Mon Mar 08 20:26:30 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.978805	102.364014	0.000000
-1.159086	104.940887	0.005005
-2.279346	81.280836	0.010010
-5.392917	81.255524	0.015014
-8.928590	75.464820	0.020019
-13.210964	34.298642	0.025024
-17.337233	59.886615	0.030029
-21.569670	45.315311	0.035034
-26.260481	26.135536	0.040038
-29.933551	46.581684	0.045043
-33.512678	53.660217	0.050048
-37.649237	41.829963	0.055053
-41.120740	28.465014	0.060058
-45.370335	44.745706	0.065062
-48.405408	29.158759	0.070067
-52.879343	21.398573	0.075072
-56.720433	39.968315	0.080077
-59.985880	36.529805	0.085082
-63.508972	42.136133	0.090086
-67.055518	39.267567	0.095091
-71.363254	44.351016	0.100096
-75.332325	50.391191	0.105101
-78.890254	33.372367	0.110106
-82.538530	33.210136	0.115110
-85.965399	46.012005	0.120115
-89.585763	24.706297	0.125120
-94.166111	34.402941	0.130125
-97.741593	30.050510	0.135130
-101.700687	23.419276	0.140134
-105.543573	34.628714	0.145139
-109.456903	49.748919	0.150144
-113.151766	31.971470	0.155149
-116.904599	29.850203	0.160154
-120.428458	35.276971	0.165158
-123.974083	41.951341	0.170163
-127.721014	41.169456	0.175168
-131.670316	44.380877	0.180173
-134.733623	34.183443	0.185178
-139.291911	37.383253	0.190182
-142.695911	44.766701	0.195187
-146.497223	26.689360	0.200192
-150.511699	29.007684	0.205197
-154.118374	52.209168	0.210202
-158.196082	30.577615	0.215206
-161.332305	43.566567	0.220211
-165.252751	47.503511	0.225216
-169.426404	38.192897	0.230221
-173.148113	36.727443	0.235226
-176.991609	45.934514	0.240230
-180.592870	42.437809	0.245235
-184.318269	40.922503	0.250240
-188.010186	41.530583	0.255245
-191.319897	36.647057	0.260250
-195.236424	45.823237	0.265254
-199.149623	41.559547	0.270259
-203.036855	42.238244	0.275264
-207.126580	46.058780	0.280269
-210.367665	32.274149	0.285274
-214.341851	46.377699	0.290278
-217.857991	36.769856	0.295283
-221.776426	35.351646	0.300288
-225.809065	44.226308	0.305293
-229.410808	32.497118	0.310298
-233.275506	46.960083	0.315302
-236.748413	32.649565	0.320307
-240.593771	27.939916	0.325312
-244.494216	33.381239	0.330317
-247.874921	25.579380	0.335322
-251.990927	33.401447	0.340326
-255.935857	33.283678	0.345331
-259.703638	33.142368	0.350336
-263.400254	39.235531	0.355341
-266.690703	35.038114	0.360346
-271.079008	44.888915	0.365350
-274.461019	31.551046	0.370355
-278.272291	28.329275	0.375360
-282.264132	38.058458	0.380365
-285.538905	34.104552	0.385370
-289.539883	34.755818	0.390374
-293.099099	35.979913	0.395379
-297.124188	42.909250	0.400384
-300.928287	35.957164	0.405389
-304.638619	43.809168	0.410394
-308.737927	44.990210	0.415398
-312.174594	41.290826	0.420403
-316.230193	40.263648	0.425408
-319.743646	36.921861	0.430413
-323.084492	35.373760	0.435418
-327.131734	45.463496	0.440422
-330.762941	39.835198	0.445427
-334.773720	44.001282	0.450432
-338.341411	35.483565	0.455437
-342.370018	37.646779	0.460442
-346.392808	43.426319	0.465446
-349.850497	38.837862	0.470451
-353.709254	50.982117	0.475456
-357.340972	41.148535	0.480461
-360.855536	35.074342	0.485466
-364.834360	44.864653	0.490470
-368.821145	37.535027	0.495475
-372.511252	33.614448	0.500480
-376.143431	37.523041	0.505485
-379.537853	31.278319	0.510490
-383.814316	40.220545	0.515494
-387.711282	38.393935	0.520499
-391.445548	39.808541	0.525504
-395.035774	28.675404	0.530509
-398.556928	43.939965	0.535514
-402.453392	34.691167	0.540518
-406.219741	32.766467	0.545523
-409.875185	42.789035	0.550528
-413.549567	47.413998	0.555533
-417.527499	35.084496	0.560538
-421.340567	47.130097	0.565542
-425.148200	37.659009	0.570547
-428.567199	31.482934	0.575552
-432.695428	33.554983	0.580557
-436.327279	26.094688	0.585562
-440.389053	51.374929	0.590566
-443.799722	44.202562	0.595571
-447.849592	37.129135	0.600576
-451.479778	37.581115	0.605581
-455.112524	18.835646	0.610586
-458.820909	50.043526	0.615590
-462.813126	38.261968	0.620595
-466.475880	41.018187	0.625600
-470.295350	35.626745	0.630605
-474.120226	45.933490	0.635610
-477.617620	21.147688	0.640614
-481.497577	43.111253	0.645619
-485.386329	30.900088	0.650624
-489.410868	26.564796	0.655629
-492.333187	43.041018	0.660634
-496.106930	41.660069	0.665638
-499.882178	29.282580	0.670643
-503.969033	41.827731	0.675648
-507.645102	34.765662	0.680653
-511.632754	24.495651	0.685658
-515.584165	58.505034	0.690662
-518.820204	31.780613	0.695667
-522.778058	29.445179	0.700672
-526.707540	47.859407	0.705677
-530.301228	46.512824	0.710682
-534.454052	50.500091	0.715686
-538.076734	31.092452	0.720691
-541.579381	40.151009	0.725696
-545.721884	24.169304	0.730701
-548.784965	43.254064	0.735706
-552.924518	42.709020	0.740710
-556.843307	34.105826	0.745715
-560.415078	33.829607	0.750720
-564.506255	36.309091	0.755725
-567.983016	43.898680	0.760730
-571.865181	39.149729	0.765734
-575.784380	57.707465	0.770739
-579.460518	27.016786	0.775744
-583.164256	66.403097	0.780749
-586.594807	21.849159	0.785754
-590.362384	58.109353	0.790758
-594.272255	37.743247	0.795763
-597.714920	33.988480	0.800768
-601.618476	58.141484	0.805773
-605.354635	40.139687	0.810778
-609.761892	51.063193	0.815782
-613.382088	45.802560	0.820787
-617.365771	39.430007	0.825792
-620.867292	51.304710	0.830797
-624.111804	20.735960	0.835802
-628.335137	39.720782	0.840806
-631.845337	50.549873	0.845811
-635.327949	38.042280	0.850816
-639.754477	35.780353	0.855821
-643.039587	43.039826	0.860826
-647.219009	31.851448	0.865830
-650.675592	53.802801	0.870835
-654.315664	15.720675	0.875840
-658.192083	57.542446	0.880845
-661.807283	23.612854	0.885850
-666.298071	37.102671	0.890854
-669.787866	38.136473	0.895859
-673.756804	41.405520	0.900864
-677.112276	38.199863	0.905869
-680.568503	30.325573	0.910874
-684.486459	37.421323	0.915878
-688.131106	29.723799	0.920883
-691.938177	36.379252	0.925888
-695.771647	44.150593	0.930893
-699.707970	19.984062	0.935898
-703.569482	42.529987	0.940902
-707.244867	35.862340	0.945907
-710.866789	26.456678	0.950912
-714.602236	45.217026	0.955917
-718.296837	35.204871	0.960922
-722.246678	31.365783	0.965926
-726.019959	31.085753	0.970931
-730.024860	25.625046	0.975936
-733.736931	46.426823	0.980941
-737.359395	34.113624	0.985946
-741.256955	26.387231	0.990950
-745.109491	37.249108	0.995955
-748.433669	41.958934	1.000960
-752.087564	40.087772	1.005965
-755.898330	27.197630	1.010970
-759.610072	35.230282	1.015974
-763.697987	26.640297	1.020979
-767.017622	36.187107	1.025984
-771.312576	48.911018	1.030989
-774.740017	33.042510	1.035994
-778.659251	37.953139	1.040998
-782.311346	51.756929	1.046003
-786.251939	32.063100	1.051008
-789.961186	36.446635	1.056013
-793.566000	32.768541	1.061018
-797.556452	36.714532	1.066022
-801.270078	39.700145	1.071027
-804.867149	38.195266	1.076032
-808.737943	40.636783	1.081037
-812.680188	30.798408	1.086042
-816.535475	38.152408	1.091046
-820.409702	37.803519	1.096051
-823.669991	32.845205	1.101056
-827.746868	32.629641	1.106061
-831.374035	33.978930	1.111066
-835.232336	37.012953	1.116070
-838.682273	31.052163	1.121075
-842.590495	38.137146	1.126080
-846.765955	34.619746	1.131085
-850.060644	31.619074	1.136090
-853.903691	36.788856	1.141094
-857.430914	31.685626	1.146099
-861.128279	32.212046	1.151104
-865.226815	41.055688	1.156109
-868.894966	36.667231	1.161114
-872.680424	40.768214	1.166118
-876.502821	33.977705	1.171123
-879.850868	27.694785	1.176128
-884.083549	37.195363	1.181133
-887.733864	40.740219	1.186138
-891.758861	34.526133	1.191142
-895.057960	35.122955	1.196147
-898.682435	26.807593	1.201152
-903.064468	40.573728	1.206157
-906.786483	31.745738	1.211162
-910.713117	44.347913	1.216166
-913.792024	28.855955	1.221171
-917.260500	21.360857	1.226176
-921.544344	34.754957	1.231181
-925.298657	35.492416	1.236186
-928.966266	34.162999	1.241190
-932.864076	30.943527	1.246195
-936.809889	26.331525	1.251200
-940.517115	33.160611	1.256205
-944.462233	22.988652	1.261210
-948.075496	35.176519	1.266214
-951.703795	39.853260	1.271219
-955.061887	37.220815	1.276224
-959.304652	42.699096	1.281229
-963.104578	20.482289	1.286234
-966.938166	32.394782	1.291238
-970.652765	40.784569	1.296243
-974.226745	23.823447	1.301248
-977.705135	29.017098	1.306253
-981.712056	25.372076	1.311258
-985.669907	43.771007	1.316262
-989.337456	36.508108	1.321267
-993.103830	26.941526	1.326272
-997.106646	25.131289	1.331277
-1000.477019	38.084561	1.336282
-1004.363349	28.152440	1.341286
-1008.383615	32.630205	1.346291
-1011.873792	35.209853	1.351296
-1015.654746	37.809209	1.356301
-1018.991211	22.055863	1.361306
-1022.959198	33.248834	1.366310
-1026.921525	33.622370	1.371315
-1030.542625	25.987871	1.376320
-1034.760015	28.546688	1.381325
-1038.295695	33.025832	1.386330
-1042.155980	29.236045	1.391334
-1045.829638	27.661798	1.396339
-1049.531558	26.476821	1.401344
-1053.241432	22.904247	1.406349
-1056.646163	8.667755	1.411354
-1060.555614	29.121509	1.416358
-1064.786326	35.149930	1.421363
-1068.222002	17.168730	1.426368
-1072.228770	37.166612	1.431373
-1075.877047	26.468050	1.436378
-1079.872281	20.844005	1.441382
-1083.389650	28.718321	1.446387
-1086.810971	25.052336	1.451392
-1090.704082	33.130264	1.456397
-1094.274704	26.039679	1.461402
-1098.282346	34.028720	1.466406
-1102.218029	28.075091	1.471411
-1105.779357	23.220540	1.476416
-1110.010495	43.167658	1.481421
-1113.212846	28.764830	1.486426
-1117.274762	34.763184	1.491430
-1120.793387	25.461512	1.496435
-1124.777881	23.998618	1.501440
-1128.374554	32.320889	1.506445
-1132.260465	37.538968	1.511450
-1136.133717	29.842490	1.516454
-1139.627757	27.884871	1.521459
-1143.347068	32.954896	1.526464
-1147.458640	39.065317	1.531469
-1150.718305	26.626970	1.536474
-1154.666957	33.114998	1.541478
-1158.936355	39.372106	1.546483
-1162.417280	29.458969	1.551488
-1165.990124	22.781983	1.556493
-1169.803860	24.994202	1.561498
-1173.696396	33.702896	1.566502
-1177.802567	40.447961	1.571507
-1181.180774	26.462853	1.576512
-1184.982406	34.141551	1.581517
-1188.611327	25.885721	1.586522
-1192.186482	27.503184	1.591526
-1196.089796	30.508726	1.596531
-1199.600651	28.629577	1.601536
-1203.660156	46.195201	1.606541
-1207.229133	25.737880	1.611546
-1211.485411	34.304587	1.616550
-1215.263261	32.882890	1.621555
-1218.672433	21.181299	1.626560
-1222.628847	36.630130	1.631565
-1226.177933	29.403858	1.636570
-1229.718537	25.280981	1.641574
-1234.066338	21.782414	1.646579
-1237.161867	24.173088	1.651584
-1241.405273	29.377598	1.656589
-1245.036944	29.012673	1.661594
-1249.208881	24.765384	1.666598
-1252.752487	37.125445	1.671603
-1255.815456	28.556815	1.676608
-1260.108002	32.641804	1.681613
-1263.828792	32.062534	1.686618
-1267.362686	25.483546	1.691622
-1271.597636	35.239014	1.696627
-1275.640429	28.624806	1.701632
-1279.069333	35.985396	1.706637
-1282.282177	17.393353	1.711642
-1285.972090	24.494553	1.716646
-1290.322485	21.854295	1.721651
-1294.014582	32.626677	1.726656
-1298.003483	34.140233	1.731661
-1301.899820	32.848021	1.736666
-1305.280703	25.639106	1.741670
-1308.691121	22.025324	1.746675
-1312.542792	41.013240	1.751680
-1316.495328	41.772021	1.756685
-1320.232798	20.466749	1.761690
-1323.907962	27.582992	1.766694
-1327.968769	26.575751	1.771699
-1331.548838	30.816451	1.776704
-1335.555645	32.157911	1.781709
-1338.993032	22.108797	1.786714
-1342.815753	33.876632	1.791718
-1346.811925	30.586892	1.796723
-1350.033979	22.564215	1.801728
-1354.263795	37.336416	1.806733
-1358.004732	29.098799	1.811738
-1361.579737	25.776350	1.816742
-1365.668441	30.074878	1.821747
-1369.012404	16.925042	1.826752
-1373.222712	33.474365	1.831757
-1376.400574	20.238026	1.836762
-1380.312246	25.306100	1.841766
-1384.130188	24.491867	1.846771
-1387.911955	18.808969	1.851776
-1392.217480	30.107024	1.856781
-1395.669559	13.168125	1.861786
-1399.190341	27.654996	1.866790
-1403.273682	25.722756	1.871795
-1406.610212	27.136775	1.876800
-1410.602448	41.658165	1.881805
-1414.458145	26.666620	1.886810
-1418.255205	45.571842	1.891814
-1421.926045	26.301206	1.896819
-1425.237007	23.720254	1.901824
-1429.046266	40.985981	1.906829
-1433.207452	34.750528	1.911834
-1436.888125	10.434148	1.916838
-1441.031324	42.863918	1.921843
-1444.365286	12.826550	1.926848
-1448.244370	36.095349	1.931853
-1451.852560	33.659792	1.936858
-1455.618742	34.217097	1.941862
-1459.548286	36.221274	1.946867
-1463.107969	27.510152	1.951872
-1466.822202	20.233458	1.956877
-1470.455453	34.765251	1.961882
-1474.319121	25.008525	1.966886
-1478.179976	11.173741	1.971891
-1481.566380	22.113461	1.976896
-1485.607232	33.943253	1.981901
-1489.698042	28.286365	1.986906
-1493.297837	34.386372	1.991910
-1497.210516	17.521406	1.996915
-1501.193965	37.202694	2.006912
-1501.896766	23.865095	2.016909
-1499.439349	32.887521	2.026906
-1496.585489	28.996386	2.036902
-1494.573700	22.472433	2.046899
-1492.444704	21.765053	2.056896
-1490.649403	25.214487	2.066893
-1489.169836	34.728242	2.076890
-1487.064592	27.650945	2.086886
-1485.081134	25.430681	2.096883
-1483.330466	28.666234	2.106880
-1481.085929	28.063510	2.116877
-1479.093352	21.889988	2.126874
-1477.646711	30.499617	2.136870
-1475.455360	30.486425	2.146867
-1473.375141	14.319109	2.156864
-1471.671972	29.054556	2.166861
-1470.130497	21.630224	2.176858
-1467.756324	31.442801	2.186854
-1465.815427	23.741365	2.196851
-1464.282631	42.939042	2.206848
-1462.584512	24.223109	2.216845
-1460.184434	32.659545	2.226842
-1458.273029	26.099593	2.236838
-1456.691835	36.485979	2.246835
-1454.842842	27.400425	2.256832
-1452.678464	22.718245	2.266829
-1450.725289	25.927710	2.276826
-1449.399353	28.441890	2.286822
-1447.316709	33.563114	2.296819
-1445.267557	23.888190	2.306816
-1443.510495	30.447763	2.316813
-1441.410122	27.079952	2.326810
-1439.531265	31.404930	2.336806
-1437.632883	21.983086	2.346803
-1435.879093	33.666486	2.356800
-1434.239560	19.273315	2.366797
-1432.036854	26.315704	2.376794
-1430.078939	20.413015	2.386790
-1428.334703	27.299891	2.396787
-1426.729613	28.796827	2.406784
-1424.658275	22.474958	2.416781
-1422.788434	20.195577	2.426778
-1420.960709	18.593944	2.436774
-1418.849871	29.115005	2.446771
-1416.992283	18.804515	2.456768
-1415.076253	25.695470	2.466765
-1413.222970	25.640158	2.476762
-1411.501663	21.459978	2.486758
-1409.775463	20.837694	2.496755
-1407.585464	21.071079	2.506752
-1405.714923	24.200664	2.516749
-1404.352938	27.517460	2.526746
-1402.273099	28.328973	2.536742
-1400.161025	21.669047	2.546739
-1397.866580	35.253662	2.556736
-1396.155149	25.703896	2.566733
-1394.667458	36.799987	2.576730
-1392.992855	32.077862	2.586726
-1390.579766	30.164651	2.596723
-1388.679119	18.454759	2.606720
-1386.892384	25.039623	2.616717
-1385.038471	23.460665	2.626714
-1383.170982	28.090645	2.636710
-1381.518656	14.821165	2.646707
-1379.742805	24.685424	2.656704
-1377.620016	23.039741	2.666701
-1375.607280	25.330332	2.676698
-1373.968279	32.403038	2.686694
-1372.077825	28.018975	2.696691
-1370.040098	32.692761	2.706688
-1368.063352	25.279321	2.716685
-1366.431030	31.686837	2.726682
-1364.609907	19.479731	2.736678
-1362.605181	26.935964	2.746675
-1360.630755	29.297435	2.756672
-1359.027450	28.765910	2.766669
-1357.138550	24.652088	2.776666
-1354.918911	30.023025	2.786662
-1353.113751	27.673533	2.796659
-1351.364878	24.333655	2.806656
-1349.500371	24.533948	2.816653
-1347.378879	26.860834	2.826650
-1345.586102	23.989159	2.836646
-1343.872039	23.708315	2.846643
-1341.910815	25.861930	2.856640
-1339.872341	21.653130	2.866637
-1338.151271	33.978123	2.876634
-1336.163389	23.842602	2.886630
-1334.366644	31.011657	2.896627
-1332.929236	30.677221	2.906624
-1330.877935	23.063996	2.916621
-1329.065970	40.118835	2.926618
-1326.944463	30.798706	2.936614
-1324.923090	28.556718	2.946611
-1322.892178	27.719943	2.956608
-1321.238053	28.752824	2.966605
-1319.619967	32.139196	2.976602
-1317.525775	36.483492	2.986598
-1315.488177	35.427774	2.996595
-1313.656310	25.105680	3.006592
-1312.080060	37.308629	3.016589
-1310.332364	28.124136	3.026586
-1308.167212	32.207625	3.036582
-1306.343235	31.572923	3.046579
-1304.302011	30.169293	3.056576
-1302.351815	34.178257	3.066573
-1300.500308	34.525922	3.076570
-1298.950918	39.034805	3.086566
-1296.878650	35.780557	3.096563
-1294.852285	40.100997	3.106560
-1293.315147	41.389450	3.116557
-1291.339967	27.267864	3.126554
-1289.367311	37.695930	3.136550
-1287.225393	31.323402	3.146547
-1285.288049	29.672751	3.156544
-1284.230286	33.753528	3.166541
-1281.730646	34.084303	3.176538
-1279.818988	33.776616	3.186534
-1278.152385	39.892949	3.196531
-1276.195885	34.978951	3.206528
-1274.271079	30.692087	3.216525
-1272.490611	35.917104	3.226522
-1270.866922	33.001500	3.236518
-1268.858160	34.230271	3.246515
-1266.880958	31.018106	3.256512
-1264.842494	25.055287	3.266509
-1262.785492	27.550458	3.276506
-1261.439038	39.769705	3.286502
-1259.701177	33.188733	3.296499
-1257.515027	37.223126	3.306496
-1255.432700	34.380958	3.316493
-1253.815933	30.126045	3.326490
-1251.805738	34.471216	3.336486
-1249.931182	24.164436	3.346483
-1247.876633	30.752345	3.356480
-1246.096076	20.604288	3.366477
-1244.318426	34.366519	3.376474
-1242.513272	30.831408	3.386470
-1240.906609	28.756909	3.396467
-1238.483281	41.400627	3.406464
-1236.717456	28.225149	3.416461
-1235.021616	27.432603	3.426458
-1233.263406	31.953897	3.436454
-1231.225585	41.189047	3.446451
-1229.247991	24.908856	3.456448
-1227.457388	29.150253	3.466445
-1225.315289	32.647030	3.476442
-1223.900459	29.509111	3.486438
-1221.679577	39.074947	3.496435
-1220.007145	22.949382	3.506432
-1217.855557	39.037413	3.516429
-1216.227190	25.253994	3.526426
-1214.416056	33.968106	3.536422
-1212.264990	25.437496	3.546419
-1210.776031	34.346843	3.556416
-1208.948433	32.841701	3.566413
-1206.740875	33.793995	3.576410
-1204.688524	27.764270	3.586406
-1203.000917	30.373869	3.596403
-1201.154895	41.292780	3.606400
-1199.119413	25.664875	3.616397
-1197.377321	29.822488	3.626394
-1195.682250	24.925130	3.636390
-1193.818562	34.805501	3.646387
-1191.689823	25.345391	3.656384
-1189.788262	38.795764	3.666381
-1188.118534	37.154859	3.676378
-1186.296433	31.094103	3.686374
-1184.420860	31.701676	3.696371
-1182.301388	37.745616	3.706368
-1180.278313	25.558411	3.716365
-1178.710777	27.994624	3.726362
-1176.813465	33.576784	3.736358
-1174.871705	30.293003	3.746355
-1173.023054	30.562287	3.756352
-1171.306669	29.182331	3.766349
-1169.138473	34.789044	3.776346
-1167.305050	31.476817	3.786342
-1165.916406	36.145717	3.796339
-1163.586723	29.762197	3.806336
-1161.297979	29.468475	3.816333
-1159.684887	28.992360	3.826330
-1158.077267	28.315030	3.836326
-1156.474665	34.056462	3.846323
-1154.358545	28.858093	3.856320
-1152.229578	21.295738	3.866317
-1150.602108	27.219494	3.876314
-1148.757118	39.671664	3.886310
-1146.664717	24.339406	3.896307
-1144.623932	23.944858	3.906304
-1142.927958	28.514074	3.916301
-1140.891907	29.298097	3.926298
-1139.321123	23.915436	3.936294
-1137.416282	33.618760	3.946291
-1135.457341	23.505386	3.956288
-1133.797458	26.929414	3.966285
-1131.768821	33.084244	3.976282
-1129.753032	27.092007	3.986278
-1127.993672	26.052551	3.996275
-1125.987017	21.812706	4.006272
-1124.395396	33.860200	4.016269
-1122.333130	34.359013	4.026266
-1120.413658	25.944473	4.036262
-1118.238082	18.066819	4.046259
-1116.904397	26.456376	4.056256
-1114.871593	24.280628	4.066253
-1113.049711	33.577277	4.076250
-1110.871044	32.173929	4.086246
-1109.358628	36.630445	4.096243
-1107.444967	32.451277	4.106240
-1105.426338	27.625363	4.116237
-1103.673404	41.716924	4.126234
-1101.551388	38.693289	4.136230
-1100.230672	36.550953	4.146227
-1097.742575	28.335965	4.156224
-1096.235646	30.384066	4.166221
-1094.487448	32.357257	4.176218
-1091.928755	35.517536	4.186214
-1090.360104	30.649945	4.196211
-1088.466559	19.628188	4.206208
-1086.673308	33.909083	4.216205
-1084.596019	25.995074	4.226202
-1083.381576	36.514637	4.236198
-1081.272929	28.685607	4.246195
-1079.135146	21.845008	4.256192
-1077.448230	28.094025	4.266189
-1074.998557	32.487465	4.276186
-1073.480086	33.305402	4.286182
-1071.807703	30.012694	4.296179
-1069.745895	36.182802	4.306176
-1067.849547	31.134917	4.316173
-1065.893024	23.904934	4.326170
-1064.314524	22.888141	4.336166
-1062.505253	36.579172	4.346163
-1060.497157	42.724729	4.356160
-1058.526260	27.293555	4.366157
-1056.575339	33.647191	4.376154
-1054.648145	41.877126	4.386150
-1052.756566	35.873239	4.396147
-1051.286052	40.304924	4.406144
-1048.992165	18.293614	4.416141
-1047.371073	12.781396	4.426138
-1045.751236	62.823874	4.436134
-1043.410443	35.705391	4.446131
-1041.273206	9.956792	4.456128
-1039.898461	35.389666	4.466125
-1038.180269	32.839600	4.476122
-1036.017446	45.241040	4.486118
-1033.992583	32.723673	4.496115
-1031.998228	7.978394	4.506112
-1030.518890	22.570049	4.516109
-1028.833484	41.858952	4.526106
-1026.545567	28.296957	4.536102
-1024.879426	34.197260	4.546099
-1022.830100	28.768125	4.556096
-1020.822401	30.390414	4.566093
-1019.191411	15.312047	4.576090
-1017.463022	51.378693	4.586086
-1015.413359	21.243876	4.596083
-1013.521121	27.332217	4.606080
-1011.795525	40.932480	4.616077
-1009.650932	32.890929	4.626074
-1007.676793	17.418232	4.636070
-1006.156169	38.162353	4.646067
-1004.412420	29.289720	4.656064
-1002.184748	15.033232	4.666061
-1000.135136	30.458906	4.676058
-998.444648	35.360670	4.686054
-996.590933	13.648737	4.696051
-994.867527	19.951975	4.706048
-992.852130	20.347880	4.716045
-990.963110	34.269361	4.726042
-989.135502	26.676395	4.736038
-987.376036	26.049103	4.746035
-985.403578	31.944653	4.756032
-983.376023	38.535557	4.766029
-981.746113	28.268087	4.776026
-979.732392	29.085821	4.786022
-977.761631	31.637675	4.796019
-976.036162	32.771494	4.806016
-974.176184	31.335560	4.816013
-972.188231	22.603884	4.826010
-970.294087	28.019375	4.836006
-968.611401	25.844485	4.846003
-966.629545	20.388296	4.856000
-964.771743	38.313990	4.865997
-962.833044	21.511290	4.875994
-960.881910	29.816418	4.885990
-958.999253	37.041526	4.895987
-957.297981	32.547517	4.905984
-955.429162	32.772699	4.915981
-953.408519	37.159101	4.925978
-951.595774	37.061698	4.935974
-949.620641	30.004074	4.945971
-947.921384	26.317181	4.955968
-945.934101	32.647734	4.965965
-943.989373	30.325174	4.975962
-942.111821	29.816390	4.985958
-940.408257	25.855674	4.995955
-938.551497	26.438037	5.005952
-936.380854	27.177034	5.015949
-934.664917	25.323670	5.025946
-932.892446	24.451197	5.035942
-930.861626	32.268382	5.045939
-929.264227	24.721744	5.055936
-927.229319	26.434494	5.065933
-925.467471	30.837042	5.075930
-923.364719	22.559118	5.085926
-921.677907	33.386904	5.095923
-919.581702	38.784341	5.105920
-917.720112	36.176695	5.115917
-915.766270	26.807927	5.125914
-914.110728	40.032663	5.135910
-912.468623	34.611893	5.145907
-910.177469	31.561380	5.155904
-908.180773	35.522208	5.165901
-906.646582	31.460711	5.175898
-904.730195	37.621075	5.185894
-903.090488	38.459210	5.195891
-900.921797	32.106412	5.205888
-898.963489	35.888662	5.215885
-897.044683	32.463519	5.225882
-895.508988	37.311172	5.235878
-893.565641	32.165910	5.245875
-891.436270	33.172058	5.255872
-889.626138	29.851133	5.265869
-887.844064	38.578075	5.275866
-885.650967	24.931893	5.285862
-884.072656	37.415895	5.295859
-882.615151	36.508562	5.305856
-880.136186	31.607648	5.315853
-878.228731	26.291308	5.325850
-876.689204	29.343221	5.335846
-874.671971	33.504466	5.345843
-872.688846	36.916481	5.355840
-871.143023	28.092948	5.365837
-869.163363	27.076878	5.375834
-867.019004	31.629879	5.385830
-865.255751	30.308962	5.395827
-863.360354	31.399908	5.405824
-861.330088	34.446000	5.415821
-859.593219	26.842370	5.425818
-857.833415	30.904269	5.435814
-855.930258	32.612886	5.445811
-853.964903	24.342775	5.455808
-852.362979	34.611073	5.465805
-850.343835	27.925411	5.475802
-848.315416	29.205088	5.485798
-846.552063	30.571352	5.495795
-844.541319	29.430341	5.505792
-842.734585	29.842369	5.515789
-841.001001	22.722403	5.525786
-839.161255	33.004792	5.535782
-837.133846	29.987041	5.545779
-835.016613	26.421285	5.555776
-833.379290	35.913467	5.565773
-831.325666	37.263336	5.575770
-829.779651	37.462862	5.585766
-827.745089	32.380431	5.595763
-825.820784	28.375031	5.605760
-824.164906	30.690008	5.615757
-822.003566	25.329966	5.625754
-820.361484	31.532675	5.635750
-818.138086	26.252709	5.645747
-816.357360	27.576747	5.655744
-814.642550	32.359510	5.665741
-812.867612	44.970028	5.675738
-811.083205	34.725319	5.685734
-808.785955	26.462179	5.695731
-807.178732	34.462454	5.705728
-805.430739	37.997374	5.715725
-803.113693	25.539255	5.725722
-801.436513	30.222260	5.735718
-799.796142	36.982591	5.745715
-797.859321	39.082164	5.755712
-795.897396	26.390311	5.765709
-793.790889	34.021857	5.775706
-792.015134	33.630510	5.785702
-790.350372	32.930087	5.795699
-788.447342	29.052845	5.805696
-786.373576	29.084360	5.815693
-784.408139	30.880969	5.825690
-782.663199	37.078319	5.835686
-780.982728	37.188494	5.845683
-778.945964	32.407309	5.855680
-776.884253	36.285236	5.865677
-775.142145	34.719887	5.875674
-773.578401	32.306792	5.885670
-771.657819	38.859735	5.895667
-769.576609	35.359787	5.905664
-767.445681	23.755604	5.915661
-766.104860	27.031972	5.925658
-764.044576	34.612519	5.935654
-761.988479	26.602688	5.945651
-760.046850	34.513235	5.955648
-758.529531	41.651665	5.965645
-756.700656	43.369081	5.975642
-754.248599	36.577982	5.985638
-752.639821	38.393734	5.995635
-750.712067	30.900180	6.005632
-748.869927	26.126446	6.015629
-747.280884	35.959550	6.025626
-745.401775	27.777507	6.035622
-743.088827	30.524329	6.045619
-741.546598	22.219306	6.055616
-739.460298	22.754087	6.065613
-737.490246	24.775772	6.075610
-735.819708	26.188531	6.085606
-734.204600	28.543246	6.095603
-732.266550	25.421451	6.105600
-729.912523	26.158172	6.115597
-728.167698	23.902470	6.125594
-726.419573	27.678991	6.135590
-724.679894	22.296431	6.145587
-722.500829	21.985932	6.155584
-720.739627	13.399629	6.165581
-719.031573	30.392714	6.175578
-717.043808	29.276008	6.185574
-715.217814	27.716242	6.195571
-713.419646	28.033429	6.205568
-711.594304	21.430954	6.215565
-709.400977	26.737281	6.225562
-707.724709	34.693442	6.235558
-705.936695	35.894831	6.245555
-703.725329	27.459206	6.255552
-702.010813	30.124877	6.265549
-700.037456	35.357431	6.275546
-698.412108	22.891530	6.285542
-696.283454	27.546672	6.295539
-694.610235	29.388478	6.305536
-692.686545	25.725888	6.315533
-690.927562	33.348339	6.325530
-688.974122	28.691063	6.335526
-686.975812	25.755451	6.345523
-685.154141	17.959978	6.355520
-683.196530	18.115928	6.365517
-681.512178	22.908395	6.375514
-679.470902	28.385883	6.385510
-677.394928	22.895933	6.395507
-675.879761	20.138584	6.405504
-674.068967	22.953089	6.415501
-672.022407	25.494673	6.425498
-670.095333	25.780243	6.435494
-668.236824	30.985389	6.445491
-666.304042	23.931594	6.455488
-664.625074	34.778217	6.465485
-662.727953	23.165690	6.475482
-660.971112	19.998704	6.485478
-658.605656	26.210671	6.495475
-656.825689	19.875994	6.505472
-655.234131	27.659426	6.515469
-653.318308	29.486178	6.525466
-651.413184	28.006967	6.535462
-649.453881	28.836841	6.545459
-647.710565	30.547489	6.555456
-645.595056	36.853094	6.565453
-643.932020	24.576976	6.575450
-642.333829	29.891631	6.585446
-639.984511	25.629001	6.595443
-638.043278	22.317312	6.605440
-636.528221	28.996742	6.615437
-634.548296	24.605260	6.625434
-632.711230	26.411457	6.635430
-630.704459	27.896876	6.645427
-628.702431	29.280429	6.655424
-626.948284	27.241189	6.665421
-625.178952	21.795542	6.675418
-623.439815	27.899213	6.685414
-621.179316	29.126219	6.695411
-619.176870	28.880349	6.705408
-617.793688	31.502714	6.715405
-615.977174	23.240772	6.725402
-613.732017	33.239129	6.735398
-611.801519	33.348948	6.745395
-610.135235	25.379415	6.755392
-608.203263	30.675500	6.765389
-606.446986	24.616201	6.775386
-604.396325	32.384740	6.785382
-602.481546	29.620425	6.795379
-600.811791	32.476471	6.805376
-598.858294	26.164628	6.815373
-597.005682	28.438866	6.825370
-595.295206	32.079410	6.835366
-592.857475	32.158727	6.845363
-591.224484	32.202418	6.855360
-589.803863	29.930720	6.865357
-587.819554	37.122549	6.875354
-585.854177	29.015250	6.885350
-583.756400	25.834898	6.895347
-581.910481	32.467825	6.905344
-579.765298	40.737573	6.915341
-578.228757	33.047714	6.925338
-576.445439	30.680187	6.935334
-574.568251	32.909467	6.945331
-572.548410	35.558035	6.955328
-570.414162	37.392591	6.965325
-568.664624	32.546944	6.975322
-567.183361	36.639365	6.985318
-564.884191	34.617301	6.995315
-563.357122	28.095733	7.005312
-561.498498	35.501861	7.015309
-559.515391	36.623252	7.025306
-557.436409	34.440595	7.035302
-555.663871	41.506822	7.045299
-553.775476	24.775567	7.055296
-551.957842	32.106151	7.065293
-550.100268	31.569291	7.075290
-548.129191	31.611105	7.085286
-546.341883	33.624255	7.095283
-544.372527	38.808644	7.105280
-542.569677	25.919760	7.115277
-540.753724	38.486071	7.125274
-538.608067	28.738008	7.135270
-537.333458	36.903723	7.145267
-535.095063	29.892775	7.155264
-532.860251	35.712092	7.165261
-531.228158	28.494862	7.175258
-529.687639	34.019326	7.185254
-527.680504	31.301891	7.195251
-525.543903	27.040193	7.205248
-523.712368	29.829402	7.215245
-522.043753	24.968297	7.225242
-520.164573	36.411440	7.235238
-517.992452	37.264268	7.245235
-516.262663	30.389838	7.255232
-514.235490	27.002941	7.265229
-512.594402	32.217688	7.275226
-510.579604	32.983554	7.285222
-508.972923	32.879935	7.295219
-506.849303	32.851630	7.305216
-505.007290	33.634048	7.315213
-503.354229	30.679524	7.325210
-501.127677	37.619595	7.335206
-499.381700	40.834571	7.345203
-497.483096	29.476107	7.355200
-495.559716	28.357237	7.365197
-493.852263	28.856440	7.375194
-491.881054	36.137284	7.385190
-489.956583	35.940290	7.395187
-488.042492	27.034466	7.405184
-486.261858	26.972547	7.415181
-484.398430	30.034571	7.425178
-482.568376	27.395980	7.435174
-480.894144	33.199103	7.445171
-478.690117	28.345660	7.455168
-476.936583	31.594178	7.465165
-474.857419	28.727923	7.475162
-473.338869	39.192988	7.485158
-471.385491	39.693979	7.495155
-469.146345	30.848347	7.505152
-467.477643	22.036993	7.515149
-465.445218	30.231706	7.525146
-463.714015	33.310128	7.535142
-461.925186	29.917133	7.545139
-460.139045	29.410698	7.555136
-457.991247	30.711121	7.565133
-456.209499	30.821141	7.575130
-454.225579	30.745725	7.585126
-452.788317	26.390530	7.595123
-450.461845	22.861156	7.605120
-448.613505	27.536039	7.615117
-447.062915	32.785813	7.625114
-444.989985	32.754607	7.635110
-443.094721	27.677366	7.645107
-441.031842	25.830517	7.655104
-439.174631	42.986355	7.665101
-437.601420	25.157684	7.675098
-435.657130	36.582612	7.685094
-433.570122	28.972284	7.695091
-432.196185	30.293692	7.705088
-429.924006	27.543483	7.715085
-428.097340	25.094935	7.725082
-426.209708	35.635294	7.735078
-424.214885	33.216732	7.745075
-422.520006	29.720355	7.755072
-420.530167	27.591522	7.765069
-418.624843	33.540934	7.775066
-417.115342	31.788792	7.785062
-414.911155	41.830221	7.795059
-412.868826	30.163090	7.805056
-410.827773	35.178262	7.815053
-409.459121	31.404009	7.825050
-407.585712	34.516605	7.835046
-405.547025	33.444125	7.845043
-403.631637	31.832426	7.855040
-401.877776	31.247510	7.865037
-400.033220	36.597209	7.875034
-398.358631	43.503957	7.885030
-396.236901	31.977305	7.895027
-394.140260	34.016962	7.905024
-392.058026	34.663221	7.915021
-390.518332	35.413483	7.925018
-389.051407	37.422655	7.935014
-386.828443	38.122231	7.945011
-384.917528	37.586455	7.955008
-382.999618	38.746825	7.965005
-381.351544	38.385646	7.975002
-379.188802	28.851283	7.984998
-377.251781	30.586463	7.994995
-375.768202	30.870461	8.004992
-373.782850	25.614687	8.014989
-371.914224	39.214780	8.024986
-370.063567	32.300619	8.034982
-367.988190	34.127393	8.044979
-366.197088	30.541483	8.054976
-363.911962	36.902376	8.064973
-362.296538	32.472995	8.074970
-360.806821	43.321675	8.084966
-358.840116	36.038487	8.094963
-356.680466	31.760620	8.104960
-354.831310	38.480062	8.114957
-352.917774	34.696203	8.124954
-351.264170	46.148685	8.134950
-349.319293	30.494777	8.144947
-347.193439	29.875769	8.154944
-345.498828	27.101020	8.164941
-343.656958	29.173505	8.174938
-341.780863	28.449125	8.184934
-339.971320	33.015039	8.194931
-337.991607	29.787432	8.204928
-335.984880	37.149585	8.214925
-334.202809	36.891772	8.224922
-332.663493	38.043160	8.234918
-330.606126	38.661866	8.244915
-328.937280	37.263260	8.254912
-326.626082	39.445554	8.264909
-324.496819	39.133897	8.274906
-322.868825	27.438253	8.284902
-321.569623	43.290750	8.294899
-319.378685	24.424096	8.304896
-317.196806	31.597257	8.314893
-315.507411	39.775834	8.324890
-313.852298	33.740773	8.334886
-311.610890	29.309375	8.344883
-309.569925	34.450960	8.354880
-307.997133	34.359202	8.364877
-306.073457	38.332223	8.374874
-304.225857	37.482955	8.384870
-302.406964	34.814701	8.394867
-300.611635	34.790045	8.404864
-298.597739	27.272018	8.414861
-296.269266	31.077796	8.424858
-295.272760	33.995759	8.434854
-293.420291	38.264351	8.444851
-291.119155	27.238057	8.454848
-289.345801	35.002221	8.464845
-287.491408	34.033468	8.474842
-285.353080	25.870362	8.484838
-283.472323	40.213819	8.494835
-281.983414	35.289979	8.504832
-279.701177	25.008772	8.514829
-277.870733	37.241448	8.524826
-276.192749	36.520324	8.534822
-274.273663	34.682360	8.544819
-272.305257	25.595923	8.554816
-270.268445	31.846558	8.564813
-268.937159	36.683074	8.574810
-266.897193	34.557415	8.584807
-264.923540	37.311515	8.594803
-262.876352	25.564777	8.604800
-261.057423	39.667087	8.614797
-259.063041	28.317177	8.624794
-257.507208	41.367346	8.634791
-255.596563	34.344220	8.644787
-253.265514	40.333184	8.654784
-251.734662	30.023525	8.664781
-249.717696	38.631414	8.674778
-248.135895	29.677752	8.684775
-245.893579	31.733760	8.694771
-244.162413	25.876067	8.704768
-242.419162	39.759962	8.714765
-240.923245	34.746611	8.724762
-238.581279	33.182206	8.734759
-236.640168	42.973725	8.744755
-234.816345	25.694054	8.754752
-232.968611	31.098642	8.764749
-231.098861	28.941765	8.774746
-229.323878	28.132564	8.784743
-227.391563	24.478427	8.794739
-225.275086	33.760411	8.804736
-223.407268	38.378694	8.814733
-221.456731	33.008598	8.824730
-219.852102	36.601590	8.834727
-217.818591	33.166555	8.844723
-216.167783	30.646764	8.854720
-214.667167	23.880158	8.864717
-212.289414	31.375822	8.874714
-210.451721	25.494833	8.884711
-208.605007	25.612036	8.894707
-206.580834	34.139870	8.904704
-204.824796	25.744179	8.914701
-203.017482	35.383405	8.924698
-201.099288	37.772223	8.934695
-199.146439	33.088575	8.944691
-197.209455	24.270876	8.954688
-194.967360	36.591074	8.964685
-193.626225	35.047507	8.974682
-191.955838	34.002411	8.984679
-189.876415	37.737528	8.994675
-187.692539	32.945969	9.004672
-185.910392	24.640854	9.014669
-183.949349	33.655598	9.024666
-182.379871	27.413248	9.034663
-180.556302	31.304461	9.044659
-178.667238	25.574760	9.054656
-176.619847	20.493963	9.064653
-174.660572	26.267615	9.074650
-172.934620	22.392259	9.084647
-170.796397	29.529902	9.094643
-169.197896	24.956512	9.104640
-167.367208	18.345666	9.114637
-165.324647	26.990593	9.124634
-163.612486	20.881793	9.134631
-162.078019	31.243500	9.144627
-160.039206	21.149655	9.154624
-158.234555	28.413170	9.164621
-155.960783	31.809425	9.174618
-153.910313	20.153820	9.184615
-152.467298	28.117643	9.194611
-150.329961	18.704358	9.204608
-148.527293	23.041007	9.214605
-146.934801	24.305601	9.224602
-144.790492	27.784100	9.234599
-142.986968	33.396333	9.244595
-141.120911	38.805970	9.254592
-138.884015	28.570006	9.264589
-137.211997	32.262821	9.274586
-135.514865	32.304482	9.284583
-133.618439	27.459373	9.294579
-131.485140	29.543939	9.304576
-130.002109	28.811397	9.314573
-127.659346	27.856407	9.324570
-126.045403	26.469859	9.334567
-124.286359	27.445801	9.344563
-122.183778	33.341888	9.354560
-120.245701	27.062861	9.364557
-118.547279	30.397813	9.374554
-116.510237	25.250823	9.384551
-114.988884	29.322935	9.394547
-113.065918	31.371611	9.404544
-110.809289	20.205740	9.414541
-109.285728	33.310114	9.424538
-107.139181	25.750539	9.434535
-105.342265	18.843564	9.444531
-103.696360	23.468931	9.454528
-101.533606	36.919716	9.464525
-99.558221	23.692539	9.474522
-97.850719	21.046946	9.484519
-96.271555	27.487596	9.494515
-93.661492	22.726007	9.504512
-92.466331	18.022823	9.514509
-90.679178	29.899433	9.524506
-88.283302	29.357560	9.534503
-86.609255	27.282541	9.544499
-84.721793	24.822966	9.554496
-82.678639	25.954122	9.564493
-80.901186	35.539799	9.574490
-79.071043	26.728177	9.584487
-77.472119	34.277203	9.594483
-75.561844	25.699099	9.604480
-73.271229	36.475463	9.614477
-71.627472	30.238693	9.624474
-70.089909	32.653613	9.634471
-67.824226	33.460348	9.644467
-65.720737	33.227237	9.654464
-64.162650	32.899577	9.664461
-62.077025	36.488565	9.674458
-60.344287	36.881419	9.684455
-58.400654	34.635519	9.694451
-56.666486	35.392863	9.704448
-54.867383	34.824663	9.714445
-52.719639	35.408664	9.724442
-51.085850	36.069928	9.734439
-49.504304	39.766191	9.744435
-47.136035	31.846044	9.754432
-45.145624	42.547186	9.764429
-43.325683	29.071699	9.774426
-41.687431	35.433497	9.784423
-39.649318	40.315273	9.794419
-37.864327	38.146800	9.804416
-35.963309	33.417864	9.814413
-34.017702	31.189036	9.824410
-32.275130	34.445960	9.834407
-30.193198	37.037731	9.844403
-28.333524	37.383517	9.854400
-26.535043	38.351662	9.864397
-24.963681	35.819408	9.874394
-23.317413	36.529224	9.884391
-21.053976	40.745108	9.894387
-18.870562	43.413853	9.904384
-17.447132	51.393538	9.914381
-15.392002	49.497756	9.924378
-13.833636	64.402891	9.934375
-11.622955	64.027998	9.944371
-9.700142	73.544786	9.954368
-7.957224	73.085051	9.964365
-6.092703	82.541677	9.974362
-4.395027	97.873028	9.984359
-2.467139	99.861023	9.994355
-0.799442	110.310598	10.004352
0.000000	135.204264	10.009357
0.710968	144.616517	10.014362
0.888420	174.564044	10.019367
1.702950	171.876394	10.024371
1.691923	195.336910	10.029376
2.258769	213.287207	10.034381
2.314213	210.890940	10.039386
2.260565	228.981237	10.044391
2.505541	226.570502	10.049395
2.389176	224.334096	10.054400
2.575069	232.904553	10.059405
2.891657	222.620189	10.064410
2.632785	235.047628	10.069415
2.458305	228.824736	10.074419
2.770983	240.418307	10.079424
2.412296	234.730969	10.084429
2.701759	229.957312	10.089434
2.590963	235.233740	10.094439
2.966393	235.195864	10.099443
2.842440	237.092033	10.104448
2.817186	241.612117	10.109453
2.955030	235.856610	10.114458
2.660247	245.017807	10.119463
2.972798	242.077504	10.124467
2.901077	249.507999	10.129472
3.019565	254.673747	10.134477
3.055745	254.467650	10.139482
2.861433	259.886712	10.144487
3.387677	264.504898	10.149491
3.483706	268.111564	10.154496
3.555446	271.704760	10.159501
3.452511	268.751887	10.164506
3.474717	268.857084	10.169511
3.690222	275.516419	10.174515
3.303419	273.155998	10.179520
3.818601	277.358085	10.184525
3.775362	271.085856	10.189530
3.301669	272.750831	10.194535
3.844423	280.583187	10.199539
3.790671	289.012143	10.204544
3.887663	282.569314	10.209549
3.724026	291.823155	10.214554
3.779804	295.057801	10.219559
3.846721	291.232630	10.224563
4.073069	293.735209	10.229568
4.203934	301.010419	10.234573
4.356486	308.561278	10.239578
3.950466	305.863314	10.244583
4.093830	301.563924	10.249587
4.072700	307.198214	10.254592
3.777255	302.632950	10.259597
3.791948	303.076795	10.264602
3.679205	314.984279	10.269607
4.067042	310.877687	10.274611
3.909229	329.714814	10.279616
4.038312	339.689925	10.284621
4.559694	333.275565	10.289626
4.590841	340.696005	10.294631
5.095977	335.583575	10.299635
4.872005	349.121967	10.304640
4.508714	352.855538	10.309645
4.480171	348.861085	10.314650
4.732035	350.746201	10.319655
4.928374	350.859889	10.324659
4.806186	358.669056	10.329664
4.552795	365.239235	10.334669
4.758159	355.358853	10.339674
4.406972	365.298636	10.344679
4.869853	372.665992	10.349683
4.884837	372.669845	10.354688
5.003368	366.728142	10.359693
5.123257	378.363615	10.364698
5.134315	381.860868	10.369703
5.362814	379.881647	10.374707
5.310412	391.172472	10.379712
5.244395	399.776906	10.384717
5.432508	398.855900	10.389722
5.159173	401.280519	10.394727
5.199051	395.474347	10.399731
5.475598	400.460400	10.404736
5.100504	406.122809	10.409741
5.734320	399.939630	10.414746
5.646922	401.669148	10.419751
5.789891	404.107780	10.424755
5.760457	408.824116	10.429760
5.556335	414.374104	10.434765
5.661557	408.962761	10.439770
5.685970	408.179826	10.444775
5.733590	396.777663	10.449779
5.586820	413.605776	10.454784
5.695732	429.603107	10.459789
5.968391	426.982929	10.464794
5.957639	443.891877	10.469799
6.156529	442.597006	10.474803
6.122710	449.048622	10.479808
5.705533	452.201061	10.484813
6.197863	450.545580	10.489818
6.236446	450.381673	10.494823
6.246770	450.083509	10.499827
6.161650	452.041317	10.504832
6.425635	449.067721	10.509837
6.486568	460.447749	10.514842
6.196226	446.912324	10.519847
6.319594	455.734150	10.524851
6.131102	467.053051	10.529856
6.332307	481.886170	10.534861
6.884727	478.773521	10.539866
6.524564	492.486729	10.544871
6.519139	485.369472	10.549875
6.709283	489.964079	10.554880
6.756497	503.722696	10.559885
6.984212	494.344835	10.564890
6.971561	493.268199	10.569895
7.130149	487.996541	10.574899
6.647225	496.267007	10.579904
6.819903	497.871474	10.584909
7.122836	492.338679	10.589914
6.887028	500.487730	10.594919
6.980187	512.129153	10.599923
7.218098	522.891243	10.604928
7.288402	524.981957	10.609933
7.454032	524.996471	10.614938
6.902672	543.686927	10.619943
7.404788	521.074591	10.624947
7.100730	523.409518	10.629952
7.274837	530.214341	10.634957
7.226709	537.483531	10.639962
7.508360	533.518390	10.644967
7.626605	528.013465	10.649971
7.569262	543.108654	10.654976
7.578283	542.329744	10.659981
7.924380	542.578811	10.664986
7.597031	563.020176	10.669991
8.031959	564.896619	10.674995
8.289898	574.770917	10.680000
7.803000	564.510406	10.685005
8.026372	567.850839	10.690010
8.124607	566.893699	10.695015
8.328418	565.511303	10.700019
8.097527	557.616299	10.705024
7.984511	558.886316	10.710029
8.388231	568.779931	10.715034
8.066495	572.125320	10.720039
8.430820	579.119011	10.725043
8.685143	578.518580	10.730048
8.264395	580.933629	10.735053
8.608060	571.370071	10.740058
8.310405	587.315740	10.745063
8.482673	572.366041	10.750067
8.438893	575.501519	10.755072
8.352745	591.287302	10.760077
8.339522	578.805067	10.765082
8.293548	591.400692	10.770087
8.412055	585.499903	10.775091
8.273130	584.301482	10.780096
7.983967	600.881301	10.785101
8.529770	610.260287	10.790106
8.573606	619.320397	10.795111
8.706363	621.282895	10.800115
8.868208	622.125886	10.805120
8.523088	626.536271	10.810125
8.798925	636.292641	10.815130
8.729332	656.448601	10.820135
8.891334	644.780424	10.825139
9.053718	647.261731	10.830144
9.032019	648.848338	10.835149
9.031164	659.352160	10.840154
9.027289	662.159602	10.845159
9.151057	667.923879	10.850163
9.431885	684.846518	10.855168
9.731359	689.474211	10.860173
9.720503	677.086128	10.865178
9.681026	681.064586	10.870183
9.722812	663.778133	10.875187
10.009389	654.810235	10.880192
9.497339	670.377047	10.885197
9.994176	661.914906	10.890202
9.913361	653.664760	10.895207
9.710285	664.982988	10.900211
9.685057	660.871229	10.905216
9.875953	663.106725	10.910221
9.837987	673.386249	10.915226
9.722138	694.901048	10.920231
10.008989	703.927177	10.925235
9.716566	709.488208	10.930240
9.863913	708.982106	10.935245
10.055481	706.516736	10.940250
9.841287	705.226236	10.945255
10.199840	702.565501	10.950259
10.267643	704.767024	10.955264
9.954767	709.407250	10.960269
10.497404	718.687467	10.965274
10.581420	738.049506	10.970279
10.526295	722.784274	10.975283
10.568623	732.902802	10.980288
10.664301	738.277360	10.985293
10.764810	744.922141	10.990298
10.752788	742.891354	10.995303
10.798811	740.048660	11.000307
10.604723	734.063637	11.005312
10.673615	735.842378	11.010317
11.003898	747.793086	11.015322
10.627889	743.770374	11.020327
10.931162	748.782246	11.025331
10.987238	747.888588	11.030336
11.001989	749.472546	11.035341
11.135398	750.450964	11.040346
11.395668	749.439581	11.045351
11.054167	750.812291	11.050355
11.233456	749.774403	11.055360
10.818128	755.008136	11.060365
10.731436	748.297941	11.065370
10.792349	752.348712	11.070375
10.824632	760.505605	11.075379
11.341335	772.268904	11.080384
11.142327	784.783455	11.085389
11.751722	783.740032	11.090394
11.609388	788.927077	11.095399
11.373426	786.250777	11.100403
11.500632	799.083880	11.105408
11.468618	790.526257	11.110413
11.879748	784.299595	11.115418
11.874729	785.158174	11.120423
11.767541	793.548640	11.125427
11.860199	787.544662	11.130432
11.825298	794.408181	11.135437
11.647847	791.440279	11.140442
11.592550	789.933617	11.145447
11.784529	785.623175	11.150451
12.047667	797.450597	11.155456
12.010864	809.649142	11.160461
12.204364	810.398787	11.165466
12.194858	822.965142	11.170471
11.948969	825.510029	11.175475
12.014144	823.102648	11.180480
12.050989	818.212982	11.185485
12.130340	815.191496	11.190490
12.064078	833.978404	11.195495
12.278190	812.089635	11.200499
12.118664	834.734376	11.205504
12.118055	843.637716	11.210509
12.802274	844.594508	11.215514
12.624392	858.233253	11.220519
12.580540	859.020762	11.225523
12.868021	853.602257	11.230528
12.902930	855.328087	11.235533
12.964726	850.677277	11.240538
12.652500	865.368767	11.245543
12.710154	854.721568	11.250547
12.734096	855.881455	11.255552
12.622047	863.044312	11.260557
12.916102	856.257564	11.265562
12.810440	857.423932	11.270567
12.723703	860.599439	11.275571
13.242338	865.764653	11.280576
13.204950	882.530131	11.285581
13.617500	879.070710	11.290586
12.941500	871.798461	11.295591
13.186667	878.948498	11.300595
13.472964	891.281650	11.305600
13.415029	892.542909	11.310605
13.643553	879.503043	11.315610
13.750911	886.820144	11.320615
13.423037	890.854125	11.325619
13.503023	888.097446	11.330624
13.369183	887.776538	11.335629
13.749204	882.057837	11.340634
13.656186	888.612131	11.345639
13.674374	902.172333	11.350643
13.796704	885.577655	11.355648
13.721941	901.290998	11.360653
13.656372	887.118494	11.365658
13.742273	888.902426	11.370663
13.637451	892.476633	11.375667
13.626000	894.490557	11.380672
14.135507	913.491649	11.385677
14.231402	925.905664	11.390682
14.272105	926.216070	11.395687
14.262880	919.946019	11.400691
14.191960	918.790338	11.405696
14.338420	922.091083	11.410701
14.774073	914.315062	11.415706
14.530710	926.524577	11.420711
14.388793	928.622394	11.425715
14.452677	926.945322	11.430720
14.553153	925.055834	11.435725
14.652885	927.974533	11.440730
14.729487	931.573426	11.445735
14.477139	927.944092	11.450739
14.962078	922.811028	11.455744
14.376659	930.465738	11.460749
14.757472	926.006863	11.465754
14.644133	924.075790	11.470759
14.770993	919.028231	11.475763
14.726768	927.744617	11.480768
14.710049	923.011692	11.485773
15.108757	917.212727	11.490778
14.747317	930.371471	11.495783
14.792467	930.080356	11.500787
14.894721	929.177745	11.505792
15.029951	951.949114	11.510797
15.401488	954.184225	11.515802
15.141122	960.244857	11.520807
15.341512	956.699415	11.525811
15.398316	958.388649	11.530816
15.363936	966.914257	11.535821
15.687478	958.414935	11.540826
15.422054	962.320703	11.545831
15.463366	959.253216	11.550835
15.568931	957.017563	11.555840
15.274358	968.270198	11.560845
15.415095	955.698425	11.565850
15.545493	966.154725	11.570855
15.333496	972.565611	11.575859
15.727926	954.844094	11.580864
15.439682	955.279512	11.585869
15.923737	971.127716	11.590874
15.695194	985.425936	11.595879
15.804181	984.142205	11.600883
15.878155	983.133715	11.605888
15.957285	995.178307	11.610893
16.411341	980.389818	11.615898
16.373155	983.636454	11.620903
16.239634	995.101537	11.625907
16.337059	988.016512	11.630912
16.330678	993.393252	11.635917
16.468595	991.231281	11.640922
16.364017	987.070586	11.645927
16.405945	990.435330	11.650931
16.710111	995.341492	11.655936
16.102329	993.911900	11.660941
16.289088	992.612608	11.665946
16.399223	1000.635794	11.670951
16.440390	991.653220	11.675955
16.301575	990.273400	11.680960
16.419458	990.238762	11.685965
16.751569	984.713743	11.690970
16.696102	1003.098606	11.695975
16.680383	1022.623590	11.700979
16.902901	1015.009245	11.705984
17.059332	1032.661760	11.710989
16.981537	1030.874812	11.715994
17.084828	1019.813361	11.720999
17.124363	1020.668001	11.726003
17.304441	1018.447262	11.731008
17.091310	1035.163679	11.736013
17.397956	1015.451796	11.741018
17.232023	1020.794073	11.746023
17.052829	1018.001443	11.751027
17.462311	1015.526493	11.756032
17.158491	1023.601530	11.761037
17.544905	1018.031566	11.766042
17.247481	1021.324293	11.771047
17.515833	1021.587350	11.776051
17.735489	1015.857908	11.781056
17.686483	1030.588001	11.786061
17.981869	1021.801399	11.791066
17.755295	1029.428881	11.796071
17.637853	1027.574142	11.801075
17.872135	1013.184951	11.806080
17.630062	1024.659488	11.811085
18.096783	1018.919020	11.816090
17.871565	1026.946828	11.821095
18.047790	1023.201798	11.826099
18.085314	1028.331853	11.831104
17.566412	1027.228699	11.836109
18.068822	1016.507283	11.841114
17.953531	1015.074823	11.846119
17.910392	1030.734376	11.851123
18.289136	1017.153187	11.856128
17.851887	1021.201496	11.861133
18.070700	1041.296217	11.866138
18.248412	1048.799297	11.871143
18.484505	1053.758915	11.876147
18.606391	1050.117163	11.881152
18.526043	1057.106326	11.886157
18.445159	1053.861192	11.891162
18.569770	1058.362357	11.896167
18.421116	1063.296618	11.901171
18.744987	1051.854606	11.906176
18.479450	1057.149707	11.911181
18.327104	1052.949304	11.916186
18.648317	1059.035478	11.921191
18.351776	1051.168022	11.926195
18.778836	1060.113663	11.931200
18.620793	1057.180456	11.936205
18.713155	1060.224936	11.941210
18.914725	1076.991945	11.946215
18.944184	1096.795250	11.951219
18.903737	1093.647736	11.956224
19.042723	1091.099227	11.961229
19.050851	1095.357210	11.966234
19.151817	1091.501166	11.971239
19.106413	1086.045789	11.976243
19.347031	1097.653122	11.981248
19.039865	1094.835158	11.986253
18.874329	1093.435936	11.991258
18.950855	1089.791948	11.996263
19.253513	1115.402186	12.001267
19.587264	1115.995435	12.006272
19.409259	1118.761356	12.011277
19.432989	1120.242997	12.016282
19.517698	1122.610621	12.021287
19.294342	1126.586993	12.026291
19.556219	1126.847931	12.031296
19.378566	1125.397022	12.036301
19.673330	1120.013527	12.041306
19.939907	1116.835957	12.046311
19.652868	1120.341515	12.051315
19.829708	1115.667538	12.056320
19.936354	1120.390784	12.061325
20.162546	1114.582991	12.066330
19.739052	1105.144610	12.071335
19.630775	1099.218286	12.076339
19.781191	1090.397997	12.081344
19.473927	1093.864197	12.086349
19.626351	1088.137567	12.091354
19.503151	1083.957737	12.096359
19.531115	1085.162733	12.101363
19.911312	1095.161388	12.106368
19.693096	1099.939601	12.111373
19.889133	1077.225416	12.116378
19.769138	1087.827400	12.121383
19.734110	1093.651871	12.126387
19.909647	1092.180896	12.131392
19.499063	1100.003347	12.136397
19.560615	1084.681275	12.141402
19.766796	1101.827623	12.146407
19.727189	1101.089555	12.151411
19.881319	1091.551160	12.156416
19.773062	1078.232100	12.161421
19.670498	1077.150840	12.166426
19.250521	1080.795864	12.171431
19.365725	1070.096750	12.176435
19.778816	1068.302458	12.181440
19.395142	1073.398790	12.186445
19.800539	1078.353488	12.191450
19.915612	1078.898039	12.196455
19.141681	1072.675785	12.201459
19.465897	1060.714894	12.206464
19.528514	1080.599620	12.211469
19.988750	1083.468731	12.216474
19.490415	1069.603198	12.221479
19.741911	1073.319308	12.226483
19.984064	1062.965801	12.231488
19.671007	1069.071153	12.236493
19.596744	1065.612072	12.241498
19.597567	1055.164602	12.246503
19.836562	1079.050291	12.251507
19.706975	1073.501114	12.256512
19.466888	1077.052788	12.261517
19.630575	1071.444216	12.266522
19.948235	1068.190700	12.271527
19.475922	1075.035814	12.276531
19.842499	1052.895281	12.281536
19.660898	1079.517831	12.286541
20.083926	1066.350578	12.291546
19.574009	1071.260466	12.296551
19.591353	1064.008406	12.301555
20.031654	1044.308279	12.306560
19.268896	1038.338146	12.311565
19.271013	1041.884293	12.316570
19.056369	1062.115994	12.321575
19.233476	1075.447582	12.326579
20.062512	1068.144893	12.331584
19.663153	1070.004675	12.336589
19.554555	1086.657169	12.341594
19.722662	1073.123720	12.346599
19.648007	1070.259210	12.351603
19.573567	1094.068764	12.356608
19.576574	1075.403443	12.361613
19.745708	1073.813644	12.366618
19.289497	1078.357001	12.371623
19.235114	1076.687738	12.376627
19.591585	1071.084684	12.381632
19.470013	1096.349399	12.386637
19.614163	1078.612461	12.391642
19.349990	1078.156220	12.396647
19.364400	1102.352160	12.401651
19.866833	1073.196146	12.406656
19.457651	1073.983594	12.411661
19.884384	1101.841670	12.416666
19.936448	1093.532230	12.421671
19.473213	1076.805234	12.426675
19.932174	1082.833177	12.431680
19.550209	1071.839629	12.436685
19.476777	1052.393325	12.441690
19.760859	1048.467082	12.446695
19.532896	1065.558060	12.451699
19.385909	1049.554932	12.456704
19.224385	1053.122454	12.461709
19.376905	1076.704966	12.466714
19.573924	1080.732542	12.471719
19.486800	1085.713766	12.476723
19.725395	1081.976119	12.481728
19.317279	1086.060799	12.486733
19.590805	1094.445904	12.491738
19.699127	1094.173094	12.496743
19.829584	1077.546939	12.501747
19.876497	1100.361015	12.506752
19.594226	1059.821611	12.511757
19.438119	1083.410786	12.516762
19.708935	1051.718180	12.521767
19.333471	1050.513296	12.526771
19.855892	1085.575337	12.531776
19.822579	1061.800203	12.536781
19.354725	1055.754637	12.541786
19.647863	1078.608249	12.546791
19.530586	1055.636570	12.551795
19.700898	1052.263059	12.556800
19.432667	1056.727539	12.561805
19.560671	1064.681678	12.566810
19.452774	1056.952860	12.571815
19.162352	1066.812465	12.576819
19.751178	1084.719345	12.581824
19.640989	1081.691768	12.586829
19.996887	1090.459545	12.591834
19.715221	1085.824023	12.596839
19.806332	1069.899587	12.601843
20.122476	1051.761510	12.606848
19.653066	1070.163602	12.611853
19.841930	1071.819170	12.616858
19.843946	1060.791188	12.621863
19.566256	1080.813776	12.626867
19.538636	1066.822699	12.631872
19.408168	1062.609342	12.636877
19.576695	1070.531790	12.641882
19.639329	1068.299815	12.646887
19.593888	1077.626764	12.651891
19.903300	1066.005698	12.656896
19.856945	1075.492064	12.661901
19.817302	1060.080504	12.666906
19.838043	1039.091135	12.671911
19.452076	1036.615333	12.676915
19.679776	1037.113532	12.681920
19.511431	1044.878390	12.686925
19.345968	1032.322277	12.691930
19.438876	1035.767209	12.696935
19.372040	1056.647103	12.701939
19.825750	1048.538548	12.706944
19.689762	1031.825637	12.711949
19.460931	1045.322874	12.716954
19.494890	1039.899010	12.721959
19.757114	1043.316935	12.726963
19.580565	1040.192719	12.731968
19.436372	1039.592762	12.736973
19.510504	1042.029869	12.741978
19.546204	1037.651242	12.746983
19.566357	1042.098101	12.751987
19.675102	1033.822232	12.756992
19.511606	1044.058965	12.761997
19.605246	1045.168326	12.767002
19.894720	1041.663846	12.772007
19.452684	1061.547043	12.777011
19.885332	1023.984518	12.782016
19.425804	1055.643959	12.787021
19.723253	1030.237593	12.792026
19.497961	1028.554597	12.797031
19.428079	1035.639850	12.802035
19.483915	1044.934855	12.807040
19.410225	1035.697763	12.812045
19.280457	1036.562064	12.817050
19.675819	1045.673600	12.822055
19.496417	1045.645383	12.827059
19.608999	1047.510234	12.832064
19.701834	1046.156534	12.837069
19.729227	1042.089889	12.842074
20.021992	1044.646662	12.847079
19.259648	1036.821976	12.852083
19.326512	1020.816306	12.857088
19.320395	1041.747995	12.862093
19.351803	1052.461420	12.867098
19.476600	1032.136704	12.872103
19.561319	1066.399622	12.877107
19.866457	1067.390093	12.882112
19.505926	1070.560433	12.887117
19.512774	1074.302952	12.892122
19.695209	1066.061041	12.897127
19.491629	1069.528043	12.902131
19.851823	1057.058370	12.907136
19.588611	1049.008980	12.912141
19.343144	1042.301898	12.917146
19.699914	1035.019364	12.922151
19.566698	1044.789223	12.927155
19.493849	1035.504689	12.932160
19.019062	1046.101736	12.937165
19.359437	1053.840644	12.942170
19.585019	1067.366342	12.947175
19.258844	1071.256599	12.952179
19.770141	1072.854426	12.957184
19.585496	1085.679181	12.962189
19.387586	1079.327194	12.967194
20.043088	1078.443556	12.972199
19.863878	1094.079151	12.977203
19.900789	1067.000134	12.982208
19.531461	1052.814420	12.987213
19.603594	1048.463094	12.992218
19.759279	1041.477559	12.997223
19.307856	1052.264848	13.002227
19.466401	1040.945409	13.007232
19.720865	1046.302639	13.012237
19.590983	1041.201374	13.017242
19.673425	1049.459238	13.022247
19.677680	1048.539136	13.027251
19.588184	1044.841218	13.032256
19.482000	1051.700459	13.037261
19.691652	1050.086853	13.042266
19.502957	1049.410416	13.047271
19.194679	1051.958985	13.052275
19.581760	1042.935395	13.057280
19.644640	1037.874345	13.062285
19.588533	1054.772318	13.067290
19.465625	1055.059940	13.072295
19.534192	1054.883359	13.077299
19.497402	1049.877629	13.082304
19.275128	1052.213784	13.087309
19.295165	1072.792840	13.092314
20.018759	1075.515861	13.097319
19.671824	1093.677674	13.102323
20.044360	1069.872482	13.107328
19.848372	1053.244809	13.112333
19.400308	1057.715898	13.117338
19.740771	1050.595229	13.122343
19.594342	1068.110018	13.127347
19.804218	1050.203359	13.132352
19.346242	1061.100509	13.137357
19.446617	1052.004375	13.142362
19.635442	1048.809260	13.147367
19.460706	1050.303628	13.152371
19.560756	1042.927999	13.157376
20.019606	1044.215647	13.162381
19.482196	1062.551306	13.167386
19.903165	1039.003365	13.172391
19.387654	1036.434688	13.177395
19.661589	1052.791159	13.182400
19.624036	1061.214827	13.187405
19.497562	1047.267923	13.192410
19.604614	1048.920768	13.197415
19.596948	1059.925859	13.202419
19.564176	1057.422099	13.207424
19.438616	1065.410378	13.212429
19.530736	1056.548946	13.217434
20.063423	1058.876640	13.222439
19.537166	1054.179218	13.227443
19.691723	1068.539412	13.232448
19.416665	1060.028283	13.237453
19.528526	1056.848597	13.242458
19.940863	1040.242176	13.247463
19.664645	1065.399041	13.252467
19.394471	1053.170272	13.257472
19.272828	1051.541702	13.262477
19.679798	1063.929870	13.267482
19.614274	1059.502728	13.272487
19.542721	1056.847461	13.277491
19.718049	1052.011320	13.282496
19.449977	1064.825709	13.287501
19.483961	1058.135545	13.292506
19.567595	1059.677010	13.297511
19.444030	1070.779444	13.302515
19.604131	1066.921858	13.307520
19.630840	1058.980757	13.312525
19.467871	1062.283584	13.317530
19.671852	1060.670882	13.322535
19.424152	1062.255737	13.327539
19.553783	1064.062677	13.332544
19.577656	1057.965481	13.337549
19.520226	1065.821467	13.342554
19.664673	1061.135328	13.347559
19.450180	1067.636540	13.352563
19.464340	1068.892622	13.357568
19.746516	1075.218418	13.362573
19.753260	1057.025609	13.367578
19.496780	1071.913418	13.372583
19.496087	1072.355010	13.377587
19.580089	1065.973830	13.382592
19.389178	1056.383264	13.387597
19.061923	1080.319855	13.392602
19.610269	1069.966387	13.397607
19.484352	1072.358138	13.402611
19.773393	1065.827558	13.407616
19.915008	1065.432744	13.412621
19.631572	1068.387361	13.417626
19.735604	1074.615417	13.422631
19.610737	1075.417438	13.427635
19.773455	1062.685947	13.432640
19.956713	1059.334024	13.437645
19.481804	1073.796208	13.442650
19.937168	1060.727880	13.447655
19.867625	1055.025631	13.452659
19.719684	1041.694011	13.457664
19.561770	1045.928003	13.462669
19.139272	1031.301362	13.467674
19.592798	1046.790245	13.472679
19.518834	1031.832042	13.477683
19.359569	1035.657818	13.482688
19.772720	1054.638199	13.487693
19.379746	1062.779518	13.492698
19.762238	1068.072178	13.497703
19.528553	1070.514236	13.502707
19.549010	1061.001914	13.507712
19.531458	1057.529058	13.512717
19.337161	1066.569087	13.517722
20.118631	1061.379213	13.522727
19.449094	1054.079029	13.527731
19.545838	1045.576410	13.532736
19.590565	1048.384059	13.537741
19.355192	1052.155748	13.542746
19.520222	1046.966439	13.547751
19.698475	1068.381263	13.552755
19.655272	1069.409953	13.557760
19.892871	1053.681364	13.562765
19.834262	1053.504569	13.567770
19.964431	1036.088456	13.572775
19.693408	1048.463335	13.577779
19.565820	1048.477314	13.582784
19.700304	1036.795866	13.587789
19.838331	1040.608914	13.592794
19.803947	1038.094377	13.597799
19.533850	1033.111675	13.602803
19.683172	1049.268825	13.607808
19.708342	1051.024617	13.612813
19.372839	1049.409661	13.617818
19.654315	1049.432507	13.622823
19.606408	1062.497202	13.627827
19.396671	1050.746071	13.632832
19.445404	1054.847755	13.637837
19.449515	1057.827465	13.642842
19.636623	1047.416517	13.647847
19.323832	1066.619942	13.652851
19.329062	1051.950283	13.657856
19.565190	1053.177264	13.662861
19.386046	1051.531059	13.667866
19.566468	1050.021463	13.672871
19.355171	1059.045275	13.677875
19.371256	1051.246221	13.682880
19.108535	1047.363046	13.687885
19.223524	1052.944375	13.692890
19.561242	1076.983046	13.697895
19.531661	1079.463510	13.702899
19.520045	1080.499777	13.707904
19.674355	1087.870993	13.712909
19.425637	1088.542959	13.717914
19.648846	1079.889260	13.722919
19.690510	1091.020547	13.727923
19.716273	1078.377121	13.732928
19.687187	1066.606623	13.737933
19.567813	1060.313080	13.742938
19.750716	1046.454021	13.747943
19.592265	1057.637703	13.752947
19.553292	1052.257006	13.757952
19.514998	1045.846457	13.762957
19.331486	1058.182154	13.767962
19.617083	1049.505906	13.772967
19.358202	1052.076558	13.777971
19.804213	1064.225110	13.782976
19.612816	1052.914174	13.787981
19.389247	1059.667565	13.792986
19.345217	1061.948482	13.797991
19.672051	1079.159135	13.802995
19.904828	1074.419479	13.808000
19.749440	1063.779301	13.813005
19.358164	1054.621242	13.818010
19.861378	1041.464874	13.823015
19.511679	1046.631471	13.828019
19.615941	1052.510977	13.833024
19.810351	1045.763689	13.838029
19.576484	1048.481737	13.843034
19.512758	1060.967062	13.848039
19.446137	1060.657504	13.853043
19.343722	1039.714588	13.858048
19.537967	1047.943578	13.863053
19.116178	1065.380862	13.868058
19.755150	1053.948510	13.873063
20.014271	1065.751562	13.878067
19.783460	1046.655221	13.883072
19.636735	1057.255140	13.888077
19.066087	1067.042750	13.893082
19.057155	1037.009593	13.898087
19.588918	1082.463782	13.903091
19.757103	1065.131457	13.908096
19.667211	1071.850915	13.913101
19.414103	1066.903338	13.918106
19.774462	1057.865077	13.923111
19.506353	1057.234423	13.928115
19.647842	1055.803576	13.933120
19.701486	1052.464444	13.938125
19.712429	1057.365361	13.943130
19.659640	1053.281541	13.948135
19.630808	1065.672995	13.953139
19.443417	1050.747058	13.958144
19.423312	1053.598165	13.963149
19.608736	1062.921396	13.968154
19.501478	1059.133267	13.973159
19.520830	1057.431744	13.978163
19.504424	1059.586829	13.983168
19.784125	1054.935888	13.988173
19.501241	1053.372462	13.993178
19.571654	1051.626525	13.998183
19.680539	1056.637975	14.003187
19.381098	1043.341558	14.008192
19.508137	1057.183836	14.013210
19.359410	1064.008820	14.018227
19.594505	1054.865597	14.023245
19.443307	1071.556360	14.028263
19.624243	1078.364942	14.033280
20.098101	1077.169368	14.038298
19.702927	1092.585679	14.043315
19.585519	1070.320692	14.048333
19.379549	1069.614207	14.053351
19.683833	1080.508451	14.058368
20.049028	1103.171074	14.063386
19.866449	1089.057936	14.068403
19.576954	1061.878276	14.073421
19.457591	1086.647238	14.078439
19.744293	1089.903016	14.083456
19.925635	1089.976265	14.088474
19.796369	1091.799396	14.093491
19.860001	1093.936227	14.098509
19.480422	1093.070256	14.103527
19.644215	1098.920524	14.108544
19.506428	1102.635675	14.113562
19.593225	1107.625253	14.118579
20.129083	1092.063669	14.123597
20.020397	1096.980612	14.128615
20.015275	1098.010060	14.133632
20.112752	1100.283057	14.138650
19.989763	1098.715526	14.143667
19.942348	1094.045137	14.148685
20.057348	1100.373494	14.153703
20.051369	1107.597274	14.158720
20.066997	1088.203656	14.163738
19.907152	1104.527770	14.168755
20.126035	1096.689492	14.173773
20.048721	1105.491286	14.178791
19.872649	1103.554719	14.183808
19.982543	1113.946773	14.188826
19.975093	1133.192709	14.193843
20.161205	1134.610055	14.198861
20.271998	1125.277416	14.203879
19.968796	1122.536909	14.208896
20.278836	1143.073925	14.213914
20.148292	1127.245817	14.218931
20.135365	1137.651188	14.223949
20.124188	1129.490961	14.228967
20.260418	1115.894772	14.233984
20.574931	1123.534597	14.239002
20.323354	1141.735736	14.244019
20.539021	1121.632231	14.249037
20.295876	1122.160133	14.254055
20.369718	1148.002579	14.259072
20.663150	1115.355120	14.264090
20.347876	1126.008472	14.269107
20.285664	1133.963210	14.274125
20.509892	1126.597516	14.279143
20.636107	1135.521010	14.284160
20.546436	1127.543182	14.289178
20.367595	1148.164479	14.294195
20.496345	1136.107793	14.299213
20.550348	1124.678057	14.304231
20.531532	1158.697244	14.309248
21.075878	1142.523954	14.314266
20.592687	1149.285932	14.319283
20.733247	1135.251758	14.324301
20.533152	1124.416225	14.329319
20.355324	1158.193378	14.334336
20.909956	1142.348763	14.339354
20.613205	1162.886649	14.344371
21.058636	1161.920533	14.349389
21.510296	1153.968020	14.354407
20.724019	1152.300231	14.359424
21.001423	1134.145164	14.364442
20.790506	1140.931343	14.369459
20.682741	1122.416183	14.374477
20.986047	1127.451452	14.379495
20.722282	1135.960554	14.384512
21.288319	1128.546629	14.389530
20.814601	1124.626882	14.394547
20.714658	1127.315170	14.399565
21.173757	1137.470652	14.404583
20.877354	1141.565023	14.409600
21.216813	1135.895441	14.414618
20.984322	1131.295458	14.419635
21.003793	1139.133355	14.424653
21.162249	1144.504749	14.429671
20.401981	1153.624711	14.434688
21.084695	1170.196724	14.439706
21.231679	1173.361556	14.444723
21.318057	1161.847979	14.449741
21.375600	1164.643280	14.454759
21.297251	1175.010352	14.459776
21.539189	1161.625334	14.464794
21.609185	1167.588113	14.469811
21.425571	1145.247061	14.474829
21.411807	1143.454475	14.479847
21.193055	1149.867550	14.484864
21.320444	1138.651026	14.489882
21.235248	1133.684647	14.494899
20.871276	1132.426096	14.499917
21.384329	1146.528902	14.504935
21.479571	1159.535969	14.509952
21.524825	1167.483020	14.514970
21.388871	1158.623849	14.519987
21.444062	1179.673449	14.525005
21.591084	1166.866678	14.530023
21.471782	1170.728326	14.535040
21.720754	1163.825829	14.540058
21.528008	1168.786091	14.545075
21.274054	1168.549698	14.550093
21.399239	1163.120339	14.555111
21.201497	1169.531645	14.560128
21.724529	1163.618851	14.565146
21.970111	1174.096263	14.570163
21.590340	1172.286555	14.575181
21.896909	1168.707921	14.580199
21.687763	1172.808831	14.585216
21.450227	1166.057864	14.590234
21.757815	1169.505372	14.595251
21.515141	1180.334363	14.600269
21.762155	1172.724352	14.605287
21.371906	1178.222606	14.610304
21.457198	1175.700102	14.615322
21.343200	1176.422898	14.620339
21.565577	1177.985466	14.625357
21.535985	1168.344875	14.630375
21.910765	1191.183849	14.635392
22.186355	1194.144137	14.640410
21.885238	1188.238533	14.645427
22.140678	1182.555595	14.650445
21.928921	1175.920055	14.655463
21.812333	1173.220553	14.660480
22.096384	1185.398474	14.665498
22.116894	1205.127656	14.670515
21.788448	1191.662143	14.675533
22.187149	1195.397128	14.680551
22.051759	1196.700605	14.685568
22.019476	1210.725303	14.690586
21.951057	1208.494712	14.695603
21.792092	1200.222747	14.700621
22.242497	1199.071801	14.705639
21.891701	1201.104878	14.710656
22.131659	1204.188823	14.715674
21.979117	1193.529687	14.720691
21.894764	1199.528111	14.725709
22.221165	1198.955339	14.730727
21.884954	1202.150064	14.735744
21.923534	1198.175320	14.740762
22.209200	1216.474890	14.745779
22.507373	1230.517678	14.750797
22.632231	1230.481967	14.755815
22.490835	1239.662133	14.760832
22.119229	1213.236142	14.765850
22.346799	1224.071949	14.770867
22.551564	1226.612555	14.775885
22.484050	1241.375893	14.780903
22.630271	1239.578225	14.785920
23.022312	1230.148749	14.790938
22.900004	1206.732940	14.795955
22.754253	1201.697550	14.800973
22.831313	1194.509445	14.805991
22.690361	1201.790978	14.811008
22.790616	1210.877526	14.816026
22.731406	1193.469746	14.821043
22.583955	1199.580476	14.826061
22.777731	1197.960833	14.831079
22.546343	1201.480166	14.836096
22.792201	1196.849474	14.841114
22.570516	1195.461261	14.846131
22.337992	1204.375957	14.851149
22.760225	1194.494973	14.856167
22.729580	1201.140746	14.861184
22.569446	1189.740397	14.866202
22.591225	1203.876008	14.871219
22.716184	1225.724610	14.876237
22.932276	1220.898896	14.881255
22.670964	1230.581076	14.886272
23.163334	1227.064021	14.891290
22.953619	1228.351044	14.896307
22.764111	1240.643873	14.901325
23.100742	1236.818193	14.906343
22.990812	1239.945373	14.911360
22.922523	1238.741889	14.916378
23.230227	1219.982591	14.921395
23.036896	1241.740423	14.926413
23.212484	1234.624667	14.931431
23.130348	1231.141052	14.936448
23.235821	1224.977104	14.941466
22.925561	1232.919555	14.946483
22.969194	1234.754447	14.951501
23.239807	1239.139053	14.956519
23.154498	1246.584757	14.961536
23.279090	1226.141722	14.966554
23.322650	1228.088304	14.971571
23.294383	1249.494220	14.976589
23.136399	1207.902442	14.981607
22.647425	1236.881608	14.986624
23.212144	1220.459602	14.991642
22.995190	1226.592441	14.996659
22.811512	1256.985785	15.001677
23.325930	1255.566661	15.006695
23.072928	1262.452414	15.011712
23.264716	1263.845273	15.016730
23.301708	1265.948630	15.021747
23.216784	1270.361644	15.026765
23.662969	1264.594768	15.031783
23.908581	1265.238185	15.036800
23.713033	1254.851691	15.041818
23.677037	1275.725650	15.046835
23.487848	1270.395159	15.051853
23.854304	1264.230462	15.056871
24.007057	1264.781730	15.061888
23.553171	1265.077424	15.066906
24.097804	1269.300358	15.071923
23.747025	1255.383766	15.076941
23.787004	1272.550753	15.081959
23.897723	1264.558187	15.086976
23.768116	1264.443523	15.091994
23.937430	1261.937488	15.097011
23.630519	1257.459441	15.102029
23.391115	1276.794474	15.107047
23.661000	1255.349849	15.112064
23.469576	1268.096015	15.117082
23.678834	1263.832919	15.122099
23.656583	1260.207617	15.127117
23.870114	1256.816826	15.132135
23.743562	1256.969075	15.137152
23.869072	1251.052019	15.142170
23.761420	1260.519383	15.147187
24.006652	1276.428309	15.152205
24.481566	1284.676533	15.157223
23.998584	1277.635918	15.162240
24.031059	1295.154896	15.167258
24.305226	1273.344637	15.172275
24.046952	1272.300437	15.177293
24.117889	1274.390515	15.182311
24.344188	1305.520768	15.187328
24.292488	1288.975225	15.192346
24.535075	1288.082354	15.197363
24.331290	1285.277196	15.202381
24.222640	1258.305835	15.207399
24.202196	1265.409310	15.212416
24.166594	1262.424754	15.217434
24.169768	1247.210655	15.222451
24.368244	1293.563568	15.227469
24.486782	1289.642108	15.232487
24.513649	1286.274793	15.237504
24.440008	1289.506302	15.242522
24.426394	1287.485597	15.247539
24.570039	1293.268375	15.252557
24.188333	1300.500275	15.257575
24.374953	1288.913982	15.262592
24.092258	1283.246061	15.267610
24.423424	1309.741420	15.272627
24.366935	1277.191883	15.277645
24.436331	1314.672008	15.282663
24.047486	1277.631228	15.287680
24.123312	1300.470873	15.292698
24.650355	1303.191310	15.297715
24.323798	1317.458096	15.302733
24.404261	1316.133355	15.307751
25.177216	1295.174690	15.312768
24.504618	1328.128285	15.317786
25.128173	1313.169075	15.322803
25.192070	1302.665662	15.327821
24.823757	1321.433033	15.332839
25.070298	1299.859938	15.337856
24.751414	1324.535296	15.342874
25.136077	1317.724334	15.347891
24.865331	1303.743022	15.352909
24.974684	1308.840751	15.357927
25.072777	1312.634728	15.362944
24.949905	1330.471097	15.367962
25.210409	1322.020473	15.372979
25.259242	1308.633090	15.377997
24.800797	1326.847010	15.383015
25.054809	1314.767049	15.388032
25.126506	1319.378455	15.393050
25.449204	1317.085460	15.398067
25.302172	1313.986539	15.403085
25.213716	1318.853141	15.408103
25.199021	1317.244718	15.413120
25.304557	1323.230206	15.418138
25.066769	1319.299512	15.423155
25.230332	1319.389756	15.428173
25.399559	1302.327634	15.433191
25.404992	1317.969705	15.438208
25.322915	1321.740516	15.443226
25.578993	1316.324826	15.448243
25.724736	1320.155248	15.453261
25.720090	1299.649358	15.458279
25.827853	1294.914827	15.463296
25.403372	1305.738306	15.468314
25.645754	1286.795868	15.473331
25.307107	1278.975641	15.478349
25.095619	1286.616089	15.483367
25.760463	1315.611131	15.488384
25.217853	1316.883624	15.493402
25.637153	1296.770990	15.498419
25.471440	1319.528075	15.503437
25.439868	1314.109508	15.508455
26.006887	1306.464113	15.513472
25.517858	1314.697807	15.518490
25.753427	1318.320427	15.523507
25.941593	1316.637175	15.528525
25.775238	1318.329402	15.533543
25.743958	1330.833011	15.538560
25.792075	1329.549607	15.543578
25.840738	1306.625439	15.548595
25.747570	1332.096897	15.553613
25.672079	1327.113174	15.558631
26.145033	1312.630998	15.563648
25.715773	1309.882248	15.568666
25.638598	1309.897640	15.573683
25.701607	1332.571074	15.578701
25.822893	1301.226322	15.583719
25.765122	1317.139583	15.588736
25.861372	1355.557729	15.593754
26.234289	1348.185509	15.598771
26.150964	1359.967594	15.603789
25.932187	1356.612705	15.608807
26.138311	1344.861241	15.613824
25.776095	1359.283187	15.618842
26.231117	1349.934820	15.623859
26.234075	1354.635849	15.628877
26.179110	1366.297016	15.633895
26.290202	1362.640981	15.638912
26.092792	1347.723030	15.643930
26.242169	1353.393238	15.648947
26.461176	1353.954390	15.653965
26.179861	1362.103071	15.658983
26.462797	1328.239339	15.664000
26.215866	1378.559776	15.669018
26.257025	1359.658778	15.674035
26.348133	1354.450279	15.679053
26.453238	1363.537722	15.684071
26.390019	1359.547712	15.689088
26.416528	1387.329727	15.694106
26.524629	1385.756762	15.699123
26.859201	1386.290044	15.704141
26.601906	1378.856319	15.709159
26.683071	1383.817004	15.714176
26.818487	1384.931017	15.719194
26.892575	1388.370208	15.724211
26.745154	1363.822474	15.729229
26.474918	1366.201356	15.734247
27.036753	1371.315018	15.739264
26.968936	1374.290797	15.744282
27.009490	1375.896547	15.749299
27.221650	1359.898694	15.754317
26.531828	1361.392864	15.759335
26.478160	1349.052081	15.764352
26.848440	1372.610901	15.769370
27.006597	1375.998929	15.774387
27.120567	1372.878811	15.779405
26.788874	1387.572757	15.784423
27.300956	1378.699741	15.789440
27.174697	1380.851176	15.794458
27.520130	1384.519206	15.799475
27.488694	1364.203107	15.804493
27.013528	1359.994101	15.809511
27.076191	1346.464484	15.814528
26.933792	1347.361697	15.819546
26.805005	1357.018104	15.824563
27.107861	1362.756639	15.829581
26.999397	1380.796829	15.834599
27.400444	1383.450867	15.839616
27.265016	1395.823287	15.844634
27.089326	1389.619178	15.849651
27.299821	1377.369936	15.854669
27.297064	1387.056594	15.859687
27.424786	1380.240972	15.864704
27.380182	1373.754849	15.869722
27.520398	1381.065553	15.874739
27.790907	1388.070771	15.879757
27.691475	1381.406208	15.884775
27.942743	1377.164691	15.889792
27.674616	1376.345414	15.894810
27.652465	1372.567491	15.899827
27.919024	1364.746632	15.904845
27.634658	1384.858157	15.909863
27.693220	1373.871071	15.914880
27.973752	1377.933254	15.919898
27.419922	1382.724678	15.924915
27.288685	1382.624429	15.929933
27.130399	1386.780205	15.934951
27.598728	1374.415909	15.939968
27.645706	1372.410694	15.944986
27.145366	1391.650654	15.950003
27.723483	1362.304490	15.955021
27.639864	1410.035067	15.960039
27.900319	1393.096708	15.965056
27.628561	1422.264955	15.970074
27.935882	1412.672703	15.975091
28.032932	1405.808481	15.980109
28.164147	1413.290517	15.985127
28.135235	1406.289090	15.990144
28.299151	1418.093131	15.995162
28.172617	1407.193744	16.000179
28.083460	1408.220888	16.005197
28.154485	1415.078622	16.010215
28.323608	1405.525721	16.015232
28.368123	1401.131567	16.020250
28.081365	1417.520319	16.025267
28.621059	1404.770249	16.030285
28.197991	1412.216433	16.035303
28.538265	1400.443527	16.040320
28.725510	1402.611022	16.045338
28.162374	1404.357111	16.050355
28.512740	1384.639154	16.055373
28.423731	1400.134362	16.060391
28.200735	1409.288327	16.065408
28.286645	1396.041234	16.070426
28.321459	1416.138068	16.075443
28.190815	1422.483728	16.080461
28.542727	1394.302970	16.085479
28.404333	1401.371845	16.090496
28.198249	1413.060301	16.095514
28.217696	1408.693737	16.100531
28.487474	1398.445266	16.105549
28.345274	1405.159262	16.110567
28.599168	1428.771343	16.115584
28.695948	1425.990571	16.120602
28.829255	1425.406121	16.125619
28.832639	1413.546948	16.130637
28.780398	1424.751568	16.135655
28.942462	1424.672172	16.140672
29.214209	1412.666377	16.145690
28.842165	1416.256958	16.150707
29.627574	1410.748937	16.155725
28.969052	1412.546420	16.160743
28.897849	1387.594819	16.165760
29.304927	1394.587695	16.170778
29.196325	1404.264508	16.175795
29.426204	1387.134412	16.180813
29.151606	1389.993746	16.185831
28.887222	1389.620592	16.190848
28.980897	1392.768809	16.195866
28.992989	1393.424313	16.200883
29.181334	1386.581716	16.205901
28.997941	1399.391208	16.210919
29.002552	1412.606433	16.215936
29.137178	1397.781752	16.220954
29.271855	1408.590045	16.225971
29.318430	1410.868066	16.230989
29.206928	1424.938639	16.236007
29.254373	1413.656006	16.241024
29.418856	1408.685885	16.246042
28.986958	1424.608605	16.251059
29.363239	1417.050205	16.256077
29.318391	1413.381280	16.261095
29.256853	1421.532688	16.266112
29.154224	1414.813566	16.271130
29.230918	1417.980226	16.276147
29.447146	1427.655576	16.281165
29.578799	1445.495531	16.286183
29.628337	1446.956715	16.291200
29.833295	1452.896512	16.296218
29.868935	1449.705505	16.301235
29.899481	1437.093247	16.306253
29.826749	1438.943581	16.311271
29.605002	1447.425713	16.316288
30.038517	1446.197224	16.321306
29.847720	1445.736827	16.326323
30.002700	1447.822963	16.331341
29.742375	1438.848183	16.336359
30.148128	1436.834494	16.341376
30.120990	1433.266555	16.346394
29.717904	1447.157152	16.351411
29.954059	1446.230693	16.356429
30.223589	1436.362894	16.361447
29.974201	1438.975980	16.366464
30.436821	1431.605139	16.371482
30.160218	1436.275285	16.376499
30.353651	1430.293841	16.381517
30.073188	1439.589119	16.386535
30.239010	1443.611419	16.391552
30.599849	1431.295680	16.396570
30.085009	1441.881998	16.401587
30.145495	1442.671352	16.406605
30.360751	1433.010405	16.411623
30.305598	1440.056584	16.416640
30.488182	1439.495734	16.421658
30.261570	1435.758272	16.426675
30.201270	1450.604040	16.431693
30.143308	1438.644523	16.436711
30.048302	1453.429764	16.441728
30.552288	1442.151363	16.446746
30.368301	1444.838958	16.451763
30.154070	1440.706279	16.456781
30.746578	1440.997082	16.461799
30.618110	1461.181369	16.466816
30.559639	1456.116238	16.471834
30.758476	1473.780350	16.476851
30.861531	1468.840455	16.481869
30.787697	1466.237894	16.486887
30.771878	1482.248460	16.491904
31.156608	1475.363486	16.496922
30.671070	1456.241218	16.501939
31.008124	1470.171076	16.506957
30.765052	1463.211648	16.511975
30.573126	1466.908786	16.516992
30.810956	1478.137963	16.522010
30.992297	1473.341303	16.527027
31.080959	1474.291326	16.532045
31.125303	1477.502484	16.537063
30.996859	1481.735321	16.542080
31.193897	1471.518850	16.547098
31.268770	1477.446375	16.552115
30.957412	1477.230142	16.557133
30.971018	1485.386903	16.562151
31.167755	1487.870637	16.567168
30.808191	1466.420714	16.572186
30.813764	1472.057281	16.577203
30.891165	1480.276219	16.582221
31.040708	1495.497533	16.587239
31.204976	1474.942430	16.592256
31.635851	1510.779852	16.597274
31.356445	1490.308081	16.602291
31.249746	1504.444029	16.607309
31.731530	1494.979620	16.612327
31.514308	1507.618430	16.617344
31.726858	1497.161948	16.622362
31.673523	1505.126484	16.627379
31.996348	1500.217589	16.632397
31.902292	1497.644988	16.637415
31.637695	1484.118681	16.642432
31.780778	1484.644761	16.647450
31.657890	1466.990414	16.652467
31.729431	1482.864355	16.657485
31.933020	1490.882280	16.662503
31.943948	1488.406190	16.667520
31.591133	1486.110811	16.672538
31.786814	1504.887554	16.677555
32.104480	1495.551566	16.682573
32.123852	1483.954043	16.687591
31.806588	1512.270888	16.692608
32.268855	1485.856101	16.697626
32.083236	1514.276216	16.702643
31.944252	1489.176382	16.707661
32.444252	1510.883799	16.712679
31.692254	1482.885243	16.717696
32.588778	1506.163720	16.722714
32.350389	1485.982704	16.727731
32.247010	1490.189523	16.732749
32.377164	1466.229674	16.737767
32.092354	1471.083604	16.742784
32.413401	1486.010147	16.747802
32.011659	1492.955911	16.752819
32.102082	1493.688585	16.757837
32.390751	1497.681867	16.762855
32.126877	1494.076171	16.767872
32.394383	1490.955133	16.772890
32.417408	1506.879309	16.777907
32.052726	1491.954857	16.782925
32.117356	1485.243628	16.787943
32.209495	1501.741919	16.792960
32.507555	1492.729947	16.797978
32.428515	1506.583070	16.802995
32.163293	1511.142889	16.808013
32.325802	1515.291574	16.813031
32.452435	1513.806873	16.818048
32.975023	1512.312495	16.823066
32.577186	1530.479250	16.828083
32.664616	1521.055705	16.833101
32.774748	1518.861077	16.838119
32.430671	1531.483964	16.843136
32.590297	1520.413009	16.848154
32.931983	1535.902582	16.853171
32.832592	1553.655258	16.858189
33.266890	1552.483263	16.863207
33.469388	1543.794806	16.868224
33.261339	1527.838627	16.873242
32.784103	1524.284259	16.878259
32.672426	1521.473799	16.883277
33.356649	1537.086484	16.888295
32.838720	1556.008578	16.893312
33.306262	1553.439195	16.898330
33.360211	1546.995475	16.903347
33.789928	1545.419956	16.908365
33.769301	1539.332616	16.913383
33.627103	1528.894945	16.918400
33.547893	1517.294244	16.923418
33.245936	1512.620277	16.928435
33.430835	1512.230509	16.933453
33.574943	1505.083464	16.938471
33.267065	1508.155762	16.943488
33.484277	1505.333743	16.948506
33.264455	1524.356107	16.953523
33.354416	1530.687074	16.958541
33.403688	1537.452384	16.963559
33.983304	1543.829519	16.968576
33.993606	1539.852899	16.973594
33.936816	1538.359701	16.978611
33.683200	1544.918505	16.983629
34.252729	1543.319112	16.988647
33.908655	1538.790277	16.993664
33.793895	1518.613090	16.998682
34.172405	1518.716240	17.003699
33.650338	1521.865175	17.008717
34.024579	1519.867513	17.013735
33.751062	1522.297278	17.018752
34.182214	1533.242413	17.023770
34.186439	1547.042970	17.028787
34.051110	1547.011010	17.033805
34.312295	1541.229493	17.038823
33.918318	1538.851011	17.043840
33.891657	1544.352752	17.048858
33.732569	1533.795079	17.053875
33.688326	1534.104083	17.058893
33.942419	1548.862052	17.063911
33.908047	1550.132144	17.068928
34.220802	1538.450030	17.073946
34.117073	1554.204146	17.078963
34.023331	1571.968527	17.083981
34.549720	1558.602265	17.088999
34.356493	1578.953557	17.094016
34.543039	1572.399802	17.099034
34.665949	1566.764596	17.104051
34.582156	1575.574000	17.109069
34.394381	1570.526307	17.114087
34.346790	1562.439283	17.119104
34.740103	1571.951208	17.124122
34.743113	1565.554929	17.129139
34.527000	1576.505815	17.134157
35.073136	1573.626599	17.139175
34.618706	1573.461499	17.144192
34.287889	1580.676768	17.149210
34.630459	1567.899012	17.154227
34.479197	1566.295042	17.159245
34.886975	1578.377271	17.164263
34.896170	1599.340439	17.169280
34.991217	1607.762696	17.174298
35.509948	1596.209699	17.179315
34.976207	1599.898473	17.184333
35.381315	1579.296942	17.189351
35.170632	1575.897453	17.194368
34.961076	1574.464797	17.199386
35.290084	1582.237045	17.204403
35.306144	1584.228959	17.209421
35.167731	1575.399023	17.214439
35.147603	1578.349148	17.219456
35.119779	1589.287314	17.224474
35.500567	1605.535195	17.229491
35.275977	1599.944393	17.234509
35.272698	1593.281698	17.239527
35.558167	1591.114147	17.244544
35.325075	1592.283809	17.249562
35.453393	1602.942256	17.254579
35.288854	1599.415068	17.259597
35.466281	1605.455272	17.264615
35.705069	1593.209200	17.269632
35.702036	1588.622804	17.274650
35.677334	1586.259343	17.279667
35.489328	1593.801828	17.284685
35.718237	1589.178436	17.289703
35.587410	1583.545944	17.294720
35.559665	1582.120465	17.299738
36.228497	1591.690700	17.304755
35.807067	1599.064359	17.309773
35.877248	1590.068226	17.314791
35.815734	1593.280565	17.319808
36.016074	1608.682654	17.324826
36.423598	1608.913308	17.329843
35.920299	1599.528882	17.334861
36.202749	1590.917304	17.339879
36.172252	1587.540193	17.344896
36.080188	1578.271080	17.349914
36.404278	1589.827922	17.354931
36.141621	1590.487935	17.359949
36.109424	1587.236934	17.364967
36.492525	1601.209910	17.369984
36.373319	1597.559091	17.375002
36.560610	1587.430608	17.380019
35.924796	1597.621067	17.385037
36.273171	1610.336486	17.390055
36.276495	1610.810932	17.395072
36.341910	1615.156027	17.400090
36.185225	1607.073795	17.405107
36.436628	1617.344542	17.410125
36.755147	1604.285094	17.415143
36.475484	1603.775948	17.420160
36.489785	1609.656561	17.425178
36.725559	1598.307566	17.430195
36.647098	1610.056045	17.435213
36.603437	1611.931650	17.440231
36.602910	1599.874752	17.445248
36.832140	1615.582118	17.450266
36.588126	1624.725412	17.455283
36.747236	1637.706992	17.460301
36.806528	1636.637277	17.465319
36.751100	1639.200585	17.470336
36.653080	1642.627964	17.475354
37.192729	1634.898679	17.480371
37.050259	1648.131287	17.485389
36.881094	1639.366778	17.490407
36.824411	1640.157530	17.495424
37.044194	1638.344933	17.500442
37.507002	1642.972708	17.505459
37.346097	1643.729748	17.510477
37.356779	1629.382340	17.515495
37.510336	1629.964955	17.520512
37.504046	1635.210230	17.525530
37.683092	1625.333141	17.530547
37.501158	1633.466120	17.535565
37.164592	1631.015546	17.540583
37.731934	1635.203511	17.545600
37.464589	1631.942817	17.550618
37.732659	1630.433971	17.555635
37.545080	1640.996546	17.560653
37.845170	1644.844906	17.565671
37.691247	1648.491984	17.570688
37.420854	1654.748353	17.575706
38.166529	1651.977291	17.580723
38.182063	1659.663519	17.585741
38.406642	1638.343530	17.590759
38.255740	1632.516025	17.595776
38.393931	1615.975998	17.600794
38.344093	1607.618753	17.605811
38.360164	1624.286616	17.610829
38.456410	1613.754223	17.615847
38.595047	1605.110520	17.620864
38.194449	1589.479133	17.625882
38.595128	1575.605172	17.630899
38.426035	1583.868992	17.635917
38.045899	1583.762825	17.640935
38.355648	1580.323580	17.645952
38.217777	1586.585523	17.650970
38.139455	1584.653746	17.655987
38.077749	1586.933336	17.661005
37.996919	1576.558985	17.666023
38.268600	1589.169433	17.671040
38.153342	1606.470113	17.676058
38.401929	1605.096508	17.681075
38.534465	1603.247497	17.686093
38.118496	1609.682792	17.691111
38.563051	1618.708388	17.696128
38.238871	1614.627801	17.701146
38.483880	1618.676844	17.706163
38.486265	1607.105527	17.711181
38.649364	1607.924139	17.716199
38.530561	1615.903898	17.721216
38.607907	1642.578778	17.726234
39.032373	1645.314073	17.731251
38.857302	1652.840368	17.736269
38.646435	1653.383586	17.741287
38.933299	1650.338077	17.746304
38.465949	1645.240572	17.751322
38.795227	1646.496712	17.756339
38.683810	1648.183360	17.761357
38.894154	1642.310814	17.766375
38.905640	1656.130765	17.771392
38.870839	1675.189879	17.776410
39.120910	1677.691881	17.781427
39.261598	1674.512383	17.786445
39.428112	1687.300922	17.791463
39.418308	1670.933873	17.796480
39.221457	1678.400735	17.801498
39.894002	1666.458215	17.806515
39.592267	1677.341038	17.811533
39.395348	1672.667567	17.816551
39.356774	1669.282288	17.821568
39.105042	1677.868435	17.826586
39.374524	1669.326518	17.831603
39.727463	1669.018480	17.836621
39.327940	1675.017035	17.841639
39.864065	1667.746035	17.846656
40.162149	1669.744886	17.851674
40.186435	1671.516854	17.856691
40.328740	1674.459179	17.861709
40.007675	1666.878176	17.866727
40.288775	1662.774961	17.871744
39.893843	1674.058029	17.876762
40.025044	1673.009875	17.881779
40.309041	1673.088778	17.886797
39.789420	1676.166570	17.891815
40.007212	1667.584136	17.896832
39.801564	1673.687044	17.901850
39.857186	1665.935848	17.906867
40.141811	1676.081791	17.911885
40.212270	1675.238376	17.916903
40.272054	1666.080263	17.921920
40.072990	1670.775866	17.926938
40.063340	1676.215171	17.931955
40.161933	1695.186969	17.936973
40.036705	1690.860699	17.941991
40.322012	1682.832192	17.947008
40.426912	1703.269023	17.952026
40.024232	1710.373911	17.957043
40.649929	1703.300961	17.962061
40.576052	1683.614089	17.967079
40.511195	1706.582205	17.972096
40.227804	1714.157269	17.977114
40.426514	1709.999543	17.982131
40.947130	1721.336386	17.987149
40.884482	1725.041282	17.992167
41.069683	1709.517671	17.997184
40.981578	1737.099992	18.002202
41.297010	1723.836440	18.007219
41.206902	1717.720783	18.012237
41.029481	1734.926140	18.017255
41.162551	1694.315280	18.022272
40.955493	1713.570231	18.027290
41.263099	1724.409379	18.032307
41.286291	1716.819056	18.037325
41.020917	1721.581880	18.042343
41.247472	1725.437272	18.047360
41.597641	1729.334295	18.052378
41.313077	1717.868433	18.057395
41.441010	1735.242159	18.062413
41.353713	1735.886791	18.067431
41.650789	1717.378654	18.072448
41.414889	1720.335697	18.077466
41.280598	1718.719563	18.082483
41.443949	1721.611352	18.087501
41.366124	1729.943279	18.092519
41.639092	1713.678940	18.097536
41.523611	1714.172340	18.102554
41.726308	1733.361959	18.107571
41.807037	1716.958395	18.112589
41.683697	1712.218120	18.117607
41.894111	1713.593898	18.122624
41.713144	1726.374976	18.127642
41.614922	1725.206112	18.132659
41.974764	1718.122078	18.137677
41.644029	1764.365859	18.142695
42.033048	1733.889808	18.147712
41.790237	1747.317833	18.152730
41.898013	1754.828953	18.157747
42.103978	1744.579407	18.162765
42.004243	1760.396030	18.167783
42.130726	1735.888917	18.172800
42.141283	1743.771035	18.177818
41.816285	1743.365066	18.182835
42.341611	1746.350131	18.187853
42.535700	1776.136903	18.192871
42.525822	1781.920771	18.197888
42.632879	1768.481206	18.202906
42.575605	1764.041830	18.207923
43.105261	1783.736208	18.212941
42.687553	1756.050308	18.217959
42.685282	1736.839571	18.222976
42.769127	1748.774629	18.227994
42.373826	1731.220038	18.233011
42.736381	1754.311962	18.238029
42.601195	1777.313430	18.243047
42.899893	1763.698586	18.248064
42.612832	1784.172882	18.253082
42.967280	1780.367817	18.258099
42.957404	1766.558373	18.263117
42.861546	1763.031200	18.268135
42.702113	1778.690627	18.273152
43.006257	1769.068762	18.278170
43.010103	1767.528117	18.283187
43.044428	1771.231714	18.288205
43.051448	1777.126141	18.293223
43.071681	1771.571726	18.298240
43.197773	1797.860023	18.303258
43.220698	1798.023041	18.308275
43.347805	1788.489175	18.313293
43.079275	1787.007702	18.318311
43.496522	1783.560702	18.323328
43.640314	1792.826287	18.328346
43.560148	1797.358250	18.333363
43.978198	1779.228709	18.338381
43.850297	1794.862674	18.343399
43.996471	1780.930800	18.348416
43.862336	1799.887947	18.353434
43.929127	1785.013917	18.358451
43.973854	1765.611605	18.363469
43.907000	1798.950985	18.368487
43.958066	1789.534638	18.373504
43.893420	1795.039387	18.378522
43.816838	1789.242435	18.383539
43.871171	1777.326074	18.388557
43.654699	1785.124878	18.393575
43.845939	1789.844780	18.398592
44.003732	1790.142013	18.403610
43.695181	1786.850104	18.408627
43.879881	1799.030235	18.413645
44.043893	1816.841892	18.418663
44.767762	1810.435918	18.423680
44.366017	1811.206212	18.428698
44.615628	1811.973286	18.433715
44.766417	1808.191260	18.438733
44.462319	1815.291486	18.443751
44.730982	1816.577759	18.448768
45.165272	1817.927277	18.453786
44.820729	1792.024437	18.458803
44.562132	1776.711538	18.463821
44.211701	1791.567752	18.468839
44.650415	1798.455109	18.473856
44.915514	1801.470682	18.478874
44.427493	1803.170226	18.483891
44.874882	1823.853043	18.488909
44.736308	1829.945318	18.493927
44.892651	1810.400876	18.498944
45.020532	1800.921934	18.503962
44.921986	1801.464544	18.508979
45.330756	1808.422748	18.513997
45.134901	1818.039822	18.519015
44.916885	1802.462450	18.524032
45.234481	1805.526278	18.529050
44.974451	1807.076201	18.534067
45.182513	1809.575490	18.539085
45.194831	1811.116579	18.544103
44.996965	1829.904608	18.549120
45.518435	1830.180014	18.554138
45.598176	1839.765728	18.559155
45.586720	1824.676051	18.564173
45.203549	1836.482753	18.569191
45.222115	1851.821288	18.574208
45.739075	1829.545184	18.579226
45.583825	1842.536191	18.584243
45.616883	1834.692551	18.589261
45.857430	1839.399886	18.594279
45.850993	1835.073502	18.599296
45.782631	1835.186587	18.604314
45.511979	1830.789090	18.609331
45.978299	1830.142072	18.614349
46.121504	1842.751998	18.619367
45.821968	1842.933415	18.624384
46.174051	1852.521316	18.629402
45.894959	1860.910589	18.634419
45.890125	1860.277372	18.639437
46.182599	1883.040910	18.644455
46.134242	1868.762457	18.649472
46.345999	1870.564322	18.654490
46.217456	1863.902606	18.659507
46.462134	1868.477159	18.664525
46.210984	1866.365273	18.669543
46.408042	1856.153249	18.674560
46.803675	1846.288654	18.679578
46.491645	1867.847708	18.684595
46.573048	1862.670463	18.689613
46.601458	1861.869923	18.694631
46.480749	1865.379625	18.699648
47.042080	1883.636074	18.704666
46.593971	1893.420846	18.709683
46.982967	1883.816832	18.714701
46.975083	1892.702409	18.719719
46.823069	1888.542373	18.724736
47.017878	1885.413972	18.729754
47.212325	1886.506025	18.734771
47.053937	1894.452924	18.739789
47.406291	1866.901959	18.744807
47.003286	1876.915478	18.749824
47.266648	1897.262815	18.754842
47.605082	1896.925627	18.759859
47.426649	1870.344924	18.764877
47.450389	1883.966511	18.769895
47.028363	1884.842290	18.774912
47.324164	1863.386343	18.779930
47.393186	1894.111946	18.784947
47.568850	1875.910835	18.789965
47.634695	1882.063334	18.794983
47.381473	1889.208962	18.800000
47.593978	1872.738586	18.805018
47.381329	1875.959363	18.810035
47.464912	1883.398904	18.815053
47.473598	1885.546191	18.820071
47.136648	1888.535114	18.825088
47.786314	1901.523631	18.830106
47.630404	1914.286720	18.835123
47.877666	1913.723402	18.840141
47.768833	1928.626163	18.845159
47.985862	1913.872756	18.850176
48.013138	1914.790129	18.855194
47.851111	1916.003536	18.860211
48.279630	1926.114120	18.865229
48.538156	1914.610242	18.870247
48.167597	1926.885337	18.875264
48.432914	1933.254578	18.880282
48.758958	1936.999778	18.885299
48.423438	1929.246336	18.890317
48.605449	1921.021816	18.895335
48.689735	1923.723337	18.900352
48.864396	1904.595843	18.905370
48.474926	1912.461633	18.910387
48.910145	1913.647418	18.915405
48.821043	1904.775596	18.920423
48.859453	1912.088650	18.925440
49.010525	1899.315195	18.930458
48.746661	1905.438496	18.935475
48.449772	1918.743170	18.940493
48.687607	1930.018317	18.945511
48.979586	1943.746613	18.950528
49.223223	1937.661000	18.955546
48.857390	1943.997208	18.960563
48.837742	1940.094469	18.965581
49.198348	1934.333120	18.970599
49.114503	1938.310437	18.975616
49.188559	1934.472978	18.980634
49.154930	1935.834220	18.985651
49.068987	1941.767136	18.990669
49.666467	1956.698841	18.995687
49.708839	1962.907028	19.000704
49.424440	1947.489525	19.005722
49.470580	1949.213997	19.010739
49.474952	1967.693095	19.015757
49.701087	1958.737926	19.020775
49.398213	1968.864524	19.025792
49.851864	1954.372209	19.030810
49.897453	1961.830434	19.035827
49.648127	1961.841823	19.040845
49.930299	1963.494043	19.045863
49.525762	1962.347275	19.050880
49.971414	1958.750987	19.055898
49.445231	1963.141783	19.060915
49.583771	1970.580468	19.065933
49.892290	1972.720843	19.070951
49.835507	1994.470607	19.075968
50.212468	1983.525084	19.080986
50.229460	1981.658276	19.086003
50.198013	1988.285661	19.091021
50.155667	1997.957019	19.096039
50.160196	1989.258974	19.101056
50.702123	1990.408871	19.106074
50.526176	2002.912538	19.111091
50.609619	2016.689895	19.116109
50.866490	2015.047517	19.121127
50.918646	2016.228343	19.126144
50.527023	2010.204698	19.131162
50.648189	2014.581920	19.136179
50.930336	2012.602030	19.141197
51.254690	2001.774996	19.146215
51.023381	2014.893119	19.151232
51.498932	2002.739502	19.156250
50.918967	1993.096483	19.161267
50.923036	1997.339793	19.166285
51.326133	1992.106473	19.171303
51.104190	2021.645503	19.176320
51.191481	2001.429123	19.181338
51.293195	1998.545209	19.186355
51.354212	2000.995625	19.191373
51.560665	2012.071348	19.196391
51.559310	2012.288578	19.201408
51.585354	2007.727299	19.206426
51.741443	1997.152050	19.211443
51.545736	2002.857106	19.216461
51.692404	2004.107800	19.221479
51.604137	2016.007609	19.226496
51.647160	2010.210368	19.231514
51.890726	2003.015755	19.236531
51.808178	2009.923434	19.241549
51.792483	2003.704552	19.246567
51.833467	2000.997064	19.251584
51.935564	1988.961226	19.256602
51.764340	1995.530684	19.261619
51.841158	1998.530712	19.266637
51.971312	1992.964972	19.271655
51.760251	1997.443943	19.276672
51.992870	2019.079944	19.281690
52.177893	2019.769243	19.286707
52.289423	2032.626633	19.291725
52.374103	2022.489046	19.296743
52.032084	2035.588666	19.301760
52.264970	2040.902906	19.306778
52.219255	2031.187233	19.311795
51.907582	2035.043613	19.316813
52.696673	2040.091386	19.321831
52.678119	2054.122575	19.326848
52.802440	2059.844250	19.331866
52.669311	2053.999581	19.336883
52.603593	2057.448648	19.341901
52.951394	2058.859176	19.346919
52.766237	2057.148870	19.351936
52.644878	2055.511759	19.356954
53.042679	2053.412742	19.361971
52.414427	2059.367710	19.366989
53.267372	2054.613179	19.372007
53.157887	2055.800913	19.377024
52.886300	2068.714722	19.382042
53.705202	2066.564269	19.387059
53.605425	2078.758549	19.392077
53.305328	2060.172192	19.397095
53.183462	2070.323473	19.402112
53.474241	2076.089391	19.407130
53.399988	2080.224094	19.412147
53.163472	2084.082655	19.417165
53.606771	2076.724015	19.422183
53.768612	2074.580833	19.427200
53.793873	2082.227980	19.432218
53.632037	2083.140920	19.437235
53.720666	2085.390318	19.442253
53.609955	2072.516891	19.447271
53.504099	2085.350798	19.452288
53.932899	2109.758794	19.457306
54.287741	2107.853813	19.462323
54.204429	2093.876445	19.467341
54.338022	2112.492420	19.472359
54.505454	2087.183799	19.477376
54.358265	2111.211755	19.482394
54.594920	2105.923144	19.487411
54.304872	2095.373364	19.492429
54.615070	2109.682508	19.497447
54.589560	2091.393664	19.502464
54.381774	2106.822054	19.507482
55.018011	2086.335528	19.512499
54.564901	2101.206861	19.517517
54.592144	2113.196865	19.522535
54.929722	2101.941355	19.527552
54.753378	2096.669855	19.532570
54.987052	2104.470964	19.537587
54.581605	2112.026375	19.542605
54.699277	2091.089292	19.547623
54.905143	2095.715727	19.552640
55.174531	2100.836976	19.557658
55.355332	2105.479995	19.562675
54.993328	2105.989132	19.567693
55.074420	2093.943973	19.572711
55.094439	2087.492840	19.577728
54.877624	2099.457265	19.582746
55.429347	2116.408350	19.587763
55.392238	2129.163690	19.592781
55.875104	2131.666396	19.597799
55.463153	2122.131773	19.602816
55.446055	2126.609734	19.607834
55.587579	2124.638101	19.612851
55.472141	2143.416533	19.617869
55.586824	2134.356335	19.622887
55.508570	2112.714289	19.627904
55.545762	2120.652139	19.632922
55.734528	2130.371668	19.637939
55.858348	2139.307176	19.642957
55.783952	2141.208200	19.647975
56.241721	2160.920853	19.652992
56.104127	2169.183913	19.658010
56.328355	2160.686680	19.663027
55.981030	2167.114414	19.668045
56.071774	2164.938514	19.673063
56.158883	2165.819618	19.678080
56.014209	2170.115018	19.683098
56.097464	2170.713589	19.688115
55.793686	2173.613906	19.693133
56.396208	2179.729698	19.698151
56.400012	2185.599634	19.703168
56.467864	2191.168344	19.708186
56.771164	2179.199360	19.713203
56.768705	2181.090489	19.718221
57.089857	2183.708661	19.723239
57.292852	2166.975198	19.728256
56.745703	2181.043627	19.733274
56.898217	2174.670425	19.738291
57.052525	2176.599472	19.743309
57.158655	2170.704010	19.748327
57.278363	2178.524910	19.753344
57.080122	2178.260732	19.758362
57.484893	2186.438869	19.763379
57.489475	2196.028941	19.768397
57.391024	2206.209616	19.773415
57.591358	2205.754449	19.778432
57.370656	2201.559659	19.783450
57.673113	2200.668200	19.788467
57.831228	2198.055253	19.793485
57.807866	2202.227492	19.798503
57.730537	2195.099698	19.803520
57.629759	2199.009000	19.808538
58.126985	2192.012940	19.813555
57.685353	2198.048310	19.818573
57.849640	2198.330360	19.823591
58.048521	2185.382286	19.828608
58.223680	2196.131228	19.833626
58.125650	2190.979339	19.838643
58.142492	2202.812199	19.843661
58.278023	2201.354325	19.848679
58.147630	2192.580149	19.853696
57.720338	2202.604054	19.858714
58.162944	2192.645218	19.863731
58.200827	2205.660802	19.868749
58.287632	2209.455243	19.873767
58.729725	2210.073662	19.878784
58.498486	2208.370688	19.883802
58.600139	2212.935129	19.888819
58.650836	2212.657987	19.893837
58.871650	2215.463631	19.898855
58.884225	2209.270039	19.903872
59.069490	2210.832352	19.908890
59.088203	2213.706410	19.913907
58.885867	2217.193034	19.918925
58.929418	2219.172785	19.923943
59.052872	2222.544527	19.928960
59.121683	2214.416550	19.933978
59.169414	2208.837132	19.938995
59.066239	2220.050490	19.944013
59.314606	2233.767142	19.949031
59.752870	2237.744639	19.954048
59.667581	2240.226296	19.959066
59.777791	2241.622828	19.964083
59.591687	2240.107709	19.969101
59.503303	2242.380645	19.974119
59.853172	2237.012581	19.979136
59.861763	2244.203141	19.984154
59.841916	2235.700749	19.989171
60.096928	2227.105758	19.994189
60.459747	2230.285165	19.999207
60.453418	2236.814274	20.004224
59.902055	2237.654068	20.009242
60.366495	2224.015507	20.014259
60.412302	2231.148215	20.019277
60.108334	2234.322285	20.024295
60.437674	2231.895958	20.029312
60.135987	2224.264376	20.034330
60.327709	2224.619131	20.039347
60.320744	2241.908013	20.044365
60.353652	2233.073160	20.049383
60.459989	2230.542399	20.054400
60.469411	2236.472809	20.059418
60.230230	2225.980888	20.064435
60.383948	2239.830620	20.069453
60.687136	2251.312676	20.074471
60.415456	2255.773078	20.079488
60.742433	2260.602050	20.084506
60.985802	2258.628313	20.089523
61.165073	2258.256730	20.094541
60.909727	2267.356614	20.099559
60.737080	2257.694069	20.104576
60.809442	2271.128937	20.109594
61.221065	2293.435235	20.114611
61.305559	2297.060178	20.119629
61.203381	2293.290059	20.124647
61.414046	2291.886261	20.129664
61.239912	2286.925805	20.134682
61.372401	2298.653779	20.139699
61.687456	2287.261717	20.144717
61.535575	2291.445041	20.149735
61.730090	2301.041069	20.154752
61.674062	2305.721927	20.159770
62.033138	2312.129867	20.164787
62.187425	2300.629726	20.169805
61.997860	2315.374296	20.174823
62.034365	2307.212094	20.179840
62.085286	2310.271374	20.184858
62.369497	2312.550962	20.189875
62.276888	2315.099869	20.194893
62.478891	2307.229028	20.199911
62.800047	2317.210718	20.204928
62.333085	2308.943194	20.209946
62.508377	2307.254020	20.214963
62.807397	2300.567954	20.219981
62.646509	2302.476502	20.224999
62.824703	2306.188752	20.230016
62.451748	2309.785983	20.235034
62.959090	2300.961936	20.240051
62.720904	2303.650466	20.245069
62.735525	2310.276942	20.250087
62.911026	2299.699951	20.255104
62.745682	2304.686113	20.260122
62.852517	2329.570558	20.265139
63.232206	2337.815705	20.270157
62.885244	2333.869108	20.275175
63.368396	2338.430946	20.280192
63.494474	2335.384200	20.285210
63.459339	2337.798098	20.290227
63.575168	2336.808980	20.295245
63.115177	2335.118878	20.300263
63.326328	2336.658199	20.305280
63.257557	2328.803792	20.310298
63.555807	2350.228469	20.315315
63.751907	2354.977671	20.320333
63.449188	2366.043637	20.325351
63.799651	2352.445159	20.330368
63.863916	2363.454165	20.335386
63.947756	2366.847989	20.340403
63.913903	2368.544370	20.345421
63.962563	2368.907788	20.350439
64.170725	2379.874979	20.355456
64.203391	2382.429086	20.360474
64.041247	2392.362066	20.365491
64.588623	2387.794600	20.370509
64.544645	2385.237449	20.375527
64.939714	2388.558043	20.380544
64.665927	2380.275397	20.385562
64.961925	2381.848383	20.390579
65.144309	2384.115908	20.395597
64.850636	2387.593544	20.400615
64.741919	2387.604527	20.405632
64.761653	2387.708284	20.410650
64.761171	2386.602430	20.415667
65.044146	2378.517284	20.420685
64.721535	2391.551204	20.425703
65.093126	2380.234998	20.430720
65.116438	2384.714458	20.435738
64.964064	2379.843310	20.440755
65.194882	2387.102320	20.445773
65.126808	2400.234081	20.450791
65.326218	2408.545776	20.455808
65.668460	2409.859697	20.460826
65.681532	2407.810983	20.465843
65.807850	2405.629374	20.470861
65.587253	2415.949229	20.475879
65.657191	2420.814532	20.480896
65.802632	2398.230293	20.485914
65.497383	2400.876051	20.490931
65.933993	2400.043412	20.495949
65.767615	2407.814107	20.500967
66.124812	2415.863106	20.505984
65.999807	2435.650993	20.511002
65.754444	2433.284833	20.516019
66.253920	2441.296210	20.521037
66.096690	2433.982834	20.526055
66.321179	2433.688982	20.531072
66.381808	2428.165627	20.536090
66.606689	2448.099080	20.541107
66.736725	2453.756290	20.546125
66.665731	2467.638147	20.551143
66.931659	2459.668151	20.556160
67.141525	2458.264465	20.561178
66.966825	2470.071461	20.566195
67.019343	2454.793955	20.571213
67.627011	2448.295343	20.576231
67.252660	2450.313463	20.581248
67.324010	2450.591465	20.586266
67.123303	2450.365427	20.591283
67.586450	2447.297933	20.596301
67.288325	2450.164368	20.601319
67.546076	2442.341194	20.606336
67.455872	2451.037315	20.611354
67.578157	2458.642445	20.616371
67.797610	2447.613942	20.621389
67.433454	2450.104718	20.626407
67.810234	2450.532214	20.631424
67.790179	2455.814589	20.636442
67.664674	2457.988082	20.641459
67.956078	2449.386371	20.646477
67.775118	2463.328236	20.651495
67.834052	2454.251562	20.656512
67.687760	2453.629869	20.661530
67.683536	2480.238286	20.666547
68.118168	2470.166487	20.671565
68.068005	2486.775116	20.676583
68.140627	2486.351323	20.681600
68.157406	2488.484037	20.686618
67.756460	2489.157488	20.691635
68.520693	2496.502157	20.696653
68.499995	2513.779396	20.701671
68.543635	2513.179319	20.706688
68.917755	2507.845830	20.711706
68.543135	2517.613002	20.716723
69.008495	2503.852121	20.721741
69.091369	2513.613180	20.726759
68.779660	2503.990740	20.731776
69.157683	2513.563147	20.736794
69.334774	2529.982992	20.741811
69.696995	2540.231217	20.746829
69.694893	2535.457177	20.751847
69.215708	2516.277427	20.756864
69.519682	2514.354554	20.761882
69.603276	2524.249217	20.766899
69.726669	2525.281079	20.771917
69.784318	2537.747161	20.776935
69.903238	2536.982488	20.781952
70.208623	2532.923139	20.786970
70.076647	2537.550901	20.791987
70.312731	2539.295488	20.797005
70.062214	2532.477518	20.802023
70.309572	2528.163148	20.807040
70.389229	2523.203818	20.812058
69.922223	2534.555673	20.817075
69.772817	2527.627194	20.822093
70.330045	2524.090059	20.827111
70.319453	2528.504969	20.832128
70.311758	2534.653743	20.837146
70.315924	2539.977118	20.842163
70.584612	2521.714745	20.847181
70.286843	2538.728666	20.852199
70.128293	2548.103520	20.857216
70.794370	2543.756184	20.862234
70.418773	2552.545863	20.867251
70.691663	2548.736307	20.872269
70.915779	2558.818589	20.877287
70.976329	2569.339901	20.882304
71.153041	2581.438592	20.887322
71.039009	2594.391446	20.892339
71.345898	2572.138279	20.897357
71.348900	2576.775201	20.902375
70.995604	2576.269105	20.907392
71.238120	2579.292379	20.912410
71.427681	2595.192761	20.917427
71.627694	2606.280193	20.922445
71.366873	2615.071266	20.927463
71.725093	2601.997519	20.932480
71.642756	2604.894063	20.937498
71.696848	2604.380409	20.942515
71.659218	2603.222258	20.947533
72.180831	2599.774160	20.952551
71.938982	2634.930397	20.957568
72.255727	2625.914750	20.962586
72.240378	2627.738776	20.967603
72.793428	2626.874971	20.972621
72.795804	2626.338102	20.977639
72.875228	2619.285776	20.982656
72.528952	2619.157674	20.987674
72.517521	2634.642612	20.992691
72.860611	2627.352380	20.997709
72.868422	2606.332187	21.002727
72.510880	2618.375326	21.007744
72.819229	2628.207471	21.012762
72.935007	2627.308795	21.017779
72.931113	2622.800078	21.022797
72.877631	2632.188904	21.027815
73.060441	2624.029146	21.032832
73.326644	2638.933383	21.037850
73.313661	2655.543353	21.042867
73.527301	2649.662801	21.047885
73.910616	2657.361689	21.052903
73.703041	2660.179114	21.057920
73.889520	2653.810512	21.062938
73.830321	2655.940424	21.067955
73.775715	2648.660125	21.072973
73.797836	2650.049509	21.077991
73.970675	2652.101513	21.083008
73.855166	2645.243866	21.088026
73.774964	2660.824747	21.093043
73.660842	2645.743513	21.098061
74.137874	2659.639614	21.103079
74.131232	2676.441301	21.108096
74.735158	2674.437534	21.113114
74.737456	2671.569344	21.118131
74.809115	2673.834125	21.123149
74.733154	2678.090398	21.128167
74.834265	2662.674356	21.133184
75.064380	2666.127509	21.138202
74.616857	2667.529661	21.143219
74.814971	2670.479022	21.148237
75.088270	2663.614414	21.153255
74.837109	2666.331821	21.158272
74.924527	2658.192763	21.163290
75.043205	2661.475703	21.168307
75.315828	2655.636081	21.173325
75.304622	2657.307646	21.178343
75.307881	2664.005312	21.183360
75.218773	2677.157981	21.188378
75.555350	2696.892269	21.193395
75.336329	2701.125745	21.198413
75.716956	2688.412520	21.203431
75.293658	2695.971075	21.208448
75.602818	2692.335818	21.213466
75.671399	2687.017960	21.218483
75.702191	2700.989204	21.223501
75.731418	2713.658181	21.228519
75.779267	2727.504814	21.233536
76.060199	2720.101748	21.238554
75.788592	2731.749796	21.243571
75.973797	2723.642299	21.248589
76.092380	2736.868868	21.253607
76.368482	2744.133421	21.258624
76.453980	2752.375387	21.263642
76.956858	2757.746725	21.268659
76.957949	2745.684685	21.273677
76.996607	2735.491018	21.278695
77.000238	2744.074815	21.283712
77.208895	2746.977677	21.288730
77.212044	2740.370062	21.293747
77.134362	2738.657476	21.298765
77.126573	2740.050853	21.303783
77.077721	2736.297283	21.308800
77.139374	2732.904422	21.313818
77.578987	2733.705745	21.318835
77.448077	2740.380798	21.323853
77.617061	2743.382013	21.328871
77.591836	2758.944792	21.333888
78.001130	2765.268631	21.338906
77.954634	2773.866733	21.343923
77.940320	2769.224345	21.348941
78.150343	2763.935027	21.353959
77.732030	2770.053430	21.358976
78.010741	2759.897756	21.363994
78.563959	2763.715489	21.369011
77.943664	2763.550858	21.374029
77.998718	2762.807372	21.379047
78.039918	2764.685321	21.384064
78.384034	2755.861867	21.389082
78.674149	2773.745830	21.394099
78.664204	2786.978786	21.399117
79.084116	2773.545029	21.404135
78.799137	2771.150522	21.409152
79.193610	2782.790699	21.414170
79.369099	2790.636068	21.419187
79.192712	2787.827029	21.424205
79.181960	2782.685392	21.429223
79.108386	2785.770921	21.434240
79.423662	2775.332537	21.439258
79.125985	2779.928597	21.444275
78.802272	2776.207842	21.449293
79.264665	2775.571645	21.454311
79.352109	2778.419909	21.459328
79.443681	2786.036401	21.464346
79.660494	2796.182938	21.469363
79.838587	2814.781706	21.474381
79.851319	2809.577322	21.479399
79.733228	2822.546758	21.484416
79.576452	2819.417601	21.489434
79.824957	2818.291668	21.494451
79.832593	2822.032826	21.499469
80.055638	2816.614776	21.504487
80.181290	2838.733917	21.509504
79.839632	2841.377694	21.514522
80.146553	2847.276637	21.519539
80.245570	2860.760498	21.524557
80.413326	2841.131839	21.529575
80.277351	2855.476700	21.534592
80.469460	2871.212588	21.539610
80.326340	2873.112083	21.544627
80.585919	2871.131748	21.549645
80.945385	2874.580053	21.554663
81.018531	2896.644731	21.559680
80.978052	2898.575052	21.564698
81.199292	2897.119172	21.569715
81.464167	2900.589649	21.574733
81.703470	2895.039981	21.579751
81.349345	2895.744522	21.584768
82.004205	2899.907113	21.589786
81.912880	2895.590806	21.594803
81.595511	2901.844183	21.599821
81.855707	2885.459447	21.604839
81.827510	2888.376515	21.609856
82.043886	2897.967881	21.614874
82.211637	2897.948142	21.619891
82.360819	2917.489233	21.624909
82.373775	2919.293051	21.629927
82.593358	2922.802219	21.634944
82.390015	2919.186506	21.639962
82.702055	2919.787163	21.644979
82.402166	2928.948834	21.649997
82.746468	2923.535789	21.655015
82.891630	2923.448076	21.660032
82.846851	2918.419577	21.665050
82.997306	2921.335689	21.670067
82.864025	2919.346426	21.675085
82.867120	2920.170186	21.680103
82.914492	2923.720978	21.685120
83.017032	2912.273443	21.690138
83.196549	2918.925025	21.695155
83.182594	2935.782451	21.700173
83.480574	2939.316874	21.705191
83.389484	2935.867310	21.710208
83.669243	2936.389741	21.715226
83.551884	2935.997021	21.720243
83.654478	2941.616325	21.725261
83.736816	2935.058131	21.730279
83.620381	2955.311001	21.735296
83.412051	2959.247884	21.740314
84.242651	2961.715735	21.745331
83.800690	2982.811845	21.750349
83.918380	2959.435157	21.755367
83.838765	2967.993822	21.760384
83.959321	2986.816718	21.765402
84.512701	2983.080303	21.770419
84.379499	2994.442986	21.775437
84.777120	2992.765472	21.780455
84.686037	3001.550943	21.785472
84.931831	2991.074721	21.790490
85.022432	2981.795241	21.795507
84.940333	2986.769144	21.800525
85.127779	2992.433141	21.805543
85.233501	3010.461642	21.810560
85.406299	3019.949132	21.815578
85.555444	3015.055638	21.820595
85.573066	3015.914842	21.825613
85.896999	3009.532030	21.830631
85.692003	3016.986714	21.835648
85.803553	3012.712740	21.840666
86.049970	3011.093948	21.845683
85.696822	3009.076026	21.850701
85.555113	3011.278141	21.855719
85.840759	3007.788141	21.860736
85.904620	3014.529003	21.865754
86.370305	3012.617246	21.870771
86.437747	3010.258521	21.875789
86.403228	3000.706380	21.880807
86.290386	3006.939768	21.885824
86.227642	3025.454511	21.890842
86.719190	3026.003734	21.895859
86.391479	3043.010431	21.900877
86.240494	3039.668716	21.905895
86.536256	3029.426760	21.910912
86.510750	3068.686105	21.915930
86.980862	3055.171721	21.920947
87.331330	3067.381543	21.925965
87.295106	3071.436523	21.930983
87.347338	3061.502392	21.936000
87.285034	3070.775708	21.941018
87.490724	3043.904274	21.946035
87.312648	3064.459730	21.951053
87.577201	3075.785785	21.956071
87.801754	3084.027000	21.961088
87.654997	3092.650718	21.966106
87.975313	3088.079926	21.971123
87.981585	3092.664576	21.976141
88.321203	3095.596177	21.981159
88.113877	3089.427056	21.986176
87.950296	3084.344296	21.991194
88.088232	3084.190875	21.996211
88.186895	3096.996201	22.001229
88.474204	3106.918551	22.006247
88.770030	3117.409816	22.011264
88.619321	3092.822709	22.016282
88.730148	3112.922354	22.021299
88.784715	3120.273555	22.026317
88.999497	3109.025060	22.031335
89.032100	3109.235317	22.036352
88.903486	3098.940648	22.041370
89.241195	3117.018020	22.046387
89.225705	3114.154152	22.051405
89.343333	3098.226104	22.056423
89.197908	3107.277515	22.061440
89.336583	3131.728786	22.066458
89.515480	3128.307696	22.071475
89.457273	3139.947991	22.076493
89.718698	3133.973102	22.081511
89.740610	3135.681916	22.086528
89.798995	3140.924499	22.091546
90.273195	3145.731865	22.096563
90.178953	3155.623857	22.101581
90.564237	3165.317460	22.106599
90.842788	3154.220795	22.111616
90.764856	3151.649259	22.116634
90.723821	3136.044586	22.121651
90.756153	3134.215299	22.126669
90.715306	3117.100393	22.131687
91.196587	3141.806166	22.136704
91.071182	3151.143870	22.141722
91.314165	3132.695270	22.146739
91.147059	3130.497424	22.151757
91.031273	3131.384990	22.156775
91.366475	3145.920854	22.161792
91.391703	3141.382161	22.166810
91.519553	3145.490439	22.171827
91.503809	3156.484490	22.176845
91.882790	3152.461217	22.181863
92.083011	3151.033836	22.186880
91.837679	3153.444423	22.191898
91.982279	3151.773422	22.196915
91.892481	3146.356377	22.201933
91.670341	3149.150259	22.206951
91.746694	3144.317099	22.211968
91.883205	3158.577899	22.216986
92.003802	3168.777011	22.222003
92.222034	3181.708072	22.227021
92.168721	3177.355728	22.232039
92.422441	3184.287418	22.237056
92.439371	3191.097986	22.242074
92.608344	3199.045299	22.247091
92.938591	3197.820565	22.252109
92.913136	3210.055852	22.257127
93.118270	3196.287844	22.262144
92.904276	3203.882496	22.267162
93.103091	3197.239536	22.272179
92.945158	3208.087974	22.277197
93.241786	3218.605928	22.282215
93.583270	3217.506827	22.287232
93.436468	3226.188051	22.292250
93.768133	3226.492986	22.297267
93.965721	3230.284973	22.302285
93.488127	3223.251971	22.307303
93.811967	3225.614273	22.312320
93.710275	3224.743165	22.317338
94.060374	3239.990175	22.322355
94.471541	3260.705999	22.327373
94.415596	3256.666324	22.332391
94.479331	3247.680422	22.337408
94.462735	3259.966251	22.342426
94.525823	3249.511117	22.347443
94.897532	3254.069002	22.352461
94.466317	3258.829664	22.357479
94.945157	3256.632611	22.362496
94.631377	3253.725044	22.367514
94.755928	3253.038882	22.372531
94.817568	3281.525266	22.377549
94.732287	3280.286564	22.382567
95.319863	3278.705365	22.387584
95.093862	3284.889272	22.392602
95.003239	3288.068869	22.397619
95.294179	3298.636556	22.402637
95.443344	3305.979844	22.407655
95.807803	3315.401565	22.412672
95.742115	3317.548340	22.417690
96.200109	3312.645607	22.422707
96.318118	3329.222083	22.427725
96.259750	3331.301619	22.432743
96.723114	3329.290298	22.437760
96.677778	3326.323387	22.442778
96.484642	3329.255835	22.447795
96.714094	3314.173389	22.452813
96.724249	3318.999759	22.457831
96.724278	3330.593949	22.462848
96.760076	3328.416414	22.467866
97.028737	3323.749172	22.472883
97.216552	3321.532450	22.477901
97.005645	3315.867217	22.482919
97.467022	3319.319043	22.487936
97.209850	3322.503184	22.492954
97.123517	3325.306118	22.497971
97.426070	3340.335853	22.502989
97.440127	3344.150060	22.508007
97.659309	3347.081256	22.513024
97.727986	3342.860432	22.518042
97.718588	3349.138822	22.523059
97.871868	3351.474857	22.528077
97.945978	3368.420995	22.533095
98.553410	3358.826022	22.538112
98.500559	3359.894705	22.543130
98.368477	3373.213744	22.548147
98.688385	3372.978600	22.553165
98.262099	3365.351337	22.558183
98.520790	3368.445353	22.563200
98.557664	3378.112072	22.568218
98.529934	3365.618345	22.573235
98.787409	3382.805056	22.578253
98.757247	3399.719877	22.583271
99.183028	3387.293032	22.588288
98.928889	3399.350209	22.593306
98.997714	3397.356965	22.598323
99.533917	3392.794912	22.603341
99.594189	3408.658598	22.608359
99.698225	3410.889228	22.613376
99.829322	3414.990772	22.618394
100.203500	3406.030776	22.623411
100.055679	3400.320839	22.628429
99.937433	3419.623656	22.633447
100.232330	3402.164619	22.638464
100.176643	3407.530107	22.643482
100.310174	3403.044855	22.648499
100.491176	3402.582514	22.653517
100.149939	3408.181536	22.658535
100.118709	3415.689729	22.663552
100.655800	3429.389786	22.668570
100.675952	3428.868931	22.673587
100.886541	3437.479126	22.678605
100.779106	3440.399502	22.683623
101.113012	3436.113542	22.688640
101.360280	3439.374579	22.693658
101.445141	3465.758995	22.698675
101.737862	3460.176999	22.703693
101.540983	3463.870706	22.708711
101.335899	3457.944913	22.713728
101.452566	3467.988330	22.718746
101.530927	3460.122432	22.723763
102.033785	3455.874022	22.728781
101.899894	3468.254246	22.733799
102.200877	3478.330417	22.738816
102.686079	3477.563131	22.743834
102.292852	3492.102242	22.748851
102.562259	3486.322586	22.753869
102.806058	3480.142708	22.758887
102.692478	3481.347726	22.763904
102.579217	3488.194928	22.768922
102.542178	3483.678645	22.773939
102.821224	3482.894681	22.778957
102.673793	3493.739296	22.783975
102.989335	3511.159169	22.788992
103.267684	3505.308073	22.794010
103.441255	3501.411070	22.799027
103.501359	3496.708600	22.804045
103.550145	3506.705448	22.809063
103.677345	3506.917930	22.814080
103.869072	3495.112761	22.819098
103.753177	3498.599272	22.824115
104.238487	3512.377673	22.829133
104.154790	3532.003139	22.834151
104.430245	3542.790575	22.839168
104.557399	3538.174937	22.844186
104.494930	3532.987008	22.849203
104.570593	3527.987073	22.854221
104.567522	3532.029028	22.859239
104.841693	3527.612554	22.864256
104.709656	3528.604205	22.869274
104.801549	3535.763241	22.874291
105.147931	3528.514517	22.879309
104.741289	3540.093495	22.884327
104.725775	3532.362092	22.889344
104.935926	3540.420228	22.894362
105.001240	3549.875651	22.899379
105.262639	3566.038590	22.904397
105.349716	3560.893663	22.909415
105.321147	3552.118943	22.914432
105.518290	3573.762921	22.919450
105.633716	3591.817339	22.924467
106.073672	3588.572399	22.929485
105.768347	3597.313734	22.934503
105.729969	3587.474715	22.939520
106.293522	3590.517015	22.944538
106.177777	3615.823016	22.949555
106.542403	3615.237781	22.954573
106.706724	3615.563908	22.959591
106.986637	3612.254813	22.964608
106.814583	3605.273581	22.969626
106.716028	3615.557512	22.974643
107.237363	3617.646111	22.979661
107.415245	3636.628252	22.984679
107.275926	3622.921856	22.989696
107.787466	3626.379131	22.994714
107.417203	3640.401861	22.999731
107.630015	3632.185630	23.004749
107.637199	3632.940344	23.009767
107.903200	3636.012800	23.014784
107.977606	3630.469489	23.019802
107.977278	3623.004634	23.024819
108.028516	3625.613419	23.029837
108.267156	3648.093340	23.034855
108.268198	3648.352688	23.039872
108.579635	3660.988496	23.044890
108.519406	3663.430213	23.049907
108.610538	3653.370699	23.054925
108.790364	3652.258018	23.059943
108.930586	3646.224378	23.064960
108.705507	3657.101162	23.069978
108.775197	3662.379887	23.074995
109.193645	3678.263047	23.080013
109.390224	3682.394341	23.085031
109.356642	3683.662918	23.090048
109.612976	3681.787614	23.095066
109.297999	3690.439297	23.100083
109.461276	3689.901902	23.105101
109.660387	3691.423628	23.110119
109.958530	3699.705375	23.115136
109.881469	3705.597472	23.120154
109.921472	3698.277962	23.125171
110.320943	3704.942811	23.130189
110.364882	3696.561543	23.135207
109.875087	3703.021314	23.140224
110.508300	3714.477862	23.145242
110.758032	3731.184030	23.150259
110.620679	3725.520279	23.155277
110.878481	3731.225262	23.160295
110.920706	3725.439266	23.165312
111.279443	3727.673377	23.170330
110.856249	3734.898921	23.175347
111.558554	3745.810369	23.180365
111.452060	3755.867548	23.185383
111.489685	3760.729014	23.190400
111.614658	3744.726724	23.195418
111.540384	3750.069343	23.200435
111.829302	3751.508319	23.205453
112.031537	3753.203394	23.210471
111.741071	3772.486158	23.215488
112.115867	3778.569740	23.220506
112.177267	3776.809678	23.225523
112.664862	3768.798119	23.230541
112.741992	3770.157600	23.235559
112.561458	3779.686989	23.240576
112.851665	3763.250863	23.245594
113.044837	3786.030080	23.250611
113.089201	3796.607563	23.255629
113.210418	3800.999478	23.260647
113.077221	3796.385161	23.265664
113.374619	3792.331464	23.270682
113.272856	3797.669832	23.275699
113.387286	3800.093944	23.280717
113.396609	3811.085276	23.285735
113.368401	3820.135739	23.290752
113.746503	3823.665472	23.295770
114.026411	3844.890763	23.300787
113.850518	3832.684566	23.305805
114.179173	3838.854979	23.310823
114.297629	3852.331940	23.315840
114.781572	3847.416243	23.320858
114.592181	3851.985138	23.325875
115.049235	3846.157326	23.330893
115.044110	3843.510341	23.335911
114.861080	3859.267793	23.340928
114.898313	3852.471745	23.345946
115.249137	3847.110029	23.350963
115.155309	3837.973477	23.355981
115.411975	3858.888636	23.360999
115.393066	3869.775962	23.366016
115.192698	3875.048275	23.371034
115.027555	3885.755986	23.376051
115.481421	3894.562855	23.381069
115.948326	3898.316003	23.386087
115.791294	3906.534371	23.391104
116.239674	3915.080971	23.396122
116.068970	3909.709581	23.401139
116.361443	3904.552231	23.406157
116.339175	3916.854463	23.411175
116.721102	3920.728935	23.416192
117.057847	3926.904389	23.421210
116.729113	3933.096297	23.426227
116.871512	3927.451570	23.431245
117.631714	3908.272127	23.436263
117.447346	3911.349602	23.441280
117.560132	3916.270716	23.446298
117.700716	3921.953563	23.451315
117.670091	3919.964309	23.456333
117.612369	3919.824779	23.461351
117.842461	3923.430845	23.466368
117.493019	3915.665176	23.471386
117.872872	3937.387537	23.476403
118.059070	3942.568336	23.481421
118.247698	3944.065803	23.486439
118.056362	3946.673999	23.491456
118.044259	3947.248523	23.496474
118.653484	3957.131921	23.501491
118.501871	3968.160835	23.506509
118.784113	3972.388678	23.511527
119.019611	3984.959003	23.516544
119.473915	3982.097135	23.521562
119.301856	3978.771935	23.526579
119.413277	3978.412709	23.531597
119.762350	3965.921309	23.536615
119.062306	3966.220096	23.541632
119.503389	3994.416095	23.546650
119.488962	3993.611259	23.551667
119.549704	4006.329823	23.556685
119.970919	4004.599670	23.561703
119.735499	4009.063467	23.566720
120.075304	4032.668450	23.571738
120.029529	4037.703779	23.576755
120.116038	4035.885406	23.581773
120.727471	4032.638985	23.586791
120.760628	4043.047736	23.591808
120.999509	4049.272674	23.596826
120.960211	4050.620856	23.601843
121.205232	4057.345898	23.606861
121.618770	4059.903279	23.611879
121.396533	4055.414779	23.616896
121.674697	4046.228214	23.621914
121.902532	4049.589244	23.626931
121.545146	4057.518705	23.631949
121.840531	4040.617336	23.636967
121.968239	4047.439743	23.641984
122.242267	4062.900340	23.647002
122.213883	4075.889617	23.652019
122.129542	4081.775161	23.657037
122.407731	4076.228290	23.662055
122.345605	4083.984819	23.667072
122.722865	4071.678412	23.672090
122.588316	4070.322424	23.677107
122.681652	4094.918627	23.682125
123.231531	4090.612985	23.687143
123.052219	4090.919195	23.692160
123.375257	4104.411748	23.697178
123.248187	4102.749353	23.702195
123.098649	4095.923979	23.707213
123.267548	4094.246639	23.712231
123.488988	4113.426191	23.717248
123.627565	4119.710419	23.722266
123.799833	4119.054368	23.727283
123.533619	4133.409450	23.732301
124.100439	4130.395886	23.737319
123.968146	4156.250593	23.742336
124.087433	4147.654101	23.747354
124.415946	4151.631550	23.752371
124.024596	4158.325966	23.757389
124.197864	4178.209452	23.762407
124.675436	4181.778477	23.767424
125.076826	4172.128524	23.772442
125.346854	4182.632541	23.777459
125.301852	4198.746716	23.782477
125.565602	4193.034552	23.787495
125.778027	4205.052597	23.792512
125.715990	4197.967793	23.797530
125.929719	4200.660112	23.802547
126.039529	4192.947705	23.807565
126.523448	4191.811666	23.812583
126.452172	4191.373014	23.817600
126.469655	4183.876714	23.822618
126.714809	4186.740224	23.827635
126.559083	4200.310000	23.832653
127.126508	4200.076283	23.837671
127.251732	4205.769557	23.842688
127.096629	4212.268211	23.847706
127.088719	4208.939593	23.852723
127.399206	4210.834571	23.857741
127.551948	4215.266423	23.862759
127.270632	4219.410362	23.867776
127.433847	4209.198952	23.872794
127.812981	4200.201501	23.877811
127.388036	4224.702007	23.882829
127.956293	4235.464506	23.887847
127.843816	4236.189561	23.892864
127.564117	4240.333249	23.897882
128.398400	4263.386199	23.902899
128.512126	4260.772103	23.907917
128.700678	4256.283324	23.912935
128.609259	4270.435246	23.917952
128.777342	4263.877731	23.922970
129.069923	4253.701511	23.927987
129.009700	4269.596360	23.933005
129.281454	4276.272402	23.938023
129.407618	4294.022335	23.943040
129.470729	4295.808885	23.948058
129.531384	4287.838385	23.953075
129.469733	4298.545626	23.958093
129.933129	4288.089633	23.963111
129.634495	4297.635830	23.968128
129.702980	4305.983652	23.973146
130.343175	4307.011897	23.978163
130.225897	4324.810914	23.983181
130.387515	4326.826404	23.988199
130.607403	4312.845752	23.993216
130.689099	4330.583154	23.998234
130.416867	4341.783404	24.003251
130.587583	4345.943399	24.008269
130.887800	4340.130966	24.013287
130.854031	4350.251685	24.018304
130.591281	4367.912691	24.023322
131.366020	4372.164379	24.028339
131.381177	4384.121994	24.033357
131.881928	4402.846758	24.038375
132.266095	4410.750192	24.043392
132.055469	4400.893255	24.048410
132.218622	4396.911148	24.053427
131.915753	4401.839711	24.058445
132.648501	4402.335594	24.063463
132.587413	4413.412551	24.068480
132.820868	4415.640004	24.073498
133.027342	4417.089051	24.078515
133.254737	4435.850369	24.083533
133.468332	4424.059847	24.088551
133.585624	4419.726338	24.093568
133.666449	4425.308782	24.098586
133.997233	4419.754970	24.103603
133.498203	4421.691749	24.108621
133.678863	4419.369023	24.113639
133.554413	4423.524976	24.118656
133.651472	4438.818318	24.123674
134.098277	4442.494579	24.128691
134.215635	4451.539525	24.133709
134.004964	4452.774263	24.138727
134.404786	4452.896876	24.143744
134.549869	4479.973635	24.148762
134.562851	4474.396535	24.153779
134.913505	4492.653697	24.158797
134.945846	4481.024976	24.163815
135.243563	4487.593138	24.168832
134.928581	4494.934738	24.173850
135.848497	4490.015389	24.178867
135.615937	4501.129196	24.183885
135.656101	4496.027609	24.188903
135.540638	4503.718134	24.193920
135.838886	4522.963067	24.198938
136.112944	4523.719323	24.203955
135.942212	4525.701307	24.208973
136.219499	4520.341637	24.213991
136.970762	4534.483728	24.219008
136.340429	4562.577137	24.224026
136.683922	4532.875802	24.229043
136.745885	4549.886605	24.234061
136.878943	4559.652833	24.239079
137.161040	4558.036842	24.244096
137.159925	4565.241108	24.249114
137.644599	4570.376109	24.254131
137.486460	4576.555239	24.259149
137.630471	4579.530928	24.264167
137.827921	4575.059514	24.269184
138.085435	4594.763363	24.274202
138.157974	4598.201205	24.279219
138.132684	4605.273254	24.284237
138.450692	4600.714955	24.289255
138.548601	4591.446664	24.294272
138.357661	4613.013258	24.299290
138.595891	4623.951391	24.304307
139.004950	4630.930591	24.309325
138.802608	4633.012815	24.314343
139.426359	4622.264341	24.319360
139.159153	4633.173735	24.324378
139.505940	4647.507085	24.329395
139.503868	4646.358047	24.334413
139.829999	4651.553759	24.339431
139.960615	4656.448681	24.344448
139.845169	4662.882209	24.349466
140.201181	4674.268873	24.354483
140.024326	4684.293854	24.359501
140.286557	4688.280449	24.364519
140.596798	4699.174116	24.369536
140.672129	4709.412205	24.374554
141.288074	4715.407384	24.379571
141.157678	4721.208487	24.384589
141.153557	4712.135749	24.389607
141.367309	4700.127864	24.394624
141.153943	4717.681508	24.399642
141.815891	4722.597924	24.404659
141.664215	4755.739676	24.409677
141.928184	4732.590926	24.414695
142.019613	4715.988771	24.419712
142.058919	4731.795089	24.424730
142.300629	4759.528764	24.429747
142.430545	4758.136045	24.434765
142.591601	4759.802408	24.439783
142.874336	4748.659824	24.444800
142.874036	4785.264774	24.449818
143.250410	4760.911767	24.454835
142.942013	4807.260725	24.459853
143.039660	4794.717465	24.464871
143.660463	4786.016242	24.469888
143.324972	4788.863903	24.474906
143.613204	4798.805359	24.479923
143.914850	4825.184406	24.484941
144.022065	4806.723101	24.489959
143.898376	4818.287851	24.494976
144.109307	4830.165837	24.499994
144.556069	4838.865856	24.505011
144.724492	4842.853292	24.510029
144.974349	4853.349211	24.515047
145.330911	4852.895809	24.520064
145.071647	4846.852221	24.525082
145.200415	4844.751677	24.530099
145.216685	4842.772126	24.535117
145.284049	4840.577534	24.540135
145.642494	4850.753269	24.545152
145.678572	4867.776436	24.550170
145.972929	4854.965757	24.555187
146.181345	4871.886714	24.560205
145.672682	4873.641790	24.565223
146.171746	4865.600282	24.570240
146.213233	4887.909016	24.575258
146.586093	4892.177747	24.580275
146.565364	4896.015213	24.585293
146.491414	4899.612579	24.590311
147.174433	4906.958868	24.595328
146.979390	4916.343411	24.600346
146.878289	4924.315066	24.605363
147.052042	4916.555112	24.610381
147.274487	4946.533436	24.615399
147.544363	4936.508262	24.620416
147.715742	4945.827315	24.625434
147.584091	4952.295020	24.630451
148.305374	4969.072948	24.635469
148.243341	4981.572002	24.640487
148.646461	4969.411767	24.645504
148.482663	4979.244491	24.650522
148.914812	4992.951751	24.655539
149.210722	4990.053594	24.660557
149.028244	5004.903576	24.665575
149.273898	5011.977456	24.670592
149.106406	5000.445484	24.675610
149.487598	5020.289093	24.680627
149.613984	5027.931886	24.685645
149.536042	5009.388930	24.690663
150.035318	5034.136742	24.695680
149.812561	5029.135110	24.700698
150.472807	5062.434435	24.705715
150.619060	5046.104010	24.710733
150.814487	5066.786007	24.715751
151.135627	5052.626454	24.720768
150.801618	5051.974000	24.725786
150.967115	5040.801117	24.730803
151.214032	5071.700927	24.735821
151.499826	5062.079056	24.740839
151.613363	5056.105736	24.745856
151.389658	5083.172401	24.750874
151.859197	5072.106775	24.755891
151.828411	5093.632014	24.760909
151.984252	5111.795145	24.765927
152.245514	5100.131792	24.770944
152.403346	5114.054404	24.775962
152.174503	5103.561112	24.780979
152.462432	5116.442657	24.785997
152.171168	5131.901697	24.791015
152.977492	5127.710635	24.796032
152.772388	5158.453781	24.801050
153.347631	5156.355162	24.806067
153.537832	5154.324234	24.811085
153.225624	5161.070200	24.816103
153.829716	5161.832868	24.821120
153.907036	5154.363505	24.826138
153.920893	5173.198366	24.831155
154.204200	5194.314154	24.836173
154.242489	5195.738177	24.841191
154.289244	5189.238147	24.846208
154.279895	5199.114831	24.851226
154.800792	5210.740735	24.856243
154.787096	5214.949265	24.861261
154.727886	5219.490742	24.866279
155.212231	5241.157475	24.871296
155.496587	5232.501776	24.876314
155.306884	5248.482837	24.881331
155.674341	5248.723908	24.886349
155.625372	5243.875428	24.891367
156.099834	5274.394025	24.896384
156.169311	5286.164347	24.901402
156.475789	5263.601937	24.906419
156.133536	5277.869559	24.911437
156.838245	5265.911946	24.916455
156.770015	5282.892437	24.921472
156.957021	5307.770748	24.926490
157.339681	5298.463689	24.931507
157.240061	5294.376131	24.936525
157.271081	5299.461795	24.941543
157.590954	5319.111048	24.946560
157.488588	5333.889584	24.951578
157.904420	5335.601138	24.956595
158.249395	5324.572495	24.961613
158.015903	5335.813734	24.966631
158.463763	5336.796425	24.971648
158.607766	5341.046714	24.976666
158.486971	5351.883730	24.981683
158.911795	5341.201860	24.986701
159.275428	5360.732480	24.991719
159.272726	5374.019327	24.996736
159.304283	5380.744406	25.001754
159.254908	5383.861234	25.006771
159.474494	5376.539000	25.011789
159.355327	5389.809030	25.016807
159.720058	5410.130957	25.021824
159.938444	5414.431556	25.026842
159.848789	5412.398802	25.031859
160.120296	5446.513856	25.036877
160.223143	5443.266422	25.041895
160.518919	5440.611290	25.046912
160.696921	5481.591119	25.051930
160.896150	5467.123341	25.056947
161.301383	5448.144054	25.061965
160.992482	5482.942551	25.066983
161.229559	5483.437280	25.072000
161.430940	5496.349481	25.077018
161.749172	5497.667534	25.082035
161.852943	5500.375270	25.087053
161.920792	5519.519792	25.092071
162.177251	5527.418238	25.097088
162.303837	5526.199054	25.102106
162.333061	5529.106704	25.107123
162.857842	5545.927645	25.112141
162.772647	5550.616547	25.117159
163.057098	5565.129093	25.122176
163.427384	5550.087199	25.127194
162.990748	5576.195112	25.132211
163.992851	5548.779874	25.137229
163.894351	5593.234919	25.142247
164.254055	5578.297742	25.147264
164.314581	5572.997433	25.152282
163.929229	5572.872365	25.157299
164.361692	5599.666993	25.162317
164.489812	5604.706599	25.167335
164.440398	5600.526773	25.172352
165.141879	5631.521275	25.177370
165.395042	5615.008751	25.182387
165.175840	5649.927080	25.187405
165.464498	5634.787189	25.192423
165.251989	5633.827397	25.197440
165.800572	5648.920196	25.202458
165.688713	5671.944514	25.207475
166.116113	5658.621807	25.212493
166.144208	5666.917841	25.217511
166.168914	5658.287561	25.222528
166.338793	5687.076833	25.227546
166.608857	5676.826130	25.232563
166.612853	5697.123369	25.237581
167.061874	5698.845411	25.242599
167.015666	5724.124286	25.247616
167.582649	5694.190662	25.252634
167.431093	5738.141667	25.257651
168.088999	5724.877338	25.262669
167.583991	5741.799768	25.267687
167.669026	5754.519908	25.272704
168.451048	5750.530020	25.277722
168.330216	5762.635526	25.282739
168.713356	5777.164801	25.287757
168.790074	5780.426818	25.292775
169.126682	5771.087471	25.297792
169.491004	5750.400853	25.302810
169.287646	5762.528172	25.307827
169.550311	5784.334116	25.312845
169.678447	5780.776543	25.317863
169.742931	5784.191560	25.322880
169.803623	5782.320447	25.327898
169.592126	5789.620221	25.332915
170.297167	5814.038377	25.337933
170.304887	5816.438933	25.342951
170.401709	5817.431216	25.347968
170.205799	5823.174753	25.352986
170.289703	5849.867285	25.358003
170.613807	5848.449010	25.363021
171.035555	5860.872457	25.368039
170.785527	5884.877364	25.373056
171.141365	5884.405172	25.378074
171.170538	5900.875209	25.383091
171.706883	5912.488197	25.388109
172.044203	5908.210430	25.393127
172.259980	5906.692201	25.398144
172.676844	5928.974915	25.403162
172.791475	5948.336752	25.408179
172.865656	5941.964187	25.413197
173.100449	5941.050273	25.418215
172.869957	5939.127229	25.423232
173.093305	5944.523101	25.428250
173.113575	5958.550268	25.433267
173.722443	5968.151880	25.438285
173.575527	5974.421850	25.443303
173.703974	5994.913645	25.448320
174.247472	5985.899136	25.453338
173.961253	5983.834706	25.458355
174.164737	6023.008799	25.463373
174.680906	6012.506208	25.468391
174.723480	6023.381391	25.473408
174.828381	6029.298114	25.478426
175.024369	6030.804070	25.483443
175.037442	6053.283526	25.488461
175.356768	6064.025711	25.493479
175.365589	6073.337571	25.498496
176.075036	6065.390899	25.503514
175.555865	6101.274664	25.508531
176.407898	6097.916286	25.513549
176.623705	6111.072188	25.518567
176.583089	6130.326059	25.523584
177.012949	6110.878611	25.528602
177.003506	6113.543148	25.533619
177.249557	6136.032000	25.538637
177.967981	6140.240497	25.543655
177.490690	6135.946219	25.548672
177.917322	6129.972896	25.553690
178.037642	6137.046065	25.558707
177.940479	6143.919467	25.563725
177.996188	6145.926924	25.568743
178.184551	6162.669256	25.573760
178.094391	6156.480150	25.578778
178.321491	6184.399007	25.583795
178.679408	6191.840275	25.588813
179.022184	6203.837605	25.593831
179.076648	6210.184135	25.598848
179.381807	6210.537438	25.603866
179.385333	6229.098363	25.608883
179.554219	6234.906624	25.613901
179.728405	6236.361793	25.618919
179.920596	6246.084312	25.623936
180.008965	6242.734375	25.628954
180.020706	6245.171336	25.633971
180.494244	6261.299497	25.638989
180.582610	6282.469173	25.644007
180.780243	6279.045162	25.649024
180.898170	6273.812550	25.654042
181.091746	6299.825186	25.659059
181.004246	6311.666200	25.664077
181.730405	6328.701397	25.669095
181.678267	6328.638839	25.674112
182.443854	6337.422669	25.679130
182.195024	6344.871855	25.684148
182.592256	6352.824616	25.689165
183.056178	6346.762653	25.694183
182.659515	6358.787533	25.699200
183.068755	6355.902516	25.704218
183.132391	6361.838541	25.709236
183.372459	6362.767899	25.714253
183.827616	6383.474062	25.719271
183.678954	6388.693389	25.724288
183.999211	6382.123263	25.729306
184.031763	6378.770394	25.734324
184.450838	6414.926231	25.739341
184.716893	6387.515880	25.744359
184.716648	6403.211500	25.749376
184.933981	6390.787057	25.754394
184.929482	6399.444310	25.759412
185.173241	6426.656829	25.764429
185.428976	6428.368870	25.769447
185.672015	6432.158385	25.774464
185.619137	6425.860157	25.779482
185.873575	6434.443102	25.784500
185.909532	6451.672673	25.789517
185.824069	6451.842799	25.794535
186.304927	6469.169819	25.799552
186.610603	6488.379957	25.804570
186.926184	6486.453955	25.809588
186.915085	6481.819319	25.814605
187.324409	6519.279831	25.819623
187.950663	6502.643894	25.824640
187.836209	6502.607005	25.829658
187.962522	6521.452407	25.834676
188.028330	6513.068410	25.839693
188.370247	6526.406773	25.844711
188.061707	6540.953465	25.849728
188.333287	6537.054991	25.854746
188.855164	6555.989999	25.859764
188.827465	6577.733268	25.864781
188.733602	6551.401213	25.869799
189.418924	6586.248341	25.874816
189.720507	6601.864577	25.879834
189.495719	6590.026574	25.884852
189.549983	6611.393342	25.889869
189.840042	6597.887922	25.894887
189.869838	6618.326290	25.899904
190.234861	6628.535261	25.904922
190.040039	6631.360050	25.909940
190.270374	6632.345264	25.914957
190.668936	6654.256710	25.919975
190.976674	6665.455933	25.924992
190.985990	6677.698002	25.930010
191.549247	6680.534108	25.935028
191.524378	6689.409565	25.940045
192.021098	6696.220791	25.945063
191.533545	6723.330950	25.950080
192.042067	6713.486824	25.955098
192.567211	6728.722160	25.960116
192.425089	6739.953827	25.965133
193.112639	6735.906369	25.970151
193.073821	6731.590782	25.975168
193.115873	6743.268294	25.980186
193.304774	6753.102607	25.985204
193.723106	6765.915244	25.990221
193.762890	6755.285888	25.995239
193.886782	6768.002280	26.000256
193.998133	6788.688301	26.005274
194.371279	6782.930169	26.010292
194.173231	6791.858476	26.015309
194.942496	6819.700747	26.020327
194.771726	6824.074824	26.025344
194.770595	6806.787998	26.030362
195.453121	6858.182017	26.035380
195.399954	6837.603723	26.040397
195.841464	6870.472324	26.045415
196.168408	6877.107716	26.050432
196.029586	6874.752939	26.055450
196.296653	6876.492339	26.060468
196.396004	6898.201659	26.065485
196.744768	6907.330026	26.070503
196.959829	6913.087134	26.075520
197.029742	6916.878415	26.080538
197.475414	6938.547527	26.085556
197.491067	6933.834528	26.090573
197.768409	6948.205594	26.095591
197.993620	6945.943039	26.100608
198.081720	6960.182212	26.105626
198.648956	6958.264022	26.110644
198.244083	6974.075113	26.115661
198.941752	6981.712811	26.120679
198.973900	6999.818528	26.125696
198.923373	6988.722680	26.130714
199.414034	6996.177813	26.135732
199.189083	7015.208094	26.140749
199.445703	7020.527462	26.145767
199.801902	7026.984379	26.150784
200.062891	7055.108763	26.155802
200.701426	7046.928195	26.160820
200.789544	7056.239045	26.165837
200.977254	7056.862871	26.170855
201.048178	7057.899495	26.175872
201.018589	7044.501284	26.180890
201.170934	7066.834190	26.185908
201.013719	7082.531953	26.190925
201.191350	7075.134536	26.195943
201.387010	7095.588030	26.200960
201.698613	7100.970259	26.205978
202.229907	7111.851723	26.210996
202.402971	7123.636107	26.216013
202.449122	7122.979585	26.221031
202.649773	7128.518775	26.226048
202.926501	7151.193113	26.231066
203.184720	7156.552402	26.236084
202.956862	7160.363683	26.241101
203.541227	7184.015784	26.246119
203.787634	7183.979581	26.251136
203.995859	7198.888273	26.256154
204.125990	7211.976206	26.261172
204.181650	7233.691410	26.266189
204.399741	7229.973594	26.271207
204.630774	7240.975411	26.276224
205.096700	7243.031701	26.281242
205.258920	7254.088559	26.286260
205.414477	7269.111937	26.291277
205.698894	7264.208852	26.296295
205.907024	7274.362247	26.301312
206.053063	7309.936730	26.306330
206.640696	7300.461205	26.311348
206.714800	7304.041842	26.316365
206.907942	7308.708165	26.321383
206.942249	7319.868868	26.326400
207.206948	7322.778668	26.331418
207.666243	7336.121082	26.336436
207.442757	7340.652419	26.341453
207.712567	7335.820092	26.346471
207.863408	7376.382276	26.351488
208.193750	7374.239014	26.356506
208.526909	7375.184283	26.361524
208.579444	7394.281748	26.366541
208.511116	7400.343087	26.371559
209.052474	7405.828062	26.376576
208.830432	7406.940531	26.381594
209.292258	7417.683806	26.386612
209.030015	7460.091041	26.391629
209.798359	7444.105697	26.396647
210.191734	7459.258942	26.401664
210.225095	7475.533362	26.406682
210.696444	7468.177831	26.411700
210.772897	7465.749296	26.416717
211.336385	7484.307493	26.421735
211.705872	7491.524913	26.426752
211.537073	7500.234969	26.431770
211.971277	7500.125552	26.436788
211.942481	7496.554037	26.441805
211.963214	7491.502511	26.446823
212.132469	7493.141133	26.451840
212.181290	7516.642322	26.456858
212.597648	7521.506021	26.461876
212.768381	7530.714302	26.466893
212.610261	7533.050307	26.471911
213.081983	7543.533236	26.476928
213.050752	7554.686466	26.481946
213.440771	7559.001249	26.486964
213.621626	7582.300525	26.491981
213.664647	7572.904576	26.496999
214.160150	7590.275432	26.502016
213.722187	7613.237521	26.507034
214.482529	7624.130844	26.512052
214.614320	7632.269035	26.517069
214.729794	7633.251389	26.522087
214.870568	7671.916616	26.527104
215.168835	7657.095733	26.532122
215.537680	7680.015844	26.537140
215.487789	7701.049081	26.542157
215.925198	7716.947768	26.547175
216.200944	7721.538894	26.552192
216.286499	7743.334268	26.557210
216.945514	7745.932653	26.562228
217.112187	7744.135670	26.567245
217.185687	7781.744192	26.572263
217.286149	7762.563484	26.577280
217.573364	7806.181574	26.582298
218.469372	7783.211340	26.587316
218.238820	7795.967815	26.592333
218.409097	7814.461651	26.597351
218.714148	7807.765075	26.602368
218.747987	7824.544943	26.607386
219.023876	7820.346459	26.612404
219.364632	7844.154907	26.617421
219.763015	7844.409994	26.622439
219.590990	7850.636758	26.627456
220.015844	7864.734201	26.632474
220.259564	7877.401757	26.637492
220.056785	7888.534591	26.642509
220.373456	7888.761004	26.647527
220.627215	7909.514010	26.652544
220.401037	7918.090254	26.657562
220.824650	7932.846536	26.662580
221.190610	7946.677268	26.667597
221.112819	7970.743848	26.672615
221.725817	7969.535047	26.677632
221.960660	7994.430714	26.682650
222.304572	7991.400015	26.687668
222.678076	8002.389128	26.692685
222.381335	8011.199349	26.697703
223.307963	8013.001332	26.702720
223.406543	8032.235479	26.707738
223.660384	8032.030497	26.712756
223.735450	8021.906840	26.717773
224.058007	8043.882038	26.722791
224.471537	8040.827641	26.727808
224.219269	8042.329737	26.732826
224.565250	8036.172598	26.737844
224.478222	8046.031305	26.742861
224.747299	8068.113419	26.747879
225.115093	8066.920886	26.752896
225.155871	8082.999653	26.757914
225.738914	8097.776320	26.762932
226.157641	8092.987677	26.767949
225.776309	8102.430680	26.772967
226.024336	8123.303712	26.777984
226.178045	8136.262807	26.783002
226.466228	8128.175282	26.788020
226.863646	8161.806395	26.793037
226.844766	8168.956235	26.798055
227.481910	8174.119362	26.803072
227.230537	8200.005628	26.808090
227.647788	8199.913078	26.813108
227.786906	8209.233832	26.818125
228.123360	8222.431396	26.823143
228.425164	8237.854976	26.828160
228.238038	8257.134177	26.833178
228.817492	8266.335982	26.838196
229.164338	8280.958497	26.843213
229.061549	8293.848463	26.848231
229.889252	8303.368731	26.853248
229.860674	8319.080335	26.858266
230.095819	8317.793264	26.863284
230.268255	8326.909707	26.868301
230.221317	8343.463048	26.873319
230.813136	8344.980107	26.878336
230.812817	8366.923851	26.883354
231.679364	8362.978841	26.888372
231.868203	8364.413792	26.893389
231.850090	8383.888891	26.898407
232.992822	8374.737297	26.903424
232.625850	8383.237109	26.908442
232.857278	8383.910679	26.913460
232.899930	8381.213560	26.918477
233.143626	8408.671296	26.923495
233.596303	8408.886267	26.928512
233.505120	8413.995631	26.933530
233.761723	8412.089023	26.938548
234.252375	8418.534562	26.943565
234.170037	8443.350930	26.948583
234.632361	8435.087549	26.953600
234.583753	8446.810755	26.958618
234.677762	8457.045317	26.963636
235.303508	8462.369311	26.968653
235.071890	8463.207981	26.973671
235.320442	8485.766890	26.978688
234.979931	8508.120736	26.983706
235.188447	8500.596515	26.988724
235.844733	8527.097180	26.993741
235.423927	8549.707029	26.998759
235.613188	8566.453513	27.003776
236.422667	8584.030427	27.008794
236.328091	8597.957221	27.013812
236.928050	8609.255331	27.018829
236.909685	8622.981150	27.023847
237.638370	8650.166871	27.028864
237.939165	8668.382083	27.033882
238.141423	8661.762105	27.038900
238.449318	8675.353339	27.043917
238.688308	8682.978502	27.048935
238.769886	8687.526920	27.053952
239.164859	8706.529773	27.058970
239.196874	8723.631988	27.063988
239.309067	8732.071345	27.069005
239.544701	8749.690366	27.074023
240.143942	8771.910528	27.079040
240.267584	8778.947449	27.084058
240.594109	8782.714036	27.089076
241.095595	8791.181069	27.094093
241.098386	8812.094164	27.099111
241.160377	8814.436193	27.104128
241.810074	8830.122041	27.109146
241.658687	8856.538809	27.114164
242.388435	8847.820246	27.119181
242.184050	8873.598679	27.124199
242.845700	8858.916971	27.129216
242.568506	8873.604932	27.134234
242.835427	8896.561271	27.139252
243.117376	8916.369292	27.144269
243.194313	8924.275364	27.149287
243.370722	8929.852932	27.154304
243.953007	8956.943735	27.159322
244.130855	8966.474397	27.164340
244.362100	8987.079054	27.169357
244.673056	8996.055006	27.174375
244.881186	8990.365621	27.179392
245.256219	9024.892617	27.184410
245.338179	9026.415493	27.189428
245.755226	9029.174267	27.194445
245.863161	9044.075229	27.199463
246.009278	9051.407714	27.204480
246.479588	9078.936002	27.209498
246.919264	9080.526973	27.214516
247.506414	9079.423725	27.219533
247.209193	9099.911341	27.224551
247.705335	9104.250584	27.229568
247.909737	9105.442733	27.234586
248.175169	9124.542314	27.239604
248.531035	9126.806461	27.244621
248.571606	9130.950007	27.249639
248.803517	9139.519626	27.254656
249.129040	9153.421671	27.259674
249.338901	9156.158023	27.264692
249.714596	9155.363893	27.269709
249.449274	9161.852765	27.274727
250.149341	9181.000379	27.279744
250.266433	9190.619559	27.284762
250.186377	9193.569351	27.289780
250.476567	9213.181696	27.294797
250.365120	9230.580416	27.299815
250.250792	9252.344549	27.304832
250.811599	9264.196693	27.309850
251.030139	9290.578469	27.314868
251.609588	9297.493791	27.319885
251.908203	9325.195089	27.324903
251.982839	9328.010079	27.329920
252.196424	9345.959493	27.334938
252.341188	9363.937998	27.339956
252.826750	9369.621468	27.344973
253.078222	9386.584012	27.349991
253.511342	9414.087372	27.355008
253.708217	9419.338836	27.360026
253.911771	9435.321896	27.365044
254.452998	9438.845502	27.370061
254.369218	9459.698546	27.375079
254.895113	9470.511010	27.380096
255.147185	9481.666552	27.385114
255.200218	9490.233806	27.390132
255.758641	9495.920662	27.395149
255.876461	9517.934217	27.400167
256.041769	9540.360053	27.405184
256.669371	9539.352627	27.410202
256.716014	9556.377526	27.415220
257.064183	9549.490347	27.420237
257.379577	9566.507433	27.425255
257.841439	9581.145944	27.430272
258.131893	9581.989582	27.435290
258.372703	9589.367042	27.440308
258.842763	9598.949105	27.445325
258.894276	9608.596715	27.450343
258.890958	9609.332162	27.455360
259.095651	9619.923664	27.460378
259.313620	9645.966997	27.465396
259.558972	9635.429512	27.470413
259.557857	9659.811193	27.475431
259.917901	9676.644622	27.480448
260.309747	9698.033617	27.485466
259.996965	9707.714182	27.490484
260.507871	9717.969712	27.495501
260.687651	9733.195926	27.500519
261.005905	9772.877443	27.505536
261.444089	9774.351479	27.510554
261.539317	9796.262809	27.515572
262.090922	9801.283162	27.520589
262.101280	9810.734435	27.525607
262.661855	9837.736264	27.530624
263.189923	9830.590890	27.535642
262.923801	9856.648804	27.540660
263.591771	9853.402794	27.545677
263.563961	9870.398210	27.550695
263.717534	9886.089113	27.555712
264.216396	9894.990013	27.560730
264.300824	9897.698101	27.565748
265.089102	9909.654969	27.570765
264.914976	9933.692848	27.575783
265.505033	9936.896379	27.580800
265.725975	9941.282103	27.585818
265.981084	9941.736355	27.590836
266.106097	9950.415160	27.595853
266.299324	9962.450796	27.600871
266.115982	9968.559838	27.605888
266.709917	9989.200922	27.610906
266.776721	9995.309447	27.615924
267.148808	10024.592702	27.620941
267.185489	10038.318520	27.625959
267.564970	10055.173673	27.630976
267.834522	10064.414596	27.635994
267.981761	10089.710969	27.641012
268.176483	10108.072335	27.646029
268.723744	10122.171300	27.651047
268.355658	10139.565947	27.656064
269.054764	10160.331366	27.661082
269.281659	10183.918540	27.666100
270.053076	10198.163630	27.671117
270.588382	10209.535835	27.676135
270.798130	10227.216995	27.681152
271.166975	10223.405163	27.686170
271.276145	10254.870499	27.691188
271.749580	10248.371071	27.696205
272.008402	10257.937655	27.701223
271.702126	10273.664887	27.706240
271.895824	10272.733670	27.711258
272.269361	10302.296606	27.716276
272.489132	10315.834133	27.721293
273.028461	10346.886012	27.726311
273.112899	10355.721829	27.731328
273.508762	10372.316214	27.736346
273.672314	10386.399867	27.741364
274.298713	10391.027219	27.746381
274.791009	10401.354655	27.751399
274.977255	10409.269271	27.756416
275.345241	10416.590275	27.761434
275.884145	10422.545417	27.766452
276.126658	10415.128144	27.771469
276.249260	10433.609220	27.776487
276.301248	10448.681433	27.781504
276.570785	10450.614468	27.786522
276.755569	10464.428029	27.791540
276.784531	10471.454478	27.796557
277.105071	10483.205425	27.801575
277.461688	10504.081006	27.806592
277.559427	10517.301741	27.811610
277.866810	10523.229297	27.816628
278.225292	10533.923635	27.821645
278.633712	10540.103842	27.826663
278.354652	10563.637694	27.831680
278.849841	10564.699013	27.836698
279.251134	10593.947641	27.841716
279.431517	10607.075797	27.846733
279.762651	10607.691874	27.851751
279.997386	10626.790399	27.856768
280.239710	10640.526484	27.861786
280.478191	10656.405337	27.866804
280.828136	10657.964754	27.871821
280.984728	10694.874429	27.876839
281.031329	10709.525550	27.881856
281.625903	10720.719106	27.886874
281.927202	10749.374856	27.891892
282.085404	10764.221118	27.896909
282.379655	10770.434573	27.901927
282.713431	10801.408016	27.906944
283.046697	10822.114626	27.911962
283.095180	10821.648810	27.916980
283.647293	10844.441484	27.921997
283.876022	10855.478612	27.927015
284.066572	10878.972726	27.932032
284.857012	10886.614214	27.937050
284.911538	10889.259961	27.942068
285.260783	10929.928055	27.947085
285.600723	10923.359118	27.952103
286.001121	10940.503122	27.957120
286.033536	10945.982022	27.962138
286.325656	10972.613164	27.967156
286.621819	10961.223790	27.972173
286.898780	11002.238860	27.977191
286.898449	11026.664737	27.982208
287.623591	11033.899210	27.987226
287.921274	11036.160341	27.992244
288.015865	11056.617280	27.997261
288.647691	11075.211969	28.002279
288.543123	11091.956964	28.007296
288.927149	11105.704729	28.012314
289.388058	11114.602575	28.017332
289.894192	11117.547840	28.022349
290.124761	11136.856233	28.027367
290.053310	11163.534648	28.032384
290.496700	11171.994601	28.037402
290.839719	11184.088796	28.042420
290.931998	11190.877258	28.047437
291.199482	11221.730311	28.052455
291.539180	11229.046782	28.057472
291.796524	11228.647217	28.062490
292.137122	11256.683414	28.067508
291.972165	11293.768584	28.072525
292.448298	11272.256533	28.077543
292.557896	11316.600234	28.082560
293.267543	11319.144780	28.087578
293.308948	11318.367635	28.092596
293.478793	11373.256866	28.097613
294.198558	11349.436524	28.102631
294.231825	11405.155901	28.107648
294.780697	11385.088070	28.112666
294.947684	11416.093694	28.117684
295.387433	11417.828157	28.122701
295.756800	11419.466806	28.127719
295.366405	11466.867721	28.132736
296.484055	11436.461033	28.137754
296.804636	11496.073171	28.142772
297.036567	11464.263086	28.147789
297.234329	11505.080836	28.152807
297.735420	11483.814778	28.157824
297.558348	11517.163311	28.162842
297.971234	11510.536060	28.167860
298.281261	11526.029414	28.172877
299.013008	11542.985532	28.177895
298.966634	11551.293563	28.182912
299.161489	11568.303413	28.187930
299.881070	11571.801080	28.192948
299.618437	11586.329199	28.197965
300.196169	11601.088955	28.202983
300.529871	11610.164779	28.208000
300.750524	11639.620136	28.213018
301.014792	11649.614098	28.218036
300.980846	11662.401928	28.223053
301.532145	11700.045655	28.228071
301.903953	11691.878757	28.233088
301.912049	11734.211300	28.238106
302.618600	11715.759644	28.243124
302.550099	11758.819087	28.248141
302.749461	11767.781837	28.253159
303.440226	11775.708841	28.258176
303.548453	11796.383012	28.263194
303.913733	11826.335124	28.268212
304.100124	11827.961665	28.273229
304.709006	11848.315274	28.278247
304.753699	11878.142291	28.283264
305.377457	11878.413499	28.288282
305.863194	11887.820212	28.293300
306.234755	11905.812047	28.298317
306.752719	11926.515927	28.303335
306.538579	11912.946799	28.308352
306.510517	11954.853245	28.313370
307.028326	11930.396380	28.318388
307.107929	11980.948693	28.323405
308.098059	11978.265583	28.328423
308.142571	11989.964904	28.333440
308.074207	12024.224757	28.338458
308.526819	12013.899716	28.343476
308.957349	12055.438990	28.348493
309.521185	12056.962502	28.353511
309.698754	12076.875555	28.358528
309.941681	12082.424813	28.363546
310.287828	12094.768345	28.368564
310.110693	12112.238315	28.373581
310.892388	12130.920616	28.378599
311.108180	12140.775453	28.383616
311.117757	12155.101744	28.388634
311.302602	12173.810757	28.393652
311.850835	12179.359397	28.398669
311.928024	12199.220532	28.403687
312.188829	12226.766751	28.408704
312.476689	12243.999050	28.413722
312.712027	12246.328548	28.418740
313.133024	12283.929965	28.423757
313.931598	12285.654959	28.428775
314.138041	12303.549626	28.433792
314.142677	12310.638266	28.438810
314.884566	12343.042885	28.443828
314.798862	12369.215880	28.448845
315.118579	12368.863017	28.453863
315.527818	12393.616207	28.458880
315.767637	12412.480463	28.463898
316.164172	12428.262208	28.468916
316.545364	12458.703381	28.473933
317.059400	12469.472103	28.478951
317.337128	12479.984527	28.483968
317.739710	12496.428485	28.488986
318.349901	12502.628707	28.494004
318.183364	12519.976248	28.499021
318.530190	12532.554186	28.504039
319.108885	12559.484636	28.509056
319.273924	12567.727061	28.514074
319.620187	12566.437676	28.519092
319.506082	12619.686650	28.524109
320.429733	12618.478586	28.529127
320.595298	12632.063440	28.534144
320.638268	12658.377185	28.539162
321.172425	12671.816353	28.544180
321.315671	12697.131712	28.549197
321.819867	12706.885659	28.554215
321.756826	12734.300242	28.559232
322.199686	12759.685029	28.564250
322.782985	12768.621222	28.569268
322.833273	12783.849717	28.574285
323.250925	12793.440027	28.579303
323.585381	12832.144156	28.584320
323.959022	12853.201315	28.589338
324.444068	12847.810310	28.594356
324.635404	12883.712720	28.599373
324.730140	12902.770329	28.604391
325.347620	12913.929219	28.609408
325.220065	12929.876288	28.614426
325.931841	12934.378288	28.619444
325.973566	12985.899063	28.624461
326.852912	12964.765064	28.629479
326.702727	12995.362259	28.634496
326.914845	13024.324427	28.639514
327.781532	13027.288374	28.644532
327.822086	13042.542489	28.649549
328.568048	13066.446767	28.654567
328.753025	13080.086781	28.659584
328.877021	13083.041405	28.664602
329.308806	13093.338044	28.669620
329.528581	13111.933046	28.674637
329.969914	13132.309589	28.679655
330.304806	13139.702930	28.684672
330.558351	13156.220752	28.689690
330.774044	13156.461403	28.694708
331.290093	13191.266727	28.699725
331.279345	13200.803771	28.704743
331.395352	13214.638491	28.709760
331.695122	13234.755950	28.714778
331.845961	13252.266260	28.719796
331.974339	13292.765173	28.724813
332.750892	13304.719171	28.729831
333.587162	13331.739229	28.734848
333.564644	13355.428775	28.739866
334.181182	13372.989562	28.744884
334.279456	13396.516469	28.749901
334.928472	13402.917302	28.754919
335.364718	13412.621733	28.759936
335.445501	13447.925211	28.764954
336.127013	13433.325869	28.769972
336.074538	13463.132332	28.774989
336.536952	13466.331020	28.780007
336.836535	13499.021139	28.785024
337.063896	13509.825869	28.790042
337.422073	13535.965154	28.795060
337.455253	13568.534554	28.800077
337.996190	13566.900984	28.805095
338.480011	13613.764880	28.810112
338.904433	13598.448550	28.815130
339.228846	13656.118870	28.820148
339.422903	13641.298895	28.825165
339.769538	13687.391851	28.830183
340.676651	13690.600393	28.835200
340.837699	13722.116632	28.840218
341.429564	13712.068154	28.845236
341.682221	13734.877121	28.850253
342.208210	13735.053767	28.855271
342.234257	13760.025331	28.860288
342.465485	13784.621043	28.865306
343.194354	13789.144984	28.870324
343.485523	13810.064702	28.875341
343.356094	13814.097898	28.880359
343.797612	13831.813646	28.885376
344.124206	13851.834570	28.890394
344.249024	13862.158029	28.895412
344.517978	13888.510697	28.900429
344.535542	13896.879483	28.905447
344.928499	13940.314137	28.910464
345.254344	13943.064770	28.915482
345.784124	13970.659057	28.920500
346.043004	13979.143217	28.925517
346.231556	14019.317548	28.930535
346.946473	14022.922428	28.935552
346.969892	14037.148615	28.940570
346.946678	14080.300600	28.945588
347.902422	14072.498577	28.950605
347.964489	14131.266110	28.955623
348.465692	14134.671490	28.960640
348.685570	14140.890425	28.965658
349.067428	14185.205815	28.970676
349.126278	14193.616496	28.975693
349.540815	14225.242739	28.980711
350.340832	14232.492136	28.985728
350.542905	14265.692894	28.990746
350.940400	14296.144703	28.995764
351.396279	14322.826516	29.000781
351.667504	14339.627172	29.005799
352.203364	14349.459005	29.010816
352.289263	14375.803317	29.015834
352.849266	14394.472892	29.020852
353.308979	14437.450230	29.025869
353.472870	14446.275088	29.030887
353.980454	14454.773504	29.035904
354.152936	14482.495034	29.040922
354.183328	14515.617035	29.045940
354.825281	14526.737703	29.050957
355.456526	14543.039896	29.055975
355.858868	14557.579693	29.060992
355.850195	14595.886240	29.066010
356.414836	14606.324209	29.071028
356.991480	14616.993081	29.076045
356.958152	14646.011722	29.081063
357.703681	14681.882203	29.086080
358.175799	14690.136080	29.091098
358.341805	14708.039042	29.096116
358.709734	14740.366309	29.101133
358.737629	14747.815169	29.106151
359.392347	14759.268333	29.111168
359.118459	14811.537712	29.116186
360.235803	14813.112058	29.121204
360.607155	14829.212639	29.126221
360.539599	14865.903894	29.131239
361.378022	14878.896351	29.136256
361.570045	14918.762048	29.141274
362.040900	14926.495526	29.146292
362.064600	14946.440309	29.151309
362.717371	14979.282284	29.156327
362.995932	14951.862744	29.161344
363.375244	15014.836439	29.166362
364.054051	15008.240980	29.171380
364.285420	15054.783791	29.176397
364.347937	15038.009422	29.181415
364.745390	15087.006629	29.186432
364.947269	15109.491677	29.191450
365.539607	15087.847696	29.196468
366.027844	15144.146078	29.201485
366.288070	15137.152649	29.206503
366.888625	15150.940222	29.211520
366.807895	15187.947165	29.216538
367.066457	15188.387469	29.221556
368.154455	15205.068458	29.226573
367.411152	15240.615754	29.231591
368.521439	15239.487796	29.236608
368.476282	15298.703277	29.241626
369.210827	15270.302645	29.246644
369.611723	15309.197419	29.251661
369.645718	15340.552351	29.256679
370.362069	15323.769019	29.261696
370.395347	15380.762505	29.266714
370.548920	15423.669389	29.271732
370.900515	15414.510464	29.276749
371.112796	15464.217169	29.281767
371.743974	15463.559655	29.286784
371.742357	15515.728804	29.291802
372.466152	15526.967649	29.296820
372.771036	15544.399658	29.301837
372.999275	15600.622208	29.306855
373.622481	15598.553473	29.311872
373.965199	15663.011918	29.316890
374.286962	15661.012469	29.321908
375.042448	15710.189306	29.326925
374.947214	15722.518362	29.331943
375.787150	15744.412704	29.336960
375.966644	15793.476918	29.341978
376.140165	15800.032299	29.346996
376.611179	15818.656793	29.352013
376.933580	15859.895610	29.357031
377.532655	15878.460112	29.362048
377.624250	15894.977193	29.367066
378.007662	15945.674125	29.372084
378.817560	15941.907812	29.377101
379.040521	15992.642671	29.382119
379.590519	16008.239053	29.387136
379.857922	16023.558204	29.392154
380.052183	16050.260399	29.397172
380.653410	16064.357616	29.402189
380.736660	16113.167669	29.407207
381.478413	16119.373921	29.412224
381.523990	16145.466037	29.417242
381.640218	16192.188690	29.422260
382.435033	16185.529871	29.427277
383.013892	16231.080690	29.432295
383.333392	16255.869918	29.437312
383.985451	16281.369247	29.442330
384.271554	16305.201446	29.447348
384.447213	16323.266149	29.452365
384.591774	16351.619912	29.457383
385.132073	16392.998045	29.462400
385.522451	16393.890926	29.467418
385.533002	16422.718856	29.472436
386.648469	16454.497419	29.477453
386.412968	16475.537587	29.482471
387.046511	16495.965944	29.487488
387.282082	16514.114025	29.492506
387.867820	16540.684127	29.497524
388.284959	16571.023870	29.502541
388.371024	16579.973664	29.507559
388.951934	16613.865384	29.512576
389.221165	16642.407461	29.517594
389.372235	16671.957447	29.522612
390.107427	16688.182296	29.527629
390.468847	16715.785742	29.532647
390.986031	16728.381735	29.537664
391.269225	16754.191088	29.542682
391.702011	16795.218395	29.547700
392.090929	16821.681785	29.552717
392.513831	16840.855766	29.557735
393.073433	16860.406948	29.562752
393.417541	16873.736057	29.567770
393.612073	16912.338197	29.572788
394.157934	16934.299808	29.577805
394.218475	16962.284277	29.582823
394.455363	16993.192089	29.587840
394.690435	17009.663096	29.592858
395.400156	17055.932322	29.597876
395.890223	17083.862932	29.602893
396.176854	17114.304455	29.607911
396.606359	17122.267861	29.612928
396.956330	17185.663250	29.617946
397.402555	17194.081457	29.622964
397.416935	17229.390645	29.627981
398.113303	17272.588389	29.632999
398.695853	17274.597822	29.638016
399.321200	17323.501090	29.643034
399.784130	17344.685642	29.648052
400.239251	17358.057515	29.653069
400.163778	17410.406050	29.658087
400.971230	17410.559965	29.663104
401.389247	17438.409796	29.668122
401.617297	17483.959111	29.673140
402.312369	17519.332325	29.678157
402.894399	17516.020524	29.683175
402.797048	17567.135987	29.688192
403.308465	17584.863653	29.693210
403.327730	17621.368519	29.698228
404.196497	17614.604019	29.703245
404.363974	17680.719853	29.708263
405.044135	17674.859325	29.713280
405.301736	17732.128883	29.718298
405.315469	17742.635047	29.723316
406.226206	17759.482614	29.728333
406.536067	17816.161721	29.733351
406.304149	17824.351749	29.738368
407.519361	17842.811594	29.743386
407.701633	17908.623703	29.748404
408.210917	17898.915588	29.753421
409.093335	17903.443880	29.758439
409.221005	17940.246573	29.763456
409.741238	17970.444108	29.768474
409.701142	17955.678952	29.773492
410.120172	18025.017966	29.778509
410.422905	18036.027259	29.783527
411.236699	18056.141587	29.788544
411.425539	18066.576173	29.793562
411.830688	18084.506180	29.798580
412.185131	18128.918026	29.803597
412.230212	18141.048313	29.808615
412.723083	18182.022294	29.813632
413.594199	18207.406553	29.818650
413.691023	18230.782446	29.823668
414.130925	18242.731795	29.828685
414.283893	18302.613322	29.833703
414.694071	18312.936823	29.838720
415.402856	18337.469641	29.843738
415.507227	18372.745639	29.848756
416.172199	18398.582730	29.853773
416.171561	18448.058974	29.858791
416.828900	18473.187193	29.863808
417.552992	18500.333889	29.868826
417.716145	18536.195363	29.873844
418.254468	18569.738928	29.878861
418.779730	18599.743392	29.883879
419.000300	18607.557995	29.888896
419.322456	18661.625895	29.893914
419.576808	18698.078709	29.898932
420.400620	18705.561022	29.903949
420.790818	18775.661517	29.908967
421.352004	18789.321863	29.913984
421.704921	18818.897134	29.919002
421.887842	18819.904526	29.924020
422.568594	18886.973428	29.929037
423.126592	18895.651728	29.934055
423.865461	18915.201168	29.939072
424.380677	18943.270111	29.944090
425.120906	18952.173343	29.949108
425.499646	18958.605048	29.954125
426.347800	19006.633650	29.959143
426.738595	18991.120501	29.964160
427.104414	19025.733882	29.969178
427.339451	19033.755845	29.974196
427.954121	19031.514129	29.979213
428.096740	19069.035623	29.984231
428.304180	19083.259687	29.989248
428.608892	19097.477320	29.994266
428.789022	19129.746486	29.999284
429.233852	19155.186845	30.004301
429.784440	19180.048576	30.009319
429.931043	19209.081079	30.014336
430.187994	19234.263705	30.019354
430.348265	19278.203472	30.024372
430.672782	19289.441295	30.029389
431.315739	19318.053960	30.034407
431.501789	19353.642405	30.039424
431.739611	19385.704872	30.044442
432.075328	19415.594658	30.049460
432.584991	19466.868080	30.054477
433.243231	19482.165991	30.059495
433.591917	19509.606173	30.064512
434.018027	19553.611055	30.069530
434.321830	19596.248092	30.074548
434.938558	19633.926908	30.079565
435.504913	19659.503067	30.084583
435.890359	19685.297866	30.089600
436.034339	19739.195529	30.094618
436.402687	19747.911223	30.099636
437.253574	19812.793910	30.104653
437.751785	19833.550245	30.109671
438.115123	19873.201224	30.114688
438.974998	19903.604133	30.119706
439.033619	19938.224393	30.124724
439.335612	19976.254992	30.129741
440.094847	20004.396429	30.134759
440.487425	20025.548222	30.139776
441.031579	20046.724322	30.144794
441.424865	20093.830661	30.149812
442.299553	20109.193925	30.154829
442.529528	20139.668525	30.159847
442.718832	20178.952706	30.164864
443.553496	20199.699231	30.169882
444.082699	20237.406053	30.174900
443.907257	20287.667229	30.179917
444.997707	20313.924802	30.184935
444.960039	20339.678643	30.189952
445.552498	20365.077378	30.194970
445.806050	20393.004001	30.199988
446.222297	20450.791410	30.205005
446.794105	20460.813403	30.210023
447.029700	20486.472366	30.215040
447.487262	20524.659452	30.220058
448.099196	20568.473793	30.225076
448.536326	20602.002824	30.230093
449.325311	20630.601725	30.235111
449.668114	20659.658033	30.240128
450.182173	20689.643118	30.245146
450.771619	20727.015110	30.250164
451.309397	20759.148760	30.255181
451.438237	20780.743253	30.260199
451.431859	20819.276664	30.265216
452.378788	20839.527361	30.270234
453.092676	20872.621098	30.275252
453.214060	20899.374263	30.280269
453.593457	20935.647798	30.285287
454.044859	20958.638568	30.290304
454.889521	20996.288298	30.295322
454.900871	21030.072725	30.300340
455.089624	21051.797827	30.305357
455.934351	21075.847904	30.310375
456.069637	21113.480214	30.315392
456.753574	21140.394587	30.320410
457.007291	21157.052091	30.325428
457.410735	21191.305176	30.330445
458.100651	21228.825769	30.335463
458.122982	21265.628287	30.340480
458.628443	21285.355723	30.345498
459.091655	21351.900508	30.350516
459.393275	21380.746572	30.355533
459.971555	21393.337432	30.360551
460.182595	21462.383874	30.365568
461.422900	21479.236949	30.370586
461.976768	21506.718433	30.375604
461.965382	21555.298990	30.380621
462.757871	21573.804881	30.385639
463.171804	21602.020757	30.390656
463.596493	21634.827089	30.395674
463.644140	21672.585744	30.400692
463.971479	21710.392070	30.405709
464.884839	21746.022071	30.410727
464.805776	21784.122498	30.415744
465.434905	21817.987388	30.420762
465.891606	21880.926134	30.425780
466.483449	21916.011574	30.430797
467.281486	21942.124748	30.435815
467.908024	21999.590997	30.440832
468.074820	22016.531425	30.445850
468.865548	22042.678222	30.450868
468.620386	22108.851575	30.455885
469.739899	22117.200051	30.460903
469.903437	22172.250434	30.465920
470.535130	22197.355680	30.470938
470.868990	22242.510215	30.475956
471.046873	22277.055989	30.480973
471.990592	22306.081037	30.485991
472.181220	22339.748354	30.491008
473.161849	22403.775260	30.496026
473.812475	22413.733584	30.501044
473.791141	22484.761326	30.506061
474.408079	22483.110654	30.511079
474.706629	22530.180728	30.516096
475.110582	22567.438201	30.521114
476.056047	22612.292370	30.526132
475.995966	22647.426602	30.531149
476.857297	22664.963538	30.536167
476.952024	22733.374870	30.541184
477.971500	22741.058360	30.546202
478.085761	22797.074908	30.551220
478.751085	22794.631267	30.556237
479.668656	22842.474729	30.561255
479.920114	22887.200822	30.566272
480.389742	22907.294759	30.571290
481.054484	22932.781052	30.576308
481.197343	22962.673677	30.581325
481.645003	22991.486825	30.586343
481.961660	23007.465620	30.591360
482.228011	23052.976626	30.596378
483.029538	23096.071966	30.601396
483.016380	23111.711970	30.606413
483.740606	23165.043772	30.611431
484.317438	23193.515365	30.616448
484.500527	23227.579582	30.621466
485.015430	23277.395332	30.626484
485.719356	23317.271294	30.631501
486.156102	23334.386726	30.636519
486.636135	23389.128647	30.641536
487.155787	23389.987791	30.646554
487.945907	23454.100510	30.651572
487.796255	23473.812592	30.656589
488.682541	23505.268599	30.661607
489.192784	23549.886026	30.666624
489.623561	23588.351435	30.671642
490.000770	23603.540643	30.676660
490.488385	23676.308143	30.681677
490.942774	23718.323925	30.686695
491.526541	23747.397956	30.691712
492.038305	23774.983841	30.696730
492.507238	23828.149827	30.701748
492.849485	23869.293049	30.706765
493.343170	23896.017977	30.711783
494.487270	23946.086096	30.716800
494.567559	23967.590294	30.721818
494.997722	24013.159089	30.726836
495.514028	24068.292193	30.731853
496.349250	24085.042497	30.736871
496.694484	24148.709050	30.741888
497.010614	24179.061564	30.746906
497.486185	24198.852950	30.751924
497.996531	24271.633737	30.756941
498.355418	24276.529347	30.761959
499.036644	24348.457787	30.766976
499.371358	24387.526466	30.771994
500.301530	24407.911274	30.777012
500.583759	24458.922536	30.782029
501.427867	24501.581702	30.787047
501.865682	24533.137983	30.792064
502.259778	24569.493546	30.797082
503.019923	24595.611649	30.802100
502.997233	24649.040659	30.807117
503.738982	24679.691023	30.812135
504.151167	24739.032750	30.817152
504.885900	24758.204596	30.822170
505.217490	24797.116453	30.827188
505.735994	24858.815795	30.832205
506.123556	24879.285292	30.837223
506.928909	24914.363073	30.842240
507.096244	24974.809654	30.847258
509.060024	24950.592386	30.852276
509.488112	24972.348164	30.857293
510.108339	25004.071672	30.862311
510.368322	24999.114926	30.867328
510.602451	25027.186758	30.872346
511.405749	25040.841975	30.877364
511.459311	25072.137583	30.882381
512.241534	25075.950651	30.887399
512.232164	25090.764906	30.892416
512.797027	25131.428516	30.897434
513.134277	25161.797661	30.902452
513.570258	25176.530809	30.907469
513.644588	25214.459070	30.912487
514.078614	25254.279715	30.917504
514.690323	25297.714559	30.922522
515.194794	25332.810478	30.927540
515.607912	25387.111494	30.932557
515.825654	25409.304692	30.937575
516.630898	25459.389037	30.942592
517.011771	25521.998277	30.947610
517.878352	25543.068978	30.952628
518.039802	25586.650384	30.957645
518.434854	25640.072879	30.962663
519.365642	25685.546232	30.967680
519.319766	25722.490484	30.972698
519.822990	25758.275233	30.977716
520.884351	25811.174654	30.982733
521.252525	25869.693380	30.987751
521.668639	25914.572702	30.992768
522.214375	25963.390732	30.997786
522.773291	26011.905891	31.002804
523.173122	26049.508566	31.007821
523.800679	26096.041296	31.012839
524.790504	26150.451550	31.017856
525.328677	26170.190519	31.022874
526.267509	26214.617167	31.027892
527.027290	26223.072443	31.032909
527.404678	26265.204112	31.037927
528.189029	26297.897425	31.042944
528.823039	26315.026404	31.047962
529.623936	26361.993929	31.052980
530.141666	26372.176822	31.057997
530.423668	26378.166945	31.063015
531.192113	26430.072860	31.068032
531.355240	26451.477404	31.073050
532.004731	26482.047469	31.078068
532.381550	26505.398513	31.083085
532.730526	26532.833928	31.088103
532.932870	26579.631959	31.093120
533.390157	26611.355476	31.098138
534.025078	26644.351390	31.103156
534.342149	26688.175698	31.108173
534.740804	26725.160949	31.113191
535.300447	26760.370960	31.118208
536.061980	26815.421717	31.123226
536.415856	26828.073948	31.128244
536.533256	26897.876605	31.133261
537.308889	26892.239991	31.138279
537.618233	26950.244999	31.143296
537.741296	27000.407392	31.148314
538.668003	27025.243263	31.153332
539.123808	27078.911400	31.158349
539.702185	27133.707240	31.163367
540.300597	27164.296199	31.168384
540.938636	27218.436032	31.173402
541.178571	27255.011339	31.178420
541.807247	27308.592832	31.183437
542.407434	27331.592009	31.188455
543.025823	27397.082510	31.193472
543.583024	27422.529332	31.198490
544.069105	27470.918702	31.203508
544.700728	27513.912059	31.208525
544.960216	27572.503153	31.213543
545.971324	27603.529845	31.218560
546.254346	27655.969265	31.223578
547.134607	27677.516467	31.228596
547.375683	27745.573801	31.233613
548.561801	27769.613183	31.238631
549.028059	27829.629777	31.243648
549.489893	27841.031852	31.248666
550.148439	27915.805941	31.253684
550.726538	27936.681532	31.258701
551.010238	27993.028873	31.263719
552.057804	28018.063694	31.268736
552.373632	28047.865014	31.273754
552.639076	28090.083116	31.278772
553.468491	28129.729746	31.283789
554.185395	28157.912156	31.288807
554.788496	28204.860645	31.293824
555.140279	28251.499491	31.298842
555.876332	28299.857837	31.303860
556.567230	28324.436262	31.308877
556.623215	28374.229922	31.313895
557.276016	28407.362914	31.318912
557.346294	28449.023714	31.323930
557.987252	28496.419259	31.328948
558.806426	28546.719032	31.333965
559.280062	28594.387335	31.338983
560.131590	28617.809228	31.344000
560.402268	28673.023316	31.349018
561.382160	28707.277192	31.354036
561.551411	28753.889835	31.359053
561.922542	28805.667371	31.364071
562.920455	28854.436341	31.369088
563.792400	28886.301572	31.374106
564.527127	28919.536023	31.379124
564.698154	28957.318248	31.384141
565.818376	28996.614987	31.389159
566.287158	29025.862706	31.394176
567.054436	29058.977226	31.399194
567.537909	29074.579398	31.404212
568.154465	29104.930423	31.409229
568.449626	29131.684697	31.414247
569.012767	29166.746563	31.419264
569.677113	29160.354762	31.424282
569.821028	29240.457318	31.429300
570.114494	29241.507281	31.434317
570.949250	29286.762678	31.439335
571.678759	29308.295114	31.444352
571.738078	29380.102499	31.449370
572.458280	29413.283550	31.454388
572.899821	29440.809241	31.459405
572.715992	29486.347200	31.464423
573.741101	29538.303412	31.469440
574.084705	29569.141597	31.474458
574.947465	29647.008986	31.479476
575.480850	29685.397052	31.484493
576.111106	29730.708323	31.489511
576.495433	29776.087258	31.494528
576.616794	29838.737274	31.499546
577.632108	29867.467671	31.504564
578.379871	29926.568649	31.509581
578.700277	29977.819053	31.514599
579.195204	30033.925525	31.519616
580.132361	30083.968596	31.524634
580.640534	30117.555198	31.529652
581.634851	30181.837234	31.534669
582.281457	30225.787271	31.539687
583.085849	30264.300586	31.544704
583.383007	30322.513464	31.549722
584.030349	30361.672939	31.554740
584.668425	30393.973951	31.559757
585.081517	30444.996735	31.564775
585.843447	30475.325597	31.569792
586.306791	30527.683337	31.574810
586.905115	30573.504770	31.579828
587.832830	30633.025648	31.584845
588.154953	30669.418280	31.589863
588.555454	30702.646585	31.594880
589.178348	30755.526504	31.599898
589.721644	30810.964466	31.604916
590.571118	30857.485828	31.609933
590.807737	30906.620200	31.614951
591.437665	30939.022879	31.619968
592.503916	31006.350972	31.624986
592.829500	31053.504779	31.630004
593.390510	31078.439039	31.635021
593.821218	31148.318043	31.640039
594.723303	31184.034753	31.645056
595.461865	31228.953128	31.650074
595.592967	31280.570313	31.655092
596.767025	31319.881452	31.660109
597.026116	31375.569903	31.665127
597.640260	31420.867956	31.670144
598.426395	31457.680163	31.675162
599.022480	31498.376135	31.680180
599.911607	31531.646508	31.685197
599.883889	31561.964470	31.690215
600.902408	31607.031574	31.695232
601.314412	31648.721781	31.700250
601.319184	31681.463487	31.705268
602.127905	31730.822851	31.710285
602.567926	31781.721011	31.715303
603.235321	31816.477260	31.720320
603.453724	31856.357981	31.725338
603.991871	31947.980984	31.730356
604.477622	31972.646478	31.735373
604.747474	32031.735056	31.740391
605.641273	32092.425080	31.745408
606.117558	32156.039296	31.750426
607.094336	32210.314418	31.755444
607.933431	32266.595973	31.760461
608.414180	32317.311207	31.765479
609.120618	32375.362177	31.770496
609.693564	32426.598946	31.775514
610.513081	32480.594241	31.780532
611.408731	32529.934287	31.785549
611.495351	32570.266438	31.790567
612.274728	32644.509480	31.795584
613.202921	32688.838975	31.800602
613.464697	32740.517167	31.805620
614.123065	32796.419520	31.810637
614.700363	32847.248682	31.815655
615.417558	32898.895820	31.820672
615.729206	32966.033764	31.825690
616.767173	33007.662404	31.830708
617.327014	33066.511491	31.835725
617.261530	33126.989286	31.840743
618.204215	33187.547899	31.845760
619.178671	33246.717766	31.850778
619.728941	33291.796301	31.855796
620.316257	33365.617658	31.860813
620.968736	33428.040751	31.865831
621.476557	33467.338637	31.870848
622.495948	33540.874446	31.875866
622.913465	33565.715552	31.880884
623.641129	33648.314373	31.885901
624.260941	33690.150046	31.890919
624.872320	33752.147442	31.895936
625.936603	33777.388690	31.900954
626.275721	33846.001212	31.905972
627.118409	33906.879459	31.910989
627.427483	33925.073915	31.916007
628.110344	34000.566348	31.921024
629.519780	34041.660835	31.926042
629.629774	34097.035451	31.931060
630.152958	34135.252723	31.936077
630.561923	34200.152884	31.941095
631.377378	34222.382734	31.946112
632.315989	34279.437164	31.951130
632.623586	34341.713713	31.956148
633.473767	34360.552307	31.961165
634.136640	34398.724298	31.966183
634.279891	34439.390897	31.971200
634.902865	34504.809880	31.976218
635.413771	34539.521142	31.981236
636.099465	34596.027395	31.986253
636.460664	34653.373688	31.991271
637.146583	34709.547684	31.996288
637.766569	34738.921830	32.001306
637.893154	34831.911101	32.006324
638.912979	34868.094716	32.011341
639.227451	34924.902390	32.016359
640.189976	34996.253119	32.021376
640.841371	35060.482758	32.026394
641.600305	35106.942291	32.031412
642.198325	35152.409235	32.036429
642.774053	35239.036320	32.041447
643.544058	35272.430974	32.046464
644.103938	35346.175668	32.051482
644.815181	35399.723252	32.056500
645.689428	35448.656105	32.061517
646.269420	35515.317092	32.066535
646.603972	35571.258319	32.071552
647.538212	35636.343702	32.076570
647.948442	35706.801739	32.081588
648.744700	35734.915226	32.086605
649.534433	35817.212281	32.091623
649.721469	35883.839579	32.096640
650.829924	35928.595199	32.101658
651.617335	35979.983805	32.106676
652.215720	36058.190065	32.111693
653.259955	36103.088806	32.116711
653.823020	36154.852619	32.121728
654.451567	36215.674117	32.126746
655.069741	36278.682507	32.131764
656.066657	36328.875374	32.136781
656.676918	36386.662496	32.141799
656.984230	36432.247016	32.146816
657.718303	36490.689526	32.151834
658.270826	36537.542214	32.156852
658.903530	36608.094746	32.161869
659.928974	36644.639211	32.166887
660.753975	36690.837246	32.171904
661.512164	36742.303798	32.176922
661.873670	36802.996538	32.181940
662.494920	36854.021736	32.186957
662.998470	36914.819962	32.191975
663.657379	36965.391761	32.196992
664.498465	37034.013153	32.202010
665.080002	37083.708449	32.207028
665.629217	37123.320549	32.212045
665.864767	37197.694203	32.217063
666.940950	37239.887084	32.222080
667.616993	37292.831478	32.227098
667.916112	37374.252602	32.232116
668.638020	37411.852950	32.237133
669.297021	37463.562966	32.242151
669.763741	37516.224501	32.247168
670.700404	37575.448913	32.252186
671.175263	37635.473894	32.257204
671.552034	37676.776519	32.262221
672.389791	37744.371812	32.267239
672.933916	37813.895061	32.272256
674.223420	37846.745464	32.277274
674.468905	37914.708512	32.282292
675.064445	37978.945644	32.287309
676.347098	38028.363391	32.292327
676.912794	38093.532788	32.297344
677.511518	38128.352628	32.302362
678.369283	38200.151537	32.307380
679.020728	38259.699697	32.312397
679.770751	38306.483307	32.317415
680.231279	38362.435860	32.322432
680.756410	38417.723984	32.327450
681.614950	38480.998787	32.332468
682.541397	38537.380698	32.337485
683.307863	38587.587073	32.342503
683.655996	38646.495875	32.347520
684.429918	38711.259245	32.352538
685.047629	38769.051802	32.357556
685.739435	38825.341170	32.362573
686.535679	38872.300315	32.367591
686.944621	38944.922812	32.372608
687.937067	39015.816042	32.377626
688.213480	39051.734498	32.382644
689.331261	39127.183975	32.387661
690.190999	39185.043483	32.392679
690.396490	39234.896460	32.397696
691.303694	39314.382145	32.402714
691.697015	39351.626036	32.407732
692.363955	39465.338473	32.412749
693.251515	39509.383553	32.417767
693.959900	39552.930628	32.422784
694.589365	39633.602061	32.427802
695.177434	39714.234741	32.432820
695.834732	39751.514742	32.437837
696.595011	39817.377254	32.442855
697.188063	39891.705844	32.447872
698.145210	39941.133730	32.452890
698.716303	40031.515463	32.457908
699.264031	40073.611955	32.462925
700.031384	40168.173348	32.467943
700.876205	40222.903987	32.472960
701.809871	40282.106840	32.477978
702.382571	40346.695628	32.482996
703.175473	40433.346413	32.488013
703.862859	40469.413734	32.493031
704.426400	40531.894813	32.498048
705.203234	40596.141396	32.503066
705.912830	40661.343493	32.508084
706.651145	40718.733998	32.513101
707.267087	40770.765333	32.518119
707.512309	40810.932793	32.523136
708.431888	40892.787693	32.528154
708.955779	40952.605319	32.533172
709.707519	41009.374933	32.538189
710.509260	41069.169229	32.543207
711.069040	41152.166019	32.548224
711.833312	41201.046388	32.553242
712.388067	41267.051316	32.558260
713.107996	41337.587625	32.563277
714.105218	41417.570286	32.568295
714.688426	41488.485382	32.573312
715.417757	41542.336620	32.578330
715.863336	41606.379550	32.583348
716.869316	41678.051307	32.588365
717.929943	41742.025204	32.593383
718.469566	41800.225290	32.598400
719.151438	41873.088068	32.603418
719.802111	41941.527851	32.608436
720.522547	42023.673778	32.613453
721.355672	42077.876047	32.618471
722.195804	42146.090930	32.623488
722.898521	42213.252420	32.628506
723.627076	42283.125740	32.633524
724.091555	42351.817594	32.638541
725.145886	42406.960307	32.643559
725.886543	42481.907498	32.648576
726.645190	42543.144211	32.653594
727.378990	42600.180603	32.658612
727.972301	42675.584219	32.663629
728.629160	42748.265446	32.668647
729.617518	42811.097257	32.673664
730.460020	42879.500777	32.678682
731.490521	42940.055319	32.683700
731.543331	42994.845240	32.688717
732.881002	43066.428989	32.693735
733.476214	43140.225674	32.698752
734.123791	43209.781304	32.703770
734.878706	43260.747709	32.708788
735.202765	43346.521097	32.713805
736.609404	43410.925586	32.718823
736.892956	43468.210029	32.723840
737.513047	43554.817376	32.728858
738.194619	43619.681907	32.733876
738.976181	43677.095941	32.738893
739.986152	43738.085553	32.743911
740.636043	43816.500730	32.748928
741.336980	43893.911346	32.753946
742.192238	43955.424753	32.758964
742.854678	44025.924476	32.763981
743.734072	44096.437261	32.768999
744.558808	44166.053710	32.774016
745.564989	44223.007949	32.779034
746.144502	44277.595057	32.784052
746.528359	44342.995490	32.789069
747.602742	44388.977610	32.794087
747.839204	44461.016915	32.799104
748.416251	44511.971171	32.804122
748.718792	44578.697715	32.809140
749.627470	44666.466555	32.814157
750.491586	44719.571277	32.819175
751.375139	44808.493091	32.824192
752.089253	44863.571655	32.829210
752.788635	44922.507640	32.834228
753.139837	45006.638237	32.839245
754.233293	45089.067454	32.844263
754.835638	45141.139420	32.849280
755.682606	45211.661907	32.854298
756.365405	45319.151793	32.859316
757.342856	45379.149188	32.864333
757.863473	45461.494709	32.869351
758.771294	45558.057136	32.874368
759.464304	45602.081032	32.879386
760.274241	45683.201681	32.884404
760.809670	45782.528233	32.889421
761.892782	45830.251052	32.894439
762.701935	45931.055462	32.899456
763.673682	46010.855268	32.904474
764.420597	46092.691371	32.909492
765.295078	46159.802988	32.914509
766.020654	46234.582697	32.919527
766.394787	46324.669151	32.924544
767.471959	46372.845546	32.929562
768.383761	46452.404526	32.934580
768.945424	46545.289017	32.939597
769.931739	46624.026113	32.944615
770.583500	46675.230356	32.949632
771.235760	46770.016641	32.954650
772.170777	46855.082245	32.959668
772.827618	46919.543425	32.964685
773.934424	46988.173471	32.969703
774.699199	47078.760043	32.974720
775.445027	47148.801668	32.979738
776.847557	47220.130385	32.984756
777.027901	47297.247792	32.989773
778.042168	47355.902092	32.994791
778.751258	47432.377481	32.999808
779.193472	47511.741543	33.004826
779.948730	47582.316601	33.009844
780.563505	47662.549911	33.014861
781.624027	47734.910087	33.019879
782.529881	47817.486171	33.024896
783.052151	47892.573505	33.029914
783.977605	47972.563154	33.034932
784.540724	48044.883894	33.039949
785.716261	48131.463418	33.044967
786.422791	48205.730809	33.049984
786.947159	48265.349585	33.055002
787.569379	48342.978628	33.060020
788.514480	48408.033577	33.065037
789.432066	48477.838603	33.070055
790.217697	48557.916274	33.075072
790.754778	48605.689419	33.080090
791.645869	48675.019846	33.085108
792.257461	48761.398800	33.090125
792.837611	48826.450285	33.095143
794.011417	48892.373027	33.100160
794.635866	48977.766539	33.105178
795.580063	49049.200886	33.110196
796.321767	49131.847121	33.115213
797.211516	49197.115735	33.120231
797.993732	49293.529390	33.125248
798.800816	49353.504410	33.130266
799.746528	49423.923998	33.135284
800.360781	49523.580987	33.140301
801.164266	49589.032015	33.145319
802.245502	49658.610554	33.150336
802.850321	49727.006181	33.155354
803.661273	49834.134099	33.160372
804.493175	49893.516926	33.165389
805.660257	49974.723592	33.170407
805.998532	50061.452163	33.175424
806.696463	50129.222350	33.180442
807.713610	50196.203589	33.185460
808.330510	50285.754122	33.190477
808.992799	50361.971953	33.195495
810.144862	50440.131715	33.200512
810.760009	50536.054886	33.205530
811.630770	50613.007416	33.210548
812.191152	50711.849717	33.215565
812.926172	50785.072566	33.220583
813.615537	50862.187583	33.225600
814.666568	50962.915986	33.230618
815.692010	51032.212154	33.235636
816.523364	51140.594333	33.240653
817.421297	51218.324608	33.245671
818.217575	51303.493664	33.250688
819.044175	51401.858762	33.255706
820.108036	51472.131960	33.260724
820.825038	51548.090534	33.265741
821.580620	51635.820668	33.270759
822.668500	51712.853833	33.275776
823.342685	51803.198120	33.280794
824.202738	51882.963346	33.285812
824.751627	51967.281841	33.290829
825.397163	52055.470208	33.295847
826.499351	52139.212283	33.300864
827.192253	52233.263906	33.305882
828.122876	52312.098290	33.310900
828.819313	52395.880901	33.315917
829.758468	52491.374803	33.320935
830.863200	52576.251494	33.325952
831.268497	52647.792364	33.330970
832.667699	52728.826285	33.335988
833.221525	52808.189906	33.341005
834.195375	52861.023959	33.346023
835.050925	52948.962364	33.351040
835.727522	53029.601385	33.356058
836.597109	53076.572990	33.361076
837.402965	53169.601600	33.366093
838.399147	53236.701720	33.371111
839.098446	53300.223015	33.376128
839.571436	53404.774998	33.381146
840.902519	53462.253382	33.386164
841.437764	53542.721518	33.391181
842.358087	53631.167389	33.396199
843.111209	53710.512728	33.401216
843.950883	53797.959129	33.406234
844.967769	53878.128010	33.411252
845.522449	53959.983627	33.416269
846.197723	54051.342690	33.421287
847.215643	54125.045438	33.426304
848.173782	54203.085195	33.431322
848.680972	54311.326608	33.436340
850.045650	54383.359217	33.441357
850.361528	54472.195781	33.446375
851.033816	54565.656837	33.451392
852.122216	54655.857958	33.456410
853.089040	54744.210333	33.461428
853.555985	54846.921993	33.466445
854.632833	54933.711170	33.471463
855.847072	55013.206611	33.476480
856.349116	55140.388871	33.481498
857.703149	55215.125199	33.486516
858.054570	55296.968693	33.491533
859.363037	55401.339237	33.496551
860.234864	55494.463977	33.501568
861.034317	55586.347593	33.506586
862.172301	55664.406042	33.511604
862.719528	55753.982222	33.516621
863.715011	55845.870667	33.521639
864.509537	55940.326255	33.526656
865.460645	56034.157666	33.531674
866.345517	56127.302500	33.536692
867.092921	56215.542265	33.541709
868.001788	56305.625463	33.546727
868.848797	56399.478474	33.551744
869.588952	56486.401236	33.556762
870.452548	56566.230731	33.561780
871.591656	56672.299049	33.566797
872.619019	56778.849797	33.571815
873.838974	56831.470016	33.576832
874.355651	56945.233965	33.581850
875.273551	57026.644647	33.586868
876.367147	57109.303049	33.591885
876.876444	57183.736786	33.596903
877.705388	57292.730696	33.601920
878.493595	57383.346634	33.606938
879.453261	57455.752591	33.611956
880.075332	57531.887085	33.616973
881.034923	57611.819498	33.621991
882.105766	57685.894411	33.627008
882.560740	57779.813717	33.632026
883.448510	57866.296501	33.637044
884.339560	57978.634022	33.642061
884.916616	58039.198567	33.647079
885.791071	58158.207181	33.652096
886.599173	58249.575560	33.657114
887.825196	58312.932627	33.662132
889.069121	58435.464200	33.667149
889.874381	58495.425671	33.672167
890.937802	58595.654634	33.677184
891.770248	58690.866534	33.682202
892.801779	58771.644919	33.687220
893.442298	58855.680801	33.692237
894.313509	58946.420646	33.697255
895.208408	59041.955904	33.702272
896.087743	59140.745924	33.707290
896.870845	59233.117621	33.712308
897.840113	59307.837159	33.717325
898.653179	59410.298251	33.722343
899.644624	59527.248075	33.727360
900.546903	59610.431176	33.732378
901.283307	59700.874136	33.737396
902.598847	59818.042574	33.742413
903.438539	59900.551823	33.747431
904.518867	59983.976625	33.752448
905.227835	60072.263059	33.757466
906.445515	60183.059120	33.762484
907.640032	60269.179113	33.767501
908.202063	60368.089299	33.772519
909.388184	60450.315372	33.777536
909.850466	60530.863643	33.782554
910.572664	60659.561290	33.787572
912.197701	60738.201511	33.792589
912.597478	60829.641253	33.797607
913.699608	60931.935264	33.802624
914.804850	61039.391692	33.807642
915.675174	61099.657487	33.812660
916.848523	61217.372007	33.817677
917.389403	61293.534855	33.822695
918.372586	61372.077814	33.827712
918.991748	61489.916970	33.832730
919.748227	61584.637930	33.837748
920.871234	61680.058845	33.842765
921.431655	61777.808458	33.847783
922.657284	61877.426187	33.852800
923.433382	61977.595929	33.857818
923.971691	62093.456158	33.862836
925.452922	62186.817581	33.867853
926.206020	62273.778031	33.872871
927.091205	62391.795225	33.877888
927.859545	62497.599024	33.882906
928.806686	62580.946085	33.887924
930.168304	62673.760582	33.892941
931.037981	62768.466335	33.897959
932.022160	62841.969291	33.902976
932.733095	62940.474625	33.907994
933.581046	63034.834665	33.913012
934.860174	63110.915815	33.918029
935.697230	63213.176013	33.923047
936.611991	63300.668082	33.928064
937.393390	63392.946893	33.933082
938.062717	63489.191252	33.938100
939.068361	63583.279470	33.943117
939.403896	63685.887284	33.948135
940.769689	63811.399911	33.953152
941.433394	63908.793601	33.958170
942.502953	64014.599010	33.963188
943.554743	64118.361507	33.968205
944.372269	64215.779664	33.973223
945.577398	64325.231594	33.978240
946.460589	64429.227884	33.983258
947.049924	64539.467472	33.988276
948.348706	64660.590985	33.993293
949.331325	64765.034359	33.998311
950.308551	64859.780820	34.003328
951.135286	64973.528465	34.008346
952.305339	65072.720272	34.013364
953.285673	65176.357797	34.018381
954.285693	65298.894045	34.023399
955.501420	65407.238854	34.028416
956.367689	65498.756429	34.033434
957.248901	65607.108226	34.038452
958.145595	65709.893460	34.043469
959.055707	65836.139371	34.048487
960.206091	65929.483455	34.053504
961.016480	66037.890016	34.058522
961.952466	66162.583268	34.063540
963.453855	66250.766171	34.068557
964.030962	66374.118788	34.073575
965.002957	66476.356083	34.078592
966.131204	66594.076433	34.083610
966.926150	66698.809735	34.088628
968.103682	66812.803055	34.093645
969.087800	66921.389096	34.098663
969.884326	67025.609110	34.103680
970.636582	67135.243936	34.108698
971.947681	67240.561326	34.113716
972.906971	67351.045640	34.118733
973.826710	67480.765640	34.123751
974.602610	67560.166261	34.128768
975.878363	67676.549512	34.133786
976.745033	67787.420605	34.138804
977.904314	67892.825725	34.143821
978.606227	67996.175325	34.148839
979.750395	68115.873372	34.153856
980.403337	68229.914312	34.158874
981.655529	68336.450476	34.163892
982.751595	68413.125157	34.168909
983.337949	68524.468326	34.173927
984.445411	68616.587759	34.178944
985.407995	68711.750369	34.183962
986.191868	68816.190517	34.188980
987.441802	68905.268947	34.193997
988.310605	69017.972469	34.199015
989.162939	69116.780817	34.204032
990.220496	69212.429850	34.209050
990.769869	69351.492232	34.214068
992.282924	69440.423853	34.219085
992.938421	69554.402663	34.224103
994.213376	69682.776280	34.229120
995.389618	69752.253999	34.234138
996.401382	69873.575994	34.239156
997.313503	69984.894635	34.244173
998.410107	70091.193504	34.249191
999.298405	70195.453848	34.254208
1000.171687	70319.390949	34.259226
1001.070581	70423.037986	34.264244
1002.200729	70537.780974	34.269261
1003.029986	70652.585141	34.274279
1003.915831	70779.119836	34.279296
1005.204702	70897.074496	34.284314
1005.909541	71017.214069	34.289332
1006.890414	71129.343306	34.294349
1007.875183	71252.238708	34.299367
1009.179629	71367.015676	34.304384
1010.369442	71480.920681	34.309402
1011.058700	71614.846458	34.314420
1012.177838	71730.994506	34.319437
1013.149237	71846.452769	34.324455
1014.446482	71973.460434	34.329472
1015.658730	72089.235631	34.334490
1016.380592	72205.272760	34.339508
1017.458946	72327.149018	34.344525
1018.768503	72440.509761	34.349543
1020.026500	72561.682802	34.354560
1020.808211	72672.835208	34.359578
1021.655065	72792.640746	34.364596
1023.172025	72894.742850	34.369613
1023.986371	73021.878305	34.374631
1024.986907	73132.821551	34.379648
1026.131048	73235.344892	34.384666
1027.143275	73369.938866	34.389684
1027.679636	73479.024327	34.394701
1028.451594	73596.394906	34.399719
1030.237848	73714.470511	34.404736
1031.151788	73829.601928	34.409754
1032.051099	73971.844949	34.414772
1033.276982	74089.443214	34.419789
1034.139328	74176.041641	34.424807
1035.041489	74320.789057	34.429824
1036.273914	74419.266521	34.434842
1037.293626	74533.399382	34.439860
1038.460439	74628.280049	34.444877
1039.529879	74731.265319	34.449895
1040.487632	74839.975216	34.454912
1041.473243	74930.551103	34.459930
1042.021861	75034.126332	34.464948
1043.326708	75154.410350	34.469965
1044.141151	75275.442965	34.474983
1045.327664	75376.365429	34.480000
1046.565965	75483.991476	34.485018
1047.598326	75603.158744	34.490036
1048.274020	75717.871277	34.495053
1049.239977	75834.004439	34.500071
1050.104782	75955.311198	34.505088
1051.596300	76073.049481	34.510106
1052.276218	76198.058852	34.515124
1053.197906	76316.521178	34.520141
1054.309261	76445.678735	34.525159
1054.902677	76567.866563	34.530176
1056.440804	76694.682679	34.535194
1057.257875	76832.238087	34.540212
1058.639886	76950.643544	34.545229
1059.347135	77077.505754	34.550247
1060.401254	77216.947347	34.555264
1061.893079	77351.693967	34.560282
1062.728956	77484.883632	34.565300
1064.318967	77587.547889	34.570317
1065.660952	77751.292640	34.575335
1066.106225	77856.105937	34.580352
1067.428311	77983.994689	34.585370
1068.602060	78135.463703	34.590388
1069.865075	78239.952966	34.595405
1070.765127	78372.891742	34.600423
1071.543611	78493.772352	34.605440
1073.146888	78618.479100	34.610458
1073.962204	78766.280730	34.615476
1074.773171	78857.110563	34.620493
1076.337919	79024.211599	34.625511
1077.576678	79133.481355	34.630528
1078.493188	79258.857470	34.635546
1080.259621	79387.088858	34.640564
1081.242937	79489.663264	34.645581
1082.256253	79599.875236	34.650599
1083.330304	79738.439666	34.655616
1084.632721	79855.680032	34.660634
1085.223601	79973.312366	34.665652
1086.458018	80094.237352	34.670669
1087.656971	80215.212936	34.675687
1088.502275	80336.871263	34.680704
1089.632823	80454.117095	34.685722
1090.606125	80581.856318	34.690740
1091.884173	80705.274779	34.695757
1092.991591	80836.009418	34.700775
1093.796889	80955.996330	34.705792
1094.982179	81068.154700	34.710810
1095.818159	81192.291152	34.715828
1096.738295	81311.155635	34.720845
1098.247081	81406.070435	34.725863
1099.157300	81556.038896	34.730880
1100.413713	81650.027787	34.735898
1101.418657	81762.060566	34.740916
1102.393270	81866.354966	34.745933
1103.522288	82032.418157	34.750951
1104.432311	82120.395610	34.755968
1105.650483	82274.258602	34.760986
1106.149300	82387.089593	34.766004
1107.038871	82505.466363	34.771021
1108.778522	82636.630167	34.776039
1109.300938	82784.722079	34.781056
1110.790400	82884.457568	34.786074
1111.735277	83080.226549	34.791092
1113.018210	83186.090586	34.796109
1114.284268	83308.900563	34.801127
1114.965242	83471.158491	34.806144
1116.776421	83589.198837	34.811162
1117.390734	83756.166816	34.816180
1118.527141	83875.447745	34.821197
1120.063325	83984.208986	34.826215
1121.267135	84115.625348	34.831232
1122.172461	84300.449393	34.836250
1123.180349	84399.042184	34.841268
1124.369636	84543.866684	34.846285
1125.710802	84683.338302	34.851303
1126.453700	84837.087070	34.856320
1127.953600	84926.265937	34.861338
1128.899391	85098.641744	34.866356
1130.080071	85264.621162	34.871373
1131.566544	85373.593486	34.876391
1132.796420	85494.095285	34.881408
1133.369807	85652.201573	34.886426
1135.152364	85760.300538	34.891444
1136.029907	85923.172006	34.896461
1137.159229	86039.254366	34.901479
1138.234190	86198.815053	34.906496
1139.805062	86331.350207	34.911514
1140.936155	86452.214591	34.916532
1141.600559	86600.924026	34.921549
1143.102356	86752.966291	34.926567
1144.200547	86867.534294	34.931584
1145.127168	87037.665258	34.936602
1146.027572	87139.462053	34.941620
1147.565661	87307.619973	34.946637
1148.547035	87416.449151	34.951655
1149.487493	87594.694933	34.956672
1151.176024	87707.896271	34.961690
1152.333894	87888.398925	34.966708
1152.960271	87998.488940	34.971725
1154.457648	88156.827259	34.976743
1155.832319	88287.426544	34.981760
1156.807261	88435.131850	34.986778
1157.592327	88554.330519	34.991796
1158.772238	88689.800677	34.996813
1159.883497	88813.198303	35.001831
1160.954858	88926.036274	35.006848
1162.309696	89099.150790	35.011866
1163.340741	89192.197284	35.016884
1164.349736	89359.430971	35.021901
1165.451176	89471.843323	35.026919
1166.510063	89605.510914	35.031936
1167.525473	89780.360663	35.036954
1168.892714	89891.563016	35.041972
1169.975680	90051.176349	35.046989
1171.453368	90179.139950	35.052007
1172.465095	90329.989027	35.057024
1173.605132	90489.039990	35.062042
1175.005657	90610.447730	35.067060
1175.554912	90790.015276	35.072077
1176.855708	90906.906133	35.077095
1178.538376	91038.212968	35.082112
1179.539572	91238.468352	35.087130
1180.487745	91376.382708	35.092148
1181.610798	91508.780604	35.097165
1183.221723	91679.705702	35.102183
1183.839004	91829.160608	35.107200
1185.517749	91965.324471	35.112218
1186.968202	92129.283741	35.117236
1187.819663	92302.630263	35.122253
1189.050715	92420.994949	35.127271
1190.504881	92597.309054	35.132288
1191.808371	92721.482512	35.137306
1192.820896	92885.599280	35.142324
1193.815179	93023.624169	35.147341
1195.527897	93187.600216	35.152359
1196.730771	93330.862426	35.157376
1197.786955	93513.534047	35.162394
1199.232841	93629.037499	35.167412
1200.260702	93803.379746	35.172429
1201.554996	93926.201568	35.177447
1202.685401	94100.896700	35.182464
1204.118484	94221.060530	35.187482
1205.074220	94412.692907	35.192500
1206.540643	94534.282617	35.197517
1207.691164	94727.999351	35.202535
1208.770609	94850.866774	35.207552
1210.023470	95018.686703	35.212570
1211.542118	95139.708461	35.217588
1212.494677	95335.631549	35.222605
1213.767960	95458.977531	35.227623
1214.918179	95592.091349	35.232640
1216.070503	95785.057901	35.237658
1216.997510	95907.917421	35.242676
1218.633032	96078.138778	35.247693
1220.059941	96233.896142	35.252711
1221.049282	96362.460325	35.257728
1222.304073	96540.532679	35.262746
1223.780209	96653.902557	35.267764
1224.735664	96805.430978	35.272781
1226.827024	96922.854138	35.277799
1227.272282	97077.495602	35.282816
1228.452427	97165.465986	35.287834
1229.367297	97334.052818	35.292852
1230.799888	97453.588827	35.297869
1231.984264	97598.848719	35.302887
1233.252247	97759.582545	35.307904
1234.387639	97885.785198	35.312922
1235.506159	98032.007259	35.317940
1236.685192	98189.759668	35.322957
1238.124648	98307.059607	35.327975
1239.262621	98485.659294	35.332992
1240.186572	98631.966761	35.338010
1241.762489	98751.455191	35.343028
1242.855095	98937.663616	35.348045
1243.737999	99068.955145	35.353063
1245.527095	99252.398282	35.358080
1246.571031	99396.831577	35.363098
1248.179582	99537.455975	35.368116
1249.271079	99718.021281	35.373133
1250.462922	99844.833164	35.378151
1251.701272	100034.696817	35.383168
1252.879244	100164.638079	35.388186
1254.386423	100336.607351	35.393204
1255.532644	100472.667107	35.398221
1256.904655	100657.263361	35.403239
1258.319712	100781.609066	35.408256
1259.090731	100970.725912	35.413274
1260.742086	101089.398360	35.418292
1261.939042	101282.809358	35.423309
1263.162354	101423.943110	35.428327
1264.592822	101590.568533	35.433344
1265.662681	101761.504369	35.438362
1267.430620	101882.927345	35.443380
1268.270091	102095.143245	35.448397
1269.833145	102221.073964	35.453415
1271.518462	102391.739423	35.458432
1272.286404	102547.334535	35.463450
1274.333984	102667.407380	35.468468
1274.921114	102867.648279	35.473485
1276.273836	103003.924183	35.478503
1277.865293	103169.193880	35.483520
1279.019910	103330.585754	35.488538
1280.458040	103464.256435	35.493556
1281.711170	103632.829289	35.498573
1283.095809	103794.428242	35.503591
1284.532395	103937.928877	35.508608
1285.290287	104103.938829	35.513626
1287.353785	104221.859339	35.518644
1288.495065	104418.437473	35.523661
1289.185560	104538.229436	35.528679
1290.801077	104710.580818	35.533696
1292.097599	104843.250393	35.538714
1293.285208	105003.091804	35.543732
1294.302420	105135.491019	35.548749
1295.679797	105258.854074	35.553767
1297.270758	105430.828597	35.558784
1298.108319	105543.033751	35.563802
1299.612647	105722.662332	35.568820
1300.670439	105838.175199	35.573837
1301.604995	106011.201197	35.578855
1302.888704	106135.020356	35.583872
1303.879597	106321.025492	35.588890
1305.488087	106464.134425	35.593908
1306.347819	106623.216163	35.598925
1307.366933	106795.569916	35.603943
1309.112451	106948.165462	35.608960
1309.927166	107132.831619	35.613978
1311.699076	107286.925021	35.618996
1312.759665	107465.763909	35.624013
1314.016349	107634.421595	35.629031
1315.676920	107795.908995	35.634048
1316.735168	108002.466168	35.639066
1318.645298	108140.220915	35.644084
1319.890385	108358.700427	35.649101
1320.763017	108513.862351	35.654119
1322.217137	108655.597533	35.659136
1323.627207	108861.011203	35.664154
1325.116545	109006.331443	35.669172
1326.729117	109203.671497	35.674189
1327.878946	109358.206155	35.679207
1329.428538	109505.697067	35.684224
1330.704122	109723.291614	35.689242
1332.240415	109874.907271	35.694260
1333.595376	110059.484600	35.699277
1334.935531	110207.145976	35.704295
1336.522854	110399.651392	35.709312
1337.523098	110575.642916	35.714330
1339.181065	110734.764078	35.719348
1340.259683	110889.762837	35.724365
1341.350365	111088.346772	35.729383
1343.214859	111248.824645	35.734400
1344.291704	111417.081449	35.739418
1345.725775	111611.272812	35.744436
1347.121635	111765.042993	35.749453
1348.433254	111964.212876	35.754471
1350.099636	112120.708444	35.759488
1351.517105	112295.626843	35.764506
1352.487156	112494.678058	35.769524
1353.663639	112644.469014	35.774541
1355.109428	112806.852980	35.779559
1356.750240	112993.571802	35.784576
1357.777218	113191.182611	35.789594
1359.509418	113332.894334	35.794612
1360.554107	113498.758585	35.799629
1362.110088	113673.702667	35.804647
1363.730159	113895.704222	35.809664
1364.577894	114060.020912	35.814682
1366.043524	114175.223638	35.819700
1367.322029	114362.409128	35.824717
1368.295675	114553.746674	35.829735
1369.900763	114687.845315	35.834752
1371.040057	114865.788703	35.839770
1372.508832	115043.155535	35.844788
1373.939313	115184.539547	35.849805
1374.731004	115386.250417	35.854823
1376.847645	115536.662648	35.859840
1377.640386	115726.296894	35.864858
1379.155900	115893.602560	35.869876
1380.426573	116067.507101	35.874893
1381.836425	116260.086115	35.879911
1383.159964	116459.112644	35.884928
1384.512911	116607.417775	35.889946
1386.176445	116772.078323	35.894964
1387.468818	116993.032318	35.899981
1388.410817	117201.647381	35.904999
1390.298341	117377.210266	35.910016
1391.501250	117566.729745	35.915034
1392.889923	117728.489769	35.920052
1394.348683	117908.448766	35.925069
1396.211333	118074.814551	35.930087
1398.002058	118267.905371	35.935104
1399.048226	118461.755463	35.940122
1400.391193	118678.049628	35.945140
1401.517732	118844.214480	35.950157
1403.367332	119016.907408	35.955175
1404.999383	119248.229791	35.960192
1406.104018	119438.367544	35.965210
1407.503990	119618.537798	35.970228
1408.839571	119783.054522	35.975245
1410.800176	119942.432769	35.980263
1412.035072	120170.445279	35.985280
1412.664938	120346.095325	35.990298
1414.361551	120531.157394	35.995316
1416.327799	120693.262129	36.000333
1417.450904	120906.944037	36.005351
1419.131134	121141.068091	36.010368
1420.534648	121315.487245	36.015386
1421.757510	121491.342035	36.020404
1423.426412	121677.119510	36.025421
1424.684618	121894.777366	36.030439
1426.287849	122047.057028	36.035456
1427.920947	122241.380267	36.040474
1429.459244	122469.826860	36.045492
1430.704795	122641.772249	36.050509
1431.964961	122812.019302	36.055527
1433.580623	123021.118652	36.060544
1434.556433	123218.086588	36.065562
1436.146264	123395.820901	36.070580
1437.291499	123622.072786	36.075597
1438.670650	123790.407377	36.080615
1440.202702	123995.727999	36.085632
1441.629365	124219.014447	36.090650
1443.128692	124368.132177	36.095668
1444.691909	124578.316042	36.100685
1445.830151	124734.826823	36.105703
1447.625625	124936.705639	36.110720
1448.749477	125107.635006	36.115738
1449.770969	125281.393655	36.120756
1451.676464	125439.230585	36.125773
1452.943004	125691.776193	36.130791
1454.075432	125854.741691	36.135808
1454.907471	126049.435321	36.140826
1457.265216	126216.122300	36.145844
1458.942891	126411.646837	36.150861
1459.863452	126659.848394	36.155879
1461.435806	126820.001061	36.160896
1462.959255	127017.137854	36.165914
1464.463829	127222.474787	36.170932
1466.079654	127432.621849	36.175949
1467.955922	127621.511179	36.180967
1469.244966	127838.997076	36.185984
1470.877025	128010.408700	36.191002
1472.365501	128233.477797	36.196020
1474.185030	128389.610073	36.201037
1475.446067	128640.967815	36.206055
1476.926058	128799.588615	36.211072
1478.886645	128997.189602	36.216090
1480.199820	129227.832124	36.221108
1481.438673	129395.881794	36.226125
1483.267982	129577.647148	36.231143
1484.378034	129815.205752	36.236160
1485.958726	129996.645976	36.241178
1487.666283	130161.750062	36.246196
1489.133450	130404.425753	36.251213
1490.316019	130584.830899	36.256231
1492.135160	130789.637686	36.261248
1493.470815	131009.978963	36.266266
1494.970917	131197.292888	36.271284
1496.161190	131423.703670	36.276301
1498.116447	131587.129843	36.281319
1499.560715	131825.070533	36.286336
1500.983627	132012.414836	36.291354
1502.608892	132225.117974	36.296372
1504.362992	132405.520043	36.301389
1505.405124	132636.689888	36.306407
1507.037411	132855.566814	36.311424
1508.516514	133037.182231	36.316442
1509.977931	133228.899598	36.321460
1512.100425	133447.069705	36.326477
1512.830357	133667.692695	36.331495
1514.481099	133838.326258	36.336512
1515.973059	134074.301705	36.341530
1517.717156	134293.070566	36.346548
1519.667871	134459.567625	36.351565
1520.556169	134712.217303	36.356583
1522.000609	134923.689617	36.361600
1523.438498	135094.947345	36.366618
1525.450859	135277.810052	36.371636
1526.634411	135510.551878	36.376653
1527.643366	135696.300922	36.381671
1529.857588	135858.962901	36.386688
1531.285860	136064.135917	36.391706
1532.087695	136293.700851	36.396724
1534.400491	136455.172086	36.401741
1535.122404	136683.219554	36.406759
1536.678787	136851.719139	36.411776
1538.092538	137108.753977	36.416794
1539.159068	137307.150518	36.421812
1541.060290	137496.507477	36.426829
1542.840730	137720.859423	36.431847
1544.186275	137956.839092	36.436864
1545.975533	138130.732688	36.441882
1547.734241	138385.645688	36.446900
1549.290104	138582.439763	36.451917
1550.871795	138785.972770	36.456935
1552.260196	139044.511237	36.461952
1553.813299	139222.035108	36.466970
1555.411188	139436.430432	36.471988
1557.298825	139682.070384	36.477005
1558.853042	139871.016148	36.482023
1559.913858	140105.005170	36.487040
1561.497961	140348.468391	36.492058
1563.197027	140546.646768	36.497076
1564.963381	140753.813772	36.502093
1566.334591	141039.277579	36.507111
1567.833928	141244.640076	36.512128
1569.825058	141434.768297	36.517146
1571.028025	141708.808303	36.522164
1572.710138	141928.543690	36.527181
1574.135542	142145.051604	36.532199
1576.235505	142352.607509	36.537216
1578.047490	142612.376829	36.542234
1579.511150	142830.505829	36.547252
1581.573244	143046.627520	36.552269
1582.781376	143248.589797	36.557287
1584.310424	143508.399022	36.562304
1585.920858	143719.286646	36.567322
1587.822981	143921.409281	36.572340
1589.363945	144186.811842	36.577357
1590.628194	144427.810994	36.582375
1592.336892	144631.236494	36.587392
1594.104688	144843.070110	36.592410
1595.660978	145042.618646	36.597428
1597.176541	145264.242309	36.602445
1599.023571	145535.235577	36.607463
1600.295763	145738.953166	36.612480
1602.751885	145920.099286	36.617498
1604.157939	146167.718652	36.622516
1605.653085	146419.204555	36.627533
1606.993418	146613.372307	36.632551
1608.804731	146823.437889	36.637568
1610.355137	147075.579413	36.642586
1611.571469	147270.531473	36.647604
1613.921473	147428.100602	36.652621
1615.352883	147661.061588	36.657639
1616.712030	147881.435649	36.662656
1618.227477	148042.284097	36.667674
1619.669659	148280.698711	36.672692
1621.326632	148481.305262	36.677709
1622.520771	148681.542917	36.682727
1624.538717	148875.794401	36.687744
1626.115704	149130.128410	36.692762
1627.323797	149315.498092	36.697780
1628.808226	149555.779000	36.702797
1630.817189	149755.741831	36.707815
1631.709882	150014.894679	36.712832
1633.649164	150215.124973	36.717850
1635.538440	150451.494425	36.722868
1636.557270	150699.983895	36.727885
1638.248624	150906.507754	36.732903
1639.971681	151190.258999	36.737920
1641.252626	151403.709720	36.742938
1643.135785	151642.713073	36.747956
1644.803217	151907.323464	36.752973
1646.926196	152128.987151	36.757991
1648.286654	152398.772117	36.763008
1649.938184	152608.850218	36.768026
1651.336433	152860.490716	36.773044
1652.784099	153124.702081	36.778061
1655.095729	153363.307591	36.783079
1656.754008	153636.465841	36.788096
1658.957681	153851.510161	36.793114
1660.991898	154093.334611	36.798132
1662.089456	154335.740654	36.803149
1664.249127	154566.759054	36.808167
1665.640044	154794.427136	36.813184
1667.550550	155049.007731	36.818202
1669.249617	155282.956988	36.823220
1671.041000	155502.946169	36.828237
1672.516740	155773.361451	36.833255
1674.782867	155992.809298	36.838272
1676.107058	156236.194713	36.843290
1677.504448	156459.232348	36.848308
1679.232288	156719.256003	36.853325
1681.318790	156919.592211	36.858343
1682.766627	157203.958260	36.863360
1684.398060	157419.166956	36.868378
1686.332441	157638.031428	36.873396
1687.915302	157892.178186	36.878413
1689.517889	158168.564606	36.883431
1691.433117	158374.401651	36.888448
1693.050068	158617.935027	36.893466
1694.456868	158866.093784	36.898484
1696.263961	159108.750829	36.903501
1698.017628	159342.465586	36.908519
1699.879784	159554.493494	36.913536
1701.590846	159834.236322	36.918554
1703.048789	160051.581259	36.923572
1704.916851	160243.614791	36.928589
1706.609501	160488.100278	36.933607
1707.927918	160692.409954	36.938624
1709.995252	160902.067442	36.943642
1711.517111	161164.769460	36.948660
1713.127346	161360.590982	36.953677
1714.970318	161593.355440	36.958695
1716.514382	161834.919085	36.963712
1718.198770	162041.308909	36.968730
1719.613849	162304.061671	36.973748
1721.232764	162505.506068	36.978765
1723.166038	162752.999872	36.983783
1724.609955	163029.842823	36.988800
1726.083965	163231.961083	36.993818
1727.899293	163502.572587	36.998836
1729.347807	163761.995322	37.003853
1731.183258	164008.397254	37.008871
1732.672947	164302.896320	37.013888
1734.571461	164556.191129	37.018906
1736.003614	164794.621787	37.023924
1737.716244	165050.460673	37.028941
1740.025878	165305.103157	37.033959
1741.832469	165583.696218	37.038976
1743.844512	165860.635360	37.043994
1745.210770	166093.605924	37.049012
1747.206266	166365.922213	37.054029
1749.106312	166653.234419	37.059047
1750.683852	166928.525634	37.064064
1752.504370	167180.062526	37.069082
1754.493960	167434.833896	37.074100
1756.497847	167660.546912	37.079117
1758.196218	167947.748897	37.084135
1759.809102	168244.136930	37.089152
1761.513929	168492.466654	37.094170
1763.172920	168736.442053	37.099188
1765.140776	168987.802748	37.104205
1766.994501	169296.096329	37.109223
1767.950747	169551.883198	37.114240
1770.444573	169799.512720	37.119258
1772.100975	170109.658033	37.124276
1773.494925	170369.439830	37.129293
1776.215085	170601.982262	37.134311
1777.751308	170913.129831	37.139328
1780.023794	171187.986417	37.144346
1781.323138	171449.756613	37.149364
1783.668813	171687.058371	37.154381
1785.290397	171973.909511	37.159399
1787.262908	172202.635247	37.164416
1789.145169	172468.226691	37.169434
1790.775897	172754.993300	37.174452
1792.681979	172980.233015	37.179469
1794.513419	173239.786887	37.184487
1795.976536	173554.696535	37.189504
1798.062010	173799.980733	37.194522
1799.463496	174028.338347	37.199540
1801.297608	174248.002364	37.204557
1802.939447	174531.849672	37.209575
1804.420416	174760.287647	37.214592
1806.043457	174991.990000	37.219610
1807.383867	175292.547059	37.224628
1808.886186	175522.863488	37.229645
1811.458728	175756.791772	37.234663
1812.533943	176057.003337	37.239680
1814.322987	176339.051221	37.244698
1816.102525	176582.155461	37.249716
1817.556827	176902.154504	37.254733
1819.522881	177165.061509	37.259751
1820.758392	177436.078735	37.264768
1823.188354	177703.279720	37.269786
1824.860497	177995.075530	37.274804
1826.751281	178336.203317	37.279821
1828.741920	178588.166678	37.284839
1830.467268	178912.464473	37.289856
1832.503538	179176.096227	37.294874
1834.700092	179473.832821	37.299892
1836.140983	179770.435435	37.304909
1838.142231	180068.651284	37.309927
1840.249963	180352.109459	37.314944
1841.795545	180690.748249	37.319962
1843.489320	180977.498946	37.324980
1845.066353	181254.272142	37.329997
1847.917270	181533.902667	37.335015
1849.588450	181825.217546	37.340032
1851.578561	182130.719711	37.345050
1854.158723	182461.278192	37.350068
1855.800696	182740.474024	37.355085
1857.908378	182994.056228	37.360103
1859.710889	183324.440177	37.365120
1861.643371	183595.182963	37.370138
1864.074829	183850.812316	37.375156
1865.737656	184185.564370	37.380173
1867.862434	184456.979787	37.385191
1869.292839	184709.245545	37.390208
1871.194446	185019.552811	37.395226
1873.174888	185277.533272	37.400244
1874.905662	185594.622143	37.405261
1877.085030	185855.619710	37.410279
1879.022599	186167.528018	37.415296
1880.852651	186449.851514	37.420314
1882.335071	186719.200008	37.425332
1884.581590	187010.952493	37.430349
1886.281690	187312.665992	37.435367
1888.329549	187566.397794	37.440384
1889.874666	187866.984781	37.445402
1892.327257	188187.733243	37.450420
1893.959794	188470.240105	37.455437
1895.956241	188716.347115	37.460455
1897.315691	189048.074102	37.465472
1899.558021	189294.424310	37.470490
1901.361213	189585.628877	37.475508
1903.236967	189837.128847	37.480525
1904.809791	190124.617013	37.485543
1906.724940	190358.131419	37.490560
1908.562339	190623.765972	37.495578
1910.407855	190946.101700	37.500596
1911.806467	191200.121181	37.505613
1913.940991	191490.942182	37.510631
1916.078080	191753.083584	37.515648
1917.750684	192059.882756	37.520666
1919.591108	192315.602001	37.525684
1921.150970	192619.960582	37.530701
1922.997308	192939.492087	37.535719
1924.417696	193230.957176	37.540736
1927.003205	193511.070870	37.545754
1928.953353	193853.017076	37.550772
1930.451903	194127.443429	37.555789
1932.690174	194411.945062	37.560807
1934.382766	194770.221475	37.565824
1936.565723	195056.004697	37.570842
1938.904515	195371.057038	37.575860
1940.255912	195690.925901	37.580877
1942.527429	195983.122311	37.585895
1944.488525	196310.741822	37.590912
1946.113116	196631.258592	37.595930
1948.480991	196941.683490	37.600948
1950.696333	197245.902657	37.605965
1952.419568	197587.986253	37.610983
1954.467115	197868.145994	37.616000
1956.472211	198215.786257	37.621018
1958.571012	198543.309207	37.626036
1960.634259	198855.773882	37.631053
1962.691102	199155.003107	37.636071
1964.812282	199493.532831	37.641088
1966.676670	199789.876872	37.646106
1968.809541	200110.803905	37.651124
1970.559608	200441.859028	37.656141
1972.822011	200745.012007	37.661159
1975.072184	201061.166243	37.666176
1976.896980	201385.424530	37.671194
1979.320086	201683.327702	37.676212
1980.797386	201995.294332	37.681229
1983.282341	202307.762877	37.686247
1984.964766	202626.643747	37.691264
1986.883702	202936.552749	37.696282
1989.417017	203235.614598	37.701300
1991.248937	203562.473993	37.706317
1993.379571	203871.922999	37.711335
1995.604044	204166.062906	37.716352
1997.260302	204495.024645	37.721370
1999.437262	204792.881916	37.726388
2001.401498	205099.787164	37.731405
2003.583556	205399.360455	37.736423
2005.773663	205734.667741	37.741440
2007.229276	206014.734507	37.746458
2009.358783	206295.241537	37.751476
2011.550001	206570.586267	37.756493
2013.682100	206860.336989	37.761511
2015.381494	207144.229537	37.766528
2017.271591	207414.649810	37.771546
2019.233937	207721.759552	37.776564
2021.463630	207974.521259	37.781581
2023.204809	208296.623197	37.786599
2025.081710	208564.841910	37.791616
2026.802931	208887.419871	37.796634
2028.939685	209171.773110	37.801652
2030.694061	209474.672028	37.806669
2032.499636	209773.413087	37.811687
2034.503417	210106.425939	37.816704
2036.468218	210416.468759	37.821722
2038.667120	210707.039798	37.826740
2040.532304	211050.591236	37.831757
2042.619605	211376.666071	37.836775
2044.801628	211668.729586	37.841792
2046.537900	212001.287153	37.846810
2048.781819	212329.652596	37.851828
2051.277915	212640.434565	37.856845
2052.981422	212980.492748	37.861863
2055.095342	213319.433867	37.866880
2057.131662	213644.157214	37.871898
2059.549548	213969.215205	37.876916
2061.283462	214301.950017	37.881933
2063.391351	214647.145293	37.886951
2065.877747	214968.731364	37.891968
2067.417736	215304.967954	37.896986
2069.734241	215635.293630	37.902004
2071.479764	215984.260534	37.907021
2073.720355	216320.873481	37.912039
2076.072449	216650.335109	37.917056
2078.027950	216990.449954	37.922074
2080.453823	217330.796563	37.927092
2082.671108	217673.120485	37.932109
2084.659005	218010.353094	37.937127
2086.757724	218354.527449	37.942144
2089.038897	218684.213094	37.947162
2091.059523	219020.543870	37.952180
2093.293368	219363.584364	37.957197
2095.597023	219684.903911	37.962215
2097.430980	220049.163952	37.967232
2099.662345	220365.038332	37.972250
2101.854797	220696.385145	37.977268
2103.531264	221065.487368	37.982285
2105.908933	221396.287357	37.987303
2108.187038	221728.069590	37.992320
2110.529202	222070.496072	37.997338
2112.773414	222405.232414	38.002356
2114.651990	222732.168599	38.007373
2116.748986	223094.700330	38.012391
2118.759291	223465.437357	38.017408
2120.634241	223804.860236	38.022426
2122.691775	224124.053849	38.027444
2125.131342	224423.875134	38.032461
2126.712836	224746.981453	38.037479
2129.235094	225049.204538	38.042496
2131.378304	225378.827106	38.047514
2133.061983	225691.610471	38.052532
2135.270270	226007.994197	38.057549
2137.201459	226331.686293	38.062567
2139.412714	226658.624004	38.067584
2141.134614	227004.535231	38.072602
2143.384789	227320.536416	38.077620
2145.630379	227651.015333	38.082637
2147.244731	227999.449247	38.087655
2149.930191	228340.095780	38.092672
2152.156504	228681.299033	38.097690
2154.162629	229023.198873	38.102708
2156.314391	229368.556304	38.107725
2158.203716	229713.880535	38.112743
2160.444245	230069.258367	38.117760
2162.293767	230420.839302	38.122778
2164.691455	230773.502936	38.127796
2166.760633	231135.972570	38.132813
2168.842568	231500.955955	38.137831
2171.290331	231862.606509	38.142848
2173.234884	232234.802052	38.147866
2175.539536	232599.906838	38.152884
2177.837114	232968.950803	38.157901
2179.960150	233336.703206	38.162919
2182.564371	233701.942509	38.167936
2184.529247	234080.364552	38.172954
2186.851378	234432.393613	38.177972
2188.937081	234810.265960	38.182989
2191.010222	235181.081026	38.188007
2193.565017	235551.846476	38.193024
2195.756402	235924.804395	38.198042
2197.927319	236293.347584	38.203060
2200.285195	236665.088067	38.208077
2202.559550	237051.371193	38.213095
2205.014816	237415.784081	38.218112
2207.115863	237800.167133	38.223130
2209.348757	238154.204276	38.228148
2211.638233	238523.447647	38.233165
2213.751231	238905.470632	38.238183
2216.085879	239256.218732	38.243200
2218.373616	239632.654087	38.248218
2220.640787	240009.805151	38.253236
2223.177686	240382.495184	38.258253
2225.593417	240749.541543	38.263271
2227.917982	241099.103170	38.268288
2229.890324	241481.080945	38.273306
2232.736965	241840.010680	38.278324
2235.061511	242212.232229	38.283341
2237.195795	242556.418149	38.288359
2239.413169	242920.505483	38.293376
2241.850230	243253.240733	38.298394
2244.002001	243597.274387	38.303412
2246.100566	243909.871935	38.308429
2248.311553	244248.386121	38.313447
2250.187380	244567.218271	38.318464
2252.227922	244906.853428	38.323482
2254.321721	245247.446238	38.328500
2256.514917	245582.004229	38.333517
2258.449433	245926.103906	38.338535
2260.782864	246280.022062	38.343552
2263.110258	246623.222975	38.348570
2265.123680	246973.764555	38.353588
2267.481505	247336.394013	38.358605
2269.334887	247697.173914	38.363623
2271.780886	248062.763140	38.368640
2273.966908	248425.498784	38.373658
2276.187728	248797.247199	38.378676
2278.653100	249172.945745	38.383693
2280.607745	249547.532345	38.388711
2282.845462	249914.429173	38.393728
2285.447213	250296.154344	38.398746
2287.633577	250680.562645	38.403764
2289.798544	251062.562115	38.408781
2292.171905	251450.371789	38.413799
2294.803794	251829.733444	38.418816
2297.518396	252205.983834	38.423834
2299.810160	252588.677928	38.428852
2302.328029	252950.380547	38.433869
2304.404772	253329.376288	38.438887
2307.129329	253710.810299	38.443904
2309.388350	254087.314739	38.448922
2311.739309	254466.040738	38.453940
2314.462204	254842.142918	38.458957
2316.295713	255227.938028	38.463975
2318.765678	255588.586484	38.468992
2320.990192	255987.174555	38.474010
2323.360880	256365.647068	38.479028
2325.958032	256749.444245	38.484045
2327.888585	257133.068379	38.489063
2330.258225	257519.570251	38.494080
2332.951466	257897.613299	38.499098
2335.055051	258294.726097	38.504116
2337.547778	258674.453384	38.509133
2339.838722	259072.655513	38.514151
2342.299986	259442.863065	38.519168
2344.622018	259845.837211	38.524186
2346.848429	260228.581248	38.529204
2349.599358	260608.295983	38.534221
2351.822403	260999.399164	38.539239
2353.989744	261392.061307	38.544256
2356.855357	261780.904492	38.549274
2359.145719	262157.493629	38.554292
2361.398850	262536.324601	38.559309
2363.539030	262927.392743	38.564327
2366.302098	263302.384191	38.569344
2368.991149	263669.919344	38.574362
2371.262926	264034.498102	38.579380
2373.728646	264377.733385	38.584397
2375.366416	264729.229226	38.589415
2377.857153	265083.943393	38.594432
2379.965817	265433.434626	38.599450
2382.274115	265780.405025	38.604468
2384.684967	266155.988783	38.609485
2386.653425	266523.564813	38.614503
2389.256596	266881.615967	38.619520
2391.583237	267254.064043	38.624538
2393.568241	267643.510508	38.629556
2396.040715	268006.511466	38.634573
2397.995846	268393.321317	38.639591
2400.406967	268796.418862	38.644608
2402.775934	269180.521726	38.649626
2405.055333	269563.216450	38.654644
2407.530817	269972.528391	38.659661
2409.492119	270375.850691	38.664679
2411.982213	270791.232189	38.669696
2414.594541	271199.227560	38.674714
2417.306904	271617.267002	38.679732
2419.811806	272021.062822	38.684749
2422.206719	272436.917438	38.689767
2424.764541	272844.261651	38.694784
2427.520321	273275.453806	38.699802
2429.690273	273681.869013	38.704820
2432.202822	274086.324754	38.709837
2434.532830	274504.222507	38.714855
2437.294068	274916.259995	38.719872
2440.049608	275330.787966	38.724890
2442.123350	275756.703148	38.729908
2444.964506	276174.545437	38.734925
2447.456199	276594.246751	38.739943
2450.136970	277000.149420	38.744960
2452.880867	277415.923972	38.749978
2455.207948	277828.893942	38.754996
2458.108111	278240.147188	38.760013
2460.234934	278650.379758	38.765031
2463.114953	279064.887630	38.770048
2465.518938	279465.829205	38.775066
2467.456345	279875.024477	38.780084
2470.367618	280285.487831	38.785101
2472.947853	280707.231754	38.790119
2475.287831	281116.235672	38.795136
2477.960746	281533.112451	38.800154
2480.395075	281935.953376	38.805172
2483.055675	282349.198956	38.810189
2485.246982	282771.613018	38.815207
2488.000043	283165.359095	38.820224
2490.704771	283581.264182	38.825242
2492.883618	283992.197050	38.830260
2495.500700	284410.020611	38.835277
2498.201300	284819.955594	38.840295
2500.602087	285219.954289	38.845312
2503.104267	285617.421646	38.850330
2505.145493	286005.689547	38.855348
2508.095125	286384.998252	38.860365
2510.117896	286766.409509	38.865383
2512.581099	287150.214680	38.870400
2515.082996	287526.646447	38.875418
2517.085124	287922.666495	38.880436
2519.630856	288301.478357	38.885453
2521.805086	288693.380353	38.890471
2524.409806	289097.813481	38.895488
2526.677846	289509.996499	38.900506
2529.033998	289909.209558	38.905524
2531.373870	290331.287151	38.910541
2534.077991	290750.842334	38.915559
2536.568057	291171.472310	38.920576
2538.970512	291587.593839	38.925594
2541.248185	292033.049097	38.930612
2543.853741	292461.203274	38.935629
2546.744216	292895.357366	38.940647
2549.277875	293324.004075	38.945664
2551.783774	293763.577448	38.950682
2554.245143	294197.035062	38.955700
2557.049399	294635.467168	38.960717
2559.604940	295086.232509	38.965735
2562.169550	295531.457779	38.970752
2564.864966	295965.255798	38.975770
2567.545071	296423.593766	38.980788
2570.324849	296851.508629	38.985805
2572.724379	297294.952624	38.990823
2575.717360	297750.926327	38.995840
2578.531912	298188.256814	39.000858
2580.698915	298639.583654	39.005876
2583.776870	299076.387639	39.010893
2586.420624	299528.627362	39.015911
2588.860514	299973.861958	39.020928
2591.720234	300408.792044	39.025946
2594.166604	300865.606368	39.030964
2597.012479	301311.712930	39.035981
2599.595604	301751.966775	39.040999
2602.269513	302204.016606	39.046016
2605.418427	302642.806646	39.051034
2607.690282	303088.414880	39.056052
2610.633544	303519.233615	39.061069
2613.406411	303961.000516	39.066087
2615.797341	304401.937558	39.071104
2618.637182	304834.851669	39.076122
2621.375383	305286.323100	39.081140
2623.668041	305731.488090	39.086157
2626.537226	306167.695497	39.091175
2628.843865	306604.320825	39.096192
2631.567087	307050.734086	39.101210
2634.011299	307499.577662	39.106228
2636.878166	307938.421233	39.111245
2639.754588	308381.630609	39.116263
2642.072426	308826.044519	39.121280
2644.784259	309257.059442	39.126298
2646.898423	309685.983142	39.131316
2649.558708	310099.680535	39.136333
2652.118843	310510.268200	39.141351
2654.875474	310923.109277	39.146368
2657.477023	311343.593318	39.151386
2659.748320	311762.832773	39.156404
2662.322698	312189.032892	39.161421
2664.804420	312621.367293	39.166439
2667.016992	313061.692581	39.171456
2670.096149	313498.119777	39.176474
2672.494586	313945.041215	39.181492
2674.959840	314388.902352	39.186509
2677.677981	314839.604629	39.191527
2680.260207	315294.491871	39.196544
2682.871021	315744.267496	39.201562
2685.619607	316209.105963	39.206580
2688.212426	316682.576984	39.211597
2690.681138	317156.065426	39.216615
2693.388174	317634.136296	39.221632
2696.449569	318105.367467	39.226650
2698.909596	318585.403034	39.231668
2701.637554	319072.682877	39.236685
2704.497357	319549.043800	39.241703
2707.211396	320033.857317	39.246720
2709.976622	320504.336146	39.251738
2712.600440	321016.029063	39.256756
2715.100338	321498.049671	39.261773
2718.240588	322001.909119	39.266791
2720.482166	322499.203320	39.271808
2723.586621	322983.126439	39.276826
2726.715288	323479.868204	39.281844
2729.258238	323975.252279	39.286861
2732.386392	324480.496049	39.291879
2734.870836	324979.692920	39.296896
2737.748667	325476.208728	39.301914
2740.781521	325970.512967	39.306932
2743.839610	326464.835613	39.311949
2746.543372	326957.205121	39.316967
2749.118870	327470.822271	39.321984
2752.158182	327943.273522	39.327002
2755.248052	328450.530262	39.332020
2757.845932	328933.025612	39.337037
2760.922289	329416.584917	39.342055
2763.623453	329931.613400	39.347072
2766.871080	330402.264371	39.352090
2769.395594	330887.501502	39.357108
2772.209939	331380.790206	39.362125
2775.660481	331867.016983	39.367143
2778.261192	332355.279618	39.372160
2780.765673	332826.210538	39.377178
2783.444080	333306.988774	39.382196
2786.275902	333792.437173	39.387213
2789.258755	334280.549955	39.392231
2792.109345	334760.910124	39.397248
2794.701425	335220.892345	39.402266
2796.960482	335695.194712	39.407284
2800.038203	336133.789752	39.412301
2803.197203	336570.693214	39.417319
2805.232028	337031.589379	39.422336
2808.427700	337480.059773	39.427354
2811.085650	337925.844612	39.432372
2813.572986	338392.525092	39.437389
2816.134522	338850.075082	39.442407
2818.500069	339309.404853	39.447424
2821.610892	339781.867305	39.452442
2824.087919	340276.389448	39.457460
2826.944314	340755.461113	39.462477
2829.650504	341220.740668	39.467495
2832.226603	341721.811823	39.472512
2834.612059	342217.780386	39.477530
2837.774425	342714.129728	39.482548
2840.458981	343205.675940	39.487565
2843.561838	343714.213435	39.492583
2846.362294	344234.321082	39.497600
2849.170298	344754.981556	39.502618
2851.896710	345263.590854	39.507636
2854.751982	345781.035853	39.512653
2858.133847	346298.519831	39.517671
2860.899371	346817.010736	39.522688
2863.675626	347343.746229	39.527706
2866.980737	347861.507568	39.532724
2869.815266	348384.644589	39.537741
2872.837776	348902.796549	39.542759
2875.819114	349430.876394	39.547776
2878.561637	349946.041970	39.552794
2881.581184	350477.152140	39.557812
2884.732265	351004.352289	39.562829
2887.960217	351524.731799	39.567847
2890.780401	352029.051114	39.572864
2893.496047	352559.173560	39.577882
2896.569440	353091.264882	39.582900
2899.663146	353610.223767	39.587917
2902.631509	354142.701865	39.592935
2905.479035	354675.599802	39.597952
2908.208857	355196.022022	39.602970
2911.542354	355713.931966	39.607988
2914.711668	356245.366601	39.613005
2917.852621	356756.671367	39.618023
2920.472896	357280.110227	39.623040
2923.531583	357805.479440	39.628058
2926.610812	358333.022737	39.633076
2929.319862	358850.593107	39.638093
2932.428510	359360.708677	39.643111
2935.023510	359879.732995	39.648128
2937.986591	360427.805760	39.653146
2940.995298	360950.687192	39.658164
2943.590209	361476.394917	39.663181
2946.668153	361999.152398	39.668199
2949.841627	362532.574007	39.673216
2952.568258	363064.385235	39.678234
2955.710620	363555.009778	39.683252
2958.524197	364046.087257	39.688269
2961.353259	364532.588851	39.693287
2964.044209	365023.675334	39.698304
2966.942316	365510.967742	39.703322
2969.897124	366008.270338	39.708340
2972.381175	366522.543660	39.713357
2975.481387	367008.290653	39.718375
2978.187467	367519.522845	39.723392
2980.998988	368039.563680	39.728410
2984.227752	368555.091432	39.733428
2987.177468	369077.661205	39.738445
2990.189023	369596.839923	39.743463
2992.611970	370135.441982	39.748480
2995.627520	370666.939902	39.753498
2998.718665	371204.280955	39.758516
3001.557690	371764.188033	39.763533
3004.841415	372301.256407	39.768551
3007.556703	372864.695592	39.773568
3010.272814	373410.695257	39.778586
3013.217163	373973.068333	39.783604
3016.283291	374535.845868	39.788621
3019.588307	375114.562804	39.793639
3022.488698	375685.622396	39.798656
3025.646893	376241.460677	39.803674
3028.686883	376828.035255	39.808692
3031.709393	377401.740784	39.813709
3035.212536	377971.632507	39.818727
3038.214165	378540.885083	39.823744
3041.355582	379120.889745	39.828762
3044.891093	379681.009605	39.833780
3047.858513	380276.145252	39.838797
3050.923766	380864.152975	39.843815
3054.066091	381428.876418	39.848832
3057.442471	381998.171608	39.853850
3060.632857	382582.454929	39.858868
3063.485208	383158.259272	39.863885
3066.834932	383723.220455	39.868903
3069.949262	384308.427839	39.873920
3072.966519	384877.888881	39.878938
3076.127904	385447.825759	39.883956
3079.359186	386025.428646	39.888973
3082.308496	386595.406804	39.893991
3085.375898	387169.593384	39.899008
3088.671797	387781.299625	39.904026
3091.731536	388328.481354	39.909044
3094.550010	388905.977264	39.914061
3097.754896	389505.519560	39.919079
3101.445659	390079.256997	39.924096
3104.123472	390648.935311	39.929114
3107.377002	391234.719732	39.934132
3110.838007	391807.197466	39.939149
3113.820543	392378.169178	39.944167
3116.935212	392974.750418	39.949184
3120.057259	393523.287713	39.954202
3123.048897	394053.856710	39.959220
3126.113388	394570.711817	39.964237
3129.005861	395137.645437	39.969255
3132.294008	395653.814808	39.974272
3134.841847	396207.040674	39.979290
3138.048413	396750.491874	39.984308
3141.026303	397281.874913	39.989325
3143.683410	397822.834581	39.994343
3146.484940	398417.214649	39.999360
3149.805786	398951.027152	40.004378
3153.006704	399552.550211	40.009396
3155.804237	400106.914319	40.014413
3158.831455	400703.448746	40.019431
3161.716210	401275.755883	40.024448
3164.723933	401870.699999	40.029466
3167.819955	402464.934635	40.034484
3170.868748	403088.828883	40.039501
3174.040957	403658.817121	40.044519
3176.977928	404306.866291	40.049536
3179.883914	404901.617991	40.054554
3183.147621	405573.572132	40.059572
3185.859544	406182.831120	40.064589
3189.514944	406797.886233	40.069607
3192.870237	407479.519281	40.074624
3195.791279	408106.629565	40.079642
3199.198920	408764.423165	40.084660
3202.275607	409418.173956	40.089677
3205.879644	410067.264754	40.094695
3209.587780	410692.423072	40.099712
3212.804575	411365.804190	40.104730
3216.862188	412003.223626	40.109748
3219.647657	412654.694527	40.114765
3222.780399	413323.457303	40.119783
3226.400164	413938.981339	40.124800
3229.248669	414628.313570	40.129818
3233.206151	415244.466431	40.134836
3236.331866	415916.263105	40.139853
3239.542714	416554.579536	40.144871
3242.722117	417234.395834	40.149888
3245.719856	417863.898209	40.154906
3249.781468	418510.728486	40.159924
3252.761485	419184.296319	40.164941
3256.002964	419809.510771	40.169959
3259.260170	420485.715035	40.174976
3262.817106	421124.659780	40.179994
3265.973663	421804.268745	40.185012
3269.100900	422431.773779	40.190029
3272.754582	423052.619309	40.195047
3275.977684	423750.437276	40.200064
3278.896581	424388.318250	40.205082
3282.207406	425070.862505	40.210100
3285.539602	425693.548429	40.215117
3288.926447	426395.528870	40.220135
3292.360299	427018.902840	40.225152
3295.559640	427685.110032	40.230170
3298.891979	428316.930643	40.235188
3302.367646	428894.328960	40.240205
3305.598712	429534.850334	40.245223
3308.494837	430129.866986	40.250240
3311.092827	430721.523273	40.255258
3314.989705	431368.226905	40.260276
3317.685024	432006.645131	40.265293
3320.884752	432600.468461	40.270311
3323.914956	433273.576442	40.275328
3327.214352	433914.435360	40.280346
3330.179452	434538.869860	40.285364
3333.418622	435223.517864	40.290381
3336.757365	435854.141524	40.295399
3340.153477	436556.860572	40.300416
3342.842801	437226.600824	40.305434
3346.451064	437893.265919	40.310452
3349.635002	438563.677225	40.315469
3352.681798	439290.024758	40.320487
3356.248948	439957.881811	40.325504
3359.378616	440692.707798	40.330522
3362.755695	441358.050409	40.335540
3365.872988	442117.546212	40.340557
3369.589187	442800.113016	40.345575
3372.868061	443543.082940	40.350592
3376.150398	444261.473812	40.355610
3379.911263	444962.908192	40.360628
3383.431795	445708.912035	40.365645
3386.613820	446421.431886	40.370663
3390.186284	447181.404692	40.375680
3394.176511	447911.672871	40.380698
3397.505516	448621.825184	40.385716
3400.818260	449395.080932	40.390733
3404.710649	450107.630033	40.395751
3408.086493	450839.624962	40.400768
3411.520680	451582.014117	40.405786
3415.545174	452303.534725	40.410804
3418.899213	453012.485807	40.415821
3422.098281	453786.725974	40.420839
3425.742062	454508.135949	40.425856
3428.496222	455267.415994	40.430874
3432.192225	456025.003450	40.435892
3435.557628	456746.993119	40.440909
3439.397049	457503.799493	40.445927
3442.936978	458231.279722	40.450944
3446.163227	458982.313755	40.455962
3449.995400	459716.681499	40.460980
3453.363905	460464.910357	40.465997
3457.027880	461176.032987	40.471015
3460.934084	461947.095302	40.476032
3463.567892	462678.821128	40.481050
3467.386040	463415.798474	40.486068
3470.584687	464183.908320	40.491085
3474.200178	464903.920467	40.496103
3477.631692	465685.344502	40.501120
3480.880900	466376.450665	40.506125
3484.019133	467097.242002	40.511130
3487.124119	467714.115954	40.516135
3490.287043	468299.423931	40.521140
3493.225804	468863.962375	40.526144
3495.894239	469309.985078	40.531149
3498.749894	469757.337614	40.536154
3500.706161	470097.539518	40.541159
3503.158265	470439.786889	40.546164
3505.274693	470677.995539	40.551168
3506.850721	470898.542190	40.556173
3508.398553	471068.544403	40.561178
3510.147946	471204.241287	40.566183
3511.508541	471282.912668	40.571188
3512.349405	471337.128064	40.576192
3513.479480	471372.995647	40.581197
3514.839199	471348.394921	40.586202
3515.351603	471321.595989	40.591207
3516.099987	471267.585498	40.596212
3517.092718	471164.865773	40.601216
3517.440371	471078.166898	40.606221
3518.071724	470941.129458	40.611226
3518.330755	470808.408712	40.616231
3518.664300	470639.070152	40.621236
3518.990963	470486.462348	40.626240
3519.229846	470304.207489	40.631245
3519.173231	470094.974089	40.636250
3519.484841	469892.677200	40.641255
3519.174250	469691.896358	40.646260
3519.438574	469475.507725	40.651264
3519.372857	469262.414020	40.656269
3519.264736	469029.094096	40.661274
3519.538651	468822.128070	40.666279
3519.114986	468578.965700	40.671284
3519.007822	468363.739811	40.676288
3518.831266	468135.136355	40.681293
3518.509102	467907.770385	40.686298
3518.584533	467655.442004	40.691303
3517.887135	467458.250420	40.696308
3518.064392	467199.156399	40.701312
3517.452569	466992.718073	40.706317
3517.764878	466762.247675	40.711322
3517.304948	466516.683936	40.716327
3516.701201	466325.755000	40.721332
3516.606970	466093.465328	40.726336
3516.020315	465905.014735	40.731341
3515.709871	465652.977071	40.736346
3516.136396	465473.237062	40.741351
3515.348158	465261.789301	40.746356
3515.397298	465059.386167	40.751360
3515.323223	464870.946845	40.756365
3515.125709	464644.489797	40.761370
3514.917942	464459.415123	40.766375
3514.203334	464275.737560	40.771380
3514.182870	464084.239951	40.776384
3514.148849	463891.221302	40.781389
3513.714514	463707.139567	40.786394
3513.505189	463549.646993	40.791399
3513.351084	463357.656882	40.796404
3513.202921	463179.357882	40.801408
3512.941718	463014.109808	40.806413
3512.326991	462862.559592	40.811418
3512.324339	462673.075379	40.816423
3512.193572	462539.654440	40.821428
3511.974256	462381.546310	40.826432
3511.614277	462217.829360	40.831437
3511.403051	462077.723279	40.836442
3511.599779	461939.783511	40.841447
3511.054423	461782.736972	40.846452
3511.215757	461639.170877	40.851456
3510.886545	461513.941125	40.856461
3510.409029	461375.140654	40.861466
3510.309161	461245.967529	40.866471
3510.158246	461113.454031	40.871476
3509.803721	460984.979010	40.876480
3509.373740	460869.348082	40.881485
3509.649453	460741.583575	40.886490
3509.488314	460632.756542	40.891495
3509.062282	460516.818787	40.896500
3509.427350	460398.016265	40.901504
3509.056804	460291.300327	40.906509
3508.816289	460189.280701	40.911514
3508.594178	460075.134461	40.916519
3508.290482	459949.080126	40.921524
3508.129087	459877.836671	40.926528
3507.826982	459784.042393	40.931533
3507.661589	459679.776606	40.936538
3507.808238	459612.034397	40.941543
3507.559804	459510.672312	40.946548
3507.438632	459427.652578	40.951552
3507.386834	459347.310070	40.956557
3507.129426	459238.744990	40.961562
3507.157514	459188.013677	40.966567
3506.982221	459109.465265	40.971572
3507.192397	459028.674371	40.976576
3506.870005	458944.822267	40.981581
3506.888911	458897.287566	40.986586
3507.107635	458775.810877	40.991591
3506.283801	458756.461553	40.996596
3506.562346	458641.417108	41.001600
3506.572067	458614.732500	41.006605
3506.406202	458513.707888	41.011610
3506.098783	458482.812067	41.016615
3506.179420	458379.566553	41.021620
3506.313343	458353.166370	41.026624
3506.257398	458265.870748	41.031629
3505.700274	458227.556883	41.036634
3506.061830	458142.426858	41.041639
3505.661352	458127.727881	41.046644
3505.767937	458028.027681	41.051648
3505.944654	457991.626586	41.056653
3505.415093	457923.529540	41.061658
3505.521981	457894.596597	41.066663
3504.895199	457821.898194	41.071668
3505.226134	457786.943555	41.076672
3505.326773	457726.507986	41.081677
3505.073816	457715.843832	41.086682
3505.284755	457623.176825	41.091687
3504.930302	457619.428008	41.096692
3504.464568	457564.306765	41.101696
3505.136074	457490.488900	41.106701
3504.834746	457494.493467	41.111706
3504.762227	457424.749994	41.116711
3505.049055	457361.443073	41.121716
3504.983685	457339.486792	41.126720
3504.857452	457313.938199	41.131725
3504.728378	457266.220478	41.136730
3504.864099	457239.615766	41.141735
3504.497315	457206.647571	41.146740
3504.758296	457160.440638	41.151744
3504.734427	457119.098140	41.156749
3504.873655	457080.875148	41.161754
3504.640252	457053.821248	41.166759
3504.533715	456997.170603	41.171764
3504.135675	456973.744593	41.176768
3504.089071	456932.811200	41.181773
3504.076059	456927.334135	41.186778
3504.047772	456858.647276	41.191783
3503.969426	456868.958227	41.196788
3503.966230	456810.160021	41.201792
3504.128005	456797.654237	41.206797
3504.070639	456767.984816	41.211802
3504.046371	456755.609883	41.216807
3504.006175	456714.421415	41.221812
3504.018486	456685.704788	41.226816
3504.071532	456674.687368	41.231821
3504.138263	456629.068104	41.236826
3503.986253	456616.104495	41.241831
3503.933046	456570.047476	41.246836
3504.103115	456572.709368	41.251840
3504.048121	456519.905061	41.256845
3503.942622	456512.108800	41.261850
3503.822004	456473.012653	41.266855
3503.992933	456456.091456	41.271860
3503.990489	456413.171542	41.276864
3503.917159	456405.167224	41.281869
3503.524230	456377.782592	41.286874
3504.008504	456342.446326	41.291879
3503.702221	456346.401147	41.296884
3503.485758	456287.381615	41.301888
3503.850456	456293.919252	41.306893
3503.383377	456256.602433	41.311898
3503.795247	456240.201055	41.316903
3503.282563	456233.534468	41.321908
3503.806096	456185.356146	41.326912
3503.271422	456184.273727	41.331917
3503.494423	456150.855609	41.336922
3503.385098	456163.353334	41.341927
3503.542787	456119.849475	41.346932
3503.312467	456117.754998	41.351936
3503.235889	456114.672274	41.356941
3503.719661	456071.268976	41.361946
3503.439723	456063.043527	41.366951
3503.315624	456061.997667	41.371956
3503.310297	456020.295073	41.376960
3503.733477	456022.054541	41.381965
3503.479697	455972.933225	41.386970
3503.682107	455994.666119	41.391975
3503.461139	455943.104312	41.396980
3503.190040	455946.698500	41.401984
3503.434023	455901.658550	41.406989
3503.404671	455916.528285	41.411994
3503.620895	455883.922590	41.416999
3503.186385	455867.857673	41.422004
3503.430353	455863.811024	41.427008
3503.259371	455838.622963	41.432013
3503.207177	455822.548313	41.437018
3503.204502	455791.955735	41.442023
3503.254579	455794.890361	41.447028
3503.475363	455774.916696	41.452032
3503.240832	455748.318011	41.457037
3503.179931	455745.435697	41.462042
3503.210810	455721.991310	41.467047
3502.997830	455703.709662	41.472052
3503.036769	455728.563476	41.477056
3503.276600	455689.814866	41.482061
3503.037491	455688.432025	41.487066
3503.119560	455656.760436	41.492071
3503.126464	455677.205434	41.497076
3503.294690	455645.469475	41.502080
3503.261480	455634.668120	41.507085
3503.286732	455624.161929	41.512090
3503.367442	455578.791999	41.517095
3502.842949	455608.301168	41.522100
3503.141884	455563.201121	41.527104
3503.077149	455590.709701	41.532109
3503.016841	455535.874521	41.537114
3503.073648	455570.213160	41.542119
3503.007615	455552.415511	41.547124
3503.028899	455502.539395	41.552128
3503.024491	455530.038512	41.557133
3502.844126	455496.378776	41.562138
3503.098225	455480.762816	41.567143
3502.700745	455497.466754	41.572148
3502.844493	455473.192503	41.577152
3502.881045	455483.384456	41.582157
3502.336650	455475.606478	41.587162
3503.174260	455436.255584	41.592167
3502.950439	455473.479912	41.597172
3502.881049	455438.077545	41.602176
3502.898209	455412.098236	41.607181
3502.971551	455435.881490	41.612186
3503.125224	455406.024704	41.617191
3502.680628	455378.139666	41.622196
3502.667713	455422.941065	41.627200
3503.092363	455389.692884	41.632205
3502.871974	455343.558310	41.637210
3502.790004	455373.860337	41.642215
3502.725031	455382.191170	41.647220
3502.957525	455326.193014	41.652224
3502.925831	455368.562179	41.657229
3502.593016	455333.302760	41.662234
3503.073775	455334.799504	41.667239
3502.693701	455323.241062	41.672244
3502.835015	455300.133929	41.677248
3502.956399	455320.459683	41.682253
3502.872576	455269.737161	41.687258
3502.733472	455304.665266	41.692263
3502.683844	455279.660340	41.697268
3503.364241	455256.011324	41.702272
3502.966601	455283.674375	41.707277
3503.012519	455245.006390	41.712282
3503.383679	455204.561905	41.717287
3502.945380	455249.075741	41.722292
3502.903348	455218.234927	41.727296
3503.362935	455175.544033	41.732301
3502.824137	455211.600920	41.737306
3503.246420	455158.616501	41.742311
3502.528368	455130.317760	41.747316
3502.793666	455147.526018	41.752320
3502.695594	455180.164708	41.757325
3502.455293	455136.468185	41.762330
3503.142007	455142.955255	41.767335
3502.528557	455141.479346	41.772340
3502.790598	455112.569027	41.777344
3503.064344	455123.281745	41.782349
3502.741328	455105.321422	41.787354
3503.010942	455117.252463	41.792359
3503.169531	455085.618713	41.797364
3503.156437	455084.047898	41.802368
3502.746775	455076.349955	41.807373
3503.085901	455027.082116	41.812378
3502.832425	455031.079553	41.817383
3502.747482	455088.577073	41.822388
3502.684372	455051.853968	41.827392
3503.209404	455002.658160	41.832397
3503.031612	455036.324387	41.837402
3502.901936	455027.973333	41.842407
3502.914874	454984.439430	41.847412
3503.003143	455016.490798	41.852416
3502.947640	454983.368658	41.857421
3503.167904	454955.986835	41.862426
3502.897028	454970.590953	41.867431
3503.151988	454935.390208	41.872436
3502.745850	454949.457620	41.877440
3503.208453	454926.147107	41.882445
3503.004169	454938.812731	41.887450
3502.953504	454894.578398	41.892455
3503.279917	454869.615048	41.897460
3503.120141	454880.396411	41.902464
3503.245282	454889.356949	41.907469
3502.825277	454846.905952	41.912474
3503.026087	454835.762802	41.917479
3502.461624	454872.889757	41.922484
3502.577608	454845.930178	41.927488
3502.308862	454823.902115	41.932493
3502.376168	454813.338162	41.937498
3503.209153	454773.428744	41.942503
3502.790190	454814.490270	41.947508
3502.903204	454822.285805	41.952512
3502.614150	454776.820507	41.957517
3502.901996	454761.756823	41.962522
3502.759840	454781.769562	41.967527
3502.612785	454758.149356	41.972532
3502.609028	454768.906109	41.977536
3502.629046	454748.050010	41.982541
3502.484567	454733.764965	41.987546
3502.675550	454753.268436	41.992551
3502.635506	454761.646293	41.997556
3502.783551	454744.727431	42.002560
3502.305097	454727.806118	42.007565
3502.548069	454739.132727	42.012570
3503.045709	454701.813042	42.017575
3503.047773	454737.785184	42.022580
3502.639386	454674.580602	42.027584
3502.761798	454707.844701	42.032589
3502.500674	454690.026475	42.037594
3503.476594	454662.981479	42.042599
3502.799709	454644.163461	42.047604
3502.808951	454662.325835	42.052608
3503.027428	454677.360157	42.057613
3502.801083	454631.428020	42.062618
3503.030542	454655.035205	42.067623
3502.687770	454641.796191	42.072628
3503.017754	454585.577843	42.077632
3502.843203	454624.419373	42.082637
3502.857537	454602.092659	42.087642
3503.063025	454602.770434	42.092647
3502.421046	454570.146297	42.097652
3502.876777	454542.117904	42.102656
3503.002405	454582.484913	42.107661
3502.937009	454563.722376	42.112666
3503.287233	454519.068777	42.117671
3502.849073	454500.973963	42.122676
3503.071761	454540.513904	42.127680
3502.529577	454517.412544	42.132685
3502.846474	454487.325795	42.137690
3502.841688	454480.730609	42.142695
3502.612806	454510.498902	42.147700
3502.592182	454469.912089	42.152704
3502.849397	454473.524469	42.157709
3502.474200	454503.112951	42.162714
3502.563144	454450.940634	42.167719
3502.504454	454461.097366	42.172724
3502.327773	454459.044991	42.177728
3503.025456	454448.279744	42.182733
3502.374669	454461.777279	42.187738
3502.702750	454419.156487	42.192743
3502.517943	454422.483586	42.197748
3502.568884	454446.169946	42.202752
3503.054952	454422.601520	42.207757
3502.729858	454416.615064	42.212762
3503.095470	454406.003766	42.217767
3502.634437	454422.566328	42.222772
3502.742356	454402.152655	42.227776
3502.306721	454389.689238	42.232781
3502.612893	454369.548623	42.237786
3502.444168	454387.587136	42.242791
3502.485431	454360.385104	42.247796
3502.473252	454404.072172	42.252800
3502.655899	454357.415237	42.257805
3502.365301	454381.104917	42.262810
3502.371970	454352.741376	42.267815
3502.507975	454345.870206	42.272820
3502.360777	454357.766062	42.277824
3502.443424	454347.909796	42.282829
3502.286958	454359.350475	42.287834
3502.461745	454371.246163	42.292839
3502.497963	454344.755238	42.297844
3502.539795	454365.855493	42.302848
3502.538862	454316.233963	42.307853
3502.241191	454356.313124	42.312858
3502.664835	454320.171478	42.317863
3502.566418	454367.829803	42.322868
3502.763219	454327.462054	42.327872
3502.737781	454333.250129	42.332877
3502.528430	454311.364392	42.337882
3502.677993	454285.210646	42.342887
3502.779755	454322.030232	42.347892
3502.802607	454279.863332	42.352896
3502.852091	454297.562995	42.357901
3502.550951	454277.974943	42.362906
3502.963817	454256.904078	42.367911
3502.809247	454276.817749	42.372916
3502.932375	454220.123817	42.377920
3502.597889	454264.927602	42.382925
3502.361366	454258.368985	42.387930
3502.910036	454235.754492	42.392935
3502.568540	454228.146960	42.397940
3502.699119	454233.910397	42.402944
3502.610977	454222.508195	42.407949
3502.842565	454225.870975	42.412954
3502.572749	454233.828706	42.417959
3502.558643	454194.711775	42.422964
3502.593137	454207.390798	42.427968
3502.738323	454218.124268	42.432973
3502.612328	454201.045368	42.437978
3502.995450	454165.163574	42.442983
3502.902345	454183.342510	42.447988
3502.674613	454188.046360	42.452992
3503.322979	454142.330127	42.457997
3502.836710	454115.820053	42.463002
3502.758593	454159.822444	42.468007
3502.452880	454147.795000	42.473012
3502.801389	454106.996971	42.478016
3502.617927	454123.414396	42.483021
3502.497663	454100.804037	42.488026
3502.447376	454123.441229	42.493031
3502.624566	454097.029208	42.498036
3502.372221	454113.812697	42.503040
3502.008702	454087.892047	42.508045
3502.588887	454057.864586	42.513050
3502.516556	454091.211112	42.518055
3502.258841	454078.313491	42.523060
3503.081264	454085.286800	42.528064
3502.768019	454099.796697	42.533069
3502.659029	454038.674028	42.538074
3502.627275	454054.661612	42.543079
3502.749119	454079.960777	42.548084
3502.435867	454059.816329	42.553088
3502.322228	454061.204167	42.558093
3502.229391	454050.614437	42.563098
3502.793516	454012.775726	42.568103
3502.484667	454010.541249	42.573108
3502.733097	453997.208401	42.578112
3502.820065	454009.168899	42.583117
3502.555325	454013.219033	42.588122
3502.843409	453968.168267	42.593127
3503.037935	453971.587683	42.598132
3502.512953	453966.546001	42.603136
3503.063135	453956.767876	42.608141
3502.912333	453962.778817	42.613146
3502.853044	453988.969274	42.618151
3502.528157	453997.798350	42.623156
3502.635068	453975.760818	42.628160
3503.023957	453953.830906	42.633165
3502.462801	453943.721066	42.638170
3502.241535	453934.217096	42.643175
3502.471460	453928.751639	42.648180
3502.744988	453894.408905	42.653184
3502.754727	453901.104828	42.658189
3502.491198	453930.422707	42.663194
3502.758689	453919.725217	42.668199
3502.343105	453912.180029	42.673204
3502.475952	453879.838325	42.678208
3503.184698	453845.375980	42.683213
3502.489159	453908.402078	42.688218
3502.707149	453887.615372	42.693223
3503.083818	453854.575484	42.698228
3502.807170	453872.885160	42.703232
3502.625730	453830.140854	42.708237
3502.791971	453827.881995	42.713242
3502.559434	453815.284679	42.718247
3502.348741	453837.034211	42.723252
3502.119582	453804.191496	42.728256
3503.164277	453781.345925	42.733261
3502.758630	453846.355933	42.738266
3502.618518	453818.522318	42.743271
3502.631092	453766.715677	42.748276
3502.744595	453809.064803	42.753280
3502.858168	453785.757558	42.758285
3502.556624	453775.606604	42.763290
3503.318031	453727.537672	42.768295
3502.814017	453771.405181	42.773300
3502.664745	453749.255710	42.778304
3503.068541	453752.642077	42.783309
3502.419399	453742.850491	42.788314
3502.813555	453698.442034	42.793319
3502.740136	453708.855126	42.798324
3502.628865	453721.151548	42.803329
3502.539207	453698.180776	42.808333
3502.393986	453690.694254	42.813338
3502.402780	453688.105096	42.818343
3502.579749	453667.070977	42.823348
3502.622116	453715.723199	42.828353
3502.591126	453675.085867	42.833357
3502.763024	453644.716490	42.838362
3502.262765	453662.097634	42.843367
3502.417884	453697.489095	42.848372
3502.334287	453669.747843	42.853377
3503.017178	453641.682434	42.858381
3502.757777	453678.610894	42.863386
3502.737589	453658.166065	42.868391
3502.722073	453662.785737	42.873396
3502.571553	453668.999668	42.878401
3502.970781	453645.900821	42.883405
3502.768676	453638.879929	42.888410
3502.921861	453638.754171	42.893415
3502.487445	453617.512216	42.898420
3502.645705	453568.726463	42.903425
3502.857928	453562.350405	42.908429
3502.375550	453577.851423	42.913434
3502.873886	453585.484993	42.918439
3503.056215	453596.669540	42.923444
3502.834479	453575.901322	42.928449
3503.172928	453561.691417	42.933453
3502.683353	453530.107223	42.938458
3503.130515	453485.436274	42.943463
3502.866369	453515.059223	42.948468
3502.787206	453525.980703	42.953473
3502.698355	453492.963141	42.958477
3502.738108	453493.261232	42.963482
3502.976852	453471.912729	42.968487
3503.220582	453444.271679	42.973492
3502.663240	453469.983326	42.978497
3502.805984	453459.203860	42.983501
3502.745960	453453.733385	42.988506
3502.938842	453423.715576	42.993511
3502.718690	453414.414172	42.998516
3502.609427	453399.716801	43.003521
3503.208935	453377.600823	43.008525
3502.898545	453337.362236	43.013530
3503.162471	453376.187321	43.018535
3503.023756	453344.344446	43.023540
3502.538932	453339.600716	43.028545
3502.889890	453326.606450	43.033549
3502.696933	453349.216224	43.038554
3502.884325	453318.691745	43.043559
3502.935669	453292.603126	43.048564
3502.739486	453282.283076	43.053569
3502.564713	453281.752498	43.058573
3502.455578	453272.534967	43.063578
3503.333929	453215.566932	43.068583
3503.239305	453214.617760	43.073588
3502.718342	453248.239398	43.078593
3503.026840	453237.179924	43.083597
3503.045946	453203.840437	43.088602
3502.845800	453185.656209	43.093607
3502.932106	453216.898578	43.098612
3502.816542	453213.009776	43.103617
3502.442049	453172.831773	43.108621
3502.050176	453166.551099	43.113626
3502.540033	453143.538899	43.118631
3503.132327	453127.309719	43.123636
3502.859544	453128.418327	43.128641
3502.884725	453131.255754	43.133645
3502.968437	453153.821986	43.138650
3502.884191	453150.384886	43.143655
3502.772965	453131.729895	43.148660
3501.977478	453097.859395	43.153665
3502.552268	453080.415173	43.158669
3502.509106	453085.952662	43.163674
3503.105729	453053.079809	43.168679
3503.141126	453052.414521	43.173684
3502.882584	453054.637178	43.178689
3502.946581	453071.777351	43.183693
3502.557351	453094.266181	43.188698
3503.056160	453075.971376	43.193703
3502.630856	453052.900791	43.198708
3502.602898	453056.203293	43.203713
3502.791880	453031.462618	43.208717
3502.391090	453020.413682	43.213722
3502.021719	452997.689384	43.218727
3503.199648	452965.840812	43.223732
3502.964820	452956.084873	43.228737
3502.883858	452943.260149	43.233741
3502.657435	452981.909713	43.238746
3502.856530	452962.647379	43.243751
3502.033023	452947.910402	43.248756
3502.694573	452920.659339	43.253761
3502.766240	452926.178716	43.258765
3502.414803	452936.788331	43.263770
3502.541401	452890.593925	43.268775
3502.757134	452908.522092	43.273780
3502.587743	452942.697494	43.278785
3502.805388	452908.565077	43.283789
3502.534341	452912.717884	43.288794
3502.769567	452860.772510	43.293799
3502.560790	452897.897192	43.298804
3502.055659	452890.518042	43.303809
3502.384806	452875.903255	43.308813
3502.762099	452860.824177	43.313818
3502.502954	452851.985378	43.318823
3502.567692	452883.130130	43.323828
3502.499926	452878.675563	43.328833
3502.556917	452855.376314	43.333837
3502.761649	452825.051400	43.338842
3502.588180	452843.345589	43.343847
3502.593213	452837.002082	43.348852
3502.330542	452819.639305	43.353857
3502.706291	452803.748575	43.358861
3502.626602	452857.699009	43.363866
3502.468054	452821.241096	43.368871
3503.008367	452786.702302	43.373876
3502.300685	452816.447009	43.378881
3502.276686	452767.739100	43.383885
3502.505698	452814.080377	43.388890
3502.317920	452823.801572	43.393895
3502.312880	452806.245836	43.398900
3502.188904	452792.413002	43.403905
3503.128828	452759.383977	43.408909
3502.534012	452752.374149	43.413914
3502.437218	452789.379822	43.418919
3502.736181	452785.831349	43.423924
3502.746152	452784.611918	43.428929
3502.484673	452736.448896	43.433933
3502.723133	452707.336288	43.438938
3502.911200	452702.891986	43.443943
3502.455437	452725.340954	43.448948
3502.184964	452731.777067	43.453953
3502.901500	452688.026068	43.458957
3502.722059	452665.575865	43.463962
3502.181883	452701.839903	43.468967
3502.032818	452682.530888	43.473972
3502.359849	452684.356564	43.478977
3502.514157	452698.286024	43.483981
3502.634755	452674.418380	43.488986
3502.704425	452699.981030	43.493991
3502.460813	452677.693208	43.498996
3502.705843	452649.340611	43.504001
3502.705482	452679.531841	43.509005
3502.549673	452701.324518	43.514010
3502.510693	452673.422778	43.519015
3502.741572	452622.390900	43.524020
3502.634037	452644.784899	43.529025
3502.595646	452631.750305	43.534029
3502.717413	452614.935502	43.539034
3502.579402	452586.440411	43.544039
3502.459833	452629.589692	43.549044
3502.581505	452623.633621	43.554049
3502.509955	452584.573754	43.559053
3502.972039	452556.998599	43.564058
3502.815671	452536.777263	43.569063
3502.766540	452573.420556	43.574068
3502.574681	452547.724727	43.579073
3502.898351	452537.626614	43.584077
3502.181766	452567.626759	43.589082
3502.272440	452552.542046	43.594087
3502.530684	452519.924887	43.599092
3502.165961	452524.194055	43.604097
3502.117881	452523.947883	43.609101
3502.517488	452505.313113	43.614106
3502.363490	452543.901224	43.619111
3502.534145	452512.261995	43.624116
3502.667913	452515.082332	43.629121
3502.612813	452542.491591	43.634125
3502.089182	452517.761527	43.639130
3502.100554	452475.339400	43.644135
3502.544730	452496.327038	43.649140
3502.081209	452516.037372	43.654145
3502.560218	452484.247877	43.659149
3502.540900	452514.797514	43.664154
3502.279720	452503.371064	43.669159
3502.589147	452484.598307	43.674164
3502.741486	452507.813972	43.679169
3502.528559	452478.112784	43.684173
3502.734691	452451.339093	43.689178
3502.813101	452480.046614	43.694183
3502.727390	452456.769518	43.699188
3502.447078	452427.687821	43.704193
3502.791258	452443.870815	43.709197
3502.769584	452432.609437	43.714202
3502.671482	452435.669406	43.719207
3502.593063	452439.791847	43.724212
3502.786576	452410.077063	43.729217
3503.104357	452395.666736	43.734221
3502.575065	452403.463150	43.739226
3502.749507	452385.625009	43.744231
3502.729217	452369.745842	43.749236
3502.547202	452378.299244	43.754241
3503.018393	452362.139410	43.759245
3502.722271	452333.060092	43.764250
3502.943775	452311.358038	43.769255
3502.795307	452344.719146	43.774260
3502.371335	452346.105403	43.779265
3502.108396	452321.587629	43.784269
3502.632351	452290.399669	43.789274
3502.963974	452316.783958	43.794279
3502.892192	452297.614629	43.799284
3502.613186	452306.893782	43.804289
3502.701539	452305.408223	43.809293
3502.709110	452276.940477	43.814298
3502.450361	452261.200415	43.819303
3502.489182	452257.236302	43.824308
3503.138664	452226.840293	43.829313
3503.004187	452237.111478	43.834317
3502.551805	452234.899513	43.839322
3502.795911	452196.600967	43.844327
3502.770856	452238.365992	43.849332
3502.321684	452196.625062	43.854337
3502.851259	452167.009068	43.859341
3502.511280	452203.749671	43.864346
3502.311925	452176.177135	43.869351
3502.422174	452179.965342	43.874356
3502.334023	452211.439631	43.879361
3502.457219	452171.028967	43.884365
3502.513672	452140.980303	43.889370
3502.454504	452161.946331	43.894375
3502.685312	452172.159801	43.899380
3502.470064	452160.472206	43.904385
3502.462691	452143.931186	43.909389
3502.638185	452177.444296	43.914394
3502.662810	452145.827648	43.919399
3502.562498	452152.237023	43.924404
3502.292932	452124.523295	43.929409
3502.349885	452138.468485	43.934413
3501.799377	452150.682956	43.939418
3501.856125	452137.836013	43.944423
3502.722204	452133.487393	43.949428
3501.855377	452152.246937	43.954433
3502.286320	452133.403941	43.959437
3502.585598	452141.982834	43.964442
3502.419668	452156.419930	43.969447
3502.205720	452148.436340	43.974452
3502.248255	452111.742541	43.979457
3502.546706	452119.053003	43.984461
3502.229991	452124.329511	43.989466
3502.506352	452097.036878	43.994471
3502.821985	452094.703493	43.999476
3502.366712	452139.733503	44.004481
3502.660428	452125.225326	44.009485
3502.151815	452099.173124	44.014490
3502.954794	452073.826930	44.019495
3502.611411	452096.816918	44.024500
3502.457199	452066.395515	44.029505
3502.697315	452095.280926	44.034509
3502.904696	452068.506593	44.039514
3502.729418	452065.591149	44.044519
3502.318643	452046.982627	44.049524
3502.898236	452034.864862	44.054529
3502.674823	452041.851901	44.059533
3502.915005	451998.783809	44.064538
3502.674430	452026.730432	44.069543
3502.527196	452007.166843	44.074548
3501.809965	452009.157651	44.079553
3502.879944	451999.042812	44.084557
3502.328847	451996.389740	44.089562
3502.352912	452003.439155	44.094567
3502.448686	451954.152414	44.099572
3502.216072	452000.923508	44.104577
3502.137237	451969.119999	44.109581
3502.632993	451947.881681	44.114586
3502.340375	451977.155913	44.119591
3502.267079	451953.977831	44.124596
3501.946622	451978.791065	44.129601
3501.941652	451980.669282	44.134605
3502.003635	451957.368333	44.139610
3502.018634	451975.633419	44.144615
3502.526561	451988.898493	44.149620
3502.392355	451965.983768	44.154625
3502.399814	452004.496518	44.159629
3502.048807	451984.203977	44.164634
3502.408284	451987.293158	44.169639
3502.842755	451948.608906	44.174644
3502.132107	451975.919495	44.179649
3502.379245	451948.783536	44.184653
3502.312525	451949.047735	44.189658
3502.491840	451955.971137	44.194663
3502.686799	451958.731126	44.199668
3502.426591	451933.857305	44.204673
3502.558733	451959.309418	44.209677
3502.544006	451914.200995	44.214682
3502.325437	451937.171411	44.219687
3502.235680	451914.351094	44.224692
3502.057544	451934.676473	44.229697
3502.040449	451918.999462	44.234701
3502.608817	451932.711704	44.239706
3502.093947	451938.831469	44.244711
3502.647894	451922.708989	44.249716
3502.601031	451930.074098	44.254721
3502.707343	451924.069530	44.259725
3502.304309	451932.810265	44.264730
3502.040562	451898.803189	44.269735
3502.759108	451859.566449	44.274740
3502.206693	451925.721457	44.279745
3501.968113	451918.502829	44.284749
3502.171662	451892.490045	44.289754
3501.972359	451904.547641	44.294759
3501.990287	451938.542696	44.299764
3501.968852	451930.071909	44.304769
3502.362556	451902.100835	44.309773
3502.522664	451889.592617	44.314778
3502.242769	451936.777262	44.319783
3502.743125	451930.000002	44.324788
3502.155255	451902.387067	44.329793
3502.641736	451862.425867	44.334797
3502.426672	451858.654049	44.339802
3502.315739	451901.955561	44.344807
3502.477744	451869.555667	44.349812
3502.462320	451860.170524	44.354817
3502.794541	451894.471165	44.359821
3502.256428	451879.079462	44.364826
3502.816274	451833.220390	44.369831
3502.640838	451820.460716	44.374836
3502.582187	451865.225592	44.379841
3502.575302	451847.314211	44.384845
3503.061428	451824.910204	44.389850
3502.837547	451792.266742	44.394855
3502.879084	451803.728140	44.399860
3502.305596	451831.220192	44.404865
3502.129384	451808.920871	44.409869
3502.538909	451790.385443	44.414874
3502.354332	451770.675326	44.419879
3502.656054	451803.915309	44.424884
3502.347292	451781.383197	44.429889
3502.089830	451780.713423	44.434893
3502.627160	451774.640683	44.439898
3503.076865	451754.475081	44.444903
3502.943256	451784.231858	44.449908
3502.487261	451754.720388	44.454913
3502.756430	451728.240354	44.459917
3502.897995	451712.944071	44.464922
3502.567804	451753.134414	44.469927
3502.753539	451716.924785	44.474932
3502.136999	451704.387008	44.479937
3503.007223	451679.892395	44.484941
3502.902766	451706.447808	44.489946
3502.213246	451683.468353	44.494951
3502.685670	451650.308668	44.499956
3502.396928	451635.892258	44.504961
3502.645368	451667.923008	44.509965
3502.456991	451669.728755	44.514970
3501.634642	451670.264637	44.519975
3502.288241	451665.137620	44.524980
3502.672759	451649.193964	44.529985
3502.617587	451625.657480	44.534989
3502.213973	451666.164045	44.539994
3502.437320	451677.596765	44.544999
3502.520793	451680.983337	44.550004
3501.998722	451686.038688	44.555009
3502.390036	451680.597930	44.560013
3502.650228	451679.694092	44.565018
3502.484506	451676.168163	44.570023
3502.796743	451649.985693	44.575028
3502.699665	451626.912530	44.580033
3502.239218	451611.711345	44.585037
3502.613249	451596.530469	44.590042
3502.943890	451574.607495	44.595047
3502.448532	451550.531591	44.600052
3502.433034	451546.931150	44.605057
3502.530791	451541.283045	44.610061
3502.590764	451549.392547	44.615066
3502.241986	451565.431983	44.620071
3501.960639	451585.824728	44.625076
3501.927669	451589.787905	44.630081
3502.330744	451577.241110	44.635085
3502.863468	451562.390333	44.640090
3502.837287	451534.637421	44.645095
3502.943999	451544.414091	44.650100
3502.417970	451568.702078	44.655105
3502.672464	451549.328316	44.660109
3502.860458	451510.327084	44.665114
3502.736246	451537.190279	44.670119
3502.697780	451510.403417	44.675124
3501.947757	451502.199879	44.680129
3502.022556	451506.754963	44.685133
3502.932339	451485.349283	44.690138
3502.617076	451493.467378	44.695143
3502.299348	451486.413358	44.700148
3502.553042	451447.452378	44.705153
3502.527307	451476.380591	44.710157
3502.520942	451461.462736	44.715162
3502.614729	451470.023619	44.720167
3502.540217	451487.136126	44.725172
3502.602675	451425.928639	44.730177
3502.437519	451430.369437	44.735181
3502.440362	451446.251883	44.740186
3502.569470	451417.053442	44.745191
3502.507418	451439.238447	44.750196
3502.482582	451408.186792	44.755201
3502.573555	451421.010663	44.760205
3502.564608	451418.830008	44.765210
3501.810528	451406.060087	44.770215
3502.657183	451369.999159	44.775220
3502.925249	451388.681406	44.780225
3502.754167	451417.226714	44.785229
3502.400255	451379.275067	44.790234
3502.585513	451341.897804	44.795239
3502.671580	451389.888372	44.800244
3502.491090	451363.986445	44.805249
3502.656615	451377.306000	44.810253
3502.370637	451366.897792	44.815258
3502.527725	451348.249682	44.820263
3502.604822	451356.255056	44.825268
3502.189817	451327.041026	44.830273
3502.201578	451331.301642	44.835277
3501.989431	451342.651138	44.840282
3502.515853	451310.243597	44.845287
3502.585536	451360.368088	44.850292
3502.175884	451348.254110	44.855297
3502.815508	451314.509324	44.860301
3502.628811	451288.557550	44.865306
3502.073523	451309.907246	44.870311
3502.339745	451331.380781	44.875316
3502.256537	451318.809229	44.880321
3502.225670	451301.307171	44.885325
3502.668768	451272.870827	44.890330
3502.425181	451312.946756	44.895335
3502.265686	451308.810851	44.900340
3502.582347	451279.075143	44.905345
3502.310216	451308.194750	44.910349
3502.043470	451274.948396	44.915354
3502.053402	451263.072515	44.920359
3502.679221	451239.529476	44.925364
3502.463093	451231.698146	44.930369
3502.432749	451280.214791	44.935373
3502.201584	451290.755405	44.940378
3502.017885	451280.432479	44.945383
3503.270868	451247.047337	44.950388
3502.299948	451269.731390	44.955393
3502.425137	451270.421962	44.960397
3502.047122	451238.106548	44.965402
3502.442301	451215.462604	44.970407
3502.316232	451260.898991	44.975412
3502.247999	451240.764072	44.980417
3502.352789	451248.409894	44.985421
3502.116512	451247.787499	44.990426
3502.203309	451228.490723	44.995431
3502.226770	451260.405368	45.000436
3501.829493	451254.125022	45.005441
3502.434900	451244.489254	45.010445
3502.747976	451248.550020	45.015450
3502.187600	451288.320856	45.020455
3502.416658	451270.929922	45.025460
3502.418809	451237.438028	45.030465
3502.207645	451204.436510	45.035469
3502.690080	451212.834562	45.040474
3501.920681	451242.185094	45.045479
3502.369451	451210.195646	45.050484
3502.246197	451223.002747	45.055489
3502.282202	451220.155286	45.060493
3502.547117	451200.119902	45.065498
3502.398116	451225.465034	45.070503
3502.480812	451223.726576	45.075508
3502.439832	451181.208853	45.080513
3502.073244	451202.173604	45.085517
3502.517794	451164.602832	45.090522
3502.106577	451204.654702	45.095527
3502.004899	451195.485903	45.100532
3502.436480	451171.263073	45.105537
3502.238511	451194.535440	45.110541
3502.064755	451206.335637	45.115546
3502.104812	451185.371635	45.120551
3502.093859	451201.357920	45.125556
3502.166981	451176.938036	45.130561
3502.495250	451212.813407	45.135565
3502.412487	451173.093236	45.140570
3502.263834	451214.930398	45.145575
3502.487366	451225.449907	45.150580
3502.159939	451197.794956	45.155585
3501.735439	451167.212114	45.160589
3502.494716	451172.775450	45.165594
3502.613709	451182.854801	45.170599
3502.798392	451171.560186	45.175604
3502.744036	451175.780538	45.180609
3502.440226	451175.371797	45.185613
3502.710750	451178.982598	45.190618
3502.265462	451144.597149	45.195623
3502.606080	451152.307213	45.200628
3502.279248	451141.397912	45.205633
3502.053354	451137.018748	45.210637
3502.375797	451153.358323	45.215642
3502.637394	451142.761964	45.220647
3502.623338	451156.515993	45.225652
3502.545704	451136.128745	45.230657
3502.418152	451134.017557	45.235661
3502.945081	451080.043002	45.240666
3502.311502	451107.190197	45.245671
3502.219106	451111.061359	45.250676
3502.656213	451126.367927	45.255681
3502.371691	451097.995644	45.260685
3502.412709	451078.097038	45.265690
3502.653393	451118.096752	45.270695
3502.103698	451083.068030	45.275700
3502.491577	451067.072698	45.280705
3502.485735	451086.661155	45.285709
3502.940468	451069.589610	45.290714
3502.808936	451048.297393	45.295719
3502.480067	451058.752066	45.300724
3502.290212	451028.131948	45.305729
3502.627377	451025.947288	45.310733
3502.357503	451064.251721	45.315738
3502.526791	451057.374308	45.320743
3502.520871	451031.698139	45.325748
3502.484723	450995.725436	45.330753
3502.299468	451023.055585	45.335757
3502.610424	451004.484364	45.340762
3502.638679	450996.360596	45.345767
3502.671703	451021.981648	45.350772
3502.472809	451003.795494	45.355777
3501.927263	450987.693936	45.360781
3502.184678	450970.196802	45.365786
3501.813317	450982.637294	45.370791
3502.594058	450961.353021	45.375796
3502.194626	450996.785563	45.380801
3502.186531	450958.017379	45.385805
3502.382640	450976.051645	45.390810
3502.237972	450975.922215	45.395815
3502.044616	450970.776696	45.400820
3502.600629	450949.629428	45.405825
3502.439747	450934.989386	45.410829
3502.324965	450987.275151	45.415834
3501.779315	450992.131398	45.420839
3502.275612	450964.396699	45.425844
3502.528648	450955.425458	45.430849
3502.437928	451012.223697	45.435853
3502.551852	450960.648432	45.440858
3502.070186	450978.231640	45.445863
3502.020571	450943.123654	45.450868
3502.167990	450936.604879	45.455873
3502.634604	450911.615060	45.460877
3502.567245	450965.162014	45.465882
3502.340119	450968.953007	45.470887
3502.568540	450964.501993	45.475892
3502.371994	450969.861257	45.480897
3502.396170	450962.245574	45.485901
3502.646296	450936.884042	45.490906
3502.327574	450904.863260	45.495911
3502.240433	450921.572218	45.500916
3501.910249	450924.567583	45.505921
3501.506666	450918.389632	45.510925
3502.019723	450901.816198	45.515930
3501.861245	450913.157420	45.520935
3502.125668	450970.762293	45.525940
3502.086643	450990.203842	45.530945
3501.844150	450987.654103	45.535949
3501.981386	450972.611741	45.540954
3502.057690	450943.370305	45.545959
3501.756993	450947.071441	45.550964
3502.094611	450943.567322	45.555969
3502.470165	450953.809198	45.560973
3502.457212	450994.255183	45.565978
3502.166532	450997.903982	45.570983
3502.245348	451000.783938	45.575988
3501.843816	450981.411914	45.580993
3501.823618	450987.453731	45.585997
3501.689930	450976.361585	45.591002
3502.496377	450960.249266	45.596007
3502.264298	451006.210364	45.601012
3501.849893	451008.863816	45.606017
3502.190005	450978.261345	45.611021
3502.332955	450965.907576	45.616026
3502.045848	451014.566858	45.621031
3502.341886	450977.628202	45.626036
3502.363175	451011.573345	45.631041
3502.180039	450946.191559	45.636045
3502.350359	450950.985380	45.641050
3502.092768	450973.201742	45.646055
3502.671219	450931.296074	45.651060
3502.487767	450981.106184	45.656065
3502.396749	450957.676177	45.661069
3502.672931	450925.612128	45.666074
3502.502274	450956.035518	45.671079
3502.411039	450960.667701	45.676084
3502.146359	450943.202334	45.681089
3501.844979	450918.942871	45.686093
3502.118737	450928.997867	45.691098
3502.133256	450950.511546	45.696103
3501.973319	450916.791084	45.701108
3502.385084	450923.221342	45.706113
3502.331890	450928.202737	45.711117
3502.280010	450949.473186	45.716122
3502.130429	450930.315018	45.721127
3502.317676	450950.431266	45.726132
3502.411019	450933.822712	45.731137
3501.998939	450933.583318	45.736141
3502.313270	450915.569692	45.741146
3502.000108	450958.955684	45.746151
3502.076456	450951.078024	45.751156
3502.360702	450912.466532	45.756161
3502.149951	450936.197887	45.761165
3502.280847	450964.797508	45.766170
3502.154990	450959.489081	45.771175
3502.289434	450931.659308	45.776180
3502.291815	450966.520924	45.781185
3502.167412	450935.687355	45.786189
3502.532084	450941.617599	45.791194
3502.284810	450924.250957	45.796199
3502.444287	450911.437838	45.801204
3502.357253	450922.311052	45.806209
3502.253775	450893.808409	45.811213
3502.424460	450930.825528	45.816218
3502.018788	450906.379556	45.821223
3502.048593	450897.798799	45.826228
3502.218672	450940.144273	45.831233
3501.635048	450925.012852	45.836237
3502.129255	450907.376748	45.841242
3501.744704	450934.129561	45.846247
3502.051656	450917.842446	45.851252
3501.657437	450964.285967	45.856257
3501.659591	450933.939843	45.861261
3502.688771	450909.368545	45.866266
3502.054181	450931.746033	45.871271
3501.958229	450942.265431	45.876276
3501.710034	450922.513901	45.881281
3502.316823	450912.674796	45.886285
3502.321451	450911.354619	45.891290
3502.315405	450947.638468	45.896295
3502.103445	450946.098805	45.901300
3502.130671	450929.449954	45.906305
3502.008910	450939.364488	45.911309
3502.165435	450951.823039	45.916314
3502.178169	450918.684229	45.921319
3501.999447	450967.630948	45.926324
3501.986960	450968.292547	45.931329
3501.872715	450947.910920	45.936333
3502.178642	450945.781937	45.941338
3501.943412	450969.415637	45.946343
3502.357503	450937.025332	45.951348
3502.186286	450958.213147	45.956353
3502.370515	450967.774826	45.961357
3502.148775	450945.126650	45.966362
3502.469481	450938.884955	45.971367
3502.007550	450956.820277	45.976372
3502.558222	450947.548257	45.981377
3501.869304	450968.411937	45.986381
3502.615966	450930.691538	45.991386
3502.200666	450968.105702	45.996391
3502.277640	450973.776944	46.001396
3502.069430	450947.016262	46.006401
3502.331255	450961.284995	46.011405
3502.233926	450958.763051	46.016410
3502.177584	450932.587289	46.021415
3502.000055	450955.146230	46.026420
3501.891326	450940.903910	46.031425
3502.276856	450925.314814	46.036429
3502.323004	450956.262131	46.041434
3502.176122	450980.287817	46.046439
3502.104967	450938.738578	46.051444
3502.188026	450913.758647	46.056449
3502.095605	450955.485898	46.061453
3502.454447	450926.757976	46.066458
3502.305422	450942.055830	46.071463
3502.003211	450949.309380	46.076468
3502.256254	450922.678737	46.081473
3501.933300	450951.908317	46.086477
3502.302779	450930.384556	46.091482
3502.285095	450952.157051	46.096487
3502.748935	450954.062732	46.101492
3502.368813	450952.042199	46.106497
3502.403108	450944.221930	46.111501
3502.296577	450945.558086	46.116506
3502.324149	450945.401427	46.121511
3502.341210	450923.984116	46.126516
3502.388004	450907.941101	46.131521
3502.300337	450910.948877	46.136525
3502.187142	450905.993654	46.141530
3502.038265	450933.673376	46.146535
3502.329520	450898.308456	46.151540
3502.029448	450939.510361	46.156545
3502.300553	450911.354488	46.161549
3502.278020	450910.850532	46.166554
3502.106438	450935.742841	46.171559
3502.121010	450920.618346	46.176564
3502.118002	450918.893414	46.181569
3502.224387	450919.079515	46.186573
3502.543276	450925.676690	46.191578
3502.177420	450946.793793	46.196583
3502.171507	450903.458090	46.201588
3502.434810	450930.615949	46.206593
3501.986715	450942.713374	46.211597
3502.223394	450917.556927	46.216602
3502.113326	450948.833421	46.221607
3502.095486	450920.418763	46.226612
3502.415403	450935.541001	46.231617
3502.320807	450892.320787	46.236621
3502.438605	450933.202918	46.241626
3501.716203	450910.887580	46.246631
3501.731780	450894.240546	46.251636
3501.990081	450907.545705	46.256641
3501.764938	450938.586676	46.261645
3502.206281	450907.765128	46.266650
3502.301692	450965.548968	46.271655
3501.925788	450965.963544	46.276660
3501.722565	450952.446603	46.281665
3502.341757	450933.268401	46.286669
3502.524378	450969.217919	46.291674
3501.963354	450961.441018	46.296679
3502.554830	450932.574838	46.301684
3502.429270	450935.639345	46.306689
3502.376836	450941.990742	46.311693
3502.590281	450889.638406	46.316698
3502.197443	450935.878783	46.321703
3502.219565	450909.944319	46.326708
3502.213431	450939.428305	46.331713
3502.277291	450913.284265	46.336717
3502.522054	450952.776165	46.341722
3502.247769	450927.801993	46.346727
3502.301299	450916.680223	46.351732
3502.339963	450910.432359	46.356737
3502.368295	450892.108708	46.361741
3502.481233	450889.299790	46.366746
3502.560550	450895.833354	46.371751
3502.437194	450877.279942	46.376756
3502.459536	450898.284977	46.381761
3502.755065	450891.742777	46.386765
3502.656907	450868.415299	46.391770
3502.568692	450867.211287	46.396775
3502.236328	450858.383294	46.401780
3502.708834	450857.242881	46.406785
3502.205764	450859.352164	46.411789
3502.665438	450862.527150	46.416794
3502.320448	450875.978441	46.421799
3502.239472	450831.030612	46.426804
3502.594666	450815.395492	46.431809
3502.144304	450828.406757	46.436813
3502.809538	450791.155714	46.441818
3502.421791	450841.658112	46.446823
3502.857418	450805.001589	46.451828
3502.676868	450833.396876	46.456833
3502.309518	450801.941842	46.461837
3502.287050	450781.799289	46.466842
3502.506679	450818.402885	46.471847
3502.311678	450776.669950	46.476852
3502.633669	450785.499488	46.481857
3502.141851	450810.899265	46.486861
3502.579414	450776.982656	46.491866
3501.989242	450819.042565	46.496871
3502.444309	450789.487332	46.501876
3502.392508	450803.704249	46.506881
3502.013195	450791.635928	46.511885
3502.468447	450765.582088	46.516890
3502.587156	450743.945559	46.521895
3502.256481	450788.654029	46.526900
3502.444654	450766.397591	46.531905
3502.217121	450760.090276	46.536909
3502.589957	450763.735715	46.541914
3502.738032	450731.640903	46.546919
3502.827318	450741.978872	46.551924
3502.295454	450744.853904	46.556929
3502.070113	450723.880692	46.561933
3502.906021	450690.865159	46.566938
3502.310337	450737.493218	46.571943
3502.365246	450754.535062	46.576948
3502.119184	450734.072593	46.581953
3501.813526	450718.186654	46.586957
3502.408969	450679.525580	46.591962
3502.478580	450683.117474	46.596967
3502.029621	450726.779097	46.601972
3502.283232	450715.676348	46.606977
3501.968098	450693.347164	46.611981
3502.127763	450687.181605	46.616986
3502.276572	450706.289223	46.621991
3502.604225	450714.102975	46.626996
3502.511110	450710.869895	46.632001
3502.263093	450707.864285	46.637005
3502.405945	450691.247732	46.642010
3502.433857	450701.290945	46.647015
3501.686454	450704.250800	46.652020
3502.004649	450697.400486	46.657025
3502.051749	450703.583976	46.662029
3501.717153	450703.180092	46.667034
3502.051974	450700.133093	46.672039
3501.826306	450705.497021	46.677044
3501.974933	450700.297382	46.682049
3502.514266	450692.447938	46.687053
3502.257939	450698.882378	46.692058
3501.696398	450707.648630	46.697063
3501.543565	450714.218943	46.702068
3502.135188	450717.271600	46.707073
3501.947219	450717.199758	46.712077
3502.384610	450692.366560	46.717082
3502.204706	450685.747220	46.722087
3502.286138	450711.766930	46.727092
3502.492298	450741.674321	46.732097
3502.455550	450757.664989	46.737101
3502.337307	450738.298725	46.742106
3501.951720	450714.306087	46.747111
3502.581067	450690.457460	46.752116
3502.294349	450745.460484	46.757121
3501.957795	450727.854078	46.762125
3502.460795	450705.091101	46.767130
3502.105745	450728.743988	46.772135
3502.479360	450677.634500	46.777140
3502.620652	450707.501443	46.782145
3502.304307	450719.781140	46.787149
3501.932732	450695.989252	46.792154
3502.783076	450677.028029	46.797159
3502.372498	450683.334619	46.802164
3502.936874	450668.427523	46.807169
3502.250979	450650.673298	46.812173
3502.443781	450687.585818	46.817178
3501.826463	450690.728095	46.822183
3502.020945	450687.906262	46.827188
3502.174956	450684.634113	46.832193
3502.086035	450681.349620	46.837197
3502.290854	450693.749930	46.842202
3502.595784	450699.435951	46.847207
3501.864020	450683.109887	46.852212
3501.388081	450664.916517	46.857217
3501.856730	450674.027389	46.862221
3501.756107	450683.431231	46.867226
3502.159300	450694.024074	46.872231
3502.785975	450680.528023	46.877236
3502.634807	450706.635253	46.882241
3501.947555	450723.083998	46.887245
3502.216753	450705.381818	46.892250
3502.430043	450701.795826	46.897255
3502.288592	450684.818243	46.902260
3502.293228	450677.814507	46.907265
3502.483040	450669.462102	46.912269
3502.931530	450649.244985	46.917274
3502.507544	450642.461233	46.922279
3502.078385	450635.323074	46.927284
3502.248230	450654.072188	46.932289
3502.006867	450659.895322	46.937293
3502.329837	450625.641385	46.942298
3502.386287	450664.300862	46.947303
3502.195640	450675.850269	46.952308
3502.453715	450623.946992	46.957313
3502.466014	450611.004734	46.962317
3502.266521	450644.782332	46.967322
3501.584221	450659.403482	46.972327
3502.275149	450661.374783	46.977332
3502.586295	450657.012125	46.982337
3502.205939	450667.322875	46.987341
3502.054470	450657.958749	46.992346
3502.049014	450656.792391	46.997351
3502.225959	450645.245013	47.002356
3502.768279	450619.633960	47.007361
3502.510573	450617.441807	47.012365
3502.385056	450634.309276	47.017370
3502.087040	450649.072669	47.022375
3502.179128	450638.147655	47.027380
3502.582273	450616.669027	47.032385
3502.272901	450641.075973	47.037389
3502.506015	450644.642027	47.042394
3502.089202	450630.143741	47.047399
3502.000737	450621.124864	47.052404
3502.411340	450614.818125	47.057409
3501.989638	450651.218890	47.062413
3502.023012	450648.574758	47.067418
3501.989622	450661.367964	47.072423
3502.002972	450651.876289	47.077428
3501.910254	450625.350709	47.082433
3501.734656	450639.942518	47.087437
3501.630706	450632.955934	47.092442
3501.836029	450628.204030	47.097447
3501.783348	450629.886914	47.102452
3501.926717	450632.655220	47.107457
3502.114475	450641.912000	47.112461
3502.404640	450652.319745	47.117466
3502.155222	450662.153085	47.122471
3502.069314	450646.739819	47.127476
3502.497662	450599.681188	47.132481
3502.817952	450617.391627	47.137485
3502.060694	450636.541040	47.142490
3502.470171	450648.959768	47.147495
3502.376351	450670.744563	47.152500
3502.351686	450678.512529	47.157505
3502.143948	450666.163291	47.162509
3502.562611	450647.016553	47.167514
3502.706238	450627.964022	47.172519
3502.206683	450617.183270	47.177524
3502.956580	450578.345374	47.182529
3502.839400	450586.990680	47.187533
3502.360329	450560.932069	47.192538
3502.674532	450541.852504	47.197543
3502.947144	450539.779496	47.202548
3502.631698	450539.981537	47.207553
3502.215889	450571.865078	47.212557
3502.199007	450584.858701	47.217562
3502.222240	450567.956491	47.222567
3501.571424	450551.262315	47.227572
3502.338355	450537.033561	47.232577
3502.218809	450522.792694	47.237581
3502.216023	450515.688590	47.242586
3502.290902	450532.727440	47.247591
3502.166675	450539.445520	47.252596
3502.295908	450532.117566	47.257601
3501.975989	450551.705378	47.262605
3502.312031	450566.977547	47.267610
3501.994427	450574.233647	47.272615
3501.962905	450582.307207	47.277620
3502.151931	450554.975815	47.282625
3502.106782	450522.556036	47.287629
3502.055808	450514.089399	47.292634
3501.835207	450525.643616	47.297639
3502.082744	450526.264123	47.302644
3502.248982	450559.933284	47.307649
3501.701411	450574.634681	47.312653
3501.920992	450531.262637	47.317658
3502.343608	450545.201731	47.322663
3502.453299	450554.876857	47.327668
3502.638546	450555.963926	47.332673
3502.459136	450590.195144	47.337677
3502.276461	450565.713561	47.342682
3502.353721	450550.781900	47.347687
3502.571527	450534.051892	47.352692
3502.372044	450584.829566	47.357697
3502.231515	450582.212917	47.362701
3502.249790	450560.845824	47.367706
3502.413129	450563.610981	47.372711
3502.396066	450564.273315	47.377716
3502.259886	450532.375402	47.382721
3501.897979	450532.381802	47.387725
3502.226218	450523.550745	47.392730
3502.442515	450509.104541	47.397735
3502.078384	450499.875462	47.402740
3502.405550	450540.572950	47.407745
3502.171889	450539.138182	47.412749
3502.659138	450514.398406	47.417754
3502.224016	450528.270115	47.422759
3501.433084	450542.350302	47.427764
3502.461034	450536.656400	47.432769
3502.419910	450552.343424	47.437773
3502.102030	450546.151825	47.442778
3502.274781	450534.655802	47.447783
3502.806892	450518.840278	47.452788
3503.233950	450474.369657	47.457793
3502.416756	450495.457024	47.462797
3502.666861	450530.635359	47.467802
3502.558638	450518.777774	47.472807
3502.013951	450508.308583	47.477812
3502.366080	450501.097624	47.482817
3502.206920	450496.454057	47.487821
3502.086903	450499.314760	47.492826
3502.039439	450447.713120	47.497831
3502.101443	450467.240629	47.502836
3502.438881	450482.918604	47.507841
3501.670229	450469.541509	47.512845
3502.245683	450431.542887	47.517850
3502.383668	450487.849538	47.522855
3502.260820	450491.218154	47.527860
3501.954778	450467.720150	47.532865
3502.490502	450455.253273	47.537869
3502.370365	450490.439451	47.542874
3502.407897	450484.648369	47.547879
3502.648727	450457.613153	47.552884
3502.699564	450437.966178	47.557889
3502.714379	450424.363715	47.562893
3502.459145	450424.099519	47.567898
3502.459399	450465.965239	47.572903
3501.752849	450457.449975	47.577908
3502.603148	450417.124293	47.582913
3502.438209	450472.920655	47.587917
3502.262625	450452.193064	47.592922
3502.457320	450422.577031	47.597927
3502.173259	450459.057832	47.602932
3502.129157	450426.942232	47.607937
3502.201058	450408.154592	47.612941
3502.662550	450386.514289	47.617946
3502.300761	450378.147483	47.622951
3502.310045	450405.701339	47.627956
3502.385949	450428.119236	47.632961
3502.212971	450421.092753	47.637965
3502.355107	450420.055291	47.642970
3502.289522	450439.400006	47.647975
3502.393688	450441.058110	47.652980
3502.623530	450423.108205	47.657985
3502.181088	450424.751223	47.662989
3502.051534	450420.001468	47.667994
3502.340467	450414.627346	47.672999
3502.115393	450417.200188	47.678004
3502.068445	450389.398440	47.683009
3502.507922	450363.295896	47.688013
3502.677464	450374.940754	47.693018
3502.560962	450408.401096	47.698023
3502.094139	450426.185361	47.703028
3502.370458	450409.040042	47.708033
3502.072812	450399.292948	47.713037
3502.412612	450383.659972	47.718042
3502.202126	450367.910987	47.723047
3502.272614	450364.499757	47.728052
3502.138486	450355.335755	47.733057
3501.979899	450364.951875	47.738061
3502.096511	450359.097515	47.743066
3502.138889	450379.998359	47.748071
3501.921771	450398.250638	47.753076
3502.407249	450374.931896	47.758081
3502.055426	450367.223216	47.763085
3502.124215	450368.277957	47.768090
3501.789059	450358.638268	47.773095
3501.987174	450358.505393	47.778100
3502.695309	450336.927549	47.783105
3502.097954	450333.774126	47.788109
3502.670038	450329.877626	47.793114
3502.860052	450340.758064	47.798119
3502.203903	450345.378178	47.803124
3502.519294	450344.668551	47.808129
3502.124703	450364.572804	47.813133
3502.009060	450348.199854	47.818138
3502.254730	450365.516308	47.823143
3502.273425	450390.785096	47.828148
3502.009769	450351.599577	47.833153
3502.124544	450335.291687	47.838157
3501.966902	450349.779347	47.843162
3502.048682	450375.900872	47.848167
3501.919678	450370.948033	47.853172
3502.510797	450335.687095	47.858177
3502.390468	450329.565702	47.863181
3502.441888	450321.641023	47.868186
3502.467132	450321.230995	47.873191
3502.401178	450329.157845	47.878196
3502.195765	450337.867938	47.883201
3502.513903	450332.996647	47.888205
3502.456639	450316.411460	47.893210
3502.493340	450306.205499	47.898215
3502.384997	450295.159766	47.903220
3502.496012	450294.634686	47.908225
3501.860215	450303.717307	47.913229
3501.870252	450314.372474	47.918234
3501.805478	450314.839371	47.923239
3502.236809	450302.338169	47.928244
3503.064141	450274.753305	47.933249
3502.121000	450293.171182	47.938253
3502.194873	450292.195252	47.943258
3502.742035	450282.568295	47.948263
3502.091297	450314.286340	47.953268
3502.095778	450312.560179	47.958273
3502.037641	450313.685733	47.963277
3502.238935	450293.608878	47.968282
3502.362668	450343.777771	47.973287
3502.152883	450355.330362	47.978292
3501.898629	450347.910732	47.983297
3501.904307	450342.479877	47.988301
3501.911968	450328.371021	47.993306
3502.312313	450311.764239	47.998311
3502.108836	450323.214355	48.003316
3501.976184	450338.915992	48.008321
3502.153453	450297.884548	48.013325
3502.258423	450341.814557	48.018330
3502.126609	450332.294952	48.023335
3502.173655	450307.675289	48.028340
3502.516741	450333.704808	48.033345
3502.228894	450344.407050	48.038349
3501.966669	450325.113949	48.043354
3501.851502	450314.323038	48.048359
3501.719647	450322.514041	48.053364
3502.348950	450332.766827	48.058369
3502.071210	450338.240564	48.063373
3502.093989	450342.195141	48.068378
3502.054099	450337.735675	48.073383
3502.056398	450348.138316	48.078388
3502.360062	450350.069370	48.083393
3502.419916	450366.552503	48.088397
3502.347926	450345.808441	48.093402
3502.625134	450338.660022	48.098407
3502.464615	450281.240014	48.103412
3502.460005	450280.682464	48.108417
3502.290426	450296.237727	48.113421
3502.185689	450294.224348	48.118426
3501.825796	450306.308161	48.123431
3502.059723	450330.071335	48.128436
3502.154524	450334.572741	48.133441
3502.196736	450331.774937	48.138445
3502.110622	450337.472116	48.143450
3502.639794	450328.000262	48.148455
3502.220003	450321.165005	48.153460
3502.362776	450307.187019	48.158465
3503.119613	450288.088021	48.163469
3503.194444	450261.078817	48.168474
3502.549477	450281.530189	48.173479
3502.000186	450281.819944	48.178484
3502.284372	450261.577718	48.183489
3502.199455	450263.570205	48.188493
3502.438013	450250.693474	48.193498
3503.163703	450222.058931	48.198503
3502.901795	450206.064231	48.203508
3502.814166	450200.191370	48.208513
3502.900643	450225.500369	48.213517
3502.382083	450206.958147	48.218522
3502.522670	450174.863751	48.223527
3502.515557	450187.551569	48.228532
3502.434217	450213.749809	48.233537
3501.986345	450188.954521	48.238541
3502.431795	450170.818098	48.243546
3502.626598	450154.903407	48.248551
3502.429017	450188.935100	48.253556
3502.370873	450152.254109	48.258561
3502.938222	450138.513388	48.263565
3502.736409	450181.477252	48.268570
3502.169968	450128.333037	48.273575
3502.209878	450118.938441	48.278580
3502.533250	450127.565023	48.283585
3502.528749	450128.732855	48.288589
3502.143164	450124.277248	48.293594
3502.160611	450118.032526	48.298599
3502.241359	450120.506308	48.303604
3502.039624	450117.341063	48.308609
3502.757522	450101.140657	48.313613
3502.760832	450096.775810	48.318618
3502.593830	450069.347888	48.323623
3502.335931	450061.776500	48.328628
3502.327311	450057.210543	48.333633
3502.466012	450050.033183	48.338637
3502.239626	450099.344497	48.343642
3502.240628	450082.090218	48.348647
3502.573181	450048.442884	48.353652
3502.426960	450057.600451	48.358657
3502.513034	450095.494982	48.363661
3502.243203	450048.647098	48.368666
3502.508172	450023.485212	48.373671
3502.008388	450040.158539	48.378676
3501.901976	450052.659138	48.383681
3502.291503	450016.516133	48.388685
3502.155574	450023.946675	48.393690
3502.254172	450051.689821	48.398695
3502.091558	450073.080072	48.403700
3502.226486	450064.685379	48.408705
3502.072532	450033.246315	48.413709
3502.698350	450009.702034	48.418714
3502.687276	450014.524724	48.423719
3502.283898	450018.749712	48.428724
3502.682624	449999.554847	48.433729
3502.497984	450019.020226	48.438733
3502.009542	450025.440797	48.443738
3502.624314	449989.008406	48.448743
3502.330532	450033.915485	48.453748
3502.224839	450022.006499	48.458753
3502.387034	450003.813227	48.463757
3501.959658	450024.230428	48.468762
3502.459048	449996.849319	48.473767
3502.310351	450036.861703	48.478772
3502.337116	450003.262642	48.483777
3502.480382	450022.574689	48.488781
3502.059584	449982.601432	48.493786
3502.332930	449991.388214	48.498791
3502.151894	449973.249177	48.503796
3502.169412	449989.587028	48.508801
3502.586642	449954.961972	48.513805
3502.084445	449987.265950	48.518810
3502.424885	449949.861915	48.523815
3502.159323	449991.719761	48.528820
3501.853513	449976.696044	48.533825
3502.617409	449948.156621	48.538829
3502.340598	449962.308127	48.543834
3502.180018	450010.239044	48.548839
3502.383846	449981.280723	48.553844
3502.254555	449965.417135	48.558849
3501.671212	449978.855875	48.563853
3501.603221	449976.633670	48.568858
3502.233211	449965.674056	48.573863
3502.079971	449962.145891	48.578868
3502.743748	449950.419716	48.583873
3502.721537	449956.360624	48.588877
3502.143891	449928.388479	48.593882
3502.554472	449919.594926	48.598887
3502.345142	449917.851787	48.603892
3502.798427	449908.645498	48.608897
3502.421597	449958.995844	48.613901
3502.281173	449966.934589	48.618906
3502.435736	449927.530002	48.623911
3502.261193	449920.351372	48.628916
3502.019132	449894.457536	48.633921
3502.521170	449882.604652	48.638925
3502.490808	449883.878080	48.643930
3502.460143	449897.584733	48.648935
3501.632797	449920.196652	48.653940
3501.663878	449912.833272	48.658945
3501.722654	449920.233068	48.663949
3502.154021	449891.289413	48.668954
3502.681025	449914.093225	48.673959
3502.334445	449945.712941	48.678964
3502.069454	449943.217390	48.683969
3502.174380	449922.292740	48.688973
3501.918726	449923.297295	48.693978
3502.562955	449898.329059	48.698983
3502.138249	449944.322706	48.703988
3502.089196	449930.425565	48.708993
3501.984036	449914.558129	48.713997
3502.116671	449901.444211	48.719002
3502.212056	449937.206127	48.724007
3502.037155	449952.001247	48.729012
3501.980446	449926.382632	48.734017
3502.347689	449910.136030	48.739021
3502.086578	449934.536087	48.744026
3502.132219	449951.123257	48.749031
3502.212618	449921.981383	48.754036
3502.486989	449960.100107	48.759041
3502.210532	449941.570149	48.764045
3502.549652	449917.512873	48.769050
3502.504040	449928.024772	48.774055
3502.296080	449921.054415	48.779060
3502.407340	449886.122391	48.784065
3502.287649	449886.597977	48.789069
3502.080953	449931.288496	48.794074
3502.331861	449933.735400	48.799079
3501.952627	449950.541977	48.804084
3502.453245	449947.773157	48.809089
3502.304373	449930.694700	48.814093
3501.669815	449918.361787	48.819098
3502.814089	449900.926647	48.824103
3502.609426	449889.591462	48.829108
3502.379924	449924.085317	48.834113
3502.605241	449921.816741	48.839117
3502.504318	449903.309752	48.844122
3502.519377	449891.229368	48.849127
3501.907187	449882.191498	48.854132
3502.421495	449861.202079	48.859137
3502.664675	449853.297674	48.864141
3502.220095	449888.434554	48.869146
3502.325012	449901.561548	48.874151
3502.041660	449892.217961	48.879156
3501.838239	449886.566315	48.884161
3502.003320	449882.277351	48.889165
3502.684124	449854.207678	48.894170
3502.503269	449867.938090	48.899175
3501.945621	449865.133559	48.904180
3502.373806	449829.034900	48.909185
3502.274787	449864.370929	48.914189
3501.931399	449849.556061	48.919194
3502.504459	449818.965990	48.924199
3502.456009	449867.183963	48.929204
3502.117951	449878.960058	48.934209
3502.209652	449864.837637	48.939213
3502.298528	449837.977965	48.944218
3502.455042	449840.998027	48.949223
3501.852780	449865.452085	48.954228
3502.485408	449817.090887	48.959233
3502.251812	449831.946109	48.964237
3501.837620	449863.272139	48.969242
3502.007212	449878.621821	48.974247
3501.960247	449847.064098	48.979252
3502.076004	449838.723102	48.984257
3502.436776	449825.979060	48.989261
3502.211815	449864.938091	48.994266
3502.103803	449862.214725	48.999271
3501.418864	449860.039288	49.004276
3502.166044	449832.872555	49.009281
3502.073118	449843.848701	49.014285
3501.944612	449870.917494	49.019290
3502.203489	449834.185888	49.024295
3502.310757	449862.029385	49.029300
3501.990611	449876.289288	49.034305
3501.980154	449849.293089	49.039309
3502.085305	449850.088367	49.044314
3502.289754	449887.000318	49.049319
3501.976042	449887.100593	49.054324
3502.417318	449844.402691	49.059329
3502.108156	449850.845717	49.064333
3501.998730	449887.452049	49.069338
3502.147027	449873.929659	49.074343
3502.302606	449861.979290	49.079348
3502.532850	449843.419902	49.084353
3502.432301	449866.576703	49.089357
3502.212775	449855.700580	49.094362
3502.399039	449836.336176	49.099367
3501.907680	449824.488054	49.104372
3502.286092	449823.463963	49.109377
3502.424253	449825.928702	49.114381
3502.545180	449795.257829	49.119386
3502.443167	449842.063381	49.124391
3502.407289	449825.220723	49.129396
3502.658887	449802.039877	49.134401
3502.162291	449832.161026	49.139405
3502.282153	449828.944903	49.144410
3502.334524	449800.670021	49.149415
3501.844904	449802.574279	49.154420
3502.041104	449782.650032	49.159425
3502.817406	449764.308749	49.164429
3502.611098	449764.290551	49.169434
3502.451155	449811.257566	49.174439
3502.484931	449808.004301	49.179444
3501.981600	449789.713078	49.184449
3502.405504	449766.403462	49.189453
3502.232227	449774.956441	49.194458
3502.270960	449807.682636	49.199463
3501.834623	449762.890412	49.204468
3502.586898	449735.570517	49.209473
3502.534437	449760.242261	49.214477
3502.136816	449776.544391	49.219482
3502.593627	449739.933590	49.224487
3502.011619	449779.710425	49.229492
3502.129452	449729.146767	49.234497
3502.280649	449773.628768	49.239501
3501.713967	449774.428756	49.244506
3502.431135	449749.245839	49.249511
3502.096717	449758.027289	49.254516
3502.702035	449741.590691	49.259521
3502.426995	449730.368050	49.264525
3502.344018	449738.247044	49.269530
3502.288268	449769.161301	49.274535
3502.074479	449775.437027	49.279540
3501.966822	449740.031912	49.284545
3501.843465	449725.892654	49.289549
3502.219895	449729.131706	49.294554
3502.250955	449770.334084	49.299559
3502.024766	449753.166223	49.304564
3502.227207	449725.679494	49.309569
3502.178678	449725.484110	49.314573
3501.993768	449761.747337	49.319578
3502.073875	449742.501131	49.324583
3501.823743	449736.400101	49.329588
3502.522289	449715.482923	49.334593
3502.568700	449742.879451	49.339597
3502.185865	449768.922859	49.344602
3502.201864	449751.006241	49.349607
3502.097904	449734.580264	49.354612
3502.465314	449710.518303	49.359617
3502.380852	449723.167853	49.364621
3501.907801	449777.492147	49.369626
3501.896023	449775.819264	49.374631
3501.986306	449778.342324	49.379636
3502.368943	449762.093186	49.384641
3502.241462	449775.003248	49.389645
3501.821672	449780.144335	49.394650
3502.464653	449774.714099	49.399655
3501.834001	449775.371956	49.404660
3502.032948	449763.262436	49.409665
3502.177207	449752.075019	49.414669
3501.832960	449755.580235	49.419674
3502.165245	449753.852961	49.424679
3502.275661	449776.925754	49.429684
3502.239295	449761.453321	49.434689
3501.951217	449756.119514	49.439693
3502.623494	449749.162202	49.444698
3502.666184	449735.554930	49.449703
3502.117899	449753.860064	49.454708
3501.779402	449763.149637	49.459713
3502.319178	449744.541240	49.464717
3502.411489	449755.335901	49.469722
3502.678298	449724.235890	49.474727
3502.439320	449701.233990	49.479732
3502.287848	449744.190702	49.484737
3502.409525	449756.503160	49.489741
3502.201352	449737.251774	49.494746
3502.066246	449723.266616	49.499751
3502.248602	449726.840836	49.504756
3502.158470	449746.190007	49.509761
3502.148886	449725.435527	49.514765
3501.996528	449706.073795	49.519770
3502.201066	449725.833135	49.524775
3502.254043	449731.305483	49.529780
3502.377481	449720.781066	49.534785
3502.629867	449731.702678	49.539789
3502.127311	449722.951903	49.544794
3502.362973	449682.316128	49.549799
3502.326699	449664.813692	49.554804
3502.703665	449659.679222	49.559809
3501.999342	449687.498979	49.564813
3502.159941	449688.742231	49.569818
3502.766290	449656.877982	49.574823
3502.633564	449654.412239	49.579828
3502.944847	449652.992768	49.584833
3502.195475	449653.263409	49.589837
3502.279454	449659.035362	49.594842
3502.761012	449677.583743	49.599847
3502.373246	449673.280638	49.604852
3502.848425	449669.348600	49.609857
3502.511784	449664.479182	49.614861
3502.429496	449639.168783	49.619866
3502.102606	449603.138389	49.624871
3501.743176	449576.704522	49.629876
3502.216684	449586.018049	49.634881
3502.518889	449574.399592	49.639885
3501.989934	449602.496218	49.644890
3501.488804	449607.345711	49.649895
3502.152483	449582.526309	49.654900
3502.378050	449576.096297	49.659905
3502.215347	449602.663324	49.664909
3502.185957	449641.541063	49.669914
3502.306123	449633.453038	49.674919
3502.167356	449647.075430	49.679924
3502.095626	449643.585080	49.684929
3501.962224	449616.303557	49.689933
3501.993796	449622.692782	49.694938
3502.083550	449632.320695	49.699943
3502.172689	449637.838096	49.704948
3502.086004	449648.813347	49.709953
3501.883390	449645.089946	49.714957
3501.940835	449656.397647	49.719962
3502.354802	449633.647699	49.724967
3502.453912	449638.554546	49.729972
3502.250600	449622.651678	49.734977
3502.452721	449635.357469	49.739981
3501.915167	449622.907568	49.744986
3502.148418	449617.440570	49.749991
3502.725953	449610.954929	49.754996
3502.430641	449643.683411	49.760001
3502.464235	449608.560256	49.765005
3502.226469	449582.462402	49.770010
3502.326086	449585.339245	49.775015
3501.905202	449601.594426	49.780020
3501.816827	449606.936902	49.785025
3502.031019	449613.956989	49.790029
3501.818408	449617.187675	49.795034
3502.004619	449618.071644	49.800039
3501.776320	449628.054326	49.805044
3502.022357	449613.298377	49.810049
3502.435116	449596.790620	49.815053
3502.205385	449630.371476	49.820058
3502.338492	449651.207884	49.825063
3502.246556	449620.976416	49.830068
3501.873437	449600.786775	49.835073
3502.324321	449588.282100	49.840077
3502.186682	449571.201604	49.845082
3502.148210	449601.149134	49.850087
3502.077613	449621.155049	49.855092
3502.072563	449598.572802	49.860097
3502.047627	449579.647557	49.865101
3502.588857	449571.442201	49.870106
3502.388018	449577.005456	49.875111
3502.645201	449574.985552	49.880116
3502.245075	449589.410518	49.885121
3502.528272	449578.860783	49.890125
3502.417923	449574.006322	49.895130
3502.288193	449599.147186	49.900135
3502.005368	449611.066930	49.905140
3502.239624	449623.615403	49.910145
3502.672646	449604.770030	49.915149
3502.321164	449607.261446	49.920154
3502.375543	449599.894284	49.925159
3502.442751	449585.065090	49.930164
3502.027049	449572.037668	49.935169
3502.677105	449550.214537	49.940173
3502.462764	449537.155265	49.945178
3502.509926	449532.529638	49.950183
3502.453648	449527.057639	49.955188
3502.333197	449569.654529	49.960193
3502.625111	449559.763136	49.965197
3502.307529	449561.944708	49.970202
3502.329923	449550.725710	49.975207
3502.233400	449554.547034	49.980212
3501.973338	449543.321935	49.985217
3502.559872	449506.182778	49.990221
3502.368524	449502.406825	49.995226
3502.226591	449536.582918	50.000231
3501.926012	449543.887394	50.005236
3501.756396	449524.832731	50.010241
3502.765334	449505.084262	50.015245
3502.624179	449488.917734	50.020250
3502.484354	449473.258471	50.025255
3502.344002	449511.341991	50.030260
3502.009743	449498.453899	50.035265
3502.535642	449467.464835	50.040269
3502.343015	449459.324699	50.045274
3502.612560	449509.167847	50.050279
3502.189641	449506.443471	50.055284
3502.567164	449463.907197	50.060289
3502.844913	449478.631062	50.065293
3502.533161	449436.051452	50.070298
3502.358222	449447.751229	50.075303
3502.357587	449475.206256	50.080308
3501.881263	449453.814836	50.085313
3502.540942	449426.864460	50.090317
3502.372116	449437.497554	50.095322
3502.107327	449461.797189	50.100327
3501.811833	449447.532729	50.105332
3502.578543	449422.290880	50.110337
3502.673782	449441.255760	50.115341
3501.835892	449462.195083	50.120346
3502.070492	449432.622233	50.125351
3502.220770	449414.836376	50.130356
3502.628015	449399.750317	50.135361
3502.668975	449405.782876	50.140365
3501.970619	449415.738457	50.145370
3502.186482	449421.489621	50.150375
3501.645863	449421.879510	50.155380
3501.703585	449434.658986	50.160385
3502.863648	449405.904030	50.165389
3502.115790	449422.160274	50.170394
3502.241552	449413.157812	50.175399
3502.223646	449416.357747	50.180404
3501.885720	449463.861083	50.185409
3502.215009	449466.041903	50.190413
3502.134401	449468.439766	50.195418
3502.225548	449475.327100	50.200423
3502.055015	449464.595295	50.205428
3501.883043	449444.069229	50.210433
3502.310267	449438.419280	50.215437
3501.740058	449435.109195	50.220442
3502.129730	449415.763036	50.225447
3502.244117	449463.702358	50.230452
3502.097370	449463.573246	50.235457
3502.356408	449432.271081	50.240461
3502.392487	449423.638040	50.245466
3502.549794	449459.492397	50.250471
3502.263167	449417.923754	50.255476
3502.208374	449376.166143	50.260481
3502.235204	449409.909753	50.265485
3501.745984	449427.596820	50.270490
3501.952533	449408.381100	50.275495
3501.642284	449408.277834	50.280500
3501.688386	449429.838676	50.285505
3501.910323	449431.427485	50.290509
3501.728255	449445.107589	50.295514
3502.613271	449423.399444	50.300519
3502.381163	449424.654040	50.305524
3502.287461	449430.504886	50.310529
3502.609504	449426.647764	50.315533
3502.446026	449412.159418	50.320538
3502.843800	449393.776186	50.325543
3502.318832	449379.903200	50.330548
3502.292631	449420.252518	50.335553
3502.168483	449431.893526	50.340557
3502.032293	449414.508194	50.345562
3502.752999	449383.335978	50.350567
3502.357105	449420.343569	50.355572
3502.045441	449447.594053	50.360577
3502.386697	449445.510099	50.365581
3501.919916	449438.022276	50.370586
3502.255776	449428.986608	50.375591
3502.395009	449386.335615	50.380596
3502.248789	449344.440154	50.385601
3502.728525	449348.728654	50.390605
3502.567992	449346.165777	50.395610
3502.565681	449337.082033	50.400615
3502.625379	449358.843786	50.405620
3502.431679	449364.304465	50.410625
3502.510015	449319.379281	50.415629
3502.075884	449323.558505	50.420634
3502.290066	449364.631153	50.425639
3502.246610	449376.919167	50.430644
3502.577039	449377.374357	50.435649
3502.654232	449374.520159	50.440653
3502.118803	449379.019880	50.445658
3502.319511	449363.611204	50.450663
3502.289739	449370.923675	50.455668
3502.023116	449380.354283	50.460673
3502.289558	449345.396919	50.465677
3501.963944	449334.537324	50.470682
3502.309133	449295.609024	50.475687
3502.477518	449336.739710	50.480692
3502.355683	449320.925254	50.485697
3501.967609	449303.224415	50.490701
3501.837656	449294.668322	50.495706
3502.729953	449278.947269	50.500711
3502.407807	449274.176975	50.505716
3502.129824	449329.181960	50.510721
3502.349689	449305.548898	50.515725
3502.024326	449278.551070	50.520730
3501.868911	449317.398522	50.525735
3501.890950	449307.346688	50.530740
3501.645711	449269.881901	50.535745
3501.944063	449193.508036	50.540749
3501.746530	449196.584148	50.545754
3501.758278	449117.667133	50.550759
3501.580174	449040.251600	50.555764
3501.431529	448950.346729	50.560769
3501.962531	448892.712489	50.565773
3501.455639	448789.059673	50.570778
3501.377733	448645.550332	50.575783
3501.224247	448563.612550	50.580788
3500.526801	448444.255659	50.585793
3500.406187	448294.863833	50.590797
3500.355114	448146.627347	50.595802
3500.165725	447985.470091	50.600807
3499.931295	447854.110337	50.605812
3499.332093	447738.439234	50.610817
3498.992740	447538.527823	50.615821
3498.682582	447376.319687	50.620826
3498.524200	447234.996856	50.625831
3498.306184	447034.655975	50.630836
3497.750539	446831.575289	50.635841
3497.928513	446611.729343	50.640845
3497.277525	446423.277593	50.645850
3496.954773	446228.478772	50.650855
3497.104304	445983.659771	50.655860
3496.152068	445763.832390	50.660865
3495.627137	445585.454632	50.665869
3495.056396	445335.311851	50.670874
3495.039105	445081.069083	50.675879
3494.443412	444891.429059	50.680884
3493.503760	444639.966860	50.685889
3493.564115	444371.441037	50.690893
3493.081201	444130.053198	50.695898
3492.439018	443921.377864	50.700903
3491.869974	443656.090717	50.705908
3491.403559	443397.281912	50.710913
3490.729650	443134.594461	50.715917
3490.059997	442874.289334	50.720922
3489.311239	442622.928241	50.725927
3488.821346	442353.705565	50.730932
3488.390111	442092.034519	50.735937
3488.152206	441821.040142	50.740941
3487.829285	441562.899842	50.745946
3487.358423	441302.038848	50.750951
3487.063858	441026.780301	50.755956
3486.558123	440701.546465	50.760961
3486.184894	440415.657794	50.765965
3485.399480	440098.887656	50.770970
3484.973340	439800.536582	50.775975
3483.744019	439530.587541	50.780980
3483.063950	439250.851636	50.785985
3483.270274	438964.727655	50.790989
3482.320695	438668.603473	50.795994
3481.648342	438346.944431	50.800999
3481.053943	438058.423421	50.806004
3480.113986	437763.505523	50.811009
3480.119417	437437.691174	50.816013
3479.245619	437137.703466	50.821018
3478.708480	436821.055520	50.826023
3477.659285	436507.048721	50.831028
3476.877488	436196.880132	50.836033
3476.932019	435871.037779	50.841037
3475.410870	435589.692996	50.846042
3475.065113	435280.535981	50.851047
3474.811506	434948.967203	50.856052
3474.080583	434692.191444	50.861057
3473.447971	434363.975643	50.866061
3472.949070	434048.048792	50.871066
3471.929531	433711.887868	50.876071
3471.617864	433409.075900	50.881076
3470.701225	433101.023858	50.886081
3470.596226	432747.845992	50.891085
3469.626958	432464.729201	50.896090
3469.124189	432107.441225	50.901095
3468.403204	431824.963790	50.906100
3467.251041	431481.888099	50.911105
3467.148936	431140.724123	50.916109
3466.168291	430852.843079	50.921114
3465.478519	430545.791420	50.926119
3464.389813	430213.735333	50.931124
3464.189940	429882.728066	50.936129
3463.581167	429556.936409	50.941133
3462.756977	429275.895326	50.946138
3462.106691	428927.958084	50.951143
3461.517106	428641.794128	50.956148
3460.719560	428293.948047	50.961153
3460.050477	428006.647015	50.966157
3459.154019	427668.814501	50.971162
3459.010154	427349.372993	50.976167
3458.664092	427020.003991	50.981172
3457.594319	426695.291505	50.986177
3456.736733	426410.746091	50.991181
3456.270560	426102.718887	50.996186
3455.332271	425777.288819	51.001191
3454.726567	425442.531781	51.006196
3453.444179	425117.452980	51.011201
3453.102747	424776.067643	51.016205
3452.352752	424511.271256	51.021210
3451.673893	424159.492387	51.026215
3451.624582	423816.524899	51.031220
3450.243490	423539.626853	51.036225
3449.635682	423194.250667	51.041229
3448.997595	422889.719685	51.046234
3448.131631	422572.622367	51.051239
3448.379649	422230.248578	51.056244
3447.142478	421962.151701	51.061249
3446.320836	421632.107115	51.066253
3445.508431	421293.115517	51.071258
3444.811741	421006.862884	51.076263
3444.266588	420679.379801	51.081268
3443.490259	420351.904043	51.086273
3443.031577	420030.750539	51.091277
3442.110491	419759.457951	51.096282
3441.231410	419463.590408	51.101287
3440.356003	419132.559592	51.106292
3440.025966	418796.052900	51.111297
3439.564977	418492.284488	51.116301
3438.359539	418223.511849	51.121306
3437.594526	417879.593990	51.126311
3437.748787	417543.834337	51.131316
3436.617914	417249.050648	51.136321
3435.964363	416959.269721	51.141325
3434.873515	416688.279631	51.146330
3434.247926	416358.041036	51.151335
3433.913382	416021.477100	51.156340
3432.647362	415760.186116	51.161345
3432.424413	415453.603997	51.166349
3431.295725	415125.361901	51.171354
3431.135796	414804.559982	51.176359
3430.519837	414532.839498	51.181364
3429.335027	414205.256568	51.186369
3429.133173	413916.491898	51.191373
3428.538136	413633.249538	51.196378
3427.445722	413303.024816	51.201383
3427.023033	413003.690386	51.206388
3425.973792	412694.999490	51.211393
3425.877210	412409.887917	51.216397
3424.689095	412111.961451	51.221402
3424.037494	411780.303349	51.226407
3423.625326	411504.736654	51.231412
3422.339938	411192.357546	51.236417
3421.619301	410927.532463	51.241421
3420.924989	410587.558378	51.246426
3419.860711	410328.830370	51.251431
3419.530360	410026.325903	51.256436
3418.290888	409735.778973	51.261441
3417.650630	409446.837169	51.266445
3417.091289	409173.864581	51.271450
3416.206833	408886.480854	51.276455
3416.931218	408569.309616	51.281460
3415.378556	408311.836118	51.286465
3414.533180	408045.252109	51.291469
3414.080258	407737.661577	51.296474
3413.500973	407419.363082	51.301479
3412.973972	407162.302329	51.306484
3411.992125	406894.687964	51.311489
3411.359142	406568.968090	51.316493
3411.189214	406261.521479	51.321498
3410.513967	405974.026735	51.326503
3409.689773	405723.278738	51.331508
3408.426703	405418.284104	51.336513
3407.915016	405105.314064	51.341517
3407.349117	404825.365556	51.346522
3406.685747	404548.886653	51.351527
3405.860545	404252.478601	51.356532
3405.281111	403972.905941	51.361537
3404.886634	403709.721224	51.366541
3403.967378	403426.740726	51.371546
3403.080596	403122.909929	51.376551
3402.952751	402804.010381	51.381556
3401.836051	402524.230381	51.386561
3401.144796	402287.541380	51.391565
3400.617137	401978.686343	51.396570
3399.829502	401656.295696	51.401575
3399.328853	401426.179185	51.406580
3398.372252	401148.853024	51.411585
3397.949375	400835.547532	51.416589
3397.361754	400532.560143	51.421594
3396.234302	400269.793698	51.426599
3395.689924	400002.687747	51.431604
3395.094949	399712.124460	51.436609
3394.272006	399418.112005	51.441613
3393.705753	399150.163698	51.446618
3392.878099	398851.342368	51.451623
3392.331213	398591.216201	51.456628
3391.805569	398280.648113	51.461633
3391.098021	398039.787217	51.466637
3390.242855	397717.826157	51.471642
3389.447965	397477.712253	51.476647
3389.092686	397159.658067	51.481652
3387.765379	396912.073817	51.486657
3387.445600	396605.728631	51.491661
3386.814717	396345.725391	51.496666
3385.901777	396077.985218	51.501671
3385.499352	395787.942032	51.506676
3384.694730	395497.146409	51.511681
3384.113686	395254.847276	51.516685
3383.151049	394976.809588	51.521690
3382.371922	394680.155413	51.526695
3382.147926	394434.615958	51.531700
3381.015045	394164.581904	51.536705
3380.814180	393846.853666	51.541709
3380.000907	393626.521503	51.546714
3378.946854	393332.162022	51.551719
3378.670394	393035.795582	51.556724
3377.724542	392760.737574	51.561729
3377.416229	392537.826920	51.566733
3376.221526	392250.726917	51.571738
3375.744405	391956.823949	51.576743
3375.000844	391702.702365	51.581748
3374.120558	391470.645532	51.586753
3373.800063	391186.882041	51.591757
3373.023785	390899.247143	51.596762
3372.623173	390607.812683	51.601767
3372.194436	390379.771082	51.606772
3371.192397	390108.718772	51.611777
3370.926973	389801.974288	51.616781
3369.632037	389570.530011	51.621786
3369.136417	389260.638779	51.626791
3368.932353	389015.185414	51.631796
3367.833909	388728.448537	51.636801
3367.079689	388463.498337	51.641805
3366.306970	388186.292323	51.646810
3365.300170	387929.464595	51.651815
3364.983936	387666.371928	51.656820
3363.941498	387386.125504	51.661825
3363.120936	387150.598267	51.666829
3362.806220	386855.000252	51.671834
3361.880023	386637.261971	51.676839
3361.832712	386351.382784	51.681844
3360.703782	386083.880681	51.686849
3360.335500	385828.539372	51.691853
3359.556795	385546.635089	51.696858
3358.875465	385302.910716	51.701863
3358.272115	385015.328981	51.706868
3357.126383	384767.046060	51.711873
3356.838762	384484.572885	51.716877
3356.188487	384248.593361	51.721882
3355.197785	383975.077793	51.726887
3355.098546	383724.460762	51.731892
3354.623112	383446.434687	51.736897
3353.547095	383198.969659	51.741901
3352.728323	382903.572656	51.746906
3351.867087	382672.525164	51.751911
3351.660588	382384.886051	51.756916
3350.774903	382135.501972	51.761921
3349.980498	381861.762118	51.766925
3349.531415	381608.058193	51.771930
3348.767942	381351.045070	51.776935
3348.250739	381072.779441	51.781940
3347.556896	380833.657314	51.786945
3346.974202	380550.769302	51.791949
3346.150906	380278.676037	51.796954
3345.215129	380032.872570	51.801959
3344.935106	379772.949319	51.806964
3344.165751	379502.241032	51.811969
3343.797863	379223.124683	51.816973
3342.925861	378982.696792	51.821978
3342.175608	378711.395042	51.826983
3340.931350	378459.704087	51.831988
3340.471608	378181.307113	51.836993
3340.099276	377946.084551	51.841997
3339.434064	377648.563116	51.847002
3338.544576	377429.647527	51.852007
3338.078530	377135.015948	51.857012
3337.077046	376911.460384	51.862017
3336.700863	376634.260404	51.867021
3336.299924	376381.354676	51.872026
3335.318769	376101.219737	51.877031
3334.845023	375862.338112	51.882036
3333.914312	375610.274490	51.887041
3333.689613	375324.494665	51.892045
3332.939822	375046.935966	51.897050
3332.368487	374838.868868	51.902055
3331.684633	374543.871416	51.907060
3330.565687	374293.203136	51.912065
3329.990494	374017.365130	51.917069
3329.122871	373776.142480	51.922074
3328.485377	373524.223240	51.927079
3327.710053	373247.648627	51.932084
3326.950224	373002.359683	51.937089
3326.199434	372748.418574	51.942093
3325.761107	372490.559743	51.947098
3324.884560	372240.883824	51.952103
3324.315555	372004.182855	51.957108
3323.553808	371723.449437	51.962113
3322.864643	371496.380862	51.967117
3322.989746	371221.889283	51.972122
3321.548594	370964.892116	51.977127
3321.227088	370695.581277	51.982132
3319.873820	370472.860847	51.987137
3319.838878	370199.202137	51.992141
3319.027599	369977.207527	51.997146
3318.653284	369719.957879	52.002151
3317.555574	369446.131771	52.007156
3316.743879	369212.837476	52.012161
3316.171540	368950.424593	52.017165
3315.603805	368676.637045	52.022170
3315.172028	368454.243921	52.027175
3314.767753	368186.406259	52.032180
3313.991215	367935.748297	52.037185
3313.337852	367680.337201	52.042189
3312.546606	367415.481924	52.047194
3311.225574	367183.097045	52.052199
3311.169163	366916.188956	52.057204
3310.016362	366680.645423	52.062209
3309.286045	366421.677323	52.067213
3308.640648	366175.008700	52.072218
3308.136248	365909.157767	52.077223
3307.649712	365704.340795	52.082228
3306.762356	365441.702652	52.087233
3306.295103	365178.106024	52.092237
3305.819004	364948.680109	52.097242
3304.898045	364685.381395	52.102247
3304.142134	364422.462167	52.107252
3303.695515	364198.727285	52.112257
3302.609831	363940.895396	52.117261
3302.405673	363671.345460	52.122266
3301.386369	363470.266777	52.127271
3301.143288	363187.336402	52.132276
3300.435258	362940.634864	52.137281
3300.058848	362680.393781	52.142285
3299.220800	362449.486057	52.147290
3298.462002	362191.007567	52.152295
3297.979509	361919.735862	52.157300
3297.101141	361687.024172	52.162305
3296.692154	361427.086685	52.167309
3295.939126	361154.861029	52.172314
3294.801152	360934.222547	52.177319
3294.615239	360655.313879	52.182324
3293.443084	360431.116054	52.187329
3292.906713	360169.792365	52.192333
3292.373982	359908.619368	52.197338
3291.290827	359675.446839	52.202343
3291.057060	359427.532482	52.207348
3290.114084	359202.198523	52.212353
3289.400731	358923.414222	52.217357
3288.849368	358689.872960	52.222362
3288.094391	358425.724448	52.227367
3287.384345	358213.047233	52.232372
3286.544791	357949.342159	52.237377
3286.050193	357695.251178	52.242381
3285.595730	357475.354179	52.247386
3284.695513	357223.055393	52.252391
3284.164231	356964.793070	52.257396
3283.431276	356722.695363	52.262401
3282.622907	356486.028875	52.267405
3282.489708	356210.980303	52.272410
3281.487095	356006.916074	52.277415
3281.119309	355720.526533	52.282420
3280.265425	355516.360470	52.287425
3278.932348	355249.970898	52.292429
3278.975310	354977.916223	52.297434
3277.906556	354785.411380	52.302439
3277.647162	354488.945485	52.307444
3276.457725	354293.098618	52.312449
3275.921552	354020.926931	52.317453
3275.333841	353802.943898	52.322458
3274.663660	353563.340871	52.327463
3274.182524	353289.578803	52.332468
3272.939817	353088.315067	52.337473
3272.180758	352815.434345	52.342477
3271.666740	352587.738202	52.347482
3271.482588	352357.851092	52.352487
3270.615864	352109.721322	52.357492
3269.933770	351875.635258	52.362497
3269.530195	351630.967612	52.367501
3268.897252	351379.667075	52.372506
3267.806836	351159.742129	52.377511
3267.676958	350892.300346	52.382516
3266.246523	350666.089925	52.387521
3266.036889	350415.074276	52.392525
3265.314431	350201.933591	52.397530
3264.535909	349924.663724	52.402535
3264.040878	349709.779920	52.407540
3263.452589	349466.989739	52.412545
3262.756638	349208.053747	52.417549
3261.952661	348988.252951	52.422554
3261.656741	348734.010948	52.427559
3260.794793	348492.608758	52.432564
3260.074860	348236.700843	52.437569
3259.312959	348021.114644	52.442573
3259.233266	347762.583538	52.447578
3258.596726	347514.320299	52.452583
3257.548923	347279.050903	52.457588
3256.746126	347023.557866	52.462593
3256.326711	346808.014708	52.467597
3255.465318	346539.420644	52.472602
3254.581595	346314.735167	52.477607
3254.209859	346052.755502	52.482612
3253.428768	345818.506980	52.487617
3252.603466	345596.532971	52.492621
3252.451805	345335.737028	52.497626
3251.316739	345093.141994	52.502631
3250.643347	344859.279858	52.507636
3250.164908	344611.819160	52.512641
3249.535506	344355.345223	52.517645
3248.716312	344136.113765	52.522650
3248.125721	343865.504689	52.527655
3247.771421	343660.172179	52.532660
3246.857500	343387.626683	52.537665
3245.974877	343166.416297	52.542669
3245.636672	342897.086574	52.547674
3244.823123	342678.154377	52.552679
3243.831457	342439.165916	52.557684
3243.343656	342175.125773	52.562689
3242.591547	341969.417761	52.567693
3241.932462	341706.420898	52.572698
3241.159265	341459.095786	52.577703
3240.606743	341256.662982	52.582708
3239.682384	341020.152987	52.587713
3239.212869	340761.144060	52.592717
3238.613697	340537.588441	52.597722
3238.362796	340273.757321	52.602727
3237.475516	340067.886250	52.607732
3236.747844	339796.288262	52.612737
3236.350260	339544.034185	52.617741
3235.538822	339335.221343	52.622746
3234.542340	339082.907464	52.627751
3234.385862	338820.048192	52.632756
3233.633878	338620.540542	52.637761
3232.426570	338360.671281	52.642765
3231.992923	338130.386109	52.647770
3231.304494	337874.225819	52.652775
3230.743135	337669.542918	52.657780
3229.969492	337406.673780	52.662785
3229.186519	337186.877776	52.667789
3228.636271	336932.677603	52.672794
3227.950433	336700.925407	52.677799
3227.610610	336459.316746	52.682804
3226.726031	336224.335859	52.687809
3226.247003	335986.133313	52.692813
3225.614433	335726.519245	52.697818
3225.045354	335509.687883	52.702823
3224.294770	335234.587118	52.707828
3223.426066	335034.705371	52.712833
3222.675577	334763.879567	52.717837
3222.432907	334553.688899	52.722842
3221.550547	334294.032577	52.727847
3220.991259	334064.288054	52.732852
3220.325713	333808.159726	52.737857
3218.997501	333588.336596	52.742861
3218.851925	333329.145681	52.747866
3217.961172	333112.434129	52.752871
3217.725633	332878.255729	52.757876
3216.566831	332635.083085	52.762881
3216.062843	332378.185760	52.767885
3215.501178	332159.637177	52.772890
3214.700747	331899.806407	52.777895
3214.009191	331690.696647	52.782900
3213.718666	331425.411738	52.787905
3212.633962	331191.387696	52.792909
3212.239346	330964.356776	52.797914
3211.633588	330717.704210	52.802919
3210.800605	330482.721582	52.807924
3210.160047	330252.341341	52.812929
3209.468857	330003.739579	52.817933
3209.124074	329764.731282	52.822938
3208.145934	329530.277831	52.827943
3207.514433	329288.716537	52.832948
3206.569641	329056.573168	52.837953
3206.039338	328803.792122	52.842957
3205.492165	328568.401916	52.847962
3204.732380	328343.304935	52.852967
3204.486539	328100.278613	52.857972
3203.563910	327865.403960	52.862977
3202.690480	327609.439907	52.867981
3202.181910	327377.833556	52.872986
3201.323587	327141.749949	52.877991
3200.567831	326898.647840	52.882996
3200.158851	326667.685635	52.888001
3199.318396	326439.133390	52.893005
3198.597637	326193.324807	52.898010
3197.989950	325971.099536	52.903015
3197.580888	325708.843568	52.908020
3196.606990	325514.019725	52.913025
3195.954579	325253.328446	52.918029
3195.968974	325007.094461	52.923034
3194.626969	324794.784626	52.928039
3194.229444	324532.675868	52.933044
3193.771250	324301.511106	52.938049
3192.682825	324065.887878	52.943053
3192.052798	323826.015828	52.948058
3191.298981	323592.655318	52.953063
3190.820533	323347.563837	52.958068
3189.898821	323134.113965	52.963073
3189.180071	322879.078294	52.968077
3188.815969	322663.807657	52.973082
3188.130251	322427.887070	52.978087
3187.012916	322199.061567	52.983092
3186.467185	321958.509005	52.988097
3185.665859	321721.128035	52.993101
3185.314019	321504.273993	52.998106
3184.523953	321279.391858	53.003111
3184.455627	321031.530065	53.008116
3183.634553	320792.036414	53.013121
3182.495568	320574.082497	53.018125
3182.242330	320321.002819	53.023130
3181.285818	320084.329587	53.028135
3180.709513	319870.664488	53.033140
3180.053847	319622.611727	53.038145
3179.201892	319392.871431	53.043149
3179.003109	319165.420705	53.048154
3178.209050	318935.975682	53.053159
3177.352453	318675.577389	53.058164
3176.734051	318447.783933	53.063169
3175.872803	318241.595348	53.068173
3175.455518	317970.584034	53.073178
3174.375095	317770.260118	53.078183
3174.037125	317526.174778	53.083188
3173.755190	317281.417924	53.088193
3172.544199	317070.265981	53.093197
3171.856175	316826.692632	53.098202
3171.530178	316575.167806	53.103207
3171.212342	316350.250192	53.108212
3170.660350	316112.408286	53.113217
3169.680067	315877.969295	53.118221
3168.950517	315635.749201	53.123226
3167.907983	315423.370373	53.128231
3167.387655	315162.094816	53.133236
3166.833595	314936.218393	53.138241
3166.211571	314709.613789	53.143245
3165.597692	314456.219549	53.148250
3165.272531	314243.062756	53.153255
3164.307229	313977.831384	53.158260
3163.259598	313771.357643	53.163265
3162.867388	313526.558387	53.168269
3162.462864	313285.962092	53.173274
3161.985391	313049.680239	53.178279
3161.054159	312803.895161	53.183284
3160.320981	312574.808173	53.188289
3159.604788	312343.247994	53.193293
3158.999278	312100.490996	53.198298
3157.865941	311870.600099	53.203303
3157.510856	311634.321349	53.208308
3156.781249	311406.148139	53.213313
3156.075771	311168.446934	53.218317
3155.338572	310924.766088	53.223322
3154.433153	310704.691579	53.228327
3153.875941	310470.505068	53.233332
3153.302753	310240.420439	53.238337
3152.533208	310015.612175	53.243341
3152.083753	309784.717680	53.248346
3151.491807	309551.018691	53.253351
3151.098957	309312.296627	53.258356
3150.406803	309077.721314	53.263361
3149.526776	308848.777582	53.268365
3148.993854	308622.452331	53.273370
3148.450134	308382.326299	53.278375
3147.723802	308136.091604	53.283380
3147.048395	307903.828762	53.288385
3146.286871	307674.482161	53.293389
3145.746058	307428.089416	53.298394
3144.539449	307207.623402	53.303399
3144.001119	306982.620292	53.308404
3143.969171	306735.687341	53.313409
3142.969856	306506.580036	53.318413
3142.356191	306268.167333	53.323418
3141.457274	306046.581144	53.328423
3140.920844	305813.070266	53.333428
3140.361180	305563.239190	53.338433
3139.992115	305337.569900	53.343437
3138.841575	305098.858124	53.348442
3137.917284	304869.888994	53.353447
3137.642051	304629.000648	53.358452
3137.397124	304400.636298	53.363457
3136.557904	304164.700391	53.368461
3135.860417	303918.249705	53.373466
3134.948172	303690.550080	53.378471
3134.661943	303450.629215	53.383476
3133.828618	303208.935513	53.388481
3132.833965	302981.706228	53.393485
3132.475991	302743.680072	53.398490
3131.349578	302500.580043	53.403495
3130.947823	302280.513748	53.408500
3130.677980	302031.496601	53.413505
3129.878001	301801.535338	53.418509
3129.301941	301558.423144	53.423514
3128.500009	301342.748135	53.428519
3128.028090	301080.722689	53.433524
3127.431958	300856.101219	53.438529
3126.403992	300624.773693	53.443533
3126.323063	300363.500152	53.448538
3125.073996	300129.150941	53.453543
3124.235760	299900.670106	53.458548
3124.239903	299645.595836	53.463553
3123.130086	299444.712257	53.468557
3122.847831	299182.501027	53.473562
3121.866727	298933.642697	53.478567
3121.248336	298715.159403	53.483572
3120.595787	298470.526848	53.488577
3119.630628	298237.123370	53.493581
3119.711205	297979.971792	53.498586
3118.358702	297766.747836	53.503591
3117.744880	297511.844716	53.508596
3117.279054	297271.459468	53.513601
3116.560636	297050.647072	53.518605
3115.922220	296811.663778	53.523610
3115.151142	296568.244449	53.528615
3114.662399	296332.445734	53.533620
3113.617136	296092.328999	53.538625
3112.931409	295872.910803	53.543629
3112.933958	295625.929840	53.548634
3111.928345	295394.872324	53.553639
3111.004340	295159.548611	53.558644
3110.578288	294919.892801	53.563649
3109.570198	294691.992851	53.568653
3108.916625	294450.284208	53.573658
3108.680413	294210.113693	53.578663
3107.884125	293978.588589	53.583668
3107.082022	293762.166332	53.588673
3106.342428	293518.891319	53.593677
3106.141550	293277.338985	53.598682
3105.167412	293054.601897	53.603687
3104.359653	292819.766678	53.608692
3103.713076	292552.434634	53.613697
3103.024007	292343.837186	53.618701
3102.536115	292120.665744	53.623706
3101.857152	291886.089395	53.628711
3101.269962	291648.162049	53.633716
3100.349740	291414.158269	53.638721
3099.701953	291180.111167	53.643725
3099.213278	290944.332343	53.648730
3098.765628	290717.384115	53.653735
3097.567241	290484.620531	53.658740
3096.952229	290244.913604	53.663745
3096.269405	290010.590907	53.668749
3095.831710	289777.375275	53.673754
3095.166062	289550.333276	53.678759
3094.601461	289313.419063	53.683764
3093.856117	289084.020817	53.688769
3093.218981	288852.746122	53.693773
3092.680379	288610.377132	53.698778
3092.029002	288373.679682	53.703783
3090.817703	288143.004700	53.708788
3090.471840	287903.227878	53.713793
3089.558343	287671.741404	53.718797
3089.201755	287454.505106	53.723802
3088.667726	287224.715570	53.728807
3087.914258	286983.194398	53.733812
3087.171463	286752.520755	53.738817
3086.090422	286518.029360	53.743821
3085.869337	286277.034710	53.748826
3084.957724	286050.920676	53.753831
3084.542462	285822.741450	53.758836
3083.960646	285593.162243	53.763841
3083.177250	285362.494217	53.768845
3082.737392	285118.833890	53.773850
3081.864555	284889.911602	53.778855
3081.175898	284661.443943	53.783860
3080.498669	284431.369869	53.788865
3079.779045	284198.959321	53.793869
3079.261273	283959.691243	53.798874
3078.744079	283737.766803	53.803879
3077.789964	283498.261949	53.808884
3077.254760	283275.372372	53.813889
3076.382457	283041.941274	53.818893
3076.071515	282794.566511	53.823898
3075.145774	282578.054595	53.828903
3074.507317	282335.774191	53.833908
3073.896852	282101.333491	53.838913
3073.104238	281882.864678	53.843917
3072.774932	281645.119379	53.848922
3072.249042	281411.301762	53.853927
3071.191772	281179.962193	53.858932
3070.332664	280943.573934	53.863937
3069.814764	280709.602030	53.868941
3069.456381	280472.599551	53.873946
3068.495389	280254.946443	53.878951
3067.466435	280022.838025	53.883956
3067.460892	279785.066412	53.888961
3066.600116	279555.019673	53.893965
3065.719165	279319.755067	53.898970
3064.753481	279091.049193	53.903975
3064.492226	278853.241453	53.908980
3064.010350	278623.771278	53.913985
3063.827463	278400.366155	53.918989
3063.179300	278161.600806	53.923994
3062.230149	277931.746059	53.928999
3061.453377	277693.179284	53.934004
3060.870370	277456.823034	53.939009
3059.843158	277229.094446	53.944013
3059.375141	276982.430727	53.949018
3058.792868	276748.748485	53.954023
3058.274371	276520.175283	53.959028
3057.533650	276291.713651	53.964033
3057.041590	276053.865757	53.969037
3056.261012	275806.054447	53.974042
3055.437421	275577.580456	53.979047
3054.811536	275330.890744	53.984052
3054.505376	275092.096573	53.989057
3053.736625	274865.957014	53.994061
3052.730764	274631.730582	53.999066
3052.079458	274398.466783	54.004071
3051.826453	274157.015547	54.009076
3051.035664	273915.318366	54.014081
3050.186622	273679.004260	54.019085
3049.913919	273436.639363	54.024090
3048.748443	273200.044317	54.029095
3047.845150	272964.324671	54.034100
3047.548749	272732.762222	54.039105
3046.816289	272503.204428	54.044109
3046.192262	272262.576251	54.049114
3045.463398	272028.841171	54.054119
3044.723105	271785.429982	54.059124
3044.359855	271562.868676	54.064129
3043.467293	271327.275013	54.069133
3043.042978	271082.336827	54.074138
3042.318067	270853.949758	54.079143
3041.493515	270619.568004	54.084148
3041.043987	270384.592127	54.089153
3040.076000	270151.557571	54.094157
3039.446985	269913.528592	54.099162
3038.742198	269673.525163	54.104167
3038.324880	269441.880846	54.109172
3037.716155	269205.147791	54.114177
3036.774323	268977.737994	54.119181
3036.462894	268738.869668	54.124186
3035.619565	268505.383024	54.129191
3034.937642	268269.706131	54.134196
3034.446870	268021.927158	54.139201
3033.577072	267793.411312	54.144205
3032.512253	267554.000590	54.149210
3032.223557	267321.521816	54.154215
3031.709458	267102.831636	54.159220
3030.992871	266859.444045	54.164225
3030.360145	266620.220083	54.169229
3029.565680	266392.507971	54.174234
3028.902545	266164.214892	54.179239
3028.041372	265918.303902	54.184244
3027.641513	265687.906496	54.189249
3027.104180	265458.626109	54.194253
3026.074859	265214.499461	54.199258
3025.237333	264989.927520	54.204263
3024.864053	264758.202121	54.209268
3024.311483	264534.451261	54.214273
3023.551918	264292.854786	54.219277
3023.002668	264049.646171	54.224282
3022.220682	263815.668494	54.229287
3021.144439	263592.485021	54.234292
3020.701986	263359.498101	54.239297
3020.235537	263131.481383	54.244301
3019.745270	262891.218552	54.249306
3019.024933	262669.965871	54.254311
3018.357889	262434.519330	54.259316
3017.856157	262196.576425	54.264321
3016.793065	261962.950223	54.269325
3016.146657	261728.901699	54.274330
3015.684008	261493.907437	54.279335
3014.760717	261273.859441	54.284340
3014.019047	261029.741350	54.289345
3013.486119	260794.529591	54.294349
3012.712339	260562.666957	54.299354
3012.282479	260330.750084	54.304359
3010.981263	260096.424586	54.309364
3011.050400	259863.002951	54.314369
3010.251213	259640.160687	54.319373
3009.922335	259399.009406	54.324378
3008.927766	259165.884136	54.329383
3008.132296	258931.785274	54.334388
3007.788707	258699.754376	54.339393
3007.045656	258461.572879	54.344397
3006.173917	258230.695678	54.349402
3005.537833	258011.241734	54.354407
3004.732349	257767.875483	54.359412
3004.357590	257540.409338	54.364417
3003.258684	257306.640292	54.369421
3002.988157	257075.669100	54.374426
3002.657111	256846.006564	54.379431
3001.682356	256613.721178	54.384436
3001.133749	256371.614645	54.389441
3000.226334	256149.047586	54.394445
3000.067437	255922.822339	54.399450
2999.207053	255683.618285	54.404455
2998.423559	255442.161238	54.409460
2997.901431	255196.995849	54.414465
2996.871597	254970.400203	54.419469
2996.686933	254732.389142	54.424474
2995.841403	254490.179074	54.429479
2994.800889	254262.847405	54.434484
2994.509443	254035.371962	54.439489
2993.881679	253812.839677	54.444493
2993.126286	253558.366970	54.449498
2992.541288	253333.816612	54.454503
2991.569903	253103.470339	54.459508
2991.351933	252870.127350	54.464513
2990.215198	252634.256108	54.469517
2989.714081	252406.281097	54.474522
2989.562547	252162.665456	54.479527
2988.574751	251925.218131	54.484532
2987.604246	251687.946665	54.489537
2987.134333	251464.806615	54.494541
2986.766828	251225.835949	54.499546
2986.005210	250992.174111	54.504551
2985.046679	250756.251799	54.509556
2984.546634	250521.046705	54.514561
2983.987709	250290.333355	54.519565
2983.210165	250051.964118	54.524570
2982.720076	249809.220465	54.529575
2982.013658	249571.044425	54.534580
2981.207209	249343.860521	54.539585
2980.653951	249111.492703	54.544589
2979.795217	248865.014432	54.549594
2979.213827	248640.138828	54.554599
2978.381842	248417.162255	54.559604
2978.370495	248166.400015	54.564609
2977.245973	247923.530615	54.569613
2976.708892	247691.162444	54.574618
2975.927436	247448.137662	54.579623
2974.835746	247213.922653	54.584628
2974.840762	246985.442471	54.589633
2973.975027	246757.176906	54.594637
2973.253706	246519.084550	54.599642
2972.616893	246292.897156	54.604647
2971.906884	246061.526732	54.609652
2971.548482	245819.532816	54.614657
2970.329532	245586.181057	54.619661
2969.753856	245351.480054	54.624666
2969.049675	245111.935905	54.629671
2968.719816	244883.817824	54.634676
2967.934656	244658.420616	54.639681
2967.036258	244424.510843	54.644685
2966.755839	244182.991400	54.649690
2966.105996	243949.628835	54.654695
2965.165577	243724.818068	54.659700
2964.943590	243478.859760	54.664705
2964.282791	243242.036971	54.669709
2963.145126	243013.031496	54.674714
2962.809088	242766.074042	54.679719
2962.006662	242529.886191	54.684724
2961.374765	242295.734453	54.689729
2960.574800	242068.383420	54.694733
2960.225897	241823.365235	54.699738
2959.571185	241599.327978	54.704743
2958.553124	241362.361676	54.709748
2958.000536	241116.002097	54.714753
2957.253792	240892.133537	54.719757
2956.688468	240653.161678	54.724762
2956.107946	240422.163100	54.729767
2955.492836	240187.732763	54.734772
2954.643555	239940.429539	54.739777
2953.810707	239707.766238	54.744781
2953.729323	239469.687873	54.749786
2952.915195	239241.300569	54.754791
2952.081395	239005.710488	54.759796
2951.839646	238770.307278	54.764801
2951.107623	238541.144493	54.769805
2950.302782	238291.189628	54.774810
2949.346559	238059.797055	54.779815
2948.846639	237812.774298	54.784820
2948.430040	237583.818237	54.789825
2947.638664	237351.764495	54.794829
2946.858304	237103.030780	54.799834
2946.344720	236869.202583	54.804839
2945.694386	236631.144136	54.809844
2945.280880	236376.191873	54.814849
2944.539474	236152.535844	54.819853
2944.036679	235905.518023	54.824858
2943.564587	235659.667253	54.829863
2942.407485	235417.159373	54.834868
2941.547010	235168.162911	54.839873
2940.912955	234945.638387	54.844877
2940.297825	234693.192196	54.849882
2940.012427	234449.326415	54.854887
2939.042529	234223.113616	54.859892
2938.508267	233976.767572	54.864897
2937.714849	233730.361331	54.869901
2937.108892	233492.277835	54.874906
2936.615862	233249.975694	54.879911
2935.732933	233013.745091	54.884916
2935.204567	232755.357387	54.889921
2934.362104	232523.704864	54.894925
2934.069438	232279.591094	54.899930
2933.341455	232040.741217	54.904935
2932.383757	231802.412107	54.909940
2931.734911	231559.731583	54.914945
2931.303997	231307.417937	54.919949
2930.526794	231080.443726	54.924954
2929.898893	230836.157684	54.929959
2929.011923	230598.609829	54.934964
2928.505029	230346.641883	54.939969
2927.836331	230117.768723	54.944973
2927.005811	229862.466951	54.949978
2926.522355	229630.204756	54.954983
2925.903248	229383.298726	54.959988
2925.354431	229161.003629	54.964993
2924.291037	228910.426422	54.969997
2923.638071	228675.952979	54.975002
2923.165268	228429.459329	54.980007
2922.459075	228188.452060	54.985012
2922.094653	227945.863680	54.990017
2920.882268	227717.846740	54.995021
2920.400310	227468.938497	55.000026
2919.985489	227223.062950	55.005031
2919.005972	226989.753404	55.010036
2918.336668	226756.879148	55.015041
2917.594357	226515.449540	55.020045
2917.104742	226271.269055	55.025050
2916.474354	226041.547781	55.030055
2915.988821	225796.209601	55.035060
2915.393810	225557.432846	55.040065
2914.438355	225312.819773	55.045069
2913.497848	225080.069604	55.050074
2913.147854	224825.088887	55.055079
2912.389932	224591.063672	55.060084
2911.929998	224358.404998	55.065089
2911.123083	224111.442476	55.070093
2910.500142	223873.006148	55.075098
2909.992226	223642.814068	55.080103
2909.380408	223401.334955	55.085108
2908.918906	223152.258515	55.090113
2907.827371	222921.995490	55.095117
2907.320069	222666.435652	55.100122
2906.697419	222430.104123	55.105127
2906.099566	222195.093289	55.110132
2905.332433	221956.291082	55.115137
2904.752612	221696.481536	55.120141
2904.234213	221454.624606	55.125146
2903.773998	221213.675770	55.130151
2902.741407	220983.243810	55.135156
2902.367024	220723.265084	55.140161
2901.624358	220475.031194	55.145165
2900.665886	220239.574419	55.150170
2900.217376	219990.951891	55.155175
2899.344944	219741.175321	55.160180
2898.810932	219501.071169	55.165185
2898.266710	219261.389494	55.170189
2897.733992	219015.571334	55.175194
2896.911843	218781.205140	55.180199
2896.028150	218531.600020	55.185204
2895.617091	218268.288139	55.190209
2894.700976	218034.588463	55.195213
2894.036692	217796.241804	55.200218
2893.643963	217549.070009	55.205223
2893.086234	217314.221291	55.210228
2892.044493	217065.830174	55.215233
2891.304772	216823.285541	55.220237
2890.780948	216574.712342	55.225242
2889.960474	216331.622160	55.230247
2889.205684	216097.508856	55.235252
2888.909789	215849.767737	55.240257
2888.066152	215621.728944	55.245261
2887.280167	215379.718622	55.250266
2886.899290	215139.719755	55.255271
2886.193813	214891.754248	55.260276
2885.663679	214643.380042	55.265281
2884.828175	214405.568705	55.270285
2884.140187	214159.970616	55.275290
2883.493016	213917.752681	55.280295
2882.393211	213685.369825	55.285300
2882.300339	213431.050508	55.290305
2881.642871	213190.657008	55.295309
2880.584014	212959.593968	55.300314
2880.468890	212696.982359	55.305319
2879.597322	212468.729752	55.310324
2879.285592	212216.193578	55.315329
2877.948184	211978.941494	55.320333
2877.467682	211728.177685	55.325338
2876.461775	211492.822268	55.330343
2876.026750	211252.171694	55.335348
2875.491685	211013.867037	55.340353
2874.934208	210769.393945	55.345357
2873.955608	210534.712343	55.350362
2873.600308	210276.743410	55.355367
2872.718235	210041.297457	55.360372
2872.432383	209801.634302	55.365377
2871.611295	209571.615079	55.370381
2871.008393	209309.476630	55.375386
2870.487650	209077.731689	55.380391
2869.691559	208826.164067	55.385396
2869.172738	208584.620752	55.390401
2868.527184	208345.122075	55.395405
2867.777289	208093.181091	55.400410
2867.015532	207846.053843	55.405415
2866.556078	207598.599747	55.410420
2865.812622	207355.735149	55.415425
2865.139075	207100.375443	55.420429
2864.354000	206867.293641	55.425434
2863.886595	206611.216151	55.430439
2862.807843	206370.444966	55.435444
2862.379314	206119.428678	55.440449
2861.682651	205879.693489	55.445453
2860.831058	205644.616274	55.450458
2860.164553	205389.924668	55.455463
2859.671943	205153.889012	55.460468
2858.869804	204909.109426	55.465473
2858.522747	204660.695448	55.470477
2857.709066	204424.013686	55.475482
2857.508040	204185.059702	55.480487
2856.648329	203928.483517	55.485492
2856.086735	203682.271218	55.490497
2855.341293	203431.876790	55.495501
2854.563160	203196.543478	55.500506
2853.768736	202935.749170	55.505511
2852.876363	202698.616235	55.510516
2852.204872	202446.547409	55.515521
2851.544485	202219.038663	55.520525
2850.892682	201970.379383	55.525530
2850.611341	201721.497119	55.530535
2849.310156	201501.371877	55.535540
2849.162173	201246.031500	55.540545
2848.423785	200988.164370	55.545549
2847.813709	200751.542297	55.550554
2847.163909	200516.187357	55.555559
2846.254192	200274.702831	55.560564
2846.158735	200020.657871	55.565569
2845.230717	199781.214493	55.570573
2844.251748	199530.594869	55.575578
2843.921953	199286.210692	55.580583
2842.994806	199034.821685	55.585588
2842.415547	198802.962467	55.590593
2841.857213	198548.806941	55.595597
2841.271123	198308.501647	55.600602
2840.521231	198059.379677	55.605607
2839.992724	197827.122246	55.610612
2839.078728	197570.279242	55.615617
2838.875577	197323.975406	55.620621
2837.887545	197081.538055	55.625626
2837.774143	196827.129562	55.630631
2836.774681	196585.103531	55.635636
2836.189944	196337.783250	55.640641
2835.540671	196084.824798	55.645645
2834.407806	195844.375754	55.650650
2833.993089	195590.822735	55.655655
2833.200464	195342.598610	55.660660
2832.621405	195096.110518	55.665665
2831.947411	194849.931316	55.670669
2831.154317	194601.189225	55.675674
2830.440821	194354.077137	55.680679
2829.823813	194114.343508	55.685684
2829.395704	193877.354887	55.690689
2828.851204	193623.043470	55.695693
2828.345779	193384.746182	55.700698
2827.592283	193119.299129	55.705703
2826.557644	192880.579148	55.710708
2825.997667	192627.178677	55.715713
2825.453744	192376.410705	55.720717
2824.710401	192135.726993	55.725722
2824.182443	191887.732678	55.730727
2823.672349	191636.492396	55.735732
2822.875071	191399.205233	55.740737
2822.296449	191130.217010	55.745741
2821.435921	190889.125470	55.750746
2820.706860	190645.024441	55.755751
2819.727365	190402.452892	55.760756
2819.214394	190143.701679	55.765761
2818.748576	189906.267627	55.770765
2818.004698	189664.591277	55.775770
2817.851158	189420.303596	55.780775
2816.882399	189167.774896	55.785780
2816.166813	188918.349891	55.790785
2815.671178	188668.458816	55.795789
2814.621346	188422.231815	55.800794
2814.691802	188161.325347	55.805799
2813.706017	187923.360282	55.810804
2812.862451	187662.321496	55.815809
2812.476053	187411.771044	55.820813
2811.495322	187168.058717	55.825818
2811.221541	186906.692246	55.830823
2810.378676	186652.770600	55.835828
2809.723049	186417.229056	55.840833
2808.760477	186159.830635	55.845837
2808.097658	185919.534904	55.850842
2807.596037	185664.368892	55.855847
2806.715114	185419.276181	55.860852
2806.205867	185166.276839	55.865857
2805.615994	184920.135758	55.870861
2804.714968	184674.197965	55.875866
2804.549492	184429.875102	55.880871
2803.596308	184172.740978	55.885876
2803.005739	183931.439474	55.890881
2802.394906	183668.834883	55.895885
2801.862418	183431.661214	55.900890
2801.149353	183172.319594	55.905895
2800.264367	182924.697094	55.910900
2799.761224	182661.877916	55.915905
2799.235924	182420.103687	55.920909
2798.361929	182173.399582	55.925914
2797.595174	181916.490809	55.930919
2796.896274	181667.065110	55.935924
2796.308501	181421.591981	55.940929
2795.657145	181178.470842	55.945933
2794.851244	180927.018409	55.950938
2794.484595	180671.109445	55.955943
2793.797930	180434.510792	55.960948
2793.140963	180164.200914	55.965953
2792.328328	179922.982276	55.970957
2791.457324	179667.451776	55.975962
2791.026892	179426.124544	55.980967
2790.236366	179174.616420	55.985972
2789.893315	178926.218808	55.990977
2789.236558	178680.696078	55.995981
2788.575359	178426.246462	56.000986
2787.839313	178169.291823	56.005991
2786.912596	177933.699157	56.010996
2786.430841	177674.303351	56.016001
2786.027776	177424.130767	56.021005
2785.228592	177173.272016	56.026010
2784.641210	176929.198596	56.031015
2783.514928	176670.216433	56.036020
2783.269940	176413.627346	56.041025
2782.460461	176165.243818	56.046029
2781.859468	175920.517179	56.051034
2781.532102	175652.168462	56.056039
2780.844091	175398.326823	56.061044
2780.083454	175157.420167	56.066049
2779.456521	174891.247905	56.071053
2778.787846	174643.843404	56.076058
2777.862118	174381.817107	56.081063
2777.221806	174133.431955	56.086068
2776.814626	173878.283596	56.091073
2775.889329	173624.401701	56.096077
2775.263988	173375.281252	56.101082
2774.776062	173104.660315	56.106087
2773.981105	172868.211356	56.111092
2773.341918	172610.017489	56.116097
2772.946174	172349.472163	56.121101
2771.848326	172093.338264	56.126106
2771.431822	171852.982068	56.131111
2770.564278	171593.114209	56.136116
2770.110628	171340.138811	56.141121
2769.567373	171082.601093	56.146125
2768.852233	170846.189831	56.151130
2768.116756	170572.942280	56.156135
2767.221889	170323.820318	56.161140
2766.786734	170071.664136	56.166145
2766.365689	169806.905146	56.171149
2765.296916	169563.830634	56.176154
2764.909703	169302.948321	56.181159
2764.184689	169048.975448	56.186164
2763.735151	168816.756435	56.191169
2762.972714	168485.439806	56.196173
2762.066715	168248.871321	56.201178
2761.816103	167989.642188	56.206183
2760.933686	167742.417074	56.211188
2760.154980	167480.261407	56.216193
2759.750781	167217.590473	56.221197
2758.983460	166970.148754	56.226202
2758.344070	166709.286127	56.231207
2757.568795	166453.240608	56.236212
2757.066428	166165.186971	56.241217
2756.120243	165908.155044	56.246221
2755.171643	165686.740775	56.251226
2754.912208	165427.136636	56.256231
2753.856048	165164.507188	56.261236
2753.387466	164912.365427	56.266241
2753.113430	164624.783519	56.271245
2752.016828	164367.709882	56.276250
2751.232262	164147.741108	56.281255
2750.726825	163907.614835	56.286260
2750.420080	163645.805742	56.291265
2749.617778	163387.586238	56.296269
2748.171310	163123.253282	56.301274
2748.588197	162831.736348	56.306279
2747.703799	162572.658388	56.311284
2746.641146	162353.176854	56.316289
2746.554176	162111.661241	56.321293
2745.382970	161830.562520	56.326298
2745.073984	161575.939488	56.331303
2744.107097	161346.061759	56.336308
2743.638002	161051.559365	56.341313
2742.974424	160806.838385	56.346317
2742.105631	160594.965115	56.351322
2741.354653	160314.828900	56.356327
2741.158644	160049.392555	56.361332
2740.035483	159823.986420	56.366337
2739.533984	159540.409710	56.371341
2739.139792	159281.519682	56.376346
2738.312938	159056.885181	56.381351
2737.845618	158757.863194	56.386356
2737.421919	158518.014616	56.391361
2736.596728	158285.871604	56.396365
2735.469099	157997.791954	56.401370
2735.395469	157746.121448	56.406375
2734.598007	157502.677935	56.411380
2733.244084	157223.068911	56.416385
2733.311350	156945.181980	56.421389
2732.638759	156694.186111	56.426394
2732.104985	156485.882349	56.431399
2731.068618	156209.282183	56.436404
2730.449482	155911.135263	56.441409
2730.022847	155704.598959	56.446413
2729.176607	155414.259233	56.451418
2728.575843	155167.203857	56.456423
2727.556371	154933.322080	56.461428
2726.938776	154669.824462	56.466433
2725.974149	154395.452254	56.471437
2725.875380	154115.517480	56.476442
2725.149253	153886.223371	56.481447
2724.299186	153650.595014	56.486452
2723.378066	153374.215975	56.491457
2723.434777	153094.176167	56.496461
2722.276584	152838.227129	56.501466
2721.799186	152575.905937	56.506471
2721.228656	152366.400654	56.511476
2720.261642	152127.039375	56.516481
2719.538389	151857.759455	56.521485
2718.643155	151587.314240	56.526490
2718.029205	151342.805987	56.531495
2717.519405	151110.827772	56.536500
2717.222348	150856.460883	56.541505
2716.338738	150597.867596	56.546509
2715.095175	150361.804045	56.551514
2714.995240	150110.601886	56.556519
2714.229359	149859.634275	56.561524
2713.521870	149610.997885	56.566529
2712.921780	149353.055934	56.571533
2712.124078	149069.551142	56.576538
2711.868119	148803.666706	56.581543
2710.675428	148608.950453	56.586548
2710.272902	148345.990681	56.591553
2710.006514	148052.713869	56.596557
2709.114608	147844.356287	56.601562
2708.384890	147573.105151	56.606567
2708.116597	147283.978718	56.611572
2707.573776	147028.232338	56.616577
2706.935524	146766.809864	56.621581
2705.845551	146508.587324	56.626586
2705.371247	146269.890536	56.631591
2704.374261	146060.519316	56.636596
2703.745008	145799.268669	56.641601
2703.116593	145507.953616	56.646605
2702.127920	145260.348965	56.651610
2701.960625	144977.263881	56.656615
2701.395122	144760.322897	56.661620
2700.242796	144530.921578	56.666625
2699.400673	144247.263876	56.671629
2699.451437	143988.169879	56.676634
2698.309211	143747.882803	56.681639
2697.919536	143473.055428	56.686644
2697.260799	143249.659325	56.691649
2696.608601	143003.213886	56.696653
2695.667685	142729.674937	56.701658
2695.415833	142475.190601	56.706663
2694.468516	142247.679821	56.711668
2694.093324	141942.800655	56.716673
2693.309385	141720.070897	56.721677
2692.580181	141487.042204	56.726682
2691.770869	141198.223518	56.731687
2690.963093	140942.772813	56.736692
2690.655425	140669.584102	56.741697
2689.994295	140448.635770	56.746701
2688.904484	140222.369846	56.751706
2688.214262	139951.611504	56.756711
2688.038095	139661.373201	56.761716
2687.078559	139448.725254	56.766721
2686.434577	139178.042830	56.771725
2685.909060	138905.667044	56.776730
2685.579635	138671.110423	56.781735
2684.807837	138438.226547	56.786740
2683.196958	138163.933263	56.791745
2682.941068	137911.876732	56.796749
2682.658298	137644.835404	56.801754
2682.563219	137369.483559	56.806759
2681.517819	137136.145153	56.811764
2680.304606	136899.798917	56.816769
2680.112316	136658.439909	56.821773
2679.239137	136427.112511	56.826778
2678.823891	136158.619367	56.831783
2677.955561	135893.046107	56.836788
2676.813010	135633.578313	56.841793
2676.513720	135379.708474	56.846797
2675.733762	135133.005473	56.851802
2675.256212	134873.807522	56.856807
2674.845489	134621.651526	56.861812
2673.991595	134378.701405	56.866817
2673.315467	134118.055474	56.871821
2672.481738	133839.564114	56.876826
2672.158445	133561.998093	56.881831
2671.491409	133347.061818	56.886836
2670.575623	133089.016448	56.891841
2670.417445	132806.033097	56.896845
2669.792904	132601.841852	56.901850
2668.705583	132323.303877	56.906855
2668.437992	132046.493241	56.911860
2667.587871	131789.147902	56.916865
2666.706232	131563.919858	56.921869
2665.920024	131276.732727	56.926874
2665.536810	131028.033662	56.931879
2664.743460	130804.258388	56.936884
2663.641442	130536.803325	56.941889
2663.773418	130251.106974	56.946893
2662.753969	130050.718253	56.951898
2662.444986	129784.706966	56.956903
2661.646871	129519.995004	56.961908
2660.433641	129248.975602	56.966913
2659.965101	128989.398359	56.971917
2659.198339	128746.686191	56.976922
2658.411318	128480.852068	56.981927
2658.265685	128247.761617	56.986932
2657.542834	128001.124689	56.991937
2656.937636	127752.731434	56.996941
2656.310540	127511.862224	57.001946
2655.550052	127246.543834	57.006951
2654.966736	127001.316168	57.011956
2653.892926	126725.080007	57.016961
2653.398138	126455.256983	57.021965
2652.579427	126196.206141	57.026970
2652.585502	125926.664579	57.031975
2651.789895	125674.548789	57.036980
2650.888513	125426.249083	57.041985
2650.214885	125197.116142	57.046989
2649.837183	124925.156415	57.051994
2649.173255	124634.400166	57.056999
2648.053320	124402.487546	57.062004
2647.489939	124179.695018	57.067009
2647.054861	123919.589401	57.072013
2646.229071	123638.177388	57.077018
2645.598341	123354.108964	57.082023
2645.157830	123100.373852	57.087028
2644.153062	122904.301917	57.092033
2643.110646	122611.964268	57.097037
2642.412004	122361.362636	57.102042
2642.460941	122086.977107	57.107047
2641.844296	121881.734574	57.112052
2640.874080	121630.230622	57.117057
2640.534466	121351.317969	57.122061
2639.325754	121110.128628	57.127066
2639.344435	120840.915797	57.132071
2638.153049	120582.257897	57.137076
2637.555705	120338.426771	57.142081
2636.918095	120071.757229	57.147085
2635.920981	119832.920360	57.152090
2636.100954	119558.997581	57.157095
2635.155344	119347.891631	57.162100
2634.086516	119058.797187	57.167105
2633.901809	118811.791813	57.172109
2632.659788	118547.975984	57.177114
2632.219892	118315.311040	57.182119
2631.875713	118043.372641	57.187124
2631.085761	117820.492278	57.192129
2630.621782	117522.959396	57.197133
2629.457365	117294.925260	57.202138
2629.188703	116994.936471	57.207143
2628.281288	116782.994958	57.212148
2627.861435	116504.978719	57.217153
2626.987460	116261.160169	57.222157
2626.599277	115993.985565	57.227162
2625.785148	115752.110997	57.232167
2625.170850	115489.039690	57.237172
2624.241005	115253.573342	57.242177
2623.987104	114956.278357	57.247181
2622.941294	114736.981735	57.252186
2622.207666	114470.163582	57.257191
2621.833427	114200.041791	57.262196
2621.143851	113983.494192	57.267201
2620.332850	113687.521049	57.272205
2619.339094	113469.496573	57.277210
2619.161842	113198.123144	57.282215
2618.399103	112932.912600	57.287220
2617.595753	112707.344141	57.292225
2617.128632	112426.575364	57.297229
2616.151411	112197.935764	57.302234
2615.720618	111932.835600	57.307239
2615.031610	111686.087610	57.312244
2614.629066	111441.384523	57.317249
2614.015098	111164.162681	57.322253
2612.996935	110936.290069	57.327258
2612.431666	110664.752044	57.332263
2611.704502	110430.181256	57.337268
2611.056405	110142.137817	57.342273
2610.374556	109922.756256	57.347277
2609.441175	109637.175310	57.352282
2609.030469	109409.258712	57.357287
2608.644046	109163.947594	57.362292
2607.897331	108898.359189	57.367297
2607.537610	108638.873626	57.372301
2606.705072	108383.843970	57.377306
2605.784167	108137.593658	57.382311
2605.294774	107854.387160	57.387316
2604.474419	107635.352777	57.392321
2604.013163	107348.937174	57.397325
2603.100476	107129.059117	57.402330
2602.388207	106860.765697	57.407335
2602.073730	106569.050896	57.412340
2600.900340	106365.108390	57.417345
2600.287979	106068.701073	57.422349
2599.573072	105856.359784	57.427354
2599.426653	105568.386534	57.432359
2598.683088	105351.308622	57.437364
2597.957498	105068.844992	57.442369
2597.775679	104830.137448	57.447373
2596.640298	104564.925068	57.452378
2596.002028	104302.815290	57.457383
2595.507031	104063.841557	57.462388
2594.428017	103782.071017	57.467393
2594.155503	103553.185872	57.472397
2593.326903	103278.601069	57.477402
2592.764050	103045.503810	57.482407
2591.928441	102762.165380	57.487412
2591.035207	102531.745549	57.492417
2590.521379	102255.663805	57.497421
2589.974545	101987.063209	57.502426
2589.200363	101752.680195	57.507431
2588.750322	101515.704473	57.512436
2587.589177	101240.891843	57.517441
2587.468696	100978.724521	57.522445
2586.758980	100773.672301	57.527450
2586.314083	100472.627732	57.532455
2585.123609	100246.673433	57.537460
2584.576231	99961.433243	57.542465
2584.132309	99709.594481	57.547469
2583.299869	99467.854387	57.552474
2582.804370	99194.095992	57.557479
2582.156043	98963.006875	57.562484
2581.266101	98683.323266	57.567489
2580.124531	98465.294317	57.572493
2579.732279	98178.358255	57.577498
2579.291735	97947.081577	57.582503
2578.286388	97700.941550	57.587508
2577.998506	97415.996384	57.592513
2577.372424	97163.136371	57.597517
2576.390728	96971.879433	57.602522
2575.944381	96699.386270	57.607527
2575.748991	96439.432749	57.612532
2574.330661	96182.390382	57.617537
2574.407610	95890.696867	57.622541
2574.013083	95683.553974	57.627546
2572.584227	95437.493037	57.632551
2571.865250	95189.096378	57.637556
2571.378554	94922.738095	57.642561
2570.712019	94654.312458	57.647565
2569.979847	94384.029736	57.652570
2569.038424	94142.490618	57.657575
2568.680327	93912.707136	57.662580
2567.664495	93683.239534	57.667585
2567.327350	93387.947361	57.672589
2566.347075	93173.419055	57.677594
2565.672154	92887.108946	57.682599
2565.232155	92657.617759	57.687604
2564.579745	92415.385841	57.692609
2564.139918	92140.613821	57.697613
2563.226465	91913.063259	57.702618
2562.727908	91672.254459	57.707623
2562.337529	91385.113489	57.712628
2561.117258	91165.950761	57.717633
2560.642679	90889.456260	57.722637
2560.052078	90668.062001	57.727642
2559.326668	90391.410662	57.732647
2559.067849	90146.345353	57.737652
2558.080579	89902.514118	57.742657
2557.914519	89608.836957	57.747661
2557.161197	89412.023480	57.752666
2556.185223	89117.961451	57.757671
2555.552232	88878.295241	57.762676
2554.688258	88609.036389	57.767681
2554.059669	88380.849904	57.772685
2553.513574	88120.225758	57.777690
2552.475041	87864.101453	57.782695
2552.064325	87608.476593	57.787700
2551.211153	87384.177962	57.792705
2551.034525	87105.294553	57.797709
2549.842245	86873.935992	57.802714
2549.376024	86582.997383	57.807719
2549.097375	86371.784666	57.812724
2547.906024	86097.157595	57.817729
2547.384629	85832.931439	57.822733
2546.625845	85640.134202	57.827738
2545.850672	85367.757916	57.832743
2545.649752	85103.819637	57.837748
2544.653336	84889.052627	57.842753
2544.201356	84602.842089	57.847757
2543.449103	84361.419879	57.852762
2542.795778	84121.429902	57.857767
2542.094949	83870.263047	57.862772
2541.202018	83618.800047	57.867777
2541.013973	83347.256761	57.872781
2540.199410	83137.758451	57.877786
2539.370547	82852.398338	57.882791
2538.974778	82627.995116	57.887796
2537.799288	82355.150791	57.892801
2537.814309	82116.700279	57.897805
2536.824784	81875.350603	57.902810
2535.960305	81620.864983	57.907815
2535.954278	81365.542929	57.912820
2534.968916	81101.658867	57.917825
2534.247321	80877.040952	57.922829
2533.665816	80618.986471	57.927834
2533.049516	80354.261255	57.932839
2532.355068	80107.289568	57.937844
2531.682755	79863.675990	57.942849
2530.900957	79612.776051	57.947853
2530.416665	79341.876968	57.952858
2529.402293	79117.654118	57.957863
2529.055212	78855.186751	57.962868
2528.321265	78596.212225	57.967873
2527.626062	78362.315237	57.972877
2527.007666	78112.706738	57.977882
2526.128668	77848.467301	57.982887
2525.579047	77597.821345	57.987892
2524.367758	77368.199577	57.992897
2524.089008	77099.135128	57.997901
2523.253908	76859.695312	58.002906
2522.586246	76616.632874	58.007911
2522.110871	76377.306465	58.012916
2521.421620	76130.084180	58.017921
2521.231053	75863.081325	58.022925
2520.195679	75651.438632	58.027930
2519.458464	75365.635674	58.032935
2518.818314	75150.945132	58.037940
2517.836203	74881.141013	58.042945
2517.546338	74647.083227	58.047949
2516.833895	74392.543111	58.052954
2515.968718	74141.882310	58.057959
2515.585674	73905.864989	58.062964
2514.865004	73643.809421	58.067969
2514.276899	73430.947233	58.072973
2513.641983	73145.869220	58.077978
2512.795180	72929.296739	58.082983
2512.565053	72664.141848	58.087988
2511.298316	72433.749008	58.092993
2510.945715	72177.267002	58.097997
2510.440866	71913.933056	58.103002
2509.572052	71691.372358	58.108007
2509.362672	71427.928357	58.113012
2507.816381	71203.611885	58.118017
2507.666500	70912.534762	58.123021
2506.571591	70715.668467	58.128026
2506.168542	70450.019577	58.133031
2505.546759	70211.385715	58.138036
2505.125086	69936.460980	58.143041
2504.448213	69726.927384	58.148045
2503.500362	69482.311534	58.153050
2502.702314	69198.247439	58.158055
2502.172240	68998.832353	58.163060
2501.483123	68744.126859	58.168065
2501.108416	68494.327653	58.173069
2499.470717	68257.430399	58.178074
2499.549343	67983.308857	58.183079
2499.040095	67769.241379	58.188084
2498.126095	67520.914496	58.193089
2497.499881	67249.698490	58.198093
2496.930442	67054.970753	58.203098
2495.857303	66777.163535	58.208103
2495.948332	66509.878292	58.213108
2494.762187	66310.183212	58.218113
2494.117866	66080.187714	58.223117
2493.306411	65831.556002	58.228122
2492.587771	65588.555101	58.233127
2491.955806	65341.734551	58.238132
2490.857045	65096.577446	58.243137
2489.922027	64863.333939	58.248141
2490.051209	64603.246854	58.253146
2489.396850	64366.007276	58.258151
2488.924607	64180.329260	58.263156
2488.285134	63959.296211	58.268161
2487.744791	63681.192943	58.273165
2486.947194	63437.269468	58.278170
2486.422718	63165.135832	58.283175
2485.822114	62935.858249	58.288180
2484.706412	62735.220643	58.293185
2483.730007	62479.152662	58.298189
2483.243807	62224.672438	58.303194
2482.885210	61984.338658	58.308199
2481.823698	61772.882395	58.313204
2481.035562	61509.697183	58.318209
2480.627871	61302.517408	58.323213
2479.196213	61054.496022	58.328218
2478.581334	60825.667366	58.333223
2478.471738	60583.039193	58.338228
2477.633231	60376.216502	58.343233
2477.328278	60116.506819	58.348237
2477.065710	59933.809602	58.353242
2475.882041	59661.318336	58.358247
2475.751784	59443.131599	58.363252
2474.612456	59189.090461	58.368257
2474.115857	58945.443417	58.373261
2473.130262	58735.326158	58.378266
2472.603130	58481.713547	58.383271
2472.133883	58260.378700	58.388276
2471.325475	58042.401374	58.393281
2470.586133	57782.274075	58.398285
2470.254266	57548.389528	58.403290
2469.263096	57350.524481	58.408295
2468.561238	57072.370848	58.413300
2468.131966	56870.481637	58.418305
2467.740545	56613.746307	58.423309
2466.694510	56410.317414	58.428314
2466.426211	56140.128567	58.433319
2465.542401	55932.115779	58.438324
2464.890972	55663.200432	58.443329
2464.147191	55472.984218	58.448333
2463.885308	55198.086705	58.453338
2462.921843	54984.581559	58.458343
2462.481705	54706.722935	58.463348
2461.320812	54520.569970	58.468353
2460.579333	54270.046141	58.473357
2460.226553	54004.803857	58.478362
2459.253683	53804.347866	58.483367
2458.879392	53554.212362	58.488372
2457.909472	53352.431921	58.493377
2457.228156	53085.767987	58.498381
2456.562402	52878.631989	58.503386
2455.940914	52634.424156	58.508391
2455.105009	52398.325074	58.513396
2454.173992	52197.006993	58.518401
2453.973284	51955.684157	58.523405
2453.245270	51725.455422	58.528410
2452.217995	51520.686191	58.533415
2451.881759	51276.666691	58.538420
2450.912667	51053.109878	58.543425
2450.394033	50848.046217	58.548429
2449.715597	50613.337682	58.553434
2448.995242	50372.801887	58.558439
2448.446028	50175.353107	58.563444
2447.406117	49943.567454	58.568449
2446.640010	49725.521880	58.573453
2446.230695	49483.556793	58.578458
2445.197340	49304.969922	58.583463
2445.343800	49047.465848	58.588468
2444.210472	48865.432115	58.593473
2443.550798	48614.857137	58.598477
2442.531765	48406.487653	58.603482
2442.032447	48182.221771	58.608487
2441.736616	47987.623066	58.613492
2440.549608	47758.913343	58.618497
2440.369704	47517.365754	58.623501
2439.602687	47333.265290	58.628506
2438.432015	47139.811034	58.633511
2438.072556	46926.692031	58.638516
2437.106741	46715.857402	58.643521
2436.312943	46483.037422	58.648525
2435.762365	46249.656919	58.653530
2435.049809	46059.301709	58.658535
2434.517269	45866.693363	58.663540
2433.485633	45645.068192	58.668545
2433.093777	45422.344947	58.673549
2432.133877	45268.207290	58.678554
2431.278878	45036.349276	58.683559
2430.800001	44836.798440	58.688564
2429.634544	44661.195659	58.693569
2429.085969	44440.454836	58.698573
2428.534663	44272.579745	58.703578
2427.470280	44086.289868	58.708583
2427.199690	43875.385626	58.713588
2425.740657	43721.767760	58.718593
2424.908654	43507.614267	58.723597
2424.537957	43317.225337	58.728602
2423.582406	43137.246905	58.733607
2423.034065	42976.790182	58.738612
2421.735179	42842.944711	58.743617
2421.089659	42682.958341	58.748621
2420.415011	42496.528920	58.753626
2419.251916	42323.128280	58.758631
2418.100936	42159.495491	58.763636
2417.679955	42005.361497	58.768641
2417.438562	41828.967412	58.773645
2416.532449	41717.829487	58.778650
2415.428640	41582.701209	58.783655
2414.674974	41409.244870	58.788660
2414.288689	41253.777729	58.793665
2413.072678	41153.775521	58.798669
2412.203186	41008.436104	58.803674
2411.423897	40864.466975	58.808679
2411.241968	40719.169602	58.813684
2410.301199	40625.011200	58.818689
2409.721313	40453.119531	58.823693
2409.189523	40355.131965	58.828698
2407.971508	40202.656684	58.833703
2407.466497	40046.620175	58.838708
2406.673711	39976.236087	58.843713
2406.062457	39835.662147	58.848717
2405.735055	39699.700022	58.853722
2404.721088	39616.585382	58.858727
2404.008758	39444.935136	58.863732
2403.404560	39343.656158	58.868737
2402.805882	39218.403654	58.873741
2402.535291	39066.951807	58.878746
2401.381463	38990.944452	58.883751
2400.448956	38843.790275	58.888756
2400.166894	38715.973072	58.893761
2399.062802	38633.337551	58.898765
2398.572508	38495.033418	58.903770
2398.030624	38411.168524	58.908775
2397.754958	38279.917044	58.913780
2396.533720	38144.991165	58.918785
2396.018705	38021.054153	58.923789
2395.447010	37949.902067	58.928794
2394.639276	37823.597600	58.933799
2393.805843	37700.644464	58.938804
2393.557553	37576.015600	58.943809
2392.739426	37486.086643	58.948813
2392.722163	37348.643152	58.953818
2391.636393	37272.070037	58.958823
2391.365816	37111.902632	58.963828
2390.527713	37035.401966	58.968833
2389.711797	36877.208955	58.973837
2388.896036	36804.967115	58.978842
2388.143308	36680.940144	58.983847
2387.504315	36562.564005	58.988852
2387.132237	36426.317587	58.993857
2386.881976	36322.185622	58.998861
2385.811632	36221.693164	59.003866
2385.155863	36081.922495	59.008871
2384.685786	35994.260236	59.013876
2383.727492	35873.263771	59.018881
2383.180419	35749.283783	59.023885
2382.938123	35626.229965	59.028890
2382.434835	35510.223121	59.033895
2381.756138	35389.610966	59.038900
2381.117139	35279.416500	59.043905
2380.403337	35133.952765	59.048909
2379.813686	35043.289487	59.053914
2378.529198	34905.814098	59.058919
2378.613079	34756.881401	59.063924
2377.762058	34681.978700	59.068929
2376.746921	34572.890038	59.073933
2376.388532	34408.466915	59.078938
2375.729126	34286.152882	59.083943
2375.277532	34197.394039	59.088948
2374.435866	34097.737831	59.093953
2373.827076	33955.569082	59.098957
2373.645977	33811.010657	59.103962
2372.488156	33682.768582	59.108967
2372.034068	33592.812335	59.113972
2371.363390	33496.356431	59.118977
2370.712821	33352.581261	59.123981
2370.262380	33189.052381	59.128986
2368.971803	33102.167575	59.133991
2368.352907	32995.336781	59.138996
2366.988227	32859.047811	59.144001
2366.409415	32733.330231	59.149005
2366.581149	32611.750069	59.154010
2365.400240	32556.053478	59.159015
2365.135930	32413.351903	59.164020
2364.382319	32275.286372	59.169025
2363.653841	32146.599412	59.174029
2362.949335	32065.882980	59.179034
2362.153109	31943.709094	59.184039
2361.731762	31792.345454	59.189044
2361.323260	31707.679348	59.194049
2360.472759	31572.234371	59.199053
2359.674570	31454.934310	59.204058
2358.537706	31368.810109	59.209063
2358.841604	31225.527830	59.214068
2358.201253	31113.204523	59.219073
2357.369063	31005.614636	59.224077
2356.808967	30859.107070	59.229082
2356.188642	30769.522826	59.234087
2355.619593	30619.109841	59.239092
2354.952910	30517.366660	59.244097
2354.125455	30383.909171	59.249101
2353.602886	30269.217211	59.254106
2352.534205	30130.439183	59.259111
2352.371008	30038.109990	59.264116
2351.649511	29883.977129	59.269121
2350.559187	29788.006107	59.274125
2349.799097	29667.393383	59.279130
2349.284044	29533.229739	59.284135
2348.847792	29412.641797	59.289140
2347.661404	29314.309482	59.294145
2347.528981	29180.983851	59.299149
2346.883359	29057.388911	59.304154
2345.696276	28971.999425	59.309159
2345.614249	28814.757749	59.314164
2345.065835	28728.672654	59.319169
2343.971872	28601.474446	59.324173
2343.605264	28477.774893	59.329178
2342.606846	28346.285423	59.334183
2342.169733	28249.516889	59.339188
2341.438291	28099.938072	59.344193
2340.868639	28021.092283	59.349197
2340.329285	27860.137803	59.354202
2339.295477	27788.554600	59.359207
2338.996271	27635.789961	59.364212
2337.910937	27549.907657	59.369217
2337.453239	27405.080755	59.374221
2336.656414	27287.822350	59.379226
2336.009968	27196.153852	59.384231
2335.911542	27047.549871	59.389236
2335.023471	26939.349687	59.394241
2334.040516	26815.751910	59.399245
2333.330512	26721.157270	59.404250
2332.732698	26565.819238	59.409255
2332.069250	26478.097091	59.414260
2331.191262	26361.527267	59.419265
2330.919115	26237.709835	59.424269
2330.025141	26122.280004	59.429274
2329.627078	26004.493832	59.434279
2329.199119	25878.326639	59.439284
2328.181851	25770.588402	59.444289
2327.421595	25659.809811	59.449293
2327.028359	25525.360000	59.454298
2326.209078	25421.012364	59.459303
2325.383493	25314.988986	59.464308
2324.839327	25193.274521	59.469313
2324.273203	25065.513512	59.474317
2323.607669	24955.433166	59.479322
2322.649482	24847.502240	59.484327
2322.196417	24704.491620	59.489332
2321.461962	24618.341135	59.494337
2320.584548	24499.148717	59.499341
2320.031046	24366.649896	59.504346
2319.043185	24280.629086	59.509351
2318.835316	24136.862880	59.514356
2318.031829	24051.733262	59.519361
2317.304158	23927.257333	59.524365
2317.048037	23796.067231	59.529370
2315.904540	23712.477152	59.534375
2315.705382	23579.240089	59.539380
2314.851838	23492.596569	59.544385
2314.113368	23382.641314	59.549389
2313.432832	23261.677073	59.554394
2312.561933	23133.326072	59.559399
2312.305449	23045.768279	59.564404
2311.819947	22912.027906	59.569409
2311.063837	22798.872025	59.574413
2310.438099	22697.259433	59.579418
2309.736578	22576.296644	59.584423
2309.300924	22451.921783	59.589428
2308.660430	22315.889586	59.594433
2307.880358	22230.957114	59.599437
2307.208008	22078.300005	59.604442
2306.178316	22007.140042	59.609447
2305.492129	21862.982338	59.614452
2304.896501	21765.093816	59.619457
2304.177614	21640.537343	59.624461
2304.060473	21529.100470	59.629466
2302.674758	21437.636827	59.634471
2302.668768	21283.849764	59.639476
2301.876237	21184.778596	59.644481
2300.809536	21106.107401	59.649485
2300.314146	20958.098058	59.654490
2299.368010	20849.036597	59.659495
2298.959629	20746.429008	59.664500
2298.078746	20627.127350	59.669505
2297.695246	20523.021144	59.674509
2296.615027	20416.212743	59.679514
2295.890251	20310.017396	59.684519
2295.190890	20212.746720	59.689524
2294.692614	20096.602833	59.694529
2293.715896	19994.008996	59.699533
2293.422052	19889.491718	59.704538
2292.381241	19782.310338	59.709543
2291.856190	19688.035398	59.714548
2290.955654	19573.629709	59.719553
2290.456731	19495.934819	59.724557
2289.780138	19377.942090	59.729562
2288.337520	19286.823714	59.734567
2288.171785	19195.386102	59.739572
2287.778142	19081.118348	59.744577
2286.788605	19004.892736	59.749581
2286.405594	18885.753929	59.754586
2285.633202	18786.904732	59.759591
2284.984910	18707.813343	59.764596
2284.459585	18579.060671	59.769601
2283.728041	18510.685142	59.774605
2283.137682	18404.980334	59.779610
2282.199780	18303.610691	59.784615
2281.778500	18231.872103	59.789620
2281.044623	18121.508912	59.794625
2280.115412	18018.226673	59.799629
2279.459280	17938.579586	59.804634
2278.807394	17835.033946	59.809639
2278.221655	17737.339955	59.814644
2277.429331	17647.555420	59.819649
2276.538033	17560.494408	59.824653
2276.471963	17463.454013	59.829658
2275.462255	17381.115569	59.834663
2274.654759	17276.286838	59.839668
2274.453209	17191.733194	59.844673
2273.502311	17110.155484	59.849677
2273.222196	17011.126042	59.854682
2272.335248	16918.143631	59.859687
2271.339709	16822.497088	59.864692
2270.637931	16731.599047	59.869697
2270.096162	16649.699580	59.874701
2269.201672	16550.708583	59.879706
2268.462985	16473.950869	59.884711
2267.624906	16389.953075	59.889716
2267.264086	16308.415249	59.894721
2266.288831	16218.904228	59.899725
2266.039348	16157.090701	59.904730
2265.137210	16050.392298	59.909735
2264.666769	15962.770764	59.914740
2263.642539	15890.099594	59.919745
2263.266958	15806.615383	59.924750
2262.884703	15727.006300	59.929754
2262.016841	15648.888128	59.934759
2261.186958	15559.398433	59.939764
2260.916012	15468.360478	59.944769
2260.033158	15381.783978	59.949774
2259.691348	15301.423757	59.954778
2258.573197	15236.993513	59.959783
2258.049329	15130.547321	59.964788
2257.106547	15049.336967	59.969793
2256.359516	14982.211907	59.974798
2255.940804	14878.024746	59.979802
2255.086625	14834.766280	59.984807
2254.496773	14726.636930	59.989812
2253.919612	14657.298053	59.994817
2252.995768	14602.336924	59.999822
2252.681778	14499.817524	60.004826
2251.945552	14421.352471	60.009831
2251.127593	14351.950188	60.014836
2250.548481	14260.639387	60.019841
2249.645782	14188.647552	60.024846
2249.302087	14119.298051	60.029850
2248.347206	14050.280501	60.034855
2247.642455	13970.324454	60.039860
2247.135918	13878.238433	60.044865
2246.244286	13835.051951	60.049870
2245.969108	13728.648855	60.054874
2244.810360	13669.145981	60.059879
2244.261554	13605.568049	60.064884
2243.828548	13505.639447	60.069889
2242.783058	13462.939391	60.074894
2242.930764	13365.157416	60.079898
2241.778419	13284.766405	60.084903
2241.182776	13224.806820	60.089908
2240.828603	13148.916813	60.094913
2240.005751	13075.809035	60.099918
2239.147582	12989.480295	60.104922
2238.614281	12923.654732	60.109927
2238.098655	12846.645054	60.114932
2237.397049	12787.585645	60.119937
2236.702332	12706.242867	60.124942
2236.327306	12612.069066	60.129946
2235.183515	12543.755903	60.134951
2234.657343	12470.897715	60.139956
2233.994409	12408.159806	60.144961
2233.494434	12316.822949	60.149966
2232.573464	12241.512086	60.154970
2231.848678	12170.840262	60.159975
2231.259376	12097.602497	60.164980
2230.643265	12032.557171	60.169985
2229.487607	11966.084676	60.174990
2229.390714	11879.640494	60.179994
2228.416105	11811.426497	60.184999
2227.642596	11730.413924	60.190004
2227.082940	11680.271225	60.195009
2226.427922	11611.213641	60.200014
2225.994705	11522.307774	60.205018
2225.069738	11480.577743	60.210023
2224.330208	11402.373698	60.215028
2224.144043	11330.828939	60.220033
2223.196797	11259.883415	60.225038
2222.479800	11183.103899	60.230042
2221.851549	11119.054466	60.235047
2221.289278	11048.588950	60.240052
2220.799927	10980.527386	60.245057
2219.926346	10909.638890	60.250062
2219.247211	10843.500902	60.255066
2218.376274	10789.828822	60.260071
2218.018299	10703.587030	60.265076
2217.225021	10635.162986	60.270081
2216.526464	10575.399266	60.275086
2215.861260	10508.137795	60.280090
2214.822170	10441.113465	60.285095
2214.387070	10360.114525	60.290100
2213.770874	10321.514794	60.295105
2213.054141	10242.545860	60.300110
2212.229778	10193.827269	60.305114
2211.775520	10110.065765	60.310119
2211.256022	10035.353127	60.315124
2210.860280	9992.648968	60.320129
2209.939828	9912.433987	60.325134
2209.149928	9868.902763	60.330138
2208.670750	9776.144626	60.335143
2208.001454	9724.499989	60.340148
2207.541715	9655.302836	60.345153
2206.395706	9582.629116	60.350158
2205.828563	9528.381992	60.355162
2205.225590	9466.067911	60.360167
2204.549657	9388.337606	60.365172
2203.987027	9334.748046	60.370177
2203.623907	9265.100295	60.375182
2202.881900	9187.099474	60.380186
2202.179526	9121.389703	60.385191
2201.214617	9055.625624	60.390196
2200.341209	8989.043807	60.395201
2199.984469	8932.818022	60.400206
2199.432624	8867.282713	60.405210
2198.617694	8802.534158	60.410215
2198.241689	8729.984610	60.415220
2197.923541	8666.425987	60.420225
2197.215002	8593.264030	60.425230
2196.100234	8525.772741	60.430234
2195.294675	8466.811068	60.435239
2194.897972	8394.460498	60.440244
2194.072411	8332.144250	60.445249
2193.339258	8263.883609	60.450254
2192.810319	8181.146607	60.455258
2191.828738	8133.267873	60.460263
2191.354775	8068.255807	60.465268
2190.862310	7993.242593	60.470273
2190.333123	7927.733450	60.475278
2189.521197	7864.131154	60.480282
2188.807777	7799.059252	60.485287
2188.028011	7740.366149	60.490292
2187.542455	7667.376878	60.495297
2186.627025	7604.125798	60.500302
2186.141334	7543.819382	60.505306
2185.542923	7490.946946	60.510311
2184.846083	7414.503414	60.515316
2184.181412	7359.780312	60.520321
2183.501436	7288.348555	60.525326
2182.717305	7206.391852	60.530330
2182.106988	7157.866531	60.535335
2181.410422	7099.117797	60.540340
2181.156021	7034.433531	60.545345
2180.483442	6974.263989	60.550350
2179.879746	6894.525329	60.555354
2178.971973	6832.225256	60.560359
2178.296639	6774.376039	60.565364
2177.747946	6690.494867	60.570369
2176.968448	6638.979370	60.575374
2176.405860	6580.524583	60.580378
2175.455695	6511.417455	60.585383
2175.053455	6438.828801	60.590388
2174.536705	6385.124649	60.595393
2173.270439	6323.032677	60.600398
2173.008430	6253.070600	60.605402
2172.213132	6196.858865	60.610407
2171.315751	6126.376648	60.615412
2170.914105	6073.480412	60.620417
2170.476135	6001.435927	60.625422
2170.167807	5937.450430	60.630426
2169.030106	5881.992267	60.635431
2168.304391	5810.786273	60.640436
2167.811568	5743.937761	60.645441
2166.731809	5690.491887	60.650446
2166.158057	5614.732988	60.655450
2165.682168	5559.644272	60.660455
2164.888483	5504.798637	60.665460
2164.503782	5436.235435	60.670465
2163.630005	5353.760565	60.675470
2162.942634	5313.026388	60.680474
2162.448494	5254.439788	60.685479
2161.521862	5174.145649	60.690484
2160.999134	5117.114741	60.695489
2160.072666	5057.782781	60.700494
2159.523060	4987.876266	60.705498
2159.060259	4954.139532	60.710503
2158.205381	4891.085257	60.715508
2157.848115	4815.893942	60.720513
2156.809820	4767.072115	60.725518
2156.235494	4686.018070	60.730522
2155.651984	4634.468223	60.735527
2155.202476	4569.391125	60.740532
2154.452626	4519.913124	60.745537
2153.520180	4462.228912	60.750542
2153.220525	4392.026091	60.755546
2152.378639	4334.279904	60.760551
2151.161967	4276.533473	60.765556
2150.845338	4217.097891	60.770561
2150.098726	4160.257640	60.775566
2149.873282	4099.800946	60.780570
2149.103488	4045.680948	60.785575
2148.142393	3986.582789	60.790580
2148.103460	3925.907151	60.795585
2147.014074	3867.970209	60.800590
2146.185225	3801.752445	60.805594
2145.925177	3739.509357	60.810599
2145.052920	3679.232736	60.815604
2144.611574	3624.285374	60.820609
2143.628365	3554.489968	60.825614
2143.024365	3495.427032	60.830618
2142.274712	3446.380847	60.835623
2141.383482	3391.826713	60.840628
2141.123690	3332.327337	60.845633
2140.137098	3267.073895	60.850638
2139.717659	3207.009691	60.855642
2138.955903	3154.513880	60.860647
2138.354287	3097.483620	60.865652
2137.648678	3045.318391	60.870657
2136.636355	2983.563794	60.875662
2136.568972	2931.100551	60.880666
2135.584347	2863.541965	60.885671
2135.197818	2814.717864	60.890676
2134.525081	2752.661954	60.895681
2133.662520	2703.987887	60.900686
2133.254911	2645.353022	60.905690
2132.798572	2587.010011	60.910695
2131.950909	2523.882770	60.915700
2131.201099	2455.850366	60.920705
2130.416040	2405.706148	60.925710
2130.089227	2345.578741	60.930714
2129.265384	2294.378079	60.935719
2128.449236	2229.032053	60.940724
2127.820951	2175.090514	60.945729
2127.058969	2113.694944	60.950734
2126.531231	2064.472310	60.955738
2125.957034	2003.379384	60.960743
2125.199935	1951.430474	60.965748
2124.384148	1886.199479	60.970753
2123.393851	1844.825964	60.975758
2122.835080	1775.339177	60.980762
2122.497426	1723.567389	60.985767
2121.623132	1679.080178	60.990772
2121.224770	1625.815441	60.995777
2120.352603	1570.016085	61.000782
2119.787340	1517.241880	61.005786
2119.105291	1461.316573	61.010791
2118.409289	1408.464157	61.015796
2117.564134	1343.550933	61.020801
2116.853942	1294.761997	61.025806
2116.340260	1245.494173	61.030810
2115.788266	1198.816508	61.035815
2115.031307	1149.235944	61.040820
2114.692343	1087.640383	61.045825
2113.888219	1047.838667	61.050830
2112.780530	988.776721	61.055834
2112.335593	931.342935	61.060839
2111.556384	878.114568	61.065844
2110.709888	842.096972	61.070849
2109.869217	792.896768	61.075854
2109.589062	762.487037	61.080858
2108.824783	691.648754	61.085863
2108.024631	650.245327	61.090868
2107.734407	599.578608	61.095873
2107.151859	554.383090	61.100878
2105.923126	497.474369	61.105882
2105.464020	450.952316	61.110887
2104.736072	397.386431	61.115892
2104.401586	377.031066	61.120897
2103.234518	322.067043	61.125902
2102.797175	265.639180	61.130906
2102.141989	243.299121	61.135911
2101.124008	177.448762	61.140916
2100.500065	150.154039	61.145921
2099.266636	99.206687	61.150926
2098.540409	87.949419	61.155930
2097.960444	38.279927	61.160935
2097.010452	5.298982	61.165940
2096.518368	-19.248938	61.170945
2093.259304	33.757454	61.175950
2089.250950	90.680074	61.180954
2090.321354	118.116578	61.185959
2091.271500	77.924031	61.190964
2092.166398	65.371932	61.195969
2091.046874	113.611210	61.200974
2090.619679	74.271161	61.205978
2090.493829	106.706961	61.210983
2089.276270	91.662735	61.215988
2088.809157	96.612510	61.220993
2087.254171	118.700589	61.225998
2086.429333	98.070219	61.231002
2086.054201	103.853761	61.236007
2085.668672	126.014869	61.241012
2085.169946	105.983987	61.246017
2084.130392	124.724559	61.251022
2084.100033	121.517205	61.256026
2083.994188	121.781509	61.261031
2082.923208	107.778403	61.266036
2082.283417	119.572446	61.271041
2081.552359	102.683321	61.276046
2080.332194	108.526860	61.281050
2079.572206	137.977410	61.286055
2078.660109	106.332161	61.291060
2078.911805	132.440001	61.296065
2078.173284	113.178841	61.301070
2077.839403	128.762472	61.306074
2076.838983	105.733139	61.311079
2075.998955	132.506224	61.316084
2075.277618	102.183678	61.321089
2074.333661	116.362927	61.326094
2073.737124	120.617349	61.331098
2073.807834	106.942391	61.336103
2073.165477	107.734946	61.341108
2072.642914	110.806003	61.346113
2071.279576	129.976421	61.351118
2070.568733	114.317202	61.356122
2070.067721	97.210238	61.361127
2069.284755	112.341599	61.366132
2069.024033	110.555309	61.371137
2068.080966	114.103093	61.376142
2067.468874	111.439054	61.381146
2066.970417	97.329335	61.386151
2066.685140	114.064242	61.391156
2066.299738	101.846179	61.396161
2064.469837	116.610716	61.401166
2063.954678	117.856150	61.406170
2064.082298	116.374063	61.411175
2063.129176	117.763118	61.416180
2062.830182	111.063035	61.421185
2062.169822	111.174083	61.426190
2060.804901	106.730963	61.431194
2060.160754	105.339826	61.436199
2059.630593	116.258647	61.441204
2059.452014	110.887686	61.446209
2058.911718	109.133153	61.451214
2058.041908	105.814616	61.456218
2057.423615	103.891122	61.461223
2055.848522	115.221777	61.466228
2055.742116	101.417249	61.471233
2055.196164	108.254454	61.476238
2054.721702	111.425108	61.481242
2054.039941	110.382125	61.486247
2053.324134	112.965062	61.491252
2052.816186	112.066373	61.496257
2052.139964	118.840684	61.501262
2051.493001	107.449421	61.506266
2050.361760	113.490162	61.511271
2049.676919	110.293650	61.516276
2049.536611	107.999418	61.521281
2048.854245	115.384956	61.526286
2047.929076	107.587407	61.531290
2047.022613	107.584562	61.536295
2046.665512	113.609665	61.541300
2046.586189	110.479469	61.546305
2045.253633	100.203076	61.551310
2044.469050	109.892887	61.556314
2044.312762	104.411165	61.561319
2042.919465	112.078264	61.566324
2042.633321	101.545908	61.571329
2041.990331	106.622951	61.576334
2041.716217	104.649564	61.581338
2040.925998	106.712906	61.586343
2039.657937	113.399810	61.591348
2039.497149	106.024969	61.596353
2039.081016	106.226564	61.601358
2038.141516	105.915167	61.606362
2037.291361	112.245597	61.611367
2035.968011	115.557295	61.616372
2036.536895	106.278461	61.621377
2036.245699	120.858718	61.626382
2034.801418	114.961707	61.631386
2033.956417	92.338244	61.636391
2033.206091	116.235029	61.641396
2032.821733	105.067010	61.646401
2031.782439	102.185372	61.651406
2031.693593	109.760546	61.656410
2031.042069	107.290424	61.661415
2030.016134	109.723903	61.666420
2029.755876	99.868655	61.671425
2028.916980	96.690297	61.676430
2028.354040	123.816760	61.681434
2028.087332	106.300469	61.686439
2026.998961	111.192752	61.691444
2026.625466	101.029063	61.696449
2026.237904	109.066367	61.701454
2024.893528	126.330492	61.706458
2024.657003	84.891322	61.711463
2023.035206	125.806921	61.716468
2023.083279	105.917922	61.721473
2022.423835	99.314486	61.726478
2021.771708	109.032159	61.731482
2020.833391	110.836752	61.736487
2020.218577	116.341394	61.741492
2019.821457	103.390378	61.746497
2019.019271	94.499474	61.751502
2018.301200	118.216110	61.756506
2017.716668	102.765525	61.761511
2017.182100	112.500811	61.766516
2016.812561	95.136469	61.771521
2016.428719	118.751173	61.776526
2015.779260	106.407884	61.781530
2014.342424	98.264235	61.786535
2013.190225	125.919450	61.791540
2012.901316	98.496003	61.796545
2012.041967	96.566631	61.801550
2012.170578	122.159401	61.806554
2011.466548	110.329374	61.811559
2010.422010	102.553946	61.816564
2009.911778	108.461437	61.821569
2009.312828	119.268186	61.826574
2008.740697	100.031128	61.831578
2008.309436	108.966305	61.836583
2007.517158	112.562710	61.841588
2006.511822	98.363165	61.846593
2005.310603	120.057669	61.851598
2004.762064	103.707285	61.856602
2004.949220	97.247004	61.861607
2004.139015	128.656102	61.866612
2003.548225	94.134161	61.871617
2002.725503	103.421617	61.876622
2002.020958	114.861685	61.881626
2001.559898	99.238555	61.886631
2000.827781	100.780198	61.891636
2000.300215	116.812429	61.896641
1998.910738	103.774520	61.901646
1997.996124	99.159040	61.906650
1997.958763	102.230357	61.911655
1997.600239	128.654206	61.916660
1996.953832	94.383936	61.921665
1995.933596	116.573233	61.926670
1995.220616	113.445855	61.931674
1994.902278	102.029260	61.936679
1994.288187	112.833679	61.941684
1994.135589	105.582119	61.946689
1992.742675	104.693035	61.951694
1991.546056	110.876632	61.956698
1991.073196	101.354745	61.961703
1990.260208	112.190736	61.966708
1990.358399	108.502535	61.971713
1989.233482	107.563028	61.976718
1988.642754	109.156345	61.981722
1988.090443	111.071556	61.986727
1987.620015	108.467049	61.991732
1987.179731	101.907678	61.996737
1986.676298	111.958129	62.001742
1985.578527	110.402486	62.006746
1984.785481	119.712053	62.011751
1983.857180	111.066666	62.016756
1983.406045	102.911640	62.021761
1982.712599	104.525994	62.026766
1982.251643	105.029589	62.031770
1982.053998	104.414379	62.036775
1981.118030	109.905353	62.041780
1980.694112	97.256637	62.046785
1979.207134	115.817517	62.051790
1978.075710	113.043561	62.056794
1978.486705	106.684933	62.061799
1977.573367	93.487891	62.066804
1976.836049	128.621039	62.071809
1976.551767	106.758516	62.076814
1975.552007	119.308269	62.081818
1975.634090	113.239959	62.086823
1974.573990	108.898303	62.091828
1973.460927	125.674737	62.096833
1972.696027	97.418585	62.101838
1971.592954	106.550290	62.106842
1971.646695	109.181390	62.111847
1970.447824	103.480421	62.116852
1970.251856	105.954050	62.121857
1969.675226	123.034816	62.126862
1969.214424	110.918625	62.131866
1969.269563	102.714772	62.136871
1968.335411	119.898018	62.141876
1967.445303	106.463904	62.146881
1966.489347	100.052627	62.151886
1965.617048	116.926445	62.156890
1965.425919	109.586390	62.161895
1964.523744	108.239392	62.166900
1963.482219	111.985756	62.171905
1962.511056	114.960896	62.176910
1961.989515	116.473854	62.181914
1962.353202	100.798654	62.186919
1961.027041	128.099891	62.191924
1960.921631	104.187422	62.196929
1960.133143	101.193464	62.201934
1959.205915	127.273943	62.206938
1958.238352	109.898887	62.211943
1957.174003	104.723747	62.216948
1957.374849	144.656242	62.221953
1956.479313	112.786096	62.226958
1955.900605	146.793444	62.231962
1955.615441	116.994607	62.236967
1955.259806	96.244096	62.241972
1953.700138	135.705451	62.246977
1952.792555	102.828038	62.251982
1952.069321	114.321539	62.256986
1951.673486	114.032670	62.261991
1950.847183	116.126996	62.266996
1950.802344	118.720131	62.272001
1950.172116	113.799334	62.277006
1949.308642	105.624623	62.282010
1949.329700	130.375062	62.287015
1948.014355	105.366362	62.292020
1947.401578	132.533860	62.297025
1946.586753	99.223861	62.302030
1945.761455	127.226141	62.307034
1945.758200	92.335013	62.312039
1944.632263	125.221296	62.317044
1943.950752	105.303065	62.322049
1942.935400	116.303652	62.327054
1941.828337	139.298368	62.332058
1942.236800	94.918434	62.337063
1941.492031	134.762906	62.342068
1941.264445	93.707097	62.347073
1940.691924	133.990976	62.352078
1939.412784	110.887705	62.357082
1938.616474	108.101565	62.362087
1937.791345	116.000196	62.367092
1937.542034	125.299146	62.372097
1937.013075	98.355366	62.377102
1936.349762	117.518751	62.382106
1935.262794	115.120937	62.387111
1934.252749	120.663111	62.392116
1933.737718	114.959244	62.397121
1933.502835	111.118925	62.402126
1932.885704	114.479396	62.407130
1932.550889	117.664167	62.412135
1932.044514	110.678502	62.417140
1930.794270	107.395178	62.422145
1930.186649	115.035363	62.427150
1929.007877	123.601972	62.432154
1929.002181	111.083974	62.437159
1928.518025	125.843091	62.442164
1927.769576	109.756269	62.447169
1926.513717	109.436791	62.452174
1925.524393	112.306022	62.457178
1925.437177	101.324238	62.462183
1924.810112	109.831636	62.467188
1924.469023	105.125131	62.472193
1924.104832	103.061986	62.477198
1923.248187	109.674159	62.482202
1922.124738	106.072679	62.487207
1921.241000	119.524922	62.492212
1920.991512	111.087170	62.497217
1920.262763	124.956338	62.502222
1919.742497	113.568657	62.507226
1919.469694	108.722006	62.512231
1917.939381	111.139412	62.517236
1917.525718	110.624732	62.522241
1916.577819	104.964366	62.527246
1916.430618	114.557742	62.532250
1915.789192	106.302062	62.537255
1915.195518	112.820450	62.542260
1914.091039	97.996483	62.547265
1913.522399	93.975783	62.552270
1912.586187	108.607968	62.557274
1912.608896	102.216370	62.562279
1911.791127	108.525920	62.567284
1911.359457	113.542632	62.572289
1910.265911	97.133747	62.577294
1909.755665	107.336663	62.582298
1909.193783	104.926457	62.587303
1908.507386	116.943949	62.592308
1908.063784	112.053456	62.597313
1907.116607	110.371440	62.602318
1906.037517	113.179239	62.607322
1905.796282	103.478682	62.612327
1904.873216	121.290931	62.617332
1904.697719	119.639355	62.622337
1904.437986	113.701006	62.627342
1903.007694	112.288074	62.632346
1902.409816	92.900625	62.637351
1902.008120	124.102931	62.642356
1901.219349	94.035632	62.647361
1900.384068	120.133041	62.652366
1899.366076	128.134844	62.657370
1898.766159	100.037032	62.662375
1898.131947	126.395828	62.667380
1897.714337	99.595228	62.672385
1897.513265	137.951536	62.677390
1896.912910	90.619040	62.682394
1896.269046	126.013288	62.687399
1894.996471	135.887851	62.692404
1894.660938	82.429736	62.697409
1894.026817	123.609560	62.702414
1893.331297	119.692577	62.707418
1892.826443	94.440144	62.712423
1891.391738	131.000704	62.717428
1890.927900	108.944376	62.722433
1890.485862	129.766212	62.727438
1889.602310	118.967625	62.732442
1889.536781	98.806555	62.737447
1889.020237	111.197603	62.742452
1888.179808	115.336246	62.747457
1887.007845	99.802375	62.752462
1886.147143	109.166849	62.757466
1886.117756	112.642158	62.762471
1885.340151	104.367112	62.767476
1884.625869	114.011102	62.772481
1884.393021	116.545783	62.777486
1883.266970	112.377057	62.782490
1882.886606	107.602681	62.787495
1881.803136	112.349166	62.792500
1881.495637	112.278083	62.797505
1880.765585	103.539772	62.802510
1878.964284	97.231218	62.807514
1878.693029	120.645114	62.812519
1878.879707	104.086583	62.817524
1878.127421	122.835194	62.822529
1877.887053	100.696096	62.827534
1876.825683	116.808354	62.832538
1876.531359	101.767466	62.837543
1875.538417	108.158452	62.842548
1874.998002	107.644981	62.847553
1874.347611	98.949217	62.852558
1872.766574	108.659869	62.857562
1872.318796	100.934827	62.862567
1871.594617	108.254496	62.867572
1871.503485	90.819196	62.872577
1871.179225	116.177902	62.877582
1870.266610	114.138768	62.882586
1870.260565	92.826608	62.887591
1868.844418	107.208590	62.892596
1868.037643	108.438864	62.897601
1867.734825	95.100783	62.902606
1866.847127	90.178325	62.907610
1866.092190	108.684500	62.912615
1865.440733	112.242813	62.917620
1864.366276	96.691900	62.922625
1863.934382	115.328130	62.927630
1863.691152	93.831291	62.932634
1863.307585	123.851208	62.937639
1861.985348	104.290209	62.942644
1861.466363	110.574406	62.947649
1860.965126	98.682288	62.952654
1860.227222	129.371883	62.957658
1860.333246	90.664741	62.962663
1858.880579	134.404524	62.967668
1858.129727	88.311736	62.972673
1857.551319	129.913210	62.977678
1856.747686	86.668768	62.982682
1856.225209	113.826617	62.987687
1856.050790	98.814004	62.992692
1854.718688	119.184247	62.997697
1854.277482	86.661797	63.002702
1853.335835	128.153794	63.007706
1853.115536	85.004383	63.012711
1852.592459	121.798620	63.017716
1851.598027	110.793747	63.022721
1851.041244	101.630562	63.027726
1850.466644	115.112570	63.032730
1850.083089	97.892426	63.037735
1848.818644	120.954694	63.042740
1848.138375	95.512525	63.047745
1847.567767	111.050141	63.052750
1846.902087	105.187304	63.057754
1846.784045	89.364698	63.062759
1845.518697	117.572446	63.067764
1844.959743	90.587761	63.072769
1844.148314	114.003841	63.077774
1843.655422	91.427073	63.082778
1843.066195	112.187102	63.087783
1842.776702	91.181721	63.092788
1841.771537	122.667485	63.097793
1841.102516	99.517884	63.102798
1840.098673	117.823912	63.107802
1839.496377	98.698946	63.112807
1838.810162	121.519596	63.117812
1838.872494	101.724566	63.122817
1838.672492	91.922870	63.127822
1837.327006	107.318613	63.132826
1836.531901	101.711287	63.137831
1835.569967	104.457932	63.142836
1834.448767	107.833812	63.147841
1833.904680	114.366416	63.152846
1833.322322	110.474060	63.157850
1833.271101	99.157010	63.162855
1832.564099	112.470817	63.167860
1832.295784	114.763563	63.172865
1832.066919	99.575106	63.177870
1830.531935	104.901060	63.182874
1830.208996	116.577008	63.187879
1829.231867	89.546778	63.192884
1828.213469	120.703497	63.197889
1827.606318	111.501005	63.202894
1826.703763	97.755145	63.207898
1826.487595	115.584450	63.212903
1826.219582	89.450818	63.217908
1825.755561	99.722085	63.222913
1825.352948	110.860352	63.227918
1824.243237	105.657784	63.232922
1823.256230	89.304579	63.237927
1822.262407	128.688695	63.242932
1821.533773	102.098357	63.247937
1820.993364	108.729720	63.252942
1820.345823	100.449816	63.257946
1819.934134	113.546427	63.262951
1819.458132	90.385123	63.267956
1819.203303	114.570636	63.272961
1818.171456	94.074211	63.277966
1817.062374	94.221886	63.282970
1816.830391	114.890496	63.287975
1816.188212	102.246525	63.292980
1815.266850	99.696319	63.297985
1814.611114	93.302088	63.302990
1813.803093	119.275327	63.307994
1813.597571	93.018234	63.312999
1812.891043	117.575089	63.318004
1812.134101	77.365090	63.323009
1811.210632	92.350051	63.328014
1809.957556	97.464096	63.333018
1809.709959	112.581431	63.338023
1809.505076	103.398643	63.343028
1808.727499	98.834013	63.348033
1808.845812	99.292954	63.353038
1807.627978	120.687380	63.358042
1806.684936	85.778416	63.363047
1806.245860	91.928503	63.368052
1805.576454	103.200591	63.373057
1804.421794	99.183099	63.378062
1803.908104	104.603910	63.383066
1803.135947	106.174040	63.388071
1803.093467	102.773096	63.393076
1802.371575	100.322098	63.398081
1801.542346	120.603037	63.403086
1800.312368	98.933347	63.408090
1799.980644	108.475595	63.413095
1799.686575	109.466780	63.418100
1799.345817	97.878764	63.423105
1798.680983	94.811611	63.428110
1797.448339	105.821505	63.433114
1797.214117	96.974527	63.438119
1796.291696	100.569575	63.443124
1795.432836	105.486990	63.448129
1794.740588	109.163753	63.453134
1793.938413	92.251377	63.458138
1793.438185	117.125534	63.463143
1793.449330	86.571757	63.468148
1792.071399	123.795044	63.473153
1791.455195	93.107506	63.478158
1790.410544	112.840780	63.483162
1790.504071	96.738587	63.488167
1789.866707	110.556976	63.493172
1789.502439	101.675458	63.498177
1788.717771	91.234954	63.503182
1787.683575	118.783139	63.508186
1786.834032	87.281160	63.513191
1785.483971	109.727849	63.518196
1785.067254	99.508012	63.523201
1785.063892	85.961563	63.528206
1784.011333	125.208346	63.533210
1783.853605	90.023290	63.538215
1783.713136	120.703133	63.543220
1782.784406	92.957225	63.548225
1781.861989	120.314205	63.553230
1781.010107	96.761616	63.558234
1780.511722	106.476982	63.563239
1779.339083	110.739372	63.568244
1778.321294	108.557713	63.573249
1778.095083	109.380435	63.578254
1777.662886	90.319952	63.583258
1777.347021	117.566406	63.588263
1776.699856	97.832037	63.593268
1776.048524	93.740931	63.598273
1774.852018	113.706474	63.603278
1774.238354	107.262993	63.608282
1774.034783	104.255045	63.613287
1773.313100	107.930180	63.618292
1771.991824	104.986209	63.623297
1771.830271	109.811809	63.628302
1770.848250	93.304880	63.633306
1770.595109	113.812847	63.638311
1770.059907	100.413928	63.643316
1769.017832	109.021951	63.648321
1768.403212	114.012544	63.653326
1767.917582	102.602075	63.658330
1767.349388	94.449933	63.663335
1766.596364	115.822577	63.668340
1765.178141	119.373387	63.673345
1765.232966	103.453946	63.678350
1764.409984	102.162248	63.683354
1763.938643	119.477017	63.688359
1763.629517	88.068986	63.693364
1762.298945	109.916529	63.698369
1761.792649	93.796073	63.703374
1760.715170	108.274113	63.708378
1761.138089	77.929342	63.713383
1760.118260	121.929916	63.718388
1758.638254	100.462381	63.723393
1758.801134	68.142110	63.728398
1757.888512	121.916447	63.733402
1757.461935	80.141788	63.738407
1756.382065	132.479390	63.743412
1755.642411	120.628308	63.748417
1755.253891	82.118041	63.753422
1754.504387	121.252028	63.758426
1754.502865	94.976746	63.763431
1753.631265	93.475166	63.768436
1752.137749	118.688421	63.773441
1752.139301	100.188218	63.778446
1751.525813	97.980203	63.783450
1750.745311	114.494133	63.788455
1749.940398	107.087603	63.793460
1749.032217	110.085926	63.798465
1748.559864	91.093329	63.803470
1747.951099	114.075122	63.808474
1747.577219	85.115239	63.813479
1746.647278	107.433710	63.818484
1745.605107	110.230976	63.823489
1745.311300	87.378222	63.828494
1744.994183	113.516320	63.833498
1744.586647	116.917652	63.838503
1743.352333	98.228987	63.843508
1742.733403	121.728045	63.848513
1742.627472	88.321385	63.853518
1741.105619	124.324964	63.858522
1740.334460	103.151688	63.863527
1739.869720	113.069865	63.868532
1739.218958	110.238598	63.873537
1739.268596	102.786227	63.878542
1738.503679	90.194906	63.883546
1737.628962	105.996855	63.888551
1737.060603	105.117287	63.893556
1736.076986	103.830612	63.898561
1735.066977	93.441689	63.903566
1734.072375	116.899487	63.908570
1733.897565	90.913504	63.913575
1733.264836	96.227079	63.918580
1732.547356	111.250314	63.923585
1732.595908	89.902713	63.928590
1731.850480	114.959302	63.933594
1731.179451	90.687355	63.938599
1730.489573	113.002398	63.943604
1729.979561	111.391355	63.948609
1728.814433	96.829431	63.953614
1727.895261	118.551730	63.958618
1727.487461	102.540206	63.963623
1727.007758	98.525927	63.968628
1726.041069	102.148528	63.973633
1725.267001	101.667471	63.978638
1724.274150	110.767559	63.983642
1723.846161	88.696177	63.988647
1723.882586	103.121866	63.993652
1722.942450	98.860616	63.998657
1723.010773	92.920659	64.003662
1721.854330	113.140034	64.008666
1721.114993	104.814821	64.013671
1720.766694	91.897147	64.018676
1719.124770	106.349739	64.023681
1718.874617	99.470089	64.028686
1717.985120	110.505930	64.033690
1717.770298	102.918958	64.038695
1717.271407	95.093273	64.043700
1715.837198	106.217210	64.048705
1715.206301	98.313150	64.053710
1714.598638	104.302381	64.058714
1714.519201	96.041083	64.063719
1714.247932	93.204739	64.068724
1713.218569	100.572909	64.073729
1712.579305	101.636279	64.078734
1711.812578	103.194534	64.083738
1711.230280	99.358973	64.088743
1710.180303	103.195072	64.093748
1709.145807	96.638697	64.098753
1708.899180	95.629188	64.103758
1708.223243	106.925981	64.108762
1708.228136	94.552996	64.113767
1707.391704	91.153599	64.118772
1706.230140	106.275756	64.123777
1705.832776	83.871535	64.128782
1705.271599	111.451806	64.133786
1704.412961	89.530834	64.138791
1703.466395	94.588352	64.143796
1702.783747	100.557957	64.148801
1702.618664	84.131035	64.153806
1701.770543	111.542430	64.158810
1701.595765	74.389066	64.163815
1700.799076	112.116064	64.168820
1699.518290	91.730218	64.173825
1699.083463	86.972420	64.178830
1698.404851	111.712477	64.183834
1697.539648	100.423824	64.188839
1697.162589	80.224009	64.193844
1696.403198	119.258633	64.198849
1696.220105	86.015635	64.203854
1695.296656	105.217181	64.208858
1694.745906	99.041263	64.213863
1693.940279	96.311879	64.218868
1693.204955	97.663310	64.223873
1693.077107	100.638614	64.228878
1691.808485	101.694733	64.233882
1691.031095	101.562703	64.238887
1690.937359	97.591196	64.243892
1689.646486	103.187513	64.248897
1688.939156	90.738445	64.253902
1688.116773	107.235374	64.258906
1687.657506	103.525347	64.263911
1687.510588	94.398031	64.268916
1686.736019	99.346236	64.273921
1686.477820	91.699936	64.278926
1685.386984	104.915463	64.283930
1684.863051	104.763672	64.288935
1684.197048	103.667826	64.293940
1682.599675	103.448446	64.298945
1682.347991	97.746970	64.303950
1681.703243	104.224621	64.308954
1681.308016	90.494441	64.313959
1681.053444	107.189740	64.318964
1680.428443	104.258210	64.323969
1679.368434	96.930080	64.328974
1678.772367	100.492246	64.333978
1677.954843	94.804967	64.338983
1677.170345	106.180508	64.343988
1676.448842	102.255110	64.348993
1675.682039	95.530078	64.353998
1675.137097	101.793188	64.359002
1675.114120	99.966026	64.364007
1674.394330	94.083460	64.369012
1673.180538	103.639680	64.374017
1672.725553	89.168405	64.379022
1672.240343	99.373665	64.384026
1671.391085	95.854899	64.389031
1670.547629	95.356498	64.394036
1669.850222	104.673002	64.399041
1669.683890	98.276760	64.404046
1669.133841	104.859212	64.409050
1668.547836	105.666563	64.414055
1667.537542	94.587047	64.419060
1667.033438	104.249716	64.424065
1666.001433	92.538172	64.429070
1664.904687	99.417194	64.434074
1664.310236	100.623258	64.439079
1664.280235	86.456618	64.444084
1663.373787	90.151665	64.449089
1663.487576	92.309606	64.454094
1662.350509	108.752458	64.459098
1661.523704	96.152074	64.464103
1660.889273	82.172916	64.469108
1660.439848	116.487598	64.474113
1659.486567	104.836078	64.479118
1658.459137	96.835766	64.484122
1658.079357	96.452934	64.489127
1657.593539	87.776836	64.494132
1656.962736	102.491427	64.499137
1656.309364	96.744964	64.504142
1655.464307	95.083092	64.509146
1655.023626	86.980114	64.514151
1654.511056	96.492743	64.519156
1653.315606	108.953811	64.524161
1652.844776	98.714223	64.529166
1652.054963	92.885366	64.534170
1651.717512	93.612235	64.539175
1651.324524	99.602062	64.544180
1650.343046	102.817051	64.549185
1649.424745	96.035676	64.554190
1648.563016	83.049793	64.559194
1648.127429	100.803535	64.564199
1648.177047	93.958274	64.569204
1646.822863	93.593055	64.574209
1646.362357	86.376277	64.579214
1645.841003	88.748654	64.584218
1644.962327	100.855057	64.589223
1644.295015	96.438539	64.594228
1643.250969	97.637190	64.599233
1642.962001	93.256757	64.604238
1642.216962	92.963492	64.609242
1641.801428	97.752172	64.614247
1641.267930	101.159332	64.619252
1640.137485	105.976440	64.624257
1639.879758	98.989203	64.629262
1639.823450	107.301892	64.634266
1637.860177	95.200597	64.639271
1637.331115	87.562650	64.644276
1636.629193	102.725334	64.649281
1636.629085	94.825161	64.654286
1636.064228	101.681191	64.659290
1635.095792	104.550356	64.664295
1634.335180	98.724747	64.669300
1633.663516	115.885265	64.674305
1633.633677	101.486789	64.679310
1632.726882	107.247606	64.684314
1631.349935	111.165643	64.689319
1631.246239	97.504266	64.694324
1630.171577	104.248913	64.699329
1630.046961	97.445524	64.704334
1629.188311	103.577141	64.709338
1628.274938	107.549256	64.714343
1627.747622	106.636385	64.719348
1627.555750	107.341706	64.724353
1626.745155	97.198682	64.729358
1625.425714	99.155416	64.734362
1624.834398	115.738649	64.739367
1624.886891	102.042993	64.744372
1624.138905	114.432985	64.749377
1623.650974	106.034751	64.754382
1622.787185	100.760098	64.759386
1621.975264	101.363667	64.764391
1620.641202	96.354532	64.769396
1619.823520	117.504082	64.774401
1619.423783	93.488694	64.779406
1618.956324	89.494573	64.784410
1617.988464	109.677697	64.789415
1618.601710	93.381003	64.794420
1617.704562	119.447249	64.799425
1617.111037	83.536779	64.804430
1616.231696	123.002021	64.809434
1615.499572	95.904615	64.814439
1614.884931	111.873417	64.819444
1613.661413	84.161858	64.824449
1613.204818	123.968347	64.829454
1612.686113	90.844926	64.834458
1611.965587	115.129624	64.839463
1611.220646	98.793258	64.844468
1610.457302	107.240354	64.849473
1609.987807	110.722504	64.854478
1609.400626	103.130058	64.859482
1609.047724	101.962411	64.864487
1608.086418	102.383148	64.869492
1607.171792	100.390164	64.874497
1606.901445	90.263815	64.879502
1606.148149	113.948199	64.884506
1605.108243	114.271044	64.889511
1604.871886	94.875169	64.894516
1604.097938	110.747862	64.899521
1603.610833	117.970000	64.904526
1602.639907	95.767312	64.909530
1601.768641	99.535634	64.914535
1601.589631	108.128000	64.919540
1600.792881	109.525485	64.924545
1600.340086	98.308541	64.929550
1599.517217	103.898345	64.934554
1599.078978	112.855159	64.939559
1598.379200	104.566283	64.944564
1596.954643	115.316602	64.949569
1596.661778	105.811957	64.954574
1596.117344	99.349650	64.959578
1595.625509	103.224836	64.964583
1594.871385	88.517280	64.969588
1593.638378	104.011920	64.974593
1592.963608	98.850742	64.979598
1592.607566	108.713810	64.984602
1592.304767	90.060170	64.989607
1592.105994	114.332926	64.994612
1590.642035	93.613580	64.999617
1589.819050	108.158454	65.004622
1589.369866	99.596390	65.009626
1589.067828	99.046682	65.014631
1588.768444	79.577273	65.019636
1587.741080	108.277062	65.024641
1587.088938	88.742271	65.029646
1586.219415	121.057997	65.034650
1585.248285	111.766770	65.039655
1584.771839	97.349386	65.044660
1583.958228	112.022078	65.049665
1583.679860	106.668613	65.054670
1583.342330	107.143204	65.059674
1582.415490	92.239176	65.064679
1581.625040	96.672716	65.069684
1580.887626	112.637375	65.074689
1580.416677	88.672748	65.079694
1579.555318	95.643700	65.084698
1578.796597	95.483507	65.089703
1578.231119	89.973829	65.094708
1577.381468	105.920046	65.099713
1577.138270	108.137861	65.104718
1575.948795	93.294489	65.109722
1575.285204	123.472379	65.114727
1575.131241	99.750667	65.119732
1574.506860	102.806446	65.124737
1574.314160	103.636474	65.129742
1573.107774	104.520344	65.134746
1571.947543	90.117009	65.139751
1571.869719	116.787888	65.144756
1571.235783	93.992386	65.149761
1570.439439	100.003736	65.154766
1569.513108	100.598693	65.159770
1568.884458	115.126890	65.164775
1569.158107	94.085733	65.169780
1566.977226	109.650580	65.174785
1566.808370	84.299201	65.179790
1566.351704	113.259961	65.184794
1565.464081	85.663790	65.189799
1565.491027	130.511968	65.194804
1564.795920	98.020529	65.199809
1563.774585	98.605354	65.204814
1563.279013	115.763126	65.209818
1562.700721	80.723863	65.214823
1561.758882	122.275765	65.219828
1560.461663	108.248982	65.224833
1560.507300	106.152312	65.229838
1560.193372	95.159309	65.234842
1559.116204	107.765605	65.239847
1558.518956	81.613450	65.244852
1557.253555	133.015457	65.249857
1556.735945	97.318421	65.254862
1556.794033	97.458929	65.259866
1555.795349	110.366555	65.264871
1555.226725	78.107369	65.269876
1554.012449	120.990857	65.274881
1554.245643	84.856021	65.279886
1553.638800	119.826450	65.284890
1552.564414	95.396345	65.289895
1552.071788	93.872461	65.294900
1551.681385	110.642951	65.299905
1550.740566	99.240231	65.304910
1549.826824	108.269451	65.309914
1548.822672	85.466575	65.314919
1548.520220	120.435941	65.319924
1547.922619	97.992621	65.324929
1547.340812	114.309431	65.329934
1546.662029	105.638787	65.334938
1545.721167	96.215052	65.339943
1545.271666	95.177877	65.344948
1544.762044	108.893990	65.349953
1543.844238	89.382511	65.354958
1543.005440	113.403741	65.359962
1542.643995	99.988331	65.364967
1542.411793	109.842760	65.369972
1541.211316	104.052389	65.374977
1539.970197	105.862685	65.379982
1540.121015	82.792712	65.384986
1539.333772	124.931877	65.389991
1539.405155	96.849012	65.394996
1537.881436	100.490809	65.400001
1537.303562	100.981522	65.405006
1536.570008	94.691205	65.410010
1536.171424	105.300584	65.415015
1535.451687	91.115839	65.420020
1534.609787	95.707369	65.425025
1534.153542	104.942997	65.430030
1533.465173	99.102791	65.435034
1532.531159	99.919743	65.440039
1532.021069	105.726353	65.445044
1531.252618	97.738562	65.450049
1530.723199	96.843392	65.455054
1530.453463	92.226544	65.460058
1529.176573	101.214130	65.465063
1528.676558	95.496952	65.470068
1528.045133	111.400620	65.475073
1527.779423	98.209686	65.480078
1526.935481	90.451505	65.485082
1525.707213	103.390885	65.490087
1525.374548	107.254981	65.495092
1524.699716	104.552173	65.500097
1524.413041	87.143301	65.505102
1523.442479	103.089815	65.510106
1522.610595	106.268462	65.515111
1522.377832	89.716722	65.520116
1521.884085	98.740698	65.525121
1520.809805	90.661174	65.530126
1520.006804	104.089611	65.535130
1519.308624	102.049647	65.540135
1519.224147	89.192603	65.545140
1518.262047	96.096006	65.550145
1517.513253	98.775773	65.555150
1516.788255	81.540640	65.560154
1516.211916	101.555898	65.565159
1515.910796	83.102288	65.570164
1514.592864	96.145796	65.575169
1513.881350	99.458271	65.580174
1513.683746	90.469920	65.585178
1513.302195	98.328107	65.590183
1512.311651	93.165102	65.595188
1511.495432	98.148352	65.600193
1510.826753	92.429600	65.605198
1510.661461	90.336493	65.610202
1509.754027	93.926094	65.615207
1508.810960	88.222566	65.620212
1508.136704	90.974062	65.625217
1507.844952	92.480543	65.630222
1507.061399	100.131396	65.635226
1505.998802	99.964326	65.640231
1505.652925	89.170373	65.645236
1505.085377	107.724063	65.650241
1504.634822	91.730459	65.655246
1503.702673	84.429408	65.660250
1502.653234	109.658876	65.665255
1502.531252	87.873252	65.670260
1501.929585	103.538808	65.675265
1500.795569	83.825191	65.680270
1500.255627	92.225760	65.685274
1499.666866	95.797835	65.690279
1499.274605	94.502426	65.695284
1498.574635	100.916348	65.700289
1497.456887	94.444264	65.705294
1496.783335	85.042729	65.710298
1496.091240	104.983354	65.715303
1496.148232	89.993979	65.720308
1495.290529	98.413515	65.725313
1494.469857	91.682920	65.730318
1493.961971	90.016402	65.735322
1493.210353	93.448789	65.740327
1492.287618	100.539900	65.745332
1491.439370	99.633911	65.750337
1490.782324	86.361695	65.755342
1490.566730	91.031886	65.760346
1490.044696	93.451705	65.765351
1489.365666	102.333254	65.770356
1488.563648	98.411253	65.775361
1487.713033	88.717755	65.780366
1487.514495	92.368156	65.785370
1486.045171	105.650196	65.790375
1485.843749	108.091601	65.795380
1484.847748	81.093004	65.800385
1484.524373	100.807875	65.805390
1484.339825	99.399037	65.810394
1483.123099	100.377626	65.815399
1482.869890	87.612058	65.820404
1482.101613	95.903848	65.825409
1481.027545	106.582740	65.830414
1480.200401	100.479193	65.835418
1479.590630	106.855133	65.840423
1479.360436	98.311909	65.845428
1478.957550	105.135913	65.850433
1477.625868	103.559324	65.855438
1477.398107	91.955016	65.860442
1476.489741	111.553151	65.865447
1476.299585	96.943655	65.870452
1475.116003	84.412685	65.875457
1474.409010	89.864257	65.880462
1473.657633	86.268512	65.885466
1473.345501	102.014200	65.890471
1473.112834	92.269800	65.895476
1472.134806	95.250924	65.900481
1471.032363	100.651817	65.905486
1470.937760	96.981647	65.910490
1470.040688	104.492865	65.915495
1469.251114	96.773370	65.920500
1468.504995	100.761525	65.925505
1467.935191	111.171055	65.930510
1467.520256	91.018328	65.935514
1466.507381	98.473837	65.940519
1465.711081	89.191162	65.945524
1465.024769	90.053920	65.950529
1464.393054	105.587068	65.955534
1464.241076	103.253740	65.960538
1463.930621	100.980291	65.965543
1463.023560	88.337570	65.970548
1462.492593	92.042384	65.975553
1461.159209	97.625056	65.980558
1460.840686	100.143416	65.985562
1459.819709	100.099054	65.990567
1459.535248	96.913198	65.995572
1459.109916	80.147679	66.000577
1457.810883	110.647290	66.005582
1457.672256	93.678500	66.010586
1456.598289	95.802870	66.015591
1456.493947	75.890947	66.020596
1455.463262	109.211493	66.025601
1454.430322	101.302035	66.030606
1454.182261	85.159583	66.035610
1453.485128	111.807435	66.040615
1453.405173	90.923419	66.045620
1452.163092	89.793049	66.050625
1451.300108	103.521173	66.055630
1451.171611	98.505015	66.060634
1450.014390	82.953323	66.065639
1449.321487	109.425467	66.070644
1448.430866	81.322105	66.075649
1447.849052	111.293007	66.080654
1448.114421	91.290765	66.085658
1446.859904	95.429112	66.090663
1446.313211	101.966909	66.095668
1445.640793	94.326568	66.100673
1445.068820	81.493415	66.105678
1444.132964	102.125605	66.110682
1443.078027	94.801517	66.115687
1442.701529	90.950664	66.120692
1442.199477	93.756802	66.125697
1442.117906	93.938428	66.130702
1440.981529	81.650700	66.135706
1440.054041	107.630299	66.140711
1439.856688	97.183314	66.145716
1439.160098	91.484790	66.150721
1437.969477	91.960960	66.155726
1437.454657	96.152041	66.160730
1437.010465	101.244904	66.165735
1436.573335	91.299634	66.170740
1435.816531	112.360671	66.175745
1434.562996	92.232445	66.180750
1433.870249	107.418926	66.185754
1433.396082	72.363213	66.190759
1433.124135	99.293524	66.195764
1432.800380	98.673174	66.200769
1431.381207	95.754412	66.205774
1431.101233	90.200971	66.210778
1430.523322	87.697243	66.215783
1429.938197	101.089482	66.220788
1429.185122	92.369200	66.225793
1428.283274	92.018925	66.230798
1427.897435	89.361672	66.235802
1426.996629	93.025935	66.240807
1426.229918	80.185898	66.245812
1425.718987	104.596528	66.250817
1424.911270	91.884419	66.255822
1424.894313	82.239781	66.260826
1423.661912	86.052940	66.265831
1422.887866	98.617392	66.270836
1422.365264	91.738528	66.275841
1422.280517	88.689660	66.280846
1420.860249	81.392123	66.285850
1419.998689	113.097892	66.290855
1419.769653	80.008982	66.295860
1419.563193	115.030847	66.300865
1418.841830	90.593611	66.305870
1417.922095	82.721378	66.310874
1416.886710	88.242507	66.315879
1416.689293	87.245706	66.320884
1415.977957	104.067197	66.325889
1415.069848	91.011524	66.330894
1414.927688	83.805703	66.335898
1413.975033	86.167834	66.340903
1413.118077	101.038232	66.345908
1412.453545	92.237654	66.350913
1411.232991	86.948840	66.355918
1411.354399	94.607241	66.360922
1410.988575	91.457980	66.365927
1409.946056	78.103583	66.370932
1409.346690	111.961091	66.375937
1408.646888	88.420830	66.380942
1408.015445	87.802088	66.385946
1406.970991	100.355914	66.390951
1406.824125	89.752689	66.395956
1406.304232	76.383026	66.400961
1405.023914	103.443667	66.405966
1404.516310	90.064154	66.410970
1403.542252	77.220822	66.415975
1403.426390	90.951600	66.420980
1402.965373	93.178818	66.425985
1402.099615	97.309002	66.430990
1401.390618	86.516032	66.435994
1400.426506	97.697828	66.440999
1400.096121	94.218100	66.446004
1399.120372	92.044110	66.451009
1397.896971	98.686328	66.456014
1397.728250	69.752371	66.461018
1397.364752	104.053309	66.466023
1397.046212	75.198347	66.471028
1396.644176	73.652212	66.476033
1395.316249	97.962478	66.481038
1394.932222	76.578084	66.486042
1393.983459	75.730683	66.491047
1392.296623	96.436521	66.496052
1392.559972	76.861958	66.501057
1391.824922	91.979462	66.506062
1391.929212	75.330043	66.511066
1391.060413	77.350863	66.516071
1390.404316	83.828784	66.521076
1389.569850	77.862056	66.526081
1388.784308	92.011508	66.531086
1388.034712	85.179779	66.536090
1387.044582	83.845397	66.541095
1386.506676	89.202304	66.546100
1385.934879	88.876843	66.551105
1385.720138	82.578224	66.556110
1385.251544	78.396692	66.561114
1383.714245	97.730545	66.566119
1383.372309	88.254258	66.571124
1382.849836	85.128328	66.576129
1382.266532	80.562931	66.581134
1381.424444	82.499089	66.586138
1380.382090	81.013748	66.591143
1379.806361	77.383806	66.596148
1379.613253	103.415383	66.601153
1379.273241	84.841848	66.606158
1378.372702	82.999669	66.611162
1377.184702	100.131886	66.616167
1377.051062	85.658513	66.621172
1376.525754	86.243400	66.626177
1375.763500	100.551577	66.631182
1375.047070	83.871781	66.636186
1374.465919	95.929360	66.641191
1373.134925	97.929052	66.646196
1372.452117	92.316664	66.651201
1371.973283	93.799286	66.656206
1371.448652	87.810113	66.661210
1371.005289	92.584322	66.666215
1370.716810	93.284517	66.671220
1370.394923	79.515977	66.676225
1369.292811	82.535782	66.681230
1368.413945	83.906966	66.686234
1366.993085	83.924634	66.691239
1366.488156	92.742253	66.696244
1366.420531	82.399241	66.701249
1365.843936	81.410688	66.706254
1365.321225	86.183318	66.711258
1364.029802	92.825323	66.716263
1363.604191	88.714226	66.721268
1363.178345	90.540066	66.726273
1362.054215	96.633535	66.731278
1361.221639	88.063108	66.736282
1360.646117	86.101460	66.741287
1360.110894	106.143303	66.746292
1359.684264	88.097599	66.751297
1359.617560	94.959621	66.756302
1358.618988	101.145090	66.761306
1357.558804	100.902009	66.766311
1357.030378	92.067197	66.771316
1356.946418	90.986136	66.776321
1355.348844	81.873473	66.781326
1354.946325	94.259025	66.786330
1354.411645	99.254325	66.791335
1354.005899	77.487067	66.796340
1353.058644	105.768879	66.801345
1352.419168	92.293658	66.806350
1351.909294	72.734805	66.811354
1351.128164	95.392322	66.816359
1350.082049	97.471308	66.821364
1349.900259	87.816613	66.826369
1348.688908	79.337952	66.831374
1348.794041	80.579511	66.836378
1348.192271	78.800226	66.841383
1346.972401	91.307835	66.846388
1346.817732	88.910295	66.851393
1346.082442	83.061849	66.856398
1344.968392	73.473380	66.861402
1343.751074	82.158261	66.866407
1343.284621	85.483849	66.871412
1342.905428	87.991365	66.876417
1342.459618	87.932874	66.881422
1342.646901	83.073099	66.886426
1341.643665	79.776046	66.891431
1340.840144	79.430669	66.896436
1340.142314	89.382761	66.901441
1338.851006	81.951239	66.906446
1338.526632	80.742831	66.911450
1337.494133	76.589465	66.916455
1337.271287	95.082032	66.921460
1337.073244	67.318069	66.926465
1335.587031	93.094758	66.931470
1335.207102	70.099766	66.936474
1334.546248	84.183665	66.941479
1334.270833	70.163341	66.946484
1333.271823	92.163252	66.951489
1332.013099	84.415909	66.956494
1331.745577	73.316258	66.961498
1331.253450	98.252129	66.966503
1330.997416	84.003219	66.971508
1329.739479	87.489338	66.976513
1329.011840	95.594936	66.981518
1328.762502	98.472872	66.986522
1328.059281	78.883262	66.991527
1327.599274	84.298750	66.996532
1326.649258	86.668377	67.001537
1325.884484	83.517910	67.006542
1325.908688	84.035940	67.011546
1324.675341	89.374121	67.016551
1324.168216	88.115926	67.021556
1323.726333	84.059463	67.026561
1322.389009	82.136947	67.031566
1321.831963	88.367335	67.036570
1321.183875	96.217450	67.041575
1320.738239	82.988960	67.046580
1320.412899	72.775241	67.051585
1319.657947	95.073803	67.056590
1318.620924	81.877843	67.061594
1318.049831	77.811966	67.066599
1317.572133	85.914090	67.071604
1316.942400	72.800032	67.076609
1315.669350	98.758876	67.081614
1315.268735	78.689100	67.086618
1314.750453	85.093087	67.091623
1314.289019	92.117207	67.096628
1313.326830	100.056687	67.101633
1312.786821	89.823475	67.106638
1312.469091	70.585732	67.111642
1312.019422	70.947306	67.116647
1310.784053	91.929878	67.121652
1310.100260	82.700343	67.126657
1309.315819	84.083339	67.131662
1308.946214	83.355186	67.136666
1307.643977	83.011848	67.141671
1306.755904	84.056527	67.146676
1306.836298	83.698348	67.151681
1306.213365	81.422571	67.156686
1306.278538	89.255467	67.161690
1304.984199	80.082013	67.166695
1304.152631	84.138980	67.171700
1304.055545	88.744604	67.176705
1302.872530	76.357149	67.181710
1302.256165	80.266365	67.186714
1301.348263	87.862915	67.191719
1301.000440	90.098958	67.196724
1300.812702	77.786631	67.201729
1299.705569	82.436162	67.206734
1298.982199	86.789724	67.211738
1298.363162	84.860240	67.216743
1297.311673	78.338308	67.221748
1296.344865	69.292550	67.226753
1295.917342	83.884948	67.231758
1295.745299	80.637093	67.236762
1294.963512	86.176284	67.241767
1294.451090	83.198580	67.246772
1293.410794	79.587338	67.251777
1292.839256	89.364824	67.256782
1292.657633	70.901762	67.261786
1291.747094	77.633032	67.266791
1290.853979	79.038043	67.271796
1290.504203	68.785644	67.276801
1289.757235	77.370525	67.281806
1289.450271	76.597724	67.286810
1287.955953	89.402865	67.291815
1287.503368	81.293995	67.296820
1287.267393	69.613785	67.301825
1286.538608	90.323434	67.306830
1285.729261	77.606930	67.311834
1285.082290	82.161222	67.316839
1284.406434	90.217594	67.321844
1284.236690	85.986987	67.326849
1282.951246	94.624386	67.331854
1282.252719	83.151749	67.336858
1281.707878	78.566073	67.341863
1281.215631	81.643473	67.346868
1280.526045	76.461106	67.351873
1279.377619	81.355317	67.356878
1279.241690	80.413403	67.361882
1278.717782	79.440146	67.366887
1277.908076	95.832606	67.371892
1276.690081	80.416838	67.376897
1276.024576	84.620862	67.381902
1276.247222	79.938380	67.386906
1275.582942	86.006062	67.391911
1274.316875	82.750830	67.396916
1273.929728	73.436301	67.401921
1273.222646	83.047691	67.406926
1272.716544	84.242945	67.411930
1271.532004	76.434963	67.416935
1270.794045	87.009998	67.421940
1270.848518	78.817352	67.426945
1270.021632	81.047577	67.431950
1269.356020	80.506839	67.436954
1268.509047	81.593879	67.441959
1267.913655	89.263741	67.446964
1267.617700	81.175699	67.451969
1266.393002	80.391146	67.456974
1265.677145	74.862898	67.461978
1265.223336	83.585664	67.466983
1264.713561	84.817772	67.471988
1263.836650	76.800037	67.476993
1263.155190	85.451777	67.481998
1262.682031	75.193771	67.487002
1262.443412	82.450527	67.492007
1261.420488	69.608740	67.497012
1260.502443	75.636353	67.502017
1260.117040	81.700690	67.507022
1259.631203	75.801572	67.512026
1258.412959	81.448019	67.517031
1257.672803	89.263898	67.522036
1257.491253	75.719067	67.527041
1256.634150	84.833953	67.532046
1256.186668	83.395988	67.537050
1255.034261	79.143461	67.542055
1254.140182	79.271379	67.547060
1254.262817	77.421077	67.552065
1253.735353	83.217862	67.557070
1252.628355	78.324217	67.562074
1251.375656	94.772931	67.567079
1251.105791	80.653971	67.572084
1250.717644	76.051270	67.577089
1250.339049	79.892726	67.582094
1249.611780	77.537368	67.587098
1248.678573	75.069688	67.592103
1248.063341	81.342451	67.597108
1247.644094	76.184911	67.602113
1246.612992	80.857062	67.607118
1246.033977	78.719390	67.612122
1245.628129	80.519990	67.617127
1244.801344	85.301570	67.622132
1243.773325	71.710013	67.627137
1243.044502	82.289905	67.632142
1242.756597	82.524847	67.637146
1242.335955	78.886048	67.642151
1241.724849	80.189463	67.647156
1240.787672	83.198860	67.652161
1240.088324	86.301317	67.657166
1239.450631	87.648383	67.662170
1239.075727	79.751088	67.667175
1237.837145	78.711728	67.672180
1237.553749	78.324670	67.677185
1236.622326	81.946552	67.682190
1236.686847	91.334332	67.687194
1235.620200	67.002606	67.692199
1234.608905	96.914027	67.697204
1234.479942	71.242648	67.702209
1234.001860	81.598173	67.707214
1232.847632	79.148301	67.712218
1232.265904	79.970834	67.717223
1231.564959	78.746636	67.722228
1231.117460	84.270527	67.727233
1230.409548	81.226161	67.732238
1229.312943	75.113538	67.737242
1229.027267	82.541772	67.742247
1228.289654	69.403909	67.747252
1227.204702	77.861213	67.752257
1226.623547	90.235751	67.757262
1226.761692	72.278487	67.762266
1226.110475	69.441139	67.767271
1224.860928	92.622555	67.772276
1224.116201	74.816729	67.777281
1223.555601	76.501600	67.782286
1223.181830	73.145495	67.787290
1222.362597	84.026758	67.792295
1221.419167	79.372028	67.797300
1221.149290	72.793641	67.802305
1220.349196	75.128422	67.807310
1219.535993	78.138609	67.812314
1218.514603	79.557736	67.817319
1217.894607	82.106715	67.822324
1217.521507	87.666082	67.827329
1217.116393	92.196120	67.832334
1216.972726	75.207713	67.837338
1215.746995	74.812833	67.842343
1214.928263	88.097158	67.847348
1214.467973	83.362441	67.852353
1213.937590	82.046472	67.857358
1213.078335	77.491894	67.862362
1212.127593	76.581802	67.867367
1211.854246	88.910543	67.872372
1211.359802	74.023115	67.877377
1210.052234	72.627331	67.882382
1209.704263	93.391537	67.887386
1209.355186	80.540369	67.892391
1208.820671	74.369901	67.897396
1207.791006	70.493673	67.902401
1206.665945	83.623297	67.907406
1206.635647	71.957699	67.912410
1206.164324	83.362342	67.917415
1204.989210	83.812500	67.922420
1204.355665	80.358946	67.927425
1203.494602	81.730506	67.932430
1203.250369	77.833437	67.937434
1202.795931	72.339326	67.942439
1201.736944	75.191498	67.947444
1201.238507	74.458621	67.952449
1200.754838	81.689700	67.957454
1199.771879	73.382949	67.962458
1199.021224	81.482764	67.967463
1198.093575	85.972910	67.972468
1198.138020	73.741946	67.977473
1197.343602	76.966758	67.982478
1196.395062	88.363729	67.987482
1195.709462	85.834612	67.992487
1195.005116	69.616592	67.997492
1195.144336	75.988557	68.002497
1193.921608	85.577898	68.007502
1192.978314	79.155496	68.012506
1192.385077	80.336239	68.017511
1191.803806	83.820451	68.022516
1191.554770	82.899685	68.027521
1190.440831	82.472846	68.032526
1189.992720	86.648623	68.037530
1189.726377	72.953302	68.042535
1188.480102	86.718764	68.047540
1187.803552	89.111175	68.052545
1187.004350	92.245295	68.057550
1186.501548	67.872809	68.062554
1186.079741	89.784090	68.067559
1185.695632	78.105380	68.072564
1184.678946	72.159832	68.077569
1184.032326	91.134488	68.082574
1183.507764	92.320080	68.087578
1182.687669	77.006664	68.092583
1181.611674	86.053885	68.097588
1181.279338	77.042878	68.102593
1180.459291	85.817594	68.107598
1180.387693	94.027025	68.112602
1179.582211	89.408713	68.117607
1178.520848	84.988787	68.122612
1178.379842	78.271644	68.127617
1177.488563	81.101884	68.132622
1176.548127	80.425118	68.137626
1175.998622	92.829321	68.142631
1175.446549	78.796265	68.147636
1175.086603	82.548036	68.152641
1173.851559	96.828937	68.157646
1173.157814	73.387206	68.162650
1173.161364	81.015430	68.167655
1172.336337	92.458993	68.172660
1171.499229	55.980523	68.177665
1170.746351	86.869477	68.182670
1169.949455	81.708943	68.187674
1169.574270	71.432230	68.192679
1168.881743	91.363459	68.197684
1168.346440	61.868205	68.202689
1167.082785	92.355891	68.207694
1167.204735	72.239334	68.212698
1166.455753	76.215397	68.217703
1165.401454	89.718538	68.222708
1164.767618	73.366317	68.227713
1164.288588	72.523134	68.232718
1163.465550	87.221019	68.237722
1162.692772	75.910047	68.242727
1161.754870	88.879041	68.247732
1161.529982	79.923482	68.252737
1160.866298	97.681949	68.257742
1160.477258	97.915641	68.262746
1159.711388	81.114510	68.267751
1158.781373	82.162756	68.272756
1158.457735	62.533378	68.277761
1157.676935	95.604433	68.282766
1156.770850	87.649723	68.287770
1156.444497	78.949987	68.292775
1155.718252	84.461455	68.297780
1154.792035	81.033967	68.302785
1153.764877	73.973681	68.307790
1153.303205	87.117649	68.312794
1153.033196	81.564251	68.317799
1152.857831	81.767112	68.322804
1152.124967	76.293644	68.327809
1151.240955	77.654679	68.332814
1150.543685	79.534758	68.337818
1149.507346	74.055949	68.342823
1148.518986	93.676289	68.347828
1148.186545	78.759958	68.352833
1147.502394	79.352810	68.357838
1147.103476	74.805458	68.362842
1146.798921	86.336536	68.367847
1145.645608	61.950861	68.372852
1145.458089	76.870909	68.377857
1144.529482	77.169927	68.382862
1143.498069	74.199123	68.387866
1143.212405	93.632003	68.392871
1142.607492	88.693237	68.397876
1141.644310	75.190763	68.402881
1140.633304	83.413999	68.407886
1140.281676	87.077724	68.412890
1139.942085	76.836352	68.417895
1139.155148	82.847881	68.422900
1138.623418	81.540027	68.427905
1137.580770	77.711622	68.432910
1137.052616	91.414916	68.437914
1137.050396	78.079691	68.442919
1135.371509	88.367628	68.447924
1135.184627	72.020017	68.452929
1134.452901	79.818806	68.457934
1133.774416	79.973970	68.462938
1132.869529	74.777017	68.467943
1132.060648	96.771950	68.472948
1131.544875	80.609101	68.477953
1130.954688	72.001802	68.482958
1130.895257	90.895674	68.487962
1130.488520	79.704674	68.492967
1129.253759	77.452154	68.497972
1128.704210	87.111049	68.502977
1127.903845	83.245685	68.507982
1127.150272	87.077420	68.512986
1126.387550	75.692329	68.517991
1125.330827	93.331973	68.522996
1125.393163	87.378803	68.528001
1124.720110	80.609110	68.533006
1124.002166	81.841242	68.538010
1123.107133	69.855920	68.543015
1122.616918	91.748120	68.548020
1122.050882	75.689465	68.553025
1120.599041	83.799915	68.558030
1120.361677	85.190555	68.563034
1119.804045	80.543881	68.568039
1119.195262	86.575959	68.573044
1119.234726	83.097371	68.578049
1117.980712	81.090755	68.583054
1117.673753	79.034411	68.588058
1117.079074	77.325015	68.593063
1115.302469	94.349089	68.598068
1114.955226	73.523474	68.603073
1114.246220	76.758375	68.608078
1113.992786	71.577644	68.613082
1113.919497	78.065400	68.618087
1112.660417	78.856944	68.623092
1112.176653	81.130399	68.628097
1111.176906	76.334874	68.633102
1110.711273	84.556516	68.638106
1110.152395	81.855889	68.643111
1108.764641	83.388528	68.648116
1108.854359	76.150597	68.653121
1107.993523	83.034854	68.658126
1107.656958	84.417622	68.663130
1107.017008	80.216106	68.668135
1106.112190	74.563440	68.673140
1105.674456	67.142928	68.678145
1104.701268	63.629902	68.683150
1103.792422	81.427352	68.688154
1103.252984	72.206474	68.693159
1102.927400	80.479949	68.698164
1102.406681	84.973197	68.703169
1101.347715	72.260223	68.708174
1100.934267	76.941396	68.713178
1100.494595	93.517849	68.718183
1099.375343	83.081983	68.723188
1098.540096	85.310436	68.728193
1097.896282	85.791235	68.733198
1097.442567	78.496258	68.738202
1097.367038	74.780513	68.743207
1095.825646	80.393282	68.748212
1095.235323	72.845665	68.753217
1094.640465	83.308083	68.758222
1094.320789	83.278453	68.763226
1094.103309	80.592902	68.768231
1092.787272	81.350941	68.773236
1092.383099	80.059073	68.778241
1091.966092	75.945093	68.783246
1090.688814	72.447331	68.788250
1090.030342	84.056785	68.793255
1089.611525	87.644476	68.798260
1089.383484	84.269940	68.803265
1087.947912	86.811504	68.808270
1087.144975	79.163677	68.813274
1086.813803	75.546945	68.818279
1086.289767	81.445704	68.823284
1085.829329	81.304435	68.828289
1084.671205	84.792131	68.833294
1084.386602	84.236559	68.838298
1084.074113	74.591674	68.843303
1082.881299	80.555827	68.848308
1082.151828	69.893979	68.853313
1081.665144	63.764825	68.858318
1081.163658	76.971887	68.863322
1080.661181	92.303150	68.868327
1079.711563	73.142354	68.873332
1079.151303	68.398348	68.878337
1078.368863	69.361648	68.883342
1077.059853	81.970249	68.888346
1076.762244	78.258298	68.893351
1075.838489	73.149520	68.898356
1075.691409	98.068321	68.903361
1075.422976	72.423912	68.908366
1074.445490	75.130711	68.913370
1073.941367	81.858885	68.918375
1073.003526	78.945760	68.923380
1072.504178	66.074396	68.928385
1071.534778	69.550993	68.933390
1070.538597	87.638300	68.938394
1070.098599	83.203146	68.943399
1069.451024	77.213119	68.948404
1069.592011	74.524158	68.953409
1068.966890	95.132183	68.958414
1067.844826	93.062025	68.963418
1067.192162	67.584404	68.968423
1066.362088	93.196867	68.973428
1065.602915	67.676271	68.978433
1064.583316	86.054291	68.983438
1064.269598	78.959386	68.988442
1064.314040	67.297691	68.993447
1063.165559	98.508206	68.998452
1062.532564	77.280237	69.003457
1061.668130	77.066059	69.008462
1061.601409	84.774837	69.013466
1060.711670	77.762113	69.018471
1059.744015	91.090659	69.023476
1059.027868	71.561593	69.028481
1058.840157	86.322410	69.033486
1057.708028	73.034507	69.038490
1057.330767	84.313815	69.043495
1056.642609	70.636756	69.048500
1056.380647	89.673214	69.053505
1055.418939	79.813094	69.058510
1054.495791	67.818089	69.063514
1053.982212	85.890114	69.068519
1053.044118	74.911403	69.073524
1051.981475	73.301705	69.078529
1051.503502	77.020228	69.083534
1051.502973	85.869582	69.088538
1050.943118	86.873168	69.093543
1049.969321	75.597380	69.098548
1049.013307	95.521658	69.103553
1049.199805	78.267884	69.108558
1047.973899	82.882794	69.113562
1046.907994	74.524662	69.118567
1045.950393	91.938829	69.123572
1045.731991	72.833596	69.128577
1045.203683	96.573630	69.133582
1045.059074	83.779855	69.138586
1044.638710	67.657065	69.143591
1043.343953	85.129597	69.148596
1043.190325	81.057295	69.153601
1041.836454	70.001249	69.158606
1040.785365	91.214750	69.163610
1040.543581	80.339709	69.168615
1039.983617	85.287039	69.173620
1039.974746	72.763398	69.178625
1038.710798	80.107598	69.183630
1038.022948	90.225299	69.188634
1037.649427	74.892942	69.193639
1036.577561	78.163518	69.198644
1035.868721	75.576650	69.203649
1035.133256	76.854169	69.208654
1034.500166	87.508748	69.213658
1034.269026	75.983930	69.218663
1033.654915	77.675777	69.223668
1032.653934	86.133981	69.228673
1032.266911	80.769522	69.233678
1031.327350	62.346716	69.238682
1031.029953	99.278272	69.243687
1029.697758	72.877513	69.248692
1029.265598	91.395456	69.253697
1028.740807	70.945035	69.258702
1028.335577	70.924295	69.263706
1027.824858	70.587622	69.268711
1026.637395	80.316482	69.273716
1026.186317	83.609710	69.278721
1025.724038	86.564119	69.283726
1024.287919	83.528454	69.288730
1023.886207	78.816000	69.293735
1023.139377	72.058085	69.298740
1022.852124	80.041629	69.303745
1022.711744	96.122636	69.308750
1021.849761	83.919217	69.313754
1021.104531	64.243429	69.318759
1020.424571	82.944283	69.323764
1019.173356	79.924930	69.328769
1018.469107	77.321569	69.333774
1017.800106	81.909381	69.338778
1017.741180	82.164683	69.343783
1017.008635	79.783430	69.348788
1016.430839	93.964536	69.353793
1015.796636	70.574917	69.358798
1014.765703	83.186603	69.363802
1014.856075	68.069015	69.368807
1013.479920	78.222116	69.373812
1012.939120	83.978483	69.378817
1012.526670	72.709588	69.383822
1011.633171	76.825372	69.388826
1010.841050	72.020510	69.393831
1010.243166	89.473634	69.398836
1009.572953	74.939079	69.403841
1009.218191	86.329920	69.408846
1008.161576	106.397951	69.413850
1007.612872	81.501427	69.418855
1006.808710	90.030821	69.423860
1006.665517	67.119717	69.428865
1005.381540	89.819409	69.433870
1004.764800	78.381180	69.438874
1004.346854	69.297114	69.443879
1003.877726	92.013803	69.448884
1003.548247	89.229394	69.453889
1002.070278	78.243573	69.458894
1001.185886	83.501135	69.463898
1000.972575	82.144223	69.468903
1000.935835	92.070024	69.473908
999.930772	78.637360	69.478913
998.984296	96.997464	69.483918
998.436776	88.911657	69.488922
998.062395	74.432531	69.493927
996.699298	108.949204	69.498932
996.396973	71.849597	69.503937
995.865611	72.060231	69.508942
995.196996	98.485903	69.513946
994.529983	73.652377	69.518951
993.483300	80.078985	69.523956
992.678713	88.141698	69.528961
992.990103	78.127918	69.533966
991.828691	66.151936	69.538970
991.056808	75.366851	69.543975
990.252967	86.646235	69.548980
990.162859	76.057715	69.553985
989.476060	78.150622	69.558990
988.268032	66.380744	69.563994
987.791112	78.112695	69.568999
987.205933	82.028050	69.574004
986.453856	68.690757	69.579009
985.734059	69.502199	69.584014
984.755418	71.840229	69.589018
984.393988	77.976462	69.594023
984.482006	79.379987	69.599028
983.470424	80.953754	69.604033
982.650380	73.583067	69.609038
981.739153	88.783841	69.614042
981.337980	76.645885	69.619047
980.338787	86.064127	69.624052
979.435787	66.571148	69.629057
978.936118	90.565216	69.634062
978.843322	69.226111	69.639066
978.347674	74.768726	69.644071
977.060477	87.913184	69.649076
976.212207	83.807930	69.654081
975.919383	75.654802	69.659086
975.095299	78.181118	69.664090
975.357601	77.582684	69.669095
974.059404	82.094019	69.674100
973.352447	69.113806	69.679105
972.938458	72.724393	69.684110
971.836295	76.312032	69.689114
971.233420	82.420461	69.694119
970.428818	74.014479	69.699124
970.133804	85.268087	69.704129
969.689507	80.423657	69.709134
968.534239	76.747283	69.714138
968.233662	74.803479	69.719143
967.631546	87.821578	69.724148
966.723516	67.425866	69.729153
966.331675	90.043524	69.734158
965.691016	74.326371	69.739162
964.150859	78.459923	69.744167
963.379002	76.129096	69.749172
962.680685	75.481688	69.754177
962.468086	84.262283	69.759182
962.065500	83.006454	69.764186
961.893412	60.073167	69.769191
961.461015	89.772628	69.774196
960.771161	80.643531	69.779201
960.074701	79.675726	69.784206
958.549202	77.147881	69.789210
957.595401	88.496865	69.794215
957.249188	85.899620	69.799220
957.236488	73.012345	69.804225
956.276066	68.450317	69.809230
954.935028	89.943346	69.814234
954.728132	72.796345	69.819239
954.240533	73.690686	69.824244
953.441136	87.216391	69.829249
952.938466	81.906620	69.834254
951.691966	76.391965	69.839258
951.830062	69.247264	69.844263
951.282227	79.232310	69.849268
950.220379	68.968741	69.854273
949.526173	74.555573	69.859278
948.684049	83.646070	69.864282
948.593656	69.208498	69.869287
947.660070	78.460195	69.874292
946.770791	68.790448	69.879297
946.505724	73.678245	69.884302
945.466207	81.546554	69.889306
944.549326	69.845477	69.894311
943.817512	70.043870	69.899316
943.439986	81.573940	69.904321
943.133970	86.100851	69.909326
942.675705	77.836870	69.914330
941.772621	69.977976	69.919335
940.913600	61.486064	69.924340
940.199230	92.133938	69.929345
939.364648	67.021209	69.934350
938.063091	72.816654	69.939354
938.093976	64.340806	69.944359
937.683643	74.315005	69.949364
937.276384	77.777878	69.954369
936.909375	76.491162	69.959374
936.231394	82.311946	69.964378
935.461796	63.204596	69.969383
934.259986	77.347812	69.974388
933.267760	64.990148	69.979393
932.384463	82.857673	69.984398
932.148018	79.022477	69.989402
932.315129	64.343672	69.994407
931.065230	81.567838	69.999412
930.399484	82.488958	70.004417
929.833598	64.960738	70.009422
929.154314	93.201480	70.014426
928.507448	74.181814	70.019431
927.977886	70.213507	70.024436
927.253114	75.324267	70.029441
926.680710	79.429975	70.034446
925.323844	75.911855	70.039450
925.135846	71.600625	70.044455
924.596149	78.684540	70.049460
923.763357	76.957898	70.054465
922.947718	61.606073	70.059470
922.023778	76.279045	70.064474
921.989981	79.919014	70.069479
921.467478	75.798205	70.074484
920.554863	63.442071	70.079489
919.739238	61.074075	70.084494
919.096428	84.788154	70.089498
918.926308	66.995112	70.094503
917.669558	79.338426	70.099508
916.970288	80.490376	70.104513
916.739623	69.175235	70.109518
915.665284	80.720015	70.114522
915.156506	88.585867	70.119527
914.230047	78.116271	70.124532
913.666656	66.797320	70.129537
913.656068	79.759119	70.134542
912.252597	82.798685	70.139546
911.886045	68.564335	70.144551
910.906686	58.584115	70.149556
910.335109	86.254225	70.154561
910.302140	70.110823	70.159566
909.446092	77.804871	70.164570
908.645442	74.471034	70.169575
908.067036	68.020651	70.174580
907.569873	75.629198	70.179585
906.657856	89.073494	70.184590
905.839476	54.557008	70.189594
905.468436	79.892983	70.194599
904.634337	76.616506	70.199604
903.512218	78.535882	70.204609
903.262040	64.079603	70.209614
902.686429	96.673315	70.214618
902.369500	62.274112	70.219623
901.195450	95.954909	70.224628
900.529979	74.442050	70.229633
900.034323	76.100882	70.234638
899.269404	91.609528	70.239642
899.155545	75.715524	70.244647
897.671160	91.620936	70.249652
897.542893	85.204555	70.254657
897.114084	65.904219	70.259662
895.757612	88.183417	70.264666
895.001185	83.447025	70.269671
894.561923	79.997330	70.274676
894.249736	71.801574	70.279681
893.485747	77.301760	70.284686
892.176392	96.194270	70.289690
891.796382	75.873813	70.294695
891.194837	82.354182	70.299700
890.773825	88.332762	70.304705
890.516873	65.646371	70.309710
889.587516	59.825830	70.314714
888.801526	85.109591	70.319719
888.414114	76.019115	70.324724
887.408886	73.988792	70.329729
886.603734	78.910518	70.334734
885.759945	70.726840	70.339738
885.688426	80.883649	70.344743
884.997274	73.691171	70.349748
883.794174	73.781676	70.354753
883.265081	76.781430	70.359758
882.766166	81.003175	70.364762
882.686326	75.356483	70.369767
881.657252	87.285134	70.374772
880.918005	85.051638	70.379777
880.793693	81.315288	70.384782
879.451479	78.529677	70.389786
878.637516	77.105964	70.394791
878.091392	81.234305	70.399796
877.358124	62.559570	70.404801
877.086721	102.574432	70.409806
876.111252	87.700600	70.414810
875.423243	73.350274	70.419815
874.869546	93.912242	70.424820
874.464001	64.180460	70.429825
873.632488	86.923275	70.434830
872.671757	76.933789	70.439834
872.133848	81.002480	70.444839
871.984557	70.656777	70.449844
870.717700	74.880913	70.454849
870.073512	83.115228	70.459854
869.409981	79.898342	70.464858
869.292507	69.522346	70.469863
868.660956	89.500649	70.474868
867.505877	89.930427	70.479873
867.064249	69.201930	70.484878
866.510235	77.943829	70.489882
865.869754	92.942271	70.494887
864.878964	81.642472	70.499892
864.162636	78.172233	70.504897
863.993869	96.113698	70.509902
862.404830	80.948059	70.514906
862.263495	85.737327	70.519911
861.457554	83.432457	70.524916
861.112226	83.572510	70.529921
861.086475	65.162031	70.534926
859.648372	99.266468	70.539930
859.008748	73.490426	70.544935
858.496212	87.367853	70.549940
857.494210	98.079608	70.554945
856.881367	68.797112	70.559950
855.865027	93.840029	70.564954
855.831283	81.366094	70.569959
855.532170	69.555691	70.574964
854.970143	92.977821	70.579969
854.055425	86.344450	70.584974
853.053819	77.979334	70.589978
851.970318	81.314909	70.594983
851.237020	85.135602	70.599988
850.787231	59.564324	70.604993
850.381352	84.795465	70.609998
849.715175	84.499342	70.615002
849.720012	67.914724	70.620007
848.530476	84.981086	70.625012
847.729563	88.766815	70.630017
847.671569	77.223937	70.635022
846.475376	79.702297	70.640026
845.388258	94.773415	70.645031
845.076968	77.983655	70.650036
844.315371	72.866509	70.655041
844.140492	82.812701	70.660046
843.143969	91.557243	70.665050
842.632239	63.548540	70.670055
841.799234	96.252596	70.675060
841.221009	85.022744	70.680065
840.975274	72.659830	70.685070
839.635456	82.897106	70.690074
839.319182	77.384241	70.695079
838.800575	70.932244	70.700084
837.380029	93.606418	70.705089
837.342801	74.070308	70.710094
836.447708	90.985738	70.715098
836.348611	78.746126	70.720103
835.330416	79.660300	70.725108
834.576099	57.422097	70.730113
834.188080	97.651024	70.735118
833.628463	99.029910	70.740122
832.221314	78.023050	70.745127
832.090421	59.629322	70.750132
831.318308	101.428448	70.755137
830.713513	94.714212	70.760142
829.935961	70.672613	70.765146
829.050174	99.493402	70.770151
828.629405	72.053647	70.775156
827.823374	97.356391	70.780161
827.722843	89.768727	70.785166
826.646140	81.877595	70.790170
826.075195	96.762481	70.795175
825.483516	67.739971	70.800180
824.577089	95.770882	70.805185
823.967897	79.711328	70.810190
823.056521	76.977006	70.815194
822.974803	84.109451	70.820199
822.439530	82.012227	70.825204
821.258623	86.363047	70.830209
820.409243	86.036175	70.835214
819.921281	60.428411	70.840218
819.279339	63.152843	70.845223
819.017939	99.283872	70.850228
817.942752	64.505549	70.855233
817.161764	98.879102	70.860238
816.849599	67.464162	70.865242
816.312474	89.201394	70.870247
815.807405	72.250122	70.875252
814.893473	68.532255	70.880257
814.547145	77.775651	70.885262
813.223708	80.873487	70.890266
812.466740	72.720170	70.895271
812.006132	79.794664	70.900276
811.218873	89.147682	70.905281
811.304071	59.462391	70.910286
810.298443	83.601630	70.915290
809.261888	75.590586	70.920295
809.038027	80.798242	70.925300
808.121913	69.343100	70.930305
807.389704	85.453633	70.935310
806.546621	75.718248	70.940314
806.206824	87.444157	70.945319
805.979889	83.735188	70.950324
804.915214	76.403516	70.955329
804.351013	75.033103	70.960334
803.578751	96.301608	70.965338
802.831411	69.937237	70.970343
802.398144	73.908860	70.975348
801.214296	74.338517	70.980353
800.659009	90.351510	70.985358
800.158872	72.190010	70.990362
799.542830	91.371114	70.995367
799.276359	75.976061	71.000372
798.167298	79.184846	71.005377
797.856719	77.537530	71.010382
797.177717	93.360499	71.015386
796.475052	78.375486	71.020391
795.821341	68.236249	71.025396
794.998044	76.779766	71.030401
794.816104	75.294887	71.035406
793.691816	80.642736	71.040410
793.299442	84.426514	71.045415
792.122377	77.167931	71.050420
791.230418	76.202914	71.055425
790.900012	74.992391	71.060430
789.992836	77.342768	71.065434
789.772261	80.088432	71.070439
789.570769	72.438012	71.075444
788.061031	84.121530	71.080449
787.939136	84.262290	71.085454
787.204315	71.162019	71.090458
786.136895	105.248468	71.095463
785.534924	67.403531	71.100468
784.909153	91.548541	71.105473
784.630875	81.743743	71.110478
784.036974	81.060840	71.115482
782.861865	84.541905	71.120487
782.478282	78.755933	71.125492
781.440339	95.392940	71.130497
781.153683	92.120808	71.135502
780.853628	84.462423	71.140506
779.753313	73.413485	71.145511
779.147569	74.660961	71.150516
778.492348	84.218452	71.155521
777.865502	79.180793	71.160526
776.876587	88.242667	71.165530
776.248119	74.564105	71.170535
775.894501	80.188210	71.175540
775.221762	95.327409	71.180545
774.405191	82.758933	71.185550
773.626600	91.653293	71.190554
773.040037	78.691834	71.195559
772.732489	72.538968	71.200564
771.877801	88.123416	71.205569
771.110445	84.953048	71.210574
770.725825	77.087372	71.215578
770.112581	84.821646	71.220583
769.389774	78.353293	71.225588
768.142057	82.184947	71.230593
767.999357	78.079398	71.235598
767.357011	81.787867	71.240602
766.642045	79.507967	71.245607
765.844824	77.198589	71.250612
764.904766	79.019656	71.255617
765.279288	92.300154	71.260622
763.705453	71.911216	71.265626
762.773263	63.068354	71.270631
762.484440	79.185559	71.275636
762.173572	74.397201	71.280641
761.831519	77.364044	71.285646
760.606754	87.255053	71.290650
759.955123	81.634755	71.295655
759.421996	79.135107	71.300660
758.375535	75.619700	71.305665
757.716985	89.138783	71.310670
757.081200	76.809603	71.315674
756.507014	78.529846	71.320679
756.226295	89.792218	71.325684
754.989814	73.080413	71.330689
754.526344	78.614783	71.335694
754.082207	75.839212	71.340698
753.744687	86.779485	71.345703
753.360182	76.346677	71.350708
752.161883	75.873544	71.355713
751.709361	83.347280	71.360718
751.015787	84.570902	71.365722
749.933197	93.934689	71.370727
749.581533	65.846932	71.375732
748.752900	80.430656	71.380737
748.161338	90.020595	71.385742
747.179528	82.473918	71.390746
746.450947	76.302941	71.395751
746.081856	68.464764	71.400756
745.494863	81.020029	71.405761
744.841596	79.223868	71.410766
744.021150	81.448496	71.415770
743.181292	74.834797	71.420775
742.941241	82.522269	71.425780
742.548514	83.360547	71.430785
741.892944	70.266601	71.435790
740.928959	81.443802	71.440794
739.965958	82.500603	71.445799
739.000801	85.602929	71.450804
738.213407	83.460718	71.455809
738.025157	76.844189	71.460814
737.539279	84.332699	71.465818
737.109768	84.162917	71.470823
736.462972	86.197482	71.475828
735.212536	92.140995	71.480833
734.961316	87.157073	71.485838
734.621032	81.376830	71.490842
733.641762	72.601392	71.495847
732.523533	72.006717	71.500852
732.055113	81.454050	71.505857
731.798428	73.653166	71.510862
731.041894	76.643432	71.515866
730.106773	78.755443	71.520871
729.769734	73.014110	71.525876
728.836046	85.307635	71.530881
728.442587	72.509404	71.535886
727.503994	72.504256	71.540890
727.154192	84.876689	71.545895
726.767809	74.939320	71.550900
725.186862	86.990577	71.555905
724.373897	73.123808	71.560910
724.073814	89.146626	71.565914
723.840368	77.005693	71.570919
723.260896	88.183176	71.575924
722.030407	80.128941	71.580929
721.330601	70.050683	71.585934
721.079550	89.526885	71.590938
720.544763	83.605737	71.595943
719.852344	73.452189	71.600948
718.680328	74.324674	71.605953
718.499638	78.506811	71.610958
717.963153	81.342202	71.615962
717.359512	84.759109	71.620967
716.609765	78.823309	71.625972
715.815211	81.557876	71.630977
715.180982	81.980478	71.635982
713.863328	64.218839	71.640986
713.245921	88.520196	71.645991
713.071005	71.625197	71.650996
712.677141	76.785812	71.656001
711.978020	69.444866	71.661006
710.902741	78.074255	71.666010
710.396990	91.144842	71.671015
710.102749	71.217632	71.676020
709.022245	75.448436	71.681025
707.979918	90.939782	71.686030
707.416556	71.640438	71.691034
707.084116	68.888090	71.696039
706.891101	73.259833	71.701044
706.353034	81.031027	71.706049
705.639248	66.350594	71.711054
704.892484	69.566376	71.716058
703.574015	85.268834	71.721063
703.039496	65.477660	71.726068
702.366247	68.361636	71.731073
702.471330	71.385009	71.736078
701.226455	68.145636	71.741082
700.395575	76.710882	71.746087
700.311874	73.382796	71.751092
699.225158	73.573121	71.756097
698.172476	66.624351	71.761102
697.781334	88.697855	71.766106
697.043214	57.909027	71.771111
696.990755	76.333363	71.776116
695.709185	79.423013	71.781121
695.151073	80.623502	71.786126
694.585493	75.870986	71.791130
694.252404	65.513587	71.796135
693.320072	84.757666	71.801140
692.281444	84.957682	71.806145
691.705228	70.431952	71.811150
691.558327	85.153122	71.816154
690.566353	72.664662	71.821159
689.693063	74.038335	71.826164
688.918175	71.887844	71.831169
688.918569	81.784042	71.836174
688.606941	67.304487	71.841178
687.189948	61.060247	71.846183
686.709266	84.388983	71.851188
686.021553	72.304632	71.856193
685.333172	69.873879	71.861198
684.332315	88.184341	71.866202
683.829557	74.663983	71.871207
683.426752	68.829061	71.876212
682.739444	80.827909	71.881217
682.090578	77.758545	71.886222
681.335881	74.688690	71.891226
680.526423	75.650104	71.896231
680.296235	66.093132	71.901236
679.310101	80.654644	71.906241
678.396962	68.505278	71.911246
677.800227	70.360007	71.916250
677.193646	72.334568	71.921255
676.824836	84.096632	71.926260
676.427059	78.076415	71.931265
675.485777	75.294877	71.936270
674.687501	80.336983	71.941274
674.337140	85.126425	71.946279
673.753025	71.585915	71.951284
672.687352	82.156471	71.956289
672.270507	72.976128	71.961294
671.641984	73.699011	71.966298
670.374624	87.691921	71.971303
670.028771	83.200866	71.976308
669.200530	79.422104	71.981313
669.317602	72.875230	71.986318
668.105078	74.120018	71.991322
667.170107	77.898759	71.996327
666.691949	69.139742	72.001332
666.526125	84.202945	72.006337
665.724507	75.888071	72.011342
664.549637	83.033753	72.016346
663.971861	75.988867	72.021351
663.659651	74.814886	72.026356
663.093201	83.915162	72.031361
662.350778	72.276321	72.036366
661.560487	76.437275	72.041370
661.331777	79.491727	72.046375
660.455348	73.574548	72.051380
659.245912	76.428814	72.056385
658.661714	75.449526	72.061390
658.269052	77.793699	72.066394
657.726572	82.676810	72.071399
656.895854	69.200811	72.076404
655.956131	76.599186	72.081409
655.814087	79.081631	72.086414
655.313080	69.239806	72.091418
653.992437	80.335064	72.096423
653.479980	76.752008	72.101428
653.026483	72.632894	72.106433
652.530828	78.129827	72.111438
651.427882	78.832081	72.116442
650.632467	73.587934	72.121447
650.416671	73.134990	72.126452
649.926296	86.677759	72.131457
649.036345	69.299026	72.136462
648.133399	69.151045	72.141466
647.371294	66.495517	72.146471
647.013791	77.279705	72.151476
646.660699	83.846695	72.156481
645.871025	81.047331	72.161486
645.242802	81.500531	72.166490
644.694265	82.075073	72.171495
643.657799	64.770141	72.176500
642.766950	84.576864	72.181505
642.098829	78.915079	72.186510
642.214722	71.652504	72.191514
641.372241	82.312095	72.196519
640.737773	65.130789	72.201524
639.787670	84.726189	72.206529
639.330351	72.904766	72.211534
638.466668	71.323485	72.216538
637.408618	78.163584	72.221543
637.082901	66.721728	72.226548
636.427006	77.104036	72.231553
636.011749	61.991343	72.236558
634.809916	62.291487	72.241562
634.231863	75.591184	72.246567
633.854353	72.349317	72.251572
633.314090	76.487803	72.256577
632.367939	81.542434	72.261582
631.861751	75.985743	72.266586
631.219892	82.403193	72.271591
630.789455	70.586955	72.276596
629.366215	83.365297	72.281601
629.063834	80.985039	72.286606
628.513299	80.987506	72.291610
628.024705	94.416466	72.296615
627.949178	77.540344	72.301620
626.308318	63.751874	72.306625
625.865863	78.799204	72.311630
625.208863	74.909613	72.316634
624.042010	84.006176	72.321639
623.570837	78.461255	72.326644
622.934611	78.870006	72.331649
622.555241	77.262054	72.336654
622.495732	64.480057	72.341658
621.566459	76.134273	72.346663
620.735139	63.913565	72.351668
619.759106	72.457794	72.356673
619.416307	67.236186	72.361678
618.705409	74.781041	72.366682
618.007924	66.940008	72.371687
617.826538	73.610526	72.376692
616.518090	71.716916	72.381697
615.454385	73.824216	72.386702
615.051374	68.615352	72.391706
614.560080	86.207620	72.396711
614.463036	74.822377	72.401716
613.193479	85.559459	72.406721
612.621748	79.557501	72.411726
612.121095	78.055594	72.416730
611.386424	82.226627	72.421735
611.205726	74.306436	72.426740
609.814663	76.863245	72.431745
609.380040	70.262326	72.436750
609.195704	75.255547	72.441754
607.905621	83.881342	72.446759
607.433097	78.005502	72.451764
606.573109	82.232762	72.456769
606.422309	82.034380	72.461774
605.117903	84.047568	72.466778
604.381761	88.039077	72.471783
604.177444	71.538272	72.476788
603.393665	79.911549	72.481793
602.873922	75.333096	72.486798
602.289208	71.808867	72.491802
601.482247	73.408533	72.496807
600.881665	68.048226	72.501812
599.693325	80.432796	72.506817
598.950676	79.535526	72.511822
598.841665	71.506157	72.516826
598.158693	80.049447	72.521831
598.046222	72.334422	72.526836
597.023631	82.636383	72.531841
596.296057	68.781309	72.536846
595.870223	69.888215	72.541850
594.480732	78.933520	72.546855
594.109999	72.991013	72.551860
593.531849	65.742800	72.556865
593.040209	76.579890	72.561870
592.480858	70.441937	72.566874
591.099988	84.968583	72.571879
590.942394	70.436135	72.576884
590.212493	73.718644	72.581889
589.640401	78.273766	72.586894
588.963400	70.443671	72.591898
587.909637	73.842416	72.596903
587.811984	59.713567	72.601908
586.915595	69.978075	72.606913
585.950028	90.154659	72.611918
585.572641	84.467082	72.616922
584.816239	86.036625	72.621927
584.657227	78.595499	72.626932
583.590097	77.647423	72.631937
582.875594	66.288007	72.636942
582.257842	69.812834	72.641946
581.490289	72.282957	72.646951
581.703259	74.398217	72.651956
580.289561	79.666098	72.656961
579.786579	83.109574	72.661966
579.301029	71.237478	72.666970
577.939480	75.183537	72.671975
577.469412	74.375312	72.676980
576.892574	78.808198	72.681985
576.536931	75.958647	72.686990
576.046633	62.671305	72.691994
574.677556	79.305896	72.696999
574.486298	78.834858	72.702004
574.138684	79.853620	72.707009
572.846620	85.827484	72.712014
572.238036	75.531337	72.717018
571.570699	87.703633	72.722023
571.461948	75.620139	72.727028
570.287710	78.123509	72.732033
569.203115	69.300279	72.737038
569.007518	92.670337	72.742042
568.166776	85.364608	72.747047
568.219166	74.393935	72.752052
567.280131	79.220386	72.757057
566.340865	80.710259	72.762062
566.177512	76.182272	72.767066
565.367384	81.677274	72.772071
564.110762	73.516918	72.777076
563.524049	83.139217	72.782081
563.000976	87.539891	72.787086
562.997064	76.835211	72.792090
561.646008	71.296434	72.797095
560.713167	76.665912	72.802100
560.085860	91.126152	72.807105
559.973457	78.428268	72.812110
559.673432	77.646572	72.817114
558.570455	86.947438	72.822119
557.888441	74.628856	72.827124
557.140075	83.977305	72.832129
556.804425	84.189969	72.837134
555.762325	71.532960	72.842138
554.984320	90.069709	72.847143
554.431509	69.333820	72.852148
553.894797	82.130237	72.857153
553.348146	85.342569	72.862158
552.492605	83.356347	72.867162
551.927049	81.948365	72.872167
551.788261	80.894998	72.877172
550.289786	77.073245	72.882177
549.612527	78.565539	72.887182
549.429089	56.441548	72.892186
548.712469	94.163501	72.897191
548.373734	74.437383	72.902196
547.144629	74.119058	72.907201
546.703205	67.043032	72.912206
546.223726	73.267482	72.917210
544.839856	79.503546	72.922215
544.444730	65.135101	72.927220
543.879670	86.439984	72.932225
543.868106	57.758875	72.937230
543.003994	65.154694	72.942234
542.011139	72.930547	72.947239
541.525021	76.916931	72.952244
540.228248	88.036822	72.957249
539.322010	69.344074	72.962254
538.882924	79.712359	72.967258
538.591260	84.817293	72.972263
538.024457	76.761513	72.977268
537.710800	74.529714	72.982273
537.108034	72.914790	72.987278
536.639092	76.778597	72.992282
535.445454	72.173483	72.997287
534.986350	73.462305	73.002292
533.833441	79.866573	73.007297
533.305781	66.749186	73.012302
532.688589	73.468630	73.017306
532.059194	88.823276	73.022311
531.672905	72.214292	73.027316
531.179512	70.030049	73.032321
530.606785	69.766432	73.037326
529.314026	63.876213	73.042330
528.372227	80.695052	73.047335
528.138160	71.260142	73.052340
527.568250	70.444179	73.057345
526.782163	68.204069	73.062350
526.275811	79.521296	73.067354
525.124869	80.593926	73.072359
524.790065	85.806652	73.077364
524.365690	76.422555	73.082369
523.602562	78.849416	73.087374
522.855532	75.374719	73.092378
521.971423	97.257112	73.097383
521.939065	70.518826	73.102388
520.795659	76.246692	73.107393
519.685983	88.789064	73.112398
519.454022	81.115156	73.117402
519.141722	76.893159	73.122407
518.432859	77.226781	73.127412
517.453508	69.746057	73.132417
517.014661	84.788089	73.137422
516.576689	75.098676	73.142426
515.040680	78.233677	73.147431
514.564240	77.560511	73.152436
514.081895	71.052369	73.157441
513.474624	82.584359	73.162446
513.347571	74.898473	73.167450
512.333567	76.860712	73.172455
511.424225	65.625401	73.177460
511.094404	86.746161	73.182465
510.455573	74.665130	73.187470
510.018667	69.553146	73.192474
508.552399	75.543750	73.197479
508.205587	75.606822	73.202484
507.841096	72.891149	73.207489
507.049983	75.978441	73.212494
506.239222	70.653222	73.217498
505.591002	71.600042	73.222503
505.361648	69.868870	73.227508
504.262690	66.365099	73.232513
503.232144	79.943466	73.237518
502.972605	70.982521	73.242522
502.420858	63.752207	73.247527
502.140084	67.258055	73.252532
500.879865	74.076795	73.257537
500.159361	84.803713	73.262542
499.849617	70.618780	73.267546
499.463449	77.377115	73.272551
498.672237	79.456820	73.277556
497.939848	70.024042	73.282561
497.024902	74.819870	73.287566
496.483303	75.656672	73.292570
495.271927	73.835965	73.297575
495.046426	71.221145	73.302580
494.340082	65.469317	73.307585
493.937753	80.724709	73.312590
493.059045	73.768819	73.317594
492.329609	78.385294	73.322599
491.662850	66.874816	73.327604
491.160574	75.911272	73.332609
490.655985	78.599706	73.337614
490.076371	68.093988	73.342618
489.126153	79.608082	73.347623
488.603368	74.158146	73.352628
487.770478	77.897032	73.357633
486.792853	76.766015	73.362638
486.594580	79.724171	73.367642
486.097057	72.964581	73.372647
485.220950	64.609620	73.377652
484.277287	76.097439	73.382657
483.273111	85.672728	73.387662
483.316462	77.269036	73.392666
482.756229	60.850210	73.397671
482.144860	77.572257	73.402676
481.269263	59.863357	73.407681
480.446428	75.534223	73.412686
480.174154	77.315225	73.417690
479.073001	66.367515	73.422695
478.216008	85.777810	73.427700
477.656636	79.173143	73.432705
477.114660	68.382330	73.437710
477.127298	91.731807	73.442714
475.803961	78.766430	73.447719
475.248939	80.365417	73.452724
474.901881	78.468509	73.457729
474.099507	69.354377	73.462734
473.580999	83.376265	73.467738
472.255064	90.412062	73.472743
472.414104	75.446014	73.477748
471.490194	66.994602	73.482753
470.118259	95.727284	73.487758
469.799227	78.481588	73.492762
469.160777	77.209812	73.497767
468.834717	89.089643	73.502772
468.785077	63.935719	73.507777
467.122879	86.683192	73.512782
466.863106	60.944630	73.517786
465.659494	93.335579	73.522791
465.474968	71.817275	73.527796
464.418643	86.729049	73.532801
463.822935	77.384882	73.537806
463.945000	65.471207	73.542810
462.887087	72.954696	73.547815
461.989737	81.010232	73.552820
461.215762	90.559891	73.557825
461.020043	72.465135	73.562830
460.331099	62.790505	73.567834
458.866397	85.706772	73.572839
458.465139	67.479202	73.577844
457.974383	77.718538	73.582849
458.019275	65.738318	73.587854
457.214984	81.849333	73.592858
456.140304	60.635295	73.597863
455.602437	81.927953	73.602868
454.674468	85.961102	73.607873
453.475418	64.809450	73.612878
453.215105	48.551007	73.617882
452.497244	92.604176	73.622887
452.639768	78.000280	73.627892
452.231433	74.217769	73.632897
450.748738	85.126060	73.637902
450.324716	76.799993	73.642906
449.718146	59.380960	73.647911
449.065296	72.686281	73.652916
447.962702	81.551909	73.657921
447.058455	63.267308	73.662926
446.995696	62.931915	73.667930
446.196995	74.368261	73.672935
445.405854	60.811954	73.677940
444.516771	71.294516	73.682945
443.945273	77.120508	73.687950
443.879480	70.303177	73.692954
443.480784	71.659655	73.697959
442.505221	70.358029	73.702964
441.588728	79.304385	73.707969
441.083873	81.448859	73.712974
440.522359	54.932128	73.717978
439.464240	87.634177	73.722983
439.075249	74.305499	73.727988
438.500294	69.398442	73.732993
437.073570	67.145334	73.737998
436.896135	71.885161	73.743002
436.407736	74.979428	73.748007
436.042868	70.671212	73.753012
434.866640	68.143240	73.758017
434.068071	72.100583	73.763022
434.039641	70.241215	73.768026
432.878452	90.508916	73.773031
432.391873	71.167500	73.778036
431.767486	64.864929	73.783041
430.974593	87.338292	73.788046
430.777361	59.293889	73.793050
429.395347	96.538427	73.798055
428.790089	60.044054	73.803060
428.397796	78.852054	73.808065
427.976454	82.580570	73.813070
427.449333	64.366764	73.818074
426.080792	80.017373	73.823079
425.511927	86.897864	73.828084
425.232249	65.595004	73.833089
424.596819	87.157088	73.838094
423.789714	65.974538	73.843098
422.995039	65.363139	73.848103
422.742692	72.833387	73.853108
422.022865	62.239661	73.858113
420.741735	82.187443	73.863118
420.394740	58.250948	73.868122
419.673338	96.847226	73.873127
419.303079	67.537366	73.878132
418.153202	85.630367	73.883137
417.457053	76.131922	73.888142
417.222613	70.027396	73.893146
416.726586	77.400868	73.898151
415.987413	88.783594	73.903156
415.131956	84.313872	73.908161
414.620988	70.019113	73.913166
414.569963	64.238577	73.918170
413.197403	75.099368	73.923175
412.377201	81.255139	73.928180
412.136951	71.655668	73.933185
410.872773	74.679608	73.938190
410.320827	70.795420	73.943194
409.431903	69.079483	73.948199
408.987547	70.837454	73.953204
408.699855	71.580200	73.958209
408.347233	85.763304	73.963214
407.615676	73.365953	73.968218
406.535147	76.400052	73.973223
405.774445	67.555258	73.978228
405.625927	85.168591	73.983233
404.719483	76.810610	73.988238
403.880271	76.149547	73.993242
403.141293	81.188583	73.998247
402.319704	74.767643	74.003252
401.671582	61.560701	74.008257
400.898849	77.141601	74.013262
400.706116	70.666180	74.018266
400.391649	72.614751	74.023271
399.355625	85.853425	74.028276
398.790331	66.570302	74.033281
398.159932	75.772254	74.038286
397.644037	88.738824	74.043290
396.671532	82.083328	74.048295
395.826485	68.183992	74.053300
395.472792	71.733006	74.058305
395.055504	85.475436	74.063310
394.107358	78.868098	74.068314
393.051862	72.449747	74.073319
392.581835	76.260136	74.078324
392.423516	80.433986	74.083329
391.365736	78.727617	74.088334
390.732953	69.439848	74.093338
389.881607	72.527311	74.098343
389.590937	70.460594	74.103348
388.804335	93.620471	74.108353
387.763140	68.060068	74.113358
387.474926	85.662547	74.118362
386.907038	75.311100	74.123367
386.234051	67.893573	74.128372
385.100459	87.587642	74.133377
384.585053	83.888433	74.138382
384.370946	72.911366	74.143386
383.567207	69.160347	74.148391
382.798390	75.273242	74.153396
382.394275	81.424209	74.158401
381.503210	69.697223	74.163406
381.151811	88.287419	74.168410
379.986078	80.440669	74.173415
379.503343	83.882527	74.178420
379.388640	46.609924	74.183425
378.125579	84.103543	74.188430
377.348700	74.173310	74.193434
376.904638	74.415890	74.198439
376.441651	77.491926	74.203444
375.411297	59.036670	74.208449
374.193604	69.689880	74.213454
374.058057	76.315250	74.218458
373.640033	81.427715	74.223463
373.465657	73.044540	74.228468
372.726139	74.234586	74.233473
371.231833	62.230035	74.238478
371.090513	75.144784	74.243482
370.355301	77.214025	74.248487
369.251381	90.304270	74.253492
368.704822	66.215096	74.258497
368.337050	77.666356	74.263502
367.512102	68.048124	74.268506
367.021472	83.521002	74.273511
366.288050	52.148218	74.278516
365.446647	78.557221	74.283521
365.024092	84.422565	74.288526
364.833859	68.086730	74.293530
363.517843	74.037695	74.298535
362.581006	66.635421	74.303540
362.631241	74.822219	74.308545
362.016717	83.610095	74.313550
361.249169	76.914070	74.318554
360.296624	56.420179	74.323559
359.542269	86.353762	74.328564
359.171721	61.441818	74.333569
358.033327	65.377651	74.338574
357.375607	74.427855	74.343578
357.217627	59.693697	74.348583
356.393174	65.427558	74.353588
355.975500	71.325235	74.358593
354.900927	78.275291	74.363598
354.567523	67.243136	74.368602
354.092664	77.349069	74.373607
353.005421	77.679968	74.378612
352.243327	70.182043	74.383617
351.405126	59.878431	74.388622
351.335468	81.139040	74.393626
350.787557	50.600814	74.398631
349.813319	77.855676	74.403636
349.457873	55.943655	74.408641
348.341126	86.269286	74.413646
347.243541	40.818148	74.418650
346.477272	85.222740	74.423655
345.851580	64.288849	74.428660
346.209527	77.485122	74.433665
345.677873	67.873768	74.438670
345.120173	62.046267	74.443674
344.275365	70.435630	74.448679
343.593969	63.784231	74.453684
342.205863	74.697990	74.458689
341.614895	71.315170	74.463694
341.364620	56.187325	74.468698
340.626523	77.642766	74.473703
339.936468	73.066296	74.478708
339.081129	63.011407	74.483713
338.392193	71.516269	74.488718
338.375294	50.988385	74.493722
337.399613	74.414897	74.498727
336.497067	64.550445	74.503732
335.957569	64.423493	74.508737
335.197157	64.368018	74.513742
334.833929	73.994143	74.518746
333.965622	57.801090	74.523751
333.273604	80.859149	74.528756
333.008658	69.530678	74.533761
331.444142	76.005358	74.538766
330.774249	60.638484	74.543770
330.352293	65.762613	74.548775
329.831879	49.059992	74.553780
329.867327	77.169414	74.558785
328.891902	70.774601	74.563790
328.167372	57.013785	74.568794
327.320669	62.286030	74.573799
326.693936	70.134473	74.578804
325.858927	62.622955	74.583809
325.173500	68.375665	74.588814
324.715519	56.756296	74.593818
324.064705	69.124658	74.598823
323.565362	64.822131	74.603828
322.680474	80.015672	74.608833
321.806944	63.247903	74.613838
321.392039	67.573027	74.618842
321.034360	70.077236	74.623847
320.082824	76.793242	74.628852
319.294140	49.593752	74.633857
318.648942	75.635611	74.638862
318.277409	59.776518	74.643866
317.300809	55.291463	74.648871
316.467070	66.859560	74.653876
315.881395	71.621884	74.658881
315.855850	64.202107	74.663886
314.969414	71.978414	74.668890
314.196866	49.899525	74.673895
313.473089	89.246723	74.678900
313.306140	50.052408	74.683905
311.688552	81.936942	74.688910
311.531015	58.008138	74.693914
311.060811	80.972499	74.698919
310.035960	58.649982	74.703924
309.195392	73.253022	74.708929
308.314382	70.414724	74.713934
308.267314	66.085840	74.718938
307.845932	70.448266	74.723943
307.120383	74.398736	74.728948
306.198957	57.785264	74.733953
305.423508	88.152689	74.738958
305.340579	44.678054	74.743962
303.904347	81.142791	74.748967
303.105507	62.100355	74.753972
302.786624	69.858734	74.758977
302.273885	77.364184	74.763982
302.020340	61.159882	74.768986
300.724233	80.938209	74.773991
300.076382	63.163143	74.778996
299.813217	72.609326	74.784001
299.016372	83.791540	74.789006
298.574303	56.814325	74.794010
297.388258	78.386898	74.799015
296.892128	70.600613	74.804020
296.767596	54.501902	74.809025
295.710954	69.446867	74.814030
294.803281	67.785998	74.819034
294.228538	85.648593	74.824039
293.715453	65.441048	74.829044
292.833490	69.123160	74.834049
291.989976	73.593874	74.839054
291.647048	55.098482	74.844058
291.510684	81.532295	74.849063
290.347891	67.970646	74.854068
289.629721	54.737079	74.859073
288.824362	59.233244	74.864078
288.522931	75.037055	74.869082
287.876627	63.618011	74.874087
286.680113	63.072287	74.879092
286.299323	66.299224	74.884097
285.811503	65.662609	74.889102
284.977859	56.476285	74.894106
283.967760	72.374134	74.899111
283.321452	58.537794	74.904116
283.219419	51.414051	74.909121
282.581257	62.135748	74.914126
282.162942	68.123414	74.919130
281.502402	63.564338	74.924135
280.357365	62.587817	74.929140
280.025126	45.161414	74.934145
278.781890	67.552013	74.939150
278.168432	60.550787	74.944154
277.735328	64.371073	74.949159
277.050764	65.501927	74.954164
276.829065	67.530333	74.959169
275.973353	68.500825	74.964174
275.327632	66.132779	74.969178
274.956606	60.762787	74.974183
273.667339	59.508084	74.979188
272.944951	62.641251	74.984193
272.450406	69.809511	74.989198
272.212891	57.689845	74.994202
271.301026	52.787667	74.999207
270.425103	72.137914	75.004212
270.185098	63.798337	75.009217
269.354966	76.494897	75.014222
268.573156	54.105288	75.019226
267.920627	59.646196	75.024231
267.452502	66.162161	75.029236
266.755372	61.820220	75.034241
265.417874	72.279697	75.039246
264.973059	55.787379	75.044250
264.801456	63.099684	75.049255
263.951206	68.210100	75.054260
263.373824	61.988396	75.059265
262.514709	67.018229	75.064270
261.953191	55.213551	75.069274
261.413037	59.000444	75.074279
260.181332	59.262956	75.079284
259.593629	65.014292	75.084289
259.097349	62.590891	75.089294
258.780782	60.849998	75.094298
258.415574	60.261647	75.099303
257.654116	57.549384	75.104308
256.850604	59.541238	75.109313
256.037875	66.898983	75.114318
255.159811	63.823712	75.119322
254.639338	59.964512	75.124327
253.900696	59.601261	75.129332
253.699642	56.228845	75.134337
252.362330	71.524473	75.139342
251.619081	56.028995	75.144346
251.309364	59.921069	75.149351
250.756341	64.827998	75.154356
250.399115	50.950325	75.159361
249.443231	65.019856	75.164366
248.417191	61.217600	75.169370
247.901458	55.134299	75.174375
247.087984	63.703179	75.179380
247.050041	57.877999	75.184385
246.233936	70.441444	75.189390
245.376029	54.137983	75.194394
245.391476	59.630751	75.199399
243.895592	60.813688	75.204404
243.222068	46.712075	75.209409
242.577352	57.816415	75.214414
242.387240	48.956425	75.219418
241.750453	64.036300	75.224423
240.724780	62.227119	75.229428
240.343429	56.666407	75.234433
239.725929	70.816032	75.239438
238.701658	50.923398	75.244442
237.831440	70.559723	75.249447
236.919134	49.474494	75.254452
236.853598	67.020940	75.259457
236.692341	61.171267	75.264462
235.887935	65.940092	75.269466
235.095608	48.725810	75.274471
234.301424	67.526898	75.279476
233.572658	57.291045	75.284481
232.671603	48.709966	75.289486
231.869858	50.712583	75.294490
231.654370	69.260578	75.299495
231.142325	61.377513	75.304500
230.303867	47.718485	75.309505
229.340658	50.978358	75.314510
228.897553	57.900313	75.319514
228.709905	58.858925	75.324519
227.284490	62.965140	75.329524
226.904129	52.277961	75.334529
226.120086	57.016732	75.339534
225.570107	57.470177	75.344538
225.410425	52.943228	75.349543
224.589308	45.027453	75.354548
224.106907	45.131103	75.359553
222.708049	58.244732	75.364558
221.776948	55.964775	75.369562
221.512747	56.148748	75.374567
221.036691	65.094318	75.379572
220.805494	46.005601	75.384577
219.643187	47.409740	75.389582
218.890807	66.931088	75.394586
218.557222	53.014963	75.399591
217.466241	57.009521	75.404596
216.822889	53.944152	75.409601
215.895047	51.704676	75.414606
215.403429	58.446723	75.419610
215.190124	56.515922	75.424615
214.615821	59.475694	75.429620
214.049106	65.692014	75.434625
213.267408	70.681138	75.439630
212.496751	74.927386	75.444634
212.169786	54.693372	75.449639
210.778967	54.590220	75.454644
210.389524	70.026457	75.459649
209.609215	69.256730	75.464654
209.320834	53.259853	75.469658
208.387810	47.891178	75.474663
207.327684	67.948837	75.479668
207.139584	67.180880	75.484673
206.492290	43.123654	75.489678
206.124081	74.342264	75.494682
205.379829	39.872840	75.499687
204.255779	76.929585	75.504692
204.437327	50.754955	75.509697
202.915659	64.668715	75.514702
202.160038	58.514870	75.519706
201.655759	68.538773	75.524711
201.250015	66.925638	75.529716
200.969971	51.845158	75.534721
199.534606	66.565119	75.539726
198.644868	62.085188	75.544730
198.689950	64.454237	75.549735
198.058696	46.884735	75.554740
197.553872	65.131947	75.559745
196.877976	54.988599	75.564750
195.996263	49.436718	75.569754
195.237250	73.063651	75.574759
194.333130	63.380856	75.579764
193.636322	49.305050	75.584769
193.073194	68.657467	75.589774
192.630360	66.749071	75.594778
191.662711	56.258030	75.599783
191.092770	57.679692	75.604788
190.698291	74.688847	75.609793
190.213770	65.902603	75.614798
189.476565	49.162069	75.619802
188.358142	68.062166	75.624807
187.938127	52.494686	75.629812
187.166019	68.994805	75.634817
186.949819	59.230716	75.639822
185.917927	62.575669	75.644826
185.606883	66.251935	75.649831
184.827810	58.914474	75.654836
184.341707	75.908279	75.659841
183.246803	58.010602	75.664846
182.632169	64.529437	75.669850
182.373113	59.494824	75.674855
181.131550	57.379494	75.679860
180.668807	72.177762	75.684865
180.231145	63.724648	75.689870
179.713751	60.565094	75.694874
178.807641	65.119931	75.699879
177.860824	74.832805	75.704884
177.672316	67.374373	75.709889
176.831466	54.174608	75.714894
175.459011	87.024555	75.719898
175.208381	47.126197	75.724903
174.475175	88.354469	75.729908
174.303057	54.840831	75.734913
173.685172	74.950986	75.739918
172.885232	62.474771	75.744922
172.521386	72.471557	75.749927
171.627757	52.045660	75.754932
170.741691	64.405819	75.759937
169.793493	60.324702	75.764942
169.093501	61.104832	75.769946
168.883149	67.101923	75.774951
168.418674	66.157280	75.779956
167.458228	68.371291	75.784961
167.058153	63.244056	75.789966
166.405272	51.644781	75.794970
165.651434	63.998049	75.799975
164.602141	57.097893	75.804980
163.895039	47.803149	75.809985
163.569937	80.230633	75.814990
163.223663	61.183916	75.819994
162.331841	67.606615	75.824999
161.468093	76.964075	75.830004
161.214991	64.200410	75.835009
159.835865	70.539975	75.840014
158.889119	85.265632	75.845018
158.882307	71.633269	75.850023
158.313471	71.594607	75.855028
157.934595	56.506241	75.860033
156.953468	75.427037	75.865038
156.299642	65.336944	75.870042
155.834236	56.041502	75.875047
154.988937	63.311430	75.880052
154.527737	64.851369	75.885057
153.717178	61.270246	75.890062
152.935779	60.204266	75.895066
152.272303	54.936124	75.900071
151.106699	68.394194	75.905076
150.739683	46.425767	75.910081
149.966219	70.220570	75.915086
149.495928	65.903993	75.920090
149.590771	44.451661	75.925095
148.820094	66.490991	75.930100
148.200796	72.947506	75.935105
147.123427	53.514371	75.940110
146.142708	59.651646	75.945114
145.575378	56.187850	75.950119
144.736374	71.217991	75.955124
144.743297	57.662296	75.960129
143.615760	56.542712	75.965134
142.843218	56.889749	75.970138
142.386038	59.774093	75.975143
141.889871	66.449074	75.980148
141.231332	56.241482	75.985153
140.404505	61.464883	75.990158
139.643342	61.797491	75.995162
139.292699	58.068924	76.000167
138.357539	59.148318	76.005172
137.911934	64.173745	76.010177
137.270582	69.725516	76.015182
136.566747	69.219566	76.020186
135.871008	61.364244	76.025191
134.711707	65.492725	76.030196
134.277325	62.130723	76.035201
133.933843	69.686466	76.040206
133.434520	68.906647	76.045210
132.426773	59.642504	76.050215
131.568694	72.990049	76.055220
131.249236	67.496752	76.060225
130.594938	57.088228	76.065230
129.203841	58.713384	76.070234
128.932050	62.079064	76.075239
128.190127	64.072175	76.080244
127.950472	62.971849	76.085249
127.652250	70.766362	76.090254
126.784838	67.591677	76.095258
126.219947	56.874028	76.100263
125.341558	76.488027	76.105268
124.723121	69.522332	76.110273
123.837209	73.526804	76.115278
122.894706	67.472168	76.120282
122.873169	61.415739	76.125287
121.991091	69.456311	76.130292
121.373565	68.504547	76.135297
120.422268	70.888993	76.140302
120.127874	71.680145	76.145306
119.433538	67.974850	76.150311
118.167614	74.192313	76.155316
117.755052	64.877412	76.160321
117.113046	56.829041	76.165326
117.034577	68.249931	76.170330
116.514637	63.185974	76.175335
115.144326	67.933122	76.180340
114.795942	60.881794	76.185345
114.040696	64.758205	76.190350
113.011256	62.795149	76.195354
112.447191	55.830256	76.200359
111.631338	55.752155	76.205364
111.238974	68.678526	76.210369
111.060361	64.799534	76.215374
109.993995	64.780306	76.220378
109.260699	63.687747	76.225383
108.705661	72.546587	76.230388
108.311951	64.190555	76.235393
107.152397	56.786078	76.240398
106.293415	66.838172	76.245402
105.979863	61.086916	76.250407
105.073852	67.486664	76.255412
105.173594	55.764232	76.260417
104.189620	66.079092	76.265422
103.485990	66.758903	76.270426
103.217316	69.166947	76.275431
102.006920	66.404913	76.280436
100.955048	60.501763	76.285441
100.327103	54.608274	76.290446
100.190359	59.773669	76.295450
99.794113	60.210508	76.300455
98.988624	56.830433	76.305460
98.017625	61.066084	76.310465
97.721399	58.568242	76.315470
96.987722	67.982234	76.320474
96.264699	64.945372	76.325479
95.222706	63.793246	76.330484
94.993649	60.237670	76.335489
94.780693	72.812181	76.340494
93.433908	70.503957	76.345498
92.941760	68.910930	76.350503
92.313067	62.981292	76.355508
91.560999	80.657717	76.360513
90.465983	75.165118	76.365518
89.928312	63.970084	76.370522
89.676415	52.051441	76.375527
89.036705	61.611282	76.380532
88.318811	64.377954	76.385537
87.632183	59.074104	76.390542
87.096500	63.303407	76.395546
86.283059	53.670860	76.400551
85.252563	73.287042	76.405556
84.549626	59.562310	76.410561
84.424990	55.001405	76.415566
84.030767	61.042012	76.420570
83.223418	67.995272	76.425575
82.059924	77.950874	76.430580
81.746932	68.984350	76.435585
81.315351	57.963201	76.440590
80.012684	60.238130	76.445594
79.405421	56.315552	76.450599
78.838563	64.854601	76.455604
78.616703	62.715458	76.460609
77.585640	68.546999	76.465614
76.721649	70.515442	76.470618
76.433163	45.313036	76.475623
75.964772	66.760152	76.480628
75.132685	73.204888	76.485633
74.298478	54.628664	76.490638
73.585519	58.635525	76.495642
73.269447	77.696258	76.500647
72.266864	57.629964	76.505652
71.395205	54.079117	76.510657
70.909765	64.549424	76.515662
70.422119	62.403790	76.520666
70.350432	57.448115	76.525671
69.219909	70.416529	76.530676
68.360926	53.831080	76.535681
68.183804	62.516113	76.540686
66.984971	66.053306	76.545690
66.270112	60.720851	76.550695
65.515959	59.678937	76.555700
65.276968	62.659373	76.560705
64.751779	49.898142	76.565710
63.795508	80.084665	76.570714
63.419017	50.757083	76.575719
62.517988	56.191020	76.580724
61.530014	44.810805	76.585729
60.945693	56.596192	76.590734
60.123548	72.675413	76.595738
60.044337	50.891330	76.600743
59.358189	59.818385	76.605748
58.656208	62.047978	76.610753
57.946630	72.109372	76.615758
57.102199	58.142312	76.620762
56.863605	54.405351	76.625767
55.594734	53.724636	76.630772
54.847201	51.339781	76.635777
54.454503	71.163301	76.640782
53.977902	59.740938	76.645786
53.187298	52.649781	76.650791
52.478318	54.484705	76.655796
51.921106	57.175298	76.660801
51.710313	59.209864	76.665806
50.695260	68.110543	76.670810
49.877839	58.715168	76.675815
48.939880	67.455328	76.680820
48.693692	53.150026	76.685825
48.233920	65.366531	76.690830
47.046180	60.967308	76.695834
46.701795	61.638717	76.700839
46.358317	70.757112	76.705844
45.390122	60.285153	76.710849
44.183640	54.857670	76.715854
43.681039	68.156413	76.720858
43.470438	56.415682	76.725863
42.786860	59.124856	76.730868
41.584030	60.477198	76.735873
40.979633	58.621410	76.740878
40.207506	55.571902	76.745882
40.155315	56.702872	76.750887
39.815839	63.467981	76.755892
38.932022	62.708513	76.760897
38.070117	60.674618	76.765902
37.599231	68.919266	76.770906
36.956159	55.721137	76.775911
35.941482	67.907892	76.780916
35.291617	72.379330	76.785921
34.926106	60.915600	76.790926
34.098156	68.849799	76.795930
33.203660	59.780516	76.800935
32.541200	56.350846	76.805940
32.300390	57.267491	76.810945
31.541379	56.518078	76.815950
30.344656	59.821578	76.820954
29.908664	60.654247	76.825959
29.236927	55.348043	76.830964
28.821003	54.012512	76.835969
28.758577	60.837501	76.840974
27.326775	57.035420	76.845978
27.153467	56.340808	76.850983
26.283657	52.901640	76.855988
25.404498	68.545287	76.860993
24.894711	58.470118	76.865998
24.170116	67.012260	76.871002
23.651585	49.327091	76.876007
22.772334	58.999261	76.881012
21.952904	51.687228	76.886017
21.646887	56.922196	76.891022
20.859609	68.410412	76.896026
20.292136	54.940052	76.901031
19.318955	55.998749	76.906036
18.705561	63.022002	76.911041
18.512417	58.032093	76.916046
17.501987	59.090424	76.921050
16.439136	58.581857	76.926055
16.060313	55.095911	76.931060
15.634064	60.875146	76.936065
15.644725	66.204674	76.941070
14.357272	69.737106	76.946074
13.731952	58.045187	76.951079
13.008390	63.887618	76.956084
11.948125	69.334361	76.961089
11.264729	51.151982	76.966094
10.694543	66.402594	76.971098
10.426060	56.534926	76.976103
9.863015	62.198800	76.981108
9.088876	58.794834	76.986113
8.287189	57.866170	76.991118
7.677083	71.030690	76.996122
7.543841	64.895900	77.001127
6.089210	65.354937	77.006132
5.846586	61.730579	77.011137
5.496109	58.295302	77.016142
4.274363	63.056651	77.021147
3.715574	57.402878	77.026151
2.781450	55.922949	77.031156
2.616178	67.646236	77.036161