27.073984
241.186208	9237.406507	27.079002
241.510718	9291.247790	27.084020
242.015955	9301.869126	27.089037
242.335793	9281.833085	27.094055
242.368932	9302.437986	27.099072
242.974723	9327.533789	27.104090
242.959918	9317.742670	27.109108
243.158546	9357.468674	27.114125
243.496955	9331.378676	27.119143
243.434846	9362.594156	27.124160
243.975033	9363.204819	27.129178
243.981777	9389.456577	27.134196
244.481337	9398.880425	27.139213
244.736039	9403.944871	27.144231
244.646617	9427.474756	27.149248
245.247760	9419.151341	27.154266
245.458963	9428.790752	27.159284
245.782152	9425.770968	27.164301
246.048501	9461.032138	27.169319
245.992838	9460.397281	27.174336
246.344614	9461.906343	27.179354
246.493271	9498.848719	27.184372
246.836567	9480.086232	27.189389
246.486667	9529.045656	27.194407
247.085982	9523.504228	27.199424
247.535692	9563.091210	27.204442
247.521754	9567.931376	27.209460
247.974763	9552.226985	27.214477
248.047342	9614.891999	27.219495
247.896237	9603.075243	27.224512
248.354373	9591.871183	27.229530
248.858196	9626.756908	27.234548
249.118122	9679.121418	27.239565
249.249661	9659.816040	27.244583
249.307113	9663.213835	27.249600
249.846839	9652.293396	27.254618
250.296060	9713.490584	27.259636
250.227852	9714.687714	27.264653
250.625243	9736.650438	27.269671
250.904493	9740.115197	27.274688
251.269758	9759.234788	27.279706
251.466862	9747.316378	27.284724
251.631890	9791.359686	27.289741
252.119982	9789.990888	27.294759
251.966273	9789.472766	27.299776
252.032747	9804.963896	27.304794
252.627677	9814.692301	27.309812
252.679281	9818.365310	27.314829
252.843863	9863.087630	27.319847
252.645635	9869.909262	27.324864
253.400802	9857.675563	27.329882
253.518151	9896.677810	27.334900
253.961461	9901.834732	27.339917
254.593021	9906.374200	27.344935
254.630738	9949.491188	27.349952
255.041814	9937.246171	27.354970
255.290595	9951.313544	27.359988
255.708067	9969.865176	27.365005
255.936567	9968.046298	27.370023
255.941428	9991.020230	27.375040
256.278778	9997.252511	27.380058
256.351916	10014.919084	27.385076
256.539472	10015.026081	27.390093
256.989926	10040.042788	27.395111
257.059921	10036.708331	27.400128
257.536180	10079.063278	27.405146
257.851424	10059.911068	27.410164
257.749850	10099.387460	27.415181
258.144203	10079.373106	27.420199
258.245135	10132.216643	27.425216
259.074966	10105.048727	27.430234
259.021769	10138.700397	27.435252
259.651168	10145.325700	27.440269
260.068812	10129.288352	27.445287
259.576183	10178.535090	27.450304
259.872816	10152.011210	27.455322
260.564711	10197.675871	27.460340
260.292156	10195.642514	27.465357
261.085936	10198.579163	27.470375
261.078344	10224.473063	27.475392
261.454523	10208.699968	27.480410
261.632965	10248.390632	27.485428
261.962266	10265.615715	27.490445
262.200167	10258.156766	27.495463
262.012754	10295.191661	27.500480
262.591852	10277.452595	27.505498
262.573985	10325.048255	27.510516
262.892521	10308.287167	27.515533
263.353132	10343.714617	27.520551
263.503135	10383.558907	27.525568
263.789061	10357.320466	27.530586
263.798937	10415.638269	27.535604
264.493715	10396.850882	27.540621
264.872264	10433.937165	27.545639
265.097630	10412.353735	27.550656
265.194511	10459.078854	27.555674
265.839294	10448.576290	27.560692
265.646469	10480.307569	27.565709
265.787097	10473.017872	27.570727
266.083788	10474.644424	27.575744
266.674858	10471.918164	27.580762
266.600672	10516.512473	27.585780
266.691247	10513.903364	27.590797
267.466872	10517.417856	27.595815
267.392999	10576.259587	27.600832
267.798116	10546.114570	27.605850
268.092374	10551.432805	27.610868
268.378033	10613.950766	27.615885
268.308057	10601.863343	27.620903
268.432678	10602.880675	27.625920
268.656443	10608.270764	27.630938
269.225286	10598.752508	27.635956
269.286512	10677.421369	27.640973
269.604833	10674.505604	27.645991
270.158608	10680.462074	27.651008
270.089277	10711.563854	27.656026
271.063530	10695.123576	27.661044
270.596423	10764.531739	27.666061
271.018610	10757.613733	27.671079
271.768949	10733.225965	27.676096
271.873372	10759.945001	27.681114
272.301310	10772.538511	27.686132
272.164239	10787.263918	27.691149
272.176964	10841.268282	27.696167
272.487788	10875.489230	27.701184
272.286686	10866.989123	27.706202
273.529782	10856.715938	27.711220
273.482455	10925.638468	27.716237
273.778623	10944.034358	27.721255
274.218815	10930.710050	27.726272
274.427434	10948.020868	27.731290
274.724418	10988.497716	27.736308
274.715102	10993.693325	27.741325
275.358048	11015.492868	27.746343
275.676922	11051.025247	27.751360
275.817705	11020.205251	27.756378
276.148708	11071.717269	27.761396
276.518771	11072.638061	27.766413
276.892239	11086.805857	27.771431
277.324930	11092.224599	27.776448
277.165611	11091.571172	27.781466
277.731600	11117.108390	27.786484
277.894975	11113.410958	27.791501
278.363130	11132.584768	27.796519
278.478885	11161.775862	27.801536
278.644630	11167.985227	27.806554
279.159264	11159.686460	27.811572
279.250410	11195.489612	27.816589
279.591642	11202.069637	27.821607
280.104270	11218.902213	27.826624
280.326336	11213.400635	27.831642
280.646906	11213.253884	27.836660
280.542291	11245.048657	27.841677
281.011361	11237.085293	27.846695
281.231908	11260.881868	27.851712
281.267078	11262.478969	27.856730
281.499693	11293.758513	27.861748
281.394372	11309.442668	27.866765
281.351187	11303.376552	27.871783
281.890170	11347.774849	27.876800
282.230510	11349.583819	27.881818
282.529135	11393.738222	27.886836
282.672656	11388.226867	27.891853
283.253081	11421.379622	27.896871
283.652684	11469.601389	27.901888
283.719489	11476.030489	27.906906
284.500943	11474.552227	27.911924
284.609596	11497.335227	27.916941
284.993967	11529.376518	27.921959
285.578874	11517.716400	27.926976
285.404872	11568.742773	27.931994
285.806977	11548.152289	27.937012
285.844183	11588.386465	27.942029
286.349387	11583.375590	27.947047
286.820651	11580.709556	27.952064
286.859747	11636.487303	27.957082
287.184347	11616.761824	27.962100
287.646817	11631.105229	27.967117
288.068425	11660.734135	27.972135
288.603325	11656.145467	27.977152
288.680706	11698.092796	27.982170
288.972495	11681.458804	27.987188
289.225644	11687.784312	27.992205
289.856953	11719.966488	27.997223
290.094446	11688.661824	28.002240
289.970978	11741.649483	28.007258
290.752826	11707.725345	28.012276
291.035880	11749.735661	28.017293
290.665031	11748.053816	28.022311
290.786521	11764.893075	28.027328
290.933443	11792.284016	28.032346
291.727748	11779.990602	28.037364
292.008496	11857.402460	28.042381
291.876725	11839.524990	28.047399
292.784823	11826.623516	28.052416
292.444057	11888.567789	28.057434
293.197623	11882.793548	28.062452
293.447971	11913.009834	28.067469
293.387990	11927.477326	28.072487
294.117640	11912.543351	28.077504
294.022387	11987.815237	28.082522
294.706105	11955.351597	28.087540
294.583158	12017.362814	28.092557
294.745997	11996.101123	28.097575
295.313659	12043.769045	28.102592
295.281954	12031.345783	28.107610
295.921115	12083.583056	28.112628
296.062640	12061.484493	28.117645
296.305733	12102.703698	28.122663
296.708000	12116.278375	28.127680
297.066003	12111.018864	28.132698
297.159780	12129.360706	28.137716
297.662511	12120.801623	28.142733
297.854088	12183.629149	28.147751
298.394065	12157.910628	28.152768
298.429011	12210.168690	28.157786
298.403327	12204.575591	28.162804
298.797614	12200.797411	28.167821
298.962912	12266.630125	28.172839
299.494033	12239.609308	28.177856
299.705903	12295.013476	28.182874
300.207662	12296.531796	28.187892
300.427530	12323.864654	28.192909
300.740797	12364.313674	28.197927
300.884938	12364.030541	28.202944
301.508457	12392.151973	28.207962
301.912200	12412.105466	28.212980
302.276396	12429.391812	28.217997
301.995482	12448.478312	28.223015
302.519341	12437.389192	28.228032
302.849010	12478.766417	28.233050
303.377631	12493.602255	28.238068
303.640802	12511.786514	28.243085
303.543345	12543.757997	28.248103
304.213629	12534.179478	28.253120
304.153239	12579.940579	28.258138
304.116467	12582.554383	28.263156
305.317596	12609.334086	28.268173
305.325104	12622.172661	28.273191
305.783941	12654.395143	28.278208
305.860606	12647.131716	28.283226
306.678300	12689.130071	28.288244
306.653565	12694.367683	28.293261
307.155946	12701.120637	28.298279
307.900476	12726.350554	28.303296
307.687138	12730.167838	28.308314
308.134119	12737.411727	28.313332
308.273865	12768.346281	28.318349
308.344725	12766.197816	28.323367
308.881637	12818.825038	28.328384
309.092141	12823.552358	28.333402
309.789032	12814.204766	28.338420
309.488953	12862.305579	28.343437
309.502064	12848.246012	28.348455
310.275290	12907.337247	28.353472
310.292843	12901.274582	28.358490
310.404047	12946.002548	28.363508
310.998149	12948.813194	28.368525
311.318216	12964.273056	28.373543
311.782038	12998.795570	28.378560
312.187815	13002.217906	28.383578
312.571394	13007.364378	28.388596
313.057011	13043.236149	28.393613
312.963190	13045.144044	28.398631
313.572814	13048.998882	28.403648
313.593029	13087.997704	28.408666
313.678415	13073.663714	28.413684
314.400868	13115.217585	28.418701
314.801495	13099.454323	28.423719
314.910679	13150.933809	28.428736
315.044778	13143.797751	28.433754
315.454140	13176.168547	28.438772
316.031343	13159.206652	28.443789
316.037575	13207.117860	28.448807
316.259062	13249.226173	28.453824
316.246066	13236.675759	28.458842
316.787233	13263.272744	28.463860
317.097414	13285.142193	28.468877
317.687497	13284.269659	28.473895
317.927018	13330.970491	28.478912
318.326810	13326.306641	28.483930
318.519604	13376.302644	28.488948
318.932960	13370.727694	28.493965
319.176406	13413.939848	28.498983
319.916650	13438.407936	28.504000
320.334029	13427.972640	28.509018
320.245690	13481.708932	28.514036
320.724102	13453.671698	28.519053
320.821398	13512.126824	28.524071
321.362845	13481.868262	28.529088
321.525638	13540.506101	28.534106
322.133098	13550.157422	28.539124
321.985757	13550.908568	28.544141
322.314343	13601.373261	28.549159
322.857365	13585.923106	28.554176
323.238511	13609.534452	28.559194
323.343720	13642.501575	28.564212
323.608060	13661.434016	28.569229
324.077098	13658.667040	28.574247
324.236685	13702.529185	28.579264
324.442142	13705.122288	28.584282
324.772931	13764.534535	28.589300
325.617892	13750.680424	28.594317
325.321227	13800.922700	28.599335
326.327722	13811.136961	28.604352
326.654352	13826.533097	28.609370
326.492846	13846.283388	28.614388
327.056255	13865.025161	28.619405
327.197140	13886.905534	28.624423
327.761796	13908.671666	28.629440
327.885903	13932.651832	28.634458
328.421522	13951.774201	28.639476
328.866361	13962.376603	28.644493
329.424624	13993.841149	28.649511
330.371625	13964.132454	28.654528
331.056594	13963.202162	28.659546
330.989374	13971.429586	28.664564
331.340252	13963.608119	28.669581
331.418652	13945.144553	28.674599
331.450993	13971.916462	28.679616
331.545853	13983.751541	28.684634
331.941621	13999.978888	28.689652
332.542960	13999.341066	28.694669
332.577288	14023.102884	28.699687
332.749503	14014.708087	28.704704
332.944782	14058.521686	28.709722
333.049034	14045.080049	28.714740
333.359140	14091.677510	28.719757
333.523869	14087.261458	28.724775
333.807733	14135.567129	28.729792
334.040829	14152.772926	28.734810
334.013013	14168.810066	28.739828
334.600456	14203.970143	28.744845
335.125740	14227.748497	28.749863
335.278750	14273.007715	28.754880
336.208318	14263.639168	28.759898
335.972212	14323.978557	28.764916
336.481519	14308.140352	28.769933
337.106981	14361.822270	28.774951
337.294287	14356.349803	28.779968
337.817698	14405.078154	28.784986
338.186562	14406.859839	28.790004
338.352300	14437.751727	28.795021
338.869900	14457.237245	28.800039
338.590647	14473.690061	28.805056
339.562981	14511.271175	28.810074
339.860703	14514.052117	28.815092
340.314136	14555.886007	28.820109
340.845011	14542.994667	28.825127
340.934957	14607.708015	28.830144
341.445805	14615.342916	28.835162
341.556369	14611.989087	28.840180
342.260731	14630.871111	28.845197
342.488419	14688.213321	28.850215
342.530423	14674.571364	28.855232
343.295750	14672.293069	28.860250
343.275730	14737.896596	28.865268
343.849977	14705.957616	28.870285
343.785723	14773.518600	28.875303
343.828762	14781.634425	28.880320
344.721681	14775.100698	28.885338
344.379563	14835.225177	28.890356
345.233419	14831.412287	28.895373
345.327317	14893.826235	28.900391
345.705058	14895.695912	28.905408
346.530155	14898.641439	28.910426
346.443768	14943.264076	28.915444
346.778997	14966.581971	28.920461
347.502290	14966.647136	28.925479
347.775583	15015.062267	28.930496
348.421943	15023.666474	28.935514
347.890870	15050.880463	28.940532
348.940886	15048.214707	28.945549
349.387638	15087.948400	28.950567
348.998227	15094.489399	28.955584
349.882210	15086.817413	28.960602
350.195221	15142.585495	28.965620
350.423260	15149.086497	28.970637
350.666509	15154.640721	28.975655
350.774067	15185.318349	28.980672
351.410721	15198.829119	28.985690
351.318167	15249.110532	28.990708
351.992309	15241.429279	28.995725
352.284251	15256.694137	29.000743
352.305004	15326.819089	29.005760
352.981785	15313.919600	29.010778
353.536815	15332.032188	29.015796
353.756612	15387.861602	29.020813
354.156980	15398.455172	29.025831
354.199883	15412.921284	29.030848
354.939789	15454.175686	29.035866
354.822482	15465.839668	29.040884
355.435798	15503.693292	29.045901
356.108483	15500.708350	29.050919
356.255782	15560.804615	29.055936
356.773283	15569.503471	29.060954
357.111710	15570.830505	29.065972
357.696830	15620.729120	29.070989
358.257551	15633.933942	29.076007
358.205906	15652.921869	29.081024
358.973432	15679.373746	29.086042
359.033308	15690.227445	29.091060
359.746880	15719.858390	29.096077
360.093126	15732.678174	29.101095
360.165937	15761.995550	29.106112
360.433752	15763.506751	29.111130
360.702166	15797.262584	29.116148
360.854476	15790.842722	29.121165
361.121974	15852.998016	29.126183
361.601721	15853.856974	29.131200
362.426757	15879.151836	29.136218
362.181877	15907.295652	29.141236
362.970896	15908.588011	29.146253
363.184652	15969.916187	29.151271
363.487973	15979.030931	29.156288
363.854594	15997.829328	29.161306
363.895731	16043.218352	29.166324
364.629939	16060.043742	29.171341
364.945182	16075.656624	29.176359
365.272002	16117.931223	29.181376
365.612694	16155.152171	29.186394
366.071211	16153.822995	29.191412
366.615556	16183.303590	29.196429
366.922648	16207.589895	29.201447
367.011888	16236.578351	29.206464
367.580837	16244.747539	29.211482
368.030345	16264.446479	29.216500
368.168291	16288.399495	29.221517
368.656307	16296.416676	29.226535
368.621245	16328.336036	29.231552
369.366770	16337.878378	29.236570
369.390143	16363.528228	29.241588
369.670546	16393.883630	29.246605
370.651570	16414.982075	29.251623
370.535253	16427.581613	29.256640
371.058218	16477.205859	29.261658
371.360584	16469.378754	29.266676
371.592894	16519.810357	29.271693
372.295361	16524.629508	29.276711
372.233661	16563.756128	29.281728
373.172837	16575.845716	29.286746
373.288657	16617.368029	29.291764
373.832134	16615.057706	29.296781
374.496956	16649.919787	29.301799
374.692241	16676.643783	29.306816
375.150426	16668.501240	29.311834
375.530458	16716.150309	29.316852
375.795659	16736.407103	29.321869
376.498675	16720.781296	29.326887
376.626500	16789.554609	29.331904
376.923462	16769.059887	29.336922
377.082264	16821.597601	29.341940
377.687747	16813.774771	29.346957
377.796956	16862.866865	29.351975
377.809576	16856.922304	29.356992
378.352672	16919.070857	29.362010
378.867794	16925.372559	29.367028
378.966284	16962.464491	29.372045
379.847361	16966.876435	29.377063
379.735642	17042.490943	29.382080
380.427399	17023.083623	29.387098
380.838353	17084.077074	29.392116
380.902305	17093.683230	29.397133
381.904764	17093.490782	29.402151
381.856819	17169.487830	29.407168
382.250856	17160.337061	29.412186
382.619873	17197.694879	29.417204
383.124175	17241.292361	29.422221
383.903238	17225.937955	29.427239
384.007858	17300.413861	29.432256
384.336849	17291.587324	29.437274
384.375146	17338.840457	29.442292
385.005200	17350.329396	29.447309
385.739751	17404.891114	29.452327
385.905124	17386.090987	29.457344
386.412643	17439.572579	29.462362
386.534948	17451.643242	29.467380
387.330207	17443.709749	29.472397
387.865872	17508.588177	29.477415
387.783777	17506.155581	29.482432
388.604182	17519.079339	29.487450
388.757585	17550.351074	29.492468
389.216703	17545.783004	29.497485
390.050057	17583.311840	29.502503
389.758051	17610.328469	29.507520
390.399431	17601.013631	29.512538
390.663506	17642.675104	29.517556
390.704272	17645.665570	29.522573
391.381576	17656.840741	29.527591
391.494197	17719.206572	29.532608
392.041270	17709.107940	29.537626
392.367433	17751.265285	29.542644
392.594789	17754.004404	29.547661
393.021554	17803.388033	29.552679
393.499796	17801.797927	29.557696
393.950806	17862.347944	29.562714
394.103078	17872.010191	29.567732
394.785815	17899.542825	29.572749
394.828483	17914.390924	29.577767
395.186549	17952.434159	29.582784
395.544439	17983.375779	29.587802
396.312867	17983.021819	29.592820
396.268734	18049.558785	29.597837
397.143622	18038.966787	29.602855
397.433444	18099.362913	29.607872
398.062659	18119.592261	29.612890
398.329835	18138.158544	29.617908
399.084008	18145.917469	29.622925
399.158011	18189.436594	29.627943
399.743189	18207.623171	29.632960
399.975462	18228.724929	29.637978
400.499729	18258.148332	29.642996
400.796687	18286.866309	29.648013
401.140680	18298.360599	29.653031
401.545920	18325.137061	29.658048
401.820289	18363.520614	29.663066
402.121784	18368.175520	29.668084
402.487345	18410.862616	29.673101
403.242194	18439.741767	29.678119
403.352638	18474.723870	29.683136
403.653988	18482.059858	29.688154
404.158497	18534.074497	29.693172
404.404718	18554.933931	29.698189
404.934176	18585.118922	29.703207
405.611618	18594.971754	29.708224
406.176469	18645.231913	29.713242
406.411444	18658.573731	29.718260
406.829378	18680.881540	29.723277
407.736111	18703.212283	29.728295
408.235113	18709.554303	29.733312
408.211003	18770.319199	29.738330
408.788478	18753.567483	29.743348
408.857155	18756.038368	29.748365
409.083260	18820.902526	29.753383
409.229084	18852.646006	29.758400
409.722690	18857.347222	29.763418
410.566119	18867.537954	29.768436
410.953854	18888.948910	29.773453
411.800351	18890.818718	29.778471
411.677178	18966.568644	29.783488
411.510184	18978.516908	29.788506
412.289217	18967.152553	29.793524
412.466068	19052.610635	29.798541
412.722654	19081.129820	29.803559
413.157428	19114.804193	29.808576
413.593180	19137.171631	29.813594
413.814903	19146.048598	29.818612
414.401493	19174.482695	29.823629
414.853261	19234.007417	29.828647
414.821736	19242.135797	29.833664
415.586330	19247.766023	29.838682
416.044474	19330.800053	29.843700
416.418002	19343.055396	29.848717
416.931842	19381.014714	29.853735
417.292820	19429.485431	29.858752
418.245122	19423.423237	29.863770
418.608920	19478.682853	29.868788
418.589107	19494.860574	29.873805
419.772601	19535.278233	29.878823
419.909422	19551.202700	29.883840
420.144718	19587.436360	29.888858
420.917230	19592.172896	29.893876
421.365227	19615.685186	29.898893
421.841536	19666.318676	29.903911
422.020955	19693.863043	29.908928
422.423981	19684.792054	29.913946
422.880286	19739.944152	29.918964
422.942383	19752.397478	29.923981
423.686924	19799.540056	29.928999
423.818723	19812.025240	29.934016
424.295101	19871.168532	29.939034
425.486142	19864.610234	29.944052
425.213774	19934.232746	29.949069
425.725598	19918.794665	29.954087
426.435522	19968.048128	29.959104
426.889355	19964.320422	29.964122
427.160643	20017.291415	29.969140
427.461477	20016.896181	29.974157
428.269504	20087.047678	29.979175
428.422167	20098.640725	29.984192
428.894700	20107.128253	29.989210
429.416423	20134.450737	29.994228
429.353647	20166.584093	29.999245
430.289709	20188.949717	30.004263
430.785908	20202.129578	30.009280
431.137855	20248.379295	30.014298
431.549610	20256.836035	30.019316
431.910548	20258.754646	30.024333
432.235389	20332.564854	30.029351
432.875652	20325.263342	30.034368
433.278037	20331.955316	30.039386
433.656154	20397.531012	30.044404
433.835738	20424.854181	30.049421
434.086173	20420.994587	30.054439
434.528749	20444.192427	30.059456
434.610568	20474.683142	30.064474
435.242030	20528.645831	30.069492
435.374543	20542.525330	30.074509
436.156722	20583.124630	30.079527
436.427450	20592.750207	30.084544
436.743252	20664.306092	30.089562
436.800086	20683.516476	30.094580
437.980149	20691.310431	30.099597
437.970511	20755.951657	30.104615
438.482080	20787.662063	30.109632
439.169695	20810.630046	30.114650
439.788626	20841.845446	30.119668
440.100936	20884.307224	30.124685
440.796358	20893.004586	30.129703
441.049483	20955.116659	30.134720
441.330305	20958.064792	30.139738
441.785849	21010.795985	30.144756
442.525427	21022.632474	30.149773
442.973710	21063.028704	30.154791
443.361416	21103.067709	30.159808
443.584269	21121.369379	30.164826
444.118148	21145.112060	30.169844
444.410986	21208.493400	30.174861
445.411676	21216.651686	30.179879
445.596104	21274.750183	30.184896
445.647611	21287.295802	30.189914
446.698848	21296.284786	30.194932
446.914729	21364.474232	30.199949
447.382893	21368.630979	30.204967
447.872560	21395.496531	30.209984
448.303421	21452.491295	30.215002
448.520648	21474.416907	30.220020
449.216751	21473.550728	30.225037
449.272529	21554.574109	30.230055
449.755688	21549.539573	30.235072
450.255549	21602.747666	30.240090
450.734204	21664.746680	30.245108
451.453550	21655.713946	30.250125
451.801389	21737.768305	30.255143
452.381802	21756.178347	30.260160
453.039165	21759.980588	30.265178
453.731319	21782.336569	30.270196
454.093867	21850.718182	30.275213
454.800260	21844.136683	30.280231
454.896197	21887.665761	30.285248
454.940072	21910.552059	30.290266
455.415190	21920.189995	30.295284
455.602219	21990.346181	30.300301
456.140838	21983.639356	30.305319
456.685420	22037.937287	30.310336
456.769354	22070.166539	30.315354
457.805087	22085.584946	30.320372
457.972920	22122.168749	30.325389
458.009612	22185.428658	30.330407
458.670944	22196.778406	30.335424
458.937322	22236.415919	30.340442
460.222551	22230.171270	30.345460
460.400030	22275.491958	30.350477
460.876339	22347.250454	30.355495
461.327484	22347.780251	30.360512
461.895740	22352.729369	30.365530
461.990962	22414.554576	30.370548
462.348010	22404.066207	30.375565
462.637096	22485.493521	30.380583
463.551908	22493.737840	30.385600
463.890135	22546.180206	30.390618
464.227246	22567.136053	30.395636
464.799023	22623.293520	30.400653
465.505705	22638.482154	30.405671
465.729408	22694.879624	30.410688
465.761463	22711.106737	30.415706
466.380550	22771.779547	30.420724
466.792024	22799.269557	30.425741
467.262097	22854.711585	30.430759
468.405612	22849.498983	30.435776
468.452315	22936.923846	30.440794
469.106484	22946.920605	30.445812
469.462910	23002.533265	30.450829
469.698172	23010.707334	30.455847
470.600695	23036.420661	30.460864
470.768725	23119.430777	30.465882
471.453903	23121.786812	30.470900
471.938746	23165.938741	30.475917
472.052908	23189.252033	30.480935
472.702790	23254.927089	30.485952
472.570432	23286.784506	30.490970
473.477279	23314.580067	30.495988
473.917911	23390.092549	30.501005
474.306575	23407.942783	30.506023
475.178239	23448.512400	30.511040
475.343375	23512.569985	30.516058
476.340819	23517.416448	30.521076
476.657488	23589.059515	30.526093
476.731598	23614.078742	30.531111
477.840467	23611.102008	30.536128
478.381870	23688.801304	30.541146
478.150591	23725.518560	30.546164
479.341355	23747.178821	30.551181
479.744732	23810.353727	30.556199
480.265707	23813.328341	30.561216
480.626554	23853.692884	30.566234
481.055181	23910.569283	30.571252
481.353640	23925.027093	30.576269
482.362434	23949.615969	30.581287
482.546172	24005.170654	30.586304
482.762707	24012.262836	30.591322
483.307665	24036.679991	30.596340
484.100256	24111.124548	30.601357
484.619584	24120.310981	30.606375
485.403862	24127.478967	30.611392
485.360742	24191.252678	30.616410
485.742318	24196.545617	30.621428
486.547573	24191.605455	30.626445
486.685341	24257.830974	30.631463
487.379849	24276.904764	30.636480
487.634462	24319.719740	30.641498
487.970313	24359.891060	30.646516
488.705950	24379.338869	30.651533
488.711440	24408.789133	30.656551
488.963817	24479.577652	30.661568
489.506191	24532.532844	30.666586
489.985679	24549.267931	30.671604
490.583246	24592.346443	30.676621
490.785324	24665.608468	30.681639
491.860976	24673.817301	30.686656
492.360002	24745.767363	30.691674
492.567979	24763.394273	30.696692
493.523795	24797.103375	30.701709
493.782331	24864.722152	30.706727
494.712955	24855.497223	30.711744
495.002751	24938.439155	30.716762
495.153477	24956.781181	30.721780
496.319017	24952.989372	30.726797
496.411713	25045.737866	30.731815
496.872578	25072.293672	30.736832
498.000365	25096.228124	30.741850
497.784357	25149.091921	30.746868
498.676214	25180.211000	30.751885
498.895726	25214.792124	30.756903
499.971043	25242.049076	30.761920
500.008848	25290.143455	30.766938
500.787949	25324.968094	30.771956
501.257604	25348.062502	30.776973
501.516368	25407.988289	30.781991
502.177764	25431.879386	30.787008
502.718040	25454.917010	30.792026
503.048250	25513.532850	30.797044
503.512210	25551.415741	30.802061
503.915645	25567.922184	30.807079
504.654120	25633.607929	30.812096
504.854061	25669.588237	30.817114
505.087600	25705.059908	30.822132
506.012846	25749.586059	30.827149
506.521604	25799.508558	30.832167
506.905936	25842.514923	30.837184
507.605422	25875.113885	30.842202
507.997393	25912.697153	30.847220
508.878267	25945.818790	30.852237
508.936652	25975.031129	30.857255
509.703485	26011.318143	30.862272
510.001641	26042.320789	30.867290
510.660600	26066.284125	30.872308
511.228435	26101.708939	30.877325
511.336814	26154.741015	30.882343
512.020065	26173.870088	30.887360
512.612847	26215.757927	30.892378
512.357820	26276.080763	30.897396
513.022227	26296.726287	30.902413
513.321300	26354.624632	30.907431
514.308551	26371.680157	30.912448
515.155872	26415.139755	30.917466
515.399987	26460.433393	30.922484
515.721855	26508.389283	30.927501
516.066570	26548.773462	30.932519
516.754011	26582.491285	30.937536
517.388686	26632.238768	30.942554
517.699740	26684.294966	30.947572
518.751508	26698.305220	30.952589
518.834981	26758.356152	30.957607
519.542531	26792.360334	30.962624
519.858492	26848.054311	30.967642
520.098562	26901.950996	30.972660
521.186899	26919.592099	30.977677
521.470896	26981.925692	30.982695
521.891514	27038.870445	30.987712
522.756533	27064.201598	30.992730
523.167645	27107.281145	30.997748
523.738412	27160.480018	31.002765
524.295519	27195.039216	31.007783
525.097621	27225.980422	31.012800
525.609077	27259.643408	31.017818
526.151752	27333.294318	31.022836
526.857443	27336.987045	31.027853
527.190465	27403.742798	31.032871
527.750818	27426.031637	31.037888
528.318336	27459.597875	31.042906
528.870783	27514.774343	31.047924
529.576113	27541.165319	31.052941
529.704946	27589.056703	31.057959
530.382239	27619.823956	31.062976
530.921401	27658.259999	31.067994
531.084984	27711.286050	31.073012
531.870126	27749.548411	31.078029
532.318623	27799.962588	31.083047
532.618757	27834.200897	31.088064
533.400415	27864.234269	31.093082
533.854712	27915.704385	31.098100
534.398411	27959.584456	31.103117
535.018444	27988.626690	31.108135
535.232833	28065.499612	31.113152
536.153382	28111.340132	31.118170
536.361321	28132.826533	31.123188
536.878261	28202.513918	31.128205
537.282868	28240.771091	31.133223
538.199502	28258.139276	31.138240
538.702154	28281.865317	31.143258
539.255485	28346.839242	31.148276
539.721357	28412.774383	31.153293
539.826143	28430.727458	31.158311
540.737121	28451.776123	31.163328
541.418632	28529.114176	31.168346
541.660730	28543.121873	31.173364
542.043163	28597.785488	31.178381
542.689105	28624.516250	31.183399
543.188788	28668.751928	31.188416
543.751960	28722.536262	31.193434
544.259620	28766.988395	31.198452
544.841251	28802.650183	31.203469
545.090847	28866.785834	31.208487
545.721848	28885.438766	31.213504
546.617034	28957.530543	31.218522
546.834634	29003.755025	31.223540
547.382588	29008.078384	31.228557
548.167162	29101.460189	31.233575
548.885932	29176.513625	31.238592
549.363575	29202.537819	31.243610
549.736172	29238.944558	31.248628
550.329747	29267.615111	31.253645
551.115155	29298.283254	31.258663
551.897247	29384.397780	31.263680
552.227874	29406.939478	31.268698
552.630353	29436.201766	31.273716
553.484482	29505.407695	31.278733
554.707303	29517.698364	31.283751
554.767534	29579.815236	31.288768
555.455304	29603.524765	31.293786
555.720663	29636.435309	31.298804
556.442488	29705.699411	31.303821
556.699725	29717.718542	31.308839
556.956753	29792.769578	31.313856
557.662511	29801.538788	31.318874
558.153934	29902.652731	31.323892
558.817243	29924.103649	31.328909
559.449404	29969.387079	31.333927
559.707244	30017.393525	31.338944
560.633619	30055.913852	31.343962
561.115688	30125.720642	31.348980
562.051461	30142.640262	31.353997
562.380568	30208.108068	31.359015
562.910227	30243.942048	31.364032
563.588353	30266.344493	31.369050
563.670844	30346.394768	31.374068
564.390058	30381.563761	31.379085
565.086413	30428.009163	31.384103
565.114699	30507.796225	31.389120
566.015345	30520.184683	31.394138
566.624285	30574.883489	31.399156
567.126006	30654.305887	31.404173
567.253418	30695.813775	31.409191
567.867546	30730.365145	31.414208
568.770086	30752.210872	31.419226
569.344785	30835.445834	31.424244
569.639878	30845.489797	31.429261
570.995220	30890.892280	31.434279
570.720800	30957.083302	31.439296
571.889463	30981.583474	31.444314
571.935785	31056.186898	31.449332
572.466072	31062.847689	31.454349
573.002147	31149.288106	31.459367
573.689453	31176.314356	31.464384
574.212384	31235.944657	31.469402
574.979491	31310.558948	31.474420
575.387424	31330.443277	31.479437
576.083726	31381.983548	31.484455
576.268531	31458.306685	31.489472
577.170675	31494.372505	31.494490
577.615135	31524.107824	31.499508
578.323218	31609.472054	31.504525
579.115293	31622.929880	31.509543
579.270690	31711.840531	31.514560
580.378947	31738.204917	31.519578
580.607084	31795.620976	31.524596
581.246161	31852.736953	31.529613
581.840012	31897.209123	31.534631
582.404611	31944.188897	31.539648
582.890645	32001.975963	31.544666
583.480638	32051.074993	31.549684
584.112122	32114.800087	31.554701
584.643487	32167.871124	31.559719
584.841399	32230.508856	31.564736
586.035441	32293.014973	31.569754
586.458085	32336.174324	31.574772
586.947287	32395.336647	31.579789
588.056155	32451.628075	31.584807
588.166207	32498.568346	31.589824
589.052486	32573.565014	31.594842
589.767719	32619.911187	31.599860
590.201191	32647.914954	31.604877
591.140866	32714.600590	31.609895
591.745705	32757.257606	31.614912
592.108716	32825.608543	31.619930
592.701979	32837.841255	31.624948
593.145143	32921.287431	31.629965
593.655676	32980.153714	31.634983
594.287613	33008.832619	31.640000
595.022228	33075.062180	31.645018
595.562971	33136.140339	31.650036
595.777942	33172.960807	31.655053
596.424470	33242.283393	31.660071
597.281283	33288.213272	31.665088
598.224326	33338.809340	31.670106
598.479406	33393.591242	31.675124
599.380168	33417.237722	31.680141
600.112177	33500.992327	31.685159
600.286590	33510.711952	31.690176
600.934817	33599.637842	31.695194
601.216363	33626.631876	31.700212
601.728649	33675.514844	31.705229
602.276684	33715.749656	31.710247
602.434702	33799.518370	31.715264
603.932533	33805.482394	31.720282
604.690491	33859.805876	31.725300
604.465038	33921.828619	31.730317
605.296067	33997.069122	31.735335
605.589800	34030.215678	31.740352
606.139776	34124.123754	31.745370
606.660377	34172.742050	31.750388
607.607980	34217.769450	31.755405
608.628805	34281.032650	31.760423
608.790366	34365.601273	31.765440
609.206665	34397.584639	31.770458
610.358258	34450.955177	31.775476
610.473226	34512.627988	31.780493
611.181334	34584.725464	31.785511
611.866262	34620.596291	31.790528
612.454904	34701.484061	31.795546
612.957170	34782.844700	31.800564
613.703087	34838.275181	31.805581
614.229882	34887.400597	31.810599
614.783495	34948.797091	31.815616
615.938775	34997.892109	31.820634
616.430054	35072.548435	31.825652
616.927280	35124.663356	31.830669
617.382771	35211.721152	31.835687
618.307395	35236.329623	31.840704
619.153966	35304.161353	31.845722
619.252524	35372.260662	31.850740
620.245634	35422.301810	31.855757
620.856157	35509.470469	31.860775
620.981784	35547.631479	31.865792
621.991290	35590.076868	31.870810
622.446779	35703.006505	31.875828
623.145579	35746.253734	31.880845
624.192625	35761.375353	31.885863
625.040058	35853.800223	31.890880
625.452751	35922.089795	31.895898
625.662869	35960.198883	31.900916
626.674905	36006.251888	31.905933
627.669011	36036.420160	31.910951
628.137768	36118.208845	31.915968
628.595298	36213.319486	31.920986
629.585745	36249.055317	31.926004
630.102442	36261.909721	31.931021
630.429796	36362.327929	31.936039
631.027535	36412.349882	31.941056
632.104893	36422.245881	31.946074
632.544548	36529.700522	31.951092
632.494813	36557.969144	31.956109
633.597734	36575.909320	31.961127
633.885844	36684.126897	31.966144
634.366738	36730.339003	31.971162
635.213465	36767.344299	31.976180
635.578014	36827.426715	31.981197
636.336868	36886.845890	31.986215
636.702212	36951.880583	31.991232
637.556700	36995.609181	31.996250
638.211429	37043.006847	32.001268
639.000600	37127.883659	32.006285
639.652220	37144.321316	32.011303
640.326189	37225.340159	32.016320
640.566730	37272.766592	32.021338
641.542043	37319.273668	32.026356
642.172396	37403.637969	32.031373
642.643438	37442.678490	32.036391
643.150986	37528.541830	32.041408
643.948487	37570.084779	32.046426
644.359307	37641.315741	32.051444
644.986579	37692.226029	32.056461
645.452806	37793.951900	32.061479
645.778850	37829.978226	32.066496
646.775850	37901.525299	32.071514
647.656997	37991.107584	32.076532
648.420270	38040.255061	32.081549
649.272485	38119.545458	32.086567
650.231416	38172.520278	32.091584
650.712811	38215.611423	32.096602
651.300479	38309.347805	32.101620
651.541459	38353.685327	32.106637
652.458336	38386.722381	32.111655
653.236348	38489.881744	32.116672
653.623877	38533.691858	32.121690
654.366487	38600.667384	32.126708
655.224630	38694.422750	32.131725
655.791043	38719.487589	32.136743
656.569570	38814.517679	32.141760
657.556824	38833.278115	32.146778
658.154593	38926.532255	32.151796
658.666995	38974.380594	32.156813
659.113184	39033.945438	32.161831
660.229070	39100.284839	32.166848
660.447545	39149.213254	32.171866
660.934730	39232.821117	32.176884
661.443760	39280.874264	32.181901
662.213897	39351.750909	32.186919
662.282795	39434.095562	32.191936
663.574875	39501.814982	32.196954
664.566937	39565.066476	32.201972
664.949610	39628.598149	32.206989
665.877307	39690.930044	32.212007
666.390016	39759.285481	32.217024
666.873065	39831.969580	32.222042
667.740723	39884.369841	32.227060
668.310290	39953.973745	32.232077
668.670605	40012.016701	32.237095
669.571901	40081.161478	32.242112
670.243519	40148.774135	32.247130
671.230646	40194.968742	32.252148
671.447345	40250.312137	32.257165
672.133069	40307.645157	32.262183
672.846987	40377.650413	32.267200
673.493016	40431.136277	32.272218
674.240218	40488.879571	32.277236
674.712778	40568.889991	32.282253
675.299287	40625.183357	32.287271
675.988672	40695.463476	32.292288
676.481005	40759.065487	32.297306
677.340874	40828.295591	32.302324
678.149081	40890.881146	32.307341
679.072382	40957.564400	32.312359
679.581066	41007.489574	32.317376
679.808895	41091.537372	32.322394
681.233942	41135.319892	32.327412
681.953353	41222.934397	32.332429
682.627069	41283.779769	32.337447
683.180924	41344.064118	32.342464
683.859227	41418.896961	32.347482
684.834250	41470.056550	32.352500
685.283873	41531.957216	32.357517
685.802609	41618.391419	32.362535
686.782021	41661.694301	32.367552
687.219943	41730.255634	32.372570
688.192977	41793.086344	32.377588
688.725369	41887.161923	32.382605
689.296916	41923.146807	32.387623
689.934797	42013.730528	32.392640
690.817748	42048.133221	32.397658
691.146026	42140.050608	32.402676
692.061200	42187.194109	32.407693
692.729094	42292.646077	32.412711
693.047206	42335.964488	32.417728
693.926867	42388.927243	32.422746
694.510560	42506.256613	32.427764
695.053075	42559.188410	32.432781
696.080740	42605.816795	32.437799
696.817807	42701.286776	32.442816
697.437832	42795.599404	32.447834
698.056463	42840.325328	32.452852
698.863389	42919.834555	32.457869
699.314863	43024.562145	32.462887
699.899947	43068.426585	32.467904
701.485365	43123.174945	32.472922
701.850983	43233.664545	32.477940
702.067302	43283.521455	32.482957
703.417793	43323.700333	32.487975
704.148414	43437.624937	32.492992
704.833529	43492.470499	32.498010
706.009266	43556.171221	32.503028
706.597642	43617.256103	32.508045
707.223123	43684.915301	32.513063
708.274550	43752.327150	32.518080
707.713533	43793.158440	32.523098
708.818559	43818.763292	32.528116
709.568420	43920.824360	32.533133
710.133794	43984.778407	32.538151
710.666431	44020.773879	32.543168
711.573171	44135.088272	32.548186
712.129519	44167.178221	32.553204
713.078279	44242.466076	32.558221
713.645544	44326.972459	32.563239
714.445359	44364.474962	32.568256
715.388589	44413.695755	32.573274
715.899946	44528.753912	32.578292
716.359409	44573.465507	32.583309
717.529986	44619.297428	32.588327
718.100804	44732.927930	32.593344
718.306832	44777.494280	32.598362
719.557684	44839.626270	32.603380
720.123470	44923.959141	32.608397
720.535807	44977.303936	32.613415
721.735351	45061.801565	32.618432
722.123652	45155.264887	32.623450
723.094540	45188.527350	32.628468
723.821827	45297.843170	32.633485
724.420716	45359.140728	32.638503
724.605259	45422.734826	32.643520
725.733024	45496.611568	32.648538
726.996283	45547.447158	32.653556
727.485791	45624.274753	32.658573
727.888686	45754.762783	32.663591
728.787852	45784.709557	32.668608
729.419354	45870.512973	32.673626
729.837905	45969.903647	32.678644
730.972194	46027.812111	32.683661
731.656458	46113.731361	32.688679
732.492371	46196.459448	32.693696
732.958983	46263.683918	32.698714
733.799956	46330.139208	32.703732
734.830139	46400.533440	32.708749
735.167542	46513.310418	32.713767
735.927058	46551.745287	32.718784
736.861026	46659.582331	32.723802
737.203636	46725.074187	32.728820
738.083387	46816.559437	32.733837
738.788732	46864.443181	32.738855
739.872836	46988.664057	32.743872
740.249520	47043.181869	32.748890
741.442728	47105.558284	32.753908
742.425188	47205.257417	32.758925
742.355638	47283.212983	32.763943
743.597199	47327.775584	32.768960
744.227735	47441.026129	32.773978
745.038657	47529.733841	32.778996
745.992440	47568.250446	32.784013
746.641257	47684.610547	32.789031
747.596903	47719.091828	32.794048
748.175527	47819.896764	32.799066
748.636744	47839.971873	32.804084
749.620606	47952.415390	32.809101
749.830168	48004.031665	32.814119
751.350304	48035.505197	32.819136
751.825280	48151.750922	32.824154
752.161184	48238.556379	32.829172
752.777751	48281.908344	32.834189
753.841964	48320.692989	32.839207
754.610869	48443.604965	32.844224
755.010830	48522.043430	32.849242
756.117245	48570.811398	32.854260
756.841160	48668.310288	32.859277
757.582086	48716.641466	32.864295
758.355897	48823.535987	32.869312
758.846987	48922.802444	32.874330
759.400987	48964.935477	32.879348
760.577325	49022.364380	32.884365
761.144343	49134.695623	32.889383
762.105136	49253.922481	32.894400
762.341875	49313.666487	32.899418
763.443609	49367.164163	32.904436
764.473422	49484.074994	32.909453
765.252431	49542.518616	32.914471
766.300350	49639.409613	32.919488
766.932281	49731.031485	32.924506
767.136413	49792.158070	32.929524
768.324794	49857.318660	32.934541
768.989094	49981.207755	32.939559
769.892304	50035.041981	32.944576
770.465264	50148.296944	32.949594
770.923232	50225.155946	32.954612
772.662503	50268.662242	32.959629
773.152989	50392.342047	32.964647
773.647971	50443.929461	32.969664
774.608175	50554.351610	32.974682
775.516259	50599.631942	32.979700
776.235569	50671.033089	32.984717
777.293759	50796.853201	32.989735
777.850950	50849.063015	32.994752
778.606277	50929.967448	32.999770
778.965152	51026.442375	33.004788
780.654813	51083.692111	33.009805
780.620757	51194.090300	33.014823
781.826057	51227.655097	33.019840
782.490042	51360.765373	33.024858
782.808712	51454.118511	33.029876
783.727767	51506.275801	33.034893
784.781322	51594.873718	33.039911
785.166158	51693.929542	33.044928
786.359835	51748.868269	33.049946
786.788902	51881.931447	33.054964
787.955811	51923.248086	33.059981
788.391474	52017.993043	33.064999
789.255904	52103.701257	33.070016
789.766035	52160.772968	33.075034
790.540876	52265.201141	33.080052
792.010347	52303.971027	33.085069
792.428021	52427.228344	33.090087
793.671962	52476.338616	33.095104
794.366504	52553.400348	33.100122
794.651182	52631.783725	33.105140
796.360347	52672.125801	33.110157
796.549706	52784.057250	33.115175
797.362783	52876.206082	33.120192
798.203201	52924.472882	33.125210
798.862349	53019.474739	33.130228
799.357087	53087.610586	33.135245
800.226640	53154.588723	33.140263
801.076607	53248.788181	33.145280
801.997248	53333.246661	33.150298
802.386719	53414.283653	33.155316
803.691159	53529.586541	33.160333
803.963123	53594.003973	33.165351
804.757787	53652.524819	33.170368
805.599815	53793.300498	33.175386
806.197648	53853.128415	33.180404
807.415316	53964.436387	33.185421
807.779907	54056.091354	33.190439
809.008552	54137.237887	33.195456
809.951805	54230.654339	33.200474
810.353004	54353.106794	33.205492
810.915020	54427.811484	33.210509
812.195377	54500.887126	33.215527
812.929292	54607.175479	33.220544
814.197488	54685.155550	33.225562
814.859124	54783.919143	33.230580
815.761854	54872.266799	33.235597
816.483724	54979.588219	33.240615
817.737140	55034.426467	33.245632
818.467521	55159.675864	33.250650
819.164862	55221.629344	33.255668
819.884857	55320.733769	33.260685
820.758781	55391.172624	33.265703
821.077529	55522.780829	33.270720
821.870650	55593.668920	33.275738
823.422454	55664.749026	33.280756
824.119485	55792.526960	33.285773
824.438152	55863.892493	33.290791
825.490862	55923.506473	33.295808
826.058555	56053.800484	33.300826
826.764203	56177.173177	33.305844
827.716033	56247.950164	33.310861
828.672112	56323.392214	33.315879
829.517545	56435.863584	33.320896
830.490687	56565.575862	33.325914
831.230142	56656.253028	33.330932
831.818628	56729.207828	33.335949
833.021297	56784.766521	33.340967
834.004311	56892.171255	33.345984
834.996388	56998.179905	33.351002
835.573745	57076.933602	33.356020
836.313186	57130.707754	33.361037
837.827108	57181.820771	33.366055
838.037409	57290.499876	33.371072
839.000681	57401.998756	33.376090
839.544680	57462.307977	33.381108
840.651881	57548.012722	33.386125
841.240776	57657.391373	33.391143
841.836182	57711.310108	33.396160
842.769178	57808.338985	33.401178
843.594621	57908.116189	33.406196
844.706424	57981.974464	33.411213
845.308959	58101.531397	33.416231
845.753954	58182.479687	33.421248
847.339393	58246.193053	33.426266
847.789467	58374.921665	33.431284
848.746923	58437.425499	33.436301
849.344897	58572.553223	33.441319
849.893177	58651.100442	33.446336
851.186051	58728.017280	33.451354
852.157023	58826.781825	33.456372
852.702942	58937.273540	33.461389
853.621514	59071.078427	33.466407
854.390345	59172.933038	33.471424
855.255439	59247.271314	33.476442
856.866356	59318.173061	33.481460
857.401128	59456.682775	33.486477
858.199277	59525.248937	33.491495
858.790456	59655.959304	33.496512
859.868288	59721.100343	33.501530
860.535113	59859.857246	33.506548
861.414410	59931.231380	33.511565
862.425030	60049.555124	33.516583
863.318276	60127.551687	33.521600
864.138220	60254.987350	33.526618
865.287116	60337.029623	33.531636
865.866801	60457.476776	33.536653
866.893264	60543.227181	33.541671
867.862401	60636.337392	33.546688
868.787934	60720.945932	33.551706
869.436346	60855.015019	33.556724
869.960724	60920.611433	33.561741
871.449310	61047.718763	33.566759
872.199147	61123.058511	33.571776
873.122790	61251.880050	33.576794
874.019235	61328.848639	33.581812
874.986851	61434.829714	33.586829
875.593415	61539.899496	33.591847
876.752231	61629.268095	33.596864
877.811541	61709.770843	33.601882
878.442232	61836.865334	33.606900
879.117439	61912.545358	33.611917
880.486804	62047.250263	33.616935
880.924058	62102.536238	33.621952
882.584986	62179.541383	33.626970
883.510958	62245.782669	33.631988
884.667628	62335.432842	33.637005
885.136711	62397.996111	33.642023
886.006036	62485.984447	33.647040
887.234888	62575.415872	33.652058
887.134596	62651.219119	33.657076
888.419797	62710.154843	33.662093
889.202990	62820.802255	33.667111
889.699461	62943.612143	33.672128
890.335196	63014.465238	33.677146
891.355920	63077.786094	33.682164
892.451090	63208.949419	33.687181
893.204633	63322.642265	33.692199
892.978613	63409.546092	33.697216
894.580645	63489.111161	33.702234
895.353662	63634.352581	33.707252
895.721353	63731.622185	33.712269
897.447127	63811.168920	33.717287
898.026858	63955.227772	33.722304
898.923101	64039.565369	33.727322
899.793588	64169.719512	33.732340
901.101808	64267.960107	33.737357
901.476658	64366.744482	33.742375
902.454513	64505.640880	33.747392
903.290510	64593.148508	33.752410
904.311445	64716.120101	33.757428
904.905165	64838.421485	33.762445
906.137896	64956.794398	33.767463
906.857012	65068.532535	33.772480
907.959223	65170.751858	33.777498
909.089344	65315.166070	33.782516
909.861938	65419.274044	33.787533
910.931899	65507.509750	33.792551
911.963615	65624.728167	33.797568
912.665849	65747.918185	33.802586
913.803630	65839.486001	33.807604
914.386189	65986.790584	33.812621
915.261222	66070.774185	33.817639
916.345923	66201.492367	33.822656
917.541916	66302.951150	33.827674
918.432917	66438.000191	33.832692
919.248509	66515.283795	33.837709
920.049083	66670.208380	33.842727
920.998575	66749.344517	33.847744
921.919862	66898.358235	33.852762
923.079388	66999.043218	33.857780
923.586091	67104.118574	33.862797
924.603154	67264.673373	33.867815
925.498956	67356.151110	33.872832
926.679831	67436.257643	33.877850
927.587051	67594.937585	33.882868
928.308833	67716.406237	33.887885
929.841984	67787.576431	33.892903
930.245268	67928.528365	33.897920
931.354782	68015.079465	33.902938
932.812749	68073.186223	33.907956
933.305543	68222.837405	33.912973
934.378348	68332.365108	33.917991
935.297750	68436.914562	33.923008
936.148011	68535.846867	33.928026
936.945037	68642.678495	33.933044
937.753452	68732.262490	33.938061
939.151248	68788.529987	33.943079
939.300366	68893.431887	33.948096
940.570991	69038.802415	33.953114
941.507842	69150.289507	33.958132
942.395551	69226.470072	33.963149
943.038680	69336.507712	33.968167
944.120430	69501.072906	33.973184
944.850093	69596.574060	33.978202
946.221774	69686.982569	33.983220
946.699757	69840.666581	33.988237
948.090077	69926.303355	33.993255
949.158800	70032.966704	33.998272
949.644299	70197.487324	34.003290
950.908519	70294.757964	34.008308
951.894498	70389.293483	34.013325
952.948159	70502.178599	34.018343
953.834413	70639.901688	34.023360
955.156294	70767.062200	34.028378
956.115449	70856.650914	34.033396
957.298664	70945.383040	34.038413
958.306313	71093.514826	34.043431
958.843894	71192.756746	34.048448
960.048660	71272.932141	34.053466
961.270088	71420.400558	34.058484
961.986664	71501.968752	34.063501
963.194446	71590.573517	34.068519
964.099765	71754.427499	34.073536
964.921193	71829.510391	34.078554
966.197190	71940.637164	34.083572
966.732544	72093.274486	34.088589
967.879250	72159.758029	34.093607
969.129643	72297.390547	34.098624
969.800921	72396.465605	34.103642
971.050177	72471.697703	34.108660
971.979479	72618.431726	34.113677
972.887798	72740.217807	34.118695
973.915917	72866.794100	34.123712
974.803254	72974.127796	34.128730
975.925747	73069.393746	34.133748
976.378747	73176.007791	34.138765
977.878301	73286.651604	34.143783
978.791412	73404.946691	34.148800
979.461038	73509.695590	34.153818
980.691481	73603.095491	34.158836
981.169633	73716.046309	34.163853
982.829407	73795.622438	34.168871
983.562000	73925.917503	34.173888
984.562055	74047.652765	34.178906
985.457995	74148.242666	34.183924
986.255596	74238.674925	34.188941
986.935624	74327.110487	34.193959
987.613518	74429.891328	34.198976
989.124456	74525.348898	34.203994
990.363211	74659.359750	34.209012
991.106460	74756.924805	34.214029
992.485513	74823.380308	34.219047
993.409345	74970.025092	34.224064
994.161166	75081.777325	34.229082
995.296575	75175.022759	34.234100
995.720575	75271.402501	34.239117
997.368888	75377.895008	34.244135
997.748280	75496.217868	34.249152
998.670651	75604.419584	34.254170
1000.175927	75745.681744	34.259188
1001.106565	75830.898993	34.264205
1001.921661	75983.831223	34.269223
1002.414504	76081.448866	34.274240
1003.660016	76181.987037	34.279258
1004.662461	76344.169569	34.284276
1005.290689	76445.230677	34.289293
1006.339171	76590.129482	34.294311
1007.517021	76690.819989	34.299328
1008.387685	76844.780039	34.304346
1009.708219	76963.789690	34.309364
1010.857980	77054.639951	34.314381
1011.754237	77208.118370	34.319399
1012.814533	77362.355546	34.324416
1013.839208	77445.314688	34.329434
1015.047090	77598.727526	34.334452
1015.678811	77732.842735	34.339469
1016.473432	77842.909616	34.344487
1018.045626	77955.937697	34.349504
1018.727023	78094.414705	34.354522
1019.673297	78264.768433	34.359540
1020.540886	78385.887314	34.364557
1021.495321	78501.936732	34.369575
1022.948798	78642.513120	34.374592
1024.016817	78785.205970	34.379610
1025.457944	78897.640711	34.384628
1026.091795	79037.256736	34.389645
1027.425999	79158.685208	34.394663
1028.462362	79267.324447	34.399680
1029.328892	79428.409133	34.404698
1030.427673	79520.877653	34.409716
1031.900052	79666.306099	34.414733
1032.657797	79770.081047	34.419751
1033.969308	79905.018885	34.424768
1035.392454	80017.721791	34.429786
1036.686489	80114.997436	34.434804
1037.227758	80266.614755	34.439821
1038.868728	80348.672244	34.444839
1040.019336	80457.792646	34.449856
1040.679871	80548.464468	34.454874
1041.881969	80633.292009	34.459892
1042.866801	80731.321395	34.464909
1044.004923	80832.259887	34.469927
1045.110041	80932.609930	34.474944
1045.898012	81040.710174	34.479962
1047.159137	81133.703745	34.484980
1047.378922	81236.743561	34.489997
1048.183783	81356.309601	34.495015
1049.473569	81462.081829	34.500032
1049.934878	81570.761472	34.505050
1050.559731	81719.284977	34.510068
1051.796174	81822.589523	34.515085
1052.941063	81968.339140	34.520103
1053.672260	82090.323302	34.525120
1054.277498	82245.143631	34.530138
1055.666355	82352.137346	34.535156
1056.134865	82510.439328	34.540173
1057.424893	82632.641216	34.545191
1058.877998	82787.406567	34.550208
1059.514469	82940.627680	34.555226
1060.433900	83062.043907	34.560244
1061.921104	83196.064881	34.565261
1062.977073	83363.111560	34.570279
1064.167286	83508.877371	34.575296
1065.085585	83638.237534	34.580314
1066.520223	83770.506702	34.585332
1067.702253	83932.429638	34.590349
1068.611150	84057.558065	34.595367
1069.952465	84212.143094	34.600384
1071.181593	84335.477315	34.605402
1072.204795	84480.068884	34.610420
1073.540382	84618.700390	34.615437
1074.814053	84758.562872	34.620455
1076.288396	84891.351210	34.625472
1076.857660	85011.348633	34.630490
1078.038868	85127.139799	34.635508
1078.977380	85282.220346	34.640525
1080.589081	85398.975100	34.645543
1081.875314	85504.483808	34.650560
1082.654641	85665.573646	34.655578
1083.777919	85769.819778	34.660596
1084.976145	85921.051129	34.665613
1085.764956	86031.377283	34.670631
1086.937624	86157.152724	34.675648
1087.877374	86303.059867	34.680666
1089.372569	86410.670639	34.685684
1090.510897	86549.630691	34.690701
1091.673447	86678.458458	34.695719
1092.986327	86792.549550	34.700736
1093.944036	86915.025133	34.705754
1094.901423	87048.497235	34.710772
1095.960191	87180.885446	34.715789
1096.736519	87281.216947	34.720807
1097.957455	87411.822972	34.725824
1099.009704	87526.345149	34.730842
1099.715329	87645.532693	34.735860
1100.880426	87749.642750	34.740877
1101.510497	87902.432855	34.745895
1102.866417	87976.174528	34.750912
1103.973976	88150.219005	34.755930
1104.558677	88280.387699	34.760948
1105.755642	88377.040441	34.765965
1106.346675	88554.439551	34.770983
1107.687128	88668.371840	34.776000
1108.868102	88825.734993	34.781018
1109.446843	88945.828896	34.786036
1110.856162	89120.351752	34.791053
1111.606812	89252.947175	34.796071
1113.527412	89367.960777	34.801088
1114.576919	89564.658511	34.806106
1115.587584	89699.182011	34.811124
1116.554364	89811.282614	34.816141
1117.535063	89998.028834	34.821159
1118.990127	90110.799551	34.826176
1120.132971	90299.552560	34.831194
1121.323581	90422.744630	34.836212
1122.646670	90570.649759	34.841229
1123.317095	90737.834414	34.846247
1124.718154	90870.159198	34.851264
1126.243939	91003.135316	34.856282
1127.204650	91160.386000	34.861300
1128.565215	91288.665925	34.866317
1129.504566	91425.810716	34.871335
1130.977126	91550.583345	34.876352
1131.664547	91742.121756	34.881370
1133.122182	91854.344538	34.886388
1134.328381	92018.348472	34.891405
1135.436558	92162.269850	34.896423
1136.498317	92291.918673	34.901440
1137.963891	92451.495343	34.906458
1139.084805	92590.376781	34.911476
1140.087203	92708.716373	34.916493
1140.721734	92900.798233	34.921511
1142.303276	93010.755610	34.926528
1143.502459	93181.827777	34.931546
1144.833386	93303.407223	34.936564
1145.854332	93422.133507	34.941581
1147.021803	93597.451611	34.946599
1148.306996	93756.263134	34.951616
1149.349685	93882.243189	34.956634
1149.887305	94037.779072	34.961652
1151.391895	94167.526610	34.966669
1152.561317	94336.885674	34.971687
1154.067388	94480.499544	34.976704
1155.084514	94608.840757	34.981722
1156.080866	94786.586393	34.986740
1157.021608	94901.576127	34.991757
1158.230399	95041.641786	34.996775
1159.440853	95218.743259	35.001792
1160.654356	95324.526291	35.006810
1161.434903	95477.187139	35.011828
1162.641716	95612.904767	35.016845
1163.965038	95759.921105	35.021863
1165.358922	95875.419416	35.026880
1166.250494	96039.072960	35.031898
1167.478490	96161.304294	35.036916
1169.152150	96266.898419	35.041933
1169.667715	96459.093120	35.046951
1170.960643	96568.873597	35.051968
1172.140712	96732.283884	35.056986
1173.198865	96835.770843	35.062004
1174.489242	97019.288229	35.067021
1175.522497	97159.913746	35.072039
1176.848350	97295.280998	35.077056
1178.011498	97439.316283	35.082074
1179.429185	97608.584657	35.087092
1180.583993	97730.077007	35.092109
1181.267982	97905.670176	35.097127
1182.787802	98007.374701	35.102144
1183.843016	98193.311315	35.107162
1185.195707	98333.260696	35.112180
1186.158741	98479.706759	35.117197
1187.127474	98656.456121	35.122215
1188.588959	98785.484335	35.127232
1189.633849	98966.753695	35.132250
1190.807721	99108.944205	35.137268
1191.892362	99268.946321	35.142285
1192.934949	99419.763727	35.147303
1194.168118	99608.726660	35.152320
1195.855744	99736.971423	35.157338
1196.863329	99934.697380	35.162356
1198.544081	100057.965907	35.167373
1199.203934	100226.425194	35.172391
1200.506762	100387.191267	35.177408
1201.910922	100546.468188	35.182426
1202.875138	100706.784181	35.187444
1204.281657	100863.766244	35.192461
1205.840350	100992.291594	35.197479
1206.800235	101193.825817	35.202496
1208.223034	101345.987349	35.207514
1209.226540	101474.046867	35.212532
1210.423533	101654.427420	35.217549
1211.526759	101794.583094	35.222567
1212.784531	101979.942369	35.227584
1214.333406	102108.057875	35.232602
1215.136090	102307.469152	35.237620
1216.559393	102430.588802	35.242637
1217.306135	102612.807395	35.247655
1218.776067	102758.643242	35.252672
1220.230248	102955.564685	35.257690
1220.848523	103097.602326	35.262708
1223.039569	103246.142339	35.267725
1223.845107	103405.477103	35.272743
1225.233969	103576.609967	35.277760
1226.339903	103704.836305	35.282778
1227.418041	103864.687688	35.287796
1228.575348	103979.391212	35.292813
1229.913427	104139.778969	35.297831
1230.739871	104311.398932	35.302848
1232.334517	104419.346475	35.307866
1233.426749	104618.503572	35.312884
1234.793124	104765.773177	35.317901
1235.408055	104903.728025	35.322919
1236.573748	105056.530437	35.327936
1239.044703	105193.704631	35.332954
1239.347231	105393.955687	35.337972
1240.710043	105512.728337	35.342989
1241.758603	105701.523199	35.348007
1242.494131	105855.247138	35.353024
1244.232310	106011.154157	35.358042
1245.224944	106203.752584	35.363060
1246.968856	106342.998169	35.368077
1248.007262	106536.756444	35.373095
1249.503353	106687.422083	35.378112
1250.483029	106864.485017	35.383130
1251.668149	107034.447518	35.388148
1253.076922	107195.692728	35.393165
1254.117794	107387.653828	35.398183
1255.765253	107538.458980	35.403200
1256.566443	107713.392120	35.408218
1258.346141	107882.126916	35.413236
1259.814534	108051.463001	35.418253
1260.578203	108257.322742	35.423271
1262.033003	108387.942857	35.428288
1263.358461	108555.045754	35.433306
1264.297586	108774.565374	35.438324
1266.145947	108926.619425	35.443341
1267.170822	109132.489393	35.448359
1268.390800	109269.063055	35.453376
1269.943865	109465.490971	35.458394
1271.108576	109630.196399	35.463412
1272.871948	109775.148812	35.468429
1273.706490	109991.866842	35.473447
1274.707338	110128.511814	35.478464
1276.426799	110286.898997	35.483482
1277.187796	110518.627936	35.488500
1278.739258	110679.943304	35.493517
1279.586437	110835.535782	35.498535
1281.101245	111014.715052	35.503552
1282.551998	111211.825241	35.508570
1284.061465	111362.669767	35.513588
1285.054186	111564.944725	35.518605
1286.347561	111726.016827	35.523623
1287.391099	111929.862834	35.528640
1289.205333	112072.940787	35.533658
1290.551613	112247.300760	35.538676
1292.006937	112451.269182	35.543693
1292.920753	112624.782706	35.548711
1294.325923	112755.744237	35.553728
1295.957887	112945.705434	35.558746
1296.784747	113090.224920	35.563764
1298.411651	113242.138391	35.568781
1299.603885	113427.419163	35.573799
1300.448359	113561.987383	35.578816
1302.339144	113718.014505	35.583834
1303.291248	113916.516892	35.588852
1304.315427	114054.686528	35.593869
1306.021800	114210.043362	35.598887
1306.650674	114428.903061	35.603904
1307.950573	114573.647148	35.608922
1309.519673	114726.781654	35.613940
1311.174746	114895.033693	35.618957
1312.257731	115066.055681	35.623975
1313.477837	115246.432865	35.628992
1314.932650	115407.693042	35.634010
1315.881744	115579.372875	35.639028
1316.919709	115781.560892	35.644045
1318.273876	116000.122698	35.649063
1319.405230	116191.979732	35.654080
1320.907456	116368.109977	35.659098
1322.099559	116532.293370	35.664116
1323.584605	116742.547077	35.669133
1324.565307	116942.531228	35.674151
1325.828882	117129.619619	35.679168
1327.949128	117297.364182	35.684186
1328.781112	117521.074406	35.689204
1330.157274	117734.360972	35.694221
1331.469138	117930.032880	35.699239
1332.598030	118138.809832	35.704256
1334.029088	118308.582675	35.709274
1335.361105	118506.573107	35.714292
1337.074837	118704.035853	35.719309
1338.675450	118895.996895	35.724327
1340.177472	119082.707067	35.729344
1341.826424	119270.161377	35.734362
1343.033031	119490.644324	35.739380
1343.909081	119661.375416	35.744397
1345.879650	119826.855503	35.749415
1347.103146	120021.195975	35.754432
1348.814380	120227.649427	35.759450
1349.966108	120452.201728	35.764468
1351.289567	120634.974947	35.769485
1352.482923	120783.500730	35.774503
1353.752242	121009.368881	35.779520
1355.379982	121163.666042	35.784538
1356.538402	121389.935036	35.789556
1357.951264	121564.823223	35.794573
1359.254873	121751.824712	35.799591
1360.363117	121962.605047	35.804608
1361.749541	122142.351895	35.809626
1363.214716	122368.631220	35.814644
1364.494615	122539.050949	35.819661
1365.848378	122744.225885	35.824679
1367.412090	122908.536280	35.829696
1369.010532	123114.929062	35.834714
1369.858933	123269.691732	35.839732
1371.381790	123473.705557	35.844749
1372.575970	123623.767094	35.849767
1374.005149	123818.159946	35.854784
1375.003003	124005.821252	35.859802
1376.507177	124186.880497	35.864820
1378.124537	124340.045277	35.869837
1379.758148	124576.297396	35.874855
1380.695912	124767.203437	35.879872
1382.164889	124923.726332	35.884890
1383.343396	125106.363501	35.889908
1384.037917	125350.244789	35.894925
1385.789864	125511.298708	35.899943
1387.328541	125719.507085	35.904960
1388.667446	125939.554155	35.909978
1389.935754	126136.003375	35.914996
1391.501154	126294.520265	35.920013
1392.999984	126542.173212	35.925031
1394.036808	126771.306588	35.930048
1395.637989	126954.915114	35.935066
1397.166419	127152.850418	35.940084
1398.747317	127348.068014	35.945101
1400.610667	127537.478446	35.950119
1402.051947	127730.149479	35.955136
1403.036844	127950.813792	35.960154
1404.211679	128193.808215	35.965172
1405.440928	128384.085340	35.970189
1406.891055	128571.491074	35.975207
1408.677667	128764.709889	35.980224
1409.934205	129007.179129	35.985242
1411.723796	129178.003188	35.990260
1413.085779	129403.749839	35.995277
1414.671628	129646.261033	36.000295
1415.875925	129836.134082	36.005312
1417.725902	130028.262178	36.010330
1419.017824	130233.985066	36.015348
1420.629041	130459.231960	36.020365
1422.277631	130624.791804	36.025383
1423.206555	130858.106370	36.030400
1425.257363	131029.647785	36.035418
1426.358221	131265.598922	36.040436
1428.119390	131433.426110	36.045453
1429.512823	131675.580119	36.050471
1430.827513	131871.771454	36.055488
1432.091479	132048.879312	36.060506
1433.714998	132224.803559	36.065524
1435.276461	132485.498733	36.070541
1436.612278	132668.351093	36.075559
1437.793718	132841.815481	36.080576
1439.344873	133089.734003	36.085594
1440.700900	133272.992492	36.090612
1442.451804	133454.833715	36.095629
1443.863705	133651.934193	36.100647
1445.161300	133880.463834	36.105664
1446.285992	134056.453366	36.110682
1447.466913	134231.472093	36.115700
1449.421834	134406.508280	36.120717
1450.298898	134601.102833	36.125735
1451.337931	134792.403928	36.130752
1453.687071	134972.715297	36.135770
1454.916493	135166.003281	36.140788
1455.720281	135396.143965	36.145805
1457.016978	135618.808263	36.150823
1458.587365	135798.348895	36.155840
1460.205347	136042.037509	36.160858
1461.446749	136224.091275	36.165876
1463.097036	136438.710091	36.170893
1464.241923	136646.910311	36.175911
1465.398252	136858.227415	36.180928
1467.245007	137091.079600	36.185946
1468.974562	137330.009385	36.190964
1470.427024	137557.795858	36.195981
1471.913481	137766.304596	36.200999
1473.348062	137981.602621	36.206016
1474.603324	138195.511431	36.211034
1476.288735	138414.168910	36.216052
1477.147703	138635.265691	36.221069
1478.962243	138855.895488	36.226087
1480.915805	139069.687010	36.231104
1482.570217	139283.426225	36.236122
1483.846999	139501.421652	36.241140
1485.094329	139757.251765	36.246157
1486.681560	139950.235667	36.251175
1488.391249	140198.024834	36.256192
1490.065089	140433.275351	36.261210
1491.687473	140662.908980	36.266228
1492.929452	140884.240414	36.271245
1494.700995	141123.929162	36.276263
1496.449407	141320.039291	36.281280
1497.736077	141520.190888	36.286298
1499.565400	141762.879179	36.291316
1500.870349	142009.099999	36.296333
1502.643431	142189.648445	36.301351
1503.656705	142413.270697	36.306368
1505.178645	142641.135631	36.311386
1507.089596	142894.124011	36.316404
1508.604943	143077.532341	36.321421
1510.393019	143295.626076	36.326439
1511.248395	143530.625127	36.331456
1512.758220	143758.411600	36.336474
1514.337477	143982.006112	36.341492
1515.639332	144201.577741	36.346509
1517.346216	144415.851902	36.351527
1519.227804	144639.289082	36.356544
1520.763323	144902.024587	36.361562
1522.555703	145121.930431	36.366580
1523.664753	145314.707474	36.371597
1525.420078	145504.087483	36.376615
1527.229941	145714.957311	36.381632
1528.450024	145930.396678	36.386650
1529.786236	146132.230960	36.391668
1531.455108	146349.883511	36.396685
1533.135699	146571.503197	36.401703
1534.753608	146780.940334	36.406720
1536.299143	146963.137339	36.411738
1537.682899	147112.898151	36.416756
1538.584903	147332.720155	36.421773
1540.372737	147554.963531	36.426791
1541.867797	147792.060723	36.431808
1543.119138	147964.093264	36.436826
1545.032935	148156.075400	36.441844
1545.889598	148414.942461	36.446861
1547.415324	148654.018735	36.451879
1549.318229	148892.352348	36.456896
1550.729086	149115.300352	36.461914
1552.680712	149330.088905	36.466932
1553.952736	149541.602137	36.471949
1555.591149	149743.335356	36.476967
1557.048576	149976.398133	36.481984
1558.547961	150209.747504	36.487002
1560.227411	150425.004951	36.492020
1561.900936	150658.570767	36.497037
1562.912871	150893.092744	36.502055
1564.664689	151171.084049	36.507072
1565.856215	151400.028415	36.512090
1567.821102	151610.595711	36.517108
1569.140109	151883.185091	36.522125
1570.793422	152130.836993	36.527143
1572.154415	152370.854360	36.532160
1573.073047	152621.073504	36.537178
1575.298071	152870.909539	36.542196
1577.058445	153130.025677	36.547213
1578.718103	153376.291330	36.552231
1580.233680	153634.499425	36.557248
1581.580972	153883.671109	36.562266
1583.677334	154126.006005	36.567284
1585.142642	154383.619324	36.572301
1586.794459	154653.097734	36.577319
1588.774222	154854.047433	36.582336
1590.003833	155129.809399	36.587354
1592.119029	155391.562023	36.592372
1593.955811	155636.954028	36.597389
1595.473758	155883.197254	36.602407
1596.982792	156116.320537	36.607424
1598.659928	156358.852240	36.612442
1600.359939	156581.639987	36.617460
1601.830463	156784.558636	36.622477
1603.777179	157018.594920	36.627495
1605.358579	157278.621018	36.632512
1606.667179	157513.713030	36.637530
1608.589908	157726.557200	36.642548
1610.090997	157975.075245	36.647565
1612.276867	158200.966382	36.652583
1613.301234	158425.407729	36.657600
1615.023967	158639.506607	36.662618
1617.382045	158848.268904	36.667636
1618.744098	159061.476648	36.672653
1620.301129	159262.012242	36.677671
1622.132346	159468.756982	36.682688
1623.144441	159677.826802	36.687706
1625.096391	159890.819124	36.692724
1626.357067	160131.896465	36.697741
1627.604794	160343.012491	36.702759
1628.823654	160574.943889	36.707776
1630.521498	160846.315032	36.712794
1632.014676	161055.164468	36.717812
1632.764867	161300.312765	36.722829
1635.125363	161519.578007	36.727847
1637.046924	161754.106661	36.732864
1638.581345	161993.606091	36.737882
1640.172875	162236.522091	36.742900
1641.932654	162498.638457	36.747917
1642.865272	162763.906371	36.752935
1644.609523	163023.568773	36.757952
1646.401880	163254.411993	36.762970
1648.327372	163517.371844	36.767988
1649.670872	163799.550709	36.773005
1651.045064	164050.135435	36.778023
1652.528749	164303.532658	36.783040
1654.452757	164536.645960	36.788058
1656.343190	164802.689828	36.793076
1658.030882	165073.929643	36.798093
1659.600943	165342.957994	36.803111
1661.325913	165604.924773	36.808128
1662.646955	165896.559374	36.813146
1664.834248	166163.301556	36.818164
1666.096519	166434.885290	36.823181
1667.742783	166697.164015	36.828199
1669.967750	166968.991948	36.833216
1671.901340	167271.130574	36.838234
1673.615716	167530.816942	36.843252
1675.338160	167786.381686	36.848269
1676.972753	168052.895383	36.853287
1679.110962	168310.668029	36.858304
1680.648678	168576.414420	36.863322
1682.703979	168830.259121	36.868340
1683.831779	169061.485123	36.873357
1685.530655	169320.729640	36.878375
1688.040588	169546.525974	36.883392
1689.442680	169846.105919	36.888410
1691.037936	170112.348572	36.893428
1693.010677	170366.863501	36.898445
1694.466310	170634.425744	36.903463
1696.229486	170863.481471	36.908480
1697.611856	171118.653224	36.913498
1699.226798	171365.785678	36.918516
1701.590569	171605.012341	36.923533
1702.888123	171900.692526	36.928551
1704.471086	172112.012722	36.933568
1706.434439	172338.901593	36.938586
1707.833235	172584.262121	36.943604
1709.461114	172854.818622	36.948621
1711.325961	173049.291238	36.953639
1712.930791	173314.514061	36.958656
1714.529460	173541.328224	36.963674
1716.213755	173804.727695	36.968692
1718.118476	174010.298496	36.973709
1719.656264	174307.747216	36.978727
1721.051450	174524.691797	36.983744
1722.753320	174782.081893	36.988762
1723.952618	175030.305433	36.993780
1725.821836	175291.097398	36.998797
1727.350790	175577.888026	37.003815
1729.395041	175817.431845	37.008832
1730.995224	176078.284281	37.013850
1732.731593	176368.637752	37.018868
1734.477163	176632.058649	37.023885
1735.919923	176919.303740	37.028903
1737.764017	177196.731161	37.033920
1739.743521	177455.832145	37.038938
1741.871976	177704.025915	37.043956
1743.611729	177978.950505	37.048973
1744.990147	178267.661481	37.053991
1746.897570	178533.136767	37.059008
1748.804195	178820.968430	37.064026
1750.546115	179130.624714	37.069044
1752.429714	179379.577815	37.074061
1754.011483	179630.331155	37.079079
1755.875239	179938.603806	37.084096
1756.963265	180220.028308	37.089114
1759.411678	180469.278773	37.094132
1761.346944	180787.886574	37.099149
1763.356350	181056.901379	37.104167
1765.337164	181361.219857	37.109184
1766.927627	181614.584488	37.114202
1768.896833	181911.752739	37.119220
1770.438836	182156.678062	37.124237
1772.061845	182481.882306	37.129255
1773.988163	182769.674026	37.134272
1775.684547	183006.129271	37.139290
1777.345739	183301.528799	37.144308
1778.934826	183598.819650	37.149325
1781.301971	183848.343556	37.154343
1783.175418	184133.284999	37.159360
1784.693268	184444.892909	37.164378
1786.425684	184698.379733	37.169396
1789.308021	184951.012935	37.174413
1790.445683	185230.989992	37.179431
1792.069304	185557.561792	37.184448
1793.464001	185816.298360	37.189466
1795.147198	186070.054529	37.194484
1797.208532	186368.671960	37.199501
1798.685212	186677.129566	37.204519
1800.221719	186908.631265	37.209536
1802.461531	187156.138090	37.214554
1803.969685	187480.343732	37.219572
1805.629802	187714.659645	37.224589
1807.357697	187960.564351	37.229607
1809.033802	188257.034546	37.234624
1810.822900	188536.953843	37.239642
1812.461470	188799.094781	37.244660
1815.071197	189057.123752	37.249677
1816.499990	189359.008072	37.254695
1818.532118	189607.436561	37.259712
1819.845375	189925.471998	37.264730
1821.256933	190174.078120	37.269748
1823.635444	190480.298511	37.274765
1825.072834	190769.322441	37.279783
1826.866736	191047.923382	37.284800
1828.709947	191364.881750	37.289818
1830.172537	191683.514339	37.294836
1831.809384	191967.310634	37.299853
1834.145240	192246.568538	37.304871
1835.599213	192574.637628	37.309888
1837.559676	192882.462545	37.314906
1839.624934	193178.749275	37.319924
1841.753183	193517.530430	37.324941
1843.331157	193787.056394	37.329959
1845.486681	194134.302485	37.334976
1846.854371	194413.827905	37.339994
1849.500397	194706.807979	37.345012
1851.128312	195062.317564	37.350029
1852.741778	195340.374992	37.355047
1854.872920	195667.062473	37.360064
1856.886996	195973.654183	37.365082
1858.591063	196289.105087	37.370100
1860.815801	196592.786032	37.375117
1862.523416	196917.238814	37.380135
1864.720974	197216.866319	37.385152
1866.119989	197562.339449	37.390170
1867.894938	197848.875916	37.395188
1870.525731	198156.943878	37.400205
1872.089200	198474.511960	37.405223
1874.582671	198747.256918	37.410240
1876.260994	199090.309616	37.415258
1878.026451	199375.307424	37.420276
1880.203013	199700.972288	37.425293
1882.039458	199982.877758	37.430311
1883.685093	200329.649898	37.435328
1885.547273	200616.136715	37.440346
1887.676729	200911.493088	37.445364
1889.378478	201230.527988	37.450381
1891.315505	201564.048331	37.455399
1892.972179	201831.547196	37.460416
1895.005632	202170.044336	37.465434
1896.514952	202473.859721	37.470452
1899.060025	202748.723787	37.475469
1900.726742	203101.831440	37.480487
1902.438521	203382.352537	37.485504
1904.682603	203642.442735	37.490522
1906.593823	203968.847822	37.495540
1908.293034	204214.480201	37.500557
1910.040796	204536.966755	37.505575
1911.947350	204804.084743	37.510592
1913.569082	205082.711776	37.515610
1915.110119	205418.386988	37.520628
1917.401929	205681.715883	37.525645
1919.248211	205983.160897	37.530663
1920.677632	206341.403894	37.535680
1922.379451	206646.163049	37.540698
1924.464617	206930.082361	37.545716
1927.437900	207191.583487	37.550733
1928.876586	207509.222861	37.555751
1930.849440	207839.803716	37.560768
1932.765371	208180.855759	37.565786
1934.252052	208489.276458	37.570804
1936.816424	208779.615485	37.575821
1938.643376	209098.382248	37.580839
1940.015093	209461.769102	37.585856
1942.095231	209787.341798	37.590874
1943.605919	210095.005110	37.595892
1945.866547	210401.433780	37.600909
1947.970801	210759.621317	37.605927
1949.554803	211107.991225	37.610944
1951.742550	211431.156061	37.615962
1952.945656	211784.833286	37.620980
1955.524430	212127.312675	37.625997
1957.638503	212464.675204	37.631015
1959.352564	212785.903508	37.636032
1961.952648	213100.035640	37.641050
1963.857999	213481.528346	37.646068
1965.453286	213793.246054	37.651085
1967.548478	214138.351971	37.656103
1969.392631	214484.642154	37.661120
1971.916254	214823.564270	37.666138
1973.998440	215157.467073	37.671156
1975.584704	215524.726537	37.676173
1977.975116	215855.536850	37.681191
1979.761416	216196.474603	37.686208
1982.607013	216507.993877	37.691226
1984.229116	216854.090236	37.696244
1986.081256	217204.849479	37.701261
1988.028182	217537.642729	37.706279
1989.727091	217912.362585	37.711296
1992.160523	218251.176342	37.716314
1993.931108	218608.176858	37.721332
1995.836651	218932.984409	37.726349
1998.322453	219238.656294	37.731367
2000.074687	219589.405142	37.736384
2002.111973	219956.654442	37.741402
2003.858090	220276.960569	37.746420
2006.415630	220585.508947	37.751437
2008.204534	220964.217268	37.756455
2010.303147	221275.456929	37.761472
2012.833198	221558.695780	37.766490
2013.822292	221904.320132	37.771508
2016.096012	222192.947554	37.776525
2017.965990	222519.325638	37.781543
2019.925897	222838.237518	37.786560
2021.844509	223142.644171	37.791578
2023.481092	223503.727320	37.796596
2025.455951	223866.053621	37.801613
2027.619188	224209.216499	37.806631
2029.068319	224544.075655	37.811648
2031.614777	224878.317710	37.816666
2033.488449	225220.007184	37.821684
2035.417087	225546.883795	37.826701
2038.161608	225897.847025	37.831719
2039.997433	226239.191269	37.836736
2041.863781	226570.411845	37.841754
2043.890707	226930.216814	37.846772
2045.935763	227261.361009	37.851789
2048.267997	227609.070042	37.856807
2049.959211	227970.697773	37.861824
2052.331053	228312.638460	37.866842
2054.014022	228672.543521	37.871860
2055.716323	229035.545400	37.876877
2057.891278	229385.445310	37.881895
2059.993483	229762.888280	37.886912
2062.037004	230114.208765	37.891930
2064.280185	230471.035509	37.896948
2066.436351	230850.887249	37.901965
2068.528878	231212.744062	37.906983
2070.527486	231588.788907	37.912000
2072.912272	231941.611592	37.917018
2075.082359	232315.549609	37.922036
2076.994654	232678.812227	37.927053
2079.289572	233032.973966	37.932071
2081.351915	233402.336405	37.937088
2083.673487	233783.443769	37.942106
2085.661933	234147.284046	37.947124
2088.100960	234518.572039	37.952141
2090.132491	234887.564042	37.957159
2091.913103	235250.349244	37.962176
2094.253122	235602.582894	37.967194
2096.626936	235969.645110	37.972212
2098.546993	236345.339935	37.977229
2100.884157	236707.076911	37.982247
2102.875667	237074.813278	37.987264
2104.936610	237438.222122	37.992282
2107.149224	237804.021050	37.997300
2109.163267	238170.767091	38.002317
2111.857194	238538.727287	38.007335
2113.618845	238907.725573	38.012352
2115.910046	239261.757144	38.017370
2117.895773	239627.445786	38.022388
2119.897876	239998.873288	38.027405
2122.004055	240350.219902	38.032423
2124.150057	240696.684563	38.037440
2126.130165	241030.019563	38.042458
2127.926584	241377.176692	38.047476
2130.215172	241716.916241	38.052493
2132.088898	242061.573933	38.057511
2133.743880	242412.769689	38.062528
2135.941715	242758.216157	38.067546
2137.951466	243108.570241	38.072564
2139.807945	243472.081499	38.077581
2141.976519	243830.286463	38.082599
2143.825945	244207.694874	38.087616
2146.179409	244567.269597	38.092634
2148.303442	244959.521262	38.097652
2150.702274	245327.066617	38.102669
2153.108622	245704.467219	38.107687
2154.859345	246083.522302	38.112704
2156.992816	246463.584561	38.117722
2158.876863	246851.790276	38.122740
2160.983788	247238.564669	38.127757
2163.386577	247611.094073	38.132775
2165.561442	248009.620407	38.137792
2167.899030	248395.777104	38.142810
2170.349570	248779.605392	38.147828
2172.740534	249172.207523	38.152845
2175.058867	249552.883593	38.157863
2177.195237	249932.852823	38.162880
2179.412817	250325.586988	38.167898
2181.991597	250715.369075	38.172916
2183.826892	251103.339498	38.177933
2186.133889	251480.973799	38.182951
2188.298052	251882.661540	38.187968
2190.719124	252271.303831	38.192986
2192.769802	252645.780767	38.198004
2194.873240	253048.115900	38.203021
2197.283464	253434.095305	38.208039
2199.593343	253834.545128	38.213056
2201.955633	254211.084269	38.218074
2204.273827	254595.963017	38.223092
2206.238728	254989.281245	38.228109
2208.814391	255384.052941	38.233127
2210.949739	255767.134051	38.238144
2213.551774	256161.344252	38.243162
2215.546116	256556.388240	38.248180
2217.699186	256932.737110	38.253197
2220.113500	257323.194318	38.258215
2222.026769	257716.043293	38.263232
2224.252186	258098.199840	38.268250
2227.014979	258487.867154	38.273268
2229.032970	258877.958054	38.278285
2231.152780	259268.947936	38.283303
2233.368316	259652.632720	38.288320
2235.549511	260047.297476	38.293338
2237.876614	260434.014069	38.298356
2240.150895	260826.074176	38.303373
2242.822618	261203.516060	38.308391
2244.667260	261563.231454	38.313408
2247.194294	261920.806876	38.318426
2249.372898	262265.584152	38.323444
2251.277903	262621.226831	38.328461
2253.505642	262980.146530	38.333479
2255.496924	263339.129534	38.338496
2257.642035	263701.238512	38.343514
2259.781427	264062.104046	38.348532
2262.156051	264447.954624	38.353549
2264.581405	264811.849357	38.358567
2266.513471	265192.918925	38.363584
2268.252883	265573.689182	38.368602
2270.562225	265955.893629	38.373620
2272.655549	266348.903614	38.378637
2275.002522	266735.294328	38.383655
2277.413224	267123.656723	38.388672
2279.522464	267528.884160	38.393690
2281.707186	267922.008037	38.398708
2284.230496	268330.041042	38.403725
2286.484233	268724.678777	38.408743
2288.861189	269135.860186	38.413760
2291.137480	269556.914316	38.418778
2293.513561	269954.607263	38.423796
2295.812727	270364.201393	38.428813
2298.246552	270764.298959	38.433831
2300.280216	271184.884463	38.438848
2302.772619	271589.240909	38.443866
2304.901367	272007.373004	38.448884
2307.056218	272432.766496	38.453901
2309.696517	272840.148390	38.458919
2312.404042	273264.819466	38.463936
2314.396168	273696.361384	38.468954
2317.410340	274092.938707	38.473972
2319.586233	274519.218570	38.478989
2321.875608	274936.944958	38.484007
2324.337672	275356.168219	38.489024
2326.935307	275778.901089	38.494042
2329.271128	276183.207190	38.499060
2331.234187	276606.243885	38.504077
2333.686873	277018.152448	38.509095
2336.124511	277445.457818	38.514112
2338.147792	277864.090038	38.519130
2340.564944	278275.191138	38.524148
2342.734549	278717.272717	38.529165
2345.023772	279137.793131	38.534183
2347.641225	279566.111019	38.539200
2349.536530	280000.004945	38.544218
2352.079058	280434.126330	38.549236
2354.840885	280857.187695	38.554253
2357.274047	281273.238822	38.559271
2359.810048	281701.289188	38.564288
2361.837242	282125.228408	38.569306
2364.493453	282549.016840	38.574324
2367.035195	282975.465067	38.579341
2369.276498	283386.998096	38.584359
2371.384338	283790.651569	38.589376
2373.879166	284171.786956	38.594394
2376.345883	284563.163990	38.599412
2378.390901	284973.634514	38.604429
2380.490661	285361.715823	38.609447
2383.001648	285751.713046	38.614464
2385.191764	286162.057834	38.619482
2387.591353	286565.687994	38.624500
2389.816262	286986.441661	38.629517
2392.340344	287376.231971	38.634535
2394.846002	287794.018859	38.639552
2397.041234	288205.681529	38.644570
2399.475324	288621.649730	38.649588
2401.674600	289048.527046	38.654605
2404.328897	289456.609759	38.659623
2406.696213	289881.655681	38.664640
2408.309017	290323.383182	38.669658
2410.934838	290755.499620	38.674676
2413.432796	291191.166621	38.679693
2415.758291	291632.448832	38.684711
2418.211730	292068.350067	38.689728
2420.697102	292512.094883	38.694746
2423.574746	292945.514113	38.699764
2425.692169	293401.026184	38.704781
2428.314309	293836.186247	38.709799
2431.231451	294281.789905	38.714816
2433.248698	294732.691964	38.719834
2436.272036	295175.431924	38.724852
2438.527498	295621.188510	38.729869
2441.100022	296050.839728	38.734887
2443.625749	296503.435551	38.739904
2446.109811	296949.356209	38.744922
2448.693920	297380.425232	38.749940
2450.593529	297835.936802	38.754957
2453.403613	298287.949924	38.759975
2456.302499	298730.320574	38.764992
2458.374212	299179.247859	38.770010
2461.118092	299620.142154	38.775028
2463.728756	300075.128923	38.780045
2466.049647	300522.412923	38.785063
2468.972696	300978.567009	38.790080
2471.349390	301421.343665	38.795098
2474.080624	301851.895679	38.800116
2476.718154	302301.563110	38.805133
2478.775403	302742.379977	38.810151
2481.369808	303188.266871	38.815168
2484.066762	303645.515849	38.820186
2486.088750	304078.790268	38.825204
2488.703807	304522.967991	38.830221
2491.276205	304965.703249	38.835239
2493.849415	305411.662875	38.840256
2496.327238	305868.025039	38.845274
2499.043329	306310.530025	38.850292
2501.130247	306758.187945	38.855309
2503.639579	307206.996635	38.860327
2506.583603	307617.786873	38.865344
2508.402864	308036.069289	38.870362
2510.552071	308452.037436	38.875380
2513.025400	308875.166459	38.880397
2515.461798	309296.267893	38.885415
2517.873791	309725.702901	38.890432
2520.031095	310166.505037	38.895450
2522.600020	310594.311887	38.900468
2524.574049	311044.461479	38.905485
2527.036166	311502.507429	38.910503
2529.963799	311935.256207	38.915520
2532.082463	312411.843674	38.920538
2534.468900	312867.406971	38.925556
2537.023159	313332.898234	38.930573
2539.515018	313801.851657	38.935591
2542.010935	314266.611589	38.940608
2544.364018	314747.418722	38.945626
2547.125972	315219.523348	38.950644
2549.738122	315713.873247	38.955661
2551.874797	316197.450995	38.960679
2554.846411	316668.779185	38.965696
2557.170758	317178.533484	38.970714
2559.482109	317661.212955	38.975732
2562.356493	318162.112705	38.980749
2564.999348	318652.303299	38.985767
2567.816524	319160.140494	38.990784
2570.053099	319664.003349	38.995802
2572.960972	320147.032909	39.000820
2575.848280	320650.711121	39.005837
2578.166699	321160.724357	39.010855
2581.215717	321657.564954	39.015872
2583.930617	322163.547762	39.020890
2586.078616	322666.544490	39.025908
2589.048675	323162.144697	39.030925
2591.284453	323682.213464	39.035943
2594.352257	324176.090786	39.040960
2596.860276	324689.888200	39.045978
2599.483577	325194.648666	39.050996
2602.394860	325707.969581	39.056013
2604.882914	326206.675702	39.061031
2608.067388	326700.494100	39.066048
2610.629047	327210.940429	39.071066
2613.375196	327704.974435	39.076084
2616.078471	328199.088322	39.081101
2618.679673	328701.747889	39.086119
2621.886316	329192.525193	39.091136
2624.627568	329683.753991	39.096154
2627.183213	330175.745447	39.101172
2629.778360	330658.585554	39.106189
2632.286240	331152.508111	39.111207
2635.018457	331637.173896	39.116224
2637.434193	332139.027279	39.121242
2639.980242	332620.364067	39.126260
2642.851520	333108.324543	39.131277
2645.339483	333594.107810	39.136295
2648.291081	334053.685008	39.141312
2650.644006	334510.510039	39.146330
2652.863034	334963.417434	39.151348
2655.715698	335420.055750	39.156365
2658.078921	335875.879822	39.161383
2660.659775	336334.535673	39.166400
2663.297636	336809.404797	39.171418
2665.430705	337275.412631	39.176436
2668.279873	337755.929295	39.181453
2670.874800	338232.978724	39.186471
2673.240246	338720.903047	39.191488
2675.770487	339219.868061	39.196506
2678.364032	339705.514429	39.201524
2681.307077	340201.791181	39.206541
2683.758369	340708.120352	39.211559
2686.329187	341202.213856	39.216576
2689.154400	341709.161259	39.221594
2691.826968	342223.060094	39.226612
2694.587135	342729.984031	39.231629
2697.038550	343250.307442	39.236647
2699.948490	343766.186839	39.241664
2702.276833	344283.093310	39.246682
2704.823048	344809.456155	39.251700
2707.901649	345333.927427	39.256717
2710.261754	345869.856334	39.261735
2713.688278	346391.978086	39.266752
2717.010073	346922.235791	39.271770
2719.674936	347446.271150	39.276788
2722.511557	347970.909175	39.281805
2725.400791	348496.600261	39.286823
2728.336053	349018.318799	39.291840
2730.753256	349546.537300	39.296858
2733.829995	350061.090026	39.301876
2736.522701	350571.662368	39.306893
2739.199605	351111.273837	39.311911
2741.834199	351632.532863	39.316928
2744.812451	352156.651736	39.321946
2747.097727	352694.532387	39.326964
2750.382823	353218.008375	39.331981
2752.943769	353768.679179	39.336999
2755.854947	354288.522956	39.342016
2758.439939	354824.836673	39.347034
2761.132336	355363.006217	39.352052
2764.089797	355897.472918	39.357069
2766.709485	356437.165684	39.362087
2769.579275	356965.187690	39.367104
2772.635805	357505.002927	39.372122
2775.115256	358039.776459	39.377140
2778.187199	358579.602990	39.382157
2780.910439	359117.397513	39.387175
2783.923898	359645.342879	39.392192
2786.848436	360186.139552	39.397210
2789.579018	360717.493761	39.402228
2792.393882	361241.366806	39.407245
2795.204088	361769.270341	39.412263
2798.128434	362273.241774	39.417280
2800.830462	362763.791654	39.422298
2803.193186	363254.846964	39.427316
2806.038111	363748.054147	39.432333
2808.391277	364252.500773	39.437351
2811.078013	364749.681470	39.442368
2814.176423	365266.460002	39.447386
2816.625987	365783.411545	39.452404
2819.846973	366271.126478	39.457421
2822.271741	366783.274072	39.462439
2824.760356	367313.905857	39.467456
2827.823303	367834.264166	39.472474
2830.447235	368354.051453	39.477492
2833.625124	368874.455448	39.482509
2836.383224	369410.196214	39.487527
2839.324367	369932.807444	39.492544
2842.091720	370479.140697	39.497562
2844.869394	370996.791320	39.502580
2847.821116	371542.498231	39.507597
2850.675029	372086.919529	39.512615
2853.221577	372635.848369	39.517632
2856.401077	373179.138322	39.522650
2858.776374	373717.321569	39.527668
2861.782868	374286.353385	39.532685
2864.960117	374844.668330	39.537703
2867.754374	375404.990027	39.542720
2870.641008	375961.914919	39.547738
2873.678452	376525.202041	39.552756
2876.328354	377076.059862	39.557773
2879.285663	377652.055102	39.562791
2882.387191	378216.247149	39.567808
2885.332025	378789.462528	39.572826
2888.234314	379352.122370	39.577844
2890.946505	379933.070487	39.582861
2893.733347	380504.941298	39.587879
2896.788792	381081.302241	39.592896
2899.593610	381660.586299	39.597914
2902.182165	382249.561173	39.602932
2905.691469	382801.699322	39.607949
2908.501077	383417.257442	39.612967
2911.731579	383985.074232	39.617984
2914.735455	384561.999608	39.623002
2917.654343	385139.436878	39.628020
2920.711664	385731.428678	39.633037
2923.487880	386313.588343	39.638055
2926.638097	386870.897918	39.643072
2929.983857	387445.821913	39.648090
2932.732461	388034.451998	39.653108
2935.852884	388600.947100	39.658125
2938.414077	389181.877569	39.663143
2941.282384	389761.684786	39.668160
2944.790005	390330.627635	39.673178
2947.429722	390903.122656	39.678196
2950.350234	391476.198018	39.683213
2953.210338	392058.226202	39.688231
2956.226890	392603.142133	39.693248
2959.230529	393126.393595	39.698266
2961.869087	393677.337639	39.703284
2965.193223	394202.576291	39.708301
2967.833050	394749.293261	39.713319
2970.615053	395269.250538	39.718336
2973.591511	395817.317242	39.723354
2976.680654	396366.422303	39.728372
2979.252480	396915.067792	39.733389
2982.221150	397460.852203	39.738407
2985.040306	398024.020926	39.743424
2987.904933	398577.917779	39.748442
2990.229176	399164.346766	39.753460
2993.656476	399732.461446	39.758477
2996.578457	400316.949692	39.763495
2999.353669	400895.213435	39.768512
3002.391142	401487.902723	39.773530
3005.162153	402075.248309	39.778548
3008.276628	402674.318170	39.783565
3011.185119	403275.412319	39.788583
3014.276019	403868.454908	39.793600
3017.719882	404480.824827	39.798618
3020.291942	405090.025155	39.803636
3023.329419	405697.314768	39.808653
3026.513016	406313.340750	39.813671
3029.455257	406931.674248	39.818688
3032.262919	407546.569190	39.823706
3035.158717	408185.975731	39.828724
3038.242819	408800.928630	39.833741
3041.152026	409444.692072	39.838759
3044.408695	410076.727123	39.843776
3047.481978	410707.814821	39.848794
3050.329231	411356.160564	39.853812
3053.843567	411992.474233	39.858829
3057.102499	412632.895331	39.863847
3060.140414	413294.880563	39.868864
3063.415503	413922.370814	39.873882
3066.257854	414591.276842	39.878900
3069.507099	415218.059215	39.883917
3072.624061	415859.826428	39.888935
3075.844338	416502.551435	39.893952
3079.004453	417162.579769	39.898970
3081.665507	417818.972170	39.903988
3085.088806	418479.257994	39.909005
3088.622887	419112.296303	39.914023
3091.292480	419767.375480	39.919040
3094.708943	420416.493456	39.924058
3097.781107	421073.226911	39.929076
3101.007559	421707.015692	39.934093
3104.116519	422353.400946	39.939111
3107.182826	423001.196694	39.944128
3110.496863	423649.419415	39.949146
3113.524782	424304.208498	39.954164
3116.735198	424946.640591	39.959181
3119.796411	425586.978441	39.964199
3122.743681	426194.360877	39.969216
3125.755142	426790.522523	39.974234
3128.545578	427425.641112	39.979252
3131.795575	428020.015137	39.984269
3134.462374	428630.046611	39.989287
3137.464428	429274.789377	39.994304
3140.555941	429868.159241	39.999322
3142.991039	430528.462788	40.004340
3146.040013	431136.324248	40.009357
3149.199560	431796.329248	40.014375
3151.923404	432449.142886	40.019392
3155.302980	433092.820125	40.024410
3158.123360	433784.030325	40.029428
3161.399703	434431.312013	40.034445
3164.353684	435131.125954	40.039463
3167.354275	435799.334554	40.044480
3170.769870	436467.535868	40.049498
3173.759043	437165.844677	40.054516
3176.279578	437859.042593	40.059533
3179.926196	438569.767891	40.064551
3182.760916	439267.156279	40.069568
3186.319503	439972.892621	40.074586
3189.368004	440707.426350	40.079604
3192.593446	441410.566387	40.084621
3195.788899	442137.944991	40.089639
3198.788436	442875.510143	40.094656
3202.372060	443588.606689	40.099674
3205.552980	444349.085020	40.104692
3208.861857	445043.853897	40.109709
3212.385000	445805.750803	40.114727
3215.619344	446528.383745	40.119744
3219.282458	447224.754312	40.124762
3222.482745	448004.299475	40.129780
3225.753121	448703.523347	40.134797
3229.485910	449441.680626	40.139815
3232.481951	450189.649648	40.144832
3236.235345	450888.124250	40.149850
3239.315357	451674.854525	40.154868
3242.437938	452380.267289	40.159885
3246.140678	453081.264656	40.164903
3249.180521	453850.162158	40.169920
3252.633107	454548.168018	40.174938
3256.443971	455259.101541	40.179956
3259.627128	456037.922181	40.184973
3262.864439	456727.291884	40.189991
3266.464179	457452.206438	40.195008
3269.922058	458207.631469	40.200026
3272.811651	458904.376365	40.205044
3276.537060	459629.604715	40.210061
3279.461908	460352.304851	40.215079
3283.264050	461053.896888	40.220096
3286.048076	461804.346961	40.225114
3289.432303	462498.926376	40.230132
3292.683274	463239.185654	40.235149
3296.022158	463933.675574	40.240167
3299.073731	464597.635269	40.245184
3302.208157	465313.914920	40.250202
3305.285485	465971.757900	40.255220
3308.750824	466625.927993	40.260237
3311.730189	467334.475951	40.265255
3314.848762	467982.336635	40.270272
3318.055725	468687.970805	40.275290
3320.699179	469397.058745	40.280308
3324.181563	470085.761283	40.285325
3326.845299	470793.230807	40.290343
3329.580844	471525.797250	40.295360
3333.093221	472248.607258	40.300378
3336.845001	472965.033434	40.305396
3339.557178	473720.178400	40.310413
3343.368343	474462.531999	40.315431
3346.621124	475194.177697	40.320448
3349.754195	475974.148636	40.325466
3353.329910	476694.263076	40.330484
3356.546370	477463.142109	40.335501
3360.083153	478246.954774	40.340519
3363.025185	478998.377892	40.345536
3366.797141	479744.738264	40.350554
3370.109161	480556.650402	40.355572
3372.966169	481316.642272	40.360589
3377.141151	482068.663491	40.365607
3380.198348	482901.392728	40.370624
3383.339834	483663.724911	40.375642
3387.466921	484430.419546	40.380660
3390.329266	485277.884599	40.385677
3393.863559	486064.518177	40.390695
3396.776206	486848.590273	40.395712
3400.755334	487634.027954	40.400730
3404.653034	488441.222394	40.405748
3407.691730	489277.973078	40.410765
3411.085130	490082.145918	40.415783
3414.902785	490906.172105	40.420800
3418.349592	491707.690476	40.425818
3421.622004	492494.502423	40.430836
3425.088271	493303.930311	40.435853
3428.617043	494100.534016	40.440871
3431.899099	494920.325305	40.445888
3435.320954	495739.047859	40.450906
3439.243817	496542.554243	40.455924
3442.482361	497362.091675	40.460941
3446.239648	498176.662326	40.465959
3449.638512	498991.253011	40.470976
3453.503732	499773.417082	40.475994
3457.005187	500594.483284	40.481012
3460.209355	501442.974568	40.486029
3463.855955	502255.711799	40.491047
3467.059901	503077.165217	40.496064
3470.433219	503896.181110	40.501082
3474.482324	504697.586099	40.506100
3477.604680	505507.278440	40.511117
3481.011466	506306.478607	40.516122
3484.615851	507053.473084	40.521127
3487.946475	507738.746465	40.526132
3490.915424	508363.686024	40.531136
3493.538693	508922.932430	40.536141
3497.056155	509433.953841	40.541146
3499.448222	509918.070210	40.546151
3500.923877	510349.246141	40.551156
3503.923698	510688.903190	40.556160
3505.795631	510960.535398	40.561165
3507.774673	511230.729838	40.566170
3509.580965	511457.491064	40.571175
3511.275340	511631.249890	40.576180
3512.869670	511729.595327	40.581184
3514.004103	511814.050505	40.586189
3515.147632	511863.294477	40.591194
3516.086691	511869.823665	40.596199
3516.894054	511871.567790	40.601204
3517.803626	511864.139300	40.606208
3518.364483	511797.931725	40.611213
3519.377969	511694.874414	40.616218
3519.817063	511571.621064	40.621223
3520.178582	511427.789178	40.626228
3521.008084	511239.615888	40.631232
3521.154175	511084.786534	40.636237
3520.565822	510923.950350	40.641242
3520.765082	510741.537384	40.646247
3521.152569	510541.334909	40.651252
3522.122629	510318.676039	40.656256
3521.865863	510100.053282	40.661261
3521.673460	509888.601925	40.666266
3521.730855	509707.971196	40.671271
3521.524124	509475.975630	40.676276
3521.596790	509215.447257	40.681280
3520.976986	508981.182902	40.686285
3521.068728	508744.728417	40.691290
3520.689733	508505.713998	40.696295
3520.487518	508270.665640	40.701300
3521.245133	508005.355692	40.706304
3520.994833	507779.466790	40.711309
3520.806404	507522.901022	40.716314
3520.553203	507285.013720	40.721319
3520.478252	507023.008267	40.726324
3520.006094	506770.018409	40.731328
3519.577885	506549.454984	40.736333
3518.962100	506341.923748	40.741338
3519.164500	506119.433467	40.746343
3518.708920	505910.707874	40.751348
3518.599889	505688.362546	40.756352
3518.363534	505424.334378	40.761357
3518.822133	505183.218929	40.766362
3518.299207	504961.132232	40.771367
3517.651658	504746.248902	40.776372
3517.489913	504521.164242	40.781376
3517.233008	504314.766929	40.786381
3517.007486	504110.639725	40.791386
3516.975992	503915.235262	40.796391
3516.432998	503745.012979	40.801396
3516.419421	503558.408200	40.806400
3516.322262	503324.390292	40.811405
3516.132709	503123.788922	40.816410
3515.398176	502964.420717	40.821415
3515.296620	502796.346561	40.826420
3515.532731	502612.324315	40.831424
3514.837759	502449.149097	40.836429
3514.766782	502255.554736	40.841434
3514.794651	502080.569566	40.846439
3514.332319	501902.926831	40.851444
3514.377749	501746.107133	40.856448
3514.388126	501592.581766	40.861453
3514.100335	501417.235034	40.866458
3513.690498	501259.065697	40.871463
3513.500254	501094.836545	40.876468
3513.253966	500917.149855	40.881472
3513.131664	500749.616503	40.886477
3512.931369	500622.691784	40.891482
3512.596380	500480.398638	40.896487
3512.336242	500370.996499	40.901492
3512.420964	500234.102177	40.906496
3512.094788	500054.495937	40.911501
3511.723591	499949.411680	40.916506
3511.631150	499840.688523	40.921511
3511.718053	499675.896349	40.926516
3511.730459	499536.325107	40.931520
3511.364879	499415.796584	40.936525
3511.069184	499300.369280	40.941530
3510.773512	499196.888677	40.946535
3510.492297	499091.683944	40.951540
3510.461200	498989.020957	40.956544
3510.449230	498902.149548	40.961549
3510.523586	498801.139470	40.966554
3510.075714	498689.276121	40.971559
3509.830394	498607.249662	40.976564
3509.980924	498491.088516	40.981568
3510.133638	498352.700994	40.986573
3509.234521	498278.826090	40.991578
3509.294115	498197.660874	40.996583
3509.148728	498122.501768	41.001588
3509.106094	498035.428536	41.006592
3509.082201	497979.235121	41.011597
3509.353799	497894.035415	41.016602
3508.957806	497764.741984	41.021607
3508.856392	497675.296764	41.026612
3508.854195	497632.262380	41.031616
3508.774446	497540.889168	41.036621
3508.462921	497445.046094	41.041626
3508.500901	497387.170291	41.046631
3507.868415	497328.033265	41.051636
3507.987264	497254.195812	41.056640
3508.187080	497214.065060	41.061645
3508.081223	497145.224448	41.066650
3508.156187	497084.911575	41.071655
3507.954421	497028.338291	41.076660
3508.009324	496946.712556	41.081664
3507.728367	496901.037059	41.086669
3507.780588	496827.259039	41.091674
3507.859332	496753.020845	41.096679
3507.735225	496665.802043	41.101684
3507.197789	496636.064799	41.106688
3507.343150	496573.764467	41.111693
3507.593072	496542.839351	41.116698
3507.541380	496452.468892	41.121703
3507.434129	496383.220567	41.126708
3507.152643	496309.341302	41.131712
3507.224473	496265.127438	41.136717
3507.214614	496217.939028	41.141722
3507.739891	496160.134214	41.146727
3507.680760	496109.408988	41.151732
3507.295080	496052.152882	41.156736
3506.876087	496022.041482	41.161741
3506.773963	496008.082714	41.166746
3506.543714	495952.422005	41.171751
3506.439887	495872.943182	41.176756
3506.926529	495851.599940	41.181760
3506.563465	495785.934172	41.186765
3506.567589	495740.261349	41.191770
3507.278939	495705.717484	41.196775
3507.004113	495666.519142	41.201780
3506.354603	495630.671191	41.206784
3506.279676	495626.581591	41.211789
3506.377306	495577.956774	41.216794
3506.602554	495520.096095	41.221799
3506.087884	495483.618924	41.226804
3506.463235	495453.077227	41.231808
3506.338508	495450.666419	41.236813
3506.111460	495393.940169	41.241818
3506.277414	495346.468552	41.246823
3506.637731	495288.889610	41.251828
3506.000590	495274.660398	41.256832
3506.112934	495261.122885	41.261837
3506.221691	495230.319140	41.266842
3505.974289	495211.369787	41.271847
3505.971411	495163.063573	41.276852
3506.087063	495111.092698	41.281856
3505.706727	495077.277200	41.286861
3505.619296	495047.364973	41.291866
3506.138071	495030.927420	41.296871
3505.944017	495016.273520	41.301876
3505.869846	494996.537020	41.306880
3505.868164	494936.330461	41.311885
3506.006622	494865.569110	41.316890
3505.596729	494867.709969	41.321895
3505.433645	494858.469181	41.326900
3506.072714	494845.151931	41.331904
3506.018001	494826.830004	41.336909
3505.537473	494807.360075	41.341914
3505.926353	494778.384866	41.346919
3505.679832	494740.445999	41.351924
3505.557612	494688.207706	41.356928
3505.818149	494646.238795	41.361933
3505.866919	494623.089758	41.366938
3505.925855	494595.888085	41.371943
3505.856138	494553.009048	41.376948
3505.780501	494520.359669	41.381952
3505.860442	494495.382587	41.386957
3505.489341	494510.632538	41.391962
3505.556168	494503.633931	41.396967
3505.628773	494469.593812	41.401972
3505.566318	494445.348099	41.406976
3505.188220	494416.341634	41.411981
3504.668703	494391.003417	41.416986
3505.443868	494358.118000	41.421991
3505.459202	494330.770913	41.426996
3505.708055	494307.134111	41.432000
3505.462895	494311.274528	41.437005
3505.036983	494302.378832	41.442010
3505.092852	494282.975482	41.447015
3505.114196	494275.528232	41.452020
3505.495546	494254.807447	41.457024
3505.643737	494253.163560	41.462029
3505.465866	494193.184977	41.467034
3505.747387	494187.519559	41.472039
3505.109363	494150.046466	41.477044
3505.204356	494111.090190	41.482048
3505.535909	494071.235579	41.487053
3505.516576	494072.453935	41.492058
3505.238369	494069.915287	41.497063
3504.951180	494064.592915	41.502068
3505.350206	494058.706329	41.507072
3505.028441	494052.174083	41.512077
3504.985649	494001.288545	41.517082
3505.267892	493999.572808	41.522087
3504.853461	494000.397865	41.527092
3504.916911	493978.967431	41.532096
3505.336284	493912.614276	41.537101
3505.532244	493895.973543	41.542106
3505.462887	493868.942996	41.547111
3505.009452	493855.088762	41.552116
3505.090561	493822.666572	41.557120
3505.268564	493816.207169	41.562125
3504.917623	493806.590428	41.567130
3504.306563	493812.763736	41.572135
3504.245671	493822.091021	41.577140
3504.645136	493813.013991	41.582144
3504.853145	493803.967218	41.587149
3504.841551	493819.312834	41.592154
3505.064836	493767.574363	41.597159
3505.176930	493734.235605	41.602164
3505.267955	493723.991926	41.607168
3504.665685	493729.454914	41.612173
3505.233448	493701.209342	41.617178
3505.327190	493663.518321	41.622183
3504.795969	493658.436962	41.627188
3504.797114	493646.283124	41.632192
3504.704870	493657.084010	41.637197
3504.943632	493660.084643	41.642202
3504.908902	493660.039457	41.647207
3504.691665	493650.249582	41.652212
3505.130363	493644.154035	41.657216
3504.826829	493585.408705	41.662221
3504.801310	493570.777657	41.667226
3505.273637	493597.592958	41.672231
3504.968846	493574.802333	41.677236
3504.529213	493555.172696	41.682240
3504.801858	493549.711048	41.687245
3504.589939	493530.602437	41.692250
3504.675623	493518.992198	41.697255
3504.425467	493524.399590	41.702260
3504.981154	493511.297126	41.707264
3505.043719	493497.512987	41.712269
3504.658749	493494.687290	41.717274
3504.728798	493470.824480	41.722279
3504.827266	493460.022433	41.727284
3504.758317	493456.336530	41.732288
3504.914873	493450.842562	41.737293
3504.965522	493448.808896	41.742298
3505.040127	493394.712774	41.747303
3504.972199	493369.301777	41.752308
3505.400649	493347.205232	41.757312
3505.584716	493326.514593	41.762317
3505.089068	493316.717905	41.767322
3505.798247	493299.944879	41.772327
3505.137295	493297.213413	41.777332
3504.880974	493291.784656	41.782336
3504.866578	493289.305484	41.787341
3504.575262	493232.228259	41.792346
3504.899151	493252.534801	41.797351
3505.033296	493228.661548	41.802356
3505.141862	493181.750495	41.807360
3504.833030	493202.916717	41.812365
3504.706036	493222.231090	41.817370
3505.064019	493165.658729	41.822375
3505.129978	493133.490936	41.827380
3505.088682	493103.669554	41.832384
3505.089242	493105.644453	41.837389
3504.971449	493107.232926	41.842394
3504.756812	493122.509927	41.847399
3504.670229	493094.468142	41.852404
3504.803153	493085.686096	41.857408
3504.667271	493065.501512	41.862413
3504.301911	493057.557835	41.867418
3504.806192	493080.722630	41.872423
3504.978839	493020.583564	41.877428
3504.483915	493034.284401	41.882432
3504.513433	493052.915868	41.887437
3504.739570	492993.072108	41.892442
3504.939669	492978.354291	41.897447
3504.495542	493003.998614	41.902452
3504.586153	493012.036313	41.907456
3504.780670	492954.071174	41.912461
3504.561580	492966.006635	41.917466
3505.169480	492982.875569	41.922471
3504.727745	492920.402474	41.927476
3505.048493	492886.826646	41.932480
3505.211194	492874.545483	41.937485
3504.960971	492860.506456	41.942490
3505.243809	492853.473084	41.947495
3504.185755	492868.529107	41.952500
3504.714983	492882.270749	41.957504
3504.719820	492865.152879	41.962509
3504.788586	492816.120218	41.967514
3504.932667	492819.439807	41.972519
3504.577148	492823.699282	41.977524
3504.441487	492820.834075	41.982528
3504.685642	492810.616332	41.987533
3504.731255	492818.104161	41.992538
3504.911055	492779.283610	41.997543
3504.787287	492767.857934	42.002548
3504.467650	492770.086049	42.007552
3504.652228	492782.666819	42.012557
3504.619908	492720.330910	42.017562
3505.161420	492709.154544	42.022567
3504.187479	492728.552653	42.027572
3504.568230	492725.757736	42.032576
3504.613047	492731.929017	42.037581
3504.274261	492690.658117	42.042586
3504.994054	492668.514718	42.047591
3504.187953	492710.422340	42.052596
3504.280211	492712.180217	42.057600
3504.651743	492669.125790	42.062605
3504.831167	492647.270346	42.067610
3504.609926	492673.183753	42.072615
3504.554977	492682.966455	42.077620
3504.672227	492651.903862	42.082624
3504.725584	492619.281387	42.087629
3504.476735	492660.543971	42.092634
3504.909381	492624.519129	42.097639
3504.534391	492587.659655	42.102644
3504.489949	492602.960825	42.107648
3504.722359	492621.256798	42.112653
3505.092658	492566.199955	42.117658
3504.540803	492565.274285	42.122663
3504.482069	492602.860647	42.127668
3504.789552	492574.249362	42.132672
3504.621616	492537.053202	42.137677
3504.528704	492561.477829	42.142682
3504.992913	492539.425317	42.147687
3504.846580	492504.808479	42.152692
3504.163091	492528.668132	42.157696
3504.870071	492510.172878	42.162701
3504.454076	492479.953931	42.167706
3504.746472	492497.531538	42.172711
3504.673371	492457.889355	42.177716
3505.030620	492472.418134	42.182720
3504.914718	492457.901783	42.187725
3504.814317	492436.292894	42.192730
3505.059561	492436.406027	42.197735
3504.680142	492425.172479	42.202740
3504.812118	492403.324248	42.207744
3504.979594	492392.004239	42.212749
3504.732858	492375.837266	42.217754
3504.972992	492388.105661	42.222759
3504.621186	492347.646355	42.227764
3504.793590	492349.037093	42.232768
3504.832471	492352.221463	42.237773
3504.590512	492330.077745	42.242778
3504.906509	492304.959116	42.247783
3504.616360	492318.628110	42.252788
3504.120569	492308.425760	42.257792
3504.770738	492273.226803	42.262797
3504.322298	492287.123415	42.267802
3504.476002	492264.511931	42.272807
3504.128866	492297.687831	42.277812
3504.284657	492259.933512	42.282816
3504.257483	492273.662262	42.287821
3504.027356	492247.465067	42.292826
3504.387800	492255.257868	42.297831
3504.251415	492249.708560	42.302836
3504.467574	492256.055492	42.307840
3504.451366	492246.233100	42.312845
3504.746410	492250.339233	42.317850
3504.572787	492217.346779	42.322855
3504.577731	492217.092743	42.327860
3504.575285	492209.749713	42.332864
3504.856477	492227.278703	42.337869
3504.680815	492197.375818	42.342874
3505.098285	492171.734531	42.347879
3504.557854	492182.505824	42.352884
3504.591545	492145.631523	42.357888
3504.806356	492145.192382	42.362893
3504.501209	492158.256134	42.367898
3504.668818	492121.512551	42.372903
3504.583372	492123.906302	42.377908
3504.912785	492144.668981	42.382912
3505.181620	492080.662717	42.387917
3504.362765	492097.757967	42.392922
3504.658752	492065.754550	42.397927
3504.614118	492084.499995	42.402932
3504.596511	492093.821305	42.407936
3504.625723	492063.733890	42.412941
3504.790033	492028.206111	42.417946
3504.549595	492042.221962	42.422951
3504.395122	492045.791457	42.427956
3504.315086	492010.352909	42.432960
3504.467699	492016.507389	42.437965
3504.695196	492047.921636	42.442970
3504.570991	491993.650287	42.447975
3504.492358	491988.243707	42.452980
3504.512265	491995.583996	42.457984
3504.658108	491967.858289	42.462989
3504.478298	491990.271611	42.467994
3504.736156	491941.004183	42.472999
3504.286523	491940.315545	42.478004
3504.360781	491968.715461	42.483008
3504.873139	491958.201637	42.488013
3504.336143	491922.784505	42.493018
3504.594963	491944.571460	42.498023
3504.933406	491905.622726	42.503028
3504.658284	491915.440631	42.508032
3504.696521	491916.447449	42.513037
3504.673385	491913.969475	42.518042
3504.677987	491891.533041	42.523047
3504.695635	491839.872358	42.528052
3504.526574	491870.589908	42.533056
3504.838570	491835.139709	42.538061
3504.567463	491862.834698	42.543066
3504.646450	491802.098764	42.548071
3504.619288	491830.312340	42.553076
3504.880450	491803.783644	42.558080
3504.295351	491796.481899	42.563085
3504.705528	491815.307663	42.568090
3504.980234	491760.060973	42.573095
3504.652028	491760.771202	42.578100
3504.451887	491771.742171	42.583104
3504.859414	491766.208040	42.588109
3504.839633	491722.706829	42.593114
3505.133769	491698.553104	42.598119
3504.431350	491710.109952	42.603124
3504.654248	491723.900871	42.608128
3504.826447	491701.640299	42.613133
3504.742809	491662.200673	42.618138
3504.447707	491698.509433	42.623143
3504.582794	491690.232843	42.628148
3504.540301	491641.417261	42.633152
3504.816089	491662.087662	42.638157
3504.615419	491620.893853	42.643162
3504.602010	491610.614874	42.648167
3504.244313	491633.309969	42.653172
3504.595753	491615.021965	42.658176
3504.209699	491589.253656	42.663181
3504.328982	491620.685727	42.668186
3504.686243	491610.601388	42.673191
3504.748187	491554.881264	42.678196
3504.166965	491573.863971	42.683200
3504.671481	491588.471456	42.688205
3504.607363	491558.549917	42.693210
3504.343417	491547.652107	42.698215
3504.139733	491563.992214	42.703220
3504.494739	491556.693720	42.708224
3504.698927	491512.447579	42.713229
3503.821535	491550.773206	42.718234
3504.356890	491543.243618	42.723239
3504.571907	491559.517550	42.728244
3504.300433	491524.716089	42.733248
3504.758228	491497.244253	42.738253
3504.542547	491485.731027	42.743258
3504.220691	491503.305368	42.748263
3504.483199	491508.784249	42.753268
3504.565246	491487.550591	42.758272
3504.787216	491455.456537	42.763277
3504.711171	491453.695910	42.768282
3504.817286	491428.153464	42.773287
3504.706244	491433.387532	42.778292
3503.809083	491461.941759	42.783296
3504.767375	491476.933423	42.788301
3504.627399	491418.813800	42.793306
3504.172091	491411.592681	42.798311
3504.329151	491429.293980	42.803316
3504.458794	491446.290550	42.808321
3504.734449	491384.559900	42.813325
3504.461228	491387.084717	42.818330
3504.189350	491391.989695	42.823335
3503.843002	491398.121952	42.828340
3504.529683	491399.026307	42.833345
3504.508680	491408.449787	42.838349
3504.699664	491371.599744	42.843354
3504.125040	491369.867267	42.848359
3504.577844	491378.962641	42.853364
3504.591239	491330.593232	42.858369
3504.564115	491337.941213	42.863373
3503.727223	491365.979596	42.868378
3504.460812	491368.953036	42.873383
3504.533603	491366.155949	42.878388
3504.256856	491342.497168	42.883393
3504.623290	491300.858494	42.888397
3504.555821	491298.083567	42.893402
3504.527120	491297.733543	42.898407
3504.307902	491314.278909	42.903412
3504.304495	491324.155469	42.908417
3504.582627	491320.464930	42.913421
3504.344323	491308.549999	42.918426
3504.590716	491294.937762	42.923431
3504.323234	491286.876563	42.928436
3504.375082	491271.674369	42.933441
3504.383260	491250.755998	42.938445
3504.329202	491244.686912	42.943450
3504.453934	491230.030277	42.948455
3503.847379	491279.202683	42.953460
3503.743649	491277.142536	42.958465
3503.799068	491277.336328	42.963469
3503.527522	491295.611964	42.968474
3504.234270	491300.159700	42.973479
3504.462395	491288.373619	42.978484
3504.511221	491282.794748	42.983489
3504.548261	491257.870746	42.988493
3504.271429	491260.193565	42.993498
3504.362707	491241.996965	42.998503
3504.055815	491254.555156	43.003508
3504.291298	491255.581480	43.008513
3504.907527	491256.041158	43.013517
3504.628494	491246.563662	43.018522
3504.947709	491181.887955	43.023527
3504.452131	491198.477103	43.028532
3504.133509	491189.714890	43.033537
3504.095407	491180.908335	43.038541
3504.078848	491190.533810	43.043546
3504.537313	491180.331951	43.048551
3504.817774	491145.999662	43.053556
3504.046026	491167.393298	43.058561
3504.487715	491167.475392	43.063565
3504.180454	491180.590805	43.068570
3504.514192	491119.761745	43.073575
3504.358660	491146.375938	43.078580
3504.227755	491146.396595	43.083585
3504.134672	491147.120330	43.088589
3504.478980	491168.641443	43.093594
3504.859168	491126.341800	43.098599
3504.605074	491104.299839	43.103604
3504.488042	491133.744198	43.108609
3505.218788	491086.172420	43.113613
3504.354933	491103.984744	43.118618
3504.790991	491068.462838	43.123623
3504.612592	491091.889955	43.128628
3504.397781	491041.226104	43.133633
3504.521360	491059.844694	43.138637
3504.470738	491025.868398	43.143642
3504.542766	491041.253732	43.148647
3504.489074	491028.954912	43.153652
3504.143966	491031.946964	43.158657
3504.656499	490992.158460	43.163661
3504.344616	491034.346247	43.168666
3504.615270	491012.980946	43.173671
3504.546053	491004.027284	43.178676
3504.426375	491007.844712	43.183681
3504.365954	490984.303227	43.188685
3504.263188	490988.978991	43.193690
3504.498885	490984.636679	43.198695
3504.553635	490967.559828	43.203700
3503.744673	490966.522767	43.208705
3504.346415	490973.163724	43.213709
3504.285758	490931.693032	43.218714
3504.694280	490927.171448	43.223719
3504.717554	490933.194786	43.228724
3504.568524	490931.040465	43.233729
3503.782921	490929.290645	43.238733
3503.856154	490935.913856	43.243738
3504.349462	490894.355522	43.248743
3504.534159	490886.577212	43.253748
3504.114999	490909.080307	43.258753
3504.381402	490920.636450	43.263757
3504.241425	490945.121274	43.268762
3504.226291	490945.022337	43.273767
3504.042753	490898.050419	43.278772
3504.157472	490917.480912	43.283777
3504.202280	490870.067652	43.288781
3504.162064	490917.429470	43.293786
3504.552507	490925.167440	43.298791
3504.646545	490927.381032	43.303796
3504.577150	490891.584151	43.308801
3504.720935	490867.605063	43.313805
3504.401361	490884.875736	43.318810
3504.088662	490864.615423	43.323815
3504.501902	490882.580633	43.328820
3504.313473	490859.413758	43.333825
3504.326690	490878.151267	43.338829
3504.475151	490830.063104	43.343834
3504.560925	490847.320391	43.348839
3504.263374	490858.965709	43.353844
3504.288302	490812.669696	43.358849
3504.225778	490847.170669	43.363853
3504.216238	490865.709197	43.368858
3504.188513	490805.240136	43.373863
3504.501673	490819.726525	43.378868
3504.323888	490800.609717	43.383873
3504.262003	490807.659513	43.388877
3504.236716	490819.160527	43.393882
3504.370904	490798.373678	43.398887
3504.475203	490791.975528	43.403892
3504.185849	490795.617227	43.408897
3504.632504	490762.321573	43.413901
3504.321013	490782.477995	43.418906
3504.367118	490760.844013	43.423911
3504.333037	490792.605601	43.428916
3504.420566	490788.286663	43.433921
3504.634646	490724.638955	43.438925
3504.418212	490758.404698	43.443930
3504.509363	490732.205246	43.448935
3504.258315	490754.732601	43.453940
3504.677557	490706.854563	43.458945
3504.451456	490707.346099	43.463949
3504.436228	490717.478087	43.468954
3504.049455	490687.758100	43.473959
3504.230006	490729.767441	43.478964
3504.880843	490693.552455	43.483969
3504.760662	490654.622965	43.488973
3503.994176	490669.938544	43.493978
3504.772166	490678.780270	43.498983
3504.682523	490650.330112	43.503988
3504.366936	490639.490583	43.508993
3504.431161	490659.131918	43.513997
3504.353351	490644.912026	43.519002
3504.160808	490634.914067	43.524007
3504.324431	490626.277960	43.529012
3503.855095	490654.816436	43.534017
3504.367820	490617.255631	43.539021
3504.478319	490614.705715	43.544026
3504.510229	490609.534505	43.549031
3504.266838	490595.239451	43.554036
3504.426478	490606.508772	43.559041
3504.463423	490586.142246	43.564045
3504.384714	490584.635199	43.569050
3504.186023	490582.691281	43.574055
3504.063452	490548.016415	43.579060
3503.961565	490572.799595	43.584065
3504.713195	490564.830247	43.589069
3504.379495	490566.301114	43.594074
3504.288484	490558.211708	43.599079
3504.198621	490550.274062	43.604084
3504.309686	490553.801868	43.609089
3504.330488	490531.411893	43.614093
3504.141221	490529.061291	43.619098
3504.228632	490556.448298	43.624103
3504.267246	490565.710834	43.629108
3504.343949	490526.091528	43.634113
3504.080927	490531.451167	43.639117
3504.584467	490536.183156	43.644122
3504.604277	490511.514130	43.649127
3504.562922	490511.419335	43.654132
3504.114659	490540.815679	43.659137
3504.448502	490496.850543	43.664141
3504.621569	490492.821909	43.669146
3504.250941	490489.081805	43.674151
3504.233417	490473.687336	43.679156
3503.842314	490494.667028	43.684161
3504.523030	490502.713834	43.689165
3504.078604	490467.026069	43.694170
3503.857450	490492.182748	43.699175
3504.170379	490505.757740	43.704180
3504.566748	490457.224251	43.709185
3503.843417	490471.469545	43.714189
3503.628773	490477.935824	43.719194
3504.132840	490502.673969	43.724199
3504.434743	490468.640946	43.729204
3504.460347	490449.694229	43.734209
3504.423351	490450.561071	43.739213
3504.572970	490480.166903	43.744218
3504.474865	490460.125477	43.749223
3504.775049	490458.963724	43.754228
3504.464348	490445.135033	43.759233
3504.807213	490395.698163	43.764237
3504.182935	490416.866744	43.769242
3504.065702	490415.720316	43.774247
3504.394989	490400.726810	43.779252
3504.229761	490423.747486	43.784257
3504.425891	490398.645251	43.789261
3504.513707	490411.546807	43.794266
3504.430452	490422.601386	43.799271
3504.773592	490413.734212	43.804276
3504.400544	490393.482929	43.809281
3504.283648	490359.667850	43.814285
3504.244433	490374.615472	43.819290
3504.363724	490383.966643	43.824295
3504.811021	490372.398591	43.829300
3504.477004	490324.537342	43.834305
3504.856964	490280.057919	43.839309
3504.751993	490306.361414	43.844314
3504.475593	490296.680424	43.849319
3504.560367	490288.968311	43.854324
3504.647606	490250.410393	43.859329
3505.027214	490250.603605	43.864333
3504.430446	490256.573215	43.869338
3504.432495	490273.945560	43.874343
3504.461447	490279.563017	43.879348
3504.449141	490280.223368	43.884353
3504.997411	490236.730224	43.889357
3504.972193	490185.071759	43.894362
3504.203034	490210.112833	43.899367
3504.617773	490214.453746	43.904372
3504.354704	490194.032915	43.909377
3504.601413	490162.287290	43.914381
3504.123205	490171.479758	43.919386
3504.120220	490191.436102	43.924391
3504.409579	490197.215021	43.929396
3504.440717	490150.967047	43.934401
3503.997664	490144.098046	43.939405
3504.462635	490153.040147	43.944410
3504.128412	490108.014756	43.949415
3504.152312	490140.831924	43.954420
3504.288100	490144.102652	43.959425
3504.073472	490144.237840	43.964429
3504.164299	490163.926137	43.969434
3504.415583	490139.118736	43.974439
3504.675910	490101.242250	43.979444
3504.314280	490082.609617	43.984449
3504.582660	490082.972361	43.989453
3504.117964	490107.003103	43.994458
3504.340594	490126.873205	43.999463
3504.593420	490129.365691	44.004468
3504.304390	490092.791610	44.009473
3504.421184	490046.023342	44.014477
3503.708642	490072.929694	44.019482
3504.019351	490087.974183	44.024487
3504.262676	490082.161616	44.029492
3504.168325	490059.586682	44.034497
3504.468844	490038.367505	44.039501
3504.117535	490051.389366	44.044506
3504.484063	490061.309417	44.049511
3504.519619	490025.392999	44.054516
3504.603734	490009.222336	44.059521
3504.549992	490003.304749	44.064525
3504.494894	490030.968295	44.069530
3504.592855	490029.129380	44.074535
3504.541939	490030.910141	44.079540
3504.095057	490005.250567	44.084545
3504.319489	489998.427960	44.089549
3504.373626	490011.284464	44.094554
3504.258071	489992.460898	44.099559
3504.316309	489953.704357	44.104564
3504.361001	489956.280415	44.109569
3503.718480	489977.351071	44.114573
3504.313272	489991.996185	44.119578
3504.297033	489956.999524	44.124583
3504.917634	489946.416822	44.129588
3504.329035	489954.512541	44.134593
3503.667295	489947.323482	44.139597
3503.975462	489942.260375	44.144602
3504.025081	489944.936956	44.149607
3504.213179	489947.135797	44.154612
3503.857360	489947.445254	44.159617
3503.977873	489947.375521	44.164621
3504.677927	489926.751520	44.169626
3504.363724	489915.708753	44.174631
3504.663231	489936.377308	44.179636
3503.603843	489964.199690	44.184641
3503.930734	489973.011751	44.189645
3504.441671	489993.646825	44.194650
3503.962121	489951.277830	44.199655
3504.564048	489900.887013	44.204660
3503.871992	489942.782783	44.209665
3504.278531	489907.212704	44.214669
3504.371399	489898.587448	44.219674
3504.212775	489941.867764	44.224679
3504.254329	489953.611993	44.229684
3504.197441	489953.722250	44.234689
3504.420738	489954.294723	44.239693
3504.454703	489915.744541	44.244698
3503.654318	489896.674571	44.249703
3504.466584	489873.753514	44.254708
3504.187115	489860.527260	44.259713
3503.865371	489861.540437	44.264717
3504.034392	489881.925775	44.269722
3503.413500	489902.385292	44.274727
3504.131011	489907.640775	44.279732
3504.097815	489882.574101	44.284737
3503.884353	489907.426442	44.289741
3504.537839	489930.875467	44.294746
3504.286456	489917.340913	44.299751
3504.735146	489876.547140	44.304756
3503.814713	489881.099166	44.309761
3503.899639	489866.852965	44.314765
3504.118790	489873.706738	44.319770
3503.985372	489885.731917	44.324775
3504.296784	489868.816103	44.329780
3504.212414	489879.668575	44.334785
3504.033579	489874.125272	44.339789
3503.412096	489879.085899	44.344794
3503.897574	489875.868811	44.349799
3504.294712	489906.246828	44.354804
3503.942834	489901.845189	44.359809
3504.294876	489850.480729	44.364813
3504.433194	489866.312400	44.369818
3504.214403	489879.060182	44.374823
3504.686375	489872.350355	44.379828
3504.407503	489841.193765	44.384833
3504.031579	489839.176481	44.389837
3503.990656	489857.974214	44.394842
3503.971429	489881.732230	44.399847
3504.031745	489862.526184	44.404852
3503.940546	489844.002522	44.409857
3504.431511	489856.435534	44.414861
3504.415077	489875.330680	44.419866
3503.974264	489883.352420	44.424871
3504.411958	489876.242810	44.429876
3503.994188	489846.830294	44.434881
3504.426667	489804.114212	44.439885
3504.179461	489791.186713	44.444890
3504.282040	489817.660687	44.449895
3504.124624	489845.239377	44.454900
3503.963464	489847.594734	44.459905
3504.039645	489847.228106	44.464909
3504.287842	489861.776153	44.469914
3504.352989	489841.556315	44.474919
3504.337211	489820.994692	44.479924
3504.476301	489803.498251	44.484929
3504.479248	489778.527027	44.489933
3504.666454	489760.009928	44.494938
3504.478705	489781.211525	44.499943
3504.195403	489775.684704	44.504948
3504.027277	489755.805548	44.509953
3504.276739	489727.452348	44.514957
3504.262646	489730.189681	44.519962
3504.332392	489733.268316	44.524967
3504.943569	489728.765067	44.529972
3504.312654	489729.725817	44.534977
3504.715775	489708.793957	44.539981
3504.876623	489691.749830	44.544986
3504.680126	489691.527600	44.549991
3504.595897	489687.032955	44.554996
3504.666168	489662.202888	44.560001
3504.499092	489684.870201	44.565005
3504.325872	489714.325661	44.570010
3503.848419	489703.460524	44.575015
3503.816812	489687.966337	44.580020
3503.712255	489690.312767	44.585025
3503.716064	489684.841841	44.590029
3504.289009	489670.163799	44.595034
3504.226066	489662.424127	44.600039
3504.384899	489707.073030	44.605044
3503.734201	489686.307711	44.610049
3503.787548	489658.745168	44.615053
3504.086479	489682.807704	44.620058
3503.623694	489702.685287	44.625063
3503.830296	489695.764089	44.630068
3504.027284	489722.324576	44.635073
3503.839464	489702.651080	44.640077
3504.342832	489696.290784	44.645082
3504.074916	489714.111522	44.650087
3504.036589	489677.902216	44.655092
3503.767111	489670.347144	44.660097
3504.173552	489646.274336	44.665101
3504.040675	489698.465705	44.670106
3503.900306	489701.476254	44.675111
3503.918781	489671.893211	44.680116
3503.563722	489680.509293	44.685121
3503.753184	489683.163807	44.690125
3503.946235	489682.272195	44.695130
3503.770592	489678.197203	44.700135
3503.922574	489701.067321	44.705140
3504.421814	489712.941962	44.710145
3504.340719	489676.587461	44.715149
3504.461398	489683.203614	44.720154
3503.982389	489711.896997	44.725159
3504.028186	489705.862282	44.730164
3504.127799	489714.761039	44.735169
3504.186958	489723.159678	44.740173
3504.309744	489726.584486	44.745178
3504.332622	489730.683544	44.750183
3504.498718	489700.013547	44.755188
3504.621749	489655.775866	44.760193
3504.015717	489653.085820	44.765197
3504.213398	489651.484361	44.770202
3504.517357	489638.925500	44.775207
3504.484979	489631.535541	44.780212
3504.309513	489623.408430	44.785217
3504.498694	489649.818300	44.790221
3504.222295	489652.749056	44.795226
3504.170005	489657.873030	44.800231
3504.436742	489656.311308	44.805236
3504.320653	489669.194951	44.810241
3504.384980	489656.522024	44.815245
3504.522488	489639.532190	44.820250
3504.103740	489626.732994	44.825255
3503.800383	489601.151486	44.830260
3504.553965	489578.239348	44.835265
3504.528857	489566.137658	44.840269
3504.336748	489611.602024	44.845274
3504.058369	489601.769035	44.850279
3503.985874	489568.148122	44.855284
3503.614523	489574.335572	44.860289
3503.470677	489576.941482	44.865293
3503.736268	489592.246754	44.870298
3503.683941	489611.299791	44.875303
3503.925698	489612.274565	44.880308
3504.117258	489621.209485	44.885313
3504.209975	489619.118104	44.890317
3504.415387	489639.852508	44.895322
3504.230176	489609.288542	44.900327
3504.351938	489560.036383	44.905332
3504.277265	489574.483731	44.910337
3503.947100	489586.996058	44.915341
3505.027740	489549.647272	44.920346
3504.757453	489538.901249	44.925351
3504.373552	489531.313556	44.930356
3504.310323	489542.922649	44.935361
3504.396053	489551.418468	44.940365
3504.381799	489582.773752	44.945370
3504.165844	489593.748489	44.950375
3504.785695	489582.405938	44.955380
3504.329578	489567.586562	44.960385
3504.212508	489549.168002	44.965389
3504.266018	489516.945316	44.970394
3504.004493	489498.600190	44.975399
3504.647187	489486.696806	44.980404
3504.428704	489483.844177	44.985409
3504.296596	489467.403317	44.990413
3504.345927	489447.185556	44.995418
3504.473247	489454.459210	45.000423
3504.765906	489446.409986	45.005428
3504.812716	489447.668839	45.010433
3504.513520	489427.759403	45.015437
3504.539089	489415.801562	45.020442
3504.256098	489418.632093	45.025447
3504.496917	489440.576757	45.030452
3504.096714	489446.971414	45.035457
3504.299471	489427.590457	45.040461
3504.113920	489405.738277	45.045466
3504.382800	489381.382965	45.050471
3504.192436	489385.110590	45.055476
3504.290377	489433.112773	45.060481
3504.002567	489438.831198	45.065485
3504.326531	489434.423929	45.070490
3504.310862	489422.523262	45.075495
3504.187335	489409.474649	45.080500
3503.976610	489394.869609	45.085505
3504.091803	489398.447632	45.090509
3503.893192	489398.276384	45.095514
3503.664884	489385.092361	45.100519
3503.892113	489359.527964	45.105524
3504.277656	489343.157133	45.110529
3504.448967	489353.766887	45.115533
3504.009452	489374.958081	45.120538
3504.306749	489387.624622	45.125543
3504.528599	489399.847214	45.130548
3504.500820	489353.961160	45.135553
3503.897423	489362.414032	45.140557
3504.456333	489348.193825	45.145562
3504.367757	489326.326225	45.150567
3503.792236	489356.858866	45.155572
3504.314130	489363.411715	45.160577
3504.070272	489380.722448	45.165581
3504.333082	489366.194495	45.170586
3504.207541	489322.147276	45.175591
3503.981175	489353.941682	45.180596
3504.124362	489366.176730	45.185601
3504.062704	489351.446792	45.190605
3504.296799	489335.657060	45.195610
3503.877702	489347.980994	45.200615
3504.553061	489292.258516	45.205620
3504.225994	489316.471115	45.210625
3504.131082	489347.079762	45.215629
3504.212731	489301.226936	45.220634
3504.705231	489287.371744	45.225639
3505.032956	489277.898653	45.230644
3504.203412	489285.982087	45.235649
3503.538983	489289.176837	45.240653
3504.545544	489291.550302	45.245658
3504.322965	489313.821617	45.250663
3504.084841	489316.138553	45.255668
3504.333498	489326.837401	45.260673
3504.022190	489310.779292	45.265677
3503.996535	489291.940817	45.270682
3504.128691	489289.995122	45.275687
3504.325016	489254.507694	45.280692
3503.806741	489250.638721	45.285697
3504.131347	489248.409344	45.290701
3504.440998	489217.766527	45.295706
3504.204500	489259.237240	45.300711
3504.056350	489282.864430	45.305716
3504.118673	489260.618340	45.310721
3504.324603	489237.691048	45.315725
3504.151571	489264.969141	45.320730
3503.954356	489290.427548	45.325735
3504.220675	489264.907498	45.330740
3504.217767	489250.066891	45.335745
3503.970517	489235.315545	45.340749
3503.568828	489219.372947	45.345754
3504.020795	489221.530167	45.350759
3504.320530	489200.867348	45.355764
3504.229920	489204.781850	45.360769
3504.051453	489253.537308	45.365773
3504.092445	489263.610539	45.370778
3503.700950	489270.054531	45.375783
3503.997543	489259.826572	45.380788
3503.911831	489268.298964	45.385793
3503.972964	489261.096688	45.390797
3504.278492	489222.198255	45.395802
3504.571952	489207.260119	45.400807
3503.774879	489238.030578	45.405812
3503.975346	489252.384031	45.410817
3504.259275	489258.822574	45.415821
3504.397661	489267.614110	45.420826
3503.742257	489233.173000	45.425831
3503.928362	489215.060759	45.430836
3504.047852	489205.823153	45.435841
3503.567812	489216.535937	45.440845
3503.812683	489217.206328	45.445850
3503.578178	489248.090460	45.450855
3503.978293	489241.796985	45.455860
3504.625331	489230.247318	45.460865
3504.641068	489203.551142	45.465869
3504.567493	489181.022525	45.470874
3504.453691	489185.396566	45.475879
3504.673588	489187.337210	45.480884
3504.490194	489205.094416	45.485889
3504.111244	489213.967746	45.490893
3504.397731	489210.224825	45.495898
3504.139522	489178.658658	45.500903
3504.227701	489155.699227	45.505908
3504.305991	489163.487264	45.510913
3504.269685	489192.314070	45.515917
3504.384033	489188.345093	45.520922
3504.442194	489184.384996	45.525927
3504.461981	489174.251395	45.530932
3504.710553	489130.853730	45.535937
3503.980125	489153.965288	45.540941
3504.803252	489159.356247	45.545946
3504.429657	489139.306309	45.550951
3504.609942	489076.418167	45.555956
3504.228714	489102.615046	45.560961
3504.021393	489121.946336	45.565965
3504.281138	489132.238323	45.570970
3504.182907	489104.192407	45.575975
3504.066047	489094.282971	45.580980
3504.301007	489109.340216	45.585985
3504.039809	489118.245631	45.590989
3504.201167	489109.254623	45.595994
3504.348411	489056.704720	45.600999
3504.044379	489058.626884	45.606004
3504.004254	489090.088380	45.611009
3504.578848	489105.699774	45.616013
3504.632800	489075.958234	45.621018
3504.607656	489028.602053	45.626023
3505.032699	489027.420480	45.631028
3504.184889	489043.003487	45.636033
3503.738017	489063.993580	45.641037
3504.310321	489064.156351	45.646042
3504.385790	489074.325538	45.651047
3504.399167	489058.773073	45.656052
3504.244660	489051.047623	45.661057
3504.283466	489056.866496	45.666061
3504.422400	489041.496781	45.671066
3504.076085	489030.559875	45.676071
3503.819239	489024.674083	45.681076
3504.624295	488983.670102	45.686081
3504.067983	488984.467135	45.691085
3503.951370	489000.035911	45.696090
3503.863817	488981.662784	45.701095
3504.178656	488953.247440	45.706100
3504.225226	488963.066685	45.711105
3504.035544	488997.287224	45.716109
3504.227614	488995.990514	45.721114
3503.769157	488991.656158	45.726119
3504.267469	488964.579454	45.731124
3503.996943	488975.005994	45.736129
3503.809233	488982.278969	45.741133
3504.209956	488966.867816	45.746138
3504.503731	488964.693931	45.751143
3504.473958	488960.291811	45.756148
3504.391307	488976.108502	45.761153
3504.237953	488936.370264	45.766157
3504.529498	488933.791506	45.771162
3503.989720	488939.803171	45.776167
3504.432711	488925.297054	45.781172
3504.263342	488946.395374	45.786177
3503.783135	488963.034705	45.791181
3503.994618	488948.717156	45.796186
3503.800399	488943.783844	45.801191
3504.508966	488932.325578	45.806196
3504.411247	488899.720521	45.811201
3504.194210	488892.156848	45.816205
3504.374195	488890.254206	45.821210
3503.981014	488904.296531	45.826215
3504.054084	488902.967971	45.831220
3504.371852	488953.975800	45.836225
3504.253258	488963.719846	45.841229
3504.196305	488938.706327	45.846234
3503.926339	488921.172420	45.851239
3504.343663	488892.588827	45.856244
3504.437268	488925.093172	45.861249
3504.095770	488923.880792	45.866253
3504.322434	488892.237508	45.871258
3504.460437	488864.407164	45.876263
3504.149136	488895.000091	45.881268
3503.983512	488892.139016	45.886273
3504.450888	488866.535997	45.891277
3503.886386	488879.744318	45.896282
3503.948327	488844.834546	45.901287
3504.181154	488842.315710	45.906292
3503.880006	488879.593264	45.911297
3503.946987	488846.506207	45.916301
3504.055717	488869.333515	45.921306
3503.857140	488850.825851	45.926311
3504.228549	488864.696702	45.931316
3504.421131	488858.841128	45.936321
3503.430158	488860.567971	45.941325
3504.098369	488848.457543	45.946330
3504.221230	488842.309066	45.951335
3504.223990	488830.860992	45.956340
3504.294609	488837.029476	45.961345
3503.908197	488896.303912	45.966349
3504.359373	488895.877994	45.971354
3504.246650	488889.158933	45.976359
3503.839058	488864.504655	45.981364
3503.607820	488857.652356	45.986369
3504.022880	488883.571718	45.991373
3504.323906	488889.957032	45.996378
3503.901318	488876.043566	46.001383
3503.828342	488866.481646	46.006388
3504.176030	488873.416773	46.011393
3503.852443	488885.421992	46.016397
3504.170289	488859.386722	46.021402
3504.141683	488854.477862	46.026407
3504.150066	488826.313378	46.031412
3504.356777	488828.053530	46.036417
3503.905106	488844.333883	46.041421
3504.189951	488844.339479	46.046426
3504.115243	488853.164889	46.051431
3504.199410	488854.569837	46.056436
3504.483622	488830.312700	46.061441
3504.322333	488818.991855	46.066445
3504.687979	488791.783914	46.071450
3504.241712	488779.697636	46.076455
3504.150861	488823.071107	46.081460
3504.158962	488818.662967	46.086465
3504.014936	488795.689149	46.091469
3504.587152	488779.592245	46.096474
3504.366509	488781.906482	46.101479
3503.976406	488802.634625	46.106484
3504.311725	488755.170133	46.111489
3504.304489	488764.542106	46.116493
3504.512048	488785.175803	46.121498
3504.436770	488752.617599	46.126503
3504.334912	488778.618808	46.131508
3504.032158	488752.124296	46.136513
3504.187909	488705.599822	46.141517
3504.275014	488703.813149	46.146522
3504.007334	488708.667502	46.151527
3504.107890	488719.288796	46.156532
3504.114040	488765.129085	46.161537
3503.824651	488751.802314	46.166541
3504.241417	488720.280657	46.171546
3504.183970	488711.779925	46.176551
3503.830116	488760.817640	46.181556
3504.090462	488770.197969	46.186561
3503.686778	488771.781340	46.191565
3504.140246	488772.925309	46.196570
3504.209735	488778.283539	46.201575
3504.020882	488734.954107	46.206580
3504.217845	488709.849499	46.211585
3504.154999	488721.509688	46.216589
3504.314710	488706.187071	46.221594
3504.323588	488703.754267	46.226599
3503.761758	488732.462222	46.231604
3504.318896	488732.272820	46.236609
3503.793350	488745.728344	46.241613
3504.186078	488725.404882	46.246618
3503.432292	488713.924356	46.251623
3503.469191	488716.957696	46.256628
3504.506316	488694.455558	46.261633
3504.359525	488690.173177	46.266637
3504.771757	488691.374324	46.271642
3504.522398	488686.753580	46.276647
3504.696596	488676.595307	46.281652
3504.202191	488661.781271	46.286657
3504.050622	488700.048607	46.291661
3504.313304	488719.761900	46.296666
3504.113346	488707.130110	46.301671
3503.842459	488691.622274	46.306676
3503.834211	488693.700336	46.311681
3504.120521	488681.396898	46.316685
3504.090576	488667.167951	46.321690
3504.088806	488711.135439	46.326695
3504.014047	488689.771454	46.331700
3504.273619	488671.951004	46.336705
3504.406915	488648.730560	46.341709
3504.271736	488641.356462	46.346714
3504.137726	488681.393938	46.351719
3504.012377	488683.085282	46.356724
3504.249002	488661.570742	46.361729
3504.191076	488651.905027	46.366733
3503.895004	488647.443618	46.371738
3503.952351	488648.498245	46.376743
3503.992364	488651.227181	46.381748
3504.316201	488631.876927	46.386753
3504.264252	488628.288693	46.391757
3504.245421	488610.461536	46.396762
3503.788833	488622.842518	46.401767
3503.561347	488668.314740	46.406772
3504.343390	488659.022799	46.411777
3503.953304	488649.460238	46.416781
3504.582854	488609.546916	46.421786
3504.559136	488649.567026	46.426791
3504.369745	488632.273383	46.431796
3503.965973	488623.270162	46.436801
3504.186436	488618.676449	46.441805
3504.714394	488623.607681	46.446810
3504.139364	488602.322670	46.451815
3504.174726	488613.359558	46.456820
3504.284832	488601.945033	46.461825
3504.236992	488593.392076	46.466829
3504.203912	488611.024771	46.471834
3504.167609	488614.626888	46.476839
3503.883418	488594.055703	46.481844
3503.699349	488578.787321	46.486849
3503.762717	488582.069767	46.491853
3504.557583	488559.656416	46.496858
3504.457124	488560.837298	46.501863
3504.205693	488541.071339	46.506868
3504.215597	488535.193886	46.511873
3504.207570	488565.942023	46.516877
3504.235848	488549.880247	46.521882
3504.121239	488569.349407	46.526887
3504.068408	488601.776144	46.531892
3503.966396	488599.006277	46.536897
3504.066959	488607.094946	46.541901
3504.112388	488583.331119	46.546906
3504.165744	488558.907509	46.551911
3504.078057	488553.349409	46.556916
3504.471158	488555.161435	46.561921
3504.239821	488523.235350	46.566925
3503.830926	488518.842397	46.571930
3504.060884	488554.719641	46.576935
3504.082750	488551.524956	46.581940
3503.877510	488528.611143	46.586945
3504.010038	488536.188250	46.591949
3504.004439	488531.731556	46.596954
3504.633044	488508.381998	46.601959
3504.448172	488549.187601	46.606964
3504.408308	488570.164563	46.611969
3504.040351	488540.944754	46.616973
3504.391633	488530.454490	46.621978
3504.145661	488529.530909	46.626983
3504.196175	488491.127171	46.631988
3504.494092	488483.937828	46.636993
3503.848819	488525.576063	46.641997
3504.164416	488499.793925	46.647002
3504.548968	488486.816331	46.652007
3504.100744	488538.858123	46.657012
3504.200687	488506.271801	46.662017
3503.924054	488485.597996	46.667021
3504.260157	488461.534803	46.672026
3504.039645	488507.158270	46.677031
3503.829825	488491.184731	46.682036
3504.570003	488443.807432	46.687041
3503.906408	488494.920956	46.692045
3504.433825	488472.296504	46.697050
3504.572190	488470.400399	46.702055
3504.068915	488509.382213	46.707060
3504.421481	488491.901473	46.712065
3504.087298	488452.494727	46.717069
3504.180179	488414.843950	46.722074
3504.262612	488465.535711	46.727079
3503.892720	488437.987635	46.732084
3504.255350	488423.544492	46.737089
3504.142920	488473.760489	46.742093
3504.076727	488467.793735	46.747098
3504.157235	488461.499866	46.752103
3503.707555	488444.500464	46.757108
3503.848312	488444.022294	46.762113
3504.405132	488432.334442	46.767117
3504.542790	488445.381427	46.772122
3504.496000	488448.478691	46.777127
3504.161214	488428.269903	46.782132
3504.048595	488414.459066	46.787137
3504.145456	488400.412493	46.792141
3503.946071	488391.326201	46.797146
3504.389105	488433.501781	46.802151
3504.277817	488431.543823	46.807156
3504.309960	488414.670854	46.812161
3504.174581	488413.273899	46.817165
3504.155604	488388.101689	46.822170
3504.392871	488405.337264	46.827175
3504.138496	488373.009334	46.832180
3504.604573	488353.788278	46.837185
3504.302058	488397.550756	46.842189
3504.017098	488378.144507	46.847194
3504.630442	488340.715246	46.852199
3503.806186	488383.040591	46.857204
3504.240189	488367.015840	46.862209
3504.206625	488355.117331	46.867213
3504.126145	488356.295068	46.872218
3503.819659	488343.021366	46.877223
3504.294635	488320.405023	46.882228
3504.493681	488348.891984	46.887233
3504.221359	488370.868341	46.892237
3504.093964	488378.182668	46.897242
3504.055867	488349.822206	46.902247
3503.940096	488331.959454	46.907252
3504.634406	488316.248098	46.912257
3504.234850	488299.595224	46.917261
3504.594954	488289.609979	46.922266
3504.686729	488297.142968	46.927271
3504.404990	488298.707102	46.932276
3504.672512	488260.015324	46.937281
3504.221129	488250.006356	46.942285
3504.097775	488283.356568	46.947290
3504.446409	488303.360635	46.952295
3504.144179	488298.140299	46.957300
3503.923104	488288.500186	46.962305
3504.022658	488269.742214	46.967309
3504.909214	488243.970793	46.972314
3504.441561	488229.608083	46.977319
3504.215042	488262.265471	46.982324
3504.597088	488246.147522	46.987329
3504.327725	488233.374422	46.992333
3504.563915	488206.844618	46.997338
3504.267454	488216.211921	47.002343
3503.966703	488224.516148	47.007348
3504.001142	488189.660174	47.012353
3504.267473	488171.686222	47.017357
3504.332884	488188.898502	47.022362
3504.222085	488215.205825	47.027367
3503.834348	488199.564090	47.032372
3503.829839	488185.887964	47.037377
3504.344058	488173.801450	47.042381
3504.523872	488173.418410	47.047386
3504.943512	488162.765175	47.052391
3504.810948	488148.906643	47.057396
3504.773814	488127.282803	47.062401
3504.769392	488118.520150	47.067405
3504.384795	488086.769520	47.072410
3503.984326	488093.569912	47.077415
3503.774045	488099.732380	47.082420
3504.262962	488134.809660	47.087425
3504.191404	488118.054129	47.092429
3504.383293	488103.789696	47.097434
3504.361732	488091.990435	47.102439
3504.498811	488073.125028	47.107444
3504.012578	488066.110125	47.112449
3503.757101	488083.373220	47.117453
3503.907130	488065.062965	47.122458
3504.669597	488055.165965	47.127463
3504.002711	488068.391029	47.132468
3504.460089	488057.934391	47.137473
3504.557931	488056.905788	47.142477
3503.973346	488084.149316	47.147482
3503.966134	488055.023706	47.152487
3504.164772	488031.792180	47.157492
3504.064000	488062.454481	47.162497
3503.864660	488031.231684	47.167501
3504.541776	488001.845862	47.172506
3504.541273	488050.829556	47.177511
3503.899477	488075.853310	47.182516
3503.986662	488044.939833	47.187521
3503.888999	488046.930789	47.192525
3503.962725	488037.041331	47.197530
3504.131806	488034.633775	47.202535
3503.721660	488073.753727	47.207540
3503.568590	488046.829329	47.212545
3503.907931	488037.404441	47.217549
3504.129416	488012.345692	47.222554
3504.230934	488066.277441	47.227559
3504.065866	488073.293909	47.232564
3504.118247	488064.218321	47.237569
3504.083820	488045.430650	47.242573
3504.103161	488028.407396	47.247578
3504.184141	488044.097689	47.252583
3503.935944	488065.462722	47.257588
3504.086577	488027.954017	47.262593
3503.563592	488018.614763	47.267597
3503.560315	488035.230175	47.272602
3504.171570	488042.579847	47.277607
3503.955096	488060.647281	47.282612
3503.936925	488056.952290	47.287617
3504.009470	488070.921618	47.292621
3503.446539	488064.729319	47.297626
3504.017291	488047.061720	47.302631
3503.778955	488060.421674	47.307636
3503.942352	488084.912906	47.312641
3503.928907	488051.989142	47.317645
3503.472128	488067.815068	47.322650
3503.833787	488078.800692	47.327655
3503.705910	488062.256634	47.332660
3504.255342	488054.824755	47.337665
3504.160844	488098.048491	47.342669
3504.012927	488067.729417	47.347674
3504.214041	488046.422415	47.352679
3504.033886	488097.106008	47.357684
3504.217545	488072.610523	47.362689
3503.595719	488070.530602	47.367693
3503.665130	488079.789488	47.372698
3504.081348	488065.489569	47.377703
3503.690649	488115.497219	47.382708
3503.442449	488090.208880	47.387713
3503.924650	488061.056578	47.392717
3503.979571	488084.703818	47.397722
3503.912265	488113.841092	47.402727
3504.068274	488076.382287	47.407732
3503.985107	488098.025131	47.412737
3504.041884	488088.594274	47.417741
3504.261400	488089.218060	47.422746
3504.163084	488098.503447	47.427751
3504.346649	488084.240316	47.432756
3503.840843	488099.314138	47.437761
3503.851626	488064.360362	47.442765
3504.200712	488059.087668	47.447770
3504.313178	488025.181508	47.452775
3504.028927	488062.711270	47.457780
3504.110217	488044.513169	47.462785
3504.012728	488062.004589	47.467789
3504.005241	488035.816992	47.472794
3504.030598	488040.574543	47.477799
3503.755376	488075.772711	47.482804
3504.074576	488041.378006	47.487809
3504.185305	488063.699415	47.492813
3503.801273	488068.926908	47.497818
3504.236217	488037.603867	47.502823
3504.040411	488047.056654	47.507828
3504.143132	488075.204664	47.512833
3504.035537	488062.608501	47.517837
3503.533905	488055.596028	47.522842
3504.428562	488025.112099	47.527847
3504.174624	488033.105078	47.532852
3503.946533	488068.143845	47.537857
3503.996098	488060.183114	47.542861
3504.142621	488045.925809	47.547866
3503.875768	488035.026422	47.552871
3503.981642	488006.693347	47.557876
3504.324229	488021.987721	47.562881
3504.200247	488041.154971	47.567885
3503.839273	488022.165615	47.572890
3504.802449	487981.185138	47.577895
3504.230063	488003.817211	47.582900
3504.314729	488035.362041	47.587905
3504.181706	488054.986604	47.592909
3504.106093	488048.160068	47.597914
3504.339570	488026.999894	47.602919
3503.823699	488003.729303	47.607924
3504.198920	487999.212291	47.612929
3504.005775	487991.391205	47.617933
3503.871705	487992.425469	47.622938
3503.896949	487989.787365	47.627943
3503.733585	487982.873365	47.632948
3504.524879	487969.020644	47.637953
3504.389811	487957.695139	47.642957
3504.448341	487958.850929	47.647962
3504.454950	487958.596573	47.652967
3504.416981	487962.199077	47.657972
3504.469177	487930.075214	47.662977
3504.329405	487946.053757	47.667981
3504.225557	487987.050381	47.672986
3504.056616	487943.817308	47.677991
3504.544283	487925.301585	47.682996
3504.217989	487971.044368	47.688001
3504.153397	487939.952089	47.693005
3504.392230	487944.726577	47.698010
3504.027803	487946.101187	47.703015
3504.045411	487923.506009	47.708020
3504.434497	487944.010617	47.713025
3504.096098	487930.539048	47.718029
3504.449686	487910.879426	47.723034
3504.221286	487948.907140	47.728039
3504.276258	487960.498518	47.733044
3504.310434	487930.454377	47.738049
3504.036320	487896.507779	47.743053
3503.962039	487883.247708	47.748058
3504.354771	487861.656934	47.753063
3503.909067	487863.854887	47.758068
3504.412270	487867.827773	47.763073
3504.283236	487847.991090	47.768077
3504.428151	487861.391919	47.773082
3504.034387	487875.688373	47.778087
3503.608538	487874.286633	47.783092
3503.763735	487889.762700	47.788097
3503.907827	487923.324548	47.793101
3504.136276	487896.542257	47.798106
3504.558945	487855.444320	47.803111
3503.860936	487859.708382	47.808116
3504.055651	487834.856254	47.813121
3504.500021	487814.473002	47.818125
3504.149614	487814.781632	47.823130
3504.226675	487809.298587	47.828135
3504.016049	487843.727135	47.833140
3504.305467	487868.958563	47.838145
3504.025863	487875.486650	47.843149
3504.173074	487883.517598	47.848154
3504.193955	487881.184103	47.853159
3504.192271	487863.860091	47.858164
3504.045400	487822.497515	47.863169
3503.790170	487828.667174	47.868173
3503.176477	487830.030535	47.873178
3503.423519	487851.368187	47.878183
3503.403912	487855.525022	47.883188
3504.281895	487833.908173	47.888193
3504.338217	487838.407601	47.893197
3503.916322	487887.762255	47.898202
3504.061504	487882.471085	47.903207
3503.954637	487883.906301	47.908212
3503.839873	487892.890454	47.913217
3504.174705	487894.711754	47.918221
3503.811494	487896.136831	47.923226
3504.112025	487888.136361	47.928231
3503.970486	487887.246896	47.933236
3503.694803	487872.701605	47.938241
3504.015003	487862.013264	47.943245
3504.171048	487854.136928	47.948250
3504.144126	487896.489294	47.953255
3503.793088	487902.167517	47.958260
3504.154679	487877.947591	47.963265
3503.961993	487878.889815	47.968269
3503.986461	487879.949682	47.973274
3503.706990	487874.928253	47.978279
3504.131561	487880.129301	47.983284
3504.359446	487888.248807	47.988289
3504.189940	487862.897072	47.993293
3503.638634	487842.873850	47.998298
3504.100485	487828.161295	48.003303
3504.129707	487861.741408	48.008308
3504.454929	487811.287469	48.013313
3504.078302	487835.560443	48.018317
3503.793114	487850.548935	48.023322
3503.874224	487837.669518	48.028327
3503.688954	487853.857952	48.033332
3503.590149	487847.490912	48.038337
3503.757164	487851.364971	48.043341
3503.835662	487843.703511	48.048346
3504.634219	487816.324440	48.053351
3504.273475	487822.206844	48.058356
3504.403338	487824.364483	48.063361
3504.600405	487821.800510	48.068365
3504.235444	487811.372404	48.073370
3504.035574	487791.040300	48.078375
3504.246710	487787.967539	48.083380
3504.310897	487778.028799	48.088385
3504.643139	487795.756475	48.093389
3503.826346	487818.579366	48.098394
3504.382248	487813.324572	48.103399
3504.069629	487808.713612	48.108404
3504.292015	487794.900030	48.113409
3504.223727	487817.959205	48.118413
3503.957553	487802.247273	48.123418
3503.870695	487773.994971	48.128423
3504.114339	487754.453877	48.133428
3504.029400	487778.782131	48.138433
3504.167948	487812.547675	48.143437
3504.009374	487807.203184	48.148442
3504.559727	487792.071366	48.153447
3503.961045	487776.361313	48.158452
3504.226167	487750.130235	48.163457
3504.125958	487799.484928	48.168461
3504.291949	487782.843522	48.173466
3504.327598	487756.243476	48.178471
3504.181313	487773.894840	48.183476
3504.410406	487731.003618	48.188481
3504.380983	487750.662775	48.193485
3503.742634	487739.568657	48.198490
3504.384419	487723.358556	48.203495
3504.087483	487754.254982	48.208500
3503.745978	487732.881427	48.213505
3503.938467	487735.991643	48.218509
3503.936498	487778.998854	48.223514
3504.414844	487735.511030	48.228519
3504.645265	487771.946894	48.233524
3504.070142	487731.259680	48.238529
3504.477072	487698.876734	48.243533
3504.137437	487740.873623	48.248538
3504.081102	487709.880976	48.253543
3504.388955	487679.438589	48.258548
3504.357058	487732.480559	48.263553
3503.852330	487719.440379	48.268557
3503.486178	487707.036816	48.273562
3503.901839	487701.145628	48.278567
3503.867918	487709.965121	48.283572
3504.052795	487702.540071	48.288577
3503.989105	487712.326735	48.293581
3503.732955	487726.196300	48.298586
3504.602930	487699.059052	48.303591
3504.520920	487687.421064	48.308596
3504.369751	487677.161717	48.313601
3504.334116	487703.711146	48.318605
3504.216135	487714.418200	48.323610
3504.415813	487706.636220	48.328615
3504.186387	487712.801838	48.333620
3504.294391	487708.985524	48.338625
3504.070043	487703.043527	48.343629
3504.159806	487685.248994	48.348634
3504.031582	487661.663432	48.353639
3504.045771	487659.381623	48.358644
3503.964215	487670.386883	48.363649
3504.127280	487670.158449	48.368653
3503.898498	487660.215298	48.373658
3503.951428	487639.589794	48.378663
3504.405442	487623.510600	48.383668
3504.234087	487610.417652	48.388673
3504.654771	487612.681318	48.393677
3504.184116	487631.245242	48.398682
3504.696394	487610.749728	48.403687
3504.542128	487588.789196	48.408692
3504.851028	487576.937384	48.413697
3504.639065	487571.145357	48.418701
3503.799316	487581.460003	48.423706
3504.225785	487550.998664	48.428711
3504.268702	487544.913060	48.433716
3504.170450	487537.076788	48.438721
3504.384293	487572.147927	48.443725
3504.199959	487592.591580	48.448730
3504.225194	487575.465677	48.453735
3503.758981	487577.210995	48.458740
3503.601910	487576.526597	48.463745
3503.716720	487561.767377	48.468749
3503.961793	487555.193916	48.473754
3503.790626	487558.209671	48.478759
3503.718426	487563.236043	48.483764
3504.343370	487544.799567	48.488769
3504.458342	487543.666916	48.493773
3504.105179	487601.116494	48.498778
3504.398811	487577.717432	48.503783
3504.521243	487534.386718	48.508788
3504.288858	487562.689766	48.513793
3504.292947	487558.687221	48.518797
3504.176100	487556.324798	48.523802
3504.047114	487531.371469	48.528807
3504.450291	487525.482200	48.533812
3504.359184	487510.603518	48.538817
3504.348397	487479.957895	48.543821
3504.320364	487478.594559	48.548826
3504.605502	487504.637654	48.553831
3504.483825	487527.249709	48.558836
3504.208452	487521.062437	48.563841
3504.383757	487495.351772	48.568845
3503.924892	487477.137193	48.573850
3504.301545	487460.360896	48.578855
3504.148635	487459.675835	48.583860
3503.647005	487458.336698	48.588865
3504.505233	487428.820056	48.593869
3504.371048	487429.398456	48.598874
3504.189851	487453.286428	48.603879
3504.025389	487487.758979	48.608884
3503.894661	487466.706406	48.613889
3504.305046	487460.613351	48.618893
3504.096193	487444.436152	48.623898
3504.507473	487481.755808	48.628903
3504.266859	487446.232754	48.633908
3503.704091	487429.706227	48.638913
3504.588199	487390.611287	48.643917
3504.610110	487389.240051	48.648922
3504.464743	487387.844598	48.653927
3504.394736	487394.593005	48.658932
3504.327909	487376.974905	48.663937
3504.918043	487364.622597	48.668941
3504.409867	487363.740401	48.673946
3504.285372	487376.120356	48.678951
3504.653821	487358.534755	48.683956
3504.379125	487336.187710	48.688961
3504.389184	487322.508662	48.693965
3504.049729	487377.474546	48.698970
3504.087963	487361.460851	48.703975
3503.649182	487353.171756	48.708980
3503.799039	487348.994156	48.713985
3504.033221	487349.463677	48.718989
3504.313636	487331.588023	48.723994
3504.380436	487351.738953	48.728999
3504.308981	487375.812304	48.734004
3504.031044	487364.053115	48.739009
3504.184188	487345.437735	48.744013
3504.167955	487321.783394	48.749018
3504.156304	487302.535476	48.754023
3504.719762	487280.157202	48.759028
3504.209442	487272.436609	48.764033
3504.250057	487279.927431	48.769037
3504.558394	487284.691100	48.774042
3504.011526	487267.402060	48.779047
3503.843434	487302.331435	48.784052
3503.506760	487279.943464	48.789057
3503.891427	487290.115392	48.794061
3503.800642	487309.430102	48.799066
3504.171576	487295.643338	48.804071
3504.496108	487283.434272	48.809076
3504.099412	487287.042946	48.814081
3504.263957	487239.804300	48.819085
3504.330770	487249.215972	48.824090
3504.108948	487262.776504	48.829095
3504.268533	487274.757022	48.834100
3504.283368	487291.674164	48.839105
3504.245857	487298.366811	48.844109
3503.758809	487303.306850	48.849114
3504.228858	487291.935962	48.854119
3503.818384	487275.435888	48.859124
3503.815886	487257.452909	48.864129
3504.102863	487268.096206	48.869133
3503.896182	487266.913064	48.874138
3503.831687	487255.221386	48.879143
3503.961743	487265.281600	48.884148
3504.287288	487290.001511	48.889153
3504.270579	487269.589243	48.894157
3504.123586	487218.955091	48.899162
3503.939756	487226.025493	48.904167
3503.615576	487260.371727	48.909172
3503.964164	487241.978640	48.914177
3504.381604	487219.522061	48.919181
3504.008103	487275.000195	48.924186
3504.051115	487258.681714	48.929191
3504.677361	487221.248220	48.934196
3504.253219	487234.283518	48.939201
3504.234622	487234.387738	48.944205
3503.401771	487255.694115	48.949210
3503.855570	487256.331556	48.954215
3503.892582	487248.473785	48.959220
3503.580992	487257.438691	48.964225
3504.385744	487252.195068	48.969229
3504.240174	487282.004529	48.974234
3504.244653	487281.193271	48.979239
3504.264964	487262.700120	48.984244
3504.160804	487254.358092	48.989249
3504.216617	487232.515916	48.994253
3504.120538	487215.712810	48.999258
3504.776462	487186.278428	49.004263
3504.268318	487192.285637	49.009268
3504.491600	487214.944853	49.014273
3504.589624	487160.675141	49.019277
3504.106036	487142.717438	49.024282
3503.907466	487158.250015	49.029287
3504.279055	487154.189298	49.034292
3503.847298	487176.242889	49.039297
3504.159626	487188.199319	49.044301
3504.304997	487145.421330	49.049306
3504.538425	487141.990340	49.054311
3503.726597	487157.923794	49.059316
3504.034794	487176.770314	49.064321
3504.587221	487169.844196	49.069325
3504.309956	487161.478830	49.074330
3504.350257	487156.204038	49.079335
3504.430569	487148.947274	49.084340
3504.061403	487142.369442	49.089345
3504.159052	487120.824472	49.094349
3504.523702	487098.274779	49.099354
3504.674531	487103.975228	49.104359
3504.127363	487128.124082	49.109364
3503.999018	487136.249557	49.114369
3504.539258	487117.522113	49.119373
3503.836607	487127.562043	49.124378
3504.040382	487136.901465	49.129383
3504.455521	487109.733960	49.134388
3504.041153	487098.502748	49.139393
3504.072971	487072.662221	49.144397
3504.454288	487055.124965	49.149402
3504.643361	487023.687151	49.154407
3504.405821	487044.038483	49.159412
3504.071942	487081.729991	49.164417
3504.062940	487061.620229	49.169421
3503.889120	487055.416754	49.174426
3504.563292	487030.487797	49.179431
3504.379084	487012.280019	49.184436
3503.990995	487021.763705	49.189441
3504.102922	487043.528882	49.194445
3503.906459	487026.234896	49.199450
3503.891651	487016.814825	49.204455
3504.458115	487002.490365	49.209460
3504.420482	486987.298876	49.214465
3504.270448	487006.217992	49.219469
3504.261244	487034.334572	49.224474
3504.136166	487046.968122	49.229479
3504.362184	487049.718546	49.234484
3504.036020	487007.622673	49.239489
3503.818468	486983.189206	49.244493
3503.911177	486983.630440	49.249498
3504.544513	486958.150605	49.254503
3504.299744	486991.978188	49.259508
3503.937281	487005.510473	49.264513
3503.869391	486975.632935	49.269517
3503.965955	486990.409787	49.274522
3503.759998	487004.525231	49.279527
3503.919922	486972.484045	49.284532
3504.001232	486988.935025	49.289537
3504.239215	487011.389526	49.294541
3503.957152	486992.639959	49.299546
3504.105090	486996.415892	49.304551
3504.210427	487005.466990	49.309556
3503.908307	486997.561403	49.314561
3504.600327	486966.398606	49.319565
3504.468934	487004.362209	49.324570
3504.443945	487004.062177	49.329575
3504.126974	486990.282607	49.334580
3504.058970	486976.970256	49.339585
3503.731897	486962.736341	49.344589
3503.647103	486970.449738	49.349594
3503.339642	486973.791075	49.354599
3503.663118	486969.484634	49.359604
3503.728808	486969.879482	49.364609
3504.355301	486956.659977	49.369613
3504.138416	486960.848188	49.374618
3503.982944	486971.612242	49.379623
3504.279907	486959.559303	49.384628
3504.193159	486993.564539	49.389633
3504.269680	486990.158322	49.394637
3503.580807	487008.959972	49.399642
3503.793534	486995.907210	49.404647
3504.203427	486986.774603	49.409652
3503.526290	486982.119740	49.414657
3503.626834	486966.906394	49.419661
3503.638330	486969.336131	49.424666
3504.103724	486949.252584	49.429671
3504.258908	486957.181347	49.434676
3504.067374	486992.317625	49.439681
3504.205735	486991.687826	49.444685
3503.988818	487001.600388	49.449690
3504.171470	487003.851094	49.454695
3504.054536	487003.514936	49.459700
3504.024115	487010.814459	49.464705
3503.893806	487006.782383	49.469709
3504.115930	486955.531953	49.474714
3503.983422	486957.984452	49.479719
3503.755716	486986.135639	49.484724
3504.053763	486991.356930	49.489729
3504.181872	487001.214959	49.494733
3503.805870	486998.690797	49.499738
3503.514014	486987.845419	49.504743
3503.837514	486987.287673	49.509748
3503.513490	486995.545453	49.514753
3503.636879	486996.792366	49.519757
3503.877350	486980.797044	49.524762
3503.847700	486974.317464	49.529767
3503.992460	486977.232717	49.534772
3503.703733	487001.999435	49.539777
3504.212754	487014.178176	49.544781
3504.231502	487006.880430	49.549786
3503.853905	486997.315060	49.554791
3504.642194	486979.814725	49.559796
3504.259529	486978.558065	49.564801
3504.381651	487010.098671	49.569805
3504.202759	487013.470337	49.574810
3504.413885	486995.909269	49.579815
3504.562801	486977.395515	49.584820
3504.128652	486961.456149	49.589825
3504.393660	486940.441762	49.594829
3504.463086	486926.347782	49.599834
3504.253504	486932.713147	49.604839
3504.306544	486902.461774	49.609844
3504.012611	486901.697666	49.614849
3504.265258	486930.938149	49.619853
3504.334256	486909.296154	49.624858
3504.267102	486883.977597	49.629863
3504.280904	486906.872922	49.634868
3504.315328	486943.290690	49.639873
3504.410732	486915.058967	49.644877
3504.459837	486886.986494	49.649882
3504.056775	486881.325779	49.654887
3504.543954	486899.485725	49.659892
3504.092334	486892.363599	49.664897
3504.330939	486900.633807	49.669901
3504.311006	486884.476931	49.674906
3504.021000	486878.393079	49.679911
3504.296814	486862.442730	49.684916
3503.886379	486850.298900	49.689921
3504.419326	486849.556069	49.694925
3504.048172	486863.647070	49.699930
3503.850004	486854.610509	49.704935
3503.906089	486836.769850	49.709940
3503.508588	486837.187254	49.714945
3503.996628	486826.927733	49.719949
3504.301842	486823.181389	49.724954
3504.479227	486810.083428	49.729959
3504.397944	486812.477191	49.734964
3504.054526	486826.158567	49.739969
3504.732663	486853.862821	49.744973
3504.679766	486844.144735	49.749978
3504.112348	486823.312451	49.754983
3504.330259	486802.406674	49.759988
3504.355810	486820.740977	49.764993
3504.015208	486821.959923	49.769997
3503.971945	486831.693150	49.775002
3504.313464	486823.381807	49.780007
3504.380525	486797.737972	49.785012
3504.019888	486783.914496	49.790017
3504.079506	486753.155262	49.795021
3504.482033	486735.006457	49.800026
3504.015018	486761.929331	49.805031
3504.192979	486780.746169	49.810036
3504.089513	486762.525391	49.815041
3504.007613	486729.914118	49.820045
3504.212616	486728.564554	49.825050
3504.353164	486719.575709	49.830055
3504.321520	486747.645599	49.835060
3503.909416	486772.077504	49.840065
3503.640804	486724.754075	49.845069
3503.820174	486727.562578	49.850074
3504.196919	486713.166572	49.855079
3504.334969	486722.465927	49.860084
3504.073820	486761.565013	49.865089
3504.011673	486749.467385	49.870093
3503.617495	486728.455639	49.875098
3504.028879	486698.147304	49.880103
3504.484012	486727.660046	49.885108
3504.094052	486751.328597	49.890113
3504.005206	486743.743806	49.895117
3504.235445	486737.577679	49.900122
3504.068066	486743.683142	49.905127
3504.252524	486748.871796	49.910132
3503.812635	486756.134819	49.915137
3504.155449	486713.071362	49.920141
3504.296019	486696.483688	49.925146
3503.881840	486701.361704	49.930151
3504.139179	486695.748527	49.935156
3503.816468	486710.845159	49.940161
3503.730710	486700.473630	49.945165
3504.093691	486720.173142	49.950170
3503.708836	486722.868192	49.955175
3504.028267	486700.730448	49.960180
3504.217531	486678.461277	49.965185
3504.088830	486694.692410	49.970189
3503.998368	486722.974267	49.975194
3503.870128	486676.084459	49.980199
3504.184265	486689.712658	49.985204
3503.937647	486706.165055	49.990209
3503.719454	486696.574338	49.995213
3503.698158	486691.309153	50.000218
3504.061914	486725.598270	50.005223
3504.255996	486689.093243	50.010228
3504.334094	486663.751437	50.015233
3504.457042	486679.537536	50.020237
3503.771877	486699.656032	50.025242
3503.900583	486728.156534	50.030247
3504.308080	486724.545980	50.035252
3504.295858	486683.463605	50.040257
3504.029144	486706.403508	50.045261
3503.989855	486723.988271	50.050266
3503.992748	486700.988702	50.055271
3504.082657	486679.191165	50.060276
3504.066190	486691.199876	50.065281
3504.084179	486675.594077	50.070285
3504.402836	486627.519019	50.075290
3503.820635	486654.308273	50.080295
3503.921001	486667.109075	50.085300
3503.858932	486656.784437	50.090305
3504.134840	486643.214860	50.095309
3503.698998	486655.695152	50.100314
3503.520174	486658.965552	50.105319
3503.864917	486687.381309	50.110324
3503.964366	486682.654284	50.115329
3504.355730	486626.563634	50.120333
3503.836306	486666.058350	50.125338
3503.914390	486681.091656	50.130343
3504.353457	486669.370686	50.135348
3504.250240	486645.729257	50.140353
3503.949361	486669.991736	50.145357
3504.165632	486645.894538	50.150362
3503.739948	486675.141312	50.155367
3504.123605	486689.366430	50.160372
3504.253866	486703.530271	50.165377
3503.848391	486656.126987	50.170381
3504.346191	486650.627766	50.175386
3503.804462	486677.258615	50.180391
3504.197126	486685.403249	50.185396
3504.283923	486656.969870	50.190401
3504.203335	486655.158852	50.195405
3504.199495	486664.430003	50.200410
3504.223368	486658.195151	50.205415
3504.465399	486661.905620	50.210420
3504.303614	486655.750771	50.215425
3504.237068	486615.639357	50.220429
3504.438586	486610.744204	50.225434
3503.776380	486642.105433	50.230439
3504.185659	486661.645710	50.235444
3504.019865	486613.647189	50.240449
3503.835340	486583.939452	50.245453
3504.248477	486610.875399	50.250458
3503.923057	486624.402097	50.255463
3504.412795	486602.743912	50.260468
3504.319244	486592.829488	50.265473
3503.911112	486608.091679	50.270477
3504.227610	486623.188665	50.275482
3503.774417	486631.061746	50.280487
3504.408564	486613.180170	50.285492
3504.254874	486617.459785	50.290497
3504.175937	486626.388211	50.295501
3504.363888	486626.915718	50.300506
3504.083030	486606.341858	50.305511
3503.906112	486547.453232	50.310516
3504.314789	486532.596112	50.315521
3504.585087	486530.678962	50.320525
3504.590188	486539.644805	50.325530
3504.262174	486557.731289	50.330535
3504.194944	486547.660704	50.335540
3503.878110	486550.699640	50.340545
3503.865072	486551.208258	50.345549
3504.117058	486560.641661	50.350554
3503.825473	486548.124238	50.355559
3504.080943	486538.407915	50.360564
3503.976625	486550.481260	50.365569
3504.203706	486548.469625	50.370573
3504.416357	486550.664983	50.375578
3504.031441	486550.928425	50.380583
3503.916799	486546.488502	50.385588
3503.918834	486550.642200	50.390593
3503.885351	486551.863278	50.395597
3504.140923	486535.054651	50.400602
3503.916107	486553.783397	50.405607
3504.118291	486554.815248	50.410612
3503.905316	486560.016112	50.415617
3504.166405	486553.135822	50.420621
3504.291813	486540.603143	50.425626
3504.140275	486508.205137	50.430631
3503.987078	486526.871930	50.435636
3504.200339	486525.622365	50.440641
3503.489452	486534.904016	50.445645
3503.952042	486534.830865	50.450650
3504.146882	486541.942984	50.455655
3504.470985	486540.473264	50.460660
3504.004614	486545.612865	50.465665
3504.246761	486525.817458	50.470669
3504.517837	486472.278332	50.475674
3503.834115	486464.990093	50.480679
3504.187271	486456.068840	50.485684
3504.142042	486525.529917	50.490689
3504.073729	486533.494181	50.495693
3504.062076	486497.223944	50.500698
3504.072685	486507.303436	50.505703
3504.098453	486507.653944	50.510708
3504.267548	486500.180264	50.515713
3504.277784	486512.083548	50.520717
3504.250408	486461.175187	50.525722
3504.045070	486462.372775	50.530727
3504.084616	486488.506734	50.535732
3503.992973	486451.742460	50.540737
3503.934899	486400.686812	50.545741
3504.193834	486342.843178	50.550746
3503.837616	486332.412879	50.555751
3503.576959	486268.622635	50.560756
3503.400623	486210.746082	50.565761
3503.212330	486124.957432	50.570765
3503.425740	486018.182093	50.575770
3503.027855	485937.846418	50.580775
3503.027963	485835.207301	50.585780
3502.908554	485722.606239	50.590785
3502.563672	485580.251073	50.595789
3502.645999	485433.115751	50.600794
3502.087550	485319.264509	50.605799
3501.990433	485143.885683	50.610804
3501.933770	484974.679798	50.615809
3501.827704	484803.403023	50.620813
3501.711617	484637.851372	50.625818
3500.724149	484493.715179	50.630823
3500.651025	484319.186374	50.635828
3500.329711	484104.568100	50.640833
3500.161393	483893.317900	50.645837
3499.725805	483728.264973	50.650842
3499.142977	483489.969255	50.655847
3499.050723	483274.444257	50.660852
3498.624657	483101.277656	50.665857
3498.004177	482877.167486	50.670861
3498.016213	482620.272975	50.675866
3497.653867	482395.964469	50.680871
3497.363891	482148.384113	50.685876
3496.485103	481891.975536	50.690881
3496.089069	481642.429365	50.695885
3496.014647	481372.154732	50.700890
3495.618457	481100.153675	50.705895
3495.335645	480829.752508	50.710900
3494.869954	480577.315408	50.715905
3493.626124	480334.981126	50.720909
3493.238815	480050.802094	50.725914
3492.443654	479775.551890	50.730919
3492.377075	479507.277547	50.735924
3492.117396	479225.803091	50.740929
3491.463984	478953.306373	50.745933
3491.037241	478676.563685	50.750938
3490.729757	478378.005755	50.755943
3490.655596	478065.114394	50.760948
3490.000693	477755.806986	50.765953
3488.861519	477439.475761	50.770957
3488.412878	477117.759300	50.775962
3488.019617	476802.922005	50.780967
3488.124531	476480.347577	50.785972
3487.248816	476186.003003	50.790977
3486.287999	475868.047595	50.795981
3486.395804	475505.161153	50.800986
3485.729045	475184.867580	50.805991
3485.413931	474890.973115	50.810996
3484.334635	474538.851054	50.816001
3483.291182	474208.717070	50.821005
3483.083144	473880.574732	50.826010
3482.506353	473551.978485	50.831015
3481.557374	473196.619020	50.836020
3481.047507	472854.263087	50.841025
3481.007905	472499.761682	50.846029
3480.418506	472138.598512	50.851034
3479.596189	471837.845694	50.856039
3478.783108	471506.719238	50.861044
3478.311514	471158.093262	50.866049
3477.717004	470797.769322	50.871053
3476.428943	470437.447353	50.876058
3476.363100	470083.010054	50.881063
3475.464998	469729.458811	50.886068
3474.775528	469391.383620	50.891073
3473.921306	469046.382622	50.896077
3473.974591	468699.305718	50.901082
3473.037451	468373.422279	50.906087
3472.878170	468010.547581	50.911092
3471.860813	467656.828095	50.916097
3471.157370	467298.996435	50.921101
3470.872928	466934.145403	50.926106
3470.024634	466578.961305	50.931111
3469.256368	466201.496774	50.936116
3468.542298	465842.780127	50.941121
3467.823217	465491.665037	50.946125
3467.519653	465131.857294	50.951130
3466.366630	464789.014735	50.956135
3465.768171	464401.399481	50.961140
3465.197520	464034.059037	50.966145
3464.058533	463681.966347	50.971149
3463.411029	463320.153946	50.976154
3462.788903	462960.867371	50.981159
3461.891855	462613.486496	50.986164
3461.919760	462241.861992	50.991169
3461.115517	461874.268160	50.996173
3460.647119	461541.764937	51.001178
3459.394238	461219.880128	51.006183
3458.943656	460846.532182	51.011188
3458.444196	460476.026127	51.016193
3457.824140	460102.945918	51.021197
3457.178202	459767.197421	51.026202
3456.241725	459431.743363	51.031207
3455.615034	459068.741187	51.036212
3454.860272	458688.657993	51.041217
3453.835901	458320.024869	51.046221
3453.374183	457959.819245	51.051226
3452.554700	457614.173235	51.056231
3452.001975	457250.064273	51.061236
3452.190318	456870.460412	51.066241
3450.958483	456518.115253	51.071245
3449.829975	456207.755645	51.076250
3449.332438	455833.163801	51.081255
3448.678310	455459.503712	51.086260
3448.097442	455117.282201	51.091265
3447.221039	454777.283909	51.096269
3446.362631	454390.497605	51.101274
3446.236358	454015.563249	51.106279
3445.208811	453713.017866	51.111284
3444.551746	453338.815882	51.116289
3443.818282	452961.270946	51.121293
3442.806656	452620.145497	51.126298
3441.917613	452284.881700	51.131303
3441.965333	451905.978068	51.136308
3440.955305	451607.207815	51.141313
3440.092490	451253.657063	51.146317
3439.423684	450873.987092	51.151322
3438.183143	450546.416138	51.156327
3437.910452	450187.934929	51.161332
3437.635468	449825.997712	51.166337
3436.745082	449530.023628	51.171341
3435.904227	449164.054976	51.176346
3435.696126	448791.535318	51.181351
3434.721103	448449.276922	51.186356
3434.022478	448147.621711	51.191361
3433.223865	447771.880395	51.196365
3432.832400	447435.859019	51.201370
3431.536968	447102.107427	51.206375
3430.807095	446749.533365	51.211380
3430.869732	446385.865663	51.216385
3430.209244	446023.321841	51.221389
3429.433163	445673.987510	51.226394
3428.625567	445331.454538	51.231399
3427.571130	445006.924048	51.236404
3426.576977	444686.846401	51.241409
3426.303789	444362.589751	51.246413
3425.623997	444020.525449	51.251418
3424.895022	443696.281127	51.256423
3423.913694	443327.199132	51.261428
3423.888105	442985.067505	51.266433
3422.541300	442671.364168	51.271437
3422.242093	442304.646159	51.276442
3421.462036	441952.618827	51.281447
3420.902951	441630.604466	51.286452
3420.117035	441332.837009	51.291457
3419.146131	440998.441828	51.296461
3418.649017	440631.070056	51.301466
3417.865917	440295.671047	51.306471
3417.621774	439945.103991	51.311476
3416.772799	439613.133008	51.316481
3415.763914	439324.997313	51.321485
3415.001796	438985.566402	51.326490
3414.176311	438631.899527	51.331495
3413.858014	438290.383502	51.336500
3413.063000	437996.410603	51.341505
3411.829119	437642.870447	51.346509
3411.994012	437288.748735	51.351514
3411.003057	436956.510974	51.356519
3410.206441	436663.741313	51.361524
3409.606042	436334.505509	51.366529
3408.749359	435997.943328	51.371533
3408.233122	435662.795391	51.376538
3407.424843	435336.702292	51.381543
3406.563167	435036.713643	51.386548
3405.835335	434709.711172	51.391553
3405.428377	434374.071985	51.396557
3404.851509	434076.642194	51.401562
3403.537417	433725.726067	51.406567
3403.284538	433426.282443	51.411572
3402.424780	433082.496714	51.416577
3401.979202	432802.881454	51.421581
3401.447221	432470.233395	51.426586
3400.205447	432134.544666	51.431591
3399.987974	431807.932502	51.436596
3399.201128	431503.650325	51.441601
3398.873370	431158.307597	51.446605
3398.112672	430856.629233	51.451610
3397.270803	430505.340940	51.456615
3396.315667	430218.592086	51.461620
3395.717357	429868.069371	51.466625
3394.805303	429587.249101	51.471629
3394.626316	429236.372355	51.476634
3393.728658	428924.306967	51.481639
3393.171437	428645.731570	51.486644
3392.084924	428286.605231	51.491649
3391.480009	427977.631526	51.496653
3390.993476	427682.679755	51.501658
3390.229512	427348.251292	51.506663
3389.859136	427022.823174	51.511668
3388.846019	426736.477658	51.516673
3388.674263	426372.787273	51.521677
3387.533257	426095.674518	51.526682
3386.604477	425789.292037	51.531687
3386.237101	425433.518789	51.536692
3385.538259	425154.802582	51.541697
3384.491762	424826.508666	51.546701
3384.069142	424505.325585	51.551706
3383.366581	424223.450916	51.556711
3382.744823	423877.730457	51.561716
3381.923758	423576.386068	51.566721
3381.340941	423297.022973	51.571725
3380.842493	422943.371703	51.576730
3379.936609	422678.608113	51.581735
3379.497752	422332.305920	51.586740
3378.540631	422043.158986	51.591745
3377.827757	421713.987733	51.596749
3377.667328	421395.546607	51.601754
3376.502013	421128.370646	51.606759
3376.115893	420780.923114	51.611764
3375.142510	420481.194988	51.616769
3374.147541	420192.771574	51.621773
3373.998183	419836.790205	51.626778
3373.289878	419575.700304	51.631783
3372.396938	419265.607131	51.636788
3371.620999	418920.586297	51.641793
3370.856231	418656.270478	51.646797
3370.075354	418344.574432	51.651802
3369.599579	418012.096007	51.656807
3368.866554	417733.717476	51.661812
3368.223304	417444.651603	51.666817
3367.535619	417119.005077	51.671821
3367.347602	416833.595772	51.676826
3366.414713	416514.840901	51.681831
3365.827171	416217.598371	51.686836
3365.197887	415916.853201	51.691841
3364.350643	415597.464916	51.696845
3363.534434	415325.529797	51.701850
3362.854407	415007.226533	51.706855
3362.323307	414679.291937	51.711860
3361.665338	414370.404709	51.716865
3360.479850	414108.248117	51.721869
3360.254977	413767.880857	51.726874
3359.183003	413508.826286	51.731879
3358.573880	413182.640575	51.736884
3358.342720	412905.966003	51.741889
3357.573490	412586.227714	51.746893
3356.578826	412307.686316	51.751898
3356.141164	411978.665137	51.756903
3354.876765	411710.223392	51.761908
3354.487995	411404.743956	51.766913
3353.610514	411114.941227	51.771917
3353.330824	410811.700115	51.776922
3352.656566	410520.665184	51.781927
3351.367951	410225.379137	51.786932
3351.201015	409947.777670	51.791937
3350.584877	409632.303798	51.796941
3349.764382	409360.111526	51.801946
3349.138990	409029.080246	51.806951
3348.533577	408773.570503	51.811956
3347.810127	408479.042183	51.816961
3347.000389	408177.993346	51.821965
3346.921235	407878.859149	51.826970
3346.079381	407590.592879	51.831975
3345.186309	407303.119865	51.836980
3344.510792	406991.414968	51.841985
3343.700246	406701.076866	51.846989
3343.289090	406411.969069	51.851994
3342.542130	406113.457149	51.856999
3342.070167	405819.524543	51.862004
3341.067541	405534.390751	51.867009
3340.503376	405240.391044	51.872013
3340.013186	404941.979854	51.877018
3339.113440	404648.332681	51.882023
3338.242293	404363.624988	51.887028
3337.920242	404073.032806	51.892033
3337.163192	403781.057965	51.897037
3336.237674	403471.721471	51.902042
3335.614586	403202.824703	51.907047
3335.092146	402916.803439	51.912052
3334.683638	402596.675729	51.917057
3333.816778	402326.310473	51.922061
3333.322610	402024.542745	51.927066
3332.774181	401729.440539	51.932071
3331.784427	401438.167468	51.937076
3331.299464	401134.432698	51.942081
3330.074162	400868.280710	51.947085
3329.697310	400564.447259	51.952090
3328.782299	400275.185535	51.957095
3328.064503	399972.951124	51.962100
3327.394804	399705.507040	51.967105
3326.618817	399418.427355	51.972109
3325.887057	399127.931762	51.977114
3325.498086	398839.972365	51.982119
3324.823194	398580.425966	51.987124
3324.348018	398267.587673	51.992129
3323.455899	397998.487120	51.997133
3322.885215	397708.868808	52.002138
3322.125897	397408.549613	52.007143
3321.515482	397148.295458	52.012148
3321.220581	396848.152022	52.017153
3320.298728	396558.045425	52.022157
3319.318093	396268.250705	52.027162
3319.032002	395988.767239	52.032167
3318.275947	395694.254189	52.037172
3317.574465	395420.933395	52.042177
3317.071743	395126.604178	52.047181
3316.309172	394827.508338	52.052186
3315.210353	394555.057022	52.057191
3314.789848	394272.148440	52.062196
3314.328789	393979.557077	52.067201
3313.000941	393708.559061	52.072205
3312.749205	393416.717997	52.077210
3312.142600	393126.862932	52.082215
3311.507201	392854.833406	52.087220
3311.130854	392563.589667	52.092225
3310.322632	392281.488916	52.097229
3309.614740	391990.903061	52.102234
3308.834404	391703.707981	52.107239
3308.273656	391413.653459	52.112244
3307.743870	391122.015183	52.117249
3306.731228	390853.208151	52.122253
3306.122949	390568.468474	52.127258
3305.639365	390269.162238	52.132263
3304.529366	389999.347033	52.137268
3304.194130	389713.845358	52.142273
3303.568501	389435.278357	52.147277
3302.486426	389148.364598	52.152282
3301.956817	388854.622609	52.157287
3301.308462	388592.886370	52.162292
3300.855565	388308.180428	52.167297
3299.994150	388026.868073	52.172301
3299.513251	387738.652867	52.177306
3298.858346	387457.913752	52.182311
3297.862386	387172.776214	52.187316
3297.322349	386886.063980	52.192321
3296.745582	386610.951451	52.197325
3295.881260	386320.878456	52.202330
3295.045106	386042.267886	52.207335
3294.286434	385770.890710	52.212340
3293.908079	385482.183823	52.217345
3293.279947	385213.808202	52.222349
3292.558980	384942.597029	52.227354
3291.669741	384645.648433	52.232359
3290.836579	384385.844259	52.237364
3290.555102	384098.281206	52.242369
3289.527483	383828.509220	52.247373
3289.343194	383547.894967	52.252378
3288.655834	383278.675612	52.257383
3287.729644	383000.005770	52.262388
3287.491641	382717.079500	52.267393
3286.284130	382443.002537	52.272397
3285.737101	382155.034387	52.277402
3285.033636	381883.823942	52.282407
3284.378599	381619.801602	52.287412
3283.925613	381337.255215	52.292417
3283.007828	381049.693501	52.297421
3282.385940	380785.812819	52.302426
3281.572396	380511.507193	52.307431
3280.768558	380247.677069	52.312436
3280.390517	379968.033819	52.317441
3279.875106	379699.550718	52.322445
3278.786933	379415.335844	52.327450
3278.505301	379146.328724	52.332455
3277.686249	378879.159803	52.337460
3277.132438	378609.098356	52.342465
3276.305417	378333.253522	52.347469
3275.870996	378044.041751	52.352474
3275.118194	377782.247363	52.357479
3274.569868	377507.675407	52.362484
3273.830390	377223.822108	52.367489
3272.957756	376953.570960	52.372493
3272.516113	376679.103653	52.377498
3271.908477	376406.950053	52.382503
3271.016328	376129.167170	52.387508
3270.613624	375857.384463	52.392513
3269.584542	375581.323790	52.397517
3269.301758	375301.531080	52.402522
3268.607541	375031.595054	52.407527
3267.600283	374743.264306	52.412532
3267.192072	374494.952593	52.417537
3266.749155	374201.695572	52.422541
3265.813746	373931.637869	52.427546
3265.269199	373657.090280	52.432551
3264.523256	373386.286790	52.437556
3263.714366	373102.008892	52.442561
3263.090634	372842.375660	52.447565
3262.707121	372551.641551	52.452570
3261.792791	372283.681332	52.457575
3261.178732	372016.333348	52.462580
3260.368698	371719.987963	52.467585
3260.005127	371456.947027	52.472589
3259.032836	371190.642667	52.477594
3258.633089	370901.884149	52.482599
3257.980715	370620.261511	52.487604
3257.238077	370366.559571	52.492609
3256.590319	370079.844564	52.497613
3255.822223	369796.148712	52.502618
3255.455331	369511.115494	52.507623
3254.634830	369251.466139	52.512628
3254.317308	368977.208679	52.517633
3253.515627	368689.058698	52.522637
3252.423812	368391.284881	52.527642
3251.775110	368138.140268	52.532647
3251.256524	367858.361315	52.537652
3250.408697	367583.543007	52.542657
3249.766499	367326.856272	52.547661
3249.252943	367035.698639	52.552666
3248.542949	366760.319162	52.557671
3247.782639	366502.043489	52.562676
3247.047630	366207.328077	52.567681
3246.071500	365945.139695	52.572685
3245.507825	365667.669504	52.577690
3244.941147	365401.673056	52.582695
3244.341543	365134.611635	52.587700
3244.121738	364862.094516	52.592705
3243.110763	364594.866020	52.597709
3242.415563	364321.046918	52.602714
3241.952652	364040.039646	52.607719
3240.882899	363777.599203	52.612724
3240.247875	363504.478185	52.617729
3239.628825	363244.278879	52.622733
3239.181348	362956.265352	52.627738
3238.449771	362694.197873	52.632743
3237.779569	362432.882573	52.637748
3237.207527	362145.519902	52.642753
3236.180009	361877.667749	52.647757
3235.741705	361605.980398	52.652762
3235.300942	361339.279220	52.657767
3234.338266	361070.089090	52.662772
3233.914359	360784.781313	52.667777
3233.041351	360509.339606	52.672781
3232.224274	360242.895423	52.677786
3231.751827	359980.822914	52.682791
3230.892306	359696.926265	52.687796
3230.457477	359425.047918	52.692801
3229.661894	359177.653991	52.697805
3229.090322	358907.270304	52.702810
3228.602487	358620.102298	52.707815
3227.871441	358348.544756	52.712820
3226.984350	358081.311000	52.717825
3226.699271	357818.459322	52.722829
3225.810111	357543.054371	52.727834
3225.067922	357265.766968	52.732839
3224.403002	356997.219869	52.737844
3223.702370	356721.144379	52.742849
3222.962067	356454.234980	52.747853
3222.480572	356184.560268	52.752858
3222.049521	355914.570763	52.757863
3221.049858	355631.792818	52.762868
3220.465164	355366.278211	52.767873
3220.038119	355095.265799	52.772877
3219.470883	354817.148434	52.777882
3218.623151	354548.261059	52.782887
3217.620067	354275.121398	52.787892
3217.323790	354001.613998	52.792897
3216.383412	353728.461551	52.797901
3215.722451	353462.185770	52.802906
3215.252912	353188.294339	52.807911
3214.287792	352915.548776	52.812916
3213.889544	352647.496732	52.817921
3213.003519	352385.755778	52.822925
3212.365629	352107.202571	52.827930
3211.874009	351837.863264	52.832935
3211.106983	351574.470690	52.837940
3211.029993	351305.241278	52.842945
3209.993697	351039.140020	52.847949
3209.336971	350747.017506	52.852954
3209.126896	350475.030881	52.857959
3207.830634	350203.469244	52.862964
3207.154735	349934.760471	52.867969
3206.532772	349653.519767	52.872973
3205.897056	349384.318379	52.877978
3205.358461	349111.995221	52.882983
3204.186060	348835.851423	52.887988
3204.067028	348549.842447	52.892993
3203.057666	348293.980800	52.897997
3202.465991	348023.493291	52.903002
3201.860226	347746.058247	52.908007
3200.692351	347485.127562	52.913012
3200.452801	347222.623482	52.918017
3199.572748	346957.674261	52.923021
3199.332941	346681.728759	52.928026
3198.537747	346423.432268	52.933031
3197.661457	346155.322607	52.938036
3197.398298	345885.842055	52.943041
3196.486487	345615.597465	52.948045
3195.806092	345350.049333	52.953050
3195.446474	345078.314975	52.958055
3194.762237	344799.732804	52.963060
3193.953780	344525.114294	52.968065
3193.136051	344254.492227	52.973069
3192.340405	343982.490927	52.978074
3191.749135	343708.979726	52.983079
3191.076097	343435.480217	52.988084
3190.692003	343167.533693	52.993089
3189.802389	342908.396807	52.998093
3188.950474	342651.263756	53.003098
3188.853713	342363.642836	53.008103
3187.898800	342098.454652	53.013108
3187.296573	341822.722148	53.018113
3186.420980	341560.624591	53.023117
3185.615925	341289.758238	53.028122
3185.502505	341025.501446	53.033127
3184.587919	340756.482880	53.038132
3183.888281	340482.490816	53.043137
3183.260620	340217.039214	53.048141
3182.345106	339946.311826	53.053146
3181.685967	339667.575097	53.058151
3181.240823	339409.193387	53.063156
3180.689809	339136.419351	53.068161
3180.108275	338869.020207	53.073165
3179.522535	338590.394479	53.078170
3179.001709	338318.426818	53.083175
3177.725997	338054.647107	53.088180
3177.497976	337771.022765	53.093185
3176.644526	337506.944944	53.098189
3175.757518	337244.678799	53.103194
3175.099347	336959.515265	53.108199
3174.586134	336687.997907	53.113204
3173.741155	336426.842001	53.118209
3173.058536	336159.880647	53.123213
3172.308109	335896.951196	53.128218
3172.386236	335621.059192	53.133223
3171.277551	335358.973520	53.138228
3170.981378	335079.930927	53.143233
3170.398339	334810.504628	53.148237
3169.593888	334537.039088	53.153242
3169.057322	334259.456849	53.158247
3168.249881	333983.622040	53.163252
3167.694019	333708.255503	53.168257
3166.925179	333431.164981	53.173261
3166.186189	333164.811990	53.178266
3165.480039	332882.032243	53.183271
3164.649292	332608.232427	53.188276
3164.039209	332332.690942	53.193281
3163.038623	332061.614515	53.198285
3162.384744	331788.318238	53.203290
3161.738367	331528.181910	53.208295
3160.896544	331261.150784	53.213300
3160.455063	330998.637953	53.218305
3159.884117	330741.796570	53.223309
3159.348564	330474.714150	53.228314
3158.750768	330191.295833	53.233319
3157.762037	329924.970551	53.238324
3157.456679	329638.550610	53.243329
3156.979777	329386.985263	53.248333
3156.267125	329123.592242	53.253338
3155.497396	328839.814186	53.258343
3154.717089	328559.499280	53.263348
3153.950209	328298.454312	53.268353
3153.517874	328029.055611	53.273357
3152.766710	327749.242374	53.278362
3151.967465	327480.052600	53.283367
3151.152959	327220.793785	53.288372
3150.322761	326946.973349	53.293377
3150.012339	326685.876281	53.298381
3149.069044	326423.758239	53.303386
3148.519643	326150.094341	53.308391
3147.447273	325887.434854	53.313396
3147.274824	325626.007009	53.318401
3146.514748	325362.914515	53.323405
3145.971296	325094.720204	53.328410
3145.404004	324813.620116	53.333415
3144.524919	324553.599193	53.338420
3143.669166	324282.752817	53.343425
3143.161762	324030.997238	53.348429
3142.580235	323755.777389	53.353434
3142.003747	323489.900155	53.358439
3141.052573	323231.032338	53.363444
3140.700552	322956.333758	53.368449
3139.859585	322692.049058	53.373453
3139.058033	322430.914561	53.378458
3138.844663	322158.610382	53.383463
3138.146767	321896.948664	53.388468
3137.287448	321637.246815	53.393473
3136.807407	321362.945439	53.398477
3135.958158	321091.145994	53.403482
3135.268307	320826.755437	53.408487
3134.677102	320558.732876	53.413492
3134.233236	320278.668043	53.418497
3133.302616	320016.426601	53.423501
3132.357898	319754.186646	53.428506
3132.084207	319482.800606	53.433511
3131.096623	319230.216228	53.438516
3130.531592	318965.316806	53.443521
3129.876824	318689.940226	53.448525
3129.093607	318435.717244	53.453530
3128.873856	318171.244773	53.458535
3127.654489	317903.466796	53.463540
3127.040413	317632.460363	53.468545
3126.560398	317362.603264	53.473549
3125.705304	317120.534066	53.478554
3125.357543	316840.112897	53.483559
3124.738649	316575.801130	53.488564
3124.020493	316325.509176	53.493569
3123.595547	316050.801786	53.498573
3122.836305	315779.813281	53.503578
3122.308040	315516.477481	53.508583
3121.298967	315246.316466	53.513588
3120.733696	314980.617045	53.518593
3120.224056	314702.278161	53.523597
3119.373041	314445.942303	53.528602
3118.805747	314163.842486	53.533607
3118.185910	313901.026389	53.538612
3117.619971	313638.252047	53.543617
3116.362170	313367.947344	53.548621
3115.810484	313094.907439	53.553626
3115.398644	312829.942315	53.558631
3114.740814	312567.536435	53.563636
3114.283280	312293.257367	53.568641
3113.948977	312031.486567	53.573645
3112.954151	311770.660003	53.578650
3112.473824	311475.629098	53.583655
3111.351053	311224.548942	53.588660
3110.891196	310948.790059	53.593665
3110.402690	310682.507887	53.598669
3109.404398	310404.362853	53.603674
3108.745847	310130.543335	53.608679
3107.782517	309879.256814	53.613684
3107.291264	309606.479143	53.618689
3106.774294	309339.994753	53.623693
3106.310905	309082.821472	53.628698
3105.462687	308813.001514	53.633703
3104.895784	308539.240300	53.638708
3104.155961	308268.587127	53.643713
3103.562755	308010.184379	53.648717
3102.918471	307743.716715	53.653722
3102.388904	307467.451681	53.658727
3101.420564	307208.138996	53.663732
3100.833161	306925.260975	53.668737
3100.205192	306662.379124	53.673741
3099.356767	306392.324908	53.678746
3099.101216	306127.575020	53.683751
3098.066883	305863.991937	53.688756
3097.541374	305599.843979	53.693761
3097.287568	305329.948205	53.698765
3096.203970	305058.095025	53.703770
3095.609829	304781.707352	53.708775
3094.609656	304529.881512	53.713780
3094.264722	304251.670762	53.718785
3093.841578	303980.118454	53.723789
3092.986811	303713.472475	53.728794
3092.294130	303437.505265	53.733799
3091.729231	303176.542295	53.738804
3090.849788	302899.559534	53.743809
3090.238335	302634.375615	53.748813
3089.304806	302357.680550	53.753818
3088.928203	302099.843737	53.758823
3088.027862	301840.739665	53.763828
3087.278336	301574.302464	53.768833
3087.031039	301306.537486	53.773837
3086.251439	301048.609932	53.778842
3085.413788	300765.555769	53.783847
3084.674451	300508.843378	53.788852
3084.177709	300242.695048	53.793857
3083.288457	299970.623766	53.798861
3082.895424	299713.218687	53.803866
3082.150334	299437.609346	53.808871
3081.305038	299177.499171	53.813876
3080.834997	298904.850529	53.818881
3080.279268	298643.293070	53.823885
3079.456495	298381.752022	53.828890
3079.015057	298115.413418	53.833895
3078.416488	297860.355652	53.838900
3078.006191	297584.537674	53.843905
3076.978290	297312.789873	53.848909
3076.211304	297050.321309	53.853914
3075.669093	296769.582429	53.858919
3075.071470	296507.468333	53.863924
3074.161088	296231.727557	53.868929
3073.597900	295974.624327	53.873933
3073.049099	295702.008994	53.878938
3072.580766	295435.008814	53.883943
3071.723228	295158.392341	53.888948
3071.106037	294902.722489	53.893953
3070.557398	294630.513214	53.898957
3069.697318	294358.403820	53.903962
3069.240076	294079.023078	53.908967
3068.421703	293820.378652	53.913972
3067.476772	293555.616315	53.918977
3066.836238	293281.331612	53.923981
3066.205318	293017.614067	53.928986
3065.585756	292758.682320	53.933991
3065.039904	292484.814661	53.938996
3064.154512	292214.693227	53.944001
3063.464335	291956.612238	53.949005
3062.894800	291691.635639	53.954010
3062.661372	291423.091043	53.959015
3061.894539	291147.372305	53.964020
3061.284890	290890.423556	53.969025
3060.788318	290607.887090	53.974029
3059.960639	290337.066958	53.979034
3059.140173	290061.610292	53.984039
3058.359944	289794.296684	53.989044
3057.585967	289525.682984	53.994049
3057.377599	289259.398971	53.999053
3055.931286	289000.696322	54.004058
3055.887620	288731.100431	54.009063
3054.540616	288461.404967	54.014068
3054.392100	288207.462514	54.019073
3054.127312	287938.741399	54.024077
3053.191294	287670.100833	54.029082
3052.616298	287394.653908	54.034087
3051.639254	287123.498085	54.039092
3051.084918	286858.845905	54.044097
3050.727050	286577.913839	54.049101
3049.713086	286328.181889	54.054106
3049.056545	286040.649539	54.059111
3048.611715	285788.484110	54.064116
3047.806960	285521.400249	54.069121
3047.493563	285244.713379	54.074125
3046.598962	284969.315319	54.079130
3046.024702	284703.493349	54.084135
3045.399511	284427.542958	54.089140
3044.485643	284163.149709	54.094145
3043.830530	283883.561794	54.099149
3042.939512	283617.229057	54.104154
3042.573209	283352.901532	54.109159
3042.050763	283085.236785	54.114164
3041.012390	282819.232597	54.119169
3040.471339	282541.459650	54.124173
3040.003736	282291.206141	54.129178
3039.291307	282006.812862	54.134183
3038.352836	281742.727988	54.139188
3037.934962	281468.016746	54.144193
3037.620666	281190.869517	54.149197
3036.584418	280927.996831	54.154202
3036.236337	280652.433793	54.159207
3035.560240	280382.118118	54.164212
3034.674954	280100.935024	54.169217
3034.115362	279820.540754	54.174221
3033.486165	279563.970329	54.179226
3032.871928	279292.905982	54.184231
3032.051691	279012.425416	54.189236
3031.145752	278743.113496	54.194241
3030.646670	278484.739465	54.199245
3029.660328	278207.901535	54.204250
3029.306921	277939.826378	54.209255
3028.824953	277671.236695	54.214260
3027.901063	277404.677991	54.219265
3027.588624	277132.317562	54.224269
3026.556254	276866.234407	54.229274
3025.938081	276591.782981	54.234279
3025.263580	276331.093388	54.239284
3024.528006	276051.796058	54.244289
3024.186761	275783.540529	54.249293
3023.077676	275517.571345	54.254298
3022.620795	275239.910820	54.259303
3021.824781	274978.119852	54.264308
3020.941807	274722.506012	54.269313
3020.460458	274449.280903	54.274317
3019.636333	274188.665986	54.279322
3019.208414	273918.641489	54.284327
3018.562186	273655.375232	54.289332
3017.953310	273376.338175	54.294337
3017.490588	273111.336571	54.299341
3016.681062	272850.617655	54.304346
3016.143425	272576.688611	54.309351
3015.351854	272302.596072	54.314356
3014.426924	272047.218473	54.319361
3014.011909	271777.778105	54.324365
3013.177737	271506.723244	54.329370
3012.492946	271235.390132	54.334375
3011.917212	270985.942595	54.339380
3011.178847	270716.681059	54.344385
3010.938311	270447.875649	54.349389
3010.036606	270171.814649	54.354394
3009.256269	269898.357778	54.359399
3008.765011	269622.664986	54.364404
3008.124412	269355.375006	54.369409
3007.238004	269080.661848	54.374413
3006.438408	268818.210766	54.379418
3006.130749	268547.532102	54.384423
3005.308735	268277.622625	54.389428
3004.624424	268014.440560	54.394433
3004.101064	267733.430886	54.399437
3003.503187	267471.152271	54.404442
3003.033012	267199.353959	54.409447
3002.628079	266926.654091	54.414452
3001.774737	266645.238856	54.419457
3000.604452	266369.400548	54.424461
3000.060835	266107.190527	54.429466
2999.333339	265828.506458	54.434471
2998.609629	265564.185968	54.439476
2997.783830	265294.457118	54.444481
2997.509148	265032.256161	54.449485
2996.710366	264765.554102	54.454490
2996.434740	264494.745481	54.459495
2996.020190	264220.342602	54.464500
2995.245390	263949.969961	54.469505
2994.700354	263663.592768	54.474509
2993.651035	263387.915761	54.479514
2993.408370	263117.408620	54.484519
2992.700361	262841.296032	54.489524
2991.738581	262569.247775	54.494529
2991.279047	262284.564619	54.499533
2990.510232	262014.600141	54.504538
2989.727072	261728.084125	54.509543
2989.367335	261455.432227	54.514548
2988.283889	261183.837453	54.519553
2987.684557	260905.086291	54.524557
2986.859463	260628.153886	54.529562
2986.469848	260356.220894	54.534567
2985.693497	260078.899329	54.539572
2985.090888	259813.927808	54.544577
2984.248438	259530.683347	54.549581
2983.655127	259268.588760	54.554586
2983.007771	258988.573877	54.559591
2982.616160	258712.160684	54.564596
2981.709847	258440.337024	54.569601
2981.320504	258163.007283	54.574605
2980.292297	257886.313819	54.579610
2979.983307	257616.561301	54.584615
2979.025681	257338.405695	54.589620
2978.576204	257071.859490	54.594625
2977.978317	256783.486188	54.599629
2977.314839	256517.916830	54.604634
2976.729385	256238.965173	54.609639
2976.008613	255963.549777	54.614644
2975.580952	255680.295409	54.619649
2974.866078	255395.329672	54.624653
2973.842595	255127.272387	54.629658
2973.338886	254835.601654	54.634663
2972.678724	254564.431581	54.639668
2971.684263	254287.584747	54.644673
2971.145627	254010.564291	54.649677
2970.629643	253730.611967	54.654682
2969.653547	253457.354281	54.659687
2968.919824	253186.579849	54.664692
2968.213421	252918.984843	54.669697
2967.571487	252639.079605	54.674701
2966.648067	252371.417912	54.679706
2966.067003	252106.631098	54.684711
2965.870229	251838.294931	54.689716
2964.767667	251565.289396	54.694721
2964.618990	251293.126493	54.699725
2963.655187	251022.671994	54.704730
2963.169102	250750.206865	54.709735
2962.524138	250473.692719	54.714740
2962.218969	250208.304983	54.719745
2961.450428	249918.823517	54.724749
2960.394044	249653.122704	54.729754
2960.026712	249369.588774	54.734759
2959.394683	249094.220975	54.739764
2958.388473	248832.868345	54.744769
2957.905786	248549.023137	54.749773
2957.051216	248280.109501	54.754778
2956.900602	247990.202802	54.759783
2956.308174	247720.764831	54.764788
2955.179668	247442.040778	54.769793
2954.913173	247160.150366	54.774797
2953.550732	246893.229632	54.779802
2953.266935	246619.364757	54.784807
2953.010727	246341.981783	54.789812
2952.086811	246063.355390	54.794817
2951.518006	245787.041644	54.799821
2950.664804	245510.493361	54.804826
2949.961421	245227.861142	54.809831
2949.637672	244946.773743	54.814836
2948.400934	244672.121425	54.819841
2948.305328	244389.904083	54.824845
2947.273271	244113.285172	54.829850
2946.673011	243847.650398	54.834855
2946.318155	243568.531721	54.839860
2945.302818	243295.477055	54.844865
2944.943190	243011.674786	54.849869
2944.003680	242730.435070	54.854874
2943.950499	242449.845089	54.859879
2942.467970	242171.188183	54.864884
2941.884655	241905.656725	54.869889
2941.570395	241624.677079	54.874893
2941.102313	241352.736948	54.879898
2940.110381	241076.933355	54.884903
2939.426548	240781.117405	54.889908
2938.670335	240504.615763	54.894913
2938.083629	240228.571770	54.899917
2937.071950	239960.769790	54.904922
2936.434880	239681.984935	54.909927
2936.002285	239412.793888	54.914932
2935.471837	239142.524018	54.919937
2934.729736	238864.139785	54.924941
2933.726895	238584.880826	54.929946
2933.150499	238318.363463	54.934951
2932.628736	238040.608499	54.939956
2931.741817	237777.120908	54.944961
2931.623896	237489.245193	54.949965
2930.757904	237222.929169	54.954970
2930.196970	236943.680891	54.959975
2929.573912	236668.211806	54.964980
2928.621807	236393.101106	54.969985
2928.332897	236104.543271	54.974989
2927.497358	235835.424984	54.979994
2926.691004	235562.254112	54.984999
2926.434770	235271.885556	54.990004
2925.708971	235000.282171	54.995009
2924.941891	234720.334149	55.000013
2924.137635	234444.645134	55.005018
2923.368788	234161.745255	55.010023
2923.030309	233891.229422	55.015028
2922.254458	233617.702582	55.020033
2921.809689	233328.795504	55.025037
2921.014655	233057.997804	55.030042
2920.323507	232778.501666	55.035047
2919.935975	232485.081192	55.040052
2919.173954	232208.831702	55.045057
2918.572891	231932.150144	55.050061
2917.829134	231650.832395	55.055066
2917.237678	231362.743894	55.060071
2916.476353	231088.610995	55.065076
2915.393297	230812.594738	55.070081
2915.296897	230513.507299	55.075085
2914.690425	230241.924101	55.080090
2913.749089	229954.481089	55.085095
2912.778869	229681.327628	55.090100
2912.277868	229403.670386	55.095105
2911.610034	229119.063954	55.100109
2911.079580	228850.910302	55.105114
2910.353411	228564.990914	55.110119
2909.492729	228284.644345	55.115124
2908.707873	228001.715095	55.120129
2908.076115	227726.477285	55.125133
2907.431597	227450.504013	55.130138
2906.880306	227175.064295	55.135143
2906.534130	226905.028916	55.140148
2905.956696	226620.276454	55.145153
2905.402299	226337.010777	55.150157
2904.537706	226060.147626	55.155162
2903.906239	225776.985191	55.160167
2903.524344	225486.438864	55.165172
2902.321600	225217.588521	55.170177
2901.759475	224923.482832	55.175181
2901.242283	224651.636086	55.180186
2900.597372	224374.451124	55.185191
2899.992491	224087.433207	55.190196
2899.156315	223814.634159	55.195201
2898.631242	223515.232143	55.200205
2898.194079	223236.325211	55.205210
2897.268229	222950.126075	55.210215
2896.932618	222669.168329	55.215220
2895.755198	222394.684316	55.220225
2895.128603	222102.979887	55.225229
2894.762708	221822.755638	55.230234
2893.592753	221536.371312	55.235239
2893.311237	221258.783556	55.240244
2892.812725	220979.410867	55.245249
2892.206542	220691.311129	55.250253
2891.164867	220408.195021	55.255258
2890.713618	220120.582153	55.260263
2890.102473	219840.022313	55.265268
2889.314442	219564.659644	55.270273
2888.553932	219267.679444	55.275277
2888.197315	218985.364161	55.280282
2887.313701	218707.448602	55.285287
2886.872968	218423.379502	55.290292
2886.139469	218139.446995	55.295297
2885.614100	217849.398225	55.300301
2885.156463	217559.594502	55.305306
2884.215725	217266.037084	55.310311
2883.577718	216984.219843	55.315316
2882.667881	216705.959925	55.320321
2882.030816	216404.542610	55.325325
2881.431257	216122.824624	55.330330
2880.833702	215851.875875	55.335335
2880.411816	215568.782811	55.340340
2879.200518	215279.438951	55.345345
2878.784020	214982.549804	55.350349
2877.933958	214709.749077	55.355354
2877.363054	214416.641760	55.360359
2877.244218	214129.115504	55.365364
2876.066019	213852.399031	55.370369
2875.539581	213563.437849	55.375373
2874.988047	213272.992724	55.380378
2874.091730	212985.658218	55.385383
2873.290271	212696.349851	55.390388
2872.691336	212419.420449	55.395393
2872.041613	212124.121216	55.400397
2871.447267	211857.184898	55.405402
2870.809012	211572.119571	55.410407
2870.530392	211283.383904	55.415412
2869.251414	210993.917023	55.420417
2868.779550	210705.112779	55.425421
2867.835769	210437.728677	55.430426
2866.905647	210147.154078	55.435431
2866.789170	209862.993894	55.440436
2866.036631	209588.710351	55.445441
2865.405045	209309.903408	55.450445
2864.895561	209022.945681	55.455450
2863.934200	208739.611742	55.460455
2863.745243	208452.402308	55.465460
2862.867719	208162.465132	55.470465
2862.113669	207883.620478	55.475469
2861.575166	207601.153984	55.480474
2861.056739	207314.613039	55.485479
2860.027639	207029.248845	55.490484
2859.329961	206752.818641	55.495489
2858.790868	206466.883218	55.500493
2857.928322	206187.554628	55.505498
2857.338164	205906.262519	55.510503
2857.321736	205619.166703	55.515508
2856.321794	205342.358312	55.520513
2855.743251	205042.856972	55.525517
2855.101801	204750.888411	55.530522
2854.530429	204465.616981	55.535527
2853.658477	204180.534560	55.540532
2853.021685	203900.341344	55.545537
2852.453628	203606.305377	55.550541
2851.774535	203321.871211	55.555546
2850.867934	203031.009726	55.560551
2850.433374	202742.276577	55.565556
2849.567593	202466.084509	55.570561
2848.974570	202174.796050	55.575565
2848.359326	201892.102480	55.580570
2847.811335	201609.094291	55.585575
2846.869384	201313.538920	55.590580
2846.226691	201032.953828	55.595585
2845.796109	200750.771361	55.600589
2844.992966	200465.009905	55.605594
2844.376509	200172.908650	55.610599
2843.878056	199882.597270	55.615604
2842.722492	199609.799526	55.620609
2842.022337	199317.258069	55.625613
2841.414583	199033.318419	55.630618
2840.869426	198749.217673	55.635623
2840.194396	198473.804662	55.640628
2839.293013	198196.520212	55.645633
2838.733972	197898.365326	55.650637
2838.132055	197625.681000	55.655642
2837.277872	197354.654072	55.660647
2836.980418	197062.684868	55.665652
2836.269216	196778.799246	55.670657
2835.745466	196494.287452	55.675661
2834.859806	196218.321673	55.680666
2834.122351	195929.724166	55.685671
2833.791044	195641.420248	55.690676
2833.015541	195369.106177	55.695681
2832.661655	195078.658651	55.700685
2832.015668	194787.546508	55.705690
2830.933371	194506.760609	55.710695
2830.600507	194219.584749	55.715700
2829.683942	193931.586865	55.720705
2829.007895	193646.555345	55.725709
2828.324743	193366.654201	55.730714
2827.743155	193086.471361	55.735719
2827.270167	192786.564268	55.740724
2826.354853	192514.898635	55.745729
2825.966438	192217.259115	55.750733
2825.115499	191933.333969	55.755738
2824.393780	191651.731079	55.760743
2823.853740	191366.309571	55.765748
2823.396503	191083.319454	55.770753
2822.959888	190792.910260	55.775757
2821.981353	190501.125518	55.780762
2821.500579	190204.289117	55.785767
2820.874558	189913.139172	55.790772
2820.098733	189623.923129	55.795777
2819.321440	189331.299443	55.800781
2818.963113	189041.410164	55.805786
2818.098865	188759.567013	55.810791
2817.629362	188450.704457	55.815796
2816.612972	188169.970351	55.820801
2816.014926	187871.589667	55.825805
2815.481307	187585.922769	55.830810
2814.850764	187296.672663	55.835815
2814.350637	186996.628257	55.840820
2813.468986	186712.383138	55.845825
2812.780368	186418.377073	55.850829
2812.570213	186122.795969	55.855834
2811.363222	185830.682271	55.860839
2810.985984	185528.134627	55.865844
2810.091069	185242.094347	55.870849
2809.562859	184948.288676	55.875853
2808.979697	184660.650717	55.880858
2808.012640	184372.375743	55.885863
2807.439244	184074.970149	55.890868
2806.752707	183784.148501	55.895873
2805.986993	183500.477739	55.900877
2805.263466	183200.532163	55.905882
2804.441395	182922.038707	55.910887
2803.774871	182634.147246	55.915892
2803.123279	182353.098992	55.920897
2802.364754	182057.326415	55.925901
2802.028893	181781.154680	55.930906
2801.141018	181487.708865	55.935911
2800.710076	181195.782706	55.940916
2799.883638	180915.191230	55.945921
2799.132188	180620.648498	55.950925
2798.821597	180333.161165	55.955930
2797.969615	180056.827836	55.960935
2797.300560	179752.788984	55.965940
2796.534414	179473.024224	55.970945
2796.013020	179182.181889	55.975949
2795.084363	178909.874873	55.980954
2794.361562	178622.121000	55.985959
2794.188097	178331.839972	55.990964
2793.215007	178057.942881	55.995969
2792.220837	177770.873810	56.000973
2792.011853	177474.880719	56.005978
2791.056223	177207.778481	56.010983
2790.582307	176912.734422	56.015988
2789.736043	176630.355850	56.020993
2789.204218	176349.112262	56.025997
2788.706204	176069.289743	56.031002
2788.007384	175777.240205	56.036007
2787.319285	175488.383408	56.041012
2786.403672	175218.998462	56.046017
2785.876444	174930.196471	56.051021
2785.162648	174645.203413	56.056026
2784.665276	174372.591022	56.061031
2783.795766	174082.272267	56.066036
2783.165951	173810.435038	56.071041
2782.707997	173520.729225	56.076045
2782.076202	173228.089804	56.081050
2781.006865	172951.686052	56.086055
2780.355880	172660.567264	56.091060
2779.692101	172378.812749	56.096065
2779.383317	172106.262316	56.101069
2778.736865	171822.080010	56.106074
2778.079954	171543.725926	56.111079
2777.489785	171245.092091	56.116084
2777.152255	170972.872031	56.121089
2776.319839	170691.626902	56.126093
2775.628940	170311.271530	56.131098
2774.596490	170044.254805	56.136103
2774.170652	169750.451546	56.141108
2773.809681	169448.603385	56.146113
2772.869752	169163.622333	56.151117
2772.585504	168891.535696	56.156122
2772.013583	168585.989143	56.161127
2770.964175	168283.318237	56.166132
2770.431851	168023.688101	56.171137
2769.859110	167710.633522	56.176141
2769.291469	167415.548284	56.181146
2768.245790	167122.308576	56.186151
2767.904994	166835.050328	56.191156
2767.473080	166524.818930	56.196161
2766.173438	166259.880261	56.201165
2766.177429	165940.213366	56.206170
2765.440212	165657.108635	56.211175
2764.583090	165358.944847	56.216180
2763.903232	165072.911016	56.221185
2763.055513	164783.701820	56.226189
2762.595398	164486.791860	56.231194
2761.410523	164191.537598	56.236199
2761.275302	163901.739352	56.241204
2760.099814	163607.950521	56.246209
2759.601145	163321.863551	56.251213
2759.339041	163021.946269	56.256218
2758.368175	162733.306874	56.261223
2757.984296	162454.379441	56.266228
2757.372930	162157.372654	56.271233
2756.526088	161856.273588	56.276237
2756.173278	161542.817224	56.281242
2754.555641	161286.890258	56.286247
2754.435387	160965.672172	56.291252
2753.559250	160697.096353	56.296257
2752.998285	160390.179756	56.301261
2752.586663	160115.737449	56.306266
2751.805002	159833.727954	56.311271
2751.350079	159529.675252	56.316276
2750.303974	159248.653123	56.321281
2749.529183	158960.649023	56.326285
2749.024227	158662.256331	56.331290
2748.064575	158374.324504	56.336295
2747.791000	158086.845746	56.341300
2747.031747	157806.654294	56.346305
2746.243855	157503.460230	56.351309
2745.980171	157211.029370	56.356314
2744.861539	156939.749649	56.361319
2744.505415	156637.664355	56.366324
2743.597693	156360.076063	56.371329
2743.221459	156077.193981	56.376333
2742.829055	155764.939972	56.381338
2741.737518	155510.294297	56.386343
2741.148377	155184.170271	56.391348
2740.515379	154937.032346	56.396353
2739.625452	154613.745287	56.401357
2739.300566	154341.419979	56.406362
2738.181081	154045.236921	56.411367
2738.088517	153751.041970	56.416372
2737.049361	153455.321726	56.421377
2736.691251	153174.469497	56.426381
2736.375947	152868.852525	56.431386
2735.294624	152600.093150	56.436391
2735.001532	152274.611586	56.441396
2733.912511	152004.383877	56.446401
2733.388137	151717.393161	56.451405
2732.756979	151396.765585	56.456410
2731.829147	151129.773328	56.461415
2731.476821	150813.886247	56.466420
2730.578054	150534.819909	56.471425
2729.789188	150260.250477	56.476429
2729.563458	149939.852630	56.481434
2728.389779	149663.315700	56.486439
2727.673363	149366.691588	56.491444
2727.388409	149091.569311	56.496449
2726.787319	148776.186359	56.501453
2726.022128	148506.508393	56.506458
2725.127624	148207.279755	56.511463
2724.997625	147894.067630	56.516468
2723.889131	147630.335584	56.521473
2723.159971	147324.264548	56.526477
2722.498902	147035.291116	56.531482
2722.011644	146748.542149	56.536487
2721.362678	146461.287666	56.541492
2720.670625	146162.910425	56.546497
2719.857532	145863.170037	56.551501
2719.128870	145584.577560	56.556506
2718.527732	145286.893191	56.561511
2718.071332	145024.197971	56.566516
2717.204639	144702.988787	56.571521
2716.530357	144434.729103	56.576525
2716.166673	144129.902119	56.581530
2714.850267	143833.742791	56.586535
2714.113813	143570.773883	56.591540
2714.019400	143272.583858	56.596545
2713.343031	142984.349316	56.601549
2712.678477	142696.382452	56.606554
2711.690441	142424.454274	56.611559
2711.503133	142113.583799	56.616564
2710.605368	141833.285833	56.621569
2709.962594	141541.158803	56.626573
2709.337063	141256.731678	56.631578
2708.481788	140965.317289	56.636583
2707.699357	140685.037101	56.641588
2706.959675	140369.431165	56.646593
2706.396824	140120.326423	56.651597
2705.988435	139798.765952	56.656602
2705.019274	139551.572588	56.661607
2704.860737	139232.214755	56.666612
2703.778259	138970.738205	56.671617
2703.294536	138673.163455	56.676621
2702.777974	138371.493260	56.681626
2701.818357	138082.334155	56.686631
2701.289375	137808.888651	56.691636
2700.636649	137519.419651	56.696641
2699.841140	137224.614927	56.701645
2699.054690	136934.880677	56.706650
2698.497246	136669.517411	56.711655
2697.878195	136374.769512	56.716660
2697.330309	136080.534172	56.721665
2696.636070	135790.136081	56.726669
2695.945079	135524.880622	56.731674
2695.478974	135233.245130	56.736679
2694.596668	134942.275570	56.741684
2694.174669	134662.097196	56.746689
2693.381504	134361.947710	56.751693
2693.168552	134068.111682	56.756698
2691.938185	133784.817994	56.761703
2691.464204	133478.225006	56.766708
2690.889533	133198.339169	56.771713
2690.240683	132917.515156	56.776717
2689.650819	132619.333323	56.781722
2688.893562	132338.722738	56.786727
2688.407146	132042.232665	56.791732
2687.675451	131756.720843	56.796737
2686.547800	131466.295573	56.801741
2686.101234	131171.434155	56.806746
2685.140493	130883.604984	56.811751
2684.632694	130596.380177	56.816756
2684.403702	130312.492660	56.821761
2683.151548	130018.545782	56.826765
2682.975093	129732.077531	56.831770
2682.077625	129451.111599	56.836775
2681.662931	129159.339963	56.841780
2680.820659	128870.522161	56.846785
2680.357253	128568.667550	56.851789
2679.824010	128280.594379	56.856794
2678.730966	127992.968518	56.861799
2678.259153	127708.879440	56.866804
2677.804361	127412.154247	56.871809
2676.926718	127126.268628	56.876813
2676.125232	126826.429789	56.881818
2675.289598	126548.290315	56.886823
2674.808629	126256.191736	56.891828
2674.337414	125969.352213	56.896833
2673.603873	125687.433722	56.901837
2673.006035	125380.848080	56.906842
2672.427392	125099.025474	56.911847
2671.473742	124803.791976	56.916852
2671.047511	124520.821095	56.921857
2670.351782	124237.997483	56.926861
2669.752313	123932.038132	56.931866
2668.728088	123651.748915	56.936871
2668.259552	123368.415974	56.941876
2667.658387	123066.301597	56.946881
2667.069371	122779.591001	56.951885
2666.423633	122483.674079	56.956890
2665.764719	122207.100683	56.961895
2665.087123	121910.636531	56.966900
2664.304822	121611.310056	56.971905
2663.748284	121319.874122	56.976909
2663.027322	121040.935762	56.981914
2662.355038	120751.479788	56.986919
2661.628262	120462.587948	56.991924
2660.802568	120177.720694	56.996929
2660.377378	119881.366444	57.001933
2659.952208	119573.716011	57.006938
2659.040299	119295.556579	57.011943
2658.286272	119014.816902	57.016948
2657.918873	118680.373332	57.021953
2656.968030	118430.559803	57.026957
2656.410308	118133.478456	57.031962
2655.730907	117842.361202	57.036967
2654.967685	117536.159677	57.041972
2654.370739	117262.847192	57.046977
2653.627833	116982.216783	57.051981
2653.185011	116673.200987	57.056986
2652.207483	116393.782133	57.061991
2651.725081	116105.312945	57.066996
2651.444369	115805.453707	57.072001
2650.199728	115527.045126	57.077005
2650.013381	115224.429531	57.082010
2649.219883	114944.768991	57.087015
2648.473101	114657.557752	57.092020
2647.701714	114354.429648	57.097025
2646.779856	114074.621403	57.102029
2646.818787	113776.201717	57.107034
2645.697908	113495.009836	57.112039
2644.868848	113211.077627	57.117044
2644.847580	112901.222533	57.122049
2643.827166	112618.063581	57.127053
2643.323320	112333.994644	57.132058
2642.517912	112050.560590	57.137063
2641.909029	111746.016879	57.142068
2641.187245	111454.193205	57.147073
2640.411926	111164.627931	57.152077
2639.946851	110881.305667	57.157082
2639.024158	110594.740321	57.162087
2638.414727	110284.179904	57.167092
2637.701037	109990.773189	57.172097
2636.964267	109726.087386	57.177101
2636.497705	109414.379512	57.182106
2635.603359	109158.767172	57.187111
2634.995127	108852.685606	57.192116
2634.461523	108543.689936	57.197121
2633.529366	108297.204468	57.202125
2633.335827	107989.297773	57.207130
2632.289348	107700.127493	57.212135
2631.592435	107425.809640	57.217140
2631.039767	107142.601877	57.222145
2630.331206	106842.138843	57.227149
2629.751459	106551.157244	57.232154
2628.761906	106275.300027	57.237159
2628.203598	105986.897829	57.242164
2627.758706	105708.771958	57.247169
2627.060659	105426.838366	57.252173
2626.624396	105126.886682	57.257178
2625.787719	104854.752172	57.262183
2625.180475	104557.918100	57.267188
2624.900018	104264.100184	57.272193
2623.858680	103984.801167	57.277197
2623.382166	103685.787662	57.282202
2622.662469	103402.289271	57.287207
2621.861625	103123.476217	57.292212
2621.472678	102816.333445	57.297217
2620.201973	102542.315164	57.302221
2620.225806	102249.305220	57.307226
2619.609968	101954.915933	57.312231
2618.256802	101655.064983	57.317236
2617.889010	101381.602348	57.322241
2617.377184	101092.967251	57.327245
2616.598802	100797.711283	57.332250
2615.701801	100511.986212	57.337255
2615.025797	100217.444542	57.342260
2614.480898	99919.498714	57.347265
2613.678062	99658.202380	57.352269
2613.364310	99353.579903	57.357274
2612.439608	99068.574833	57.362279
2611.573849	98806.904908	57.367284
2610.985693	98501.950328	57.372289
2610.287059	98239.873511	57.377293
2609.838776	97945.134645	57.382298
2609.037889	97665.302866	57.387303
2608.548183	97390.162883	57.392308
2608.352959	97089.946997	57.397313
2606.971049	96798.840118	57.402317
2606.473251	96527.219068	57.407322
2606.100007	96240.830199	57.412327
2605.259753	95946.236512	57.417332
2604.820393	95644.277432	57.422337
2603.697004	95371.995746	57.427341
2603.546629	95077.684615	57.432346
2602.926781	94805.190497	57.437351
2601.985228	94513.960965	57.442356
2601.463976	94218.483323	57.447361
2600.361764	93934.820349	57.452365
2599.987508	93649.384234	57.457370
2599.347874	93364.361623	57.462375
2598.532469	93073.505068	57.467380
2597.964372	92790.850038	57.472385
2597.232165	92501.585732	57.477389
2596.718530	92219.011814	57.482394
2596.020928	91933.014983	57.487399
2595.534805	91637.547161	57.492404
2594.952417	91347.170996	57.497409
2594.027417	91066.642636	57.502413
2593.113246	90771.596691	57.507418
2592.768849	90486.019246	57.512423
2591.992691	90210.233499	57.517428
2591.517341	89911.617149	57.522433
2590.630293	89657.469467	57.527437
2590.390602	89341.515262	57.532442
2589.683362	89060.185707	57.537447
2588.737603	88773.026956	57.542452
2588.079482	88471.720586	57.547457
2587.437415	88191.767710	57.552461
2586.739727	87904.758695	57.557466
2585.940092	87614.574579	57.562471
2585.273446	87321.837556	57.567476
2584.591503	87039.148369	57.572481
2583.990804	86769.122095	57.577485
2583.499928	86477.211862	57.582490
2582.992218	86187.038838	57.587495
2582.443113	85903.291331	57.592500
2581.822436	85615.387975	57.597505
2580.732377	85328.038312	57.602509
2579.955878	85041.035843	57.607514
2579.253299	84747.763006	57.612519
2578.650574	84461.469785	57.617524
2577.903787	84185.775774	57.622529
2577.367834	83897.787248	57.627533
2576.815409	83605.362148	57.632538
2576.029286	83330.490516	57.637543
2575.334499	83044.224796	57.642548
2574.795271	82758.096777	57.647553
2574.193165	82483.422570	57.652557
2573.548048	82188.851654	57.657562
2572.612108	81912.704099	57.662567
2571.987151	81621.382922	57.667572
2571.543170	81336.716936	57.672577
2571.090876	81054.641856	57.677581
2570.341139	80760.994962	57.682586
2569.315463	80478.245430	57.687591
2568.754852	80195.799950	57.692596
2568.304671	79898.036651	57.697601
2567.448214	79625.386030	57.702605
2566.617280	79333.464277	57.707610
2566.106164	79058.618200	57.712615
2565.183163	78769.855792	57.717620
2564.842790	78479.630046	57.722625
2564.013449	78213.476302	57.727629
2563.264966	77921.143359	57.732634
2562.757264	77633.649153	57.737639
2561.799374	77369.028522	57.742644
2561.627322	77078.979745	57.747649
2560.889050	76799.352802	57.752653
2559.962215	76505.218284	57.757658
2559.625452	76223.945276	57.762663
2559.033830	75949.806445	57.767668
2558.418180	75660.792300	57.772673
2557.528357	75379.415947	57.777677
2556.827548	75093.109780	57.782682
2555.969350	74807.618237	57.787687
2555.208884	74526.036908	57.792692
2554.836510	74241.838528	57.797697
2553.910747	73971.188024	57.802701
2553.256959	73680.599226	57.807706
2552.601138	73401.228103	57.812711
2551.810631	73130.808276	57.817716
2551.371776	72841.046524	57.822721
2550.324868	72575.761817	57.827725
2550.219766	72293.772331	57.832730
2549.570502	72012.006125	57.837735
2548.731314	71742.214696	57.842740
2548.004479	71456.047161	57.847745
2547.340897	71180.363498	57.852749
2546.763242	70883.310797	57.857754
2546.247070	70620.058502	57.862759
2545.538163	70339.902819	57.867764
2545.070036	70048.267368	57.872769
2544.170169	69770.417657	57.877773
2543.505566	69473.811742	57.882778
2542.697966	69202.517329	57.887783
2541.811622	68926.723257	57.892788
2541.664444	68632.226880	57.897793
2540.756427	68364.272494	57.902797
2539.977650	68088.739236	57.907802
2539.429262	67806.200399	57.912807
2538.815466	67521.465751	57.917812
2538.115115	67236.562176	57.922817
2537.211072	66968.889249	57.927821
2536.427382	66697.717836	57.932826
2536.059695	66418.438406	57.937831
2535.031095	66143.795701	57.942836
2534.824305	65860.236911	57.947841
2534.063625	65594.878095	57.952845
2533.483777	65320.043043	57.957850
2532.700348	65043.521787	57.962855
2531.948467	64756.728527	57.967860
2531.466102	64473.028124	57.972865
2530.629997	64214.441029	57.977869
2530.111475	63938.014089	57.982874
2529.676347	63662.169976	57.987879
2528.878897	63379.428595	57.992884
2528.563902	63097.903461	57.997889
2527.626533	62812.083819	58.002893
2526.607486	62533.106860	58.007898
2526.143888	62262.286380	58.012903
2525.467610	61985.450694	58.017908
2524.770850	61710.268450	58.022913
2524.228640	61444.777780	58.027917
2523.466052	61159.306835	58.032922
2522.833917	60865.013123	58.037927
2522.026433	60605.692102	58.042932
2521.479835	60321.864688	58.047937
2520.503128	60049.486065	58.052941
2520.405586	59773.664297	58.057946
2519.594834	59504.321846	58.062951
2518.775211	59228.423182	58.067956
2518.459932	58947.393875	58.072961
2517.617346	58672.542105	58.077965
2516.774214	58393.526076	58.082970
2516.330676	58111.152938	58.087975
2515.200552	57839.350051	58.092980
2514.900107	57564.628166	58.097985
2513.897168	57302.086295	58.102989
2513.308661	57019.316054	58.107994
2512.858623	56741.193115	58.112999
2512.245633	56468.648016	58.118004
2511.647472	56194.272243	58.123009
2511.017456	55925.655803	58.128013
2509.992719	55656.188130	58.133018
2509.424078	55375.243872	58.138023
2508.830390	55101.621093	58.143028
2508.175480	54821.990136	58.148033
2507.235002	54554.936671	58.153037
2506.862068	54283.819537	58.158042
2506.273700	54015.291040	58.163047
2505.169108	53741.238072	58.168052
2504.982137	53468.439210	58.173057
2503.774265	53198.983125	58.178061
2503.395808	52923.757918	58.183066
2502.751372	52658.947782	58.188071
2502.253166	52382.629709	58.193076
2501.399861	52114.234684	58.198081
2500.753255	51849.607631	58.203085
2499.720833	51566.318503	58.208090
2499.434626	51288.249802	58.213095
2498.409828	51024.685134	58.218100
2498.041428	50750.513457	58.223105
2497.131716	50496.378967	58.228109
2496.561840	50224.933271	58.233114
2496.201701	49963.262494	58.238119
2495.464254	49704.436144	58.243124
2494.835470	49422.872752	58.248129
2494.143172	49158.163040	58.253133
2493.735007	48882.390858	58.258138
2492.923640	48619.327724	58.263143
2491.725730	48339.997508	58.268148
2491.453394	48075.341770	58.273153
2490.693879	47810.628037	58.278157
2490.306545	47540.823483	58.283162
2489.593713	47272.899782	58.288167
2488.441944	46994.352179	58.293172
2488.129699	46740.803072	58.298177
2487.291275	46468.179625	58.303181
2486.853012	46206.184559	58.308186
2486.128474	45933.535549	58.313191
2484.958735	45678.524650	58.318196
2484.434843	45402.531113	58.323201
2483.886346	45150.696602	58.328205
2482.835194	44885.428001	58.333210
2482.571123	44611.426752	58.338215
2481.763744	44362.465755	58.343220
2480.813817	44106.990738	58.348225
2480.415640	43840.562442	58.353229
2479.508887	43584.692953	58.358234
2479.007047	43329.711778	58.363239
2478.252913	43075.122215	58.368244
2477.753985	42810.740160	58.373249
2476.927937	42557.627454	58.378253
2476.300438	42295.563162	58.383258
2475.621061	42040.237047	58.388263
2474.773143	41779.037726	58.393268
2474.455750	41522.125115	58.398273
2473.755255	41273.191676	58.403277
2472.950333	41011.244649	58.408282
2472.427369	40746.455442	58.413287
2471.478170	40506.887663	58.418292
2470.936260	40260.191920	58.423297
2470.388540	40000.431315	58.428301
2469.377395	39749.133128	58.433306
2469.304958	39494.207198	58.438311
2468.465088	39241.521905	58.443316
2467.678963	38975.535652	58.448321
2467.115787	38727.975475	58.453325
2466.795970	38473.535622	58.458330
2465.929637	38209.734994	58.463335
2464.983355	37967.091631	58.468340
2464.396193	37706.529834	58.473345
2463.780172	37457.202532	58.478349
2463.211740	37196.394313	58.483354
2462.481394	36935.949309	58.488359
2461.596073	36682.854220	58.493364
2461.195468	36440.245897	58.498369
2460.171995	36180.895916	58.503373
2459.493875	35927.591273	58.508378
2458.972522	35666.107064	58.513383
2457.794663	35425.120741	58.518388
2457.328088	35175.637657	58.523393
2456.720054	34931.152757	58.528397
2455.824083	34689.896868	58.533402
2455.438460	34442.750906	58.538407
2454.676229	34203.837204	58.543412
2454.108561	33958.830749	58.548417
2453.248173	33715.560509	58.553421
2452.175403	33467.913752	58.558426
2451.902908	33221.850507	58.563431
2450.951287	32986.246027	58.568436
2450.626597	32744.913594	58.573441
2449.684614	32510.346252	58.578445
2448.872794	32272.277314	58.583450
2448.447133	32030.233387	58.588455
2447.363360	31807.456449	58.593460
2446.924750	31571.296250	58.598465
2446.182852	31341.038589	58.603469
2445.627077	31114.956040	58.608474
2445.101370	30868.313893	58.613479
2443.737570	30646.246497	58.618484
2443.301594	30413.619656	58.623489
2442.725211	30184.423229	58.628493
2441.823666	29965.546533	58.633498
2441.125228	29736.352041	58.638503
2440.280516	29521.982991	58.643508
2439.534109	29295.507108	58.648513
2438.360258	29078.143733	58.653517
2437.293481	28882.252237	58.658522
2436.704188	28681.416778	58.663527
2435.497040	28492.054827	58.668532
2434.186447	28306.378190	58.673537
2433.197720	28141.606815	58.678541
2432.033536	27973.421053	58.683546
2431.521805	27794.430820	58.688551
2430.198245	27637.213557	58.693556
2429.523610	27480.153218	58.698561
2428.565509	27324.640854	58.703565
2427.690396	27179.594873	58.708570
2426.952316	27034.969197	58.713575
2425.955279	26901.623553	58.718580
2425.255797	26758.508339	58.723585
2424.587281	26621.582423	58.728589
2423.516756	26499.031163	58.733594
2422.841666	26373.330800	58.738599
2421.987576	26245.223279	58.743604
2421.840524	26119.734979	58.748609
2421.055262	26006.048715	58.753613
2420.149611	25894.863041	58.758618
2419.347122	25764.815423	58.763623
2418.497587	25652.958330	58.768628
2418.150672	25532.946223	58.773633
2417.630638	25434.106599	58.778637
2416.832222	25318.528723	58.783642
2416.306350	25210.426842	58.788647
2415.251171	25106.588922	58.793652
2414.837815	24976.692125	58.798657
2414.086781	24881.803304	58.803661
2413.489071	24775.747725	58.808666
2413.244786	24653.303856	58.813671
2411.953470	24548.732294	58.818676
2411.589860	24441.554382	58.823681
2410.845753	24321.208435	58.828685
2410.079354	24222.778631	58.833690
2409.309656	24131.227386	58.838695
2408.782116	24029.452093	58.843700
2408.594496	23926.736739	58.848705
2408.018476	23830.334716	58.853709
2407.016248	23725.080720	58.858714
2406.396590	23617.353539	58.863719
2405.630798	23511.800508	58.868724
2405.411142	23406.412692	58.873729
2404.724833	23290.999145	58.878733
2403.936906	23196.513147	58.883738
2403.593299	23082.803736	58.888743
2402.468966	22993.340707	58.893748
2402.127411	22875.905375	58.898753
2401.528993	22768.514600	58.903757
2400.587428	22662.622389	58.908762
2400.494212	22557.431779	58.913767
2399.427255	22457.904581	58.918772
2399.011117	22362.296266	58.923777
2398.554277	22249.659383	58.928781
2397.408746	22138.668264	58.933786
2397.426394	22034.149709	58.938791
2396.337600	21931.522263	58.943796
2395.607330	21815.966156	58.948801
2394.922867	21713.456039	58.953805
2394.121160	21613.087536	58.958810
2393.718652	21506.226181	58.963815
2392.869254	21413.172327	58.968820
2392.299580	21302.275015	58.973825
2391.280227	21205.051298	58.978829
2390.749608	21108.689449	58.983834
2390.136317	21002.687637	58.988839
2389.186340	20912.171712	58.993844
2388.709678	20809.642031	58.998849
2387.866006	20719.832380	59.003853
2387.212228	20623.982931	59.008858
2386.685313	20524.535486	59.013863
2385.546544	20439.688947	59.018868
2384.734421	20353.321411	59.023873
2384.125791	20268.407921	59.028877
2383.631989	20183.760901	59.033882
2383.615061	20086.671350	59.038887
2382.206324	20006.840599	59.043892
2382.033430	19906.871190	59.048897
2381.287850	19812.769433	59.053901
2380.066382	19727.769344	59.058906
2379.966304	19636.761281	59.063911
2379.090569	19550.657340	59.068916
2378.631130	19458.941123	59.073921
2377.826530	19371.860590	59.078925
2377.793724	19278.850176	59.083930
2377.119563	19195.856262	59.088935
2376.093191	19091.344811	59.093940
2375.375109	19011.213460	59.098945
2374.883876	18917.109135	59.103949
2373.910162	18833.381538	59.108954
2373.542659	18739.161567	59.113959
2372.867363	18653.552208	59.118964
2371.974089	18564.746817	59.123969
2371.322247	18475.461974	59.128973
2370.629323	18387.853353	59.133978
2370.185465	18290.689517	59.138983
2369.306714	18209.883232	59.143988
2368.687152	18121.044076	59.148993
2368.499000	18022.373099	59.153997
2367.525384	17933.577741	59.159002
2366.764333	17851.186553	59.164007
2366.109849	17755.331151	59.169012
2365.592746	17679.874715	59.174017
2364.897772	17586.054865	59.179021
2363.898965	17497.378288	59.184026
2363.886583	17409.655230	59.189031
2362.824307	17328.485794	59.194036
2362.124741	17234.779309	59.199041
2361.657453	17151.934794	59.204045
2360.838290	17076.469997	59.209050
2360.335212	16976.052769	59.214055
2359.485045	16880.765032	59.219060
2358.777892	16804.201831	59.224065
2358.044455	16731.877880	59.229069
2357.252441	16650.905153	59.234074
2357.025075	16559.234565	59.239079
2355.602222	16484.999477	59.244084
2355.288021	16399.396020	59.249089
2355.002960	16311.477546	59.254093
2354.326398	16230.438794	59.259098
2353.637205	16137.947503	59.264103
2352.598797	16076.315214	59.269108
2352.294932	15976.938033	59.274113
2351.480765	15889.000704	59.279117
2350.584960	15821.744829	59.284122
2350.232992	15733.445822	59.289127
2349.321191	15651.728201	59.294132
2348.544697	15571.051013	59.299137
2348.327312	15495.502964	59.304141
2347.677057	15418.364628	59.309146
2347.091194	15332.951157	59.314151
2346.098839	15249.696096	59.319156
2345.506481	15166.019146	59.324161
2344.627958	15095.741317	59.329165
2343.801597	15010.747402	59.334170
2343.498694	14932.426143	59.339175
2342.835223	14859.741886	59.344180
2341.974971	14776.169751	59.349185
2341.521373	14698.298876	59.354189
2340.586613	14625.864442	59.359194
2340.188238	14541.746982	59.364199
2339.573762	14476.641359	59.369204
2339.081678	14397.160842	59.374209
2338.222163	14321.250735	59.379213
2337.318081	14237.958766	59.384218
2337.066153	14151.101460	59.389223
2336.236920	14074.281199	59.394228
2335.218482	14001.332466	59.399233
2334.810083	13936.176611	59.404237
2333.925488	13850.863962	59.409242
2333.651487	13763.126317	59.414247
2332.785297	13701.755447	59.419252
2332.437085	13630.323140	59.424257
2331.881026	13549.182679	59.429261
2330.707678	13463.156555	59.434266
2330.164829	13390.104349	59.439271
2329.373116	13317.059015	59.444276
2328.453459	13244.974583	59.449281
2327.955344	13179.070649	59.454285
2327.534743	13097.480537	59.459290
2326.864598	13025.672043	59.464295
2326.068669	12961.541123	59.469300
2325.354163	12886.416917	59.474305
2324.812001	12812.984450	59.479309
2324.009021	12737.083133	59.484314
2323.563642	12661.843967	59.489319
2323.011624	12585.253380	59.494324
2322.337405	12515.283999	59.499329
2321.591548	12435.258183	59.504333
2320.784438	12366.894086	59.509338
2320.354691	12295.454540	59.514343
2319.825809	12230.647953	59.519348
2318.873032	12141.432655	59.524353
2318.424590	12065.868669	59.529357
2317.150862	12006.028886	59.534362
2316.512255	11930.838588	59.539367
2316.087578	11859.854401	59.544372
2315.269320	11788.459530	59.549377
2314.817663	11715.290643	59.554381
2314.072308	11642.060195	59.559386
2313.638388	11565.119103	59.564391
2312.680791	11508.869480	59.569396
2312.247423	11437.341446	59.574401
2311.770401	11364.545975	59.579405
2310.828344	11299.127566	59.584410
2309.950461	11229.489753	59.589415
2309.529686	11159.494529	59.594420
2308.596761	11088.379560	59.599425
2308.359868	11029.401198	59.604429
2307.426250	10965.590933	59.609434
2307.020988	10884.588056	59.614439
2306.329257	10814.442123	59.619444
2305.680619	10750.165449	59.624449
2305.379128	10669.232087	59.629453
2304.290687	10614.711599	59.634458
2303.570714	10531.829838	59.639463
2302.916018	10455.532605	59.644468
2302.097744	10398.021182	59.649473
2301.368809	10333.106526	59.654477
2300.422720	10250.818412	59.659482
2299.787108	10203.050349	59.664487
2299.277938	10141.588574	59.669492
2298.683314	10089.771245	59.674497
2298.052546	10019.697851	59.679501
2297.385973	9948.331029	59.684506
2296.864829	9893.791824	59.689511
2296.219969	9818.246572	59.694516
2295.707025	9761.900609	59.699521
2295.023286	9686.604791	59.704525
2294.170629	9626.343194	59.709530
2293.850427	9549.465359	59.714535
2293.197342	9486.405434	59.719540
2292.353336	9412.430282	59.724545
2291.954065	9332.412306	59.729549
2291.368547	9273.090802	59.734554
2290.792708	9199.107699	59.739559
2290.097062	9131.908611	59.744564
2289.519354	9067.631830	59.749569
2288.645538	8987.061010	59.754573
2287.692116	8919.147585	59.759578
2286.964407	8838.768975	59.764583
2286.284386	8789.116709	59.769588
2285.391442	8714.468784	59.774593
2285.257816	8656.987985	59.779597
2284.335008	8595.149271	59.784602
2283.782501	8526.428533	59.789607
2282.833203	8457.937502	59.794612
2282.183036	8385.550360	59.799617
2281.686589	8323.640016	59.804621
2280.884423	8259.400735	59.809626
2280.289206	8186.769176	59.814631
2279.724743	8136.189994	59.819636
2278.730280	8073.771180	59.824641
2278.354400	8006.432954	59.829645
2277.655602	7939.744210	59.834650
2276.699190	7882.723879	59.839655
2276.314066	7826.281314	59.844660
2275.863817	7755.565506	59.849665
2275.359589	7692.378313	59.854669
2274.763960	7626.027225	59.859674
2274.020479	7554.683629	59.864679
2273.355512	7486.693112	59.869684
2272.366430	7421.811055	59.874689
2272.062121	7344.656079	59.879693
2271.180837	7283.693012	59.884698
2270.295107	7215.746638	59.889703
2269.488001	7148.491734	59.894708
2269.140776	7092.068028	59.899713
2268.547906	7025.949515	59.904718
2267.708568	6973.227347	59.909722
2267.244177	6900.274464	59.914727
2266.403273	6835.586812	59.919732
2265.834418	6773.035749	59.924737
2265.427896	6716.618930	59.929742
2264.204093	6657.415784	59.934746
2263.855236	6587.263692	59.939751
2263.589460	6529.755656	59.944756
2262.667653	6459.770772	59.949761
2262.269520	6384.418318	59.954766
2261.159530	6325.029650	59.959770
2260.642834	6257.112744	59.964775
2260.005964	6193.454855	59.969780
2259.018711	6135.938163	59.974785
2258.564512	6065.063809	59.979790
2257.957365	6003.805387	59.984794
2257.323727	5936.518213	59.989799
2256.392127	5882.686642	59.994804
2255.581433	5823.495453	59.999809
2255.436554	5758.787286	60.004814
2254.607613	5706.038801	60.009818
2254.218911	5640.148063	60.014823
2253.521228	5563.858218	60.019828
2252.511952	5506.093500	60.024833
2252.019782	5437.883056	60.029838
2251.297656	5378.680390	60.034842
2250.773612	5311.354228	60.039847
2249.849328	5249.627104	60.044852
2249.123952	5185.385804	60.049857
2248.763029	5119.856579	60.054862
2247.938755	5066.965307	60.059866
2247.241430	4995.177155	60.064871
2246.836575	4945.683790	60.069876
2245.900567	4886.790708	60.074881
2245.240390	4816.756338	60.079886
2244.330386	4758.409368	60.084890
2244.118330	4698.805947	60.089895
2243.698547	4633.889990	60.094900
2242.756301	4565.142167	60.099905
2242.405159	4504.787106	60.104910
2241.467123	4441.527626	60.109914
2240.638144	4369.007070	60.114919
2240.194077	4311.582481	60.119924
2239.031862	4244.888470	60.124929
2238.688916	4185.856801	60.129934
2238.331506	4123.162757	60.134938
2237.640181	4079.171339	60.139943
2236.988482	4011.329564	60.144948
2235.871836	3946.752739	60.149953
2235.244006	3878.942491	60.154958
2234.643297	3828.685843	60.159962
2234.223860	3759.552077	60.164967
2233.320262	3702.220116	60.169972
2232.744901	3645.385202	60.174977
2232.178904	3572.495639	60.179982
2231.348637	3516.367266	60.184986
2230.974074	3450.999056	60.189991
2230.140676	3396.506458	60.194996
2229.391578	3329.699033	60.200001
2228.983407	3265.981247	60.205006
2227.897979	3213.470093	60.210010
2227.175389	3152.681901	60.215015
2226.625596	3089.589058	60.220020
2225.868377	3040.108331	60.225025
2225.585146	2984.847852	60.230030
2224.823117	2919.584486	60.235034
2223.875239	2862.072794	60.240039
2223.212689	2810.155272	60.245044
2222.782114	2753.590266	60.250049
2222.212379	2681.441486	60.255054
2220.990996	2637.270374	60.260058
2220.749811	2573.837449	60.265063
2220.270802	2514.569924	60.270068
2219.455734	2458.606440	60.275073
2218.676813	2394.040469	60.280078
2217.825019	2348.203717	60.285082
2217.263068	2289.245187	60.290087
2216.928123	2220.054823	60.295092
2216.116542	2178.175520	60.300097
2215.734940	2122.920501	60.305102
2214.622922	2065.329173	60.310106
2214.101686	2010.197666	60.315111
2213.784693	1943.759371	60.320116
2212.987497	1890.717576	60.325121
2212.298968	1832.090085	60.330126
2211.297896	1779.841188	60.335130
2210.566131	1714.382862	60.340135
2209.721146	1667.664020	60.345140
2209.193864	1617.357602	60.350145
2208.769882	1551.499499	60.355150
2207.966215	1504.566458	60.360154
2207.279493	1459.458569	60.365159
2206.825415	1386.193930	60.370164
2205.988271	1338.858286	60.375169
2205.574822	1286.372859	60.380174
2204.514817	1227.442449	60.385178
2203.822308	1181.774927	60.390183
2203.532827	1134.814340	60.395188
2202.657267	1087.089786	60.400193
2201.856484	1013.391585	60.405198
2201.244155	970.996869	60.410202
2200.423007	912.575483	60.415207
2199.835135	873.050422	60.420212
2199.244309	822.413060	60.425217
2198.695611	764.704414	60.430222
2197.675927	719.607497	60.435226
2197.448841	667.315517	60.440231
2196.437277	618.037139	60.445236
2195.752118	575.018052	60.450241
2195.168475	514.149456	60.455246
2194.282440	479.261646	60.460250
2193.532765	428.613017	60.465255
2192.869752	384.490292	60.470260
2192.329127	335.795739	60.475265
2191.806594	303.969818	60.480270
2190.601607	257.829867	60.485274
2190.422136	207.004823	60.490279
2189.630908	176.317756	60.495284
2188.757584	127.214658	60.500289
2188.206685	89.122422	60.505294
2187.210715	36.902665	60.510298
2186.392349	10.569292	60.515303
2185.832920	-27.056104	60.520308
2184.771968	-52.507248	60.525313
2182.292658	-34.210144	60.530318
2177.134144	76.923462	60.535322
2177.556404	84.706165	60.540327
2178.496119	89.196237	60.545332
2178.985037	105.740592	60.550337
2179.730675	101.858230	60.555342
2179.407655	104.552306	60.560346
2178.822916	91.599462	60.565351
2178.234807	81.261639	60.570356
2177.323115	83.541349	60.575361
2176.585881	67.189305	60.580366
2176.004905	63.519003	60.585370
2175.131073	68.320448	60.590375
2174.507331	62.733134	60.595380
2173.220537	57.213174	60.600385
2172.340540	55.791643	60.605390
2171.290826	73.327512	60.610394
2170.707500	70.755093	60.615399
2170.973593	62.587164	60.620404
2170.470251	67.903815	60.625409
2170.287823	70.241280	60.630414
2169.491422	62.530493	60.635418
2168.029971	71.670138	60.640423
2167.641068	67.601950	60.645428
2166.214497	73.180192	60.650433
2165.620642	71.628111	60.655438
2165.670919	71.815634	60.660442
2164.924227	78.615323	60.665447
2164.570298	67.086081	60.670452
2163.374091	69.103442	60.675457
2163.430473	71.262676	60.680462
2163.077602	76.218004	60.685466
2161.995338	73.962857	60.690471
2160.816790	59.234079	60.695476
2160.349778	72.533453	60.700481
2160.322966	57.959395	60.705486
2159.393682	67.113951	60.710490
2158.677968	61.943340	60.715495
2158.125437	67.034418	60.720500
2156.939278	65.133211	60.725505
2156.470240	62.817042	60.730510
2155.670249	63.156814	60.735514
2154.691761	75.830900	60.740519
2154.578361	54.663445	60.745524
2154.047374	77.637682	60.750529
2153.774907	66.171209	60.755534
2153.024899	74.348044	60.760538
2152.383348	68.457644	60.765543
2151.782608	63.084297	60.770548
2150.420456	70.427895	60.775553
2149.917125	63.367597	60.780558
2149.281897	75.351738	60.785562
2148.987977	78.946326	60.790567
2148.050163	68.093176	60.795572
2147.056981	68.197111	60.800577
2146.465171	74.264207	60.805582
2145.851216	67.131579	60.810586
2144.965575	70.151453	60.815591
2145.477842	69.844645	60.820596
2144.338395	73.385739	60.825601
2143.419377	75.870039	60.830606
2142.933138	70.380757	60.835610
2142.271824	67.696146	60.840615
2141.497029	68.009849	60.845620
2141.175573	67.217187	60.850625
2140.545015	71.559015	60.855630
2139.353112	71.722867	60.860634
2138.460912	64.793655	60.865639
2138.693262	71.502657	60.870644
2137.945253	69.911967	60.875649
2136.550353	73.458905	60.880654
2136.480487	66.774513	60.885658
2135.747951	72.927015	60.890663
2135.208465	63.373099	60.895668
2134.248298	70.941490	60.900673
2133.499011	79.425709	60.905678
2133.162577	73.300829	60.910682
2132.071888	71.062801	60.915687
2131.850335	63.558847	60.920692
2131.331524	80.053326	60.925697
2130.703986	78.014610	60.930702
2129.401745	80.911367	60.935706
2128.459688	80.422172	60.940711
2128.558434	72.605629	60.945716
2128.196880	81.495085	60.950721
2127.560778	80.608853	60.955726
2126.113516	81.986431	60.960730
2125.294664	75.004583	60.965735
2125.250547	76.066483	60.970740
2124.539921	77.782896	60.975745
2124.179778	77.693356	60.980750
2122.964283	69.552364	60.985754
2122.256915	76.945037	60.990759
2122.188769	69.535006	60.995764
2121.176355	74.117194	61.000769
2120.388955	76.247895	61.005774
2119.868525	74.685751	61.010778
2119.258297	81.403877	61.015783
2118.543509	76.381353	61.020788
2117.586572	73.612775	61.025793
2117.122652	67.476591	61.030798
2116.571217	74.888674	61.035802
2116.050183	71.147376	61.040807
2115.182245	67.569929	61.045812
2114.598518	75.302513	61.050817
2114.112057	74.039318	61.055822
2113.512048	74.659593	61.060826
2112.920725	73.964947	61.065831
2112.332835	71.189849	61.070836
2111.793174	68.892778	61.075841
2111.086693	75.025383	61.080846
2110.295448	81.819540	61.085850
2108.887881	71.933461	61.090855
2108.550068	69.856663	61.095860
2108.203328	78.190282	61.100865
2107.829154	73.867464	61.105870
2106.546070	68.621325	61.110874
2105.835238	83.255597	61.115879
2105.065050	75.017143	61.120884
2104.234137	79.638344	61.125889
2104.172803	76.879035	61.130894
2103.947987	79.371458	61.135898
2102.745182	85.297411	61.140903
2102.218595	66.362156	61.145908
2101.365192	81.400656	61.150913
2101.178403	68.663821	61.155918
2100.681772	67.298170	61.160922
2099.813858	73.796999	61.165927
2099.158401	75.629238	61.170932
2097.554121	70.416725	61.175937
2097.028411	68.256209	61.180942
2097.316677	72.406514	61.185946
2096.788521	73.330767	61.190951
2095.869193	64.904687	61.195956
2095.054029	77.529218	61.200961
2094.199112	72.489518	61.205966
2093.945989	71.153032	61.210970
2093.202100	68.659726	61.215975
2092.314884	78.298040	61.220980
2090.721293	66.978149	61.225985
2091.001961	66.419513	61.230990
2090.342487	61.310959	61.235994
2089.044683	69.882223	61.240999
2089.219657	59.950033	61.246004
2088.227655	71.347425	61.251009
2087.510582	70.023064	61.256014
2086.714842	73.853399	61.261018
2086.208754	74.428815	61.266023
2085.750092	70.453709	61.271028
2085.228142	70.763573	61.276033
2084.685719	69.690606	61.281038
2084.107703	71.449060	61.286042
2083.321414	80.306574	61.291047
2082.617938	68.388141	61.296052
2081.301591	77.741334	61.301057
2080.349256	79.595459	61.306062
2080.357093	71.753923	61.311066
2080.172444	78.251560	61.316071
2079.143643	71.344047	61.321076
2078.349442	72.290024	61.326081
2077.697326	76.062878	61.331086
2077.576049	66.311731	61.336090
2076.577697	77.481491	61.341095
2076.115273	75.514353	61.346100
2075.115250	70.537110	61.351105
2074.014414	73.750421	61.356110
2073.865913	66.618064	61.361114
2073.162977	67.038649	61.366119
2072.577966	65.135120	61.371124
2072.120742	80.856618	61.376129
2071.220833	74.404871	61.381134
2071.099869	67.925705	61.386138
2070.332597	73.001993	61.391143
2068.950009	68.861289	61.396148
2068.009935	69.710575	61.401153
2067.456911	77.321604	61.406158
2067.587047	75.470158	61.411162
2066.790141	79.365336	61.416167
2066.515452	65.915518	61.421172
2065.977972	76.777187	61.426177
2064.744496	71.709268	61.431182
2063.603581	70.346526	61.436186
2062.528520	73.273488	61.441191
2062.605647	67.615979	61.446196
2061.760919	72.978938	61.451201
2060.941056	76.191817	61.456206
2060.638999	66.841506	61.461210
2059.715528	75.640371	61.466215
2059.645905	66.155407	61.471220
2058.805368	80.147975	61.476225
2058.422883	69.922641	61.481230
2058.217448	64.343090	61.486234
2056.548318	70.234255	61.491239
2055.813690	68.958419	61.496244
2054.642005	64.481494	61.501249
2054.262278	63.800588	61.506254
2054.337713	70.045645	61.511258
2053.219086	76.160095	61.516263
2052.941049	62.217251	61.521268
2052.361456	70.920543	61.526273
2052.126538	78.249290	61.531278
2051.081775	67.175051	61.536282
2049.634767	72.453831	61.541287
2049.271109	78.598272	61.546292
2048.600058	60.797675	61.551297
2047.741947	81.579928	61.556302
2047.526787	68.951682	61.561306
2046.940590	65.889340	61.566311
2047.009704	61.768987	61.571316
2045.921646	70.869927	61.576321
2044.812383	68.504004	61.581326
2044.160654	66.937485	61.586330
2043.213856	81.959278	61.591335
2043.341111	66.994944	61.596340
2042.555099	75.147553	61.601345
2041.274916	63.281244	61.606350
2040.569968	66.371815	61.611354
2039.642899	71.471894	61.616359
2039.936175	58.510666	61.621364
2038.935328	72.610669	61.626369
2038.123122	70.025724	61.631374
2037.657531	63.702178	61.636378
2036.844730	75.735013	61.641383
2036.704931	67.314545	61.646388
2036.129098	66.682111	61.651393
2034.776428	71.288366	61.656398
2034.351763	63.398791	61.661402
2033.526014	77.013716	61.666407
2033.182946	59.496949	61.671412
2032.376136	76.196398	61.676417
2031.668421	77.314734	61.681422
2030.776467	77.888326	61.686426
2029.623529	77.088876	61.691431
2029.657730	71.036074	61.696436
2028.949070	72.361132	61.701441
2028.046360	69.322221	61.706446
2027.851577	73.210150	61.711450
2026.900854	74.408054	61.716455
2026.612997	67.324628	61.721460
2026.073079	75.253688	61.726465
2025.600802	61.677556	61.731470
2024.732786	68.395605	61.736474
2023.604670	77.401993	61.741479
2023.297236	65.110084	61.746484
2022.822354	64.215638	61.751489
2021.865217	71.444551	61.756494
2021.004109	69.599046	61.761498
2019.876994	77.756915	61.766503
2019.412898	69.881483	61.771508
2018.955476	72.450249	61.776513
2018.509018	80.834390	61.781518
2018.181272	78.779660	61.786522
2017.417373	66.093442	61.791527
2016.758411	71.939414	61.796532
2015.815940	68.219299	61.801537
2014.811882	74.359731	61.806542
2014.346496	66.594887	61.811546
2013.912707	65.148320	61.816551
2013.422367	72.150190	61.821556
2013.058640	76.046013	61.826561
2012.018971	69.525016	61.831566
2010.704914	67.669407	61.836570
2010.192523	72.598027	61.841575
2009.741067	68.041503	61.846580
2009.194944	67.404359	61.851585
2008.697865	71.562608	61.856590
2008.495507	58.938655	61.861594
2007.316769	74.457709	61.866599
2006.379064	61.121027	61.871604
2005.865372	60.568619	61.876609
2004.988078	74.052962	61.881614
2004.645210	60.077847	61.886618
2004.406702	67.358275	61.891623
2003.847902	66.652185	61.896628
2002.767222	63.826027	61.901633
2001.814986	62.586323	61.906638
2001.364566	63.351606	61.911642
2000.368154	64.287123	61.916647
2000.357827	56.560444	61.921652
1999.749942	71.083762	61.926657
1998.642200	65.087641	61.931662
1998.168590	71.733637	61.936666
1996.943592	73.394534	61.941671
1996.735556	69.400168	61.946676
1996.269486	70.235741	61.951681
1995.678593	75.232015	61.956686
1994.758607	71.908866	61.961690
1993.673837	62.305932	61.966695
1993.337409	70.377728	61.971700
1992.745695	67.917067	61.976705
1992.143125	64.471003	61.981710
1992.088979	62.729227	61.986714
1990.489115	72.580018	61.991719
1989.733870	71.298012	61.996724
1989.194424	66.265049	62.001729
1988.613907	73.643919	62.006734
1988.554253	68.416534	62.011738
1987.856885	79.097017	62.016743
1987.005737	62.473001	62.021748
1985.992742	69.381222	62.026753
1985.515444	67.977833	62.031758
1985.163798	63.017561	62.036762
1984.034847	68.156006	62.041767
1983.729461	66.592873	62.046772
1982.776529	62.242104	62.051777
1982.175988	66.995493	62.056782
1981.620661	72.367727	62.061786
1980.978422	64.334512	62.066791
1980.697077	69.324228	62.071796
1979.486767	64.525480	62.076801
1978.384038	72.969636	62.081806
1977.755737	51.936001	62.086810
1977.336607	76.395236	62.091815
1976.851133	70.610997	62.096820
1976.596366	75.818837	62.101825
1976.237671	71.608700	62.106830
1975.346760	66.767140	62.111834
1974.208553	67.990090	62.116839
1973.795217	66.251714	62.121844
1973.153989	63.589193	62.126849
1972.373244	69.948067	62.131854
1971.414120	71.358625	62.136858
1970.315039	65.652866	62.141863
1969.821596	66.995813	62.146868
1969.372332	66.786406	62.151873
1968.735257	69.069897	62.156878
1968.673148	60.726993	62.161882
1968.092436	77.243912	62.166887
1967.532608	63.990762	62.171892
1966.569283	70.569422	62.176897
1965.635526	63.492345	62.181902
1965.545909	66.942555	62.186906
1964.594279	66.407633	62.191911
1963.607687	69.665926	62.196916
1962.734817	66.251736	62.201921
1962.103414	57.496177	62.206926
1961.617307	63.958086	62.211930
1961.053735	64.509535	62.216935
1960.298734	69.943428	62.221940
1960.116707	64.604591	62.226945
1959.057266	65.591127	62.231950
1958.549350	62.150547	62.236954
1957.535465	70.090196	62.241959
1957.219283	55.708759	62.246964
1956.982737	69.473000	62.251969
1955.935653	67.338510	62.256974
1954.919703	62.870028	62.261978
1954.191132	66.908919	62.266983
1953.763392	69.026726	62.271988
1953.407814	61.427389	62.276993
1952.841397	71.320722	62.281998
1951.811278	58.468650	62.287002
1950.570875	74.114197	62.292007
1950.253728	61.841197	62.297012
1949.705631	69.520837	62.302017
1949.355575	71.626314	62.307022
1949.220369	63.851652	62.312026
1948.234937	68.003855	62.317031
1947.355447	59.822243	62.322036
1946.872782	70.482836	62.327041
1945.998196	59.241301	62.332046
1945.318928	65.222965	62.337050
1944.053915	59.720172	62.342055
1943.632203	65.824947	62.347060
1943.170580	63.920786	62.352065
1942.627168	63.298995	62.357070
1942.269338	59.777827	62.362074
1941.466441	59.488950	62.367079
1940.911411	59.671635	62.372084
1939.966540	65.954071	62.377089
1938.802093	65.653206	62.382094
1938.664927	59.619733	62.387098
1937.843293	64.096004	62.392103
1937.909823	65.681209	62.397108
1936.968707	56.966939	62.402113
1935.914247	73.700979	62.407118
1935.237167	65.234937	62.412122
1934.821285	60.056225	62.417127
1934.100043	65.596721	62.422132
1933.017054	57.111546	62.427137
1932.252461	63.608204	62.432142
1931.775271	60.446591	62.437146
1930.895109	65.266453	62.442151
1930.971322	59.645365	62.447156
1930.506836	63.386884	62.452161
1929.751565	73.209280	62.457166
1928.820210	64.105548	62.462170
1928.284539	58.685669	62.467175
1927.695932	66.245592	62.472180
1927.266532	61.039066	62.477185
1925.765622	60.252328	62.482190
1925.205508	68.230331	62.487194
1924.504009	60.736376	62.492199
1924.019364	58.328119	62.497204
1923.437424	64.527714	62.502209
1922.847469	71.048691	62.507214
1922.495461	58.781235	62.512218
1921.623072	66.848234	62.517223
1920.866661	64.151975	62.522228
1920.614805	67.588518	62.527233
1919.685028	68.634907	62.532238
1918.906770	61.086910	62.537242
1918.242178	69.925131	62.542247
1917.608403	68.177607	62.547252
1917.274094	60.235873	62.552257
1916.054590	70.188735	62.557262
1915.261480	50.318225	62.562266
1914.591453	56.836140	62.567271
1914.319476	67.745547	62.572276
1913.942947	58.430748	62.577281
1913.029839	53.581703	62.582286
1912.085547	61.135016	62.587290
1911.425345	57.767507	62.592295
1910.994200	53.414355	62.597300
1910.622095	57.327281	62.602305
1909.370463	58.159853	62.607310
1908.832796	48.407042	62.612314
1908.067855	66.208391	62.617319
1907.634028	58.463800	62.622324
1907.174559	55.964822	62.627329
1906.621960	72.582926	62.632334
1905.637336	57.285803	62.637338
1904.642704	59.030010	62.642343
1903.806189	60.209824	62.647348
1903.679713	58.570994	62.652353
1902.961574	65.249510	62.657358
1902.686433	56.713366	62.662362
1901.889853	55.906283	62.667367
1900.835179	54.684457	62.672372
1900.406800	58.636279	62.677377
1899.829630	58.999098	62.682382
1899.768446	58.639787	62.687386
1898.587396	62.834099	62.692391
1897.440819	68.956193	62.697396
1897.203443	61.096840	62.702401
1896.272954	66.564914	62.707406
1896.208414	57.601117	62.712410
1895.288714	51.710810	62.717415
1894.413015	59.445616	62.722420
1894.089939	53.861116	62.727425
1892.528085	62.551641	62.732430
1892.043968	57.642380	62.737434
1891.458566	49.369955	62.742439
1890.665352	57.872219	62.747444
1890.549571	66.807808	62.752449
1889.686447	59.888278	62.757454
1889.805020	61.621329	62.762458
1888.937576	57.520366	62.767463
1887.876514	74.214466	62.772468
1887.356953	60.177555	62.777473
1886.470367	68.300431	62.782478
1885.867488	57.917761	62.787482
1884.560573	65.057169	62.792487
1884.064838	57.879051	62.797492
1883.445687	59.719764	62.802497
1882.680164	63.048635	62.807502
1882.582244	58.620508	62.812506
1881.988239	52.241703	62.817511
1881.672727	55.776657	62.822516
1881.423646	55.734170	62.827521
1880.055750	64.477483	62.832526
1879.605937	41.882846	62.837530
1878.666952	57.288163	62.842535
1877.772653	66.599653	62.847540
1877.243797	47.414152	62.852545
1876.512184	61.641738	62.857550
1876.240216	52.111666	62.862554
1875.712967	70.324696	62.867559
1874.620420	55.221337	62.872564
1873.910143	47.098049	62.877569
1873.108603	59.029767	62.882574
1872.861251	55.147312	62.887578
1871.979495	50.488839	62.892583
1871.037434	55.074127	62.897588
1870.586228	51.435341	62.902593
1869.798744	58.897539	62.907598
1870.144132	56.688654	62.912602
1868.865625	59.581759	62.917607
1867.935159	49.741521	62.922612
1867.601642	53.224144	62.927617
1866.792840	59.412459	62.932622
1866.510578	49.951830	62.937626
1865.190860	57.470148	62.942631
1864.351519	50.840156	62.947636
1864.365344	46.362754	62.952641
1863.299337	51.536974	62.957646
1863.017016	50.265073	62.962650
1861.863013	53.139988	62.967655
1861.073471	53.839294	62.972660
1860.643625	42.773191	62.977665
1860.033231	58.255645	62.982670
1859.725376	51.506577	62.987674
1858.896824	48.489075	62.992679
1857.819019	56.667542	62.997684
1857.600297	49.888555	63.002689
1856.751177	62.499582	63.007694
1856.492656	58.161608	63.012698
1855.162199	54.094751	63.017703
1854.232335	52.189264	63.022708
1854.084228	47.928375	63.027713
1853.378641	60.854063	63.032718
1853.130056	35.871643	63.037722
1852.669858	53.410141	63.042727
1851.555270	53.311123	63.047732
1851.013508	44.498801	63.052737
1850.237354	60.468024	63.057742
1849.759848	50.117504	63.062746
1848.862724	59.629708	63.067751
1847.947676	62.712683	63.072756
1847.590339	46.365148	63.077761
1847.018652	54.922128	63.082766
1846.551763	51.520791	63.087770
1845.226755	61.113551	63.092775
1844.565234	61.462968	63.097780
1844.326103	46.444894	63.102785
1843.824214	48.184998	63.107790
1843.588247	50.149372	63.112794
1842.303215	49.605935	63.117799
1841.222745	57.035815	63.122804
1840.993008	52.677506	63.127809
1840.417107	55.217801	63.132814
1839.853573	48.353225	63.137818
1839.067618	56.245673	63.142823
1838.003236	60.489290	63.147828
1837.515725	46.698043	63.152833
1836.843606	50.095667	63.157838
1836.635995	54.526502	63.162842
1835.525284	57.452900	63.167847
1834.705305	46.637973	63.172852
1834.667458	50.775360	63.177857
1833.978909	61.047619	63.182862
1833.267112	51.183713	63.187866
1831.943832	47.771712	63.192871
1831.211128	49.695118	63.197876
1831.121241	48.080444	63.202881
1830.472663	60.022574	63.207886
1830.010848	46.528433	63.212890
1829.197280	57.772974	63.217895
1828.141181	53.310925	63.222900
1827.758618	61.577697	63.227905
1827.050389	63.773173	63.232910
1826.852515	59.693642	63.237914
1825.802383	51.815135	63.242919
1824.712929	60.607292	63.247924
1824.434110	59.121960	63.252929
1823.703404	61.186971	63.257934
1823.484939	62.809540	63.262938
1822.842817	57.557973	63.267943
1821.950864	61.980787	63.272948
1821.665920	55.477233	63.277953
1820.578357	62.074082	63.282958
1819.653593	59.628505	63.287962
1818.852571	46.356956	63.292967
1818.226872	61.037640	63.297972
1817.843929	63.700258	63.302977
1817.413324	65.804346	63.307982
1816.932481	62.547148	63.312986
1815.999420	67.110527	63.317991
1815.367499	62.626856	63.322996
1814.864056	64.387713	63.328001
1813.283369	68.101497	63.333006
1812.531965	61.807624	63.338010
1812.399700	62.221233	63.343015
1811.604572	68.692808	63.348020
1811.232727	56.433265	63.353025
1810.786209	67.750412	63.358030
1810.421921	60.838432	63.363034
1809.311145	54.844466	63.368039
1808.213928	61.906453	63.373044
1808.336123	56.803168	63.378049
1807.446585	64.546504	63.383054
1807.023931	59.006213	63.388058
1805.871591	53.211229	63.393063
1805.365308	63.680044	63.398068
1805.229141	59.444068	63.403073
1803.860134	63.518461	63.408078
1803.253570	56.148240	63.413082
1802.811702	50.506932	63.418087
1801.966224	64.933952	63.423092
1801.175599	55.964047	63.428097
1800.353259	62.091454	63.433102
1799.720669	66.190829	63.438106
1799.226561	60.732846	63.443111
1798.465874	65.508543	63.448116
1798.383565	54.931283	63.453121
1797.697586	68.416815	63.458126
1796.620064	63.187088	63.463130
1796.055613	64.199159	63.468135
1795.364916	66.812884	63.473140
1795.184273	48.510362	63.478145
1793.793210	65.627442	63.483150
1793.035595	64.547713	63.488154
1792.816914	49.777125	63.493159
1792.273908	49.413910	63.498164
1791.743380	63.108130	63.503169
1790.851077	70.224315	63.508174
1790.168530	57.418056	63.513178
1789.733259	59.257973	63.518183
1788.731878	61.887922	63.523188
1787.602500	54.488771	63.528193
1786.995262	66.903717	63.533198
1786.308815	55.682841	63.538202
1786.291740	53.239785	63.543207
1785.684934	56.923502	63.548212
1785.536141	53.812269	63.553217
1784.306119	55.915583	63.558222
1783.623687	62.884903	63.563226
1783.235654	52.879720	63.568231
1781.889732	58.366490	63.573236
1781.593085	52.929193	63.578241
1780.683996	53.860385	63.583246
1780.329836	46.645626	63.588250
1779.982390	51.645844	63.593255
1778.824681	63.648335	63.598260
1778.321151	59.521160	63.603265
1777.508069	61.148277	63.608270
1777.385674	52.255184	63.613274
1776.431808	60.753025	63.618279
1775.024853	61.809013	63.623284
1774.733526	53.308581	63.628289
1774.080332	60.817281	63.633294
1773.970945	53.983097	63.638298
1773.125063	58.710829	63.643303
1771.831120	69.530230	63.648308
1771.212441	51.502267	63.653313
1770.734591	55.140277	63.658318
1770.253503	53.117823	63.663322
1770.196540	45.825909	63.668327
1769.252186	53.664682	63.673332
1768.496576	54.722884	63.678337
1767.951779	59.079544	63.683342
1767.355977	61.132606	63.688346
1766.458428	55.910582	63.693351
1765.800536	53.807403	63.698356
1765.349588	52.153883	63.703361
1764.079416	55.666999	63.708366
1763.006147	45.628729	63.713370
1762.897976	53.752581	63.718375
1762.201401	69.870027	63.723380
1761.875210	59.519149	63.728385
1761.498240	58.336404	63.733390
1760.772005	57.228049	63.738394
1759.909815	59.427491	63.743399
1758.996308	61.046910	63.748404
1758.486880	52.905955	63.753409
1757.031424	56.839565	63.758414
1756.549163	52.934512	63.763418
1756.214354	55.040740	63.768423
1755.717281	64.877347	63.773428
1755.501297	50.464290	63.778433
1754.921714	57.243823	63.783438
1753.953535	57.815420	63.788442
1753.179205	58.138623	63.793447
1752.187239	61.195999	63.798452
1752.010866	61.381662	63.803457
1751.652054	45.781831	63.808462
1750.373512	54.082093	63.813466
1749.954669	52.973806	63.818471
1749.408890	59.549286	63.823476
1748.351158	51.629449	63.828481
1747.303733	59.812589	63.833486
1746.716134	55.164214	63.838490
1746.674494	63.216006	63.843495
1745.596226	65.304698	63.848500
1745.836151	48.354584	63.853505
1744.819923	48.463907	63.858510
1743.992690	58.147952	63.863514
1743.280469	57.702817	63.868519
1742.909444	63.129389	63.873524
1741.895909	52.972833	63.878529
1741.031150	46.804222	63.883534
1740.324011	50.494419	63.888538
1740.207297	52.936576	63.893543
1739.594117	52.278603	63.898548
1738.621201	47.754503	63.903553
1737.705612	55.222882	63.908558
1736.739450	57.891407	63.913562
1736.893323	46.970738	63.918567
1736.244436	60.029354	63.923572
1734.997828	55.588143	63.928577
1734.192841	67.086798	63.933582
1733.648025	61.105478	63.938586
1733.523561	54.784600	63.943591
1733.049073	54.765312	63.948596
1732.771692	45.160445	63.953601
1731.270731	58.146240	63.958606
1730.627014	55.329648	63.963610
1730.382602	43.644380	63.968615
1729.141516	57.645406	63.973620
1728.632062	50.330748	63.978625
1727.911659	58.047237	63.983630
1727.258065	55.300021	63.988634
1727.182351	54.690723	63.993639
1726.093143	62.393254	63.998644
1725.419463	55.904152	64.003649
1724.914741	56.979287	64.008654
1724.013403	51.693232	64.013658
1723.482825	50.306244	64.018663
1722.458984	58.463569	64.023668
1721.970913	52.974689	64.028673
1721.408589	54.323888	64.033678
1720.771382	57.250816	64.038682
1719.877631	56.670524	64.043687
1719.122259	56.525548	64.048692
1718.708894	53.475265	64.053697
1717.886166	58.429558	64.058702
1717.757149	62.136746	64.063706
1717.380888	43.896858	64.068711
1716.361252	54.453516	64.073716
1715.572144	65.672122	64.078721
1714.938566	63.140914	64.083726
1714.216543	57.257128	64.088730
1713.568270	54.002895	64.093735
1712.524793	62.186997	64.098740
1712.163185	53.467518	64.103745
1711.558077	56.925486	64.108750
1711.039863	62.979381	64.113754
1710.215316	60.191515	64.118759
1709.612831	65.281134	64.123764
1709.245205	63.204402	64.128769
1708.212480	58.254593	64.133774
1707.415918	55.974769	64.138778
1707.179381	55.416245	64.143783
1706.372886	58.250222	64.148788
1705.864144	58.684212	64.153793
1704.539507	57.899565	64.158798
1704.174077	57.487664	64.163802
1703.919245	51.096039	64.168807
1703.349390	58.993616	64.173812
1701.890021	54.802247	64.178817
1701.331094	64.177198	64.183822
1700.990869	56.663785	64.188826
1700.646002	50.590799	64.193831
1699.630683	67.840611	64.198836
1699.082737	55.618531	64.203841
1698.064604	57.882184	64.208846
1697.360803	50.002345	64.213850
1697.158707	62.542169	64.218855
1696.652353	58.164739	64.223860
1695.636963	53.191685	64.228865
1694.915847	51.678857	64.233870
1694.705282	52.196368	64.238874
1694.001132	39.899771	64.243879
1692.546673	54.519717	64.248884
1691.974809	49.370567	64.253889
1691.684567	57.513876	64.258894
1691.277734	62.711185	64.263898
1691.131904	55.885952	64.268903
1689.769397	61.730196	64.273908
1689.074756	50.600546	64.278913
1688.511820	64.883363	64.283918
1687.621352	63.367475	64.288922
1686.902474	58.527089	64.293927
1685.831764	63.528666	64.298932
1685.370128	55.465291	64.303937
1684.914890	57.596962	64.308942
1684.750821	64.122861	64.313946
1684.563051	59.333726	64.318951
1683.530937	63.674770	64.323956
1682.506158	55.051174	64.328961
1682.038602	58.460493	64.333966
1680.971586	65.377386	64.338970
1680.381375	57.651386	64.343975
1679.304454	60.332794	64.348980
1679.000003	59.594259	64.353985
1678.909384	61.101917	64.358990
1677.959690	59.934468	64.363994
1677.216341	50.613349	64.368999
1676.131711	56.933826	64.374004
1676.262436	54.893053	64.379009
1675.623097	65.086562	64.384014
1674.287062	59.633041	64.389018
1673.809506	49.653147	64.394023
1673.143712	63.286862	64.399028
1672.806412	57.037643	64.404033
1672.421880	47.790411	64.409038
1670.886416	59.966472	64.414042
1670.667148	56.948441	64.419047
1670.059969	58.840912	64.424052
1669.753253	52.867521	64.429057
1668.483450	62.096786	64.434062
1667.831375	63.058151	64.439066
1667.600646	46.966514	64.444071
1666.252484	55.033453	64.449076
1665.371574	60.375452	64.454081
1665.182917	53.240076	64.459086
1664.374816	55.766829	64.464090
1664.333578	55.164672	64.469095
1664.069039	63.590892	64.474100
1663.056786	58.571624	64.479105
1662.376407	56.479929	64.484110
1661.397149	58.647538	64.489114
1660.209663	47.028515	64.494119
1659.466412	58.826438	64.499124
1659.106768	49.825978	64.504129
1658.598926	55.988610	64.509134
1658.179628	56.607086	64.514138
1658.146693	58.338959	64.519143
1656.902130	56.199698	64.524148
1656.314025	55.998209	64.529153
1655.785168	62.954196	64.534158
1654.423506	63.687677	64.539162
1653.972782	52.296953	64.544167
1653.128193	55.532791	64.549172
1652.992948	49.505359	64.554177
1652.306439	54.289803	64.559182
1651.025494	55.787862	64.564186
1650.483414	52.365398	64.569191
1649.668081	59.142975	64.574196
1649.442234	54.339396	64.579201
1649.519779	52.072116	64.584206
1648.246351	52.159258	64.589210
1647.747929	55.914089	64.594215
1646.569600	57.309121	64.599220
1646.200536	48.964563	64.604225
1645.781810	50.015013	64.609230
1644.776196	53.774723	64.614234
1644.269623	50.017055	64.619239
1643.672363	61.282461	64.624244
1642.961589	50.097047	64.629249
1642.149087	50.166162	64.634254
1641.429325	55.715944	64.639258
1640.801506	52.420637	64.644263
1640.194976	63.465179	64.649268
1639.395110	56.838463	64.654273
1638.739068	64.016496	64.659278
1637.825868	62.633541	64.664282
1637.708589	55.499443	64.669287
1637.149951	64.197877	64.674292
1636.431327	54.395051	64.679297
1635.499186	51.916026	64.684302
1635.057597	59.701777	64.689306
1634.552534	53.709441	64.694311
1633.368678	66.753715	64.699316
1632.418607	42.398442	64.704321
1632.019816	58.031788	64.709326
1631.464369	56.338126	64.714330
1631.380931	58.193133	64.719335
1630.698487	64.432393	64.724340
1629.758677	58.102287	64.729345
1629.214622	55.312467	64.734350
1628.473316	60.061471	64.739354
1627.592902	60.040459	64.744359
1626.799414	62.493944	64.749364
1626.088281	57.571928	64.754369
1625.748380	61.650069	64.759374
1625.217375	60.851342	64.764378
1624.585506	55.729088	64.769383
1623.336887	57.081683	64.774388
1623.210731	55.340324	64.779393
1622.873964	57.164616	64.784398
1621.090641	56.246311	64.789402
1620.701396	61.811397	64.794407
1620.195596	59.499601	64.799412
1619.550299	52.395777	64.804417
1619.452922	61.095046	64.809422
1618.922918	66.269355	64.814426
1618.330892	48.648793	64.819431
1617.164564	55.836934	64.824436
1616.425021	59.874491	64.829441
1615.548199	60.737538	64.834446
1614.541311	62.406531	64.839450
1614.330617	53.986358	64.844455
1613.696231	55.856356	64.849460
1613.403616	51.686254	64.854465
1613.051468	58.839664	64.859470
1611.770030	60.385126	64.864474
1611.114023	54.661192	64.869479
1610.414294	59.290059	64.874484
1609.996997	58.336084	64.879489
1609.172974	51.929251	64.884494
1608.004290	59.076772	64.889498
1608.076555	62.289960	64.894503
1607.096455	68.792546	64.899508
1606.655977	65.711898	64.904513
1605.615513	51.896616	64.909518
1604.911148	61.107033	64.914522
1604.495290	70.419847	64.919527
1603.961721	65.554777	64.924532
1603.572658	44.830234	64.929537
1602.630641	55.163291	64.934542
1601.867638	63.187757	64.939546
1601.308865	51.189775	64.944551
1600.929649	68.346432	64.949556
1599.687510	65.169231	64.954561
1599.045592	48.121125	64.959566
1598.444812	53.208911	64.964570
1598.260588	52.539591	64.969575
1597.632580	55.414623	64.974580
1596.382146	55.532829	64.979585
1596.361925	46.095281	64.984590
1595.613435	55.159750	64.989594
1594.623332	42.172224	64.994599
1593.774290	60.769085	64.999604
1593.033567	61.812357	65.004609
1592.856543	57.075140	65.009614
1591.971954	57.508943	65.014618
1591.357228	44.649426	65.019623
1590.330181	55.391790	65.024628
1589.676778	53.327367	65.029633
1589.449097	63.871778	65.034638
1588.896483	64.352182	65.039642
1588.279863	59.971798	65.044647
1587.181506	49.626959	65.049652
1586.484236	51.330344	65.054657
1586.482187	57.210787	65.059662
1585.462119	61.778598	65.064666
1584.672854	58.814869	65.069671
1584.055105	68.593399	65.074676
1583.621200	50.697004	65.079681
1582.846481	55.515977	65.084686
1581.890317	69.485985	65.089690
1580.941165	57.936361	65.094695
1580.404016	54.286061	65.099700
1580.200526	53.037938	65.104705
1579.853542	59.941383	65.109710
1578.997626	58.040019	65.114714
1578.307381	58.476063	65.119719
1577.667473	61.509102	65.124724
1576.708348	52.074077	65.129729
1575.879605	54.979430	65.134734
1575.284891	56.614488	65.139738
1575.014692	48.408773	65.144743
1574.526940	53.153770	65.149748
1573.898075	53.762980	65.154753
1573.030599	57.011938	65.159758
1572.534345	62.851061	65.164762
1571.808617	60.594717	65.169767
1570.571360	66.554729	65.174772
1570.242916	52.233696	65.179777
1569.613627	54.136009	65.184782
1568.810459	68.647807	65.189786
1567.983254	68.050687	65.194791
1567.019264	56.776227	65.199796
1566.817424	56.161745	65.204801
1566.368168	62.849642	65.209806
1565.831128	66.569625	65.214810
1565.246507	55.460384	65.219815
1564.397021	62.577706	65.224820
1563.694597	62.328173	65.229825
1563.210626	60.782434	65.234830
1562.108474	58.972236	65.239834
1561.503678	48.031779	65.244839
1560.693264	54.966281	65.249844
1560.328190	50.858160	65.254849
1560.046118	42.061435	65.259854
1558.746932	51.986073	65.264858
1558.679198	52.461978	65.269863
1557.760196	57.557759	65.274868
1556.942896	60.057621	65.279873
1555.977383	57.415203	65.284878
1555.294460	64.313686	65.289882
1555.013494	55.718617	65.294887
1554.379411	58.777541	65.299892
1553.965649	53.964411	65.304897
1553.183641	47.104672	65.309902
1552.145499	64.525284	65.314906
1551.839081	60.357382	65.319911
1551.568775	53.624483	65.324916
1550.210176	59.323097	65.329921
1549.270223	59.619062	65.334926
1548.691868	67.059144	65.339930
1548.634390	58.832243	65.344935
1548.281494	56.806811	65.349940
1547.260220	62.382448	65.354945
1546.621409	59.002184	65.359950
1545.895139	58.390611	65.364954
1545.245168	50.199514	65.369959
1544.220628	43.375164	65.374964
1543.135820	52.759571	65.379969
1543.158644	49.509135	65.384974
1542.610952	55.845261	65.389978
1542.349102	39.432199	65.394983
1541.219361	49.875516	65.399988
1540.586472	51.841482	65.404993
1539.948985	49.605820	65.409998
1538.989580	60.234956	65.415002
1537.940668	53.160600	65.420007
1537.222493	55.250499	65.425012
1536.837359	59.283798	65.430017
1536.693487	55.949467	65.435022
1536.259694	58.596544	65.440026
1535.978658	50.167065	65.445031
1534.628722	55.383363	65.450036
1533.963687	52.716863	65.455041
1533.055302	55.628576	65.460046
1531.949146	63.969344	65.465050
1531.491494	59.338223	65.470055
1531.158257	53.663947	65.475060
1530.492871	63.347553	65.480065
1530.681979	43.407909	65.485070
1529.450873	54.874959	65.490074
1528.713223	68.539034	65.495079
1528.199781	48.515487	65.500084
1527.085203	56.641559	65.505089
1526.527255	69.300998	65.510094
1525.829758	56.289077	65.515098
1525.424373	42.636270	65.520103
1525.155811	48.857083	65.525108
1524.112026	63.966907	65.530113
1523.686338	46.324687	65.535118
1522.714400	51.283816	65.540122
1521.706080	57.995900	65.545127
1520.884400	54.417634	65.550132
1520.071684	55.264218	65.555137
1519.722972	56.940617	65.560142
1519.217119	53.402048	65.565146
1519.074183	52.401338	65.570151
1518.580047	65.250896	65.575156
1517.505768	55.260215	65.580161
1517.026469	48.740298	65.585166
1516.316748	72.942892	65.590170
1515.563530	41.402149	65.595175
1514.427490	70.406243	65.600180
1513.834176	51.075021	65.605185
1513.428908	72.054997	65.610190
1512.841784	53.282579	65.615194
1511.572007	49.721909	65.620199
1511.144738	48.808958	65.625204
1510.592895	61.003821	65.630209
1510.455062	46.078541	65.635214
1509.789433	53.795828	65.640218
1508.819529	63.267644	65.645223
1508.295170	52.451607	65.650228
1507.765689	51.261601	65.655233
1507.310048	44.324789	65.660238
1505.901333	57.097336	65.665242
1505.183941	52.665186	65.670247
1505.151864	46.321774	65.675252
1504.035554	42.452886	65.680257
1503.550423	56.633460	65.685262
1502.805419	54.957336	65.690266
1502.475636	50.982383	65.695271
1501.612720	44.269556	65.700276
1500.366157	54.718838	65.705281
1499.683034	54.261263	65.710286
1499.079287	51.455731	65.715290
1498.877009	53.515694	65.720295
1498.581694	45.736588	65.725300
1498.212756	51.454564	65.730305
1497.527119	49.857313	65.735310
1496.438129	49.990910	65.740314
1495.469183	46.358791	65.745319
1494.685746	54.575746	65.750324
1493.974118	59.493520	65.755329
1493.646882	51.071391	65.760334
1492.932074	61.436178	65.765338
1492.242471	63.404861	65.770343
1491.517286	54.752672	65.775348
1490.755661	49.192211	65.780353
1490.533808	42.454782	65.785358
1489.852631	55.876499	65.790362
1489.178304	63.268764	65.795367
1488.158500	55.478637	65.800372
1487.420690	59.782441	65.805377
1487.496288	47.300510	65.810382
1486.141469	50.075036	65.815386
1485.548857	58.411473	65.820391
1484.919032	56.737549	65.825396
1484.362679	48.616748	65.830401
1484.070255	44.571211	65.835406
1482.873134	51.705948	65.840410
1482.480726	45.266845	65.845415
1481.978988	54.315775	65.850420
1481.293022	58.921984	65.855425
1480.501872	44.196726	65.860430
1479.874574	56.102397	65.865434
1479.235328	50.126697	65.870439
1478.107703	48.205474	65.875444
1477.359258	48.226616	65.880449
1477.141550	47.650932	65.885454
1476.713713	51.482874	65.890458
1476.056967	39.778044	65.895463
1474.908896	37.850612	65.900468
1474.110107	47.784062	65.905473
1474.001573	52.435693	65.910478
1473.562074	51.612996	65.915482
1472.655020	44.416789	65.920487
1471.526798	45.961621	65.925492
1470.974984	48.419315	65.930497
1470.550632	51.962137	65.935502
1469.639618	56.999908	65.940506
1468.588039	52.278699	65.945511
1467.976366	41.211647	65.950516
1467.805568	59.549353	65.955521
1467.630115	46.471845	65.960526
1466.776037	52.755754	65.965530
1466.114856	46.602206	65.970535
1465.335315	47.303192	65.975540
1464.697428	52.400053	65.980545
1464.235170	43.294532	65.985550
1462.630601	53.800724	65.990554
1462.269625	51.942162	65.995559
1461.931976	47.001847	66.000564
1461.665232	56.855481	66.005569
1460.584544	43.593853	66.010574
1459.788284	49.199981	66.015578
1459.114744	51.896208	66.020583
1458.981578	51.075289	66.025588
1458.018119	55.036512	66.030593
1457.028198	50.089479	66.035598
1456.238128	46.345374	66.040602
1456.013434	47.719810	66.045607
1455.940345	34.670199	66.050612
1454.722413	63.775606	66.055617
1454.187274	53.476937	66.060622
1453.314821	55.465227	66.065626
1452.706174	52.944322	66.070631
1451.451373	34.970313	66.075636
1450.774931	56.393883	66.080641
1450.355212	48.046384	66.085646
1450.049959	48.659382	66.090650
1449.718289	43.390131	66.095655
1448.599003	44.706483	66.100660
1447.807779	42.785425	66.105665
1447.498024	49.607267	66.110670
1446.889260	51.645108	66.115674
1446.149147	52.943775	66.120679
1445.894937	51.295316	66.125684
1444.787999	60.624933	66.130689
1444.393460	42.689228	66.135694
1443.508749	51.557766	66.140698
1442.627207	61.215817	66.145703
1442.244752	52.277377	66.150708
1441.550815	55.609174	66.155713
1440.532443	47.421476	66.160718
1439.405535	48.611317	66.165722
1439.059467	55.893072	66.170727
1438.755120	48.966920	66.175732
1438.096042	44.172308	66.180737
1437.969826	51.461694	66.185742
1437.152248	48.620782	66.190746
1436.092947	41.705819	66.195751
1435.683869	41.496426	66.200756
1434.692382	47.847909	66.205761
1433.972819	47.263687	66.210766
1433.380854	45.027127	66.215770
1432.933424	44.631452	66.220775
1432.617019	40.487240	66.225780
1431.698667	53.296988	66.230785
1431.149150	47.549881	66.235790
1430.292894	53.129285	66.240794
1429.061020	50.349492	66.245799
1428.501785	45.076992	66.250804
1427.803290	59.759813	66.255809
1427.866555	42.350562	66.260814
1427.568558	44.449395	66.265818
1426.455265	43.156666	66.270823
1425.876640	43.087757	66.275828
1424.979650	54.610543	66.280833
1424.134289	40.639790	66.285838
1423.314550	55.461720	66.290842
1422.129226	48.612520	66.295847
1422.436127	44.750841	66.300852
1421.741741	48.912144	66.305857
1421.515802	39.852652	66.310862
1420.113240	51.432139	66.315866
1419.171956	50.112073	66.320871
1419.186833	39.645584	66.325876
1418.610958	41.037995	66.330881
1417.647920	48.504538	66.335886
1416.784030	46.549309	66.340890
1416.544611	47.382069	66.345895
1415.984735	45.638704	66.350900
1414.948864	46.883468	66.355905
1414.068743	41.017037	66.360910
1413.459311	41.806112	66.365914
1413.339501	38.182559	66.370919
1412.811644	45.624084	66.375924
1411.300409	58.258432	66.380929
1410.916288	37.091665	66.385934
1410.409394	41.934335	66.390938
1409.797008	50.324380	66.395943
1408.982797	46.975192	66.400948
1407.957180	45.168668	66.405953
1407.763301	38.422077	66.410958
1406.992296	45.910135	66.415962
1406.852725	46.189314	66.420967
1406.202122	36.225975	66.425972
1404.704434	52.630032	66.430977
1404.346417	39.072234	66.435982
1403.971253	45.295803	66.440986
1403.290523	54.333768	66.445991
1402.655859	37.611019	66.450996
1401.848560	49.278814	66.456001
1401.494607	39.498545	66.461006
1400.142745	51.464199	66.466010
1399.465744	43.097690	66.471015
1399.387988	37.168382	66.476020
1398.535837	51.708474	66.481025
1398.215739	38.396950	66.486030
1397.226825	46.834230	66.491034
1396.414985	45.585056	66.496039
1395.965068	45.416852	66.501044
1394.844764	40.869022	66.506049
1394.222136	44.418139	66.511054
1393.645655	39.443265	66.516058
1393.383222	44.199775	66.521063
1392.964257	44.277374	66.526068
1391.944661	42.827849	66.531073
1391.161670	45.044774	66.536078
1390.612764	41.718074	66.541082
1389.722468	47.780689	66.546087
1389.627556	27.548784	66.551092
1388.391267	45.027709	66.556097
1388.095268	39.886835	66.561102
1387.655368	42.563284	66.566106
1386.372460	38.310950	66.571111
1386.056756	35.748231	66.576116
1385.069304	41.480954	66.581121
1384.664142	45.485911	66.586126
1384.075191	47.064902	66.591130
1382.998644	37.752717	66.596135
1382.332853	33.610439	66.601140
1381.791941	38.685588	66.606145
1381.482594	33.327654	66.611150
1380.958872	40.267080	66.616154
1379.786156	41.527302	66.621159
1379.447207	38.242921	66.626164
1378.676971	44.803665	66.631169
1378.552956	38.916403	66.636174
1377.176110	46.289471	66.641178
1376.185366	44.704486	66.646183
1376.005335	46.808225	66.651188
1375.521483	48.553428	66.656193
1375.130242	44.529923	66.661198
1373.681031	43.170773	66.666202
1373.168108	39.371605	66.671207
1372.830853	43.466688	66.676212
1372.475676	38.754670	66.681217
1371.236784	42.426982	66.686222
1370.588268	44.438044	66.691226
1370.367515	41.290985	66.696231
1369.784320	39.199696	66.701236
1368.444639	53.634377	66.706241
1367.529397	48.109417	66.711246
1367.149361	50.703819	66.716250
1366.895219	43.593094	66.721255
1366.614960	45.053636	66.726260
1365.468262	53.575930	66.731265
1365.185559	45.723887	66.736270
1364.490240	49.253029	66.741274
1363.396674	45.497280	66.746279
1362.551439	46.169318	66.751284
1361.995632	54.089933	66.756289
1361.633311	37.926272	66.761294
1361.321896	42.589650	66.766298
1360.076053	48.265693	66.771303
1359.446462	40.899281	66.776308
1358.675734	51.473234	66.781313
1358.532030	44.447451	66.786318
1357.543227	45.702101	66.791322
1356.434215	51.796341	66.796327
1356.137010	49.205454	66.801332
1355.396588	59.145426	66.806337
1355.477004	39.885376	66.811342
1354.355668	38.018402	66.816346
1353.521780	46.379013	66.821351
1353.361910	40.297192	66.826356
1352.359487	43.026801	66.831361
1351.196857	43.011325	66.836366
1350.763834	42.884596	66.841370
1350.077260	45.671223	66.846375
1349.707238	36.883795	66.851380
1349.043709	43.815491	66.856385
1348.322998	44.404664	66.861390
1347.885897	37.452333	66.866394
1346.921268	47.450017	66.871399
1346.638220	43.898147	66.876404
1345.555520	48.690447	66.881409
1344.745167	43.789032	66.886414
1344.363335	47.959010	66.891418
1344.003650	46.469250	66.896423
1343.104833	51.637574	66.901428
1342.210164	46.189775	66.906433
1341.958173	45.189069	66.911438
1341.290637	47.710912	66.916442
1339.850059	40.626387	66.921447
1339.476658	40.720404	66.926452
1338.741836	65.863635	66.931457
1338.362092	39.620259	66.936462
1338.152360	44.027791	66.941466
1337.163317	52.066164	66.946471
1336.493424	37.737997	66.951476
1335.990808	52.004925	66.956481
1335.013366	36.910412	66.961486
1334.151279	46.021367	66.966490
1333.382254	51.746193	66.971495
1333.386835	28.978652	66.976500
1332.639093	50.191213	66.981505
1331.829337	51.937775	66.986510
1331.123762	47.704067	66.991514
1330.589232	53.948249	66.996519
1330.456580	47.578264	67.001524
1328.994423	54.146526	67.006529
1328.291440	46.006510	67.011534
1327.803436	42.517187	67.016538
1327.115018	53.227864	67.021543
1326.752169	40.486096	67.026548
1325.590854	41.282508	67.031553
1324.896280	43.360823	67.036558
1324.391572	42.266262	67.041562
1324.222506	50.790834	67.046567
1323.156913	41.704005	67.051572
1322.358044	37.576593	67.056577
1321.888263	46.175776	67.061582
1321.679649	41.487772	67.066586
1320.569439	47.350415	67.071591
1319.433608	37.503670	67.076596
1319.114686	39.429230	67.081601
1319.151955	37.173084	67.086606
1318.152686	37.978429	67.091610
1317.055155	37.067998	67.096615
1316.948994	45.741830	67.101620
1316.167473	46.372216	67.106625
1315.081066	32.349965	67.111630
1314.317305	34.596968	67.116634
1313.448944	49.689974	67.121639
1313.309705	24.816541	67.126644
1312.553582	48.972861	67.131649
1312.211096	40.143217	67.136654
1311.274895	28.514426	67.141658
1310.674542	31.725720	67.146663
1310.463498	30.127184	67.151668
1309.452529	45.655998	67.156673
1308.608186	44.235412	67.161678
1308.032177	40.328024	67.166682
1307.120754	45.736468	67.171687
1306.697553	30.937038	67.176692
1305.492509	54.243850	67.181697
1305.051453	36.758698	67.186702
1304.833388	34.655105	67.191706
1304.186821	34.803594	67.196711
1303.820797	35.021016	67.201716
1302.811528	39.990878	67.206721
1302.082921	42.990767	67.211726
1301.811679	42.142928	67.216730
1300.627268	42.927255	67.221735
1299.868388	26.744678	67.226740
1299.269494	32.778327	67.231745
1298.753103	28.456213	67.236750
1298.496537	33.268559	67.241754
1297.780244	39.954776	67.246759
1297.240464	29.559146	67.251764
1296.352028	38.048280	67.256769
1295.138547	37.091642	67.261774
1294.717255	38.047940	67.266778
1293.826826	37.806297	67.271783
1293.807246	35.540269	67.276788
1292.775545	41.764154	67.281793
1292.076357	39.931010	67.286798
1291.884346	36.801468	67.291802
1291.004134	44.655400	67.296807
1289.866816	42.390472	67.301812
1288.951045	37.836982	67.306817
1288.698076	39.083469	67.311822
1288.429711	33.296437	67.316826
1287.977627	37.562738	67.321831
1287.181017	38.375294	67.326836
1286.000791	43.542645	67.331841
1285.847461	41.925473	67.336846
1285.120893	32.057833	67.341850
1283.933741	42.789461	67.346855
1283.280686	32.467034	67.351860
1282.871842	31.347779	67.356865
1282.722560	37.853966	67.361870
1281.611870	39.959030	67.366874
1280.643041	45.242574	67.371879
1280.261494	36.854365	67.376884
1279.525062	43.215802	67.381889
1279.111077	35.031437	67.386894
1278.178589	34.228816	67.391898
1277.307403	45.268158	67.396903
1277.077950	38.180333	67.401908
1276.564452	37.656428	67.406913
1275.645650	47.123325	67.411918
1274.926359	51.096245	67.416922
1274.179129	47.838950	67.421927
1274.006429	44.610149	67.426932
1273.120125	33.364501	67.431937
1271.980751	33.816846	67.436942
1271.423324	42.879373	67.441946
1270.797310	46.200408	67.446951
1270.637877	34.030258	67.451956
1269.578925	42.772004	67.456961
1268.726635	40.132203	67.461966
1268.314952	40.281200	67.466970
1267.916805	55.237958	67.471975
1267.563658	39.187979	67.476980
1266.569050	39.071713	67.481985
1265.666267	49.149467	67.486990
1265.439584	43.470918	67.491994
1264.262925	49.090273	67.496999
1263.748994	40.000911	67.502004
1263.204949	45.565407	67.507009
1262.588607	44.200042	67.512014
1261.825531	28.500669	67.517018
1260.550510	41.327733	67.522023
1260.387885	40.207176	67.527028
1259.748891	40.967873	67.532033
1259.363026	42.308029	67.537038
1259.341560	31.136177	67.542042
1257.905212	42.482991	67.547047
1257.692742	32.016407	67.552052
1255.966498	37.817759	67.557057
1255.564715	33.556274	67.562062
1255.191744	38.298827	67.567066
1254.501204	39.758388	67.572071
1254.255274	19.903760	67.577076
1253.078583	48.018646	67.582081
1252.048025	49.253168	67.587086
1252.000534	45.920886	67.592090
1251.217147	49.935540	67.597095
1250.990726	52.568604	67.602100
1249.768316	49.639172	67.607105
1249.159644	41.080514	67.612110
1248.867196	35.350931	67.617114
1247.517474	43.222762	67.622119
1246.950594	46.313638	67.627124
1246.170464	47.293888	67.632129
1245.953880	45.566935	67.637134
1245.837061	36.395515	67.642138
1244.788966	33.312223	67.647143
1243.912105	48.930110	67.652148
1243.626919	41.505818	67.657153
1242.587845	47.079650	67.662158
1241.825762	33.762764	67.667162
1240.656989	56.231242	67.672167
1240.771389	44.243038	67.677172
1240.100096	45.761039	67.682177
1239.212020	40.630764	67.687182
1238.871977	45.104749	67.692186
1237.673575	43.746794	67.697191
1237.551353	41.534932	67.702196
1237.036023	41.531691	67.707201
1235.936090	37.187270	67.712206
1235.043716	34.273174	67.717210
1234.475055	45.095695	67.722215
1234.663139	42.861297	67.727220
1233.424915	41.814012	67.732225
1232.779629	43.004623	67.737230
1232.093905	44.149628	67.742234
1231.327059	47.428414	67.747239
1230.810048	45.671968	67.752244
1229.632657	38.600854	67.757249
1229.055607	33.675002	67.762254
1228.912621	48.070814	67.767258
1228.479203	41.690327	67.772263
1227.914977	29.729628	67.777268
1226.766216	49.306105	67.782273
1225.828028	42.192223	67.787278
1225.582972	43.393305	67.792282
1224.340752	52.239903	67.797287
1223.810909	35.281382	67.802292
1223.176741	40.134856	67.807297
1222.829430	51.344784	67.812302
1222.755688	35.775488	67.817306
1221.606606	51.569127	67.822311
1220.889133	40.205193	67.827316
1220.126636	21.504984	67.832321
1219.666149	61.756651	67.837326
1218.961463	37.227020	67.842330
1218.120513	39.557283	67.847335
1217.572749	33.685390	67.852340
1217.271073	33.370650	67.857345
1216.180835	36.871165	67.862350
1215.184471	30.687433	67.867354
1214.627204	36.755477	67.872359
1214.018154	45.108749	67.877364
1213.931194	14.894102	67.882369
1212.623069	57.488152	67.887374
1212.056227	24.818928	67.892378
1211.605407	44.886775	67.897383
1211.555636	39.456054	67.902388
1210.113145	37.327999	67.907393
1209.189029	27.644762	67.912398
1209.029799	30.142568	67.917402
1208.343396	50.454454	67.922407
1208.110318	32.316562	67.927412
1207.438391	37.513491	67.932417
1206.444485	50.615982	67.937422
1205.621791	35.307710	67.942426
1204.561166	30.618029	67.947431
1204.101152	34.308470	67.952436
1203.326314	53.027601	67.957441
1203.221993	31.791197	67.962446
1202.583601	39.471083	67.967450
1201.541155	45.047041	67.972455
1200.952261	42.764323	67.977460
1200.767659	34.177669	67.982465
1199.574957	48.838176	67.987470
1198.716676	36.115314	67.992474
1197.990161	33.681030	67.997479
1197.706045	50.792564	68.002484
1197.661902	42.416944	68.007489
1196.410252	41.780220	68.012494
1195.702882	39.461155	68.017498
1195.032385	39.487328	68.022503
1194.762760	44.558788	68.027508
1193.708517	51.998903	68.032513
1192.842789	40.707440	68.037518
1192.683681	33.141693	68.042522
1191.951759	40.804919	68.047527
1190.866392	29.179409	68.052532
1190.284507	38.018764	68.057537
1189.587484	44.219421	68.062542
1189.321294	27.382988	68.067546
1188.780664	41.837296	68.072551
1188.000163	45.737972	68.077556
1187.222888	39.801665	68.082561
1186.766702	30.968063	68.087566
1185.746700	36.155700	68.092570
1184.657256	44.404035	68.097575
1184.302212	45.802374	68.102580
1183.810722	42.796159	68.107585
1183.274626	36.791539	68.112590
1182.837937	36.206555	68.117594
1181.410288	42.387797	68.122599
1181.283285	42.541994	68.127604
1180.688342	34.697074	68.132609
1180.030588	37.196898	68.137614
1179.410724	39.875190	68.142618
1178.638851	49.976299	68.147623
1178.104167	41.243480	68.152628
1176.823581	43.236844	68.157633
1175.738609	49.149140	68.162638
1175.406987	31.194078	68.167642
1174.873331	48.165532	68.172647
1174.943444	40.047696	68.177652
1174.571148	39.143407	68.182657
1173.706484	43.760752	68.187662
1173.038521	38.871448	68.192666
1172.167083	37.049966	68.197671
1171.169474	45.001442	68.202676
1170.260071	36.331378	68.207681
1169.118432	39.647710	68.212686
1169.128360	39.133616	68.217690
1168.629005	46.271034	68.222695
1168.482351	37.213173	68.227700
1167.544288	37.326060	68.232705
1166.413330	41.208365	68.237710
1166.299495	43.721031	68.242714
1165.759382	37.095771	68.247719
1164.740130	37.049693	68.252724
1164.034740	38.787588	68.257729
1163.585328	42.714457	68.262734
1162.814857	37.204407	68.267738
1161.891872	37.436316	68.272743
1161.375668	43.519917	68.277748
1161.236771	40.675237	68.282753
1159.909094	44.918396	68.287758
1159.548922	28.801775	68.292762
1158.407055	44.980607	68.297767
1157.830971	49.569407	68.302772
1157.614071	28.103358	68.307777
1156.441505	32.008051	68.312782
1156.072845	46.718850	68.317786
1155.461019	49.143572	68.322791
1155.079609	44.175583	68.327796
1154.026440	36.209596	68.332801
1153.129301	31.416671	68.337806
1152.632961	37.785677	68.342810
1152.307788	50.384453	68.347815
1152.014272	36.064309	68.352820
1150.649013	37.959194	68.357825
1149.694655	40.041026	68.362830
1149.741338	38.929763	68.367834
1149.062416	48.965633	68.372839
1148.244453	45.587174	68.377844
1147.511724	36.259852	68.382849
1146.685495	46.658175	68.387854
1146.393510	44.894342	68.392858
1145.121268	45.214920	68.397863
1144.283063	29.212178	68.402868
1143.930312	51.435770	68.407873
1143.392018	47.140826	68.412878
1143.613049	31.940958	68.417882
1142.781815	41.291462	68.422887
1141.523571	43.976685	68.427892
1141.077127	36.089236	68.432897
1140.504115	29.943854	68.437902
1139.575501	56.262694	68.442906
1138.817485	38.276111	68.447911
1138.067798	49.767644	68.452916
1137.947910	50.344887	68.457921
1136.507610	47.306675	68.462926
1136.074536	52.610706	68.467930
1135.592713	30.269063	68.472935
1134.890725	48.123526	68.477940
1134.848865	28.277466	68.482945
1133.536487	68.527436	68.487950
1133.228502	25.439743	68.492954
1132.660148	48.806155	68.497959
1131.888845	40.487856	68.502964
1131.160084	53.753188	68.507969
1130.310813	53.408867	68.512974
1129.719214	30.931731	68.517978
1128.499152	61.977060	68.522983
1127.831714	26.919165	68.527988
1127.511853	47.647385	68.532993
1126.885369	52.048677	68.537998
1126.902963	46.723933	68.543002
1125.667238	45.217437	68.548007
1124.669867	37.225243	68.553012
1124.319810	40.585989	68.558017
1123.765776	34.262560	68.563022
1123.505484	41.492836	68.568026
1122.990603	53.836377	68.573031
1122.056637	45.116623	68.578036
1121.395051	34.661578	68.583041
1119.855269	37.795267	68.588046
1119.445284	42.234657	68.593050
1118.838290	41.916456	68.598055
1118.515336	42.606419	68.603060
1118.301094	40.730882	68.608065
1117.081095	40.888631	68.613070
1116.544151	55.750777	68.618074
1116.147180	36.773278	68.623079
1115.110460	45.185128	68.628084
1114.240129	52.146611	68.633089
1113.991969	44.117246	68.638094
1113.387395	20.366517	68.643098
1112.594105	41.814967	68.648103
1111.493054	35.723621	68.653108
1111.296735	48.790726	68.658113
1110.881328	33.017196	68.663118
1110.140826	30.820116	68.668122
1108.886894	38.563236	68.673127
1108.130135	43.068824	68.678132
1108.048656	23.240116	68.683137
1107.189230	41.594251	68.688142
1106.785146	24.771894	68.693146
1105.563334	47.017024	68.698151
1105.094454	33.697713	68.703156
1104.757409	37.840090	68.708161
1103.861202	22.843177	68.713166
1103.042309	36.753578	68.718170
1102.244135	46.507242	68.723175
1101.720973	47.382009	68.728180
1101.265530	37.239513	68.733185
1100.809024	37.372013	68.738190
1100.620810	25.805689	68.743194
1099.461397	38.983404	68.748199
1098.709627	40.339210	68.753204
1097.669548	21.861403	68.758209
1096.536957	37.133650	68.763214
1096.542792	21.774074	68.768218
1095.915366	32.148658	68.773223
1095.912808	46.832758	68.778228
1095.336678	16.617120	68.783233
1093.970992	56.520746	68.788238
1093.676487	22.855851	68.793242
1092.420493	31.476035	68.798247
1091.340806	51.426312	68.803252
1090.917922	25.418579	68.808257
1089.896459	29.564175	68.813262
1090.188901	32.885794	68.818266
1089.560506	37.965443	68.823271
1089.121871	42.638038	68.828276
1088.690560	33.120878	68.833281
1087.639719	36.634098	68.838286
1087.201285	32.966647	68.843290
1085.756400	25.310578	68.848295
1085.006370	34.662365	68.853300
1084.797371	31.109797	68.858305
1083.940740	33.072032	68.863310
1083.933919	25.133595	68.868314
1083.222623	30.261120	68.873319
1082.077581	29.311046	68.878324
1081.517335	29.567278	68.883329
1080.468392	30.907286	68.888334
1079.893941	30.423078	68.893338
1079.274800	27.738376	68.898343
1079.185868	34.080425	68.903348
1078.945443	25.567327	68.908353
1077.777101	38.937270	68.913358
1076.865063	32.729148	68.918362
1076.173954	38.880003	68.923367
1075.238902	27.960733	68.928372
1074.787802	28.078187	68.933377
1073.733516	34.498112	68.938382
1073.406629	28.315175	68.943386
1073.287383	30.478638	68.948391
1072.302062	31.412737	68.953396
1072.097393	25.041635	68.958401
1071.151016	36.274315	68.963406
1070.146950	29.131568	68.968410
1069.393642	32.442932	68.973415
1068.954299	31.479944	68.978420
1068.711648	17.705228	68.983425
1067.331106	28.544950	68.988430
1066.368342	23.205872	68.993434
1066.050071	36.164636	68.998439
1065.321129	52.083860	69.003444
1065.415530	25.646939	69.008449
1064.639618	25.508578	69.013454
1063.431011	38.825009	69.018458
1063.019388	33.008769	69.023463
1062.272461	28.567279	69.028468
1062.045011	31.372392	69.033473
1060.636795	40.321143	69.038478
1060.231193	43.952490	69.043482
1059.943463	39.734398	69.048487
1059.124283	40.864409	69.053492
1058.367331	36.178523	69.058497
1057.707080	33.451483	69.063502
1057.029676	25.786873	69.068506
1056.432228	21.323185	69.073511
1055.059476	33.536697	69.078516
1054.870313	32.166504	69.083521
1053.983116	43.608963	69.088526
1053.775824	39.398574	69.093530
1053.613171	30.650769	69.098535
1052.929414	15.940195	69.103540
1051.984723	30.386243	69.108545
1051.478327	35.220999	69.113550
1050.317881	40.073079	69.118554
1049.411027	33.094637	69.123559
1049.069060	27.579539	69.128564
1048.946645	29.628396	69.133569
1047.411006	37.615039	69.138574
1046.651889	28.266731	69.143578
1046.069980	34.349758	69.148583
1045.243114	45.394715	69.153588
1045.423026	29.791415	69.158593
1044.486918	38.113165	69.163598
1044.485187	22.467812	69.168602
1043.284217	20.151634	69.173607
1042.544748	28.697547	69.178612
1042.043432	12.280180	69.183617
1040.756114	24.541596	69.188622
1040.423887	43.270736	69.193626
1040.125796	22.032104	69.198631
1039.408964	17.335117	69.203636
1038.229542	32.537560	69.208641
1037.649675	33.724117	69.213646
1037.111751	30.742671	69.218650
1036.742628	24.361470	69.223655
1036.007253	18.098461	69.228660
1034.903252	31.639512	69.233665
1034.246093	36.769476	69.238670
1034.133305	28.581411	69.243674
1033.731808	24.258432	69.248679
1032.602357	34.329718	69.253684
1032.078042	29.931665	69.258689
1031.380780	24.717509	69.263694
1030.745117	18.331412	69.268698
1029.568647	24.844899	69.273703
1028.812041	37.201659	69.278708
1028.927227	21.917731	69.283713
1027.980851	34.216376	69.288718
1027.720063	35.665967	69.293722
1026.895743	32.506172	69.298727
1026.210407	29.671176	69.303732
1025.948616	27.699143	69.308737
1024.380742	28.636060	69.313742
1023.682688	26.536327	69.318746
1023.365081	26.884849	69.323751
1022.578118	30.865436	69.328756
1021.744706	24.211197	69.333761
1021.192224	28.539231	69.338766
1020.815453	30.101886	69.343770
1020.581798	27.568746	69.348775
1019.195155	31.685740	69.353780
1018.477263	20.104365	69.358785
1017.753538	28.497977	69.363790
1017.657185	27.589233	69.368794
1016.859600	25.448571	69.373799
1016.084814	22.785496	69.378804
1015.704984	22.200958	69.383809
1014.598963	40.904977	69.388814
1014.136852	46.877497	69.393818
1013.184532	34.940771	69.398823
1012.134172	38.603746	69.403828
1011.931341	30.822646	69.408833
1011.328619	43.307887	69.413838
1011.249262	39.534438	69.418842
1010.377833	30.602957	69.423847
1009.471917	34.356484	69.428852
1009.225510	28.293211	69.433857
1008.232624	39.533309	69.438862
1007.296557	28.388743	69.443866
1006.805228	32.907313	69.448871
1006.053420	38.183221	69.453876
1005.630800	30.123298	69.458881
1004.522235	31.162181	69.463886
1004.066615	19.930144	69.468890
1003.539291	27.679113	69.473895
1002.729984	28.583657	69.478900
1002.574658	29.854053	69.483905
1001.574113	29.891791	69.488910
1000.657196	20.719991	69.493914
1000.366682	21.529378	69.498919
999.863633	37.040513	69.503924
999.060868	28.684705	69.508929
997.975116	32.958827	69.513934
997.721764	23.845443	69.518938
997.177063	12.821541	69.523943
995.790003	22.258924	69.528948
995.265912	9.080913	69.533953
994.810775	20.043064	69.538958
994.427165	24.038323	69.543962
994.196310	25.987747	69.548967
992.996677	32.210064	69.553972
992.378726	35.123043	69.558977
991.931288	31.960063	69.563982
990.737215	24.841280	69.568986
990.035328	42.413474	69.573991
989.495594	31.330426	69.578996
989.297572	18.169911	69.584001
988.680531	37.042120	69.589006
987.732941	23.157244	69.594010
986.930632	46.989777	69.599015
986.595605	28.108130	69.604020
985.733205	22.429863	69.609025
984.768701	29.876257	69.614030
984.135680	42.695884	69.619034
983.980263	29.914910	69.624039
983.235736	36.714486	69.629044
982.713797	24.059641	69.634049
981.911122	28.705018	69.639054
981.177258	26.786028	69.644058
980.244898	21.437420	69.649063
979.084022	36.510785	69.654068
978.617111	22.732348	69.659073
978.456244	35.530456	69.664078
978.249773	29.634288	69.669082
977.628676	17.630701	69.674087
976.345484	33.209198	69.679092
975.950579	30.285430	69.684097
975.323266	21.534310	69.689102
974.326669	22.694154	69.694106
973.730616	27.177353	69.699111
973.315703	31.705845	69.704116
972.703237	23.969436	69.709121
971.454005	33.913153	69.714126
970.608680	25.382792	69.719130
970.402134	31.983233	69.724135
970.042706	34.681627	69.729140
969.727490	28.504737	69.734145
968.717701	38.586967	69.739150
967.830602	29.084023	69.744154
967.584165	25.035987	69.749159
966.434882	16.525615	69.754164
966.005291	24.780975	69.759169
965.090444	33.856253	69.764174
964.487873	24.166122	69.769178
963.701568	20.243413	69.774183
962.565976	33.693326	69.779188
962.113581	30.772400	69.784193
961.891308	27.838512	69.789198
961.221198	22.211654	69.794202
961.000397	20.140073	69.799207
960.109202	35.465403	69.804212
959.440465	14.790383	69.809217
958.842779	26.172590	69.814222
958.012245	14.516134	69.819226
957.126652	17.055414	69.824231
956.369415	40.861844	69.829236
956.367756	30.063751	69.834241
955.620096	35.037830	69.839246
954.566867	23.937167	69.844250
953.958381	27.607114	69.849255
953.308531	22.249831	69.854260
953.029069	21.302423	69.859265
951.542138	27.586240	69.864270
950.892007	30.707761	69.869274
950.688181	8.504913	69.874279
949.913919	38.998339	69.879284
949.851092	26.924843	69.884289
948.512882	26.740383	69.889294
947.949525	23.886002	69.894298
947.607505	20.695221	69.899303
946.998659	36.702557	69.904308
946.392244	24.925284	69.909313
945.526687	16.382390	69.914318
944.599314	40.934940	69.919322
943.977346	19.359977	69.924327
942.605232	39.110810	69.929332
942.521611	22.699538	69.934337
942.067579	9.999223	69.939342
941.603798	31.231243	69.944346
941.443874	34.627977	69.949351
940.264286	25.395505	69.954356
939.710333	27.506728	69.959361
939.007428	20.434388	69.964366
937.774003	24.199053	69.969370
937.397190	24.937029	69.974375
936.818920	38.567910	69.979380
936.647458	19.898368	69.984385
935.598085	22.957275	69.989390
934.568733	21.033284	69.994394
934.452684	25.951009	69.999399
933.559954	27.792887	70.004404
932.544779	30.988271	70.009409
931.894738	27.930081	70.014414
931.614263	27.348667	70.019418
931.594036	19.964280	70.024423
930.394637	30.989688	70.029428
929.459084	32.862036	70.034433
929.090707	31.977661	70.039438
928.251346	30.881249	70.044442
927.312189	29.584688	70.049447
926.195696	33.092647	70.054452
926.195052	24.468886	70.059457
925.534628	27.918460	70.064462
924.787732	23.338251	70.069466
924.634279	28.085320	70.074471
923.525336	36.874550	70.079476
923.088246	27.028796	70.084481
922.411227	32.161941	70.089486
921.383264	27.047753	70.094490
920.425851	33.707766	70.099495
920.270594	37.486935	70.104500
919.952850	20.485339	70.109505
919.612880	21.094459	70.114510
918.168005	26.624171	70.119514
917.461448	25.874036	70.124519
917.102180	24.832105	70.129524
916.717155	31.919815	70.134529
915.646476	27.941457	70.139534
914.941501	19.253178	70.144538
915.017460	20.630265	70.149543
913.815940	25.820072	70.154548
912.804475	22.381040	70.159553
911.960077	31.541307	70.164558
911.795701	36.173430	70.169562
911.320760	24.413093	70.174567
909.891113	26.160662	70.179572
909.420147	23.219052	70.184577
908.654040	30.578706	70.189582
908.516454	20.579647	70.194586
908.177830	24.135698	70.199591
907.278448	35.081835	70.204596
906.449302	19.949785	70.209601
906.149767	20.517782	70.214606
905.222570	34.699323	70.219610
904.436755	23.757968	70.224615
903.770070	39.943237	70.229620
903.284936	28.840494	70.234625
902.561090	21.653235	70.239630
901.615870	26.721839	70.244634
900.997514	28.403376	70.249639
900.412323	28.036029	70.254644
900.202724	19.027661	70.259649
899.048598	21.811534	70.264654
898.431131	21.545513	70.269658
898.087276	17.617065	70.274663
897.087365	28.979720	70.279668
896.381345	26.346739	70.284673
895.510600	29.858176	70.289678
894.999785	32.377255	70.294682
894.994850	14.810259	70.299687
893.977626	41.934773	70.304692
893.257194	30.268696	70.309697
892.896331	15.675528	70.314702
891.953940	30.770908	70.319706
891.756846	18.901712	70.324711
890.085853	33.840255	70.329716
890.004754	17.370256	70.334721
889.482338	17.109608	70.339726
888.501462	15.791320	70.344730
887.592365	24.353220	70.349735
887.152225	27.338839	70.354740
886.781077	17.851591	70.359745
886.370648	9.187411	70.364750
884.898768	37.634722	70.369754
884.654696	14.170499	70.374759
883.954825	24.559789	70.379764
883.330617	20.401589	70.384769
882.930180	28.742199	70.389774
881.968185	26.071118	70.394778
881.272184	33.708187	70.399783
880.504444	28.334997	70.404788
880.234715	30.784172	70.409793
879.406636	32.204220	70.414798
878.494159	26.827259	70.419802
878.102461	20.711446	70.424807
877.423360	36.132338	70.429812
876.766364	30.422998	70.434817
875.535695	25.304826	70.439822
874.869560	34.690606	70.444826
874.699376	31.510332	70.449831
874.118405	29.245362	70.454836
873.622064	29.724844	70.459841
872.670623	22.901805	70.464846
872.009653	22.011972	70.469850
871.516118	34.314271	70.474855
871.227285	29.285883	70.479860
870.157732	22.293997	70.484865
869.847473	23.789319	70.489870
868.754977	33.042696	70.494874
867.957056	29.646961	70.499879
867.315328	23.112078	70.504884
867.123345	22.086106	70.509889
866.175913	29.026801	70.514894
865.182876	22.297113	70.519898
864.631676	29.346622	70.524903
863.996589	31.305203	70.529908
863.614116	23.631567	70.534913
863.243563	17.665348	70.539918
862.009312	19.397612	70.544922
861.115893	19.915065	70.549927
861.028761	25.588230	70.554932
860.619553	26.314027	70.559937
859.564067	27.786044	70.564942
858.861574	29.370601	70.569946
858.564442	13.485319	70.574951
857.327874	33.618274	70.579956
856.671223	18.884547	70.584961
856.000610	22.840350	70.589966
855.055584	31.193528	70.594970
854.922969	25.485886	70.599975
854.614050	17.589249	70.604980
853.730246	22.143499	70.609985
853.281446	19.885882	70.614990
852.318344	34.653432	70.619994
851.676531	19.712352	70.624999
850.475683	29.055515	70.630004
849.879476	24.090247	70.635009
849.507839	24.765914	70.640014
849.094663	27.849743	70.645018
849.069893	15.636182	70.650023
848.100145	36.813128	70.655028
847.281132	33.441255	70.660033
846.182164	29.303439	70.665038
845.125275	33.071586	70.670042
844.992401	27.770813	70.675047
844.268551	26.004803	70.680052
843.992148	14.586610	70.685057
843.208631	17.999025	70.690062
842.189000	25.878408	70.695066
841.988481	21.782084	70.700071
841.145844	23.379491	70.705076
839.996775	17.407890	70.710081
839.579849	22.510688	70.715086
838.611969	31.077231	70.720090
838.470653	12.636302	70.725095
837.989723	30.726800	70.730100
837.264289	31.417784	70.735105
836.506905	28.644773	70.740110
835.674643	40.513746	70.745114
835.348585	27.774158	70.750119
834.308325	27.471376	70.755124
833.434229	22.457311	70.760129
833.052868	37.934890	70.765134
832.710360	32.836209	70.770138
832.149626	29.826906	70.775143
831.168916	30.736710	70.780148
830.314132	21.195576	70.785153
830.136949	26.234987	70.790158
828.796393	37.568315	70.795162
828.157587	23.183394	70.800167
827.696387	27.490624	70.805172
827.309980	24.699565	70.810177
827.275372	22.459599	70.815182
825.865506	31.394523	70.820186
825.153832	29.863108	70.825191
824.527295	26.558373	70.830196
823.984218	19.077459	70.835201
823.006725	21.380692	70.840206
822.390201	31.326249	70.845210
822.076529	31.981656	70.850215
821.688296	33.216599	70.855220
820.487586	32.869980	70.860225
819.648001	33.749440	70.865230
819.380809	29.449278	70.870234
818.796176	25.682163	70.875239
817.744623	30.332509	70.880244
816.870615	24.112142	70.885249
816.431836	20.441654	70.890254
815.990481	31.792689	70.895258
815.784421	31.212058	70.900263
814.584676	30.717065	70.905268
814.215807	29.815442	70.910273
813.596148	13.696102	70.915278
811.868208	31.772223	70.920282
811.694571	27.769388	70.925287
810.971906	28.183989	70.930292
810.534908	30.489495	70.935297
810.198290	14.083843	70.940302
809.732166	24.708733	70.945306
808.725329	25.933344	70.950311
807.849014	19.591933	70.955316
807.730637	19.552398	70.960321
807.114913	20.979662	70.965326
805.965467	25.897891	70.970330
805.446310	14.398507	70.975335
804.949394	26.009103	70.980340
804.299421	26.248142	70.985345
803.328534	22.460521	70.990350
802.539379	42.180104	70.995354
801.952349	24.866613	71.000359
801.103835	24.631087	71.005364
800.527629	30.443603	71.010369
800.022755	31.911568	71.015374
799.401441	30.748953	71.020378
799.290293	17.297126	71.025383
797.900066	31.492473	71.030388
797.392114	24.054856	71.035393
797.078594	23.333648	71.040398
796.418837	33.513159	71.045402
795.361752	25.816047	71.050407
794.787984	24.267421	71.055412
794.230897	24.614671	71.060417
793.966486	22.351367	71.065422
792.557221	29.663627	71.070426
792.193238	28.858994	71.075431
791.481946	44.305528	71.080436
791.040912	31.828663	71.085441
790.150322	21.359749	71.090446
789.329605	29.746770	71.095450
789.012698	28.010607	71.100455
788.373518	25.594087	71.105460
787.290936	29.459380	71.110465
786.440405	26.245503	71.115470
785.860042	22.398875	71.120474
785.984473	27.393427	71.125479
785.502514	27.563150	71.130484
784.287224	28.803609	71.135489
783.343071	23.004405	71.140494
782.609090	28.446249	71.145498
782.363999	27.813491	71.150503
781.674599	20.043665	71.155508
780.559926	24.459659	71.160513
780.529884	31.372604	71.165518
779.775519	31.915255	71.170522
778.935532	33.786634	71.175527
778.082810	22.860716	71.180532
777.775062	28.277282	71.185537
777.346819	27.356734	71.190542
776.144950	26.893634	71.195546
775.344494	19.524667	71.200551
774.853847	30.445185	71.205556
774.474029	25.308305	71.210561
774.251556	28.702385	71.215566
772.877763	30.731279	71.220570
772.635912	23.981391	71.225575
771.759069	24.969293	71.230580
771.105477	28.463542	71.235585
770.335347	29.514876	71.240590
769.347060	38.881003	71.245594
769.447164	26.388961	71.250599
768.620852	38.502988	71.255604
767.314325	36.232132	71.260609
766.950249	25.796094	71.265614
765.990657	27.524101	71.270618
765.983705	36.492742	71.275623
765.487516	34.873428	71.280628
764.217329	35.613312	71.285633
764.088771	20.193192	71.290638
763.139221	31.429604	71.295642
762.395319	24.907867	71.300647
761.786511	24.810801	71.305652
761.169835	34.171380	71.310657
761.035205	24.252293	71.315662
760.102041	29.210221	71.320666
759.198217	25.525475	71.325671
758.891776	19.150127	71.330676
757.063573	27.238682	71.335681
756.756285	17.216209	71.340686
755.989055	32.513953	71.345690
755.809771	22.363872	71.350695
755.350475	26.626657	71.355700
754.820886	22.590616	71.360705
753.858144	30.457819	71.365710
753.109933	33.011564	71.370714
752.336432	22.044663	71.375719
752.210200	25.338272	71.380724
751.464056	34.650082	71.385729
750.875036	23.163410	71.390734
750.081070	33.346949	71.395738
749.065858	23.244801	71.400743
748.202755	27.100396	71.405748
747.403902	29.900309	71.410753
747.292574	24.197175	71.415758
746.726777	30.630899	71.420762
746.169850	22.395322	71.425767
745.230882	19.020511	71.430772
744.276415	23.092489	71.435777
744.116106	26.186532	71.440782
743.438529	21.786150	71.445786
742.492481	34.105309	71.450791
742.143808	32.527165	71.455796
741.485229	22.808186	71.460801
741.085949	21.381594	71.465806
739.881198	35.649934	71.470810
739.050209	27.965736	71.475815
738.824566	25.141215	71.480820
738.107708	30.924097	71.485825
737.480293	19.687957	71.490830
736.524727	34.148422	71.495834
736.174403	21.518379	71.500839
735.556453	30.514909	71.505844
734.320123	22.349659	71.510849
733.968136	22.120254	71.515854
733.190015	25.727372	71.520858
732.941315	34.400205	71.525863
732.010258	16.711046	71.530868
731.188349	26.200487	71.535873
730.839457	23.764573	71.540878
730.413497	25.781346	71.545882
729.846334	24.518671	71.550887
728.586355	23.875624	71.555892
727.767503	26.297128	71.560897
727.676180	18.695436	71.565902
726.729207	35.051489	71.570906
725.928671	25.782442	71.575911
725.440039	28.980796	71.580916
724.771445	34.562046	71.585921
724.614437	21.581126	71.590926
723.338193	27.144010	71.595930
722.522877	25.490365	71.600935
722.146998	25.717322	71.605940
721.719409	22.839806	71.610945
721.246267	22.337975	71.615950
719.867979	28.292398	71.620954
719.498459	33.706191	71.625959
718.974047	19.571170	71.630964
717.857683	19.927063	71.635969
717.649089	9.836854	71.640974
716.607788	26.061271	71.645978
716.442582	24.282043	71.650983
716.013502	28.626750	71.655988
714.740159	34.854611	71.660993
714.308978	23.878950	71.665998
713.711903	29.783106	71.671002
713.161982	23.479645	71.676007
712.164217	28.091505	71.681012
711.623886	33.185586	71.686017
711.317626	27.936088	71.691022
709.912539	28.987619	71.696026
709.036613	16.862293	71.701031
708.618275	25.946883	71.706036
708.083385	28.987036	71.711041
708.044552	-1.356470	71.716046
707.165008	33.977284	71.721050
706.651716	24.045961	71.726055
705.865923	19.770048	71.731060
705.198601	21.101479	71.736065
704.165246	22.962670	71.741070
703.218568	25.544874	71.746074
702.791261	19.863674	71.751079
702.524506	27.594844	71.756084
701.483143	32.981578	71.761089
700.617819	18.449866	71.766094
700.048177	23.600649	71.771098
699.513733	24.783200	71.776103
699.334979	23.819787	71.781108
698.678391	26.212310	71.786113
697.866255	26.135020	71.791118
696.979467	19.483106	71.796122
696.636020	29.908713	71.801127
695.997341	36.033951	71.806132
694.794202	22.552598	71.811137
694.554551	21.322933	71.816142
693.951559	17.812651	71.821146
693.163771	26.542933	71.826151
692.109277	19.854651	71.831156
691.850739	23.803221	71.836161
691.603749	17.661256	71.841166
690.287452	26.390541	71.846170
689.503966	28.634549	71.851175
689.065265	18.073233	71.856180
688.428494	25.063855	71.861185
688.126413	19.733279	71.866190
686.839465	27.231104	71.871194
686.059839	26.125264	71.876199
685.863387	24.858761	71.881204
685.180945	38.145149	71.886209
685.010719	26.757382	71.891214
683.745397	36.079340	71.896218
683.394970	33.687828	71.901223
682.924015	28.844581	71.906228
681.599327	31.908004	71.911233
680.579064	26.543560	71.916238
680.309412	39.964481	71.921242
679.600682	31.432991	71.926247
679.733620	25.854961	71.931252
678.633837	34.891958	71.936257
677.813483	19.074269	71.941262
677.247787	30.727366	71.946266
676.814254	19.800976	71.951271
676.293577	32.340980	71.956276
675.097156	41.025964	71.961281
674.925312	27.175411	71.966286
674.384346	33.455393	71.971290
672.865019	20.655145	71.976295
672.473346	43.788407	71.981300
671.718804	18.372975	71.986305
671.547834	30.346392	71.991310
670.857000	41.652018	71.996314
670.255346	31.342136	72.001319
669.874745	36.478596	72.006324
668.304056	38.658740	72.011329
667.347218	38.511467	72.016334
667.291747	39.572026	72.021338
666.392747	20.887531	72.026343
666.427340	31.060565	72.031348
665.626781	37.176896	72.036353
664.800388	24.461839	72.041358
663.803931	30.101615	72.046362
663.466419	35.360515	72.051367
662.814157	28.996098	72.056372
661.602888	30.751605	72.061377
661.123997	25.712521	72.066382
660.830219	31.333439	72.071386
660.263700	28.304603	72.076391
659.724512	14.708091	72.081396
658.389436	31.390866	72.086401
657.908202	48.421788	72.091406
657.924075	22.807985	72.096410
656.800796	20.839152	72.101415
656.197643	42.503348	72.106420
655.498821	32.722997	72.111425
655.041759	9.445736	72.116430
653.808244	33.911443	72.121434
652.913122	26.759433	72.126439
652.471541	21.979322	72.131444
652.006232	32.181502	72.136449
652.002679	23.667035	72.141454
651.170965	29.009362	72.146458
650.291668	23.810131	72.151463
649.738514	26.503141	72.156468
648.883871	40.704725	72.161473
647.731616	29.713028	72.166478
647.114257	31.022327	72.171482
646.617210	23.966191	72.176487
646.253167	25.083773	72.181492
645.570704	37.469786	72.186497
645.300064	31.519234	72.191502
644.196316	28.487651	72.196506
643.714137	17.422372	72.201511
643.014805	28.249983	72.206516
641.848416	30.116616	72.211521
641.492259	18.070966	72.216526
641.035839	29.664089	72.221530
640.420279	22.126967	72.226535
639.947030	8.654000	72.231540
638.133880	21.041877	72.236545
638.342845	28.484416	72.241550
637.908767	23.509160	72.246554
637.127503	26.549139	72.251559
636.365210	26.752495	72.256564
635.523638	28.676206	72.261569
635.464851	12.581158	72.266574
634.128099	28.464742	72.271578
633.282333	21.964007	72.276583
633.075360	23.190609	72.281588
632.522446	20.692591	72.286593
632.047596	14.621615	72.291598
630.976873	36.950005	72.296602
630.564930	35.473412	72.301607
630.142013	16.093423	72.306612
628.573888	18.791964	72.311617
628.011260	34.741498	72.316622
627.643637	12.992162	72.321626
627.102594	20.908927	72.326631
626.835535	24.390534	72.331636
625.655304	38.807963	72.336641
625.223598	29.068661	72.341646
625.032346	18.825901	72.346650
623.647851	25.807889	72.351655
622.773572	21.911926	72.356660
622.188489	39.855027	72.361665
621.944682	25.386785	72.366670
621.027026	19.402097	72.371674
619.832281	31.223184	72.376679
619.900443	10.244915	72.381684
619.127528	21.757558	72.386689
618.846254	33.234488	72.391694
617.688966	14.228487	72.396698
616.665899	23.716874	72.401703
616.220246	38.853051	72.406708
615.763942	23.267552	72.411713
615.644863	20.847094	72.416718
614.538905	28.932675	72.421722
613.820168	29.928565	72.426727
613.321585	30.321727	72.431732
612.576694	30.258985	72.436737
611.455404	19.684982	72.441742
610.727329	39.787488	72.446746
610.417796	28.749906	72.451751
610.409939	21.827171	72.456756
609.530514	17.228759	72.461761
608.847695	24.267727	72.466766
608.251912	31.382717	72.471770
606.989081	23.223339	72.476775
606.483112	34.846434	72.481780
605.549585	29.640087	72.486785
605.429499	4.096868	72.491790
604.815136	38.155299	72.496794
604.034218	24.930012	72.501799
603.763262	15.888898	72.506804
602.648016	30.795839	72.511809
602.091680	17.643595	72.516814
600.842526	27.074963	72.521818
600.076894	27.717226	72.526823
599.859027	24.565075	72.531828
599.333492	27.647909	72.536833
598.936286	27.417840	72.541838
597.982760	25.466150	72.546842
597.348575	20.557466	72.551847
596.762720	38.601607	72.556852
595.967655	29.621882	72.561857
595.117950	13.427318	72.566862
594.382832	41.866177	72.571866
594.069969	28.534809	72.576871
593.989106	17.561739	72.581876
592.584192	21.440598	72.586881
592.112971	26.115285	72.591886
591.625001	24.113102	72.596890
590.583135	36.491713	72.601895
589.625781	30.566969	72.606900
588.669537	36.533084	72.611905
588.434700	27.063617	72.616910
588.193462	24.826609	72.621914
587.576011	27.924084	72.626919
587.608520	21.490054	72.631924
586.308358	15.940017	72.636929
585.785078	18.152071	72.641934
584.869327	34.317110	72.646938
583.694947	21.930314	72.651943
583.466227	5.673127	72.656948
583.015486	28.681732	72.661953
582.398740	18.416869	72.666958
581.715815	19.659359	72.671962
580.522819	18.261447	72.676967
580.435317	30.921687	72.681972
579.714620	36.396155	72.686977
578.478502	17.760677	72.691982
578.300235	26.166838	72.696986
577.374450	37.883610	72.701991
576.665374	10.981918	72.706996
575.461827	39.200509	72.712001
575.454317	19.427965	72.717006
575.015388	18.416122	72.722010
574.419308	42.234744	72.727015
574.354406	14.494057	72.732020
572.981305	40.752827	72.737025
572.521216	32.363113	72.742030
571.413286	19.316080	72.747034
570.343765	49.176919	72.752039
569.844416	20.155635	72.757044
569.271237	46.293315	72.762049
569.365360	4.439730	72.767054
568.886011	25.251605	72.772058
567.423762	27.641603	72.777063
567.268190	25.105543	72.782068
566.121145	40.572621	72.787073
565.318107	30.389463	72.792078
564.824247	25.132029	72.797082
564.084781	36.983119	72.802087
564.214944	29.275205	72.807092
563.253599	29.685319	72.812097
562.245872	31.348532	72.817102
561.499859	19.856976	72.822106
561.138844	31.527943	72.827111
560.666604	30.516676	72.832116
559.061182	33.019365	72.837121
558.933121	25.795678	72.842126
558.227880	25.283542	72.847130
557.802960	19.155748	72.852135
557.194231	27.737699	72.857140
556.079957	26.962730	72.862145
555.629368	26.455762	72.867150
555.283126	25.627841	72.872154
554.675301	29.160578	72.877159
553.463761	14.315109	72.882164
552.590575	24.251120	72.887169
552.584151	26.259438	72.892174
552.133976	31.306071	72.897178
550.794382	28.091339	72.902183
550.100541	14.070100	72.907188
549.527091	17.322988	72.912193
549.230194	28.036053	72.917198
549.008673	24.381474	72.922202
547.894347	32.416378	72.927207
547.211442	19.104553	72.932212
546.662559	28.293521	72.937217
545.509363	23.763970	72.942222
544.869045	21.130096	72.947226
543.990245	35.958398	72.952231
544.104300	18.118641	72.957236
543.433700	24.400365	72.962241
542.880232	23.304276	72.967246
542.068937	22.148338	72.972250
540.779860	30.054970	72.977255
540.798297	27.672532	72.982260
539.855633	23.450049	72.987265
539.194351	16.878971	72.992270
539.038419	22.332864	72.997274
537.832317	31.508260	73.002279
537.107373	19.114555	73.007284
536.424744	27.653091	73.012289
536.105655	25.199847	73.017294
535.206864	32.197546	73.022298
533.980027	32.172175	73.027303
533.385789	20.192861	73.032308
533.062333	29.295464	73.037313
532.577211	33.165029	73.042318
532.277283	28.805475	73.047322
531.455885	27.033024	73.052327
530.943465	22.973807	73.057332
530.002403	29.986125	73.062337
529.426461	35.912178	73.067342
528.655590	27.857393	73.072346
527.553262	35.223387	73.077351
527.374243	33.775937	73.082356
526.734116	30.984350	73.087361
525.929935	32.755494	73.092366
525.216065	29.560943	73.097370
524.330829	44.475433	73.102375
524.463079	37.246546	73.107380
523.492811	41.750024	73.112385
522.370924	45.539689	73.117390
522.229584	32.611495	73.122394
521.213727	35.969557	73.127399
521.264059	23.460241	73.132404
519.861407	36.158100	73.137409
519.226152	40.827394	73.142414
519.007162	13.697862	73.147418
517.724806	21.614467	73.152423
516.995916	33.851782	73.157428
516.576698	24.213020	73.162433
516.019217	24.435823	73.167438
516.073250	17.407051	73.172442
514.946694	30.832004	73.177447
513.885847	29.737904	73.182452
513.601722	22.447629	73.187457
512.889065	26.140566	73.192462
511.867095	25.314646	73.197466
510.877111	29.021802	73.202471
510.653152	24.230709	73.207476
509.746222	33.960815	73.212481
509.850225	27.613162	73.217486
509.275259	28.494721	73.222490
508.149542	22.251508	73.227495
507.719872	35.885554	73.232500
507.062428	33.598170	73.237505
506.137527	23.770325	73.242510
505.337390	17.136228	73.247514
504.652082	31.209936	73.252519
504.402392	38.313965	73.257524
503.660265	41.142758	73.262529
502.496345	28.781145	73.267534
502.132345	25.497754	73.272538
501.390933	37.118945	73.277543
501.053858	27.542787	73.282548
500.321210	23.431935	73.287553
499.290338	15.292441	73.292558
498.749601	19.826835	73.297562
498.407056	38.262699	73.302567
497.859354	25.016078	73.307572
496.816114	27.020842	73.312577
496.059068	16.787823	73.317582
495.817871	23.366978	73.322586
494.990267	17.785865	73.327591
494.184636	38.058417	73.332596
493.731948	23.798516	73.337601
493.009720	15.048498	73.342606
492.453386	30.932380	73.347610
491.685168	30.271034	73.352615
491.206579	15.843392	73.357620
490.778659	17.050012	73.362625
489.891702	21.362039	73.367630
488.907304	25.476716	73.372634
487.808193	39.550128	73.377639
487.827056	21.728695	73.382644
486.751708	28.147446	73.387649
485.735889	22.000270	73.392654
485.619066	26.194341	73.397658
485.063515	32.314258	73.402663
484.770447	31.276040	73.407668
483.886223	30.275232	73.412673
482.872166	26.418937	73.417678
482.662134	22.773575	73.422682
481.866042	22.545576	73.427687
481.521495	31.758768	73.432692
480.461016	32.973131	73.437697
479.679525	26.656170	73.442702
479.184539	7.573142	73.447706
477.823060	30.004637	73.452711
477.349806	24.816478	73.457716
476.631283	21.674722	73.462721
476.384242	34.697815	73.467726
476.206580	28.836554	73.472730
475.434217	17.350812	73.477735
474.610901	44.884423	73.482740
474.180518	17.875305	73.487745
473.217890	33.527472	73.492750
472.435657	32.095709	73.497754
471.620960	35.511622	73.502759
471.048722	16.494506	73.507764
470.755378	35.632107	73.512769
469.781208	10.912497	73.517774
468.929328	47.284161	73.522778
468.585000	34.042986	73.527783
468.393664	26.742664	73.532788
466.779398	44.323075	73.537793
466.030486	29.416558	73.542798
465.756946	24.723251	73.547802
465.123481	46.777033	73.552807
465.164164	9.443362	73.557812
464.214192	44.203340	73.562817
463.262103	24.286433	73.567822
462.843869	24.502831	73.572826
461.477086	41.671677	73.577831
461.379708	9.044826	73.582836
460.607189	45.966775	73.587841
459.840456	26.088142	73.592846
459.532649	35.148837	73.597850
458.373811	46.469141	73.602855
457.807463	13.689931	73.607860
457.288708	34.440289	73.612865
457.094981	13.543195	73.617870
455.939948	25.288626	73.622874
454.927080	27.343758	73.627879
454.881288	20.029715	73.632884
454.323025	21.827926	73.637889
452.927914	36.476749	73.642894
452.971305	24.597710	73.647898
451.900365	29.688066	73.652903
451.753528	20.281876	73.657908
450.364141	36.150268	73.662913
449.835072	29.463538	73.667918
449.358175	13.935003	73.672922
448.797843	34.914321	73.677927
448.506620	32.434574	73.682932
447.424394	20.194018	73.687937
446.859939	24.032082	73.692942
445.951669	21.664839	73.697946
444.928752	37.829637	73.702951
444.384252	18.838071	73.707956
444.214448	35.620677	73.712961
443.853462	37.865246	73.717966
443.332231	10.719254	73.722970
442.183646	19.032440	73.727975
441.308605	40.262167	73.732980
441.104516	20.323867	73.737985
439.560899	31.115731	73.742990
439.180065	30.198728	73.747994
438.476620	35.314112	73.752999
438.284008	15.235229	73.758004
437.838231	46.217174	73.763009
436.927444	44.063207	73.768014
436.008192	16.565912	73.773018
435.274581	47.707254	73.778023
435.123126	30.546849	73.783028
434.476329	17.598303	73.788033
433.137420	29.917055	73.793038
432.643850	40.975258	73.798042
432.297398	31.096277	73.803047
431.652247	26.758631	73.808052
430.687305	22.979685	73.813057
429.976092	35.006055	73.818062
429.714264	24.993755	73.823066
429.257573	25.758722	73.828071
428.476680	23.919934	73.833076
427.667291	32.013519	73.838081
427.143025	15.723036	73.843086
426.104217	37.710511	73.848090
425.297824	19.120203	73.853095
424.973626	29.736700	73.858100
424.387700	24.382016	73.863105
423.701629	13.141154	73.868110
422.540565	22.146996	73.873114
422.029628	42.337915	73.878119
421.878633	20.811158	73.883124
421.254848	14.962649	73.888129
420.060447	52.344466	73.893134
419.221560	14.086576	73.898138
419.025255	23.044348	73.903143
418.668307	14.348113	73.908148
417.979514	26.979568	73.913153
416.694434	22.018543	73.918158
416.188540	18.593786	73.923162
415.432691	29.411517	73.928167
415.392913	21.626619	73.933172
414.421400	32.907618	73.938177
413.434500	28.110379	73.943182
413.291413	27.865080	73.948186
412.646587	20.711141	73.953191
411.576446	12.768748	73.958196
410.990864	35.302129	73.963201
410.365167	37.353931	73.968206
410.174807	26.240645	73.973210
408.772700	22.633861	73.978215
408.114487	23.484555	73.983220
407.597129	23.935939	73.988225
407.358451	30.629807	73.993230
407.227054	17.607032	73.998234
405.546019	30.349292	74.003239
405.313144	18.407058	74.008244
404.624303	11.515589	74.013249
403.094919	19.848470	74.018254
402.967958	29.660885	74.023258
402.479953	12.754396	74.028263
402.163881	41.922786	74.033268
401.173794	5.155494	74.038273
400.295399	40.487490	74.043278
400.177568	9.384004	74.048282
399.464651	37.779892	74.053287
398.602740	22.296947	74.058292
397.598187	11.184111	74.063297
396.910472	23.577291	74.068302
396.774025	24.377961	74.073306
395.685849	20.563478	74.078311
395.143683	22.970953	74.083316
394.497599	24.013670	74.088321
393.804289	16.591517	74.093326
393.726037	20.328462	74.098330
392.697289	44.698542	74.103335
391.975596	26.124706	74.108340
391.456918	17.589856	74.113345
390.309628	29.540645	74.118350
389.655105	17.552071	74.123354
388.948543	22.860334	74.128359
388.225881	40.257702	74.133364
388.354355	18.855148	74.138369
387.503603	22.278404	74.143374
386.504059	32.018568	74.148378
385.812439	31.947405	74.153383
385.183626	14.276512	74.158388
384.947448	34.478826	74.163393
384.285753	13.700478	74.168398
383.636045	19.083254	74.173402
382.787989	24.622210	74.178407
381.554410	28.319347	74.183412
380.929696	18.011676	74.188417
380.337303	26.442826	74.193422
380.258537	19.890932	74.198426
379.295959	24.175623	74.203431
378.976153	24.609724	74.208436
377.951397	20.944404	74.213441
377.446143	19.236740	74.218446
377.011762	6.166075	74.223450
375.915549	19.698181	74.228455
374.659792	25.089234	74.233460
374.267572	14.624678	74.238465
373.712155	31.087122	74.243470
373.885450	20.537176	74.248474
373.431193	8.056264	74.253479
372.245572	22.925594	74.258484
371.708065	2.416041	74.263489
370.715340	22.929695	74.268494
369.595924	21.228446	74.273498
368.921116	26.591575	74.278503
368.534629	11.159044	74.283508
368.671184	10.722538	74.288513
367.710609	26.869523	74.293518
367.195546	16.695761	74.298522
365.933290	19.749390	74.303527
365.347670	35.251623	74.308532
365.192324	5.653720	74.313537
363.879897	26.902678	74.318542
363.598516	12.254436	74.323546
363.074215	22.256311	74.328551
361.784824	14.787246	74.333556
361.045730	32.683932	74.338561
360.434647	10.486257	74.343566
360.230272	12.105097	74.348570
359.752060	19.991384	74.353575
359.440730	26.118128	74.358580
358.775626	19.317499	74.363585
357.927059	24.638939	74.368590
357.329139	8.366536	74.373594
355.910463	43.018290	74.378599
355.211131	24.105043	74.383604
355.220380	18.376431	74.388609
354.142846	18.647456	74.393614
353.339060	18.933199	74.398618
352.627403	29.791205	74.403623
352.448000	30.513573	74.408628
352.152802	29.455213	74.413633
350.674155	28.287427	74.418638
350.070588	12.006463	74.423642
349.422214	27.927092	74.428647
349.209894	25.609816	74.433652
348.653395	29.098148	74.438657
347.441220	34.073868	74.443662
347.260441	27.047831	74.448666
346.365513	36.265170	74.453671
345.050188	26.493314	74.458676
344.440559	34.205026	74.463681
343.772472	36.962142	74.468686
343.799544	20.227454	74.473690
343.296062	33.261448	74.478695
342.918984	28.302405	74.483700
342.204250	20.522585	74.488705
341.280572	26.587657	74.493710
340.517156	19.974578	74.498714
339.684495	30.907061	74.503719
338.512011	18.941133	74.508724
337.789119	37.095424	74.513729
337.751839	3.415185	74.518734
337.528349	35.279388	74.523738
336.483047	25.079754	74.528743
335.748138	28.232271	74.533748
335.416246	23.756428	74.538753
334.759816	21.226100	74.543758
333.920327	11.794715	74.548762
332.677533	28.909141	74.553767
332.392660	14.734516	74.558772
332.251598	17.705662	74.563777
331.123179	22.753186	74.568782
330.334834	20.775280	74.573786
329.509340	27.097502	74.578791
329.050184	30.887270	74.583796
328.734409	20.476767	74.588801
327.681460	24.430550	74.593806
327.549150	9.227166	74.598810
326.562703	35.487442	74.603815
325.616686	32.495523	74.608820
324.867680	21.412948	74.613825
324.341335	37.200608	74.618830
324.353117	23.942151	74.623834
323.590699	23.347738	74.628839
322.324369	30.741519	74.633844
322.075580	20.990500	74.638849
321.155889	31.069593	74.643854
320.735485	27.867759	74.648858
319.673700	26.849582	74.653863
319.166702	23.199535	74.658868
318.967799	14.161190	74.663873
318.000020	19.615171	74.668878
316.921532	21.789616	74.673882
316.228213	30.995327	74.678887
315.986765	16.291847	74.683892
315.749059	16.837442	74.688897
314.586163	43.575256	74.693902
314.180383	13.326612	74.698906
313.411104	31.828890	74.703911
312.519842	33.375874	74.708916
311.731666	22.695335	74.713921
311.054000	21.759436	74.718926
310.901361	16.466608	74.723930
310.546586	33.223486	74.728935
309.300879	19.400683	74.733940
308.916489	17.057225	74.738945
307.693155	24.724834	74.743950
307.647903	14.216035	74.748954
306.427150	30.295702	74.753959
305.394289	29.917852	74.758964
305.310837	26.846808	74.763969
304.783521	26.997046	74.768974
304.538356	21.649583	74.773978
303.366805	29.660580	74.778983
302.802888	31.144355	74.783988
302.230494	24.562341	74.788993
301.368866	39.146698	74.793998
300.784932	35.294463	74.799002
299.878509	18.110945	74.804007
299.060700	22.918178	74.809012
299.152164	16.876865	74.814017
298.269024	9.953330	74.819022
297.341048	5.768035	74.824026
296.726958	30.411036	74.829031
296.542460	24.205562	74.834036
295.701022	9.484192	74.839041
294.136351	22.739354	74.844046
293.937359	32.348794	74.849050
294.101684	20.475731	74.854055
292.850164	16.927014	74.859060
292.017042	30.239037	74.864065
291.273691	33.022353	74.869070
291.088464	14.400921	74.874074
290.216356	6.837010	74.879079
289.146881	36.294171	74.884084
288.629200	19.483906	74.889089
287.836474	18.375555	74.894094
287.854513	16.546659	74.899098
287.412505	11.795088	74.904103
286.104235	21.748474	74.909108
285.552542	19.586217	74.914113
284.912901	20.285759	74.919118
284.311716	27.920442	74.924122
283.576350	18.671161	74.929127
282.739556	16.721493	74.934132
282.635042	18.521528	74.939137
281.411751	30.181713	74.944142
280.863673	20.109427	74.949146
280.241862	23.351155	74.954151
279.675870	24.439478	74.959156
279.217856	20.608180	74.964161
277.658272	28.909679	74.969166
277.564234	20.993104	74.974170
276.907247	23.431519	74.979175
276.559329	17.632118	74.984180
276.003968	12.476022	74.989185
274.654911	29.046048	74.994190
274.523407	29.927932	74.999194
274.013844	24.275711	75.004199
273.222919	14.421900	75.009204
272.294479	17.357714	75.014209
271.376176	32.003139	75.019214
271.313910	9.164558	75.024218
270.633683	13.651842	75.029223
269.604449	24.193074	75.034228
269.029156	18.532411	75.039233
268.426790	34.215502	75.044238
267.911812	22.043892	75.049242
267.196674	17.955559	75.054247
266.507757	18.421703	75.059252
265.941243	19.158476	75.064257
264.834406	16.960143	75.069262
264.118428	14.169688	75.074266
263.554362	25.972362	75.079271
263.001503	29.408094	75.084276
262.920237	23.064753	75.089281
261.943364	31.847349	75.094286
261.474930	13.149653	75.099290
260.389544	16.634000	75.104295
259.117299	24.063437	75.109300
258.540466	26.954249	75.114305
257.958301	23.169552	75.119310
257.895085	20.230896	75.124314
257.806774	24.567068	75.129319
256.649946	28.111689	75.134324
255.997663	21.121408	75.139329
255.251718	24.450733	75.144334
254.552770	24.221514	75.149338
253.718633	22.216243	75.154343
253.164712	31.011840	75.159348
252.511535	11.873698	75.164353
251.827228	38.677142	75.169358
251.353513	28.036379	75.174362
250.541520	19.565672	75.179367
249.634843	20.512779	75.184372
249.475561	21.706576	75.189377
249.035733	17.536520	75.194382
248.298780	26.977837	75.199386
247.670940	22.367850	75.204391
246.340991	23.950095	75.209396
245.394009	22.060579	75.214401
244.732050	35.963455	75.219406
244.702929	15.808109	75.224410
243.941771	17.689165	75.229415
243.499015	29.051489	75.234420
243.454281	19.026703	75.239425
242.053276	23.803924	75.244430
241.342660	17.994543	75.249434
240.335840	24.432418	75.254439
239.222121	30.526240	75.259444
239.130236	25.539102	75.264449
238.479939	27.968576	75.269454
238.245485	12.729456	75.274458
237.832488	18.382012	75.279463
236.892804	19.053707	75.284468
236.249132	26.217386	75.289473
235.593318	17.352809	75.294478
234.444246	22.966597	75.299482
234.032915	19.963596	75.304487
233.505601	16.852937	75.309492
233.024403	13.963569	75.314497
231.792206	20.134619	75.319502
231.164222	24.470095	75.324506
230.812735	16.884709	75.329511
229.812133	25.089238	75.334516
229.926529	19.891036	75.339521
228.472369	15.661924	75.344526
227.908229	20.425584	75.349530
227.554260	23.992030	75.354535
226.667003	24.035673	75.359540
226.215131	32.081774	75.364545
225.243711	26.862712	75.369550
225.083604	20.743241	75.374554
224.737700	14.560358	75.379559
223.291861	23.630595	75.384564
222.702854	23.071644	75.389569
221.850270	35.795472	75.394574
221.628670	18.341988	75.399578
220.926161	20.089131	75.404583
219.942795	28.111157	75.409588
219.626662	14.957033	75.414593
219.311022	23.187978	75.419598
218.403923	14.033908	75.424602
217.857500	11.692646	75.429607
216.737512	23.883546	75.434612
216.224802	23.340817	75.439617
215.299023	21.619809	75.444622
214.498648	29.079692	75.449626
213.949159	33.867830	75.454631
213.764919	26.221089	75.459636
213.255567	25.524871	75.464641
212.102253	14.500498	75.469646
211.313747	23.677245	75.474650
211.168011	24.088347	75.479655
210.272595	25.595030	75.484660
209.798569	26.720743	75.489665
208.856861	23.384435	75.494670
208.045106	24.787901	75.499674
208.070613	19.004670	75.504679
206.708355	23.425673	75.509684
206.749440	16.168765	75.514689
205.307585	30.566531	75.519694
205.231299	19.192272	75.524698
204.392990	16.604252	75.529703
203.205197	22.287300	75.534708
202.815387	23.705496	75.539713
202.542722	19.746903	75.544718
201.454301	22.414954	75.549722
200.741581	23.815249	75.554727
200.233025	28.136422	75.559732
200.235663	16.432638	75.564737
199.593089	24.660517	75.569742
198.352780	34.989441	75.574746
198.090642	21.240123	75.579751
197.084264	29.964367	75.584756
195.909642	23.167759	75.589761
195.031844	23.952598	75.594766
194.734410	23.126411	75.599770
194.383706	9.586754	75.604775
194.003166	19.127362	75.609780
193.370333	32.309710	75.614785
192.220558	34.628029	75.619790
191.725369	23.662729	75.624794
191.271418	7.995028	75.629799
190.427505	38.616219	75.634804
189.841468	22.717267	75.639809
188.829454	19.177727	75.644814
188.446471	32.444813	75.649818
188.315071	23.463528	75.654823
187.134627	31.751936	75.659828
186.627072	28.489912	75.664833
186.106693	28.680067	75.669838
185.069635	22.566382	75.674842
184.067604	13.791714	75.679847
183.305656	22.316151	75.684852
183.140368	17.979345	75.689857
182.805573	20.946692	75.694862
182.192832	17.288310	75.699866
181.453578	25.861166	75.704871
180.445584	29.850414	75.709876
180.350365	26.290857	75.714881
179.417614	23.225928	75.719886
178.300101	27.240521	75.724890
177.685735	18.702070	75.729895
177.318628	22.710555	75.734900
176.685620	19.071173	75.739905
175.728513	30.822991	75.744910
175.263383	24.804192	75.749914
174.935136	16.650603	75.754919
173.799110	29.107411	75.759924
172.823361	17.515468	75.764929
172.396500	23.586529	75.769934
171.875095	29.105003	75.774938
171.854158	23.624047	75.779943
170.766769	31.257426	75.784948
169.915484	26.539595	75.789953
169.052697	28.195621	75.794958
169.060906	26.488133	75.799962
168.293040	25.673880	75.804967
167.092997	31.973869	75.809972
166.939498	13.494061	75.814977
165.900410	29.120636	75.819982
164.976260	25.469332	75.824986
164.741451	20.806168	75.829991
163.878171	24.490093	75.834996
163.788267	31.332123	75.840001
162.854023	39.308496	75.845006
161.994399	36.242950	75.850010
161.555945	29.205989	75.855015
160.876223	36.239826	75.860020
159.952403	21.080671	75.865025
158.973594	33.944476	75.870030
158.419759	33.375202	75.875034
158.147392	20.502675	75.880039
157.523395	26.699781	75.885044
157.034656	28.283557	75.890049
156.132838	24.072071	75.895054
155.331263	31.432820	75.900058
154.967810	25.084023	75.905063
153.826679	29.559677	75.910068
153.288509	26.179550	75.915073
152.800981	33.326236	75.920078
152.299779	34.158269	75.925082
151.850722	27.260188	75.930087
150.832236	35.201113	75.935092
150.134988	20.945636	75.940097
149.488082	22.586169	75.945102
149.150936	19.413672	75.950106
148.203627	23.994031	75.955111
147.192699	26.670249	75.960116
146.876197	15.575560	75.965121
146.413018	15.357662	75.970126
145.116420	20.793173	75.975130
144.822214	25.077023	75.980135
144.096817	28.945537	75.985140
143.712750	20.698359	75.990145
143.192542	20.886919	75.995150
142.171698	28.814027	76.000154
141.831050	16.229919	76.005159
141.146767	20.497124	76.010164
140.127144	19.226318	76.015169
139.555254	26.473180	76.020174
138.944647	33.404543	76.025178
138.572251	32.073112	76.030183
137.459203	27.390723	76.035188
137.171747	22.701266	76.040193
136.536735	23.620866	76.045198
135.471320	25.432205	76.050202
134.869371	21.731117	76.055207
134.001062	29.644944	76.060212
133.565212	23.720829	76.065217
133.196974	21.027922	76.070222
132.443920	23.891668	76.075226
131.466095	19.599280	76.080231
130.873341	27.797152	76.085236
130.453100	19.126845	76.090241
130.025590	26.386954	76.095246
128.818008	26.205761	76.100250
128.434270	24.901370	76.105255
127.618710	32.819405	76.110260
127.201054	26.392530	76.115265
126.717894	27.065583	76.120270
125.243520	30.619898	76.125274
125.307264	27.085457	76.130279
124.420402	31.260400	76.135284
123.548825	18.426665	76.140289
122.967444	29.104674	76.145294
122.287571	36.666785	76.150298
122.173361	21.403783	76.155303
121.003917	38.492398	76.160308
120.517466	30.671525	76.165313
119.751664	23.473902	76.170318
119.301979	25.070380	76.175322
118.564475	26.608680	76.180327
117.599620	27.393237	76.185332
117.134334	29.294956	76.190337
116.630123	33.662757	76.195342
115.566684	33.953714	76.200346
114.952269	27.165583	76.205351
114.207964	32.902525	76.210356
114.522167	25.813363	76.215361
113.231425	26.537931	76.220366
112.151863	26.727389	76.225370
111.591713	26.198555	76.230375
111.302560	29.081367	76.235380
110.890088	19.793281	76.240385
109.998599	17.611141	76.245390
109.035701	27.810709	76.250394
108.825058	29.684438	76.255399
107.950823	32.092887	76.260404
107.186370	24.191782	76.265409
106.430254	11.036897	76.270414
105.766394	20.263169	76.275418
105.616654	18.317538	76.280423
104.151498	25.462438	76.285428
103.640003	17.599842	76.290433
103.187233	25.182503	76.295438
102.622665	26.491396	76.300442
102.242381	24.983045	76.305447
101.053575	29.907840	76.310452
100.482523	28.770508	76.315457
100.112301	13.255051	76.320462
99.514488	34.243496	76.325466
98.845296	29.491924	76.330471
97.864554	21.399826	76.335476
97.597510	26.453578	76.340481
96.825107	30.689120	76.345486
95.684810	32.208087	76.350490
95.049163	18.423751	76.355495
94.795868	12.481576	76.360500
94.268753	28.341893	76.365505
93.656371	25.995409	76.370510
92.820653	32.844415	76.375514
92.562622	18.116831	76.380519
91.211814	30.335125	76.385524
90.436586	26.623836	76.390529
90.225573	35.244933	76.395534
89.360881	25.838166	76.400538
88.861478	23.082611	76.405543
87.574422	41.941866	76.410548
87.124179	23.668651	76.415553
86.877575	21.123500	76.420558
86.377128	22.419016	76.425562
85.733127	36.101442	76.430567
84.626291	25.143836	76.435572
84.357117	24.866628	76.440577
83.388364	25.796889	76.445582
82.222634	30.407374	76.450586
81.860938	22.934025	76.455591
81.136430	28.436020	76.460596
80.484953	19.093024	76.465601
80.460274	25.450017	76.470606
79.519154	34.912894	76.475610
78.890092	26.009412	76.480615
77.885677	28.221026	76.485620
77.552452	23.072133	76.490625
77.222926	20.917073	76.495630
76.110327	27.397104	76.500634
75.736247	31.343640	76.505639
74.732594	29.980435	76.510644
74.341798	28.557338	76.515649
73.627366	17.627045	76.520654
72.467596	32.989062	76.525658
72.191597	22.212757	76.530663
71.598191	33.028302	76.535668
71.390925	27.419382	76.540673
70.329653	22.525360	76.545678
69.650995	27.430306	76.550682
69.273291	23.385990	76.555687
67.822946	30.809227	76.560692
67.460353	17.386606	76.565697
66.875763	28.386808	76.570702
66.305068	30.617561	76.575706
65.942933	21.420800	76.580711
64.683773	22.913008	76.585716
64.382905	28.963990	76.590721
64.137120	22.787246	76.595726
62.808651	26.160642	76.600730
62.352940	19.988995	76.605735
61.628376	26.966926	76.610740
61.049448	24.514198	76.615745
59.982162	28.861428	76.620750
59.248311	22.912322	76.625754
58.791914	27.624141	76.630759
58.198757	27.100583	76.635764
57.879699	20.211757	76.640769
57.583858	19.897807	76.645774
56.274536	16.465664	76.650778
55.615710	34.411078	76.655783
55.289242	22.794485	76.660788
54.755674	20.424405	76.665793
53.997598	20.526350	76.670798
53.098330	28.260646	76.675802
52.571647	20.384717	76.680807
51.166667	25.662530	76.685812
50.855319	18.168547	76.690817
50.503133	22.206202	76.695822
49.958613	25.408848	76.700826
49.418394	28.237097	76.705831
48.430151	17.337869	76.710836
48.138025	26.164271	76.715841
47.305046	30.527750	76.720846
46.198342	28.460376	76.725850
45.832425	17.711036	76.730855
45.065992	29.325252	76.735860
44.468548	26.796639	76.740865
43.442927	27.157284	76.745870
42.632350	33.231219	76.750874
42.521138	29.502346	76.755879
42.159859	37.527712	76.760884
41.448923	33.847183	76.765889
40.710931	34.330677	76.770894
39.846889	39.172168	76.775898
39.585538	22.272235	76.780903
38.322823	31.988248	76.785908
37.241468	32.146489	76.790913
37.051954	30.420079	76.795918
36.522099	38.499138	76.800922
36.445987	23.342031	76.805927
35.161284	24.674337	76.810932
34.302503	28.967823	76.815937
34.038581	24.572653	76.820942
33.460088	30.242169	76.825946
32.806035	17.797956	76.830951
31.724718	32.701227	76.835956
31.105580	31.212062	76.840961
30.779677	24.973990	76.845966
29.954325	32.680737	76.850970
29.101218	19.834641	76.855975
28.284579	36.455455	76.860980
27.981103	29.395423	76.865985
27.735568	25.399415	76.870990
26.743616	33.875427	76.875994
25.990099	21.177439	76.880999
25.216699	27.560814	76.886004
24.866656	32.137412	76.891009
23.982824	24.152886	76.896014
22.944439	25.679284	76.901018
22.785285	24.637113	76.906023
22.069423	15.075769	76.911028
21.341196	25.483917	76.916033
20.682614	27.361293	76.921038
20.137566	22.957352	76.926042
19.873103	19.426380	76.931047
18.594154	13.515354	76.936052
17.690918	36.222389	76.941057
17.486704	19.981933	76.946062
16.589030	14.631369	76.951066
16.642467	22.953254	76.956071
15.417745	22.088926	76.961076
14.284760	19.738775	76.966081
14.316342	21.889243	76.971086
13.558115	12.754100	76.976090
12.460743	17.848835	76.981095
11.762510	30.767264	76.986100
11.684849	14.298487	76.991105
11.434995	13.210865	76.996110
9.915446	41.754330	77.001114
9.695898	16.850006	77.006119
8.740866	19.922608	77.011124
8.289572	17.167283	77.016129
7.489800	10.881812	77.021134
6.713343	26.972699	77.026139
6.521757	23.542059	77.031143
5.432906	25.636292	77.036148
4.698723	21.883798	77.041153
4.473283	18.196804	77.046158