Mon Mar 08 20:29:50 2021

Number of Points = 14580

Depth (nm)	Load (N)	Time (s)
0.199798	93.329773	0.000000
-0.231732	98.733036	0.005005
-1.329011	85.503268	0.010010
-3.597943	64.115754	0.015014
-6.924646	41.309124	0.020019
-10.745444	22.274301	0.025024
-16.123783	29.037434	0.030029
-20.570555	26.160997	0.035034
-25.053802	13.739490	0.040038
-29.162918	26.172324	0.045043
-32.821310	20.978346	0.050048
-36.312522	27.688050	0.055053
-40.003520	16.985088	0.060058
-43.457051	12.292997	0.065062
-47.355667	17.087198	0.070067
-51.130594	23.599348	0.075072
-55.430927	28.859743	0.080077
-58.573766	36.201406	0.085082
-62.390555	20.754920	0.090086
-66.261468	15.102928	0.095091
-69.823980	29.377095	0.100096
-73.480932	4.105112	0.105101
-77.642742	31.217300	0.110106
-81.266851	22.758607	0.115110
-85.126024	16.116097	0.120115
-88.504314	24.348422	0.125120
-92.630894	27.017225	0.130125
-96.506997	19.554325	0.135130
-100.199297	14.640234	0.140134
-104.157746	28.039399	0.145139
-107.803052	17.250417	0.150144
-111.560730	27.262056	0.155149
-114.373422	23.290926	0.160154
-118.365435	14.616628	0.165158
-122.842748	25.293419	0.170163
-126.600147	11.013900	0.175168
-130.465423	14.434218	0.180173
-134.342895	24.245822	0.185178
-137.793748	13.160956	0.190182
-141.965729	19.555259	0.195187
-145.336947	13.177163	0.200192
-149.518157	9.402375	0.205197
-153.130845	14.876458	0.210202
-156.557140	26.188205	0.215206
-160.503453	23.795101	0.220211
-163.775001	14.237997	0.225216
-167.772788	20.297064	0.230221
-171.485429	19.856654	0.235226
-175.562129	28.165856	0.240230
-179.020300	23.704919	0.245235
-182.815228	12.377010	0.250240
-186.757244	23.070980	0.255245
-190.306920	20.438024	0.260250
-194.050406	21.137891	0.265254
-198.338293	18.376770	0.270259
-201.863644	10.006587	0.275264
-205.583148	37.377938	0.280269
-209.417809	22.483299	0.285274
-212.606771	20.790944	0.290278
-216.710324	15.378165	0.295283
-220.469859	15.818880	0.300288
-224.479745	26.928989	0.305293
-228.058097	23.977414	0.310298
-231.803204	18.986809	0.315302
-235.875040	21.574580	0.320307
-239.505789	21.305694	0.325312
-243.365311	22.330063	0.330317
-246.852466	26.554319	0.335322
-250.425819	23.092664	0.340326
-254.446794	24.234277	0.345331
-258.115550	12.517378	0.350336
-262.017756	25.160381	0.355341
-265.466674	22.434189	0.360346
-269.129114	13.873118	0.365350
-273.488346	21.322469	0.370355
-276.950039	20.044289	0.375360
-281.112010	18.059519	0.380365
-284.627456	20.151736	0.385370
-288.347156	12.219532	0.390374
-291.845044	19.849941	0.395379
-295.382018	17.040087	0.400384
-299.560450	17.629789	0.405389
-303.654638	15.686274	0.410394
-307.125901	5.645644	0.415398
-311.170792	18.760888	0.420403
-314.797327	18.989723	0.425408
-318.250788	26.510585	0.430413
-321.969244	18.165104	0.435418
-325.470503	11.469015	0.440422
-329.449099	11.935411	0.445427
-333.146852	21.683930	0.450432
-337.100935	14.747936	0.455437
-341.089483	16.147847	0.460442
-344.596969	1.313191	0.465446
-348.679862	26.046336	0.470451
-352.040089	14.863762	0.475456
-356.093187	20.514099	0.480461
-360.116633	20.599806	0.485466
-363.663597	14.961240	0.490470
-367.461794	20.496788	0.495475
-370.608486	12.082179	0.500480
-374.629443	12.757247	0.505485
-378.704917	22.793204	0.510490
-382.514740	23.363617	0.515494
-386.524623	28.627091	0.520499
-389.999001	9.566038	0.525504
-393.296049	20.549970	0.530509
-397.267845	4.102326	0.535514
-401.130677	24.642312	0.540518
-404.900585	26.923555	0.545523
-408.616000	5.535782	0.550528
-412.428598	15.326401	0.555533
-416.185317	5.467130	0.560538
-419.954674	19.818930	0.565542
-423.994764	17.567387	0.570547
-427.393797	10.675373	0.575552
-431.327183	6.140905	0.580557
-434.860033	9.015069	0.585562
-438.886451	13.674184	0.590566
-442.843654	23.743392	0.595571
-446.104235	21.892491	0.600576
-450.132242	20.930486	0.605581
-453.727080	23.106582	0.610586
-457.599525	27.756912	0.615590
-461.544668	15.535750	0.620595
-464.545786	1.639055	0.625600
-468.961090	12.347535	0.630605
-472.355934	7.033326	0.635610
-476.514191	16.344700	0.640614
-480.230175	19.766955	0.645619
-483.699208	14.813087	0.650624
-487.529652	15.893123	0.655629
-491.475783	17.575067	0.660634
-495.417219	11.104070	0.665638
-499.212185	17.650048	0.670643
-502.614100	13.262608	0.675648
-506.481419	27.057795	0.680653
-510.331251	15.756557	0.685658
-514.300126	12.621811	0.690662
-518.003886	23.636172	0.695667
-521.221462	19.432187	0.700672
-525.102025	18.694321	0.705677
-529.121822	11.508981	0.710682
-532.480305	28.089603	0.715686
-536.601130	20.314907	0.720691
-540.394734	3.425937	0.725696
-544.062922	30.135116	0.730701
-548.037069	-6.200382	0.735706
-551.329580	22.394585	0.740710
-555.425104	8.985039	0.745715
-558.805757	18.651692	0.750720
-563.053047	13.136343	0.755725
-566.994540	23.546982	0.760730
-570.388587	-1.018674	0.765734
-574.330372	34.616510	0.770739
-577.564756	3.044737	0.775744
-582.077481	1.094458	0.780749
-585.727497	24.073163	0.785754
-589.020327	16.740256	0.790758
-593.095050	16.416689	0.795763
-597.018972	10.162249	0.800768
-600.638771	18.547359	0.805773
-604.091468	29.233179	0.810778
-607.823000	22.744605	0.815782
-611.876241	28.655563	0.820787
-615.484161	14.792939	0.825792
-619.422898	22.260862	0.830797
-623.208398	16.384863	0.835802
-626.573781	10.522170	0.840806
-630.571377	35.625276	0.845811
-634.267387	19.244369	0.850816
-638.074477	28.430529	0.855821
-642.023953	23.916329	0.860826
-645.577556	25.537387	0.865830
-649.764298	20.605409	0.870835
-653.083216	17.458505	0.875840
-656.976292	16.123662	0.880845
-660.354529	10.334031	0.885850
-664.345246	20.514582	0.890854
-668.097531	13.964778	0.895859
-672.147615	19.222522	0.900864
-675.818950	22.237428	0.905869
-679.580025	9.985675	0.910874
-683.111692	6.823931	0.915878
-687.249164	-2.512025	0.920883
-690.928918	21.247358	0.925888
-694.543043	7.991366	0.930893
-698.472937	20.421839	0.935898
-702.046337	14.147833	0.940902
-705.877648	14.280686	0.945907
-709.592649	19.021358	0.950912
-713.219366	9.783579	0.955917
-717.318202	9.311128	0.960922
-720.900042	19.074795	0.965926
-724.557161	11.234227	0.970931
-728.360990	8.593824	0.975936
-732.555499	11.031734	0.980941
-736.049495	7.950776	0.985946
-739.408720	2.180304	0.990950
-743.675103	24.988080	0.995955
-747.188600	16.530131	1.000960
-750.794256	5.083075	1.005965
-754.749057	18.845298	1.010970
-758.445739	18.743847	1.015974
-762.469437	26.222423	1.020979
-766.151663	22.860956	1.025984
-769.856757	23.811033	1.030989
-773.360718	23.968939	1.035994
-777.152359	2.649207	1.040998
-781.233874	5.911165	1.046003
-784.973963	15.416386	1.051008
-788.571299	14.960087	1.056013
-792.411639	13.225989	1.061018
-796.238006	7.575993	1.066022
-799.884505	10.126684	1.071027
-803.313780	10.606983	1.076032
-807.457711	8.484658	1.081037
-811.292740	21.529292	1.086042
-814.867335	7.267479	1.091046
-818.852190	4.960487	1.096051
-822.365025	8.431209	1.101056
-826.357658	15.827653	1.106061
-829.907767	-0.738623	1.111066
-833.762645	4.390416	1.116070
-837.737418	19.417414	1.121075
-841.221261	0.487945	1.126080
-844.830261	14.038916	1.131085
-848.797434	11.981439	1.136090
-852.439144	1.044902	1.141094
-856.717295	21.847440	1.146099
-859.972630	2.529838	1.151104
-863.783218	5.343381	1.156109
-867.723353	8.333746	1.161114
-871.054551	1.988181	1.166118
-875.283030	15.534162	1.171123
-878.814471	9.351493	1.176128
-882.428514	0.479371	1.181133
-886.481936	18.756227	1.186138
-890.076855	23.903719	1.191142
-894.334017	12.400222	1.196147
-897.821613	2.758918	1.201152
-901.251961	10.123924	1.206157
-905.564333	18.252805	1.211162
-908.918991	13.629775	1.216166
-912.753943	22.700963	1.221171
-916.335958	-0.313991	1.226176
-920.425996	15.381207	1.231181
-924.241575	16.347614	1.236186
-927.325880	8.636547	1.241190
-931.093662	17.922505	1.246195
-935.241250	20.406882	1.251200
-939.248342	12.488597	1.256205
-943.008216	15.209010	1.261210
-946.287962	11.909624	1.266214
-950.608848	18.223449	1.271219
-954.040289	3.842797	1.276224
-957.614865	11.555769	1.281229
-961.675871	8.442831	1.286234
-965.275118	0.263856	1.291238
-969.200933	10.743561	1.296243
-973.089727	10.387766	1.301248
-976.478128	13.342116	1.306253
-980.556737	12.250354	1.311258
-984.057838	13.311634	1.316262
-987.996127	31.401527	1.321267
-991.761661	26.644067	1.326272
-995.578551	7.309258	1.331277
-999.697106	20.188220	1.336282
-1002.910393	23.177677	1.341286
-1006.707265	14.218305	1.346291
-1010.354049	17.923595	1.351296
-1014.185491	10.541855	1.356301
-1018.391970	12.662089	1.361306
-1021.912917	18.610005	1.366310
-1026.059675	23.175809	1.371315
-1029.212463	15.885806	1.376320
-1032.927086	18.665351	1.381325
-1036.671583	29.131942	1.386330
-1040.306780	19.041416	1.391334
-1044.473078	15.179130	1.396339
-1048.298232	24.206386	1.401344
-1051.892699	16.219151	1.406349
-1055.744806	21.385948	1.411354
-1059.377481	25.358693	1.416358
-1063.134057	24.896751	1.421363
-1066.751885	22.523593	1.426368
-1070.423088	17.196139	1.431373
-1074.411351	26.266872	1.436378
-1078.082896	13.279305	1.441382
-1082.388260	20.007162	1.446387
-1085.974805	10.027199	1.451392
-1089.593858	11.731922	1.456397
-1093.238180	6.855910	1.461402
-1096.918425	21.279576	1.466406
-1101.140103	33.615439	1.471411
-1104.608029	15.085941	1.476416
-1108.235646	8.684075	1.481421
-1112.149575	6.733643	1.486426
-1115.715427	6.853080	1.491430
-1119.766903	18.993016	1.496435
-1123.399578	29.441847	1.501440
-1126.795730	23.551707	1.506445
-1130.497651	21.220487	1.511450
-1134.575782	13.646627	1.516454
-1138.377726	20.886928	1.521459
-1142.469157	18.042504	1.526464
-1145.758902	13.505628	1.531469
-1149.849483	30.421746	1.536474
-1153.574318	20.060346	1.541478
-1157.319921	23.091026	1.546483
-1160.982574	25.887686	1.551488
-1164.860000	10.063406	1.556493
-1168.624163	14.975058	1.561498
-1172.255716	14.936375	1.566502
-1175.760495	18.776878	1.571507
-1179.643045	5.337596	1.576512
-1183.551843	11.180657	1.581517
-1187.534693	24.831353	1.586522
-1191.214246	21.752394	1.591526
-1195.085613	26.149857	1.596531
-1198.858717	16.813308	1.601536
-1201.931831	1.226229	1.606541
-1205.817698	12.294372	1.611546
-1209.847691	13.349163	1.616550
-1213.805427	16.972068	1.621555
-1217.215812	13.298197	1.626560
-1221.129048	14.285443	1.631565
-1224.820293	12.198651	1.636570
-1228.478782	5.626897	1.641574
-1232.852414	17.919483	1.646579
-1236.291831	14.054761	1.651584
-1239.983585	32.871911	1.656589
-1243.883234	20.438322	1.661594
-1247.158846	13.150946	1.666598
-1251.580720	18.104911	1.671603
-1255.217967	19.439097	1.676608
-1258.701484	32.290973	1.681613
-1262.962508	20.199079	1.686618
-1265.842309	17.943071	1.691622
-1269.819631	34.510125	1.696627
-1273.881476	7.993221	1.701632
-1277.691835	16.219015	1.706637
-1281.504994	25.217906	1.711642
-1285.145319	10.677272	1.716646
-1288.740897	13.554848	1.721651
-1292.226437	17.534356	1.726656
-1296.101033	-15.775378	1.731661
-1300.013401	35.058057	1.736666
-1303.872703	0.815531	1.741670
-1307.905263	21.530601	1.746675
-1311.500950	24.360927	1.751680
-1315.245780	21.303655	1.756685
-1319.215501	15.395243	1.761690
-1322.465350	2.469910	1.766694
-1326.225225	19.068455	1.771699
-1330.261383	15.974270	1.776704
-1334.183608	0.777172	1.781709
-1338.107901	28.985320	1.786714
-1341.319531	8.702789	1.791718
-1345.289600	7.023492	1.796723
-1349.170920	27.731768	1.801728
-1352.478264	8.396474	1.806733
-1356.682734	12.680377	1.811738
-1359.915723	29.141026	1.816742
-1364.021471	17.800271	1.821747
-1368.057936	15.832047	1.826752
-1371.689588	16.315617	1.831757
-1375.617328	21.193864	1.836762
-1379.191154	-0.036617	1.841766
-1383.380164	18.626950	1.846771
-1386.853182	18.610528	1.851776
-1390.607256	5.108491	1.856781
-1394.149041	10.047968	1.861786
-1397.551751	21.720247	1.866790
-1401.235432	6.455119	1.871795
-1405.174419	10.379665	1.876800
-1409.314077	-5.551957	1.881805
-1413.083157	16.861879	1.886810
-1417.110091	-3.174872	1.891814
-1421.090671	30.556507	1.896819
-1424.471519	11.445966	1.901824
-1427.857553	23.393136	1.906829
-1431.753163	17.499864	1.911834
-1435.439020	14.371856	1.916838
-1439.268150	14.907649	1.921843
-1442.986159	3.802992	1.926848
-1446.808452	24.673826	1.931853
-1450.721535	10.978174	1.936858
-1454.186830	15.492369	1.941862
-1457.879677	26.403863	1.946867
-1461.615330	10.128541	1.951872
-1465.631417	-3.296710	1.956877
-1469.917385	34.484007	1.961882
-1473.126318	2.009362	1.966886
-1477.107598	33.471908	1.971891
-1480.650674	7.750645	1.976896
-1484.413885	31.858733	1.981901
-1488.018770	18.832815	1.986906
-1491.969490	-1.342140	1.991910
-1495.991245	35.360344	1.996915
-1499.638628	12.007332	2.006912
-1500.480807	13.332561	2.016909
-1498.286158	23.639709	2.026906
-1495.067446	7.856921	2.036902
-1492.930880	12.795882	2.046899
-1491.197160	18.441940	2.056896
-1489.722355	14.389668	2.066893
-1487.611585	14.828368	2.076890
-1485.604846	13.828049	2.086886
-1483.528147	16.195223	2.096883
-1481.757510	13.481794	2.106880
-1480.012766	17.242554	2.116877
-1477.746615	15.734947	2.126874
-1476.093597	18.866236	2.136870
-1474.253814	8.729140	2.146867
-1472.340550	23.352104	2.156864
-1470.213227	11.312262	2.166861
-1468.644537	26.961389	2.176858
-1466.796959	7.612158	2.186854
-1464.678304	18.570932	2.196851
-1462.811518	26.091884	2.206848
-1460.701476	11.328177	2.216845
-1459.008385	18.482233	2.226842
-1457.278365	19.529782	2.236838
-1455.257140	16.773091	2.246835
-1453.242085	11.263911	2.256832
-1451.531796	18.031564	2.266829
-1450.077672	20.522139	2.276826
-1447.704258	10.424343	2.286822
-1445.860741	17.143828	2.296819
-1443.996483	21.640162	2.306816
-1442.228011	12.136563	2.316813
-1439.733546	16.918806	2.326810
-1438.277186	27.168982	2.336806
-1436.349020	12.778597	2.346803
-1434.556164	15.101270	2.356800
-1432.827208	18.285165	2.366797
-1430.796680	22.699629	2.376794
-1429.158831	12.105456	2.386790
-1427.025770	21.667859	2.396787
-1425.388192	13.989831	2.406784
-1423.161311	15.178890	2.416781
-1421.408999	22.107198	2.426778
-1419.445264	14.987960	2.436774
-1417.468436	16.032338	2.446771
-1415.693293	17.658440	2.456768
-1413.876999	17.741754	2.466765
-1412.032062	17.004228	2.476762
-1410.139711	21.039811	2.486758
-1408.122663	14.848293	2.496755
-1406.538434	11.811107	2.506752
-1404.513132	21.158697	2.516749
-1402.697235	23.308773	2.526746
-1400.763148	16.592161	2.536742
-1398.405069	17.799712	2.546739
-1396.716236	24.202980	2.556736
-1395.179333	17.731525	2.566733
-1393.501268	23.500251	2.576730
-1391.368375	17.241256	2.586726
-1389.419572	11.592746	2.596723
-1387.691597	20.874277	2.606720
-1385.586493	16.755894	2.616717
-1383.869012	16.490341	2.626714
-1382.133868	25.968086	2.636710
-1379.980771	8.846669	2.646707
-1378.321019	19.579022	2.656704
-1376.549813	14.655216	2.666701
-1374.472856	20.649025	2.676698
-1372.174561	24.453879	2.686694
-1370.480434	22.168012	2.696691
-1368.908022	19.532185	2.706688
-1366.896963	25.871265	2.716685
-1365.144503	20.419979	2.726682
-1362.900121	17.417657	2.736678
-1361.154533	12.736368	2.746675
-1359.676641	14.883747	2.756672
-1357.850742	24.770111	2.766669
-1355.569393	15.811263	2.776666
-1353.536761	15.329506	2.786662
-1351.692459	13.278542	2.796659
-1349.996188	16.682455	2.806656
-1348.039881	18.895355	2.816653
-1346.624409	19.792829	2.826650
-1344.166830	20.172989	2.836646
-1342.482100	16.900298	2.846643
-1340.548708	11.451647	2.856640
-1338.767120	17.158057	2.866637
-1337.100393	23.031267	2.876634
-1335.167050	16.569016	2.886630
-1332.988535	13.252027	2.896627
-1331.148403	13.121606	2.906624
-1329.351533	12.906539	2.916621
-1327.416899	15.617100	2.926618
-1325.711360	21.296224	2.936614
-1323.800748	22.787040	2.946611
-1321.718406	26.838077	2.956608
-1319.679221	13.625177	2.966605
-1318.388228	24.823947	2.976602
-1316.133463	21.976311	2.986598
-1314.366622	17.722673	2.996595
-1312.783767	-0.867296	3.006592
-1310.755115	26.428005	3.016589
-1308.490498	19.811704	3.026586
-1306.850170	16.434048	3.036582
-1305.001464	28.231935	3.046579
-1302.857108	16.655250	3.056576
-1301.175819	14.584631	3.066573
-1299.328773	27.810052	3.076570
-1297.326398	19.835310	3.086566
-1295.608320	10.797735	3.096563
-1293.864505	11.462702	3.106560
-1291.670211	10.891972	3.116557
-1289.657144	22.183597	3.126554
-1288.201672	10.938221	3.136550
-1286.390306	12.823871	3.146547
-1284.310032	13.665505	3.156544
-1282.502506	19.022047	3.166541
-1280.528793	15.954183	3.176538
-1278.736200	14.819381	3.186534
-1276.658424	23.291921	3.196531
-1274.885040	9.979502	3.206528
-1273.241589	20.796652	3.216525
-1271.117891	19.452560	3.226522
-1269.124444	13.528596	3.236518
-1267.484634	16.594266	3.246515
-1265.544796	14.108110	3.256512
-1263.706692	5.188709	3.266509
-1261.845553	12.516541	3.276506
-1259.846655	10.728255	3.286502
-1257.954157	15.655985	3.296499
-1256.161044	9.363071	3.306496
-1253.999028	12.468327	3.316493
-1252.581981	8.963822	3.326490
-1250.251525	2.779118	3.336486
-1248.665084	14.068004	3.346483
-1247.089905	13.242736	3.356480
-1244.776238	9.528437	3.366477
-1242.904948	17.730916	3.376474
-1241.125266	18.731212	3.386470
-1239.347347	16.354666	3.396467
-1237.453720	9.093644	3.406464
-1235.462176	11.743075	3.416461
-1233.703178	15.032837	3.426458
-1231.523061	11.999874	3.436454
-1229.850712	15.207195	3.446451
-1227.923471	12.009453	3.456448
-1226.191400	19.743209	3.466445
-1224.141883	21.251352	3.476442
-1222.548186	18.405387	3.486438
-1220.531629	11.516255	3.496435
-1218.563618	6.411083	3.506432
-1216.601937	14.595962	3.516429
-1214.911999	12.154572	3.526426
-1213.214913	8.654222	3.536422
-1211.331282	13.491839	3.546419
-1209.062549	11.916189	3.556416
-1207.430677	17.261430	3.566413
-1205.479541	10.040172	3.576410
-1203.435489	11.825502	3.586406
-1201.553844	13.810494	3.596403
-1199.999170	19.397025	3.606400
-1197.880229	14.989243	3.616397
-1196.018789	13.625608	3.626394
-1194.287277	11.929105	3.636390
-1192.193130	6.274862	3.646387
-1190.592799	15.914852	3.656384
-1188.938434	10.681479	3.666381
-1186.692178	14.561160	3.676378
-1184.616315	7.582049	3.686374
-1182.933150	13.626417	3.696371
-1181.314566	12.838455	3.706368
-1178.998535	13.492474	3.716365
-1177.200643	11.428547	3.726362
-1175.395732	8.510928	3.736358
-1173.667150	15.342191	3.746355
-1171.850832	6.178461	3.756352
-1169.917098	9.121390	3.766349
-1167.751583	10.427878	3.776346
-1165.949006	11.254055	3.786342
-1164.360467	18.573490	3.796339
-1162.585820	8.208624	3.806336
-1160.225771	10.897051	3.816333
-1158.354472	12.501655	3.826330
-1156.746231	13.256307	3.836326
-1154.576075	6.661580	3.846323
-1153.007384	7.736750	3.856320
-1151.253399	16.744338	3.866317
-1149.171652	21.232968	3.876314
-1147.082526	12.159807	3.886310
-1145.382279	10.147839	3.896307
-1143.674163	10.864417	3.906304
-1141.554757	9.645857	3.916301
-1139.782175	15.082313	3.926298
-1138.092459	13.342015	3.936294
-1136.181334	11.143170	3.946291
-1134.333987	9.390287	3.956288
-1132.215721	13.794147	3.966285
-1130.287751	13.007247	3.976282
-1128.584449	11.586865	3.986278
-1126.611165	14.100377	3.996275
-1124.786319	10.110735	4.006272
-1122.918309	15.070919	4.016269
-1121.058495	20.310293	4.026266
-1119.269539	12.347731	4.036262
-1117.317182	11.462210	4.046259
-1115.157520	15.717369	4.056256
-1113.625976	11.697293	4.066253
-1111.897186	14.646219	4.076250
-1109.650442	13.808340	4.086246
-1107.915572	8.847911	4.096243
-1105.987522	10.947129	4.106240
-1104.008342	8.726370	4.116237
-1102.100699	7.721708	4.126234
-1100.378549	2.697010	4.136230
-1098.474413	8.308229	4.146227
-1096.415706	19.804308	4.156224
-1094.848961	4.226274	4.166221
-1093.059740	12.271499	4.176218
-1090.907695	3.117275	4.186214
-1088.829311	6.922861	4.196211
-1087.503108	8.657347	4.206208
-1085.671116	10.549331	4.216205
-1083.477244	6.454904	4.226202
-1081.488352	3.465298	4.236198
-1079.662311	14.507589	4.246195
-1077.932418	17.720031	4.256192
-1076.199427	19.930997	4.266189
-1074.117484	13.843043	4.276186
-1072.051187	14.451859	4.286182
-1070.568349	18.000646	4.296179
-1068.536720	10.288229	4.306176
-1066.602336	8.590946	4.316173
-1064.481880	10.206296	4.326170
-1062.862020	4.948529	4.336166
-1061.173358	8.824372	4.346163
-1058.940738	3.959613	4.356160
-1057.435090	7.312140	4.366157
-1055.404384	12.292144	4.376154
-1053.455198	9.196813	4.386150
-1051.425482	6.023871	4.396147
-1049.502373	5.965658	4.406144
-1048.001425	5.641835	4.416141
-1045.892989	10.104187	4.426138
-1044.143104	8.115928	4.436134
-1042.015153	2.611131	4.446131
-1040.345201	9.665021	4.456128
-1038.442039	12.050888	4.466125
-1036.726389	10.892262	4.476122
-1034.920272	8.014026	4.486118
-1032.850620	14.277732	4.496115
-1030.947264	9.227255	4.506112
-1029.306212	12.749185	4.516109
-1027.348724	11.101918	4.526106
-1025.325349	12.083930	4.536102
-1023.190123	14.330071	4.546099
-1021.418540	11.648406	4.556096
-1019.567803	8.556217	4.566093
-1017.823768	6.237358	4.576090
-1016.034063	11.570130	4.586086
-1013.798700	13.525547	4.596083
-1012.413501	13.651281	4.606080
-1010.588796	7.528738	4.616077
-1008.425054	7.188933	4.626074
-1006.616587	12.345041	4.636070
-1004.711747	0.773755	4.646067
-1002.615597	5.449676	4.656064
-1001.091982	15.534686	4.666061
-998.886226	11.537900	4.676058
-997.189833	3.797055	4.686054
-995.317899	4.497018	4.696051
-993.354917	0.210667	4.706048
-991.625973	-1.861040	4.716045
-989.897574	-1.850174	4.726042
-987.745085	0.767421	4.736038
-985.747872	6.993809	4.746035
-984.202460	0.221264	4.756032
-982.562424	-1.103638	4.766029
-980.309012	12.219705	4.776026
-978.444883	-0.484973	4.786022
-976.607955	17.090477	4.796019
-974.278831	3.678324	4.806016
-972.728183	7.481575	4.816013
-970.867849	-2.961594	4.826010
-969.136362	15.979049	4.836006
-967.029192	7.302594	4.846003
-965.432543	4.971028	4.856000
-963.230424	9.876341	4.865997
-961.589638	11.491128	4.875994
-959.673454	2.063697	4.885990
-957.744715	11.472946	4.895987
-956.100676	3.388419	4.905984
-954.088284	2.021361	4.915981
-952.021250	-0.356994	4.925978
-950.278330	8.979349	4.935974
-948.271465	-0.952012	4.945971
-946.415749	5.911206	4.955968
-944.971784	3.525126	4.965965
-942.883772	6.190966	4.975962
-940.725137	3.163281	4.985958
-939.013254	-3.676905	4.995955
-936.954518	8.114564	5.005952
-935.078562	10.185943	5.015949
-933.735534	3.545253	5.025946
-931.966833	2.267702	5.035942
-929.675313	9.260185	5.045939
-927.638408	-1.762203	5.055936
-925.977194	12.312687	5.065933
-924.124904	9.005599	5.075930
-921.929378	5.479434	5.085926
-920.192396	11.025965	5.095923
-918.127741	13.100342	5.105920
-916.278885	9.070702	5.115917
-914.993917	15.047907	5.125914
-912.794363	5.662036	5.135910
-910.699095	10.347659	5.145907
-908.770360	3.824899	5.155904
-907.229195	12.243078	5.165901
-905.315286	9.960292	5.175898
-903.401448	5.386625	5.185894
-901.519417	1.455897	5.195891
-899.707240	10.656483	5.205888
-897.706046	8.100818	5.215885
-895.724273	13.050901	5.225882
-894.089591	9.388655	5.235878
-892.123064	11.895558	5.245875
-889.918509	6.520736	5.255872
-888.511953	14.201030	5.265869
-886.415736	14.402624	5.275866
-884.624784	10.934858	5.285862
-882.706313	12.025339	5.295859
-881.009509	13.361247	5.305856
-879.375311	13.163060	5.315853
-877.172763	13.609750	5.325850
-875.108189	3.451335	5.335846
-873.354629	9.276285	5.345843
-871.375443	6.523648	5.355840
-869.672837	9.064869	5.365837
-867.434839	13.430895	5.375834
-865.791202	11.404491	5.385830
-863.903401	8.129665	5.395827
-862.169382	5.956192	5.405824
-860.191740	7.029338	5.415821
-858.114243	10.674240	5.425818
-856.494922	18.817880	5.435814
-854.550998	0.306183	5.445811
-852.790988	11.444491	5.455808
-851.070109	6.216494	5.465805
-848.913916	8.058420	5.475802
-846.952432	10.731946	5.485798
-845.030159	10.595092	5.495795
-843.371222	7.808415	5.505792
-841.739810	11.350971	5.515789
-839.620877	3.957915	5.525786
-837.591977	9.712039	5.535782
-835.711722	1.416154	5.545779
-833.687703	15.881521	5.555776
-832.098017	19.342341	5.565773
-830.456059	10.790882	5.575770
-828.289023	11.393284	5.585766
-826.510784	11.344202	5.595763
-824.438706	8.169413	5.605760
-822.892305	11.447696	5.615757
-820.763466	15.169684	5.625754
-818.748256	12.818671	5.635750
-816.963258	14.945737	5.645747
-815.078846	9.364803	5.655744
-813.697940	19.322782	5.665741
-811.148475	7.583848	5.675738
-809.412503	5.994272	5.685734
-807.849525	16.189973	5.695731
-805.639740	8.790315	5.705728
-804.159091	3.346557	5.715725
-801.978769	13.816189	5.725722
-799.996750	10.911588	5.735718
-798.328217	5.475693	5.745715
-796.347910	10.138750	5.755712
-794.526768	10.502806	5.765709
-792.665515	13.648686	5.775706
-790.901964	9.744870	5.785702
-788.805404	3.340629	5.795699
-787.133000	13.029413	5.805696
-785.301753	6.834936	5.815693
-783.208442	12.825116	5.825690
-781.265336	8.250021	5.835686
-779.626972	12.252533	5.845683
-777.546485	6.052960	5.855680
-775.913040	9.031592	5.865677
-774.050136	13.756064	5.875674
-771.964443	1.030316	5.885670
-770.184726	12.162389	5.895667
-768.047533	4.577012	5.905664
-766.154750	11.851278	5.915661
-764.556830	11.458456	5.925658
-762.882415	16.145173	5.935654
-760.796273	14.013382	5.945651
-758.835496	13.729928	5.955648
-756.937109	7.837351	5.965645
-755.005111	20.703935	5.975642
-753.329260	18.519311	5.985638
-751.547155	14.214689	5.995635
-749.611749	24.488279	6.005632
-747.544823	17.591466	6.015629
-745.918267	13.267500	6.025626
-743.719664	14.674881	6.035622
-742.011165	15.792721	6.045619
-740.203223	16.572586	6.055616
-738.405084	15.137325	6.065613
-736.404315	8.552656	6.075610
-734.188931	14.112876	6.085606
-732.561198	8.266728	6.095603
-730.804375	12.160351	6.105600
-728.898593	9.141684	6.115597
-726.883951	15.982856	6.125594
-724.988556	12.905855	6.135590
-723.311750	15.988117	6.145587
-721.401017	11.749797	6.155584
-719.650881	12.567334	6.165581
-717.747667	12.473101	6.175578
-715.849763	13.132826	6.185574
-713.384810	6.541888	6.195571
-711.946950	16.231903	6.205568
-710.329974	18.561155	6.215565
-708.317043	11.331975	6.225562
-706.095168	2.915276	6.235558
-704.491415	9.501622	6.245555
-702.927682	14.419215	6.255552
-700.701753	7.335993	6.265549
-698.812266	8.912804	6.275546
-697.217053	4.132859	6.285542
-695.250322	9.767584	6.295539
-693.273145	5.734972	6.305536
-690.998040	9.967357	6.315533
-689.305829	13.617144	6.325530
-687.507867	9.878418	6.335526
-685.549250	9.699573	6.345523
-683.957692	3.374533	6.355520
-681.957955	14.326275	6.365517
-679.791187	10.639142	6.375514
-678.100356	5.603945	6.385510
-676.648818	12.296735	6.395507
-674.310951	8.691207	6.405504
-672.612624	7.080904	6.415501
-670.881541	12.113874	6.425498
-668.889788	2.464589	6.435494
-666.890615	7.295261	6.445491
-664.876613	8.046995	6.455488
-663.181432	18.730074	6.465485
-661.276175	5.821669	6.475482
-659.648663	10.285446	6.485478
-657.640772	10.687660	6.495475
-655.582632	8.367815	6.505472
-653.979536	9.586239	6.515469
-651.922341	8.788554	6.525466
-649.841423	10.004841	6.535462
-648.080268	4.184795	6.545459
-646.411123	9.413983	6.555456
-644.182683	11.032993	6.565453
-642.760020	11.926592	6.575450
-640.823446	3.391333	6.585446
-638.634181	-7.636234	6.595443
-636.913441	2.764895	6.605440
-634.980347	14.313081	6.615437
-633.187052	-0.756216	6.625434
-631.288966	16.224049	6.635430
-629.478668	7.270052	6.645427
-627.482102	12.101178	6.655424
-625.702928	16.141304	6.665421
-623.950198	8.915868	6.675418
-621.996252	11.186609	6.685414
-620.014648	8.288535	6.695411
-618.489316	16.707884	6.705408
-616.243702	5.279769	6.715405
-614.347572	18.270630	6.725402
-612.364620	15.958097	6.735398
-610.495615	19.983884	6.745395
-608.920891	17.348177	6.755392
-606.966628	15.818602	6.765389
-605.002383	16.335195	6.775386
-603.309155	17.738190	6.785382
-601.181008	18.329647	6.795379
-599.202136	1.713451	6.805376
-597.564249	14.908202	6.815373
-595.678380	7.170495	6.825370
-593.783346	10.055368	6.835366
-591.951692	6.251333	6.845363
-590.178482	17.634065	6.855360
-588.116628	6.450052	6.865357
-586.273463	4.901929	6.875354
-584.453134	13.526790	6.885350
-582.413020	10.952535	6.895347
-580.615017	5.772395	6.905344
-578.730661	21.506047	6.915341
-576.810083	17.882013	6.925338
-574.794025	18.906636	6.935334
-573.112064	17.190076	6.945331
-571.321232	10.838005	6.955328
-569.565025	20.278337	6.965325
-567.518930	4.109285	6.975322
-565.662918	21.480002	6.985318
-563.964494	15.804231	6.995315
-561.684889	10.616640	7.005312
-560.025122	14.645894	7.015309
-558.107849	14.009578	7.025306
-556.391471	10.651849	7.035302
-554.326179	12.216485	7.045299
-552.409065	16.845648	7.055296
-550.548793	14.636440	7.065293
-548.740154	18.496669	7.075290
-546.964675	6.554798	7.085286
-544.827479	8.324257	7.095283
-543.110305	16.270942	7.105280
-541.168421	10.549984	7.115277
-539.518673	19.150033	7.125274
-537.612733	6.778407	7.135270
-535.658403	9.252830	7.145267
-533.615180	5.598189	7.155264
-531.930996	12.353386	7.165261
-529.931078	9.532980	7.175258
-528.106925	8.690523	7.185254
-526.210532	8.594376	7.195251
-524.384661	5.230232	7.205248
-522.226950	8.316350	7.215245
-520.810037	13.868537	7.225242
-518.805275	10.093743	7.235238
-516.733563	19.992115	7.245235
-514.725156	3.445460	7.255232
-513.377194	14.443049	7.265229
-511.549815	13.969540	7.275226
-509.265930	14.731983	7.285222
-507.263733	16.341473	7.295219
-505.621834	8.120198	7.305216
-503.842512	8.398006	7.315213
-501.734923	15.723457	7.325210
-499.921008	5.295906	7.335206
-497.995026	7.523851	7.345203
-496.208379	12.780175	7.355200
-494.254747	12.376509	7.365197
-492.350926	7.908957	7.375194
-490.674010	11.810793	7.385190
-488.400835	9.775673	7.395187
-486.931165	6.978413	7.405184
-485.162812	10.804075	7.415181
-483.245290	16.391592	7.425178
-481.133367	13.993834	7.435174
-479.189017	10.860259	7.445171
-477.247709	11.156425	7.455168
-475.653012	8.913903	7.465165
-473.716486	15.313078	7.475162
-471.590948	19.462211	7.485158
-470.074786	11.415763	7.495155
-467.899193	8.392100	7.505152
-466.257896	9.194052	7.515149
-464.411092	10.923125	7.525146
-462.285286	11.227732	7.535142
-460.526670	3.380979	7.545139
-458.848093	9.072985	7.555136
-456.954478	9.845701	7.565133
-454.845652	14.021201	7.575130
-453.028000	9.957413	7.585126
-451.276348	7.955089	7.595123
-449.699210	14.435358	7.605120
-447.308159	13.718735	7.615117
-445.234315	12.350183	7.625114
-443.540784	9.161958	7.635110
-441.823166	7.480845	7.645107
-439.920258	8.026316	7.655104
-437.936947	12.951301	7.665101
-436.096844	5.855713	7.675098
-434.273923	13.809280	7.685094
-432.589715	9.043705	7.695091
-430.531498	10.889035	7.705088
-428.475569	15.025641	7.715085
-426.726009	15.477197	7.725082
-425.108174	13.428368	7.735078
-423.113531	17.456352	7.745075
-420.971186	14.567504	7.755072
-419.402564	19.817657	7.765069
-417.146879	22.926125	7.775066
-415.522514	14.841902	7.785062
-413.635413	11.752253	7.795059
-411.723096	2.352666	7.805056
-409.815908	20.369004	7.815053
-407.958747	8.865724	7.825050
-406.376226	8.000367	7.835046
-404.527917	14.884185	7.845043
-402.104819	13.445692	7.855040
-400.468992	10.336180	7.865037
-398.776823	15.007707	7.875034
-396.639646	13.212267	7.885030
-394.767810	10.393475	7.895027
-393.095489	9.719039	7.905024
-391.201945	19.423364	7.915021
-389.242183	23.188545	7.925018
-387.144584	17.883336	7.935014
-385.340426	5.084406	7.945011
-383.697315	21.895648	7.955008
-381.628477	18.642803	7.965005
-380.036091	16.801738	7.975002
-378.322080	12.070910	7.984998
-376.119241	11.790172	7.994995
-374.241848	14.483846	8.004992
-372.313536	19.725548	8.014989
-370.358316	23.456736	8.024986
-368.447844	19.051364	8.034982
-366.594707	10.872229	8.044979
-365.009052	20.737834	8.054976
-363.332236	22.418344	8.064973
-361.134462	21.622145	8.074970
-359.343217	13.007659	8.084966
-357.189874	13.450059	8.094963
-355.348825	15.251186	8.104960
-353.280396	14.534062	8.114957
-352.083652	9.655323	8.124954
-349.883596	19.174969	8.134950
-348.089587	10.285331	8.144947
-345.937152	13.615601	8.154944
-344.232255	9.899872	8.164941
-342.382820	5.404801	8.174938
-340.379533	8.092612	8.184934
-338.612781	13.735900	8.194931
-336.629115	10.692468	8.204928
-334.960338	22.663643	8.214925
-332.702066	8.167609	8.224922
-331.203360	15.565168	8.234918
-329.178303	14.952877	8.244915
-327.454764	13.975065	8.254912
-325.411103	12.235667	8.264909
-323.805335	15.692700	8.274906
-321.840092	16.390936	8.284902
-319.474941	10.713093	8.294899
-318.140974	25.203895	8.304896
-316.175191	12.953901	8.314893
-314.149082	11.106795	8.324890
-312.414590	20.811321	8.334886
-310.270771	18.484403	8.344883
-308.472493	22.352795	8.354880
-306.799523	23.623458	8.364877
-304.825908	24.290375	8.374874
-302.907567	14.340454	8.384870
-300.942549	20.766811	8.394867
-299.337464	14.686138	8.404864
-297.447690	13.809697	8.414861
-295.436927	28.303001	8.424858
-293.224568	24.332624	8.434854
-291.697475	21.300532	8.444851
-290.035821	24.104499	8.454848
-288.095968	29.718624	8.464845
-286.161815	20.711918	8.474842
-284.000036	23.718671	8.484838
-282.367922	29.735586	8.494835
-280.182627	24.189109	8.504832
-278.352631	22.332285	8.514829
-276.770506	26.937796	8.524826
-274.801151	28.625355	8.534822
-273.042089	15.397921	8.544819
-271.240597	26.223826	8.554816
-269.098752	15.660392	8.564813
-267.281670	29.928867	8.574810
-265.264250	26.468021	8.584807
-263.614498	24.518406	8.594803
-261.654285	25.643786	8.604800
-259.698768	20.437143	8.614797
-257.963179	28.366916	8.624794
-256.071808	24.763575	8.634791
-254.177523	27.825683	8.644787
-251.922727	23.183871	8.654784
-250.236908	20.818008	8.664781
-248.895035	19.517508	8.674778
-246.598800	29.509780	8.684775
-244.909811	21.219561	8.694771
-242.833226	28.005513	8.704768
-240.951998	25.384269	8.714765
-239.217419	20.506572	8.724762
-237.295200	23.328985	8.734759
-235.347555	20.793456	8.744755
-233.528784	13.600362	8.754752
-231.730399	20.156001	8.764749
-229.699463	21.592205	8.774746
-227.827086	24.083128	8.784743
-225.973808	16.294040	8.794739
-224.159597	22.341928	8.804736
-222.175764	24.167739	8.814733
-220.346984	24.172619	8.824730
-218.503005	19.591667	8.834727
-216.238956	15.369966	8.844723
-214.557187	11.256986	8.854720
-212.909123	10.392347	8.864717
-211.005274	14.646572	8.874714
-209.163826	16.556691	8.884711
-207.522031	14.251564	8.894707
-205.351498	14.580839	8.904704
-203.186178	14.273091	8.914701
-201.685930	19.169596	8.924698
-199.817236	13.130593	8.934695
-197.817369	12.088248	8.944691
-195.909583	18.078595	8.954688
-194.178865	7.694513	8.964685
-192.484333	9.219168	8.974682
-190.474193	9.965607	8.984679
-188.436236	10.336579	8.994675
-186.421795	8.343028	9.004672
-184.801273	4.342468	9.014669
-182.896388	10.109090	9.024666
-181.093645	11.133356	9.034663
-179.108292	7.974524	9.044659
-177.161774	9.700542	9.054656
-175.329249	16.040791	9.064653
-173.652908	16.046349	9.074650
-171.617990	10.377133	9.084647
-169.499008	16.082762	9.094643
-167.808267	12.795699	9.104640
-165.990039	23.814801	9.114637
-164.142709	14.102083	9.124634
-162.459106	18.053621	9.134631
-160.305270	12.911720	9.144627
-158.389446	12.471730	9.154624
-156.445782	15.311312	9.164621
-154.848931	18.282022	9.174618
-152.812330	12.964635	9.184615
-150.810651	11.505223	9.194611
-149.066791	11.580546	9.204608
-147.331703	16.387512	9.214605
-145.238883	19.367504	9.224602
-143.264176	13.529506	9.234599
-141.538833	16.032907	9.244595
-139.854545	10.798588	9.254592
-137.883207	8.958788	9.264589
-136.137318	18.500597	9.274586
-134.155372	12.951960	9.284583
-132.176673	14.824450	9.294579
-130.411367	9.796671	9.304576
-128.425382	19.132819	9.314573
-126.648060	14.392054	9.324570
-124.706327	19.650774	9.334567
-122.638702	20.841230	9.344563
-120.845186	17.468329	9.354560
-118.945044	22.026365	9.364557
-117.300896	12.976060	9.374554
-115.392113	10.658392	9.384551
-113.386421	8.904704	9.394547
-111.773083	18.398212	9.404544
-109.685535	21.641168	9.414541
-107.823030	18.389893	9.424538
-105.884669	18.132653	9.434535
-103.842177	21.016509	9.444531
-102.185785	10.893797	9.454528
-100.505805	15.415925	9.464525
-98.673821	25.449266	9.474522
-96.658639	19.532216	9.484519
-94.436587	17.073009	9.494515
-92.729108	19.381940	9.504512
-91.003828	10.718157	9.514509
-89.075846	20.426733	9.524506
-87.059258	17.515605	9.534503
-85.327941	23.155279	9.544499
-83.410156	14.051863	9.554496
-81.633876	14.278369	9.564493
-79.920951	14.729708	9.574490
-77.571436	13.645888	9.584487
-75.992499	13.296023	9.594483
-74.113834	13.313580	9.604480
-72.282501	13.843923	9.614477
-70.382136	19.140867	9.624474
-68.107312	18.477895	9.634471
-66.607903	19.646951	9.644467
-64.660454	17.607347	9.654464
-62.813233	12.692852	9.664461
-61.063214	16.281786	9.674458
-59.126155	21.511311	9.684455
-56.999550	17.224840	9.694451
-55.041887	15.897257	9.704448
-53.490553	24.616016	9.714445
-51.564233	15.574413	9.724442
-49.610037	23.310013	9.734439
-47.854730	21.613687	9.744435
-46.007151	25.117601	9.754432
-44.187823	22.321654	9.764429
-42.049202	22.315134	9.774426
-40.097001	9.944345	9.784423
-38.374903	13.299342	9.794419
-36.369174	15.745462	9.804416
-34.395788	15.638999	9.814413
-32.785303	17.429793	9.824410
-31.210235	10.250450	9.834407
-28.957926	16.474912	9.844403
-27.067383	14.269162	9.854400
-25.468293	13.802438	9.864397
-23.699028	18.482476	9.874394
-21.354878	8.632186	9.884391
-19.640664	14.476729	9.894387
-17.654592	18.880624	9.904384
-15.831385	13.265824	9.914381
-14.100843	15.372197	9.924378
-12.541667	22.780863	9.934375
-10.259380	33.230325	9.944371
-8.702871	44.750775	9.954368
-7.012761	60.332857	9.964365
-5.167178	75.114937	9.974362
-3.175223	88.144831	9.984359
-1.449696	104.250235	9.994355
0.000000	120.635183	9.999360
1.018174	136.436755	10.004365
1.112593	134.182531	10.009370
1.469174	134.858852	10.014375
1.593351	140.296485	10.019379
1.608700	147.377211	10.024384
2.038552	131.551150	10.029389
2.066380	134.452807	10.034394
2.302819	142.868548	10.039399
2.242729	146.414971	10.044403
2.396332	146.548118	10.049408
2.167472	149.269963	10.054413
2.364398	150.044286	10.059418
2.576686	143.499572	10.064423
2.252184	142.611492	10.069427
1.724650	135.123568	10.074432
2.028277	143.615319	10.079437
2.363928	141.639563	10.084442
2.653703	163.757526	10.089447
2.571327	166.701998	10.094451
2.148710	149.994821	10.099456
2.514608	146.377469	10.104461
2.393392	151.707601	10.109466
2.772451	152.700438	10.114471
2.436152	145.136277	10.119475
2.633607	147.564631	10.124480
2.844904	148.661493	10.129485
2.447000	149.743570	10.134490
3.157569	148.023382	10.139495
2.509636	152.335310	10.144499
2.993737	150.061502	10.149504
3.009499	141.785217	10.154509
2.422640	152.986123	10.159514
3.275330	140.916472	10.164519
3.183221	151.242152	10.169523
2.842562	145.373801	10.174528
3.014301	151.169681	10.179533
2.967937	164.605509	10.184538
3.413789	157.686087	10.189543
3.561783	158.955463	10.194547
3.164415	145.719646	10.199552
3.101676	144.687318	10.204557
3.396378	171.617055	10.209562
3.628031	152.919599	10.214567
3.663497	144.249109	10.219571
3.093188	150.008818	10.224576
3.532690	149.028835	10.229581
3.541342	156.437042	10.234586
3.855410	160.163470	10.239591
3.745900	160.029523	10.244595
3.558211	159.285189	10.249600
3.868089	159.541634	10.254605
3.910730	162.094027	10.259610
3.868287	172.042817	10.264615
3.854153	161.193134	10.269619
3.707876	161.530222	10.274624
4.003307	160.354036	10.279629
4.218657	157.768303	10.284634
4.322968	165.079261	10.289639
4.036687	170.101435	10.294643
3.951054	163.249440	10.299648
4.083942	160.402487	10.304653
4.292926	177.280865	10.309658
4.593005	164.154543	10.314663
4.054734	172.919362	10.319667
4.176613	180.615431	10.324672
4.754134	175.510457	10.329677
4.371991	174.797139	10.334682
4.486279	173.129484	10.339687
4.409465	181.147387	10.344691
4.847616	180.993889	10.349696
4.828648	170.102395	10.354701
4.319611	172.624521	10.359706
4.756728	182.629282	10.364711
4.773070	191.887508	10.369715
4.839642	180.275931	10.374720
5.358950	172.542167	10.379725
4.724378	168.868361	10.384730
4.785939	167.305305	10.389735
4.816028	165.553315	10.394739
5.207999	177.681410	10.399744
5.287552	172.178080	10.404749
4.642890	178.883156	10.409754
4.972998	171.813466	10.414759
5.429993	177.481861	10.419763
5.482768	189.230434	10.424768
5.233042	175.685628	10.429773
5.056737	190.832595	10.434778
5.697555	184.344081	10.439783
5.652221	183.942870	10.444787
5.233996	166.701995	10.449792
5.282289	198.743824	10.454797
5.742516	184.786165	10.459802
5.948525	176.716042	10.464807
5.424654	193.113705	10.469811
5.440559	173.575480	10.474816
6.150281	186.665239	10.479821
5.866931	190.923755	10.484826
5.719834	182.679730	10.489831
5.741235	178.136516	10.494835
5.854980	192.023042	10.499840
6.108663	175.548562	10.504845
5.690798	174.946591	10.509850
6.203065	176.657728	10.514855
6.309946	196.035959	10.519859
5.778332	167.697915	10.524864
5.924205	202.871588	10.529869
6.047002	190.768516	10.534874
6.270045	182.667289	10.539879
6.604808	188.191192	10.544883
6.311487	201.417302	10.549888
6.628628	191.907120	10.554893
6.329238	198.371064	10.559898
6.605705	198.932442	10.564903
6.634051	194.913208	10.569907
6.577316	190.918584	10.574912
6.745213	195.179238	10.579917
6.078245	198.846127	10.584922
6.615236	198.697363	10.589927
6.666537	201.633134	10.594931
6.700717	199.820568	10.599936
7.082591	192.886105	10.604941
6.872950	203.299951	10.609946
6.778550	197.452219	10.614951
7.025613	192.240687	10.619955
6.555406	193.607095	10.624960
6.572131	186.327203	10.629965
6.888455	201.378259	10.634970
7.147544	196.355607	10.639975
6.907191	200.520541	10.644979
7.114762	203.590649	10.649984
7.193497	209.149090	10.654989
6.819579	200.873429	10.659994
7.431471	197.718268	10.664999
7.751831	204.201626	10.670003
7.090837	218.448280	10.675008
7.695120	205.956178	10.680013
7.494425	197.903609	10.685018
7.468812	206.902048	10.690023
7.792318	206.162901	10.695027
7.425141	206.084244	10.700032
8.100595	218.329573	10.705037
7.892318	214.400113	10.710042
7.726168	194.514028	10.715047
7.663127	216.029222	10.720051
7.600126	205.570477	10.725056
8.010035	210.170978	10.730061
8.005678	213.967133	10.735066
8.264365	232.881257	10.740071
7.996090	198.334050	10.745075
7.723762	205.525342	10.750080
8.162167	202.549230	10.755085
8.716370	230.345958	10.760090
8.537516	205.157329	10.765095
8.227602	211.602458	10.770099
8.126685	214.401672	10.775104
8.040077	195.519972	10.780109
7.979961	215.058898	10.785114
8.665773	215.297957	10.790119
8.836258	211.959326	10.795123
8.675287	225.959085	10.800128
8.510565	203.907731	10.805133
8.108665	212.245569	10.810138
8.590494	219.583066	10.815143
8.814350	217.623556	10.820147
8.555946	238.085066	10.825152
9.105142	205.957235	10.830157
9.131228	215.183962	10.835162
8.767372	229.706488	10.840167
8.981366	219.365967	10.845171
9.145285	212.474144	10.850176
9.027569	208.809344	10.855181
8.814955	213.903356	10.860186
8.983421	227.126792	10.865191
9.487908	218.551748	10.870195
9.354130	213.443530	10.875200
8.987447	215.064646	10.880205
9.095613	225.132945	10.885210
9.183822	220.022430	10.890215
9.377968	218.887625	10.895219
9.124848	248.527204	10.900224
9.707496	217.273901	10.905229
9.645128	225.494516	10.910234
9.448747	239.134104	10.915239
9.697016	222.281988	10.920243
9.703323	228.332931	10.925248
9.966306	202.690654	10.930253
9.665304	241.045261	10.935258
9.578281	210.515340	10.940263
9.696383	233.764596	10.945267
9.663704	230.144570	10.950272
9.649742	211.667552	10.955277
9.577882	231.813888	10.960282
9.488259	234.683840	10.965287
9.566456	232.468457	10.970291
9.537006	221.499752	10.975296
9.891169	247.970746	10.980301
10.343863	245.451214	10.985306
10.293265	243.202759	10.990311
10.862935	238.986789	10.995315
10.230121	239.972307	11.000320
10.093869	230.020361	11.005325
9.951972	240.896487	11.010330
10.524366	221.502810	11.015335
10.682167	245.978857	11.020339
10.459640	251.358298	11.025344
10.775546	246.187803	11.030349
10.280950	245.205428	11.035354
10.434341	244.447684	11.040359
10.605259	245.366502	11.045363
10.607350	243.074952	11.050368
10.880972	256.554440	11.055373
10.786602	250.656221	11.060378
10.904859	246.666784	11.065383
11.143641	236.826893	11.070387
10.888320	242.791846	11.075392
10.875681	245.632176	11.080397
10.891882	250.196146	11.085402
10.729499	257.740490	11.090407
10.713955	245.342489	11.095411
10.805382	242.722894	11.100416
10.746709	247.798671	11.105421
10.909405	258.720839	11.110426
11.233034	251.671067	11.115431
11.640578	247.597642	11.120435
11.335826	259.713942	11.125440
11.503505	250.812577	11.130445
11.405205	250.869218	11.135450
11.416322	275.411287	11.140455
11.755198	263.675789	11.145459
11.495140	249.809303	11.150464
11.753116	251.398594	11.155469
11.634000	271.946739	11.160474
11.703399	242.553948	11.165479
12.029871	266.798136	11.170483
11.769321	254.904380	11.175488
11.774118	257.106455	11.180493
11.751688	262.507598	11.185498
12.200784	262.994139	11.190503
11.989837	259.416732	11.195507
11.582112	256.924056	11.200512
11.902971	256.529086	11.205517
12.103051	261.139420	11.210522
12.240619	274.538129	11.215527
12.543129	279.852759	11.220531
11.992615	256.787437	11.225536
12.131242	290.677338	11.230541
12.346923	255.693275	11.235546
12.292342	271.754414	11.240551
12.843653	263.450981	11.245555
12.595682	287.734791	11.250560
12.819606	257.448471	11.255565
12.504925	301.789616	11.260570
12.594610	283.396894	11.265575
12.711274	256.044886	11.270579
12.611244	282.044370	11.275584
12.875358	253.468854	11.280589
12.789206	284.220369	11.285594
13.073332	251.101870	11.290599
12.813391	270.199685	11.295603
12.593476	270.387681	11.300608
12.976578	262.844320	11.305613
12.774865	282.101588	11.310618
12.926616	265.419349	11.315623
12.903722	286.253348	11.320627
12.601710	280.709917	11.325632
12.783029	258.508673	11.330637
13.126288	289.240590	11.335642
13.162988	261.516570	11.340647
13.233922	294.859069	11.345651
13.040950	281.230997	11.350656
13.522498	281.657173	11.355661
12.973708	284.207733	11.360666
13.512161	280.659015	11.365671
13.944007	295.016846	11.370675
13.883728	290.248518	11.375680
13.607550	290.980046	11.380685
13.576593	265.107014	11.385690
13.377179	285.789405	11.390695
13.730694	277.659431	11.395699
13.530987	300.011789	11.400704
14.195339	289.846953	11.405709
13.870602	279.448822	11.410714
13.917276	299.219975	11.415719
14.059513	276.086701	11.420723
14.039677	316.837650	11.425728
14.257130	282.856127	11.430733
13.823417	281.673237	11.435738
13.736554	304.909571	11.440743
14.402046	289.334320	11.445747
14.362577	289.862521	11.450752
14.400585	288.393090	11.455757
14.408264	300.957881	11.460762
14.484939	297.369279	11.465767
14.670740	292.932263	11.470771
13.913658	295.587007	11.475776
14.323882	273.962630	11.480781
14.536745	308.313792	11.485786
14.704216	294.822170	11.490791
14.918188	275.936573	11.495795
14.640876	317.665250	11.500800
14.735877	283.854635	11.505805
14.299131	321.636629	11.510810
14.760132	279.549004	11.515815
14.954544	311.167255	11.520819
14.606465	290.713997	11.525824
15.016728	311.999310	11.530829
14.685770	282.790137	11.535834
14.528145	315.035372	11.540839
14.706528	280.099774	11.545843
14.529581	329.343587	11.550848
14.908758	300.751201	11.555853
15.591955	312.372516	11.560858
14.992808	312.644653	11.565863
15.481273	305.056081	11.570867
15.344268	320.788241	11.575872
15.334100	308.837159	11.580877
15.242055	325.191323	11.585882
15.432825	315.682294	11.590887
15.992666	319.025807	11.595891
15.463036	326.903138	11.600896
15.477152	281.840271	11.605901
15.579944	302.515482	11.610906
15.655904	339.293278	11.615911
16.239527	293.103534	11.620915
15.666090	324.386995	11.625920
15.510354	288.706772	11.630925
16.026359	329.008033	11.635930
15.913506	306.916710	11.640935
15.571489	334.970124	11.645939
15.493294	313.153947	11.650944
16.023121	316.552706	11.655949
15.704533	322.611357	11.660954
16.016007	341.362673	11.665959
15.983603	329.957563	11.670963
15.912719	326.524947	11.675968
16.144912	330.365400	11.680973
16.201128	323.403975	11.685978
16.429926	332.388721	11.690983
16.590308	305.091144	11.695987
15.709342	338.300159	11.700992
16.535193	294.601078	11.705997
16.524749	339.537176	11.711002
16.455220	323.002122	11.716007
16.924851	313.268853	11.721011
16.474846	342.895877	11.726016
16.851763	304.232366	11.731021
16.434211	352.204257	11.736026
17.080625	327.501916	11.741031
16.972929	340.561358	11.746035
16.604543	314.040351	11.751040
16.719283	344.848258	11.756045
17.134732	323.913643	11.761050
16.688117	345.947505	11.766055
17.340237	315.056628	11.771059
17.167138	354.783513	11.776064
16.923444	318.562185	11.781069
17.477998	354.478403	11.786074
16.975373	331.249211	11.791079
17.281277	343.714435	11.796083
17.313102	328.289097	11.801088
17.376300	357.397501	11.806093
17.383772	339.588648	11.811098
17.366619	350.496997	11.816103
17.673071	338.807609	11.821107
17.508904	334.309712	11.826112
17.668399	359.916301	11.831117
16.878996	319.445608	11.836122
17.492126	372.184044	11.841127
17.695894	344.212455	11.846131
17.742327	345.937995	11.851136
17.890333	350.897269	11.856141
17.963583	332.858747	11.861146
17.565991	371.453023	11.866151
17.911272	320.575312	11.871155
17.673434	371.230818	11.876160
17.700194	331.561847	11.881165
17.860780	354.288885	11.886170
17.730026	359.317854	11.891175
18.226453	322.494367	11.896179
17.432322	368.976314	11.901184
18.327727	331.619258	11.906189
18.406321	379.141538	11.911194
18.659365	364.899802	11.916199
17.952781	359.752012	11.921203
18.513161	332.833685	11.926208
18.441534	359.987780	11.931213
18.282519	377.144276	11.936218
18.850020	351.714926	11.941223
18.736724	359.754516	11.946227
18.477076	351.383272	11.951232
18.344363	371.654621	11.956237
18.381499	342.046011	11.961242
18.895836	381.209184	11.966247
18.991968	349.372484	11.971251
18.536188	381.600772	11.976256
18.825635	346.576338	11.981261
18.803835	393.986953	11.986266
19.083229	355.781962	11.991271
19.265142	383.024964	11.996275
18.682792	370.095971	12.001280
19.074186	346.334670	12.006285
19.043015	384.619814	12.011290
18.991002	396.785798	12.016295
19.052893	364.041515	12.021299
19.457607	340.968768	12.026304
19.355621	378.519331	12.031309
19.346584	363.627149	12.036314
18.870323	383.918620	12.041319
18.773188	368.698302	12.046323
18.888158	342.691473	12.051328
18.989020	395.757694	12.056333
19.362017	385.140971	12.061338
18.661614	358.344847	12.066343
19.188337	377.517595	12.071347
19.154780	373.995439	12.076352
19.260665	335.974285	12.081357
18.793084	387.309855	12.086362
18.463212	357.666714	12.091367
19.511371	368.770995	12.096371
18.888206	378.397834	12.101376
18.974189	343.524126	12.106381
19.104407	355.795044	12.111386
18.889783	400.737093	12.116391
19.163061	376.709166	12.121395
18.883784	351.429069	12.126400
19.107503	380.392075	12.131405
19.033655	365.489729	12.136410
18.918994	373.140056	12.141415
18.925542	362.868788	12.146419
19.138933	353.466508	12.151424
18.856037	381.545274	12.156429
19.381032	357.915601	12.161434
19.158646	392.520881	12.166439
18.726918	349.022219	12.171443
18.766353	372.399359	12.176448
19.144189	375.317775	12.181453
19.396274	350.255688	12.186458
18.804060	386.645041	12.191463
18.972594	350.681142	12.196467
19.189607	367.709845	12.201472
18.718063	375.945349	12.206477
19.214896	360.609802	12.211482
19.006349	368.109529	12.216487
19.039101	351.280599	12.221491
18.608732	367.103754	12.226496
19.287026	354.267001	12.231501
19.208420	358.849282	12.236506
18.969647	376.545174	12.241511
19.220492	359.498532	12.246515
18.762674	360.440374	12.251520
18.973248	372.493496	12.256525
18.946706	358.343666	12.261530
18.713185	382.812980	12.266535
19.529433	336.505573	12.271539
18.974998	377.032894	12.276544
18.802362	366.951045	12.281549
19.465428	346.498848	12.286554
18.756685	382.670246	12.291559
19.317861	350.869749	12.296563
18.769866	375.502744	12.301568
19.100574	346.708274	12.306573
18.979072	378.228835	12.311578
19.096110	344.178032	12.316583
19.261558	374.271476	12.321587
18.959192	355.739353	12.326592
19.184913	357.117769	12.331597
19.133651	359.552718	12.336602
19.378336	346.930204	12.341607
19.196513	383.911649	12.346611
19.071879	347.748524	12.351616
18.952182	363.030138	12.356621
19.415353	361.871336	12.361626
19.114491	352.107978	12.366631
19.153075	376.773566	12.371635
18.847669	362.847974	12.376640
19.478787	368.704707	12.381645
19.240641	344.938168	12.386650
18.742935	373.171023	12.391655
19.014015	346.335082	12.396659
19.026003	375.697684	12.401664
18.855837	363.100327	12.406669
18.785519	360.035024	12.411674
19.174330	377.015837	12.416679
19.401155	342.349891	12.421683
19.071490	389.730753	12.426688
18.428376	364.524434	12.431693
19.081343	353.232329	12.436698
18.662833	358.452267	12.441703
19.240097	367.337303	12.446707
19.227597	342.960795	12.451712
19.430848	364.881571	12.456717
19.313959	356.266792	12.461722
18.696231	338.015215	12.466727
18.800127	369.297966	12.471731
18.417451	348.460656	12.476736
18.763063	391.608719	12.481741
19.439095	372.381229	12.486746
19.594771	346.079333	12.491751
19.218631	377.943268	12.496755
18.704883	343.322905	12.501760
18.868183	369.304199	12.506765
19.164782	336.948297	12.511770
18.742901	377.966962	12.516775
19.462574	335.580884	12.521779
18.989427	375.705750	12.526784
18.635854	336.553145	12.531789
19.134849	364.590741	12.536794
19.025618	357.876451	12.541799
19.201133	342.026076	12.546803
18.534407	347.684549	12.551808
19.260989	372.167858	12.556813
19.652405	352.058588	12.561818
18.818251	343.772674	12.566823
18.685120	358.539212	12.571827
18.914502	335.956463	12.576832
18.943199	378.059109	12.581837
19.109308	348.224920	12.586842
19.133225	382.838198	12.591847
19.084816	333.073437	12.596851
18.816719	359.599736	12.601856
18.582623	340.747676	12.606861
19.514091	338.378835	12.611866
19.077453	388.249290	12.616871
19.134946	341.299680	12.621875
18.939712	372.822528	12.626880
18.493176	338.257686	12.631885
19.286696	386.536394	12.636890
18.906450	364.470285	12.641895
19.323922	346.619682	12.646899
19.065060	372.655702	12.651904
18.727974	339.211904	12.656909
19.009988	364.554544	12.661914
19.007387	350.959116	12.666919
19.075316	343.439176	12.671923
19.121960	363.259305	12.676928
18.994413	348.695108	12.681933
19.088026	335.406030	12.686938
18.826852	368.629793	12.691943
18.966242	343.678728	12.696947
18.889229	349.530134	12.701952
19.210542	375.483083	12.706957
19.239765	352.951155	12.711962
19.047280	345.936351	12.716967
18.861019	373.684315	12.721971
18.717936	348.287888	12.726976
19.106469	366.916566	12.731981
19.029344	366.799526	12.736986
18.845490	370.031447	12.741991
19.221259	376.083445	12.746995
18.992261	348.278640	12.752000
19.228737	365.279006	12.757005
19.151585	349.243430	12.762010
18.590444	333.644595	12.767015
19.132195	374.239906	12.772019
18.886297	341.350811	12.777024
19.340520	375.846556	12.782029
18.698903	358.190092	12.787034
19.172899	338.171743	12.792039
19.016939	371.569533	12.797043
18.919945	342.631987	12.802048
19.242782	357.682171	12.807053
19.294610	346.321957	12.812058
18.669770	357.261008	12.817063
19.092649	333.672892	12.822067
19.179642	359.876064	12.827072
18.860626	349.383934	12.832077
19.081948	358.655304	12.837082
19.100464	358.485165	12.842087
19.015585	346.791959	12.847091
19.022084	374.651098	12.852096
19.283591	336.540469	12.857101
19.454987	351.483920	12.862106
19.011433	371.323902	12.867111
19.597544	329.977805	12.872115
19.234878	365.978850	12.877120
19.195451	346.799280	12.882125
19.451607	363.446439	12.887130
18.701609	359.007283	12.892135
19.024288	337.467734	12.897139
19.082537	374.076565	12.902144
19.050762	364.172513	12.907149
19.013604	351.375765	12.912154
18.402104	366.656981	12.917159
19.489656	340.171772	12.922163
19.374166	378.541308	12.927168
19.115147	348.346017	12.932173
19.026955	363.769256	12.937178
18.785706	343.478647	12.942183
18.658635	356.429236	12.947187
18.779213	351.387625	12.952192
19.178406	346.500263	12.957197
19.653891	361.057772	12.962202
18.968141	339.065660	12.967207
18.762720	347.968294	12.972211
18.963055	338.705293	12.977216
18.836762	356.615021	12.982221
18.994397	338.392730	12.987226
18.867174	373.671880	12.992231
19.081497	346.898605	12.997235
19.122348	371.812969	13.002240
19.004640	363.210931	13.007245
19.496308	320.102788	13.012250
18.736701	359.685127	13.017255
18.420888	355.389598	13.022259
19.195483	341.499914	13.027264
19.143476	385.573929	13.032269
19.556610	374.297984	13.037274
18.307455	355.219895	13.042279
19.304109	322.826480	13.047283
19.365657	343.390064	13.052288
18.818196	383.172006	13.057293
18.376263	352.682622	13.062298
18.748336	353.282372	13.067303
19.579786	328.135800	13.072307
19.258376	361.780718	13.077312
19.132565	385.099084	13.082317
18.482535	358.093086	13.087322
18.712448	349.437188	13.092327
19.510255	344.572976	13.097331
19.254506	386.762014	13.102336
18.437706	365.689584	13.107341
18.952868	329.947979	13.112346
19.130210	380.075272	13.117351
18.996488	365.046865	13.122355
19.035361	351.220905	13.127360
19.318324	364.077718	13.132365
19.393440	353.035467	13.137370
19.047115	374.099367	13.142375
18.935659	349.886857	13.147379
18.930418	325.559680	13.152384
18.618042	367.615777	13.157389
19.560696	338.476148	13.162394
19.100953	369.341047	13.167399
19.024715	335.961301	13.172403
18.959562	371.719376	13.177408
18.657959	336.073339	13.182413
18.944415	358.368744	13.187418
18.816385	348.219872	13.192423
19.355782	350.644183	13.197427
19.099219	363.377325	13.202432
18.818223	357.887278	13.207437
19.092444	343.478190	13.212442
18.877930	358.792268	13.217447
19.144146	361.422572	13.222451
19.280678	343.257254	13.227456
18.978354	366.400327	13.232461
19.086960	340.214755	13.237466
18.759599	371.829635	13.242471
19.078123	333.262087	13.247475
19.081412	351.252060	13.252480
19.028043	356.880512	13.257485
18.989039	355.473818	13.262490
19.032279	337.485806	13.267495
19.170409	340.223263	13.272499
18.889800	366.065631	13.277504
18.927745	338.912092	13.282509
18.943555	357.573399	13.287514
18.948600	323.799114	13.292519
18.785885	371.113865	13.297523
19.091901	350.270780	13.302528
19.172540	362.776681	13.307533
19.426272	363.453652	13.312538
18.964784	344.175832	13.317543
19.108384	370.543451	13.322547
19.352939	331.110964	13.327552
19.079425	364.615792	13.332557
19.331678	361.394966	13.337562
19.089280	356.348173	13.342567
19.261817	362.197626	13.347571
19.399860	342.970831	13.352576
19.070261	382.886750	13.357581
18.998746	346.033946	13.362586
18.907564	367.214829	13.367591
19.296463	350.918845	13.372595
18.869393	351.920434	13.377600
18.602424	362.007665	13.382605
19.319738	339.154707	13.387610
18.470678	371.869880	13.392615
19.038051	340.498905	13.397619
18.841837	366.140164	13.402624
18.996024	334.727877	13.407629
19.142746	360.049513	13.412634
18.833062	341.556420	13.417639
18.963842	365.251699	13.422643
19.069965	346.510938	13.427648
18.753894	369.613633	13.432653
19.448916	340.026244	13.437658
18.890959	350.290759	13.442663
19.026588	356.817845	13.447667
19.133344	349.394206	13.452672
18.658600	344.064371	13.457677
18.949202	363.760438	13.462682
19.143187	332.201467	13.467687
18.889975	364.410022	13.472691
19.119463	350.260362	13.477696
18.683622	341.228133	13.482701
19.146402	349.253100	13.487706
18.626382	360.963872	13.492711
19.145637	352.167210	13.497715
19.161990	349.136969	13.502720
18.891304	348.894692	13.507725
19.286135	359.210661	13.512730
19.187286	362.545710	13.517735
19.603836	348.547556	13.522739
19.413977	342.462690	13.527744
19.226326	360.040027	13.532749
19.156305	338.110549	13.537754
18.529354	358.386598	13.542759
19.156543	349.325153	13.547763
19.297682	349.960161	13.552768
18.766334	337.094022	13.557773
19.180446	352.568012	13.562778
19.003143	359.378388	13.567783
18.812604	332.228190	13.572787
18.947778	357.859154	13.577792
19.038110	356.906469	13.582797
19.325218	346.297166	13.587802
18.806579	346.092861	13.592807
18.886361	362.353432	13.597811
19.078896	353.861181	13.602816
18.662222	346.478456	13.607821
19.218937	361.947056	13.612826
19.282013	353.186886	13.617831
18.755208	353.080073	13.622835
19.217748	338.144237	13.627840
18.809412	367.231682	13.632845
19.262945	342.620002	13.637850
18.855836	350.206581	13.642855
18.987758	369.716664	13.647859
19.084730	328.013373	13.652864
19.151534	379.896008	13.657869
18.834425	329.686861	13.662874
18.891026	362.654932	13.667879
19.177789	355.022816	13.672883
19.241620	345.119297	13.677888
18.637530	345.488411	13.682893
19.203326	347.197341	13.687898
18.894331	369.398513	13.692903
18.994110	352.905803	13.697907
19.272502	354.274242	13.702912
18.438874	366.064998	13.707917
18.941659	355.213140	13.712922
18.973243	356.113191	13.717927
18.921025	357.540669	13.722931
18.993206	364.448443	13.727936
19.069734	346.355768	13.732941
19.322998	367.383946	13.737946
19.244927	346.602127	13.742951
18.949572	377.600088	13.747955
19.286027	338.871978	13.752960
18.593965	371.866445	13.757965
19.123123	332.106302	13.762970
19.072307	376.832925	13.767975
19.118489	343.337447	13.772979
18.767273	358.309071	13.777984
19.051067	340.445106	13.782989
19.150566	369.796891	13.787994
19.249717	346.889562	13.792999
18.891884	351.016508	13.798003
18.886711	363.414678	13.803008
18.884895	349.856970	13.808013
19.257711	354.244252	13.813018
18.623406	341.468643	13.818023
19.001817	371.752031	13.823027
19.374273	338.628703	13.828032
18.865467	370.174753	13.833037
19.074882	343.473226	13.838042
18.419599	374.758813	13.843047
19.214570	344.728139	13.848051
19.329309	380.452812	13.853056
19.303246	370.486347	13.858061
18.726116	350.875320	13.863066
18.723969	357.460649	13.868071
19.128964	362.197597	13.873075
19.387056	358.723539	13.878080
18.797944	365.859786	13.883085
19.054074	349.398910	13.888090
18.956302	365.834454	13.893095
19.144600	355.168368	13.898099
18.833753	374.037909	13.903104
19.147525	356.173873	13.908109
19.225018	350.122051	13.913114
18.610301	369.047937	13.918119
19.183237	351.345988	13.923123
19.106556	351.782360	13.928128
18.638586	366.879843	13.933133
19.313041	361.087598	13.938138
19.102805	357.642510	13.943143
18.884075	367.067647	13.948147
18.950152	345.166911	13.953152
19.091479	378.662372	13.958157
18.904816	356.686818	13.963162
18.786849	365.665396	13.968167
19.330641	357.747867	13.973171
18.894670	345.229189	13.978176
18.518813	361.936154	13.983181
19.566811	358.553715	13.988186
19.405182	362.483798	13.993191
18.862680	351.786051	13.998195
19.010792	348.787289	14.003213
18.741202	350.379509	14.008231
19.348304	348.535203	14.013248
19.056490	354.412267	14.018266
18.626947	349.788929	14.023283
19.323535	351.948982	14.028301
19.327208	360.726441	14.033319
19.441609	349.896380	14.038336
18.865388	365.471397	14.043354
18.649208	337.568870	14.048371
19.193866	377.682463	14.053389
19.112357	368.587036	14.058407
19.509683	355.201573	14.063424
19.598274	377.355183	14.068442
19.259478	347.885184	14.073459
19.112574	339.913783	14.078477
19.068329	361.294268	14.083495
19.427601	349.240793	14.088512
19.743016	373.025440	14.093530
19.499576	348.463261	14.098547
18.986331	365.354146	14.103565
19.243045	359.304870	14.108583
19.682271	360.801337	14.113600
19.433777	357.366506	14.118618
19.126108	361.552141	14.123635
19.615335	363.207355	14.128653
19.545876	367.690015	14.133671
19.796480	369.674268	14.138688
19.509945	357.755249	14.143706
19.115799	349.700595	14.148723
19.730609	354.547539	14.153741
19.599125	372.190705	14.158759
19.962339	362.738089	14.163776
19.560466	351.696249	14.168794
19.191610	346.956278	14.173811
19.667509	372.478492	14.178829
19.709936	371.518539	14.183847
19.927604	365.854546	14.188864
20.003834	366.329934	14.193882
19.365045	357.927375	14.198899
19.759013	359.426341	14.203917
19.546149	371.802426	14.208935
20.048729	361.800677	14.213952
20.086377	357.058779	14.218970
19.604546	354.512078	14.223987
19.799598	356.178037	14.229005
19.840600	359.823621	14.234023
19.793285	361.366233	14.239040
19.706897	359.662422	14.244058
19.621735	365.895023	14.249075
19.850756	355.276313	14.254093
19.704254	357.713969	14.259111
20.161212	365.409362	14.264128
20.001504	359.692317	14.269146
19.936571	364.663411	14.274163
20.024987	356.470444	14.279181
20.111219	355.261286	14.284199
20.085817	360.336173	14.289216
20.290892	357.837196	14.294234
20.161693	369.567648	14.299251
20.385506	364.391832	14.304269
20.201017	363.161366	14.309287
20.134905	362.571045	14.314304
20.258541	364.688794	14.319322
19.728780	366.190393	14.324339
20.458946	354.219313	14.329357
20.096058	369.821650	14.334375
20.160288	363.988669	14.339392
20.134673	365.713418	14.344410
20.147679	365.247315	14.349427
20.192977	359.936397	14.354445
19.732295	364.528642	14.359463
19.783809	362.043146	14.364480
20.131658	356.279750	14.369498
19.955768	373.857650	14.374515
20.168012	364.168019	14.379533
20.341684	371.290469	14.384551
20.767502	380.864104	14.389568
20.839144	383.392799	14.394586
20.329428	375.336117	14.399603
19.968122	368.949730	14.404621
20.791410	390.989324	14.409639
20.847548	364.356644	14.414656
20.775938	394.137428	14.419674
20.695834	354.747054	14.424691
20.535626	371.828575	14.429709
20.290207	378.424906	14.434727
20.396203	364.412720	14.439744
20.543346	372.547599	14.444762
20.630859	393.886670	14.449779
20.888633	373.989808	14.454797
20.850456	375.156626	14.459815
20.350104	385.972694	14.464832
20.751066	373.206338	14.469850
20.482698	392.533868	14.474867
21.012034	378.732541	14.479885
21.199219	383.749936	14.484903
20.444622	375.700854	14.489920
20.721733	388.955098	14.494938
20.686711	389.014124	14.499955
21.189613	383.428885	14.504973
20.896278	384.257343	14.509991
21.288867	393.976271	14.515008
20.920068	385.467718	14.520026
20.560860	379.573295	14.525043
21.093358	378.124661	14.530061
21.271276	382.489227	14.535079
20.961869	375.830319	14.540096
20.631877	383.220278	14.545114
20.997245	394.997696	14.550131
21.271925	380.099810	14.555149
21.022526	382.929795	14.560167
20.998857	401.296615	14.565184
21.372923	383.979550	14.570202
21.234696	389.795955	14.575219
21.177676	387.673795	14.580237
21.204010	404.974113	14.585255
20.996485	397.012349	14.590272
21.126877	393.792327	14.595290
20.926006	396.564243	14.600307
20.766546	406.390105	14.605325
21.051961	397.267593	14.610343
20.312964	396.196346	14.615360
21.010783	400.179151	14.620378
21.137395	408.809629	14.625395
21.803750	402.921489	14.630413
21.704712	400.788727	14.635431
21.209273	388.237685	14.640448
21.194972	396.085329	14.645466
21.594758	405.921082	14.650483
21.372882	408.682194	14.655501
21.164778	401.596602	14.660519
21.497017	412.143054	14.665536
21.808796	423.078127	14.670554
21.580883	420.289588	14.675571
21.329430	402.965315	14.680589
21.826984	406.711106	14.685607
21.419241	402.104720	14.690624
21.680083	410.624137	14.695642
21.671391	424.666387	14.700659
21.995554	403.370063	14.705677
21.439294	403.376960	14.710695
21.069025	403.218926	14.715712
21.851259	407.880326	14.720730
21.948161	423.566670	14.725747
22.045899	415.946276	14.730765
22.183720	397.798658	14.735783
21.518819	415.471906	14.740800
21.655230	398.235197	14.745818
21.795261	404.902182	14.750835
21.938414	426.430605	14.755853
21.962061	402.495772	14.760871
22.041451	433.696435	14.765888
22.159067	399.629989	14.770906
21.439098	423.597164	14.775923
21.588491	417.303887	14.780941
22.314998	413.342337	14.785959
22.130822	416.529973	14.790976
22.029115	402.522566	14.795994
22.242862	421.175553	14.801011
22.263263	408.281122	14.806029
22.236909	408.675357	14.811047
21.534232	408.891204	14.816064
21.963544	407.054802	14.821082
21.787762	434.260216	14.826099
21.975689	407.541949	14.831117
22.049544	406.720112	14.836135
21.862420	422.947206	14.841152
22.132420	422.490443	14.846170
21.975765	425.613923	14.851187
22.019895	415.951072	14.856205
22.264083	408.071395	14.861223
22.165576	418.604766	14.866240
22.360463	408.280867	14.871258
22.096242	429.890000	14.876275
22.474329	418.729997	14.881293
22.636103	425.516206	14.886311
22.254459	422.994407	14.891328
22.522747	427.582074	14.896346
22.605192	416.193977	14.901363
22.348385	417.998074	14.906381
22.730778	418.682580	14.911399
22.471597	424.084183	14.916416
22.386716	401.725363	14.921434
22.525442	426.288532	14.926451
22.878881	431.658486	14.931469
22.768313	422.504745	14.936487
22.105771	424.354682	14.941504
22.692443	419.202760	14.946522
22.856433	431.204217	14.951539
22.859094	429.269138	14.956557
22.859451	405.111523	14.961575
22.441863	422.764209	14.966592
22.977181	426.851583	14.971610
22.514020	419.265599	14.976627
23.061930	432.437370	14.981645
22.850916	418.736788	14.986663
22.639641	429.920443	14.991680
23.210609	425.301077	14.996698
22.796155	401.467578	15.001715
22.717972	426.512036	15.006733
22.769534	428.855199	15.011751
22.932115	436.868115	15.016768
22.906037	431.946041	15.021786
23.080215	438.307179	15.026803
23.153240	444.865332	15.031821
23.335893	438.385862	15.036839
23.090130	422.230866	15.041856
22.751583	427.879485	15.046874
22.789759	444.380522	15.051891
23.038630	441.654345	15.056909
23.364274	424.241146	15.061927
23.223049	439.493631	15.066944
23.260437	436.373368	15.071962
23.491829	431.967020	15.076979
23.116296	422.632195	15.081997
23.451159	424.312038	15.087015
23.594870	436.426833	15.092032
23.350698	427.656156	15.097050
23.166216	421.510501	15.102067
22.989981	433.482863	15.107085
23.520072	424.675202	15.112103
23.038096	441.921372	15.117120
23.465495	431.969315	15.122138
23.579432	429.195456	15.127155
23.160755	420.329934	15.132173
23.199898	428.019650	15.137191
23.182202	436.113224	15.142208
23.480820	441.279589	15.147226
23.658622	431.129840	15.152243
23.272261	429.629578	15.157261
23.718225	425.837027	15.162279
23.316160	422.414091	15.167296
23.496323	436.850903	15.172314
23.532960	432.418995	15.177331
23.795676	429.533326	15.182349
23.425256	432.042885	15.187367
23.068473	423.688105	15.192384
23.697747	426.241113	15.197402
24.353586	449.774984	15.202419
23.690221	439.389771	15.207437
23.830977	433.940917	15.212455
23.701774	438.326174	15.217472
23.661008	443.414550	15.222490
24.075443	438.414349	15.227507
24.099724	439.233045	15.232525
24.091289	434.518920	15.237543
23.855053	428.417692	15.242560
23.603813	441.375624	15.247578
24.139695	440.940940	15.252595
24.164476	443.451954	15.257613
23.999581	440.689536	15.262631
23.656083	451.387835	15.267648
24.077539	454.117125	15.272666
24.273006	451.490690	15.277683
24.382494	460.356714	15.282701
24.642535	448.056317	15.287719
23.973998	438.159517	15.292736
24.093288	430.947767	15.297754
24.234172	433.877516	15.302771
23.972805	431.566169	15.307789
24.253881	425.354121	15.312807
24.159607	447.838996	15.317824
24.770087	450.711151	15.322842
24.646964	443.434250	15.327859
24.186544	441.481804	15.332877
24.097264	435.583626	15.337895
24.388946	431.670978	15.342912
24.728511	448.273371	15.347930
24.160737	448.565219	15.352947
24.216824	452.623655	15.357965
24.695072	445.228816	15.362983
24.560708	461.106228	15.368000
24.827194	456.186241	15.373018
24.770727	443.428296	15.378035
23.936282	449.796171	15.383053
24.611729	443.623451	15.388071
24.823847	448.831927	15.393088
24.660852	449.310871	15.398106
24.804563	450.407790	15.403123
24.765827	446.296181	15.408141
24.706072	436.071072	15.413159
24.755909	439.803347	15.418176
24.512276	448.580983	15.423194
24.592083	447.313074	15.428211
24.396367	449.613892	15.433229
24.959249	446.236797	15.438247
24.820249	442.197804	15.443264
24.685518	459.855751	15.448282
24.816389	453.466322	15.453299
24.842467	456.461573	15.458317
24.822979	447.677067	15.463335
25.164825	457.152475	15.468352
24.745765	451.308462	15.473370
25.261188	448.818166	15.478387
25.061903	455.300220	15.483405
25.124923	450.079241	15.488423
25.199760	446.547205	15.493440
25.012700	452.874739	15.498458
25.068322	446.618426	15.503475
24.846691	450.222560	15.508493
25.079801	449.340717	15.513511
24.841571	449.930751	15.518528
24.806244	461.470145	15.523546
25.688514	440.724904	15.528563
25.359578	457.517293	15.533581
25.446763	456.092493	15.538599
25.242279	448.410185	15.543616
24.861600	445.639715	15.548634
25.478527	459.566487	15.553651
25.539298	465.101098	15.558669
26.069236	466.337743	15.563687
25.768686	452.365148	15.568704
25.108753	458.810574	15.573722
25.385268	454.615651	15.578739
25.154478	448.829691	15.583757
25.475544	454.280315	15.588775
25.597391	452.993117	15.593792
25.806559	472.469507	15.598810
25.363945	455.778066	15.603827
25.456166	465.091967	15.608845
26.032892	472.584292	15.613863
26.138015	463.573856	15.618880
25.524923	466.395803	15.623898
25.514488	446.343440	15.628915
25.697930	475.408955	15.633933
26.067589	459.890286	15.638951
25.465054	458.962418	15.643968
25.843330	463.449193	15.648986
26.070736	460.191663	15.654003
25.955315	474.304462	15.659021
26.017512	474.005098	15.664039
25.826985	470.889722	15.669056
25.834597	471.250229	15.674074
25.610384	465.294917	15.679091
25.527091	476.038240	15.684109
25.892163	476.041318	15.689127
25.957644	467.092252	15.694144
25.977698	474.316325	15.699162
26.178456	473.474243	15.704179
26.029915	469.194543	15.709197
26.174708	466.204992	15.714215
26.324516	464.188244	15.719232
25.892440	480.509522	15.724250
26.130244	471.293894	15.729267
26.284179	455.675943	15.734285
26.190239	464.182774	15.739303
26.121961	469.319588	15.744320
25.974578	486.551766	15.749338
26.404397	452.131838	15.754355
26.257820	479.162810	15.759373
26.623153	498.365815	15.764391
26.731611	467.160142	15.769408
26.214158	470.791017	15.774426
26.169189	482.245458	15.779443
26.852143	472.063869	15.784461
26.694831	479.847862	15.789479
26.335273	469.560446	15.794496
26.355419	474.197144	15.799514
27.035003	481.367932	15.804531
26.521336	474.362496	15.809549
26.713382	473.249698	15.814567
26.944390	468.211110	15.819584
26.510934	484.170855	15.824602
26.524499	468.164761	15.829619
26.904440	488.501031	15.834637
26.871557	480.418566	15.839655
27.072545	465.758839	15.844672
26.703235	473.919525	15.849690
26.648549	467.034350	15.854707
26.659575	483.039591	15.859725
27.156767	476.344786	15.864743
27.596137	476.439822	15.869760
26.984883	474.017549	15.874778
26.748092	469.972125	15.879795
26.844747	479.917620	15.884813
26.940320	491.500647	15.889831
27.427289	475.805964	15.894848
26.759430	480.777318	15.899866
27.346641	473.616744	15.904883
27.341302	478.905528	15.909901
26.932072	485.097070	15.914919
27.335654	478.189129	15.919936
27.010742	483.980297	15.924954
27.326845	485.935246	15.929971
27.530757	491.336936	15.934989
27.397500	487.164893	15.940007
27.142878	475.847811	15.945024
26.946589	488.808031	15.950042
27.486037	481.766744	15.955059
27.558157	481.129204	15.960077
27.173158	491.016262	15.965095
27.595871	475.940527	15.970112
27.432033	497.285237	15.975130
27.620826	501.103893	15.980147
27.882698	483.590694	15.985165
27.371766	494.477735	15.990183
27.457956	474.969861	15.995200
27.654967	493.278008	16.000218
27.547764	491.264500	16.005235
27.501067	491.866454	16.010253
27.523857	496.170862	16.015271
27.546848	487.925341	16.020288
27.646525	499.414921	16.025306
27.407556	497.442875	16.030323
27.922743	490.429047	16.035341
27.737771	492.361680	16.040359
27.852029	485.432248	16.045376
27.837885	490.591893	16.050394
27.767612	481.606275	16.055411
28.359310	483.573891	16.060429
27.857223	498.199797	16.065447
27.932248	490.711961	16.070464
27.510298	484.335194	16.075482
27.587323	497.081959	16.080499
27.741490	503.158483	16.085517
28.055566	499.615015	16.090535
28.546868	495.730280	16.095552
27.929226	506.653225	16.100570
28.159567	498.953441	16.105587
28.468197	485.295743	16.110605
27.984107	500.818460	16.115623
28.455598	496.334477	16.120640
28.270370	492.532482	16.125658
27.977708	497.214360	16.130675
28.593394	494.675035	16.135693
28.521180	494.752576	16.140711
28.044584	490.349032	16.145728
27.987243	504.628758	16.150746
28.663641	499.495529	16.155763
29.091798	504.343985	16.160781
28.338887	510.813700	16.165799
28.611562	502.651031	16.170816
29.007551	504.805578	16.175834
28.265794	495.601466	16.180851
28.164389	504.394200	16.185869
28.573385	503.984472	16.190887
28.989866	494.682135	16.195904
28.767785	497.734276	16.200922
28.951095	495.169542	16.205939
28.684248	488.900154	16.210957
28.519177	492.517298	16.215975
28.724722	508.919363	16.220992
28.892539	513.908436	16.226010
28.995308	504.796114	16.231027
29.041125	506.050209	16.236045
28.561911	490.915411	16.241063
28.971385	491.005779	16.246080
28.819126	513.172848	16.251098
28.954290	505.183105	16.256115
29.370778	498.323428	16.261133
29.129114	505.328163	16.266151
28.927015	505.044213	16.271168
28.682311	503.187901	16.276186
28.927405	498.853273	16.281203
29.224705	499.914689	16.286221
29.128854	511.314354	16.291239
29.416398	505.115397	16.296256
29.172774	510.192111	16.301274
28.917133	504.087654	16.306291
29.192531	495.474715	16.311309
29.097791	505.189658	16.316327
29.216509	497.628789	16.321344
29.221912	505.009355	16.326362
29.044981	505.778358	16.331379
29.361761	503.041339	16.336397
29.069360	508.548934	16.341415
29.132990	506.080356	16.346432
29.784198	514.631947	16.351450
29.900364	512.162853	16.356467
29.902975	509.079579	16.361485
29.448806	511.099190	16.366503
29.612914	505.789716	16.371520
29.690094	504.835222	16.376538
29.347471	510.511260	16.381555
29.595289	500.826875	16.386573
30.067189	523.897899	16.391591
29.808567	496.590084	16.396608
29.494421	517.899030	16.401626
29.588375	520.918072	16.406643
30.002558	528.574764	16.411661
30.099475	518.532227	16.416679
30.213104	508.884967	16.421696
29.710717	512.934977	16.426714
29.776722	520.338915	16.431731
30.141338	519.826165	16.436749
30.198270	526.283113	16.441767
29.942280	523.153000	16.446784
30.166603	516.004672	16.451802
29.991351	517.901155	16.456819
30.378613	517.365918	16.461837
30.367476	542.459653	16.466855
30.068743	514.697350	16.471872
29.959603	503.369625	16.476890
29.947660	519.889753	16.481907
30.193155	517.400031	16.486925
30.269934	519.501684	16.491943
30.272943	521.939114	16.496960
30.434792	520.054132	16.501978
30.046255	530.391621	16.506995
30.249447	518.523333	16.512013
30.095641	533.235284	16.517031
29.975973	528.062289	16.522048
30.429553	527.459851	16.527066
30.097942	528.693930	16.532083
30.390472	514.945973	16.537101
30.892124	528.455514	16.542119
30.692206	542.007759	16.547136
30.685963	532.746081	16.552154
30.246412	526.082694	16.557171
30.843157	526.542702	16.562189
31.198446	532.818374	16.567207
30.705205	527.903143	16.572224
30.734415	528.603093	16.577242
30.852271	527.248892	16.582259
31.063462	525.304135	16.587277
30.684553	522.275416	16.592295
30.855187	535.246361	16.597312
31.261927	528.470014	16.602330
30.778650	545.194322	16.607347
31.212957	540.735131	16.612365
30.684349	534.298281	16.617383
30.895229	527.927516	16.622400
31.270646	541.667969	16.627418
30.909339	537.684852	16.632435
31.267658	527.124037	16.637453
31.445357	533.066273	16.642471
30.982656	539.431517	16.647488
31.049786	540.233948	16.652506
30.918726	535.176014	16.657523
30.887096	538.663358	16.662541
31.078025	541.703113	16.667559
31.275840	537.984716	16.672576
31.309924	534.975060	16.677594
31.087308	541.279992	16.682611
31.370855	531.347666	16.687629
31.684842	542.648958	16.692647
31.585241	535.234564	16.697664
31.635676	528.268105	16.702682
31.290165	545.660930	16.707699
31.824489	546.410867	16.712717
31.830291	533.594150	16.717735
31.510837	533.547546	16.722752
31.527274	545.029992	16.727770
31.768381	550.419482	16.732787
32.087794	553.500089	16.737805
32.032122	553.002466	16.742823
31.660067	542.032792	16.747840
31.499149	532.004630	16.752858
31.818438	549.967763	16.757875
32.375473	545.701334	16.762893
32.186543	537.703495	16.767911
31.583313	541.458168	16.772928
31.739483	539.608692	16.777946
32.137730	540.806580	16.782963
32.488684	542.633294	16.787981
32.108454	537.926529	16.792999
31.663450	550.537973	16.798016
32.142066	546.301353	16.803034
32.310510	547.899227	16.808051
32.485248	550.982462	16.813069
32.247745	543.102468	16.818087
32.050140	539.675204	16.823104
32.215990	545.202523	16.828122
32.388446	555.415952	16.833139
32.620942	551.811558	16.838157
32.571664	555.097248	16.843175
32.075565	554.503146	16.848192
32.534640	541.912973	16.853210
32.430084	545.679338	16.858227
32.580561	550.007438	16.863245
32.933749	547.228428	16.868263
32.556165	547.080994	16.873280
32.735889	541.385236	16.878298
32.443371	551.957513	16.883315
32.551182	543.780220	16.888333
32.894873	544.368671	16.893351
32.554344	541.961403	16.898368
32.927172	541.263316	16.903386
32.791606	555.275598	16.908403
32.728968	550.637713	16.913421
33.023510	548.544392	16.918439
32.890730	554.661986	16.923456
33.062180	550.480647	16.928474
32.937753	553.739000	16.933491
32.838450	547.096833	16.938509
33.133132	550.914343	16.943527
32.726908	553.748925	16.948544
33.045882	547.702224	16.953562
32.908316	546.374604	16.958579
32.758653	551.131209	16.963597
32.819614	546.586859	16.968615
32.602931	559.819356	16.973632
33.336275	551.715306	16.978650
33.343542	559.946527	16.983667
33.133439	563.207537	16.988685
33.288331	562.072347	16.993703
33.645356	569.401583	16.998720
33.665205	552.447523	17.003738
33.330108	560.174979	17.008755
33.296613	562.814847	17.013773
33.500072	562.794943	17.018791
33.915984	562.951919	17.023808
33.789692	561.686987	17.028826
33.471164	560.229367	17.033843
33.476884	554.885368	17.038861
33.766795	554.913017	17.043879
33.284140	569.457252	17.048896
34.102891	560.538983	17.053914
33.849828	562.759310	17.058931
33.639903	555.952329	17.063949
34.065219	559.006610	17.068967
33.693240	561.384317	17.073984
33.621772	565.225626	17.079002
33.857694	563.780239	17.084019
34.081023	566.720460	17.089037
34.492815	559.652311	17.094055
33.743755	574.935824	17.099072
33.864472	576.597937	17.104090
33.924974	571.525166	17.109107
33.948474	566.183045	17.114125
34.153078	552.184834	17.119143
33.989422	568.342288	17.124160
34.334154	562.461344	17.129178
34.316365	565.795491	17.134195
33.936932	570.892314	17.139213
34.294023	575.676632	17.144231
33.851095	577.784113	17.149248
33.874790	562.350398	17.154266
34.155493	581.228846	17.159283
34.195129	583.278236	17.164301
34.631798	576.481364	17.169319
34.802194	592.270992	17.174336
34.725689	582.924542	17.179354
34.475387	584.633248	17.184371
34.281870	577.457159	17.189389
34.551541	568.966201	17.194407
34.901842	585.263478	17.199424
35.217416	579.478404	17.204442
34.636727	573.551589	17.209459
34.498074	575.093063	17.214477
35.006609	584.323342	17.219495
35.065689	586.303570	17.224512
34.952148	577.963380	17.229530
34.789812	570.077674	17.234547
34.727408	576.103836	17.239565
35.255381	580.376456	17.244583
34.889698	597.701781	17.249600
34.857095	598.988840	17.254618
35.732434	593.745206	17.259635
34.873637	591.592032	17.264653
35.000129	574.707445	17.269671
35.155653	589.763336	17.274688
35.367575	573.252053	17.279706
35.425305	578.502503	17.284723
35.324839	593.213872	17.289741
35.579859	587.329924	17.294759
35.095646	593.201593	17.299776
35.299633	583.815125	17.304794
35.504298	585.646304	17.309811
35.084203	593.566642	17.314829
35.221994	596.301882	17.319847
35.471445	591.507252	17.324864
35.472491	590.796108	17.329882
35.412246	592.326651	17.334899
35.158765	586.604023	17.339917
35.506777	590.453933	17.344935
35.367492	601.524001	17.349952
35.496186	591.102000	17.354970
35.882593	585.763334	17.359987
35.585746	589.412529	17.365005
35.982745	598.641731	17.370023
35.833189	587.310948	17.375040
36.196856	600.507544	17.380058
35.837249	591.478350	17.385075
35.640920	593.456847	17.390093
36.151577	593.354917	17.395111
36.380222	595.594366	17.400128
36.104825	592.459468	17.405146
35.969613	592.460549	17.410163
35.825869	602.938355	17.415181
36.453314	592.438380	17.420199
36.550958	598.446889	17.425216
36.247442	599.950172	17.430234
35.975886	589.771317	17.435251
35.920603	598.479681	17.440269
36.460281	593.596294	17.445287
36.545969	592.001849	17.450304
36.631949	599.762831	17.455322
36.551892	600.695696	17.460339
36.718644	596.291745	17.465357
36.480983	591.088787	17.470375
36.760755	588.118578	17.475392
36.468341	588.721977	17.480410
36.446987	590.109477	17.485427
36.495417	602.104343	17.490445
36.585178	591.889880	17.495463
36.666119	597.488959	17.500480
36.725870	594.780335	17.505498
36.945579	599.539386	17.510515
36.806920	585.166495	17.515533
36.686551	609.212932	17.520551
36.938180	599.899072	17.525568
36.678024	595.712633	17.530586
37.066357	598.483412	17.535603
36.615406	595.587278	17.540621
36.795420	598.034240	17.545639
36.535303	604.810752	17.550656
37.075619	611.211091	17.555674
37.747938	611.106970	17.560691
37.312060	603.739882	17.565709
37.195984	601.686878	17.570727
37.135809	599.436213	17.575744
36.953262	612.370758	17.580762
37.299579	605.324040	17.585779
37.465297	614.736419	17.590797
38.114127	606.136207	17.595815
37.604654	597.607493	17.600832
36.913089	589.431838	17.605850
37.494973	600.209150	17.610867
37.548688	617.667364	17.615885
37.720061	607.490206	17.620903
37.943998	608.295943	17.625920
37.317725	606.509910	17.630938
37.729779	595.386822	17.635955
37.665314	605.759186	17.640973
37.890063	613.905419	17.645991
37.863874	611.595854	17.651008
37.748421	615.945940	17.656026
37.816587	609.061549	17.661043
37.740766	614.595983	17.666061
37.803036	608.071150	17.671079
37.655151	606.451041	17.676096
37.811855	607.478267	17.681114
38.175187	607.719129	17.686131
38.043514	610.926745	17.691149
37.934952	607.285507	17.696167
37.970218	604.936256	17.701184
37.885623	609.069080	17.706202
38.219858	603.186648	17.711219
38.012105	605.324257	17.716237
38.510691	616.177781	17.721255
37.944503	613.974788	17.726272
38.238884	632.962798	17.731290
38.611857	624.722721	17.736307
38.902892	619.389816	17.741325
38.780605	630.419446	17.746343
38.697912	609.624969	17.751360
37.989968	616.460329	17.756378
38.502799	613.078599	17.761395
38.650103	618.552282	17.766413
39.069175	622.518271	17.771431
39.269512	622.344723	17.776448
38.605792	619.727888	17.781466
38.559975	611.642694	17.786483
38.611641	616.286993	17.791501
39.163969	616.747800	17.796519
39.070093	622.694066	17.801536
39.191351	628.442442	17.806554
39.486701	622.698326	17.811571
38.769791	618.617759	17.816589
38.537318	614.120187	17.821607
38.848066	619.333444	17.826624
39.203356	620.742665	17.831642
39.453290	609.105926	17.836659
39.356815	618.989521	17.841677
39.447598	619.476754	17.846695
39.512352	611.638168	17.851712
39.396887	612.331312	17.856730
39.609173	614.872220	17.861747
39.149704	624.870337	17.866765
39.094543	617.470833	17.871783
39.429144	613.488377	17.876800
39.443006	616.627169	17.881818
39.554609	607.612464	17.886835
39.365398	617.167961	17.891853
39.200879	622.378375	17.896871
39.473721	620.120207	17.901888
39.620392	622.879202	17.906906
39.906857	612.229122	17.911923
39.772816	615.347463	17.916941
39.414936	623.279914	17.921959
39.835965	616.938508	17.926976
39.435535	620.759946	17.931994
39.978696	620.418473	17.937011
40.345553	621.453078	17.942029
40.020421	633.650682	17.947047
40.146514	621.052207	17.952064
39.870238	637.606765	17.957082
40.299123	629.161158	17.962099
40.259840	645.465588	17.967117
40.318004	628.019307	17.972135
40.419395	628.355425	17.977152
40.101782	638.958506	17.982170
40.394727	627.063231	17.987187
40.300561	635.897358	17.992205
40.597898	639.392028	17.997223
40.895014	627.302624	18.002240
40.088143	618.676624	18.007258
40.257451	623.879410	18.012275
40.620861	632.587078	18.017293
40.581107	641.031892	18.022311
40.839332	633.981909	18.027328
40.533012	639.719840	18.032346
40.982823	631.414027	18.037363
40.906265	633.164235	18.042381
40.330171	648.402935	18.047399
40.522268	632.549065	18.052416
40.350756	639.780181	18.057434
40.623479	636.480782	18.062451
40.522755	631.982640	18.067469
41.071694	641.264709	18.072487
41.682043	643.232522	18.077504
41.006429	643.922205	18.082522
40.871142	625.657424	18.087539
40.867958	638.703372	18.092557
40.944025	649.242100	18.097575
41.638321	640.364081	18.102592
41.587039	643.005228	18.107610
41.785131	637.666693	18.112627
41.300387	635.735398	18.117645
40.947330	631.455236	18.122663
41.520449	628.598667	18.127680
41.712948	642.755321	18.132698
41.753371	644.840771	18.137715
41.362822	642.254288	18.142733
41.113569	632.557866	18.147751
41.860424	634.672205	18.152768
41.746678	643.778422	18.157786
42.009500	644.463139	18.162803
41.840299	648.189509	18.167821
41.358227	637.311231	18.172839
41.930394	646.919905	18.177856
41.599652	636.995825	18.182874
41.960104	636.719669	18.187891
42.064026	634.445972	18.192909
42.016507	647.308681	18.197927
41.977174	644.093653	18.202944
42.093432	651.297753	18.207962
41.749790	636.424295	18.212979
41.838197	636.839554	18.217997
41.862428	648.761248	18.223015
41.959474	644.660956	18.228032
41.796540	658.487384	18.233050
42.269504	659.196784	18.238067
42.634708	659.070866	18.243085
42.657489	656.044113	18.248103
42.395704	651.859489	18.253120
42.542230	653.619733	18.258138
42.931708	658.356447	18.263155
42.464246	653.503120	18.268173
42.039317	656.466534	18.273191
42.681973	652.356292	18.278208
42.748016	668.286905	18.283226
43.205257	658.531265	18.288243
43.231393	646.749308	18.293261
42.423055	666.042210	18.298279
42.954135	652.183724	18.303296
43.048388	657.214466	18.308314
42.816155	659.689438	18.313331
43.117265	650.128576	18.318349
42.999283	658.304331	18.323367
43.492339	671.442609	18.328384
42.920222	656.144713	18.333402
43.020977	639.076982	18.338419
43.047218	654.078063	18.343437
43.027513	667.661453	18.348455
43.311785	655.445097	18.353472
43.041425	659.351183	18.358490
42.996531	655.989189	18.363507
43.267911	658.407433	18.368525
42.957780	660.113106	18.373543
43.210420	652.958621	18.378560
43.369559	674.799447	18.383578
43.770371	678.288635	18.388595
44.257762	664.498448	18.393613
43.459756	679.149710	18.398631
43.558834	662.175020	18.403648
43.869452	665.153246	18.408666
43.910341	664.084990	18.413683
44.139449	660.745355	18.418701
43.903051	668.304556	18.423719
43.943188	653.678157	18.428736
43.864783	659.448953	18.433754
43.669140	670.167872	18.438771
44.118847	662.036649	18.443789
44.003310	673.853250	18.448807
44.536317	659.533595	18.453824
44.565231	660.688162	18.458842
43.694001	658.911303	18.463859
43.934541	656.622106	18.468877
43.829896	682.553618	18.473895
44.257729	676.947213	18.478912
44.464030	671.423329	18.483930
44.249199	664.673701	18.488947
44.613120	668.950494	18.493965
44.439388	670.963147	18.498983
44.766111	666.690950	18.504000
44.664888	666.617402	18.509018
44.478099	673.717276	18.514035
44.639249	665.570730	18.519053
44.559502	666.025393	18.524071
44.804177	664.820825	18.529088
44.900844	677.218584	18.534106
44.600491	669.002508	18.539123
44.984150	660.520056	18.544141
44.598411	677.574993	18.549159
44.543407	660.135712	18.554176
44.591757	677.156020	18.559194
45.022407	678.306286	18.564211
45.644710	675.663642	18.569229
45.666355	690.281709	18.574247
45.314720	678.931177	18.579264
45.325509	664.682221	18.584282
45.173379	660.907930	18.589299
45.432114	665.344631	18.594317
45.375903	682.801582	18.599335
45.555657	667.289387	18.604352
45.711689	658.325761	18.609370
45.106750	680.496078	18.614387
45.626766	672.394531	18.619405
45.646609	678.720623	18.624423
45.871158	677.393433	18.629440
45.869886	672.846386	18.634458
45.728431	687.188469	18.639475
46.080291	681.576877	18.644493
45.644307	685.350523	18.649511
45.771312	677.501973	18.654528
45.987173	689.339660	18.659546
45.904106	675.226774	18.664563
46.231689	679.454315	18.669581
45.845814	674.665040	18.674599
46.280037	665.510763	18.679616
46.498703	680.448151	18.684634
45.955749	696.877010	18.689651
46.236541	672.796902	18.694669
45.933802	684.111734	18.699687
46.072826	684.997080	18.704704
46.465155	678.082977	18.709722
46.156266	687.692210	18.714739
46.593028	688.163588	18.719757
46.286688	695.136261	18.724775
46.121012	682.491466	18.729792
46.327377	678.100047	18.734810
46.274694	687.761219	18.739827
46.614004	680.345955	18.744845
46.416458	696.390992	18.749863
47.179668	693.368826	18.754880
47.216338	701.144020	18.759898
47.155287	692.864598	18.764915
47.236050	695.069453	18.769933
46.806532	684.140288	18.774951
46.598919	686.045099	18.779968
46.932770	683.228254	18.784986
47.071099	690.067089	18.790003
47.161801	695.584434	18.795021
47.054534	699.766513	18.800039
47.539040	703.836912	18.805056
47.350917	689.682570	18.810074
47.297904	703.516677	18.815091
47.582649	696.721961	18.820109
47.100291	692.368028	18.825127
47.483731	698.925551	18.830144
47.727972	693.486835	18.835162
47.330617	703.635533	18.840179
47.580769	700.262648	18.845197
47.639034	702.263471	18.850215
47.379400	699.703284	18.855232
47.492200	690.109513	18.860250
47.374540	690.442819	18.865267
47.750518	693.610385	18.870285
47.602378	697.257909	18.875303
47.306278	698.509929	18.880320
48.060998	699.784675	18.885338
48.189890	730.723284	18.890355
48.464719	704.660657	18.895373
48.384819	700.445438	18.900391
47.740250	698.135390	18.905408
48.050490	698.027677	18.910426
48.325250	697.790354	18.915443
48.649960	708.830544	18.920461
48.669368	715.815762	18.925479
48.355142	700.435793	18.930496
48.721150	686.870992	18.935514
48.252195	701.394298	18.940531
48.375583	695.355138	18.945549
48.502323	707.509048	18.950567
48.375490	713.164903	18.955584
48.554520	718.352018	18.960602
48.566682	711.820974	18.965619
48.764552	714.181745	18.970637
48.656171	712.701602	18.975655
48.443954	705.655834	18.980672
48.731837	711.256557	18.985690
48.485939	714.825303	18.990707
48.571840	719.044215	18.995725
48.931759	723.279195	19.000743
49.265350	725.764602	19.005760
49.714642	714.615037	19.010778
49.393413	723.313986	19.015795
48.698922	706.003377	19.020813
49.341357	719.426163	19.025831
49.298043	725.913346	19.030848
49.847508	723.431736	19.035866
49.731153	725.458838	19.040883
49.237195	709.273891	19.045901
49.330098	709.007375	19.050919
49.593193	727.673341	19.055936
49.659214	724.046697	19.060954
49.548259	728.915154	19.065971
49.554705	713.897697	19.070989
49.888582	719.626357	19.076007
49.791021	727.471733	19.081024
49.798875	727.467298	19.086042
49.733744	732.716952	19.091059
49.980421	738.291227	19.096077
50.030794	711.833412	19.101095
50.114868	724.945740	19.106112
50.372291	722.814275	19.111130
50.114863	738.947554	19.116147
49.852356	712.563232	19.121165
49.963618	715.101397	19.126183
49.900195	732.460467	19.131200
50.287626	724.409922	19.136218
50.032462	727.316389	19.141235
50.594885	735.827228	19.146253
51.108246	753.762814	19.151271
50.800620	739.397839	19.156288
50.362028	723.826911	19.161306
50.521220	734.580514	19.166323
50.752190	745.583778	19.171341
51.043509	726.390456	19.176359
50.843873	743.143680	19.181376
51.157894	728.745633	19.186394
50.626080	724.593043	19.191411
51.069170	737.545887	19.196429
51.378506	733.921330	19.201447
50.971585	731.600113	19.206464
51.308064	712.571053	19.211482
50.894431	722.870212	19.216499
51.042442	732.192692	19.221517
51.424303	742.385442	19.226535
51.434050	739.514893	19.231552
51.683839	734.254587	19.236570
51.686483	729.897217	19.241587
51.195799	733.236043	19.246605
51.279991	736.373082	19.251623
51.428131	730.803400	19.256640
51.489599	718.155377	19.261658
51.507861	741.575936	19.266675
51.452418	726.020970	19.271693
51.958129	729.833187	19.276711
51.464525	738.819163	19.281728
51.661531	720.449358	19.286746
51.625622	734.087301	19.291763
51.642231	725.718403	19.296781
51.973745	726.461377	19.301799
51.943998	734.437502	19.306816
52.050962	734.917439	19.311834
51.983489	727.791951	19.316851
51.995484	723.963156	19.321869
52.466398	747.431073	19.326887
52.337944	743.291219	19.331904
52.554086	742.471836	19.336922
52.493048	734.168794	19.341939
52.176583	757.686805	19.346957
52.644945	731.132406	19.351975
52.430816	750.244142	19.356992
52.495192	747.887080	19.362010
52.685846	746.494510	19.367027
52.500174	735.962107	19.372045
52.720518	743.475242	19.377063
52.949796	743.575480	19.382080
52.695923	720.022548	19.387098
52.437875	760.361190	19.392115
52.662625	736.702012	19.397133
52.727114	730.499212	19.402151
53.102384	748.236611	19.407168
53.571596	757.142969	19.412186
53.099217	746.208009	19.417203
53.096557	736.413989	19.422221
53.532206	754.530271	19.427239
53.234049	750.304231	19.432256
53.552924	765.304371	19.437274
53.792011	741.971633	19.442291
53.282042	747.572213	19.447309
53.962706	750.873655	19.452327
53.334264	740.009202	19.457344
53.713413	764.119367	19.462362
53.742100	736.225766	19.467379
53.673797	751.177538	19.472397
53.900561	746.517027	19.477415
53.848154	758.205663	19.482432
53.961996	765.413352	19.487450
54.194598	738.434109	19.492467
53.762230	764.858448	19.497485
54.050925	754.549226	19.502503
53.755728	755.635952	19.507520
53.913310	738.213003	19.512538
53.779330	744.892392	19.517555
53.837594	749.348508	19.522573
53.781223	752.345961	19.527591
54.568719	767.708631	19.532608
54.451324	787.226524	19.537626
54.932867	755.410208	19.542643
54.634204	776.443382	19.547661
54.742711	751.316331	19.552679
54.345295	749.276716	19.557696
54.414850	764.794779	19.562714
55.019327	745.136244	19.567731
55.039138	758.861271	19.572749
55.278252	771.011470	19.577767
54.855937	745.453177	19.582784
54.620481	758.905909	19.587802
55.082320	748.370893	19.592819
55.024678	771.665193	19.597837
55.360503	762.215115	19.602855
55.210470	761.369195	19.607872
55.056468	786.135387	19.612890
55.393636	759.952615	19.617907
55.078872	763.735259	19.622925
55.420962	766.840612	19.627943
55.110288	753.402545	19.632960
55.322299	764.973517	19.637978
55.394508	781.371996	19.642995
55.516570	741.831918	19.648013
55.497125	763.594407	19.653031
55.319061	757.450726	19.658048
56.091784	746.218098	19.663066
55.972780	776.746496	19.668083
55.659047	767.941086	19.673101
56.111844	758.864006	19.678119
56.333115	783.353284	19.683136
55.912705	742.655557	19.688154
56.300060	772.717831	19.693171
56.097454	769.462753	19.698189
56.049593	777.937253	19.703207
56.249815	786.551503	19.708224
56.361983	763.227962	19.713242
56.281465	788.111415	19.718259
56.369278	784.542623	19.723277
56.334131	761.505253	19.728295
56.459151	772.602508	19.733312
56.435590	795.701090	19.738330
56.799509	774.311370	19.743347
56.489130	771.444682	19.748365
56.516770	778.208413	19.753383
56.648155	780.886515	19.758400
56.773265	767.350621	19.763418
57.065404	792.251721	19.768435
56.955794	786.499773	19.773453
57.319584	782.454421	19.778471
57.136385	784.087957	19.783488
57.101573	781.364494	19.788506
57.646540	777.175427	19.793523
57.256083	775.601849	19.798541
56.818053	772.618677	19.803559
57.279899	780.458229	19.808576
57.637544	778.376835	19.813594
57.727236	791.559109	19.818611
57.662085	787.034796	19.823629
57.747533	784.600441	19.828647
58.007353	783.758362	19.833664
57.232882	777.322857	19.838682
57.858731	788.993002	19.843699
58.099057	771.143145	19.848717
57.797167	794.605413	19.853735
57.999546	775.457668	19.858752
57.917810	778.913739	19.863770
58.237055	783.573617	19.868787
57.854759	797.803222	19.873805
57.974893	783.234712	19.878823
57.945166	778.929676	19.883840
57.859303	793.538256	19.888858
58.027253	780.012820	19.893875
57.872403	780.336330	19.898893
58.257695	790.261176	19.903911
58.675165	795.528260	19.908928
58.758630	798.549035	19.913946
59.134693	797.963674	19.918963
58.823739	793.510018	19.923981
58.343837	784.145980	19.928999
58.692734	784.299495	19.934016
58.658763	804.798180	19.939034
59.131509	808.381314	19.944051
58.893777	804.446045	19.949069
59.008346	799.536017	19.954087
59.103930	807.468601	19.959104
58.995094	807.888584	19.964122
59.103035	795.873251	19.969139
59.010511	800.974727	19.974157
58.906495	794.092542	19.979175
59.266273	797.360235	19.984192
59.089281	809.182031	19.989210
59.774819	808.819425	19.994227
59.679595	813.112866	19.999245
59.602072	806.509571	20.004263
59.888909	811.283157	20.009280
59.662611	807.171471	20.014298
60.075161	800.301273	20.019315
59.892676	820.444596	20.024333
59.774666	802.917669	20.029351
60.286385	805.025499	20.034368
60.114844	811.037707	20.039386
60.070927	801.284826	20.044403
60.358040	804.417831	20.049421
60.390688	810.943270	20.054439
60.081601	802.431230	20.059456
59.774706	812.647367	20.064474
60.363921	796.550673	20.069491
60.347754	808.445912	20.074509
60.406426	801.264092	20.079527
60.733214	800.628392	20.084544
60.482555	823.624823	20.089562
60.823635	812.358746	20.094579
60.296388	808.575032	20.099597
60.293150	809.454763	20.104615
60.450449	805.947238	20.109632
60.547102	812.261139	20.114650
61.293347	820.369937	20.119667
60.917517	828.464224	20.124685
61.507221	817.759341	20.129703
61.286580	814.870468	20.134720
60.651284	824.135476	20.139738
61.322140	815.408947	20.144755
61.377714	825.170915	20.149773
61.693159	819.676755	20.154791
61.842278	823.665410	20.159808
61.516446	811.121540	20.164826
61.701549	813.259440	20.169843
61.658425	825.577384	20.174861
61.581447	821.820950	20.179879
61.827350	799.205848	20.184896
61.647668	815.100316	20.189914
61.982558	815.666593	20.194931
62.238463	815.869544	20.199949
61.691441	812.642643	20.204967
61.991226	814.952575	20.209984
62.012811	811.293673	20.215002
62.000830	816.847889	20.220019
61.637182	823.628430	20.225037
61.919271	817.230454	20.230055
62.465334	807.735808	20.235072
62.275858	816.420091	20.240090
62.285425	830.969449	20.245107
62.963929	833.940948	20.250125
62.934070	832.284687	20.255143
62.833755	821.015071	20.260160
62.456252	819.389088	20.265178
62.689991	832.354960	20.270195
62.879164	835.676611	20.275213
63.204330	839.958066	20.280231
63.287412	823.965654	20.285248
62.808332	834.154215	20.290266
63.101449	830.648617	20.295283
63.214759	833.774743	20.300301
63.166571	835.391471	20.305319
63.387091	826.743048	20.310336
63.264761	832.904707	20.315354
63.480940	827.157409	20.320371
63.164509	828.536940	20.325389
63.030199	835.702450	20.330407
63.111128	826.646885	20.335424
63.143133	831.698627	20.340442
63.812739	843.258029	20.345459
63.968786	850.227814	20.350477
64.287245	856.100552	20.355495
63.867286	836.726385	20.360512
63.417452	845.471083	20.365530
63.900558	843.182496	20.370547
64.056002	848.615648	20.375565
63.872831	859.991766	20.380583
64.381057	838.018982	20.385600
64.213915	844.706851	20.390618
64.323369	848.778911	20.395635
64.092656	846.443728	20.400653
64.320038	844.548254	20.405671
64.675227	832.743551	20.410688
64.257247	842.216139	20.415706
64.353105	846.063868	20.420723
64.473090	846.428485	20.425741
64.750103	842.829505	20.430759
65.116312	874.350304	20.435776
65.331939	865.770272	20.440794
64.682066	838.294551	20.445811
65.223060	853.647871	20.450829
64.864009	851.001271	20.455847
65.163711	846.099452	20.460864
65.459275	863.391992	20.465882
65.452899	858.002621	20.470899
65.512129	857.327799	20.475917
65.586689	861.598895	20.480935
65.730224	855.682288	20.485952
65.284483	845.965147	20.490970
65.555150	847.085894	20.495987
65.666950	852.503988	20.501005
65.685896	838.145027	20.506023
65.738783	858.106159	20.511040
65.686476	865.961695	20.516058
65.608180	867.874217	20.521075
65.950719	848.291921	20.526093
65.513361	854.046114	20.531111
65.745767	864.141675	20.536128
66.269173	870.626626	20.541146
66.607241	863.946016	20.546163
66.721423	865.757060	20.551181
66.472622	863.873037	20.556199
66.419571	853.258052	20.561216
66.269778	865.503386	20.566234
66.723697	868.255899	20.571251
67.376926	859.335543	20.576269
66.605384	856.951338	20.581287
66.739815	846.454312	20.586304
66.736672	863.114995	20.591322
66.997162	869.858936	20.596339
67.178284	864.567067	20.601357
67.122124	867.235772	20.606375
67.385597	863.336948	20.611392
67.409479	878.247412	20.616410
67.004417	869.360556	20.621427
67.356403	857.518593	20.626445
67.172326	872.710736	20.631463
67.480810	866.759953	20.636480
67.462304	863.824678	20.641498
67.455567	870.007240	20.646515
67.411230	874.360218	20.651533
67.718834	863.620073	20.656551
67.605664	869.371331	20.661568
67.650012	863.072593	20.666586
67.298825	869.325817	20.671603
67.582678	860.272473	20.676621
68.186965	877.739149	20.681639
68.460548	880.575477	20.686656
67.791397	881.061227	20.691674
68.098297	875.061933	20.696691
68.502370	876.177136	20.701709
68.465246	895.325325	20.706727
68.766672	876.800252	20.711744
68.667739	879.353094	20.716762
68.546829	883.356517	20.721779
68.872748	868.143241	20.726797
68.692916	867.100734	20.731815
68.650973	883.751900	20.736832
68.869452	869.633199	20.741850
68.721946	882.085807	20.746867
68.911680	882.121573	20.751885
68.690274	874.248263	20.756903
68.927650	869.471198	20.761920
68.837168	877.593931	20.766938
68.694167	873.420181	20.771955
69.208663	877.498435	20.776973
69.193924	884.778597	20.781991
69.501214	906.369654	20.787008
69.818028	906.180676	20.792026
69.423304	890.192036	20.797043
69.777733	894.258073	20.802061
69.558056	905.811495	20.807079
69.835763	895.054074	20.812096
69.713134	889.409545	20.817114
69.584415	894.219547	20.822131
69.764732	886.475631	20.827149
69.506114	901.907764	20.832167
70.095584	911.216584	20.837184
70.714713	898.864830	20.842202
70.684505	903.858884	20.847219
70.571172	896.378855	20.852237
70.050909	883.178567	20.857255
70.672963	885.993926	20.862272
71.140258	886.877268	20.867290
70.603174	889.359998	20.872307
70.619443	880.283253	20.877325
70.727317	883.081520	20.882343
70.752633	890.921545	20.887360
71.332894	900.716283	20.892378
71.119993	882.399059	20.897395
70.911665	884.104248	20.902413
71.274589	897.354723	20.907431
71.168801	883.342775	20.912448
71.489847	884.096867	20.917466
70.867928	885.268737	20.922483
70.924332	880.305041	20.927501
71.048326	890.529588	20.932519
71.331027	890.583560	20.937536
71.426729	884.875901	20.942554
71.580340	890.650684	20.947571
71.511598	884.206389	20.952589
71.591069	890.842367	20.957607
71.724914	905.741615	20.962624
72.608230	892.462185	20.967642
72.106959	900.697631	20.972659
72.055316	897.745612	20.977677
72.138572	886.396335	20.982695
72.280319	906.473915	20.987712
72.592949	904.059935	20.992730
72.256748	893.710283	20.997747
72.655967	894.848283	21.002765
72.308736	904.886887	21.007783
72.788794	904.816583	21.012800
72.703282	889.480149	21.017818
72.497840	926.007573	21.022835
72.889621	909.017368	21.027853
72.787374	910.461841	21.032871
72.935022	901.999588	21.037888
72.923505	903.173206	21.042906
72.668383	910.850341	21.047923
72.923100	912.884354	21.052941
72.958606	913.860152	21.057959
73.052371	909.865694	21.062976
73.751554	898.740628	21.067994
73.448008	909.958243	21.073011
73.709220	910.729744	21.078029
73.379890	919.365611	21.083047
73.751630	911.919893	21.088064
74.019704	912.095739	21.093082
73.899973	908.179371	21.098099
74.269127	907.104361	21.103117
74.079943	911.645606	21.108135
73.810788	908.729846	21.113152
73.810894	921.692164	21.118170
73.781530	903.358226	21.123187
73.710653	917.296055	21.128205
73.925385	897.842606	21.133223
74.045379	906.781161	21.138240
74.185913	927.475546	21.143258
74.516020	920.637316	21.148275
74.060813	915.418595	21.153293
74.679943	932.492891	21.158311
74.833472	923.697801	21.163328
74.973773	923.920764	21.168346
74.631590	923.851037	21.173363
74.973579	913.712516	21.178381
74.961198	907.619420	21.183399
74.991627	917.514440	21.188416
75.306425	921.626128	21.193434
75.012796	916.587690	21.198451
75.705845	931.923139	21.203469
75.623265	923.165704	21.208487
75.299388	938.232357	21.213504
75.540844	934.642171	21.218522
75.528884	931.587869	21.223539
76.153395	936.845585	21.228557
76.266386	931.898014	21.233575
75.828196	932.735440	21.238592
75.738623	918.648516	21.243610
75.543125	908.252821	21.248627
76.026071	943.025241	21.253645
76.169682	910.059195	21.258663
75.888955	954.071603	21.263680
76.352837	916.054167	21.268698
76.111983	932.727674	21.273715
75.975563	935.720628	21.278733
76.472418	932.270599	21.283751
76.718027	930.966770	21.288768
77.246120	934.092834	21.293786
76.601102	954.294378	21.298803
76.896691	923.816013	21.303821
76.973233	925.093558	21.308839
77.121678	957.081822	21.313856
77.641141	937.759034	21.318874
76.961753	934.082909	21.323891
77.156971	934.404073	21.328909
77.219800	939.309375	21.333927
77.426240	943.454080	21.338944
77.815178	960.193911	21.343962
77.598538	948.750849	21.348979
77.611966	937.854657	21.353997
77.526249	952.224292	21.359015
77.511370	943.791079	21.364032
77.909537	942.873451	21.369050
77.777858	936.229972	21.374067
77.795925	933.004151	21.379085
77.725738	944.669036	21.384103
77.790375	938.260071	21.389120
78.143901	955.980752	21.394138
78.580323	953.455794	21.399155
78.799575	955.341323	21.404173
78.598950	944.131648	21.409191
78.199632	947.311238	21.414208
78.650408	951.214073	21.419226
78.829340	965.189183	21.424243
78.865707	957.513801	21.429261
78.715886	959.980397	21.434279
78.782770	963.644029	21.439296
79.263679	956.195035	21.444314
78.717085	965.685067	21.449331
78.913316	953.449470	21.454349
79.002215	956.832757	21.459367
78.729265	957.201842	21.464384
79.192956	947.665192	21.469402
79.451132	960.403932	21.474419
79.639271	973.905707	21.479437
79.852325	961.909650	21.484455
79.406720	956.813641	21.489472
80.115163	964.785422	21.494490
80.225669	961.157916	21.499507
79.668722	952.027831	21.504525
79.958185	960.241019	21.509543
80.161858	966.133683	21.514560
80.258462	960.293725	21.519578
80.543799	960.061008	21.524595
80.612505	965.865091	21.529613
80.584446	959.024190	21.534631
80.091451	962.023681	21.539648
80.668604	958.216372	21.544666
80.742888	960.469490	21.549683
80.510567	953.176708	21.554701
80.502093	952.188658	21.559719
80.619345	956.717225	21.564736
81.020285	960.187594	21.569754
80.758175	957.601012	21.574771
80.870802	959.336817	21.579789
80.899059	959.049148	21.584807
81.204886	968.198764	21.589824
81.388708	963.744793	21.594842
81.325999	973.878060	21.599859
81.547190	976.507274	21.604877
81.642196	975.540470	21.609895
81.610218	972.188923	21.614912
81.688818	966.677428	21.619930
81.864288	973.653615	21.624947
81.903673	973.656735	21.629965
81.837943	956.514509	21.634983
81.936362	976.103629	21.640000
81.770540	970.958278	21.645018
82.408901	982.228646	21.650035
82.451153	979.112209	21.655053
82.816008	985.812825	21.660071
82.684602	982.422079	21.665088
82.918534	981.676923	21.670106
82.555797	972.290925	21.675123
82.745786	973.196476	21.680141
83.059323	980.471524	21.685159
82.682341	992.666686	21.690176
82.762685	988.189887	21.695194
83.063325	985.604786	21.700211
83.031806	986.456006	21.705229
83.101192	987.556959	21.710247
83.392381	989.492365	21.715264
83.192654	980.585274	21.720282
83.362868	973.476809	21.725299
83.175234	985.449873	21.730317
83.694004	1000.290982	21.735335
83.927070	995.961274	21.740352
83.854830	988.680696	21.745370
83.659244	997.999949	21.750387
84.136551	988.684455	21.755405
84.296394	986.266516	21.760423
84.085814	1001.151582	21.765440
84.347233	997.967159	21.770458
84.322372	988.730174	21.775475
84.318502	991.791658	21.780493
84.597488	1001.194097	21.785511
84.382909	992.736076	21.790528
84.722213	978.127698	21.795546
84.667084	998.825078	21.800563
84.759497	994.440728	21.805581
84.776776	980.160536	21.810599
84.737779	996.017039	21.815616
84.917433	1000.334334	21.820634
84.938767	993.386447	21.825651
84.653952	989.661538	21.830669
85.218138	1005.531965	21.835687
85.235060	1011.393086	21.840704
85.678595	1014.052912	21.845722
85.790473	1008.355208	21.850739
85.730077	1011.304596	21.855757
85.730326	1011.801563	21.860775
85.620540	1008.726667	21.865792
85.666462	1001.277811	21.870810
85.862205	1014.298671	21.875827
85.939573	1002.083561	21.880845
86.309911	994.364337	21.885863
86.186093	1011.325991	21.890880
86.248909	994.205689	21.895898
86.402133	1021.421093	21.900915
86.069497	1015.416772	21.905933
86.753175	1015.638022	21.910951
86.755776	1010.119755	21.915968
86.954603	1017.246385	21.920986
86.980855	1023.673849	21.926003
86.890864	1018.783785	21.931021
87.040581	1014.560166	21.936039
87.151124	1030.488808	21.941056
87.214606	1022.161021	21.946074
87.433828	1017.987661	21.951091
87.289118	1002.896484	21.956109
87.276608	1020.274524	21.961127
87.522313	1011.504005	21.966144
87.489110	1011.230856	21.971162
87.468515	1004.105617	21.976179
87.340215	1024.179241	21.981197
87.794219	1031.815709	21.986215
88.082095	1011.832949	21.991232
88.090357	1025.917129	21.996250
88.626001	1029.922850	22.001267
88.244572	1003.503468	22.006285
88.152436	1020.238298	22.011303
88.407680	1001.918617	22.016320
88.744614	1020.319957	22.021338
88.990742	1012.139216	22.026355
88.135872	1009.626704	22.031373
88.517292	1012.079372	22.036391
88.738835	1019.095422	22.041408
89.097070	1019.925387	22.046426
88.979130	1014.500268	22.051443
88.900243	1018.511184	22.056461
89.181400	1011.163226	22.061479
89.343190	1016.829799	22.066496
89.070610	1019.054876	22.071514
89.251804	1010.024102	22.076531
89.387294	1002.858244	22.081549
89.123533	1013.773885	22.086567
89.529083	1015.200306	22.091584
89.733278	1026.450291	22.096602
90.039679	1027.412783	22.101619
89.804490	1029.339335	22.106637
90.016884	1020.817926	22.111655
90.161301	1024.629648	22.116672
90.346866	1018.778627	22.121690
90.378164	1021.238371	22.126707
90.366411	1020.316901	22.131725
90.477469	1015.866654	22.136743
90.524343	1030.254547	22.141760
90.464849	1022.032882	22.146778
90.827846	1011.980600	22.151795
90.539948	1028.834742	22.156813
90.606960	1023.737180	22.161831
91.070275	1040.561196	22.166848
91.006106	1038.197847	22.171866
91.605818	1040.713232	22.176883
91.131576	1038.514370	22.181901
91.486394	1029.830253	22.186919
91.596526	1036.585671	22.191936
91.601887	1036.687019	22.196954
91.992177	1026.941814	22.201971
91.597189	1030.850568	22.206989
91.783917	1028.142062	22.212007
91.974042	1030.087300	22.217024
91.924855	1022.175430	22.222042
92.049719	1028.662671	22.227059
91.899739	1035.023868	22.232077
92.286126	1039.769076	22.237095
92.539325	1046.613361	22.242112
92.405868	1047.540613	22.247130
92.869532	1038.117160	22.252147
92.298362	1041.877844	22.257165
92.748159	1049.788683	22.262183
92.755775	1039.122987	22.267200
92.567512	1044.678663	22.272218
92.838548	1035.525015	22.277235
92.816139	1037.271354	22.282253
93.435014	1048.744647	22.287271
93.571744	1053.183628	22.292288
93.304340	1046.328947	22.297306
93.540169	1043.963371	22.302323
93.624885	1061.050695	22.307341
93.670688	1056.236484	22.312359
94.254444	1049.865802	22.317376
93.615480	1039.941823	22.322394
93.907263	1049.589205	22.327411
93.868650	1055.059676	22.332429
94.326285	1035.175646	22.337447
94.433379	1053.888944	22.342464
94.465096	1059.389098	22.347482
94.693564	1044.902141	22.352499
94.211006	1055.286450	22.357517
94.532279	1048.432268	22.362535
94.487470	1046.138185	22.367552
94.407962	1054.761032	22.372570
94.603564	1045.962305	22.377587
94.517474	1044.955167	22.382605
95.095728	1048.151907	22.387623
95.362454	1050.435696	22.392640
95.436675	1051.572060	22.397658
95.874106	1040.254265	22.402675
95.327759	1048.040830	22.407693
95.400211	1056.758988	22.412711
95.972885	1047.587117	22.417728
95.678842	1050.457375	22.422746
95.887384	1052.685952	22.427763
95.684263	1056.243238	22.432781
95.982949	1052.986797	22.437799
96.226711	1050.862186	22.442816
95.925200	1050.342403	22.447834
96.002164	1043.648298	22.452851
96.055432	1044.676326	22.457869
96.189806	1050.238752	22.462887
96.580981	1058.775532	22.467904
96.835646	1058.511529	22.472922
97.131848	1065.149205	22.477939
96.927374	1065.851843	22.482957
97.215701	1069.719275	22.487975
97.264650	1060.140159	22.492992
96.622682	1060.871666	22.498010
96.843231	1055.936787	22.503027
97.135278	1061.519689	22.508045
96.945405	1074.407056	22.513063
97.765936	1070.748089	22.518080
97.795559	1075.746819	22.523098
98.008493	1075.003434	22.528115
98.165492	1068.342170	22.533133
98.122282	1084.451112	22.538151
98.662225	1077.105896	22.543168
98.282190	1076.707166	22.548186
98.104051	1058.335408	22.553203
98.455267	1063.713833	22.558221
98.571860	1057.013402	22.563239
98.191117	1060.138146	22.568256
98.037585	1085.348347	22.573274
98.690606	1059.825627	22.578291
98.469711	1096.433024	22.583309
98.090045	1083.224278	22.588327
98.974894	1064.215841	22.593344
98.529067	1093.661378	22.598362
99.266610	1074.855732	22.603379
99.208826	1087.316230	22.608397
99.290268	1070.164554	22.613415
99.528762	1091.957193	22.618432
99.477149	1087.716898	22.623450
99.539709	1078.344799	22.628467
99.402685	1083.440887	22.633485
99.221061	1089.950291	22.638503
100.080202	1079.274611	22.643520
100.198970	1099.911375	22.648538
100.419218	1102.794007	22.653555
100.836546	1099.905578	22.658573
100.654211	1100.139099	22.663591
100.510125	1097.554116	22.668608
100.674598	1093.051286	22.673626
100.682145	1081.265642	22.678643
100.482422	1107.843834	22.683661
100.824477	1102.606434	22.688679
101.039617	1080.148371	22.693696
101.105827	1082.399650	22.698714
101.232046	1088.073497	22.703731
101.389377	1088.267009	22.708749
100.937352	1086.659163	22.713767
101.125019	1087.448697	22.718784
101.337374	1112.094115	22.723802
101.923640	1098.297192	22.728819
102.128554	1112.164492	22.733837
101.936794	1107.070415	22.738855
102.331815	1097.554058	22.743872
102.287971	1108.496045	22.748890
102.239643	1107.852520	22.753907
102.540752	1105.849310	22.758925
102.237869	1100.036822	22.763943
102.487171	1096.885769	22.768960
102.462328	1102.319459	22.773978
102.639996	1088.855100	22.778995
102.303771	1090.675082	22.784013
102.653488	1093.439544	22.789031
103.025541	1102.798900	22.794048
103.387439	1116.518482	22.799066
103.425657	1091.343843	22.804083
103.619649	1108.284818	22.809101
103.155701	1105.126386	22.814119
103.672358	1104.913407	22.819136
103.608137	1108.744267	22.824154
103.681022	1105.786502	22.829171
103.932025	1112.315012	22.834189
103.645013	1111.857404	22.839207
104.098305	1105.955790	22.844224
103.888101	1105.522111	22.849242
103.766377	1099.682308	22.854259
104.082595	1115.225912	22.859277
104.060594	1099.198042	22.864295
104.471193	1105.298428	22.869312
104.816668	1125.527866	22.874330
105.072416	1111.393548	22.879347
105.183650	1118.947881	22.884365
104.800927	1115.241696	22.889383
105.294046	1107.815848	22.894400
105.300432	1106.366120	22.899418
105.446077	1115.695525	22.904435
105.629750	1120.095584	22.909453
105.148308	1111.574658	22.914471
105.601946	1094.129233	22.919488
105.581291	1096.891414	22.924506
105.838191	1103.068215	22.929523
105.962068	1118.423856	22.934541
105.530214	1093.582133	22.939559
105.852627	1109.549435	22.944576
105.755227	1110.963268	22.949594
105.960964	1106.438124	22.954611
106.713483	1098.086928	22.959629
106.653018	1131.760481	22.964647
106.477961	1120.952404	22.969664
106.513054	1100.514355	22.974682
106.714294	1115.058606	22.979699
106.855150	1118.167821	22.984717
106.795147	1113.156545	22.989735
106.922214	1106.526776	22.994752
107.194077	1120.669684	22.999770
107.378270	1125.510083	23.004787
107.752015	1112.720684	23.009805
107.633647	1134.875446	23.014823
107.990606	1125.464235	23.019840
107.744494	1124.287564	23.024858
108.099011	1130.831035	23.029875
108.647583	1122.726266	23.034893
108.065734	1121.732114	23.039911
108.326953	1127.500847	23.044928
108.305509	1116.753215	23.049946
108.300776	1118.672914	23.054963
108.344470	1113.383994	23.059981
108.631345	1118.264643	23.064999
108.289575	1119.885749	23.070016
108.440723	1118.431812	23.075034
108.875390	1128.522053	23.080051
109.215037	1128.192591	23.085069
108.793958	1137.245888	23.090087
108.751286	1132.930225	23.095104
109.372203	1136.524431	23.100122
109.155814	1134.421278	23.105139
110.076953	1148.765829	23.110157
109.952732	1136.897337	23.115175
109.465629	1129.577453	23.120192
110.142741	1136.256664	23.125210
110.272501	1147.606702	23.130227
110.501529	1133.536395	23.135245
110.044644	1139.245047	23.140263
110.298409	1129.354814	23.145280
110.881471	1135.176043	23.150298
110.806403	1149.311384	23.155315
110.648051	1134.014612	23.160333
110.469629	1139.326522	23.165351
110.727255	1140.741944	23.170368
110.983446	1133.305104	23.175386
111.069602	1144.555133	23.180403
111.272909	1131.472016	23.185421
110.991511	1133.509762	23.190439
111.401226	1136.082206	23.195456
111.575750	1132.299739	23.200474
111.378492	1131.838828	23.205491
111.865751	1141.906537	23.210509
112.010879	1147.130679	23.215527
112.241132	1149.588606	23.220544
112.624001	1137.699023	23.225562
112.427704	1152.934307	23.230579
112.717159	1140.441453	23.235597
112.501715	1130.770750	23.240615
112.698062	1152.743228	23.245632
112.528745	1150.382470	23.250650
112.404527	1144.632703	23.255667
112.626671	1140.998361	23.260685
112.460171	1149.072025	23.265703
112.817231	1155.457809	23.270720
113.346869	1160.142468	23.275738
113.613333	1160.430258	23.280755
114.279310	1157.055456	23.285773
113.770202	1159.769702	23.290791
113.927943	1154.462581	23.295808
114.178177	1149.933474	23.300826
113.621726	1143.505486	23.305843
113.932542	1152.567918	23.310861
114.125236	1142.091271	23.315879
114.185294	1154.901105	23.320896
114.480541	1142.215428	23.325914
114.198864	1174.074581	23.330931
114.666517	1137.891578	23.335949
114.389105	1163.288403	23.340967
114.754583	1150.802293	23.345984
115.406961	1141.081284	23.351002
115.148464	1166.001643	23.356019
115.252890	1172.857133	23.361037
115.739900	1157.591126	23.366055
115.107394	1165.905840	23.371072
115.448448	1169.595017	23.376090
115.396886	1170.169461	23.381107
115.742897	1151.644790	23.386125
115.812815	1172.797511	23.391143
115.548469	1174.719292	23.396160
115.662696	1155.695203	23.401178
115.742958	1188.133713	23.406195
116.375732	1170.137416	23.411213
116.459052	1175.887349	23.416231
116.317502	1190.266127	23.421248
116.527207	1174.852422	23.426266
116.592772	1175.644130	23.431283
116.852799	1188.145270	23.436301
117.163214	1167.191340	23.441319
117.165889	1178.717389	23.446336
117.402316	1177.962390	23.451354
117.119837	1168.138764	23.456371
117.102280	1162.529276	23.461389
117.678769	1178.355474	23.466407
117.587150	1177.122704	23.471424
118.127264	1180.668464	23.476442
117.842697	1174.006780	23.481459
118.076216	1192.365067	23.486477
118.217644	1160.315815	23.491495
118.160471	1202.475024	23.496512
118.453974	1177.739272	23.501530
117.962037	1175.244346	23.506547
118.246617	1198.340063	23.511565
118.750532	1202.818064	23.516583
119.010247	1177.810861	23.521600
119.304630	1214.242020	23.526618
119.064327	1177.272083	23.531635
119.687966	1203.775788	23.536653
119.390079	1181.753283	23.541671
119.162625	1201.292439	23.546688
119.745866	1178.717324	23.551706
119.575470	1179.202185	23.556723
119.723809	1202.856007	23.561741
119.465373	1183.556268	23.566759
120.092657	1193.512029	23.571776
120.313533	1188.141349	23.576794
119.997235	1211.167742	23.581811
120.572341	1196.022921	23.586829
120.547446	1212.558502	23.591847
120.527519	1192.157408	23.596864
121.133892	1186.011141	23.601882
121.000940	1209.414116	23.606899
120.989679	1178.331365	23.611917
121.121402	1189.176210	23.616935
121.106763	1206.103384	23.621952
121.515677	1185.427861	23.626970
121.734231	1219.116902	23.631987
121.637638	1205.810992	23.637005
122.101507	1209.711820	23.642023
122.024125	1207.737492	23.647040
122.555487	1208.640536	23.652058
122.406846	1209.244617	23.657075
122.240632	1210.740215	23.662093
122.382155	1196.933898	23.667111
122.132457	1198.699196	23.672128
122.563847	1200.344881	23.677146
122.448981	1226.977400	23.682163
122.440435	1180.753030	23.687181
122.580882	1213.919714	23.692199
122.487374	1204.515792	23.697216
123.203675	1205.842353	23.702234
123.227441	1216.050088	23.707251
123.372302	1208.217278	23.712269
123.748167	1202.087313	23.717287
123.374913	1209.685918	23.722304
123.882090	1216.604617	23.727322
123.494760	1221.020257	23.732339
123.543761	1222.402891	23.737357
124.084386	1211.732294	23.742375
124.140069	1216.472101	23.747392
124.863474	1219.302841	23.752410
124.647568	1233.584986	23.757427
124.854257	1226.437550	23.762445
124.935142	1222.404164	23.767463
124.895151	1227.498987	23.772480
125.323343	1208.269042	23.777498
125.317983	1213.587988	23.782515
125.178527	1217.427728	23.787533
125.418651	1206.190030	23.792551
124.994440	1230.940308	23.797568
125.443704	1222.675152	23.802586
125.756288	1231.553320	23.807603
125.532805	1234.028560	23.812621
126.216769	1225.552954	23.817639
126.158578	1225.134354	23.822656
126.304899	1248.182990	23.827674
126.490502	1237.447868	23.832691
126.311967	1239.222272	23.837709
126.842955	1229.688868	23.842727
126.744234	1223.275937	23.847744
127.099461	1236.175626	23.852762
127.368202	1244.085565	23.857779
127.715301	1239.890180	23.862797
127.251033	1217.478890	23.867815
127.520714	1223.965152	23.872832
127.634686	1224.950482	23.877850
127.604760	1241.754300	23.882867
127.640577	1226.350965	23.887885
128.305863	1229.033680	23.892903
128.109538	1236.924969	23.897920
127.920756	1232.160688	23.902938
128.198355	1234.005497	23.907955
128.006817	1230.967181	23.912973
128.675236	1231.356040	23.917991
128.639496	1247.165116	23.923008
129.049330	1239.837423	23.928026
129.299028	1243.516022	23.933043
129.051040	1248.798168	23.938061
129.183676	1239.889819	23.943079
129.162337	1258.389499	23.948096
129.201819	1247.237243	23.953114
129.537523	1235.804965	23.958131
129.310108	1243.004398	23.963149
129.440797	1237.045641	23.968167
129.240786	1251.743674	23.973184
130.100142	1256.970369	23.978202
130.108132	1244.512869	23.983219
130.124866	1259.250277	23.988237
130.754634	1258.166728	23.993255
130.536481	1255.005241	23.998272
130.326893	1248.672895	24.003290
130.813595	1260.919317	24.008307
130.799005	1276.545736	24.013325
131.458822	1267.930818	24.018343
131.773153	1263.153941	24.023360
131.813951	1264.715631	24.028378
131.887077	1263.865551	24.033395
131.500024	1258.022373	24.038413
131.889432	1262.046770	24.043431
131.629396	1276.996634	24.048448
131.808880	1266.965575	24.053466
131.801686	1255.454257	24.058483
131.755425	1281.075542	24.063501
132.560279	1257.381205	24.068519
132.745844	1268.777497	24.073536
133.318233	1273.765253	24.078554
133.228282	1277.343869	24.083571
132.745084	1266.424371	24.088589
133.017004	1283.016521	24.093607
133.313374	1279.722652	24.098624
133.148623	1277.754380	24.103642
133.456810	1273.713049	24.108659
133.682165	1279.973608	24.113677
133.753539	1281.780524	24.118695
133.783043	1283.298401	24.123712
133.840825	1278.737025	24.128730
134.453573	1285.085246	24.133747
134.309195	1295.142105	24.138765
134.997617	1283.656694	24.143783
134.725058	1290.608530	24.148800
134.746706	1288.096179	24.153818
135.237062	1291.155998	24.158835
134.904765	1284.446818	24.163853
134.910610	1282.592909	24.168871
134.979699	1289.087592	24.173888
135.422638	1279.426631	24.178906
135.417584	1268.349096	24.183923
135.140683	1278.203715	24.188941
136.010515	1281.097635	24.193959
136.054750	1306.868124	24.198976
136.041457	1307.047951	24.203994
136.415370	1305.155799	24.209011
136.179743	1303.944407	24.214029
136.619646	1281.731747	24.219047
136.629206	1293.859233	24.224064
136.636176	1297.653625	24.229082
136.642406	1284.186533	24.234099
136.538046	1296.111972	24.239117
137.092438	1287.947989	24.244135
136.773303	1288.252084	24.249152
137.034560	1303.854998	24.254170
137.578480	1307.883085	24.259187
137.231290	1315.150413	24.264205
137.909884	1302.647280	24.269223
137.799740	1292.693843	24.274240
137.794311	1293.215320	24.279258
137.918889	1316.138552	24.284275
138.410441	1313.725868	24.289293
138.975355	1316.594488	24.294311
138.724893	1310.889949	24.299328
138.808406	1327.400513	24.304346
138.939362	1322.276919	24.309363
138.862275	1311.261172	24.314381
139.132766	1310.428381	24.319399
138.667877	1319.534389	24.324416
139.238977	1303.227681	24.329434
139.633549	1310.493132	24.334451
139.642955	1313.049223	24.339469
139.973972	1340.623843	24.344487
140.336668	1317.750212	24.349504
140.310455	1308.090108	24.354522
140.567747	1302.748185	24.359539
140.183091	1321.422277	24.364557
140.632375	1305.852259	24.369575
140.483997	1313.380455	24.374592
140.795151	1309.772777	24.379610
141.074240	1303.272828	24.384627
141.273447	1316.079498	24.389645
141.383300	1313.518473	24.394663
141.860566	1325.417262	24.399680
141.718542	1317.188135	24.404698
141.893266	1322.969170	24.409715
142.025236	1318.765596	24.414733
142.297141	1299.867177	24.419751
141.862030	1316.540644	24.424768
142.081046	1317.720008	24.429786
142.474246	1305.016997	24.434803
142.488009	1304.648267	24.439821
142.316528	1303.055428	24.444839
142.953343	1307.317231	24.449856
143.115149	1328.996632	24.454874
143.289984	1319.903761	24.459891
143.291146	1319.017964	24.464909
143.603946	1333.761723	24.469927
143.795274	1334.000156	24.474944
143.540161	1323.070984	24.479962
143.713350	1309.121089	24.484979
143.643388	1325.299061	24.489997
143.656333	1318.816375	24.495015
144.179590	1321.103352	24.500032
144.226756	1337.534784	24.505050
144.935392	1334.722559	24.510067
144.833387	1341.843844	24.515085
144.864262	1335.158525	24.520103
144.922173	1332.860599	24.525120
144.517209	1344.289765	24.530138
145.128898	1332.709592	24.535155
144.948469	1328.733571	24.540173
145.072058	1326.201813	24.545191
145.577247	1335.036755	24.550208
145.802105	1346.985246	24.555226
146.013208	1336.876741	24.560243
146.256341	1335.845400	24.565261
146.441724	1332.839766	24.570279
146.277068	1350.313253	24.575296
146.296064	1333.437047	24.580314
146.732400	1324.031928	24.585331
146.541733	1334.341577	24.590349
147.103623	1335.716373	24.595367
147.677193	1343.912807	24.600384
147.445915	1348.338206	24.605402
147.811160	1338.791837	24.610419
147.540821	1352.146868	24.615437
147.382547	1359.950362	24.620455
147.740507	1350.409865	24.625472
147.901466	1348.869403	24.630490
147.877503	1349.280583	24.635507
147.938319	1347.483966	24.640525
148.242517	1349.540047	24.645543
148.748732	1362.966317	24.650560
148.757992	1364.518890	24.655578
149.195466	1361.982695	24.660595
149.136689	1361.211840	24.665613
148.993824	1361.597937	24.670631
148.823759	1357.846762	24.675648
149.135887	1362.597637	24.680666
149.929699	1364.372741	24.685683
150.295273	1378.853314	24.690701
149.958286	1380.417054	24.695719
150.355953	1367.109259	24.700736
150.406222	1360.458586	24.705754
150.626301	1364.952017	24.710771
150.449391	1381.373612	24.715789
150.509241	1365.109028	24.720807
150.467479	1361.845462	24.725824
150.925727	1374.418980	24.730842
151.085873	1375.340333	24.735859
151.564016	1381.063577	24.740877
151.636582	1378.628032	24.745895
151.755893	1370.330464	24.750912
152.032205	1375.426815	24.755930
152.163774	1379.199789	24.760947
152.353228	1373.716079	24.765965
152.434110	1372.164788	24.770983
152.558286	1362.625381	24.776000
152.081281	1364.275935	24.781018
152.547112	1358.015164	24.786035
152.440826	1372.841516	24.791053
152.199917	1378.363242	24.796071
152.737689	1375.869253	24.801088
153.054619	1381.939086	24.806106
153.326582	1376.468960	24.811123
153.479104	1384.045167	24.816141
153.166568	1380.418945	24.821159
153.799273	1371.375728	24.826176
153.954606	1396.755875	24.831194
154.469273	1392.508565	24.836211
154.477000	1402.512933	24.841229
154.596897	1398.234186	24.846247
154.942131	1398.199552	24.851264
155.043714	1392.251664	24.856282
155.258253	1387.990863	24.861299
155.041050	1389.456856	24.866317
154.845279	1389.094792	24.871335
155.098763	1387.113300	24.876352
154.958904	1392.741611	24.881370
155.605867	1397.656181	24.886387
155.848411	1392.642181	24.891405
155.727394	1405.267191	24.896423
156.414422	1398.514974	24.901440
156.091394	1410.774237	24.906458
156.661427	1396.197862	24.911475
156.274291	1397.722410	24.916493
156.697754	1411.548871	24.921511
157.422720	1417.191879	24.926528
157.745378	1414.601626	24.931546
157.629554	1396.066911	24.936563
158.040971	1390.152990	24.941581
157.664086	1392.073863	24.946599
157.984819	1393.627113	24.951616
157.899314	1403.927908	24.956634
157.967726	1385.727186	24.961651
158.388757	1397.119073	24.966669
158.039842	1389.756561	24.971687
158.435999	1392.255721	24.976704
158.152984	1401.494795	24.981722
158.702521	1399.598227	24.986739
159.299312	1407.012381	24.991757
159.096500	1406.275499	24.996775
159.525513	1419.062925	25.001792
159.399964	1411.582994	25.006810
159.729764	1404.307308	25.011827
159.538352	1407.136098	25.016845
159.820828	1398.016578	25.021863
160.188593	1420.251571	25.026880
160.429109	1420.773163	25.031898
160.575298	1413.440234	25.036915
160.909279	1425.577453	25.041933
160.932872	1415.220374	25.046951
161.027415	1406.462709	25.051968
160.830239	1410.667193	25.056986
161.092736	1408.531683	25.062003
161.331445	1405.663818	25.067021
160.970199	1405.941594	25.072039
161.580201	1392.128031	25.077056
161.752213	1411.864895	25.082074
162.026395	1418.997023	25.087091
162.344767	1409.432914	25.092109
162.113962	1432.715009	25.097127
162.358600	1406.158863	25.102144
162.246399	1421.354283	25.107162
162.474560	1412.407002	25.112179
163.046419	1417.169968	25.117197
163.120435	1428.483506	25.122215
163.504397	1421.288835	25.127232
163.464224	1427.868641	25.132250
163.451284	1427.510457	25.137267
163.986280	1424.389290	25.142285
163.473422	1430.040908	25.147303
163.897315	1428.541883	25.152320
163.905876	1437.284621	25.157338
164.527254	1443.030672	25.162355
164.531810	1441.905234	25.167373
164.282143	1452.082806	25.172391
164.942264	1427.325921	25.177408
164.994346	1437.549750	25.182426
165.320742	1446.485630	25.187443
165.957143	1438.059962	25.192461
166.187643	1440.289826	25.197479
166.124693	1445.828819	25.202496
165.962485	1448.527123	25.207514
166.218057	1443.415078	25.212531
166.350772	1429.537584	25.217549
166.276472	1442.466626	25.222567
166.433267	1443.591432	25.227584
166.513828	1438.861211	25.232602
166.506543	1443.417659	25.237619
167.238294	1443.766552	25.242637
167.451840	1461.879849	25.247655
167.759575	1452.517176	25.252672
167.832434	1450.875923	25.257690
167.933632	1455.333285	25.262707
168.045027	1452.921423	25.267725
168.091510	1458.145682	25.272743
168.138083	1455.879430	25.277760
168.084191	1447.692801	25.282778
168.223763	1460.205528	25.287795
168.746026	1460.469849	25.292813
168.917592	1457.606388	25.297831
169.392080	1457.933381	25.302848
169.075025	1458.642970	25.307866
169.207834	1460.564380	25.312883
169.629393	1454.049515	25.317901
169.835169	1465.552854	25.322919
170.351590	1461.193566	25.327936
169.879402	1466.481647	25.332954
170.143689	1476.372806	25.337971
170.680367	1462.161895	25.342989
170.852388	1467.194688	25.348007
170.768581	1449.166013	25.353024
170.815099	1460.469805	25.358042
170.818453	1461.166061	25.363059
171.046633	1455.890071	25.368077
171.030770	1466.088575	25.373095
171.583664	1468.995329	25.378112
171.840712	1473.921762	25.383130
171.487795	1463.986462	25.388147
171.837371	1466.022744	25.393165
171.978287	1477.731483	25.398183
172.616094	1480.709642	25.403200
173.066125	1486.239220	25.408218
173.271945	1490.329139	25.413235
173.704949	1481.204443	25.418253
172.893308	1483.454182	25.423271
173.484712	1478.288581	25.428288
173.514709	1486.427056	25.433306
173.309949	1488.609924	25.438323
173.557615	1466.075284	25.443341
173.429218	1482.504990	25.448359
174.125020	1493.245980	25.453376
174.310680	1486.202441	25.458394
174.428436	1496.228657	25.463411
174.613673	1483.697071	25.468429
174.847394	1488.424314	25.473447
175.054591	1497.788206	25.478464
175.804997	1504.270315	25.483482
175.658460	1496.691441	25.488499
175.852430	1492.997015	25.493517
175.488528	1505.819709	25.498535
176.148012	1493.143291	25.503552
175.907863	1482.736980	25.508570
176.255537	1502.384618	25.513587
176.463612	1495.710296	25.518605
176.501110	1493.711319	25.523623
176.622386	1504.537626	25.528640
177.163297	1507.246531	25.533658
177.094994	1511.081295	25.538675
177.259240	1499.710753	25.543693
177.578491	1512.163420	25.548711
177.717562	1519.321861	25.553728
178.124326	1518.100832	25.558746
178.556357	1515.376725	25.563763
178.663396	1498.737961	25.568781
178.590573	1506.966770	25.573799
178.717684	1523.667237	25.578816
179.112941	1505.557393	25.583834
179.105922	1514.615686	25.588851
179.655005	1506.183455	25.593869
179.186390	1504.782677	25.598887
179.385754	1496.601258	25.603904
179.358385	1496.034594	25.608922
179.515066	1503.485939	25.613939
179.723811	1492.125611	25.618957
179.996245	1508.093478	25.623975
180.241585	1516.073372	25.628992
180.357802	1514.952148	25.634010
180.394743	1517.478718	25.639027
180.489612	1507.018976	25.644045
180.507020	1503.587071	25.649063
181.258091	1516.464811	25.654080
181.652173	1513.633501	25.659098
181.563142	1516.994959	25.664115
182.110367	1505.264487	25.669133
182.168561	1509.917480	25.674151
182.348042	1504.896195	25.679168
182.591855	1495.581437	25.684186
182.695423	1498.916903	25.689204
182.609741	1495.976475	25.694221
183.389205	1512.442366	25.699239
183.407159	1513.087534	25.704256
183.751651	1513.065607	25.709274
183.433090	1512.328296	25.714292
183.848230	1515.607799	25.719309
183.915721	1504.949509	25.724327
183.790559	1511.558634	25.729344
184.178839	1502.816998	25.734362
184.185623	1498.317163	25.739380
184.378718	1495.967772	25.744397
184.770529	1490.461195	25.749415
184.933636	1524.966750	25.754432
185.782612	1501.113982	25.759450
185.190498	1523.734978	25.764468
185.539350	1508.533105	25.769485
185.225893	1529.479292	25.774503
185.586610	1504.882478	25.779520
186.037086	1512.257102	25.784538
186.044583	1542.232948	25.789556
186.433399	1525.332943	25.794573
186.407989	1520.569255	25.799591
186.413787	1532.275201	25.804608
187.092529	1539.545808	25.809626
187.276942	1535.645262	25.814644
187.406390	1563.529307	25.819661
187.805646	1522.235390	25.824679
187.992160	1564.195595	25.829696
188.442212	1531.764402	25.834714
188.189680	1541.311728	25.839732
188.322389	1538.509501	25.844749
188.175395	1520.567098	25.849767
188.218702	1530.615434	25.854784
189.179838	1531.800770	25.859802
189.633497	1541.727851	25.864820
189.480595	1549.898669	25.869837
189.584803	1546.143038	25.874855
189.544150	1527.692114	25.879872
189.800313	1549.952975	25.884890
189.881382	1546.926178	25.889908
190.041379	1538.338890	25.894925
190.096144	1537.158251	25.899943
189.981720	1539.749855	25.904960
190.726935	1538.289255	25.909978
190.708914	1562.789732	25.914996
191.247570	1570.230551	25.920013
191.152795	1545.502585	25.925031
190.814656	1552.329722	25.930048
191.344001	1557.939493	25.935066
191.404778	1556.234090	25.940084
191.758164	1552.577154	25.945101
192.159993	1584.647568	25.950119
192.254582	1548.876929	25.955136
192.654362	1571.792884	25.960154
193.000322	1570.811203	25.965172
193.287477	1575.551981	25.970189
193.694397	1568.037410	25.975207
193.680816	1594.394928	25.980224
193.478125	1559.063332	25.985242
194.240244	1568.802834	25.990260
194.300438	1565.530829	25.995277
194.360148	1562.990340	26.000295
194.322999	1558.845120	26.005312
194.897394	1551.395091	26.010330
194.679706	1554.722014	26.015348
194.282400	1562.903490	26.020365
194.726387	1561.763040	26.025383
194.952287	1571.039059	26.030400
195.388642	1561.849288	26.035418
195.473949	1586.737590	26.040436
195.736234	1577.671513	26.045453
196.330971	1589.680794	26.050471
196.231825	1585.056251	26.055488
196.729481	1576.179160	26.060506
196.712162	1582.450235	26.065524
196.863279	1578.745318	26.070541
197.265943	1583.826325	26.075559
197.479645	1589.521038	26.080576
198.185168	1586.954662	26.085594
198.053646	1583.562211	26.090612
198.244946	1590.094178	26.095629
198.508166	1584.524700	26.100647
198.427796	1584.554779	26.105664
198.735262	1576.933366	26.110682
198.769339	1575.222780	26.115700
198.627014	1564.899908	26.120717
198.656166	1579.234560	26.125735
198.872962	1587.601284	26.130752
199.583583	1584.680174	26.135770
199.351251	1577.077180	26.140788
199.490997	1585.701572	26.145805
200.117525	1586.355112	26.150823
199.928122	1593.408660	26.155840
200.408070	1597.893773	26.160858
200.448309	1600.336465	26.165876
200.983681	1600.551517	26.170893
201.210326	1595.226960	26.175911
201.137081	1600.401148	26.180928
201.311953	1592.593232	26.185946
201.582610	1599.060644	26.190964
201.566828	1603.003460	26.195981
202.274113	1602.705052	26.200999
202.566832	1606.405209	26.206016
202.864502	1606.282213	26.211034
202.654792	1602.408304	26.216052
202.684004	1608.069517	26.221069
203.000157	1590.978891	26.226087
202.768790	1597.845654	26.231104
203.346901	1600.761007	26.236122
203.844421	1616.655364	26.241140
204.202591	1608.253514	26.246157
204.353439	1586.575668	26.251175
204.335893	1617.714173	26.256192
204.627437	1585.188581	26.261210
204.460055	1589.522069	26.266228
204.342406	1616.600920	26.271245
205.231812	1602.799247	26.276263
205.392838	1607.393408	26.281280
205.489704	1611.102769	26.286298
205.752326	1632.211303	26.291316
205.981883	1604.093638	26.296333
206.131949	1608.129563	26.301351
205.985320	1614.125545	26.306368
206.782384	1616.400395	26.311386
206.882460	1610.342548	26.316404
206.930499	1646.340637	26.321421
207.541959	1611.017538	26.326439
207.355653	1624.398748	26.331456
207.565155	1611.957560	26.336474
207.812381	1608.575506	26.341492
207.654933	1640.771393	26.346509
208.450613	1631.670583	26.351527
208.268989	1626.919178	26.356544
208.503626	1622.994873	26.361562
208.744222	1635.792095	26.366580
208.488820	1625.104968	26.371597
209.432518	1625.959627	26.376615
209.530588	1637.658029	26.381632
209.551396	1637.662540	26.386650
209.901786	1637.394290	26.391668
210.061909	1626.197334	26.396685
210.517304	1649.546563	26.401703
210.617249	1652.275468	26.406720
210.910339	1650.536165	26.411738
210.988524	1649.446162	26.416756
211.000502	1635.851979	26.421773
211.250045	1641.231121	26.426791
211.156651	1642.589309	26.431808
211.400824	1636.486457	26.436826
211.810307	1641.114952	26.441844
211.647417	1663.154942	26.446861
212.635594	1648.156162	26.451879
212.644605	1646.414957	26.456896
212.779408	1630.666645	26.461914
212.957891	1661.556923	26.466932
213.222979	1648.295176	26.471949
213.350341	1659.763989	26.476967
213.516840	1670.797144	26.481984
214.062683	1650.324068	26.487002
214.098620	1653.159130	26.492020
214.104605	1664.585950	26.497037
214.310959	1656.930280	26.502055
214.724355	1660.548294	26.507072
214.908740	1656.746820	26.512090
214.985916	1676.810630	26.517108
215.285598	1670.003651	26.522125
215.291123	1652.696635	26.527143
215.531610	1686.526448	26.532160
216.324326	1670.951629	26.537178
216.478877	1668.210389	26.542196
216.518730	1679.828446	26.547213
217.001053	1672.224726	26.552231
216.918205	1672.313401	26.557248
217.051636	1662.330307	26.562266
217.410054	1668.322875	26.567284
217.536291	1671.690948	26.572301
217.801343	1676.893029	26.577319
217.888845	1676.408716	26.582336
218.310535	1660.119143	26.587354
218.460576	1691.193341	26.592372
218.458154	1666.305723	26.597389
218.814090	1676.064444	26.602407
218.854220	1688.492558	26.607424
219.354412	1691.843492	26.612442
219.904386	1692.125434	26.617460
219.761266	1687.877522	26.622477
219.978806	1686.585979	26.627495
220.247496	1681.377383	26.632512
220.315211	1666.726667	26.637530
220.554293	1676.947602	26.642548
221.120002	1693.867785	26.647565
221.820671	1680.453202	26.652583
221.923043	1683.195883	26.657600
221.541737	1685.406921	26.662618
221.986929	1676.448476	26.667636
221.879217	1677.414127	26.672653
221.959791	1683.751438	26.677671
222.076010	1677.779077	26.682688
222.392806	1687.989204	26.687706
222.882809	1685.951096	26.692724
222.615557	1701.759835	26.697741
222.860142	1704.874673	26.702759
223.131796	1690.279510	26.707776
223.383161	1695.387828	26.712794
223.908343	1697.693455	26.717812
224.269829	1713.782643	26.722829
224.410952	1708.098878	26.727847
224.328646	1709.812375	26.732864
224.418594	1709.307223	26.737882
224.643352	1713.035548	26.742900
224.892689	1717.541738	26.747917
225.577169	1722.554279	26.752935
225.620177	1709.774612	26.757952
225.566679	1711.990024	26.762970
226.214883	1727.819593	26.767988
226.313845	1724.697099	26.773005
226.570618	1708.130173	26.778023
226.877352	1726.244690	26.783040
227.179854	1723.789736	26.788058
227.236969	1709.260215	26.793076
227.327547	1706.577929	26.798093
227.955224	1721.635274	26.803111
228.370066	1729.259516	26.808128
228.385963	1721.992818	26.813146
228.686624	1713.747939	26.818164
228.366951	1726.793433	26.823181
228.588393	1731.876648	26.828199
228.789650	1723.391210	26.833216
229.107275	1720.106446	26.838234
229.564910	1721.768478	26.843252
229.874179	1732.373088	26.848269
230.096469	1722.684096	26.853287
230.397813	1726.902004	26.858304
230.389217	1712.592164	26.863322
230.983297	1716.025666	26.868340
231.293850	1757.805446	26.873357
231.450197	1722.933719	26.878375
231.716043	1738.012584	26.883392
231.685515	1723.819485	26.888410
232.145381	1709.850241	26.893428
231.946505	1717.696579	26.898445
231.795776	1734.768775	26.903463
232.606382	1710.632354	26.908480
232.553617	1739.941051	26.913498
233.130565	1723.967998	26.918516
233.076780	1724.160577	26.923533
233.204947	1740.573277	26.928551
233.800458	1728.367752	26.933568
233.874616	1754.250695	26.938586
234.510617	1735.892976	26.943604
234.593263	1746.462940	26.948621
234.595779	1742.298757	26.953639
235.040120	1738.375600	26.958656
235.428187	1758.393114	26.963674
235.617561	1748.303516	26.968692
235.827583	1748.631791	26.973709
236.080806	1738.697187	26.978727
236.221759	1735.741028	26.983744
236.361812	1745.188152	26.988762
236.273911	1739.424481	26.993780
236.585657	1745.073745	26.998797
236.381635	1738.630171	27.003815
237.080800	1737.428588	27.008832
237.489607	1760.374880	27.013850
237.489059	1766.986279	27.018868
237.383738	1755.724572	27.023885
237.608800	1736.947875	27.028903
238.362784	1772.896675	27.033920
238.280357	1763.742290	27.038938
238.839841	1752.188995	27.043956
238.978081	1761.935291	27.048973
239.464546	1775.162205	27.053991
239.696585	1771.578046	27.059008
240.110833	1780.158801	27.064026
240.268657	1765.141266	27.069044
240.312423	1789.242181	27.074061
240.436419	1766.604087	27.079079
240.557272	1778.165270	27.084096
240.749928	1783.965667	27.089114
241.167813	1784.587993	27.094132
241.372640	1782.987015	27.099149
241.395966	1780.411390	27.104167
242.428944	1778.821542	27.109184
242.431954	1815.613747	27.114202
242.535658	1791.832121	27.119220
243.217878	1770.970625	27.124237
243.538716	1780.041320	27.129255
243.778360	1778.437938	27.134272
243.309525	1795.419345	27.139290
243.657591	1776.729952	27.144308
243.689331	1767.538489	27.149325
243.938819	1789.044182	27.154343
244.578749	1789.336961	27.159360
244.691745	1788.277579	27.164378
244.897293	1791.725848	27.169396
245.421727	1797.748639	27.174413
245.320596	1814.473254	27.179431
246.001794	1808.675044	27.184448
245.841980	1794.104511	27.189466
246.283267	1789.960034	27.194484
246.514717	1786.058217	27.199501
246.283859	1807.986572	27.204519
247.327341	1805.259334	27.209536
247.224102	1805.549458	27.214554
247.535641	1800.513314	27.219572
247.797962	1797.679367	27.224589
247.871706	1799.671591	27.229607
248.186288	1792.479939	27.234624
248.034717	1804.668157	27.239642
248.918431	1797.480161	27.244660
248.953401	1801.795611	27.249677
248.957966	1816.607902	27.254695
249.117087	1814.358260	27.259712
249.071536	1805.745377	27.264730
249.554253	1807.537131	27.269748
249.936212	1816.022384	27.274765
250.006013	1820.310266	27.279783
250.532705	1821.717488	27.284800
250.838652	1817.805361	27.289818
251.363812	1816.631514	27.294836
251.844941	1834.336132	27.299853
251.702991	1829.487096	27.304871
252.203501	1831.320062	27.309888
252.156165	1826.636842	27.314906
252.130557	1823.378456	27.319924
252.437670	1822.612170	27.324941
252.620630	1813.690725	27.329959
252.978339	1818.451806	27.334976
253.081048	1835.442826	27.339994
253.438702	1836.609584	27.345012
253.814942	1821.884360	27.350029
253.644569	1845.377716	27.355047
254.662686	1839.464443	27.360064
254.960382	1834.573638	27.365082
255.050225	1840.393594	27.370100
255.453624	1847.086931	27.375117
255.425703	1827.705504	27.380135
255.521337	1830.885015	27.385152
255.401335	1846.750664	27.390170
256.076421	1841.703747	27.395188
256.578497	1826.469252	27.400205
256.104130	1855.445847	27.405223
256.858389	1844.529966	27.410240
256.954117	1850.021800	27.415258
257.480296	1851.021698	27.420276
257.842469	1853.947944	27.425293
257.793099	1852.343434	27.430311
258.481927	1859.615767	27.435328
258.662444	1870.354266	27.440346
258.882581	1877.493680	27.445364
259.633285	1854.813749	27.450381
259.265213	1858.888297	27.455399
259.576706	1860.098595	27.460416
259.840178	1849.422964	27.465434
259.860549	1867.276576	27.470452
260.327676	1858.399469	27.475469
260.371108	1871.980242	27.480487
260.939852	1853.898938	27.485504
260.982656	1869.658438	27.490522
261.475970	1884.902552	27.495540
261.916742	1860.761915	27.500557
261.557956	1886.333442	27.505575
261.952755	1874.192826	27.510592
262.069614	1879.569620	27.515610
262.608071	1896.346537	27.520628
263.232890	1895.137923	27.525645
263.267126	1896.892641	27.530663
263.611131	1881.979013	27.535680
263.584224	1877.004656	27.540698
263.514241	1883.320439	27.545716
264.388183	1880.053932	27.550733
264.362810	1893.611087	27.555751
264.954710	1889.541677	27.560768
264.935454	1892.602663	27.565786
265.115426	1877.192943	27.570804
265.359115	1875.651829	27.575821
265.379867	1879.436316	27.580839
265.772320	1883.133241	27.585856
266.205119	1895.631082	27.590874
266.218029	1884.306381	27.595892
267.112564	1886.671152	27.600909
267.162858	1897.219645	27.605927
267.644801	1892.923943	27.610944
267.888497	1891.379680	27.615962
268.187959	1881.406148	27.620980
268.692439	1882.227039	27.625997
268.645233	1895.738913	27.631015
268.855691	1872.176088	27.636032
268.818254	1873.341334	27.641050
268.971074	1888.035688	27.646068
269.766628	1887.045253	27.651085
269.522975	1887.815509	27.656103
269.910003	1885.030882	27.661120
270.394257	1899.331073	27.666138
270.920848	1905.921434	27.671156
271.266468	1895.951546	27.676173
271.313541	1910.157839	27.681191
271.654564	1901.019236	27.686208
271.735597	1890.761192	27.691226
271.774135	1897.042380	27.696244
272.411729	1885.132041	27.701261
272.444883	1902.024118	27.706279
272.917417	1908.333662	27.711296
272.964300	1901.971139	27.716314
273.121129	1900.783641	27.721332
273.503965	1903.138744	27.726349
273.676480	1917.446172	27.731367
274.027621	1916.298486	27.736384
274.306899	1919.750767	27.741402
274.772693	1931.373500	27.746420
275.411839	1924.494993	27.751437
275.508756	1924.526699	27.756455
275.708387	1928.425832	27.761472
275.983624	1926.964628	27.766490
275.873700	1921.399446	27.771508
276.621860	1922.348241	27.776525
276.881567	1932.150801	27.781543
277.326787	1920.977386	27.786560
277.048470	1944.802718	27.791578
277.113762	1922.818673	27.796596
277.819137	1929.712458	27.801613
278.103874	1931.040288	27.806631
278.406811	1953.870070	27.811648
278.722400	1920.723253	27.816666
278.699010	1943.542112	27.821684
279.266735	1919.758668	27.826701
279.204486	1936.428466	27.831719
279.428667	1931.359013	27.836736
279.858328	1924.141090	27.841754
279.930579	1934.557124	27.846772
280.048739	1930.626138	27.851789
280.166954	1938.881376	27.856807
280.469764	1952.095267	27.861824
281.391952	1929.886539	27.866842
281.230222	1962.319792	27.871860
281.764872	1949.404915	27.876877
282.027718	1950.786573	27.881895
282.420070	1966.982825	27.886912
282.900791	1938.855926	27.891930
282.596924	1969.474556	27.896948
283.613927	1952.090895	27.901965
284.238913	1949.553048	27.906983
284.172790	1969.635400	27.912000
284.344919	1946.514291	27.917018
284.626867	1952.089743	27.922036
284.930014	1943.949732	27.927053
285.013360	1948.603584	27.932071
285.059220	1946.250853	27.937088
285.885208	1952.055769	27.942106
285.724478	1957.199985	27.947124
286.384943	1962.271515	27.952141
286.380423	1962.633995	27.957159
287.048102	1975.184137	27.962176
287.249480	1972.783018	27.967194
287.556498	1982.099872	27.972212
287.553221	1959.720856	27.977229
287.614807	1980.168260	27.982247
287.979340	1964.919365	27.987264
288.558724	1983.654585	27.992282
288.646605	1972.851120	27.997300
289.016527	1970.302015	28.002317
289.583999	1982.551957	28.007335
290.025269	1994.604945	28.012352
290.480318	1985.783173	28.017370
290.706583	1992.308189	28.022388
291.114204	1970.686360	28.027405
291.318851	1981.746718	28.032423
291.355090	1980.476188	28.037440
291.824827	1960.450538	28.042458
291.653875	1967.575258	28.047476
291.916499	1970.550434	28.052493
292.169341	1965.032806	28.057511
292.390733	1969.129832	28.062528
292.818503	1969.749028	28.067546
292.860530	1968.299824	28.072564
293.115892	1962.648088	28.077581
293.270491	1991.872349	28.082599
293.544432	1988.748652	28.087616
293.899066	1989.750742	28.092634
294.257408	1991.271342	28.097652
294.798220	1993.639037	28.102669
295.581102	1991.225457	28.107687
295.427934	2011.889608	28.112704
296.045315	1982.921290	28.117722
295.785057	1981.781388	28.122740
296.047411	1980.270324	28.127757
296.490387	1999.588881	28.132775
296.742620	2002.369091	28.137792
297.128717	2008.478529	28.142810
297.198846	2004.946863	28.147828
297.711147	2008.810343	28.152845
298.344491	2010.889586	28.157863
298.546422	2000.313317	28.162880
299.186669	1999.303594	28.167898
298.914125	2008.179582	28.172916
299.018526	1989.535043	28.177933
299.374626	2020.242077	28.182951
299.437774	2017.472871	28.187968
300.259891	1998.602242	28.192986
300.607030	2012.214970	28.198004
301.190742	2028.158999	28.203021
301.302877	2016.204892	28.208039
301.488268	2013.516877	28.213056
301.763558	2003.465318	28.218074
301.782233	2009.178711	28.223092
302.393673	2015.024147	28.228109
302.698583	2019.000910	28.233127
302.625235	2021.795264	28.238144
303.321498	2009.570309	28.243162
303.342111	2025.844759	28.248180
303.647874	2030.987010	28.253197
304.311479	2022.847708	28.258215
304.562773	2018.483343	28.263232
305.194948	2028.520767	28.268250
305.254269	2025.417113	28.273268
305.574064	2031.393983	28.278285
305.961198	2017.563457	28.283303
306.060009	2017.212614	28.288320
306.562812	2009.750186	28.293338
306.858016	2021.084010	28.298356
307.015385	2025.276201	28.303373
307.288189	2026.373136	28.308391
307.369026	2029.940447	28.313408
307.807172	2014.912577	28.318426
308.196405	2024.910068	28.323444
308.482657	2036.312971	28.328461
308.839805	2033.567691	28.333479
309.104211	2036.349115	28.338496
309.747737	2025.538849	28.343514
309.412162	2032.935232	28.348532
309.977877	2038.165045	28.353549
310.338248	2037.904650	28.358567
310.514856	2035.043424	28.363584
310.835929	2019.466342	28.368602
310.822994	2033.805023	28.373620
311.346803	2042.404670	28.378637
311.899020	2053.370366	28.383655
311.974920	2057.059595	28.388672
312.284518	2040.468135	28.393690
312.400432	2046.118855	28.398708
312.831690	2059.960473	28.403725
313.232925	2059.158732	28.408743
313.271222	2062.142941	28.413760
313.923522	2065.068617	28.418778
314.173608	2068.700200	28.423796
314.660027	2062.789802	28.428813
315.055229	2058.864965	28.433831
315.132938	2067.180220	28.438848
315.739207	2066.227822	28.443866
316.071023	2063.848374	28.448884
316.671583	2067.870842	28.453901
316.985535	2060.652421	28.458919
317.203488	2061.432483	28.463936
317.603267	2045.676086	28.468954
317.366616	2055.339194	28.473972
317.466563	2054.508393	28.478989
318.116039	2049.471792	28.484007
318.103629	2066.695377	28.489024
318.561359	2063.775185	28.494042
318.927698	2066.781045	28.499060
319.423834	2079.311439	28.504077
319.993609	2074.773603	28.509095
320.154541	2076.045677	28.514112
320.747278	2068.630236	28.519130
320.890860	2081.465361	28.524148
321.023456	2075.353371	28.529165
321.559102	2074.670209	28.534183
321.471906	2082.475349	28.539200
322.155431	2077.425448	28.544218
322.572300	2073.843223	28.549236
323.038361	2070.597655	28.554253
323.230723	2072.119553	28.559271
323.219626	2072.626231	28.564288
323.377945	2074.181869	28.569306
323.730479	2094.443071	28.574324
324.382702	2077.925953	28.579341
324.256129	2082.797352	28.584359
324.446260	2097.522163	28.589376
324.908201	2100.526953	28.594394
325.855138	2094.058652	28.599412
325.766202	2087.313420	28.604429
326.230928	2109.425540	28.609447
326.785590	2105.737976	28.614464
327.127321	2100.651305	28.619482
327.579740	2108.279221	28.624500
327.726314	2095.726520	28.629517
327.998003	2086.303122	28.634535
327.962021	2096.285065	28.639552
328.385850	2089.549347	28.644570
328.712987	2100.443989	28.649588
328.510386	2100.218262	28.654605
329.137262	2093.911084	28.659623
329.195186	2117.488060	28.664640
329.724358	2114.391303	28.669658
330.006983	2109.270003	28.674676
330.649965	2119.076113	28.679693
331.268037	2123.668399	28.684711
331.302461	2114.119200	28.689728
331.648310	2118.765881	28.694746
331.855923	2107.019854	28.699764
332.154736	2119.111393	28.704781
332.948714	2113.721405	28.709799
333.552022	2119.834034	28.714816
333.665008	2104.175191	28.719834
333.905226	2106.858239	28.724852
334.137033	2098.963898	28.729869
335.044983	2097.659827	28.734887
334.993275	2117.963468	28.739904
334.856669	2113.472131	28.744922
335.437692	2104.265268	28.749940
335.428883	2108.669590	28.754957
336.314771	2116.255173	28.759975
336.552484	2123.969228	28.764992
336.840023	2131.063431	28.770010
337.270698	2117.680482	28.775028
337.106827	2115.216428	28.780045
337.729032	2116.048475	28.785063
338.155418	2128.807114	28.790080
338.551577	2107.581740	28.795098
339.024599	2128.242224	28.800116
339.263313	2129.536515	28.805133
339.711705	2118.780879	28.810151
339.856968	2122.962447	28.815168
340.108848	2112.903532	28.820186
340.417149	2132.742402	28.825204
340.405910	2143.282012	28.830221
341.434063	2132.993976	28.835239
341.595650	2136.996766	28.840256
342.103369	2138.245042	28.845274
342.657954	2133.547589	28.850292
342.653199	2140.400511	28.855309
343.082497	2129.131950	28.860327
343.227396	2141.237029	28.865344
343.732373	2142.967095	28.870362
344.177875	2146.432276	28.875380
344.211738	2147.557866	28.880397
344.513145	2132.438408	28.885415
345.118498	2141.671653	28.890432
345.419647	2162.545198	28.895450
346.138486	2154.505570	28.900468
346.123808	2153.070103	28.905485
346.366593	2142.078225	28.910503
346.654076	2137.015919	28.915520
346.465092	2144.349669	28.920538
346.984075	2146.974143	28.925556
347.227311	2148.804126	28.930573
347.901925	2140.271324	28.935591
348.002364	2154.688017	28.940608
348.264405	2156.263317	28.945626
349.205489	2160.141889	28.950644
349.218705	2163.090791	28.955661
349.704542	2157.029441	28.960679
350.367364	2165.153981	28.965696
350.843171	2154.655077	28.970714
351.097279	2143.705439	28.975732
351.161802	2147.481451	28.980749
351.735097	2141.498979	28.985767
351.871663	2147.830728	28.990784
352.340423	2161.520186	28.995802
352.562656	2159.587632	29.000820
353.062949	2164.787030	29.005837
352.937963	2161.074058	29.010855
353.592520	2167.014949	29.015872
353.643737	2173.767731	29.020890
354.234613	2164.488476	29.025908
354.567149	2175.895135	29.030925
355.168317	2163.302963	29.035943
355.845231	2168.533992	29.040960
355.386261	2169.980373	29.045978
356.099374	2170.698838	29.050996
356.418697	2187.400937	29.056013
356.777448	2184.875606	29.061031
357.360550	2199.673187	29.066048
357.450634	2194.189279	29.071066
358.153755	2186.737317	29.076084
358.325128	2185.766137	29.081101
359.110991	2192.908378	29.086119
359.283320	2200.310422	29.091136
359.724818	2198.874615	29.096154
359.775667	2195.139905	29.101172
360.065266	2195.507431	29.106189
360.596948	2186.338272	29.111207
361.213693	2200.521721	29.116224
361.811806	2197.514642	29.121242
361.763688	2198.864090	29.126260
362.076149	2184.243049	29.131277
362.330558	2186.373284	29.136295
362.351048	2205.312720	29.141312
362.538467	2188.630446	29.146330
363.285498	2195.717530	29.151348
363.879574	2211.119003	29.156365
364.145083	2213.625008	29.161383
364.701761	2214.489533	29.166400
365.055219	2205.285841	29.171418
365.278405	2195.802461	29.176436
365.613192	2216.118588	29.181453
366.257652	2211.672639	29.186471
366.446465	2187.974308	29.191488
366.734629	2197.906241	29.196506
366.947438	2204.150360	29.201524
367.334524	2178.380194	29.206541
367.363732	2184.112432	29.211559
367.698075	2200.198664	29.216576
367.976886	2198.522937	29.221594
368.526341	2196.849700	29.226612
368.607727	2221.742911	29.231629
369.304748	2216.258232	29.236647
369.965304	2207.095265	29.241664
370.128967	2214.144761	29.246682
370.752360	2217.095542	29.251700
370.830772	2221.942187	29.256717
371.479194	2207.848043	29.261735
371.578552	2207.970602	29.266752
372.040164	2222.776561	29.271770
372.963974	2217.479116	29.276788
372.949087	2217.583700	29.281805
373.269334	2223.128000	29.286823
373.412676	2224.138620	29.291840
373.823484	2232.438650	29.296858
374.231638	2217.750414	29.301876
374.597889	2227.264076	29.306893
375.281809	2236.764877	29.311911
375.707828	2234.305901	29.316928
376.019807	2242.563482	29.321946
376.479448	2238.277543	29.326964
376.585996	2241.019676	29.331981
376.859146	2257.771692	29.336999
377.659380	2228.573965	29.342016
377.609354	2248.767415	29.347034
378.404887	2248.799487	29.352052
378.676821	2236.704895	29.357069
379.236627	2246.428406	29.362087
379.704525	2255.433523	29.367104
379.886921	2241.485970	29.372122
380.414919	2260.119661	29.377140
380.520394	2237.477468	29.382157
380.381662	2238.589669	29.387175
381.286840	2264.067426	29.392192
381.466154	2253.563789	29.397210
381.929699	2253.214600	29.402228
382.504811	2249.591394	29.407245
382.732467	2272.671243	29.412263
383.220613	2243.649063	29.417280
383.319293	2271.827306	29.422298
384.313892	2269.903802	29.427316
384.646252	2253.451618	29.432333
385.042253	2263.366417	29.437351
385.755844	2243.955913	29.442368
385.592411	2244.420803	29.447386
385.851216	2259.606768	29.452404
386.255655	2270.250128	29.457421
386.749285	2263.635351	29.462439
386.911035	2252.741248	29.467456
386.719541	2269.933845	29.472474
387.441060	2270.451207	29.477492
387.712527	2268.915074	29.482509
388.307026	2267.881185	29.487527
388.751299	2270.981651	29.492544
389.075416	2268.263623	29.497562
389.672464	2276.884798	29.502580
389.670108	2270.279838	29.507597
389.883868	2287.418892	29.512615
390.464580	2296.237742	29.517632
390.849934	2301.435064	29.522650
391.739182	2290.989738	29.527668
391.999421	2294.198189	29.532685
392.217108	2304.165027	29.537703
393.116169	2291.144599	29.542720
393.142607	2302.310699	29.547738
393.650240	2303.990035	29.552756
394.217114	2301.873558	29.557773
394.185192	2295.856905	29.562791
394.948756	2284.306869	29.567808
395.004693	2312.178965	29.572826
395.673485	2310.378164	29.577844
395.901588	2293.520966	29.582861
396.755957	2304.043895	29.587879
397.273297	2293.494231	29.592896
397.708447	2295.726252	29.597914
397.888225	2300.517447	29.602932
397.941245	2292.286539	29.607949
398.219753	2296.077261	29.612967
398.674972	2299.836680	29.617984
398.973285	2306.779822	29.623002
399.264751	2317.957189	29.628020
399.923147	2313.520008	29.633037
400.162466	2314.063872	29.638055
400.787528	2326.982962	29.643072
401.044060	2335.834619	29.648090
401.730509	2318.378952	29.653108
402.037959	2327.453731	29.658125
402.550818	2315.127197	29.663143
403.566884	2307.914763	29.668160
403.270205	2323.566848	29.673178
404.064708	2310.657450	29.678196
404.303303	2297.572367	29.683213
404.149651	2299.147858	29.688231
404.662659	2316.081960	29.693248
405.285883	2320.764749	29.698266
405.905477	2305.161816	29.703284
406.090472	2318.029894	29.708301
406.130740	2347.545270	29.713319
406.513428	2302.815345	29.718336
407.083673	2353.396202	29.723354
407.991088	2325.412921	29.728372
408.165790	2323.178029	29.733389
407.866588	2342.638154	29.738407
408.547449	2338.615038	29.743424
408.886191	2335.916692	29.748442
409.230475	2351.841854	29.753460
409.732051	2357.880366	29.758477
410.056125	2366.358688	29.763495
410.384567	2354.710400	29.768512
410.907072	2380.626893	29.773530
410.877796	2380.419942	29.778548
411.467776	2379.021817	29.783565
411.871944	2395.108165	29.788583
412.420710	2407.035863	29.793600
412.934828	2399.002780	29.798618
413.158496	2393.820778	29.803636
413.980212	2426.969100	29.808653
414.673977	2420.636984	29.813671
415.008108	2423.721217	29.818688
415.429365	2431.126196	29.823706
415.566664	2420.483622	29.828724
416.090885	2445.061267	29.833741
415.936633	2449.981245	29.838759
417.202275	2422.185316	29.843776
417.609621	2445.764589	29.848794
417.755449	2457.821817	29.853812
418.110922	2464.199846	29.858829
418.495085	2463.956120	29.863847
418.796503	2466.262965	29.868864
419.372938	2494.039111	29.873882
419.932444	2473.775860	29.878900
420.549298	2490.675534	29.883917
420.523661	2492.321100	29.888935
421.321669	2493.908579	29.893952
421.929390	2507.461410	29.898970
422.502467	2496.128762	29.903988
422.696029	2489.912499	29.909005
422.894589	2498.233927	29.914023
423.435265	2496.695780	29.919040
423.651993	2505.741085	29.924058
424.111125	2502.475306	29.929076
424.535738	2526.949409	29.934093
424.770370	2517.467930	29.939111
425.199384	2524.222036	29.944128
425.550910	2529.241572	29.949146
426.498848	2526.028472	29.954164
427.128013	2541.519116	29.959181
427.173776	2544.299310	29.964199
427.753307	2539.190338	29.969216
428.135360	2552.012285	29.974234
428.122554	2558.780960	29.979252
428.974594	2554.727370	29.984269
429.234067	2553.066489	29.989287
429.601214	2568.827796	29.994304
430.092328	2579.780857	29.999322
430.421505	2591.659540	30.004340
430.667089	2581.566698	30.009357
430.893853	2601.218658	30.014375
431.463183	2595.622844	30.019392
431.892329	2604.666616	30.024410
431.932735	2618.022853	30.029428
432.894539	2624.579641	30.034445
433.253990	2643.418460	30.039463
433.605653	2644.577616	30.044480
434.073209	2638.428539	30.049498
434.423238	2650.666549	30.054516
434.889389	2650.335038	30.059533
435.183254	2662.915506	30.064551
436.161751	2657.727197	30.069568
436.495087	2669.469209	30.074586
436.755960	2684.136175	30.079604
437.241453	2675.394100	30.084621
437.555923	2692.385455	30.089639
438.033775	2695.225043	30.094656
438.782596	2700.252131	30.099674
439.239014	2719.605739	30.104692
439.498678	2721.371051	30.109709
439.812911	2723.988949	30.114727
440.171040	2739.947734	30.119744
441.034542	2743.212767	30.124762
441.414495	2758.048036	30.129780
441.596767	2753.010153	30.134797
441.923773	2758.394709	30.139815
442.539940	2772.808518	30.144832
443.078120	2777.632440	30.149850
443.256981	2801.105548	30.154868
443.808517	2794.295686	30.159885
444.196939	2819.652284	30.164903
444.962434	2809.296327	30.169920
445.466666	2823.803532	30.174938
446.069069	2828.385991	30.179956
446.293789	2826.607914	30.184973
447.032210	2842.549485	30.189991
447.155868	2848.938666	30.195008
447.572770	2859.414524	30.200026
447.899769	2855.004036	30.205044
448.436531	2857.094902	30.210061
448.794127	2882.496637	30.215079
449.307544	2881.880723	30.220096
449.689818	2888.322319	30.225114
449.820282	2899.144311	30.230132
450.164685	2911.371643	30.235149
450.708521	2929.785030	30.240167
451.393481	2939.541791	30.245184
451.976194	2945.743824	30.250202
452.513217	2959.749618	30.255220
453.163912	2960.010879	30.260237
453.590517	2980.384263	30.265255
454.144508	2969.921097	30.270272
454.664565	2964.189844	30.275290
454.838293	2989.323737	30.280308
455.230221	2984.849380	30.285325
455.362682	2986.510715	30.290343
455.811389	3002.894268	30.295360
456.235196	3017.692929	30.300378
456.509038	3022.599168	30.305396
457.277914	3031.800674	30.310413
457.420050	3032.321514	30.315431
457.820289	3043.522237	30.320448
458.435942	3051.458972	30.325466
458.488231	3078.769156	30.330484
459.403461	3080.013972	30.335501
459.956527	3093.102552	30.340519
460.275275	3098.783520	30.345536
460.896348	3100.982126	30.350554
461.357679	3119.154837	30.355572
462.191107	3130.111206	30.360589
462.023795	3153.510250	30.365607
462.809256	3138.860092	30.370624
463.505366	3156.390566	30.375642
463.739445	3168.736376	30.380660
464.351692	3159.759873	30.385677
464.676352	3184.759152	30.390695
465.270322	3196.110043	30.395712
465.798626	3195.151945	30.400730
466.034146	3202.862225	30.405748
466.723509	3212.212596	30.410765
467.009930	3225.125109	30.415783
467.086959	3232.158235	30.420800
468.000720	3240.634376	30.425818
468.246293	3260.152090	30.430836
468.810211	3276.513667	30.435853
469.557127	3276.093371	30.440871
470.076180	3285.491376	30.445888
470.469552	3285.039308	30.450906
470.614743	3311.670462	30.455924
471.565858	3320.107664	30.460941
471.960633	3326.139228	30.465959
472.190559	3322.683256	30.470976
473.317898	3330.765168	30.475994
473.476719	3360.096964	30.481012
473.858526	3350.151009	30.486029
474.366092	3348.718747	30.491047
474.699233	3357.221386	30.496064
475.137779	3368.212533	30.501082
475.501300	3381.066493	30.506100
476.243315	3390.586365	30.511117
476.757719	3396.009743	30.516135
477.168671	3407.043859	30.521152
477.791681	3394.141185	30.526170
478.140673	3409.358838	30.531188
478.519922	3427.885612	30.536205
478.782765	3440.927142	30.541223
479.116556	3453.376874	30.546240
479.419288	3457.590388	30.551258
479.828148	3484.094901	30.556276
480.335253	3504.286296	30.561293
481.265509	3484.223742	30.566311
481.670680	3531.072729	30.571328
482.390259	3500.911516	30.576346
482.590685	3531.120379	30.581364
483.102655	3532.896731	30.586381
483.757922	3532.603519	30.591399
484.159151	3549.801525	30.596416
484.761771	3542.036908	30.601434
484.821228	3547.449442	30.606452
485.287442	3565.725772	30.611469
486.081143	3543.713666	30.616487
486.459792	3571.786917	30.621504
487.059286	3566.316519	30.626522
487.514254	3594.272251	30.631540
487.908536	3593.750025	30.636557
488.196684	3612.718675	30.641575
488.859029	3616.486365	30.646592
489.795330	3630.364706	30.651610
490.154953	3640.585176	30.656628
490.262785	3652.581808	30.661645
490.969898	3663.498146	30.666663
491.083703	3682.421507	30.671680
492.002571	3678.497793	30.676698
492.423599	3689.086088	30.681716
492.848190	3707.795571	30.686733
493.867307	3704.385269	30.691751
494.225411	3723.067606	30.696768
494.536725	3727.850127	30.701786
494.531072	3747.123766	30.706804
495.153576	3760.919287	30.711821
495.629812	3768.983257	30.716839
496.294972	3793.122278	30.721856
497.041960	3795.285212	30.726874
497.516210	3800.225869	30.731892
498.295882	3819.241559	30.736909
498.697607	3816.094778	30.741927
499.093683	3838.712948	30.746944
499.414092	3846.939444	30.751962
499.973197	3863.425957	30.756980
500.400050	3867.685110	30.761997
501.176784	3877.662313	30.767015
501.177197	3888.973800	30.772032
502.044470	3894.507922	30.777050
502.683783	3902.553856	30.782068
503.249403	3917.794173	30.787085
504.065190	3917.785319	30.792103
504.438719	3932.805321	30.797120
504.801046	3930.386911	30.802138
505.148870	3946.256640	30.807156
505.205906	3955.351108	30.812173
506.136648	3961.852920	30.817191
506.324573	3993.857452	30.822208
506.905637	3998.012630	30.827226
507.181641	4007.180804	30.832244
507.941201	4022.344712	30.837261
508.708612	4028.078080	30.842279
509.023466	4034.925039	30.847296
509.287493	4042.580884	30.852314
509.577330	4045.545103	30.857332
509.862692	4061.435921	30.862349
510.958517	4066.136062	30.867367
511.269766	4094.431091	30.872384
511.696989	4103.102472	30.877402
512.301012	4104.463056	30.882420
512.862853	4126.723312	30.887437
513.298195	4137.849287	30.892455
513.619209	4146.440857	30.897472
514.115052	4156.857892	30.902490
514.860942	4174.358083	30.907508
515.322391	4190.187954	30.912525
516.185870	4196.695871	30.917543
516.322020	4217.444511	30.922560
517.028506	4214.775361	30.927578
517.807623	4224.978195	30.932596
518.197972	4242.843468	30.937613
518.829988	4246.086757	30.942631
519.299373	4262.204139	30.947648
519.915425	4266.287747	30.952666
520.280535	4287.988035	30.957684
520.767747	4293.082556	30.962701
521.751298	4288.574144	30.967719
522.459628	4304.049369	30.972736
523.003575	4299.404094	30.977754
523.246270	4313.610705	30.982772
523.239088	4325.371340	30.987789
523.757416	4330.046357	30.992807
524.506990	4356.800264	30.997824
525.046566	4362.478027	31.002842
525.553924	4370.263628	31.007860
525.762562	4381.994650	31.012877
526.834028	4389.385971	31.017895
527.595562	4401.732199	31.022912
528.197569	4416.093284	31.027930
528.733350	4425.085826	31.032948
528.751457	4424.341881	31.037965
529.371138	4440.205034	31.042983
529.446793	4462.900391	31.048000
530.282819	4470.580201	31.053018
530.660064	4483.772792	31.058036
531.383892	4507.801398	31.063053
532.135798	4500.357850	31.068071
532.194022	4522.422821	31.073088
533.130420	4535.398167	31.078106
533.546910	4533.395830	31.083124
533.675717	4559.154757	31.088141
534.415192	4574.253225	31.093159
535.107899	4590.148175	31.098176
535.829714	4592.678691	31.103194
536.498694	4618.719836	31.108212
536.667531	4626.857643	31.113229
537.376796	4626.289153	31.118247
537.600987	4639.071243	31.123264
537.471800	4650.057832	31.128282
538.486241	4666.548255	31.133300
538.827881	4684.550844	31.138317
539.459899	4691.629221	31.143335
539.637723	4718.119296	31.148352
540.694135	4728.821121	31.153370
541.076516	4744.113527	31.158388
541.803242	4752.776927	31.163405
542.337717	4761.373409	31.168423
542.877682	4781.325355	31.173440
543.451862	4796.157745	31.178458
543.754804	4812.574439	31.183476
544.259414	4820.945219	31.188493
544.550356	4849.400710	31.193511
545.594292	4868.002026	31.198528
546.253086	4872.670583	31.203546
546.855607	4898.678761	31.208564
547.240238	4909.359499	31.213581
547.750287	4924.265169	31.218599
548.542003	4941.473431	31.223616
548.694083	4951.666529	31.228634
549.445654	4973.156814	31.233652
549.813773	4997.803005	31.238669
550.947462	5002.194573	31.243687
551.394505	5024.064632	31.248704
551.772973	5030.580179	31.253722
552.611509	5045.738097	31.258740
552.949622	5071.602256	31.263757
553.293423	5081.471474	31.268775
553.626940	5099.547458	31.273792
554.227553	5113.745041	31.278810
555.012705	5139.730067	31.283828
555.264872	5165.499518	31.288845
555.949215	5180.712032	31.293863
556.327954	5202.821377	31.298880
556.728019	5229.505119	31.303898
557.561361	5253.810165	31.308916
558.076170	5283.697238	31.313933
558.703211	5295.998002	31.318951
559.191660	5319.108819	31.323968
559.766837	5343.605395	31.328986
560.359914	5364.346605	31.334004
561.010926	5384.608957	31.339021
561.836809	5410.421197	31.344039
562.561869	5419.325210	31.349056
563.079450	5440.124182	31.354074
563.961586	5455.730300	31.359092
564.188302	5464.756985	31.364109
564.871530	5476.813729	31.369127
565.128366	5488.160345	31.374144
565.570992	5525.404882	31.379162
566.348432	5523.835049	31.384180
566.256602	5551.956369	31.389197
567.437198	5554.351058	31.394215
567.518321	5581.098040	31.399232
567.909930	5600.974039	31.404250
569.051894	5597.985128	31.409268
569.377469	5623.239410	31.414285
569.783524	5638.450312	31.419303
570.734934	5667.210499	31.424320
571.402213	5675.201057	31.429338
571.806142	5688.726419	31.434356
572.178424	5708.394802	31.439373
572.479201	5730.654251	31.444391
573.319993	5752.435150	31.449408
573.917743	5780.945856	31.454426
574.568444	5787.028171	31.459444
574.920321	5817.950076	31.464461
575.539595	5838.455705	31.469479
576.301821	5858.795410	31.474496
576.731145	5867.068647	31.479514
577.151297	5880.630938	31.484532
577.882937	5907.977452	31.489549
578.473952	5934.429875	31.494567
579.294960	5960.420880	31.499584
579.509164	5990.907198	31.504602
580.310990	6000.472789	31.509620
580.870669	6037.527687	31.514637
581.348423	6054.836053	31.519655
582.539843	6061.943237	31.524672
582.802023	6092.302540	31.529690
583.207954	6111.457085	31.534708
583.694775	6131.027545	31.539725
584.315526	6161.657166	31.544743
584.747483	6188.115710	31.549760
585.311057	6222.988817	31.554778
586.430275	6223.948157	31.559796
586.934655	6255.057540	31.564813
587.595004	6273.675339	31.569831
588.404244	6289.301046	31.574848
588.642656	6310.187414	31.579866
589.314138	6331.627945	31.584884
589.829902	6357.804379	31.589901
590.366242	6373.713600	31.594919
591.223024	6396.040494	31.599936
591.257607	6425.689316	31.604954
592.723141	6440.675667	31.609972
593.182351	6467.701560	31.614989
593.591535	6489.355610	31.620007
594.195668	6493.582598	31.625024
594.437117	6524.643948	31.630042
595.136191	6554.748947	31.635060
595.329914	6580.643479	31.640077
596.347386	6589.537838	31.645095
596.477620	6615.699816	31.650112
597.064252	6659.993383	31.655130
598.045597	6683.060108	31.660148
598.527041	6712.093891	31.665165
599.431089	6721.922984	31.670183
600.256156	6728.439765	31.675200
600.547600	6744.035918	31.680218
601.118899	6766.082333	31.685236
601.496883	6783.391713	31.690253
601.983282	6801.247965	31.695271
602.683927	6832.723846	31.700288
602.934772	6850.804926	31.705306
603.629060	6877.163135	31.710324
604.159630	6910.512840	31.715341
604.483451	6936.103248	31.720359
604.989067	6956.839401	31.725376
605.765905	6992.204363	31.730394
606.627658	7031.755760	31.735412
607.085329	7056.269977	31.740429
607.963630	7078.140506	31.745447
608.492819	7108.691479	31.750464
608.778599	7156.267376	31.755482
609.747555	7162.571822	31.760500
610.618217	7178.823644	31.765517
611.086158	7216.090455	31.770535
611.789135	7242.879887	31.775552
612.268235	7265.705716	31.780570
613.012665	7293.660184	31.785588
613.368352	7333.736741	31.790605
613.916700	7362.352797	31.795623
614.835108	7386.260732	31.800640
615.272111	7423.684059	31.805658
615.830769	7448.994045	31.810676
616.669537	7475.501053	31.815693
617.037341	7503.384501	31.820711
618.127867	7532.238709	31.825728
618.509449	7563.854298	31.830746
619.226574	7577.882295	31.835764
619.760987	7623.960552	31.840781
620.091875	7647.516351	31.845799
621.058306	7667.614393	31.850816
621.370804	7696.897327	31.855834
622.159495	7742.749768	31.860852
623.091873	7760.340240	31.865869
623.470832	7803.335847	31.870887
624.293127	7831.506327	31.875904
624.605020	7862.947961	31.880922
625.418375	7882.531695	31.885940
626.004982	7924.610184	31.890957
626.350647	7954.095281	31.895975
627.511893	7986.634102	31.900992
628.132853	8017.272265	31.906010
628.552469	8039.285726	31.911028
629.498588	8065.651985	31.916045
629.911811	8086.286412	31.921063
630.523256	8120.288488	31.926080
630.906694	8143.000288	31.931098
631.853891	8177.601322	31.936116
632.230032	8205.223529	31.941133
632.760154	8233.285507	31.946151
633.486493	8244.544531	31.951168
633.629774	8275.607087	31.956186
634.206599	8312.880559	31.961204
634.739500	8342.895279	31.966221
635.049596	8386.943765	31.971239
636.081985	8413.077766	31.976256
636.591626	8452.511992	31.981274
637.392807	8482.045200	31.986292
637.969791	8522.795542	31.991309
638.422857	8558.152072	31.996327
639.541143	8583.360715	32.001344
640.131936	8625.347672	32.006362
640.771671	8655.931444	32.011380
641.542088	8691.517094	32.016397
642.066185	8715.233456	32.021415
642.587016	8754.974371	32.026432
643.250724	8791.085576	32.031450
643.958995	8818.737081	32.036468
644.611311	8869.657063	32.041485
644.928976	8905.967653	32.046503
645.776411	8938.088770	32.051520
646.382457	8968.085235	32.056538
647.248753	9008.553981	32.061556
647.845146	9051.956869	32.066573
648.358395	9108.144070	32.071591
649.335608	9134.377052	32.076608
650.129970	9163.289871	32.081626
650.771862	9189.452017	32.086644
651.270663	9231.867669	32.091661
652.211380	9259.291761	32.096679
652.563143	9282.111856	32.101696
653.408002	9330.516914	32.106714
653.811466	9380.823560	32.111732
654.590154	9411.380463	32.116749
655.139758	9445.749526	32.121767
656.034444	9480.209298	32.126784
656.217227	9520.368851	32.131802
656.887358	9570.235489	32.136820
657.524692	9610.738397	32.141837
658.260961	9645.307978	32.146855
659.097038	9683.699591	32.151872
660.013173	9715.235416	32.156890
660.378923	9758.731383	32.161908
661.194312	9801.419701	32.166925
661.742179	9845.848948	32.171943
662.386172	9887.373775	32.176960
662.932889	9921.248228	32.181978
663.663438	9954.688603	32.186996
664.394242	9991.442046	32.192013
664.521353	10050.754700	32.197031
665.694410	10084.384594	32.202048
666.435404	10114.329611	32.207066
666.753766	10174.280814	32.212084
668.073234	10196.531914	32.217101
667.928498	10222.280100	32.222119
668.792976	10270.652026	32.227136
669.338048	10314.444885	32.232154
669.887303	10340.828805	32.237172
670.664239	10374.190332	32.242189
671.340408	10410.105156	32.247207
671.620401	10461.760735	32.252224
672.658231	10486.253153	32.257242
673.103416	10571.891744	32.262260
673.724026	10564.024271	32.267277
674.306542	10638.491140	32.272295
675.220669	10678.158014	32.277312
675.701710	10708.253822	32.282330
676.303324	10775.950292	32.287348
677.208734	10789.467757	32.292365
677.489732	10869.156241	32.297383
678.742698	10895.114683	32.302400
679.272582	10945.988429	32.307418
679.992953	10997.455316	32.312436
680.736110	11056.249256	32.317453
681.332213	11085.568439	32.322471
681.980920	11138.566132	32.327488
682.904026	11180.713149	32.332506
683.898989	11218.605688	32.337524
684.998424	11248.367225	32.342541
684.993449	11290.013829	32.347559
685.980082	11331.937875	32.352576
686.591840	11379.419235	32.357594
687.134817	11410.505705	32.362612
687.968570	11452.711787	32.367629
688.508228	11517.143909	32.372647
689.091345	11560.040280	32.377664
689.719354	11587.845847	32.382682
690.021137	11641.015847	32.387700
691.224900	11696.170553	32.392717
691.419502	11748.048373	32.397735
692.389348	11785.943983	32.402752
693.399466	11819.451434	32.407770
693.696275	11892.479731	32.412788
695.063529	11936.290824	32.417805
695.524030	11971.777790	32.422823
696.353988	12023.510924	32.427840
697.124679	12081.352543	32.432858
697.640253	12125.720080	32.437876
698.699177	12154.269931	32.442893
699.208421	12208.238648	32.447911
699.901647	12251.778027	32.452928
700.659181	12281.584640	32.457946
701.223696	12355.215184	32.462964
702.234409	12355.924324	32.467981
702.853240	12421.121776	32.472999
703.667022	12443.278481	32.478016
704.337602	12484.240541	32.483034
704.689963	12539.611422	32.488052
705.534892	12574.908138	32.493069
705.580091	12598.391675	32.498087
706.362959	12656.335877	32.503104
707.268231	12667.923177	32.508122
707.612314	12755.545758	32.513140
708.304733	12775.759279	32.518157
708.912257	12853.212025	32.523175
709.773565	12866.197076	32.528192
710.216155	12932.598739	32.533210
711.130094	12965.562068	32.538228
711.829543	13015.775877	32.543245
712.877048	13065.498775	32.548263
713.433082	13117.599618	32.553280
713.951273	13175.339811	32.558298
714.870160	13198.384495	32.563316
715.481750	13275.883813	32.568333
716.783417	13300.016699	32.573351
717.185653	13351.277004	32.578368
717.956549	13413.930815	32.583386
718.461256	13450.276108	32.588404
719.340518	13495.245624	32.593421
720.445856	13546.074676	32.598439
720.788877	13575.045820	32.603456
721.734112	13630.877673	32.608474
722.106906	13667.680953	32.613492
722.755622	13729.609905	32.618509
723.562070	13777.844307	32.623527
723.961973	13836.367009	32.628544
724.911123	13887.534666	32.633562
725.168592	13943.969233	32.638580
725.906836	14006.928326	32.643597
727.038373	14050.158285	32.648615
727.774058	14107.162589	32.653632
728.638725	14181.731849	32.658650
729.272055	14205.468809	32.663668
730.471777	14291.941411	32.668685
730.808137	14316.274874	32.673703
731.347129	14395.553231	32.678720
732.727372	14436.306918	32.683738
732.903449	14499.127396	32.688756
733.986278	14547.307149	32.693773
734.739415	14581.625010	32.698791
735.359930	14655.606400	32.703808
736.362919	14688.122708	32.708826
736.982777	14738.487519	32.713844
738.156672	14794.025691	32.718861
738.632985	14843.968939	32.723879
739.406161	14882.441567	32.728896
740.128501	14961.008610	32.733914
740.613948	14981.117709	32.738932
741.408596	15057.257490	32.743949
742.409255	15078.602380	32.748967
742.464856	15160.228818	32.753984
743.747116	15206.796512	32.759002
744.194836	15253.307491	32.764020
744.657309	15292.242725	32.769037
744.993315	15376.272741	32.774055
746.038734	15404.952705	32.779072
746.798416	15454.089519	32.784090
747.191978	15517.415356	32.789108
748.181420	15587.839444	32.794125
748.841858	15612.518471	32.799143
749.330750	15701.338591	32.804160
750.548923	15736.756724	32.809178
751.269502	15789.773675	32.814196
752.070745	15840.019258	32.819213
753.103023	15897.317604	32.824231
753.409539	15966.962761	32.829248
754.579742	16002.470728	32.834266
755.242972	16066.069717	32.839284
756.043762	16105.958094	32.844301
756.940880	16161.217502	32.849319
757.310265	16219.358083	32.854336
758.373349	16271.914962	32.859354
759.123161	16332.427872	32.864372
759.546433	16390.207526	32.869389
760.603080	16438.999581	32.874407
761.421178	16492.122215	32.879424
762.440290	16549.783209	32.884442
762.838414	16622.285607	32.889460
763.875064	16670.632238	32.894477
764.712913	16712.334045	32.899495
765.050365	16774.562632	32.904512
765.767941	16842.109775	32.909530
766.632806	16908.168009	32.914548
767.265329	16960.511079	32.919565
768.080042	17013.904327	32.924583
768.626737	17075.613476	32.929600
769.968324	17134.913517	32.934618
770.713002	17208.239583	32.939636
771.648867	17252.982828	32.944653
772.410157	17318.396386	32.949671
773.440816	17368.550905	32.954688
774.120761	17411.906555	32.959706
774.762725	17459.857321	32.964724
775.539439	17543.804501	32.969741
776.172402	17564.761348	32.974759
777.059254	17654.269075	32.979776
778.258880	17686.172807	32.984794
778.635113	17757.441005	32.989812
779.234658	17825.359051	32.994829
780.200786	17872.380618	32.999847
780.930886	17933.403410	33.004864
781.963221	17963.882667	33.009882
782.453817	18045.407002	33.014900
783.194194	18105.659588	33.019917
783.942642	18138.911214	33.024935
784.655765	18225.690191	33.029952
786.133266	18262.842396	33.034970
786.357389	18344.147345	33.039988
786.863503	18388.639274	33.045005
788.048393	18418.377255	33.050023
788.423655	18508.409139	33.055040
789.305226	18543.238437	33.060058
789.826621	18602.780587	33.065076
790.567530	18654.903090	33.070093
791.384533	18687.816249	33.075111
792.227094	18755.916418	33.080128
793.069179	18822.282717	33.085146
793.827858	18869.683448	33.090164
794.156149	18936.067846	33.095181
795.031085	19006.878538	33.100199
796.194095	19062.492335	33.105216
796.827540	19125.987992	33.110234
797.990737	19198.588347	33.115252
798.616184	19242.190874	33.120269
799.885916	19275.349760	33.125287
800.356460	19382.443626	33.130304
801.291902	19404.759988	33.135322
802.162481	19498.263362	33.140340
802.781273	19531.039384	33.145357
803.600670	19620.804636	33.150375
804.316000	19655.144761	33.155392
805.437808	19735.128592	33.160410
806.260334	19783.224348	33.165428
806.793852	19835.596434	33.170445
807.755134	19913.688507	33.175463
808.569440	19971.798235	33.180480
809.344320	20010.810702	33.185498
810.281354	20085.020205	33.190516
810.764947	20167.481253	33.195533
812.255141	20214.196762	33.200551
812.677761	20269.556321	33.205568
813.769256	20336.450055	33.210586
814.742607	20382.786879	33.215604
815.439786	20434.869153	33.220621
816.403121	20496.401944	33.225639
817.156356	20554.732247	33.230656
818.178545	20605.958548	33.235674
818.820964	20662.192485	33.240692
819.424680	20731.487471	33.245709
820.412165	20787.275942	33.250727
821.260968	20847.453769	33.255744
821.723004	20907.206319	33.260762
822.680836	20970.989390	33.265780
823.390471	21035.068560	33.270797
824.337105	21088.734001	33.275815
824.860785	21165.989652	33.280832
825.579892	21230.520542	33.285850
826.883449	21284.298765	33.290868
827.156158	21370.974371	33.295885
828.437573	21404.114288	33.300903
829.204760	21509.181864	33.305920
830.095664	21540.161808	33.310938
830.896655	21603.883822	33.315956
831.834796	21669.271966	33.320973
832.810266	21717.539524	33.325991
833.235720	21772.413299	33.331008
834.152682	21820.630634	33.336026
835.309254	21879.157624	33.341044
835.624353	21933.674652	33.346061
836.633572	21978.907133	33.351079
837.339746	22047.120149	33.356096
837.972422	22096.090020	33.361114
838.831543	22150.674785	33.366132
839.230220	22221.506538	33.371149
840.873104	22283.823023	33.376167
841.358756	22339.946161	33.381184
842.389550	22412.937718	33.386202
843.411809	22469.300391	33.391220
843.802906	22520.836596	33.396237
844.732061	22602.452718	33.401255
845.260915	22669.542047	33.406272
846.288431	22729.065418	33.411290
846.991553	22784.737313	33.416308
847.753177	22875.001762	33.421325
849.065115	22942.309434	33.426343
849.925498	23006.188343	33.431360
850.725212	23059.719293	33.436378
851.668252	23163.508156	33.441396
852.235053	23211.349933	33.446413
853.407266	23289.563066	33.451431
854.420427	23351.221589	33.456448
855.359060	23409.974051	33.461466
856.170436	23475.465481	33.466484
857.043055	23546.760182	33.471501
857.825789	23595.278413	33.476519
858.324139	23693.884837	33.481536
859.431976	23734.162636	33.486554
860.235695	23822.387367	33.491572
861.406377	23884.549837	33.496589
862.222879	23943.567103	33.501607
863.070124	24029.956339	33.506624
863.863824	24069.312230	33.511642
864.978873	24150.498747	33.516660
865.910564	24222.354992	33.521677
866.846628	24280.201336	33.526695
867.414497	24336.390936	33.531712
867.950609	24427.145155	33.536730
869.312479	24490.602087	33.541748
870.285970	24547.242234	33.546765
870.949206	24620.417479	33.551783
871.663970	24683.313361	33.556800
872.777758	24751.726804	33.561818
873.447831	24820.727100	33.566836
874.326730	24891.322641	33.571853
875.508432	24949.312713	33.576871
876.391321	25031.140122	33.581888
876.886915	25093.370656	33.586906
878.028886	25164.758941	33.591924
878.936374	25214.272908	33.596941
879.258242	25283.366071	33.601959
880.387280	25346.033219	33.606976
880.974695	25397.356106	33.611994
881.912914	25454.574624	33.617012
882.773266	25542.269738	33.622029
883.818681	25587.468979	33.627047
884.641418	25658.219436	33.632064
885.489574	25728.676271	33.637082
886.408651	25779.819204	33.642100
887.306481	25853.919887	33.647117
888.259345	25915.523128	33.652135
889.205526	25981.101108	33.657152
889.855308	26052.015539	33.662170
891.024067	26129.221479	33.667188
891.438033	26190.721691	33.672205
892.572125	26273.633330	33.677223
893.653638	26333.295551	33.682240
894.056335	26400.173334	33.687258
895.370760	26474.927472	33.692276
896.175584	26540.268698	33.697293
897.303827	26613.000936	33.702311
898.031621	26707.548127	33.707328
898.838710	26756.539280	33.712346
900.003447	26820.860902	33.717364
900.890180	26905.145762	33.722381
902.058170	26975.662754	33.727399
903.051902	27039.622504	33.732416
903.425943	27120.379562	33.737434
904.352793	27169.192993	33.742452
905.245094	27246.322261	33.747469
906.111810	27357.912150	33.752487
907.357977	27401.899693	33.757504
908.009594	27512.715789	33.762522
909.240005	27552.865581	33.767540
909.958415	27631.536219	33.772557
911.214167	27708.523991	33.777575
912.014422	27786.493001	33.782592
912.637793	27858.157819	33.787610
913.676273	27924.723321	33.792628
914.619385	28002.026966	33.797645
915.531258	28084.753265	33.802663
916.380275	28156.078598	33.807680
917.348471	28228.081753	33.812698
918.546183	28291.404214	33.817716
919.478688	28370.039657	33.822733
920.526902	28423.175606	33.827751
921.502498	28499.427017	33.832768
922.221018	28582.972940	33.837786
923.140710	28640.992870	33.842804
924.152422	28730.370524	33.847821
925.222302	28794.509495	33.852839
926.099861	28846.734827	33.857856
926.924101	28927.352069	33.862874
927.715806	28974.660804	33.867892
928.498852	29078.868839	33.872909
929.708444	29112.639860	33.877927
930.504862	29187.975964	33.882944
931.093117	29260.586261	33.887962
932.167894	29311.847245	33.892980
933.047232	29391.662232	33.897997
933.692361	29449.638929	33.903015
934.533179	29508.298557	33.908032
935.120867	29607.693746	33.913050
936.122448	29662.629797	33.918068
936.732833	29762.175177	33.923085
937.547757	29849.002719	33.928103
938.808996	29927.349150	33.933120
939.513382	30013.353630	33.938138
940.596570	30089.592250	33.943156
941.556617	30176.696296	33.948173
942.598219	30266.028800	33.953191
943.629853	30351.978268	33.958208
944.500616	30427.030920	33.963226
945.782321	30505.305963	33.968244
946.550110	30594.581400	33.973261
947.637906	30676.881604	33.978279
948.912045	30766.052196	33.983296
949.637304	30842.720074	33.988314
950.632902	30906.898124	33.993332
951.834354	31015.603442	33.998349
952.664566	31070.171212	34.003367
953.589752	31165.224426	34.008384
954.827900	31235.021491	34.013402
955.416034	31330.197063	34.018420
956.254912	31411.137908	34.023437
957.102788	31490.170705	34.028455
958.652346	31569.188377	34.033472
959.394924	31670.888281	34.038490
960.440663	31742.464406	34.043508
961.806922	31816.213690	34.048525
962.650797	31912.466238	34.053543
963.410229	31999.151704	34.058560
964.638319	32065.220145	34.063578
965.803414	32132.397424	34.068596
966.507687	32202.163777	34.073613
967.189524	32294.214056	34.078631
968.601521	32372.779930	34.083648
969.095008	32467.152839	34.088666
970.115354	32537.242294	34.093684
971.137591	32624.213929	34.098701
972.074009	32705.545984	34.103719
973.442466	32788.491474	34.108736
973.928739	32883.960204	34.113754
975.123385	32957.068895	34.118772
975.954562	33042.482768	34.123789
976.829971	33130.580624	34.128807
978.086790	33204.511181	34.133824
978.808432	33297.410310	34.138842
979.860505	33376.292018	34.143860
980.990881	33456.201959	34.148877
981.677734	33548.178056	34.153895
982.805654	33607.779248	34.158912
983.784871	33681.760843	34.163930
984.768533	33761.356710	34.168948
985.723523	33830.128547	34.173965
986.237498	33903.439580	34.178983
987.713502	33971.705094	34.184000
988.464437	34062.252048	34.189018
989.826429	34133.061588	34.194036
990.578765	34202.384243	34.199053
991.776299	34288.630579	34.204071
992.865017	34361.503834	34.209088
993.692293	34443.760320	34.214106
994.696161	34511.365461	34.219124
995.492298	34601.960191	34.224141
996.235994	34697.997442	34.229159
997.294621	34779.512580	34.234176
998.444068	34859.142522	34.239194
999.380374	34934.793306	34.244212
1000.281951	35042.100577	34.249229
1001.036701	35113.416052	34.254247
1002.711727	35215.359889	34.259264
1003.380118	35303.421844	34.264282
1004.634538	35372.757788	34.269300
1005.465555	35469.208080	34.274317
1006.623988	35560.630039	34.279335
1007.543183	35658.599692	34.284352
1008.707349	35738.281950	34.289370
1009.635449	35822.165571	34.294388
1010.806264	35913.395169	34.299405
1012.184597	36002.382033	34.304423
1013.153568	36069.415768	34.309440
1013.952694	36173.557403	34.314458
1015.267928	36258.258157	34.319476
1015.837225	36347.269945	34.324493
1016.799527	36423.836155	34.329511
1017.619218	36503.643086	34.334528
1018.764427	36619.594197	34.339546
1019.661151	36691.289542	34.344564
1020.920045	36805.918482	34.349581
1021.833952	36873.195955	34.354599
1022.890488	36998.315711	34.359616
1024.383786	37049.053384	34.364634
1025.174511	37178.995369	34.369652
1026.020997	37229.395045	34.374669
1026.920680	37347.897033	34.379687
1028.678632	37401.232904	34.384704
1029.698641	37523.789367	34.389722
1030.758918	37568.686766	34.394740
1031.973575	37669.686143	34.399757
1032.709870	37740.877020	34.404775
1034.051473	37817.393988	34.409792
1034.561833	37944.012466	34.414810
1035.361843	38018.033940	34.419828
1036.936699	38091.041656	34.424845
1037.239360	38189.917255	34.429863
1038.426775	38237.265299	34.434880
1039.497309	38356.206024	34.439898
1040.382247	38398.473650	34.444916
1041.240467	38519.491127	34.449933
1042.172974	38556.346619	34.454951
1043.157886	38668.695158	34.459968
1043.879180	38760.251412	34.464986
1045.371534	38829.455033	34.470004
1046.641214	38942.953688	34.475021
1047.193945	39021.504758	34.480039
1048.576013	39113.467103	34.485056
1049.733225	39197.482510	34.490074
1050.479665	39305.303724	34.495092
1051.708143	39379.486913	34.500109
1052.699317	39510.853005	34.505127
1053.990331	39585.355123	34.510144
1054.401872	39687.809393	34.515162
1055.457611	39765.200619	34.520180
1056.980460	39890.236109	34.525197
1057.720383	39967.268517	34.530215
1059.113109	40049.432583	34.535232
1060.214313	40185.748751	34.540250
1060.986353	40259.819176	34.545268
1061.966795	40373.620988	34.550285
1063.186709	40470.828093	34.555303
1064.309008	40570.301519	34.560320
1065.560363	40671.748212	34.565338
1066.522907	40797.294229	34.570356
1068.068917	40873.868211	34.575373
1068.826611	40973.454027	34.580391
1069.544253	41056.581891	34.585408
1070.931945	41176.199984	34.590426
1071.822430	41262.245536	34.595444
1073.314248	41367.330871	34.600461
1074.521855	41494.464163	34.605479
1075.605066	41584.807934	34.610496
1076.591825	41654.653881	34.615514
1077.447846	41772.613402	34.620532
1078.878610	41862.288322	34.625549
1079.489911	41959.726879	34.630567
1080.885200	42068.623058	34.635584
1082.286814	42168.577056	34.640602
1083.307109	42263.615098	34.645620
1084.718088	42358.061630	34.650637
1085.484888	42463.764221	34.655655
1086.823986	42547.407649	34.660672
1087.707846	42641.198354	34.665690
1088.293835	42742.490329	34.670708
1090.178742	42842.418695	34.675725
1090.900735	42933.962551	34.680743
1091.958893	43016.804462	34.685760
1093.113998	43128.704259	34.690778
1094.551298	43182.205573	34.695796
1095.623576	43312.840418	34.700813
1096.522816	43401.945525	34.705831
1097.455974	43468.684603	34.710848
1098.649779	43544.249355	34.715866
1099.327940	43654.749038	34.720884
1100.752783	43704.389860	34.725901
1101.772761	43819.895856	34.730919
1102.695210	43881.313611	34.735936
1103.991400	44004.319103	34.740954
1104.600340	44069.109008	34.745972
1105.834956	44174.930641	34.750989
1106.858169	44265.228643	34.756007
1107.781706	44341.723128	34.761024
1108.543629	44478.501166	34.766042
1109.736819	44556.395325	34.771060
1111.027826	44676.873331	34.776077
1112.246514	44773.587650	34.781095
1112.985434	44879.817350	34.786112
1114.173079	44990.257138	34.791130
1115.539315	45101.782808	34.796148
1116.228865	45203.202060	34.801165
1117.321856	45333.618566	34.806183
1118.645625	45417.546490	34.811200
1119.845221	45558.121598	34.816218
1120.660325	45676.186844	34.821236
1122.494604	45771.442809	34.826253
1123.639680	45871.809223	34.831271
1124.294284	46007.723550	34.836288
1126.215176	46099.027195	34.841306
1126.785233	46212.402826	34.846324
1128.248194	46322.696858	34.851341
1129.492557	46414.731261	34.856359
1130.633034	46538.836336	34.861376
1132.330608	46622.231071	34.866394
1132.956969	46766.434263	34.871412
1134.621026	46841.380159	34.876429
1135.276281	46955.409591	34.881447
1136.636338	47047.630844	34.886464
1137.409349	47159.869777	34.891482
1138.633885	47261.704921	34.896500
1139.484564	47363.735781	34.901517
1140.805276	47479.823988	34.906535
1142.158449	47589.361009	34.911552
1143.386715	47688.705525	34.916570
1144.053047	47821.842945	34.921588
1145.169362	47909.895409	34.926605
1146.605600	48028.278427	34.931623
1147.600050	48152.793603	34.936640
1149.085472	48258.454974	34.941658
1149.819528	48351.407360	34.946676
1151.073432	48486.750200	34.951693
1152.475215	48584.567127	34.956711
1153.681136	48691.985698	34.961728
1154.787754	48818.330414	34.966746
1156.057974	48915.444380	34.971764
1156.817454	49022.437418	34.976781
1158.025428	49118.779877	34.981799
1158.708584	49227.793099	34.986816
1160.299469	49326.420237	34.991834
1161.408410	49422.780101	34.996852
1162.329161	49530.059789	35.001869
1163.840953	49619.506230	35.006887
1164.372462	49746.485453	35.011904
1165.952033	49823.451755	35.016922
1166.531923	49960.525501	35.021940
1167.892693	50056.511122	35.026957
1169.419104	50161.587268	35.031975
1170.414605	50272.444246	35.036992
1172.101443	50383.422331	35.042010
1172.958344	50495.533414	35.047028
1174.246927	50610.198873	35.052045
1175.313953	50718.371290	35.057063
1176.548545	50824.693747	35.062080
1178.200339	50930.830579	35.067098
1179.154434	51053.879909	35.072116
1180.362846	51146.184542	35.077133
1181.189830	51258.002226	35.082151
1182.256806	51378.697445	35.087168
1183.860440	51500.469464	35.092186
1184.486775	51619.819438	35.097204
1185.996185	51736.757592	35.102221
1186.984508	51850.049176	35.107239
1187.961641	51973.511425	35.112256
1189.420572	52095.335748	35.117274
1190.636691	52216.890233	35.122292
1191.542346	52344.910900	35.127309
1193.017179	52456.298513	35.132327
1193.941600	52588.038783	35.137344
1195.273522	52707.185949	35.142362
1196.943071	52843.019686	35.147380
1198.298856	52948.918891	35.152397
1199.391970	53074.106073	35.157415
1200.637106	53187.680857	35.162432
1202.062668	53298.510273	35.167450
1202.885593	53433.387924	35.172468
1203.893249	53553.431776	35.177485
1205.493488	53672.126049	35.182503
1206.443222	53794.699326	35.187520
1207.609362	53912.536290	35.192538
1208.852736	54040.029235	35.197556
1210.040832	54161.086825	35.202573
1211.219224	54290.687610	35.207591
1212.415337	54406.430420	35.212608
1213.982252	54532.530810	35.217626
1215.260704	54657.642670	35.222644
1215.893759	54778.192933	35.227661
1217.598256	54897.958137	35.232679
1218.820112	55018.662569	35.237696
1220.084809	55151.715181	35.242714
1221.209970	55283.642011	35.247732
1222.299261	55390.219696	35.252749
1223.661884	55504.102811	35.257767
1224.523701	55624.158299	35.262784
1225.970556	55729.099710	35.267802
1227.112111	55838.124314	35.272820
1228.020947	55957.423263	35.277837
1229.346386	56076.451574	35.282855
1230.325801	56195.128478	35.287872
1231.955655	56306.549850	35.292890
1232.894628	56420.411346	35.297908
1234.534252	56539.945130	35.302925
1235.517838	56664.107516	35.307943
1236.468214	56791.634746	35.312960
1237.817653	56898.539730	35.317978
1239.067513	57028.416933	35.322996
1239.740513	57170.221462	35.328013
1241.046934	57297.862905	35.333031
1242.591101	57431.790512	35.338048
1243.849133	57558.014580	35.343066
1245.081228	57701.925149	35.348084
1246.387422	57831.233990	35.353101
1247.714184	57955.975600	35.358119
1248.861879	58101.743179	35.363136
1250.124128	58231.563765	35.368154
1251.525493	58368.182186	35.373172
1252.777831	58500.702288	35.378189
1254.129549	58629.766399	35.383207
1255.433616	58769.863342	35.388224
1256.745359	58896.495283	35.393242
1257.927050	59031.679189	35.398260
1259.177776	59167.977031	35.403277
1260.606747	59311.758336	35.408295
1261.774277	59438.167493	35.413312
1263.402830	59563.932767	35.418330
1264.796894	59693.919450	35.423348
1266.337773	59831.429439	35.428365
1267.871912	59959.400351	35.433383
1268.839345	60093.000069	35.438400
1269.790643	60215.824360	35.443418
1271.163985	60334.048482	35.448436
1272.200482	60469.988951	35.453453
1273.945539	60596.238382	35.458471
1275.082402	60739.635131	35.463488
1276.445993	60867.159471	35.468506
1278.181872	60981.440157	35.473524
1279.245164	61110.257916	35.478541
1280.822865	61234.290179	35.483559
1281.936364	61359.401140	35.488576
1283.517813	61485.224756	35.493594
1284.428948	61605.402796	35.498612
1285.539836	61725.246726	35.503629
1287.124856	61847.586292	35.508647
1287.717548	61990.324469	35.513664
1289.372363	62115.149169	35.518682
1290.632895	62234.609434	35.523700
1291.972001	62356.833530	35.528717
1293.236960	62480.756398	35.533735
1294.293032	62597.220116	35.538752
1295.472488	62709.143117	35.543770
1296.945583	62826.902927	35.548788
1297.998686	62936.785377	35.553805
1299.395458	63070.685401	35.558823
1300.317787	63196.344208	35.563840
1301.540430	63320.209845	35.568858
1302.857963	63440.676027	35.573876
1304.001561	63580.468190	35.578893
1305.367543	63707.948255	35.583911
1306.443865	63847.686769	35.588928
1308.027472	63971.335073	35.593946
1308.997805	64109.693413	35.598964
1310.414028	64258.216806	35.603981
1312.042568	64378.172128	35.608999
1313.275004	64523.243563	35.614016
1314.775621	64661.461618	35.619034
1316.087616	64795.482040	35.624052
1316.883798	64938.086917	35.629069
1318.575828	65073.902671	35.634087
1319.868825	65218.837134	35.639104
1321.205234	65357.383202	35.644122
1322.521495	65507.309171	35.649140
1323.665928	65647.356402	35.654157
1325.304981	65781.950764	35.659175
1326.469239	65939.000769	35.664192
1328.318224	66074.681834	35.669210
1329.438991	66219.130140	35.674228
1330.633930	66373.045810	35.679245
1332.109013	66506.985979	35.684263
1333.183394	66656.214018	35.689280
1334.927539	66791.332522	35.694298
1336.418130	66941.434651	35.699316
1337.172319	67082.937766	35.704333
1338.973473	67218.972471	35.709351
1339.979833	67378.582928	35.714368
1341.537368	67521.979828	35.719386
1343.150047	67657.311656	35.724404
1344.036972	67806.202529	35.729421
1345.279413	67970.628706	35.734439
1346.851278	68115.919715	35.739456
1348.316277	68256.775159	35.744474
1349.970075	68402.927075	35.749492
1351.059681	68557.167499	35.754509
1352.437318	68698.715993	35.759527
1353.731846	68846.210780	35.764544
1354.770330	68994.454940	35.769562
1356.145966	69157.037933	35.774580
1357.625636	69314.804396	35.779597
1359.197912	69452.290512	35.784615
1360.549064	69607.508506	35.789632
1361.787406	69750.571440	35.794650
1363.119993	69902.414756	35.799668
1364.425490	70053.878172	35.804685
1365.905789	70184.244947	35.809703
1367.403028	70317.427677	35.814720
1368.496255	70442.917109	35.819738
1370.141774	70580.374253	35.824756
1371.569308	70720.887023	35.829773
1372.645723	70862.625449	35.834791
1374.151164	70994.023462	35.839808
1375.492729	71118.858573	35.844826
1376.845926	71258.881557	35.849844
1377.943355	71399.167328	35.854861
1379.616453	71543.905447	35.859879
1381.011003	71689.396556	35.864896
1382.227505	71838.644880	35.869914
1383.656762	71969.954107	35.874932
1384.803717	72122.532802	35.879949
1386.179932	72272.384548	35.884967
1387.405526	72422.166590	35.889984
1389.127722	72575.617775	35.895002
1390.432639	72724.056267	35.900020
1391.261667	72889.442462	35.905037
1392.772777	73039.202746	35.910055
1394.381162	73212.378854	35.915072
1395.533641	73364.789307	35.920090
1397.228847	73520.943931	35.925108
1398.688786	73689.566577	35.930125
1400.014302	73853.359007	35.935143
1401.533457	74000.995747	35.940160
1402.888929	74170.808094	35.945178
1404.356174	74327.226437	35.950196
1405.738225	74488.992965	35.955213
1407.685300	74642.455954	35.960231
1409.034794	74802.865233	35.965248
1410.526388	74970.773263	35.970266
1412.070539	75126.528418	35.975284
1413.425638	75283.471291	35.980301
1415.123992	75424.094404	35.985319
1417.009973	75570.091907	35.990336
1418.203039	75714.557496	35.995354
1419.724519	75848.493952	36.000372
1420.854862	76032.336905	36.005389
1422.582439	76180.203046	36.010407
1424.240389	76319.726567	36.015424
1425.024842	76461.424859	36.020442
1426.744423	76625.208891	36.025460
1427.949419	76771.550841	36.030477
1429.367495	76914.421918	36.035495
1430.926593	77071.409491	36.040512
1432.055627	77240.689659	36.045530
1433.324677	77404.564235	36.050548
1434.612318	77563.191427	36.055565
1436.606987	77713.314235	36.060583
1437.939127	77872.037891	36.065600
1439.018197	78039.752585	36.070618
1440.793694	78194.628744	36.075636
1441.961035	78351.195472	36.080653
1443.558649	78495.875742	36.085671
1444.560317	78637.959204	36.090688
1446.336071	78790.709836	36.095706
1447.725683	78926.274040	36.100724
1448.832795	79086.300701	36.105741
1450.437611	79233.203598	36.110759
1451.413113	79374.164923	36.115776
1452.574070	79546.132820	36.120794
1454.159074	79704.558732	36.125812
1455.645219	79872.280646	36.130829
1456.563467	80033.817473	36.135847
1458.469323	80190.280897	36.140864
1459.586978	80360.486285	36.145882
1460.969295	80556.858300	36.150900
1462.588087	80715.021133	36.155917
1463.999431	80897.181827	36.160935
1465.800696	81059.996001	36.165952
1467.181203	81251.172506	36.170970
1468.565453	81423.702136	36.175988
1469.958704	81596.857592	36.181005
1471.719275	81768.837224	36.186023
1473.286577	81959.415320	36.191040
1474.773554	82139.855458	36.196058
1476.231866	82299.364453	36.201076
1477.871103	82484.436106	36.206093
1479.073503	82665.210490	36.211111
1480.743894	82842.763819	36.216128
1482.006843	83029.050661	36.221146
1483.426870	83200.261738	36.226164
1484.966088	83380.995114	36.231181
1486.680900	83574.339860	36.236199
1488.443526	83742.953163	36.241216
1489.864507	83943.795402	36.246234
1491.837997	84105.069730	36.251252
1493.235555	84298.117509	36.256269
1494.471997	84488.233825	36.261287
1496.340551	84627.799124	36.266304
1497.507728	84832.502537	36.271322
1499.599781	85007.528801	36.276340
1500.869283	85181.713547	36.281357
1502.007618	85363.924920	36.286375
1503.727723	85527.324187	36.291392
1504.894670	85727.534601	36.296410
1506.978310	85890.107540	36.301428
1508.107544	86098.584908	36.306445
1509.605431	86259.432784	36.311463
1511.444792	86429.952198	36.316480
1512.842061	86647.939898	36.321498
1514.786174	86796.688393	36.326516
1515.959545	87004.674421	36.331533
1517.607907	87164.974091	36.336551
1518.923288	87354.787381	36.341568
1520.540096	87541.279045	36.346586
1522.202283	87699.923849	36.351604
1523.669134	87880.808282	36.356621
1525.000885	88046.539662	36.361639
1526.978590	88194.849913	36.366656
1527.766363	88367.878866	36.371674
1529.651936	88508.434410	36.376692
1531.130895	88707.655667	36.381709
1532.180833	88839.663914	36.386727
1533.728964	89036.948530	36.391744
1534.724763	89197.133071	36.396762
1536.644394	89381.638560	36.401780
1537.873488	89550.749396	36.406797
1538.717177	89763.057726	36.411815
1541.344672	89923.861102	36.416832
1542.401392	90137.410353	36.421850
1544.042321	90317.566613	36.426868
1545.674132	90486.171752	36.431885
1547.263144	90692.400835	36.436903
1548.593331	90879.485433	36.441920
1550.172575	91081.368714	36.446938
1551.509694	91241.273774	36.451956
1553.513885	91472.140590	36.456973
1554.570106	91657.498230	36.461991
1556.379755	91858.574178	36.467008
1557.805002	92072.153364	36.472026
1559.265679	92258.716731	36.477044
1560.944804	92450.116940	36.482061
1562.298616	92678.462398	36.487079
1564.165198	92871.518858	36.492096
1565.496837	93081.473326	36.497114
1567.251143	93287.346351	36.502132
1569.171528	93487.597352	36.507149
1570.556781	93704.386459	36.512167
1572.883197	93907.258548	36.517184
1574.293659	94080.341318	36.522202
1575.715456	94310.628294	36.527220
1577.516659	94498.339269	36.532237
1579.103037	94691.854597	36.537255
1580.703669	94890.448575	36.542272
1582.055504	95115.321529	36.547290
1584.006414	95295.083399	36.552308
1585.419725	95501.847083	36.557325
1587.098901	95707.355935	36.562343
1588.820422	95890.258548	36.567360
1590.630114	96073.458604	36.572378
1592.230408	96319.273734	36.577396
1593.796734	96496.987219	36.582413
1595.662116	96674.622973	36.587431
1597.337837	96901.075456	36.592448
1598.841371	97067.435796	36.597466
1600.724402	97289.715760	36.602484
1602.112470	97448.885615	36.607501
1603.637895	97655.916966	36.612519
1605.079576	97873.351062	36.617536
1606.963264	98034.046820	36.622554
1608.512335	98253.068024	36.627572
1610.325581	98425.747040	36.632589
1611.655634	98635.798049	36.637607
1613.227931	98777.575746	36.642624
1614.477669	98954.416162	36.647642
1615.742062	99160.515741	36.652660
1617.858416	99325.947529	36.657677
1618.658593	99528.245974	36.662695
1620.445571	99717.400802	36.667712
1621.974255	99892.578205	36.672730
1623.773778	100106.807051	36.677748
1624.911620	100307.692143	36.682765
1626.385441	100500.376592	36.687783
1628.098529	100688.842542	36.692800
1629.747644	100930.884542	36.697818
1631.264157	101104.225613	36.702836
1633.391978	101345.050719	36.707853
1634.478153	101527.036555	36.712871
1636.279787	101742.691209	36.717888
1637.811007	101953.385937	36.722906
1639.615492	102182.154351	36.727924
1641.172000	102396.753051	36.732941
1643.044421	102582.178269	36.737959
1644.872240	102827.786676	36.742976
1646.425447	103045.011457	36.747994
1647.524869	103248.028859	36.753012
1649.869639	103448.243216	36.758029
1651.188137	103688.879406	36.763047
1653.015724	103903.410911	36.768064
1654.832008	104114.029221	36.773082
1656.312672	104360.145440	36.778100
1658.314800	104560.202220	36.783117
1659.630010	104794.807010	36.788135
1661.804741	105005.616821	36.793152
1663.356643	105233.214797	36.798170
1664.803425	105450.845717	36.803188
1666.902330	105678.095303	36.808205
1668.430900	105899.602913	36.813223
1670.310081	106108.286191	36.818240
1671.818138	106344.818494	36.823258
1673.813346	106551.405163	36.828276
1675.380871	106766.731687	36.833293
1677.317785	107000.341858	36.838311
1679.042217	107211.780673	36.843328
1680.582747	107429.047692	36.848346
1682.186318	107643.844759	36.853364
1684.091782	107853.336520	36.858381
1685.814221	108080.966200	36.863399
1687.409994	108293.422275	36.868416
1689.179719	108527.618136	36.873434
1690.792319	108734.493212	36.878452
1692.362110	108954.168056	36.883469
1694.178478	109209.591076	36.888487
1695.828454	109389.705913	36.893504
1697.693502	109614.865295	36.898522
1699.369244	109846.563425	36.903540
1701.030410	110056.967522	36.908557
1702.253700	110252.334489	36.913575
1703.918785	110464.304858	36.918592
1705.523455	110676.052463	36.923610
1707.117562	110861.662147	36.928628
1708.822615	111072.719969	36.933645
1710.307924	111290.505048	36.938663
1711.780237	111498.236058	36.943680
1713.369933	111732.833102	36.948698
1714.820201	111966.580990	36.953716
1716.811317	112183.540381	36.958733
1718.435072	112414.397476	36.963751
1720.179826	112639.363179	36.968768
1722.090912	112858.613704	36.973786
1723.580955	113102.354982	36.978804
1725.509736	113335.818245	36.983821
1727.137980	113602.856889	36.988839
1728.732584	113797.452306	36.993856
1730.775173	114061.461108	36.998874
1732.180006	114278.145727	37.003892
1734.180227	114535.715469	37.008909
1736.074283	114751.326263	37.013927
1737.575135	115008.119183	37.018944
1739.592508	115231.153082	37.023962
1741.491291	115483.779008	37.028980
1743.444318	115712.582097	37.033997
1744.753503	115959.019844	37.039015
1746.784089	116205.642995	37.044032
1748.861889	116446.550438	37.049050
1750.373103	116686.651114	37.054068
1752.083324	116914.389332	37.059085
1753.936271	117163.550804	37.064103
1755.673926	117412.467103	37.069120
1757.897813	117652.533362	37.074138
1759.615914	117879.044324	37.079156
1761.950053	118103.572696	37.084173
1763.720995	118347.528934	37.089191
1765.397802	118586.468824	37.094208
1767.400031	118822.598665	37.099226
1769.349892	119043.802508	37.104244
1771.752228	119250.297401	37.109261
1773.342221	119493.729696	37.114279
1774.869310	119706.528051	37.119296
1776.881628	119935.055565	37.124314
1778.320361	120164.505650	37.129332
1780.375456	120384.779774	37.134349
1781.775556	120612.631610	37.139367
1783.579216	120841.592807	37.144384
1785.346167	121071.600319	37.149402
1786.843875	121313.633214	37.154420
1788.615662	121535.146154	37.159437
1790.551172	121762.473404	37.164455
1792.096767	122033.216254	37.169472
1794.081147	122231.271361	37.174490
1795.620338	122483.237754	37.179508
1797.666310	122692.330481	37.184525
1798.526989	122947.056039	37.189543
1800.205126	123154.311024	37.194560
1802.190168	123366.458441	37.199578
1803.423743	123614.253844	37.204596
1805.741314	123829.771881	37.209613
1807.242292	124071.588872	37.214631
1808.663067	124309.570345	37.219648
1810.438372	124544.863113	37.224666
1812.217449	124794.964087	37.229684
1813.985596	125034.353461	37.234701
1815.768429	125290.639599	37.239719
1817.870540	125536.237623	37.244736
1819.727584	125782.598791	37.249754
1821.045904	126046.920506	37.254772
1823.228167	126300.961487	37.259789
1825.154551	126555.374815	37.264807
1827.036483	126810.139598	37.269824
1828.836852	127056.914035	37.274842
1830.748387	127322.167373	37.279860
1832.489900	127576.252246	37.284877
1834.300694	127832.190617	37.289895
1835.754147	128105.593527	37.294912
1838.397254	128357.160993	37.299930
1840.026041	128630.718649	37.304948
1842.100855	128886.650277	37.309965
1844.030557	129150.778296	37.314983
1845.584876	129419.934406	37.320000
1847.667569	129672.768336	37.325018
1849.388425	129947.350556	37.330036
1851.541632	130190.929977	37.335053
1853.336611	130469.407534	37.340071
1854.771121	130730.892746	37.345088
1857.349372	131001.865311	37.350106
1859.098653	131282.030536	37.355124
1860.970542	131529.847119	37.360141
1863.142387	131795.798833	37.365159
1864.421368	132068.318234	37.370176
1866.512571	132332.349383	37.375194
1868.406769	132609.261395	37.380212
1870.786670	132871.313283	37.385229
1872.286468	133141.020599	37.390247
1874.085784	133417.132015	37.395264
1875.901762	133678.596681	37.400282
1877.876501	133957.916401	37.405300
1879.924971	134241.091642	37.410317
1881.576193	134510.724521	37.415335
1883.404923	134775.402852	37.420352
1885.626609	135042.225971	37.425370
1887.106283	135326.566554	37.430388
1889.470062	135591.864366	37.435405
1891.408324	135869.649919	37.440423
1892.778607	136146.552599	37.445440
1895.207581	136412.620535	37.450458
1896.928882	136686.342801	37.455476
1898.805763	136948.613107	37.460493
1900.424507	137211.332238	37.465511
1902.357966	137479.896203	37.470528
1904.361401	137715.783116	37.475546
1906.144705	137977.760697	37.480564
1908.424095	138184.499771	37.485581
1910.054669	138469.873504	37.490599
1912.099746	138697.524678	37.495616
1914.071134	138964.816263	37.500634
1916.203298	139183.624608	37.505652
1918.022556	139479.610459	37.510669
1920.628466	139678.400368	37.515687
1922.851435	139953.011164	37.520704
1924.795566	140173.643526	37.525722
1926.414767	140425.023433	37.530740
1928.366802	140667.937587	37.535757
1930.252088	140916.351864	37.540775
1931.999842	141194.255826	37.545792
1933.548143	141415.276982	37.550810
1935.453777	141708.787137	37.555828
1937.331797	141934.829241	37.560845
1939.213574	142222.949138	37.565863
1941.175841	142486.712212	37.570880
1943.258631	142753.081990	37.575898
1944.761105	143010.826325	37.580916
1946.795587	143295.180564	37.585933
1948.921492	143577.152811	37.590951
1950.639711	143844.299727	37.595968
1952.415128	144116.788603	37.600986
1954.353472	144412.157399	37.606004
1956.359983	144677.618065	37.611021
1959.039009	144961.353071	37.616039
1960.721822	145251.915903	37.621056
1962.741980	145519.232186	37.626074
1964.470960	145802.073600	37.631092
1966.693343	146094.333217	37.636109
1969.063513	146364.719372	37.641127
1970.693732	146650.043196	37.646144
1972.947222	146932.013013	37.651162
1975.012373	147209.160360	37.656180
1976.677647	147469.463753	37.661197
1979.240228	147773.055409	37.666215
1981.160098	148052.324773	37.671232
1983.240727	148320.529950	37.676250
1985.122889	148603.575027	37.681268
1986.996674	148888.791646	37.686285
1989.047966	149154.980240	37.691303
1991.031723	149449.577854	37.696320
1992.935440	149716.314277	37.701338
1995.284230	149991.273071	37.706356
1996.941562	150292.636359	37.711373
1998.884417	150562.999244	37.716391
2000.665529	150842.251537	37.721408
2002.947755	151115.100649	37.726426
2004.913017	151414.447808	37.731444
2006.724781	151693.398278	37.736461
2009.103037	151948.363564	37.741479
2011.050216	152200.660812	37.746496
2013.074811	152442.640503	37.751514
2015.331524	152715.950753	37.756532
2016.904240	152965.029656	37.761549
2018.654016	153210.722595	37.766567
2020.467583	153497.206305	37.771584
2022.663437	153737.963867	37.776602
2024.524160	154031.430553	37.781620
2026.421787	154305.711076	37.786637
2028.428560	154575.703773	37.791655
2030.118669	154853.609821	37.796672
2031.700437	155140.258528	37.801690
2034.219710	155437.233886	37.806708
2035.868842	155753.102538	37.811725
2037.522903	156022.985306	37.816743
2039.382360	156336.759295	37.821760
2041.926767	156634.451225	37.826778
2043.739290	156952.283124	37.831796
2045.947244	157253.076968	37.836813
2048.215164	157550.757359	37.841831
2049.932264	157885.211077	37.846848
2052.130041	158187.916734	37.851866
2054.419080	158494.199082	37.856884
2056.886146	158806.314233	37.861901
2058.993705	159105.973585	37.866919
2061.047694	159440.832701	37.871936
2062.967446	159726.007885	37.876954
2065.156683	160048.234055	37.881972
2067.396969	160364.697936	37.886989
2069.891231	160658.399918	37.892007
2071.609965	160968.471956	37.897024
2073.924297	161267.470236	37.902042
2076.521026	161585.879475	37.907060
2078.370396	161894.721475	37.912077
2080.638986	162207.862112	37.917095
2082.541649	162502.611656	37.922112
2084.948630	162799.021023	37.927130
2086.751588	163111.203518	37.932148
2088.560177	163422.981998	37.937165
2091.317267	163725.329365	37.942183
2093.297118	164027.181134	37.947200
2095.460029	164329.792674	37.952218
2097.566260	164643.068984	37.957236
2099.297052	164954.150045	37.962253
2101.694488	165260.549543	37.967271
2103.310208	165561.926404	37.972288
2105.615391	165870.108521	37.977306
2107.817328	166186.718411	37.982324
2109.855451	166507.707296	37.987341
2112.638311	166814.667335	37.992359
2114.470048	167124.951614	37.997376
2116.375637	167437.243416	38.002394
2118.783933	167742.634341	38.007412
2120.711471	168042.307598	38.012429
2122.642157	168329.793686	38.017447
2124.578501	168623.686389	38.022464
2126.514024	168910.161414	38.027482
2128.614701	169202.814879	38.032500
2130.703141	169482.953325	38.037517
2133.172293	169791.775825	38.042535
2135.501102	170081.203414	38.047552
2137.492742	170381.240084	38.052570
2139.313004	170664.689592	38.057588
2141.281450	170975.072419	38.062605
2143.497867	171265.757130	38.067623
2145.186252	171575.529580	38.072640
2147.621102	171877.651262	38.077658
2149.494273	172196.925680	38.082676
2150.986378	172524.787523	38.087693
2153.486561	172841.367277	38.092711
2155.737252	173165.105598	38.097728
2157.910277	173495.176218	38.102746
2160.145972	173817.488795	38.107764
2162.297830	174149.876968	38.112781
2164.460517	174473.386186	38.117799
2166.460033	174814.506441	38.122816
2168.598095	175142.452305	38.127834
2171.121300	175477.608840	38.132852
2173.288277	175823.493692	38.137869
2175.689450	176143.883055	38.142887
2177.653782	176489.425119	38.147904
2180.025208	176824.515330	38.152922
2182.270979	177150.861800	38.157940
2184.708045	177486.860429	38.162957
2186.720605	177832.393440	38.167975
2188.725141	178170.216990	38.172992
2191.078720	178512.758219	38.178010
2193.487906	178849.558883	38.183028
2195.645440	179200.408804	38.188045
2197.989664	179533.672851	38.193063
2200.233732	179872.449048	38.198080
2201.922133	180218.928569	38.203098
2204.593038	180548.647047	38.208116
2206.783881	180894.785937	38.213133
2208.901176	181252.180665	38.218151
2211.214671	181607.491808	38.223168
2213.451905	181944.547268	38.228186
2216.236433	182283.066500	38.233204
2218.379666	182625.077821	38.238221
2220.593289	182960.749207	38.243239
2223.002350	183299.881477	38.248256
2225.072200	183640.554712	38.253274
2227.491137	183987.900163	38.258292
2229.608077	184325.221424	38.263309
2231.724067	184657.812485	38.268327
2234.152502	185012.143260	38.273344
2236.369190	185347.350080	38.278362
2238.456968	185682.389508	38.283380
2240.549164	186021.998818	38.288397
2243.002576	186342.494146	38.293415
2244.831387	186648.447300	38.298432
2246.728771	186970.748288	38.303450
2249.025893	187285.336382	38.308468
2251.177089	187616.179763	38.313485
2253.452781	187930.978705	38.318503
2255.491262	188253.964238	38.323520
2257.126646	188609.121290	38.328538
2259.977780	188932.325290	38.333556
2261.566719	189276.352999	38.338573
2263.879178	189622.324296	38.343591
2266.557933	189971.488745	38.348608
2268.328209	190339.898775	38.353626
2270.861714	190673.824957	38.358644
2273.309107	191029.912074	38.363661
2275.567607	191381.983484	38.368679
2277.706391	191735.472428	38.373696
2279.398880	192112.982255	38.378714
2282.334501	192452.872450	38.383732
2284.168398	192826.177389	38.388749
2286.812449	193203.062503	38.393767
2289.441371	193556.233096	38.398784
2291.574562	193942.875541	38.403802
2294.269770	194296.700847	38.408820
2296.537868	194656.015638	38.413837
2299.116646	195017.568222	38.418855
2301.361675	195382.691905	38.423872
2303.686962	195749.645799	38.428890
2305.888029	196098.015838	38.433908
2308.118280	196488.216146	38.438925
2310.577512	196851.196847	38.443943
2313.098024	197218.612621	38.448960
2315.363557	197586.718733	38.453978
2317.864243	197958.153619	38.458996
2320.232262	198328.774484	38.464013
2322.907195	198696.836200	38.469031
2325.259887	199065.903517	38.474048
2327.725049	199435.387122	38.479066
2330.437529	199792.928316	38.484084
2332.928902	200156.510648	38.489101
2334.523818	200531.648470	38.494119
2337.231962	200894.744471	38.499136
2339.564291	201246.478737	38.504154
2341.905531	201617.190095	38.509172
2343.852296	201992.307582	38.514189
2346.056727	202356.026260	38.519207
2348.675297	202730.572598	38.524224
2350.818119	203095.524453	38.529242
2353.611408	203460.439032	38.534260
2355.385880	203845.078403	38.539277
2357.846327	204214.544182	38.544295
2360.717764	204585.343527	38.549312
2362.975751	204949.425915	38.554330
2365.337768	205328.003328	38.559348
2367.688844	205699.539759	38.564365
2370.281097	206033.008720	38.569383
2372.477964	206374.019154	38.574400
2374.616774	206721.387914	38.579418
2377.190432	207053.951649	38.584436
2379.200279	207391.113153	38.589453
2381.222906	207744.498104	38.594471
2383.861372	208090.056524	38.599488
2385.981775	208442.554166	38.604506
2388.559232	208799.031025	38.609524
2390.599626	209174.370712	38.614541
2392.659295	209532.406543	38.619559
2395.057200	209884.932019	38.624576
2397.165357	210286.216221	38.629594
2400.013675	210619.251101	38.634612
2402.218749	211025.970902	38.639629
2404.487441	211416.179423	38.644647
2406.967500	211774.288456	38.649664
2409.354792	212167.021865	38.654682
2411.982939	212547.849237	38.659700
2414.327248	212938.512128	38.664717
2416.867372	213336.877975	38.669735
2419.684417	213712.375486	38.674752
2421.983187	214117.386118	38.679770
2424.104782	214497.797358	38.684788
2426.698468	214893.282189	38.689805
2429.011094	215291.226153	38.694823
2431.552570	215678.661934	38.699840
2434.368080	216092.553367	38.704858
2436.883622	216491.386347	38.709876
2439.105282	216865.916726	38.714893
2441.445374	217293.094910	38.719911
2444.412977	217670.875946	38.724928
2446.533849	218082.934161	38.729946
2449.187659	218479.750584	38.734964
2452.068934	218873.841480	38.739981
2454.269100	219283.862633	38.744999
2456.927193	219680.685045	38.750016
2459.191836	220082.980858	38.755034
2461.743679	220478.135777	38.760052
2464.111453	220883.390722	38.765069
2466.353825	221290.318378	38.770087
2468.938949	221697.041564	38.775104
2471.218023	222110.887805	38.780122
2473.936016	222520.463940	38.785140
2476.612132	222926.201612	38.790157
2479.231900	223339.416438	38.795175
2481.921889	223740.534329	38.800192
2484.457204	224151.481303	38.805210
2486.946921	224547.365577	38.810228
2489.304020	224947.094845	38.815245
2491.908909	225416.967290	38.820263
2494.672841	225813.182601	38.825280
2497.302443	226227.071181	38.830298
2499.581829	226618.808652	38.835316
2502.586658	227007.855317	38.840333
2504.444366	227379.054351	38.845351
2506.896792	227752.192474	38.850368
2509.247503	228122.884917	38.855386
2511.791438	228482.958034	38.860404
2514.165827	228855.986371	38.865421
2516.620084	229232.889346	38.870439
2519.084105	229603.189241	38.875456
2521.130678	229993.188631	38.880474
2523.218477	230380.694295	38.885492
2525.999812	230775.964831	38.890509
2528.375386	231175.085583	38.895527
2530.937843	231568.870427	38.900544
2533.342534	231978.326775	38.905562
2535.886184	232384.537421	38.910580
2538.223657	232790.503125	38.915597
2541.005072	233211.765870	38.920615
2544.009312	233625.096426	38.925632
2546.070033	234040.508512	38.930650
2548.737698	234456.486543	38.935668
2551.537808	234873.512070	38.940685
2553.761553	235291.824398	38.945703
2556.618318	235706.837962	38.950720
2558.948018	236137.683819	38.955738
2561.806376	236549.220964	38.960756
2564.369645	236980.312717	38.965773
2567.043130	237406.816993	38.970791
2569.779564	237828.563413	38.975808
2572.540402	238259.629069	38.980826
2575.102562	238677.139391	38.985844
2578.213620	239092.862586	38.990861
2580.459487	239540.854562	38.995879
2583.305973	239949.917456	39.000896
2585.736275	240374.617664	39.005914
2588.221760	240797.583528	39.010932
2591.037516	241222.886173	39.015949
2593.488300	241659.881284	39.020967
2596.532318	242081.721881	39.025984
2599.152644	242512.419471	39.031002
2601.165173	242937.372867	39.036020
2604.585060	243360.174334	39.041037
2607.083387	243789.879697	39.046055
2609.321062	244216.147968	39.051072
2612.132430	244651.343896	39.056090
2615.022649	245078.959443	39.061108
2617.523638	245508.085870	39.066125
2620.154566	245933.408389	39.071143
2622.839385	246363.981648	39.076160
2625.357254	246796.513160	39.081178
2628.082872	247231.654785	39.086196
2630.833855	247664.685444	39.091213
2633.244924	248092.513241	39.096231
2635.892428	248520.101620	39.101248
2638.532552	248961.459830	39.106266
2641.227155	249394.072669	39.111284
2644.198955	249819.073221	39.116301
2646.261539	250229.333758	39.121319
2648.925519	250617.400829	39.126336
2651.378665	251022.013210	39.131354
2653.814037	251427.391453	39.136372
2656.628534	251827.554092	39.141389
2658.992299	252246.002089	39.146407
2661.475989	252654.627029	39.151424
2663.972954	253066.959483	39.156442
2666.803131	253488.079952	39.161460
2669.309561	253915.603162	39.166477
2671.992907	254344.445637	39.171495
2674.753508	254761.922137	39.176512
2677.432310	255190.335398	39.181530
2680.046296	255623.941896	39.186548
2682.360199	256070.526585	39.191565
2684.745959	256514.535233	39.196583
2687.435365	256959.716030	39.201600
2690.799959	257406.187926	39.206618
2693.328181	257870.193863	39.211636
2696.244994	258312.318483	39.216653
2698.759161	258766.548516	39.221671
2701.599048	259221.058056	39.226688
2704.387738	259671.994783	39.231706
2706.550827	260140.940281	39.236724
2709.874649	260584.985951	39.241741
2712.691462	261050.476373	39.246759
2715.342111	261511.573819	39.251776
2718.208234	261971.926608	39.256794
2720.609439	262432.379162	39.261812
2723.677697	262894.809800	39.266829
2726.576463	263371.010954	39.271847
2729.368778	263834.833017	39.276864
2732.477474	264300.714055	39.281882
2734.979012	264772.737800	39.286900
2738.071379	265235.447261	39.291917
2741.025797	265702.243628	39.296935
2743.873740	266154.806249	39.301952
2746.723633	266612.017829	39.306970
2749.382083	267066.186422	39.311988
2752.708025	267512.527173	39.317005
2755.327463	267981.614504	39.322023
2757.990154	268438.400240	39.327040
2760.851990	268883.647138	39.332058
2763.197732	269341.906387	39.337076
2766.360385	269799.249095	39.342093
2769.181856	270250.930403	39.347111
2772.159908	270721.207844	39.352128
2775.055026	271160.303386	39.357146
2777.636109	271625.715963	39.362164
2780.947847	272067.845179	39.367181
2783.612463	272528.824760	39.372199
2786.350351	272976.430729	39.377216
2789.384041	273416.826239	39.382234
2791.860323	273880.147804	39.387252
2794.851823	274306.502131	39.392269
2797.525626	274725.260412	39.397287
2800.155728	275130.892098	39.402304
2802.720729	275549.566080	39.407322
2805.151177	275968.921874	39.412340
2807.887544	276374.536778	39.417357
2810.430079	276811.860421	39.422375
2812.993747	277248.520186	39.427392
2816.068775	277670.441147	39.432410
2818.324120	278124.703346	39.437428
2820.972226	278563.788218	39.442445
2823.384504	279020.616471	39.447463
2826.091786	279475.924455	39.452480
2829.030727	279928.756852	39.457498
2831.567625	280408.453251	39.462516
2834.856797	280870.705198	39.467533
2837.374127	281350.836029	39.472551
2840.036444	281818.445166	39.477568
2843.181459	282299.263478	39.482586
2845.596910	282785.125181	39.487604
2848.961609	283268.651505	39.492621
2851.903313	283755.673820	39.497639
2854.902619	284239.993820	39.502656
2857.807231	284739.011371	39.507674
2860.232662	285228.349445	39.512692
2863.229994	285724.734697	39.517709
2866.142648	286214.375544	39.522727
2869.096770	286723.264735	39.527744
2872.382434	287220.516971	39.532762
2875.235274	287721.647498	39.537780
2878.257635	288217.593661	39.542797
2881.292613	288715.188274	39.547815
2884.223186	289215.262719	39.552832
2887.275218	289712.903851	39.557850
2890.463285	290210.446400	39.562868
2893.707040	290704.473689	39.567885
2896.472696	291213.919010	39.572903
2899.227065	291713.026270	39.577920
2902.224358	292202.796760	39.582938
2904.879754	292712.485205	39.587956
2907.890782	293204.817186	39.592973
2910.545961	293714.401922	39.597991
2913.738716	294218.286496	39.603008
2917.001867	294723.301891	39.608026
2919.635421	295229.025437	39.613044
2922.747996	295722.047049	39.618061
2925.603227	296221.992199	39.623079
2928.345727	296736.966571	39.628096
2931.440546	297240.325908	39.633114
2934.381491	297750.947829	39.638132
2937.572743	298258.683723	39.643149
2940.684829	298766.913371	39.648167
2943.646005	299279.153532	39.653184
2946.983909	299767.912242	39.658202
2949.662266	300272.497532	39.663220
2952.867854	300762.874614	39.668237
2955.609057	301234.425089	39.673255
2958.189509	301681.639740	39.678272
2961.548466	302134.089565	39.683290
2964.116781	302606.145946	39.688308
2966.989238	303068.322494	39.693325
2969.661407	303529.106866	39.698343
2972.766028	303995.409560	39.703360
2975.766456	304462.514678	39.708378
2978.133697	304957.252951	39.713396
2981.326250	305436.567626	39.718413
2984.074929	305905.282640	39.723431
2986.729788	306407.895186	39.728448
2989.950854	306906.352155	39.733466
2993.017440	307406.635112	39.738484
2995.824423	307903.909200	39.743501
2998.780166	308400.116398	39.748519
3001.761948	308912.725931	39.753536
3004.764405	309422.307476	39.758554
3007.362663	309935.583036	39.763572
3010.642603	310468.433271	39.768589
3013.411237	310980.585171	39.773607
3016.310768	311514.379845	39.778624
3019.770818	312047.829326	39.783642
3022.746473	312576.146111	39.788660
3025.543247	313114.368950	39.793677
3028.545547	313648.264193	39.798695
3031.830363	314180.232571	39.803712
3035.295807	314700.537091	39.808730
3038.329252	315255.271710	39.813748
3041.620557	315790.964505	39.818765
3044.795135	316331.346260	39.823783
3047.954302	316886.433112	39.828800
3051.159030	317420.861048	39.833818
3054.249316	317952.739000	39.838836
3056.756555	318493.392344	39.843853
3060.258142	319040.209285	39.848871
3063.331397	319579.446210	39.853888
3067.057542	320111.541642	39.858906
3069.536003	320666.130176	39.863924
3073.044220	321195.307735	39.868941
3076.368436	321730.809729	39.873959
3079.246450	322280.702863	39.878976
3082.170573	322816.617155	39.883994
3085.529495	323356.319593	39.889012
3088.692732	323891.808436	39.894029
3091.818049	324444.137509	39.899047
3094.898855	324990.070225	39.904064
3098.555082	325513.585438	39.909082
3101.443456	326063.630231	39.914100
3104.638113	326603.540861	39.919117
3107.689422	327122.570264	39.924135
3110.655905	327667.436501	39.929152
3113.752938	328202.044169	39.934170
3116.785891	328741.711863	39.939188
3119.619052	329272.011414	39.944205
3122.981122	329779.038534	39.949223
3126.114955	330282.187664	39.954240
3129.155192	330771.787810	39.959258
3131.933991	331270.161591	39.964276
3134.648655	331771.132305	39.969293
3137.931419	332282.319463	39.974311
3140.808206	332801.820079	39.979328
3144.094166	333315.310193	39.984346
3147.261161	333817.312402	39.989364
3150.191537	334348.753315	39.994381
3153.102509	334868.944335	39.999399
3156.126114	335402.317668	40.004416
3159.841136	335936.059909	40.009434
3162.607759	336465.859895	40.014452
3165.373311	337019.955826	40.019469
3169.215111	337557.067656	40.024487
3172.338228	338103.328156	40.029504
3175.430262	338643.495143	40.034522
3178.525260	339196.225690	40.039540
3181.621932	339752.810620	40.044557
3184.952635	340304.275575	40.049575
3188.315532	340871.701116	40.054592
3191.559695	341420.961038	40.059610
3194.876332	341983.483524	40.064628
3197.929004	342548.403871	40.069645
3201.484290	343111.538403	40.074663
3204.598495	343676.946338	40.079680
3207.592711	344232.948667	40.084698
3211.150748	344805.511567	40.089716
3214.249628	345385.732689	40.094733
3217.610079	345949.302854	40.099751
3220.971032	346529.191895	40.104768
3224.024685	347109.936125	40.109786
3227.455559	347677.007160	40.114804
3230.603550	348258.740261	40.119821
3234.155379	348826.034513	40.124839
3237.287808	349415.297982	40.129856
3240.811179	349993.374138	40.134874
3244.300116	350571.068876	40.139892
3247.332344	351139.360843	40.144909
3250.821826	351716.510223	40.149927
3253.831289	352305.736556	40.154944
3257.126602	352866.733852	40.159962
3260.105606	353459.049182	40.164980
3263.429888	354059.248539	40.169997
3266.667825	354638.538138	40.175015
3270.025133	355241.688549	40.180032
3273.041421	355821.304523	40.185050
3276.850203	356414.114760	40.190068
3279.934667	357006.804169	40.195085
3283.495061	357580.856600	40.200103
3286.610856	358183.451736	40.205120
3289.765792	358768.291307	40.210138
3293.100019	359360.303977	40.215156
3296.408247	359941.627999	40.220173
3299.821619	360491.836538	40.225191
3302.837224	361042.228605	40.230208
3305.968381	361592.799109	40.235226
3309.089472	362146.816545	40.240244
3312.061981	362696.307968	40.245261
3315.463859	363253.288190	40.250279
3318.399509	363825.588484	40.255296
3321.623010	364382.507246	40.260314
3325.186045	364958.780300	40.265332
3327.831897	365547.347395	40.270349
3331.101079	366131.494017	40.275367
3334.147018	366727.519787	40.280384
3337.381324	367327.720491	40.285402
3340.471126	367934.762387	40.290420
3343.834198	368540.433151	40.295437
3347.517660	369155.002751	40.300455
3350.723576	369773.014226	40.305472
3354.338844	370397.651325	40.310490
3357.786318	371021.087891	40.315508
3361.048046	371647.894233	40.320525
3364.611120	372265.407366	40.325543
3367.861810	372903.564659	40.330560
3371.247587	373524.969598	40.335578
3375.070722	374164.691800	40.340596
3378.647443	374802.971457	40.345613
3382.465426	375415.043945	40.350631
3385.817716	376067.700293	40.355648
3389.100087	376688.870843	40.360666
3393.067846	377318.854193	40.365684
3396.404805	377948.699058	40.370701
3399.969831	378574.235656	40.375719
3403.747278	379212.287035	40.380736
3406.953619	379846.359218	40.385754
3410.165138	380460.150192	40.390772
3413.818565	381094.968592	40.395789
3417.358842	381719.190413	40.400807
3420.743243	382365.497018	40.405824
3423.960605	382999.262096	40.410842
3427.762707	383621.813283	40.415860
3431.166688	384272.193857	40.420877
3434.757473	384901.707808	40.425895
3438.635146	385530.277973	40.430912
3441.908531	386169.738755	40.435930
3445.488513	386802.900164	40.440948
3449.066778	387433.793458	40.445965
3452.600126	388055.602543	40.450983
3456.128605	388688.713991	40.456000
3459.575760	389315.105894	40.461018
3463.422077	389942.083185	40.466036
3466.446494	390569.483739	40.471053
3470.348909	391197.266994	40.476071
3473.462952	391817.352346	40.481088
3477.468618	392446.796201	40.486106
3480.551361	393063.668913	40.491124
3483.891844	393675.803011	40.496128
3487.238499	394243.112861	40.501133
3490.573985	394768.871883	40.506138
3493.210984	395248.283790	40.511143
3496.297771	395656.991149	40.516148
3498.747787	396023.464431	40.521152
3501.224883	396337.634202	40.526157
3503.353058	396583.672036	40.531162
3505.130022	396799.688499	40.536167
3506.887914	396956.395656	40.541172
3508.696831	397098.857408	40.546176
3510.058492	397180.299150	40.551181
3511.494852	397243.755249	40.556186
3512.298469	397275.711242	40.561191
3513.598245	397258.091404	40.566196
3514.124163	397229.255490	40.571200
3514.768199	397177.774900	40.576205
3515.621954	397085.254569	40.581210
3516.186751	396983.652948	40.586215
3516.808439	396862.669939	40.591220
3516.797315	396729.786970	40.596224
3517.273002	396577.886462	40.601229
3517.536087	396422.230846	40.606234
3517.583983	396251.608871	40.611239
3518.061582	396064.037046	40.616244
3517.636218	395878.030631	40.621248
3517.797822	395688.294839	40.626253
3517.645874	395497.107553	40.631258
3517.757552	395285.945206	40.636263
3517.284252	395086.848740	40.641268
3516.889915	394904.264341	40.646272
3516.995615	394703.421544	40.651277
3516.666969	394499.468172	40.656282
3516.282263	394291.581635	40.661287
3516.127548	394093.878240	40.666292
3515.991941	393913.866421	40.671296
3515.371775	393708.505222	40.676301
3515.122678	393524.593856	40.681306
3515.292802	393348.420815	40.686311
3515.244185	393157.000763	40.691316
3514.714723	392976.207285	40.696320
3514.702370	392763.879498	40.701325
3514.257176	392585.257281	40.706330
3513.667220	392405.995956	40.711335
3513.753013	392234.686973	40.716340
3513.543020	392056.457116	40.721344
3513.243997	391887.063380	40.726349
3513.013114	391722.209397	40.731354
3512.777947	391558.804636	40.736359
3512.416352	391395.978489	40.741364
3511.869907	391232.748555	40.746368
3512.009898	391065.671589	40.751373
3511.793392	390931.985089	40.756378
3511.360514	390780.736686	40.761383
3511.396915	390628.167518	40.766388
3510.836093	390493.033580	40.771392
3510.553951	390354.803777	40.776397
3510.547556	390222.327334	40.781402
3510.669390	390091.584637	40.786407
3510.272692	389956.117582	40.791412
3509.917306	389843.147133	40.796416
3509.762196	389700.902541	40.801421
3509.870518	389576.135660	40.806426
3508.962169	389457.046962	40.811431
3509.429442	389343.690608	40.816436
3508.834307	389234.722937	40.821440
3508.737582	389121.251612	40.826445
3508.310786	389016.274347	40.831450
3508.068204	388923.371621	40.836455
3508.388079	388825.980601	40.841460
3508.021418	388737.038437	40.846464
3507.922153	388637.500875	40.851469
3508.251057	388538.403929	40.856474
3507.774108	388439.459530	40.861479
3507.606312	388355.519899	40.866484
3507.209375	388259.512111	40.871488
3507.299923	388173.649476	40.876493
3506.834051	388100.156843	40.881498
3506.756839	388015.108654	40.886503
3506.604190	387930.911354	40.891508
3506.119599	387869.398361	40.896512
3506.252916	387800.667384	40.901517
3506.700041	387726.648229	40.906522
3506.033089	387667.274356	40.911527
3506.052279	387593.729449	40.916532
3505.681748	387543.437680	40.921536
3505.782720	387473.922887	40.926541
3505.596692	387425.178419	40.931546
3505.445484	387369.053801	40.936551
3505.100651	387291.802251	40.941556
3505.245455	387248.523480	40.946560
3505.175239	387186.282657	40.951565
3505.274464	387140.213694	40.956570
3504.899271	387093.838223	40.961575
3505.170144	387041.689715	40.966580
3504.810744	386992.183751	40.971584
3504.680870	386947.854563	40.976589
3504.832041	386914.466612	40.981594
3504.430303	386866.086087	40.986599
3504.714635	386823.166205	40.991604
3504.329513	386784.904071	40.996608
3504.566236	386739.118029	41.001613
3504.711555	386698.839270	41.006618
3504.345281	386661.642090	41.011623
3504.215177	386602.537643	41.016628
3504.282541	386584.573289	41.021632
3504.555364	386552.157553	41.026637
3504.335886	386513.131476	41.031642
3503.989903	386477.965317	41.036647
3504.169406	386428.119100	41.041652
3504.027709	386402.965518	41.046656
3503.986250	386363.962001	41.051661
3504.047289	386340.454726	41.056666
3503.847782	386298.271907	41.061671
3503.897098	386270.468715	41.066676
3503.521954	386248.607016	41.071680
3503.976280	386205.888416	41.076685
3503.806131	386180.357724	41.081690
3503.484317	386155.842776	41.086695
3503.771089	386128.129092	41.091700
3503.786263	386099.746268	41.096704
3503.654092	386073.395724	41.101709
3503.839982	386038.450231	41.106714
3503.289342	386029.763715	41.111719
3503.418585	385986.740224	41.116724
3503.747443	385967.106677	41.121728
3503.863125	385941.479774	41.126733
3503.778504	385913.672057	41.131738
3503.340609	385894.871739	41.136743
3503.551888	385854.861368	41.141748
3503.343533	385841.212586	41.146752
3503.223509	385817.886185	41.151757
3503.488928	385787.861431	41.156762
3502.860766	385769.955771	41.161767
3503.196463	385744.370243	41.166772
3503.041808	385733.179710	41.171776
3503.052821	385699.126187	41.176781
3503.126062	385683.601817	41.181786
3503.024051	385676.471865	41.186791
3502.887096	385651.698483	41.191796
3502.901858	385637.175139	41.196800
3503.139439	385618.445915	41.201805
3503.031654	385611.240570	41.206810
3503.077956	385592.414417	41.211815
3503.125361	385564.356689	41.216820
3503.001014	385546.320413	41.221824
3502.956489	385522.676722	41.226829
3502.973462	385508.585303	41.231834
3502.817770	385507.160319	41.236839
3503.066065	385468.415223	41.241844
3502.953351	385461.744678	41.246848
3502.521992	385450.063753	41.251853
3502.919352	385442.600505	41.256858
3502.568809	385423.175796	41.261863
3502.800662	385404.930558	41.266868
3502.418695	385409.797351	41.271872
3502.689532	385383.535193	41.276877
3502.783375	385376.501377	41.281882
3502.825801	385360.396831	41.286887
3502.750989	385342.937539	41.291892
3502.939313	385338.965929	41.296896
3502.754331	385329.611100	41.301901
3502.808441	385310.300380	41.306906
3502.821358	385301.092276	41.311911
3503.221275	385280.302739	41.316916
3502.752316	385270.128131	41.321920
3502.888142	385254.313947	41.326925
3502.591263	385234.880657	41.331930
3502.334356	385226.732431	41.336935
3502.826642	385211.573949	41.341940
3502.851251	385194.734647	41.346944
3502.709431	385188.679000	41.351949
3503.106976	385172.111337	41.356954
3502.755726	385151.237026	41.361959
3503.012834	385133.801458	41.366964
3502.647596	385129.078107	41.371968
3502.605602	385116.725178	41.376973
3502.935425	385082.391811	41.381978
3502.601857	385091.447136	41.386983
3502.485638	385078.114113	41.391988
3502.844092	385056.491776	41.396992
3502.496398	385042.203516	41.401997
3502.491963	385035.337759	41.407002
3502.603619	385035.345503	41.412007
3502.571167	385001.603386	41.417012
3502.543366	385001.149983	41.422016
3502.632195	384983.435772	41.427021
3502.747317	384962.436767	41.432026
3502.238698	384977.063803	41.437031
3502.259884	384947.763624	41.442036
3502.385790	384943.827270	41.447040
3502.499445	384946.479549	41.452045
3502.301248	384931.938732	41.457050
3502.091156	384928.487824	41.462055
3502.483946	384925.424804	41.467060
3502.456180	384921.767054	41.472064
3502.342182	384901.287428	41.477069
3502.469726	384896.130109	41.482074
3502.497818	384892.921289	41.487079
3502.504875	384875.575992	41.492084
3502.325381	384881.224648	41.497088
3502.718305	384866.615791	41.502093
3502.640411	384855.718035	41.507098
3502.596922	384843.110938	41.512103
3502.740842	384814.401605	41.517108
3502.394402	384830.986705	41.522112
3502.296604	384820.626143	41.527117
3502.312984	384782.222173	41.532122
3502.542356	384801.768024	41.537127
3502.800125	384790.893481	41.542132
3502.578832	384776.051078	41.547136
3502.676280	384749.688727	41.552141
3502.599319	384738.638201	41.557146
3502.498045	384748.038358	41.562151
3502.827385	384719.477660	41.567156
3502.499822	384708.721055	41.572160
3502.580962	384702.655514	41.577165
3502.424899	384673.434003	41.582170
3502.568721	384682.057920	41.587175
3502.607263	384658.604000	41.592180
3502.587779	384649.960350	41.597184
3502.522787	384640.942419	41.602189
3502.481330	384622.104218	41.607194
3502.548328	384612.887395	41.612199
3502.570437	384596.684006	41.617204
3502.337956	384591.863306	41.622208
3502.444577	384590.676565	41.627213
3502.587025	384574.911910	41.632218
3502.318262	384559.517432	41.637223
3502.490177	384555.828080	41.642228
3502.276084	384542.052570	41.647232
3502.485532	384539.476270	41.652237
3502.319030	384548.759631	41.657242
3502.265986	384516.597087	41.662247
3502.540407	384506.330186	41.667252
3502.683566	384505.875182	41.672256
3502.166368	384487.493593	41.677261
3502.482954	384468.802166	41.682266
3502.453289	384485.667953	41.687271
3502.400692	384465.432697	41.692276
3502.440309	384460.518103	41.697280
3502.553643	384437.815169	41.702285
3502.431857	384434.808024	41.707290
3502.076882	384434.075724	41.712295
3502.485788	384432.434287	41.717300
3502.292314	384427.124198	41.722304
3501.820141	384412.372174	41.727309
3502.225068	384402.262635	41.732314
3502.394978	384408.542781	41.737319
3502.625621	384400.953091	41.742324
3502.541299	384382.146977	41.747328
3502.289608	384384.373850	41.752333
3502.498840	384364.478624	41.757338
3502.370311	384347.739444	41.762343
3502.591355	384339.566332	41.767348
3502.270959	384329.927478	41.772352
3502.108892	384314.846645	41.777357
3502.686080	384318.519253	41.782362
3502.708280	384309.741776	41.787367
3502.526477	384306.286339	41.792372
3502.812930	384292.914811	41.797376
3502.446242	384265.811678	41.802381
3502.443105	384267.694085	41.807386
3502.305374	384256.703886	41.812391
3502.542287	384235.202018	41.817396
3502.347791	384233.961141	41.822400
3502.270908	384220.901342	41.827405
3502.448098	384205.436221	41.832410
3502.198177	384203.720902	41.837415
3502.267756	384205.718975	41.842420
3502.353658	384181.723204	41.847424
3502.605803	384179.369016	41.852429
3502.564036	384171.084822	41.857434
3502.181481	384157.310370	41.862439
3502.327421	384147.597750	41.867444
3502.669364	384132.081122	41.872448
3502.336197	384120.994620	41.877453
3502.245701	384114.066004	41.882458
3502.061473	384109.873408	41.887463
3502.596249	384092.724076	41.892468
3502.415590	384095.728123	41.897472
3502.231447	384088.254805	41.902477
3502.473512	384067.769300	41.907482
3502.149117	384059.148283	41.912487
3502.015531	384059.525410	41.917492
3502.194773	384060.488881	41.922496
3501.923324	384052.317265	41.927501
3502.048727	384034.647689	41.932506
3502.028675	384040.729039	41.937511
3502.270654	384032.349096	41.942516
3502.286839	384036.466464	41.947520
3502.146731	384016.473688	41.952525
3502.297584	384011.922929	41.957530
3502.324654	384012.783297	41.962535
3502.448141	384001.166796	41.967540
3502.313919	383984.860698	41.972544
3502.073912	383983.881326	41.977549
3502.158763	383989.208576	41.982554
3501.952090	383987.511841	41.987559
3502.298979	383968.281306	41.992564
3501.991815	383966.956504	41.997568
3501.767953	383962.312383	42.002573
3502.036726	383961.862947	42.007578
3501.901963	383967.174054	42.012583
3502.172379	383941.546750	42.017588
3502.474915	383940.990249	42.022592
3502.022254	383942.053616	42.027597
3502.337004	383941.266296	42.032602
3502.298488	383920.494451	42.037607
3502.183275	383903.117170	42.042612
3502.306774	383915.432110	42.047616
3501.960439	383908.543899	42.052621
3502.279067	383881.713631	42.057626
3501.755038	383885.662095	42.062631
3501.907916	383881.823095	42.067636
3502.354194	383885.948785	42.072640
3502.069016	383886.604198	42.077645
3502.097714	383859.158516	42.082650
3501.913126	383862.442954	42.087655
3502.146440	383858.998148	42.092660
3502.368838	383867.050327	42.097664
3502.336097	383863.367828	42.102669
3502.560033	383841.359146	42.107674
3502.258187	383838.278690	42.112679
3502.215854	383815.727150	42.117684
3502.384144	383805.553132	42.122688
3502.255035	383802.928574	42.127693
3502.193853	383802.633025	42.132698
3502.458389	383795.368473	42.137703
3502.276426	383776.399467	42.142708
3502.399856	383771.802150	42.147712
3502.187578	383760.950752	42.152717
3502.490964	383757.215106	42.157722
3502.145310	383750.555647	42.162727
3502.100304	383738.355333	42.167732
3502.109398	383734.310159	42.172736
3502.184252	383718.861016	42.177741
3502.342492	383714.461645	42.182746
3502.295618	383729.041603	42.187751
3502.514321	383699.836387	42.192756
3502.410456	383685.432767	42.197760
3502.423965	383694.865906	42.202765
3502.756505	383670.907117	42.207770
3502.419496	383662.491460	42.212775
3502.405674	383655.982984	42.217780
3502.518861	383632.872675	42.222784
3502.331583	383629.519769	42.227789
3502.256844	383622.664867	42.232794
3502.072159	383608.452019	42.237799
3502.296182	383605.847920	42.242804
3502.446531	383602.060155	42.247808
3501.848677	383596.228935	42.252813
3502.359821	383570.766782	42.257818
3502.010372	383573.009156	42.262823
3502.033703	383570.080730	42.267828
3502.137251	383567.877156	42.272832
3502.210225	383560.948028	42.277837
3502.450280	383548.549995	42.282842
3502.101068	383564.296828	42.287847
3502.161955	383544.170298	42.292852
3502.198395	383524.530835	42.297856
3502.095856	383522.614160	42.302861
3502.271183	383515.643411	42.307866
3502.086095	383513.383733	42.312871
3501.949400	383493.262979	42.317876
3501.959675	383494.990710	42.322880
3501.770376	383490.290203	42.327885
3501.849439	383483.588988	42.332890
3501.853914	383498.516968	42.337895
3502.016162	383500.017217	42.342900
3502.046705	383493.094784	42.347904
3502.067304	383473.508663	42.352909
3502.365174	383462.373075	42.357914
3502.250073	383463.103337	42.362919
3502.390060	383464.301920	42.367924
3502.074681	383447.693607	42.372928
3501.970918	383438.808679	42.377933
3502.349997	383438.240071	42.382938
3502.090257	383451.404146	42.387943
3502.383533	383423.280516	42.392948
3502.498164	383403.654061	42.397952
3501.840368	383421.840371	42.402957
3502.440923	383407.121830	42.407962
3501.839836	383393.585102	42.412967
3502.158081	383375.528680	42.417972
3502.244827	383381.135472	42.422976
3502.182786	383382.772911	42.427981
3502.493594	383355.816346	42.432986
3502.149034	383361.364161	42.437991
3502.229302	383353.467414	42.442996
3502.128367	383339.037766	42.448000
3501.945980	383324.493828	42.453005
3502.267753	383320.628072	42.458010
3502.106244	383335.582355	42.463015
3502.307260	383320.570888	42.468020
3502.352410	383305.380596	42.473024
3502.194693	383291.900905	42.478029
3502.249768	383281.210563	42.483034
3502.125662	383296.845624	42.488039
3502.040215	383265.882457	42.493044
3502.504970	383257.136504	42.498048
3502.334635	383264.665951	42.503053
3502.505683	383240.859581	42.508058
3502.204673	383231.471705	42.513063
3502.169865	383228.399849	42.518068
3501.914040	383229.330389	42.523072
3501.721300	383215.347558	42.528077
3501.822807	383200.478936	42.533082
3501.446244	383207.252591	42.538087
3501.656269	383199.386163	42.543092
3502.035167	383195.307904	42.548096
3501.605259	383212.949639	42.553101
3501.840415	383213.014158	42.558106
3501.691559	383218.251300	42.563111
3501.834608	383219.220514	42.568116
3502.031377	383227.658367	42.573120
3501.968981	383215.969281	42.578125
3502.298151	383193.333210	42.583130
3501.912154	383196.751275	42.588135
3502.156572	383197.907924	42.593140
3502.186339	383198.462695	42.598144
3501.961090	383186.468723	42.603149
3502.119657	383162.664278	42.608154
3502.162183	383164.056304	42.613159
3502.464718	383163.499792	42.618164
3502.078821	383146.597306	42.623168
3501.862743	383137.094250	42.628173
3502.227943	383127.931654	42.633178
3501.888855	383148.509229	42.638183
3501.649807	383142.926406	42.643188
3502.114297	383139.623017	42.648192
3502.002692	383145.769850	42.653197
3502.024909	383136.966665	42.658202
3501.790569	383137.486891	42.663207
3501.810909	383125.225183	42.668212
3501.739592	383125.160123	42.673216
3501.712337	383133.964034	42.678221
3502.244589	383121.265346	42.683226
3501.982306	383133.870418	42.688231
3502.174911	383111.433914	42.693236
3502.230691	383094.003797	42.698240
3502.269418	383101.779984	42.703245
3501.963403	383100.607564	42.708250
3501.794440	383084.001378	42.713255
3502.043318	383062.013734	42.718260
3501.933012	383068.084076	42.723264
3501.374278	383077.353506	42.728269
3501.721156	383068.219224	42.733274
3501.705389	383087.346932	42.738279
3501.887168	383083.833905	42.743284
3502.434309	383083.238724	42.748288
3502.214750	383062.622190	42.753293
3502.024408	383056.980790	42.758298
3501.747587	383048.758941	42.763303
3502.086607	383043.339046	42.768308
3501.891354	383049.549982	42.773312
3501.707019	383052.452962	42.778317
3502.270365	383049.362831	42.783322
3502.237025	383028.309920	42.788327
3501.830710	383029.111659	42.793332
3502.009482	383027.633706	42.798337
3502.099189	383030.645962	42.803341
3502.240632	383015.770955	42.808346
3501.908259	383006.006492	42.813351
3501.935243	382998.804774	42.818356
3502.006248	383009.983841	42.823361
3502.025667	382995.967391	42.828365
3502.417201	382996.693869	42.833370
3502.150716	382993.607753	42.838375
3501.848949	382977.175110	42.843380
3502.279672	382968.943123	42.848385
3502.189676	382967.558521	42.853389
3502.194834	382944.897225	42.858394
3502.136185	382947.068231	42.863399
3502.336292	382936.583759	42.868404
3502.188389	382941.006945	42.873409
3501.925105	382925.509203	42.878413
3502.095931	382908.340573	42.883418
3502.094806	382910.324460	42.888423
3502.142121	382906.349453	42.893428
3502.193608	382906.137816	42.898433
3501.865249	382892.812122	42.903437
3501.871722	382884.545453	42.908442
3502.073662	382885.149309	42.913447
3501.760018	382876.628052	42.918452
3502.032202	382887.393863	42.923457
3501.692800	382893.322421	42.928461
3502.268399	382865.993024	42.933466
3501.975028	382859.528604	42.938471
3501.706790	382860.359384	42.943476
3502.202780	382859.746854	42.948481
3501.761540	382863.046518	42.953485
3502.210167	382860.457727	42.958490
3501.870503	382839.682031	42.963495
3501.811552	382827.814252	42.968500
3502.086582	382824.184729	42.973505
3501.535487	382838.895603	42.978509
3501.764411	382834.535822	42.983514
3501.783737	382836.414749	42.988519
3501.298767	382837.279791	42.993524
3501.634834	382844.525806	42.998529
3501.406262	382843.239404	43.003533
3502.266141	382846.511412	43.008538
3502.025858	382856.035745	43.013543
3501.888367	382832.710251	43.018548
3502.116202	382821.178624	43.023553
3501.686317	382820.508998	43.028557
3501.821821	382808.330713	43.033562
3501.750406	382816.607591	43.038567
3501.492058	382813.799934	43.043572
3501.786160	382826.647778	43.048577
3501.604022	382838.197538	43.053581
3501.847771	382828.392820	43.058586
3501.828749	382834.804826	43.063591
3502.076542	382816.352354	43.068596
3501.582542	382793.083193	43.073601
3501.761499	382791.325442	43.078605
3501.979100	382788.366245	43.083610
3501.880625	382791.637163	43.088615
3502.032772	382798.988559	43.093620
3502.080512	382796.259676	43.098625
3501.921556	382781.508363	43.103629
3502.197570	382774.496129	43.108634
3501.913628	382777.694636	43.113639
3501.982426	382776.462954	43.118644
3502.073107	382774.846321	43.123649
3502.043967	382775.791901	43.128653
3501.998952	382751.002073	43.133658
3501.975827	382744.723806	43.138663
3502.080242	382739.315522	43.143668
3502.105602	382750.959671	43.148673
3502.131752	382746.911695	43.153677
3502.080481	382733.491276	43.158682
3501.995120	382736.429499	43.163687
3502.014352	382731.517903	43.168692
3502.378552	382722.609695	43.173697
3501.754525	382719.885271	43.178701
3501.824290	382692.610282	43.183706
3501.862364	382692.553361	43.188711
3501.811765	382695.130034	43.193716
3502.011153	382699.600078	43.198721
3501.612215	382702.460711	43.203725
3502.098835	382699.026622	43.208730
3502.044884	382702.900895	43.213735
3502.078004	382676.318373	43.218740
3502.162138	382673.278534	43.223745
3501.583196	382672.200111	43.228749
3501.707715	382674.774534	43.233754
3501.676264	382681.112233	43.238759
3501.803959	382672.572027	43.243764
3501.931978	382674.255749	43.248769
3501.635641	382688.672080	43.253773
3501.952577	382680.788645	43.258778
3502.083065	382669.908181	43.263783
3501.551322	382661.599384	43.268788
3502.030400	382658.878602	43.273793
3501.850086	382660.102411	43.278797
3501.762786	382661.565845	43.283802
3502.155077	382663.665581	43.288807
3502.097887	382657.952206	43.293812
3502.209160	382632.069417	43.298817
3501.842403	382643.521257	43.303821
3502.159694	382631.949999	43.308826
3501.843449	382638.714218	43.313831
3501.948703	382632.034146	43.318836
3501.980743	382616.540457	43.323841
3501.956751	382607.795321	43.328845
3501.958816	382599.274959	43.333850
3502.310376	382600.694451	43.338855
3502.147355	382595.252126	43.343860
3502.431272	382585.720757	43.348865
3501.845707	382578.920987	43.353869
3501.974550	382561.707972	43.358874
3501.886004	382574.514660	43.363879
3501.904508	382577.639939	43.368884
3502.215307	382566.451181	43.373889
3501.864388	382552.645709	43.378893
3502.192421	382539.292424	43.383898
3502.089240	382553.474807	43.388903
3501.976039	382548.177197	43.393908
3502.162061	382544.536285	43.398913
3501.941053	382527.378561	43.403917
3502.178219	382504.858357	43.408922
3502.211514	382502.589529	43.413927
3501.980022	382502.575222	43.418932
3502.305755	382501.531809	43.423937
3502.318265	382482.226218	43.428941
3502.275708	382472.619267	43.433946
3501.956154	382476.204922	43.438951
3502.081337	382467.690501	43.443956
3502.186436	382450.532056	43.448961
3501.965656	382436.807701	43.453965
3501.918646	382449.073773	43.458970
3502.023269	382436.417026	43.463975
3501.879316	382445.570172	43.468980
3502.102520	382423.408188	43.473985
3502.174871	382414.902107	43.478989
3501.937279	382405.224238	43.483994
3501.642901	382414.782666	43.488999
3501.659745	382408.447159	43.494004
3501.962050	382401.303536	43.499009
3501.494407	382409.948335	43.504013
3501.869180	382414.009193	43.509018
3501.931655	382398.408873	43.514023
3501.678359	382382.273506	43.519028
3501.953696	382380.068140	43.524033
3501.627010	382391.310257	43.529037
3501.814722	382388.889847	43.534042
3501.542650	382391.120056	43.539047
3501.335480	382389.550493	43.544052
3501.830008	382393.668720	43.549057
3501.721815	382408.513207	43.554061
3501.660516	382397.052593	43.559066
3501.977234	382406.514418	43.564071
3501.763534	382406.014072	43.569076
3502.149858	382403.918327	43.574081
3501.862850	382393.485278	43.579085
3501.754568	382371.909759	43.584090
3502.187913	382376.088526	43.589095
3502.280151	382375.895878	43.594100
3502.518297	382373.950720	43.599105
3501.944293	382353.415267	43.604109
3502.239588	382338.617407	43.609114
3502.516814	382343.634714	43.614119
3501.929313	382343.549521	43.619124
3502.112171	382317.604336	43.624129
3502.292941	382318.771075	43.629133
3502.114691	382316.866307	43.634138
3502.073226	382316.949124	43.639143
3502.195222	382306.960055	43.644148
3502.174891	382278.173032	43.649153
3501.994674	382296.894771	43.654157
3501.816209	382283.341703	43.659162
3502.038390	382285.417486	43.664167
3502.233960	382271.093160	43.669172
3502.220841	382255.326700	43.674177
3501.786631	382257.429950	43.679181
3501.764915	382252.168702	43.684186
3501.795297	382258.725594	43.689191
3501.793264	382265.236742	43.694196
3502.078240	382247.795439	43.699201
3501.816759	382231.457839	43.704205
3501.633193	382228.155087	43.709210
3501.940727	382217.500838	43.714215
3501.606336	382214.577991	43.719220
3501.966994	382219.226062	43.724225
3501.334319	382222.047382	43.729229
3501.664341	382232.778801	43.734234
3501.726358	382227.326281	43.739239
3501.673180	382235.702135	43.744244
3502.041249	382227.861390	43.749249
3501.612337	382243.367036	43.754253
3501.933204	382223.224143	43.759258
3501.516245	382220.619547	43.764263
3501.658376	382199.029777	43.769268
3501.824782	382189.186256	43.774273
3501.593143	382197.590329	43.779277
3502.094801	382194.687914	43.784282
3502.048891	382206.546960	43.789287
3501.753911	382205.042136	43.794292
3502.050941	382206.521130	43.799297
3501.855473	382215.580742	43.804301
3501.984594	382182.192064	43.809306
3501.973492	382182.905909	43.814311
3502.141269	382177.919893	43.819316
3502.251299	382174.087495	43.824321
3502.039412	382182.183252	43.829325
3502.083855	382159.871343	43.834330
3501.908452	382149.242553	43.839335
3502.200893	382144.440289	43.844340
3502.146058	382151.544766	43.849345
3502.063557	382157.712590	43.854349
3501.936660	382135.351453	43.859354
3502.012537	382115.832195	43.864359
3501.944388	382114.749306	43.869364
3501.635186	382115.255946	43.874369
3501.655244	382122.958985	43.879373
3501.688956	382111.864763	43.884378
3501.955152	382113.424934	43.889383
3501.772079	382128.281367	43.894388
3501.770671	382127.543992	43.899393
3501.813832	382105.283120	43.904397
3501.870565	382087.038532	43.909402
3502.200174	382094.616342	43.914407
3501.775191	382089.673153	43.919412
3501.959350	382094.527173	43.924417
3501.694692	382098.129618	43.929421
3502.072383	382089.575196	43.934426
3501.810594	382071.813318	43.939431
3501.698796	382065.650690	43.944436
3502.018780	382060.081066	43.949441
3501.684779	382072.952157	43.954445
3501.992179	382068.172953	43.959450
3501.677966	382066.187933	43.964455
3501.621572	382066.832642	43.969460
3502.046680	382065.213978	43.974465
3501.905115	382075.791093	43.979469
3501.752280	382053.027078	43.984474
3501.941489	382036.363815	43.989479
3502.060931	382036.548362	43.994484
3501.911590	382033.697981	43.999489
3501.902780	382041.024102	44.004493
3501.969556	382044.116360	44.009498
3502.003022	382040.957315	44.014503
3502.002781	382028.367878	44.019508
3501.922715	382010.678977	44.024513
3501.365264	382014.225983	44.029517
3501.494151	382009.551291	44.034522
3501.651187	382005.711445	44.039527
3501.653863	382009.500537	44.044532
3501.759624	382007.093057	44.049537
3501.768889	382022.326057	44.054541
3501.639189	382015.555854	44.059546
3502.148660	382014.051018	44.064551
3502.027626	382019.360225	44.069556
3501.809043	382002.939446	44.074561
3501.649626	381998.971593	44.079565
3501.429290	381986.467801	44.084570
3501.822502	381981.496988	44.089575
3501.595615	381990.892252	44.094580
3501.566811	381979.985907	44.099585
3501.706583	381989.068876	44.104589
3501.755505	381986.441482	44.109594
3501.414658	381992.039775	44.114599
3501.752522	381993.410589	44.119604
3501.978439	381991.085847	44.124609
3501.798747	382002.711772	44.129613
3501.800060	382006.043281	44.134618
3501.752452	381995.267080	44.139623
3501.902220	382013.784192	44.144628
3501.923047	382000.784483	44.149633
3501.924001	381980.081639	44.154637
3502.339585	381959.491269	44.159642
3502.212816	381975.381624	44.164647
3502.019385	381974.420269	44.169652
3502.095327	381952.281293	44.174657
3501.461617	381944.064757	44.179661
3501.774439	381942.412972	44.184666
3502.006039	381927.065491	44.189671
3501.628834	381944.267113	44.194676
3501.729825	381940.893919	44.199681
3502.211095	381953.127504	44.204685
3501.922832	381949.637813	44.209690
3501.859965	381947.485887	44.214695
3501.727379	381930.593682	44.219700
3501.926968	381914.589991	44.224705
3501.846674	381921.825702	44.229709
3501.810346	381914.125122	44.234714
3501.995195	381914.782562	44.239719
3501.575129	381925.708945	44.244724
3501.661228	381916.539314	44.249729
3501.565470	381921.997139	44.254733
3502.161122	381914.069487	44.259738
3501.815656	381898.304553	44.264743
3501.570122	381892.468238	44.269748
3501.986635	381878.032538	44.274753
3501.746620	381890.303866	44.279757
3501.821911	381891.207526	44.284762
3501.862941	381883.520144	44.289767
3501.450585	381899.150478	44.294772
3501.909058	381899.917263	44.299777
3501.673114	381890.264437	44.304781
3501.770507	381890.452470	44.309786
3502.054866	381904.828163	44.314791
3501.501194	381885.001377	44.319796
3502.127217	381870.761453	44.324801
3501.525060	381873.349073	44.329805
3501.805159	381873.381057	44.334810
3501.820777	381877.727649	44.339815
3501.825117	381872.691129	44.344820
3502.132986	381876.025055	44.349825
3501.855496	381877.009918	44.354829
3501.837885	381881.285462	44.359834
3501.897866	381862.531588	44.364839
3501.963745	381853.746638	44.369844
3502.003582	381851.018938	44.374849
3501.669132	381852.597772	44.379853
3501.487044	381858.399887	44.384858
3501.694685	381854.145093	44.389863
3501.567083	381858.692361	44.394868
3501.868813	381847.377660	44.399873
3501.868041	381854.499078	44.404877
3501.965626	381853.135649	44.409882
3501.634343	381848.025016	44.414887
3501.381228	381835.399190	44.419892
3501.836859	381829.757223	44.424897
3501.641525	381832.941801	44.429901
3501.496787	381831.311478	44.434906
3502.148087	381825.409678	44.439911
3501.684051	381837.411237	44.444916
3501.917827	381831.371975	44.449921
3501.703674	381842.901663	44.454925
3501.969000	381833.805413	44.459930
3501.714615	381836.338059	44.464935
3501.671718	381842.372505	44.469940
3501.462406	381848.458691	44.474945
3501.928823	381842.230054	44.479949
3501.669595	381836.345029	44.484954
3501.852566	381827.872197	44.489959
3501.654186	381799.748795	44.494964
3502.107836	381817.276929	44.499969
3501.611972	381820.152950	44.504973
3501.844699	381811.290749	44.509978
3501.409815	381803.704018	44.514983
3500.892995	381833.924207	44.519988
3501.659516	381803.435571	44.524993
3501.419061	381811.332456	44.529997
3501.435186	381819.951777	44.535002
3501.672473	381822.457565	44.540007
3501.646708	381829.633806	44.545012
3501.687934	381825.430750	44.550017
3501.824690	381835.302666	44.555021
3501.655276	381830.725975	44.560026
3502.073368	381836.585814	44.565031
3501.518015	381831.281701	44.570036
3501.857599	381840.129652	44.575041
3501.907168	381854.796813	44.580045
3502.018787	381835.322629	44.585050
3501.824518	381809.792786	44.590055
3501.713550	381812.455361	44.595060
3502.144166	381810.683216	44.600065
3501.896552	381810.518856	44.605069
3502.058963	381806.729007	44.610074
3501.908157	381804.209475	44.615079
3501.830056	381800.559380	44.620084
3501.880347	381776.949223	44.625089
3501.808580	381774.417193	44.630093
3501.509748	381768.665585	44.635098
3501.709301	381787.378404	44.640103
3501.722965	381781.450231	44.645108
3501.964367	381774.570453	44.650113
3501.843630	381777.539776	44.655117
3501.832023	381782.170449	44.660122
3502.009149	381777.513537	44.665127
3501.629618	381759.795560	44.670132
3501.773776	381767.275585	44.675137
3501.845330	381755.564877	44.680141
3501.967293	381751.298182	44.685146
3501.910450	381757.665481	44.690151
3501.677362	381757.549691	44.695156
3501.942155	381754.303188	44.700161
3501.875243	381760.799244	44.705165
3501.764658	381757.840982	44.710170
3501.926669	381731.339162	44.715175
3501.734923	381724.044614	44.720180
3502.003827	381717.720014	44.725185
3502.021073	381719.599324	44.730189
3501.712432	381732.491954	44.735194
3501.835625	381722.578844	44.740199
3501.625410	381729.402761	44.745204
3501.772756	381723.860380	44.750209
3501.852892	381730.027995	44.755213
3501.296792	381713.253513	44.760218
3501.802666	381714.674078	44.765223
3501.979873	381716.197467	44.770228
3501.768314	381708.041311	44.775233
3501.886445	381698.866566	44.780237
3501.547031	381698.513250	44.785242
3501.999439	381709.098302	44.790247
3501.422991	381717.480689	44.795252
3501.812199	381702.820338	44.800257
3501.705702	381706.270650	44.805261
3501.726267	381706.903198	44.810266
3501.733820	381704.562092	44.815271
3501.818014	381719.707067	44.820276
3502.081469	381703.362557	44.825281
3501.989097	381692.974849	44.830285
3502.058948	381690.776494	44.835290
3501.840431	381677.407577	44.840295
3501.694539	381688.239818	44.845300
3502.045821	381679.994680	44.850305
3501.709019	381693.959979	44.855309
3501.934185	381677.646945	44.860314
3501.964721	381657.498786	44.865319
3501.672294	381657.799312	44.870324
3501.843531	381650.091300	44.875329
3501.952424	381649.870581	44.880333
3501.738907	381652.244177	44.885338
3501.790007	381652.617564	44.890343
3501.502922	381658.690642	44.895348
3502.102030	381648.676845	44.900353
3501.603230	381641.507122	44.905357
3501.872657	381639.429816	44.910362
3501.878298	381625.491342	44.915367
3501.360207	381628.014822	44.920372
3501.565069	381606.541970	44.925377
3501.380798	381630.147906	44.930381
3501.299418	381623.904098	44.935386
3501.704551	381626.078163	44.940391
3501.517742	381633.992036	44.945396
3501.995637	381625.497970	44.950401
3501.679344	381638.010339	44.955405
3501.783913	381637.408801	44.960410
3502.014228	381634.091438	44.965415
3501.942872	381646.692250	44.970420
3502.253271	381629.806185	44.975425
3502.486437	381628.472181	44.980429
3501.984718	381613.749170	44.985434
3502.371490	381600.259107	44.990439
3502.130983	381596.889002	44.995444
3502.004026	381576.511362	45.000449
3501.824861	381580.405543	45.005453
3501.605535	381574.565037	45.010458
3501.916820	381568.310013	45.015463
3501.931352	381570.520395	45.020468
3501.798489	381575.475464	45.025473
3501.884083	381564.550917	45.030477
3502.168597	381563.564863	45.035482
3501.816747	381549.911778	45.040487
3501.331435	381541.213892	45.045492
3502.000224	381532.130091	45.050497
3502.140916	381534.778335	45.055501
3501.781511	381541.396968	45.060506
3502.044486	381530.190035	45.065511
3501.680588	381542.353890	45.070516
3502.117324	381526.897520	45.075521
3502.290388	381502.555647	45.080525
3501.642594	381515.679998	45.085530
3502.016893	381506.591878	45.090535
3501.642969	381511.890266	45.095540
3501.544585	381502.419064	45.100545
3501.868834	381498.578168	45.105549
3501.931620	381509.606372	45.110554
3502.014007	381503.540124	45.115559
3501.680620	381494.055204	45.120564
3501.684662	381483.168959	45.125569
3501.805769	381491.542857	45.130573
3501.721805	381480.390755	45.135578
3502.049588	381475.608255	45.140583
3501.766058	381488.268094	45.145588
3502.071300	381482.344648	45.150593
3501.883241	381476.397450	45.155597
3501.733172	381450.071939	45.160602
3501.913114	381441.777537	45.165607
3501.654896	381453.899279	45.170612
3502.118325	381457.869924	45.175617
3501.992775	381447.334792	45.180621
3501.960818	381440.574470	45.185626
3501.781548	381465.425962	45.190631
3501.757130	381455.434384	45.195636
3502.040261	381437.636937	45.200641
3502.001693	381423.247574	45.205645
3501.945095	381421.679601	45.210650
3502.107321	381412.497816	45.215655
3502.023528	381420.624350	45.220660
3501.953830	381399.830628	45.225665
3501.876696	381395.976873	45.230669
3501.942589	381387.802223	45.235674
3501.982522	381379.886011	45.240679
3501.864321	381396.029587	45.245684
3502.038609	381395.671361	45.250689
3502.118773	381388.562668	45.255693
3501.900144	381377.253789	45.260698
3501.801508	381356.820689	45.265703
3501.686812	381368.283929	45.270708
3501.700864	381358.616882	45.275713
3501.591939	381361.965874	45.280717
3501.669245	381365.488894	45.285722
3501.869890	381356.707961	45.290727
3501.374308	381368.612918	45.295732
3501.523481	381363.451702	45.300737
3501.858919	381364.085346	45.305741
3502.055629	381368.199898	45.310746
3501.938742	381361.554723	45.315751
3501.605228	381345.329867	45.320756
3501.630345	381321.418206	45.325761
3501.572071	381341.926924	45.330765
3501.556103	381341.191835	45.335770
3501.849471	381325.529146	45.340775
3501.603696	381321.320538	45.345780
3501.584771	381333.887730	45.350785
3501.973403	381335.225109	45.355789
3501.630003	381330.828465	45.360794
3501.652896	381343.058406	45.365799
3501.411012	381344.927831	45.370804
3501.760559	381334.266696	45.375809
3501.971264	381341.125876	45.380813
3501.727788	381350.447617	45.385818
3501.982986	381340.310072	45.390823
3501.844089	381344.325079	45.395828
3501.754724	381320.558684	45.400833
3501.735750	381313.033276	45.405837
3501.952813	381305.216216	45.410842
3501.711029	381306.933025	45.415847
3501.578955	381319.518109	45.420852
3501.686654	381312.913722	45.425857
3501.886130	381313.467127	45.430861
3501.487722	381314.267649	45.435866
3501.733462	381322.240375	45.440871
3501.476158	381326.045199	45.445876
3501.628255	381330.319410	45.450881
3501.716821	381331.907694	45.455885
3501.928390	381327.372451	45.460890
3502.036123	381309.373769	45.465895
3501.659609	381313.553511	45.470900
3501.795019	381294.583967	45.475905
3501.911995	381292.200104	45.480909
3501.698089	381295.794601	45.485914
3502.189825	381282.084363	45.490919
3501.819501	381286.339431	45.495924
3501.788927	381290.718825	45.500929
3501.786793	381297.382755	45.505933
3501.841655	381271.889472	45.510938
3501.832433	381264.082742	45.515943
3501.325061	381243.434426	45.520948
3501.528568	381268.759642	45.525953
3501.739860	381237.544454	45.530957
3501.621790	381271.135601	45.535962
3501.816371	381240.660635	45.540967
3501.434340	381269.588270	45.545972
3501.505254	381267.669495	45.550977
3501.491248	381255.768691	45.555981
3501.616181	381272.840364	45.560986
3501.811047	381273.445365	45.565991
3501.203830	381288.114835	45.570996
3501.632741	381273.168275	45.576001
3501.895264	381270.837703	45.581005
3501.422112	381282.790007	45.586010
3501.938749	381290.592747	45.591015
3501.910657	381288.689624	45.596020
3501.954246	381281.535825	45.601025
3501.670766	381282.775986	45.606029
3501.804517	381297.201149	45.611034
3501.966746	381264.696621	45.616039
3501.696980	381248.309044	45.621044
3501.810651	381253.454085	45.626049
3501.568091	381245.633371	45.631053
3501.423991	381274.548823	45.636058
3501.970904	381240.889813	45.641063
3501.586941	381272.742630	45.646068
3502.134693	381237.811799	45.651073
3501.825620	381262.073531	45.656077
3501.823745	381261.412514	45.661082
3501.866044	381247.391808	45.666087
3501.604625	381217.726489	45.671092
3501.890385	381219.894015	45.676097
3501.735971	381225.361210	45.681101
3501.697661	381223.815772	45.686106
3502.100208	381218.563614	45.691111
3501.627121	381227.896249	45.696116
3501.681150	381222.572018	45.701121
3501.708387	381228.849811	45.706125
3501.648469	381226.010667	45.711130
3501.587817	381229.326606	45.716135
3501.479638	381230.284719	45.721140
3501.575844	381234.160836	45.726145
3501.775920	381223.090926	45.731149
3501.392880	381230.857866	45.736154
3501.762997	381231.257128	45.741159
3501.987619	381234.044727	45.746164
3501.712127	381209.315771	45.751169
3501.869602	381201.660713	45.756173
3501.310731	381197.908527	45.761178
3501.763381	381186.696944	45.766183
3501.487384	381197.397286	45.771188
3501.726081	381197.766456	45.776193
3502.011126	381199.756059	45.781197
3501.724466	381207.075394	45.786202
3501.923066	381206.433552	45.791207
3501.913724	381199.440708	45.796212
3501.963444	381202.535731	45.801217
3501.882828	381185.050007	45.806221
3501.542603	381178.363805	45.811226
3501.951890	381161.639940	45.816231
3501.730373	381180.546787	45.821236
3501.775040	381171.129191	45.826241
3501.955103	381187.861548	45.831245
3501.734503	381180.800362	45.836250
3501.577170	381187.539713	45.841255
3501.596175	381187.384070	45.846260
3501.936135	381171.713953	45.851265
3501.672972	381184.396105	45.856269
3501.284379	381199.946663	45.861274
3501.949294	381181.605502	45.866279
3501.563134	381176.452587	45.871284
3501.771565	381167.848417	45.876289
3502.125247	381155.965758	45.881293
3501.758182	381152.132379	45.886298
3501.788766	381149.558694	45.891303
3501.652225	381151.894718	45.896308
3501.962523	381152.176268	45.901313
3501.998614	381152.602900	45.906317
3501.815347	381160.821515	45.911322
3501.738244	381148.727183	45.916327
3501.722724	381134.079731	45.921332
3501.623687	381128.118406	45.926337
3501.832144	381120.735044	45.931341
3501.428816	381126.470507	45.936346
3501.678984	381122.692153	45.941351
3501.661082	381131.189839	45.946356
3501.560033	381119.455356	45.951361
3501.745209	381109.532291	45.956365
3501.596371	381114.744282	45.961370
3502.098586	381121.710021	45.966375
3501.822751	381135.945654	45.971380
3501.936369	381121.633856	45.976385
3502.270084	381115.426081	45.981389
3501.858646	381096.263116	45.986394
3501.623627	381090.882826	45.991399
3501.376835	381086.954125	45.996404
3501.511891	381083.015927	46.001409
3501.526318	381091.686548	46.006413
3501.557932	381100.786825	46.011418
3502.097806	381092.918691	46.016423
3501.588339	381091.829237	46.021428
3501.694341	381102.291181	46.026433
3501.728476	381095.596651	46.031437
3501.816225	381094.641691	46.036442
3501.871302	381097.812177	46.041447
3501.753048	381100.170746	46.046452
3501.841376	381093.925458	46.051457
3501.798885	381087.370210	46.056461
3501.659871	381080.219807	46.061466
3501.964038	381064.580739	46.066471
3501.762910	381074.023021	46.071476
3501.689307	381072.381420	46.076481
3501.846358	381065.998094	46.081485
3501.689841	381078.434517	46.086490
3502.038688	381073.877543	46.091495
3502.058913	381081.326425	46.096500
3501.844126	381064.828344	46.101505
3501.954619	381041.386257	46.106509
3501.328260	381048.504984	46.111514
3501.607667	381047.061915	46.116519
3501.636015	381048.507127	46.121524
3501.535259	381052.083759	46.126529
3501.710806	381038.474288	46.131533
3501.682753	381044.074137	46.136538
3501.881070	381040.710913	46.141543
3501.765978	381051.513029	46.146548
3501.830528	381045.373227	46.151553
3502.187822	381047.554888	46.156557
3501.889825	381044.320992	46.161562
3501.614323	381032.842966	46.166567
3501.710496	381019.754714	46.171572
3501.442371	381027.350925	46.176577
3501.802106	381024.572595	46.181581
3501.755550	381021.655023	46.186586
3501.755178	381008.632897	46.191591
3501.432627	381012.982177	46.196596
3501.620201	381017.072777	46.201601
3501.760341	381028.750171	46.206605
3501.600391	381030.632092	46.211610
3501.909542	381016.263911	46.216615
3501.756591	381022.036110	46.221620
3501.764594	381013.972268	46.226625
3501.535149	381028.505814	46.231629
3501.407634	381041.115702	46.236634
3501.960932	381028.031490	46.241639
3501.692919	381033.567538	46.246644
3501.826025	381030.062019	46.251649
3501.990629	381009.714291	46.256653
3501.482244	381000.053443	46.261658
3501.745891	381010.515924	46.266663
3501.769871	380999.041412	46.271668
3501.790963	380997.613743	46.276673
3501.649520	380990.361972	46.281677
3501.449091	381017.022904	46.286682
3501.994838	380997.734008	46.291687
3501.602487	381007.003064	46.296692
3501.583234	380990.448606	46.301697
3501.848356	381013.169991	46.306701
3501.728470	380995.944730	46.311706
3502.002378	381007.244908	46.316711
3501.729225	380984.016038	46.321716
3501.895695	380974.706309	46.326721
3501.626088	380979.505034	46.331725
3501.453310	380986.959011	46.336730
3501.859975	380966.013448	46.341735
3501.539375	380972.448006	46.346740
3501.371119	380986.285179	46.351745
3501.803107	380974.237482	46.356749
3501.717109	380978.142429	46.361754
3501.674221	380979.751508	46.366759
3501.761141	380983.832590	46.371764
3501.787556	380980.013292	46.376769
3502.191573	380979.466142	46.381773
3501.979748	380979.906534	46.386778
3502.079969	380957.534245	46.391783
3501.846243	380947.041512	46.396788
3501.546061	380947.750211	46.401793
3501.924846	380948.249841	46.406797
3501.756143	380950.158584	46.411802
3502.038503	380947.392481	46.416807
3501.692724	380957.315469	46.421812
3501.483143	380952.465251	46.426817
3501.629304	380947.457059	46.431821
3501.740679	380955.451102	46.436826
3502.170532	380935.926157	46.441831
3501.856203	380939.790901	46.446836
3502.023755	380921.909753	46.451841
3502.447078	380912.279631	46.456845
3502.011901	380906.396844	46.461850
3501.974182	380914.668805	46.466855
3501.802389	380892.899026	46.471860
3501.801098	380886.311796	46.476865
3501.869028	380882.613096	46.481869
3501.597896	380880.900977	46.486874
3501.953198	380899.335265	46.491879
3502.047860	380899.879811	46.496884
3501.549390	380893.472915	46.501889
3501.832576	380877.481013	46.506893
3501.901849	380866.075604	46.511898
3501.814608	380871.862872	46.516903
3502.066893	380850.382104	46.521908
3501.936863	380849.156358	46.526913
3501.847542	380866.287514	46.531917
3501.751694	380852.975222	46.536922
3501.960914	380848.847238	46.541927
3501.953267	380839.285228	46.546932
3501.831254	380827.172461	46.551937
3502.166746	380810.078600	46.556941
3501.938912	380816.498519	46.561946
3502.057795	380818.158333	46.566951
3502.010702	380816.054719	46.571956
3501.684430	380790.748540	46.576961
3501.969868	380779.537840	46.581965
3501.668760	380784.799381	46.586970
3501.823343	380776.483411	46.591975
3501.917673	380782.572632	46.596980
3501.576507	380774.792844	46.601985
3501.714876	380779.069287	46.606989
3501.761376	380780.740546	46.611994
3501.588099	380785.167989	46.616999
3501.625307	380796.505648	46.622004
3501.686975	380785.279456	46.627009
3501.851885	380780.853261	46.632013
3501.724825	380795.294407	46.637018
3501.709823	380783.012105	46.642023
3501.858440	380781.844043	46.647028
3501.558194	380753.659680	46.652033
3501.821444	380752.117419	46.657037
3501.654506	380742.529698	46.662042
3501.893006	380739.414437	46.667047
3501.593538	380757.316450	46.672052
3501.716327	380756.839190	46.677057
3501.837271	380750.334350	46.682061
3501.695011	380763.226433	46.687066
3501.890852	380759.202291	46.692071
3501.880699	380762.891797	46.697076
3501.748534	380768.050331	46.702081
3501.958938	380740.700859	46.707085
3501.721677	380731.785538	46.712090
3501.761550	380711.355636	46.717095
3501.690844	380717.928769	46.722100
3501.594043	380728.117665	46.727105
3501.986136	380723.579248	46.732109
3501.565165	380730.207751	46.737114
3501.557356	380728.453998	46.742119
3502.036651	380722.248581	46.747124
3501.401060	380717.516547	46.752129
3501.450448	380737.499883	46.757133
3501.592296	380741.546873	46.762138
3501.627140	380727.476289	46.767143
3501.571120	380755.284539	46.772148
3501.608164	380754.897135	46.777153
3502.012270	380727.745939	46.782157
3501.551182	380745.368299	46.787162
3501.677053	380741.482387	46.792167
3501.827990	380719.152810	46.797172
3502.025421	380705.158252	46.802177
3501.997942	380686.570238	46.807181
3501.628605	380715.801488	46.812186
3501.668905	380704.807557	46.817191
3501.453892	380710.080932	46.822196
3501.575917	380706.348229	46.827201
3501.465051	380714.530059	46.832205
3501.433495	380710.312953	46.837210
3501.974722	380698.502243	46.842215
3501.695503	380710.932747	46.847220
3501.577280	380719.548119	46.852225
3502.045907	380704.925705	46.857229
3501.717749	380706.427288	46.862234
3501.706550	380695.314325	46.867239
3501.673283	380684.866133	46.872244
3501.737928	380682.363336	46.877249
3502.236081	380675.315605	46.882253
3501.860795	380674.484701	46.887258
3501.696301	380679.470319	46.892263
3501.475477	380685.355035	46.897268
3501.574931	380688.722011	46.902273
3501.773195	380677.245287	46.907277
3501.598213	380688.667389	46.912282
3501.575472	380693.783201	46.917287
3501.450023	380677.423436	46.922292
3501.594126	380691.287637	46.927297
3501.589245	380698.333616	46.932301
3501.249098	380698.463654	46.937306
3501.332434	380680.875483	46.942311
3501.597581	380704.817881	46.947316
3501.764053	380686.682454	46.952321
3501.603637	380694.312572	46.957325
3501.254093	380699.225704	46.962330
3501.675490	380700.074679	46.967335
3501.484597	380680.774906	46.972340
3501.549844	380712.023054	46.977345
3501.928073	380685.003090	46.982349
3501.718192	380708.969712	46.987354
3501.583147	380694.544462	46.992359
3501.765102	380703.366724	46.997364
3501.682857	380702.845574	47.002369
3501.679766	380705.287698	47.007373
3501.725039	380686.128633	47.012378
3501.890986	380663.745784	47.017383
3501.502474	380679.805219	47.022388
3501.066832	380665.808989	47.027393
3502.134211	380678.611612	47.032397
3501.848001	380671.382666	47.037402
3501.683136	380663.066303	47.042407
3501.758550	380665.674059	47.047412
3501.384873	380668.708886	47.052417
3501.785638	380657.963167	47.057421
3501.507270	380672.886091	47.062426
3501.730798	380674.809145	47.067431
3501.543544	380676.466493	47.072436
3501.547407	380667.741947	47.077441
3501.711480	380667.105554	47.082445
3501.380151	380687.276272	47.087450
3501.299222	380666.483931	47.092455
3501.436532	380698.203947	47.097460
3501.523024	380681.505470	47.102465
3501.771894	380666.459968	47.107469
3501.732286	380699.021842	47.112474
3502.030551	380679.721043	47.117479
3501.653223	380683.875547	47.122484
3501.675172	380703.837804	47.127489
3502.229062	380672.211925	47.132493
3501.889446	380660.820226	47.137498
3501.625765	380671.137255	47.142503
3501.824395	380665.408577	47.147508
3501.861907	380639.103730	47.152513
3502.156687	380678.022160	47.157517
3501.597071	380656.491595	47.162522
3502.045978	380673.639488	47.167527
3502.090524	380648.020255	47.172532
3501.302197	380632.070471	47.177537
3501.519278	380621.074004	47.182541
3501.431890	380632.126198	47.187546
3501.765282	380623.883666	47.192551
3501.618786	380612.944672	47.197556
3501.750001	380631.211040	47.202561
3501.946452	380628.153285	47.207565
3501.582318	380615.468308	47.212570
3501.879476	380643.220806	47.217575
3502.195110	380621.551859	47.222580
3501.669025	380636.819167	47.227585
3501.816853	380636.846630	47.232589
3501.833814	380596.301886	47.237594
3501.687613	380614.535814	47.242599
3501.940466	380598.497725	47.247604
3501.144893	380595.418752	47.252609
3501.416894	380608.347135	47.257613
3501.404832	380605.474946	47.262618
3501.859050	380596.297677	47.267623
3501.758630	380588.021979	47.272628
3501.677230	380605.126564	47.277633
3501.829081	380617.336348	47.282637
3501.741009	380597.282689	47.287642
3501.706391	380598.966780	47.292647
3501.549937	380600.593828	47.297652
3501.494151	380605.358797	47.302657
3501.701438	380607.309855	47.307661
3501.771478	380615.539410	47.312666
3501.376784	380613.236393	47.317671
3501.808490	380606.656968	47.322676
3501.253386	380619.258285	47.327681
3501.496328	380613.191951	47.332685
3501.481164	380608.717902	47.337690
3501.438286	380617.245083	47.342695
3501.188936	380635.469873	47.347700
3501.870983	380615.116441	47.352705
3501.719606	380613.461681	47.357709
3501.420984	380631.974038	47.362714
3501.671656	380621.760719	47.367719
3502.136359	380623.798254	47.372724
3501.696563	380625.546395	47.377729
3501.887263	380618.598126	47.382733
3501.562087	380608.018021	47.387738
3501.421879	380594.483745	47.392743
3501.444723	380592.292760	47.397748
3501.308579	380612.305490	47.402753
3501.922649	380615.540252	47.407757
3501.178103	380610.774560	47.412762
3501.189296	380609.221271	47.417767
3501.667506	380631.756589	47.422772
3501.343497	380640.836890	47.427777
3501.788564	380654.348317	47.432781
3501.849960	380623.995659	47.437786
3501.673045	380650.322481	47.442791
3501.846854	380617.917317	47.447796
3501.685815	380623.970629	47.452801
3502.122072	380599.154202	47.457805
3501.534220	380605.910844	47.462810
3501.655416	380610.368058	47.467815
3501.837364	380588.949134	47.472820
3501.513228	380608.304863	47.477825
3501.397191	380607.305804	47.482829
3501.701350	380615.625519	47.487834
3501.871178	380612.571972	47.492839
3501.517713	380610.821988	47.497844
3501.368096	380618.475847	47.502849
3501.917654	380610.428047	47.507853
3501.714379	380614.300701	47.512858
3501.559517	380636.834358	47.517863
3501.856775	380610.234088	47.522868
3501.729299	380607.659920	47.527873
3501.880185	380605.575865	47.532877
3501.534691	380598.051068	47.537882
3501.596712	380588.808626	47.542887
3501.655696	380584.170248	47.547892
3501.603372	380600.074833	47.552897
3502.052584	380582.098134	47.557901
3501.646061	380579.440906	47.562906
3501.474663	380589.845104	47.567911
3501.951916	380591.143066	47.572916
3501.801799	380598.924179	47.577921
3501.896002	380592.601579	47.582925
3501.597584	380604.501035	47.587930
3501.649199	380590.860131	47.592935
3501.692242	380594.617545	47.597940
3501.505178	380603.549035	47.602945
3501.728148	380595.603728	47.607949
3501.929613	380588.730054	47.612954
3501.452778	380573.494029	47.617959
3501.855756	380551.200815	47.622964
3501.584954	380558.441462	47.627969
3501.860086	380559.695075	47.632973
3501.575728	380566.047667	47.637978
3501.767904	380571.358427	47.642983
3501.684243	380565.420019	47.647988
3501.507877	380563.184222	47.652993
3501.772981	380557.572191	47.657997
3501.896694	380567.039546	47.663002
3502.016522	380574.828858	47.668007
3501.883890	380566.202169	47.673012
3501.792706	380548.972171	47.678017
3501.862979	380531.640340	47.683021
3501.671046	380542.276704	47.688026
3501.810596	380529.639246	47.693031
3501.910675	380531.429216	47.698036
3501.720523	380530.543609	47.703041
3501.770138	380528.755335	47.708045
3501.865235	380531.792369	47.713050
3501.888892	380544.124177	47.718055
3501.979851	380526.331258	47.723060
3501.874933	380516.046953	47.728065
3501.992864	380509.695155	47.733069
3501.895221	380507.294304	47.738074
3501.882767	380503.125024	47.743079
3502.022222	380498.194138	47.748084
3501.482460	380502.043694	47.753089
3501.750180	380498.771189	47.758093
3501.354906	380513.102235	47.763098
3501.346325	380512.518568	47.768103
3501.981836	380508.475764	47.773108
3501.925162	380505.763225	47.778113
3501.977259	380480.676807	47.783117
3501.712365	380470.773860	47.788122
3501.566053	380465.226854	47.793127
3501.981829	380468.289502	47.798132
3501.426482	380476.846858	47.803137
3501.653182	380468.290514	47.808141
3501.765353	380468.145574	47.813146
3501.571101	380474.102423	47.818151
3501.609319	380469.416445	47.823156
3501.302869	380460.715474	47.828161
3501.597635	380473.182486	47.833165
3501.653410	380487.900054	47.838170
3501.787280	380476.306279	47.843175
3502.041846	380460.191559	47.848180
3501.619417	380488.566608	47.853185
3501.766613	380480.099137	47.858189
3501.848962	380452.032113	47.863194
3501.864353	380440.965742	47.868199
3501.667926	380431.942161	47.873204
3501.652276	380439.549443	47.878209
3501.762904	380444.262690	47.883213
3501.299696	380451.864418	47.888218
3501.630014	380440.086972	47.893223
3501.642171	380441.483897	47.898228
3501.358965	380453.024915	47.903233
3501.618321	380454.230156	47.908237
3501.770006	380452.196835	47.913242
3501.448795	380449.475243	47.918247
3501.474526	380454.252778	47.923252
3501.349750	380459.562790	47.928257
3501.331509	380449.035858	47.933261
3501.609472	380461.124017	47.938266
3501.693771	380455.311645	47.943271
3501.795484	380456.516374	47.948276
3501.620932	380468.548895	47.953281
3501.829719	380470.118209	47.958285
3501.885501	380460.876724	47.963290
3501.718589	380463.853446	47.968295
3501.902702	380453.650605	47.973300
3501.890603	380462.808811	47.978305
3501.728202	380445.717197	47.983309
3501.627406	380436.118944	47.988314
3501.635762	380427.520806	47.993319
3501.722308	380427.125573	47.998324
3501.324962	380434.513419	48.003329
3501.427242	380435.489150	48.008333
3501.854025	380425.654888	48.013338
3501.691656	380428.681763	48.018343
3501.488551	380423.474375	48.023348
3501.460286	380425.615285	48.028353
3501.889123	380420.231694	48.033357
3501.657998	380429.119320	48.038362
3501.458574	380423.377230	48.043367
3501.860215	380427.688395	48.048372
3501.735324	380421.196929	48.053377
3501.464004	380443.087817	48.058381
3501.725346	380434.983806	48.063386
3501.763948	380432.866623	48.068391
3501.694300	380432.165437	48.073396
3501.606431	380445.837489	48.078401
3501.883149	380434.602634	48.083405
3502.112009	380435.380314	48.088410
3501.679386	380431.302884	48.093415
3501.964963	380410.427033	48.098420
3501.669291	380396.739225	48.103425
3501.595174	380403.440122	48.108429
3501.927449	380406.973792	48.113434
3501.991943	380399.028063	48.118439
3501.841052	380405.461320	48.123444
3501.808858	380413.554473	48.128449
3502.027506	380390.730753	48.133453
3501.897135	380373.634044	48.138458
3501.494297	380381.149940	48.143463
3502.065049	380373.760033	48.148468
3501.945921	380380.595221	48.153473
3501.606322	380378.003702	48.158477
3501.705635	380374.020215	48.163482
3501.541740	380370.536154	48.168487
3501.754913	380370.502418	48.173492
3501.605868	380374.137614	48.178497
3501.961279	380370.978408	48.183501
3501.752988	380370.477178	48.188506
3501.618128	380361.443847	48.193511
3501.674766	380339.561344	48.198516
3501.629406	380339.873690	48.203521
3501.544150	380330.679904	48.208525
3501.409214	380343.189453	48.213530
3501.532372	380336.480720	48.218535
3501.688792	380324.120305	48.223540
3501.430770	380359.896283	48.228545
3501.389424	380339.631630	48.233549
3501.430035	380355.267281	48.238554
3501.477885	380353.631883	48.243559
3501.645599	380350.629519	48.248564
3501.484599	380358.514137	48.253569
3501.544139	380341.056746	48.258573
3501.326043	380375.580115	48.263578
3501.654512	380375.426416	48.268583
3501.839539	380373.921940	48.273588
3501.533692	380367.459071	48.278593
3501.531856	380362.957452	48.283597
3501.924321	380345.879816	48.288602
3501.603071	380352.670658	48.293607
3501.896004	380362.874342	48.298612
3501.683553	380351.030066	48.303617
3501.473035	380361.465943	48.308621
3501.576722	380377.956380	48.313626
3501.538506	380346.016891	48.318631
3501.577153	380370.300513	48.323636
3501.389117	380354.866142	48.328641
3501.878128	380357.255929	48.333645
3501.789787	380363.450395	48.338650
3501.682278	380360.873055	48.343655
3501.950994	380363.653747	48.348660
3501.801435	380375.631477	48.353665
3502.056453	380367.655623	48.358669
3501.786995	380330.004523	48.363674
3501.591297	380350.128539	48.368679
3502.058157	380327.469018	48.373684
3501.886574	380321.137523	48.378689
3502.117421	380337.811349	48.383693
3502.119656	380337.225969	48.388698
3501.664466	380313.771132	48.393703
3501.957828	380318.913325	48.398708
3501.727671	380307.427916	48.403713
3501.822186	380293.067964	48.408717
3501.712887	380289.422659	48.413722
3501.736647	380287.104339	48.418727
3502.062198	380293.894680	48.423732
3501.686243	380290.927388	48.428737
3501.811798	380286.888874	48.433741
3501.849066	380293.724789	48.438746
3501.696859	380288.916286	48.443751
3501.679995	380270.631607	48.448756
3501.455203	380257.949920	48.453761
3501.731254	380258.440366	48.458765
3501.788209	380273.259565	48.463770
3501.530046	380267.653910	48.468775
3501.813096	380255.019112	48.473780
3501.618255	380276.363881	48.478785
3501.510183	380273.379674	48.483789
3502.019749	380263.532284	48.488794
3501.892241	380269.198835	48.493799
3501.748705	380255.664967	48.498804
3501.756725	380270.262994	48.503809
3501.729911	380268.944609	48.508813
3501.562283	380263.553551	48.513818
3501.476143	380280.277512	48.518823
3501.876145	380271.948072	48.523828
3501.747817	380249.865849	48.528833
3501.628265	380235.285373	48.533837
3501.693714	380251.731039	48.538842
3501.599482	380241.012588	48.543847
3501.589100	380238.114672	48.548852
3501.384865	380232.729397	48.553857
3501.696436	380262.590942	48.558861
3501.728057	380230.716622	48.563866
3501.298605	380256.498641	48.568871
3501.523490	380231.155838	48.573876
3501.267590	380273.798845	48.578881
3501.676855	380240.720286	48.583885
3501.489552	380250.643835	48.588890
3501.444330	380238.773089	48.593895
3501.884269	380255.642806	48.598900
3501.719370	380236.033491	48.603905
3501.748385	380271.128313	48.608909
3501.337994	380258.577704	48.613914
3501.920746	380239.308018	48.618919
3501.971173	380277.883961	48.623924
3501.670841	380252.980282	48.628929
3502.050484	380260.372503	48.633933
3501.814429	380258.451335	48.638938
3501.900381	380254.546251	48.643943
3501.547914	380233.008139	48.648948
3501.958474	380194.817024	48.653953
3501.934065	380240.272127	48.658957
3501.730345	380243.559897	48.663962
3501.504640	380213.354042	48.668967
3501.964764	380218.546189	48.673972
3501.676540	380234.539084	48.678977
3501.789190	380212.240704	48.683981
3502.065398	380237.071847	48.688986
3501.994066	380188.503368	48.693991
3501.794041	380194.384869	48.698996
3501.683714	380198.598953	48.704001
3501.563140	380176.744372	48.709005
3501.869786	380189.489377	48.714010
3501.507837	380198.702950	48.719015
3502.054682	380153.800997	48.724020
3501.931274	380180.984449	48.729025
3501.697427	380202.818678	48.734029
3501.969631	380172.584949	48.739034
3501.648857	380191.889484	48.744039
3501.907389	380169.135633	48.749044
3501.247870	380147.722317	48.754049
3501.367402	380163.523609	48.759053
3501.585855	380134.061381	48.764058
3501.176800	380177.466303	48.769063
3501.492136	380163.808994	48.774068
3501.298811	380193.572368	48.779073
3501.496047	380212.642396	48.784077
3501.753922	380194.034471	48.789082
3501.635423	380204.328672	48.794087
3501.671291	380200.049984	48.799092
3501.594167	380203.114269	48.804097
3501.751393	380217.892204	48.809101
3502.176453	380167.185040	48.814106
3501.600166	380191.082731	48.819111
3502.100022	380160.024537	48.824116
3501.664941	380172.276376	48.829121
3501.623536	380184.872928	48.834125
3501.586052	380181.445169	48.839130
3501.715679	380166.825276	48.844135
3501.915208	380166.666525	48.849140
3501.716955	380182.467177	48.854145
3501.830248	380166.756186	48.859149
3501.958696	380131.865214	48.864154
3501.819354	380146.639190	48.869159
3501.766323	380144.078657	48.874164
3501.591405	380139.019381	48.879169
3501.594002	380127.802338	48.884173
3501.629416	380150.051852	48.889178
3501.371838	380124.022216	48.894183
3501.533626	380147.014787	48.899188
3501.504885	380136.642037	48.904193
3501.475678	380149.033197	48.909197
3501.600929	380137.262643	48.914202
3501.286094	380148.198322	48.919207
3501.621881	380134.436032	48.924212
3501.467911	380152.467929	48.929217
3501.374111	380119.036408	48.934221
3501.561705	380162.168986	48.939226
3501.280629	380145.274042	48.944231
3501.628342	380143.692970	48.949236
3501.239340	380149.782393	48.954241
3501.446615	380164.984822	48.959245
3501.716418	380144.060454	48.964250
3501.256077	380185.133506	48.969255
3501.800365	380184.436999	48.974260
3501.344013	380155.183201	48.979265
3501.324872	380187.615094	48.984269
3501.688137	380170.033309	48.989274
3501.370878	380214.263016	48.994279
3501.436836	380186.452736	48.999284
3501.599669	380204.078444	49.004289
3501.158329	380216.992553	49.009293
3501.329518	380191.709082	49.014298
3501.274555	380212.243307	49.019303
3501.428061	380203.037181	49.024308
3501.322901	380222.740000	49.029313
3501.124334	380187.341217	49.034317
3501.021709	380220.218667	49.039322
3501.455795	380199.319226	49.044327
3501.392362	380199.914209	49.049332
3501.662267	380235.555974	49.054337
3501.309225	380235.688051	49.059341
3501.669246	380252.010846	49.064346
3501.216439	380259.610968	49.069351
3501.728747	380233.001879	49.074356
3501.732188	380270.923962	49.079361
3502.028206	380226.036310	49.084365
3501.564405	380243.989972	49.089370
3501.606668	380210.486152	49.094375
3502.086807	380227.578435	49.099380
3501.860546	380207.037733	49.104385
3501.712054	380235.674873	49.109389
3502.082143	380217.837687	49.114394
3501.886670	380225.015619	49.119399
3501.709761	380204.696024	49.124404
3501.795193	380218.595103	49.129409
3501.771764	380193.240661	49.134413
3501.704593	380178.702752	49.139418
3501.623462	380201.072399	49.144423
3501.637677	380183.596668	49.149428
3501.949443	380165.895850	49.154433
3501.736060	380205.251167	49.159437
3501.729811	380192.941861	49.164442
3501.957959	380164.546369	49.169447
3502.052396	380212.068341	49.174452
3501.968484	380186.341940	49.179457
3501.856621	380165.783132	49.184461
3501.806508	380148.088644	49.189466
3501.584682	380157.381814	49.194471
3501.941082	380135.706153	49.199476
3501.737358	380156.645440	49.204481
3501.506826	380155.181215	49.209485
3501.694524	380135.134593	49.214490
3501.665673	380157.699475	49.219495
3501.476365	380160.578023	49.224500
3501.535380	380153.370709	49.229505
3501.369889	380161.128905	49.234509
3501.776674	380145.040861	49.239514
3501.141629	380169.736322	49.244519
3501.788893	380133.389876	49.249524
3501.661016	380173.647348	49.254529
3501.292854	380150.051482	49.259533
3501.940449	380162.361080	49.264538
3501.569246	380152.195079	49.269543
3501.565340	380165.955693	49.274548
3501.588850	380172.208811	49.279553
3501.629725	380165.385884	49.284557
3501.869482	380169.188546	49.289562
3501.532346	380172.319372	49.294567
3501.307358	380167.496925	49.299572
3501.557265	380174.197507	49.304577
3501.262786	380175.719220	49.309581
3501.543973	380162.754039	49.314586
3501.131197	380179.656852	49.319591
3501.586690	380191.233776	49.324596
3501.535488	380160.695081	49.329601
3501.747552	380185.027708	49.334605
3501.652508	380156.632432	49.339610
3501.479564	380195.218334	49.344615
3501.822349	380160.140898	49.349620
3501.633554	380203.205758	49.354625
3501.337245	380190.484486	49.359629
3501.999332	380157.518496	49.364634
3501.892682	380173.177499	49.369639
3501.657064	380170.594964	49.374644
3501.775054	380148.397441	49.379649
3501.616707	380157.934919	49.384653
3502.072013	380130.724346	49.389658
3501.574886	380176.483162	49.394663
3501.638803	380144.832576	49.399668
3501.654022	380166.169633	49.404673
3501.354379	380145.894844	49.409677
3502.060249	380117.805314	49.414682
3501.956116	380161.162051	49.419687
3502.108550	380150.430016	49.424692
3502.227459	380136.295061	49.429697
3501.831597	380114.331357	49.434701
3502.226169	380115.489800	49.439706
3501.676511	380112.906036	49.444711
3502.124374	380095.081933	49.449716
3501.859168	380090.062359	49.454721
3501.595122	380094.631403	49.459725
3501.790953	380078.017121	49.464730
3501.555270	380061.038661	49.469735
3501.654469	380082.438791	49.474740
3501.437974	380062.227118	49.479745
3501.372389	380089.401492	49.484749
3501.717223	380053.738643	49.489754
3501.368351	380089.147712	49.494759
3501.759481	380064.007431	49.499764
3501.599684	380062.506585	49.504769
3501.731071	380074.211084	49.509773
3501.707497	380062.311427	49.514778
3501.402796	380087.514277	49.519783
3501.595747	380079.675349	49.524788
3501.867375	380071.111815	49.529793
3501.578943	380085.527865	49.534797
3501.715420	380077.545257	49.539802
3501.319296	380100.727792	49.544807
3501.851914	380092.504522	49.549812
3501.667294	380076.306465	49.554817
3501.520321	380095.710745	49.559821
3501.475354	380071.478746	49.564826
3501.328959	380094.418330	49.569831
3501.590959	380079.014443	49.574836
3501.290532	380104.674427	49.579841
3501.666708	380075.721345	49.584845
3501.878644	380073.780218	49.589850
3501.721749	380096.874067	49.594855
3501.790182	380086.740286	49.599860
3501.816543	380100.648746	49.604865
3501.711336	380091.432623	49.609869
3501.940047	380063.443920	49.614874
3501.636412	380082.618627	49.619879
3502.071622	380063.168702	49.624884
3502.056183	380051.547536	49.629889
3501.553292	380075.789778	49.634893
3502.025077	380053.231058	49.639898
3501.678575	380067.401949	49.644903
3501.785826	380063.366306	49.649908
3501.822127	380059.062100	49.654913
3501.704163	380031.992951	49.659917
3501.569260	380027.436026	49.664922
3501.621552	380031.675289	49.669927
3501.856736	380017.827124	49.674932
3501.726365	380015.227940	49.679937
3501.446004	380032.542270	49.684941
3501.578876	380020.567000	49.689946
3501.516394	380026.655694	49.694951
3501.473888	380011.299918	49.699956
3501.449125	380037.755708	49.704961
3501.559610	380015.584730	49.709965
3501.553678	380022.961646	49.714970
3501.412646	380030.843174	49.719975
3501.738351	380025.424963	49.724980
3501.792704	380021.499417	49.729985
3501.734197	380027.867262	49.734989
3501.986706	380036.297004	49.739994
3502.080038	380039.486963	49.744999
3501.724562	380017.465952	49.750004
3501.928133	380034.500303	49.755009
3501.944159	380000.415456	49.760013
3501.670811	379985.045294	49.765018
3501.557762	380007.877919	49.770023
3501.973024	379982.097906	49.775028
3501.890393	379999.177517	49.780033
3501.448220	380006.419922	49.785037
3501.800461	380001.760550	49.790042
3501.796528	379997.284655	49.795047
3501.684712	379994.301018	49.800052
3501.607025	380013.974164	49.805057
3501.653795	379978.053152	49.810061
3501.748507	380006.880923	49.815066
3501.715442	379996.127301	49.820071
3501.843860	379983.338818	49.825076
3501.879714	379981.603564	49.830081
3501.656772	379954.144004	49.835085
3501.587835	379959.928514	49.840090
3501.792650	379971.926650	49.845095
3501.595617	379944.284945	49.850100
3501.718076	379980.230033	49.855105
3501.884422	379957.872150	49.860109
3501.925229	379959.976733	49.865114
3501.573229	379989.409261	49.870119
3502.196525	379962.909617	49.875124
3501.982150	379952.718771	49.880129
3501.680137	379953.682123	49.885133
3501.867029	379929.184471	49.890138
3501.661477	379932.726903	49.895143
3501.811282	379924.716722	49.900148
3501.670649	379921.279813	49.905153
3501.681840	379945.568040	49.910157
3501.820593	379929.725756	49.915162
3501.515863	379939.845989	49.920167
3501.644731	379932.678462	49.925172
3502.001495	379948.264296	49.930177
3501.684006	379938.013443	49.935181
3502.079888	379894.330484	49.940186
3501.908697	379911.983694	49.945191
3501.919153	379891.379971	49.950196
3501.570270	379891.511391	49.955201
3501.707051	379913.948491	49.960205
3502.184925	379902.961465	49.965210
3501.699673	379904.259000	49.970215
3501.832311	379903.983649	49.975220
3502.090426	379878.711669	49.980225
3501.757550	379876.017315	49.985229
3502.185060	379870.125166	49.990234
3501.877104	379888.283265	49.995239
3501.842774	379871.883323	50.000244
3501.844907	379863.260610	50.005249
3501.822839	379892.564750	50.010253
3501.758216	379840.764583	50.015258
3501.707168	379826.376602	50.020263
3501.720691	379833.267219	50.025268
3501.765715	379834.023105	50.030273
3501.772718	379843.229305	50.035277
3501.858112	379835.127550	50.040282
3501.665596	379834.674689	50.045287
3501.539200	379832.354645	50.050292
3501.844567	379838.843041	50.055297
3501.606939	379838.677092	50.060301
3501.405122	379829.628788	50.065306
3501.436086	379847.275504	50.070311
3501.766180	379828.274470	50.075316
3502.197771	379852.750642	50.080321
3501.486412	379818.500845	50.085325
3501.645754	379858.433455	50.090330
3501.488559	379824.630186	50.095335
3501.696801	379828.285255	50.100340
3501.611312	379833.309360	50.105345
3501.264389	379800.222798	50.110349
3501.796391	379811.838609	50.115354
3501.939682	379796.682290	50.120359
3501.593189	379812.099571	50.125364
3501.944605	379806.168573	50.130369
3501.856616	379811.828942	50.135373
3501.808613	379789.047025	50.140378
3501.852285	379818.951260	50.145383
3501.889722	379788.347393	50.150388
3502.057102	379811.059497	50.155393
3501.699140	379767.597306	50.160397
3502.037353	379771.587920	50.165402
3501.645709	379779.788898	50.170407
3501.779445	379748.228693	50.175412
3501.990536	379757.021129	50.180417
3501.569067	379760.623144	50.185421
3501.634884	379773.991353	50.190426
3501.604831	379757.412644	50.195431
3501.598732	379782.059792	50.200436
3501.809279	379767.096307	50.205441
3501.633024	379771.626075	50.210445
3501.867391	379749.562537	50.215450
3501.459416	379781.878192	50.220455
3501.647808	379774.014489	50.225460
3501.512484	379756.231556	50.230465
3501.513536	379781.386268	50.235469
3501.818487	379759.515055	50.240474
3501.356761	379741.554802	50.245479
3501.617215	379777.020436	50.250484
3501.839085	379732.296548	50.255489
3501.481827	379758.983131	50.260493
3501.210501	379742.442557	50.265498
3501.852901	379726.698616	50.270503
3501.631142	379764.249835	50.275508
3501.925938	379731.926549	50.280513
3501.586047	379759.398863	50.285517
3501.950932	379749.447043	50.290522
3501.549442	379751.138297	50.295527
3501.528391	379757.474830	50.300532
3501.925351	379745.559467	50.305537
3501.403327	379766.651020	50.310541
3501.903818	379743.451717	50.315546
3501.600436	379750.901141	50.320551
3501.545816	379752.639299	50.325556
3501.849665	379751.344928	50.330561
3501.525470	379746.843328	50.335565
3501.792683	379741.815846	50.340570
3501.563862	379752.254779	50.345575
3501.778295	379752.831277	50.350580
3501.899630	379719.263667	50.355585
3501.501624	379714.417646	50.360589
3502.017638	379720.007981	50.365594
3502.267144	379695.805502	50.370599
3501.652017	379723.092439	50.375604
3502.030129	379707.593747	50.380609
3501.812957	379709.204996	50.385613
3501.912062	379706.798427	50.390618
3501.662480	379673.696370	50.395623
3501.760960	379689.882703	50.400628
3501.946167	379666.046457	50.405633
3501.307998	379687.283587	50.410637
3501.701068	379671.807951	50.415642
3502.021337	379668.323593	50.420647
3501.726216	379677.119767	50.425652
3502.102918	379669.429752	50.430657
3502.151062	379677.434054	50.435661
3501.623414	379647.173755	50.440666
3501.778182	379661.265550	50.445671
3501.549911	379648.813127	50.450676
3501.680521	379639.635924	50.455681
3501.639972	379633.919472	50.460685
3501.893493	379642.705226	50.465690
3501.815990	379633.738964	50.470695
3501.858291	379627.907674	50.475700
3501.792303	379644.348939	50.480705
3501.851085	379622.999826	50.485709
3501.651696	379642.412615	50.490714
3501.740942	379644.229774	50.495719
3501.810409	379633.790496	50.500724
3501.908652	379585.423376	50.505729
3501.619792	379627.589034	50.510733
3501.593152	379599.538628	50.515738
3501.456725	379568.300770	50.520743
3501.752620	379550.068052	50.525748
3501.582835	379492.484906	50.530753
3501.395606	379475.829186	50.535757
3501.280827	379385.324431	50.540762
3501.161162	379341.925838	50.545767
3501.157056	379233.725929	50.550772
3501.055240	379160.132907	50.555777
3500.804441	379096.737353	50.560781
3500.500482	378956.332326	50.565786
3500.036512	378882.541686	50.570791
3499.675947	378751.021786	50.575796
3499.704417	378621.194994	50.580801
3499.162193	378497.079245	50.585805
3498.941653	378365.154396	50.590810
3498.522659	378216.294877	50.595815
3497.761375	378071.812997	50.600820
3497.334102	377931.093171	50.605825
3497.228347	377784.700673	50.610829
3497.204484	377619.472001	50.615834
3496.756655	377466.417290	50.620839
3496.331054	377297.333629	50.625844
3496.040130	377117.035952	50.630849
3495.471869	376942.911509	50.635853
3495.391884	376753.065603	50.640858
3494.613203	376558.725209	50.645863
3494.060215	376377.855176	50.650868
3493.727296	376182.425031	50.655873
3493.088343	375984.981921	50.660877
3492.533266	375771.371950	50.665882
3492.251624	375571.987995	50.670887
3491.656183	375384.252168	50.675892
3491.292956	375172.999861	50.680897
3490.625743	374949.711594	50.685901
3490.568149	374724.061768	50.690906
3489.814285	374518.642255	50.695911
3489.204477	374290.940566	50.700916
3488.892915	374053.727428	50.705921
3488.189376	373831.939720	50.710925
3487.603326	373614.889269	50.715930
3487.130790	373377.087194	50.720935
3486.743011	373141.941446	50.725940
3485.991954	372893.241943	50.730945
3485.283517	372660.001233	50.735949
3485.113666	372413.521971	50.740954
3484.286086	372168.620738	50.745959
3483.754021	371924.002084	50.750964
3482.985551	371681.556332	50.755969
3482.326292	371433.698675	50.760973
3481.777141	371180.327123	50.765978
3481.418730	370927.814321	50.770983
3480.699341	370680.343406	50.775988
3480.095564	370430.359620	50.780993
3479.376018	370172.429770	50.785997
3478.959015	369919.233416	50.791002
3478.218276	369643.647858	50.796007
3477.575626	369393.358936	50.801012
3477.196620	369128.601712	50.806017
3476.672928	368889.001852	50.811021
3475.876706	368601.104849	50.816026
3475.012808	368349.598298	50.821031
3474.622618	368093.613982	50.826036
3473.972846	367818.867587	50.831041
3472.851658	367560.273459	50.836045
3472.851758	367284.428769	50.841050
3472.082913	367014.326725	50.846055
3471.233199	366756.499174	50.851060
3470.584809	366483.474426	50.856065
3469.858336	366224.174096	50.861069
3469.163154	365955.275296	50.866074
3468.676073	365693.033560	50.871079
3468.159164	365421.177436	50.876084
3467.560886	365148.492916	50.881089
3466.567735	364878.718887	50.886093
3466.159117	364606.611798	50.891098
3465.348266	364339.121160	50.896103
3464.374888	364076.590821	50.901108
3464.316094	363801.166822	50.906113
3463.485001	363536.015606	50.911117
3462.630558	363255.854284	50.916122
3461.867450	362990.409323	50.921127
3461.351465	362722.252075	50.926132
3460.680770	362449.105093	50.931137
3459.327084	362188.303619	50.936141
3459.285586	361908.107502	50.941146
3458.481786	361643.246619	50.946151
3457.728234	361374.712153	50.951156
3457.382785	361112.167731	50.956161
3456.684733	360838.303320	50.961165
3455.783077	360567.395826	50.966170
3455.116765	360300.266519	50.971175
3454.527363	360041.978878	50.976180
3454.074542	359762.598633	50.981185
3453.207079	359499.135549	50.986189
3452.477959	359215.062785	50.991194
3451.659877	358954.286303	50.996199
3450.800874	358684.964720	51.001204
3450.348909	358405.576588	51.006209
3449.642016	358150.223951	51.011213
3448.981661	357890.511137	51.016218
3448.247444	357621.138584	51.021223
3447.604896	357361.547432	51.026228
3447.276488	357075.770375	51.031233
3446.197225	356829.045758	51.036237
3445.492252	356555.082222	51.041242
3445.030638	356286.575536	51.046247
3443.791449	356017.630507	51.051252
3443.586872	355751.497944	51.056257
3443.098190	355486.223268	51.061261
3441.897603	355218.667598	51.066266
3441.358946	354957.317194	51.071271
3440.821755	354701.309522	51.076276
3440.059842	354436.199880	51.081281
3439.163488	354176.378135	51.086285
3438.680198	353894.781460	51.091290
3438.195993	353636.622419	51.096295
3437.153766	353383.054923	51.101300
3436.574557	353120.200181	51.106305
3435.847572	352862.686523	51.111309
3435.391750	352598.079084	51.116314
3434.584453	352337.547023	51.121319
3433.848830	352076.137048	51.126324
3433.471742	351802.478369	51.131329
3432.344346	351552.682262	51.136333
3431.766740	351284.295456	51.141338
3431.401320	351025.723212	51.146343
3430.470803	350769.911430	51.151348
3430.112610	350511.106538	51.156353
3429.182438	350242.821237	51.161357
3428.543805	349969.932753	51.166362
3427.861477	349721.686750	51.171367
3426.968080	349463.216059	51.176372
3426.804126	349191.037666	51.181377
3425.650757	348937.874117	51.186381
3425.275479	348674.125682	51.191386
3424.950998	348414.033055	51.196391
3423.975233	348158.216347	51.201396
3423.406987	347892.102259	51.206401
3422.762012	347632.031251	51.211405
3421.909648	347359.952845	51.216410
3421.096491	347106.574568	51.221415
3420.226803	346841.241356	51.226420
3420.122404	346564.510326	51.231425
3418.940885	346310.652276	51.236429
3418.373361	346058.605002	51.241434
3418.197767	345796.542491	51.246439
3417.088839	345542.313262	51.251444
3416.584465	345285.289279	51.256449
3415.740234	345014.191241	51.261453
3415.142402	344755.194351	51.266458
3414.314903	344490.251028	51.271463
3413.443268	344232.364205	51.276468
3413.193148	343966.105470	51.281473
3411.989030	343732.119374	51.286477
3411.832934	343457.545506	51.291482
3411.038625	343192.107562	51.296487
3410.287294	342937.759755	51.301492
3409.744716	342676.963353	51.306497
3408.740884	342429.882418	51.311501
3408.222134	342170.149178	51.316506
3407.394005	341911.914684	51.321511
3406.587746	341651.410169	51.326516
3406.396957	341393.530920	51.331521
3405.457322	341148.725655	51.336525
3404.743867	340896.247110	51.341530
3404.328191	340632.138303	51.346535
3403.480448	340375.962429	51.351540
3402.980981	340126.730707	51.356545
3401.955713	339876.333827	51.361549
3401.227324	339606.848151	51.366554
3400.642195	339365.263708	51.371559
3399.884937	339120.014471	51.376564
3399.454012	338853.227833	51.381569
3398.804474	338606.610445	51.386573
3398.096454	338357.303011	51.391578
3397.817790	338098.482446	51.396583
3397.095687	337845.967797	51.401588
3396.344759	337596.206039	51.406593
3395.180803	337341.951919	51.411597
3394.459306	337072.174647	51.416602
3394.296051	336811.039687	51.421607
3393.235282	336574.891558	51.426612
3393.016128	336305.897294	51.431617
3392.263815	336066.465567	51.436621
3391.439850	335799.601496	51.441626
3390.889117	335551.327893	51.446631
3390.219735	335289.528834	51.451636
3389.745505	335035.538815	51.456641
3388.976230	334779.659742	51.461645
3388.285093	334526.287675	51.466650
3387.479333	334259.592954	51.471655
3386.717823	334010.863450	51.476660
3386.261818	333754.472833	51.481665
3385.632175	333503.658590	51.486669
3384.746562	333246.544868	51.491674
3384.303171	332989.945822	51.496679
3383.574432	332739.450052	51.501684
3382.669437	332470.803995	51.506689
3381.611125	332215.368673	51.511693
3381.119172	331964.374511	51.516698
3380.785175	331729.673498	51.521703
3379.816815	331490.336724	51.526708
3379.079987	331220.666562	51.531713
3378.457177	330981.604452	51.536717
3377.683293	330737.244531	51.541722
3377.178561	330482.352106	51.546727
3376.563321	330234.986739	51.551732
3376.205665	329983.277210	51.556737
3375.437532	329730.231490	51.561741
3374.693562	329476.468240	51.566746
3374.052057	329227.372488	51.571751
3373.178983	328982.258779	51.576756
3372.660114	328725.529587	51.581761
3371.839825	328482.926448	51.586765
3371.362758	328220.791504	51.591770
3370.687869	327973.835611	51.596775
3369.562238	327720.483382	51.601780
3369.244862	327472.629194	51.606785
3368.423379	327236.285558	51.611789
3368.142936	326970.881915	51.616794
3367.445670	326737.088636	51.621799
3366.121728	326482.719948	51.626804
3365.780412	326226.463747	51.631809
3365.252676	325981.973530	51.636813
3364.317568	325737.165094	51.641818
3363.554642	325490.215457	51.646823
3362.806248	325250.213571	51.651828
3362.607627	324997.470002	51.656833
3362.044286	324747.151208	51.661837
3361.405612	324496.410741	51.666842
3360.525149	324259.507666	51.671847
3359.794645	324003.764421	51.676852
3359.111598	323754.811046	51.681857
3358.568146	323512.785802	51.686861
3357.896964	323265.382263	51.691866
3357.318651	323007.575056	51.696871
3356.609962	322749.660392	51.701876
3356.046263	322515.044855	51.706881
3355.485769	322265.507648	51.711885
3354.861813	322010.785574	51.716890
3354.231881	321746.871997	51.721895
3353.258286	321498.212733	51.726900
3352.579749	321250.677365	51.731905
3351.985018	320997.653725	51.736909
3351.668700	320748.302812	51.741914
3350.729205	320487.668182	51.746919
3349.952264	320238.821580	51.751924
3349.188494	319989.539363	51.756929
3348.556927	319736.339821	51.761933
3347.924413	319488.359541	51.766938
3347.450771	319238.851190	51.771943
3346.333367	318996.064259	51.776948
3346.131145	318737.523365	51.781953
3345.226579	318500.201437	51.786957
3344.366639	318240.591932	51.791962
3343.575168	317986.139856	51.796967
3342.998316	317748.280451	51.801972
3342.571688	317486.741602	51.806977
3341.741584	317260.634031	51.811981
3341.136304	317010.478683	51.816986
3340.501676	316754.445354	51.821991
3340.048930	316523.056471	51.826996
3339.683709	316262.905160	51.832001
3338.518682	316018.132223	51.837005
3337.761684	315758.092504	51.842010
3336.978972	315517.510289	51.847015
3336.569777	315271.139141	51.852020
3335.891786	315027.356279	51.857025
3335.250441	314774.629306	51.862029
3334.434533	314525.214152	51.867034
3334.048183	314283.267750	51.872039
3333.449455	314030.812357	51.877044
3332.753540	313782.751529	51.882049
3332.145261	313522.122537	51.887053
3331.386635	313273.433858	51.892058
3330.559538	313031.579813	51.897063
3329.888776	312773.759963	51.902068
3329.275394	312524.664654	51.907073
3328.615524	312286.856801	51.912077
3327.880246	312030.522358	51.917082
3327.207047	311783.344684	51.922087
3326.475641	311539.409658	51.927092
3325.784245	311289.610956	51.932097
3325.293902	311052.996001	51.937101
3324.752561	310791.076840	51.942106
3324.170526	310541.106442	51.947111
3323.313490	310291.841089	51.952116
3322.901700	310040.060176	51.957121
3322.049629	309788.322902	51.962125
3321.178023	309543.540094	51.967130
3320.706808	309283.643710	51.972135
3319.837121	309041.635262	51.977140
3319.272302	308784.502837	51.982145
3318.497772	308536.774188	51.987149
3317.747674	308301.748269	51.992154
3317.304830	308056.156207	51.997159
3316.406874	307806.051916	52.002164
3315.611673	307563.876041	52.007169
3315.005588	307312.043915	52.012173
3314.227055	307077.351289	52.017178
3313.704830	306836.276819	52.022183
3313.091727	306595.725590	52.027188
3312.261611	306345.454970	52.032193
3311.556917	306099.595046	52.037197
3310.922946	305856.702960	52.042202
3310.651867	305618.336855	52.047207
3309.457562	305378.130039	52.052212
3309.020040	305128.941037	52.057217
3308.544882	304889.587325	52.062221
3307.633664	304639.555609	52.067226
3307.230822	304396.980933	52.072231
3306.282929	304158.490199	52.077236
3305.621908	303899.377225	52.082241
3305.315822	303655.563632	52.087245
3304.222346	303422.493505	52.092250
3303.970051	303170.801603	52.097255
3303.025803	302931.238723	52.102260
3302.756948	302692.689145	52.107265
3302.133747	302433.567633	52.112269
3301.145314	302199.944210	52.117274
3300.759409	301941.191796	52.122279
3300.202159	301687.864913	52.127284
3299.529633	301444.360399	52.132289
3298.770796	301205.172984	52.137293
3297.884031	300938.985576	52.142298
3297.370219	300690.336066	52.147303
3296.255880	300444.327818	52.152308
3295.816267	300199.664073	52.157313
3295.356710	299954.391927	52.162317
3294.493840	299716.848670	52.167322
3293.940945	299463.899665	52.172327
3293.391677	299229.998794	52.177332
3292.831401	298974.401707	52.182337
3291.892021	298733.278399	52.187341
3291.050487	298483.582447	52.192346
3290.459257	298224.576632	52.197351
3289.759805	297989.882952	52.202356
3289.183494	297742.257780	52.207361
3288.822768	297497.654210	52.212365
3287.980310	297256.946565	52.217370
3287.197282	297006.730028	52.222375
3286.330824	296758.996664	52.227380
3286.089138	296503.906049	52.232385
3285.240570	296274.378188	52.237389
3284.129789	296038.270091	52.242394
3283.783502	295776.853780	52.247399
3282.850125	295547.516779	52.252404
3282.629397	295296.547007	52.257409
3282.078267	295056.758381	52.262413
3281.291398	294806.768932	52.267418
3280.748426	294557.148090	52.272423
3279.763890	294321.069023	52.277428
3279.316305	294070.362910	52.282433
3278.407177	293823.218556	52.287437
3277.922138	293577.687697	52.292442
3277.517241	293332.143899	52.297447
3276.412843	293095.293026	52.302452
3275.625117	292839.749624	52.307457
3275.273651	292591.267844	52.312461
3274.457167	292354.778177	52.317466
3273.745391	292107.473473	52.322471
3273.221584	291874.171433	52.327476
3272.687672	291619.070501	52.332481
3271.837171	291379.427318	52.337485
3271.152430	291137.109059	52.342490
3270.712363	290884.513866	52.347495
3269.604180	290631.489304	52.352500
3269.252330	290388.659297	52.357505
3268.592466	290148.933935	52.362509
3267.683200	289904.026929	52.367514
3267.352365	289661.447656	52.372519
3266.540808	289421.363671	52.377524
3265.775324	289173.122498	52.382529
3265.445945	288930.236790	52.387533
3264.736507	288693.956257	52.392538
3263.979487	288425.364317	52.397543
3263.061186	288196.094660	52.402548
3262.519271	287952.579666	52.407553
3262.188870	287706.229561	52.412557
3260.996585	287456.857593	52.417562
3260.464503	287216.702293	52.422567
3259.719736	286983.686050	52.427572
3259.421680	286731.115957	52.432577
3258.488854	286485.547947	52.437581
3257.754763	286233.861477	52.442586
3257.734642	286003.607887	52.447591
3256.663596	285750.497265	52.452596
3255.652639	285510.136499	52.457601
3255.441665	285267.789872	52.462605
3254.653055	285021.383183	52.467610
3254.119635	284766.327755	52.472615
3253.237046	284522.074983	52.477620
3252.737076	284267.294138	52.482625
3252.202070	284029.123956	52.487629
3251.063762	283790.590671	52.492634
3250.621458	283537.761380	52.497639
3249.852311	283304.059369	52.502644
3249.278566	283047.252130	52.507649
3248.918935	282812.568271	52.512653
3248.163183	282558.591113	52.517658
3247.555795	282301.203098	52.522663
3246.812477	282059.219318	52.527668
3246.109051	281812.772188	52.532673
3245.502348	281568.831028	52.537677
3244.505825	281326.887043	52.542682
3243.814034	281081.074526	52.547687
3243.525026	280834.383225	52.552692
3242.745198	280587.387470	52.557697
3242.025068	280348.684876	52.562701
3241.423178	280098.120737	52.567706
3241.271871	279845.931681	52.572711
3239.953483	279606.865115	52.577716
3239.146148	279354.423166	52.582721
3238.733951	279104.490956	52.587725
3237.766722	278869.825646	52.592730
3237.440640	278627.774912	52.597735
3236.707380	278383.241715	52.602740
3236.136667	278126.992782	52.607745
3235.332179	277889.780206	52.612749
3234.731072	277650.039524	52.617754
3234.226664	277398.364314	52.622759
3233.294787	277156.103604	52.627764
3232.778777	276915.101440	52.632769
3232.202120	276657.834553	52.637773
3231.445254	276409.510098	52.642778
3230.939300	276168.378963	52.647783
3230.326754	275924.004732	52.652788
3229.511042	275676.198939	52.657793
3228.719667	275427.370562	52.662797
3227.932027	275185.469002	52.667802
3227.716517	274923.713467	52.672807
3226.664225	274686.667325	52.677812
3225.856154	274439.904574	52.682817
3225.678701	274198.466841	52.687821
3224.736760	273953.966531	52.692826
3224.192757	273700.744042	52.697831
3223.306513	273458.017765	52.702836
3222.771883	273210.727992	52.707841
3222.099923	272970.310976	52.712845
3221.377327	272720.478716	52.717850
3221.055843	272470.302892	52.722855
3219.975538	272238.075018	52.727860
3219.468016	271991.239614	52.732865
3218.986956	271738.898918	52.737869
3218.031527	271490.402648	52.742874
3217.231648	271247.051906	52.747879
3216.729257	271001.896849	52.752884
3216.112664	270751.844546	52.757889
3215.424265	270519.427749	52.762893
3214.780603	270269.532691	52.767898
3214.378353	270009.106588	52.772903
3213.458031	269774.128953	52.777908
3212.646944	269533.352819	52.782913
3212.218642	269282.863743	52.787917
3211.517043	269034.022505	52.792922
3210.775314	268790.663390	52.797927
3210.075731	268540.039264	52.802932
3209.254789	268297.889898	52.807937
3208.649827	268066.122966	52.812941
3207.849798	267825.625938	52.817946
3207.492225	267578.029802	52.822951
3206.875637	267344.405858	52.827956
3206.081201	267091.683579	52.832961
3205.299485	266853.017839	52.837965
3204.573160	266607.135979	52.842970
3204.080585	266365.444979	52.847975
3203.260275	266126.811203	52.852980
3202.741296	265877.356886	52.857985
3202.110396	265637.802039	52.862989
3201.254594	265399.530853	52.867994
3200.967632	265141.177400	52.872999
3200.364770	264900.650782	52.878004
3199.459907	264653.754161	52.883009
3198.912763	264410.544904	52.888013
3198.197812	264165.732412	52.893018
3197.670587	263909.327938	52.898023
3197.111057	263681.758469	52.903028
3196.337305	263419.815891	52.908033
3195.633074	263181.420325	52.913037
3194.663452	262932.752434	52.918042
3194.110924	262675.741693	52.923047
3193.278754	262447.655935	52.928052
3192.776067	262195.603935	52.933057
3192.378071	261944.605230	52.938061
3191.495755	261722.742100	52.943066
3190.862133	261467.935450	52.948071
3190.250928	261218.142624	52.953076
3189.745403	260977.960094	52.958081
3189.237578	260727.438256	52.963085
3188.027524	260493.021451	52.968090
3187.697074	260228.974151	52.973095
3186.774828	259999.784046	52.978100
3185.985095	259750.861261	52.983105
3185.852460	259499.517203	52.988109
3184.999581	259255.138124	52.993114
3184.450575	259002.306928	52.998119
3183.557224	258766.466358	53.003124
3182.764687	258510.516239	53.008129
3182.222129	258268.050054	53.013133
3181.068102	258036.861064	53.018138
3180.964308	257788.977800	53.023143
3180.172435	257545.252988	53.028148
3179.264826	257302.157970	53.033153
3178.705418	257066.393643	53.038157
3178.311669	256809.058045	53.043162
3177.846211	256571.751354	53.048167
3176.869854	256334.169225	53.053172
3176.366202	256074.916397	53.058177
3175.508566	255842.893356	53.063181
3175.000489	255587.843922	53.068186
3174.372409	255347.431908	53.073191
3173.655321	255092.925516	53.078196
3172.824904	254849.235402	53.083201
3172.482064	254609.084758	53.088205
3171.508072	254374.280475	53.093210
3170.829536	254119.845660	53.098215
3169.850708	253883.591135	53.103220
3169.607464	253633.341076	53.108225
3169.219049	253383.700063	53.113229
3168.162095	253151.457131	53.118234
3168.063624	252904.979716	53.123239
3167.366282	252657.706065	53.128244
3166.384114	252410.223162	53.133249
3166.083172	252159.424020	53.138253
3165.309834	251901.620271	53.143258
3164.546422	251652.041044	53.148263
3164.085970	251401.599318	53.153268
3163.210757	251150.485066	53.158273
3162.774969	250890.337469	53.163277
3161.562277	250649.056503	53.168282
3161.083502	250394.977506	53.173287
3160.537923	250152.878663	53.178292
3159.531459	249903.340555	53.183297
3159.219381	249655.628402	53.188301
3158.230373	249421.138862	53.193306
3158.018339	249159.481642	53.198311
3157.061118	248917.067856	53.203316
3156.436730	248675.009249	53.208321
3156.241570	248419.844488	53.213325
3155.209609	248172.554244	53.218330
3154.824931	247919.865067	53.223335
3153.873647	247681.068519	53.228340
3153.236785	247423.377852	53.233345
3152.432568	247167.267544	53.238349
3151.724118	246929.452451	53.243354
3151.171997	246686.036019	53.248359
3150.251191	246439.444205	53.253364
3149.767441	246195.508494	53.258369
3149.572043	245952.673539	53.263373
3148.348463	245703.609854	53.268378
3147.978274	245447.866946	53.273383
3147.411858	245200.380923	53.278388
3146.498258	244949.206879	53.283393
3146.036117	244706.492776	53.288397
3145.067314	244462.942544	53.293402
3144.650106	244204.943060	53.298407
3144.069413	243945.187393	53.303412
3143.439020	243696.644798	53.308417
3143.061836	243452.162507	53.313421
3141.848384	243204.833607	53.318426
3141.345238	242942.597610	53.323431
3140.914670	242696.699198	53.328436
3140.354658	242438.318478	53.333441
3139.089643	242190.617790	53.338445
3138.336434	241932.166855	53.343450
3138.129957	241688.577777	53.348455
3136.851371	241449.538781	53.353460
3136.644615	241196.325087	53.358465
3136.147657	240942.979606	53.363469
3134.976280	240694.223158	53.368474
3134.810889	240461.910907	53.373479
3133.973156	240207.169476	53.378484
3133.390188	239956.615385	53.383489
3132.970683	239699.669893	53.388493
3132.312909	239458.168579	53.393498
3131.566350	239194.120530	53.398503
3130.976777	238943.544270	53.403508
3129.999252	238692.062333	53.408513
3129.559876	238432.576490	53.413517
3128.630292	238182.615978	53.418522
3127.910564	237922.564579	53.423527
3127.269443	237673.476295	53.428532
3126.677321	237417.378288	53.433537
3125.969512	237169.447604	53.438541
3125.227618	236921.650213	53.443546
3124.390990	236664.726957	53.448551
3123.638994	236433.509141	53.453556
3123.223982	236193.071649	53.458561
3122.695499	235929.175375	53.463565
3121.836819	235683.080011	53.468570
3121.414878	235444.988001	53.473575
3120.475403	235190.019920	53.478580
3120.128250	234943.539845	53.483585
3119.461215	234702.381868	53.488589
3118.566712	234456.575269	53.493594
3118.034117	234193.295312	53.498599
3117.369319	233951.909646	53.503604
3116.326077	233700.934038	53.508609
3116.074258	233453.271312	53.513613
3115.376914	233209.702841	53.518618
3114.594942	232957.414683	53.523623
3114.241001	232704.295576	53.528628
3113.413078	232455.682637	53.533633
3112.670542	232211.512774	53.538637
3111.852319	231964.554661	53.543642
3111.519867	231717.214778	53.548647
3110.907332	231467.068104	53.553652
3109.505489	231222.419549	53.558657
3109.304630	230979.873176	53.563661
3108.603978	230725.057440	53.568666
3107.788178	230479.503348	53.573671
3107.020920	230240.816965	53.578676
3106.387719	229997.526866	53.583681
3106.182959	229733.265497	53.588685
3105.274498	229512.553971	53.593690
3104.789324	229252.921525	53.598695
3104.137815	229016.664436	53.603700
3103.494691	228764.569601	53.608705
3102.978278	228510.825913	53.613709
3102.334472	228265.428995	53.618714
3101.900648	228009.051194	53.623719
3101.122958	227756.089461	53.628724
3100.222782	227495.254916	53.633729
3099.743051	227243.749763	53.638733
3098.912043	226992.453722	53.643738
3098.454031	226733.804856	53.648743
3097.872575	226480.039347	53.653748
3096.785734	226225.068832	53.658753
3096.523831	225978.968893	53.663757
3095.650387	225727.314227	53.668762
3095.010405	225470.544018	53.673767
3094.417516	225217.802645	53.678772
3093.598924	224965.976166	53.683777
3093.026304	224710.801714	53.688781
3092.113914	224464.185551	53.693786
3091.636908	224202.963526	53.698791
3090.937849	223967.912222	53.703796
3090.172117	223720.829614	53.708801
3089.743840	223452.371740	53.713805
3089.061002	223204.068302	53.718810
3088.166282	222951.458312	53.723815
3087.491113	222712.906299	53.728820
3086.478885	222452.449522	53.733825
3086.228389	222206.079445	53.738829
3085.501369	221973.253590	53.743834
3084.936959	221705.714433	53.748839
3084.015842	221456.728784	53.753844
3083.320591	221211.590728	53.758849
3082.913179	220976.260565	53.763853
3082.193336	220726.316238	53.768858
3081.849122	220475.002171	53.773863
3081.128368	220231.475292	53.778868
3080.384806	219968.502391	53.783873
3080.273330	219708.103548	53.788877
3079.355581	219456.590970	53.793882
3078.672928	219203.094488	53.798887
3077.839159	218938.663004	53.803892
3077.085377	218681.793658	53.808897
3076.285093	218418.771725	53.813901
3075.756335	218176.430642	53.818906
3075.406960	217916.648749	53.823911
3074.425346	217672.789944	53.828916
3074.004993	217406.262103	53.833921
3073.396520	217157.865463	53.838925
3072.411224	216900.148228	53.843930
3071.936330	216640.912819	53.848935
3071.172628	216387.210165	53.853940
3070.320116	216129.920294	53.858945
3069.881657	215885.205363	53.863949
3069.097686	215630.210405	53.868954
3068.602387	215371.148506	53.873959
3067.938677	215112.928877	53.878964
3067.087884	214867.519178	53.883969
3067.119349	214605.983907	53.888973
3066.018218	214356.198964	53.893978
3065.063384	214090.112350	53.898983
3064.530009	213845.445331	53.903988
3063.846109	213593.369792	53.908993
3063.337500	213331.912307	53.913997
3062.331166	213090.517720	53.919002
3061.936943	212820.910940	53.924007
3061.316505	212570.038472	53.929012
3060.194661	212323.472013	53.934017
3059.804257	212068.186684	53.939021
3059.282259	211825.167367	53.944026
3058.375971	211564.110906	53.949031
3057.951019	211312.206929	53.954036
3057.144286	211062.960828	53.959041
3056.641474	210797.172612	53.964045
3055.532493	210556.936598	53.969050
3055.497128	210296.842104	53.974055
3054.604489	210041.529909	53.979060
3053.796774	209790.672644	53.984065
3053.232678	209537.397819	53.989069
3052.489980	209285.997765	53.994074
3051.610591	209035.765830	53.999079
3050.962207	208777.734761	54.004084
3050.182255	208544.505372	54.009089
3050.141651	208282.943870	54.014093
3049.256623	208035.007824	54.019098
3048.815090	207768.739367	54.024103
3047.861979	207524.774296	54.029108
3047.162499	207270.741290	54.034113
3046.893683	207006.497917	54.039117
3046.127979	206762.404491	54.044122
3045.459507	206493.428671	54.049127
3044.380295	206238.403882	54.054132
3043.815272	205988.503994	54.059137
3043.398808	205734.521889	54.064141
3042.382411	205488.577187	54.069146
3042.123339	205225.294776	54.074151
3041.309017	204969.533659	54.079156
3040.335342	204726.067083	54.084161
3040.217177	204457.738973	54.089165
3039.417723	204206.471276	54.094170
3038.738757	203951.584112	54.099175
3038.450417	203713.205646	54.104180
3037.633861	203445.807322	54.109185
3036.973333	203177.443846	54.114189
3036.033785	202933.814114	54.119194
3035.479466	202674.051688	54.124199
3034.973129	202407.512745	54.129204
3033.803743	202164.978993	54.134209
3033.463317	201893.796805	54.139213
3032.691287	201645.005025	54.144218
3032.096593	201392.457705	54.149223
3031.438676	201139.030769	54.154228
3030.999341	200879.614894	54.159233
3030.453300	200616.145020	54.164237
3029.209985	200370.818595	54.169242
3028.719165	200109.073091	54.174247
3028.237906	199838.496046	54.179252
3027.352719	199594.859819	54.184257
3026.935303	199333.653653	54.189261
3026.135642	199072.191146	54.194266
3025.166361	198818.519004	54.199271
3024.817459	198574.675303	54.204276
3023.819000	198326.939945	54.209281
3023.280962	198062.081655	54.214285
3022.443933	197804.550571	54.219290
3021.912424	197555.548814	54.224295
3021.654526	197313.198075	54.229300
3020.414938	197052.336961	54.234305
3019.735966	196793.895139	54.239309
3018.917023	196554.830602	54.244314
3018.359273	196303.561345	54.249319
3017.799188	196053.324354	54.254324
3017.304299	195808.511514	54.259329
3016.998953	195569.026719	54.264333
3016.149355	195300.490999	54.269338
3015.592061	195047.929995	54.274343
3014.969536	194782.478469	54.279348
3014.044678	194535.729452	54.284353
3013.515022	194278.345570	54.289357
3012.575799	194020.111733	54.294362
3012.015197	193774.479396	54.299367
3011.251550	193517.632704	54.304372
3010.704005	193269.176149	54.309377
3010.562506	193008.696453	54.314381
3009.507344	192767.371611	54.319386
3008.890662	192506.308176	54.324391
3008.271824	192236.594615	54.329396
3007.266341	192001.627344	54.334401
3006.803496	191740.988962	54.339405
3006.186420	191488.710041	54.344410
3005.527896	191231.451558	54.349415
3004.792845	190976.547591	54.354420
3004.104491	190724.958266	54.359425
3003.828369	190468.890173	54.364429
3003.039130	190213.260917	54.369434
3002.376615	189959.572270	54.374439
3001.972633	189691.378397	54.379444
3001.301788	189441.536078	54.384449
3000.346477	189170.824306	54.389453
2999.780930	188910.828292	54.394458
2999.222723	188650.387274	54.399463
2998.127761	188396.737326	54.404468
2997.654394	188143.957245	54.409473
2996.888837	187879.507685	54.414477
2996.404747	187632.940493	54.419482
2995.857685	187369.451578	54.424487
2995.439126	187114.607469	54.429492
2994.530587	186847.794725	54.434497
2994.006245	186586.927402	54.439501
2993.393543	186326.266381	54.444506
2992.322052	186062.880718	54.449511
2991.736730	185801.544120	54.454516
2991.043739	185548.965750	54.459521
2990.584573	185289.787513	54.464525
2990.197900	185028.716529	54.469530
2989.285355	184758.634593	54.474535
2988.764010	184505.195304	54.479540
2987.974451	184242.704299	54.484545
2987.194019	183983.966111	54.489549
2986.617958	183719.943306	54.494554
2986.012068	183452.174129	54.499559
2985.254931	183195.815668	54.504564
2984.437979	182932.827932	54.509569
2984.339111	182663.711204	54.514573
2983.504809	182413.844354	54.519578
2982.767008	182147.045343	54.524583
2982.037255	181883.121517	54.529588
2981.278115	181619.178506	54.534593
2980.734317	181352.137421	54.539597
2979.826624	181094.288717	54.544602
2979.101383	180839.249267	54.549607
2978.588758	180582.727583	54.554612
2977.818045	180313.769980	54.559617
2977.181022	180053.099009	54.564621
2976.055271	179798.765169	54.569626
2975.743718	179538.809014	54.574631
2975.244535	179277.637630	54.579636
2974.583215	179016.786081	54.584641
2973.870766	178770.660735	54.589645
2973.229205	178513.141697	54.594650
2972.530192	178251.067083	54.599655
2971.963937	177986.759937	54.604660
2970.979288	177728.295229	54.609665
2970.463781	177464.288628	54.614669
2969.978219	177205.112206	54.619674
2969.207775	176955.928749	54.624679
2968.496878	176688.689257	54.629684
2967.506962	176433.235139	54.634689
2967.158342	176174.908399	54.639693
2966.263496	175911.582307	54.644698
2965.805361	175659.826267	54.649703
2965.435869	175403.644432	54.654708
2964.618244	175149.455642	54.659713
2963.840242	174886.690019	54.664717
2963.267686	174631.384629	54.669722
2962.370854	174367.356659	54.674727
2962.116769	174110.134584	54.679732
2961.082131	173857.285551	54.684737
2960.439618	173587.537507	54.689741
2959.619380	173331.096847	54.694746
2959.208865	173088.175536	54.699751
2959.039455	172833.173896	54.704756
2957.937394	172571.479493	54.709761
2957.400673	172308.361980	54.714765
2956.681351	172043.354804	54.719770
2955.830115	171783.737019	54.724775
2955.325939	171522.145701	54.729780
2954.565101	171268.621304	54.734785
2954.193117	171003.744216	54.739789
2953.547305	170751.616570	54.744794
2952.953729	170487.477522	54.749799
2952.123672	170216.523348	54.754804
2951.341953	169962.680156	54.759809
2951.209141	169695.548724	54.764813
2950.301326	169429.508313	54.769818
2949.481197	169165.503220	54.774823
2948.859496	168898.848958	54.779828
2948.174160	168646.436181	54.784833
2947.325551	168381.067670	54.789837
2946.678590	168117.576509	54.794842
2945.898217	167860.504475	54.799847
2945.527797	167595.828722	54.804852
2944.484584	167346.189781	54.809857
2943.754443	167080.786224	54.814861
2943.475925	166826.808026	54.819866
2942.683248	166576.498761	54.824871
2941.944763	166306.193800	54.829876
2941.410333	166062.332015	54.834881
2940.850144	165791.010767	54.839885
2940.163251	165537.907090	54.844890
2939.505385	165274.704711	54.849895
2939.045356	165009.095169	54.854900
2937.847568	164755.391144	54.859905
2937.483572	164495.466424	54.864909
2936.916490	164151.823403	54.869914
2936.044078	163922.040995	54.874919
2935.711030	163632.174433	54.879924
2934.868255	163382.594129	54.884929
2934.153200	163117.026019	54.889933
2933.440864	162863.029461	54.894938
2932.721257	162607.510135	54.899943
2932.441336	162320.595377	54.904948
2931.329802	162091.879598	54.909953
2930.619519	161800.930503	54.914957
2930.399062	161570.080881	54.919962
2929.646347	161287.610122	54.924967
2929.048670	161037.447913	54.929972
2928.420382	160768.438075	54.934977
2927.579091	160488.479565	54.939981
2927.089311	160251.108299	54.944986
2926.120047	159971.250437	54.949991
2925.469161	159727.729552	54.954996
2924.504352	159445.535946	54.960001
2924.181365	159218.277592	54.965005
2923.622077	158937.600289	54.970010
2922.791863	158704.895476	54.975015
2922.545504	158399.802476	54.980020
2921.717628	158181.758564	54.985025
2921.228486	157892.039920	54.990029
2920.379785	157637.199985	54.995034
2920.033285	157363.430016	55.000039
2919.244487	157125.720616	55.005044
2918.109835	156842.558126	55.010049
2917.676760	156567.015810	55.015053
2917.104134	156334.832836	55.020058
2916.400387	156037.282425	55.025063
2915.702329	155810.144070	55.030068
2914.820821	155544.875865	55.035073
2914.038741	155265.064687	55.040077
2913.655262	154982.141963	55.045082
2912.583472	154765.633019	55.050087
2912.499403	154484.383102	55.055092
2912.054644	154207.145822	55.060097
2910.676616	153981.792623	55.065101
2910.219935	153717.615558	55.070106
2909.657147	153427.323857	55.075111
2909.105739	153179.372406	55.080116
2908.309375	152927.546710	55.085121
2907.942456	152632.744076	55.090125
2907.702881	152354.460191	55.095130
2906.752483	152120.307139	55.100135
2906.016794	151880.681763	55.105140
2905.030305	151587.727892	55.110145
2904.545889	151297.264566	55.115149
2904.209515	151066.580619	55.120154
2902.739478	150778.235314	55.125159
2902.935637	150496.352165	55.130164
2901.704691	150269.691986	55.135169
2901.323961	149978.931681	55.140173
2900.742608	149727.515975	55.145178
2899.231911	149475.766436	55.150183
2899.313208	149191.078666	55.155188
2898.544310	148947.298857	55.160193
2897.938101	148644.525353	55.165197
2896.957442	148395.534462	55.170202
2896.371900	148154.896169	55.175207
2896.240846	147869.643750	55.180212
2895.093799	147618.194380	55.185217
2895.027612	147351.922965	55.190221
2894.105219	147066.739529	55.195226
2892.923034	146825.926208	55.200231
2892.718308	146546.339839	55.205236
2891.870262	146292.134128	55.210241
2891.155241	146015.721340	55.215245
2890.239650	145785.497614	55.220250
2889.821366	145492.153734	55.225255
2889.181909	145248.623371	55.230260
2888.410539	144974.223816	55.235265
2887.793421	144697.489507	55.240269
2887.110412	144458.521480	55.245274
2886.230743	144176.432797	55.250279
2885.720580	143932.040911	55.255284
2885.268890	143672.418734	55.260289
2884.817966	143402.861850	55.265293
2884.005744	143118.307041	55.270298
2883.191832	142888.990929	55.275303
2882.476275	142594.679673	55.280308
2881.613615	142372.783066	55.285313
2881.213822	142073.433202	55.290317
2880.562732	141843.857744	55.295322
2879.978648	141556.651186	55.300327
2879.210930	141318.839207	55.305332
2878.081011	141041.723600	55.310337
2877.987144	140767.915143	55.315341
2877.457602	140494.648276	55.320346
2876.827825	140227.803360	55.325351
2875.948917	140009.280937	55.330356
2874.665231	139736.991666	55.335361
2874.365517	139455.337773	55.340365
2873.806345	139173.079666	55.345370
2872.998839	138976.190281	55.350375
2872.696455	138670.379317	55.355380
2871.856807	138412.490001	55.360385
2870.846465	138166.851847	55.365389
2870.428602	137874.902768	55.370394
2869.744029	137667.330816	55.375399
2869.194711	137409.683783	55.380404
2868.231528	137123.977413	55.385409
2867.613760	136886.050057	55.390413
2866.995963	136614.319300	55.395418
2866.247794	136363.966936	55.400423
2865.843851	136106.130501	55.405428
2865.308391	135825.641159	55.410433
2864.614262	135598.750466	55.415437
2863.982429	135333.271335	55.420442
2862.891230	135062.316041	55.425447
2863.134975	134772.897395	55.430452
2862.504364	134532.539638	55.435457
2861.747902	134271.612308	55.440461
2861.014341	133979.129864	55.445466
2859.844273	133766.289387	55.450471
2859.152054	133482.024148	55.455476
2858.694551	133188.794719	55.460481
2857.915255	132953.732591	55.465485
2857.215490	132684.058838	55.470490
2856.523509	132429.552770	55.475495
2856.045810	132142.497873	55.480500
2855.118563	131927.282833	55.485505
2854.511155	131621.759778	55.490509
2854.174242	131393.461400	55.495514
2853.028955	131108.085060	55.500519
2852.637799	130859.807373	55.505524
2852.254520	130607.745643	55.510529
2851.413033	130314.670371	55.515533
2850.949870	130094.645635	55.520538
2850.230071	129798.990886	55.525543
2849.502028	129557.204814	55.530548
2848.761642	129282.731131	55.535553
2848.457447	129000.507225	55.540557
2847.662365	128778.830898	55.545562
2846.657663	128476.123103	55.550567
2846.383843	128248.805725	55.555572
2845.272514	127966.644017	55.560577
2844.575228	127692.103124	55.565581
2844.336270	127407.586502	55.570586
2843.526618	127152.880588	55.575591
2842.836778	126927.875197	55.580596
2842.542465	126625.075321	55.585601
2841.560793	126391.599219	55.590605
2840.969446	126098.237094	55.595610
2840.166129	125850.895221	55.600615
2839.453628	125588.810372	55.605620
2838.987869	125295.094182	55.610625
2838.055793	125065.494815	55.615629
2837.738971	124764.865384	55.620634
2836.779397	124538.716193	55.625639
2836.151757	124240.224414	55.630644
2835.646232	123997.385714	55.635649
2834.520655	123739.498545	55.640653
2833.832776	123456.465987	55.645658
2833.540316	123185.385988	55.650663
2832.975363	122931.709723	55.655668
2831.939579	122693.246028	55.660673
2831.963864	122395.382718	55.665677
2830.984241	122164.596869	55.670682
2830.245401	121898.654277	55.675687
2829.727944	121605.634441	55.680692
2828.897662	121382.996024	55.685697
2827.887861	121104.597820	55.690701
2827.103981	120834.864054	55.695706
2826.724263	120570.693650	55.700711
2826.311036	120339.751590	55.705716
2825.366955	120045.794685	55.710721
2825.000056	119801.696627	55.715725
2824.549401	119524.699459	55.720730
2823.263983	119286.084087	55.725735
2822.910368	118994.299086	55.730740
2821.788911	118779.263996	55.735745
2821.199743	118498.465624	55.740749
2820.833063	118203.930321	55.745754
2819.981866	117976.119237	55.750759
2819.630145	117700.287572	55.755764
2818.705604	117429.462590	55.760769
2817.815208	117202.166039	55.765773
2817.711669	116901.865872	55.770778
2816.659237	116692.619805	55.775783
2816.164345	116403.133560	55.780788
2815.578367	116130.091614	55.785793
2814.920924	115890.767280	55.790797
2814.243018	115613.524592	55.795802
2813.798281	115342.061872	55.800807
2813.240596	115108.263727	55.805812
2811.526325	114832.862998	55.810817
2811.550159	114541.367368	55.815821
2811.018133	114325.108676	55.820826
2809.848609	114075.943630	55.825831
2809.728160	113779.364252	55.830836
2809.028749	113553.561675	55.835841
2808.191053	113262.211016	55.840845
2807.565779	113027.484634	55.845850
2806.731664	112733.861212	55.850855
2806.157018	112500.762790	55.855860
2805.386366	112239.450517	55.860865
2804.888179	111974.480529	55.865869
2804.231377	111716.125745	55.870874
2803.575120	111441.914852	55.875879
2802.897823	111215.254277	55.880884
2802.118419	110933.408964	55.885889
2801.578872	110677.248516	55.890893
2801.176300	110410.922170	55.895898
2800.427592	110164.667859	55.900903
2800.054503	109857.438539	55.905908
2798.967264	109638.548347	55.910913
2798.143949	109360.002395	55.915917
2797.857314	109082.193177	55.920922
2797.298024	108858.492690	55.925927
2796.567626	108556.349200	55.930932
2795.576550	108318.997250	55.935937
2795.429142	108042.021796	55.940941
2794.341335	107767.051232	55.945946
2793.960308	107537.053099	55.950951
2793.331114	107252.022376	55.955956
2792.579259	106986.194977	55.960961
2791.722881	106740.912494	55.965965
2791.275339	106444.435599	55.970970
2790.274625	106208.609687	55.975975
2789.713339	105936.628462	55.980980
2789.321199	105661.476664	55.985985
2788.491099	105417.770691	55.990989
2787.939546	105139.205144	55.995994
2787.133468	104875.408303	56.000999
2786.709972	104612.074022	56.006004
2785.932408	104333.909010	56.011009
2784.691006	104089.463445	56.016013
2784.696997	103810.025858	56.021018
2783.456157	103560.992615	56.026023
2782.847111	103311.950745	56.031028
2782.097118	103035.909199	56.036033
2781.485383	102794.086160	56.041037
2781.094304	102533.675412	56.046042
2780.513227	102257.939803	56.051047
2780.178788	102003.806148	56.056052
2779.160677	101751.280617	56.061057
2778.530503	101472.276163	56.066061
2777.694793	101208.392007	56.071066
2776.984100	100969.965515	56.076071
2776.585757	100684.260713	56.081076
2776.187275	100445.124135	56.086081
2774.916812	100153.430262	56.091085
2774.622311	99905.846578	56.096090
2773.784706	99658.040785	56.101095
2773.419577	99347.717854	56.106100
2772.448416	99135.033603	56.111105
2771.578731	98850.669381	56.116109
2771.770292	98585.758203	56.121114
2770.573965	98347.816356	56.126119
2770.089562	98050.988731	56.131124
2769.542592	97786.952218	56.136129
2768.687293	97550.987887	56.141133
2768.139681	97243.462316	56.146138
2767.637541	97016.751626	56.151143
2766.937509	96717.812896	56.156148
2766.061617	96472.996837	56.161153
2765.115840	96207.551523	56.166157
2764.650366	95917.794704	56.171162
2764.198857	95690.188767	56.176167
2763.508322	95400.702562	56.181172
2762.831613	95146.020722	56.186177
2762.055421	94866.073770	56.191181
2761.470750	94612.258553	56.196186
2760.045001	94350.684410	56.201191
2760.218487	94054.280762	56.206196
2759.269296	93836.683992	56.211201
2758.425666	93546.846551	56.216205
2758.187378	93301.875371	56.221210
2757.449309	93031.241488	56.226215
2756.572335	92758.128242	56.231220
2756.280343	92512.489474	56.236225
2755.522930	92228.597024	56.241229
2754.641480	91970.433147	56.246234
2753.584018	91717.797523	56.251239
2753.688082	91436.391158	56.256244
2752.931026	91202.095186	56.261249
2752.175559	90920.305341	56.266253
2751.196808	90658.051039	56.271258
2750.583899	90376.981088	56.276263
2749.867221	90131.017774	56.281268
2749.146980	89894.219272	56.286273
2748.363965	89634.799318	56.291277
2747.835893	89354.229985	56.296282
2747.403853	89070.326967	56.301287
2746.596229	88812.518389	56.306292
2745.800699	88589.002588	56.311297
2745.302421	88303.395712	56.316301
2744.683027	88074.798284	56.321306
2743.713052	87789.963949	56.326311
2743.308125	87518.870147	56.331316
2742.438076	87299.335329	56.336321
2741.397217	87029.876232	56.341325
2741.658150	86731.865403	56.346330
2740.393075	86507.811702	56.351335
2740.279390	86220.054326	56.356340
2739.791378	85937.729225	56.361345
2738.524988	85720.086352	56.366349
2737.439160	85450.565563	56.371354
2736.904073	85188.865340	56.376359
2736.559326	84946.249243	56.381364
2735.618175	84672.969261	56.386369
2735.277483	84418.581488	56.391373
2734.782487	84166.921391	56.396378
2733.881140	83902.239978	56.401383
2733.357874	83643.954349	56.406388
2733.063177	83395.662700	56.411393
2732.077045	83137.989023	56.416397
2731.629985	82861.314065	56.421402
2730.586028	82611.749685	56.426407
2730.438949	82347.076116	56.431412
2729.423367	82080.211183	56.436417
2728.645077	81832.661126	56.441421
2728.367614	81565.799913	56.446426
2727.514325	81297.898923	56.451431
2726.742678	81060.344994	56.456436
2726.184208	80764.043944	56.461441
2725.585972	80497.944377	56.466445
2724.817025	80265.088746	56.471450
2724.180102	79969.958530	56.476455
2723.621712	79723.653555	56.481460
2723.061016	79485.856147	56.486465
2721.939488	79207.441929	56.491469
2721.979199	78914.000307	56.496474
2720.647197	78691.530006	56.501479
2720.322100	78395.454136	56.506484
2719.782492	78157.668765	56.511489
2719.036612	77886.176891	56.516493
2718.194396	77624.164175	56.521498
2717.706781	77351.447247	56.526503
2717.011347	77103.098148	56.531508
2716.284641	76817.614323	56.536513
2715.443701	76578.748266	56.541517
2715.269672	76309.892330	56.546522
2714.051598	76021.367568	56.551527
2713.738962	75787.223441	56.556532
2713.204467	75510.445723	56.561537
2712.191765	75233.848937	56.566541
2711.593668	74997.731780	56.571546
2710.505044	74723.498211	56.576551
2710.648203	74458.658742	56.581556
2709.872477	74203.072258	56.586561
2709.368346	73902.237516	56.591565
2708.110476	73680.380704	56.596570
2707.308811	73408.406672	56.601575
2706.839950	73132.411560	56.606580
2706.304935	72898.431388	56.611585
2705.544063	72630.408178	56.616589
2705.186886	72359.252254	56.621594
2703.937523	72129.587931	56.626599
2703.459429	71845.072975	56.631604
2702.727397	71579.713589	56.636609
2702.308023	71333.951329	56.641613
2701.734880	71073.894492	56.646618
2700.600060	70803.459518	56.651623
2700.172475	70543.234595	56.656628
2699.776786	70312.936739	56.661633
2698.738063	70028.397455	56.666637
2698.536721	69751.545694	56.671642
2697.562651	69529.950152	56.676647
2697.186680	69238.495755	56.681652
2696.037188	69005.393827	56.686657
2695.221943	68713.459498	56.691661
2695.041201	68440.467530	56.696666
2694.115441	68202.690956	56.701671
2693.501595	67981.847603	56.706676
2692.995188	67676.472172	56.711681
2692.225666	67458.648738	56.716685
2691.746815	67162.238505	56.721690
2690.647207	66939.403573	56.726695
2690.231945	66656.828667	56.731700
2689.586100	66425.666463	56.736705
2688.637454	66158.166908	56.741709
2688.775771	65866.244707	56.746714
2687.743134	65650.902445	56.751719
2686.760267	65367.052727	56.756724
2686.775336	65120.407181	56.761729
2685.893806	64863.303370	56.766733
2685.155278	64571.688608	56.771738
2683.982528	64352.121555	56.776743
2683.602632	64056.072815	56.781748
2682.867124	63797.465852	56.786753
2681.788428	63573.758083	56.791757
2681.511060	63291.378751	56.796762
2680.372367	63060.955809	56.801767
2679.895755	62785.039131	56.806772
2679.260276	62527.636626	56.811777
2678.400289	62291.819217	56.816781
2678.256349	62021.980330	56.821786
2677.282256	61799.460917	56.826791
2676.882140	61521.581523	56.831796
2676.105473	61291.616635	56.836801
2675.420051	61024.179206	56.841805
2675.230708	60767.442286	56.846810
2674.016731	60523.510847	56.851815
2673.396106	60244.916074	56.856820
2672.821089	60017.391204	56.861825
2672.508403	59757.284913	56.866829
2671.745220	59490.669869	56.871834
2670.784898	59248.633034	56.876839
2670.215797	58989.638432	56.881844
2669.586525	58745.463498	56.886849
2668.824294	58486.829348	56.891853
2668.086543	58226.786474	56.896858
2667.156173	57981.349480	56.901863
2666.922315	57724.506434	56.906868
2666.157524	57467.279511	56.911873
2665.750671	57219.092154	56.916877
2665.036648	56976.330706	56.921882
2664.062175	56713.273583	56.926887
2663.321340	56480.488862	56.931892
2662.789614	56203.111666	56.936897
2661.693687	55985.178170	56.941901
2661.748900	55713.427597	56.946906
2660.666053	55453.788677	56.951911
2660.015388	55221.474008	56.956916
2659.363755	54970.605846	56.961921
2658.643949	54724.786575	56.966925
2658.167858	54465.787051	56.971930
2657.241187	54216.763899	56.976935
2656.651266	53961.909584	56.981940
2656.238817	53707.252220	56.986945
2655.550574	53458.701632	56.991949
2654.741628	53207.813097	56.996954
2654.080952	52975.082554	57.001959
2653.436939	52720.241611	57.006964
2652.631165	52453.934880	57.011969
2652.256777	52222.987992	57.016973
2651.195357	51987.356350	57.021978
2650.565705	51716.416372	57.026983
2649.936345	51491.973676	57.031988
2649.469854	51225.384572	57.036993
2648.643954	50985.242428	57.041997
2648.045452	50740.343982	57.047002
2647.432404	50508.732453	57.052007
2646.506667	50235.916081	57.057012
2645.961132	50006.524419	57.062017
2645.113684	49755.272587	57.067021
2644.734227	49497.015671	57.072026
2643.786795	49280.262603	57.077031
2643.258751	49026.268822	57.082036
2642.928561	48772.845202	57.087041
2641.715288	48555.323791	57.092045
2641.378263	48287.862847	57.097050
2640.521235	48036.168684	57.102055
2639.840099	47805.805195	57.107060
2639.416002	47567.043667	57.112065
2638.562690	47324.136914	57.117069
2638.130211	47064.298006	57.122074
2637.266185	46826.378534	57.127079
2636.724755	46582.714574	57.132084
2636.489343	46339.647581	57.137089
2635.534372	46093.762789	57.142093
2634.834075	45841.806316	57.147098
2634.079659	45619.298556	57.152103
2633.608715	45358.336565	57.157108
2632.620684	45095.638676	57.162113
2632.227382	44885.351324	57.167117
2631.586512	44614.088509	57.172122
2631.042803	44390.196764	57.177127
2630.100667	44124.318333	57.182132
2629.534349	43885.895188	57.187137
2628.664631	43641.698111	57.192141
2627.799832	43390.059326	57.197146
2627.497517	43150.804356	57.202151
2627.016705	42910.480485	57.207156
2626.436780	42659.544007	57.212161
2625.398656	42427.182985	57.217165
2624.982561	42184.537867	57.222170
2624.215370	41920.815887	57.227175
2623.483132	41691.730262	57.232180
2622.739172	41445.378276	57.237185
2621.951501	41200.826463	57.242189
2620.914659	40948.447442	57.247194
2620.474279	40711.977032	57.252199
2619.781672	40472.307335	57.257204
2619.199280	40257.082063	57.262209
2618.627701	40014.844822	57.267213
2618.011853	39775.877818	57.272218
2617.366072	39528.469202	57.277223
2616.226452	39298.011579	57.282228
2616.041277	39054.624908	57.287233
2614.937026	38833.156514	57.292237
2614.754145	38581.295289	57.297242
2613.708117	38347.324844	57.302247
2612.946951	38134.661834	57.307252
2612.957114	37862.435117	57.312257
2611.804352	37636.949774	57.317261
2611.422200	37411.786321	57.322266
2610.505707	37168.013143	57.327271
2609.808752	36933.788829	57.332276
2609.360730	36685.837196	57.337281
2608.646107	36464.632102	57.342285
2607.716876	36230.814763	57.347290
2607.323675	36006.155517	57.352295
2606.269284	35758.071862	57.357300
2605.695168	35516.670761	57.362305
2604.737931	35292.799567	57.367309
2604.622124	35056.952599	57.372314
2603.862131	34826.979587	57.377319
2603.073303	34606.302323	57.382324
2602.389770	34368.709152	57.387329
2601.823814	34141.252938	57.392333
2601.176495	33901.345480	57.397338
2600.409767	33680.991472	57.402343
2599.406605	33437.333823	57.407348
2599.131476	33200.839914	57.412353
2597.855309	32999.935548	57.417357
2597.836430	32744.223361	57.422362
2597.008085	32522.819973	57.427367
2595.765088	32299.841886	57.432372
2595.515791	32077.393531	57.437377
2595.129388	31860.031086	57.442381
2594.293983	31624.966366	57.447386
2593.629008	31396.252087	57.452391
2592.692075	31178.687259	57.457396
2592.254976	30954.346677	57.462401
2591.546961	30730.195883	57.467405
2591.139912	30502.238455	57.472410
2590.583493	30276.069557	57.477415
2589.427328	30049.230978	57.482420
2588.946243	29812.129533	57.487425
2587.932955	29611.501423	57.492429
2587.565884	29375.532112	57.497434
2586.673911	29142.464748	57.502439
2586.136793	28952.760478	57.507444
2585.581341	28689.521572	57.512449
2584.492212	28500.034882	57.517453
2583.913211	28269.364922	57.522458
2583.573629	28046.807162	57.527463
2582.604714	27831.557432	57.532468
2582.195399	27617.727351	57.537473
2581.137956	27395.918676	57.542477
2580.740296	27165.689858	57.547482
2579.976401	26958.789207	57.552487
2578.938509	26750.541394	57.557492
2578.604207	26525.018220	57.562497
2577.497632	26318.293839	57.567501
2576.901340	26111.384615	57.572506
2576.423696	25898.562754	57.577511
2575.424170	25686.643050	57.582516
2574.769379	25480.836364	57.587521
2574.284288	25266.182349	57.592525
2573.488711	25048.573891	57.597530
2572.795874	24857.283204	57.602535
2571.878364	24663.100559	57.607540
2571.594997	24454.245689	57.612545
2570.404299	24244.393880	57.617549
2569.590214	24051.119917	57.622554
2569.046076	23845.928746	57.627559
2568.041080	23644.275171	57.632564
2567.524208	23465.318962	57.637569
2566.653076	23274.096060	57.642573
2566.260449	23078.236284	57.647578
2565.572477	22878.397043	57.652583
2564.867928	22701.804646	57.657588
2564.424645	22509.547958	57.662593
2563.515784	22321.127486	57.667597
2562.887783	22114.239598	57.672602
2561.966786	21926.717988	57.677607
2561.361342	21766.331253	57.682612
2560.760103	21554.555826	57.687617
2559.511942	21405.684627	57.692621
2559.172094	21194.304493	57.697626
2558.342279	21022.492734	57.702631
2557.377494	20858.230037	57.707636
2556.462227	20676.476090	57.712641
2555.170307	20523.944169	57.717645
2554.172088	20382.867109	57.722650
2553.203607	20226.130861	57.727655
2552.322149	20074.482886	57.732660
2551.336350	19935.256082	57.737665
2549.944392	19816.834441	57.742669
2549.253884	19670.388028	57.747674
2548.407959	19554.352864	57.752679
2547.403505	19441.563099	57.757684
2546.718556	19334.233881	57.762689
2545.646393	19235.272555	57.767693
2544.947905	19121.587552	57.772698
2544.478965	19015.227695	57.777703
2543.707890	18922.127589	57.782708
2542.827028	18819.073403	57.787713
2541.895358	18739.867704	57.792717
2541.179406	18632.670590	57.797722
2540.975094	18541.759992	57.802727
2540.058271	18446.956228	57.807732
2539.430528	18356.794693	57.812737
2538.539401	18271.214474	57.817741
2538.103537	18181.046435	57.822746
2537.440905	18098.749559	57.827751
2536.775734	18002.174329	57.832756
2536.252842	17913.216768	57.837761
2535.547143	17836.172757	57.842765
2534.765245	17742.676478	57.847770
2534.394515	17646.991203	57.852775
2533.695306	17578.883078	57.857780
2533.126007	17485.865958	57.862785
2532.321718	17409.440990	57.867789
2531.701976	17320.969674	57.872794
2531.376203	17233.450590	57.877799
2530.480677	17147.746238	57.882804
2530.050298	17066.817724	57.887809
2529.064229	16982.033224	57.892813
2528.572187	16888.892004	57.897818
2528.119388	16803.185685	57.902823
2527.268400	16720.673207	57.907828
2526.660362	16626.385539	57.912833
2526.032156	16554.532278	57.917837
2525.126388	16470.650105	57.922842
2524.632841	16392.316565	57.927847
2523.773826	16305.749970	57.932852
2523.114346	16230.043903	57.937857
2522.299285	16141.906484	57.942861
2521.808746	16061.533043	57.947866
2521.262230	15993.466014	57.952871
2520.387444	15920.201038	57.957876
2519.904622	15829.398254	57.962881
2519.246976	15748.444309	57.967885
2518.572327	15680.131612	57.972890
2517.933919	15592.544020	57.977895
2517.157236	15505.690067	57.982900
2516.984798	15443.442492	57.987905
2515.632908	15360.517307	57.992909
2514.989689	15280.866985	57.997914
2514.634924	15222.347024	58.002919
2513.693033	15123.311738	58.007924
2513.545565	15060.116743	58.012929
2512.300145	14990.945580	58.017933
2512.045942	14908.205959	58.022938
2511.412852	14831.988907	58.027943
2510.751163	14750.978341	58.032948
2510.541933	14672.609870	58.037953
2509.580005	14612.731399	58.042957
2508.663128	14521.481219	58.047962
2508.299416	14441.541755	58.052967
2507.119635	14371.122955	58.057972
2506.628038	14305.571956	58.062977
2506.099329	14231.250413	58.067981
2505.252261	14167.398470	58.072986
2504.631074	14090.071752	58.077991
2503.797792	14012.222479	58.082996
2503.432201	13935.777466	58.088001
2502.526714	13864.838194	58.093005
2501.611987	13803.531845	58.098010
2501.553538	13719.862632	58.103015
2500.471667	13642.440261	58.108020
2499.913279	13595.625181	58.113025
2499.350209	13515.284676	58.118029
2499.056275	13429.039522	58.123034
2498.059953	13365.150679	58.128039
2497.497858	13306.469880	58.133044
2497.060360	13221.506951	58.138049
2496.255412	13158.298667	58.143053
2495.380108	13087.952646	58.148058
2494.477277	13014.949976	58.153063
2493.853035	12957.332286	58.158068
2493.535684	12882.839693	58.163073
2492.440575	12805.576671	58.168077
2491.821006	12737.145393	58.173082
2491.241256	12684.631006	58.178087
2490.295313	12603.246916	58.183092
2490.264171	12543.213439	58.188097
2488.945533	12489.695943	58.193101
2488.632257	12413.423014	58.198106
2488.106213	12328.305313	58.203111
2487.443156	12289.549548	58.208116
2486.939674	12212.125330	58.213121
2486.049033	12146.988954	58.218125
2485.454663	12088.545430	58.223130
2484.743582	12016.334260	58.228135
2484.116301	11951.520146	58.233140
2483.951612	11886.984108	58.238145
2482.816379	11809.393424	58.243149
2481.984473	11750.919819	58.248154
2481.474043	11677.808116	58.253159
2480.829270	11622.649376	58.258164
2480.097744	11557.708486	58.263169
2479.326916	11483.582462	58.268173
2478.765293	11416.811474	58.273178
2478.518164	11352.216022	58.278183
2477.527128	11284.305673	58.283188
2477.100787	11214.417152	58.288193
2476.193364	11150.438145	58.293197
2475.407074	11076.654670	58.298202
2474.872328	11015.430632	58.303207
2473.960702	10952.843788	58.308212
2473.649783	10889.933942	58.313217
2472.723230	10828.731552	58.318221
2472.232273	10768.663201	58.323226
2471.813851	10685.553607	58.328231
2470.823069	10631.707475	58.333236
2470.188395	10552.579898	58.338241
2469.348721	10512.246349	58.343245
2468.765549	10438.202226	58.348250
2468.108738	10375.760035	58.353255
2467.190995	10320.639079	58.358260
2467.071299	10242.957389	58.363265
2466.106564	10197.187499	58.368269
2465.741156	10133.761224	58.373274
2465.233017	10066.651236	58.378279
2464.449612	10011.092750	58.383284
2463.960994	9937.531180	58.388289
2463.363721	9868.019598	58.393293
2462.279793	9809.813609	58.398298
2461.695465	9738.195625	58.403303
2461.070899	9683.811200	58.408308
2460.639489	9604.818514	58.413313
2459.713158	9528.425004	58.418317
2459.243944	9484.224870	58.423322
2458.803984	9416.322372	58.428327
2457.731088	9350.205309	58.433332
2456.846475	9272.489752	58.438337
2456.395885	9224.455578	58.443341
2455.559849	9162.498119	58.448346
2454.997236	9099.886543	58.453351
2454.362026	9031.062148	58.458356
2453.946992	8976.027374	58.463361
2453.137787	8911.552812	58.468365
2452.297060	8842.364650	58.473370
2451.899884	8776.527978	58.478375
2450.997562	8716.957488	58.483380
2450.581606	8655.213617	58.488385
2450.023225	8593.721757	58.493389
2449.223944	8533.615383	58.498394
2448.253467	8463.006266	58.503399
2447.517889	8403.859863	58.508404
2447.240733	8334.877769	58.513409
2446.814692	8283.436716	58.518413
2445.824125	8224.550761	58.523418
2445.465057	8163.481494	58.528423
2444.247334	8098.302906	58.533428
2444.008092	8021.242143	58.538433
2442.936458	7968.390699	58.543437
2442.339383	7911.848054	58.548442
2442.065103	7839.152252	58.553447
2441.151356	7787.624576	58.558452
2440.809588	7727.851623	58.563457
2439.742839	7668.886072	58.568461
2439.172838	7603.207008	58.573466
2438.780468	7542.645692	58.578471
2437.934855	7482.251145	58.583476
2437.313801	7410.848528	58.588481
2436.972280	7346.344445	58.593485
2436.048560	7283.118562	58.598490
2435.310942	7222.169180	58.603495
2434.264873	7165.048993	58.608500
2434.180497	7110.128017	58.613505
2433.264530	7043.928862	58.618509
2432.713792	6979.717485	58.623514
2432.122615	6911.811702	58.628519
2431.058598	6863.807064	58.633524
2430.732407	6790.469904	58.638529
2430.210186	6729.917499	58.643533
2429.260338	6660.749285	58.648538
2428.543548	6607.031601	58.653543
2427.757053	6546.493452	58.658548
2427.566997	6483.040277	58.663553
2426.842464	6436.072513	58.668557
2425.752269	6360.331354	58.673562
2425.474372	6298.797012	58.678567
2424.509237	6249.096229	58.683572
2423.986534	6180.566906	58.688577
2423.515101	6121.187359	58.693581
2422.622802	6060.468415	58.698586
2422.282194	5994.643359	58.703591
2421.415449	5942.693448	58.708596
2420.782473	5878.233283	58.713601
2420.290125	5818.704458	58.718605
2419.497703	5751.606514	58.723610
2419.057308	5689.572796	58.728615
2417.971249	5635.772063	58.733620
2417.415951	5568.575830	58.738625
2416.921575	5514.012873	58.743629
2416.045953	5459.326006	58.748634
2415.560543	5383.691141	58.753639
2414.676235	5330.933779	58.758644
2413.955804	5278.482674	58.763649
2413.080790	5216.034008	58.768653
2412.679084	5170.991667	58.773658
2412.157391	5092.887475	58.778663
2411.441003	5042.452519	58.783668
2410.855086	4977.969895	58.788673
2410.550100	4926.925893	58.793677
2409.817383	4860.021291	58.798682
2409.051950	4793.974762	58.803687
2407.855764	4732.274706	58.808692
2407.549086	4676.936614	58.813697
2406.875163	4614.037455	58.818701
2405.928509	4564.645438	58.823706
2405.919533	4497.950293	58.828711
2404.936109	4443.072931	58.833716
2404.003612	4378.497251	58.838721
2403.404686	4315.664767	58.843725
2402.644262	4270.192299	58.848730
2401.651745	4207.894311	58.853735
2401.324876	4153.193112	58.858740
2400.751465	4093.565022	58.863745
2400.331452	4040.721320	58.868749
2399.343001	3989.152502	58.873754
2398.966891	3919.757906	58.878759
2398.091784	3866.345823	58.883764
2397.572673	3809.403508	58.888769
2396.799504	3746.444149	58.893773
2396.456192	3691.695227	58.898778
2395.771193	3625.056032	58.903783
2394.888904	3569.442727	58.908788
2394.305619	3508.582008	58.913793
2393.853728	3451.610707	58.918797
2392.712545	3396.084855	58.923802
2392.300340	3330.202619	58.928807
2391.665724	3273.442369	58.933812
2390.778737	3224.987805	58.938817
2390.314783	3154.463328	58.943821
2389.449950	3113.674054	58.948826
2388.733978	3047.807348	58.953831
2387.861730	2998.284219	58.958836
2387.468818	2936.290863	58.963841
2386.865980	2882.000923	58.968845
2386.016390	2833.136392	58.973850
2385.447011	2783.115681	58.978855
2384.550534	2725.997690	58.983860
2384.137477	2672.686246	58.988865
2383.366261	2622.501735	58.993869
2382.624136	2568.835157	58.998874
2382.390484	2510.978883	59.003879
2381.398272	2472.804436	59.008884
2381.003179	2406.653955	59.013889
2380.665701	2347.504193	59.018893
2380.043323	2286.649241	59.023898
2379.327409	2235.760991	59.028903
2378.800420	2169.640386	59.033908
2377.889720	2114.157782	59.038913
2376.924625	2051.807864	59.043917
2376.078818	1996.060720	59.048922
2375.513468	1938.750580	59.053927
2374.969751	1879.265595	59.058932
2374.424790	1826.040458	59.063937
2373.599303	1780.740615	59.068941
2372.690058	1729.354112	59.073946
2372.124635	1677.798142	59.078951
2371.562473	1622.553111	59.083956
2370.815529	1561.928326	59.088961
2369.968223	1516.005105	59.093965
2369.094379	1466.588374	59.098970
2368.900823	1419.828464	59.103975
2367.973987	1381.406024	59.108980
2367.504749	1312.148183	59.113985
2367.282013	1255.281588	59.118989
2366.384809	1208.193959	59.123994
2365.535597	1162.078190	59.128999
2364.580534	1122.127280	59.134004
2364.262393	1055.600139	59.139009
2363.620723	1007.862342	59.144013
2362.848113	954.974549	59.149018
2362.108609	901.884577	59.154023
2361.307770	850.573885	59.159028
2360.624839	811.052981	59.164033
2360.225499	766.423594	59.169037
2359.166591	725.907562	59.174042
2358.291394	683.020738	59.179047
2357.744652	622.609404	59.184052
2357.170940	591.202506	59.189057
2356.508491	536.914218	59.194061
2355.962463	502.904333	59.199066
2355.555919	456.100881	59.204071
2354.628335	409.585210	59.209076
2353.909045	361.524394	59.214081
2353.509326	331.235309	59.219085
2352.394954	278.689609	59.224090
2351.843238	230.847074	59.229095
2350.902748	198.931512	59.234100
2350.195106	160.721978	59.239105
2349.299458	126.434126	59.244109
2348.830950	94.882319	59.249114
2348.476805	53.625656	59.254119
2347.387502	24.340668	59.259124
2346.831086	-12.602501	59.264129
2345.542908	-29.592478	59.269133
2344.318826	-41.920329	59.274138
2340.174531	27.200079	59.279143
2337.442527	87.890722	59.284148
2338.487278	90.847228	59.289153
2339.854055	75.974860	59.294157
2340.255163	83.420336	59.299162
2341.133391	74.019976	59.304167
2339.765959	71.060959	59.309172
2338.311486	83.264875	59.314177
2337.181127	71.357287	59.319181
2336.526952	79.592990	59.324186
2336.418256	82.249897	59.329191
2336.036993	84.003901	59.334196
2334.825594	85.042772	59.339201
2334.195260	90.256543	59.344205
2333.528983	94.999796	59.349210
2333.786931	90.852639	59.354215
2333.070538	90.381194	59.359220
2331.781921	91.096437	59.364225
2331.195137	83.405955	59.369229
2330.136820	102.256708	59.374234
2329.938749	86.776256	59.379239
2329.053960	86.793547	59.384244
2328.135629	84.580134	59.389249
2327.786086	86.371685	59.394253
2327.269369	90.520385	59.399258
2327.322039	80.279588	59.404263
2325.948128	93.579290	59.409268
2325.013907	91.751581	59.414273
2324.773423	83.741262	59.419277
2324.329344	98.946605	59.424282
2323.687559	84.750731	59.429287
2323.189109	95.576223	59.434292
2321.823476	88.901784	59.439297
2321.044738	93.098350	59.444301
2320.544600	97.130888	59.449306
2320.077005	93.056225	59.454311
2319.539773	95.249690	59.459316
2318.627199	89.399068	59.464321
2317.952058	75.847135	59.469325
2317.460344	95.221425	59.474330
2316.699985	90.955086	59.479335
2315.707150	91.893073	59.484340
2315.833106	92.943765	59.489345
2315.397343	95.589472	59.494349
2314.096462	88.911075	59.499354
2313.469812	76.196663	59.504359
2312.583983	90.425008	59.509364
2312.458637	91.498211	59.514369
2311.538952	87.127840	59.519373
2310.740879	98.232658	59.524378
2310.907002	93.343157	59.529383
2309.851249	92.928696	59.534388
2308.545057	88.756816	59.539393
2308.096146	90.135216	59.544397
2307.919658	95.053094	59.549402
2306.854476	88.360971	59.554407
2306.215923	94.977903	59.559412
2306.032092	91.676640	59.564417
2305.234773	94.196775	59.569421
2304.065312	96.991967	59.574426
2303.504690	86.657636	59.579431
2303.082071	94.408792	59.584436
2302.713234	98.687001	59.589441
2301.879616	92.573137	59.594445
2300.978820	95.259490	59.599450
2300.518210	91.308297	59.604455
2299.848664	102.487348	59.609460
2299.080439	87.813240	59.614465
2298.530225	92.318903	59.619469
2297.522711	93.218226	59.624474
2297.053360	85.053408	59.629479
2296.704044	93.478881	59.634484
2295.951141	94.307860	59.639489
2295.752677	96.971124	59.644493
2294.657735	95.566293	59.649498
2294.400920	99.273249	59.654503
2293.312454	88.070202	59.659508
2292.721707	90.992795	59.664513
2292.123717	92.409036	59.669517
2290.901222	97.089139	59.674522
2290.151371	89.594834	59.679527
2290.189441	88.352482	59.684532
2289.321071	100.056633	59.689537
2288.636903	90.407346	59.694541
2287.479687	99.817214	59.699546
2287.016557	95.380742	59.704551
2287.233709	93.636919	59.709556
2286.020700	91.493913	59.714561
2285.631667	91.492507	59.719565
2284.473954	96.074032	59.724570
2283.988794	91.333563	59.729575
2283.497129	83.971770	59.734580
2283.044678	88.960224	59.739585
2282.484198	79.158870	59.744589
2281.622813	95.326069	59.749594
2280.824267	84.931717	59.754599
2279.659914	95.888065	59.759604
2279.088948	92.635595	59.764609
2278.993984	88.902366	59.769613
2278.080456	92.376033	59.774618
2277.424341	92.096883	59.779623
2276.865483	84.864015	59.784628
2276.546718	92.625505	59.789633
2275.830211	86.516732	59.794637
2274.984573	98.226739	59.799642
2274.677920	90.138616	59.804647
2273.520559	84.336303	59.809652
2272.275199	100.810409	59.814657
2271.790152	89.722962	59.819661
2271.615133	99.344455	59.824666
2271.352413	86.476134	59.829671
2270.162665	88.602804	59.834676
2269.147564	91.315181	59.839681
2268.825365	81.841870	59.844685
2268.073992	92.428373	59.849690
2267.586051	96.977780	59.854695
2267.132242	95.364036	59.859700
2266.549649	98.570758	59.864705
2266.160222	83.647358	59.869709
2264.918936	96.541288	59.874714
2264.104084	77.924505	59.879719
2263.465927	84.850445	59.884724
2262.534537	86.835217	59.889729
2262.180259	75.449509	59.894733
2261.205747	88.501382	59.899738
2261.284766	88.843610	59.904743
2260.694414	87.622095	59.909748
2260.276738	91.815017	59.914753
2259.817063	79.157711	59.919758
2258.443689	96.978281	59.924762
2257.522724	88.831494	59.929767
2257.065952	89.883157	59.934772
2256.374211	96.934294	59.939777
2256.098320	85.971366	59.944782
2255.478118	91.327040	59.949786
2254.382413	79.686795	59.954791
2253.363765	104.786770	59.959796
2253.062918	89.220139	59.964801
2252.174011	78.721872	59.969806
2251.535905	87.521145	59.974810
2251.452401	98.271361	59.979815
2250.730030	88.759030	59.984820
2249.970773	85.230522	59.989825
2249.791093	82.612976	59.994830
2248.607425	93.889349	59.999834
2247.770333	85.406003	60.004839
2246.851258	86.977259	60.009844
2246.125211	91.804123	60.014849
2245.891644	84.746735	60.019854
2245.419345	90.663973	60.024858
2244.894994	89.356301	60.029863
2244.402255	86.320081	60.034868
2243.365543	88.987011	60.039873
2242.270737	93.593264	60.044878
2241.543752	91.142957	60.049882
2241.063501	84.799608	60.054887
2240.486303	81.863516	60.059892
2239.599346	104.712890	60.064897
2239.451816	86.466470	60.069902
2238.746512	74.269167	60.074906
2238.564991	79.452755	60.079911
2237.916770	83.705902	60.084916
2236.804146	89.795675	60.089921
2236.654716	88.780176	60.094926
2235.798703	87.236549	60.099930
2234.559358	94.462860	60.104935
2233.515584	93.589233	60.109940
2232.720585	96.318745	60.114945
2232.984533	74.700342	60.119950
2231.734181	99.266234	60.124954
2231.285319	81.594303	60.129959
2230.690747	91.943059	60.134964
2230.357450	76.337444	60.139969
2230.228791	79.416969	60.144974
2228.917001	86.069747	60.149978
2228.105692	81.737409	60.154983
2227.277434	82.505823	60.159988
2226.596358	87.338171	60.164993
2226.291271	88.263279	60.169998
2225.711174	97.919069	60.175002
2225.294850	80.879041	60.180007
2224.239868	87.107901	60.185012
2223.537380	77.620817	60.190017
2223.037453	76.230433	60.195022
2222.120680	90.771195	60.200026
2221.223107	94.318038	60.205031
2220.693386	80.697341	60.210036
2219.742015	90.295335	60.215041
2219.346963	74.735789	60.220046
2218.270874	89.308132	60.225050
2218.233339	79.087963	60.230055
2217.562002	82.326115	60.235060
2217.019521	91.178031	60.240065
2217.043818	85.200905	60.245070
2216.009286	87.981034	60.250074
2215.110670	93.164850	60.255079
2214.396677	79.970763	60.260084
2213.394769	95.099022	60.265089
2213.259584	78.774459	60.270094
2212.419072	83.270996	60.275098
2211.021292	74.506051	60.280103
2210.364011	80.200333	60.285108
2209.718659	85.911647	60.290113
2209.726902	87.416226	60.295118
2209.484062	85.769026	60.300122
2208.715222	86.487021	60.305127
2208.309164	80.787895	60.310132
2207.096032	89.820318	60.315137
2206.047408	77.885639	60.320142
2205.639041	81.310723	60.325146
2205.012672	88.228497	60.330151
2204.405043	84.843098	60.335156
2203.618770	82.703395	60.340161
2203.480570	90.920344	60.345166
2202.130416	76.862135	60.350170
2201.572681	73.363173	60.355175
2201.205171	74.151536	60.360180
2200.713870	88.498651	60.365185
2199.973528	84.776355	60.370190
2198.631258	78.156632	60.375194
2197.938282	78.771135	60.380199
2197.178273	85.536653	60.385204
2197.370401	87.201285	60.390209
2196.769244	82.791465	60.395214
2196.374088	83.076459	60.400218
2195.288579	85.987679	60.405223
2194.481656	80.910369	60.410228
2193.672700	89.522300	60.415233
2192.869692	82.269847	60.420238
2192.301108	83.414949	60.425242
2192.257974	81.688761	60.430247
2191.827504	86.856656	60.435252
2190.405652	83.065873	60.440257
2189.803573	78.225714	60.445262
2188.774400	93.139115	60.450266
2188.497034	86.484483	60.455271
2188.252583	72.988850	60.460276
2187.512069	73.366480	60.465281
2186.159858	87.597876	60.470286
2185.530178	80.328967	60.475290
2184.963421	78.126060	60.480295
2184.745116	83.019031	60.485300
2184.116341	77.506627	60.490305
2183.823626	72.295707	60.495310
2182.970098	84.924718	60.500314
2181.811223	79.419147	60.505319
2181.346842	72.409434	60.510324
2180.762457	71.373064	60.515329
2180.440293	75.870944	60.520334
2178.784702	94.034340	60.525338
2178.155397	83.751948	60.530343
2178.069820	77.748107	60.535348
2177.246033	82.156847	60.540353
2177.149686	69.400934	60.545358
2176.784060	66.805015	60.550362
2175.449299	75.951350	60.555367
2174.690920	80.425403	60.560372
2173.929458	83.964856	60.565377
2173.672826	83.975574	60.570382
2172.610942	83.775020	60.575386
2171.925242	82.907683	60.580391
2171.355381	81.749168	60.585396
2170.798432	84.724765	60.590401
2170.631318	82.548338	60.595406
2169.319725	81.617884	60.600410
2168.458868	80.540229	60.605415
2167.773675	87.664451	60.610420
2167.200987	88.319799	60.615425
2166.778064	82.164485	60.620430
2166.286043	87.178152	60.625434
2165.760669	80.999671	60.630439
2164.860019	77.271285	60.635444
2163.745248	89.339383	60.640449
2163.291672	73.527380	60.645454
2162.837367	86.258628	60.650458
2162.330362	80.949250	60.655463
2161.954900	83.337838	60.660468
2160.692356	85.526564	60.665473
2160.248567	84.828997	60.670478
2159.153669	83.050496	60.675482
2158.887034	80.177110	60.680487
2158.699401	84.795569	60.685492
2157.408432	93.308952	60.690497
2156.601415	75.603999	60.695502
2156.294364	87.837244	60.700506
2155.814862	80.170795	60.705511
2155.369780	83.325756	60.710516
2154.149648	86.182662	60.715521
2153.355062	83.962295	60.720526
2152.509973	84.077420	60.725530
2152.045103	80.445468	60.730535
2152.266841	81.421031	60.735540
2151.387375	84.378421	60.740545
2150.420341	84.733657	60.745550
2149.734817	71.915116	60.750554
2148.956015	81.977728	60.755559
2148.710680	87.384323	60.760564
2147.099728	87.714000	60.765569
2146.699775	79.266992	60.770574
2146.049152	83.419617	60.775578
2145.518636	85.769734	60.780583
2145.453566	73.038821	60.785588
2144.563132	75.844994	60.790593
2143.906254	79.516086	60.795598
2143.098607	80.964045	60.800602
2142.332218	88.481184	60.805607
2141.877504	82.603720	60.810612
2141.025043	86.509264	60.815617
2139.999519	83.327378	60.820622
2139.237067	78.670368	60.825626
2138.521845	94.100067	60.830631
2138.546434	77.065806	60.835636
2137.661378	95.477529	60.840641
2137.400051	67.789498	60.845646
2136.856765	78.939057	60.850650
2136.046424	94.502116	60.855655
2135.565745	76.254982	60.860660
2134.858565	73.292236	60.865665
2133.991149	85.582854	60.870670
2133.031136	82.335385	60.875674
2132.146196	76.934602	60.880679
2131.831620	88.800051	60.885684
2131.251973	90.866244	60.890689
2130.118540	74.875131	60.895694
2129.529170	81.086908	60.900698
2128.753579	74.604382	60.905703
2128.638816	96.038184	60.910708
2128.029689	76.713923	60.915713
2127.902489	70.240476	60.920718
2126.823317	78.046929	60.925722
2125.924847	88.839711	60.930727
2125.448470	75.347776	60.935732
2124.430758	89.172898	60.940737
2123.755581	81.438162	60.945742
2122.953882	74.668058	60.950746
2122.441393	85.986193	60.955751
2121.920793	85.286629	60.960756
2121.084220	74.026371	60.965761
2120.874514	77.878813	60.970766
2120.130012	77.347235	60.975770
2118.954818	76.770462	60.980775
2118.788496	67.253539	60.985780
2118.274924	75.872221	60.990785
2117.599711	71.975625	60.995790
2116.423651	83.961998	61.000794
2115.949360	88.550255	61.005799
2115.487888	84.315403	61.010804
2115.018964	73.919286	61.015809
2114.046201	76.470462	61.020814
2113.339882	77.974887	61.025818
2112.238610	87.021130	61.030823
2112.211713	76.313609	61.035828
2111.628511	84.509704	61.040833
2110.460098	71.271085	61.045838
2109.776058	77.065820	61.050842
2109.084906	89.278016	61.055847
2108.980901	95.679278	61.060852
2108.204806	85.144248	61.065857
2107.567764	85.190106	61.070862
2106.747604	75.365364	61.075866
2105.861038	82.647699	61.080871
2105.589792	83.794520	61.085876
2104.704937	86.002184	61.090881
2103.943837	76.466101	61.095886
2103.453025	72.492942	61.100890
2102.745325	73.675906	61.105895
2102.523071	79.130874	61.110900
2101.725656	84.748071	61.115905
2100.542958	85.175392	61.120910
2100.147638	80.502713	61.125914
2099.511821	79.991739	61.130919
2099.107793	77.922296	61.135924
2098.021547	83.063378	61.140929
2097.440213	66.079557	61.145934
2096.605442	77.858817	61.150938
2096.038606	83.789493	61.155943
2096.062297	71.225847	61.160948
2094.872189	76.094840	61.165953
2093.976705	77.681325	61.170958
2093.552651	83.542038	61.175962
2092.991682	74.368423	61.180967
2092.837091	62.705090	61.185972
2091.257232	69.849868	61.190977
2090.438611	70.924285	61.195982
2090.092980	80.123421	61.200986
2089.753642	83.528104	61.205991
2089.324612	79.499413	61.210996
2087.936331	76.241080	61.216001
2087.261638	68.659244	61.221006
2086.594148	75.719168	61.226010
2085.944554	78.725249	61.231015
2085.877632	66.977042	61.236020
2085.472688	76.948798	61.241025
2084.693791	70.230282	61.246030
2083.771186	67.514617	61.251034
2083.107717	72.867719	61.256039
2082.574664	66.327802	61.261044
2081.057792	71.680718	61.266049
2080.782829	73.545611	61.271054
2080.121924	67.558969	61.276058
2079.646240	73.815784	61.281063
2079.355158	63.965447	61.286068
2078.534692	75.416025	61.291073
2077.682287	75.444029	61.296078
2077.137861	75.572963	61.301082
2076.372680	70.575803	61.306087
2076.001762	74.521636	61.311092
2074.493537	79.341777	61.316097
2074.033363	73.965070	61.321102
2073.835840	82.517837	61.326106
2073.309423	72.830992	61.331111
2072.647869	75.979316	61.336116
2071.277066	71.409410	61.341121
2070.876173	82.157928	61.346126
2070.643234	72.720964	61.351130
2069.708676	78.282663	61.356135
2069.711948	67.366949	61.361140
2068.539938	73.809959	61.366145
2067.703445	71.627810	61.371150
2067.601487	76.839771	61.376154
2066.391294	76.984479	61.381159
2065.835801	72.761408	61.386164
2064.995906	75.758271	61.391169
2064.794028	77.843369	61.396174
2063.959086	80.199234	61.401178
2063.272151	75.762067	61.406183
2062.615588	80.764013	61.411188
2061.910174	77.543976	61.416193
2061.294080	77.315297	61.421198
2060.061092	75.940360	61.426202
2059.002376	77.201116	61.431207
2059.087996	64.879952	61.436212
2058.469664	73.668222	61.441217
2058.590032	79.105086	61.446222
2057.928155	64.776915	61.451226
2056.774470	82.852813	61.456231
2056.219367	79.342430	61.461236
2055.358133	82.358453	61.466241
2054.224047	72.015878	61.471246
2053.907080	77.167348	61.476250
2052.882756	82.459461	61.481255
2052.651113	67.366031	61.486260
2051.889462	71.548907	61.491265
2051.788586	70.778017	61.496270
2050.618805	74.065346	61.501274
2049.877614	84.022665	61.506279
2049.514708	72.193705	61.511284
2048.444503	77.273912	61.516289
2047.482896	71.705567	61.521294
2047.053741	80.519010	61.526298
2046.553215	82.840731	61.531303
2046.377535	77.043582	61.536308
2045.704404	80.477588	61.541313
2044.721206	74.631985	61.546318
2044.281223	76.190349	61.551322
2043.294551	83.723543	61.556327
2043.208064	73.618397	61.561332
2041.917072	71.279740	61.566337
2041.184430	73.335538	61.571342
2041.071266	74.373701	61.576346
2040.228965	86.220402	61.581351
2039.481229	70.666432	61.586356
2038.199796	73.829566	61.591361
2037.477794	76.613771	61.596366
2037.277765	69.726137	61.601370
2036.700098	76.845927	61.606375
2036.552258	69.377603	61.611380
2035.700954	74.348960	61.616385
2034.627556	74.456204	61.621390
2034.002064	78.054531	61.626394
2033.426147	83.166680	61.631399
2033.043212	77.454463	61.636404
2031.744076	81.987566	61.641409
2031.317839	70.253815	61.646414
2031.188024	77.220531	61.651418
2030.486419	85.284048	61.656423
2029.792996	75.349342	61.661428
2028.950755	77.860910	61.666433
2028.472999	75.677029	61.671438
2027.385263	72.052503	61.676442
2026.162873	75.620992	61.681447
2025.914987	75.239270	61.686452
2025.277322	76.160414	61.691457
2025.116580	78.917043	61.696462
2024.809320	73.817263	61.701466
2023.468664	73.476518	61.706471
2023.041825	75.773932	61.711476
2022.235455	76.942615	61.716481
2021.808733	77.822397	61.721486
2020.910052	65.012514	61.726490
2019.867084	78.357557	61.731495
2019.479462	77.310494	61.736500
2018.902192	70.858032	61.741505
2018.398765	75.854603	61.746510
2018.019326	76.741072	61.751514
2016.806438	75.377158	61.756519
2016.420546	77.327468	61.761524
2016.094094	82.026306	61.766529
2014.864061	80.504271	61.771534
2014.194587	68.656174	61.776538
2013.350921	82.810067	61.781543
2013.356269	61.898200	61.786548
2012.540289	73.351230	61.791553
2011.426250	74.882546	61.796558
2010.664886	69.621465	61.801562
2010.139939	81.731598	61.806567
2009.909687	75.228790	61.811572
2009.521137	75.629451	61.816577
2008.464959	82.331633	61.821582
2008.037368	75.248317	61.826586
2007.152747	70.541361	61.831591
2006.333258	63.695285	61.836596
2005.138733	74.519304	61.841601
2004.369698	70.967201	61.846606
2004.115642	67.535203	61.851610
2003.985839	82.616533	61.856615
2003.437288	72.605231	61.861620
2002.706888	78.415230	61.866625
2001.856164	64.126518	61.871630
2001.324961	75.799267	61.876634
2000.756672	77.649225	61.881639
1999.823798	72.631401	61.886644
1998.870679	74.007877	61.891649
1998.371053	72.106583	61.896654
1998.143745	66.153644	61.901658
1996.741615	77.751751	61.906663
1996.330204	64.891347	61.911668
1995.671917	65.497241	61.916673
1995.665632	67.819365	61.921678
1995.116126	66.777503	61.926682
1993.583097	71.237362	61.931687
1993.376293	67.236497	61.936692
1992.737261	72.942112	61.941697
1991.545540	70.348039	61.946702
1990.790446	58.239173	61.951706
1990.186022	71.309616	61.956711
1989.892105	56.694430	61.961716
1989.276259	71.507557	61.966721
1988.985053	68.358988	61.971726
1988.140286	69.458085	61.976730
1986.791363	85.280096	61.981735
1986.676647	66.937099	61.986740
1986.439638	60.766518	61.991745
1985.194723	73.462409	61.996750
1984.348626	66.647370	62.001754
1983.699940	75.831534	62.006759
1983.605829	70.486628	62.011764
1982.781309	63.997735	62.016769
1981.816133	68.870490	62.021774
1981.011258	66.259173	62.026778
1980.308881	69.013468	62.031783
1980.286545	70.123945	62.036788
1979.792652	73.958424	62.041793
1978.482075	74.765626	62.046798
1977.986677	63.452862	62.051802
1977.294614	68.037852	62.056807
1977.002908	66.305400	62.061812
1975.979305	65.114878	62.066817
1975.164796	65.318241	62.071822
1974.778317	66.461287	62.076826
1974.064979	64.075128	62.081831
1973.501866	71.946362	62.086836
1972.727024	77.451200	62.091841
1971.760323	69.792756	62.096846
1971.519984	67.460823	62.101850
1970.670288	71.203553	62.106855
1969.896707	55.518122	62.111860
1969.200730	73.565529	62.116865
1968.987180	71.123692	62.121870
1968.685971	64.512316	62.126874
1967.425970	72.281290	62.131879
1966.695345	56.294165	62.136884
1966.207961	59.676624	62.141889
1965.571935	67.237747	62.146894
1964.859166	62.191310	62.151898
1963.817099	66.070228	62.156903
1963.448816	63.350194	62.161908
1963.174586	63.824174	62.166913
1962.312519	55.876334	62.171918
1961.325972	60.339343	62.176922
1960.384742	67.753382	62.181927
1960.056263	55.792844	62.186932
1959.870399	59.986839	62.191937
1958.932501	63.611114	62.196942
1958.131109	60.277044	62.201946
1956.888795	63.801415	62.206951
1957.114081	63.921729	62.211956
1956.793325	62.063010	62.216961
1955.599074	69.362681	62.221966
1955.301760	63.119678	62.226970
1954.369584	74.930193	62.231975
1953.357391	69.149156	62.236980
1952.516464	74.711793	62.241985
1951.882362	71.355898	62.246990
1951.349672	62.524760	62.251994
1950.833922	72.231846	62.256999
1950.649018	64.406739	62.262004
1949.830283	73.100684	62.267009
1948.829610	73.573292	62.272014
1948.871261	56.807603	62.277018
1947.225839	81.653843	62.282023
1946.802962	61.483296	62.287028
1946.078801	64.504395	62.292033
1945.363926	72.759251	62.297038
1945.159394	66.045804	62.302042
1944.791090	75.882445	62.307047
1943.828342	76.842597	62.312052
1943.251535	74.513616	62.317057
1942.325267	73.134200	62.322062
1941.240430	70.472724	62.327066
1940.347553	86.999759	62.332071
1940.229968	74.934774	62.337076
1939.727862	67.142674	62.342081
1939.620438	73.922914	62.347086
1938.925985	63.734536	62.352090
1937.579833	74.193158	62.357095
1937.120150	71.238490	62.362100
1936.331322	76.445949	62.367105
1935.919388	70.249526	62.372110
1935.139680	64.138295	62.377114
1934.138616	72.206783	62.382119
1933.889551	75.723298	62.387124
1933.252289	74.167125	62.392129
1932.155567	74.057350	62.397134
1931.671571	76.220354	62.402138
1931.196617	68.420792	62.407143
1930.628891	73.575807	62.412148
1929.645978	62.904972	62.417153
1928.732294	74.961702	62.422158
1928.425365	71.547568	62.427162
1927.740246	76.557225	62.432167
1927.657536	72.670702	62.437172
1926.755148	67.009435	62.442177
1925.875843	66.221783	62.447182
1925.478434	63.585223	62.452186
1924.568858	79.417924	62.457191
1923.502090	66.391931	62.462196
1923.226104	73.999982	62.467201
1922.754890	70.536239	62.472206
1922.328071	62.677005	62.477210
1920.903876	61.528023	62.482215
1920.541060	67.498866	62.487220
1920.046510	70.150801	62.492225
1919.209358	72.158569	62.497230
1918.253918	61.063930	62.502234
1917.599555	70.588029	62.507239
1917.166864	56.089507	62.512244
1916.541626	67.553268	62.517249
1916.358381	65.997562	62.522254
1915.475309	62.922465	62.527258
1914.442069	72.647055	62.532263
1914.017462	68.944115	62.537268
1913.516849	64.633529	62.542273
1912.062956	68.158396	62.547278
1911.636778	69.336137	62.552282
1911.063102	71.175928	62.557287
1911.074689	68.206371	62.562292
1910.329236	68.285256	62.567297
1909.342647	62.777707	62.572302
1908.872146	57.058926	62.577306
1908.234325	59.632686	62.582311
1907.378008	65.265580	62.587316
1906.723217	71.156629	62.592321
1905.817888	65.175732	62.597326
1905.581786	57.215268	62.602330
1904.468810	70.230841	62.607335
1903.566831	72.266250	62.612340
1903.300816	72.913966	62.617345
1902.735460	82.114877	62.622350
1902.626330	64.758142	62.627354
1901.579174	67.079937	62.632359
1900.707101	66.772092	62.637364
1900.222496	75.621152	62.642369
1899.581259	76.583891	62.647374
1898.709986	66.371561	62.652378
1897.647699	82.949147	62.657383
1897.305722	69.260923	62.662388
1896.719703	68.729479	62.667393
1896.276707	87.369072	62.672398
1895.694899	69.261091	62.677402
1894.651254	75.675903	62.682407
1894.321517	75.814943	62.687412
1893.775571	68.105506	62.692417
1892.546441	71.176827	62.697422
1892.064308	70.720350	62.702426
1891.254402	80.858906	62.707431
1890.744138	80.093096	62.712436
1890.713712	73.568045	62.717441
1889.353116	67.394518	62.722446
1889.170464	61.880763	62.727450
1888.301654	72.303041	62.732455
1887.220378	67.364016	62.737460
1886.497829	67.778299	62.742465
1885.619878	74.028042	62.747470
1885.490693	64.677144	62.752474
1884.841922	77.779872	62.757479
1884.645260	79.812114	62.762484
1884.039163	74.311969	62.767489
1882.895436	78.790503	62.772494
1882.725229	70.614580	62.777498
1881.329624	65.952532	62.782503
1880.597518	65.958347	62.787508
1880.451450	72.238542	62.792513
1879.991282	67.188296	62.797518
1879.259418	57.504177	62.802522
1878.255105	71.090681	62.807527
1877.800266	71.044591	62.812532
1877.172039	69.871757	62.817537
1876.197489	71.363636	62.822542
1875.598259	63.602745	62.827546
1874.812736	67.429926	62.832551
1874.454869	62.968960	62.837556
1873.627508	74.816465	62.842561
1872.561704	74.604040	62.847566
1872.381434	62.405533	62.852570
1871.839986	66.055198	62.857575
1871.184582	77.478032	62.862580
1870.367208	67.378576	62.867585
1869.502693	72.710025	62.872590
1869.340740	56.408740	62.877594
1868.557076	66.804885	62.882599
1867.629094	65.028397	62.887604
1866.945485	69.437035	62.892609
1866.511818	67.856440	62.897614
1866.126613	60.048958	62.902618
1864.647438	75.237277	62.907623
1864.016849	67.777818	62.912628
1863.627313	65.299283	62.917633
1863.183923	62.288431	62.922638
1862.750911	52.888017	62.927642
1861.722157	75.682622	62.932647
1861.164506	66.612632	62.937652
1860.872616	65.522013	62.942657
1860.149808	77.732949	62.947662
1859.211480	68.072151	62.952666
1858.256601	73.544101	62.957671
1857.988060	59.483133	62.962676
1857.226216	60.554912	62.967681
1856.404142	74.497246	62.972686
1856.009541	62.925678	62.977690
1855.420971	62.164426	62.982695
1854.434506	64.514447	62.987700
1853.419927	64.678654	62.992705
1852.749097	69.738092	62.997710
1852.567917	70.777599	63.002714
1851.873418	68.155107	63.007719
1851.097323	72.827581	63.012724
1850.431247	73.190332	63.017729
1849.427180	66.178090	63.022734
1849.389531	58.170356	63.027738
1848.749340	76.560560	63.032743
1848.313369	66.734854	63.037748
1847.500387	59.514089	63.042753
1846.635279	62.223294	63.047758
1846.117351	70.200903	63.052762
1845.082479	72.583845	63.057767
1844.313379	72.313283	63.062772
1844.174361	58.635435	63.067777
1843.389708	71.982076	63.072782
1842.361851	68.743922	63.077786
1841.697278	58.180275	63.082791
1840.996357	69.725446	63.087796
1840.571991	74.701602	63.092801
1840.305647	74.161988	63.097806
1839.766936	72.605961	63.102810
1838.920810	62.799655	63.107815
1838.157154	70.505639	63.112820
1837.443476	68.433372	63.117825
1836.117408	66.709066	63.122830
1835.873949	70.076468	63.127834
1835.544364	61.482762	63.132839
1835.183182	72.770574	63.137844
1834.402275	67.454313	63.142849
1833.179416	74.244513	63.147854
1833.049216	59.042005	63.152858
1831.984392	72.116183	63.157863
1831.062923	70.165217	63.162868
1830.661141	73.316497	63.167873
1830.297139	75.832607	63.172878
1830.016133	61.456672	63.177882
1828.535391	73.366931	63.182887
1828.219026	62.809494	63.187892
1827.718732	59.099669	63.192897
1826.227928	65.142400	63.197902
1825.522603	58.592067	63.202906
1825.110070	71.835471	63.207911
1824.736462	66.534962	63.212916
1824.690546	59.867309	63.217921
1823.685251	66.813764	63.222926
1822.969925	67.971202	63.227930
1822.069992	73.910654	63.232935
1821.617203	65.434278	63.237940
1821.063596	60.431999	63.242945
1819.823585	68.503769	63.247950
1819.277731	74.158352	63.252954
1818.697282	70.653632	63.257959
1818.276627	68.864409	63.262964
1817.495903	65.899246	63.267969
1816.480045	71.511771	63.272974
1816.157934	65.969709	63.277978
1815.710141	64.880198	63.282983
1815.226288	66.805088	63.287988
1814.483383	63.788192	63.292993
1813.857112	64.431622	63.297998
1812.828476	54.613316	63.303002
1812.100442	67.646631	63.308007
1811.247310	64.353940	63.313012
1810.910351	57.070218	63.318017
1810.203696	63.847835	63.323022
1810.031681	62.900605	63.328026
1808.789323	64.100736	63.333031
1807.874397	63.039675	63.338036
1807.912904	55.967555	63.343041
1807.115951	63.374492	63.348046
1806.555504	56.384866	63.353050
1805.674406	66.285588	63.358055
1804.930403	56.921955	63.363060
1804.743262	60.867010	63.368065
1803.662573	64.092984	63.373070
1802.941960	53.513024	63.378074
1802.315122	55.094786	63.383079
1801.565321	62.006982	63.388084
1800.976119	59.437169	63.393089
1799.940972	72.065118	63.398094
1799.839522	66.215220	63.403098
1799.344939	67.066389	63.408103
1798.403957	59.555326	63.413108
1797.677715	59.410429	63.418113
1796.796471	65.261766	63.423118
1796.661535	64.132039	63.428122
1795.966357	59.846072	63.433127
1794.737290	63.483522	63.438132
1794.392214	68.559048	63.443137
1793.968365	64.256800	63.448142
1793.698142	52.935152	63.453146
1792.285260	62.103500	63.458151
1791.771307	63.735145	63.463156
1791.461294	61.092615	63.468161
1789.964327	70.211247	63.473166
1789.782185	64.746306	63.478170
1789.171098	54.366567	63.483175
1788.811992	72.012000	63.488180
1788.479060	65.549190	63.493185
1787.327894	66.299633	63.498190
1786.472511	60.427545	63.503194
1785.334898	61.809739	63.508199
1784.288193	83.416678	63.513204
1784.074878	59.278615	63.518209
1783.344487	58.069992	63.523214
1783.386756	66.431708	63.528218
1783.369983	69.108713	63.533223
1782.682293	64.769522	63.538228
1781.855770	57.498898	63.543233
1780.428055	72.529272	63.548238
1779.453102	58.228864	63.553242
1778.723174	67.548950	63.558247
1778.335358	75.258338	63.563252
1778.337896	68.575107	63.568257
1777.492295	70.349303	63.573262
1776.531827	57.762235	63.578266
1775.718904	64.761729	63.583271
1775.124574	65.150950	63.588276
1774.875155	57.186317	63.593281
1773.793107	63.438535	63.598286
1772.940769	61.161239	63.603290
1772.946413	72.778709	63.608295
1772.241989	69.621680	63.613300
1771.265504	52.754374	63.618305
1770.164301	73.149456	63.623310
1769.697387	63.945245	63.628314
1769.265008	65.218605	63.633319
1768.994356	58.974558	63.638324
1768.429723	50.473391	63.643329
1767.625097	69.220845	63.648334
1766.968618	73.048061	63.653338
1765.757502	71.009083	63.658343
1764.852097	71.488707	63.663348
1764.383528	66.062948	63.668353
1763.804838	73.293319	63.673358
1763.645808	70.167944	63.678362
1763.143352	66.974113	63.683367
1761.956435	78.060345	63.688372
1761.483493	63.732253	63.693377
1761.075072	77.239924	63.698382
1759.904393	73.075208	63.703386
1758.941547	72.978936	63.708391
1758.535233	68.382189	63.713396
1758.147554	69.749371	63.718401
1757.546272	70.213813	63.723406
1757.077330	72.230958	63.728410
1756.469366	79.095416	63.733415
1755.895273	70.083260	63.738420
1754.512757	57.438657	63.743425
1753.523833	73.285558	63.748430
1753.306941	74.537313	63.753434
1752.796638	70.854322	63.758439
1752.627167	68.025483	63.763444
1751.579638	68.861979	63.768449
1750.605304	72.580414	63.773454
1750.222906	72.817717	63.778458
1750.097858	72.315595	63.783463
1748.906899	77.878686	63.788468
1748.503452	68.982927	63.793473
1747.480962	71.094292	63.798478
1746.431790	68.261668	63.803482
1745.701321	74.306685	63.808487
1745.044995	70.594850	63.813492
1745.078065	59.303884	63.818497
1744.629097	74.014837	63.823502
1743.709967	68.764713	63.828506
1742.814409	70.080100	63.833511
1742.241027	72.509629	63.838516
1741.895443	54.302718	63.843521
1740.884395	67.125537	63.848526
1740.363597	63.248685	63.853530
1739.724042	75.815403	63.858535
1738.946404	77.539396	63.863540
1738.153637	68.000609	63.868545
1737.024681	82.966216	63.873550
1737.029338	74.316286	63.878554
1736.388927	65.824002	63.883559
1735.863290	58.114544	63.888564
1735.219333	70.544769	63.893569
1734.156644	71.546098	63.898574
1734.115704	74.171750	63.903578
1733.070235	74.582171	63.908583
1732.306059	70.261449	63.913588
1731.759236	66.081242	63.918593
1730.936248	77.530709	63.923598
1730.028177	76.172133	63.928602
1729.342483	78.529622	63.933607
1728.747660	81.205399	63.938612
1728.372661	90.212107	63.943617
1727.807007	78.535272	63.948622
1727.755118	63.564760	63.953626
1726.609051	73.499703	63.958631
1725.767950	68.926287	63.963636
1725.301508	67.935944	63.968641
1724.196925	75.962592	63.973646
1723.508400	74.572303	63.978650
1723.270510	59.226082	63.983655
1722.535472	59.941999	63.988660
1721.643497	63.492827	63.993665
1720.642567	67.418911	63.998670
1720.048216	75.649937	64.003674
1720.174701	69.503659	64.008679
1719.148546	70.021399	64.013684
1718.583139	62.378182	64.018689
1717.748304	79.460545	64.023694
1717.048725	70.004731	64.028698
1716.863476	65.041739	64.033703
1715.841465	64.287863	64.038708
1715.300142	63.683133	64.043713
1714.761384	69.137916	64.048718
1714.016572	66.085086	64.053722
1713.015903	59.130715	64.058727
1712.190441	73.871507	64.063732
1712.195026	58.494661	64.068737
1711.002609	72.346035	64.073742
1710.158144	63.066196	64.078746
1709.902604	67.660753	64.083751
1709.269096	72.515607	64.088756
1709.237690	58.841194	64.093761
1707.800782	69.019443	64.098766
1707.100739	67.178427	64.103770
1706.841843	58.221881	64.108775
1705.748123	66.789249	64.113780
1705.248987	61.986495	64.118785
1704.339394	68.157735	64.123790
1703.929252	68.360030	64.128794
1703.757550	60.920777	64.133799
1702.636404	66.952162	64.138804
1702.495134	66.854722	64.143809
1701.374414	67.284992	64.148814
1700.290692	63.876010	64.153818
1699.752601	55.977741	64.158823
1699.238372	63.510098	64.163828
1698.755166	66.923471	64.168833
1697.991714	64.895420	64.173838
1697.119368	68.149841	64.178842
1696.336032	73.891045	64.183847
1696.071255	67.038978	64.188852
1696.008178	74.012429	64.193857
1694.522466	73.822620	64.198862
1693.742646	67.422926	64.203866
1693.163473	67.741952	64.208871
1692.984016	76.424296	64.213876
1692.336858	64.167527	64.218881
1691.362774	78.690671	64.223886
1690.758374	71.883086	64.228890
1690.602667	65.092541	64.233895
1689.178803	63.251388	64.238900
1688.592024	65.181610	64.243905
1687.561147	73.822580	64.248910
1687.644539	73.891295	64.253914
1687.130268	74.718805	64.258919
1685.450162	71.549629	64.263924
1685.143015	65.543191	64.268929
1684.949201	72.379719	64.273934
1684.546380	67.167452	64.278938
1683.332789	68.090274	64.283943
1682.638291	69.838921	64.288948
1682.549436	76.108451	64.293953
1681.800606	69.459422	64.298958
1680.701078	69.099476	64.303962
1680.275876	72.339645	64.308967
1679.705874	74.382316	64.313972
1678.783505	68.470447	64.318977
1677.838938	70.723994	64.323982
1676.820880	71.246772	64.328986
1676.497275	62.865028	64.333991
1676.253167	71.357375	64.338996
1676.149677	56.311502	64.344001
1674.779640	61.991366	64.349006
1674.348776	71.352274	64.354010
1674.050956	63.056316	64.359015
1672.932132	71.520458	64.364020
1672.288390	69.142256	64.369025
1671.570831	66.767896	64.374030
1670.991660	72.815702	64.379034
1669.992765	60.534396	64.384039
1669.402917	73.448019	64.389044
1668.992497	68.632757	64.394049
1668.499818	72.886537	64.399054
1667.669719	70.191026	64.404058
1667.059242	62.182842	64.409063
1666.123164	79.032148	64.414068
1665.876191	68.903670	64.419073
1664.867938	74.584420	64.424078
1664.158965	66.714876	64.429082
1663.573285	72.107739	64.434087
1663.068319	75.745338	64.439092
1662.629842	71.841235	64.444097
1661.727975	73.558176	64.449102
1661.332825	72.979122	64.454106
1660.588446	65.971445	64.459111
1658.944319	76.491704	64.464116
1658.256737	66.701288	64.469121
1657.766446	72.364413	64.474126
1657.136430	65.447376	64.479130
1656.954937	64.235172	64.484135
1656.441587	71.912471	64.489140
1656.499770	63.552081	64.494145
1655.199472	70.718907	64.499150
1654.298055	72.446817	64.504154
1654.078642	65.943925	64.509159
1652.992881	66.177861	64.514164
1652.307737	71.998089	64.519169
1651.769101	70.175601	64.524174
1651.376535	67.588780	64.529178
1650.849063	57.555331	64.534183
1649.211083	70.737949	64.539188
1649.465646	59.303004	64.544193
1648.582744	70.929147	64.549198
1647.762182	70.736201	64.554202
1646.770260	61.809381	64.559207
1646.198321	67.613202	64.564212
1645.989170	64.219849	64.569217
1645.361427	68.228595	64.574222
1644.028773	61.208727	64.579226
1643.763290	73.594611	64.584231
1642.806378	68.818861	64.589236
1642.966686	64.127397	64.594241
1642.136613	79.015586	64.599246
1640.892381	75.979038	64.604250
1640.670295	63.621650	64.609255
1639.747962	66.120822	64.614260
1639.465778	65.929082	64.619265
1638.208075	65.324636	64.624270
1637.684507	63.118156	64.629274
1637.499750	64.404235	64.634279
1636.775668	70.941819	64.639284
1635.763289	62.690001	64.644289
1634.782064	63.776194	64.649294
1634.560599	67.884396	64.654298
1634.490516	56.936243	64.659303
1633.094784	67.998915	64.664308
1632.213613	66.598257	64.669313
1631.707522	68.383215	64.674318
1631.795980	68.179902	64.679322
1631.024549	63.265889	64.684327
1630.172176	65.459077	64.689332
1629.510599	64.934967	64.694337
1628.890677	63.415542	64.699342
1627.866511	68.141669	64.704346
1627.346032	64.419327	64.709351
1626.852105	65.193157	64.714356
1625.779090	63.826132	64.719361
1624.986251	72.143891	64.724366
1624.319119	66.405953	64.729370
1624.169863	66.726079	64.734375
1623.547452	70.879055	64.739380
1623.001798	66.815379	64.744385
1622.009710	72.692259	64.749390
1621.323446	73.605449	64.754394
1620.622907	61.987938	64.759399
1619.556950	66.769590	64.764404
1619.099089	65.114041	64.769409
1618.614311	71.946332	64.774414
1618.073215	61.626488	64.779418
1617.889874	66.395650	64.784423
1617.044995	69.156901	64.789428
1616.207123	65.656863	64.794433
1615.483074	69.204701	64.799438
1614.721300	64.081013	64.804442
1614.512118	60.805934	64.809447
1613.404483	61.108013	64.814452
1613.123045	67.939537	64.819457
1612.022524	77.353225	64.824462
1611.017689	68.502582	64.829466
1610.944986	59.060759	64.834471
1610.411319	62.994644	64.839476
1609.688286	56.973874	64.844481
1608.718012	69.690907	64.849486
1607.979229	69.537018	64.854490
1607.909171	51.120812	64.859495
1606.716267	60.210140	64.864500
1605.954671	58.615464	64.869505
1605.533809	63.073871	64.874510
1605.223517	62.099742	64.879514
1604.213553	71.030711	64.884519
1603.369784	74.099281	64.889524
1602.855490	64.249820	64.894529
1602.407996	59.390005	64.899534
1601.449499	65.517005	64.904538
1600.962367	65.449288	64.909543
1600.206481	70.156456	64.914548
1599.907076	63.262603	64.919553
1598.765773	67.551634	64.924558
1597.768739	60.688197	64.929562
1597.492273	62.518677	64.934567
1596.901359	71.293191	64.939572
1596.769541	62.625541	64.944577
1595.880921	62.299929	64.949582
1594.841941	66.236832	64.954586
1594.585684	59.191055	64.959591
1593.544985	73.819411	64.964596
1592.582404	60.144729	64.969601
1592.242919	68.048286	64.974606
1591.634697	67.684435	64.979610
1591.561647	60.647396	64.984615
1590.108167	71.049092	64.989620
1589.628368	64.276937	64.994625
1589.131135	64.672849	64.999630
1587.962526	68.862150	65.004634
1587.551923	64.067435	65.009639
1586.819450	67.563003	65.014644
1586.200102	56.768352	65.019649
1585.919452	60.004488	65.024654
1585.259971	49.788622	65.029658
1584.649029	61.041996	65.034663
1583.453790	63.412667	65.039668
1583.374305	53.092036	65.044673
1582.598265	63.018690	65.049678
1581.523937	62.913389	65.054682
1581.263177	54.655720	65.059687
1580.452274	55.326961	65.064692
1579.776027	63.723967	65.069697
1578.923126	55.391652	65.074702
1578.136374	66.062716	65.079706
1578.005566	58.997011	65.084711
1577.435788	61.328232	65.089716
1576.337112	52.845744	65.094721
1575.805334	66.535422	65.099726
1575.226137	62.040296	65.104730
1574.904167	50.920876	65.109735
1573.508641	63.807973	65.114740
1573.008102	60.607575	65.119745
1572.521451	57.477507	65.124750
1572.052797	56.884916	65.129754
1571.422435	53.564805	65.134759
1570.317410	64.709038	65.139764
1570.092770	63.845877	65.144769
1568.805642	53.508976	65.149774
1568.042303	62.940054	65.154778
1567.796863	58.828695	65.159783
1567.127647	66.598570	65.164788
1567.186061	62.804766	65.169793
1566.041767	62.095609	65.174798
1564.871673	63.859929	65.179802
1564.813789	61.185258	65.184807
1564.312191	55.288585	65.189812
1563.169238	59.413896	65.194817
1562.423795	60.401154	65.199822
1561.793121	66.312086	65.204826
1561.713307	66.444573	65.209831
1560.705249	65.510356	65.214836
1560.133476	64.762272	65.219841
1559.342024	60.983659	65.224846
1558.338905	69.355341	65.229850
1557.743711	65.616503	65.234855
1557.002372	62.913237	65.239860
1556.660636	61.940957	65.244865
1556.313886	59.253840	65.249870
1555.310791	60.792944	65.254874
1554.660602	57.206342	65.259879
1554.102247	62.241659	65.264884
1553.687201	53.155424	65.269889
1552.555575	56.391162	65.274894
1551.648863	59.070797	65.279898
1551.514156	62.917648	65.284903
1550.970903	67.439662	65.289908
1550.150531	63.477999	65.294913
1549.273335	67.400250	65.299918
1548.807280	72.301064	65.304922
1548.457951	57.409390	65.309927
1547.133815	67.443641	65.314932
1546.409060	68.255738	65.319937
1545.879873	58.943223	65.324942
1545.225850	71.788209	65.329946
1545.356704	67.481448	65.334951
1543.992115	71.186271	65.339956
1543.445137	62.772243	65.344961
1543.008654	67.591090	65.349966
1541.598483	68.384371	65.354970
1540.965277	60.271037	65.359975
1540.301057	61.906104	65.364980
1540.168004	59.538253	65.369985
1539.757646	67.002088	65.374990
1539.084282	67.602606	65.379994
1538.377962	60.409166	65.384999
1537.773425	74.681242	65.390004
1537.371486	65.053632	65.395009
1535.928703	56.994827	65.400014
1535.119212	69.582256	65.405018
1535.259715	56.850332	65.410023
1534.548426	75.217152	65.415028
1533.623141	63.383087	65.420033
1532.795407	67.628626	65.425038
1532.319541	78.786444	65.430042
1531.691510	63.516453	65.435047
1530.417864	69.294605	65.440052
1530.061231	72.369365	65.445057
1529.370286	68.642595	65.450062
1528.940605	63.221754	65.455066
1528.733266	59.213149	65.460071
1527.652277	66.725204	65.465076
1527.395043	61.969207	65.470081
1526.423446	62.651808	65.475086
1524.998467	68.755191	65.480090
1524.911400	61.288324	65.485095
1524.550259	68.731726	65.490100
1524.220096	70.206489	65.495105
1523.167375	71.561113	65.500110
1522.242694	60.168484	65.505114
1521.575967	62.013677	65.510119
1520.341669	64.794260	65.515124
1519.981600	60.079836	65.520129
1519.387630	60.320831	65.525134
1518.841524	67.490866	65.530138
1518.618482	60.608549	65.535143
1517.938625	72.442140	65.540148
1516.845305	70.833973	65.545153
1516.423255	72.529908	65.550158
1515.755851	71.096900	65.555162
1515.246633	56.534980	65.560167
1514.608817	59.931948	65.565172
1513.579855	55.809492	65.570177
1513.381030	65.623939	65.575182
1511.980641	72.530779	65.580186
1511.426284	55.628076	65.585191
1511.138500	56.244596	65.590196
1510.888504	66.636424	65.595201
1509.980969	64.145653	65.600206
1508.919492	60.931910	65.605210
1508.534455	60.578342	65.610215
1507.962108	74.678156	65.615220
1507.128935	78.085675	65.620225
1506.209069	63.283094	65.625230
1505.550910	63.433373	65.630234
1505.437526	58.621408	65.635239
1504.342147	72.072668	65.640244
1503.521715	68.620359	65.645249
1503.288612	60.883403	65.650254
1502.644193	71.886662	65.655258
1501.894344	67.626819	65.660263
1500.806763	74.269503	65.665268
1500.198873	65.936125	65.670273
1500.137584	64.739523	65.675278
1499.401110	72.505910	65.680282
1498.742796	61.148229	65.685287
1497.955122	63.343790	65.690292
1497.373732	73.212728	65.695297
1496.260980	70.882299	65.700302
1495.470547	74.797087	65.705306
1495.191552	67.731284	65.710311
1494.654209	70.454739	65.715316
1494.156916	72.694039	65.720321
1493.490666	70.295810	65.725326
1492.351786	71.607371	65.730330
1492.179136	69.111781	65.735335
1491.522333	67.927817	65.740340
1490.695269	60.985382	65.745345
1489.932221	63.170724	65.750350
1489.150485	84.989481	65.755354
1488.761422	74.684931	65.760359
1487.800291	79.774810	65.765364
1487.398720	81.603106	65.770369
1487.035371	61.510005	65.775374
1485.986485	70.510268	65.780378
1485.349582	65.901339	65.785383
1484.704339	74.553624	65.790388
1484.134536	66.329310	65.795393
1483.251237	63.992384	65.800398
1482.445455	67.695160	65.805402
1482.276505	61.472844	65.810407
1481.591688	61.231572	65.815412
1480.404936	64.487139	65.820417
1479.900411	61.006713	65.825422
1479.360519	68.301915	65.830426
1479.213377	52.001530	65.835431
1477.712664	61.273856	65.840436
1477.044693	62.843305	65.845441
1476.680061	56.527518	65.850446
1475.838749	65.723439	65.855450
1475.892469	66.503299	65.860455
1474.790440	74.865498	65.865460
1474.087086	63.675823	65.870465
1473.981659	54.915698	65.875470
1472.397074	61.052352	65.880474
1471.791352	60.172496	65.885479
1470.947515	73.238457	65.890484
1470.266915	61.728219	65.895489
1470.339213	68.481455	65.900494
1469.933264	72.675751	65.905498
1469.047605	72.808581	65.910503
1468.480194	64.781001	65.915508
1467.711553	54.528910	65.920513
1466.350929	60.201067	65.925518
1465.740649	67.507456	65.930522
1465.348607	59.956608	65.935527
1464.861271	75.186144	65.940532
1464.762892	71.269032	65.945537
1463.845588	62.940689	65.950542
1462.742068	61.919186	65.955546
1462.300304	72.637945	65.960551
1461.247132	69.180064	65.965556
1460.340297	71.702063	65.970561
1460.205258	66.256486	65.975566
1459.695838	76.508210	65.980570
1459.341720	73.563670	65.985575
1458.093169	74.578879	65.990580
1457.476722	78.876014	65.995585
1457.178392	71.444302	66.000590
1456.044956	70.541090	66.005594
1455.329209	63.383868	66.010599
1454.722732	63.760900	66.015604
1454.250593	78.354124	66.020609
1454.039360	71.730119	66.025614
1453.116054	77.567740	66.030618
1452.543154	76.714209	66.035623
1451.989371	81.020308	66.040628
1450.806915	75.667081	66.045633
1449.749508	67.591231	66.050638
1449.353348	70.691203	66.055642
1448.942140	73.639034	66.060647
1448.750449	62.853727	66.065652
1447.958339	69.717536	66.070657
1447.359736	69.998705	66.075662
1446.593423	69.425061	66.080666
1445.516530	63.626155	66.085671
1444.644481	66.327124	66.090676
1443.776093	70.314236	66.095681
1443.779483	64.206452	66.100686
1443.014856	72.275352	66.105690
1442.810681	60.566410	66.110695
1441.950985	58.843881	66.115700
1441.550257	63.316453	66.120705
1440.656919	66.673629	66.125710
1439.662706	79.586892	66.130714
1438.979309	66.966991	66.135719
1438.581475	65.825457	66.140724
1437.355826	65.298012	66.145729
1436.905030	65.010097	66.150734
1436.103387	74.633366	66.155738
1435.811601	64.180920	66.160743
1435.742727	66.454634	66.165748
1434.207424	63.712025	66.170753
1433.734004	62.981452	66.175758
1433.136501	80.918640	66.180762
1432.780426	68.636203	66.185767
1431.818275	67.171221	66.190772
1430.702853	84.567867	66.195777
1430.846512	67.524282	66.200782
1429.935098	70.461735	66.205786
1428.807834	75.429810	66.210791
1428.323400	71.566175	66.215796
1427.867629	70.798108	66.220801
1427.471727	70.499892	66.225806
1426.597648	73.965971	66.230810
1426.150187	71.778978	66.235815
1425.476501	78.040533	66.240820
1424.649675	76.918301	66.245825
1424.057264	64.249255	66.250830
1423.386065	68.618170	66.255834
1422.755700	58.880252	66.260839
1421.509276	75.777345	66.265844
1420.875240	72.235518	66.270849
1420.624683	53.324522	66.275854
1419.703871	66.260802	66.280858
1419.583961	70.206224	66.285863
1418.797334	74.593488	66.290868
1417.900739	67.602209	66.295873
1417.549248	63.939786	66.300878
1416.793896	69.336004	66.305882
1415.792409	68.719327	66.310887
1414.898057	63.320331	66.315892
1414.817973	64.608708	66.320897
1414.244841	58.144734	66.325902
1413.029843	69.713329	66.330906
1412.298684	65.160402	66.335911
1412.204627	64.054163	66.340916
1411.382777	72.256737	66.345921
1410.816119	65.928918	66.350926
1409.845183	69.322091	66.355930
1409.386139	72.983968	66.360935
1409.048861	62.084622	66.365940
1408.093132	67.883253	66.370945
1407.414289	67.825545	66.375950
1406.587636	67.844944	66.380954
1406.176456	65.980178	66.385959
1405.227678	70.579288	66.390964
1404.450658	66.115650	66.395969
1404.374705	64.875654	66.400974
1403.385488	83.632003	66.405978
1402.895912	61.647832	66.410983
1401.933765	73.513693	66.415988
1401.200062	73.523050	66.420993
1400.956076	62.077473	66.425998
1400.136894	68.819446	66.431002
1399.432751	74.906082	66.436007
1399.181498	75.715493	66.441012
1398.507341	65.524094	66.446017
1397.790313	68.821723	66.451022
1396.591591	70.830350	66.456026
1396.216144	54.558388	66.461031
1395.634742	69.422847	66.466036
1394.236266	70.879786	66.471041
1394.006088	54.034407	66.476046
1393.615305	68.450697	66.481050
1393.128582	59.560387	66.486055
1392.599192	60.751457	66.491060
1391.359888	64.786503	66.496065
1391.049257	56.987780	66.501070
1389.961347	64.814776	66.506074
1389.094689	60.496274	66.511079
1388.914169	70.120163	66.516084
1388.128997	71.944794	66.521089
1388.004727	62.074404	66.526094
1386.802555	65.717217	66.531098
1386.143096	66.211490	66.536103
1385.490026	69.432726	66.541108
1385.053769	64.113882	66.546113
1384.776355	67.395248	66.551118
1383.680874	72.506513	66.556122
1383.166477	57.235873	66.561127
1382.508477	71.667835	66.566132
1381.468250	66.255771	66.571137
1381.164671	54.627300	66.576142
1380.459268	72.688857	66.581146
1379.577795	69.205296	66.586151
1378.821758	62.929667	66.591156
1377.871544	73.087469	66.596161
1377.788406	62.292805	66.601166
1377.180507	58.516616	66.606170
1376.105547	61.148940	66.611175
1375.686297	60.487034	66.616180
1374.703229	68.374639	66.621185
1374.711637	65.825049	66.626190
1373.758585	72.265052	66.631194
1373.174003	73.486977	66.636199
1372.284600	70.928723	66.641204
1371.808589	68.862968	66.646209
1370.582458	65.620269	66.651214
1369.680589	65.853475	66.656218
1369.382350	61.674846	66.661223
1369.232403	64.694690	66.666228
1368.522315	64.525270	66.671233
1368.250984	66.700287	66.676238
1367.082865	69.847291	66.681242
1366.601194	73.905410	66.686247
1366.377565	65.190890	66.691252
1365.052547	68.011194	66.696257
1364.557958	64.994390	66.701262
1363.826791	71.999911	66.706266
1362.751348	76.759512	66.711271
1362.313437	67.235431	66.716276
1361.463411	76.417001	66.721281
1361.514091	69.956369	66.726286
1360.704033	77.483761	66.731290
1359.902218	78.109474	66.736295
1359.349241	72.451238	66.741300
1358.587583	76.101306	66.746305
1357.562000	66.132934	66.751310
1356.930200	62.127174	66.756314
1356.658214	75.247324	66.761319
1356.292648	61.531474	66.766324
1355.114558	73.739164	66.771329
1354.282470	60.767645	66.776334
1353.585452	67.569051	66.781338
1353.288858	73.969358	66.786343
1353.317618	66.618129	66.791348
1351.841299	69.498760	66.796353
1351.390237	66.935484	66.801358
1351.050038	69.979266	66.806362
1350.033044	74.359016	66.811367
1349.233067	71.053312	66.816372
1348.518684	70.107186	66.821377
1348.245431	66.575833	66.826382
1346.963909	68.845213	66.831386
1346.324398	73.497675	66.836391
1346.409231	61.774346	66.841396
1345.204024	73.661515	66.846401
1344.120560	67.237686	66.851406
1343.557882	67.696085	66.856410
1343.291125	62.394457	66.861415
1342.877353	63.502506	66.866420
1342.247730	69.318699	66.871425
1341.465287	54.391871	66.876430
1340.661311	70.857544	66.881434
1340.017820	64.226587	66.886439
1339.129072	65.337609	66.891444
1338.491852	59.134566	66.896449
1338.094873	67.673289	66.901454
1337.616621	67.943236	66.906458
1336.664522	66.505077	66.911463
1336.131334	57.040308	66.916468
1335.344402	67.563221	66.921473
1335.070814	64.577519	66.926478
1333.929914	62.858733	66.931482
1332.849346	71.395751	66.936487
1332.777588	65.098083	66.941492
1332.180148	65.610893	66.946497
1331.744964	60.780720	66.951502
1330.628270	69.534781	66.956506
1329.853337	65.643240	66.961511
1329.577563	61.648693	66.966516
1328.934738	72.681682	66.971521
1328.224875	65.667063	66.976526
1327.346459	67.353579	66.981530
1326.937827	65.704453	66.986535
1326.325265	62.514036	66.991540
1325.017156	61.988717	66.996545
1324.618710	61.031793	67.001550
1324.187236	65.491920	67.006554
1323.733615	73.140838	67.011559
1322.775112	62.956830	67.016564
1321.718072	73.164743	67.021569
1321.762728	63.414155	67.026574
1321.155567	66.331656	67.031578
1320.120855	63.799678	67.036583
1319.486585	69.375353	67.041588
1318.708970	71.501561	67.046593
1318.701716	62.929261	67.051598
1317.509793	64.348671	67.056602
1316.623074	69.422041	67.061607
1316.236088	62.912730	67.066612
1315.615529	72.530887	67.071617
1315.089523	65.324626	67.076622
1314.137642	67.510077	67.081626
1313.659029	69.691247	67.086631
1313.387628	59.738611	67.091636
1311.980388	65.815623	67.096641
1311.510848	68.515716	67.101646
1310.874177	75.928825	67.106650
1310.549151	63.570531	67.111655
1309.987779	68.453413	67.116660
1308.807342	69.317522	67.121665
1308.299487	58.817463	67.126670
1307.939721	63.158964	67.131674
1306.821864	54.753778	67.136679
1305.983304	58.230011	67.141684
1305.175053	56.072022	67.146689
1305.160415	63.028284	67.151694
1304.743694	57.621203	67.156698
1303.578665	64.952739	67.161703
1303.163436	59.152783	67.166708
1302.291202	62.248040	67.171713
1301.870380	67.406605	67.176718
1300.743864	62.279519	67.181722
1300.082721	59.749656	67.186727
1299.968078	59.584930	67.191732
1299.318832	70.019733	67.196737
1298.446872	65.300006	67.201742
1297.889227	62.132403	67.206746
1297.180211	72.668169	67.211751
1296.489935	70.306930	67.216756
1295.460364	65.844062	67.221761
1295.081436	60.848843	67.226766
1294.635851	62.662085	67.231770
1293.876817	62.254477	67.236775
1293.277539	62.086383	67.241780
1292.272509	61.993839	67.246785
1292.073576	61.900858	67.251790
1291.053448	64.248546	67.256794
1290.237620	71.844674	67.261799
1289.939378	56.159679	67.266804
1289.335926	60.483158	67.271809
1288.551421	58.434932	67.276814
1287.389044	62.574480	67.281818
1286.921603	60.980440	67.286823
1286.623522	67.988076	67.291828
1286.139244	66.503940	67.296833
1284.972909	53.125159	67.301838
1284.408360	62.360691	67.306842
1283.879127	58.983582	67.311847
1283.578329	47.192282	67.316852
1282.217399	70.925972	67.321857
1281.572009	65.728706	67.326862
1281.217942	62.161330	67.331866
1280.749279	52.536521	67.336871
1280.305672	65.054778	67.341876
1279.044483	56.677124	67.346881
1278.763530	58.825294	67.351886
1278.174874	69.925364	67.356890
1277.070585	63.014476	67.361895
1276.493237	56.992734	67.366900
1275.925839	63.161722	67.371905
1275.355454	60.847657	67.376910
1274.242724	63.662635	67.381914
1273.598506	55.506992	67.386919
1273.206558	50.505967	67.391924
1272.715442	64.409956	67.396929
1272.772875	60.062835	67.401934
1271.304208	61.324429	67.406938
1270.895080	60.678277	67.411943
1270.318526	67.742805	67.416948
1269.117740	70.212262	67.421953
1268.594657	64.423152	67.426958
1268.345471	70.513165	67.431962
1267.383607	70.964092	67.436967
1266.427793	59.781530	67.441972
1265.807625	54.892482	67.446977
1265.463950	63.520497	67.451982
1265.053940	71.052105	67.456986
1263.908183	62.078971	67.461991
1263.275938	63.116119	67.466996
1262.922328	65.122888	67.472001
1262.394198	62.679112	67.477006
1261.271104	69.582976	67.482010
1260.263618	72.945744	67.487015
1260.228832	64.587549	67.492020
1259.502575	64.365541	67.497025
1258.904463	55.843047	67.502030
1257.909598	62.411147	67.507034
1257.130171	62.232285	67.512039
1257.173265	61.635649	67.517044
1256.021349	67.050806	67.522049
1255.444788	58.731454	67.527054
1254.744839	68.245552	67.532058
1254.231153	65.648102	67.537063
1253.609132	61.172488	67.542068
1252.573187	63.754504	67.547073
1252.372599	55.105730	67.552078
1252.076262	65.158010	67.557082
1250.643930	65.593870	67.562087
1250.319710	55.950830	67.567092
1249.571516	64.886004	67.572097
1248.827782	64.591088	67.577102
1247.907190	70.237535	67.582106
1247.082502	63.146593	67.587111
1246.598900	62.088111	67.592116
1246.325039	67.836714	67.597121
1245.798540	56.204299	67.602126
1245.097070	53.849589	67.607130
1243.777447	58.927160	67.612135
1243.768438	56.121740	67.617140
1243.520999	51.578685	67.622145
1242.467903	53.627298	67.627150
1241.319496	60.106283	67.632154
1241.092677	63.970937	67.637159
1240.484643	58.835552	67.642164
1239.354357	62.041243	67.647169
1238.841223	64.267335	67.652174
1238.387171	68.034090	67.657178
1237.397987	54.447405	67.662183
1236.843494	46.260167	67.667188
1236.149558	74.679898	67.672193
1236.009095	51.776179	67.677198
1235.161892	64.041664	67.682202
1234.561748	63.096329	67.687207
1234.119929	50.826019	67.692212
1233.012353	68.013299	67.697217
1232.060640	70.801115	67.702222
1231.757500	52.822582	67.707226
1230.961871	62.550578	67.712231
1230.541786	74.352362	67.717236
1229.767540	58.504967	67.722241
1228.960842	63.963004	67.727246
1228.895200	65.827797	67.732250
1227.786233	58.553425	67.737255
1227.104810	74.274272	67.742260
1225.910249	53.017272	67.747265
1226.144807	47.216506	67.752270
1224.969380	73.163015	67.757274
1223.934154	72.504473	67.762279
1223.552667	41.338491	67.767284
1222.972085	75.241866	67.772289
1222.746535	59.889083	67.777294
1222.190203	57.673716	67.782298
1221.135317	67.015615	67.787303
1220.813532	51.932019	67.792308
1219.764384	65.603068	67.797313
1218.689377	63.344032	67.802318
1218.140300	61.930135	67.807322
1217.864715	72.852704	67.812327
1217.561285	57.840296	67.817332
1216.153189	69.166868	67.822337
1215.323238	61.050239	67.827342
1214.913538	55.329844	67.832346
1214.219938	63.584600	67.837351
1214.389088	58.387131	67.842356
1213.362188	68.148759	67.847361
1212.399515	64.832708	67.852366
1212.008248	57.207685	67.857370
1211.560396	59.144295	67.862375
1210.766796	48.014818	67.867380
1209.824732	61.804447	67.872385
1209.628852	57.267389	67.877390
1208.536878	56.064400	67.882394
1207.461272	64.137069	67.887399
1207.226119	59.656715	67.892404
1206.732194	54.015945	67.897409
1205.980493	61.808459	67.902414
1205.434843	54.658972	67.907418
1204.579829	56.748636	67.912423
1204.349901	50.553405	67.917428
1203.082358	54.099463	67.922433
1202.109760	52.306670	67.927438
1201.857466	62.047610	67.932442
1201.148981	55.799178	67.937447
1200.969808	47.020863	67.942452
1199.853396	56.323663	67.947457
1199.187501	63.585323	67.952462
1198.870388	63.794979	67.957466
1198.560223	65.244521	67.962471
1197.545654	49.069537	67.967476
1196.454656	70.065466	67.972481
1195.923884	59.007724	67.977486
1195.521904	56.540750	67.982490
1193.887723	57.803479	67.987495
1193.809312	44.363707	67.992500
1193.375713	58.233316	67.997505
1193.089333	60.197863	68.002510
1192.460147	49.660376	68.007514
1191.411475	57.981061	68.012519
1191.256539	45.936366	68.017524
1189.893691	68.989179	68.022529
1188.969718	47.534649	68.027534
1188.617972	56.911378	68.032538
1187.853473	72.478291	68.037543
1188.013529	59.339609	68.042548
1186.966245	61.273785	68.047553
1186.420235	54.165360	68.052558
1185.888383	56.567892	68.057562
1184.727134	57.829528	68.062567
1183.941794	51.758896	68.067572
1183.431501	63.614441	68.072577
1183.220373	55.612291	68.077582
1181.802213	52.997861	68.082586
1180.970363	55.504870	68.087591
1181.031106	54.755625	68.092596
1180.381891	59.171553	68.097601
1179.506780	57.893090	68.102606
1178.816303	51.777413	68.107610
1178.044158	68.485610	68.112615
1177.725004	57.622865	68.117620
1176.628614	64.733810	68.122625
1176.261858	69.038592	68.127630
1175.862745	64.171179	68.132634
1174.997438	64.179454	68.137639
1174.492316	55.247984	68.142644
1173.219048	59.837273	68.147649
1172.525092	51.612311	68.152654
1172.263040	53.309654	68.157658
1171.505552	55.913643	68.162663
1170.645214	50.911442	68.167668
1170.022368	68.691814	68.172673
1169.763926	53.162944	68.177678
1169.839672	50.724071	68.182682
1167.991650	69.995475	68.187687
1167.517787	58.936576	68.192692
1167.227056	59.526794	68.197697
1166.335509	46.750902	68.202702
1165.488206	52.384133	68.207706
1164.590826	60.846337	68.212711
1164.443286	54.978610	68.217716
1164.132626	55.437965	68.222721
1162.946638	54.841271	68.227726
1162.512140	59.073252	68.232730
1161.706055	53.672940	68.237735
1161.323663	58.822251	68.242740
1160.127088	61.302123	68.247745
1159.343434	54.747135	68.252750
1158.995291	38.347931	68.257754
1158.477938	59.801366	68.262759
1157.895708	48.315038	68.267764
1156.942678	51.407419	68.272769
1156.593129	47.054074	68.277774
1155.984610	56.220921	68.282778
1155.005809	50.094343	68.287783
1154.291397	60.003390	68.292788
1153.838136	49.373286	68.297793
1153.107575	62.093292	68.302798
1152.245271	49.721161	68.307802
1151.723915	38.278775	68.312807
1151.134995	64.828971	68.317812
1150.653632	55.937881	68.322817
1149.460974	53.861583	68.327822
1149.051937	51.769456	68.332826
1148.327114	70.690352	68.337831
1148.418470	67.485793	68.342836
1147.424208	45.869014	68.347841
1146.632774	69.781805	68.352846
1146.186798	63.627247	68.357850
1145.183098	53.860505	68.362855
1144.244051	67.468335	68.367860
1144.098519	61.687016	68.372865
1143.008566	46.451251	68.377870
1142.189612	73.722407	68.382874
1141.602767	56.955899	68.387879
1141.231176	53.870703	68.392884
1140.650669	70.215708	68.397889
1140.421790	58.263194	68.402894
1139.382822	54.334873	68.407898
1138.487871	65.564091	68.412903
1138.312379	58.764156	68.417908
1137.146950	52.112213	68.422913
1136.095509	68.358664	68.427918
1135.954174	53.137588	68.432922
1135.434424	57.305864	68.437927
1134.461012	51.902217	68.442932
1133.750698	55.763355	68.447937
1133.428890	53.412943	68.452942
1133.061928	54.489925	68.457946
1131.271087	66.473461	68.462951
1130.991758	67.233747	68.467956
1130.665598	62.201785	68.472961
1130.112294	60.917884	68.477966
1129.722127	60.648764	68.482970
1128.687189	68.068479	68.487975
1128.116610	59.547954	68.492980
1127.466925	63.815744	68.497985
1126.332591	55.990404	68.502990
1125.883147	60.760900	68.507994
1125.164152	59.274709	68.512999
1125.048343	53.051878	68.518004
1124.104627	57.848953	68.523009
1123.301142	61.849486	68.528014
1122.770401	54.273477	68.533018
1122.050437	72.846695	68.538023
1121.624595	57.970474	68.543028
1120.266807	70.676724	68.548033
1119.781338	58.889598	68.553038
1119.751614	56.540036	68.558042
1118.893188	56.559851	68.563047
1117.779003	60.398506	68.568052
1117.273302	64.425789	68.573057
1116.489649	54.527871	68.578062
1116.404608	58.016761	68.583066
1115.408403	68.787457	68.588071
1114.701430	60.927260	68.593076
1113.937455	65.795093	68.598081
1113.294706	64.605843	68.603086
1113.094277	51.081415	68.608090
1112.032348	60.597918	68.613095
1111.658753	53.864190	68.618100
1111.057168	58.393974	68.623105
1110.116673	67.738211	68.628110
1109.334803	56.439758	68.633114
1108.865604	63.378428	68.638119
1108.327604	52.034882	68.643124
1107.754778	51.999811	68.648129
1106.743364	46.304196	68.653134
1106.401082	55.269438	68.658138
1105.498107	58.557291	68.663143
1104.579851	56.541440	68.668148
1103.880345	55.399065	68.673153
1103.565221	53.547460	68.678158
1103.528840	53.245723	68.683162
1102.231781	62.079005	68.688167
1101.706478	58.146262	68.693172
1101.078424	62.623491	68.698177
1100.195375	58.050681	68.703182
1099.270782	55.789849	68.708186
1098.239928	69.125305	68.713191
1098.450374	61.168066	68.718196
1098.343608	55.511468	68.723201
1097.355741	58.797059	68.728206
1096.906778	58.031124	68.733210
1095.709456	62.493257	68.738215
1094.861339	56.402683	68.743220
1094.162981	65.353613	68.748225
1092.992680	62.322938	68.753230
1093.640269	56.571576	68.758234
1092.387095	56.599001	68.763239
1091.668224	57.667315	68.768244
1091.040814	72.376697	68.773249
1090.156491	56.218894	68.778254
1088.952034	62.918153	68.783258
1088.184402	66.118256	68.788263
1087.874534	54.501896	68.793268
1087.692935	60.768805	68.798273
1087.304351	57.047693	68.803278
1087.072180	60.739750	68.808282
1085.875285	56.641044	68.813287
1085.074441	60.071921	68.818292
1084.883670	61.059385	68.823297
1083.809244	60.142225	68.828302
1082.874163	62.802872	68.833306
1082.230762	64.059445	68.838311
1082.065866	49.979049	68.843316
1081.161268	50.400436	68.848321
1079.826610	71.356306	68.853326
1079.629293	64.331204	68.858330
1079.228957	62.363853	68.863335
1078.918872	56.676525	68.868340
1077.829213	54.161279	68.873345
1076.671548	69.319264	68.878350
1076.500898	47.264025	68.883354
1076.032340	54.637806	68.888359
1075.203152	49.130823	68.893364
1074.581766	54.825907	68.898369
1073.694714	57.196659	68.903374
1073.482786	62.422935	68.908378
1072.169793	53.758773	68.913383
1071.672899	60.782271	68.918388
1071.419835	47.296190	68.923393
1070.536522	57.023973	68.928398
1070.083350	57.819804	68.933402
1069.373404	66.575475	68.938407
1068.932096	60.538460	68.943412
1067.661828	50.307992	68.948417
1066.886494	45.561954	68.953422
1066.776664	47.679764	68.958426
1066.153396	57.520713	68.963431
1064.877965	50.821657	68.968436
1063.896972	53.954786	68.973441
1063.472310	56.747118	68.978446
1063.405656	60.881173	68.983450
1063.094726	68.283499	68.988455
1062.655822	59.871351	68.993460
1061.584868	44.676766	68.998465
1060.202404	75.254361	69.003470
1060.044518	49.975565	69.008474
1059.164645	60.787684	69.013479
1058.675425	68.008651	69.018484
1058.392592	48.319208	69.023489
1057.380180	55.825238	69.028494
1056.567020	50.951186	69.033498
1055.890854	64.304337	69.038503
1055.609013	49.307473	69.043508
1054.670645	53.529741	69.048513
1053.599987	60.251880	69.053518
1053.372083	47.048789	69.058522
1052.874102	56.439325	69.063527
1052.357118	50.087948	69.068532
1051.294823	49.115260	69.073537
1050.524033	46.284388	69.078542
1050.178065	47.435306	69.083546
1049.239258	53.614527	69.088551
1048.643832	59.124149	69.093556
1048.246322	56.106167	69.098561
1047.437615	64.360343	69.103566
1047.074821	55.759485	69.108570
1045.947887	57.529779	69.113575
1045.535648	50.862136	69.118580
1045.336891	62.795853	69.123585
1044.334008	63.431574	69.128590
1043.473113	70.383686	69.133594
1043.040021	61.921734	69.138599
1041.550960	59.451121	69.143604
1041.037898	43.510245	69.148609
1040.280405	68.866772	69.153614
1040.052138	57.486584	69.158618
1039.724084	59.367894	69.163623
1039.330889	56.655138	69.168628
1038.482482	50.299722	69.173633
1037.586751	63.082291	69.178638
1036.857999	69.042035	69.183642
1035.393616	56.496096	69.188647
1034.989080	64.182956	69.193652
1034.795766	53.047933	69.198657
1034.330165	53.063625	69.203662
1034.132868	52.912061	69.208666
1032.942804	57.103422	69.213671
1032.058951	59.983003	69.218676
1031.681859	55.790170	69.223681
1031.037389	55.938392	69.228686
1030.194894	36.993986	69.233690
1029.535837	51.832959	69.238695
1028.990431	63.321961	69.243700
1028.754543	54.240475	69.248705
1027.521184	58.542799	69.253710
1027.073980	41.235355	69.258714
1026.100893	75.473942	69.263719
1025.188302	50.840320	69.268724
1024.355339	50.904999	69.273729
1024.076862	54.413625	69.278734
1024.073205	58.985484	69.283738
1023.583424	58.585581	69.288743
1022.479116	52.961548	69.293748
1022.108096	47.648183	69.298753
1020.871140	58.110290	69.303758
1020.289702	54.979658	69.308762
1019.166357	51.646679	69.313767
1018.969779	54.150431	69.318772
1018.600361	52.608656	69.323777
1017.762183	63.727948	69.328782
1017.111509	48.638398	69.333786
1016.679065	57.875017	69.338791
1015.787060	60.279690	69.343796
1014.586189	48.309977	69.348801
1013.972460	51.476150	69.353806
1013.891067	56.951301	69.358810
1013.103761	59.058635	69.363815
1012.733207	52.460056	69.368820
1011.651448	67.222805	69.373825
1011.094499	58.585039	69.378830
1010.902215	47.180218	69.383834
1009.592984	62.176260	69.388839
1009.035724	54.024219	69.393844
1008.625147	51.191240	69.398849
1007.747258	52.693283	69.403854
1007.063693	55.358090	69.408858
1006.194375	51.927933	69.413863
1005.724678	54.585520	69.418868
1005.329430	56.370298	69.423873
1004.493324	55.815777	69.428878
1003.908018	59.269150	69.433882
1003.319283	67.923553	69.438887
1002.672018	56.431853	69.443892
1001.638633	53.053031	69.448897
1000.900959	65.400478	69.453902
1000.571326	64.869450	69.458906
1000.099071	65.867013	69.463911
999.315020	66.255059	69.468916
998.148695	55.342657	69.473921
997.359627	66.439950	69.478926
997.615487	51.895257	69.483930
996.834383	58.970291	69.488935
996.056752	63.881324	69.493940
995.806471	55.054431	69.498945
994.322479	60.524101	69.503950
993.318546	60.228085	69.508954
992.695395	58.028136	69.513959
992.705117	61.495642	69.518964
992.309561	51.438264	69.523969
991.244177	65.127724	69.528974
990.407108	59.361842	69.533978
989.553138	58.807016	69.538983
989.409284	56.921869	69.543988
989.090386	56.242486	69.548993
987.880018	60.258912	69.553998
987.598722	59.494703	69.559002
986.858593	61.454199	69.564007
985.881136	69.970194	69.569012
985.123205	57.491648	69.574017
984.463950	63.681603	69.579022
984.647441	49.935281	69.584026
983.667324	56.941062	69.589031
982.511655	58.526733	69.594036
981.905416	59.835760	69.599041
981.485403	68.952147	69.604046
980.178543	60.378519	69.609050
979.422706	63.941028	69.614055
979.136678	57.390503	69.619060
979.259358	57.872387	69.624065
978.283231	67.547161	69.629070
977.691350	57.639285	69.634074
976.818708	58.293731	69.639079
976.026733	65.326349	69.644084
975.437180	61.799651	69.649089
974.614943	65.855246	69.654094
974.278951	56.509016	69.659098
973.607443	73.923431	69.664103
972.782857	67.955306	69.669108
972.092376	51.069756	69.674113
971.198059	66.690460	69.679118
971.109986	64.395915	69.684122
969.933059	58.166910	69.689127
969.496336	69.783700	69.694132
969.015120	68.448943	69.699137
968.217063	63.127843	69.704142
967.294069	48.053262	69.709146
966.449623	58.014568	69.714151
965.966024	55.980068	69.719156
965.798761	61.782677	69.724161
964.797601	68.730321	69.729166
964.214927	64.127112	69.734170
963.556468	63.080742	69.739175
963.049090	61.854223	69.744180
962.523961	57.235553	69.749185
961.548706	57.731300	69.754190
960.680491	52.452908	69.759194
960.048962	71.209172	69.764199
959.382957	61.227944	69.769204
958.920662	50.443226	69.774209
957.898516	54.647320	69.779214
958.244170	57.862685	69.784218
957.295055	63.925314	69.789223
956.283445	57.747276	69.794228
955.955186	54.062320	69.799233
955.074456	54.200850	69.804238
954.049830	57.260542	69.809242
953.112413	53.059120	69.814247
952.848555	52.563361	69.819252
952.720094	47.813773	69.824257
951.444354	47.521604	69.829262
950.813385	48.186484	69.834266
950.138930	62.203229	69.839271
949.467309	47.205346	69.844276
949.245810	49.914905	69.849281
948.601077	55.996903	69.854286
948.069602	43.770916	69.859290
947.164710	43.509618	69.864295
945.942675	50.930773	69.869300
945.530523	47.684921	69.874305
944.744981	52.043745	69.879310
944.692135	52.646593	69.884314
943.704092	53.551210	69.889319
942.929949	50.544299	69.894324
942.425920	43.741489	69.899329
941.973053	55.844933	69.904334
941.704460	40.923267	69.909338
940.175325	45.840360	69.914343
939.613149	48.660897	69.919348
939.429696	55.554111	69.924353
937.990777	57.938612	69.929358
937.311473	53.439095	69.934362
937.154807	46.946840	69.939367
936.663094	49.946964	69.944372
936.089675	54.371378	69.949377
934.906889	57.481475	69.954382
934.288165	52.070357	69.959386
933.621695	44.222713	69.964391
933.261511	49.436312	69.969396
932.728435	51.471676	69.974401
931.835299	55.801898	69.979406
931.690581	47.902761	69.984410
930.806353	51.107266	69.989415
929.487107	67.602949	69.994420
929.281862	56.857750	69.999425
928.543697	56.320783	70.004430
927.925831	42.854950	70.009434
926.899899	54.382577	70.014439
926.477704	63.351086	70.019444
926.495882	57.706160	70.024449
924.791433	52.879380	70.029454
924.250946	59.395777	70.034458
923.791374	52.701003	70.039463
923.328882	45.489488	70.044468
923.025098	46.248956	70.049473
921.514509	57.990900	70.054478
921.375064	53.243062	70.059482
920.762118	72.541964	70.064487
919.928452	65.985560	70.069492
919.053634	52.576380	70.074497
918.525706	77.793896	70.079502
917.930196	55.244944	70.084506
917.541812	61.844364	70.089511
916.355364	55.914929	70.094516
915.811935	52.726241	70.099521
915.283738	59.212299	70.104526
915.144320	58.759815	70.109530
914.154284	54.358638	70.114535
913.310137	61.891551	70.119540
913.094065	62.644947	70.124545
912.048982	65.663760	70.129550
911.377165	54.343150	70.134554
910.895046	53.451648	70.139559
909.654883	56.700189	70.144564
909.117645	51.585175	70.149569
908.028508	62.695544	70.154574
908.024597	45.407474	70.159578
907.588019	51.538349	70.164583
906.958983	56.998153	70.169588
906.230289	47.238231	70.174593
905.192867	57.884656	70.179598
904.976351	48.207217	70.184602
904.236045	54.205091	70.189607
902.854211	47.280228	70.194612
902.826793	47.689806	70.199617
902.162222	54.501901	70.204622
901.552592	41.717547	70.209626
900.479381	50.415941	70.214631
899.772494	56.481034	70.219636
899.685560	46.352493	70.224641
899.008885	63.493350	70.229646
898.586714	52.782682	70.234650
897.639409	62.908601	70.239655
896.995679	54.863391	70.244660
896.435965	46.189841	70.249665
895.196552	55.297865	70.254670
895.009970	54.663665	70.259674
894.415705	60.045404	70.264679
893.114579	50.234668	70.269684
892.407224	51.506194	70.274689
892.327240	60.513276	70.279694
892.001518	53.218502	70.284698
891.400579	52.667592	70.289703
890.473604	55.544620	70.294708
890.106798	54.899681	70.299713
888.815169	62.273596	70.304718
888.071875	55.630292	70.309722
887.639966	55.400967	70.314727
886.794553	54.597247	70.319732
885.766645	47.961399	70.324737
884.920423	60.758194	70.329742
884.462993	55.346650	70.334746
884.081367	60.499019	70.339751
883.779430	52.413610	70.344756
883.647424	51.281900	70.349761
882.610322	57.997180	70.354766
882.008127	49.527501	70.359770
881.063909	51.443816	70.364775
879.821675	60.093433	70.369780
879.580565	53.147873	70.374785
878.948248	68.097731	70.379790
878.384985	61.209746	70.384794
877.389489	59.308770	70.389799
876.766249	65.464632	70.394804
876.368588	51.082302	70.399809
875.984975	64.841470	70.404814
875.300203	59.213812	70.409818
874.122105	59.726107	70.414823
873.539950	61.723566	70.419828
873.401574	59.757136	70.424833
872.139487	56.586647	70.429838
871.688755	54.682546	70.434842
871.252501	54.319883	70.439847
870.642046	55.971784	70.444852
869.729206	47.531052	70.449857
869.079274	55.879834	70.454862
868.468943	49.947039	70.459866
867.905667	57.969813	70.464871
866.824484	56.290625	70.469876
866.267931	46.724081	70.474881
865.832855	64.370504	70.479886
865.268072	57.397616	70.484890
864.442152	56.920365	70.489895
863.370159	57.420508	70.494900
863.174663	54.297874	70.499905
862.712037	59.341718	70.504910
861.888857	69.563006	70.509914
861.383817	51.161016	70.514919
860.614283	50.531298	70.519924
860.226598	51.993212	70.524929
858.661168	65.109477	70.529934
858.075566	52.663484	70.534938
857.735430	54.981948	70.539943
857.123223	55.673825	70.544948
856.820536	54.375330	70.549953
855.596082	62.364579	70.554958
855.061467	43.101615	70.559962
854.646693	60.924564	70.564967
854.032095	61.555325	70.569972
853.421789	49.509059	70.574977
852.401753	57.891523	70.579982
852.227685	55.681633	70.584986
851.420128	59.621390	70.589991
850.056068	60.555932	70.594996
849.904281	54.239516	70.600001
849.321116	59.159054	70.605006
848.812621	52.241866	70.610010
848.392976	52.767486	70.615015
847.385112	58.823730	70.620020
846.865228	53.114649	70.625025
845.683678	56.762295	70.630030
844.934251	55.449757	70.635034
844.774453	45.220866	70.640039
844.036605	62.193277	70.645044
843.835483	58.991120	70.650049
842.585332	65.328768	70.655054
841.945248	63.893176	70.660058
841.509793	52.583857	70.665063
840.328728	56.802250	70.670068
839.662998	47.301974	70.675073
838.998736	60.285845	70.680078
838.746364	56.927853	70.685082
838.553901	61.618060	70.690087
836.667299	67.653339	70.695092
836.666628	53.496395	70.700097
835.933662	59.433198	70.705102
835.856759	61.963641	70.710106
834.966601	61.509238	70.715111
834.149584	62.645281	70.720116
833.863538	55.974945	70.725121
832.542800	63.176909	70.730126
832.004141	60.063170	70.735130
831.432692	62.169314	70.740135
830.553913	66.751158	70.745140
830.404923	59.936011	70.750145
829.617663	65.432056	70.755150
828.811867	59.495690	70.760154
828.544808	57.423599	70.765159
827.114880	68.342252	70.770164
826.489432	48.548159	70.775169
826.036833	63.289649	70.780174
825.699084	52.231272	70.785178
824.946693	45.696670	70.790183
823.947450	53.774651	70.795188
823.399896	53.074920	70.800193
822.880952	60.902999	70.805198
822.243867	63.711832	70.810202
821.182558	59.643718	70.815207
820.473541	57.826468	70.820212
820.452350	48.825962	70.825217
820.100214	55.883212	70.830222
818.826015	56.995843	70.835226
818.104041	57.538055	70.840231
817.585062	61.745682	70.845236
817.194966	57.167054	70.850241
816.265254	56.312126	70.855246
815.687860	63.821526	70.860250
815.151602	52.233389	70.865255
813.856259	59.518045	70.870260
813.467762	61.178780	70.875265
812.860925	54.037573	70.880270
812.571123	46.951553	70.885274
811.944309	50.324841	70.890279
810.583880	56.240110	70.895284
809.957368	65.343647	70.900289
809.555548	55.098090	70.905294
809.150718	49.414859	70.910298
808.409316	42.424381	70.915303
807.632718	51.717370	70.920308
807.284475	51.690770	70.925313
806.353150	55.853655	70.930318
805.401422	58.832417	70.935322
805.164749	52.777087	70.940327
804.616086	61.283216	70.945332
804.199608	53.512505	70.950337
802.858452	56.275731	70.955342
802.378163	56.284343	70.960346
801.542438	58.896156	70.965351
800.288420	66.743488	70.970356
800.092146	50.119950	70.975361
799.366461	56.437200	70.980366
799.151541	59.424825	70.985370
798.884080	49.405453	70.990375
797.807041	62.040325	70.995380
797.246445	51.626096	71.000385
797.042704	66.081986	71.005390
795.635849	68.475654	71.010394
794.881471	60.265174	71.015399
794.016270	61.919800	71.020404
793.897312	62.760241	71.025409
793.292825	65.775190	71.030414
792.517495	62.166158	71.035418
791.748079	58.245546	71.040423
790.848816	65.851917	71.045428
790.716253	56.441811	71.050433
790.157943	61.128759	71.055438
788.928193	64.470310	71.060442
788.471699	58.134602	71.065447
787.840609	65.685669	71.070452
787.017884	48.736109	71.075457
786.280527	56.791336	71.080462
785.898322	61.385601	71.085466
785.574817	62.238105	71.090471
784.490808	57.194395	71.095476
784.078645	55.328323	71.100481
783.147821	61.443283	71.105486
782.160218	60.993374	71.110490
781.532784	64.284775	71.115495
780.719633	67.459093	71.120500
780.530816	59.338348	71.125505
780.121213	68.427860	71.130510
779.791847	60.895581	71.135514
778.935004	53.737417	71.140519
777.661529	62.983370	71.145524
777.382110	52.628458	71.150529
776.638799	53.733861	71.155534
775.650891	43.941146	71.160538
775.046503	54.337332	71.165543
774.868287	68.440675	71.170548
774.423614	60.318086	71.175553
773.376465	55.120290	71.180558
772.402053	55.779968	71.185562
772.349756	55.652647	71.190567
771.440394	62.705577	71.195572
770.743919	57.095586	71.200577
769.904258	63.497217	71.205582
769.154044	75.122928	71.210586
768.361044	49.114339	71.215591
767.363989	49.567901	71.220596
767.021643	65.455561	71.225601
766.795821	57.876842	71.230606
766.476266	65.159134	71.235610
765.627283	54.861782	71.240615
764.813710	56.352089	71.245620
764.539123	54.765298	71.250625
763.626748	56.586706	71.255630
762.649322	48.340796	71.260634
762.308493	49.601312	71.265639
761.585430	60.891551	71.270644
760.842018	51.171872	71.275649
760.001979	63.176128	71.280654
759.512073	68.110798	71.285658
759.249457	47.169369	71.290663
757.677103	57.722814	71.295668
757.258119	53.970339	71.300673
756.710051	69.272626	71.305678
756.261774	51.889752	71.310682
755.291957	49.478570	71.315687
754.463841	74.330723	71.320692
754.246324	62.843232	71.325697
753.458870	63.130976	71.330702
752.729662	62.818126	71.335706
752.345137	53.787165	71.340711
751.555343	62.574526	71.345716
751.203610	60.646803	71.350721
750.412124	55.960214	71.355726
749.486262	57.375369	71.360730
749.304560	54.589575	71.365735
747.755620	61.935134	71.370740
747.154492	61.407942	71.375745
746.785305	66.194092	71.380750
746.157437	66.686652	71.385754
746.107142	63.540912	71.390759
744.911272	64.294202	71.395764
744.201821	52.632743	71.400769
743.639023	75.518897	71.405774
742.613272	64.183737	71.410778
741.997018	43.407423	71.415783
741.321827	78.606200	71.420788
740.852213	54.130873	71.425793
740.386408	60.917663	71.430798
739.943481	70.073982	71.435802
739.465338	53.591520	71.440807
738.432513	60.429163	71.445812
737.754967	62.194271	71.450817
736.987464	68.191789	71.455822
736.079628	60.948723	71.460826
735.999701	59.505975	71.465831
734.753653	63.600728	71.470836
733.989813	62.840840	71.475841
733.481164	60.521813	71.480846
732.815942	60.930442	71.485850
732.892388	60.773164	71.490855
731.639227	59.643356	71.495860
731.135452	58.592921	71.500865
730.713590	56.859282	71.505870
729.390733	70.026873	71.510874
728.807365	61.227831	71.515879
727.945109	57.825039	71.520884
727.589219	56.120319	71.525889
727.557958	56.234062	71.530894
726.906516	65.429884	71.535898
726.208006	53.378784	71.540903
725.233938	61.440177	71.545908
724.432074	56.663792	71.550913
723.532116	64.765423	71.555918
722.399000	65.770490	71.560922
722.461651	53.183491	71.565927
722.170772	61.602860	71.570932
721.218294	61.677205	71.575937
720.690484	60.080278	71.580942
720.110498	43.744928	71.585946
719.351191	62.158859	71.590951
718.150224	67.291897	71.595956
717.830150	50.850507	71.600961
717.444020	60.448758	71.605966
716.548838	57.680377	71.610970
715.847216	67.705733	71.615975
715.007381	57.608782	71.620980
714.507682	56.647583	71.625985
713.751963	61.034836	71.630990
712.880864	57.601920	71.635994
712.530424	58.805630	71.640999
712.064972	55.331781	71.646004
711.512324	42.059064	71.651009
710.857120	62.006466	71.656014
709.793029	64.717742	71.661018
709.577675	57.470082	71.666023
708.196090	62.444235	71.671028
707.444558	54.370527	71.676033
707.088505	65.332701	71.681038
706.906671	70.238827	71.686042
706.238432	69.247697	71.691047
704.976925	73.734410	71.696052
704.426582	60.716763	71.701057
704.142638	52.516570	71.706062
703.046447	63.222875	71.711066
702.525370	58.934767	71.716071
701.782299	60.300335	71.721076
701.403882	53.345131	71.726081
701.020059	61.984289	71.731086
700.289023	51.297629	71.736090
699.624966	46.488277	71.741095
698.834460	76.561714	71.746100
697.742723	55.905263	71.751105
697.072827	53.790104	71.756110
696.377543	50.663496	71.761114
696.270091	52.709977	71.766119
695.250859	62.894707	71.771124
694.197593	43.220839	71.776129
693.887914	54.304923	71.781134
693.386026	58.013139	71.786138
693.261913	63.097718	71.791143
692.073526	51.988750	71.796148
691.337622	54.922148	71.801153
690.816285	46.162134	71.806158
690.106062	58.314453	71.811162
689.689525	47.473651	71.816167
688.791386	49.466271	71.821172
688.416572	67.953022	71.826177
687.422618	67.072103	71.831182
686.434715	61.970562	71.836186
686.149126	73.594839	71.841191
685.769053	55.642919	71.846196
684.893743	57.633483	71.851201
683.789371	66.165042	71.856206
683.020895	71.632905	71.861210
683.314667	46.898878	71.866215
682.322072	55.120915	71.871220
681.296344	58.034237	71.876225
681.277406	51.832300	71.881230
680.488349	56.428283	71.886234
679.541153	58.816624	71.891239
678.767359	58.807344	71.896244
678.675664	60.441336	71.901249
677.708735	50.799856	71.906254
676.373163	54.407449	71.911258
676.426398	53.591587	71.916263
675.506175	57.101507	71.921268
674.839210	49.481096	71.926273
674.112955	60.142694	71.931278
673.220364	63.757019	71.936282
673.194077	57.587787	71.941287
672.498877	60.689741	71.946292
671.674638	49.581146	71.951297
671.478170	50.823416	71.956302
670.101645	52.423893	71.961306
669.081480	54.451719	71.966311
668.577742	58.634866	71.971316
668.272866	52.659800	71.976321
668.003189	57.504221	71.981326
667.007264	56.136378	71.986330
666.216492	49.887048	71.991335
665.667773	61.791320	71.996340
665.193399	48.643337	72.001345
664.154373	53.398968	72.006350
663.235588	56.091853	72.011354
662.997414	36.657204	72.016359
662.376166	61.019111	72.021364
661.932361	55.851440	72.026369
661.165008	53.638278	72.031374
660.232005	49.530888	72.036378
660.127976	41.499168	72.041383
658.963771	52.176888	72.046388
658.399917	51.284260	72.051393
657.851797	47.525565	72.056398
657.048559	51.611334	72.061402
656.072580	53.452368	72.066407
655.492179	56.677960	72.071412
654.744682	51.574421	72.076417
654.681440	50.829143	72.081422
653.815433	55.065249	72.086426
653.074765	48.263932	72.091431
652.407977	44.245033	72.096436
651.923581	52.521760	72.101441
651.427460	50.196028	72.106446
650.161454	53.641178	72.111450
649.419227	43.065130	72.116455
649.195258	51.486454	72.121460
648.932877	63.835533	72.126465
647.728898	52.279672	72.131470
646.903043	57.420807	72.136474
646.476135	58.799117	72.141479
646.056491	54.106966	72.146484
645.319559	52.809846	72.151489
644.316018	41.036009	72.156494
643.844876	61.343583	72.161498
643.388604	49.257099	72.166503
642.325485	48.835041	72.171508
641.425542	57.739306	72.176513
641.110408	46.432967	72.181518
640.601297	51.515777	72.186522
640.312623	51.924387	72.191527
639.534402	51.564186	72.196532
639.038269	49.326763	72.201537
638.183263	46.913115	72.206542
637.097340	65.071584	72.211546
636.617536	47.972883	72.216551
636.227748	51.127125	72.221556
634.814034	49.185627	72.226561
634.222485	53.407991	72.231566
633.287916	63.058896	72.236570
633.204381	48.675504	72.241575
632.818620	56.841916	72.246580
631.948741	58.524146	72.251585
631.151987	48.086087	72.256590
630.810570	61.840110	72.261594
630.060168	49.013622	72.266599
629.027463	54.468382	72.271604
628.445496	44.210573	72.276609
628.010287	53.321508	72.281614
627.119309	56.188162	72.286618
627.298939	46.360964	72.291623
626.064636	46.513342	72.296628
625.184476	55.206314	72.301633
624.943599	53.541638	72.306638
623.968193	58.567834	72.311642
623.347332	53.010504	72.316647
622.674508	50.963638	72.321652
622.009821	57.556623	72.326657
621.759233	50.882260	72.331662
620.516323	54.287478	72.336666
620.210665	48.430811	72.341671
619.480407	52.036643	72.346676
618.627747	54.890889	72.351681
618.106267	55.410689	72.356686
617.386959	54.774625	72.361690
616.900695	45.107090	72.366695
615.769732	50.375664	72.371700
614.965364	54.086335	72.376705
614.442457	53.091008	72.381710
613.942033	50.095808	72.386714
613.907455	50.344113	72.391719
613.378926	55.406368	72.396724
612.477441	54.608520	72.401729
611.835679	47.506057	72.406734
610.728934	48.207370	72.411738
609.475972	58.366272	72.416743
608.990819	61.855808	72.421748
608.768245	54.699197	72.426753
608.571988	53.293905	72.431758
607.662710	61.885874	72.436762
606.950092	59.829581	72.441767
606.428638	59.146241	72.446772
605.662340	64.448205	72.451777
604.859386	52.544669	72.456782
603.882517	60.007340	72.461786
603.833325	51.574251	72.466791
603.219313	54.278538	72.471796
602.111367	48.275277	72.476801
601.692176	50.507017	72.481806
600.977147	65.716059	72.486810
600.257887	58.979151	72.491815
599.445650	57.490624	72.496820
598.643949	56.076109	72.501825
598.638447	52.964244	72.506830
597.573528	55.808150	72.511834
596.823148	53.095597	72.516839
596.219547	48.705552	72.521844
595.668873	54.135589	72.526849
595.409283	45.147850	72.531854
594.176617	64.225349	72.536858
593.806095	51.937577	72.541863
593.068993	53.798932	72.546868
592.044997	51.420100	72.551873
591.557753	53.241662	72.556878
590.976620	59.231604	72.561882
590.868963	53.083225	72.566887
589.645389	54.749265	72.571892
588.878340	53.936322	72.576897
588.656240	47.345732	72.581902
587.794169	65.988922	72.586906
586.913026	62.986557	72.591911
586.080094	52.290943	72.596916
585.434498	52.423689	72.601921
585.394587	53.365082	72.606926
584.496975	63.011690	72.611930
583.907988	62.454221	72.616935
583.282482	58.053474	72.621940
582.711691	61.990288	72.626945
581.730129	63.244074	72.631950
580.776080	73.371158	72.636954
580.551398	53.453423	72.641959
579.785529	60.794192	72.646964
578.537363	54.259798	72.651969
578.438732	64.039334	72.656974
577.635193	63.134440	72.661978
577.585383	59.351586	72.666983
576.583714	59.075876	72.671988
575.395964	57.205648	72.676993
575.139660	56.860105	72.681998
574.734775	63.432222	72.687002
574.210138	48.037377	72.692007
573.024556	57.707775	72.697012
572.289870	62.246246	72.702017
572.268460	48.721816	72.707022
570.879792	57.932584	72.712026
570.576526	62.186312	72.717031
569.918510	63.990927	72.722036
569.004824	56.234817	72.727041
568.751167	49.431650	72.732046
567.404533	64.042748	72.737050
567.087887	52.831276	72.742055
566.832837	55.541470	72.747060
566.067777	59.308969	72.752065
565.368426	51.045669	72.757070
564.499478	55.678060	72.762074
564.097783	57.465502	72.767079
563.055067	56.666514	72.772084
562.044174	64.367993	72.777089
562.071167	57.633656	72.782094
561.388416	62.465036	72.787098
561.162889	56.207708	72.792103
560.193003	53.569551	72.797108
559.253134	62.164830	72.802113
559.065955	58.209904	72.807118
557.914841	54.069492	72.812122
557.424386	59.712281	72.817127
556.262468	59.637135	72.822132
555.762150	70.369998	72.827137
555.086626	63.067934	72.832142
554.191377	57.112810	72.837146
553.740278	63.542489	72.842151
553.484356	60.216639	72.847156
553.287674	66.973201	72.852161
552.342963	58.326386	72.857166
551.535494	62.379747	72.862170
550.973226	61.001222	72.867175
550.161541	67.757979	72.872180
549.190613	64.355218	72.877185
548.967267	54.824002	72.882190
548.228278	64.849029	72.887194
547.197737	58.115994	72.892199
546.478223	58.369328	72.897204
545.917297	58.687282	72.902209
545.950400	51.319658	72.907214
544.621744	56.290190	72.912218
544.142469	58.624545	72.917223
543.409335	61.049795	72.922228
542.870663	68.341772	72.927233
542.081826	59.040970	72.932238
541.369020	52.869148	72.937242
540.788031	65.130212	72.942247
540.551556	57.026561	72.947252
539.031947	60.538967	72.952257
538.722571	55.670013	72.957262
537.956467	62.495200	72.962266
537.841762	57.232561	72.967271
537.083789	59.139832	72.972276
535.883323	62.278150	72.977281
535.684000	55.822700	72.982286
535.088885	59.944735	72.987290
533.952227	47.772713	72.992295
533.334211	55.794790	72.997300
532.675456	63.925856	73.002305
533.070250	50.801881	73.007310
531.785578	49.711886	73.012314
531.022398	52.165578	73.017319
530.433481	51.858830	73.022324
529.132992	58.751794	73.027329
528.507484	53.512182	73.032334
527.740182	63.472339	73.037338
527.791189	54.851420	73.042343
527.398632	60.212132	73.047348
526.509964	56.892467	73.052353
525.613002	58.754076	73.057358
524.821671	53.387924	73.062362
524.212851	51.237858	73.067367
523.573577	47.172041	73.072372
522.432693	63.734058	73.077377
522.019407	58.627785	73.082382
521.427283	60.775130	73.087386
521.271079	59.262546	73.092391
520.684052	56.156591	73.097396
519.421169	54.273130	73.102401
519.475364	49.444031	73.107406
518.520419	57.899804	73.112410
517.768399	50.952120	73.117415
516.964073	53.022888	73.122420
516.413222	55.515296	73.127425
515.694341	66.150520	73.132430
514.724263	43.355543	73.137434
514.554979	51.813884	73.142439
514.085445	58.035203	73.147444
513.090817	61.364655	73.152449
512.459219	51.912674	73.157454
511.593734	59.209405	73.162458
511.442157	69.186596	73.167463
510.182405	60.227311	73.172468
509.314217	44.534008	73.177473
509.163581	58.017953	73.182478
508.446073	62.933724	73.187482
508.064415	55.562790	73.192487
507.136328	59.179668	73.197492
506.712800	59.806881	73.202497
506.268892	48.188374	73.207502
504.688663	60.351591	73.212506
504.175774	54.688794	73.217511
504.070359	52.646185	73.222516
503.387468	55.670528	73.227521
502.361601	53.471794	73.232526
501.434711	55.335025	73.237530
501.375432	49.927954	73.242535
500.877563	73.275232	73.247540
499.939387	51.594734	73.252545
499.050079	66.771631	73.257550
498.567751	55.495110	73.262554
497.889615	51.358225	73.267559
496.779544	62.221337	73.272564
496.123184	68.228013	73.277569
495.875072	52.003871	73.282574
495.308744	69.453595	73.287578
494.957767	46.455928	73.292583
493.860717	52.411385	73.297588
493.165332	67.054376	73.302593
492.914378	57.609564	73.307598
491.864532	63.527546	73.312602
491.075068	55.636572	73.317607
490.548630	61.956841	73.322612
490.433998	57.879987	73.327617
489.785066	61.302598	73.332622
488.446301	60.259088	73.337626
487.980650	53.341482	73.342631
487.269671	52.234229	73.347636
486.182373	54.596075	73.352641
486.073871	52.325316	73.357646
485.143152	55.233037	73.362650
484.991930	46.235939	73.367655
484.019661	49.281158	73.372660
483.118048	53.693286	73.377665
482.841804	50.564638	73.382670
482.150737	51.359048	73.387674
481.206348	45.454364	73.392679
480.363655	51.785592	73.397684
479.893480	55.461983	73.402689
479.834528	53.270056	73.407694
478.582283	61.725900	73.412698
477.873488	59.847222	73.417703
477.418198	50.840221	73.422708
476.737648	57.915123	73.427713
476.517755	49.501362	73.432718
475.312111	55.149297	73.437722
474.632821	55.404127	73.442727
474.500926	61.489665	73.447732
473.170045	62.283514	73.452737
472.696892	53.265167	73.457742
471.920095	47.295943	73.462746
471.538869	48.053608	73.467751
471.012799	44.078575	73.472756
470.033738	48.944563	73.477761
469.753505	38.351757	73.482766
469.039424	54.408994	73.487770
468.241401	51.070182	73.492775
467.767543	48.073938	73.497780
467.060251	60.019258	73.502785
465.980717	54.563434	73.507790
465.095842	57.203679	73.512794
464.625810	58.279826	73.517799
464.100629	56.695153	73.522804
463.689416	52.417988	73.527809
463.020920	48.725827	73.532814
461.853682	55.493519	73.537818
461.546003	60.645185	73.542823
461.103965	40.265427	73.547828
460.082596	53.916471	73.552833
459.346465	50.495267	73.557838
459.288308	50.807250	73.562842
458.449737	57.260824	73.567847
457.395711	51.446151	73.572852
456.500363	56.492761	73.577857
456.318639	48.188032	73.582862
456.111210	56.660336	73.587866
455.085987	57.731904	73.592871
454.135022	58.387968	73.597876
453.408988	64.350562	73.602881
453.111769	54.914708	73.607886
451.941695	62.414516	73.612890
451.479692	52.628051	73.617895
451.183655	56.188398	73.622900
450.463025	62.610571	73.627905
449.742800	46.255099	73.632910
448.630490	52.492107	73.637914
448.167926	47.269135	73.642919
448.063552	48.643394	73.647924
446.959686	54.423348	73.652929
446.419648	40.968961	73.657934
445.654014	56.499866	73.662938
445.425024	60.716540	73.667943
444.421071	55.549863	73.672948
443.326529	59.563842	73.677953
443.035311	47.228790	73.682958
442.630175	46.159549	73.687962
441.634881	51.305659	73.692967
441.087961	50.774637	73.697972
440.348373	50.286927	73.702977
439.979630	51.972948	73.707982
438.820906	49.837984	73.712986
438.337642	51.400336	73.717991
437.682493	52.308875	73.722996
437.173478	46.095163	73.728001
436.647954	55.045473	73.733006
435.925472	53.307752	73.738010
435.193758	49.554713	73.743015
434.747125	54.747441	73.748020
433.433280	57.422930	73.753025
433.248938	40.819675	73.758030
432.353350	58.788596	73.763034
431.808672	48.761439	73.768039
431.052059	45.824447	73.773044
430.195139	53.253865	73.778049
429.842679	42.626844	73.783054
429.536321	61.895820	73.788058
428.726680	44.501272	73.793063
427.919683	45.274746	73.798068
427.283705	56.622120	73.803073
426.770733	46.611990	73.808078
426.023519	60.263519	73.813082
425.057551	50.716623	73.818087
424.863858	53.224676	73.823092
423.862631	61.402442	73.828097
423.277489	52.398800	73.833102
422.423006	57.443640	73.838106
422.010462	56.612109	73.843111
421.341097	58.248268	73.848116
420.171623	61.566192	73.853121
419.830545	53.435081	73.858126
419.382163	60.122942	73.863130
418.720979	61.699456	73.868135
417.853920	52.595665	73.873140
417.086154	53.132673	73.878145
416.886119	49.260234	73.883150
416.067597	51.596628	73.888154
415.056720	48.638657	73.893159
414.863019	54.874379	73.898164
414.061004	53.152491	73.903169
413.639519	48.668831	73.908174
412.350548	50.911464	73.913178
411.689761	43.318549	73.918183
411.551819	47.575902	73.923188
410.858648	57.043328	73.928193
410.026610	41.744840	73.933198
409.378057	48.877727	73.938202
408.924584	51.020347	73.943207
407.974538	52.013727	73.948212
406.957066	52.984738	73.953217
406.621919	39.612829	73.958222
405.941644	49.278456	73.963226
405.504244	54.173268	73.968231
404.766448	50.039612	73.973236
403.997349	51.478792	73.978241
403.683381	55.278527	73.983246
402.986340	50.971232	73.988250
401.472589	47.978287	73.993255
401.161761	47.029634	73.998260
400.338485	54.253440	74.003265
400.657140	40.176574	74.008270
399.712268	44.501009	74.013274
398.638986	62.413105	74.018279
398.350959	50.320389	74.023284
397.659184	51.619525	74.028289
397.062614	46.562989	74.033294
396.200498	54.810051	74.038298
395.394648	55.375210	74.043303
394.985508	48.281481	74.048308
393.573029	40.950268	74.053313
393.380489	45.474924	74.058318
392.911393	63.982984	74.063322
392.276249	59.542832	74.068327
391.784677	40.708422	74.073332
390.633674	55.827688	74.078337
390.003050	53.173387	74.083342
389.791464	47.167741	74.088346
389.002132	49.847975	74.093351
388.130582	49.076977	74.098356
387.513781	55.042675	74.103361
387.379224	50.514875	74.108366
386.173940	46.988695	74.113370
385.373097	42.521341	74.118375
385.000176	40.918734	74.123380
384.073047	56.691409	74.128385
383.810792	47.453418	74.133390
382.946770	53.792802	74.138394
382.430947	48.365458	74.143399
381.881478	43.448069	74.148404
380.793542	55.466670	74.153409
380.187294	52.879445	74.158414
379.459339	46.358461	74.163418
379.033612	46.008400	74.168423
378.260161	44.419160	74.173428
377.331984	47.077370	74.178433
377.015782	50.663011	74.183438
376.626875	48.698699	74.188442
375.766186	58.675342	74.193447
374.994675	65.253864	74.198452
374.479843	62.065485	74.203457
373.585031	37.598193	74.208462
372.477998	68.805340	74.213466
371.946963	44.638013	74.218471
371.564215	49.366434	74.223476
370.978673	59.783325	74.228481
370.960849	54.435885	74.233486
370.377611	37.978212	74.238490
369.210064	50.132492	74.243495
368.414552	52.514116	74.248500
367.430311	41.751264	74.253505
366.771014	48.244094	74.258510
366.144741	51.478629	74.263514
365.619736	56.370062	74.268519
365.659461	42.602555	74.273524
364.593419	49.958088	74.278529
363.863649	48.779755	74.283534
363.621352	51.213560	74.288538
362.394151	51.681883	74.293543
361.611421	40.913728	74.298548
360.793604	50.080922	74.303553
360.596664	52.726681	74.308558
360.215161	49.463448	74.313562
358.801059	56.231100	74.318567
358.491953	45.441079	74.323572
358.010882	57.659425	74.328577
357.356223	58.425991	74.333582
356.319489	47.321445	74.338586
355.739303	54.646863	74.343591
355.575541	46.419709	74.348596
354.616437	53.100661	74.353601
353.825297	55.144147	74.358606
353.567220	53.207872	74.363610
352.622672	53.855068	74.368615
351.493626	47.292364	74.373620
350.873518	58.523686	74.378625
350.681389	51.441112	74.383630
350.381385	40.427311	74.388634
348.982563	53.738017	74.393639
348.462768	47.146027	74.398644
347.736947	59.810206	74.403649
347.337514	55.463383	74.408654
347.072122	51.092047	74.413658
345.856458	50.311254	74.418663
345.434195	46.105258	74.423668
344.868867	56.834298	74.428673
344.134094	43.710581	74.433678
343.133360	52.058589	74.438682
342.682757	51.423936	74.443687
342.321581	49.437866	74.448692
341.219037	50.848208	74.453697
340.498018	51.374636	74.458702
340.208698	54.973342	74.463706
339.605858	48.735187	74.468711
338.660010	47.810479	74.473716
338.134579	49.819508	74.478721
337.550507	39.771861	74.483726
336.601910	50.418485	74.488730
335.630837	53.290113	74.493735
335.381846	49.945846	74.498740
334.789204	49.210838	74.503745
334.634946	43.850457	74.508750
333.560469	53.287206	74.513754
332.698119	55.126020	74.518759
332.274107	41.328353	74.523764
331.050026	42.430085	74.528769
330.358334	42.904536	74.533774
330.209767	54.771865	74.538778
329.499913	56.928552	74.543783
328.906183	36.960933	74.548788
327.933890	51.610215	74.553793
327.542370	48.902058	74.558798
327.336280	47.026882	74.563802
326.048235	60.209570	74.568807
325.176574	43.006301	74.573812
324.518973	55.858290	74.578817
324.452847	30.188293	74.583822
323.583051	61.855903	74.588826
322.446478	52.307863	74.593831
322.113779	28.176783	74.598836
321.395397	48.243052	74.603841
321.505373	48.603930	74.608846
320.630941	56.562836	74.613850
319.446640	54.156059	74.618855
318.631487	42.453289	74.623860
317.732470	52.007148	74.628865
317.208400	49.618142	74.633870
317.008389	53.324033	74.638874
316.102748	52.014483	74.643879
316.174515	42.589241	74.648884
314.774495	49.646383	74.653889
314.047251	46.286886	74.658894
313.910505	40.269327	74.663898
313.151675	60.167030	74.668903
312.110515	53.836325	74.673908
311.105133	60.977224	74.678913
310.995473	47.145226	74.683918
310.919073	44.438885	74.688922
309.625654	50.007844	74.693927
309.200283	38.384875	74.698932
308.424523	66.748211	74.703937
307.216048	37.157319	74.708942
306.712617	34.318782	74.713946
306.127034	57.530201	74.718951
305.882237	45.457429	74.723956
305.194012	50.718636	74.728961
304.403551	46.028899	74.733966
303.704284	34.813840	74.738970
303.154720	66.215969	74.743975
302.470023	31.705422	74.748980
301.647120	47.898278	74.753985
301.048985	54.483870	74.758990
300.666746	52.597351	74.763994
299.473844	57.341375	74.768999
298.940888	45.152118	74.774004
298.380580	54.722956	74.779009
298.025667	52.043660	74.784014
296.939494	51.352631	74.789018
295.911900	48.034704	74.794023
295.475159	47.553958	74.799028
294.982911	54.904790	74.804033
294.685191	48.006201	74.809038
293.983049	37.535873	74.814042
292.829128	58.351196	74.819047
292.579370	40.299823	74.824052
291.945344	54.579831	74.829057
291.239963	41.658022	74.834062
290.541301	48.086183	74.839066
289.731248	58.452141	74.844071
289.156384	49.541519	74.849076
287.975380	56.098599	74.854081
287.445107	55.907134	74.859086
287.192903	55.108414	74.864090
286.468789	54.618284	74.869095
286.412407	53.584939	74.874100
285.362727	53.102550	74.879105
284.973029	57.664945	74.884110
283.874772	55.763254	74.889114
282.540703	51.978552	74.894119
281.905928	61.315279	74.899124
281.727915	64.981400	74.904129
281.066532	58.054048	74.909134
281.003743	55.662483	74.914138
279.895496	59.106316	74.919143
279.438894	50.667246	74.924148
278.720791	47.282650	74.929153
278.230934	38.803159	74.934158
277.085256	41.185433	74.939162
276.277730	44.155583	74.944167
276.225581	35.486487	74.949172
275.574794	49.447488	74.954177
274.275018	55.331270	74.959182
274.024574	35.916046	74.964186
273.357838	44.538817	74.969191
272.672667	33.127573	74.974196
271.484968	53.740136	74.979201
270.888295	49.705449	74.984206
270.755831	40.960848	74.989210
270.145691	37.655236	74.994215
270.038617	39.640167	74.999220
268.949489	48.696097	75.004225
268.181961	52.635943	75.009230
267.099106	46.059615	75.014234
266.277584	51.879782	75.019239
266.075127	55.715367	75.024244
265.703318	57.857609	75.029249
264.831651	51.112008	75.034254
263.861162	46.515632	75.039258
263.155653	51.237170	75.044263
263.042659	44.980879	75.049268
262.295730	48.510617	75.054273
261.459163	51.343486	75.059278
260.618821	54.984303	75.064282
260.007962	58.989061	75.069287
259.532038	50.412736	75.074292
258.431254	52.661716	75.079297
257.884840	48.817704	75.084302
257.652624	48.567697	75.089306
256.994294	50.727228	75.094311
256.385667	52.606041	75.099316
255.701546	54.496890	75.104321
255.082157	55.472310	75.109326
254.223849	54.420149	75.114330
253.232890	52.670091	75.119335
252.780742	56.070848	75.124340
252.391368	55.368109	75.129345
251.261834	48.384518	75.134350
250.655288	50.840126	75.139354
250.310526	60.029709	75.144359
249.862904	51.668057	75.149364
248.769105	50.833197	75.154369
247.854714	47.503553	75.159374
247.584506	48.273514	75.164378
246.928456	54.433138	75.169383
246.398812	58.456489	75.174388
245.492829	52.250916	75.179393
244.925790	52.683444	75.184398
244.449012	50.403603	75.189402
243.190279	58.510517	75.194407
243.011710	50.799790	75.199412
242.502465	54.682703	75.204417
241.623473	50.661491	75.209422
240.739354	44.578586	75.214426
239.876192	52.251883	75.219431
239.661341	46.644146	75.224436
239.425508	49.463256	75.229441
238.401292	54.002232	75.234446
237.582987	51.527693	75.239450
236.601050	53.513326	75.244455
236.358739	50.171161	75.249460
235.439853	58.700111	75.254465
234.991366	52.956163	75.259470
234.192098	51.181864	75.264474
233.842621	51.593904	75.269479
233.482308	47.521550	75.274484
232.346666	48.809492	75.279489
231.878946	59.926658	75.284494
231.331499	45.519536	75.289498
229.992886	53.114098	75.294503
229.388380	44.017426	75.299508
228.668225	51.533897	75.304513
228.401172	57.420218	75.309518
227.938748	45.777944	75.314522
226.897365	55.561090	75.319527
226.513989	44.655218	75.324532
226.132042	52.489909	75.329537
224.988690	44.653888	75.334542
224.190395	46.414721	75.339546
223.428775	49.174157	75.344551
223.471100	53.549423	75.349556
222.806657	41.868401	75.354561
221.678269	43.369641	75.359566
221.310784	48.986561	75.364570
220.648239	55.347486	75.369575
219.665782	43.557899	75.374580
218.998242	47.663154	75.379585
218.322754	55.210352	75.384590
218.199606	55.792881	75.389594
216.935184	64.290196	75.394599
216.034983	47.170374	75.399604
215.753558	47.822286	75.404609
215.268199	48.869383	75.409614
214.972047	58.312973	75.414618
213.824527	53.249711	75.419623
213.557933	44.961708	75.424628
212.965223	46.385440	75.429633
211.682741	42.980462	75.434638
211.122790	50.107144	75.439642
210.317334	56.697421	75.444647
210.162316	50.255459	75.449652
209.104065	45.236314	75.454657
208.202709	52.078404	75.459662
207.901035	44.095596	75.464666
207.537204	45.462342	75.469671
206.632012	38.461937	75.474676
205.721599	52.905855	75.479681
205.243165	59.497612	75.484686
204.891974	50.329024	75.489690
203.374931	49.612117	75.494695
202.785229	46.547675	75.499700
202.431111	43.053042	75.504705
202.111128	43.162362	75.509710
202.001517	44.155865	75.514714
200.813446	61.367266	75.519719
200.180510	52.524273	75.524724
199.760720	34.216211	75.529729
198.533057	48.751701	75.534734
197.972620	43.175415	75.539738
197.335902	41.313718	75.544743
196.703984	37.101761	75.549748
195.660163	58.323725	75.554753
194.761892	47.108890	75.559758
194.840597	39.372930	75.564762
194.130684	47.635196	75.569767
193.838891	59.150064	75.574772
192.806175	53.746833	75.579777
191.895411	49.197734	75.584782
191.777823	42.623663	75.589786
190.641114	42.385410	75.594791
189.969487	40.612853	75.599796
189.253230	43.775045	75.604801
188.853217	52.101440	75.609806
188.086623	46.725168	75.614810
186.992183	45.180858	75.619815
186.327393	35.535616	75.624820
186.122065	40.216845	75.629825
185.806979	48.945985	75.634830
185.485775	37.443632	75.639834
184.417853	37.544473	75.644839
183.880236	44.192967	75.649844
182.427817	51.635395	75.654849
181.795426	45.789906	75.659854
181.328149	44.211837	75.664858
180.947787	57.215172	75.669863
180.425564	51.623334	75.674868
179.146598	56.892028	75.679873
178.699475	49.373929	75.684878
178.377243	48.059721	75.689882
177.630874	56.381420	75.694887
176.545313	46.431124	75.699892
176.077463	48.207092	75.704897
175.631143	59.155281	75.709902
175.377872	51.694578	75.714906
174.192092	48.586417	75.719911
173.610178	52.357933	75.724916
173.054702	44.343062	75.729921
172.411848	48.274093	75.734926
171.750709	44.271790	75.739930
171.008655	54.715232	75.744935
170.217302	47.680921	75.749940
169.348593	43.560336	75.754945
168.615717	53.638064	75.759950
168.292916	45.849430	75.764954
167.658148	51.083222	75.769959
167.088182	44.169724	75.774964
166.395116	54.168570	75.779969
165.503234	52.013273	75.784974
165.336654	54.569052	75.789978
164.006504	54.038400	75.794983
163.562950	43.649884	75.799988
163.131984	49.830402	75.804993
162.514991	56.436371	75.809998
161.497505	45.537008	75.815002
160.655433	47.845697	75.820007
160.086693	48.950250	75.825012
159.643528	44.137391	75.830017
159.561114	56.822004	75.835022
158.707074	52.703813	75.840026
157.584160	52.887546	75.845031
157.200705	54.702097	75.850036
156.665313	44.629403	75.855041
155.438417	58.605017	75.860046
155.193082	47.782801	75.865050
154.527030	59.958120	75.870055
153.781610	52.298366	75.875060
153.012213	55.166288	75.880065
152.206114	60.810578	75.885070
152.139491	59.406735	75.890074
150.849837	62.851164	75.895079
150.196452	52.179156	75.900084
149.824778	48.466573	75.905089
149.093259	55.421941	75.910094
148.836002	50.393373	75.915098
147.924343	52.577553	75.920103
147.099827	56.679473	75.925108
146.791926	50.974630	75.930113
145.354041	51.758907	75.935118
144.763677	45.176651	75.940122
144.414295	44.576356	75.945127
143.778314	48.134162	75.950132
143.507164	49.426219	75.955137
142.224413	51.141329	75.960142
142.077683	44.554565	75.965146
141.163657	50.395822	75.970151
140.777096	47.160245	75.975156
140.034614	44.998482	75.980161
138.856466	60.300338	75.985166
138.817972	54.379085	75.990170
138.292045	50.968624	75.995175
137.481862	45.733353	76.000180
136.666260	52.400952	76.005185
135.546077	49.961970	76.010190
134.893266	47.137829	76.015194
134.000916	49.702108	76.020199
133.572174	41.600816	76.025204
133.439658	62.641222	76.030209
132.887957	55.310107	76.035214
132.333442	47.331362	76.040218
131.544524	62.765111	76.045223
130.837979	54.151484	76.050228
129.752203	57.400998	76.055233
128.995293	59.994143	76.060238
128.769827	52.317718	76.065242
128.347936	52.291920	76.070247
127.364865	53.541389	76.075252
126.648249	52.848276	76.080257
125.806252	59.065960	76.085262
125.609516	50.870904	76.090266
124.274754	56.708300	76.095271
123.827034	47.924107	76.100276
123.374843	43.458024	76.105281
122.740394	46.077370	76.110286
122.474499	45.615142	76.115290
121.355758	52.231742	76.120295
120.577457	50.449408	76.125300
120.487896	56.796252	76.130305
119.083397	61.488946	76.135310
118.814673	51.810523	76.140314
117.997225	56.535754	76.145319
117.672337	53.329766	76.150324
117.077885	44.532707	76.155329
116.117390	57.160228	76.160334
115.390608	58.449254	76.165338
114.677970	56.743177	76.170343
114.186986	50.905119	76.175348
113.261932	51.634446	76.180353
112.724520	49.810549	76.185358
112.447419	44.244296	76.190362
111.382177	44.869830	76.195367
110.606465	61.367420	76.200372
110.099329	50.541231	76.205377
109.823231	58.206101	76.210382
109.017330	49.206233	76.215386
107.903429	57.261725	76.220391
107.837003	49.451143	76.225396
106.840046	56.002601	76.230401
105.723985	55.073591	76.235406
105.167783	48.597854	76.240410
104.439173	50.292422	76.245415
104.165442	45.790001	76.250420
104.227711	49.367349	76.255425
102.856241	46.044426	76.260430
102.137753	54.533570	76.265434
101.841038	55.380307	76.270439
101.046953	46.979337	76.275444
99.728055	47.583829	76.280449
98.929100	55.179122	76.285454
99.091677	48.035295	76.290458
98.553625	48.496347	76.295463
97.845429	48.796887	76.300468
96.993310	55.888185	76.305473
96.274369	61.427134	76.310478
95.929576	43.012530	76.315482
94.563536	48.791851	76.320487
94.076371	54.478328	76.325492
93.665199	46.979749	76.330497
92.874607	56.699293	76.335502
92.621252	47.155613	76.340506
91.626858	49.997935	76.345511
91.201002	53.705160	76.350516
90.505445	48.426397	76.355521
89.820356	54.314736	76.360526
89.181898	48.514395	76.365530
88.794610	44.156233	76.370535
88.029488	54.634906	76.375540
87.439767	49.929005	76.380545
86.619702	47.860050	76.385550
85.861974	45.926225	76.390554
84.920267	56.223340	76.395559
84.307958	57.513041	76.400564
83.611159	51.715697	76.405569
82.496262	62.833587	76.410574
81.934806	53.414728	76.415578
81.625446	48.924298	76.420583
80.875045	46.987729	76.425588
80.683106	50.050567	76.430593
79.625380	60.556986	76.435598
78.975780	47.150162	76.440602
78.294922	47.947783	76.445607
77.678399	49.528297	76.450612
77.506741	47.663426	76.455617
76.371626	61.244414	76.460622
75.675074	50.224531	76.465626
75.183029	59.726171	76.470631
74.865991	58.297616	76.475636
73.944739	59.827387	76.480641
72.848716	60.893055	76.485646
72.650080	52.015539	76.490650
72.318104	54.807418	76.495655
70.799723	70.717038	76.500660
70.669937	55.775037	76.505665
69.847486	61.164932	76.510670
69.573081	54.109713	76.515674
68.374563	58.242918	76.520679
68.012360	63.865322	76.525684
67.678433	47.525691	76.530689
66.402888	57.865014	76.535694
65.631855	50.477444	76.540698
65.190588	55.555828	76.545703
64.689255	60.768365	76.550708
63.758326	59.876077	76.555713
62.784783	56.018238	76.560718
62.517810	46.322206	76.565722
62.009737	51.937909	76.570727
61.788792	51.097962	76.575732
61.100704	43.337649	76.580737
60.005622	49.280341	76.585742
59.539168	40.972210	76.590746
58.307704	43.585866	76.595751
57.730288	54.823029	76.600756
57.514876	48.067468	76.605761
56.647459	61.541119	76.610766
55.759872	47.869505	76.615770
55.154037	48.152156	76.620775
54.681470	51.589311	76.625780
54.276968	50.136864	76.630785
53.492238	55.014579	76.635790
52.444818	50.236615	76.640794
52.173049	52.750831	76.645799
51.517472	54.749135	76.650804
50.607680	51.442491	76.655809
49.686739	51.532565	76.660814
49.204540	51.174224	76.665818
48.901098	50.115639	76.670823
48.341657	51.370111	76.675828
47.720502	42.992045	76.680833
47.235773	53.845445	76.685838
46.216413	44.692008	76.690842
45.445489	48.372276	76.695847
44.453765	42.798592	76.700852
44.107074	43.435702	76.705857
43.480925	48.794291	76.710862
42.510460	51.552397	76.715866
41.911045	50.794889	76.720871
41.444106	55.599847	76.725876
41.296709	53.882486	76.730881
39.980626	54.816120	76.735886
39.543557	49.980239	76.740890
38.939910	50.743481	76.745895
37.751387	56.117656	76.750900
37.477409	49.746727	76.755905
36.659439	52.346482	76.760910
36.061236	54.704620	76.765914
35.969031	47.951488	76.770919
34.622792	63.962962	76.775924
34.213945	53.226768	76.780929
33.867708	56.900803	76.785934
33.195052	45.624836	76.790938
31.883579	55.659264	76.795943
31.187458	54.169760	76.800948
30.966507	44.824339	76.805953
30.303557	43.421003	76.810958
29.598571	39.416278	76.815962
28.493414	47.517705	76.820967
27.833895	56.894682	76.825972
28.017479	44.802533	76.830977
27.002916	49.480384	76.835982
26.275668	39.946079	76.840986
25.563095	56.064624	76.845991
24.956092	60.783124	76.850996
24.724248	51.999215	76.856001
23.581785	62.668968	76.861006
23.285015	49.134933	76.866010
22.627350	49.605618	76.871015
21.592091	59.922404	76.876020
20.828926	52.065274	76.881025
20.439589	52.348094	76.886030
20.047216	48.637260	76.891034
18.962197	49.674390	76.896039
18.060156	47.244824	76.901044
18.210086	52.976341	76.906049
16.941370	54.922649	76.911054
16.367236	46.729466	76.916058
15.823068	45.923733	76.921063
15.077836	47.773930	76.926068
14.142623	41.631469	76.931073
13.084916	60.283861	76.936078
13.076473	46.946675	76.941082
12.518312	47.723168	76.946087
11.960567	42.960156	76.951092
11.288292	42.329387	76.956097
10.417426	49.212398	76.961102
9.787073	42.770596	76.966106
9.179711	48.143540	76.971111
8.195604	49.861543	76.976116
7.913493	42.405476	76.981121
7.430530	38.527761	76.986126
6.575244	42.711891	76.991130
5.740055	45.913599	76.996135
5.141336	40.676190	77.001140
4.951882	42.595425	77.006145
3.364798	53.301407	77.011150
3.106924	42.280970	77.016155
2.901950	48.081707	77.021159
1.935830	45.939893	77.026164