Mon Mar 08 20:33:00 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.460049	89.778869	0.000000
-1.538152	100.055012	0.005005
-1.830183	60.164844	0.010010
-3.512406	23.208696	0.015014
-7.912553	12.987803	0.020019
-13.293396	23.729726	0.025024
-18.376995	20.043485	0.030029
-22.567786	18.534365	0.035034
-26.624231	27.169696	0.040038
-30.524539	16.593163	0.045043
-34.029036	16.251824	0.050048
-37.628302	18.551042	0.055053
-41.304328	18.301726	0.060058
-45.364581	21.320998	0.065062
-49.048021	16.687693	0.070067
-52.690722	13.050764	0.075072
-56.323962	19.765841	0.080077
-59.781626	8.396558	0.085082
-63.475837	21.928575	0.090086
-67.543561	16.464115	0.095091
-71.145569	12.055958	0.100096
-75.478215	22.000049	0.105101
-78.985136	11.220505	0.110106
-82.816616	23.837810	0.115110
-86.701490	13.279413	0.120115
-89.924848	24.626540	0.125120
-93.773033	15.213392	0.130125
-97.789440	18.049148	0.135130
-102.115458	18.066044	0.140134
-105.393364	13.314514	0.145139
-108.638139	18.572185	0.150144
-112.647432	22.359240	0.155149
-116.182736	18.098190	0.160154
-120.290598	10.967207	0.165158
-124.027852	12.621565	0.170163
-128.047006	13.679138	0.175168
-132.179314	17.186253	0.180173
-135.314005	8.681122	0.185178
-139.667687	14.506829	0.190182
-143.479186	15.493449	0.195187
-146.943481	18.919225	0.200192
-150.674091	19.024113	0.205197
-154.124313	17.352899	0.210202
-158.514994	18.906591	0.215206
-161.853521	17.463552	0.220211
-165.438492	8.369623	0.225216
-169.349932	8.725729	0.230221
-172.843365	0.970133	0.235226
-176.887722	17.997251	0.240230
-180.704864	20.612123	0.245235
-184.298177	9.018695	0.250240
-188.066427	17.540480	0.255245
-191.801866	9.602772	0.260250
-195.988504	17.631562	0.265254
-199.606900	5.474504	0.270259
-202.951491	6.249519	0.275264
-206.831974	14.104896	0.280269
-210.755566	11.490677	0.285274
-214.425988	15.078744	0.290278
-218.518734	11.821381	0.295283
-221.853106	10.104971	0.300288
-225.743747	2.359237	0.305293
-229.166787	0.513499	0.310298
-233.230607	9.263855	0.315302
-237.048347	14.080168	0.320307
-240.769022	10.418132	0.325312
-244.725001	19.239603	0.330317
-248.076954	5.989926	0.335322
-252.149058	6.144747	0.340326
-256.091480	13.325739	0.345331
-259.600510	13.160480	0.350336
-263.390340	13.612437	0.355341
-267.240175	1.049346	0.360346
-271.191598	7.869125	0.365350
-274.413853	8.563214	0.370355
-278.053655	4.011612	0.375360
-282.186178	10.201201	0.380365
-286.171251	3.799913	0.385370
-289.763020	9.013863	0.390374
-293.542289	8.275250	0.395379
-297.528984	8.537930	0.400384
-301.004124	11.382224	0.405389
-304.384178	12.323876	0.410394
-308.398843	11.397377	0.415398
-312.191187	5.589792	0.420403
-315.852530	5.912519	0.425408
-320.035888	7.714081	0.430413
-323.538844	-5.134500	0.435418
-327.264495	6.200054	0.440422
-330.712571	-1.367011	0.445427
-334.920247	8.636400	0.450432
-338.869610	6.909535	0.455437
-342.197763	4.157901	0.460442
-346.257285	13.013401	0.465446
-349.822132	5.676298	0.470451
-353.534122	1.136341	0.475456
-357.482449	1.154893	0.480461
-361.208492	-7.457333	0.485466
-365.257399	10.698216	0.490470
-368.647284	11.960048	0.495475
-372.167229	10.954669	0.500480
-376.362749	10.711545	0.505485
-380.123253	2.527436	0.510490
-384.061124	9.966500	0.515494
-387.947971	8.798971	0.520499
-391.241027	1.292393	0.525504
-394.884262	3.283788	0.530509
-398.489768	4.545399	0.535514
-402.326063	10.637429	0.540518
-406.377021	5.722781	0.545523
-410.140984	-0.778246	0.550528
-414.028164	10.766717	0.555533
-417.813512	7.649837	0.560538
-421.243057	13.613874	0.565542
-425.273621	11.731398	0.570547
-428.948597	13.130295	0.575552
-432.626063	11.123643	0.580557
-436.471755	-1.245862	0.585562
-440.168023	2.324590	0.590566
-444.067010	7.452215	0.595571
-447.708013	9.560019	0.600576
-451.679249	14.439018	0.605581
-455.070976	6.055803	0.610586
-459.048510	12.263509	0.615590
-463.084142	14.972056	0.620595
-466.219306	3.498299	0.625600
-470.234749	11.421358	0.630605
-474.062134	-2.515217	0.635610
-477.806365	3.232666	0.640614
-481.545176	7.048077	0.645619
-485.208370	8.937148	0.650624
-489.600666	15.362521	0.655629
-492.916382	7.035027	0.660634
-496.522930	6.721700	0.665638
-500.114296	5.565506	0.670643
-504.237249	0.741371	0.675648
-507.972354	8.668596	0.680653
-511.563830	3.277078	0.685658
-515.821161	19.266477	0.690662
-519.486976	15.616621	0.695667
-522.552197	4.164887	0.700672
-526.662247	13.888117	0.705677
-530.219743	3.032223	0.710682
-533.798236	8.250712	0.715686
-538.086571	8.787459	0.720691
-541.988749	9.831766	0.725696
-545.803300	-4.396868	0.730701
-549.439723	-1.170097	0.735706
-553.226576	7.738362	0.740710
-557.007475	12.684890	0.745715
-560.292570	8.275751	0.750720
-564.120502	5.378782	0.755725
-567.786811	9.471303	0.760730
-571.979802	11.451445	0.765734
-575.636923	12.961245	0.770739
-579.257627	5.877835	0.775744
-583.585764	29.945712	0.780749
-586.839562	7.254600	0.785754
-590.890750	16.443449	0.790758
-594.654317	10.259600	0.795763
-598.028150	7.406828	0.800768
-602.003524	12.200005	0.805773
-605.914296	14.575054	0.810778
-609.588320	8.972966	0.815782
-613.201554	10.359127	0.820787
-616.918549	9.115956	0.825792
-620.909277	19.749030	0.830797
-624.264542	-1.631221	0.835802
-628.159773	13.650851	0.840806
-632.231411	10.633670	0.845811
-635.598889	11.874953	0.850816
-639.528066	11.953985	0.855821
-643.278326	2.445723	0.860826
-647.249280	8.793015	0.865830
-651.413485	15.086045	0.870835
-654.294224	8.551522	0.875840
-658.394687	11.407937	0.880845
-661.795213	0.285923	0.885850
-665.996206	14.207225	0.890854
-669.946224	17.988871	0.895859
-673.178099	6.956607	0.900864
-677.378141	20.005797	0.905869
-680.786924	17.284873	0.910874
-684.579063	15.710068	0.915878
-688.370886	12.605699	0.920883
-691.876731	7.259122	0.925888
-695.790237	19.193467	0.930893
-699.855389	14.522855	0.935898
-703.617352	13.250740	0.940902
-707.634560	13.208345	0.945907
-710.851630	9.275790	0.950912
-714.890014	19.700601	0.955917
-718.388202	8.747228	0.960922
-722.491008	15.856822	0.965926
-726.037502	13.736668	0.970931
-729.820607	10.290380	0.975936
-733.454689	16.729046	0.980941
-737.061323	17.122517	0.985946
-741.147261	16.673305	0.990950
-745.167575	21.924871	0.995955
-748.569888	9.729453	1.000960
-752.794141	15.663275	1.005965
-756.099168	3.999484	1.010970
-759.942983	10.944753	1.015974
-763.900769	19.956542	1.020979
-767.328970	12.375924	1.025984
-771.455602	26.272909	1.030989
-775.088409	17.953935	1.035994
-778.704438	17.306690	1.040998
-782.591486	21.270828	1.046003
-786.138577	11.637296	1.051008
-790.082223	19.983023	1.056013
-793.379170	24.392133	1.061018
-797.169838	19.608438	1.066022
-801.785423	18.461886	1.071027
-805.189184	15.656771	1.076032
-809.525792	25.186466	1.081037
-812.647212	4.650585	1.086042
-815.960810	3.475702	1.091046
-819.942058	39.723078	1.096051
-823.752151	14.369705	1.101056
-827.934392	20.208641	1.106061
-831.525368	11.942995	1.111066
-835.575634	19.386550	1.116070
-839.238847	13.611230	1.121075
-842.411659	13.542883	1.126080
-846.414572	18.041266	1.131085
-849.907466	20.452405	1.136090
-853.825427	13.628248	1.141094
-857.795696	16.757479	1.146099
-861.332736	8.519529	1.151104
-865.331780	14.163673	1.156109
-869.000559	10.822328	1.161114
-872.785381	26.232190	1.166118
-876.512648	16.769519	1.171123
-880.346523	12.994155	1.176128
-884.175350	17.590914	1.181133
-888.055481	22.099696	1.186138
-891.435779	18.969285	1.191142
-895.329129	21.911255	1.196147
-899.088863	9.036845	1.201152
-903.182535	19.737279	1.206157
-906.749466	22.171377	1.211162
-910.429093	18.823947	1.216166
-914.394150	19.204039	1.221171
-917.849905	2.323243	1.226176
-921.918119	25.333033	1.231181
-925.591089	15.010280	1.236186
-929.232041	16.038684	1.241190
-932.801060	5.702484	1.246195
-936.534301	9.214955	1.251200
-940.115189	13.523018	1.256205
-944.310547	8.555145	1.261210
-947.985412	19.155571	1.266214
-951.463626	14.566579	1.271219
-955.140284	3.839232	1.276224
-959.054897	7.886900	1.281229
-963.011545	7.601889	1.286234
-966.745592	10.047030	1.291238
-970.860350	23.154022	1.296243
-974.456680	17.026054	1.301248
-978.200239	21.003828	1.306253
-982.127307	7.262267	1.311258
-985.410216	35.782135	1.316262
-989.497414	32.416436	1.321267
-993.167127	6.772890	1.326272
-997.045994	31.523287	1.331277
-1000.593581	11.131532	1.336282
-1004.283935	1.431393	1.341286
-1008.525513	27.141746	1.346291
-1011.985694	23.350986	1.351296
-1015.831741	22.387687	1.356301
-1018.976958	4.322082	1.361306
-1023.066809	16.381315	1.366310
-1027.001652	18.997426	1.371315
-1030.895982	9.110772	1.376320
-1034.828962	12.929710	1.381325
-1038.423597	8.244367	1.386330
-1042.175562	20.557072	1.391334
-1045.665092	17.613081	1.396339
-1049.329463	-0.221214	1.401344
-1053.746187	9.581886	1.406349
-1057.294077	7.922895	1.411354
-1060.626946	18.968633	1.416358
-1064.539469	15.119433	1.421363
-1067.921401	21.691712	1.426368
-1072.174217	12.931554	1.431373
-1076.066962	17.389043	1.436378
-1079.788850	23.566325	1.441382
-1083.340709	7.141105	1.446387
-1087.062560	8.725118	1.451392
-1091.221213	20.114285	1.456397
-1094.794174	2.090419	1.461402
-1098.618636	18.528718	1.466406
-1102.261875	22.142160	1.471411
-1106.226111	3.733087	1.476416
-1109.919190	10.206973	1.481421
-1113.603963	24.942067	1.486426
-1116.889653	6.929042	1.491430
-1121.013300	8.146916	1.496435
-1124.654071	17.531148	1.501440
-1128.490519	7.293240	1.506445
-1132.352760	13.206071	1.511450
-1136.441188	29.953149	1.516454
-1140.291403	24.097855	1.521459
-1143.341635	3.115904	1.526464
-1147.232193	17.362035	1.531469
-1150.991681	14.410938	1.536474
-1154.950781	23.417252	1.541478
-1158.668870	17.684345	1.546483
-1162.287218	11.787267	1.551488
-1166.334188	30.442014	1.556493
-1169.602262	9.747238	1.561498
-1173.509434	13.931250	1.566502
-1177.689304	35.092348	1.571507
-1181.380799	-3.822572	1.576512
-1185.659708	25.547501	1.581517
-1188.954348	4.541652	1.586522
-1192.396103	14.479135	1.591526
-1196.012545	18.129430	1.596531
-1199.561128	4.222064	1.601536
-1203.758080	27.063656	1.606541
-1207.763951	18.314700	1.611546
-1211.255728	3.939411	1.616550
-1215.467382	1.033972	1.621555
-1219.186484	-0.411306	1.626560
-1222.850015	29.584117	1.631565
-1226.060445	12.543153	1.636570
-1229.484386	11.634079	1.641574
-1233.705816	18.403998	1.646579
-1237.438840	18.222428	1.651584
-1241.577463	2.022260	1.656589
-1245.447085	32.957366	1.661594
-1248.591757	18.037764	1.666598
-1253.304520	18.047700	1.671603
-1256.601950	29.526385	1.676608
-1259.920107	8.141245	1.681613
-1263.892264	5.747874	1.686618
-1267.573667	28.366723	1.691622
-1271.281350	21.714629	1.696627
-1275.025337	21.638943	1.701632
-1279.245407	17.766800	1.706637
-1282.719116	8.240596	1.711642
-1286.224674	11.889047	1.716646
-1290.301483	29.637361	1.721651
-1294.076207	15.053618	1.726656
-1298.000883	5.550737	1.731661
-1301.769199	30.205020	1.736666
-1305.776763	0.901166	1.741670
-1309.298555	13.133268	1.746675
-1312.672792	-2.501610	1.751680
-1316.385012	32.569604	1.756685
-1320.361968	-3.522570	1.761690
-1324.037891	27.909857	1.766694
-1327.975720	11.851158	1.771699
-1331.691849	9.820587	1.776704
-1335.297573	19.190058	1.781709
-1339.010261	6.209556	1.786714
-1342.644969	13.675730	1.791718
-1346.867203	15.378097	1.796723
-1350.336018	18.328542	1.801728
-1353.964282	9.251355	1.806733
-1358.250397	17.271221	1.811738
-1361.814028	10.176793	1.816742
-1365.604500	13.069951	1.821747
-1368.969047	10.592109	1.826752
-1373.126814	14.318292	1.831757
-1376.854759	15.261979	1.836762
-1380.247326	-1.349056	1.841766
-1384.720955	26.330616	1.846771
-1388.094077	4.864617	1.851776
-1392.239030	-0.134140	1.856781
-1395.693836	18.727315	1.861786
-1399.169391	6.059007	1.866790
-1403.386648	21.366995	1.871795
-1407.077075	-4.016996	1.876800
-1410.964239	22.491857	1.881805
-1414.520516	-3.134353	1.886810
-1417.938783	19.560815	1.891814
-1421.800471	5.560465	1.896819
-1425.179600	4.453715	1.901824
-1429.631642	20.098930	1.906829
-1433.399644	11.528330	1.911834
-1436.764038	12.847527	1.916838
-1441.015062	27.883471	1.921843
-1444.580612	6.713281	1.926848
-1448.368980	13.928275	1.931853
-1452.045067	-3.219085	1.936858
-1455.825023	32.845497	1.941862
-1459.494488	14.497113	1.946867
-1463.457959	6.277961	1.951872
-1467.250795	24.783672	1.956877
-1470.924723	6.439187	1.961882
-1474.452401	16.548500	1.966886
-1478.414021	25.666118	1.971891
-1481.865909	19.512689	1.976896
-1486.027060	22.030200	1.981901
-1489.721468	13.742776	1.986906
-1493.419723	5.388175	1.991910
-1497.274642	19.916114	1.996915
-1501.274730	18.148848	2.006912
-1501.969856	8.749283	2.016909
-1499.406600	15.445097	2.026906
-1496.758280	15.982488	2.036902
-1494.299362	15.781322	2.046899
-1492.646797	13.323675	2.056896
-1490.907164	7.702321	2.066893
-1488.810780	20.208801	2.076890
-1487.237010	15.809183	2.086886
-1485.309393	10.871361	2.096883
-1482.784077	13.643563	2.106880
-1481.203107	15.453914	2.116877
-1479.427504	10.230988	2.126874
-1477.737616	18.326590	2.136870
-1475.624273	10.338733	2.146867
-1473.570709	6.746441	2.156864
-1471.851779	2.539892	2.166861
-1470.068429	16.148013	2.176858
-1468.222091	12.094734	2.186854
-1466.114865	2.693236	2.196851
-1464.236346	-5.088067	2.206848
-1462.289346	10.955246	2.216845
-1460.284011	11.538798	2.226842
-1458.771193	5.298572	2.236838
-1456.850808	11.996329	2.246835
-1454.735689	15.225795	2.256832
-1452.857910	-2.102569	2.266829
-1451.194735	23.942314	2.276826
-1449.204075	-16.131368	2.286822
-1447.410592	25.144135	2.296819
-1445.056274	17.283492	2.306816
-1443.578531	14.662832	2.316813
-1441.478162	-4.362092	2.326810
-1439.837672	18.628233	2.336806
-1437.980202	21.482159	2.346803
-1436.104995	10.867396	2.356800
-1434.274185	1.956991	2.366797
-1431.939032	10.149822	2.376794
-1430.167047	15.134652	2.386790
-1428.634059	16.559594	2.396787
-1427.141942	17.975292	2.406784
-1424.827945	4.967826	2.416781
-1422.804844	7.511053	2.426778
-1420.959814	17.451197	2.436774
-1418.993404	16.069058	2.446771
-1416.910727	12.333215	2.456768
-1415.434171	10.810050	2.466765
-1413.620432	5.142153	2.476762
-1411.687641	18.421691	2.486758
-1409.452095	10.491686	2.496755
-1407.594119	2.339526	2.506752
-1405.885374	0.381329	2.516749
-1404.489865	5.194362	2.526746
-1402.178863	16.814002	2.536742
-1400.040085	14.793275	2.546739
-1398.164079	12.350444	2.556736
-1396.536333	9.355297	2.566733
-1394.652162	7.991082	2.576730
-1392.917960	9.057016	2.586726
-1390.884206	10.839150	2.596723
-1389.085200	0.089795	2.606720
-1386.831460	15.048370	2.616717
-1385.211710	13.456514	2.626714
-1383.450020	9.539999	2.636710
-1381.643797	9.898148	2.646707
-1379.978700	26.000901	2.656704
-1377.801113	7.091531	2.666701
-1375.661839	4.960230	2.676698
-1373.830922	9.405182	2.686694
-1371.826798	10.371084	2.696691
-1370.207254	8.176158	2.706688
-1368.274512	4.334897	2.716685
-1366.503241	21.519527	2.726682
-1364.653573	9.917395	2.736678
-1362.837615	17.827133	2.746675
-1360.796926	7.425916	2.756672
-1358.818943	22.790228	2.766669
-1356.935049	15.428101	2.776666
-1355.348385	17.150794	2.786662
-1353.449653	4.405640	2.796659
-1351.427881	16.823160	2.806656
-1349.668243	2.158312	2.816653
-1347.528605	20.886506	2.826650
-1345.597873	3.608143	2.836646
-1344.066973	19.525576	2.846643
-1341.934709	10.668022	2.856640
-1340.140934	17.436676	2.866637
-1338.263375	-0.565744	2.876634
-1336.418291	3.929072	2.886630
-1334.476860	12.044519	2.896627
-1333.022890	15.844108	2.906624
-1330.759897	8.618676	2.916621
-1328.946558	12.742820	2.926618
-1327.079672	20.897052	2.936614
-1325.139273	11.343959	2.946611
-1323.313427	31.909661	2.956608
-1321.498240	11.512654	2.966605
-1319.515473	7.213457	2.976602
-1317.578894	25.517912	2.986598
-1315.743953	13.016653	2.996595
-1313.912743	15.939617	3.006592
-1311.909519	24.612003	3.016589
-1310.205179	11.883777	3.026586
-1308.395849	16.460127	3.036582
-1306.159091	11.967139	3.046579
-1304.465493	21.715330	3.056576
-1302.723298	8.949475	3.066573
-1300.660978	11.063409	3.076570
-1299.064738	27.350930	3.086566
-1297.096019	15.693471	3.096563
-1294.958480	12.234721	3.106560
-1293.132760	23.943212	3.116557
-1291.499160	10.533212	3.126554
-1289.267626	24.148718	3.136550
-1287.611431	11.856075	3.146547
-1285.740081	-1.615646	3.156544
-1284.031450	14.975968	3.166541
-1281.934693	15.260855	3.176538
-1280.268335	14.479447	3.186534
-1278.277826	15.269202	3.196531
-1275.977796	6.972179	3.206528
-1274.737565	16.938204	3.216525
-1272.748516	11.559694	3.226522
-1270.789419	13.897003	3.236518
-1268.634743	21.659465	3.246515
-1266.845920	4.703840	3.256512
-1265.042428	11.793083	3.266509
-1263.145397	17.108540	3.276506
-1261.232743	2.446096	3.286502
-1259.619226	11.583494	3.296499
-1257.790395	15.724166	3.306496
-1255.629225	5.475843	3.316493
-1253.874010	5.655952	3.326490
-1251.964359	10.361546	3.336486
-1250.158257	7.742137	3.346483
-1247.953253	7.937105	3.356480
-1246.356833	12.823875	3.366477
-1244.454627	13.166771	3.376474
-1242.326476	10.710551	3.386470
-1240.889073	16.922154	3.396467
-1238.661105	5.695329	3.406464
-1236.829838	5.397525	3.416461
-1235.447798	11.624304	3.426458
-1233.589168	18.616340	3.436454
-1231.367637	11.255535	3.446451
-1229.339447	3.608330	3.456448
-1227.306870	14.920641	3.466445
-1225.511251	0.737970	3.476442
-1223.640728	15.495970	3.486438
-1222.241294	23.583005	3.496435
-1220.218365	15.614561	3.506432
-1218.102696	12.010968	3.516429
-1216.220581	10.591965	3.526426
-1214.443507	21.100503	3.536422
-1212.670363	14.476153	3.546419
-1210.556216	8.504559	3.556416
-1208.831885	16.282260	3.566413
-1206.966575	22.281743	3.576410
-1205.177022	12.868129	3.586406
-1203.104448	26.259714	3.596403
-1201.008964	11.080186	3.606400
-1199.238641	19.976247	3.616397
-1197.486787	10.636561	3.626394
-1195.844657	16.640186	3.636390
-1193.765657	13.230363	3.646387
-1191.990486	19.807925	3.656384
-1189.690045	26.705627	3.666381
-1188.322674	13.350910	3.676378
-1186.238959	18.813394	3.686374
-1184.686327	16.994009	3.696371
-1182.663327	22.017823	3.706368
-1180.447108	7.043191	3.716365
-1178.945543	19.398870	3.726362
-1176.922888	21.435587	3.736358
-1174.971897	10.354174	3.746355
-1173.109957	13.711253	3.756352
-1171.192077	22.451109	3.766349
-1169.446156	16.612667	3.776346
-1167.487302	26.670617	3.786342
-1165.758660	21.521735	3.796339
-1163.717777	18.182767	3.806336
-1161.656811	25.867182	3.816333
-1160.224357	14.211944	3.826330
-1158.282995	21.770244	3.836326
-1155.982378	11.087611	3.846323
-1154.264486	17.598584	3.856320
-1152.461516	13.358284	3.866317
-1150.747513	18.529451	3.876314
-1148.606305	15.775982	3.886310
-1146.795869	4.001869	3.896307
-1144.875345	17.877274	3.906304
-1143.256263	12.365439	3.916301
-1141.259314	9.174037	3.926298
-1139.098380	10.880791	3.936294
-1137.611992	9.240971	3.946291
-1135.884861	17.971903	3.956288
-1133.898756	5.812875	3.966285
-1131.902031	17.803603	3.976282
-1129.917005	9.812877	3.986278
-1128.026430	15.873117	3.996275
-1126.075076	7.838837	4.006272
-1124.243523	18.155592	4.016269
-1122.507551	22.300182	4.026266
-1120.724145	17.949357	4.036262
-1118.605292	12.092341	4.046259
-1116.842645	7.609063	4.056256
-1115.136842	6.461487	4.066253
-1112.877712	14.774196	4.076250
-1110.936904	18.205547	4.086246
-1109.627397	19.522782	4.096243
-1107.621635	22.069070	4.106240
-1105.132709	14.976630	4.116237
-1103.949782	18.136095	4.126234
-1102.046955	9.888559	4.136230
-1099.929905	19.425507	4.146227
-1097.804729	6.960066	4.156224
-1096.193080	12.420786	4.166221
-1094.492700	23.573235	4.176218
-1092.460029	23.484888	4.186214
-1090.479410	15.813819	4.196211
-1088.801608	6.468685	4.206208
-1086.785583	13.467246	4.216205
-1085.000649	13.667991	4.226202
-1083.183850	14.364132	4.236198
-1081.073240	6.122846	4.246195
-1079.425695	13.571907	4.256192
-1077.114269	13.085325	4.266189
-1075.701593	15.808609	4.276186
-1073.808178	13.944259	4.286182
-1071.727319	20.558282	4.296179
-1069.900429	16.006341	4.306176
-1068.012357	8.967422	4.316173
-1066.166645	19.847189	4.326170
-1064.488086	4.976017	4.336166
-1062.221163	21.156460	4.346163
-1060.292246	-9.816252	4.356160
-1058.696814	18.514955	4.366157
-1056.780649	19.132070	4.376154
-1055.021948	8.547258	4.386150
-1053.161949	7.821874	4.396147
-1051.053600	19.619579	4.406144
-1049.106466	23.460471	4.416141
-1047.407540	12.201586	4.426138
-1045.520579	15.891062	4.436134
-1043.802299	16.820871	4.446131
-1041.923610	14.845224	4.456128
-1039.692135	17.106014	4.466125
-1037.937270	15.135966	4.476122
-1036.327356	10.992939	4.486118
-1034.527350	15.048413	4.496115
-1032.337599	18.566324	4.506112
-1030.415845	1.576948	4.516109
-1028.533548	10.286306	4.526106
-1026.913312	17.504532	4.536102
-1025.050192	9.029734	4.546099
-1022.674205	14.646140	4.556096
-1021.040438	5.135997	4.566093
-1019.405644	13.605496	4.576090
-1017.653416	7.529327	4.586086
-1015.531756	18.357112	4.596083
-1013.840453	20.557487	4.606080
-1011.371093	14.248215	4.616077
-1009.785389	19.266341	4.626074
-1008.435852	11.528909	4.636070
-1006.597889	17.204539	4.646067
-1004.130690	13.167570	4.656064
-1001.919972	19.861938	4.666061
-1000.518108	17.094219	4.676058
-998.487456	11.414031	4.686054
-996.643954	22.332109	4.696051
-995.009267	15.599007	4.706048
-992.808203	17.657879	4.716045
-991.232374	14.829189	4.726042
-989.019145	13.188478	4.736038
-987.575797	22.165432	4.746035
-985.630040	22.277381	4.756032
-983.497069	14.356256	4.766029
-982.103223	17.954131	4.776026
-979.962082	25.790100	4.786022
-977.776410	25.964735	4.796019
-976.093709	22.462165	4.806016
-974.185408	8.867895	4.816013
-972.115659	15.327484	4.826010
-970.356093	13.770389	4.836006
-968.572417	14.743477	4.846003
-967.002639	13.008327	4.856000
-964.401021	22.351093	4.865997
-962.955007	15.523453	4.875994
-961.224156	22.300915	4.885990
-959.486412	22.327736	4.895987
-957.258870	12.048513	4.905984
-955.543987	22.404604	4.915981
-953.280209	7.334128	4.925978
-951.887393	19.101101	4.935974
-949.835751	10.866190	4.945971
-947.917213	10.418877	4.955968
-945.990687	16.209862	4.965965
-944.075567	16.153072	4.975962
-942.341123	20.321731	4.985958
-940.723468	20.950360	4.995955
-938.475650	7.290774	5.005952
-936.586055	13.146089	5.015949
-934.877419	29.738041	5.025946
-932.846608	19.330826	5.035942
-931.208702	0.441769	5.045939
-929.272231	12.292339	5.055936
-927.442326	23.403694	5.065933
-925.503233	6.972094	5.075930
-923.351823	17.799953	5.085926
-921.891810	18.539059	5.095923
-919.524088	17.693128	5.105920
-917.912119	27.385229	5.115917
-916.136547	21.029095	5.125914
-914.227864	15.554778	5.135910
-912.339532	26.320515	5.145907
-910.274153	23.871466	5.155904
-908.499835	11.039136	5.165901
-906.772981	15.253242	5.175898
-904.999718	24.835885	5.185894
-903.072834	20.105457	5.195891
-900.886495	12.760039	5.205888
-899.079004	16.977047	5.215885
-897.278510	22.071434	5.225882
-895.521635	21.302666	5.235878
-893.631123	16.988560	5.245875
-891.370147	18.834280	5.255872
-889.584477	19.710801	5.265869
-888.196472	21.541368	5.275866
-886.013572	17.358930	5.285862
-884.036469	18.743235	5.295859
-882.283830	19.790821	5.305856
-880.478484	20.340541	5.315853
-878.701401	13.717369	5.325850
-876.860102	29.434012	5.335846
-874.635791	28.708941	5.345843
-873.082012	32.249743	5.355840
-870.935227	14.839238	5.365837
-868.999186	21.433981	5.375834
-867.299641	23.912603	5.385830
-865.458050	4.046863	5.395827
-863.429971	16.563334	5.405824
-861.724866	38.805023	5.415821
-859.745018	13.418059	5.425818
-858.016610	13.855367	5.435814
-855.939675	20.883883	5.445811
-853.993958	3.404501	5.455808
-852.405177	32.420644	5.465805
-850.952090	14.386889	5.475802
-848.113401	-7.109705	5.485798
-846.569412	31.293487	5.495795
-844.914725	11.864968	5.505792
-842.737022	15.474982	5.515789
-841.072754	23.111024	5.525786
-838.704137	-8.520784	5.535782
-837.504384	27.910209	5.545779
-835.261309	19.343222	5.555776
-833.315750	11.130097	5.565773
-831.631008	16.015687	5.575770
-829.793507	23.887713	5.585766
-827.697305	24.406768	5.595763
-826.156616	4.709141	5.605760
-824.574842	16.799659	5.615757
-822.045646	24.370084	5.625754
-820.101312	10.995928	5.635750
-818.577732	23.465208	5.645747
-816.883671	19.414651	5.655744
-814.499667	15.214340	5.665741
-812.895791	19.681848	5.675738
-811.225414	25.989132	5.685734
-809.017934	14.671200	5.695731
-806.991341	5.180493	5.705728
-805.252666	31.455536	5.715725
-803.584694	23.244167	5.725722
-801.794682	14.547539	5.735718
-799.807314	8.492350	5.745715
-797.840842	14.603901	5.755712
-795.846307	13.658280	5.765709
-794.084660	20.017298	5.775706
-792.041182	21.943667	5.785702
-790.462805	15.409154	5.795699
-788.432968	17.329812	5.805696
-786.588754	14.767809	5.815693
-784.685210	29.825687	5.825690
-783.045042	18.964741	5.835686
-780.963430	19.563533	5.845683
-779.127205	15.836047	5.855680
-777.261288	13.573720	5.865677
-775.221804	4.864082	5.875674
-773.412747	16.777798	5.885670
-771.582368	22.072761	5.895667
-769.722864	6.489190	5.905664
-767.880097	1.646008	5.915661
-765.803774	22.854290	5.925658
-764.003645	13.076141	5.935654
-762.073431	13.896503	5.945651
-760.598636	15.842741	5.955648
-758.461476	12.242426	5.965645
-756.266650	10.497510	5.975642
-754.721047	5.433426	5.985638
-752.833105	13.101675	5.995635
-750.972020	28.521610	6.005632
-748.975362	15.709099	6.015629
-747.459465	20.359651	6.025626
-745.474789	18.455711	6.035622
-743.296797	15.680933	6.045619
-741.446552	7.423115	6.055616
-739.515268	20.583562	6.065613
-737.746532	17.397383	6.075610
-736.093392	8.571107	6.085606
-734.230090	14.898137	6.095603
-732.140565	25.499264	6.105600
-730.127182	18.341092	6.115597
-728.467132	16.301163	6.125594
-726.466899	16.936691	6.135590
-724.768668	19.436154	6.145587
-722.830479	18.856418	6.155584
-721.127372	18.930000	6.165581
-718.950631	12.577784	6.175578
-717.260060	19.503976	6.185574
-715.262880	25.032842	6.195571
-713.578661	0.111618	6.205568
-711.452597	21.858291	6.215565
-709.449156	29.039213	6.225562
-707.777230	27.747350	6.235558
-705.931271	13.324848	6.245555
-704.278477	34.981399	6.255552
-701.787605	13.843635	6.265549
-700.314884	22.445073	6.275546
-698.623124	16.948742	6.285542
-696.429484	12.464776	6.295539
-694.739509	13.418313	6.305536
-692.782392	12.968199	6.315533
-691.084788	15.881444	6.325530
-688.963507	21.006842	6.335526
-687.092452	12.976244	6.345523
-685.062140	27.696613	6.355520
-683.242120	15.185513	6.365517
-681.673117	20.018665	6.375514
-679.582779	16.040661	6.385510
-677.779411	20.321664	6.395507
-675.955507	22.862658	6.405504
-673.855951	2.616355	6.415501
-672.179483	25.713781	6.425498
-670.286030	18.347464	6.435494
-668.638449	22.942296	6.445491
-666.394935	18.246714	6.455488
-664.696228	10.245250	6.465485
-662.876152	15.205654	6.475482
-660.959775	20.993778	6.485478
-658.950082	29.694176	6.495475
-657.044548	15.326916	6.505472
-655.280391	15.932335	6.515469
-653.113376	10.134326	6.525466
-651.324930	22.924551	6.535462
-649.856421	20.460571	6.545459
-647.608086	18.745096	6.555456
-645.633971	9.537610	6.565453
-644.159480	29.898048	6.575450
-642.356615	24.702927	6.585446
-640.218715	20.557892	6.595443
-638.244603	11.530400	6.605440
-636.439179	16.033723	6.615437
-634.555076	18.749856	6.625434
-632.783226	15.509574	6.635430
-630.659283	20.528820	6.645427
-629.189711	18.039421	6.655424
-627.094523	11.690840	6.665421
-624.955945	2.016600	6.675418
-623.494422	30.164410	6.685414
-621.557666	5.979662	6.695411
-619.501740	20.174980	6.705408
-617.595047	13.504438	6.715405
-615.933162	15.809275	6.725402
-614.431299	3.786398	6.735398
-612.080385	11.475536	6.745395
-609.903677	16.566890	6.755392
-608.541177	17.680169	6.765389
-606.516165	8.101447	6.775386
-604.416805	15.565538	6.785382
-602.860033	24.512017	6.795379
-600.901487	10.591036	6.805376
-599.097931	22.400010	6.815373
-596.791707	4.053247	6.825370
-595.102775	34.285150	6.835366
-593.425495	18.602898	6.845363
-591.231436	0.337217	6.855360
-589.680407	45.140237	6.865357
-587.700889	8.313147	6.875354
-586.070514	17.364711	6.885350
-584.118132	21.735662	6.895347
-582.000883	9.996569	6.905344
-579.984983	17.309817	6.915341
-578.635154	29.544958	6.925338
-576.614677	15.323588	6.935334
-574.353599	8.497000	6.945331
-572.459698	11.221091	6.955328
-570.685891	22.229630	6.965325
-568.746210	14.396559	6.975322
-567.244979	15.181405	6.985318
-565.289592	3.204519	6.995315
-563.644821	28.806431	7.005312
-561.294700	3.643114	7.015309
-559.526885	11.733327	7.025306
-557.785863	13.962411	7.035302
-555.961309	12.016314	7.045299
-553.655000	20.412073	7.055296
-552.161187	11.906600	7.065293
-550.323025	11.488236	7.075290
-548.423775	22.555700	7.085286
-546.131981	21.338608	7.095283
-544.316513	7.715241	7.105280
-542.469957	-4.026358	7.115277
-541.059214	14.413401	7.125274
-538.816390	0.712309	7.135270
-536.833052	16.793392	7.145267
-535.408997	22.500801	7.155264
-533.439552	23.002473	7.165261
-531.245900	4.463754	7.175258
-529.327012	13.132982	7.185254
-527.835985	25.187718	7.195251
-525.963516	19.825257	7.205248
-523.735828	4.981925	7.215245
-522.258151	14.110029	7.225242
-520.069499	12.003178	7.235238
-517.988682	25.252058	7.245235
-516.236851	7.069687	7.255232
-514.935782	10.987390	7.265229
-512.630902	12.884884	7.275226
-510.614096	0.909280	7.285222
-508.975122	5.775583	7.295219
-507.094618	16.809761	7.305216
-505.099890	16.385372	7.315213
-503.498503	6.092858	7.325210
-501.372820	9.302586	7.335206
-499.371973	15.655215	7.345203
-497.410586	23.087768	7.355200
-495.755657	16.279114	7.365197
-493.896729	16.231663	7.375194
-492.038595	22.324482	7.385190
-490.229648	8.725871	7.395187
-488.269295	20.386750	7.405184
-486.262280	6.688619	7.415181
-484.253700	13.925760	7.425178
-482.885882	11.468488	7.435174
-480.989254	18.243544	7.445171
-478.929140	17.308238	7.455168
-476.836266	10.859102	7.465165
-475.321151	13.061173	7.475162
-473.365682	10.434272	7.485158
-471.293808	11.454866	7.495155
-469.334616	13.074473	7.505152
-467.565018	8.156355	7.515149
-465.720839	16.384444	7.525146
-463.777770	11.951749	7.535142
-462.153786	14.730089	7.545139
-460.264330	1.004970	7.555136
-457.938212	13.850012	7.565133
-456.444923	13.952555	7.575130
-454.754834	6.099434	7.585126
-452.611776	27.071639	7.595123
-450.630379	11.399321	7.605120
-448.922240	11.827537	7.615117
-446.848851	9.928620	7.625114
-445.024960	12.613473	7.635110
-443.548455	18.779905	7.645107
-441.387185	14.893398	7.655104
-439.321730	4.383139	7.665101
-437.323034	21.592330	7.675098
-435.616830	17.873227	7.685094
-433.746175	9.954969	7.695091
-431.982978	16.705587	7.705088
-430.069355	16.022649	7.715085
-428.176105	11.959493	7.725082
-426.722691	22.790387	7.735078
-424.398965	24.264987	7.745075
-422.390447	11.027681	7.755072
-420.875964	23.738710	7.765069
-418.710448	11.548375	7.775066
-416.803651	22.733169	7.785062
-415.079239	15.111414	7.795059
-413.373226	19.479224	7.805056
-411.275316	15.596544	7.815053
-409.352601	21.205465	7.825050
-407.572444	26.042991	7.835046
-405.645791	18.420525	7.845043
-403.756501	25.803101	7.855040
-401.759813	19.951976	7.865037
-400.467611	-0.125760	7.875034
-398.270094	27.918946	7.885030
-396.336359	-0.022852	7.895027
-394.501579	20.330779	7.905024
-392.489927	3.051145	7.915021
-390.799956	27.280302	7.925018
-388.708507	14.143452	7.935014
-386.722441	18.614978	7.945011
-384.945796	15.773555	7.955008
-383.124304	16.079515	7.965005
-380.941831	26.942452	7.975002
-379.622595	20.127469	7.984998
-377.568815	20.232145	7.994995
-375.664245	14.893087	8.004992
-374.140189	9.040086	8.014989
-372.181279	42.746812	8.024986
-369.935654	25.598747	8.034982
-368.283649	13.458860	8.044979
-366.093443	14.212774	8.054976
-364.238352	19.156782	8.064973
-362.972154	23.116460	8.074970
-360.815389	24.436212	8.084966
-358.572095	31.950195	8.094963
-356.942233	22.944706	8.104960
-355.021666	19.565620	8.114957
-353.279096	19.999459	8.124954
-351.174071	16.627241	8.134950
-349.319336	29.790820	8.144947
-347.666720	13.447943	8.154944
-345.833957	29.340129	8.164941
-343.708670	13.835947	8.174938
-341.767622	15.265939	8.184934
-340.049219	9.692963	8.194931
-338.011536	25.342449	8.204928
-336.430617	22.252850	8.214925
-334.368968	21.287424	8.224922
-332.650905	16.379201	8.234918
-330.406688	13.436331	8.244915
-328.720466	20.082488	8.254912
-326.701292	13.795228	8.264909
-324.904432	7.322424	8.274906
-323.386860	23.234943	8.284902
-321.572803	22.645349	8.294899
-319.384212	20.923926	8.304896
-317.249052	16.861704	8.314893
-315.460005	45.716973	8.324890
-314.058348	3.296804	8.334886
-311.926645	24.218875	8.344883
-309.798862	16.810671	8.354880
-308.043494	24.525743	8.364877
-306.442353	4.839212	8.374874
-304.431636	25.379578	8.384870
-302.383526	22.411199	8.394867
-300.519032	27.990039	8.404864
-298.681689	22.030226	8.414861
-296.904624	32.654830	8.424858
-295.218723	30.645800	8.434854
-293.126267	24.462119	8.444851
-291.174349	24.065266	8.454848
-289.111799	22.832908	8.464845
-287.631884	8.169115	8.474842
-285.514820	18.834177	8.484838
-283.852322	14.500085	8.494835
-281.993770	19.680437	8.504832
-279.685259	18.751437	8.514829
-278.072686	23.963164	8.524826
-276.384862	15.734742	8.534822
-274.419224	21.910052	8.544819
-272.471206	19.268708	8.554816
-270.629539	18.398446	8.564813
-268.774886	24.869355	8.574810
-267.163428	19.714522	8.584807
-264.862822	17.675286	8.594803
-262.830456	17.440867	8.604800
-261.219682	28.150459	8.614797
-259.324283	13.560874	8.624794
-257.570934	18.022292	8.634791
-255.564540	19.295092	8.644787
-253.417395	24.429406	8.654784
-252.058453	20.750064	8.664781
-249.689866	24.044409	8.674778
-248.217417	20.146438	8.684775
-246.252444	20.623800	8.694771
-244.258335	21.153352	8.704768
-242.440086	26.938557	8.714765
-240.761152	19.393639	8.724762
-238.640290	11.981862	8.734759
-236.862810	17.104142	8.744755
-235.003913	21.562943	8.754752
-233.157371	11.662474	8.764749
-231.192921	13.278284	8.774746
-229.307939	20.042787	8.784743
-227.343156	27.377155	8.794739
-225.448717	19.897318	8.804736
-223.904488	13.155445	8.814733
-222.021408	20.509170	8.824730
-219.900556	12.352191	8.834727
-217.931968	12.911099	8.844723
-216.065554	10.074416	8.854720
-213.764590	6.418427	8.864717
-212.434740	16.779749	8.874714
-210.772995	18.691767	8.884711
-208.636460	2.999593	8.894707
-206.697518	10.704389	8.904704
-204.899145	17.964284	8.914701
-203.089240	10.242185	8.924698
-201.226994	21.404287	8.934695
-199.235114	7.961384	8.944691
-197.566472	2.134356	8.954688
-195.472678	23.310485	8.964685
-193.451934	-0.603232	8.974682
-192.241487	30.254886	8.984679
-189.775717	-11.419310	8.994675
-187.983554	22.783118	9.004672
-186.316510	-1.262032	9.014669
-184.300961	9.904032	9.024666
-182.676844	20.294201	9.034663
-180.397611	6.289170	9.044659
-178.732570	8.739071	9.054656
-176.843519	9.272813	9.064653
-174.886578	21.109787	9.074650
-172.768397	15.713107	9.084647
-171.435762	8.997136	9.094643
-169.229876	8.247241	9.104640
-167.311306	5.989604	9.114637
-165.327115	8.666465	9.124634
-163.544066	5.653662	9.134631
-161.850729	9.742647	9.144627
-160.249640	22.313748	9.154624
-157.977898	9.209874	9.164621
-156.467587	1.073014	9.174618
-154.129321	22.281225	9.184615
-152.295294	12.221763	9.194611
-150.307999	14.225550	9.204608
-148.666900	19.172306	9.214605
-146.792993	8.948600	9.224602
-145.087407	21.814073	9.234599
-143.208802	15.596749	9.244595
-141.195987	14.741905	9.254592
-138.727401	0.943525	9.264589
-137.749474	16.643893	9.274586
-135.415934	22.204865	9.284583
-133.585195	7.706202	9.294579
-131.751526	12.131218	9.304576
-129.985978	3.191058	9.314573
-128.096903	15.814117	9.324570
-126.210322	-4.571513	9.334567
-124.295250	21.533968	9.344563
-122.127857	-4.386143	9.354560
-120.502256	30.722377	9.364557
-118.797939	-1.843459	9.374554
-116.623717	9.908368	9.384551
-114.986901	19.535556	9.394547
-113.018755	5.993874	9.404544
-110.957526	20.891454	9.414541
-109.391229	19.608960	9.424538
-107.089870	14.541508	9.434535
-105.665844	25.077344	9.444531
-103.655406	11.516284	9.454528
-101.693480	3.975251	9.464525
-99.879459	25.347697	9.474522
-98.092253	21.082242	9.484519
-96.252737	24.776926	9.494515
-94.374698	15.575690	9.504512
-92.513436	17.099138	9.514509
-89.973530	13.294618	9.524506
-88.808346	13.528681	9.534503
-86.972152	12.632590	9.544499
-84.630967	3.082755	9.554496
-82.801126	21.726009	9.564493
-81.109056	9.685674	9.574490
-79.395293	21.299445	9.584487
-77.473757	9.192505	9.594483
-75.518951	14.264517	9.604480
-73.554203	15.370441	9.614477
-71.984828	10.107187	9.624474
-69.822982	24.608257	9.634471
-67.836440	-3.493370	9.644467
-66.175555	29.553910	9.654464
-64.253543	10.880437	9.664461
-62.145450	28.413602	9.674458
-60.344957	15.855479	9.684455
-58.574604	21.981612	9.694451
-56.840614	19.368265	9.704448
-54.962023	38.441133	9.714445
-52.831499	18.532882	9.724442
-51.173547	30.523461	9.734439
-49.577845	7.890181	9.744435
-47.259303	33.666155	9.754432
-45.179877	20.124120	9.764429
-43.633652	12.374719	9.774426
-41.641711	46.712858	9.784423
-39.793995	26.909716	9.794419
-37.829912	22.470831	9.804416
-35.916939	15.665502	9.814413
-34.287223	21.626205	9.824410
-32.478481	26.634722	9.834407
-30.554111	21.108030	9.844403
-28.334602	31.599130	9.854400
-26.431104	12.333401	9.864397
-24.946622	23.527505	9.874394
-23.195518	27.605804	9.884391
-21.232232	23.523880	9.894387
-19.250875	10.534327	9.904384
-17.271963	28.326553	9.914381
-15.390375	21.613079	9.924378
-13.554424	12.824379	9.934375
-11.779194	18.670312	9.944371
-9.848723	9.276046	9.954368
-7.915423	15.298861	9.964365
-6.029600	19.575143	9.974362
-4.228090	21.390808	9.984359
-3.181354	43.744665	9.994355
-1.987279	99.685910	10.004352
-0.659694	159.793246	10.014349
0.000000	218.661890	10.019354
0.728755	249.609809	10.024359
1.258815	296.897451	10.029363
1.700250	333.653258	10.034368
2.015198	368.153903	10.039373
2.421934	397.354289	10.044378
3.121243	421.394239	10.049383
3.029198	431.926719	10.054387
3.575248	458.684492	10.059392
3.908411	470.503722	10.064397
3.709782	465.801583	10.069402
4.002170	478.037313	10.074407
4.083981	479.195885	10.079411
4.264151	477.371064	10.084416
4.333462	501.150528	10.089421
4.278159	505.103146	10.094426
4.800094	519.315987	10.099431
4.947215	507.429556	10.104435
4.593001	504.050003	10.109440
4.667586	501.429922	10.114445
4.545981	512.566394	10.119450
4.509943	495.921745	10.124455
4.456115	525.866033	10.129459
4.827048	544.280174	10.134464
5.019269	524.197722	10.139469
5.043847	532.300604	10.144474
5.332871	539.820434	10.149479
5.058453	544.399348	10.154483
4.985202	546.090419	10.159488
5.003091	537.327907	10.164493
5.135971	540.883102	10.169498
5.226892	547.876315	10.174503
5.069212	559.671411	10.179507
5.443021	544.276466	10.184512
5.465148	549.956061	10.189517
5.127181	563.684808	10.194522
5.234985	558.597882	10.199527
5.354722	574.702554	10.204531
5.300773	552.057447	10.209536
5.425549	575.255772	10.214541
5.408833	558.787736	10.219546
5.558951	557.089120	10.224551
5.331211	576.854005	10.229555
5.452313	558.981045	10.234560
5.551401	573.236156	10.239565
5.203048	559.746163	10.244570
5.775586	575.840111	10.249575
5.856028	598.711243	10.254579
6.326333	594.206706	10.259584
6.072276	563.023047	10.264589
5.869322	590.640101	10.269594
6.110130	569.352969	10.274599
5.690587	599.906080	10.279603
6.208510	594.433614	10.284608
6.114538	596.837601	10.289613
6.188179	604.240438	10.294618
6.448126	611.637215	10.299623
6.500808	601.705361	10.304627
6.267039	636.737279	10.309632
6.734430	614.559257	10.314637
6.438559	609.910428	10.319642
6.675403	610.585403	10.324647
6.340926	609.202188	10.329651
6.511542	623.084828	10.334656
6.633621	630.735411	10.339661
6.580517	630.127304	10.344666
6.742179	615.849456	10.349671
6.656220	629.429262	10.354675
6.443285	626.758828	10.359680
6.719400	629.297748	10.364685
6.535551	625.512535	10.369690
6.548424	637.849754	10.374695
6.013591	646.715267	10.379699
6.796274	631.600354	10.384704
6.851728	682.514573	10.389709
6.541116	665.836257	10.394714
6.841267	693.321221	10.399719
6.984883	660.976390	10.404723
6.901133	696.982708	10.409728
6.684947	668.555531	10.414733
7.097487	687.757981	10.419738
7.467610	690.228303	10.424743
7.319571	710.731267	10.429747
7.578073	700.686093	10.434752
7.671179	711.734856	10.439757
7.552471	702.522535	10.444762
7.682530	722.629506	10.449767
7.778519	697.400924	10.454771
7.431889	715.653779	10.459776
7.681911	724.594420	10.464781
7.586439	712.085789	10.469786
7.792282	716.780536	10.474791
7.736053	731.953110	10.479795
7.869134	711.889293	10.484800
7.898868	728.134645	10.489805
7.724199	730.075296	10.494810
8.182615	721.502599	10.499815
8.152725	718.858143	10.504819
7.757963	735.172789	10.509824
8.131486	715.311883	10.514829
7.480371	732.213027	10.519834
8.127358	727.569884	10.524839
7.941928	728.630756	10.529843
8.198871	766.358511	10.534848
8.561993	756.123150	10.539853
8.384167	757.936579	10.544858
8.416967	757.264304	10.549863
8.647559	767.417566	10.554867
8.956323	749.951245	10.559872
8.553719	753.596635	10.564877
8.342554	740.876203	10.569882
8.529322	757.290501	10.574887
8.542821	745.362112	10.579891
8.533180	779.540206	10.584896
8.939948	744.904526	10.589901
8.738221	790.293629	10.594906
8.837277	766.554628	10.599911
8.858411	773.740427	10.604915
8.890499	781.511097	10.609920
8.895253	770.560197	10.614925
8.912354	793.675124	10.619930
9.020807	765.517668	10.624935
9.035583	793.382647	10.629939
9.033427	767.125675	10.634944
8.752187	791.847760	10.639949
9.046882	788.334673	10.644954
9.214275	803.424346	10.649959
9.112077	818.288958	10.654963
9.631586	803.070769	10.659968
9.151049	788.560876	10.664973
9.568737	820.841678	10.669978
9.430815	812.510699	10.674983
10.005908	780.579318	10.679987
9.761504	823.125836	10.684992
9.737983	815.740109	10.689997
9.685644	793.106984	10.695002
9.913311	801.559238	10.700007
9.894826	823.363158	10.705011
9.838159	792.559097	10.710016
10.051038	778.006420	10.715021
9.416831	833.094897	10.720026
9.154617	817.943035	10.725031
9.963632	781.369720	10.730035
9.659857	808.323617	10.735040
9.723217	825.169253	10.740045
10.302054	819.478834	10.745050
10.460299	850.886469	10.750055
10.449299	830.665699	10.755059
10.297380	836.177628	10.760064
10.919075	792.555341	10.765069
10.530326	825.519859	10.770074
11.237172	797.708433	10.775079
10.440814	810.048720	10.780083
10.526203	827.884308	10.785088
10.694964	801.629973	10.790093
10.572790	827.121515	10.795098
10.351522	817.428748	10.800103
10.315810	816.240705	10.805107
10.181218	821.273634	10.810112
10.572763	807.256969	10.815117
10.560209	855.667451	10.820122
10.911322	831.725716	10.825127
10.804840	861.671211	10.830131
11.176567	829.817890	10.835136
10.962189	868.595630	10.840141
10.993887	835.229065	10.845146
10.883695	862.204223	10.850151
11.116518	855.484053	10.855155
11.133282	849.653043	10.860160
11.173439	832.926469	10.865165
11.078496	867.479493	10.870170
11.106527	845.806431	10.875175
10.973360	846.225050	10.880179
11.124644	867.315995	10.885184
11.227798	845.962106	10.890189
11.160264	867.214106	10.895194
11.839415	878.915408	10.900199
11.775582	877.378613	10.905203
11.621351	875.343734	10.910208
11.692026	872.517632	10.915213
11.578512	864.023461	10.920218
11.632016	854.075533	10.925223
12.017274	882.728403	10.930227
11.904805	897.195770	10.935232
11.917607	861.775836	10.940237
11.987384	878.721435	10.945242
11.743860	879.425736	10.950247
11.792488	874.411215	10.955251
11.849266	875.458696	10.960256
12.052722	888.689811	10.965261
11.953816	897.334558	10.970266
11.723147	876.109563	10.975271
12.120443	879.159049	10.980275
11.957936	885.981539	10.985280
12.031607	883.525536	10.990285
11.966527	888.787095	10.995290
12.300887	898.826129	11.000295
12.725344	914.729614	11.005299
12.732763	918.150374	11.010304
12.654323	895.786175	11.015309
12.099805	889.027572	11.020314
12.363604	921.290567	11.025319
12.753487	911.028753	11.030323
12.719665	908.203542	11.035328
12.892311	911.661024	11.040333
12.927834	925.275347	11.045338
13.182232	925.146454	11.050343
13.197001	917.429719	11.055347
13.047231	906.180091	11.060352
12.815251	900.437622	11.065357
12.490878	894.768238	11.070362
12.730050	909.116452	11.075367
13.058238	922.373434	11.080371
12.989760	931.554237	11.085376
13.316375	926.331358	11.090381
13.166779	925.863207	11.095386
13.099296	932.309444	11.100391
13.241984	935.746479	11.105395
13.183077	935.334826	11.110400
13.332586	922.299664	11.115405
13.063170	932.774067	11.120410
13.138121	934.517237	11.125415
13.510722	944.305778	11.130419
13.603884	947.913140	11.135424
13.560885	949.173658	11.140429
13.734890	955.482040	11.145434
13.878635	958.545177	11.150439
13.969574	953.246339	11.155443
14.014595	959.835491	11.160448
13.967292	929.567382	11.165453
13.621193	933.492382	11.170458
13.717410	932.469365	11.175463
14.199465	942.117446	11.180467
13.956085	951.188965	11.185472
14.085682	942.550315	11.190477
14.314617	951.548076	11.195482
14.136968	939.579054	11.200487
14.007611	940.356610	11.205491
13.936777	964.152881	11.210496
14.418881	951.633919	11.215501
14.235863	952.710191	11.220506
14.280493	954.981744	11.225511
14.456182	952.602497	11.230515
14.216164	956.581546	11.235520
14.644902	946.370279	11.240525
14.301803	951.882784	11.245530
14.795029	945.833814	11.250535
14.452204	952.158399	11.255539
14.243236	954.503516	11.260544
14.573009	945.727281	11.265549
14.334404	967.202255	11.270554
14.545649	960.045512	11.275559
15.031649	966.174826	11.280563
14.787413	985.133927	11.285568
15.025276	994.108213	11.290573
15.219545	966.034450	11.295578
15.244205	985.062624	11.300583
14.883698	953.125554	11.305587
15.000807	990.411001	11.310592
15.419866	954.364649	11.315597
15.420270	991.734946	11.320602
15.173554	939.579119	11.325607
15.162331	966.336837	11.330611
15.358804	966.835344	11.335616
15.735631	962.867573	11.340621
15.365601	979.722592	11.345626
15.854439	947.189596	11.350631
15.542010	941.822637	11.355635
15.010477	959.132319	11.360640
15.108858	963.424822	11.365645
15.382807	980.320628	11.370650
15.546310	973.087916	11.375655
15.674317	993.862638	11.380659
15.740149	982.420868	11.385664
15.841630	970.970266	11.390669
15.794230	1010.809843	11.395674
15.991221	960.202692	11.400679
15.955400	994.771821	11.405683
15.875879	972.814528	11.410688
15.852347	996.128647	11.415693
15.926237	978.615936	11.420698
15.852576	979.692114	11.425703
16.236614	983.210513	11.430707
15.587630	999.275845	11.435712
16.739817	982.855849	11.440717
16.233140	999.319527	11.445722
16.319637	1015.483609	11.450727
16.520168	1002.471776	11.455731
16.542579	1011.407899	11.460736
16.673485	1010.608001	11.465741
16.613846	996.574809	11.470746
16.010901	994.430135	11.475751
16.644748	1007.307285	11.480755
17.023150	1014.459873	11.485760
16.951787	1012.052213	11.490765
16.457948	1006.608510	11.495770
16.742480	1023.430138	11.500775
17.164151	1007.982915	11.505779
16.789699	1020.486317	11.510784
17.262457	1022.143970	11.515789
16.433174	1000.851845	11.520794
16.922472	1013.040854	11.525799
16.903456	1009.874218	11.530803
16.855352	1026.231668	11.535808
17.226781	999.764876	11.540813
17.271946	1033.140048	11.545818
17.428349	1005.983722	11.550823
17.128268	1027.314050	11.555827
17.091255	1003.545901	11.560832
17.244872	1027.251283	11.565837
17.326101	1015.803876	11.570842
17.593744	1020.167169	11.575847
17.614654	1020.330983	11.580851
17.298183	1001.442332	11.585856
17.208492	1025.577601	11.590861
17.273599	1025.054701	11.595866
17.241880	1007.995614	11.600871
17.237189	1044.493232	11.605875
17.544845	1023.825552	11.610880
18.150187	1062.719069	11.615885
17.904600	1034.620713	11.620890
18.026620	1064.470257	11.625895
17.904369	1033.608334	11.630899
17.685079	1058.948618	11.635904
17.811472	1033.077513	11.640909
17.899386	1059.368584	11.645914
17.927555	1052.215766	11.650919
18.305799	1037.521336	11.655923
17.878286	1040.814378	11.660928
18.324086	1046.500708	11.665933
18.507447	1048.463143	11.670938
18.518058	1033.546657	11.675943
18.487961	1058.214946	11.680947
18.431078	1043.686106	11.685952
18.659416	1041.326832	11.690957
18.333665	1038.950281	11.695962
18.712636	1057.521493	11.700967
18.706956	1032.920399	11.705971
18.641338	1035.310473	11.710976
18.651476	1053.022724	11.715981
18.613819	1056.006007	11.720986
18.683232	1044.049530	11.725991
18.779035	1036.296153	11.730995
18.485302	1046.777670	11.736000
18.976018	1049.465364	11.741005
18.894534	1051.345463	11.746010
19.160487	1018.997666	11.751015
18.801936	1055.269479	11.756019
18.992318	1049.049575	11.761024
19.023452	1045.996358	11.766029
18.919453	1068.487645	11.771034
19.200225	1057.874124	11.776039
19.262049	1068.464526	11.781043
19.026652	1082.611063	11.786048
19.284999	1082.655005	11.791053
19.068808	1082.430860	11.796058
19.035309	1084.022612	11.801063
19.662500	1080.003838	11.806067
19.387124	1076.168448	11.811072
19.588003	1076.139555	11.816077
19.640046	1079.455464	11.821082
19.724766	1077.448675	11.826087
19.953324	1077.215094	11.831091
19.477404	1086.336403	11.836096
19.833472	1080.698763	11.841101
19.601185	1076.629419	11.846106
19.655607	1080.025374	11.851111
19.734936	1071.457744	11.856115
19.717643	1074.270625	11.861120
19.871696	1076.455358	11.866125
19.649200	1087.009120	11.871130
19.857973	1100.794670	11.876135
20.429151	1094.502972	11.881139
20.591401	1102.680409	11.886144
20.697300	1075.949901	11.891149
20.169578	1080.089989	11.896154
20.171219	1077.536633	11.901159
20.650746	1061.592846	11.906163
20.169031	1053.713954	11.911168
20.410660	1061.907092	11.916173
20.100910	1072.101023	11.921178
20.852724	1076.883849	11.926183
20.622450	1059.943102	11.931187
20.268510	1069.582685	11.936192
20.686997	1077.388078	11.941197
21.178318	1092.673969	11.946202
20.766442	1073.488203	11.951207
20.890341	1051.398996	11.956211
20.712953	1064.796674	11.961216
20.632374	1067.758420	11.966221
20.904851	1077.082052	11.971226
21.235261	1082.096097	11.976231
21.239885	1070.113662	11.981235
20.676400	1064.610081	11.986240
21.199250	1073.857507	11.991245
21.216434	1078.440539	11.996250
20.762588	1081.111739	12.001255
21.144845	1091.034460	12.006259
21.248838	1092.968559	12.011264
21.206625	1090.579891	12.016269
21.083729	1099.968176	12.021274
21.033893	1106.673450	12.026279
21.546783	1089.282974	12.031283
21.495341	1102.103934	12.036288
21.388549	1093.228508	12.041293
21.378442	1082.699211	12.046298
21.265118	1114.407778	12.051303
21.150098	1078.722271	12.056307
20.999906	1111.058031	12.061312
21.610009	1077.709037	12.066317
21.323498	1101.785940	12.071322
21.052880	1103.011813	12.076327
21.306152	1097.248637	12.081331
21.630752	1106.157120	12.086336
21.373327	1086.164532	12.091341
21.222526	1110.828508	12.096346
21.248009	1113.883733	12.101351
21.269591	1101.983723	12.106355
21.174066	1095.676937	12.111360
21.383896	1100.500485	12.116365
21.224555	1103.738152	12.121370
21.275103	1092.136306	12.126375
21.549620	1108.191655	12.131379
21.365559	1110.832446	12.136384
21.597083	1111.017862	12.141389
21.779539	1106.992745	12.146394
21.813184	1098.908626	12.151399
21.558048	1075.447962	12.156403
21.425482	1074.939243	12.161408
21.940886	1066.015057	12.166413
21.693664	1071.067613	12.171418
21.297522	1066.089273	12.176423
21.401893	1066.224007	12.181427
21.051496	1075.402558	12.186432
21.494640	1055.672010	12.191437
21.395662	1081.600270	12.196442
21.444724	1068.569960	12.201447
21.583661	1071.566079	12.206451
21.242837	1071.148925	12.211456
21.352502	1066.943040	12.216461
21.460994	1069.425198	12.221466
21.517164	1059.126622	12.226471
21.558038	1062.182535	12.231475
21.651422	1067.917200	12.236480
21.540450	1055.555823	12.241485
21.394534	1045.816189	12.246490
21.334435	1039.841245	12.251495
21.370672	1026.601706	12.256499
20.900398	1048.027019	12.261504
21.721256	1037.806763	12.266509
21.124874	1029.365856	12.271514
21.045840	1047.169593	12.276519
21.382380	1050.260347	12.281523
21.375553	1058.083105	12.286528
21.331734	1065.490720	12.291533
21.893283	1052.932193	12.296538
21.505467	1043.929733	12.301543
21.555284	1037.118821	12.306547
21.247079	1030.238860	12.311552
21.183908	1041.192953	12.316557
21.309214	1023.109016	12.321562
21.189983	1039.219207	12.326567
21.554812	1030.134556	12.331571
21.136738	1043.658913	12.336576
21.169353	1044.498949	12.341581
20.832014	1048.622855	12.346586
21.207177	1053.338015	12.351591
21.657867	1065.135836	12.356595
20.878524	1058.963366	12.361600
21.411283	1063.017882	12.366605
21.673652	1075.385065	12.371610
21.258394	1066.230850	12.376615
21.373750	1058.313493	12.381619
21.234704	1057.802654	12.386624
21.330302	1046.680937	12.391629
21.137703	1043.846331	12.396634
21.391191	1078.262283	12.401639
21.507439	1064.082700	12.406643
20.945768	1060.739256	12.411648
21.357764	1075.927395	12.416653
21.514427	1082.752686	12.421658
21.264817	1068.103174	12.426663
21.632273	1074.677221	12.431667
21.424251	1070.662355	12.436672
21.338712	1050.451589	12.441677
21.207363	1034.597382	12.446682
21.052728	1065.072949	12.451687
21.371537	1060.660244	12.456691
20.965444	1069.533862	12.461696
21.285638	1078.979194	12.466701
21.406155	1079.199662	12.471706
21.352929	1095.950669	12.476711
21.397824	1086.778240	12.481715
21.306901	1087.000893	12.486720
21.575100	1084.397135	12.491725
21.759751	1078.274327	12.496730
21.437330	1062.247138	12.501735
21.666082	1058.041186	12.506739
21.040018	1063.885870	12.511744
21.738961	1050.589494	12.516749
21.276578	1051.464327	12.521754
21.037092	1053.390128	12.526759
21.321997	1052.477356	12.531763
20.973120	1055.671126	12.536768
21.200908	1060.288370	12.541773
21.302944	1062.732133	12.546778
20.909025	1060.525722	12.551783
21.673910	1067.604079	12.556787
21.285724	1073.893373	12.561792
21.612282	1055.286864	12.566797
21.531056	1053.090504	12.571802
21.728185	1051.382757	12.576807
21.493347	1065.902927	12.581811
21.386740	1066.568051	12.586816
21.590016	1056.774291	12.591821
21.468282	1061.947177	12.596826
21.561243	1056.047161	12.601831
21.712085	1053.280777	12.606835
21.361777	1061.095243	12.611840
21.516083	1046.942723	12.616845
21.443153	1057.953578	12.621850
21.219897	1061.062658	12.626855
21.598002	1050.274347	12.631859
21.528698	1048.426169	12.636864
21.608929	1033.585311	12.641869
21.276881	1023.552106	12.646874
20.926695	1026.274572	12.651879
21.389992	1018.968789	12.656883
21.136491	1022.491114	12.661888
21.259642	1017.491466	12.666893
21.414039	1027.748529	12.671898
21.277905	1032.646159	12.676903
21.530156	1028.430159	12.681907
21.292460	1032.552360	12.686912
21.426359	1022.315528	12.691917
21.367805	1033.637885	12.696922
21.238128	1029.979541	12.701927
21.121516	1021.255535	12.706931
21.076002	1028.776943	12.711936
21.481419	1044.115909	12.716941
21.533772	1059.238391	12.721946
21.212578	1051.173048	12.726951
21.259491	1037.714178	12.731955
21.342993	1042.464816	12.736960
21.403209	1038.309405	12.741965
21.108758	1051.096539	12.746970
21.305825	1056.846201	12.751975
21.892781	1045.068950	12.756979
21.465266	1038.528136	12.761984
21.089609	1043.019273	12.766989
21.323402	1039.765000	12.771994
20.960396	1032.453810	12.776999
21.373159	1048.934897	12.782003
21.081196	1050.588370	12.787008
21.205107	1061.621448	12.792013
21.718307	1067.080995	12.797018
21.438745	1053.625297	12.802023
21.319087	1034.787211	12.807027
21.010580	1044.323337	12.812032
21.396393	1059.905142	12.817037
21.882370	1053.833631	12.822042
21.588964	1049.080185	12.827047
21.596348	1037.824311	12.832051
21.525071	1036.511035	12.837056
21.513545	1033.042003	12.842061
21.295163	1038.586686	12.847066
21.126079	1039.400546	12.852071
21.676791	1037.122318	12.857075
21.533601	1020.796930	12.862080
21.268176	1037.474483	12.867085
21.095260	1044.095280	12.872090
21.308816	1043.272737	12.877095
21.544848	1035.400799	12.882099
21.543907	1034.304963	12.887104
21.396791	1034.974970	12.892109
21.649137	1039.208245	12.897114
21.317952	1031.551360	12.902119
21.595839	1038.817764	12.907123
21.330122	1033.843864	12.912128
21.606873	1034.239684	12.917133
21.482328	1020.350862	12.922138
21.148524	1016.662002	12.927143
21.442277	1003.570644	12.932147
21.096038	1015.041373	12.937152
21.235174	1017.736253	12.942157
21.249359	1035.454146	12.947162
21.338464	1032.942040	12.952167
21.586499	1035.114930	12.957171
21.260027	1025.225914	12.962176
21.281906	1021.467705	12.967181
21.341921	1016.389819	12.972186
21.449199	1013.346541	12.977191
21.642115	1000.837393	12.982195
21.462849	1020.760730	12.987200
21.520763	1016.411728	12.992205
21.680832	1008.255455	12.997210
21.300275	1007.895102	13.002215
21.523058	1002.912683	13.007219
21.199879	1030.996028	13.012224
21.110615	1007.838599	13.017229
21.644115	1015.682385	13.022234
21.180555	1012.203455	13.027239
21.344062	1020.932576	13.032243
21.403088	1023.490425	13.037248
21.658290	1014.803313	13.042253
21.580548	1023.285488	13.047258
21.300007	1022.360404	13.052263
21.494980	1005.508012	13.057267
21.531367	1021.500322	13.062272
21.587553	1027.132095	13.067277
21.660765	1013.106082	13.072282
21.171996	1001.180323	13.077287
21.330740	982.758367	13.082291
21.043057	1015.976856	13.087296
21.314605	1014.435438	13.092301
21.472506	1002.199955	13.097306
21.222588	1037.113993	13.102311
21.571826	1003.783122	13.107315
21.261974	1022.719622	13.112320
21.066424	982.623858	13.117325
21.015589	1035.030716	13.122330
21.108273	1028.323357	13.127335
21.444334	1010.046549	13.132339
21.151394	1031.591786	13.137344
21.464281	1033.697563	13.142349
21.402417	1016.894007	13.147354
21.131642	1045.360104	13.152359
21.497851	1017.000196	13.157363
21.557697	1019.542144	13.162368
21.615354	1015.582689	13.167373
21.438339	1019.821364	13.172378
21.030954	1035.562773	13.177383
21.571455	1011.931154	13.182387
21.110320	1019.507809	13.187392
21.180215	1026.463608	13.192397
21.650357	1030.881338	13.197402
21.418838	1017.052159	13.202407
21.354867	1008.351304	13.207411
21.511585	1022.457319	13.212416
21.412286	1004.685195	13.217421
21.375018	997.257413	13.222426
21.226273	990.577541	13.227431
21.339307	992.314644	13.232435
21.114534	995.269412	13.237440
21.326597	984.435093	13.242445
21.398700	986.817385	13.247450
21.281392	995.104006	13.252455
21.471536	986.794715	13.257459
21.206146	981.325621	13.262464
21.076684	982.251429	13.267469
21.146049	1001.056453	13.272474
21.190352	1016.101328	13.277479
21.604955	1015.066947	13.282483
21.519656	1022.725584	13.287488
21.524036	1007.430074	13.292493
21.243216	999.563323	13.297498
21.147146	1000.218878	13.302503
21.373962	1002.628536	13.307507
21.403681	1002.947063	13.312512
21.248704	998.343441	13.317517
21.139287	1005.722065	13.322522
21.402208	1006.205245	13.327527
21.501888	1015.901750	13.332531
21.145549	1020.580610	13.337536
21.141247	998.802089	13.342541
21.324651	1022.797602	13.347546
21.183474	1024.289828	13.352551
21.504362	1008.136438	13.357555
21.410255	1043.867729	13.362560
21.527404	1005.002511	13.367565
21.332942	1012.355280	13.372570
21.178682	999.302268	13.377575
21.359942	1021.637599	13.382579
21.900992	1022.953201	13.387584
21.174604	999.142049	13.392589
21.280726	1006.442141	13.397594
21.306631	983.081880	13.402599
21.249300	991.324239	13.407603
21.113146	993.798097	13.412608
21.244369	1012.162764	13.417613
21.355545	1021.625628	13.422618
21.109768	1026.946019	13.427623
21.427186	1024.641926	13.432627
21.159190	1032.939987	13.437632
21.255848	1028.803998	13.442637
21.671372	1028.829178	13.447642
21.293783	1035.018994	13.452647
21.492726	1028.107030	13.457651
21.281435	1000.813819	13.462656
21.522766	1011.916440	13.467661
21.352632	1011.867876	13.472666
20.843669	991.262683	13.477671
21.235613	1014.739222	13.482675
21.432251	1022.367083	13.487680
21.570740	1030.951968	13.492685
21.551233	1013.797885	13.497690
21.034487	1002.529443	13.502695
21.343255	997.374040	13.507699
20.941638	1014.196291	13.512704
21.049461	1016.464081	13.517709
21.377821	1024.583441	13.522714
21.178379	1033.345229	13.527719
21.667856	1028.107376	13.532723
21.844659	1036.329763	13.537728
21.368054	1015.793491	13.542733
21.515180	1016.200524	13.547738
21.443771	1002.812597	13.552743
21.278721	998.743589	13.557747
21.127301	1003.479645	13.562752
21.509799	1001.991494	13.567757
21.438354	1002.160577	13.572762
21.022548	1009.794653	13.577767
21.426293	995.752206	13.582771
21.373300	1001.103340	13.587776
21.055905	1002.011816	13.592781
21.117541	1004.296433	13.597786
21.013238	1018.655387	13.602791
21.497898	1018.259534	13.607795
21.357278	1047.138535	13.612800
21.622944	1031.189469	13.617805
21.329614	1002.999439	13.622810
21.415558	1010.186058	13.627815
21.293155	1005.326504	13.632819
21.153072	997.795273	13.637824
20.993638	1026.950046	13.642829
21.348575	1031.624271	13.647834
21.417297	1015.807559	13.652839
21.726237	1025.122188	13.657843
21.524307	1032.742662	13.662848
20.947094	1007.532604	13.667853
21.346539	1017.189183	13.672858
21.003325	1016.712487	13.677863
21.483817	1027.542009	13.682867
21.237362	1047.390944	13.687872
21.440384	1020.796433	13.692877
21.556031	1036.987430	13.697882
21.204344	1038.300345	13.702887
21.334098	999.974023	13.707891
21.115895	1023.659858	13.712896
21.554304	1011.103661	13.717901
21.672278	1016.403877	13.722906
21.509698	996.317437	13.727911
21.106943	1022.226235	13.732915
21.235111	1002.260570	13.737920
21.169516	1003.385926	13.742925
21.467592	1005.837834	13.747930
21.345314	990.969395	13.752935
21.418149	1019.246595	13.757939
21.175341	1005.338804	13.762944
20.869093	1026.181261	13.767949
21.598424	999.980657	13.772954
21.581856	1038.517569	13.777959
21.390370	1009.448692	13.782963
21.204825	1015.565291	13.787968
21.126539	1013.824206	13.792973
21.305754	999.979994	13.797978
21.446065	1047.537266	13.802983
21.138347	998.186887	13.807987
21.491648	1039.709889	13.812992
21.561155	1017.794988	13.817997
21.840280	1028.096812	13.823002
21.373213	999.245374	13.828007
21.292465	1023.328752	13.833011
21.628415	999.083231	13.838016
21.054413	1005.829485	13.843021
21.519176	999.986884	13.848026
21.081342	1015.219043	13.853031
21.522135	1008.870908	13.858035
21.731235	1002.526613	13.863040
21.353016	1013.352740	13.868045
21.631464	1017.315342	13.873050
21.206214	1007.344323	13.878055
21.280238	1023.999257	13.883059
21.679536	1019.151105	13.888064
21.276120	1000.646903	13.893069
21.362738	1022.768674	13.898074
21.255694	1025.323049	13.903079
21.280171	1009.037163	13.908083
21.305519	1025.797634	13.913088
21.164260	1000.410822	13.918093
21.196906	1006.114149	13.923098
21.011532	1015.654271	13.928103
21.058625	1015.425980	13.933107
21.274671	1013.284713	13.938112
21.245028	1013.943867	13.943117
21.168296	1015.987206	13.948122
21.050164	1027.976647	13.953127
21.133358	1023.374453	13.958131
21.438194	1019.266763	13.963136
20.928992	1012.526102	13.968141
21.239247	1034.575951	13.973146
21.550234	1056.745565	13.978151
21.308274	1031.732728	13.983155
21.359623	1034.873697	13.988160
21.255722	1024.073975	13.993165
21.420501	1016.147181	13.998170
20.975834	1039.277807	14.003175
21.449120	1045.068563	14.008179
21.561226	1044.530282	14.013184
21.150708	1039.242009	14.018189
21.564335	1035.856028	14.023207
21.474454	1027.503966	14.028224
21.304770	1000.495613	14.033242
21.284910	1026.846816	14.038259
21.229098	1010.950302	14.043277
21.672935	999.526148	14.048295
21.431604	1027.204045	14.053312
21.157531	1023.688223	14.058330
21.484962	1035.599661	14.063347
21.487320	1047.874397	14.068365
21.779359	1043.626522	14.073383
21.336512	1057.087480	14.078400
21.382448	1052.307883	14.083418
21.473321	1063.918895	14.088435
21.636501	1054.124975	14.093453
21.696295	1065.078743	14.098471
21.690582	1071.218791	14.103488
21.624815	1060.610428	14.108506
22.014680	1053.833408	14.113523
21.488377	1052.946849	14.118541
21.870230	1039.943892	14.123559
21.745924	1027.432213	14.128576
21.476317	1033.065384	14.133594
21.606165	1034.595571	14.138611
21.568801	1048.289131	14.143629
22.187692	1049.552566	14.148647
21.696817	1057.426284	14.153664
21.895378	1058.912482	14.158682
21.630659	1051.016130	14.163699
21.531219	1069.391206	14.168717
21.887287	1070.970253	14.173735
21.706730	1062.884302	14.178752
21.626491	1060.735889	14.183770
21.703704	1069.782065	14.188787
21.764119	1072.449549	14.193805
22.010411	1042.018139	14.198823
21.761192	1076.750393	14.203840
21.796659	1063.346514	14.208858
21.684964	1063.559365	14.213875
21.760853	1064.818180	14.218893
21.897259	1066.207334	14.223911
22.257731	1084.378521	14.228928
22.004648	1082.111390	14.233946
21.992148	1077.721754	14.238963
22.280116	1089.438196	14.243981
22.463378	1083.497882	14.248999
21.985333	1082.949669	14.254016
21.923468	1067.653345	14.259034
22.350254	1078.396014	14.264051
22.406569	1077.479444	14.269069
22.356741	1064.759237	14.274087
22.382731	1064.490832	14.279104
22.470882	1072.882500	14.284122
22.333092	1071.005944	14.289139
22.013747	1067.519354	14.294157
22.076591	1057.934905	14.299175
22.242480	1068.524136	14.304192
22.340148	1084.531993	14.309210
22.350832	1087.866469	14.314227
22.218898	1095.481621	14.319245
22.310509	1087.611780	14.324263
22.732988	1096.311911	14.329280
22.773211	1092.843464	14.334298
22.412745	1072.078491	14.339315
22.408836	1073.037021	14.344333
22.502581	1075.400332	14.349351
22.618773	1082.931860	14.354368
22.293033	1091.583025	14.359386
22.500016	1081.533576	14.364403
22.274923	1089.503337	14.369421
22.473081	1086.704937	14.374439
22.378751	1087.542619	14.379456
22.511997	1090.047488	14.384474
22.568301	1096.493814	14.389491
22.536883	1090.159901	14.394509
22.450539	1089.915705	14.399527
22.476798	1094.137978	14.404544
22.148276	1102.105367	14.409562
22.641484	1097.911902	14.414579
22.632096	1125.537262	14.419597
22.755953	1120.230864	14.424615
23.201128	1128.825154	14.429632
22.948406	1107.644991	14.434650
23.155891	1078.473323	14.439667
22.680231	1091.447219	14.444685
22.981281	1082.118899	14.449703
22.931981	1083.289151	14.454720
22.957770	1093.120572	14.459738
23.191789	1078.840346	14.464755
22.884920	1095.625275	14.469773
22.814713	1095.416256	14.474791
23.083205	1081.548928	14.479808
22.874934	1081.170032	14.484826
22.978425	1089.581284	14.489843
22.814495	1099.150404	14.494861
22.949696	1115.834962	14.499879
23.169660	1114.280416	14.504896
23.183976	1117.008740	14.509914
23.623468	1115.851737	14.514931
23.325932	1102.578009	14.519949
23.183877	1091.245659	14.524967
22.914407	1095.441173	14.529984
22.931819	1087.356664	14.535002
23.378060	1109.029704	14.540019
23.226291	1124.658990	14.545037
23.468731	1119.657703	14.550055
23.389949	1136.113734	14.555072
23.250241	1107.758684	14.560090
23.497052	1103.480256	14.565107
23.095865	1122.373834	14.570125
23.184977	1106.046710	14.575143
23.652236	1103.222689	14.580160
23.277915	1119.362491	14.585178
23.572668	1128.147504	14.590195
23.169668	1124.076526	14.595213
23.566721	1110.089572	14.600231
23.733289	1103.735085	14.605248
23.360050	1131.703192	14.610266
23.750474	1111.843949	14.615283
23.430826	1111.259460	14.620301
23.654024	1120.721233	14.625319
23.753856	1113.864609	14.630336
23.445066	1116.416393	14.635354
23.861106	1109.168010	14.640371
23.410202	1107.890344	14.645389
23.560926	1107.177352	14.650407
23.838481	1116.311146	14.655424
23.225245	1123.473000	14.660442
23.838774	1119.405048	14.665459
23.630981	1123.197499	14.670477
23.454015	1121.909171	14.675495
23.749222	1121.437386	14.680512
23.710567	1119.946110	14.685530
24.006515	1114.679902	14.690547
23.613068	1126.740999	14.695565
23.802692	1122.183838	14.700583
24.142511	1117.783611	14.705600
23.810707	1129.493551	14.710618
24.099007	1127.245450	14.715635
23.912201	1118.827002	14.720653
23.847859	1117.077143	14.725671
23.940342	1120.131182	14.730688
23.992100	1119.998657	14.735706
23.983888	1117.683027	14.740723
23.656609	1133.555807	14.745741
23.697813	1129.826088	14.750759
23.889340	1115.039826	14.755776
23.795901	1125.544627	14.760794
24.058144	1148.083875	14.765811
24.089094	1158.666381	14.770829
23.938786	1156.164208	14.775847
24.392348	1149.609779	14.780864
24.162060	1155.650409	14.785882
24.571619	1153.327911	14.790899
24.253677	1157.501287	14.795917
24.454296	1150.977764	14.800935
24.552769	1158.424072	14.805952
24.196408	1164.489533	14.810970
24.406986	1122.063698	14.815987
24.671843	1159.009068	14.821005
24.326354	1109.422285	14.826023
24.528355	1127.739918	14.831040
24.300139	1136.764070	14.836058
24.293266	1099.360768	14.841075
24.380753	1129.573889	14.846093
24.685796	1133.791031	14.851111
24.392745	1141.878619	14.856128
24.174058	1136.463265	14.861146
24.555284	1150.134199	14.866163
24.587202	1132.314012	14.871181
24.426509	1161.462582	14.876199
24.820693	1154.275862	14.881216
24.607230	1142.169965	14.886234
25.134305	1162.586000	14.891251
24.612588	1127.795601	14.896269
23.976559	1149.897710	14.901287
24.843364	1133.058000	14.906304
24.351256	1137.886753	14.911322
24.666439	1140.208464	14.916339
24.822130	1140.542254	14.921357
24.649225	1158.809617	14.926375
25.069796	1132.457166	14.931392
24.667276	1141.120606	14.936410
24.972238	1152.807648	14.941427
25.248062	1141.304794	14.946445
24.463429	1132.674967	14.951463
24.965228	1149.758817	14.956480
24.752430	1157.459255	14.961498
25.009007	1139.612664	14.966515
24.715196	1147.624875	14.971533
24.888929	1138.988471	14.976551
24.907726	1138.600096	14.981568
25.025120	1146.762213	14.986586
24.918123	1150.872057	14.991603
24.775870	1144.735113	14.996621
24.775793	1149.682008	15.001639
24.970002	1170.012726	15.006656
25.223901	1173.366629	15.011674
25.391784	1180.940297	15.016691
25.813544	1171.155390	15.021709
25.652245	1165.713569	15.026727
25.692740	1155.712645	15.031744
25.615794	1141.225567	15.036762
25.110689	1141.255789	15.041779
25.182209	1152.810187	15.046797
25.317420	1140.099724	15.051815
25.387880	1141.016512	15.056832
25.510908	1156.559533	15.061850
25.526972	1129.703773	15.066867
25.564269	1145.362697	15.071885
25.117854	1145.846001	15.076903
24.975538	1154.496260	15.081920
24.888651	1159.968210	15.086938
25.224234	1157.094398	15.091955
25.455239	1165.751184	15.096973
25.370233	1181.841764	15.101991
25.760708	1166.811371	15.107008
25.538381	1182.824759	15.112026
25.600663	1178.992570	15.117043
25.703668	1191.816061	15.122061
25.541523	1165.619409	15.127079
25.926474	1173.652355	15.132096
25.658696	1177.723360	15.137114
25.955138	1170.490877	15.142131
26.053746	1181.407083	15.147149
25.754767	1170.310474	15.152167
26.262105	1153.298426	15.157184
25.925339	1144.359644	15.162202
25.569973	1135.442710	15.167219
25.792575	1151.935627	15.172237
25.518379	1132.674691	15.177255
25.825946	1153.885453	15.182272
25.998011	1145.329531	15.187290
25.983602	1146.280303	15.192307
25.945388	1147.793266	15.197325
25.752489	1162.070133	15.202343
26.094276	1160.818605	15.207360
26.277737	1175.400379	15.212378
25.852097	1172.561466	15.217395
26.034406	1163.176532	15.222413
26.094015	1170.740725	15.227431
26.098986	1172.935750	15.232448
25.992353	1185.062827	15.237466
26.171128	1178.583671	15.242483
26.443301	1159.150617	15.247501
26.342013	1198.685347	15.252519
25.910147	1168.549016	15.257536
26.315895	1163.438302	15.262554
25.771726	1182.247803	15.267571
26.523514	1165.835365	15.272589
26.526416	1168.718095	15.277607
26.589778	1169.371763	15.282624
26.716366	1181.971272	15.287642
26.436350	1158.058469	15.292659
26.455988	1146.601191	15.297677
26.058231	1167.630331	15.302695
26.685380	1162.536211	15.307712
26.743318	1151.818393	15.312730
26.349485	1171.797763	15.317747
26.172623	1153.205505	15.322765
26.084821	1152.717734	15.327783
26.506488	1166.339764	15.332800
26.776836	1170.485377	15.337818
26.530900	1164.723593	15.342835
26.790216	1154.975616	15.347853
26.534911	1180.549869	15.352871
26.624776	1159.412511	15.357888
26.396864	1170.418538	15.362906
26.542211	1163.166116	15.367923
26.773863	1153.705682	15.372941
26.278406	1185.635170	15.377959
26.717804	1162.598570	15.382976
26.634393	1170.149395	15.387994
26.722463	1184.790436	15.393011
26.967644	1194.011237	15.398029
26.798389	1193.275348	15.403047
26.897592	1232.675951	15.408064
26.925124	1193.343205	15.413082
26.790676	1202.311544	15.418099
27.168879	1200.984995	15.423117
27.022082	1212.747287	15.428135
27.293608	1190.622985	15.433152
26.981090	1193.914659	15.438170
26.795949	1186.641008	15.443187
27.462015	1169.112867	15.448205
27.039280	1203.494021	15.453223
27.367635	1171.175875	15.458240
27.208208	1192.280289	15.463258
27.095993	1174.909306	15.468275
27.014158	1171.501205	15.473293
27.491772	1186.064386	15.478311
27.105266	1175.349802	15.483328
27.155545	1206.846247	15.488346
27.175761	1185.943317	15.493363
27.294087	1208.612574	15.498381
27.054957	1171.722731	15.503399
27.413034	1207.012779	15.508416
27.688960	1181.896048	15.513434
27.455170	1176.092998	15.518451
27.534924	1225.373185	15.523469
27.350378	1202.503675	15.528487
27.664954	1186.167241	15.533504
27.359828	1201.519064	15.538522
27.462101	1197.089064	15.543539
27.803292	1180.830184	15.548557
27.362693	1201.874071	15.553575
27.624404	1203.192919	15.558592
28.129700	1186.837075	15.563610
27.449194	1212.636496	15.568627
27.725237	1194.689211	15.573645
27.582781	1187.630536	15.578663
27.937728	1197.055617	15.583680
27.715985	1190.140141	15.588698
27.945653	1213.073204	15.593715
27.848556	1177.692740	15.598733
27.552974	1211.641522	15.603751
27.574628	1183.663261	15.608768
28.024494	1209.663039	15.613786
27.661116	1179.819339	15.618803
27.997133	1195.888399	15.623821
27.706107	1199.670550	15.628839
27.692013	1170.758967	15.633856
27.990289	1195.036934	15.638874
27.985081	1196.739682	15.643891
27.943493	1200.914609	15.648909
27.687301	1184.975935	15.653927
28.025819	1222.966738	15.658944
28.225355	1215.645874	15.663962
28.367075	1221.237107	15.668979
28.244548	1199.899196	15.673997
27.967662	1203.070364	15.679015
28.028614	1203.703969	15.684032
28.367026	1206.350732	15.689050
28.394014	1216.815943	15.694067
28.384629	1226.071075	15.699085
28.060760	1186.563170	15.704103
28.194937	1221.948737	15.709120
28.458401	1210.819015	15.714138
28.370953	1222.035474	15.719155
28.353221	1207.206993	15.724173
28.257108	1230.328890	15.729191
28.092730	1205.060561	15.734208
28.676291	1208.478290	15.739226
28.480582	1211.090701	15.744243
28.597177	1227.814533	15.749261
28.479013	1201.090156	15.754279
28.357438	1221.161442	15.759296
28.734143	1197.623578	15.764314
28.296638	1226.217137	15.769331
28.544513	1214.220060	15.774349
28.496107	1212.808977	15.779367
28.569530	1216.584911	15.784384
28.907965	1213.076737	15.789402
28.604050	1204.552654	15.794419
28.723511	1224.280350	15.799437
28.894196	1214.148515	15.804455
28.560711	1212.469885	15.809472
28.867831	1223.351293	15.814490
28.557698	1208.330360	15.819507
29.113134	1234.775792	15.824525
28.792433	1232.093152	15.829543
28.833664	1231.996911	15.834560
29.488765	1220.079589	15.839578
29.403131	1238.342571	15.844595
29.587046	1206.940817	15.849613
29.034924	1225.536149	15.854631
29.171452	1193.695264	15.859648
29.447290	1220.141222	15.864666
29.131200	1192.105133	15.869683
29.099924	1208.816351	15.874701
29.377741	1205.327285	15.879719
29.084528	1206.297362	15.884736
29.117587	1216.135573	15.889754
29.039254	1195.174418	15.894771
29.000084	1211.603769	15.899789
29.441228	1198.177531	15.904807
29.028683	1196.297592	15.909824
29.139208	1230.790376	15.914842
29.558455	1217.485584	15.919859
29.510755	1223.574194	15.924877
29.686071	1237.035819	15.929895
29.586857	1215.879774	15.934912
29.659136	1211.594546	15.939930
29.367848	1207.199002	15.944947
29.202070	1204.864446	15.949965
29.483202	1233.083864	15.954983
29.302472	1232.588891	15.960000
29.487450	1221.614817	15.965018
29.465091	1249.303828	15.970035
29.308661	1227.906792	15.975053
29.203243	1244.312141	15.980071
29.368128	1233.172958	15.985088
29.385386	1228.995596	15.990106
29.302018	1256.069891	15.995123
29.755117	1255.141932	16.000141
30.124282	1240.585174	16.005159
30.182847	1272.997470	16.010176
30.170313	1247.843267	16.015194
30.062756	1251.571002	16.020211
30.020138	1247.510146	16.025229
30.350793	1222.738529	16.030247
29.912457	1226.871355	16.035264
30.267853	1218.484341	16.040282
30.210884	1214.130069	16.045299
29.819381	1233.011235	16.050317
30.189608	1224.192437	16.055335
29.977939	1227.719705	16.060352
30.069983	1209.406938	16.065370
29.952386	1236.917643	16.070387
29.991280	1241.587807	16.075405
30.475274	1245.277817	16.080423
30.189182	1266.064357	16.085440
30.492539	1241.023370	16.090458
30.192559	1222.856478	16.095475
30.149197	1250.533112	16.100493
30.531924	1239.917576	16.105511
30.421183	1244.795642	16.110528
30.545651	1266.735736	16.115546
30.525622	1239.468697	16.120563
30.622388	1266.651127	16.125581
30.467949	1233.664266	16.130599
30.367747	1255.633885	16.135616
30.769429	1266.498671	16.140634
30.213228	1272.901203	16.145651
30.449163	1233.698693	16.150669
30.528234	1280.344490	16.155687
30.385630	1255.138664	16.160704
30.827040	1226.624631	16.165722
30.729593	1284.823582	16.170739
30.602410	1286.452991	16.175757
30.839133	1259.525618	16.180775
30.452278	1256.669490	16.185792
30.824137	1225.789824	16.190810
30.554805	1277.502590	16.195827
30.385651	1243.549115	16.200845
30.884215	1252.101933	16.205863
30.519866	1266.571409	16.210880
31.070238	1244.378956	16.215898
31.197781	1292.270701	16.220915
31.295472	1270.299839	16.225933
31.139244	1269.409292	16.230951
30.656805	1257.102391	16.235968
31.044143	1265.215229	16.240986
31.300030	1259.452015	16.246003
31.185460	1279.926514	16.251021
31.171628	1272.655383	16.256039
31.730603	1241.105649	16.261056
31.206197	1269.120152	16.266074
31.076063	1264.200261	16.271091
31.079228	1233.624764	16.276109
31.627576	1258.581790	16.281127
31.152856	1237.026303	16.286144
31.461259	1260.665721	16.291162
31.566460	1246.906074	16.296179
31.239712	1233.786313	16.301197
31.598790	1259.006323	16.306215
31.438075	1240.425533	16.311232
31.452222	1253.206625	16.316250
31.728320	1262.125252	16.321267
31.700909	1253.388733	16.326285
31.683240	1239.688013	16.331303
31.150567	1241.047053	16.336320
31.443751	1258.359352	16.341338
31.585934	1260.806199	16.346355
31.683468	1268.458771	16.351373
31.702541	1277.449860	16.356391
31.744298	1274.110108	16.361408
31.692292	1258.560337	16.366426
31.647925	1281.637885	16.371443
31.526288	1274.862124	16.376461
31.662652	1289.799148	16.381479
31.837637	1271.932377	16.386496
31.963984	1265.315260	16.391514
31.759375	1276.507978	16.396531
31.818628	1277.269267	16.401549
31.772491	1263.846759	16.406567
31.807070	1271.383538	16.411584
32.205914	1297.575649	16.416602
32.248213	1292.190965	16.421619
32.168422	1270.987698	16.426637
32.098154	1265.965454	16.431655
32.226575	1281.919864	16.436672
32.414913	1287.900072	16.441690
32.724021	1267.621024	16.446707
32.029713	1270.218591	16.451725
32.285269	1266.184101	16.456743
32.354948	1271.964588	16.461760
32.347987	1271.424596	16.466778
32.224399	1260.257473	16.471795
32.306967	1286.913695	16.476813
32.722876	1310.515599	16.481831
32.785179	1276.046953	16.486848
32.628534	1281.906010	16.491866
32.708577	1274.432724	16.496883
31.953966	1266.771682	16.501901
32.635181	1285.102742	16.506919
32.714756	1280.786444	16.511936
32.264210	1276.469760	16.516954
32.430501	1293.816497	16.521971
32.677879	1292.380251	16.526989
32.729939	1289.347151	16.532007
32.593978	1298.150631	16.537024
33.072060	1297.344522	16.542042
33.372717	1294.770397	16.547059
33.138480	1290.854917	16.552077
32.839914	1268.086853	16.557095
32.741337	1264.327486	16.562112
32.617716	1272.800236	16.567130
33.136135	1292.914259	16.572147
32.887484	1296.143861	16.577165
33.214927	1290.941777	16.582183
33.012525	1288.992131	16.587200
33.216766	1299.040611	16.592218
33.257947	1289.228240	16.597235
33.404675	1289.689300	16.602253
33.275803	1263.263803	16.607271
32.940778	1256.555117	16.612288
32.830749	1265.249053	16.617306
33.131813	1282.873143	16.622323
33.057078	1302.984261	16.627341
33.538959	1285.405137	16.632359
33.706407	1286.308038	16.637376
33.786974	1291.509522	16.642394
33.616866	1266.341094	16.647411
33.285869	1275.568906	16.652429
33.255142	1276.753513	16.657447
33.646145	1276.876752	16.662464
33.460460	1290.002766	16.667482
33.834879	1289.540366	16.672499
33.882341	1288.576433	16.677517
33.533454	1272.259208	16.682535
33.551366	1264.643260	16.687552
33.407941	1274.959522	16.692570
33.766491	1269.154763	16.697587
33.816823	1288.332029	16.702605
33.450564	1292.214288	16.707623
33.719101	1280.759675	16.712640
33.588619	1291.056582	16.717658
33.949583	1293.839759	16.722675
33.305129	1299.252832	16.727693
33.853268	1291.481519	16.732711
33.740623	1295.567137	16.737728
33.577798	1292.423597	16.742746
34.136006	1288.988887	16.747763
33.629615	1284.794359	16.752781
33.848302	1294.996254	16.757799
34.012067	1305.153437	16.762816
34.060706	1315.876377	16.767834
34.576698	1307.841207	16.772851
34.202685	1332.037875	16.777869
34.399792	1323.514033	16.782887
34.379793	1317.014611	16.787904
33.822924	1307.264581	16.792922
34.314752	1307.678466	16.797939
34.275286	1315.982096	16.802957
34.107782	1321.149227	16.807975
34.291293	1316.083344	16.812992
34.211937	1312.585156	16.818010
34.446817	1314.170977	16.823027
34.787616	1323.022696	16.828045
34.599298	1314.421911	16.833063
34.503001	1307.206384	16.838080
34.196015	1315.557401	16.843098
34.589026	1308.968517	16.848115
34.376065	1307.096053	16.853133
34.603035	1297.403475	16.858151
34.579901	1305.451249	16.863168
34.374231	1304.776215	16.868186
34.515284	1310.164678	16.873203
34.232183	1323.957464	16.878221
34.690812	1324.472595	16.883239
35.072288	1346.382830	16.888256
34.960431	1351.721987	16.893274
35.356960	1355.724839	16.898291
35.027117	1350.951597	16.903309
35.256031	1343.213869	16.908327
35.371646	1334.495386	16.913344
35.088438	1322.733927	16.918362
35.472853	1301.011431	16.923379
35.037413	1310.526471	16.928397
35.176870	1312.212451	16.933415
35.340629	1304.014821	16.938432
35.181089	1314.256607	16.943450
35.001496	1313.251812	16.948467
35.454792	1310.831084	16.953485
35.151839	1303.274156	16.958503
35.151042	1320.331411	16.963520
35.127527	1320.385489	16.968538
35.221559	1326.001671	16.973555
35.082257	1358.230223	16.978573
35.489743	1343.182779	16.983591
35.458043	1334.821259	16.988608
35.497715	1349.336485	16.993626
35.537102	1348.364398	16.998643
35.509146	1350.248537	17.003661
35.310020	1333.534565	17.008679
35.717802	1337.629995	17.013696
35.604609	1348.665049	17.018714
35.660738	1349.264825	17.023731
35.305048	1342.023015	17.028749
35.261352	1350.613619	17.033767
35.943418	1357.885158	17.038784
35.886142	1368.684803	17.043802
36.135492	1366.718147	17.048819
36.177824	1357.611807	17.053837
35.788637	1343.572284	17.058855
35.756424	1339.660746	17.063872
35.920534	1350.524164	17.068890
36.340030	1361.362587	17.073907
36.132210	1355.369712	17.078925
35.767160	1350.064133	17.083943
36.005546	1354.913293	17.088960
36.157227	1369.915595	17.093978
36.099799	1371.148512	17.098995
36.620085	1359.068544	17.104013
36.338434	1368.208322	17.109031
36.222850	1362.051302	17.114048
36.208478	1360.494782	17.119066
36.408214	1360.234839	17.124083
36.069549	1370.050648	17.129101
35.853317	1369.455943	17.134119
36.713438	1360.414216	17.139136
36.418311	1366.707511	17.144154
36.603704	1366.139982	17.149171
36.732790	1357.829880	17.154189
36.624321	1371.502053	17.159207
36.883737	1360.409041	17.164224
36.433186	1367.098343	17.169242
36.399332	1355.879083	17.174259
36.643709	1367.571246	17.179277
36.599677	1357.078744	17.184295
36.886072	1351.636231	17.189312
36.662402	1358.636967	17.194330
36.555280	1356.799525	17.199347
36.956207	1359.043106	17.204365
36.895778	1350.130905	17.209383
36.908896	1354.676234	17.214400
36.849712	1359.794643	17.219418
36.733020	1360.212780	17.224435
37.036641	1371.527424	17.229453
37.000847	1380.388907	17.234471
37.535487	1383.298552	17.239488
37.201365	1399.694938	17.244506
37.263732	1400.639773	17.249523
37.315787	1391.495683	17.254541
37.165597	1370.424616	17.259559
37.043002	1372.438678	17.264576
37.245477	1388.846992	17.269594
37.429068	1392.237329	17.274611
37.363441	1387.525749	17.279629
37.078891	1396.157940	17.284647
37.631042	1381.107832	17.289664
37.278285	1387.779973	17.294682
37.464099	1396.373323	17.299699
37.692906	1379.007476	17.304717
37.394660	1387.574208	17.309735
37.670414	1387.237649	17.314752
37.792064	1387.746756	17.319770
37.635515	1373.860428	17.324787
37.514595	1374.560800	17.329805
37.349987	1391.252597	17.334823
37.734693	1377.670035	17.339840
37.703456	1375.954188	17.344858
37.517507	1379.675583	17.349875
37.885143	1388.283972	17.354893
38.116150	1401.872144	17.359911
38.378209	1394.124383	17.364928
37.843009	1387.026007	17.369946
37.920099	1373.009611	17.374963
38.085661	1387.798941	17.379981
37.656922	1388.372236	17.384999
38.330982	1390.652482	17.390016
38.450031	1411.020696	17.395034
38.522862	1409.580819	17.400051
38.431937	1374.628308	17.405069
38.076683	1385.080676	17.410087
38.395137	1381.273641	17.415104
38.266954	1385.630739	17.420122
38.219316	1375.703492	17.425139
38.502344	1383.939997	17.430157
38.299962	1415.006878	17.435175
38.845288	1400.509950	17.440192
38.576601	1392.448880	17.445210
38.244132	1384.297317	17.450227
38.477173	1391.129277	17.455245
38.427568	1404.998152	17.460263
38.557385	1396.805883	17.465280
38.453678	1411.833232	17.470298
38.628525	1405.208317	17.475315
39.024384	1393.099403	17.480333
38.894490	1402.498133	17.485351
39.007820	1396.021454	17.490368
38.837038	1390.230288	17.495386
39.019746	1399.859146	17.500403
39.134866	1391.895732	17.505421
38.599419	1404.756749	17.510439
38.886896	1386.662690	17.515456
38.906208	1384.273416	17.520474
39.019530	1398.625941	17.525491
39.297516	1408.381175	17.530509
38.916995	1405.686021	17.535527
38.878174	1392.194589	17.540544
39.161590	1403.518773	17.545562
39.119663	1395.957915	17.550579
39.436882	1400.148029	17.555597
38.937715	1397.220125	17.560615
39.678892	1405.572327	17.565632
39.219877	1403.031259	17.570650
39.278346	1413.557657	17.575667
39.959704	1413.362466	17.580685
39.898475	1410.558186	17.585703
39.460413	1394.635702	17.590720
39.783611	1386.093285	17.595738
39.751931	1393.618674	17.600755
39.636086	1385.402674	17.605773
39.643668	1397.112180	17.610791
39.766647	1390.712613	17.615808
39.453255	1389.159738	17.620826
39.559369	1385.046808	17.625843
40.149265	1409.557041	17.630861
40.029336	1403.855283	17.635879
39.536305	1389.177923	17.640896
39.908889	1387.849110	17.645914
39.587793	1408.990636	17.650931
40.040430	1412.490644	17.655949
39.677991	1405.660423	17.660967
39.880925	1400.563099	17.665984
39.759527	1427.698834	17.671002
39.729483	1415.602776	17.676019
40.251602	1409.337736	17.681037
40.015432	1416.902043	17.686055
40.083699	1416.257242	17.691072
40.107176	1421.025874	17.696090
40.295443	1433.255557	17.701107
40.523577	1440.181128	17.706125
40.381047	1444.233803	17.711143
40.567898	1435.343455	17.716160
40.857488	1437.318527	17.721178
40.676951	1430.383779	17.726195
40.839425	1403.327986	17.731213
40.851660	1406.762959	17.736231
40.403131	1406.696067	17.741248
40.698092	1394.409770	17.746266
40.789162	1393.500221	17.751283
40.651301	1399.049602	17.756301
40.491802	1406.769983	17.761319
40.589746	1413.812256	17.766336
40.650290	1430.991988	17.771354
40.632628	1445.439379	17.776371
41.128011	1430.709722	17.781389
40.908530	1433.802573	17.786407
40.909938	1440.172868	17.791424
41.078633	1431.854833	17.796442
41.261747	1439.647998	17.801459
41.052967	1428.975661	17.806477
40.792865	1433.613353	17.811495
40.927714	1430.046366	17.816512
40.859728	1437.478471	17.821530
40.824540	1447.868826	17.826547
41.550904	1438.272679	17.831565
41.402850	1449.467520	17.836583
41.423910	1449.327306	17.841600
41.703742	1413.437850	17.846618
41.297290	1446.347831	17.851635
41.435225	1425.859918	17.856653
41.266150	1437.067541	17.861671
41.369115	1469.566003	17.866688
41.940689	1458.174601	17.871706
41.429514	1470.978324	17.876723
41.357607	1465.983012	17.881741
41.502318	1467.065725	17.886759
41.814295	1457.166008	17.891776
41.721061	1469.789818	17.896794
41.856543	1466.490127	17.901811
42.149421	1461.038675	17.906829
41.923114	1463.449950	17.911847
42.199585	1442.449151	17.916864
42.095628	1452.952721	17.921882
41.855697	1462.537347	17.926899
42.142865	1460.839918	17.931917
42.079868	1455.813302	17.936935
41.703287	1463.053974	17.941952
42.119501	1450.730988	17.946970
41.944269	1455.348859	17.951987
41.864406	1458.734041	17.957005
42.063049	1461.368540	17.962023
42.117092	1463.908129	17.967040
42.379545	1471.495182	17.972058
42.005706	1502.743748	17.977075
42.503771	1472.938221	17.982093
42.649826	1492.803610	17.987111
42.530936	1494.093529	17.992128
42.813204	1488.802630	17.997146
42.622803	1495.585774	18.002163
42.829917	1478.039230	18.007181
42.524578	1510.805820	18.012199
42.781805	1482.229428	18.017216
42.899433	1488.839177	18.022234
42.962958	1490.482235	18.027251
43.147457	1488.835784	18.032269
42.956735	1483.857843	18.037287
42.942377	1483.504633	18.042304
42.900593	1491.643572	18.047322
43.036848	1496.969951	18.052339
43.287352	1485.928600	18.057357
43.262877	1488.658463	18.062375
43.301378	1469.440008	18.067392
43.320139	1449.518463	18.072410
43.191568	1455.681415	18.077427
43.085503	1465.704001	18.082445
43.013766	1467.796478	18.087463
43.007788	1481.685209	18.092480
43.097815	1479.909113	18.097498
43.061880	1498.777957	18.102515
43.427643	1489.432765	18.107533
43.339170	1493.616827	18.112551
43.179448	1485.752249	18.117568
43.246419	1485.848523	18.122586
43.121473	1498.763698	18.127603
43.357506	1516.996178	18.132621
43.867219	1502.610219	18.137639
43.589703	1511.585838	18.142656
43.808973	1506.235768	18.147674
43.929808	1521.457073	18.152691
44.389216	1513.498455	18.157709
43.917087	1514.882465	18.162727
43.893968	1504.537526	18.167744
44.045173	1490.886710	18.172762
43.730266	1496.511553	18.177779
43.922696	1507.339114	18.182797
44.197912	1509.064812	18.187815
44.134531	1511.964474	18.192832
44.392118	1484.072266	18.197850
44.088670	1515.193233	18.202867
44.374560	1500.745449	18.207885
44.561354	1505.420424	18.212903
44.072992	1492.214520	18.217920
44.127950	1495.818873	18.222938
44.351139	1499.226514	18.227955
44.257688	1498.708173	18.232973
44.181643	1498.754900	18.237991
44.059359	1505.187422	18.243008
44.305231	1497.494096	18.248026
44.729633	1496.043756	18.253043
44.451036	1495.632019	18.258061
44.384761	1493.121101	18.263079
44.155904	1501.838850	18.268096
44.650430	1508.020420	18.273114
44.594380	1527.977865	18.278131
44.634638	1533.038005	18.283149
45.060406	1523.396939	18.288167
44.768653	1528.223747	18.293184
44.831566	1523.449152	18.298202
44.770247	1524.449902	18.303219
45.064284	1528.272528	18.308237
45.452415	1520.556502	18.313255
44.993345	1527.863842	18.318272
45.245990	1520.930746	18.323290
45.262404	1526.608149	18.328307
45.560785	1528.750141	18.333325
45.676769	1515.811187	18.338343
45.124460	1521.119983	18.343360
45.102692	1516.074186	18.348378
45.429766	1518.823489	18.353395
45.350500	1513.953599	18.358413
45.557259	1509.198537	18.363431
45.159448	1520.425402	18.368448
45.136456	1514.785216	18.373466
45.450809	1538.034830	18.378483
45.631492	1549.521801	18.383501
45.885744	1543.829521	18.388519
45.916178	1555.203611	18.393536
45.846816	1545.123987	18.398554
45.696318	1540.422748	18.403571
45.737517	1557.527066	18.408589
46.215950	1539.119225	18.413607
46.048376	1544.371387	18.418624
46.061794	1563.158513	18.423642
46.159368	1552.401045	18.428659
45.731529	1552.793308	18.433677
46.104857	1533.221715	18.438695
45.916343	1560.403795	18.443712
46.045423	1549.666471	18.448730
46.058552	1539.502911	18.453747
45.968191	1551.443661	18.458765
46.176255	1550.834758	18.463783
45.968326	1549.880081	18.468800
46.181420	1561.242346	18.473818
46.397848	1560.205831	18.478835
46.118591	1573.034001	18.483853
46.396521	1584.123255	18.488871
46.368115	1569.543063	18.493888
46.747544	1572.567163	18.498906
46.450041	1564.059145	18.503923
46.713138	1558.437806	18.508941
46.785218	1576.510898	18.513959
46.786928	1568.954001	18.518976
46.692559	1562.475768	18.523994
47.092577	1571.042925	18.529011
46.992580	1565.745326	18.534029
47.027877	1562.403392	18.539047
46.970033	1570.382919	18.544064
47.093828	1581.123956	18.549082
46.955078	1568.417487	18.554099
47.071803	1582.522693	18.559117
47.445992	1566.550695	18.564135
47.153770	1616.163668	18.569152
47.453990	1594.707414	18.574170
47.785906	1591.354344	18.579187
46.973285	1591.858312	18.584205
47.582210	1591.264124	18.589223
47.686595	1576.310398	18.594240
47.786239	1582.009154	18.599258
47.841580	1574.014276	18.604275
47.393969	1573.744320	18.609293
47.674115	1569.233930	18.614311
47.726788	1576.302379	18.619328
47.705446	1581.631904	18.624346
47.870247	1579.225686	18.629363
47.547221	1599.587595	18.634381
47.663888	1579.496104	18.639399
47.734703	1600.710680	18.644416
47.967990	1586.379737	18.649434
47.972758	1579.089755	18.654451
47.818883	1590.521581	18.659469
47.904589	1596.521433	18.664487
47.946900	1585.003564	18.669504
48.050009	1594.025491	18.674522
47.998122	1579.508807	18.679539
48.147958	1580.184881	18.684557
48.357657	1605.268879	18.689575
48.420714	1614.972019	18.694592
48.390833	1622.217247	18.699610
48.707148	1611.892026	18.704627
48.419928	1606.164960	18.709645
48.875254	1608.088456	18.714663
48.796730	1603.315944	18.719680
48.678616	1598.524579	18.724698
48.979936	1570.508829	18.729715
48.682333	1573.164294	18.734733
48.782347	1567.284251	18.739751
48.481571	1575.972617	18.744768
48.461765	1566.729767	18.749786
48.640032	1596.578613	18.754803
48.476328	1625.351080	18.759821
49.097425	1603.875096	18.764839
49.160596	1603.610190	18.769856
48.830484	1607.763611	18.774874
49.284878	1604.977730	18.779891
49.368433	1606.891307	18.784909
49.209316	1610.344218	18.789927
49.118430	1613.281319	18.794944
49.162329	1600.581870	18.799962
49.369668	1624.344968	18.804979
48.949527	1609.385203	18.809997
49.210981	1597.689231	18.815015
49.017273	1609.468763	18.820032
49.397683	1620.815402	18.825050
49.864676	1632.006671	18.830067
49.735048	1647.109182	18.835085
50.157546	1628.977558	18.840103
49.832099	1623.608931	18.845120
49.435293	1610.028101	18.850138
50.034185	1612.406889	18.855155
49.717536	1630.446094	18.860173
49.827320	1633.030304	18.865191
50.084469	1640.105498	18.870208
49.854328	1627.487483	18.875226
50.084440	1628.993879	18.880243
49.837372	1634.675595	18.885261
50.179748	1630.178857	18.890279
50.010037	1647.231977	18.895296
50.379070	1632.961134	18.900314
50.235559	1634.808684	18.905331
50.109727	1622.115837	18.910349
50.026606	1637.777197	18.915367
50.104104	1643.971856	18.920384
50.362444	1614.954588	18.925402
50.529082	1628.139545	18.930419
50.490254	1635.471149	18.935437
50.438751	1649.760550	18.940455
50.586136	1651.704851	18.945472
50.473265	1643.865747	18.950490
51.056940	1642.366397	18.955507
50.683860	1654.059744	18.960525
50.968136	1639.630956	18.965543
51.315796	1633.255223	18.970560
50.734840	1642.743349	18.975578
50.870680	1640.138824	18.980595
50.846408	1630.313066	18.985613
50.881268	1641.106084	18.990631
50.687386	1648.246924	18.995648
50.642625	1648.647304	19.000666
50.830427	1639.563202	19.005683
51.102556	1649.660874	19.010701
51.376087	1674.780430	19.015719
51.529896	1662.094857	19.020736
50.916112	1691.931797	19.025754
51.288512	1657.867381	19.030771
50.917697	1686.946703	19.035789
51.615542	1658.192729	19.040807
51.574685	1672.269673	19.045824
51.471633	1667.921040	19.050842
51.471101	1673.558732	19.055859
51.678598	1671.372202	19.060877
51.833437	1649.780180	19.065895
51.965142	1684.056743	19.070912
51.632991	1655.775351	19.075930
51.517768	1671.091089	19.080947
51.961052	1687.602908	19.085965
51.955212	1684.138521	19.090983
52.084288	1715.050937	19.096000
52.112228	1702.040917	19.101018
52.043435	1693.543535	19.106035
52.150735	1706.017594	19.111053
52.253251	1692.676370	19.116071
52.324566	1678.849359	19.121088
52.099853	1683.717435	19.126106
52.472334	1707.090969	19.131123
52.587587	1681.799228	19.136141
52.630623	1682.654359	19.141159
52.970187	1677.532003	19.146176
52.719076	1690.553985	19.151194
53.163549	1685.677585	19.156211
52.856286	1684.586160	19.161229
52.672461	1698.527058	19.166247
52.949498	1668.130329	19.171264
52.289253	1698.550408	19.176282
52.975687	1682.198156	19.181299
52.566096	1674.502311	19.186317
52.736969	1697.195416	19.191335
52.882629	1687.062525	19.196352
52.781434	1705.614863	19.201370
53.347787	1705.884747	19.206387
53.210614	1710.370789	19.211405
53.360367	1734.449987	19.216423
53.463232	1698.537714	19.221440
53.401020	1725.378282	19.226458
53.445596	1706.754711	19.231475
53.627385	1715.359905	19.236493
53.552413	1710.099160	19.241511
53.875839	1704.938471	19.246528
53.426237	1707.652807	19.251546
53.522283	1712.688383	19.256563
53.527631	1713.090211	19.261581
53.235929	1696.991466	19.266599
53.926242	1718.856162	19.271616
53.667281	1708.256112	19.276634
53.614988	1702.922541	19.281651
54.013586	1703.876693	19.286669
53.692355	1709.250946	19.291687
53.902158	1712.149550	19.296704
53.618818	1695.626336	19.301722
54.163303	1727.811150	19.306739
54.510455	1730.790096	19.311757
54.443010	1719.022215	19.316775
54.503320	1720.646937	19.321792
54.285924	1709.524313	19.326810
54.391151	1699.426175	19.331827
54.242804	1693.898718	19.336845
54.420859	1709.386370	19.341863
54.429064	1710.358741	19.346880
54.146920	1736.108136	19.351898
54.494344	1704.386649	19.356915
54.487557	1731.746917	19.361933
54.514810	1717.329156	19.366951
54.755542	1719.901936	19.371968
54.778512	1727.893829	19.376986
54.789909	1728.927039	19.382003
54.802527	1739.133802	19.387021
55.320784	1732.688347	19.392039
55.572288	1738.537549	19.397056
55.008275	1723.550273	19.402074
54.960623	1727.104983	19.407091
55.384463	1732.681309	19.412109
54.891464	1735.010893	19.417127
55.408713	1759.486121	19.422144
55.559006	1753.358888	19.427162
55.409281	1752.368172	19.432179
55.310318	1756.513084	19.437197
55.618047	1753.099343	19.442215
55.574765	1743.908887	19.447232
55.166606	1756.073519	19.452250
55.603912	1765.742241	19.457267
55.831075	1736.218477	19.462285
55.524574	1770.701983	19.467303
55.711690	1747.972104	19.472320
55.658545	1742.703147	19.477338
55.819958	1765.039223	19.482355
55.793541	1756.012808	19.487373
56.173154	1788.192591	19.492391
56.499051	1767.051308	19.497408
56.037122	1781.080683	19.502426
56.208641	1793.005033	19.507443
56.488054	1761.468872	19.512461
56.186843	1800.179842	19.517479
56.289644	1779.064685	19.522496
56.343352	1763.750764	19.527514
56.362153	1797.653924	19.532531
56.544275	1762.897597	19.537549
56.502755	1796.349484	19.542567
56.688715	1764.350026	19.547584
56.734624	1774.324991	19.552602
56.919192	1783.625052	19.557619
56.942417	1776.534945	19.562637
56.623250	1781.219918	19.567655
57.068035	1756.295484	19.572672
56.992938	1775.713622	19.577690
57.066724	1756.923308	19.582707
56.785055	1779.495237	19.587725
56.762846	1756.745245	19.592743
56.998440	1743.840494	19.597760
56.643876	1799.707288	19.602778
57.150234	1783.136681	19.607795
57.050269	1809.618487	19.612813
57.285372	1799.908549	19.617831
57.459377	1805.619129	19.622848
57.233887	1810.426023	19.627866
57.310089	1802.669936	19.632883
57.198957	1787.287899	19.637901
57.162823	1800.330749	19.642919
57.659626	1820.283794	19.647936
57.881066	1817.805585	19.652954
57.863195	1816.649119	19.657971
58.175750	1838.997383	19.662989
58.106363	1808.125505	19.668007
58.046879	1818.584494	19.673024
57.991892	1794.060596	19.678042
58.116357	1798.906055	19.683059
58.265001	1835.695516	19.688077
58.142098	1813.653621	19.693095
58.494864	1835.086266	19.698112
57.985265	1824.584305	19.703130
58.428051	1794.123126	19.708147
58.247494	1836.167031	19.713165
58.196914	1819.663183	19.718183
58.198130	1826.326259	19.723200
58.543112	1798.318837	19.728218
58.572746	1824.382031	19.733235
58.498346	1792.532572	19.738253
58.569154	1827.240752	19.743271
58.412060	1816.589771	19.748288
58.674512	1811.983030	19.753306
58.616940	1858.732710	19.758323
59.097112	1846.333126	19.763341
58.864873	1849.115067	19.768359
59.120109	1848.094366	19.773376
59.101045	1832.825012	19.778394
59.062476	1854.455377	19.783411
59.340931	1834.175710	19.788429
59.131745	1841.216838	19.793447
59.314481	1848.399957	19.798464
59.220499	1844.993632	19.803482
59.282049	1830.048049	19.808499
59.359410	1856.053352	19.813517
59.720366	1838.138921	19.818535
59.795397	1886.044156	19.823552
59.947745	1841.295861	19.828570
59.975055	1865.983114	19.833587
59.882895	1843.895370	19.838605
59.839515	1825.052869	19.843623
59.687883	1856.334396	19.848640
59.938950	1827.343032	19.853658
59.591698	1847.627355	19.858675
60.075178	1871.859623	19.863693
59.968532	1865.597142	19.868711
60.313586	1861.982370	19.873728
60.630118	1846.473863	19.878746
60.361986	1864.444272	19.883763
60.547872	1846.037084	19.888781
60.226973	1852.108181	19.893799
60.789849	1855.246231	19.898816
60.683640	1842.197705	19.903834
60.573907	1845.510663	19.908851
61.071107	1853.859573	19.913869
61.090231	1857.883434	19.918887
60.640801	1834.580114	19.923904
60.361801	1822.480948	19.928922
60.722743	1856.027661	19.933939
60.557954	1842.335677	19.938957
60.383924	1845.094176	19.943975
60.783188	1837.723845	19.948992
60.913240	1854.927602	19.954010
60.756954	1868.765172	19.959027
61.186588	1871.716838	19.964045
61.135427	1881.808031	19.969063
61.317111	1878.342005	19.974080
61.219946	1877.308291	19.979098
61.296363	1872.902660	19.984115
61.525557	1870.932863	19.989133
61.280648	1876.983986	19.994151
61.621785	1867.062038	19.999168
61.486576	1883.255785	20.004186
61.568142	1882.072444	20.009203
61.984958	1881.180128	20.014221
61.795138	1894.387571	20.019239
61.720056	1899.083990	20.024256
62.068055	1897.137714	20.029274
62.264333	1902.177820	20.034291
62.497568	1901.435903	20.039309
62.344006	1897.672554	20.044327
62.558547	1886.065631	20.049344
62.465010	1870.959123	20.054362
62.071654	1868.012668	20.059379
62.213384	1882.219572	20.064397
62.538269	1889.576668	20.069415
62.176421	1890.326497	20.074432
62.571478	1891.787741	20.079450
62.459570	1897.169578	20.084467
62.609955	1893.365621	20.089485
62.363071	1887.709086	20.094503
62.203751	1897.569003	20.099520
62.362987	1897.499556	20.104538
62.279523	1925.916904	20.109555
62.631697	1927.444766	20.114573
63.374674	1928.378620	20.119591
62.960127	1928.141132	20.124608
63.077590	1935.029537	20.129626
63.259267	1932.801469	20.134643
63.423586	1927.482033	20.139661
63.174740	1923.571852	20.144679
63.023723	1934.322374	20.149696
63.517159	1918.996363	20.154714
63.210202	1927.201431	20.159731
63.133382	1929.631412	20.164749
63.576390	1941.723373	20.169767
63.537239	1949.538105	20.174784
63.999963	1952.580466	20.179802
63.954267	1949.492032	20.184819
64.159185	1945.119368	20.189837
64.293225	1951.386939	20.194855
63.882361	1932.093245	20.199872
64.356413	1960.838599	20.204890
64.270997	1943.224890	20.209907
63.982511	1946.709523	20.214925
64.227645	1937.741934	20.219943
64.314881	1937.767340	20.224960
64.048756	1947.787470	20.229978
63.965478	1936.731371	20.234995
64.279323	1940.003538	20.240013
64.023142	1949.653996	20.245031
64.265369	1946.315151	20.250048
64.699528	1947.326572	20.255066
64.544652	1968.819927	20.260083
64.879915	1981.283036	20.265101
64.888379	1976.963716	20.270119
64.638617	1953.617349	20.275136
64.809125	1994.035843	20.280154
64.892133	1971.075253	20.285171
64.969603	1971.201317	20.290189
65.104877	1959.679335	20.295207
64.611154	1972.847227	20.300224
65.527643	1952.171485	20.305242
65.136023	1961.275688	20.310259
65.123126	1981.974063	20.315277
65.530544	1974.517420	20.320295
65.624825	1988.365480	20.325312
65.693388	1999.538783	20.330330
65.516790	1982.908554	20.335347
65.868787	1985.941839	20.340365
65.758456	1980.356298	20.345383
65.844211	1980.179020	20.350400
66.393368	1974.746283	20.355418
66.234801	1976.110211	20.360435
66.030862	1981.308554	20.365453
66.275217	1972.301743	20.370471
66.239760	1981.866683	20.375488
66.195105	1986.997154	20.380506
66.196573	1962.660595	20.385523
66.232977	1999.290622	20.390541
66.055735	1981.184994	20.395559
66.227984	1963.855784	20.400576
66.397568	1986.082360	20.405594
66.534568	1970.721903	20.410611
66.231840	1995.778190	20.415629
66.521387	1964.839296	20.420647
66.248771	1987.137969	20.425664
66.941748	1994.049451	20.430682
66.590011	1996.606657	20.435699
66.815544	2021.018741	20.440717
67.038814	1999.871466	20.445735
66.847442	2008.072303	20.450752
67.360566	1998.454748	20.455770
67.224479	1989.025679	20.460787
67.041909	1999.811168	20.465805
67.198385	1990.461283	20.470823
66.975898	1985.793400	20.475840
66.978992	1998.183656	20.480858
67.164516	1986.461730	20.485875
67.132680	2010.136192	20.490893
67.384447	2032.768159	20.495911
67.454890	2003.128846	20.500928
67.497592	2027.766729	20.505946
67.459698	2021.428721	20.510963
67.980314	2017.609733	20.515981
68.067959	2053.762962	20.520999
68.056331	2018.649955	20.526016
68.539589	2056.740997	20.531034
67.771830	2047.860944	20.536051
68.630401	2015.767821	20.541069
68.706775	2046.952048	20.546087
68.269880	2059.728707	20.551104
68.263863	2032.036365	20.556122
68.685648	2048.143039	20.561139
68.554716	2052.945943	20.566157
68.924840	2029.752279	20.571175
68.743786	2023.540921	20.576192
68.976813	2036.603979	20.581210
69.017023	2034.400030	20.586227
68.738334	2037.722672	20.591245
68.959196	2034.925193	20.596263
68.762547	2013.149585	20.601280
68.954501	2043.129306	20.606298
69.140070	2022.769808	20.611315
68.935276	2042.729660	20.616333
68.841998	2037.021827	20.621351
69.114224	2040.907848	20.626368
69.410936	2054.236046	20.631386
69.435995	2068.864437	20.636403
69.260232	2066.883691	20.641421
69.505826	2058.457080	20.646439
69.127555	2075.487334	20.651456
69.472384	2061.226226	20.656474
69.492199	2064.205538	20.661491
69.648290	2066.464688	20.666509
70.103692	2100.231287	20.671527
69.994542	2075.702966	20.676544
69.948373	2107.621026	20.681562
69.968093	2086.249681	20.686579
70.094801	2079.139777	20.691597
70.250893	2091.197397	20.696615
70.160038	2069.570001	20.701632
70.247868	2090.746402	20.706650
70.616532	2064.872454	20.711667
70.486907	2104.436198	20.716685
70.602531	2082.277201	20.721703
70.611532	2073.471458	20.726720
70.846808	2084.357115	20.731738
70.804630	2086.957777	20.736755
70.666141	2071.364294	20.741773
70.804980	2091.192332	20.746791
70.875777	2080.613351	20.751808
71.026664	2131.178320	20.756826
71.046808	2106.714271	20.761843
70.873154	2106.432069	20.766861
70.890138	2110.026902	20.771879
71.113817	2113.988324	20.776896
71.161061	2092.555951	20.781914
70.937787	2111.115692	20.786931
71.522997	2135.601172	20.791949
72.041385	2114.362620	20.796967
71.665476	2140.050604	20.801984
71.940127	2124.348705	20.807002
71.980850	2125.043781	20.812019
72.074091	2136.801573	20.817037
72.459749	2123.153673	20.822055
72.108013	2136.711205	20.827072
72.013414	2086.459698	20.832090
72.286434	2122.221735	20.837107
71.735159	2131.914655	20.842125
72.785376	2104.662496	20.847143
72.529715	2102.477407	20.852160
72.355705	2148.049504	20.857178
72.550628	2114.748509	20.862195
72.343516	2130.864334	20.867213
72.578990	2110.834959	20.872231
72.875369	2118.555374	20.877248
72.460045	2141.495248	20.882266
72.700852	2098.688922	20.887283
72.628272	2142.453132	20.892301
72.939622	2114.017880	20.897319
72.745388	2151.039006	20.902336
72.680927	2169.027646	20.907354
73.176468	2135.870572	20.912371
72.730318	2122.229485	20.917389
73.165914	2171.324012	20.922407
72.736351	2161.944779	20.927424
73.050273	2144.311185	20.932442
73.619702	2190.272947	20.937459
73.345295	2162.596416	20.942477
73.810451	2204.875044	20.947495
73.550197	2180.251092	20.952512
73.641180	2161.135037	20.957530
73.677937	2196.011555	20.962547
73.837354	2167.518630	20.967565
73.976957	2176.396673	20.972583
73.999181	2168.376862	20.977600
73.977747	2188.537337	20.982618
74.065668	2170.389186	20.987635
74.242799	2202.018581	20.992653
74.434726	2187.959489	20.997671
74.427878	2209.291163	21.002688
74.442478	2201.799522	21.007706
74.737493	2203.020348	21.012723
74.552868	2209.555932	21.017741
74.770295	2192.379696	21.022759
74.900188	2214.746663	21.027776
74.713989	2196.720847	21.032794
75.212216	2195.024286	21.037811
74.940719	2203.351271	21.042829
75.075140	2180.888672	21.047847
74.794041	2204.990174	21.052864
74.942029	2186.467474	21.057882
75.415889	2203.319509	21.062899
75.085383	2239.813598	21.067917
75.181262	2208.382817	21.072935
75.155035	2221.108281	21.077952
75.262291	2244.704313	21.082970
75.585252	2212.158193	21.087987
75.426137	2213.110090	21.093005
75.721604	2247.943901	21.098023
75.941919	2231.295707	21.103040
75.671577	2261.141960	21.108058
76.497161	2242.363261	21.113075
76.177565	2243.951099	21.118093
76.307693	2247.590844	21.123111
76.537801	2250.401375	21.128128
76.678616	2242.749582	21.133146
76.542196	2248.506698	21.138163
76.536475	2238.735772	21.143181
76.809363	2244.092551	21.148199
76.902197	2236.874711	21.153216
76.539330	2240.331948	21.158234
77.115927	2238.712550	21.163251
76.803513	2249.013979	21.168269
76.941252	2216.626378	21.173287
76.712581	2265.396142	21.178304
76.757840	2215.128178	21.183322
76.758768	2257.748414	21.188339
76.861157	2258.100174	21.193357
77.034882	2221.406081	21.198375
77.419930	2213.605241	21.203392
76.897324	2269.239510	21.208410
77.419849	2276.060335	21.213427
77.286634	2236.541172	21.218445
77.365466	2237.065006	21.223463
77.908943	2232.965461	21.228480
77.994981	2234.820523	21.233498
78.154085	2246.003173	21.238515
77.859414	2249.015373	21.243533
77.527357	2237.632195	21.248551
77.458683	2280.375284	21.253568
77.447109	2278.245625	21.258586
78.180908	2261.369213	21.263603
77.950176	2324.282884	21.268621
77.821543	2292.518056	21.273639
78.686022	2263.821264	21.278656
78.462960	2269.793557	21.283674
78.692042	2283.963330	21.288691
78.624868	2307.283680	21.293709
78.626263	2298.979248	21.298727
79.220647	2277.772385	21.303744
79.144485	2311.037497	21.308762
79.274877	2294.685149	21.313779
78.853277	2296.482746	21.318797
78.842485	2294.393859	21.323815
79.391194	2306.871977	21.328832
78.853603	2321.508552	21.333850
79.625893	2291.643462	21.338867
79.113265	2329.697410	21.343885
79.007986	2299.292691	21.348903
79.734063	2308.827639	21.353920
79.554008	2297.402869	21.358938
79.455174	2313.575563	21.363955
79.500160	2298.017072	21.368973
79.620312	2336.374401	21.373991
79.645896	2306.118690	21.379008
79.776703	2338.131732	21.384026
80.074619	2333.750415	21.389043
79.787732	2323.736399	21.394061
80.150179	2357.540446	21.399079
80.630419	2348.832423	21.404096
80.074543	2358.093630	21.409114
80.364371	2346.370512	21.414131
80.352523	2345.881597	21.419149
80.490834	2355.504018	21.424167
80.273066	2351.000435	21.429184
80.636053	2334.993204	21.434202
81.130849	2348.329413	21.439219
80.867503	2384.710118	21.444237
81.481251	2348.877577	21.449255
81.836855	2378.359972	21.454272
81.636022	2326.145653	21.459290
81.387006	2342.037154	21.464307
81.254682	2324.433607	21.469325
81.649525	2309.159093	21.474343
81.865081	2359.753873	21.479360
81.377319	2356.444833	21.484378
81.579162	2321.253005	21.489395
81.676064	2320.123814	21.494413
81.458982	2348.874765	21.499431
82.127498	2355.002219	21.504448
81.607528	2374.770536	21.509466
82.167609	2344.314672	21.514483
82.012217	2386.158735	21.519501
82.046178	2351.784076	21.524519
82.192689	2382.055683	21.529536
81.940043	2350.775346	21.534554
82.124394	2365.359757	21.539571
82.258403	2385.177169	21.544589
81.855731	2385.228007	21.549607
82.670306	2373.389722	21.554624
82.180495	2420.950274	21.559642
82.597613	2397.653361	21.564659
82.393695	2410.130466	21.569677
82.576180	2410.394736	21.574695
83.315844	2393.249815	21.579712
82.975880	2448.945309	21.584730
83.008044	2425.867835	21.589747
83.476380	2397.241036	21.594765
83.407474	2418.284031	21.599783
83.615039	2430.770254	21.604800
83.036613	2411.710285	21.609818
83.729463	2400.579611	21.614835
83.793481	2444.378004	21.619853
84.313204	2418.738898	21.624871
84.417560	2441.842554	21.629888
84.001093	2415.014848	21.634906
84.175518	2400.546982	21.639923
84.480154	2383.548529	21.644941
84.131180	2428.394333	21.649959
84.501988	2399.329250	21.654976
84.211635	2430.072546	21.659994
84.193916	2417.655924	21.665011
84.638997	2451.217344	21.670029
84.485100	2430.772194	21.675047
84.927564	2422.978604	21.680064
84.680252	2443.628501	21.685082
84.892145	2422.613779	21.690099
84.985952	2440.877974	21.695117
84.635791	2421.374162	21.700135
84.925998	2409.091705	21.705152
84.849538	2446.479418	21.710170
85.184507	2426.396775	21.715187
85.077540	2454.885762	21.720205
85.139750	2464.677699	21.725223
85.367141	2436.105766	21.730240
84.970270	2483.698893	21.735258
85.365578	2466.512845	21.740275
85.849517	2487.751717	21.745293
85.802074	2470.148615	21.750311
86.165107	2505.542514	21.755328
85.961941	2494.823657	21.760346
86.478013	2468.604577	21.765363
86.149700	2509.085965	21.770381
86.245620	2473.927964	21.775399
86.578668	2467.786232	21.780416
85.918235	2505.588133	21.785434
86.034789	2469.788179	21.790451
86.382347	2486.983170	21.795469
86.476181	2485.609841	21.800487
86.348781	2499.733637	21.805504
86.678873	2490.721487	21.810522
86.558358	2516.462217	21.815539
87.079085	2494.218326	21.820557
86.660987	2528.643556	21.825575
87.135717	2481.773268	21.830592
86.840089	2502.127348	21.835610
86.811371	2548.022034	21.840627
87.275109	2534.956714	21.845645
87.225194	2540.697004	21.850663
87.784929	2515.701033	21.855680
87.573757	2550.181407	21.860698
87.795401	2529.098907	21.865715
87.840497	2526.850058	21.870733
87.801415	2539.451217	21.875751
88.061779	2527.073529	21.880768
87.638346	2546.302843	21.885786
88.256490	2535.706248	21.890803
88.428925	2535.287043	21.895821
88.121336	2571.309526	21.900839
88.632416	2530.618686	21.905856
88.865702	2553.144299	21.910874
88.696090	2551.602182	21.915891
88.918295	2556.621081	21.920909
89.045110	2544.477043	21.925927
89.223011	2537.000874	21.930944
88.934975	2560.544836	21.935962
89.035502	2546.583348	21.940979
89.351548	2530.688000	21.945997
89.117016	2540.536749	21.951015
89.263170	2554.214263	21.956032
88.925583	2552.389821	21.961050
88.897461	2531.234672	21.966067
89.207588	2563.505917	21.971085
89.157863	2564.058916	21.976103
89.568659	2587.121014	21.981120
89.744548	2583.920814	21.986138
89.659241	2585.711220	21.991155
90.075382	2573.730240	21.996173
89.584398	2582.605269	22.001191
90.004239	2593.190519	22.006208
89.971175	2589.322825	22.011226
89.867537	2605.413235	22.016243
90.019677	2602.671442	22.021261
90.039509	2588.480526	22.026279
90.165405	2601.005090	22.031296
90.293972	2614.382644	22.036314
90.628503	2620.708987	22.041331
90.998711	2618.302881	22.046349
90.909593	2636.891449	22.051367
91.063583	2620.325750	22.056384
91.043630	2627.215163	22.061402
91.722137	2607.256822	22.066419
91.172285	2630.593312	22.071437
91.542274	2618.722694	22.076455
91.393822	2615.738598	22.081472
91.524492	2625.931878	22.086490
91.430960	2608.333599	22.091507
91.935009	2622.412661	22.096525
91.583007	2619.144045	22.101543
91.558241	2625.977594	22.106560
91.530837	2635.581007	22.111578
91.538427	2635.039430	22.116595
92.083195	2644.998366	22.121613
91.840505	2665.974259	22.126631
92.163975	2627.816660	22.131648
92.180220	2677.860713	22.136666
91.832625	2677.713206	22.141683
92.573710	2662.169167	22.146701
92.584704	2649.119314	22.151719
92.394014	2648.880716	22.156736
92.243996	2682.566674	22.161754
92.594279	2731.182747	22.166771
93.107854	2716.136640	22.171789
92.526802	2704.663806	22.176807
93.151554	2679.189188	22.181824
93.352016	2700.013446	22.186842
93.482081	2681.726582	22.191859
93.371070	2705.310190	22.196877
93.814729	2714.126705	22.201895
93.685112	2726.699989	22.206912
94.109682	2701.966727	22.211930
93.943292	2731.055645	22.216947
94.059585	2689.536152	22.221965
94.193613	2727.721620	22.226983
94.543249	2696.476634	22.232000
94.477936	2729.218700	22.237018
94.354245	2702.187247	22.242035
94.243586	2724.010524	22.247053
94.466791	2699.353425	22.252071
94.480783	2712.385953	22.257088
94.530717	2718.736487	22.262106
94.215463	2708.777066	22.267123
94.934063	2683.222192	22.272141
94.547891	2746.413385	22.277159
94.537065	2741.923872	22.282176
95.215622	2709.667593	22.287194
94.620815	2752.094827	22.292211
94.838698	2725.702603	22.297229
95.093501	2749.946072	22.302247
95.388068	2764.168797	22.307264
95.947264	2774.341039	22.312282
95.217810	2783.123647	22.317299
95.811990	2764.790984	22.322317
95.604858	2780.881573	22.327335
95.841511	2761.577897	22.332352
95.942357	2771.639962	22.337370
95.779580	2759.727553	22.342387
96.036406	2788.258283	22.347405
96.287474	2766.715331	22.352423
96.191602	2790.632523	22.357440
96.740874	2781.545915	22.362458
96.303567	2797.255566	22.367475
97.127551	2771.298320	22.372493
96.997793	2786.531028	22.377511
96.859796	2789.745666	22.382528
97.095444	2774.418185	22.387546
97.162125	2790.921325	22.392563
97.354516	2765.182792	22.397581
97.441158	2773.493102	22.402599
97.623233	2795.235194	22.407616
97.238305	2764.654646	22.412634
97.075607	2802.845156	22.417651
97.265082	2770.499986	22.422669
97.492665	2804.142527	22.427687
97.381728	2805.558713	22.432704
97.837137	2803.943641	22.437722
97.777464	2804.862412	22.442739
98.100380	2828.816709	22.447757
98.043621	2821.646033	22.452775
98.383552	2792.870613	22.457792
98.339436	2840.044473	22.462810
98.887130	2816.214020	22.467827
98.820518	2839.896165	22.472845
98.695949	2815.412313	22.477863
98.514558	2858.648584	22.482880
98.652178	2859.546908	22.487898
98.871553	2824.778959	22.492915
98.827753	2831.048529	22.497933
98.899627	2865.410576	22.502951
98.941337	2827.871576	22.507968
99.328605	2873.157438	22.512986
99.405320	2860.984158	22.518003
99.716810	2886.332587	22.523021
99.835770	2856.703462	22.528039
99.850068	2868.048906	22.533056
99.664741	2835.167147	22.538074
100.010751	2844.965211	22.543091
99.764281	2859.397010	22.548109
100.076180	2843.698625	22.553127
99.992692	2857.424843	22.558144
100.273201	2856.211274	22.563162
100.150987	2866.135144	22.568179
100.391758	2895.730506	22.573197
100.308058	2863.224186	22.578215
100.261433	2888.473200	22.583232
100.859647	2871.413207	22.588250
100.539133	2892.676346	22.593267
100.312250	2879.878951	22.598285
101.030748	2869.229934	22.603303
100.999020	2919.685188	22.608320
101.525197	2881.919345	22.613338
101.211592	2923.339480	22.618355
101.445072	2885.580975	22.623373
101.390661	2927.527688	22.628391
101.035131	2898.937686	22.633408
101.650119	2921.395923	22.638426
101.653059	2916.873485	22.643443
101.774310	2963.405493	22.648461
102.157884	2923.647097	22.653479
101.771759	2947.534535	22.658496
101.871491	2928.666993	22.663514
101.964068	2931.663983	22.668531
102.213409	2966.657111	22.673549
102.519707	2943.528023	22.678567
102.441138	2982.875212	22.683584
103.118015	2944.649418	22.688602
102.718084	2967.400141	22.693619
102.907778	2928.608665	22.698637
102.842175	2958.110641	22.703655
103.231893	2959.276319	22.708672
103.084594	2947.173298	22.713690
103.346092	2952.723294	22.718707
103.343705	2979.550345	22.723725
103.745585	2980.666105	22.728743
103.754157	2963.936002	22.733760
104.004745	2973.768248	22.738778
104.062099	2987.257396	22.743795
104.082826	2974.161652	22.748813
104.479440	2961.209700	22.753831
104.154301	2993.141939	22.758848
104.071458	2963.008339	22.763866
104.185482	2964.140111	22.768883
104.079891	2975.822530	22.773901
104.714477	2939.207306	22.778919
104.217072	2998.155712	22.783936
104.361469	2985.120467	22.788954
104.692509	2984.541456	22.793971
104.746516	3027.605400	22.798989
104.569285	3002.047310	22.804007
104.906336	3011.961755	22.809024
104.784567	3043.256801	22.814042
105.196008	3021.317425	22.819059
105.339640	3049.871439	22.824077
105.436352	3018.430912	22.829095
105.554169	3041.995093	22.834112
105.120246	3056.207635	22.839130
105.722252	3046.911093	22.844147
105.840585	3067.244782	22.849165
105.934736	3069.086074	22.854183
106.091965	3039.061909	22.859200
106.375112	3043.674042	22.864218
105.854589	3081.284430	22.869235
106.186038	3045.789380	22.874253
106.519737	3080.391775	22.879271
106.347543	3079.049802	22.884288
106.691601	3078.357019	22.889306
106.635367	3083.859411	22.894323
106.843798	3069.365797	22.899341
107.274399	3071.086579	22.904359
107.005716	3095.878181	22.909376
107.369282	3098.706928	22.914394
107.709600	3093.882864	22.919411
107.501007	3103.584697	22.924429
107.825852	3105.053339	22.929447
107.817005	3097.564190	22.934464
108.032702	3102.692078	22.939482
108.050114	3097.070003	22.944499
107.836883	3097.871695	22.949517
108.099458	3088.328784	22.954535
107.882519	3110.675353	22.959552
108.262100	3091.694543	22.964570
107.975714	3115.126654	22.969587
108.424446	3101.632969	22.974605
108.794769	3128.533791	22.979623
108.566298	3153.650228	22.984640
108.650940	3114.771967	22.989658
109.229260	3088.707034	22.994675
109.139384	3140.280607	22.999693
109.000430	3119.199698	23.004711
108.928755	3112.568488	23.009728
109.610873	3158.336014	23.014746
109.519636	3129.887470	23.019763
109.447022	3117.327982	23.024781
109.840010	3147.872579	23.029799
109.684622	3113.710374	23.034816
109.849952	3151.051113	23.039834
109.476248	3142.610155	23.044851
110.145962	3126.317964	23.049869
110.434226	3174.645726	23.054887
110.525481	3139.226507	23.059904
110.830431	3175.751389	23.064922
110.663409	3162.888352	23.069939
110.933692	3141.676079	23.074957
111.009149	3162.047414	23.079975
110.962350	3127.523338	23.084992
111.292228	3138.531570	23.090010
111.280784	3171.731693	23.095027
111.133705	3128.651473	23.100045
111.031085	3166.455012	23.105063
110.982218	3168.143715	23.110080
111.434504	3166.433143	23.115098
111.640059	3182.037546	23.120115
111.578651	3190.475531	23.125133
111.569309	3166.583099	23.130151
111.500018	3202.893997	23.135168
111.500197	3186.627487	23.140186
111.702300	3208.687143	23.145203
111.976942	3222.528071	23.150221
112.303781	3208.742239	23.155239
112.108522	3234.984622	23.160256
112.143070	3226.678307	23.165274
112.970798	3228.276789	23.170291
112.519799	3258.524368	23.175309
113.174738	3237.688745	23.180327
112.949429	3238.400341	23.185344
113.049147	3241.617286	23.190362
113.119223	3239.513795	23.195379
113.620225	3216.685166	23.200397
113.405947	3238.662600	23.205415
113.250815	3224.931584	23.210432
113.371081	3271.752624	23.215450
113.877961	3230.218077	23.220467
113.725423	3265.239038	23.225485
114.028157	3267.153284	23.230503
114.157707	3241.098287	23.235520
114.065531	3277.777208	23.240538
114.533319	3263.620393	23.245555
114.229845	3278.619382	23.250573
114.470991	3270.934536	23.255591
114.284002	3296.894900	23.260608
114.651183	3264.873476	23.265626
115.089465	3286.850754	23.270643
114.592300	3287.795268	23.275661
115.300238	3301.840910	23.280679
115.280780	3325.130109	23.285696
115.315095	3293.898732	23.290714
115.641513	3319.969197	23.295731
115.543933	3299.897698	23.300749
115.498083	3311.715591	23.305767
115.658286	3294.353686	23.310784
115.592485	3337.625644	23.315802
116.357237	3310.930422	23.320819
116.053074	3356.372094	23.325837
116.278299	3322.582117	23.330855
116.511113	3349.580002	23.335872
116.676238	3333.338154	23.340890
116.733229	3321.659252	23.345907
116.586984	3354.492713	23.350925
116.732733	3324.727006	23.355943
116.850755	3354.123417	23.360960
117.135552	3353.821569	23.365978
117.383490	3356.682178	23.370995
117.292718	3358.149475	23.376013
117.404849	3359.717350	23.381031
117.623645	3381.002962	23.386048
117.687515	3352.775453	23.391066
117.545225	3358.786435	23.396083
117.687588	3367.233718	23.401101
118.001007	3357.872879	23.406119
118.091813	3375.824878	23.411136
117.687970	3389.732467	23.416154
118.431216	3371.136156	23.421171
118.169697	3370.336987	23.426189
118.037418	3391.810743	23.431207
118.292200	3384.304579	23.436224
119.318067	3374.907996	23.441242
119.981033	3366.465211	23.446259
120.000603	3357.575987	23.451277
119.880114	3334.227231	23.456295
119.880914	3348.875724	23.461312
119.503691	3323.668313	23.466330
119.944873	3360.881439	23.471347
119.677234	3342.394445	23.476365
120.050424	3335.597805	23.481383
119.871061	3343.865120	23.486400
120.023716	3323.244763	23.491418
119.973017	3347.308263	23.496435
120.030203	3324.307967	23.501453
119.933895	3332.934874	23.506471
120.179989	3325.119423	23.511488
119.928754	3351.617144	23.516506
120.442337	3346.522315	23.521523
120.225099	3352.139366	23.526541
120.386480	3359.955128	23.531559
120.621602	3396.947136	23.536576
121.169988	3390.584264	23.541594
121.348944	3386.478036	23.546611
120.964007	3404.807196	23.551629
121.183292	3388.604632	23.556647
121.081240	3420.635952	23.561664
121.094843	3413.435672	23.566682
121.602467	3408.800355	23.571699
121.478920	3441.543080	23.576717
121.818555	3441.485770	23.581735
121.892054	3442.780574	23.586752
122.151098	3460.685400	23.591770
122.523558	3439.076479	23.596787
122.135059	3456.670020	23.601805
122.106289	3470.787679	23.606823
122.540950	3465.209053	23.611840
122.677287	3485.245481	23.616858
123.185202	3477.728010	23.621875
123.088947	3475.243552	23.626893
123.714011	3488.723659	23.631911
123.634710	3508.336706	23.636928
123.865493	3490.649461	23.641946
123.739791	3505.824064	23.646963
123.922642	3492.145093	23.651981
123.978761	3490.367869	23.656999
123.974891	3488.812593	23.662016
123.943623	3504.263962	23.667034
124.168984	3475.186899	23.672051
123.853834	3491.914544	23.677069
124.214637	3479.398115	23.682087
124.485061	3527.853391	23.687104
124.735961	3521.346756	23.692122
124.837481	3525.523914	23.697139
124.287658	3537.580457	23.702157
124.222633	3529.436941	23.707175
124.660442	3533.802750	23.712192
124.829290	3563.396780	23.717210
125.058695	3568.628840	23.722227
125.385629	3554.746704	23.727245
125.331689	3573.917659	23.732263
125.897299	3564.769761	23.737280
125.627060	3567.356709	23.742298
125.994441	3593.893094	23.747315
125.964901	3572.418086	23.752333
125.719327	3591.546467	23.757351
126.003356	3589.986175	23.762368
126.165573	3618.602843	23.767386
126.480104	3601.462172	23.772403
126.669494	3604.837953	23.777421
126.561281	3626.593753	23.782439
126.794809	3639.063506	23.787456
126.884795	3627.634745	23.792474
127.310609	3644.061920	23.797491
127.343185	3639.973457	23.802509
127.390493	3634.394391	23.807527
127.825847	3659.650479	23.812544
127.552485	3675.541015	23.817562
127.883336	3663.085055	23.822579
128.069806	3658.634594	23.827597
127.745327	3651.498332	23.832615
127.995743	3661.663807	23.837632
128.103745	3667.050557	23.842650
128.024989	3680.933328	23.847667
128.494040	3683.319033	23.852685
128.800012	3696.309029	23.857703
129.166658	3678.636079	23.862720
128.899342	3680.461146	23.867738
129.258635	3692.309924	23.872755
129.158482	3725.132147	23.877773
129.490589	3700.977517	23.882791
129.442740	3726.844876	23.887808
129.559201	3697.362328	23.892826
129.646679	3692.187444	23.897843
129.766895	3713.379923	23.902861
130.064308	3709.935133	23.907879
130.505260	3730.400011	23.912896
130.519193	3737.404109	23.917914
130.121930	3744.961475	23.922931
130.389024	3706.581935	23.927949
130.369745	3743.078133	23.932967
130.598166	3722.858889	23.937984
130.640482	3766.507396	23.943002
131.098234	3756.619072	23.948019
131.013149	3747.004526	23.953037
131.138507	3770.211561	23.958055
131.507418	3735.637067	23.963072
131.418876	3771.696013	23.968090
131.829598	3739.942709	23.973107
131.843144	3757.337205	23.978125
132.033490	3777.656469	23.983143
132.046702	3750.218949	23.988160
131.909672	3798.477365	23.993178
132.352829	3775.174113	23.998195
132.279019	3769.305170	24.003213
132.016549	3783.384094	24.008231
132.689756	3774.227564	24.013248
132.289168	3788.036683	24.018266
132.712717	3804.248083	24.023283
132.697351	3796.828049	24.028301
133.115550	3795.414679	24.033319
133.195344	3820.266000	24.038336
133.495867	3834.176540	24.043354
133.435513	3815.271238	24.048371
133.432597	3824.524632	24.053389
133.136979	3826.329058	24.058407
133.899450	3844.908447	24.063424
133.794641	3844.343843	24.068442
133.696596	3858.037924	24.073459
134.357834	3840.071595	24.078477
134.469186	3886.955813	24.083495
134.325969	3875.963644	24.088512
134.591832	3862.745421	24.093530
135.039918	3846.692298	24.098547
135.149368	3895.233457	24.103565
135.036875	3883.028140	24.108583
135.747366	3868.871376	24.113600
135.045471	3902.954925	24.118618
135.455897	3875.342920	24.123635
135.768307	3905.562139	24.128653
135.707709	3936.041485	24.133671
135.891271	3902.927799	24.138688
136.462469	3884.156905	24.143706
136.071095	3921.976187	24.148723
136.788498	3898.581027	24.153741
136.504363	3934.442656	24.158759
137.096936	3907.798194	24.163776
137.110197	3934.203663	24.168794
137.040891	3926.408294	24.173811
137.314895	3942.525701	24.178829
136.837836	3920.230298	24.183847
137.516019	3899.895832	24.188864
136.980293	3938.303752	24.193882
137.250341	3919.977287	24.198899
137.518494	3932.706075	24.203917
137.366183	3969.799070	24.208935
138.050651	3930.142570	24.213952
137.957002	3961.681310	24.218970
137.838853	3978.873668	24.223987
138.647793	3968.752216	24.229005
138.565395	3968.536441	24.234023
138.655117	3986.930659	24.239040
138.511322	3965.777714	24.244058
138.582067	3982.287847	24.249075
139.088268	3972.559992	24.254093
138.660187	4030.446638	24.259111
138.960170	3987.602529	24.264128
139.630810	4003.221758	24.269146
139.055917	4002.926399	24.274163
139.921085	3973.796673	24.279181
139.494072	4034.962594	24.284199
140.282196	3998.800877	24.289216
139.878592	4030.625174	24.294234
139.842947	4050.253225	24.299251
140.204425	4007.370147	24.304269
140.395147	4052.874303	24.309287
140.494093	4048.715359	24.314304
140.950169	4019.362082	24.319322
141.074010	4021.600727	24.324339
141.121127	4064.110324	24.329357
140.879842	4035.033401	24.334375
141.484802	4026.413065	24.339392
141.564804	4093.850385	24.344410
141.372516	4077.541202	24.349427
141.375508	4061.911224	24.354445
141.314052	4069.178436	24.359463
142.149175	4057.407913	24.364480
142.138676	4085.502397	24.369498
142.186250	4127.320658	24.374515
142.341653	4096.445842	24.379533
142.306484	4089.617216	24.384551
142.394454	4118.022512	24.389568
142.775071	4130.707582	24.394586
142.583817	4131.210049	24.399603
143.237931	4116.752893	24.404621
143.158168	4151.756505	24.409639
143.497330	4147.600923	24.414656
143.676550	4157.845747	24.419674
143.992585	4132.361204	24.424691
144.224324	4181.903289	24.429709
144.213786	4148.784599	24.434727
144.234257	4163.042961	24.439744
144.321277	4140.193166	24.444762
144.483087	4152.309798	24.449779
144.442979	4170.120028	24.454797
144.517131	4172.896024	24.459815
144.603550	4191.398795	24.464832
144.711636	4155.014739	24.469850
144.776092	4212.923473	24.474867
145.506820	4198.822167	24.479885
145.366143	4204.793905	24.484903
145.644409	4218.160077	24.489920
145.959407	4202.831826	24.494938
145.403108	4223.339199	24.499955
145.944907	4206.283516	24.504973
145.682932	4244.080635	24.509991
145.444318	4231.776353	24.515008
146.548721	4207.880842	24.520026
146.082724	4269.260840	24.525043
146.357348	4248.930456	24.530061
146.577062	4276.258600	24.535079
146.620762	4274.930073	24.540096
146.946763	4250.287799	24.545114
146.921345	4302.213112	24.550131
147.622572	4276.454509	24.555149
147.440920	4285.683202	24.560167
147.578907	4293.459145	24.565184
147.571856	4288.144943	24.570202
147.651103	4290.555934	24.575219
147.966720	4330.671443	24.580237
148.171527	4304.608062	24.585255
148.262705	4326.934102	24.590272
148.468859	4325.793634	24.595290
148.428168	4333.456492	24.600307
148.635011	4352.104673	24.605325
148.491503	4341.528334	24.610343
148.836674	4361.377699	24.615360
149.482163	4367.390133	24.620378
149.389128	4357.545966	24.625395
149.705913	4379.965123	24.630413
149.701666	4350.792352	24.635431
149.955520	4358.266664	24.640448
149.989006	4385.897671	24.645466
150.030093	4368.920850	24.650483
150.359073	4398.603530	24.655501
150.460733	4378.088939	24.660519
150.267521	4396.247166	24.665536
151.145593	4386.894763	24.670554
150.984210	4423.006258	24.675571
151.293937	4391.173253	24.680589
151.289342	4438.509592	24.685607
151.051260	4408.227060	24.690624
151.745720	4396.431501	24.695642
151.439341	4432.860344	24.700659
151.943163	4414.557348	24.705677
151.926127	4428.046316	24.710695
151.793293	4461.343452	24.715712
152.351549	4418.167421	24.720730
152.068528	4448.617218	24.725747
152.707262	4442.827122	24.730765
152.353071	4474.486384	24.735783
152.076324	4463.564622	24.740800
152.826670	4457.793697	24.745818
152.633007	4513.398202	24.750835
153.263438	4489.554999	24.755853
153.429288	4483.310870	24.760871
153.171988	4505.425284	24.765888
153.769964	4518.504761	24.770906
153.793709	4527.805481	24.775923
153.931328	4520.218304	24.780941
154.054629	4509.812485	24.785959
154.098346	4545.229218	24.790976
154.402921	4522.437752	24.795994
154.294061	4569.655048	24.801011
154.689016	4538.611309	24.806029
154.471966	4557.338352	24.811047
154.740089	4544.432246	24.816064
154.949228	4590.257662	24.821082
155.247391	4568.606224	24.826099
155.635185	4558.220345	24.831117
155.310485	4600.335308	24.836135
156.040470	4573.968237	24.841152
156.061387	4621.871424	24.846170
155.944644	4587.886047	24.851187
156.209819	4606.414333	24.856205
156.228251	4615.188110	24.861223
156.286291	4608.070624	24.866240
156.725052	4643.025771	24.871258
156.517611	4626.354170	24.876275
157.421889	4601.870836	24.881293
156.970818	4647.933856	24.886311
157.208041	4654.891778	24.891328
157.916470	4637.913656	24.896346
157.683654	4665.813421	24.901363
157.813674	4641.557310	24.906381
158.397355	4634.657292	24.911399
157.831731	4671.666921	24.916416
158.394388	4636.567755	24.921434
158.504247	4693.108655	24.926451
158.586974	4669.422502	24.931469
158.702847	4684.984601	24.936487
158.716983	4659.823399	24.941504
159.152752	4700.550091	24.946522
158.931295	4710.010381	24.951539
159.013130	4699.932783	24.956557
159.722444	4697.563539	24.961575
159.385126	4720.786852	24.966592
159.992519	4729.447912	24.971610
159.741663	4719.718344	24.976627
159.964657	4733.534332	24.981645
160.561999	4725.561446	24.986663
160.312496	4761.579263	24.991680
160.873381	4747.565092	24.996698
160.525578	4767.062152	25.001715
160.571738	4759.561808	25.006733
160.897286	4766.297234	25.011751
160.844671	4793.248111	25.016768
161.355203	4769.735880	25.021786
161.470245	4815.976630	25.026803
161.216267	4810.971435	25.031821
161.984560	4797.699014	25.036839
161.930535	4809.626404	25.041856
162.462301	4812.779533	25.046874
162.624290	4852.849380	25.051891
162.813484	4846.798831	25.056909
162.718385	4852.322242	25.061927
162.849312	4851.211037	25.066944
162.755192	4849.122483	25.071962
163.144430	4853.741883	25.076979
163.009016	4848.035730	25.081997
163.513085	4847.809820	25.087015
163.378366	4882.721669	25.092032
163.812715	4869.245974	25.097050
163.202097	4893.500405	25.102067
163.707776	4867.548538	25.107085
164.146397	4915.013200	25.112103
163.523364	4923.757275	25.117120
163.994857	4911.609030	25.122138
164.611977	4950.915093	25.127155
164.239905	4938.530013	25.132173
164.780816	4930.292253	25.137191
164.590576	4984.365554	25.142208
165.125062	4961.350311	25.147226
165.452469	4997.155574	25.152243
165.440657	4999.050981	25.157261
165.712404	4978.237032	25.162279
165.853590	5004.484789	25.167296
166.211723	5010.897316	25.172314
166.342923	5019.182921	25.177331
166.749956	5001.759978	25.182349
167.192034	5024.392217	25.187367
167.474523	5019.174761	25.192384
167.394771	5013.697245	25.197402
167.636297	5048.484205	25.202419
167.039260	5036.199418	25.207437
168.090123	5027.515280	25.212455
167.525879	5037.856445	25.217472
167.776269	5043.280003	25.222490
168.026945	5033.562303	25.227507
168.060202	5065.226354	25.232525
168.400659	5060.433890	25.237543
168.064308	5073.580234	25.242560
168.766546	5063.621382	25.247578
168.541522	5078.461798	25.252595
168.521110	5095.838908	25.257613
169.021655	5100.985812	25.262631
168.904676	5120.042967	25.267648
169.184416	5100.612134	25.272666
169.361366	5127.834615	25.277683
169.660711	5135.083375	25.282701
170.254091	5108.667119	25.287719
170.154448	5163.968807	25.292736
170.243362	5126.014394	25.297754
170.411434	5143.403991	25.302771
170.437957	5197.530049	25.307789
171.273859	5172.606693	25.312807
171.349065	5155.423706	25.317824
171.300721	5184.479789	25.322842
171.371581	5178.784673	25.327859
171.825093	5163.279938	25.332877
171.819865	5210.356898	25.337895
171.780114	5185.943660	25.342912
171.872674	5218.463155	25.347930
171.945086	5185.901610	25.352947
172.397175	5183.588253	25.357965
172.699965	5215.046022	25.362983
172.643588	5209.693723	25.368000
172.701250	5237.479815	25.373018
172.663359	5218.826369	25.378035
173.004289	5239.075667	25.383053
173.359440	5246.359639	25.388071
173.557608	5242.669142	25.393088
173.648485	5240.968769	25.398106
173.705838	5261.869849	25.403123
174.085908	5270.624120	25.408141
174.360625	5262.497061	25.413159
174.437727	5287.796565	25.418176
174.296136	5279.172600	25.423194
174.394114	5286.325310	25.428211
174.421218	5292.996853	25.433229
174.877774	5302.314021	25.438247
174.622090	5328.047412	25.443264
175.403141	5309.048516	25.448282
175.415002	5338.814342	25.453299
175.554122	5326.533877	25.458317
175.903673	5371.732018	25.463335
176.149567	5352.122163	25.468352
176.325403	5357.759119	25.473370
176.248676	5374.657786	25.478387
176.664551	5389.238205	25.483405
177.019985	5367.914745	25.488423
176.816038	5409.637513	25.493440
176.458560	5386.117155	25.498458
177.095267	5403.196333	25.503475
177.325839	5419.061897	25.508493
177.602826	5424.667018	25.513511
177.527355	5432.306099	25.518528
178.045897	5412.689669	25.523546
178.040953	5465.468607	25.528563
177.939727	5456.968695	25.533581
179.166099	5444.817667	25.538599
178.651892	5487.143957	25.543616
179.206895	5450.291307	25.548634
179.268671	5489.011579	25.553651
178.851402	5483.749759	25.558669
179.749528	5471.275000	25.563687
179.674864	5471.560669	25.568704
179.658990	5521.287573	25.573722
179.878067	5498.189618	25.578739
180.075421	5482.263595	25.583757
180.440272	5527.591156	25.588775
179.928713	5521.768487	25.593792
180.545944	5496.058133	25.598810
180.671308	5559.790364	25.603827
180.469387	5548.177720	25.608845
181.063805	5530.068168	25.613863
181.133445	5588.746962	25.618880
181.425755	5561.341805	25.623898
181.818748	5568.938523	25.628915
181.690767	5567.874837	25.633933
181.877856	5600.603530	25.638951
181.956068	5594.810317	25.643968
182.191516	5613.109390	25.648986
182.522209	5588.843329	25.654003
182.977380	5608.883753	25.659021
182.765592	5609.763225	25.664039
183.269683	5616.978009	25.669056
182.962365	5624.077494	25.674074
183.612393	5627.152162	25.679092
183.514070	5643.667518	25.684109
183.658757	5652.384809	25.689127
183.710849	5673.909601	25.694144
184.071733	5667.649614	25.699162
184.024500	5683.984580	25.704180
184.300746	5671.120253	25.709197
184.456508	5716.997816	25.714215
185.251726	5708.494871	25.719232
184.831447	5742.090119	25.724250
185.529761	5698.986354	25.729268
185.331341	5750.704413	25.734285
185.678246	5715.370389	25.739303
185.713519	5750.121875	25.744320
186.082998	5740.654616	25.749338
186.561320	5744.027315	25.754356
186.805050	5775.535037	25.759373
186.796731	5764.779559	25.764391
186.813128	5771.741752	25.769408
186.976661	5755.588746	25.774426
187.185089	5776.839375	25.779444
187.029206	5788.621732	25.784461
187.578310	5804.891653	25.789479
187.500743	5783.823867	25.794496
187.671380	5835.366163	25.799514
188.089030	5808.084537	25.804532
188.099522	5828.897912	25.809549
188.623117	5818.851394	25.814567
188.707689	5832.849406	25.819584
188.714291	5841.167141	25.824602
188.831301	5831.759743	25.829620
188.689752	5869.631517	25.834637
189.329429	5854.107396	25.839655
189.401920	5898.670025	25.844672
189.243943	5876.844723	25.849690
189.650732	5915.064250	25.854708
189.996434	5899.957497	25.859725
190.097633	5941.478134	25.864743
190.252132	5921.856920	25.869760
190.691877	5950.602252	25.874778
191.095193	5930.343446	25.879796
191.002019	5967.246377	25.884813
191.484481	5955.791788	25.889831
191.744840	5937.600469	25.894848
191.419579	5969.404654	25.899866
191.816430	5945.460247	25.904884
191.849208	5991.351977	25.909901
192.128544	5962.797159	25.914919
192.636679	5984.780741	25.919936
192.746929	5972.136941	25.924954
192.463071	5974.306356	25.929972
192.736620	6001.107528	25.934989
193.163046	5999.783915	25.940007
193.648547	6004.577941	25.945024
193.183485	6014.040923	25.950042
193.814837	6023.422734	25.955060
194.230996	6011.916520	25.960077
193.788130	6031.879624	25.965095
193.817533	6037.526027	25.970112
194.218210	6040.895441	25.975130
194.350391	6045.287931	25.980148
194.345776	6076.732041	25.985165
194.647287	6070.980928	25.990183
195.033871	6096.931888	25.995200
194.476316	6096.961765	26.000218
194.994811	6133.913142	26.005236
195.237085	6119.839907	26.010253
195.472798	6164.747871	26.015271
196.185978	6153.146991	26.020288
196.411565	6183.975589	26.025306
196.412901	6191.693292	26.030324
196.733573	6170.403329	26.035341
197.077650	6200.696184	26.040359
197.401044	6203.482394	26.045376
197.281609	6207.835586	26.050394
197.378059	6217.331909	26.055412
198.083970	6222.890198	26.060429
197.999202	6218.853557	26.065447
198.162466	6246.037805	26.070464
198.501655	6240.832914	26.075482
198.730608	6228.564128	26.080500
198.687100	6251.508553	26.085517
198.924286	6269.674420	26.090535
199.376551	6242.718482	26.095552
199.117470	6287.014940	26.100570
199.675163	6265.829454	26.105588
199.899237	6302.639375	26.110605
199.968532	6287.078285	26.115623
200.468732	6291.709567	26.120640
200.647498	6274.568561	26.125658
201.339771	6309.401507	26.130676
201.072815	6304.322339	26.135693
201.331876	6311.419971	26.140711
201.546269	6293.019976	26.145728
201.253051	6321.602804	26.150746
201.815858	6290.230453	26.155764
201.820064	6330.380614	26.160781
201.703265	6314.794878	26.165799
202.090171	6301.059530	26.170816
201.865810	6352.817662	26.175834
202.168352	6335.722939	26.180852
202.842406	6343.001466	26.185869
202.693069	6385.297329	26.190887
203.007386	6350.363508	26.195904
202.913845	6386.587007	26.200922
203.131778	6377.538454	26.205940
203.387386	6389.874860	26.210957
203.167811	6392.692597	26.215975
203.869767	6409.196090	26.220992
203.482131	6427.574269	26.226010
204.017133	6427.311164	26.231028
204.060135	6447.912526	26.236045
204.245455	6467.439336	26.241063
204.549481	6460.364351	26.246080
205.024414	6502.078744	26.251098
204.972571	6497.191014	26.256116
205.633012	6510.404729	26.261133
205.193542	6525.163553	26.266151
205.757321	6531.578586	26.271168
205.474432	6557.983262	26.276186
206.479400	6558.008716	26.281204
206.522724	6590.384093	26.286221
206.773920	6575.086377	26.291239
207.588646	6616.928666	26.296256
207.423908	6613.892840	26.301274
207.553148	6578.623716	26.306292
208.050585	6610.781979	26.311309
207.911481	6592.201152	26.316327
208.674298	6595.001570	26.321344
208.573926	6635.438303	26.326362
208.914288	6597.846779	26.331380
208.924355	6631.569765	26.336397
208.826932	6616.042776	26.341415
209.192978	6648.657935	26.346432
209.640386	6636.471215	26.351450
209.627274	6640.331590	26.356468
209.609069	6664.168745	26.361485
210.008621	6661.961105	26.366503
210.101130	6683.574551	26.371520
210.567776	6655.728886	26.376538
210.303075	6712.188546	26.381556
210.803381	6692.198837	26.386573
210.670315	6713.508404	26.391591
211.141337	6713.368005	26.396608
211.247379	6729.190320	26.401626
211.332411	6727.803058	26.406644
211.718227	6746.414733	26.411661
211.694523	6773.680898	26.416679
212.093216	6775.235721	26.421696
212.201141	6790.660482	26.426714
212.456584	6799.596041	26.431732
213.055813	6807.524017	26.436749
212.978923	6817.283605	26.441767
213.275977	6826.933232	26.446784
213.210540	6826.695823	26.451802
213.495545	6816.593835	26.456820
214.336704	6840.524800	26.461837
214.160936	6854.187631	26.466855
214.248661	6830.329632	26.471872
214.369494	6866.661748	26.476890
214.263192	6878.068855	26.481908
214.964511	6853.942268	26.486925
214.548626	6924.881490	26.491943
215.108972	6880.158219	26.496960
215.152004	6928.922173	26.501978
215.275602	6921.829314	26.506996
215.894042	6944.811693	26.512013
215.998821	6946.615593	26.517031
216.431159	6960.973868	26.522048
216.234670	6960.660574	26.527066
216.583923	6995.456987	26.532084
217.097809	6985.581969	26.537101
217.181512	7003.379817	26.542119
217.374011	7005.928986	26.547136
217.758859	7024.810246	26.552154
217.789041	7039.095020	26.557172
218.575409	7035.728883	26.562189
218.184470	7056.593032	26.567207
218.495752	7066.776350	26.572224
218.707110	7067.729280	26.577242
219.178880	7070.179651	26.582260
219.651645	7104.231213	26.587277
218.961631	7087.758062	26.592295
219.945248	7105.578584	26.597312
220.038639	7118.511095	26.602330
220.233903	7100.936132	26.607348
220.034698	7136.609459	26.612365
220.632300	7115.174861	26.617383
220.763567	7135.708821	26.622400
221.195990	7145.060127	26.627418
221.054039	7139.352550	26.632436
221.844288	7168.149026	26.637453
221.764340	7159.236393	26.642471
221.940711	7187.458061	26.647488
222.329097	7180.154495	26.652506
222.217497	7198.353503	26.657524
222.535094	7186.721263	26.662541
222.805745	7235.184002	26.667559
222.888106	7201.068020	26.672576
223.497589	7194.759114	26.677594
223.611269	7244.397987	26.682612
223.977195	7249.059638	26.687629
224.188736	7253.428824	26.692647
224.212702	7257.515554	26.697664
224.643670	7226.169330	26.702682
224.717680	7294.223359	26.707700
224.494772	7275.059428	26.712717
224.922601	7250.923084	26.717735
225.035991	7303.456827	26.722752
225.071809	7301.848399	26.727770
225.071080	7285.717554	26.732788
225.876284	7317.645758	26.737805
225.354964	7336.144717	26.742823
225.767489	7311.902136	26.747840
226.091522	7349.391898	26.752858
225.858972	7379.167749	26.757876
226.192849	7373.539228	26.762893
226.435381	7382.460676	26.767911
226.998618	7410.685616	26.772928
227.415688	7416.352573	26.777946
227.601874	7435.847479	26.782964
228.451910	7434.208378	26.787981
228.538708	7425.257988	26.792999
228.322568	7457.142379	26.798016
228.846896	7454.814812	26.803034
229.147196	7452.246789	26.808052
229.445757	7491.554563	26.813069
229.498299	7494.039580	26.818087
229.744553	7503.462493	26.823104
230.014759	7518.288558	26.828122
229.548802	7505.610990	26.833140
230.555584	7494.588578	26.838157
230.382038	7531.831596	26.843175
230.615874	7546.583232	26.848192
231.341646	7527.233910	26.853210
231.460240	7551.045175	26.858228
231.664942	7575.605961	26.863245
231.791080	7585.534326	26.868263
232.072363	7561.510539	26.873280
232.887557	7563.655258	26.878298
231.870062	7598.104457	26.883316
232.906577	7561.681245	26.888333
232.905712	7619.336017	26.893351
232.754461	7590.908870	26.898368
233.329179	7609.139814	26.903386
233.403507	7644.839996	26.908404
233.632458	7602.006180	26.913421
233.828640	7667.686720	26.918439
233.921576	7664.156392	26.923456
234.608830	7651.689060	26.928474
234.549404	7699.965957	26.933492
235.254504	7661.691227	26.938509
235.227658	7725.600254	26.943527
235.260947	7711.885361	26.948544
236.009065	7735.976605	26.953562
236.062704	7715.956017	26.958580
236.169176	7731.163254	26.963597
236.134497	7743.170179	26.968615
236.370836	7733.297215	26.973632
236.970268	7764.388963	26.978650
236.914602	7776.308776	26.983668
237.263902	7769.428172	26.988685
237.268628	7783.048920	26.993703
237.494875	7799.507855	26.998720
238.031628	7788.221823	27.003738
237.993272	7804.574234	27.008756
238.230321	7831.648132	27.013773
238.663458	7837.554249	27.018791
238.987759	7837.899106	27.023808
239.239933	7845.739771	27.028826
239.213091	7860.587566	27.033844
239.474509	7860.554542	27.038861
239.719565	7860.783780	27.043879
239.756630	7894.084378	27.048896
240.520809	7890.202290	27.053914
240.202927	7910.650768	27.058932
240.504775	7913.135456	27.063949
240.633631	7937.356431	27.068967
241.024248	7942.700488	27.073984
241.246909	7942.527291	27.079002
241.350812	7972.671650	27.084020
241.761412	7978.401232	27.089037
242.112597	7991.986613	27.094055
242.337753	8012.564259	27.099072
242.554992	7996.083163	27.104090
242.555706	8035.406022	27.109108
243.449225	8013.409950	27.114125
243.300408	8058.539962	27.119143
243.826681	8049.678871	27.124160
243.978859	8060.645178	27.129178
243.895743	8055.283519	27.134196
244.258679	8097.677277	27.139213
244.741436	8060.319806	27.144231
244.648513	8107.836590	27.149248
245.179858	8096.205373	27.154266
245.310158	8105.981956	27.159284
245.257465	8145.279785	27.164301
245.661958	8116.130421	27.169319
245.829053	8163.367914	27.174336
246.385964	8146.120412	27.179354
246.304528	8194.628245	27.184372
246.832178	8161.622497	27.189389
247.266689	8205.965185	27.194407
247.226326	8189.787745	27.199424
247.798148	8222.317704	27.204442
248.129974	8212.522838	27.209460
248.066754	8234.655934	27.214477
248.446479	8228.328935	27.219495
248.402930	8245.186240	27.224512
248.679379	8255.520713	27.229530
248.907977	8272.128513	27.234548
248.983818	8282.251059	27.239565
249.512490	8285.735151	27.244583
249.714751	8315.266518	27.249600
249.931710	8322.530779	27.254618
250.360534	8305.597007	27.259636
250.172284	8358.950530	27.264653
250.303638	8332.796566	27.269671
250.591389	8386.112079	27.274688
251.050827	8362.043655	27.279706
251.357150	8389.675638	27.284724
251.719345	8407.470119	27.289741
252.267434	8393.817319	27.294759
252.290537	8401.672762	27.299776
252.221915	8420.949916	27.304794
252.343398	8437.963684	27.309812
253.273763	8427.701085	27.314829
253.470546	8425.068354	27.319847
253.281652	8464.674366	27.324864
253.931027	8447.202474	27.329882
253.757604	8462.139543	27.334900
254.257079	8468.189566	27.339917
254.683379	8509.068345	27.344935
254.610638	8489.202991	27.349952
254.958875	8515.895308	27.354970
254.887823	8506.961563	27.359988
255.566026	8531.679792	27.365005
255.483715	8529.994065	27.370023
255.545321	8567.823023	27.375040
256.110241	8564.262100	27.380058
256.204536	8579.546897	27.385076
256.497482	8610.295055	27.390093
256.992073	8610.268930	27.395111
256.926712	8612.336216	27.400128
257.205613	8657.007998	27.405146
257.581888	8648.589870	27.410164
257.743416	8672.399235	27.415181
258.390422	8667.135002	27.420199
258.295905	8686.392233	27.425216
258.625619	8689.650044	27.430234
258.830247	8698.447709	27.435252
258.875445	8726.797865	27.440269
259.725334	8722.015890	27.445287
259.819411	8765.847177	27.450304
260.458498	8738.254994	27.455322
260.109464	8777.620610	27.460340
260.521070	8778.238790	27.465357
260.777615	8785.653556	27.470375
260.890080	8812.664903	27.475392
261.236095	8809.633764	27.480410
261.423306	8835.015414	27.485428
261.377158	8854.578330	27.490445
261.898844	8849.098734	27.495463
262.310566	8875.308661	27.500480
262.630923	8886.626475	27.505498
262.924148	8908.389786	27.510516
263.407597	8908.109702	27.515533
263.723039	8915.838555	27.520551
263.767196	8933.504165	27.525568
264.067433	8934.834138	27.530586
264.328131	8945.781440	27.535604
264.373652	8969.966231	27.540621
264.754876	8968.799093	27.545639
264.758449	8990.304169	27.550656
265.167866	8989.354833	27.555674
265.137410	8987.594689	27.560692
265.439450	9024.223065	27.565709
266.005348	9026.604872	27.570727
266.148716	9037.468254	27.575744
266.493903	9052.886268	27.580762
266.943390	9045.205764	27.585780
266.769057	9050.456932	27.590797
267.168466	9086.759906	27.595815
267.513856	9087.154555	27.600832
267.433580	9087.279082	27.605850
267.915761	9119.612834	27.610868
268.482145	9123.728505	27.615885
268.720309	9127.125335	27.620903
268.488717	9150.437068	27.625920
269.183912	9159.335438	27.630938
269.029354	9162.833433	27.635956
269.417992	9176.214846	27.640973
269.880926	9189.881877	27.645991
269.846478	9216.248507	27.651008
269.978629	9234.301373	27.656026
270.431303	9248.796340	27.661044
270.719216	9260.236858	27.666061
271.162271	9268.457435	27.671079
271.183617	9291.247878	27.676096
271.438899	9321.464083	27.681114
272.210209	9319.330588	27.686132
272.354465	9328.859056	27.691149
272.838260	9353.869322	27.696167
273.261855	9374.412500	27.701184
273.422623	9374.872784	27.706202
273.743839	9382.478596	27.711220
273.880817	9388.317264	27.716237
274.389840	9408.233476	27.721255
274.308596	9408.591085	27.726272
274.553387	9417.911973	27.731290
274.985328	9431.951654	27.736308
275.203164	9430.592159	27.741325
275.347324	9475.846577	27.746343
275.510113	9460.979821	27.751360
275.697384	9501.025159	27.756378
276.158062	9488.704174	27.761396
276.414147	9514.039409	27.766413
276.624729	9537.169521	27.771431
276.971932	9538.534558	27.776448
277.539260	9553.549800	27.781466
277.663996	9576.715690	27.786484
277.451367	9565.137794	27.791501
278.027067	9606.726817	27.796519
278.284096	9598.741482	27.801536
278.603379	9614.202766	27.806554
278.734598	9627.547317	27.811572
278.608515	9655.356410	27.816589
279.355260	9638.983872	27.821607
279.523089	9709.723674	27.826624
279.161520	9696.856036	27.831642
280.363825	9696.865845	27.836660
280.203287	9740.074043	27.841677
280.716591	9726.555035	27.846695
281.147122	9763.619588	27.851712
281.345838	9753.215002	27.856730
281.912863	9796.933006	27.861748
281.859486	9774.690653	27.866765
282.224146	9809.740655	27.871783
282.392024	9799.445221	27.876800
282.663479	9834.636046	27.881818
283.258023	9815.813460	27.886836
282.804107	9844.705250	27.891853
283.168844	9872.282667	27.896871
283.690254	9868.582406	27.901888
283.947783	9922.424451	27.906906
284.318618	9906.416479	27.911924
284.492079	9922.015824	27.916941
284.741185	9950.592340	27.921959
285.232816	9953.989096	27.926976
285.144634	9993.066469	27.931994
286.343009	9968.444879	27.937012
286.046435	10014.105620	27.942029
286.424533	10001.824924	27.947047
286.610563	10032.735490	27.952064
286.833679	10058.983854	27.957082
287.580213	10056.498909	27.962100
287.634752	10074.397540	27.967117
287.814991	10095.683636	27.972135
288.124811	10104.662890	27.977152
288.301370	10120.484654	27.982170
288.628168	10128.278040	27.987188
288.990039	10140.594731	27.992205
288.844670	10154.671238	27.997223
289.351469	10184.185698	28.002240
289.697189	10171.902155	28.007258
289.886105	10219.306355	28.012276
290.061929	10212.934302	28.017293
290.772834	10230.107990	28.022311
291.302870	10261.232548	28.027328
291.414571	10271.045387	28.032346
291.622692	10269.725142	28.037364
291.589943	10314.370099	28.042381
292.319535	10299.562089	28.047399
292.820932	10329.921711	28.052416
292.977159	10344.658981	28.057434
293.498508	10341.111288	28.062452
292.990505	10374.607379	28.067469
293.204798	10388.476469	28.072487
293.899988	10379.184962	28.077504
293.835882	10422.263675	28.082522
294.420384	10427.321579	28.087540
295.082733	10443.259849	28.092557
295.267863	10451.018142	28.097575
295.635682	10465.393643	28.102592
295.751772	10477.151691	28.107610
296.254300	10469.011085	28.112628
296.168125	10487.862043	28.117645
296.497828	10506.007329	28.122663
296.856517	10506.002092	28.127680
296.910029	10537.733986	28.132698
297.082495	10532.784782	28.137716
297.340434	10557.832276	28.142733
297.457415	10574.376617	28.147751
297.985923	10599.272454	28.152768
298.090723	10623.231686	28.157786
298.627132	10609.165591	28.162804
298.665755	10672.047802	28.167821
298.893042	10682.194660	28.172839
299.744520	10683.995694	28.177856
299.552037	10706.864864	28.182874
300.594595	10714.856121	28.187892
300.544831	10739.882134	28.192909
301.043372	10737.810427	28.197927
301.265929	10768.626970	28.202944
301.729708	10784.874273	28.207962
302.207259	10780.255295	28.212980
302.370505	10812.598291	28.217997
302.212150	10807.066235	28.223015
303.174101	10830.473261	28.228032
303.068918	10836.399885	28.233050
303.577079	10852.895958	28.238068
303.585525	10869.480352	28.243085
304.009234	10891.235198	28.248103
304.541804	10894.067676	28.253120
304.551730	10909.635088	28.258138
305.091711	10917.192654	28.263156
305.016138	10942.057848	28.268173
305.493759	10960.666077	28.273191
305.824335	10959.122032	28.278208
305.772526	10976.201721	28.283226
306.352838	11015.913011	28.288244
306.776720	11016.562005	28.293261
306.791934	11060.930018	28.298279
306.969949	11043.911165	28.303296
307.417226	11068.014451	28.308314
307.497239	11102.549351	28.313332
307.934791	11111.940523	28.318349
308.383727	11126.171908	28.323367
308.824573	11152.665295	28.328384
309.031295	11167.004185	28.333402
308.805877	11186.992605	28.338420
309.918766	11201.425960	28.343437
310.231985	11205.337814	28.348455
310.604651	11213.663950	28.353472
310.607003	11237.028196	28.358490
311.242730	11250.483847	28.363508
311.317457	11261.128404	28.368525
311.631963	11287.637049	28.373543
312.126435	11291.795491	28.378560
312.110814	11328.894489	28.383578
312.393723	11303.886991	28.388596
312.886459	11337.675102	28.393613
312.999099	11342.415416	28.398631
313.412570	11358.871261	28.403648
313.691283	11370.901975	28.408666
314.036068	11383.448287	28.413684
314.153153	11398.634149	28.418701
314.165250	11426.867578	28.423719
314.899537	11428.452466	28.428736
314.960074	11467.964071	28.433754
315.428777	11469.463401	28.438772
315.821374	11495.472015	28.443789
315.703053	11520.062040	28.448807
316.548595	11521.209331	28.453824
316.516928	11547.033018	28.458842
316.906703	11555.233843	28.463860
317.510502	11590.117276	28.468877
317.584344	11604.563154	28.473895
317.882974	11599.930342	28.478912
318.119684	11632.667921	28.483930
318.104914	11642.708014	28.488948
318.624300	11655.787091	28.493965
318.850442	11683.677585	28.498983
319.197789	11710.769259	28.504000
319.748089	11733.465329	28.509018
319.939646	11751.176084	28.514036
320.322595	11796.732345	28.519053
320.686633	11802.224496	28.524071
321.193095	11827.538292	28.529088
321.507376	11860.562290	28.534106
321.820493	11858.536519	28.539124
321.909731	11865.611937	28.544141
322.215540	11906.566413	28.549159
322.399073	11922.942253	28.554176
323.045285	11948.828198	28.559194
323.496478	11953.587157	28.564212
323.872351	11986.565016	28.569229
324.136433	11991.348298	28.574247
324.600784	12010.537635	28.579264
324.890730	12039.948638	28.584282
325.050309	12066.853651	28.589300
325.420546	12072.790384	28.594317
325.935195	12082.047100	28.599335
326.135093	12090.816822	28.604352
326.440025	12123.299819	28.609370
326.760755	12114.665498	28.614388
327.314118	12147.497365	28.619405
327.119129	12144.652932	28.624423
327.799228	12175.684347	28.629440
328.495786	12174.418719	28.634458
328.482577	12215.229292	28.639476
329.152664	12187.805724	28.644493
329.135223	12238.709063	28.649511
329.519035	12243.732286	28.654528
329.702933	12230.116768	28.659546
329.791528	12284.810756	28.664564
330.414347	12277.471712	28.669581
330.657231	12270.212111	28.674599
330.898680	12327.718066	28.679616
331.314970	12304.402870	28.684634
331.368494	12361.919031	28.689652
331.867904	12363.621348	28.694669
331.774320	12372.802024	28.699687
332.220933	12410.320349	28.704704
332.500210	12415.424043	28.709722
332.723564	12443.897438	28.714740
333.099213	12466.214549	28.719757
333.469954	12486.150599	28.724775
333.883440	12499.004872	28.729792
334.511977	12529.670193	28.734810
334.552913	12554.716632	28.739828
334.928085	12564.264268	28.744845
335.535010	12562.634903	28.749863
336.367186	12614.914304	28.754880
336.256082	12640.818040	28.759898
336.553300	12631.027020	28.764916
337.208768	12628.270687	28.769933
336.880753	12695.634869	28.774951
337.730427	12690.732882	28.779968
337.644434	12696.999160	28.784986
338.021957	12698.088325	28.790004
338.417550	12762.624216	28.795021
338.598712	12760.536715	28.800039
339.279130	12786.270676	28.805056
339.453155	12824.455269	28.810074
339.779264	12816.310642	28.815092
340.435947	12862.061632	28.820109
340.339502	12892.751926	28.825127
340.690179	12870.706455	28.830144
340.810455	12927.737933	28.835162
340.946209	12937.996534	28.840180
341.904206	12958.025373	28.845197
341.929991	12994.986866	28.850215
342.515288	13002.857834	28.855232
342.799451	13047.234460	28.860250
342.948082	13042.895095	28.865268
343.781747	13081.950036	28.870285
343.987231	13119.119717	28.875303
344.077917	13110.525431	28.880320
344.770568	13159.500877	28.885338
345.170509	13146.294432	28.890356
345.683195	13185.651684	28.895373
345.899937	13176.312739	28.900391
346.090527	13220.099695	28.905408
346.572710	13220.987054	28.910426
346.541009	13251.768111	28.915444
347.545146	13235.091352	28.920461
347.232343	13300.238497	28.925479
347.473143	13296.183672	28.930496
348.154898	13281.914265	28.935514
348.145912	13354.378829	28.940532
348.383665	13342.670363	28.945549
348.597241	13376.184806	28.950567
349.221641	13376.408011	28.955584
349.524245	13411.280092	28.960602
349.568228	13418.217044	28.965620
349.924885	13475.524409	28.970637
350.260228	13464.477027	28.975655
350.875846	13512.388320	28.980672
351.650972	13517.471814	28.985690
351.494700	13530.782596	28.990708
352.283843	13572.326131	28.995725
352.034000	13603.437441	29.000743
352.924227	13596.162800	29.005760
353.161479	13642.916522	29.010778
353.374813	13654.717042	29.015796
353.841925	13678.480904	29.020813
354.168050	13666.686478	29.025831
354.288169	13714.159044	29.030848
355.080134	13731.814612	29.035866
355.203523	13758.377331	29.040884
355.414303	13765.460637	29.045901
355.693455	13817.477516	29.050919
356.109699	13817.673294	29.055936
356.806804	13877.189570	29.060954
356.530962	13877.711120	29.065972
357.325252	13888.182343	29.070989
357.570439	13951.159777	29.076007
358.234992	13936.030679	29.081024
358.388762	13990.219990	29.086042
359.062130	13992.427682	29.091060
359.495009	14018.992897	29.096077
360.114272	14016.032421	29.101095
360.166821	14050.505701	29.106112
360.749729	14062.125142	29.111130
360.611476	14097.220184	29.116148
361.701709	14076.700767	29.121165
361.847273	14128.599489	29.126183
362.031602	14121.763273	29.131200
362.946691	14144.441637	29.136218
362.567659	14153.983539	29.141236
363.302473	14162.559905	29.146253
363.338238	14193.005736	29.151271
363.833460	14219.656023	29.156288
364.376662	14211.668130	29.161306
364.376064	14257.928440	29.166324
364.735129	14258.870124	29.171341
364.983075	14271.044331	29.176359
365.441286	14300.996440	29.181376
365.980415	14338.472026	29.186394
366.248166	14347.650722	29.191412
366.736716	14357.420923	29.196429
366.986072	14403.064553	29.201447
367.332362	14404.959479	29.206464
367.180985	14421.876089	29.211482
367.497805	14427.911416	29.216500
367.810452	14494.287026	29.221517
367.655399	14487.307837	29.226535
368.121139	14513.233626	29.231552
368.620777	14581.099557	29.236570
368.836914	14596.059412	29.241588
369.376705	14603.092648	29.246605
370.191474	14624.398048	29.251623
370.383337	14688.415770	29.256640
370.854667	14687.472881	29.261658
371.416168	14720.552563	29.266676
371.644876	14764.351853	29.271693
372.731767	14749.035498	29.276711
372.940108	14758.631182	29.281728
373.494029	14808.120137	29.286746
373.483811	14816.169513	29.291764
373.880107	14813.529090	29.296781
374.038247	14870.953531	29.301799
374.065635	14853.943503	29.306816
374.922685	14918.038916	29.311834
374.825393	14936.477195	29.316852
375.530447	14935.005641	29.321869
376.285011	14977.611700	29.326887
376.080367	15002.785230	29.331904
376.891352	14988.146205	29.336922
377.444226	15047.844526	29.341940
377.752654	15042.080371	29.346957
378.008412	15087.882466	29.351975
378.329858	15095.546150	29.356992
378.761929	15124.664832	29.362010
379.316023	15123.595079	29.367028
379.370191	15178.960393	29.372045
379.757411	15183.962120	29.377063
380.331083	15179.018529	29.382080
380.749158	15240.403737	29.387098
380.817303	15262.315997	29.392116
381.618405	15254.102757	29.397133
381.962601	15308.339707	29.402151
382.523355	15293.518175	29.407168
383.213321	15280.594216	29.412186
383.046520	15347.862829	29.417204
383.248697	15365.595789	29.422221
383.861804	15372.137598	29.427239
383.748380	15392.909267	29.432256
384.315964	15424.227900	29.437274
384.543314	15461.529008	29.442292
385.148793	15448.941725	29.447309
385.538846	15519.660537	29.452327
385.680261	15523.874661	29.457344
386.539269	15527.420820	29.462362
386.516180	15601.627039	29.467380
386.574371	15620.209142	29.472397
387.206812	15618.353517	29.477415
388.273487	15627.728742	29.482432
388.119904	15671.278914	29.487450
388.189452	15657.922120	29.492468
388.679582	15713.312394	29.497485
389.240470	15722.888622	29.502503
389.450159	15737.850722	29.507520
389.752083	15805.830641	29.512538
390.112458	15803.668714	29.517556
390.694544	15813.059966	29.522573
391.181779	15869.167754	29.527591
391.294171	15881.757879	29.532608
391.725849	15886.985780	29.537626
392.244579	15888.012937	29.542644
392.561582	15956.488268	29.547661
392.985007	15942.302842	29.552679
393.258332	15998.375713	29.557696
394.028308	16044.808044	29.562714
394.134155	16057.495500	29.567732
394.505998	16053.939155	29.572749
394.914361	16108.014898	29.577767
395.223342	16107.615524	29.582784
395.785382	16158.464688	29.587802
396.443611	16181.456465	29.592820
396.821500	16188.394216	29.597837
397.126110	16224.095385	29.602855
397.767049	16240.139451	29.607872
398.224002	16264.816289	29.612890
398.406294	16289.385579	29.617908
398.065538	16311.997455	29.622925
399.168076	16334.707285	29.627943
399.050200	16372.030286	29.632960
399.973113	16369.755029	29.637978
399.933704	16426.942307	29.642996
400.652090	16423.899369	29.648013
400.961950	16481.130983	29.653031
401.066792	16487.983264	29.658048
402.098423	16519.931957	29.663066
401.961344	16548.281103	29.668084
402.756447	16561.635999	29.673101
403.067649	16616.842425	29.678119
403.627987	16605.244424	29.683136
404.000656	16665.559362	29.688154
404.224316	16663.076437	29.693172
404.595311	16714.879106	29.698189
405.406780	16699.777932	29.703207
405.238689	16777.565563	29.708224
405.741047	16764.189135	29.713242
406.034061	16821.177290	29.718260
406.668979	16837.818138	29.723277
406.802760	16869.597673	29.728295
407.682824	16854.966851	29.733312
408.030840	16933.006843	29.738330
408.230467	16946.070984	29.743348
408.722212	16954.932033	29.748365
409.116017	17002.895321	29.753383
409.312701	17016.737847	29.758400
410.342466	17008.636947	29.763418
410.768113	17059.940594	29.768436
410.350684	17080.785709	29.773453
411.254644	17081.561440	29.778471
411.301734	17136.632699	29.783488
411.625848	17134.242343	29.788506
412.305521	17182.586969	29.793524
412.310055	17212.491364	29.798541
413.394002	17204.612414	29.803559
413.463628	17274.662773	29.808576
413.805723	17285.562014	29.813594
414.566943	17276.683971	29.818612
414.798320	17323.938981	29.823629
415.475709	17369.630305	29.828647
415.748814	17358.575690	29.833664
416.085996	17368.332779	29.838682
416.365965	17432.845186	29.843700
416.512438	17456.465640	29.848717
417.297648	17449.334693	29.853735
417.456267	17487.713080	29.858752
417.777869	17527.223165	29.863770
418.971664	17515.087771	29.868788
418.944576	17573.255982	29.873805
419.279534	17623.238076	29.878823
419.691715	17643.413224	29.883840
420.057353	17661.651878	29.888858
420.484370	17679.001712	29.893876
421.021348	17685.717371	29.898893
421.404294	17764.934647	29.903911
421.981399	17771.037500	29.908928
422.515225	17767.802673	29.913946
423.032547	17837.473641	29.918964
423.104704	17843.523523	29.923981
423.920872	17833.760491	29.928999
423.920140	17915.861322	29.934016
423.918498	17926.878184	29.939034
424.624296	17944.340580	29.944052
424.921915	18004.252260	29.949069
425.441435	18019.025685	29.954087
425.870248	18039.824650	29.959104
425.804017	18092.208660	29.964122
427.149504	18105.812435	29.969140
427.414312	18140.527487	29.974157
427.829599	18174.460803	29.979175
428.340721	18211.802781	29.984192
428.650558	18234.793699	29.989210
429.206375	18260.919338	29.994228
429.699515	18288.670295	29.999245
430.295710	18306.437169	30.004263
430.601809	18351.065797	30.009280
430.827453	18351.786897	30.014298
431.789522	18403.529793	30.019316
432.062042	18400.783702	30.024333
432.251433	18462.578309	30.029351
432.509639	18458.184932	30.034368
433.451046	18462.645818	30.039386
433.691256	18511.314812	30.044404
433.495142	18523.435888	30.049421
434.475050	18524.845069	30.054439
435.184438	18557.837903	30.059456
435.073293	18589.834793	30.064474
435.498165	18576.120547	30.069492
435.763023	18640.267958	30.074509
436.416279	18630.578618	30.079527
436.518455	18695.560823	30.084544
436.842938	18680.424313	30.089562
437.323802	18748.929813	30.094580
437.398938	18784.872182	30.099597
437.786486	18794.558372	30.104615
438.871391	18807.662962	30.109632
439.027050	18872.681873	30.114650
439.597533	18941.757013	30.119668
440.048488	18954.875331	30.124685
440.407561	18964.727976	30.129703
441.075217	18987.303552	30.134720
441.368989	19061.707191	30.139738
441.665306	19068.382472	30.144756
441.728700	19091.411957	30.149773
443.093490	19096.907165	30.154791
443.317717	19150.170521	30.159808
443.618051	19224.467591	30.164826
444.114019	19232.052491	30.169844
444.162100	19253.718881	30.174861
444.440525	19289.970979	30.179879
445.559572	19310.394353	30.184896
446.238389	19370.149188	30.189914
446.412151	19402.842927	30.194932
446.950761	19419.538729	30.199949
447.462992	19463.921563	30.204967
447.933905	19454.213526	30.209984
448.496542	19531.556989	30.215002
448.986720	19528.288213	30.220020
449.148097	19576.068733	30.225037
449.759274	19587.246627	30.230055
450.260524	19633.544768	30.235072
450.496843	19652.539083	30.240090
451.009184	19658.697111	30.245108
450.982752	19722.019362	30.250125
451.927267	19740.404866	30.255143
452.398717	19754.475765	30.260160
452.652241	19810.059272	30.265178
453.043751	19835.926720	30.270196
453.693650	19865.854472	30.275213
454.033780	19889.724564	30.280231
454.525361	19931.044115	30.285248
454.566450	19978.052853	30.290266
455.313679	19998.111938	30.295284
455.695489	20023.945415	30.300301
456.082729	20080.866551	30.305319
456.588451	20073.746874	30.310336
456.971718	20123.178487	30.315354
457.531837	20142.978177	30.320372
457.676967	20192.055003	30.325389
458.170208	20221.052807	30.330407
458.791681	20221.611718	30.335424
458.969151	20284.342691	30.340442
459.899692	20308.020927	30.345460
459.929735	20342.286912	30.350477
460.603609	20359.285827	30.355495
461.210223	20405.716338	30.360512
461.322787	20423.061071	30.365530
461.937426	20464.709708	30.370548
462.314791	20512.052735	30.375565
462.999298	20537.531327	30.380583
463.392696	20555.672497	30.385600
463.792985	20612.517498	30.390618
464.516018	20617.720198	30.395636
464.614613	20669.748773	30.400653
465.625988	20685.270496	30.405671
466.311712	20715.075262	30.410688
466.787954	20762.511181	30.415706
467.317790	20769.290563	30.420724
467.441640	20819.915449	30.425741
467.991018	20840.090224	30.430759
468.286868	20858.626074	30.435776
468.660423	20890.886717	30.440794
469.373371	20912.640454	30.445812
469.424121	20968.366693	30.450829
469.998722	20993.339062	30.455847
470.709729	21010.673371	30.460864
470.674805	21079.494140	30.465882
471.662293	21091.965720	30.470900
472.154629	21131.021477	30.475917
472.562465	21162.963002	30.480935
472.864748	21190.197102	30.485952
473.073162	21212.224182	30.490970
474.002987	21261.719585	30.495988
474.329803	21302.162969	30.501005
474.480887	21325.052620	30.506023
475.063215	21356.782067	30.511040
475.456058	21393.024361	30.516058
476.097654	21443.083658	30.521076
476.540539	21487.058024	30.526093
477.345118	21518.714592	30.531111
477.615690	21535.038762	30.536128
478.038277	21580.289276	30.541146
478.593428	21623.732666	30.546164
479.066617	21653.753034	30.551181
479.724845	21682.326408	30.556199
480.211306	21715.589445	30.561216
480.931096	21730.761748	30.566234
481.032477	21774.908668	30.571252
482.054298	21771.117661	30.576269
482.306247	21847.619933	30.581287
482.897238	21852.764549	30.586304
483.265494	21880.836347	30.591322
483.958575	21913.157267	30.596340
483.848409	21920.273013	30.601357
484.022626	21959.737091	30.606375
484.600008	21971.997103	30.611392
485.137946	22012.076729	30.616410
485.667991	22054.289635	30.621428
486.136642	22072.795850	30.626445
486.365497	22109.350230	30.631463
486.977510	22140.422859	30.636480
487.678384	22184.314762	30.641498
488.077142	22216.572935	30.646516
488.438319	22245.564027	30.651533
488.561615	22297.066381	30.656551
489.408662	22317.333469	30.661568
489.660416	22346.235068	30.666586
490.433635	22396.044889	30.671604
490.552109	22469.603070	30.676621
491.033391	22471.456750	30.681639
491.864939	22505.400510	30.686656
492.181366	22572.720712	30.691674
492.662105	22602.439257	30.696692
492.754759	22649.997113	30.701709
493.644760	22675.267671	30.706727
494.150322	22743.573675	30.711744
494.719226	22766.291749	30.716762
495.255861	22814.559092	30.721780
495.955132	22849.892722	30.726797
496.357182	22879.660555	30.731815
496.814800	22924.775460	30.736832
497.325835	22940.569746	30.741850
497.994463	23018.664496	30.746868
498.332109	23009.620175	30.751885
498.805968	23095.269547	30.756903
499.722687	23091.183880	30.761920
500.063403	23168.432156	30.766938
500.542647	23182.031155	30.771956
501.204240	23215.511261	30.776973
501.568256	23257.463207	30.781991
502.071807	23300.603610	30.787008
502.267828	23334.111663	30.792026
503.130923	23358.468452	30.797044
504.014376	23396.230565	30.802061
504.501158	23432.839861	30.807079
504.682053	23456.091741	30.812096
505.383681	23491.620978	30.817114
505.805056	23522.881080	30.822132
506.221966	23565.824135	30.827149
506.693400	23612.183263	30.832167
507.456345	23621.189639	30.837184
507.711089	23668.970479	30.842202
508.042513	23700.116087	30.847220
508.679090	23733.461077	30.852237
509.008580	23774.916591	30.857255
509.673953	23786.760736	30.862272
510.341261	23828.861219	30.867290
510.741065	23870.708271	30.872308
511.073612	23870.668681	30.877325
511.573376	23920.834846	30.882343
512.061498	23929.651246	30.887360
512.545372	23990.380215	30.892378
512.922065	24000.888172	30.897396
513.894172	24046.998685	30.902413
514.108923	24079.197030	30.907431
514.677580	24098.740435	30.912448
515.056227	24166.520647	30.917466
515.586886	24173.588097	30.922484
515.825587	24223.581772	30.927501
516.584823	24248.123468	30.932519
516.621714	24302.775511	30.937536
517.490399	24336.017846	30.942554
517.694305	24362.536229	30.947572
518.490780	24428.997815	30.952589
518.858075	24441.481480	30.957607
519.347301	24510.121440	30.962624
520.060712	24510.718281	30.967642
520.143666	24608.656599	30.972660
520.757143	24626.704791	30.977677
521.643725	24677.122077	30.982695
522.226235	24702.770187	30.987712
522.724068	24758.390910	30.992730
522.765373	24783.006834	30.997748
524.159355	24824.255353	31.002765
523.951747	24896.609323	31.007783
524.305395	24895.379312	31.012800
525.082647	24966.451099	31.017818
525.866804	25000.026524	31.022836
526.840586	25056.044309	31.027853
527.307337	25088.726807	31.032871
528.071849	25099.235949	31.037888
528.708445	25170.812345	31.042906
528.855719	25195.894895	31.047924
529.994741	25210.544552	31.052941
529.994592	25258.641743	31.057959
530.477881	25266.285176	31.062976
530.936030	25326.772062	31.067994
531.797533	25331.714842	31.073012
532.169810	25396.940425	31.078029
532.694658	25421.526000	31.083047
533.006875	25464.668889	31.088064
533.853611	25482.173606	31.093082
533.808094	25549.842151	31.098100
534.549687	25552.113998	31.103117
534.862721	25624.756993	31.108135
535.533056	25647.727730	31.113152
536.096907	25689.452606	31.118170
536.376699	25741.173582	31.123188
537.081989	25776.345782	31.128205
537.432229	25804.919746	31.133223
538.168705	25872.751048	31.138240
538.801300	25893.925786	31.143258
538.779769	25925.251708	31.148276
539.609015	25982.837402	31.153293
540.293874	26008.427202	31.158311
540.797706	26029.259475	31.163328
541.426264	26090.991973	31.168346
542.139907	26112.321885	31.173364
541.970070	26172.895456	31.178381
542.561873	26183.378477	31.183399
543.142146	26250.672224	31.188416
543.847018	26282.848944	31.193434
543.902375	26343.966301	31.198452
544.709033	26386.656367	31.203469
544.969210	26430.018908	31.208487
545.848193	26443.043412	31.213504
546.316664	26527.320889	31.218522
546.987308	26570.817740	31.223540
547.534709	26593.290274	31.228557
548.365818	26666.584174	31.233575
548.597027	26683.777821	31.238592
549.292724	26740.967625	31.243610
549.797728	26779.748140	31.248628
550.618010	26809.231408	31.253645
550.752464	26873.449178	31.258663
551.725296	26890.636791	31.263680
551.990570	26984.083547	31.268698
552.396383	27008.431339	31.273716
552.941316	27045.745551	31.278733
553.789814	27081.684831	31.283751
554.591028	27158.539537	31.288768
555.139035	27177.685871	31.293786
555.649683	27230.082333	31.298804
556.326689	27255.411465	31.303821
556.789258	27313.043012	31.308839
557.266473	27341.110257	31.313856
557.595554	27403.060945	31.318874
558.278614	27433.986089	31.323892
558.782286	27489.595680	31.328909
559.234401	27537.263686	31.333927
559.807669	27579.641156	31.338944
560.809629	27601.979681	31.343962
560.981645	27687.994056	31.348980
561.875456	27699.621973	31.353997
562.583092	27774.492632	31.359015
562.984847	27786.600783	31.364032
563.811832	27847.862514	31.369050
564.081436	27856.107693	31.374068
564.514824	27917.424498	31.379085
565.543460	27939.975905	31.384103
566.034588	28017.097606	31.389120
566.672787	28023.850273	31.394138
566.967343	28080.364999	31.399156
567.834488	28104.179291	31.404173
567.967724	28177.657409	31.409191
568.262601	28182.050820	31.414208
569.137169	28222.913423	31.419226
569.296246	28287.979857	31.424244
570.151512	28285.554094	31.429261
570.347042	28355.640003	31.434279
570.586413	28403.565846	31.439296
571.628994	28443.181047	31.444314
572.222236	28486.121838	31.449332
572.605400	28528.905536	31.454349
573.349416	28590.556756	31.459367
573.980543	28610.539321	31.464384
574.400769	28674.640744	31.469402
575.019284	28697.754905	31.474420
575.501164	28764.357068	31.479437
576.073830	28790.548280	31.484455
576.727515	28856.299325	31.489472
577.577126	28889.569149	31.494490
578.031566	28920.295617	31.499508
578.297596	28989.334592	31.504525
579.241742	29009.729509	31.509543
579.623601	29092.642753	31.514560
580.323929	29111.114747	31.519578
580.566916	29168.350600	31.524596
581.415756	29223.733120	31.529613
582.043824	29249.640484	31.534631
582.508480	29315.330525	31.539648
583.589216	29361.231051	31.544666
583.885300	29411.809279	31.549684
584.373080	29444.933014	31.554701
585.126984	29506.471112	31.559719
585.467618	29528.905828	31.564736
585.941357	29590.692150	31.569754
586.527980	29621.633700	31.574772
587.053124	29700.229852	31.579789
587.455523	29750.833175	31.584807
588.288965	29792.725890	31.589824
588.844117	29867.679371	31.594842
589.657716	29885.543256	31.599860
590.064639	29979.724628	31.604877
590.894808	30004.467945	31.609895
591.231278	30075.049421	31.614912
591.954544	30104.367434	31.619930
592.513200	30174.037749	31.624948
593.570737	30206.029043	31.629965
593.949987	30254.845801	31.634983
594.266842	30307.197993	31.640000
595.376355	30355.156490	31.645018
595.928483	30402.765787	31.650036
596.358466	30425.149689	31.655053
597.447508	30506.611663	31.660071
597.668897	30514.229197	31.665088
598.207186	30603.731602	31.670106
598.906991	30615.773924	31.675124
599.380341	30679.463469	31.680141
600.270251	30709.712647	31.685159
600.543014	30752.645862	31.690176
601.360215	30778.694178	31.695194
601.429755	30840.525974	31.700212
601.772770	30869.261350	31.705229
602.810107	30897.541061	31.710247
603.167837	30966.709351	31.715264
603.906341	31019.781522	31.720282
604.565984	31054.597427	31.725300
605.210999	31098.052235	31.730317
605.864514	31134.784131	31.735335
606.174558	31188.895908	31.740352
606.632161	31235.900165	31.745370
607.109879	31286.868200	31.750388
608.003360	31344.999420	31.755405
608.587721	31384.447355	31.760423
609.173959	31444.424534	31.765440
609.898396	31484.425656	31.770458
610.346916	31536.604791	31.775476
610.837982	31574.750469	31.780493
611.561397	31649.524579	31.785511
611.902060	31675.717992	31.790528
612.936473	31756.523501	31.795546
613.600441	31808.229468	31.800564
614.259501	31851.387740	31.805581
615.082478	31894.650837	31.810599
615.738277	31964.902771	31.815616
616.224187	32001.053361	31.820634
616.725984	32041.427009	31.825652
617.319050	32107.109412	31.830669
618.139103	32157.294328	31.835687
618.226503	32209.307729	31.840704
619.243631	32252.424220	31.845722
619.810902	32308.007068	31.850740
620.143206	32370.270890	31.855757
620.991424	32424.553219	31.860775
621.591847	32477.891680	31.865792
622.469145	32523.800425	31.870810
623.033615	32583.651264	31.875828
623.630067	32622.110434	31.880845
624.221651	32659.337917	31.885863
624.943182	32721.099762	31.890880
625.452171	32786.303354	31.895898
626.285982	32813.264876	31.900916
626.724888	32883.794856	31.905933
627.619962	32940.960559	31.910951
627.892601	32980.488770	31.915968
628.737188	33042.813838	31.920986
629.274471	33073.783976	31.926004
629.875139	33169.869477	31.931021
630.601192	33174.394191	31.936039
631.033385	33253.889113	31.941056
631.938645	33290.748104	31.946074
632.299561	33325.706251	31.951092
632.898208	33399.043882	31.956109
633.721028	33453.806521	31.961127
634.197505	33509.280207	31.966144
634.583637	33530.646059	31.971162
635.061995	33579.584606	31.976180
635.752018	33639.974125	31.981197
636.390235	33692.750933	31.986215
636.829767	33747.627598	31.991232
637.907661	33780.100268	31.996250
638.274683	33868.575873	32.001268
638.503996	33907.356592	32.006285
639.584590	33943.140902	32.011303
640.049194	34040.014471	32.016320
640.655375	34062.627491	32.021338
641.636370	34115.250182	32.026356
641.930037	34194.324016	32.031373
642.699937	34221.097836	32.036391
643.182577	34295.583395	32.041408
643.775266	34362.039350	32.046426
644.416749	34409.931348	32.051444
645.666679	34442.664821	32.056461
646.347044	34530.083637	32.061479
646.594619	34605.194412	32.066496
647.103477	34620.296678	32.071514
647.906398	34700.433101	32.076532
648.767499	34758.865282	32.081549
649.240727	34818.122389	32.086567
649.882704	34864.079853	32.091584
650.533142	34946.436042	32.096602
651.147635	34987.292357	32.101620
651.545338	35051.496378	32.106637
652.364920	35097.821879	32.111655
652.916878	35176.845071	32.116672
653.926701	35204.394123	32.121690
655.153631	35291.805582	32.126708
655.916496	35317.059492	32.131725
657.109038	35380.318486	32.136743
657.539170	35416.335678	32.141760
657.965871	35480.929265	32.146778
658.967258	35504.094556	32.151796
659.060525	35559.582522	32.156813
659.477259	35624.521914	32.161831
660.381254	35666.073150	32.166848
660.924902	35723.291815	32.171866
661.422062	35751.285992	32.176884
662.148132	35845.880435	32.181901
662.997312	35867.155077	32.186919
663.236952	35940.811762	32.191936
663.806077	36017.282333	32.196954
664.640091	36050.479336	32.201972
665.203698	36116.861803	32.206989
665.912782	36175.704677	32.212007
666.677331	36237.882668	32.217024
667.508403	36281.717203	32.222042
668.098666	36354.493796	32.227060
668.397468	36401.285788	32.232077
669.567375	36442.419836	32.237095
670.160547	36519.418584	32.242112
670.666964	36562.974483	32.247130
671.370300	36617.039808	32.252148
671.504551	36652.286985	32.257165
672.274138	36715.498580	32.262183
672.787450	36776.925581	32.267200
673.424963	36823.680587	32.272218
674.064996	36898.619375	32.277236
674.592903	36941.635232	32.282253
675.468725	37026.040548	32.287271
676.225248	37052.477377	32.292288
676.534606	37142.374802	32.297306
677.524666	37196.464137	32.302324
677.867033	37268.350834	32.307341
678.603128	37329.452718	32.312359
678.975485	37402.667437	32.317376
680.252072	37443.529981	32.322394
680.692395	37540.530214	32.327412
681.681256	37575.566001	32.332429
682.244337	37665.022208	32.337447
683.229902	37706.302238	32.342464
683.511534	37809.933799	32.347482
684.454699	37836.707931	32.352500
685.178258	37931.633028	32.357517
686.060733	37959.310982	32.362535
686.678994	38062.417500	32.367552
687.303970	38092.589963	32.372570
688.307459	38157.231316	32.377588
688.528304	38229.915614	32.382605
689.646483	38284.486288	32.387623
690.336990	38352.002065	32.392640
690.893460	38394.925647	32.397658
691.604172	38482.300370	32.402676
692.461526	38513.645920	32.407693
692.611242	38610.424233	32.412711
693.562019	38665.153662	32.417728
693.915926	38711.014619	32.422746
695.636335	38775.041222	32.427764
695.725436	38831.973904	32.432781
696.928461	38920.552819	32.437799
697.768739	38948.289578	32.442816
698.249414	39017.485973	32.447834
698.676418	39078.157774	32.452852
699.300274	39132.273801	32.457869
700.358714	39196.270224	32.462887
700.968528	39239.674683	32.467904
701.217995	39340.421063	32.472922
702.181176	39354.302656	32.477940
702.766541	39456.918349	32.482957
703.756142	39477.560286	32.487975
704.116042	39578.391412	32.492992
704.642356	39621.559432	32.498010
705.780745	39661.730353	32.503028
706.059708	39783.041048	32.508045
706.517863	39816.251736	32.513063
707.654727	39856.298793	32.518080
708.108172	39949.583131	32.523098
709.128707	39991.118643	32.528116
709.494172	40047.848988	32.533133
710.320489	40111.638262	32.538151
711.419930	40171.511523	32.543168
711.799770	40220.012099	32.548186
712.035457	40286.286590	32.553204
712.721180	40348.938563	32.558221
713.191160	40403.660282	32.563239
713.807319	40497.864695	32.568256
714.566077	40555.735708	32.573274
715.494548	40639.597209	32.578292
716.222512	40694.901668	32.583309
716.624140	40796.583320	32.588327
717.902043	40837.269394	32.593344
718.217590	40945.055709	32.598362
718.970247	40969.127600	32.603380
719.903750	41089.731538	32.608397
720.615697	41129.953333	32.613415
721.411082	41182.865872	32.618432
721.970268	41295.753325	32.623450
723.634109	41319.281676	32.628468
723.749537	41397.919394	32.633485
724.362925	41511.181267	32.638503
725.050671	41543.791060	32.643520
725.923254	41597.963648	32.648538
726.732969	41674.766875	32.653556
727.517766	41788.101065	32.658573
728.053706	41821.763768	32.663591
729.029737	41919.900686	32.668608
729.280603	42000.166014	32.673626
731.060051	42018.573671	32.678644
731.696077	42120.986005	32.683661
732.152454	42164.423929	32.688679
733.273919	42225.696586	32.693696
733.588969	42288.753753	32.698714
734.504920	42331.481805	32.703732
735.217204	42436.571191	32.708749
735.823130	42466.432747	32.713767
736.989218	42572.182479	32.718784
736.883262	42636.623231	32.723802
737.977208	42681.790385	32.728820
738.519692	42763.473240	32.733837
739.038357	42849.238672	32.738855
740.092858	42922.188764	32.743872
740.691751	42972.592657	32.748890
741.471881	43054.973999	32.753908
741.925724	43109.694321	32.758925
742.835164	43215.324843	32.763943
743.765976	43260.263994	32.768960
744.240378	43355.262133	32.773978
745.154399	43402.264090	32.778996
746.018834	43477.618839	32.784013
746.329767	43562.976131	32.789031
747.455106	43617.345127	32.794048
748.072886	43687.207322	32.799066
749.061444	43725.978021	32.804084
749.804187	43803.523775	32.809101
750.434791	43878.602062	32.814119
751.322743	43930.694507	32.819136
751.543818	44003.232985	32.824154
752.328197	44079.284460	32.829172
753.330755	44147.380712	32.834189
753.754114	44196.642671	32.839207
754.316589	44272.774484	32.844224
755.509436	44355.493796	32.849242
755.994322	44408.822163	32.854260
756.947067	44506.876587	32.859277
757.602982	44555.976366	32.864295
758.664824	44626.667550	32.869312
759.192643	44722.096861	32.874330
760.030809	44769.679284	32.879348
761.015436	44841.642308	32.884365
761.253613	44932.629922	32.889383
762.571230	44991.417458	32.894400
762.943924	45062.081320	32.899418
763.743780	45150.507442	32.904436
764.743476	45195.989575	32.909453
765.421643	45306.259677	32.914471
766.439715	45346.086127	32.919488
766.883198	45433.892167	32.924506
767.840391	45505.635174	32.929524
768.577206	45555.396854	32.934541
769.166460	45653.868943	32.939559
770.216624	45727.629707	32.944576
771.215962	45792.205936	32.949594
771.890762	45884.236333	32.954612
772.654692	45949.601453	32.959629
773.092576	46015.138601	32.964647
774.107922	46086.284798	32.969664
774.867120	46164.999449	32.974682
775.567821	46233.827068	32.979700
776.593410	46305.496230	32.984717
777.112297	46392.418044	32.989735
778.152565	46461.571090	32.994752
778.564847	46527.751520	32.999770
779.299781	46610.018124	33.004788
780.157967	46693.981767	33.009805
781.307268	46771.630636	33.014823
782.019437	46830.530233	33.019840
782.887891	46917.440024	33.024858
783.401574	46997.509963	33.029876
784.691831	47048.844164	33.034893
784.938711	47143.971771	33.039911
785.701480	47195.210532	33.044928
786.470805	47296.874999	33.049946
787.112031	47367.240417	33.054964
788.330753	47412.472622	33.059981
788.685405	47540.161036	33.064999
789.735543	47568.645019	33.070016
790.192648	47654.425012	33.075034
790.827433	47718.567884	33.080052
791.581770	47786.332953	33.085069
792.344679	47853.434344	33.090087
793.270181	47945.170631	33.095104
794.155286	48005.744110	33.100122
794.913791	48078.311774	33.105140
795.417666	48172.091485	33.110157
796.580541	48210.913860	33.115175
797.630066	48308.172799	33.120192
797.967079	48381.338875	33.125210
798.708365	48465.250714	33.130228
799.910054	48515.524223	33.135245
800.067610	48641.346220	33.140263
801.081080	48688.576959	33.145280
801.883127	48776.538281	33.150298
802.657961	48849.074965	33.155316
803.276959	48944.629507	33.160333
804.103431	49007.923023	33.165351
804.746645	49117.304438	33.170368
806.074595	49179.616320	33.175386
806.518349	49293.116754	33.180404
807.682400	49348.794324	33.185421
808.428351	49440.513319	33.190439
809.433770	49514.830387	33.195456
810.215357	49610.469926	33.200474
811.004120	49687.854575	33.205492
812.199362	49761.628128	33.210509
812.504016	49843.236782	33.215527
813.581365	49930.579410	33.220544
814.361117	50005.634973	33.225562
815.159027	50092.609505	33.230580
816.185113	50171.422648	33.235597
816.823863	50249.480507	33.240615
817.362114	50329.514305	33.245632
818.143071	50427.420878	33.250650
819.427586	50507.715368	33.255668
820.062639	50574.153200	33.260685
820.385938	50671.897289	33.265703
821.963586	50752.840466	33.270720
822.867412	50822.325811	33.275738
823.178296	50927.804614	33.280756
824.036341	50965.643354	33.285773
824.924493	51089.703354	33.290791
825.907612	51147.501283	33.295808
826.845147	51260.825220	33.300826
827.665341	51322.786803	33.305844
828.672448	51400.948860	33.310861
829.452297	51503.112306	33.315879
830.574276	51547.704642	33.320896
831.469464	51645.161062	33.325914
831.969503	51727.750779	33.330932
833.338264	51782.885847	33.335949
833.972945	51889.426473	33.340967
834.338161	51939.741842	33.345984
835.370401	52000.851507	33.351002
835.918315	52091.018797	33.356020
836.812852	52124.218215	33.361037
837.355210	52231.438300	33.366055
838.293175	52281.407843	33.371072
839.169724	52364.066801	33.376090
839.839372	52441.087860	33.381108
840.675950	52501.769609	33.386125
841.654100	52611.646181	33.391143
841.936314	52668.235074	33.396160
843.057842	52775.293636	33.401178
843.638784	52831.491495	33.406196
844.379954	52932.031267	33.411213
845.336163	53023.444841	33.416231
846.203765	53103.719506	33.421248
846.855738	53200.187889	33.426266
847.660063	53298.721866	33.431284
848.559887	53379.491292	33.436301
849.471340	53473.458084	33.441319
849.978734	53556.111833	33.446336
851.217707	53654.161966	33.451354
852.054991	53745.932680	33.456372
853.182251	53841.984827	33.461389
853.881885	53921.753313	33.466407
854.831862	54037.513569	33.471424
855.940753	54115.841670	33.476442
856.513224	54207.151873	33.481460
857.382872	54289.378882	33.486477
858.374289	54381.828978	33.491495
859.248712	54481.488188	33.496512
860.149248	54562.543694	33.501530
860.711658	54662.966880	33.506548
861.625568	54768.141782	33.511565
862.596328	54853.738851	33.516583
863.311622	54939.443265	33.521600
864.367595	55042.608635	33.526618
865.393300	55133.725111	33.531636
866.145740	55230.955321	33.536653
867.260798	55302.561243	33.541671
867.843460	55427.813920	33.546688
868.918025	55505.335962	33.551706
869.576498	55589.685731	33.556724
870.428848	55700.731089	33.561741
870.951657	55778.657752	33.566759
871.796163	55897.906177	33.571776
873.113910	55982.935664	33.576794
873.848415	56083.999011	33.581812
874.731765	56191.260854	33.586829
875.608288	56279.294405	33.591847
876.867820	56358.918187	33.596864
877.808679	56482.612229	33.601882
878.593325	56533.634354	33.606900
879.396821	56659.636860	33.611917
880.059732	56715.164484	33.616935
880.683952	56839.182796	33.621952
881.966396	56891.566153	33.626970
882.763622	57016.012693	33.631988
883.454701	57063.402011	33.637005
884.645237	57184.826090	33.642023
885.625385	57239.225207	33.647040
886.080421	57351.530745	33.652058
887.168098	57408.198763	33.657076
887.985869	57516.978273	33.662093
888.578314	57594.292308	33.667111
889.490812	57695.153110	33.672128
890.470954	57783.518329	33.677146
891.296712	57883.929910	33.682164
892.017486	57980.084315	33.687181
892.951055	58076.795700	33.692199
893.660291	58176.889630	33.697216
894.908396	58275.341978	33.702234
895.402604	58385.677648	33.707252
896.323566	58469.481138	33.712269
897.146482	58576.725474	33.717287
898.430923	58679.350895	33.722304
899.506939	58777.274514	33.727322
900.320726	58892.222120	33.732340
900.833487	58981.879754	33.737357
902.083654	59079.171101	33.742375
902.858270	59179.528402	33.747392
903.765125	59283.559023	33.752410
904.750413	59385.263571	33.757428
905.934505	59479.789262	33.762445
906.896015	59586.726932	33.767463
907.622156	59704.484448	33.772480
908.785992	59784.128798	33.777498
909.761690	59874.534790	33.782516
910.489980	59988.448277	33.787533
911.534189	60090.346214	33.792551
912.283343	60192.389533	33.797568
913.450952	60284.879191	33.802586
914.359569	60387.595965	33.807604
915.170463	60479.960230	33.812621
916.157307	60596.709447	33.817639
916.786122	60690.644507	33.822656
918.212091	60773.954953	33.827674
918.673619	60881.563725	33.832692
919.763171	60984.529683	33.837709
920.886555	61077.554436	33.842727
921.737799	61178.513378	33.847744
922.723456	61270.635879	33.852762
923.446080	61389.560209	33.857780
924.820402	61472.329432	33.862797
926.019366	61554.482796	33.867815
926.505917	61663.683454	33.872832
927.575712	61761.551130	33.877850
928.273936	61852.140302	33.882868
929.186594	61941.508548	33.887885
930.280455	62048.571867	33.892903
930.974101	62130.091387	33.897920
931.824691	62201.324071	33.902938
932.502315	62311.448526	33.907956
933.504187	62400.100607	33.912973
934.193264	62504.600617	33.917991
934.664537	62601.244841	33.923008
935.598940	62692.267812	33.928026
936.490701	62793.655272	33.933044
937.181635	62911.400651	33.938061
938.444332	63018.638398	33.943079
939.189913	63136.840675	33.948096
940.386664	63231.812757	33.953114
941.360747	63345.404363	33.958132
942.093296	63442.687084	33.963149
943.189567	63555.527897	33.968167
943.581447	63675.716092	33.973184
944.995273	63780.366781	33.978202
946.035560	63896.063768	33.983220
946.792358	64015.226580	33.988237
947.845965	64124.332289	33.993255
948.576532	64237.011131	33.998272
949.768670	64355.146793	34.003290
950.530899	64473.518965	34.008308
951.542064	64581.001372	34.013325
952.717856	64698.049096	34.018343
953.571123	64817.258426	34.023360
955.020933	64923.062373	34.028378
955.665085	65048.344626	34.033396
956.460700	65156.890952	34.038413
957.699648	65273.287909	34.043431
958.868402	65384.441609	34.048448
959.952035	65499.399283	34.053466
960.648357	65623.998006	34.058484
961.445795	65726.133027	34.063501
962.603841	65841.232508	34.068519
963.234879	65953.150923	34.073536
964.613791	66075.897483	34.078554
965.749863	66184.253348	34.083572
966.517018	66303.956227	34.088589
967.333911	66411.827252	34.093607
968.240787	66529.529051	34.098624
969.362194	66642.889462	34.103642
970.473787	66761.267578	34.108660
971.631839	66882.042557	34.113677
972.566077	66975.606413	34.118695
973.289115	67107.948580	34.123712
974.341438	67211.955475	34.128730
975.426876	67328.711489	34.133748
976.447357	67448.305376	34.138765
977.272233	67550.970033	34.143783
978.336812	67660.514228	34.148800
979.493677	67770.252824	34.153818
980.394888	67887.430025	34.158836
981.453626	67992.915146	34.163853
982.725311	68097.109850	34.168871
983.252745	68207.658589	34.173888
984.323694	68307.015805	34.178906
985.647766	68411.450238	34.183924
986.464034	68501.966910	34.188941
987.103325	68597.262783	34.193959
988.067872	68711.086709	34.198976
989.239354	68807.455021	34.203994
990.415897	68913.444436	34.209012
990.559469	69026.459524	34.214029
991.580500	69128.147392	34.219047
992.408989	69240.302975	34.224064
993.447630	69357.277658	34.229082
994.276307	69475.954294	34.234100
995.107599	69614.733981	34.239117
996.148685	69724.956916	34.244135
997.137570	69840.261908	34.249152
998.456542	69972.377170	34.254170
999.286402	70088.081671	34.259188
1000.105312	70212.368224	34.264205
1001.567334	70329.508819	34.269223
1002.117333	70452.885679	34.274240
1003.271038	70589.352855	34.279258
1004.673564	70704.780356	34.284276
1005.347635	70834.514740	34.289293
1006.689802	70966.171799	34.294311
1007.437802	71096.186780	34.299328
1008.525364	71217.587488	34.304346
1009.887097	71346.179672	34.309364
1011.033595	71459.750562	34.314381
1011.992344	71580.807545	34.319399
1013.406714	71713.608050	34.324416
1014.290003	71826.256222	34.329434
1015.664071	71925.153963	34.334452
1016.236158	72056.504853	34.339469
1017.304617	72160.083800	34.344487
1018.174172	72284.331157	34.349504
1019.512091	72399.197573	34.354522
1020.484722	72516.599650	34.359540
1021.389073	72644.306313	34.364557
1022.424608	72752.183942	34.369575
1023.998251	72854.858419	34.374592
1024.838243	72973.996671	34.379610
1026.096700	73082.270307	34.384628
1026.890573	73207.142091	34.389645
1028.260845	73313.857417	34.394663
1028.963491	73438.764124	34.399680
1029.844054	73545.230012	34.404698
1031.015031	73655.321577	34.409716
1031.766931	73773.499197	34.414733
1033.198125	73884.864984	34.419751
1034.285208	74003.647827	34.424768
1035.021409	74111.706832	34.429786
1036.233383	74222.079366	34.434804
1037.094686	74343.617370	34.439821
1037.785018	74450.857696	34.444839
1038.979984	74574.701086	34.449856
1040.033427	74676.039571	34.454874
1040.935961	74780.195703	34.459892
1041.316832	74899.102525	34.464909
1042.657490	74999.101495	34.469927
1043.513878	75117.668559	34.474944
1044.156987	75241.597537	34.479962
1045.531688	75351.773473	34.484980
1046.278792	75473.658789	34.489997
1047.369110	75594.510718	34.495015
1048.476684	75735.513811	34.500032
1049.838873	75853.612945	34.505050
1050.715907	75973.685846	34.510068
1051.451846	76112.538808	34.515085
1052.915464	76235.610304	34.520103
1053.733254	76372.044206	34.525120
1054.681831	76500.400434	34.530138
1055.911715	76627.139082	34.535156
1056.768604	76750.032149	34.540173
1058.002008	76883.812231	34.545191
1058.871538	77027.074193	34.550208
1059.653751	77153.293265	34.555226
1061.454559	77289.595950	34.560244
1062.028174	77435.657102	34.565261
1063.212205	77558.540955	34.570279
1064.350306	77702.276897	34.575296
1065.454501	77833.214418	34.580314
1066.756958	77977.305376	34.585332
1067.919270	78107.862523	34.590349
1069.247333	78240.353459	34.595367
1069.813420	78373.193990	34.600384
1071.454256	78497.199092	34.605402
1072.894275	78629.238636	34.610420
1073.663648	78762.093606	34.615437
1074.486653	78883.443780	34.620455
1075.497412	79020.920300	34.625472
1076.293769	79156.124805	34.630490
1077.561770	79301.987736	34.635508
1078.522055	79433.887554	34.640525
1079.645341	79578.075186	34.645543
1080.737747	79716.598955	34.650560
1081.922266	79843.965311	34.655578
1083.124002	79975.507839	34.660596
1084.009546	80125.659820	34.665613
1085.010548	80269.403999	34.670631
1086.323409	80384.477908	34.675648
1087.362644	80553.040706	34.680666
1088.517467	80666.858147	34.685684
1089.881610	80804.909860	34.690701
1090.943988	80950.185062	34.695719
1091.930268	81083.608399	34.700736
1092.632082	81218.398990	34.705754
1094.523112	81346.534593	34.710772
1095.154950	81479.340471	34.715789
1096.334860	81607.736185	34.720807
1097.390925	81723.155498	34.725824
1098.353523	81850.563203	34.730842
1099.598172	81980.310044	34.735860
1100.755093	82089.893233	34.740877
1101.768144	82222.390367	34.745895
1102.878706	82342.362323	34.750912
1103.834484	82461.032037	34.755930
1105.042677	82602.268707	34.760948
1106.137012	82709.829523	34.765965
1106.843791	82829.204717	34.770983
1108.450134	82986.475920	34.776000
1109.194664	83102.388632	34.781018
1110.257219	83240.871164	34.786036
1111.944314	83367.237270	34.791053
1112.802088	83476.451752	34.796071
1113.633091	83640.438681	34.801088
1114.614640	83768.354518	34.806106
1115.914417	83901.271883	34.811124
1116.918618	84035.646935	34.816141
1118.049844	84170.830851	34.821159
1119.150317	84316.199309	34.826176
1120.168296	84454.437726	34.831194
1121.303146	84592.822843	34.836212
1122.650303	84737.421588	34.841229
1123.651989	84875.077376	34.846247
1125.309554	85021.152397	34.851264
1126.282359	85163.082301	34.856282
1127.585303	85301.274624	34.861300
1128.555602	85437.149790	34.866317
1129.600278	85584.464236	34.871335
1131.081979	85707.513437	34.876352
1131.959950	85838.828269	34.881370
1133.050658	85995.483174	34.886388
1134.249570	86137.649200	34.891405
1135.194142	86264.422646	34.896423
1136.547836	86396.885573	34.901440
1137.253665	86561.212239	34.906458
1138.859210	86694.376745	34.911476
1140.183363	86841.402539	34.916493
1140.958469	86969.964921	34.921511
1142.444661	87116.682306	34.926528
1143.573331	87269.698460	34.931546
1144.528176	87395.225018	34.936564
1145.946857	87542.398683	34.941581
1146.876600	87683.138188	34.946599
1147.862046	87832.127949	34.951616
1148.953620	87986.464039	34.956634
1150.036189	88106.903153	34.961652
1151.258615	88272.994578	34.966669
1152.072270	88414.288500	34.971687
1153.413511	88551.705361	34.976704
1154.691159	88729.293942	34.981722
1155.747485	88841.400601	34.986740
1157.245639	88999.302703	34.991757
1158.164014	89141.963289	34.996775
1159.725521	89270.009665	35.001792
1160.672463	89410.182268	35.006810
1161.771199	89535.319004	35.011828
1163.176596	89667.724344	35.016845
1163.887887	89798.710500	35.021863
1165.486049	89923.833302	35.026880
1166.577717	90056.657693	35.031898
1167.572381	90194.405716	35.036916
1168.616887	90322.123146	35.041933
1169.712468	90453.387312	35.046951
1171.105478	90594.818358	35.051968
1171.867961	90740.353755	35.056986
1173.046930	90881.213581	35.062004
1174.457292	91012.475331	35.067021
1175.480493	91152.798827	35.072039
1176.522152	91313.351670	35.077056
1177.875261	91448.027608	35.082074
1179.227304	91589.901673	35.087092
1180.249405	91729.482768	35.092109
1181.283283	91897.567177	35.097127
1182.872730	92035.624355	35.102144
1183.754089	92193.287218	35.107162
1184.901345	92331.720150	35.112180
1186.013797	92477.805953	35.117197
1187.070197	92639.643730	35.122215
1188.526849	92786.891189	35.127232
1189.949221	92942.240767	35.132250
1191.071723	93095.412793	35.137268
1192.190538	93243.684715	35.142285
1193.199644	93396.332921	35.147303
1194.724567	93544.662460	35.152320
1195.717214	93705.601071	35.157338
1197.179027	93848.895357	35.162356
1198.297502	93997.153404	35.167373
1199.532134	94159.106788	35.172391
1201.193016	94293.093370	35.177408
1202.131816	94451.674024	35.182426
1203.479503	94601.183669	35.187444
1204.714377	94746.170713	35.192461
1205.658547	94907.163683	35.197479
1207.308981	95041.042576	35.202496
1208.269957	95206.880255	35.207514
1209.413378	95358.280795	35.212532
1211.069422	95503.509414	35.217549
1212.019185	95657.960029	35.222567
1213.343069	95791.800460	35.227584
1214.395463	95947.109677	35.232602
1215.877741	96104.850251	35.237620
1216.865166	96254.820425	35.242637
1217.656121	96408.972522	35.247655
1219.325028	96543.534317	35.252672
1220.644967	96693.979590	35.257690
1221.569082	96840.446579	35.262708
1223.205267	96989.445529	35.267725
1224.038846	97155.090111	35.272743
1224.985769	97281.256383	35.277760
1226.592194	97419.799735	35.282778
1227.853558	97558.386147	35.287796
1229.039449	97708.144645	35.292813
1230.178983	97845.347789	35.297831
1231.345622	97974.253839	35.302848
1232.132759	98123.218115	35.307866
1233.420925	98259.603029	35.312884
1235.018086	98395.047628	35.317901
1235.628341	98544.453994	35.322919
1236.819041	98703.113111	35.327936
1238.235679	98861.844960	35.332954
1239.544069	99001.679004	35.337972
1240.888288	99153.376721	35.342989
1241.799247	99321.258038	35.348007
1243.128643	99466.405887	35.353024
1244.663461	99625.427928	35.358042
1245.591364	99793.025311	35.363060
1246.815573	99936.294857	35.368077
1248.133385	100104.642344	35.373095
1249.236945	100262.636509	35.378112
1250.342696	100433.398997	35.383130
1251.484042	100594.128957	35.388148
1253.268723	100758.572905	35.393165
1254.253532	100932.768542	35.398183
1255.643990	101088.217266	35.403200
1257.102606	101257.860489	35.408218
1257.991013	101423.641155	35.413236
1259.670833	101580.217702	35.418253
1260.845175	101759.704252	35.423271
1262.113306	101920.733310	35.428288
1263.386893	102088.969416	35.433306
1264.394391	102257.356608	35.438324
1266.351295	102425.720631	35.443341
1267.166956	102597.981513	35.448359
1268.893486	102754.450983	35.453376
1269.962531	102920.529975	35.458394
1270.652409	103090.536575	35.463412
1272.440829	103256.547885	35.468429
1273.403942	103426.159138	35.473447
1275.368134	103593.593932	35.478464
1276.714885	103761.235652	35.483482
1277.926136	103903.607897	35.488500
1279.022625	104094.381917	35.493517
1280.306494	104247.318534	35.498535
1281.993505	104399.654183	35.503552
1283.371038	104580.123562	35.508570
1284.245392	104727.939458	35.513588
1285.599111	104884.558339	35.518605
1287.078344	105074.222655	35.523623
1288.245704	105225.140151	35.528640
1289.322698	105377.591740	35.533658
1290.651606	105561.999820	35.538676
1292.230830	105718.968068	35.543693
1293.033491	105876.586051	35.548711
1294.583105	106043.224501	35.553728
1295.874871	106175.794992	35.558746
1296.927423	106323.959553	35.563764
1298.405714	106478.784535	35.568781
1299.566691	106645.109265	35.573799
1300.644343	106775.698329	35.578816
1302.088677	106936.904542	35.583834
1303.458120	107098.452837	35.588852
1304.666739	107260.685969	35.593869
1305.597315	107410.749947	35.598887
1306.704152	107592.430707	35.603904
1308.265578	107743.295170	35.608922
1309.153036	107906.172295	35.613940
1310.619022	108093.476738	35.618957
1311.719957	108257.581757	35.623975
1313.325977	108430.645411	35.628992
1314.506562	108602.733640	35.634010
1315.812327	108775.024714	35.639028
1317.350622	108965.444667	35.644045
1318.362209	109146.905435	35.649063
1319.747417	109334.327271	35.654080
1321.252060	109485.521779	35.659098
1322.472023	109682.795601	35.664116
1323.783615	109850.719826	35.669133
1325.311277	110033.288771	35.674151
1326.710888	110211.999477	35.679168
1327.875387	110408.667703	35.684186
1329.486135	110577.372216	35.689204
1331.062302	110753.356099	35.694221
1332.147854	110920.652674	35.699239
1333.347683	111115.827168	35.704256
1335.455071	111288.578272	35.709274
1336.241757	111471.484604	35.714292
1337.665668	111648.828366	35.719309
1338.711650	111832.259518	35.724327
1340.235419	112018.546847	35.729344
1341.947843	112189.936495	35.734362
1342.950318	112377.493093	35.739380
1344.665571	112557.645587	35.744397
1345.940404	112739.578524	35.749415
1346.982844	112919.213905	35.754432
1348.663051	113093.172312	35.759450
1350.141672	113278.159613	35.764468
1351.325283	113453.035061	35.769485
1352.922126	113634.625847	35.774503
1353.869024	113819.935907	35.779520
1355.665978	114002.111611	35.784538
1356.699945	114188.531052	35.789556
1358.352474	114360.711181	35.794573
1359.403065	114542.395386	35.799591
1360.562717	114724.639657	35.804608
1362.222426	114910.148362	35.809626
1363.378368	115105.481461	35.814644
1364.921672	115270.075681	35.819661
1366.378916	115452.499506	35.824679
1367.357422	115635.868063	35.829696
1369.168795	115798.979700	35.834714
1370.415623	115959.409172	35.839732
1371.625279	116123.593499	35.844749
1373.106376	116302.790881	35.849767
1374.206600	116463.303824	35.854784
1375.923236	116617.293762	35.859802
1376.757184	116805.125517	35.864820
1378.015530	116977.924305	35.869837
1379.395704	117156.099102	35.874855
1380.381208	117343.264952	35.879872
1382.131683	117529.025342	35.884890
1383.224040	117718.912089	35.889908
1384.561211	117889.944406	35.894925
1385.960893	118093.745833	35.899943
1387.550121	118282.012913	35.904960
1389.019066	118464.456475	35.909978
1390.400113	118658.210856	35.914996
1391.764254	118852.235311	35.920013
1393.214599	119030.146056	35.925031
1394.772503	119250.552171	35.930048
1396.229774	119427.305845	35.935066
1397.191367	119627.408955	35.940084
1398.845700	119817.506799	35.945101
1400.218925	120009.056397	35.950119
1401.447588	120234.018865	35.955136
1403.258611	120411.432210	35.960154
1404.577510	120612.967820	35.965172
1405.660421	120823.679736	35.970189
1407.525550	121014.512683	35.975207
1408.850336	121197.302336	35.980224
1410.545842	121395.193771	35.985242
1412.003768	121602.812883	35.990260
1413.308064	121788.256820	35.995277
1415.115699	121984.070532	36.000295
1416.397353	122186.542368	36.005312
1417.915146	122363.597605	36.010330
1419.457155	122571.451635	36.015348
1421.117806	122750.589171	36.020365
1422.392634	122939.984761	36.025383
1423.721800	123139.910640	36.030400
1425.477766	123323.267134	36.035418
1426.987756	123514.795252	36.040436
1428.277581	123697.658458	36.045453
1429.707622	123879.158074	36.050471
1430.953008	124076.786492	36.055488
1432.483883	124269.583301	36.060506
1433.944067	124458.719603	36.065524
1435.224011	124635.625135	36.070541
1437.073881	124840.370132	36.075559
1438.439593	125016.745240	36.080576
1440.055877	125220.174969	36.085594
1441.254052	125405.319023	36.090612
1442.613582	125595.467316	36.095629
1444.015342	125773.652972	36.100647
1445.269319	125952.927289	36.105664
1446.957837	126114.526952	36.110682
1448.343359	126288.297887	36.115700
1449.537260	126469.523202	36.120717
1451.160343	126639.357231	36.125735
1452.383421	126812.942004	36.130752
1454.019390	126993.023869	36.135770
1454.814742	127171.505086	36.140788
1456.247494	127360.526750	36.145805
1458.134491	127552.847081	36.150823
1459.246216	127738.628844	36.155840
1460.560192	127918.248617	36.160858
1462.197860	128123.786883	36.165876
1463.357380	128307.170716	36.170893
1464.551282	128514.011192	36.175911
1466.478295	128712.147860	36.180928
1467.836104	128894.820037	36.185946
1468.932368	129130.791837	36.190964
1470.401651	129308.065075	36.195981
1471.989907	129552.766728	36.200999
1473.215654	129739.975407	36.206016
1474.928660	129962.896508	36.211034
1476.077829	130177.636370	36.216052
1477.391752	130391.680269	36.221069
1478.907579	130592.708192	36.226087
1480.672005	130824.534206	36.231104
1481.912263	131030.144539	36.236122
1483.664954	131267.436437	36.241140
1484.873956	131481.442009	36.246157
1486.839186	131695.240375	36.251175
1488.003337	131922.141128	36.256192
1490.107838	132156.597371	36.261210
1491.534798	132362.479192	36.266228
1492.991082	132586.500882	36.271245
1494.597311	132813.110505	36.276263
1496.137177	133007.158145	36.281280
1497.439234	133237.050308	36.286298
1499.055464	133458.506806	36.291316
1500.627017	133675.233470	36.296333
1502.873939	133868.883244	36.301351
1504.479304	134074.711130	36.306368
1506.387354	134271.585072	36.311386
1507.869827	134485.316469	36.316404
1509.529540	134683.221001	36.321421
1511.035840	134873.916284	36.326439
1512.717306	135081.044395	36.331456
1514.356817	135284.265351	36.336474
1515.390928	135482.553535	36.341492
1516.929111	135680.180128	36.346509
1518.650554	135867.122505	36.351527
1519.709292	136085.139919	36.356544
1521.896932	136272.517700	36.361562
1523.173856	136485.802394	36.366580
1524.175246	136686.093425	36.371597
1526.063090	136865.742347	36.376615
1527.595530	137058.652731	36.381632
1528.839811	137240.965887	36.386650
1530.233916	137435.396004	36.391668
1531.736431	137613.640810	36.396685
1533.494044	137784.509086	36.401703
1534.740348	137991.727079	36.406720
1535.872771	138191.247268	36.411738
1537.880124	138375.321731	36.416756
1539.230484	138566.192707	36.421773
1540.508036	138754.035105	36.426791
1541.635894	138966.753248	36.431808
1542.735979	139186.878127	36.436826
1544.901019	139375.052364	36.441844
1545.670708	139605.789178	36.446861
1548.059159	139819.821238	36.451879
1549.122654	140014.320853	36.456896
1550.908570	140239.337710	36.461914
1552.594594	140449.088326	36.466932
1554.199163	140667.673916	36.471949
1555.782760	140876.556670	36.476967
1557.297896	141086.972561	36.481984
1558.998255	141306.738887	36.487002
1560.297129	141538.192276	36.492020
1561.827282	141739.574068	36.497037
1563.837565	141983.680257	36.502055
1565.353384	142188.261106	36.507072
1566.601448	142411.301123	36.512090
1568.471518	142641.810381	36.517108
1569.605110	142854.314345	36.522125
1571.683058	143090.281880	36.527143
1572.522522	143312.873758	36.532160
1574.507259	143506.729864	36.537178
1576.105361	143775.225419	36.542196
1577.162553	144005.075586	36.547213
1579.519915	144203.946757	36.552231
1580.581761	144474.510850	36.557248
1582.745249	144681.553130	36.562266
1584.135883	144942.322099	36.567284
1586.090070	145145.572882	36.572301
1587.661576	145379.623082	36.577319
1588.899381	145621.054359	36.582336
1590.783065	145837.046847	36.587354
1592.509793	146054.155852	36.592372
1593.992237	146304.286946	36.597389
1595.892067	146521.346349	36.602407
1597.592457	146740.048752	36.607424
1599.021423	146977.099678	36.612442
1600.837668	147192.630548	36.617460
1602.398084	147407.214798	36.622477
1603.786876	147647.585583	36.627495
1605.194327	147876.445249	36.632512
1607.049036	148097.680467	36.637530
1608.841924	148327.711767	36.642548
1610.570804	148535.140105	36.647565
1612.052148	148778.610481	36.652583
1613.641757	148973.361894	36.657600
1615.283773	149174.900883	36.662618
1616.581864	149402.305706	36.667636
1617.973436	149578.596820	36.672653
1619.881331	149813.767358	36.677671
1621.064861	150018.946692	36.682688
1622.745223	150230.108082	36.687706
1624.527670	150427.347754	36.692724
1625.705437	150696.501497	36.697741
1627.389697	150875.821121	36.702759
1629.065826	151112.128173	36.707776
1630.279289	151313.013291	36.712794
1631.742484	151573.203970	36.717812
1633.556373	151772.602017	36.722829
1635.298467	152041.144778	36.727847
1636.544451	152256.090236	36.732864
1638.400264	152494.990399	36.737882
1640.340760	152743.260637	36.742900
1641.867905	152967.509845	36.747917
1643.368536	153241.882006	36.752935
1645.102116	153441.087396	36.757952
1646.655412	153709.508915	36.762970
1648.515596	153928.386783	36.767988
1650.576872	154163.792449	36.773005
1652.160867	154437.273736	36.778023
1653.741635	154644.992682	36.783040
1655.552350	154898.066876	36.788058
1657.272763	155134.230849	36.793076
1659.106238	155357.242990	36.798093
1660.457868	155636.971030	36.803111
1662.205421	155854.446620	36.808128
1663.853071	156117.293554	36.813146
1665.853269	156335.885938	36.818164
1667.197524	156589.084929	36.823181
1669.258502	156816.128010	36.828199
1670.889604	157054.589218	36.833216
1672.389882	157322.008200	36.838234
1674.371274	157551.947131	36.843252
1676.114103	157781.849409	36.848269
1677.613946	158028.326631	36.853287
1679.685434	158258.940709	36.858304
1681.111271	158530.793610	36.863322
1682.863632	158763.769545	36.868340
1684.385014	158987.666496	36.873357
1686.700633	159190.909024	36.878375
1687.953863	159462.073840	36.883392
1689.740873	159738.836954	36.888410
1691.564295	159945.585834	36.893428
1693.360725	160165.363459	36.898445
1694.958203	160428.606288	36.903463
1696.803331	160657.788530	36.908480
1698.441735	160872.738836	36.913498
1700.465945	161102.339370	36.918516
1701.782203	161344.608278	36.923533
1703.202753	161593.875077	36.928551
1704.684608	161842.702718	36.933568
1706.617702	162049.243604	36.938586
1708.188461	162250.897397	36.943604
1709.674905	162492.868098	36.948621
1711.418223	162723.436778	36.953639
1713.033288	162925.670698	36.958656
1714.389786	163180.386557	36.963674
1716.648347	163377.891936	36.968692
1717.762763	163633.461081	36.973709
1719.601938	163862.271701	36.978727
1721.329902	164099.573168	36.983744
1722.751567	164346.893137	36.988762
1724.524532	164610.379827	36.993780
1726.417993	164825.960120	36.998797
1727.793335	165110.059212	37.003815
1729.785855	165317.700046	37.008832
1731.082523	165598.226211	37.013850
1733.026044	165821.870650	37.018868
1734.549146	166109.289582	37.023885
1736.496146	166342.639077	37.028903
1738.289791	166624.121440	37.033920
1739.970146	166850.832463	37.038938
1741.694169	167147.296013	37.043956
1743.570567	167376.109896	37.048973
1745.665027	167661.129033	37.053991
1747.405651	167899.683212	37.059008
1748.932012	168175.626243	37.064026
1751.305118	168427.033346	37.069044
1752.933476	168683.786100	37.074061
1754.795471	168955.787604	37.079079
1756.901894	169197.538976	37.084096
1758.022701	169455.201987	37.089114
1760.037549	169716.644194	37.094132
1761.777161	169973.185030	37.099149
1763.698452	170226.920870	37.104167
1765.431851	170512.196307	37.109184
1767.379133	170738.431574	37.114202
1768.868339	171027.631045	37.119220
1770.297518	171254.522395	37.124237
1772.589860	171542.672214	37.129255
1774.554999	171798.504385	37.134272
1776.435323	172051.320001	37.139290
1777.955179	172333.978884	37.144308
1780.253783	172561.970249	37.149325
1781.672391	172841.705918	37.154343
1783.495290	173115.912035	37.159360
1785.027853	173386.906010	37.164378
1787.063977	173606.255614	37.169396
1788.842423	173855.458259	37.174413
1790.398896	174173.504356	37.179431
1792.392730	174386.928113	37.184448
1794.096194	174687.169651	37.189466
1796.209773	174945.814840	37.194484
1797.983035	175183.837661	37.199501
1799.456389	175470.344660	37.204519
1801.677511	175665.509325	37.209536
1803.141007	175918.605959	37.214554
1804.942140	176192.773145	37.219572
1806.767381	176395.692027	37.224589
1808.293080	176629.132124	37.229607
1810.360844	176901.701317	37.234624
1811.614585	177144.994156	37.239642
1813.282023	177390.988438	37.244660
1815.353619	177623.116919	37.249677
1816.793408	177899.979009	37.254695
1818.715322	178161.567569	37.259712
1820.942789	178413.454525	37.264730
1822.272543	178669.646844	37.269748
1824.240138	178942.245366	37.274765
1825.657967	179212.814176	37.279783
1827.996468	179456.227446	37.284800
1829.380790	179760.248653	37.289818
1831.473637	180025.792843	37.294836
1833.319779	180284.577367	37.299853
1834.989661	180580.730948	37.304871
1836.981544	180829.269469	37.309888
1839.035582	181096.069885	37.314906
1840.517396	181397.879636	37.319924
1842.548817	181654.333858	37.324941
1844.536658	181962.588813	37.329959
1846.191476	182219.093479	37.334976
1848.120242	182499.587494	37.339994
1849.794266	182817.731638	37.345012
1851.419832	183068.993027	37.350029
1853.631191	183351.794995	37.355047
1855.455752	183671.126835	37.360064
1857.034738	183944.021781	37.365082
1859.374080	184221.860484	37.370100
1861.306790	184537.692040	37.375117
1863.045911	184797.865414	37.380135
1865.301444	185088.589272	37.385152
1867.361495	185363.789387	37.390170
1868.787437	185653.925317	37.395188
1870.921645	185943.557332	37.400205
1872.683923	186232.831494	37.405223
1875.176016	186511.979822	37.410240
1876.623449	186807.588808	37.415258
1878.087376	187088.794577	37.420276
1880.270267	187365.789244	37.425293
1881.750870	187685.775189	37.430311
1884.614006	187945.902423	37.435328
1886.021950	188264.876048	37.440346
1887.929629	188533.584234	37.445364
1890.242614	188817.482911	37.450381
1891.923340	189109.630635	37.455399
1893.639423	189384.274969	37.460416
1895.405311	189696.551961	37.465434
1897.397933	189960.407211	37.470452
1899.269503	190254.282994	37.475469
1901.367558	190550.446988	37.480487
1903.236020	190801.293604	37.485504
1904.847120	191073.730870	37.490522
1906.879106	191345.277996	37.495540
1908.882314	191597.731789	37.500557
1910.502258	191857.506822	37.505575
1912.221394	192123.587518	37.510592
1914.367201	192401.797874	37.515610
1916.522158	192668.066200	37.520628
1918.436790	192946.862063	37.525645
1919.368992	193206.309249	37.530663
1921.448670	193496.059810	37.535680
1923.351146	193769.785808	37.540698
1925.100270	194091.371126	37.545716
1927.344744	194350.298767	37.550733
1928.707209	194653.863892	37.555751
1931.029300	194943.800176	37.560768
1932.681499	195230.976146	37.565786
1934.810478	195555.125045	37.570804
1936.918979	195814.043734	37.575821
1938.522285	196156.784445	37.580839
1940.919709	196441.615245	37.585856
1942.764749	196736.968079	37.590874
1944.446798	197047.528148	37.595892
1946.489941	197357.258564	37.600909
1948.296498	197670.036423	37.605927
1950.583869	197968.410299	37.610944
1952.423388	198297.217017	37.615962
1954.658583	198586.514985	37.620980
1956.616395	198894.668817	37.625997
1958.341163	199213.523177	37.631015
1960.583019	199504.703614	37.636032
1962.752135	199832.820258	37.641050
1964.699743	200146.694684	37.646068
1966.856580	200444.430512	37.651085
1968.487539	200756.480199	37.656103
1970.468216	201080.064895	37.661120
1972.624376	201396.388619	37.666138
1974.625341	201699.284067	37.671156
1976.829186	202012.468578	37.676173
1978.547885	202339.732551	37.681191
1980.674015	202643.349541	37.686208
1982.764940	202960.581133	37.691226
1984.650099	203275.092690	37.696244
1986.708477	203589.527751	37.701261
1988.869515	203898.908903	37.706279
1990.977571	204195.377957	37.711296
1993.331821	204506.178852	37.716314
1995.221987	204813.983169	37.721332
1997.498201	205118.808284	37.726349
1999.391592	205418.719719	37.731367
2001.062366	205721.498807	37.736384
2003.501557	206027.001031	37.741402
2005.384374	206344.944577	37.746420
2007.389731	206643.892503	37.751437
2009.408247	206937.254366	37.756455
2011.164945	207227.574496	37.761472
2012.577130	207524.488344	37.766490
2014.362540	207801.845707	37.771508
2016.565962	208081.968919	37.776525
2018.170703	208390.040416	37.781543
2019.964147	208690.174758	37.786560
2022.097983	208992.567023	37.791578
2024.130858	209278.232362	37.796596
2025.774476	209582.279486	37.801613
2027.836437	209904.186985	37.806631
2029.501286	210229.002850	37.811648
2031.661161	210548.168741	37.816666
2033.336292	210874.281242	37.821684
2035.645907	211197.387576	37.826701
2037.590736	211533.477222	37.831719
2039.596961	211868.010083	37.836736
2042.007760	212194.710933	37.841754
2043.738460	212530.763650	37.846772
2045.994215	212875.456652	37.851789
2048.050548	213195.858371	37.856807
2050.051225	213523.519721	37.861824
2052.275981	213868.718044	37.866842
2054.289252	214210.993616	37.871860
2056.576156	214542.385292	37.876877
2058.217701	214883.859998	37.881895
2060.546444	215233.454426	37.886912
2063.327740	215574.167823	37.891930
2065.095231	215912.809260	37.896948
2067.287075	216241.748669	37.901965
2069.298234	216586.372786	37.906983
2071.295249	216926.354031	37.912000
2073.478220	217281.974761	37.917018
2075.696594	217620.096019	37.922036
2078.119896	217941.401651	37.927053
2080.054392	218287.379501	37.932071
2082.307906	218637.764946	37.937088
2085.020582	218958.165928	37.942106
2086.987085	219294.392565	37.947124
2089.200132	219628.524783	37.952141
2091.576324	219960.651957	37.957159
2093.669433	220275.684741	37.962176
2095.900663	220609.209128	37.967194
2097.541906	220927.109717	37.972212
2100.009355	221249.388067	37.977229
2101.928815	221601.275543	37.982247
2103.748247	221928.065515	37.987264
2105.984691	222246.512158	37.992282
2107.544311	222592.480940	37.997300
2109.975460	222930.250227	38.002317
2112.138987	223265.396997	38.007335
2113.836767	223598.790664	38.012352
2116.258637	223940.235398	38.017370
2117.798414	224323.952070	38.022388
2120.385737	224687.391394	38.027405
2122.529877	225024.199447	38.032423
2124.222431	225348.941513	38.037440
2126.680418	225655.900858	38.042458
2128.803970	225981.135803	38.047476
2130.619383	226293.494477	38.052493
2132.730075	226601.604489	38.057511
2134.878811	226940.502213	38.062528
2137.146174	227246.596190	38.067546
2138.519073	227576.146827	38.072564
2141.102090	227889.532571	38.077581
2142.752270	228235.320791	38.082599
2145.018436	228573.952494	38.087616
2147.129804	228911.924376	38.092634
2148.950899	229248.470610	38.097652
2151.011018	229605.069057	38.102669
2152.980045	229945.378619	38.107687
2155.033644	230306.984114	38.112704
2157.026430	230670.530893	38.117722
2159.234807	231046.718128	38.122740
2161.329676	231400.118184	38.127757
2163.645899	231771.135660	38.132775
2165.675536	232145.679534	38.137792
2168.214397	232516.893262	38.142810
2170.339423	232887.716936	38.147828
2172.081600	233269.066659	38.152845
2174.622660	233642.138488	38.157863
2176.876794	234029.810300	38.162880
2179.125479	234395.921566	38.167898
2181.022455	234795.691740	38.172916
2183.421994	235164.956707	38.177933
2185.819205	235552.764204	38.182951
2187.678527	235937.534487	38.187968
2190.379754	236329.309694	38.192986
2192.465464	236702.414414	38.198004
2195.126802	237080.077151	38.203021
2197.461799	237461.018654	38.208039
2199.628637	237847.753748	38.213056
2202.043653	238215.935009	38.218074
2204.170286	238598.335949	38.223092
2206.880683	238978.029537	38.228109
2208.884739	239356.363290	38.233127
2210.867210	239728.224917	38.238144
2213.360291	240104.883488	38.243162
2215.574167	240486.184896	38.248180
2217.547598	240858.839035	38.253197
2219.604090	241235.849942	38.258215
2221.897250	241632.966539	38.263232
2224.432103	242006.475079	38.268250
2226.930961	242382.911481	38.273268
2229.293181	242762.799717	38.278285
2232.054784	243132.414964	38.283303
2233.859844	243518.947096	38.288320
2236.192671	243890.639192	38.293338
2238.192591	244250.472421	38.298356
2240.063948	244625.770470	38.303373
2242.637607	244992.144281	38.308391
2244.808155	245334.046137	38.313408
2247.251887	245695.616401	38.318426
2249.056058	246039.635601	38.323444
2251.067256	246373.995973	38.328461
2253.213790	246729.469136	38.333479
2255.391276	247098.527743	38.338496
2257.791516	247438.493363	38.343514
2260.235906	247800.094410	38.348532
2262.240971	248158.362282	38.353549
2264.150025	248514.512562	38.358567
2266.284470	248875.581180	38.363584
2268.737427	249252.501316	38.368602
2270.556185	249620.403884	38.373620
2272.748369	250008.797792	38.378637
2275.453314	250379.177975	38.383655
2277.703440	250769.012440	38.388672
2280.004319	251136.842088	38.393690
2282.209435	251535.195026	38.398708
2284.636489	251912.608185	38.403725
2287.080424	252293.804358	38.408743
2289.170779	252688.037724	38.413760
2291.496429	253075.376185	38.418778
2293.874953	253473.020257	38.423796
2295.992150	253860.418860	38.428813
2298.553884	254252.294747	38.433831
2300.547344	254652.822028	38.438848
2303.161892	255044.589570	38.443866
2305.469073	255445.373579	38.448884
2307.508378	255845.794430	38.453901
2310.080923	256252.202659	38.458919
2312.170227	256646.164984	38.463936
2315.002596	257049.180472	38.468954
2317.068679	257458.516376	38.473972
2319.409075	257868.597024	38.478989
2322.011584	258269.263359	38.484007
2324.323975	258676.428618	38.489024
2326.705294	259070.221917	38.494042
2328.786529	259487.459207	38.499060
2331.278337	259888.501445	38.504077
2333.846434	260295.578056	38.509095
2335.999267	260704.880365	38.514112
2338.608717	261103.060722	38.519130
2341.000292	261524.138693	38.524148
2343.382362	261921.670392	38.529165
2346.164669	262322.492362	38.534183
2348.497157	262721.125322	38.539200
2351.107849	263131.552452	38.544218
2353.649937	263508.865552	38.549236
2355.604006	263910.049481	38.554253
2358.190622	264309.812656	38.559271
2360.806708	264698.673718	38.564288
2363.346658	265083.279554	38.569306
2365.674740	265484.736208	38.574324
2367.526235	265882.661584	38.579341
2370.390317	266263.305128	38.584359
2372.517811	266631.592832	38.589376
2374.805595	266993.377629	38.594394
2376.934428	267362.249997	38.599412
2379.023747	267722.466421	38.604429
2381.724443	268086.701519	38.609447
2383.674518	268463.478043	38.614464
2386.306104	268819.722578	38.619482
2388.518271	269204.815732	38.624500
2390.322429	269589.592755	38.629517
2393.004471	269961.275170	38.634535
2394.816326	270359.438964	38.639552
2397.175319	270747.431126	38.644570
2399.510864	271142.336907	38.649588
2401.795879	271547.767873	38.654605
2404.251821	271954.340478	38.659623
2406.312312	272371.442119	38.664640
2408.866631	272776.907098	38.669658
2411.418396	273185.700455	38.674676
2413.514557	273611.942066	38.679693
2416.313741	274022.093609	38.684711
2418.903300	274438.730925	38.689728
2421.052937	274857.749743	38.694746
2423.735191	275280.672527	38.699764
2425.999694	275707.294241	38.704781
2428.580625	276129.216990	38.709799
2431.250338	276565.783431	38.714816
2433.919754	276987.920752	38.719834
2436.136177	277412.212904	38.724852
2438.704059	277833.654914	38.729869
2441.268526	278254.741736	38.734887
2443.807002	278694.707300	38.739904
2446.073225	279123.055730	38.744922
2448.870333	279551.853349	38.749940
2451.358111	279990.276901	38.754957
2453.582304	280403.922960	38.759975
2455.993178	280833.619562	38.764992
2458.814759	281278.721482	38.770010
2461.614918	281698.982098	38.775028
2463.958664	282141.415668	38.780045
2466.597698	282556.417409	38.785063
2468.932768	282987.191663	38.790080
2471.540530	283423.536498	38.795098
2473.973929	283843.371121	38.800116
2476.622415	284278.082996	38.805133
2479.209231	284694.005909	38.810151
2481.365728	285133.646981	38.815168
2484.076116	285550.946703	38.820186
2486.871604	285984.795352	38.825204
2489.428006	286407.199239	38.830221
2491.689254	286833.815541	38.835239
2494.396585	287257.972785	38.840256
2496.569151	287681.807826	38.845274
2499.179318	288115.429353	38.850292
2501.755449	288542.044507	38.855309
2504.072765	288961.460290	38.860327
2506.528484	289365.967508	38.865344
2508.599812	289755.674451	38.870362
2511.304681	290149.192518	38.875380
2513.629341	290559.637722	38.880397
2515.932399	290966.681782	38.885415
2518.436464	291360.102952	38.890432
2520.415586	291778.729925	38.895450
2523.105146	292191.477257	38.900468
2525.354175	292625.733468	38.905485
2528.039272	293042.290475	38.910503
2530.282623	293456.579726	38.915520
2532.709938	293891.211826	38.920538
2535.399050	294323.159769	38.925556
2537.647922	294769.249510	38.930573
2540.179114	295204.040399	38.935591
2542.631149	295642.729477	38.940608
2545.187136	296100.046335	38.945626
2547.316843	296552.171470	38.950644
2550.009933	297016.678706	38.955661
2552.544415	297468.737592	38.960679
2555.199621	297934.010668	38.965696
2557.925670	298406.917309	38.970714
2560.594540	298868.527989	38.975732
2563.148961	299340.671914	38.980749
2565.576055	299790.405085	38.985767
2568.356405	300273.814397	38.990784
2570.957634	300735.862633	38.995802
2573.632348	301228.405044	39.000820
2576.438763	301691.967550	39.005837
2579.277509	302154.101107	39.010855
2582.256262	302617.150957	39.015872
2584.989822	303100.228934	39.020890
2587.787780	303547.657499	39.025908
2590.319702	304006.074674	39.030925
2593.052849	304468.827477	39.035943
2595.621476	304931.757252	39.040960
2598.566572	305393.330428	39.045978
2601.345515	305853.810763	39.050996
2604.010775	306318.625647	39.056013
2606.692894	306771.726642	39.061031
2609.224367	307215.197813	39.066048
2611.597919	307685.032587	39.071066
2614.390093	308137.171597	39.076084
2616.783144	308591.988433	39.081101
2619.437618	309077.420002	39.086119
2622.276341	309535.515578	39.091136
2625.130235	309992.591033	39.096154
2627.750992	310450.057273	39.101172
2629.877726	310917.734447	39.106189
2632.701908	311381.997328	39.111207
2635.639352	311848.424744	39.116224
2637.878013	312302.921674	39.121242
2640.837199	312750.343247	39.126260
2643.030454	313226.305926	39.131277
2645.630266	313677.996908	39.136295
2648.412918	314127.650530	39.141312
2650.961306	314550.594463	39.146330
2653.294078	314985.406639	39.151348
2655.833111	315423.308357	39.156365
2658.636137	315863.071288	39.161383
2660.897886	316300.124249	39.166400
2662.938207	316750.315882	39.171418
2665.661106	317191.762010	39.176436
2668.342900	317652.464365	39.181453
2670.848778	318117.967216	39.186471
2673.429691	318574.846103	39.191488
2676.010201	319047.418611	39.196506
2678.572165	319531.928524	39.201524
2680.917297	320017.587758	39.206541
2683.810635	320507.017993	39.211559
2686.589114	320974.342932	39.216576
2688.972743	321471.290069	39.221594
2691.877978	321961.116915	39.226612
2694.371119	322460.428495	39.231629
2696.928344	322961.479443	39.236647
2699.786780	323462.505188	39.241664
2702.284005	323973.388165	39.246682
2705.190752	324478.920826	39.251700
2707.721123	324996.014411	39.256717
2710.645553	325498.084264	39.261735
2713.609805	326017.439160	39.266752
2716.290025	326544.682923	39.271770
2719.386361	327052.912456	39.276788
2722.312560	327573.990234	39.281805
2724.988520	328084.235169	39.286823
2728.135992	328589.094592	39.291840
2730.826642	329112.916669	39.296858
2733.965225	329606.470236	39.301876
2736.624956	330139.203621	39.306893
2739.400057	330645.403531	39.311911
2742.454891	331149.270250	39.316928
2744.742834	331674.763489	39.321946
2747.619108	332176.772310	39.326964
2750.672669	332696.017087	39.331981
2752.919311	333211.805456	39.336999
2755.903035	333728.895375	39.342016
2758.477930	334238.352219	39.347034
2761.537072	334765.198811	39.352052
2764.666909	335278.851522	39.357069
2767.647174	335784.119240	39.362087
2770.540437	336297.497062	39.367104
2772.858922	336815.710285	39.372122
2776.017046	337318.221437	39.377140
2778.671791	337836.195745	39.382157
2781.478300	338357.595165	39.387175
2784.218681	338861.709565	39.392192
2787.626643	339361.397882	39.397210
2790.196150	339867.562756	39.402228
2792.904461	340388.047263	39.407245
2795.429417	340887.457198	39.412263
2798.237861	341365.871450	39.417280
2800.539695	341848.856260	39.422298
2803.385100	342321.493792	39.427316
2806.482699	342791.193352	39.432333
2808.996068	343276.697781	39.437351
2811.577083	343754.875547	39.442368
2814.344595	344242.083817	39.447386
2817.135815	344739.135166	39.452404
2819.829433	345225.890081	39.457421
2822.227006	345729.621813	39.462439
2825.315801	346220.901172	39.467456
2827.542966	346735.872691	39.472474
2830.460916	347237.833337	39.477492
2833.464093	347755.922447	39.482509
2835.771421	348262.921277	39.487527
2838.324591	348811.079556	39.492544
2841.139437	349348.274779	39.497562
2844.050741	349875.828089	39.502580
2846.580612	350415.139759	39.507597
2849.192383	350963.724387	39.512615
2852.529454	351520.413592	39.517632
2855.405292	352084.607987	39.522650
2858.133910	352637.929535	39.527668
2861.539111	353186.264318	39.532685
2864.405185	353746.812581	39.537703
2867.306347	354299.987845	39.542720
2870.195854	354860.291983	39.547738
2873.287822	355426.243950	39.552756
2876.402854	355985.535550	39.557773
2879.161977	356548.456380	39.562791
2882.109956	357100.096417	39.567808
2885.033954	357682.548695	39.572826
2887.749691	358235.152140	39.577844
2891.430311	358796.226567	39.582861
2894.063218	359353.120171	39.587879
2896.551932	359927.644988	39.592896
2899.931842	360497.174123	39.597914
2903.336533	361056.844829	39.602932
2906.254682	361607.017537	39.607949
2909.147980	362178.050397	39.612967
2912.362877	362718.924808	39.617984
2915.386380	363298.248105	39.623002
2918.093308	363843.352191	39.628020
2921.040983	364393.792119	39.633037
2924.100872	364973.418644	39.638055
2927.099214	365515.563631	39.643072
2930.105288	366074.907303	39.648090
2933.097117	366629.652923	39.653108
2935.934558	367181.751492	39.658125
2938.832903	367744.365124	39.663143
2941.908168	368309.532056	39.668160
2945.139169	368850.508632	39.673178
2947.830644	369414.427906	39.678196
2951.050694	369962.218654	39.683213
2953.712673	370517.804980	39.688231
2956.752278	371031.125322	39.693248
2959.958386	371532.766047	39.698266
2962.566577	372056.799829	39.703284
2965.836359	372560.524435	39.708301
2968.281481	373076.299345	39.713319
2971.333139	373580.680599	39.718336
2973.973522	374107.677817	39.723354
2976.822940	374637.477041	39.728372
2979.890413	375160.815640	39.733389
2982.289133	375692.220353	39.738407
2985.241722	376226.981094	39.743424
2988.196476	376777.363455	39.748442
2990.838180	377311.702379	39.753460
2994.181953	377869.848006	39.758477
2996.733217	378428.035145	39.763495
2999.918415	378976.118191	39.768512
3002.685277	379539.228142	39.773530
3005.540641	380109.926907	39.778548
3008.565902	380693.325815	39.783565
3011.776242	381262.683054	39.788583
3014.496614	381833.377871	39.793600
3017.504695	382421.852470	39.798618
3020.461785	383017.530511	39.803636
3023.884733	383609.218925	39.808653
3026.504916	384204.322815	39.813671
3030.004920	384776.016946	39.818688
3033.018510	385384.940695	39.823706
3035.787475	385985.522498	39.828724
3038.989369	386590.718618	39.833741
3042.299672	387207.251083	39.838759
3045.000089	387789.830571	39.843776
3048.230176	388412.848650	39.848794
3051.273528	389008.721134	39.853812
3054.351954	389644.322290	39.858829
3057.383413	390242.788565	39.863847
3060.555303	390861.740654	39.868864
3063.902567	391460.161790	39.873882
3066.708557	392097.892513	39.878900
3070.177047	392704.693239	39.883917
3073.244555	393325.621926	39.888935
3075.887039	393945.668416	39.893952
3079.033082	394561.287582	39.898970
3082.134324	395189.125886	39.903988
3085.521333	395819.138977	39.909005
3088.106453	396443.155922	39.914023
3091.513770	397040.152036	39.919040
3095.116980	397707.219385	39.924058
3097.816582	398306.054553	39.929076
3101.510259	398957.335983	39.934093
3104.363858	399559.420452	39.939111
3107.763835	400205.855367	39.944128
3110.702058	400817.259470	39.949146
3113.788433	401450.078442	39.954164
3117.348721	402064.073561	39.959181
3119.879793	402687.042796	39.964199
3123.657282	403263.787201	39.969216
3126.491320	403840.518333	39.974234
3129.186439	404439.722846	39.979252
3132.475510	404985.634530	39.984269
3135.362588	405570.742437	39.989287
3138.127296	406171.424050	39.994304
3140.913433	406729.705307	39.999322
3143.878375	407351.423782	40.004340
3147.254200	407935.826874	40.009357
3150.099685	408544.992362	40.014375
3153.105753	409171.230325	40.019392
3156.644239	409772.986791	40.024410
3159.407255	410397.691753	40.029428
3162.653181	411015.869372	40.034445
3165.830155	411652.725232	40.039463
3168.903538	412274.173856	40.044480
3172.288081	412932.994819	40.049498
3175.467967	413525.684575	40.054516
3178.798699	414195.434731	40.059533
3181.690925	414805.200657	40.064551
3184.696810	415456.776849	40.069568
3187.854310	416132.820381	40.074586
3191.064103	416759.246310	40.079604
3194.482758	417440.742408	40.084621
3197.723127	418072.557877	40.089639
3200.829135	418761.902186	40.094656
3204.491272	419387.362834	40.099674
3207.314818	420087.716856	40.104692
3210.908231	420712.196147	40.109709
3213.939053	421407.442202	40.114727
3217.190294	422077.552569	40.119744
3220.729065	422736.326645	40.124762
3223.888547	423422.760884	40.129780
3227.020957	424095.121344	40.134797
3230.089590	424765.093952	40.139815
3233.318715	425459.978478	40.144832
3236.930150	426137.406221	40.149850
3239.918434	426809.646375	40.154868
3243.369962	427508.749542	40.159885
3246.837320	428172.722915	40.164903
3249.848662	428881.333638	40.169920
3253.744179	429560.909539	40.174938
3256.825006	430236.062863	40.179956
3260.280718	430923.297270	40.184973
3263.471541	431600.272391	40.189991
3266.974270	432284.981382	40.195008
3270.074448	432969.634654	40.200026
3273.798895	433656.425048	40.205044
3277.184557	434313.696119	40.210061
3280.438637	435019.189116	40.215079
3283.425176	435678.184937	40.220096
3287.324549	436369.888825	40.225114
3290.877441	437043.067161	40.230132
3293.614366	437719.040638	40.235149
3297.043057	438377.895974	40.240167
3299.699353	439017.409897	40.245184
3303.726077	439654.462493	40.250202
3306.310089	440302.639422	40.255220
3309.863631	440919.807977	40.260237
3312.792953	441555.491189	40.265255
3315.973372	442205.802185	40.270272
3319.323015	442830.296777	40.275290
3322.499201	443500.472660	40.280308
3325.366420	444140.300563	40.285325
3328.787262	444799.870526	40.290343
3331.563405	445480.585401	40.295360
3335.156535	446136.243594	40.300378
3338.209295	446809.434730	40.305396
3341.378985	447519.745776	40.310413
3344.746424	448199.377989	40.315431
3347.482699	448887.695811	40.320448
3351.235195	449614.151150	40.325466
3354.399563	450292.236141	40.330484
3357.700012	451034.359344	40.335501
3360.892329	451740.084293	40.340519
3363.934571	452474.204976	40.345536
3367.565888	453201.629596	40.350554
3370.967116	453940.505113	40.355572
3374.542029	454702.203784	40.360589
3378.092464	455439.589867	40.365607
3381.465490	456165.745730	40.370624
3385.130954	456943.395896	40.375642
3388.291142	457665.640390	40.380660
3392.111738	458409.615898	40.385677
3395.448236	459174.134944	40.390695
3398.578703	459901.624011	40.395712
3402.133338	460675.214306	40.400730
3405.765197	461416.790759	40.405748
3409.763548	462163.747821	40.410765
3413.375867	462932.139260	40.415783
3416.505869	463655.405454	40.420800
3420.368531	464425.626437	40.425818
3423.646476	465198.390781	40.430836
3426.742641	465929.982459	40.435853
3430.183493	466679.298617	40.440871
3433.976713	467449.825937	40.445888
3437.664741	468188.225835	40.450906
3441.173305	468954.848710	40.455924
3444.414175	469728.110833	40.460941
3447.974610	470476.160115	40.465959
3451.091268	471246.199499	40.470976
3455.031795	471976.839965	40.475994
3458.429255	472749.155544	40.481012
3461.465800	473529.740921	40.486029
3465.484592	474252.956290	40.491047
3468.956055	475044.993503	40.496064
3472.495096	475765.601769	40.501082
3476.216703	476552.383568	40.506100
3479.866949	477296.579592	40.511117
3483.412164	478030.264645	40.516122
3486.616327	478721.038859	40.521127
3489.577456	479375.491522	40.526132
3493.200139	479934.799953	40.531136
3495.786152	480502.263070	40.536141
3498.352364	480952.302114	40.541146
3501.386333	481341.753686	40.546151
3503.791850	481733.475753	40.551156
3505.757880	482053.560161	40.556160
3507.724451	482300.370085	40.561165
3509.770018	482498.774789	40.566170
3511.058325	482665.020794	40.571175
3512.744369	482768.322243	40.576180
3514.020916	482847.772157	40.581184
3514.995297	482900.871094	40.586189
3516.142026	482919.183932	40.591194
3517.091544	482892.078067	40.596199
3517.921477	482816.044883	40.601204
3518.521055	482742.277257	40.606208
3519.355039	482650.028644	40.611213
3519.786487	482561.795452	40.616218
3520.317997	482424.092184	40.621223
3520.536653	482253.501633	40.626228
3521.035751	482106.275207	40.631232
3521.071224	481909.969819	40.636237
3521.754020	481729.673794	40.641242
3521.682097	481526.490179	40.646247
3521.926253	481320.416825	40.651252
3521.776003	481097.833445	40.656256
3521.393087	480896.770089	40.661261
3521.902623	480626.544882	40.666266
3521.599294	480426.578993	40.671271
3521.454697	480182.194057	40.676276
3521.848927	479917.703745	40.681280
3521.547753	479711.953173	40.686285
3521.493867	479425.330586	40.691290
3521.292963	479224.018743	40.696295
3521.424455	478937.714567	40.701300
3520.900324	478728.694915	40.706304
3520.103482	478466.958197	40.711309
3520.575744	478207.804898	40.716314
3520.006621	478022.199474	40.721319
3519.602376	477739.358420	40.726324
3519.270586	477527.052137	40.731328
3519.143460	477289.623117	40.736333
3518.996952	477049.406745	40.741338
3518.505222	476846.799136	40.746343
3518.308610	476608.105938	40.751348
3518.154255	476393.022640	40.756352
3517.301006	476200.400000	40.761357
3517.505268	475960.824800	40.766362
3517.346393	475750.702645	40.771367
3516.896842	475569.313377	40.776372
3516.931878	475328.287496	40.781376
3516.517451	475168.076684	40.786381
3516.120886	474942.979926	40.791386
3515.785167	474792.131173	40.796391
3515.660881	474560.498894	40.801396
3515.512423	474420.972343	40.806400
3514.896866	474225.708149	40.811405
3515.175895	474011.544895	40.816410
3514.843757	473857.799246	40.821415
3514.516530	473719.309984	40.826420
3513.969149	473572.693099	40.831424
3514.237037	473381.083120	40.836429
3513.733780	473211.746235	40.841434
3513.160434	473052.152227	40.846439
3513.707019	472873.268265	40.851444
3513.297644	472724.342255	40.856448
3513.095751	472629.220291	40.861453
3512.764926	472480.432181	40.866458
3512.432332	472314.153317	40.871463
3512.574208	472151.448223	40.876468
3512.190476	472036.175260	40.881472
3511.935995	471944.455089	40.886477
3511.648908	471794.337000	40.891482
3511.276317	471654.624257	40.896487
3511.719294	471517.975602	40.901492
3511.555033	471454.730974	40.906496
3511.019699	471317.627255	40.911501
3510.976572	471189.367734	40.916506
3510.587123	471084.027226	40.921511
3511.067397	470948.230791	40.926516
3510.476787	470884.798315	40.931520
3510.553431	470724.475157	40.936525
3510.622704	470640.252246	40.941530
3510.113705	470533.863146	40.946535
3510.359126	470421.675836	40.951540
3510.010760	470321.547081	40.956544
3509.983797	470236.881442	40.961549
3509.384141	470125.383815	40.966554
3509.066776	470071.589536	40.971559
3509.125203	469952.736716	40.976564
3508.837848	469884.994341	40.981568
3508.972043	469789.400587	40.986573
3509.158312	469723.965807	40.991578
3508.753046	469638.191389	40.996583
3508.768208	469554.631767	41.001588
3508.864000	469503.356533	41.006592
3508.746789	469406.026177	41.011597
3508.694207	469337.484376	41.016602
3508.202431	469250.403764	41.021607
3508.689237	469192.322459	41.026612
3508.248332	469103.813507	41.031616
3508.532934	469062.749433	41.036621
3508.295973	468969.086622	41.041626
3507.748080	468927.951055	41.046631
3508.114709	468833.837308	41.051636
3508.048878	468798.608366	41.056640
3507.651055	468709.127558	41.061645
3507.546682	468658.541051	41.066650
3507.587451	468601.745520	41.071655
3507.534977	468531.781336	41.076660
3507.569979	468500.744452	41.081664
3507.626113	468406.170818	41.086669
3507.478069	468378.255695	41.091674
3507.471380	468304.480631	41.096679
3507.043541	468269.308022	41.101684
3507.370006	468189.395245	41.106688
3507.337251	468158.267155	41.111693
3506.953969	468095.300483	41.116698
3507.257254	468027.813681	41.121703
3507.171266	467965.763044	41.126708
3506.991349	467956.512250	41.131712
3506.670651	467916.606441	41.136717
3506.906075	467859.271074	41.141722
3506.650915	467844.251594	41.146727
3506.599741	467806.990417	41.151732
3506.735660	467751.648040	41.156736
3506.311014	467704.710034	41.161741
3506.483754	467671.114817	41.166746
3506.274093	467648.938339	41.171751
3505.950664	467600.564309	41.176756
3506.210486	467552.909291	41.181760
3506.346542	467482.861115	41.186765
3506.375687	467484.022769	41.191770
3505.978834	467433.428840	41.196775
3506.168658	467397.903607	41.201780
3506.183479	467397.444889	41.206784
3505.932543	467347.030519	41.211789
3505.484394	467306.078840	41.216794
3505.836543	467271.085520	41.221799
3506.159779	467218.754607	41.226804
3505.877300	467247.652044	41.231808
3505.826832	467222.559607	41.236813
3506.104044	467171.250009	41.241818
3505.234133	467137.058129	41.246823
3505.525723	467104.305263	41.251828
3506.192163	467058.968147	41.256832
3505.760158	467036.420503	41.261837
3506.341153	467003.925989	41.266842
3505.868158	467026.464575	41.271847
3505.670237	466989.022316	41.276852
3505.610342	466961.192801	41.281856
3505.396401	466931.004293	41.286861
3505.806270	466905.635883	41.291866
3505.402763	466859.453286	41.296871
3505.737023	466809.959313	41.301876
3505.543679	466827.991523	41.306880
3505.385894	466816.099868	41.311885
3505.281651	466763.429729	41.316890
3505.625444	466724.075851	41.321895
3505.353389	466728.986920	41.326900
3505.440206	466711.478542	41.331904
3505.221295	466670.540106	41.336909
3505.441923	466667.766926	41.341914
3505.302833	466673.569758	41.346919
3505.029414	466637.051577	41.351924
3505.278308	466596.495439	41.356928
3505.417448	466552.660452	41.361933
3505.646811	466583.303433	41.366938
3505.006101	466550.443529	41.371943
3505.467390	466549.914223	41.376948
3505.497145	466502.242497	41.381952
3505.341587	466468.697265	41.386957
3505.312518	466481.784958	41.391962
3504.868889	466439.664564	41.396967
3505.030682	466445.977707	41.401972
3504.923382	466414.960251	41.406976
3505.421237	466400.632076	41.411981
3505.248796	466405.273926	41.416986
3504.571544	466371.050352	41.421991
3505.452605	466347.229515	41.426996
3505.242732	466324.747422	41.432000
3505.326131	466322.502989	41.437005
3504.870265	466295.140869	41.442010
3505.086942	466289.528497	41.447015
3504.814979	466287.999463	41.452020
3504.656242	466259.271867	41.457024
3504.484139	466244.491671	41.462029
3504.901887	466221.048189	41.467034
3505.161816	466194.029190	41.472039
3504.905342	466221.351891	41.477044
3504.982771	466208.611351	41.482048
3504.654626	466173.064518	41.487053
3504.926363	466139.501936	41.492058
3504.951853	466175.198071	41.497063
3505.050442	466174.523246	41.502068
3505.339901	466123.564153	41.507072
3505.034419	466112.303976	41.512077
3505.151513	466121.413362	41.517082
3504.729881	466081.266491	41.522087
3505.505700	466026.528412	41.527092
3505.355272	466010.426148	41.532096
3504.665237	466017.634724	41.537101
3504.788688	466036.023218	41.542106
3505.036945	466032.992035	41.547111
3504.623876	466004.456428	41.552116
3505.270132	465956.280344	41.557120
3504.946853	465937.314822	41.562125
3504.771222	465968.225549	41.567130
3504.788198	465956.305789	41.572135
3504.214749	465933.120086	41.577140
3504.850437	465916.082116	41.582144
3504.885705	465885.903441	41.587149
3504.905666	465885.849568	41.592154
3504.119202	465897.333160	41.597159
3504.194548	465871.357149	41.602164
3504.361034	465859.210858	41.607168
3504.709688	465855.352402	41.612173
3504.910049	465869.418432	41.617178
3504.822343	465864.817572	41.622183
3504.490082	465835.508297	41.627188
3504.829041	465824.906773	41.632192
3504.260129	465826.365895	41.637197
3505.068704	465797.636911	41.642202
3505.051708	465772.892448	41.647207
3505.160348	465799.853710	41.652212
3505.240304	465801.565249	41.657216
3504.779048	465764.720279	41.662221
3505.025820	465735.572899	41.667226
3505.354528	465706.463240	41.672231
3504.825513	465720.593945	41.677236
3505.032611	465726.342314	41.682240
3504.916237	465714.747766	41.687245
3504.908429	465703.186762	41.692250
3505.061307	465666.903800	41.697255
3504.666595	465643.334546	41.702260
3504.973644	465633.802917	41.707264
3504.728225	465633.030314	41.712269
3504.995300	465609.052147	41.717274
3504.665916	465598.708288	41.722279
3504.572775	465582.799491	41.727284
3504.781732	465576.275339	41.732288
3504.133404	465562.533470	41.737293
3504.838639	465533.414771	41.742298
3505.197662	465520.781446	41.747303
3505.010210	465538.712392	41.752308
3505.223717	465539.794300	41.757312
3504.841584	465517.338581	41.762317
3505.177329	465507.193815	41.767322
3504.930963	465505.964950	41.772327
3504.202914	465459.830608	41.777332
3505.085476	465433.726472	41.782336
3504.710917	465442.660302	41.787341
3504.911482	465450.742538	41.792346
3504.685901	465432.521805	41.797351
3504.824663	465423.929502	41.802356
3504.949457	465398.046524	41.807360
3504.475328	465391.427438	41.812365
3504.693666	465368.166677	41.817370
3505.180082	465332.083987	41.822375
3504.747526	465321.097038	41.827380
3505.111044	465303.543766	41.832384
3504.855959	465347.044649	41.837389
3504.732856	465336.820193	41.842394
3504.844412	465308.302152	41.847399
3504.881135	465289.786273	41.852404
3504.865592	465259.056905	41.857408
3504.430050	465259.531443	41.862413
3504.426699	465244.368891	41.867418
3504.784697	465233.916203	41.872423
3504.638742	465214.820582	41.877428
3504.800082	465253.336700	41.882432
3504.542208	465227.311150	41.887437
3504.455670	465181.226944	41.892442
3505.065186	465148.370105	41.897447
3504.995376	465142.498439	41.902452
3505.110755	465124.578539	41.907456
3504.662908	465135.501884	41.912461
3504.884283	465110.161133	41.917466
3505.040969	465088.279063	41.922471
3504.911544	465127.348497	41.927476
3505.238221	465120.856312	41.932480
3505.064431	465108.002686	41.937485
3504.947660	465086.924532	41.942490
3504.668829	465070.588288	41.947495
3504.656490	465033.113252	41.952500
3504.744351	465039.235646	41.957504
3504.517734	465040.235009	41.962509
3504.866157	465026.639519	41.967514
3504.988825	465013.434698	41.972519
3504.550720	465022.835165	41.977524
3504.617384	464972.821379	41.982528
3504.367984	464982.496315	41.987533
3504.487204	464978.927535	41.992538
3504.678363	464964.697592	41.997543
3504.579571	464951.679877	42.002548
3505.048201	464945.063774	42.007552
3504.701424	464935.229475	42.012557
3504.697876	464897.042823	42.017562
3504.706955	464878.175964	42.022567
3504.734011	464895.109986	42.027572
3504.826955	464894.791007	42.032576
3504.496442	464852.751020	42.037581
3505.019780	464836.997793	42.042586
3504.612080	464869.671054	42.047591
3504.587474	464832.501886	42.052596
3504.286142	464820.631805	42.057600
3504.247981	464826.064190	42.062605
3504.405585	464803.420979	42.067610
3504.856131	464790.164193	42.072615
3504.706296	464807.836237	42.077620
3504.558697	464801.317495	42.082624
3504.287250	464768.751465	42.087629
3504.623089	464755.309934	42.092634
3504.316408	464767.935422	42.097639
3504.613125	464765.859963	42.102644
3504.961414	464752.467177	42.107648
3504.393133	464727.757929	42.112653
3504.888339	464704.199114	42.117658
3504.141353	464698.738647	42.122663
3504.039702	464707.071792	42.127668
3504.707207	464704.227724	42.132672
3504.378353	464717.668168	42.137677
3504.844096	464676.972679	42.142682
3504.479087	464646.855524	42.147687
3504.094746	464668.723302	42.152692
3504.448032	464658.473935	42.157696
3504.484672	464684.839416	42.162701
3504.670074	464679.332994	42.167706
3504.557298	464671.743715	42.172711
3504.600938	464668.592542	42.177716
3504.682183	464658.893315	42.182720
3504.300112	464656.519427	42.187725
3504.576749	464611.745868	42.192730
3504.878997	464622.094482	42.197735
3504.279099	464596.122227	42.202740
3504.968190	464553.007632	42.207744
3504.796168	464562.061956	42.212749
3504.510970	464575.546303	42.217754
3504.467176	464537.821801	42.222759
3504.705459	464526.576263	42.227764
3504.803231	464552.982957	42.232768
3504.749730	464534.379258	42.237773
3504.410036	464504.359330	42.242778
3504.837390	464479.593849	42.247783
3504.311160	464470.599132	42.252788
3504.635853	464496.107882	42.257792
3504.655365	464491.692637	42.262797
3504.465866	464491.925440	42.267802
3504.305048	464468.875778	42.272807
3503.958875	464449.303977	42.277812
3504.850066	464424.617259	42.282816
3504.338888	464423.075185	42.287821
3504.474847	464416.207217	42.292826
3504.258308	464428.412939	42.297831
3504.018942	464429.820061	42.302836
3504.878462	464395.756119	42.307840
3504.584221	464419.790638	42.312845
3504.390261	464433.717083	42.317850
3504.431251	464418.191936	42.322855
3504.476426	464409.563305	42.327860
3504.661594	464413.236196	42.332864
3504.376175	464418.859910	42.337869
3504.611583	464397.471838	42.342874
3504.477767	464368.179896	42.347879
3504.183031	464355.142076	42.352884
3504.944944	464332.808566	42.357888
3504.398822	464378.538153	42.362893
3504.208520	464375.576059	42.367898
3504.347582	464348.878123	42.372903
3504.394028	464338.322102	42.377908
3504.239381	464325.464980	42.382912
3504.694817	464290.298302	42.387917
3504.970628	464266.317253	42.392922
3505.233098	464267.594347	42.397927
3504.722460	464259.560660	42.402932
3505.228465	464236.658922	42.407936
3504.708854	464233.393855	42.412941
3504.829716	464258.225096	42.417946
3504.771251	464240.839087	42.422951
3504.395788	464215.845195	42.427956
3504.765550	464210.258797	42.432960
3504.263995	464199.180746	42.437965
3504.084707	464175.119385	42.442970
3504.766452	464151.327620	42.447975
3504.589742	464136.597408	42.452980
3504.456870	464139.914895	42.457984
3504.384725	464176.035523	42.462989
3504.219331	464166.222914	42.467994
3504.087275	464133.633886	42.472999
3504.601638	464100.587626	42.478004
3504.634648	464127.410803	42.483008
3504.222506	464146.646311	42.488013
3503.957743	464116.563280	42.493018
3504.822929	464080.215756	42.498023
3504.703270	464070.446589	42.503028
3504.742104	464061.970967	42.508032
3504.408740	464070.898853	42.513037
3504.485926	464074.284579	42.518042
3504.493985	464101.720317	42.523047
3503.771077	464080.584836	42.528052
3504.449928	464064.958610	42.533056
3504.857295	464048.411691	42.538061
3504.811351	464029.704929	42.543066
3504.636564	464025.928886	42.548071
3504.168183	464040.862557	42.553076
3504.496846	464018.749351	42.558080
3504.718720	464020.387886	42.563085
3504.420445	464001.365976	42.568090
3504.824774	463960.425261	42.573095
3504.728696	463987.421164	42.578100
3504.481711	463983.352232	42.583104
3504.075785	463973.628270	42.588109
3504.464351	463946.484672	42.593114
3504.536087	463920.304003	42.598119
3504.483318	463978.128240	42.603124
3504.470832	463949.070127	42.608128
3504.529522	463926.898069	42.613133
3504.685771	463959.889297	42.618138
3504.563305	463935.463677	42.623143
3504.825977	463895.458113	42.628148
3505.004189	463858.610212	42.633152
3504.702204	463857.187176	42.638157
3504.725063	463856.524249	42.643162
3504.750683	463856.723056	42.648167
3504.387625	463875.342456	42.653172
3504.413013	463856.979280	42.658176
3504.398452	463822.241140	42.663181
3504.424665	463819.650473	42.668186
3504.559868	463836.618952	42.673191
3503.616958	463818.510230	42.678196
3503.947926	463820.638696	42.683200
3503.395656	463824.631116	42.688205
3503.886410	463815.373941	42.693210
3504.409696	463799.062088	42.698215
3504.127856	463800.526679	42.703220
3504.162563	463809.650074	42.708224
3504.061183	463866.112963	42.713229
3504.187756	463831.859689	42.718234
3503.845248	463807.367272	42.723239
3503.981312	463799.079042	42.728244
3504.310487	463795.730460	42.733248
3503.666486	463801.918175	42.738253
3504.108913	463809.151345	42.743258
3504.369233	463797.293351	42.748263
3504.242957	463812.680266	42.753268
3504.837505	463784.844597	42.758272
3504.942497	463780.770707	42.763277
3504.609137	463775.193905	42.768282
3503.823398	463777.397456	42.773287
3503.809455	463782.065535	42.778292
3504.450283	463764.162877	42.783296
3504.750606	463750.320605	42.788301
3504.732296	463725.675418	42.793306
3504.837822	463711.965344	42.798311
3504.496208	463701.876080	42.803316
3504.783424	463734.999100	42.808321
3504.623722	463743.037496	42.813325
3504.776366	463711.518584	42.818330
3504.602117	463648.302846	42.823335
3504.361947	463637.690352	42.828340
3504.551361	463636.189629	42.833345
3504.551672	463661.497062	42.838349
3504.442426	463658.014892	42.843354
3504.551478	463649.680158	42.848359
3504.348827	463642.104721	42.853364
3504.360754	463632.162406	42.858369
3504.452998	463591.929636	42.863373
3504.470434	463586.246619	42.868378
3504.765673	463592.083065	42.873383
3504.747105	463574.132328	42.878388
3505.274994	463551.479987	42.883393
3505.118075	463549.628268	42.888397
3504.811689	463523.354736	42.893402
3505.015699	463504.151558	42.898407
3504.648207	463524.445613	42.903412
3504.475620	463497.795883	42.908417
3504.730870	463475.338708	42.913421
3504.647720	463499.138019	42.918426
3504.241674	463454.926414	42.923431
3504.717402	463431.876457	42.928436
3504.982219	463419.510377	42.933441
3504.575017	463443.868140	42.938445
3504.277807	463474.294509	42.943450
3504.370305	463446.284177	42.948455
3504.392734	463418.538470	42.953460
3504.269092	463383.918300	42.958465
3504.060829	463413.214921	42.963469
3504.077452	463428.934540	42.968474
3504.048549	463402.059113	42.973479
3503.627040	463407.755317	42.978484
3504.788529	463379.474494	42.983489
3504.419967	463423.453660	42.988493
3504.080401	463395.765142	42.993498
3504.376393	463355.702594	42.998503
3504.170234	463378.659290	43.003508
3504.190976	463410.201985	43.008513
3504.330879	463389.791631	43.013517
3504.193459	463381.090016	43.018522
3504.635705	463361.494036	43.023527
3503.997428	463385.482653	43.028532
3504.405687	463334.802459	43.033537
3504.161478	463354.265712	43.038541
3504.021050	463348.861171	43.043546
3504.324183	463321.933161	43.048551
3503.987766	463373.312055	43.053556
3504.137312	463373.592712	43.058561
3504.102589	463367.512146	43.063565
3504.274965	463333.200123	43.068570
3504.139914	463354.319789	43.073575
3503.738132	463323.192248	43.078580
3504.352215	463313.661779	43.083585
3504.409706	463340.583501	43.088589
3503.799642	463324.349000	43.093594
3504.678518	463311.378624	43.098599
3504.302453	463363.575283	43.103604
3504.262195	463311.038679	43.108609
3504.438920	463280.225372	43.113613
3504.186336	463295.987640	43.118618
3504.407593	463333.229800	43.123623
3503.921541	463316.316368	43.128628
3504.422209	463286.364775	43.133633
3504.600231	463282.583551	43.138637
3504.571970	463306.425116	43.143642
3504.583680	463269.703962	43.148647
3504.769057	463230.825165	43.153652
3504.557373	463262.151227	43.158657
3504.044424	463232.410495	43.163661
3504.273130	463209.196477	43.168666
3504.629242	463248.243296	43.173671
3504.200256	463232.487277	43.178676
3504.400793	463198.373459	43.183681
3504.739946	463219.621171	43.188685
3504.140354	463188.778290	43.193690
3504.507933	463170.106854	43.198695
3504.473349	463175.792676	43.203700
3504.565571	463190.435452	43.208705
3503.868545	463169.802157	43.213709
3504.150004	463166.258151	43.218714
3504.193696	463162.396704	43.223719
3504.339081	463162.678022	43.228724
3504.642841	463128.497061	43.233729
3504.767842	463109.863916	43.238733
3504.889032	463104.570114	43.243738
3504.471166	463110.417973	43.248743
3504.434190	463097.034340	43.253748
3504.616697	463073.218867	43.258753
3504.293895	463080.015345	43.263757
3504.401598	463089.482531	43.268762
3504.503470	463064.919028	43.273767
3503.662815	463070.275831	43.278772
3504.350243	463065.602565	43.283777
3504.639387	463040.958717	43.288781
3504.039257	463043.082283	43.293786
3504.421165	463042.413295	43.298791
3504.123452	463042.713936	43.303796
3504.830088	463011.461461	43.308801
3504.607567	463025.799072	43.313805
3504.632717	463009.058185	43.318810
3504.405557	462978.105416	43.323815
3504.044705	463025.532995	43.328820
3504.397171	463024.716507	43.333825
3504.328942	463024.017235	43.338829
3504.190231	463022.314745	43.343834
3504.268429	462995.168293	43.348839
3504.267567	462969.302254	43.353844
3504.650498	462975.277161	43.358849
3504.441771	463004.016512	43.363853
3504.239036	463014.851466	43.368858
3504.414292	462976.176682	43.373863
3504.058514	462966.748645	43.378868
3503.638689	462945.310549	43.383873
3504.302528	462937.293593	43.388877
3504.901418	462909.811141	43.393882
3504.776921	462952.129705	43.398887
3504.444137	462948.834908	43.403892
3504.563237	462919.602456	43.408897
3504.536888	462926.047815	43.413901
3504.442885	462896.950453	43.418906
3504.754216	462867.687545	43.423911
3504.259083	462897.943137	43.428916
3504.070442	462887.423564	43.433921
3504.028775	462869.171584	43.438925
3504.545522	462847.636070	43.443930
3504.459673	462840.853381	43.448935
3504.263156	462871.264682	43.453940
3504.437236	462866.520362	43.458945
3504.237849	462859.045569	43.463949
3504.110894	462860.333586	43.468954
3504.541923	462848.904554	43.473959
3504.049320	462830.571664	43.478964
3504.186258	462806.458791	43.483969
3504.418925	462832.085497	43.488973
3504.353063	462812.670772	43.493978
3504.769640	462811.793424	43.498983
3504.044555	462817.284175	43.503988
3503.876987	462793.117982	43.508993
3503.680867	462780.063619	43.513997
3503.642046	462788.387572	43.519002
3504.140178	462812.704379	43.524007
3503.944718	462823.233969	43.529012
3504.274738	462802.843729	43.534017
3504.465887	462755.848222	43.539021
3504.118417	462754.635175	43.544026
3504.374868	462771.331734	43.549031
3504.065672	462766.968093	43.554036
3504.577011	462754.258355	43.559041
3504.362415	462754.698016	43.564045
3503.555924	462770.700376	43.569050
3504.495971	462741.946542	43.574055
3504.505468	462753.965325	43.579060
3504.146663	462770.556261	43.584065
3503.605256	462767.548004	43.589069
3503.943028	462756.843724	43.594074
3504.768534	462724.506958	43.599079
3504.230152	462770.492317	43.604084
3504.084388	462746.069033	43.609089
3503.667480	462741.012353	43.614093
3503.988140	462717.783274	43.619098
3504.239961	462704.303031	43.624103
3504.375981	462707.426078	43.629108
3504.285408	462739.950999	43.634113
3504.268189	462770.384819	43.639117
3503.997953	462758.052216	43.644122
3504.209968	462729.869910	43.649127
3503.916996	462709.121589	43.654132
3504.619518	462674.014664	43.659137
3504.024243	462730.558587	43.664141
3504.054558	462721.120133	43.669146
3504.119772	462721.211255	43.674151
3504.527218	462691.932918	43.679156
3504.292851	462670.008767	43.684161
3504.301918	462659.356396	43.689165
3504.116764	462668.768619	43.694170
3504.301710	462646.930322	43.699175
3504.190184	462670.227842	43.704180
3504.093130	462673.489173	43.709185
3504.285929	462714.135051	43.714189
3503.924479	462712.670618	43.719194
3504.144094	462717.099135	43.724199
3504.084564	462691.242037	43.729204
3503.945978	462660.984875	43.734209
3503.779319	462656.243650	43.739213
3503.804426	462659.739268	43.744218
3504.154782	462653.293320	43.749223
3503.755402	462660.761377	43.754228
3503.845227	462657.602610	43.759233
3503.780953	462654.062451	43.764237
3504.323477	462642.007062	43.769242
3504.590521	462625.633394	43.774247
3504.443566	462643.357473	43.779252
3504.007919	462686.232927	43.784257
3503.977181	462682.941065	43.789261
3503.805820	462697.930149	43.794266
3504.236427	462683.356541	43.799271
3504.202642	462640.555269	43.804276
3504.449259	462656.391252	43.809281
3504.611354	462656.568498	43.814285
3503.982683	462640.792891	43.819290
3503.698545	462643.221579	43.824295
3504.012002	462636.578584	43.829300
3504.254090	462644.148128	43.834305
3504.124563	462656.899002	43.839309
3504.199127	462657.952302	43.844314
3504.457289	462635.493795	43.849319
3504.127170	462645.182537	43.854324
3503.983974	462614.976758	43.859329
3504.140133	462591.367796	43.864333
3504.144613	462618.552390	43.869338
3504.179377	462630.110778	43.874343
3504.437659	462593.603096	43.879348
3504.541583	462611.946892	43.884353
3504.163710	462618.346468	43.889357
3503.687824	462594.228787	43.894362
3503.690482	462583.830986	43.899367
3503.549568	462588.620830	43.904372
3504.080838	462590.464165	43.909377
3504.316268	462606.859861	43.914381
3504.326492	462611.473653	43.919386
3504.292071	462604.936355	43.924391
3504.075825	462575.097099	43.929396
3504.622612	462562.888837	43.934401
3504.751353	462541.110036	43.939405
3504.460695	462542.068914	43.944410
3504.436312	462548.057603	43.949415
3504.547525	462526.991625	43.954420
3504.807080	462510.619053	43.959425
3503.991979	462532.100608	43.964429
3504.467882	462559.210761	43.969434
3504.290877	462552.493108	43.974439
3504.355365	462493.800966	43.979444
3504.618640	462474.942542	43.984449
3504.752714	462477.863054	43.989453
3504.575862	462479.108261	43.994458
3504.689524	462448.658774	43.999463
3504.392840	462498.461166	44.004468
3504.273322	462478.395274	44.009473
3503.820320	462471.924099	44.014477
3503.806024	462464.521351	44.019482
3504.360485	462451.398867	44.024487
3503.709132	462479.448089	44.029492
3504.122387	462484.860428	44.034497
3504.223595	462468.867888	44.039501
3504.168427	462420.642609	44.044506
3504.455007	462409.337618	44.049511
3504.313800	462438.523519	44.054516
3504.105571	462436.882691	44.059521
3504.272926	462427.828202	44.064525
3503.792578	462435.055538	44.069530
3503.916780	462438.434089	44.074535
3504.165176	462445.901267	44.079540
3503.802034	462407.919202	44.084545
3503.980561	462397.696390	44.089549
3503.704209	462405.347966	44.094554
3504.412201	462411.119491	44.099559
3504.563999	462427.528541	44.104564
3504.705256	462383.633989	44.109569
3504.274583	462413.930784	44.114573
3504.842987	462411.203528	44.119578
3504.556638	462372.854229	44.124583
3504.211875	462382.038208	44.129588
3504.679319	462362.082308	44.134593
3505.259848	462330.899507	44.139597
3504.437992	462368.916841	44.144602
3504.390041	462340.014330	44.149607
3504.498753	462302.566131	44.154612
3504.391378	462271.035503	44.159617
3504.597281	462310.107757	44.164621
3504.503130	462302.666857	44.169626
3504.887802	462253.052974	44.174631
3504.422326	462244.047717	44.179636
3504.316018	462225.399655	44.184641
3504.653155	462220.071504	44.189645
3504.414761	462228.832976	44.194650
3503.641970	462219.622687	44.199655
3503.979115	462216.171164	44.204660
3504.340308	462209.064016	44.209665
3504.360508	462207.387063	44.214669
3503.960081	462218.963739	44.219674
3504.555544	462230.078674	44.224679
3504.144327	462251.699544	44.229684
3504.111819	462214.527114	44.234689
3504.233319	462193.002707	44.239693
3503.671228	462184.773495	44.244698
3503.600183	462180.777850	44.249703
3503.668787	462182.034995	44.254708
3503.659379	462171.638904	44.259713
3503.944915	462194.062656	44.264717
3503.841079	462208.229887	44.269722
3503.798270	462192.969985	44.274727
3503.622514	462217.140381	44.279732
3503.458199	462235.324016	44.284737
3504.021372	462219.714749	44.289741
3504.317297	462237.115557	44.294746
3504.269173	462258.273270	44.299751
3504.234159	462228.049853	44.304756
3504.076099	462198.302321	44.309761
3504.447522	462183.889894	44.314765
3504.305565	462178.282422	44.319770
3504.431397	462217.012462	44.324775
3503.820935	462201.385815	44.329780
3503.702451	462189.840418	44.334785
3504.198248	462201.934798	44.339789
3503.720407	462193.387953	44.344794
3504.232217	462161.049216	44.349799
3504.469398	462172.271533	44.354804
3504.263956	462208.010759	44.359809
3504.222078	462210.249042	44.364813
3504.288345	462209.376324	44.369818
3504.671314	462169.906475	44.374823
3504.485963	462178.355263	44.379828
3504.182991	462165.824618	44.384833
3504.791999	462120.486162	44.389837
3504.184223	462124.741262	44.394842
3504.150992	462133.419623	44.399847
3503.933356	462146.032564	44.404852
3503.704452	462114.571638	44.409857
3503.674068	462110.113073	44.414861
3504.284819	462100.582602	44.419866
3504.334035	462088.351283	44.424871
3504.052106	462135.971210	44.429876
3503.885762	462140.207252	44.434881
3504.130667	462102.534301	44.439885
3504.164818	462095.478810	44.444890
3504.395040	462138.047214	44.449895
3504.202062	462152.380731	44.454900
3504.055849	462097.119055	44.459905
3504.433699	462103.855808	44.464909
3503.979636	462087.646437	44.469914
3504.383556	462075.054723	44.474919
3504.158176	462101.921257	44.479924
3504.043207	462080.636997	44.484929
3504.571168	462068.583594	44.489933
3504.098257	462102.995828	44.494938
3504.079021	462050.757165	44.499943
3503.889945	462089.435767	44.504948
3504.129183	462049.633378	44.509953
3504.819111	462021.628213	44.514957
3504.289353	462027.443327	44.519962
3504.488770	462073.820740	44.524967
3504.122793	462072.914900	44.529972
3504.040919	462053.806347	44.534977
3504.371150	462008.511723	44.539981
3504.371474	462016.779065	44.544986
3503.973773	462046.918999	44.549991
3504.171306	462063.371815	44.554996
3503.984536	462038.041253	44.560001
3504.444604	462005.304702	44.565005
3504.241249	461986.823935	44.570010
3504.256093	461975.612392	44.575015
3504.191445	462004.786774	44.580020
3503.917197	462032.574081	44.585025
3504.077115	462005.159873	44.590029
3504.185329	461993.679979	44.595034
3504.086836	462025.598578	44.600039
3504.017837	462004.002656	44.605044
3503.935575	462034.650669	44.610049
3503.888738	462023.601061	44.615053
3503.717594	462012.418935	44.620058
3503.835186	462025.181838	44.625063
3504.171834	462003.572517	44.630068
3503.739833	462028.950192	44.635073
3503.782646	461993.642126	44.640077
3504.057624	461965.245995	44.645082
3504.240718	461957.558272	44.650087
3503.800678	461956.664133	44.655092
3503.904951	461988.347855	44.660097
3503.882711	461960.201579	44.665101
3503.692240	461963.173460	44.670106
3503.935637	461949.846242	44.675111
3503.961180	461957.095212	44.680116
3503.922214	461994.634408	44.685121
3503.884995	462028.267807	44.690125
3503.729126	461995.831481	44.695130
3504.075612	461973.814813	44.700135
3503.840016	462039.484059	44.705140
3504.040256	461995.731561	44.710145
3504.567872	462004.372043	44.715149
3503.999516	462006.896446	44.720154
3504.315642	461989.905898	44.725159
3504.141761	462015.648550	44.730164
3504.130244	461990.797434	44.735169
3504.035051	461950.895565	44.740173
3504.054380	461977.013487	44.745178
3503.978996	462002.284103	44.750183
3503.981917	462010.398876	44.755188
3503.761010	461985.733012	44.760193
3504.015364	461966.520516	44.765197
3504.309711	461947.859606	44.770202
3504.162187	461975.271913	44.775207
3504.160630	462009.711229	44.780212
3503.984158	462003.449805	44.785217
3503.759419	461992.783343	44.790221
3503.609964	461994.125687	44.795226
3503.871539	461988.555822	44.800231
3504.179636	461982.471399	44.805236
3504.003822	461990.969473	44.810241
3503.774440	461989.230513	44.815245
3504.286446	461979.918479	44.820250
3504.578512	461952.736918	44.825255
3504.336077	461947.449591	44.830260
3504.152134	461958.180660	44.835265
3504.386354	461960.020284	44.840269
3504.202004	461937.326681	44.845274
3504.300352	461916.211424	44.850279
3504.439055	461927.246552	44.855284
3503.786502	461929.378509	44.860289
3503.968792	461949.384252	44.865293
3503.953443	461960.595874	44.870298
3504.374944	461950.993812	44.875303
3504.425667	461936.479752	44.880308
3504.461052	461928.815367	44.885313
3504.474935	461934.189531	44.890317
3504.206990	461919.015744	44.895322
3504.261827	461890.705033	44.900327
3503.765056	461901.384136	44.905332
3503.288456	461899.785687	44.910337
3504.265487	461873.611609	44.915341
3504.197616	461874.890344	44.920346
3504.221996	461894.616774	44.925351
3504.156622	461895.895114	44.930356
3504.175326	461863.075952	44.935361
3504.251654	461872.802231	44.940365
3503.608562	461895.271635	44.945370
3504.164006	461907.762516	44.950375
3504.028276	461905.958026	44.955380
3503.944446	461893.595466	44.960385
3504.178064	461847.808573	44.965389
3503.988162	461841.092739	44.970394
3504.713079	461833.826536	44.975399
3504.866914	461830.758973	44.980404
3504.086948	461826.114508	44.985409
3504.344072	461805.227650	44.990413
3504.344362	461800.307686	44.995418
3504.238896	461801.186602	45.000423
3503.713712	461834.745269	45.005428
3503.477544	461849.593020	45.010433
3504.352123	461848.795403	45.015437
3504.415114	461807.498811	45.020442
3504.485269	461803.886544	45.025447
3504.424046	461785.636744	45.030452
3504.646267	461774.138714	45.035457
3504.711132	461774.128454	45.040461
3504.467616	461808.302009	45.045466
3504.390530	461804.002925	45.050471
3504.416675	461775.037230	45.055476
3504.425126	461747.037989	45.060481
3504.339841	461784.787752	45.065485
3504.194387	461797.085160	45.070490
3503.678282	461771.502019	45.075495
3503.966516	461758.319759	45.080500
3503.911014	461723.838329	45.085505
3504.282737	461748.683522	45.090509
3503.817870	461777.211377	45.095514
3504.056514	461749.023591	45.100519
3504.221292	461717.398421	45.105524
3503.709998	461713.522999	45.110529
3504.184932	461740.837212	45.115533
3504.174495	461760.366383	45.120538
3503.929795	461742.754198	45.125543
3504.420676	461730.148541	45.130548
3504.054813	461760.588163	45.135553
3504.183066	461740.178100	45.140557
3503.522514	461705.893721	45.145562
3504.152781	461697.678736	45.150567
3504.250646	461698.728400	45.155572
3503.970453	461722.915853	45.160577
3504.250998	461679.150026	45.165581
3504.027440	461681.822848	45.170586
3503.977375	461683.859595	45.175591
3504.031900	461680.604825	45.180596
3504.387372	461685.316405	45.185601
3504.711806	461680.953830	45.190605
3504.024412	461684.815832	45.195610
3504.091481	461695.963842	45.200615
3504.487414	461691.691410	45.205620
3504.189661	461659.277009	45.210625
3504.642813	461646.474383	45.215629
3504.685108	461646.619853	45.220634
3503.762432	461649.555350	45.225639
3503.929026	461639.131184	45.230644
3504.196380	461633.002383	45.235649
3504.114955	461640.319088	45.240653
3503.956765	461680.109400	45.245658
3504.348275	461630.848066	45.250663
3504.700438	461626.075328	45.255668
3503.791492	461646.659605	45.260673
3504.016309	461639.421666	45.265677
3503.990573	461646.831008	45.270682
3504.302630	461605.748270	45.275687
3504.425005	461581.636341	45.280692
3503.899932	461599.268875	45.285697
3504.214876	461595.414995	45.290701
3503.833858	461597.757668	45.295706
3504.410614	461590.565525	45.300711
3503.843191	461623.826865	45.305716
3504.124144	461660.758136	45.310721
3503.888531	461647.658612	45.315725
3503.996760	461597.072508	45.320730
3504.181428	461587.000510	45.325735
3504.426653	461579.099948	45.330740
3504.286418	461575.926668	45.335745
3503.816721	461587.818955	45.340749
3503.971272	461624.009449	45.345754
3503.822232	461625.351750	45.350759
3504.373278	461599.751890	45.355764
3504.212670	461566.301249	45.360769
3504.390843	461566.070194	45.365773
3504.594857	461545.597252	45.370778
3504.326401	461542.545677	45.375783
3504.136331	461544.908895	45.380788
3504.319315	461539.909274	45.385793
3504.489033	461535.469683	45.390797
3504.087541	461525.338143	45.395802
3504.394146	461508.906661	45.400807
3504.385311	461505.205387	45.405812
3504.036182	461542.439338	45.410817
3503.971635	461567.049369	45.415821
3504.162950	461563.925123	45.420826
3504.119212	461560.787310	45.425831
3503.959794	461564.616598	45.430836
3503.946517	461560.713150	45.435841
3504.403685	461546.236028	45.440845
3504.105688	461534.363608	45.445850
3504.142274	461517.315436	45.450855
3504.538563	461458.923105	45.455860
3504.399805	461461.075335	45.460865
3504.323297	461457.790521	45.465869
3504.325209	461455.457022	45.470874
3504.122484	461468.169440	45.475879
3503.903623	461487.681079	45.480884
3504.083111	461487.348372	45.485889
3504.100523	461492.417759	45.490893
3504.318123	461492.332635	45.495898
3503.669323	461471.132160	45.500903
3504.072973	461458.945907	45.505908
3504.086804	461442.966425	45.510913
3504.022242	461480.206224	45.515917
3503.897459	461483.877887	45.520922
3503.938248	461477.480526	45.525927
3503.649965	461471.693115	45.530932
3503.798089	461473.495668	45.535937
3504.459013	461439.001988	45.540941
3503.983687	461487.161118	45.545946
3503.663763	461455.561462	45.550951
3504.219863	461435.539980	45.555956
3504.304475	461415.694449	45.560961
3504.279768	461410.829070	45.565965
3504.142373	461413.437584	45.570970
3504.204301	461415.355211	45.575975
3504.080135	461431.960798	45.580980
3503.333062	461453.128330	45.585985
3504.065655	461448.092534	45.590989
3503.919799	461474.237169	45.595994
3503.623109	461473.624679	45.600999
3504.073303	461467.821981	45.606004
3503.801236	461477.806393	45.611009
3503.915251	461468.252722	45.616013
3503.930072	461445.730010	45.621018
3504.454737	461424.800499	45.626023
3504.171976	461437.119813	45.631028
3503.504279	461435.095040	45.636033
3503.688061	461443.384322	45.641037
3503.854377	461449.140284	45.646042
3503.587606	461458.667373	45.651047
3503.898331	461452.379502	45.656052
3503.893227	461452.481745	45.661057
3503.805031	461463.755859	45.666061
3503.779577	461462.542559	45.671066
3503.677215	461465.652745	45.676071
3503.659040	461467.278699	45.681076
3503.889122	461476.017144	45.686081
3503.878599	461469.830777	45.691085
3504.170687	461467.197804	45.696090
3504.147022	461477.142952	45.701095
3504.474276	461496.872590	45.706100
3504.188729	461432.095616	45.711105
3504.057614	461442.209929	45.716109
3503.869233	461460.296570	45.721114
3504.239408	461401.756049	45.726119
3504.334038	461417.160465	45.731124
3504.091819	461434.241206	45.736129
3503.937854	461431.070075	45.741133
3503.880270	461440.716272	45.746138
3503.594627	461436.602245	45.751143
3504.229944	461426.408219	45.756148
3504.172754	461411.505094	45.761153
3504.483208	461402.478282	45.766157
3504.034843	461394.027905	45.771162
3503.884128	461419.970486	45.776167
3504.081411	461427.344651	45.781172
3503.962989	461443.442106	45.786177
3503.989039	461431.011193	45.791181
3503.721804	461422.329310	45.796186
3504.256746	461377.001017	45.801191
3504.242712	461405.762426	45.806196
3503.874683	461428.138110	45.811201
3503.927330	461389.276997	45.816205
3504.136589	461381.026998	45.821210
3504.100408	461386.612097	45.826215
3504.189839	461425.653629	45.831220
3504.164911	461434.990337	45.836225
3504.514239	461374.627061	45.841229
3504.702810	461366.836822	45.846234
3504.529465	461352.053459	45.851239
3504.081051	461373.934686	45.856244
3503.401633	461373.281246	45.861249
3504.357533	461358.319393	45.866253
3504.279834	461375.120566	45.871258
3503.932562	461383.696699	45.876263
3504.078478	461344.719322	45.881268
3503.882871	461332.779886	45.886273
3504.092641	461356.535245	45.891277
3503.999967	461380.896323	45.896282
3503.763283	461369.419895	45.901287
3503.849489	461337.705151	45.906292
3504.114783	461378.189902	45.911297
3504.257585	461352.755727	45.916301
3504.115694	461377.936136	45.921306
3503.919088	461361.837692	45.926311
3504.535812	461335.060541	45.931316
3504.241607	461345.809339	45.936321
3504.294310	461340.272326	45.941325
3504.138107	461303.929442	45.946330
3504.125699	461329.596659	45.951335
3504.267282	461296.554334	45.956340
3503.977217	461338.851487	45.961345
3504.010866	461323.731056	45.966349
3504.059007	461305.565011	45.971354
3503.962635	461356.961450	45.976359
3504.161057	461358.198123	45.981364
3503.934336	461326.583548	45.986369
3503.706907	461297.302246	45.991373
3504.262361	461271.954916	45.996378
3503.656157	461292.745282	46.001383
3504.153592	461320.005745	46.006388
3503.916831	461324.405241	46.011393
3504.233238	461316.442611	46.016397
3503.853594	461312.292698	46.021402
3503.903117	461280.685113	46.026407
3504.473264	461260.813417	46.031412
3504.094526	461289.328295	46.036417
3503.830666	461320.919011	46.041421
3504.093858	461314.790779	46.046426
3504.016046	461291.420278	46.051431
3504.394760	461293.693617	46.056436
3503.925926	461302.390441	46.061441
3504.528087	461266.789897	46.066445
3504.127536	461298.097920	46.071450
3503.590792	461269.119082	46.076455
3504.347246	461252.514858	46.081460
3504.293721	461306.440743	46.086465
3503.827418	461279.783992	46.091469
3503.894741	461272.266494	46.096474
3504.426096	461260.110667	46.101479
3504.878220	461237.518617	46.106484
3504.168359	461214.907326	46.111489
3504.584579	461201.958112	46.116493
3504.592009	461218.999559	46.121498
3504.308107	461194.596367	46.126503
3504.309207	461173.952262	46.131508
3503.949519	461191.254649	46.136513
3504.052303	461215.737182	46.141517
3503.690685	461193.730211	46.146522
3504.046277	461166.740520	46.151527
3504.168317	461147.548218	46.156532
3504.139195	461156.936430	46.161537
3504.289657	461165.281807	46.166541
3504.309168	461169.691548	46.171546
3504.257878	461196.278067	46.176551
3504.417892	461187.630001	46.181556
3503.902510	461160.321474	46.186561
3503.733394	461163.087198	46.191565
3503.835547	461160.788544	46.196570
3503.686804	461167.355214	46.201575
3503.783980	461156.840347	46.206580
3503.583571	461169.197518	46.211585
3503.898313	461178.886422	46.216589
3504.443954	461134.367490	46.221594
3504.067552	461135.390703	46.226599
3504.239316	461144.239944	46.231604
3504.233622	461176.753784	46.236609
3504.090751	461175.051805	46.241613
3504.116418	461171.395743	46.246618
3504.144109	461147.653356	46.251623
3504.537245	461112.947880	46.256628
3504.197974	461127.051583	46.261633
3503.852290	461133.852282	46.266637
3503.631230	461140.937614	46.271642
3503.580027	461144.699148	46.276647
3504.421716	461118.089061	46.281652
3504.467866	461124.371327	46.286657
3503.701198	461142.448194	46.291661
3503.840574	461160.026776	46.296666
3503.879750	461179.396459	46.301671
3504.270679	461177.660827	46.306676
3503.855653	461190.559131	46.311681
3503.837273	461180.519040	46.316685
3503.823977	461168.449253	46.321690
3503.577493	461169.299762	46.326695
3503.716353	461160.553585	46.331700
3503.454690	461161.710827	46.336705
3504.137593	461137.408362	46.341709
3504.104224	461138.732409	46.346714
3503.957595	461145.248029	46.351719
3504.229472	461144.241325	46.356724
3503.848017	461195.784650	46.361729
3504.250085	461188.518544	46.366733
3504.016080	461155.332485	46.371738
3503.912015	461150.936091	46.376743
3504.200292	461152.817963	46.381748
3504.133478	461147.451959	46.386753
3504.051725	461140.769535	46.391757
3504.443143	461115.600120	46.396762
3503.910182	461163.464738	46.401767
3504.124706	461166.778488	46.406772
3504.041278	461171.458111	46.411777
3504.070662	461144.519955	46.416781
3504.394822	461137.418313	46.421786
3503.967777	461164.114988	46.426791
3504.233644	461115.481018	46.431796
3504.261374	461090.419783	46.436801
3504.233734	461099.452728	46.441805
3504.102536	461135.537032	46.446810
3504.103038	461114.537910	46.451815
3504.136558	461093.939328	46.456820
3504.104743	461102.364264	46.461825
3503.588022	461112.387513	46.466829
3504.375568	461077.670360	46.471834
3504.092723	461055.447909	46.476839
3503.972865	461098.935960	46.481844
3503.898864	461093.114577	46.486849
3503.953543	461053.694601	46.491853
3504.025231	461079.906766	46.496858
3503.947808	461111.417592	46.501863
3504.054560	461077.568885	46.506868
3504.225546	461050.405340	46.511873
3503.876864	461035.903091	46.516877
3504.130681	461052.804277	46.521882
3504.008517	461102.937329	46.526887
3504.090896	461088.366978	46.531892
3504.291431	461102.791151	46.536897
3503.842215	461095.000183	46.541901
3504.104485	461073.249531	46.546906
3503.857776	461080.744716	46.551911
3504.280787	461054.352898	46.556916
3504.264190	461069.978031	46.561921
3504.003990	461067.026528	46.566925
3504.166604	461074.609183	46.571930
3504.084257	461070.716565	46.576935
3503.971996	461068.654683	46.581940
3504.198168	461029.106110	46.586945
3504.095642	461040.027650	46.591949
3503.674912	461043.289664	46.596954
3503.694485	461057.691748	46.601959
3503.736872	461046.982598	46.606964
3504.036309	461054.645077	46.611969
3503.919614	461054.257736	46.616973
3504.500701	461072.020182	46.621978
3504.272558	461077.229924	46.626983
3504.272276	461034.724533	46.631988
3504.378736	460998.796127	46.636993
3504.376095	461007.774436	46.641997
3504.089527	461036.579409	46.647002
3504.156553	461037.076033	46.652007
3504.015454	461007.476362	46.657012
3504.134270	461000.102798	46.662017
3504.160530	461002.482603	46.667021
3504.450002	461013.900143	46.672026
3504.204766	461010.337597	46.677031
3504.155088	461019.982729	46.682036
3503.910235	461020.883709	46.687041
3504.297538	461018.337077	46.692045
3504.443464	460990.061523	46.697050
3504.208267	460981.374400	46.702055
3504.414413	460982.254816	46.707060
3504.135952	460984.277006	46.712065
3504.356307	460973.083186	46.717069
3504.552266	460974.269549	46.722074
3504.249875	460958.339697	46.727079
3504.173010	460939.838048	46.732084
3504.186194	460936.183920	46.737089
3504.337437	460927.587861	46.742093
3504.280680	460938.502217	46.747098
3503.864154	460925.938082	46.752103
3504.392390	460910.942080	46.757108
3503.874140	460885.459682	46.762113
3503.769277	460881.012638	46.767117
3504.052369	460876.250656	46.772122
3504.222376	460891.542082	46.777127
3504.419943	460881.467720	46.782132
3504.102902	460883.952525	46.787137
3504.249304	460878.907812	46.792141
3504.107390	460879.538911	46.797146
3504.100592	460891.662743	46.802151
3504.243904	460911.472708	46.807156
3504.387053	460838.865623	46.812161
3503.830465	460828.606105	46.817165
3503.971203	460846.641231	46.822170
3503.978437	460867.132144	46.827175
3504.171082	460860.101924	46.832180
3504.174850	460851.174086	46.837185
3504.216016	460854.921069	46.842189
3504.578647	460863.283748	46.847194
3503.797331	460864.472422	46.852199
3503.991521	460849.427733	46.857204
3504.107928	460823.642053	46.862209
3503.941122	460809.668858	46.867213
3504.217108	460787.307079	46.872218
3504.303246	460768.931689	46.877223
3504.106183	460811.519499	46.882228
3503.715123	460815.842040	46.887233
3504.061120	460795.193785	46.892237
3504.233333	460799.579464	46.897242
3504.242005	460839.953606	46.902247
3504.114211	460812.887717	46.907252
3504.396436	460765.315568	46.912257
3503.874320	460758.296848	46.917261
3504.349966	460759.946245	46.922266
3504.282902	460789.629864	46.927271
3504.495400	460774.582230	46.932276
3504.024184	460779.323233	46.937281
3504.015570	460774.658061	46.942285
3504.092090	460764.552055	46.947290
3504.318343	460729.923074	46.952295
3503.978075	460722.216197	46.957300
3504.133383	460768.603358	46.962305
3503.821814	460781.079764	46.967309
3503.868008	460758.297769	46.972314
3503.655458	460742.404282	46.977319
3504.306480	460733.627702	46.982324
3504.105782	460769.114917	46.987329
3504.033246	460737.120055	46.992333
3504.456372	460711.184316	46.997338
3504.075099	460767.496606	47.002343
3504.066459	460782.410562	47.007348
3503.969282	460778.926021	47.012353
3504.143621	460741.008261	47.017357
3504.162349	460715.085724	47.022362
3503.785743	460708.855560	47.027367
3504.209187	460721.520159	47.032372
3503.906958	460724.256256	47.037377
3504.157076	460685.616296	47.042381
3504.217278	460673.128832	47.047386
3504.285284	460691.682815	47.052391
3504.112753	460686.384131	47.057396
3504.189195	460692.154500	47.062401
3504.151082	460684.907082	47.067405
3504.351992	460666.614913	47.072410
3503.994665	460650.084839	47.077415
3504.186884	460641.177850	47.082420
3504.365142	460644.598859	47.087425
3503.984612	460667.636699	47.092429
3504.254946	460704.266926	47.097434
3504.181590	460708.184206	47.102439
3503.925767	460687.884594	47.107444
3503.815537	460642.403144	47.112449
3504.115664	460630.740030	47.117453
3504.201521	460668.261775	47.122458
3504.024546	460675.999692	47.127463
3504.209869	460664.304018	47.132468
3503.739493	460645.712152	47.137473
3504.212858	460634.427443	47.142477
3504.237102	460663.183778	47.147482
3503.667560	460650.491502	47.152487
3503.982939	460623.913286	47.157492
3503.916979	460678.400643	47.162497
3503.597923	460646.748955	47.167501
3504.349771	460624.514686	47.172506
3503.821259	460662.488617	47.177511
3504.062130	460652.356581	47.182516
3504.152698	460624.748709	47.187521
3503.887785	460652.891359	47.192525
3503.858501	460643.613596	47.197530
3504.065982	460617.255321	47.202535
3504.149485	460600.351188	47.207540
3503.869536	460639.300340	47.212545
3503.792951	460651.891846	47.217549
3503.940803	460637.716634	47.222554
3503.454993	460638.097758	47.227559
3503.911423	460620.323118	47.232564
3504.262345	460608.601239	47.237569
3503.807054	460653.512731	47.242573
3503.628671	460629.345845	47.247578
3503.561676	460632.450558	47.252583
3504.247625	460603.531187	47.257588
3503.908576	460599.019655	47.262593
3504.356110	460605.441519	47.267597
3504.524622	460594.002083	47.272602
3504.147478	460615.061224	47.277607
3504.266128	460599.115281	47.282612
3504.320115	460618.736737	47.287617
3503.858277	460643.309158	47.292621
3504.151164	460627.487865	47.297626
3503.895098	460614.492400	47.302631
3503.686756	460599.156102	47.307636
3503.769053	460601.729986	47.312641
3504.021020	460584.241254	47.317645
3504.204064	460602.472788	47.322650
3503.841473	460639.304615	47.327655
3503.724824	460601.026820	47.332660
3504.337442	460585.510023	47.337665
3503.870701	460634.531970	47.342669
3504.074724	460602.696091	47.347674
3504.519993	460583.553651	47.352679
3504.312349	460637.759163	47.357684
3503.788738	460630.487022	47.362689
3503.769043	460611.722442	47.367693
3504.408905	460635.613496	47.372698
3504.008454	460623.908945	47.377703
3503.893889	460593.188603	47.382708
3503.806297	460577.072349	47.387713
3503.580694	460588.520805	47.392717
3503.843173	460572.755002	47.397722
3504.261496	460549.051668	47.402727
3504.253238	460581.668244	47.407732
3503.880981	460621.798659	47.412737
3503.989138	460612.296265	47.417741
3504.183642	460615.055305	47.422746
3503.967232	460598.705812	47.427751
3503.806161	460577.934609	47.432756
3504.262056	460560.971583	47.437761
3503.946047	460585.216677	47.442765
3504.173789	460613.890187	47.447770
3503.960276	460605.757446	47.452775
3503.615194	460586.435595	47.457780
3504.207117	460577.059612	47.462785
3504.479999	460552.466246	47.467789
3504.574754	460565.791573	47.472794
3503.984429	460577.652750	47.477799
3503.832148	460564.995915	47.482804
3504.135844	460534.057207	47.487809
3503.789043	460528.684583	47.492813
3503.911691	460576.649747	47.497818
3504.111468	460545.575310	47.502823
3504.282132	460537.178923	47.507828
3503.731875	460564.605934	47.512833
3504.266734	460554.072319	47.517837
3504.108105	460560.488562	47.522842
3504.058143	460522.656602	47.527847
3503.976851	460556.248511	47.532852
3503.686160	460527.635585	47.537857
3503.930845	460495.336610	47.542861
3504.254386	460510.604034	47.547866
3504.142681	460549.932540	47.552871
3503.889135	460535.009131	47.557876
3504.175638	460504.275993	47.562881
3503.973354	460515.061392	47.567885
3504.503522	460495.246047	47.572890
3504.482343	460503.314465	47.577895
3504.284391	460530.229317	47.582900
3504.238867	460498.280561	47.587905
3504.387003	460462.243240	47.592909
3504.443894	460462.335688	47.597914
3503.871965	460520.707701	47.602919
3504.187358	460507.976911	47.607924
3503.965645	460485.794941	47.612929
3503.976020	460455.511171	47.617933
3504.193669	460425.093149	47.622938
3503.853629	460435.951085	47.627943
3504.149715	460423.476917	47.632948
3504.217660	460414.386584	47.637953
3503.852381	460453.400277	47.642957
3504.088072	460457.420924	47.647962
3504.019329	460482.083562	47.652967
3504.202566	460484.895124	47.657972
3503.967987	460475.903360	47.662977
3503.938622	460461.705322	47.667981
3503.818853	460442.652073	47.672986
3504.384928	460425.164288	47.677991
3504.045583	460419.841183	47.682996
3504.084499	460450.320092	47.688001
3503.778887	460428.557117	47.693005
3504.069569	460410.402716	47.698010
3503.991257	460426.240958	47.703015
3504.035102	460425.929677	47.708020
3504.501782	460413.428538	47.713025
3503.884411	460438.533012	47.718029
3504.160795	460394.765275	47.723034
3503.879503	460419.360132	47.728039
3504.050461	460447.079081	47.733044
3503.941823	460407.379414	47.738049
3503.825543	460424.643930	47.743053
3503.920201	460445.679382	47.748058
3503.795979	460428.960123	47.753063
3504.113419	460420.692662	47.758068
3504.586852	460404.893395	47.763073
3504.200721	460425.700518	47.768077
3503.875131	460409.621761	47.773082
3504.483647	460378.888272	47.778087
3504.050466	460412.992538	47.783092
3504.101687	460385.745653	47.788097
3504.307305	460406.966499	47.793101
3504.162467	460371.685474	47.798106
3503.991005	460400.067296	47.803111
3504.160495	460363.823542	47.808116
3504.328027	460347.565345	47.813121
3504.376625	460357.702476	47.818125
3504.355222	460359.176850	47.823130
3504.136253	460350.486911	47.828135
3504.249140	460331.295342	47.833140
3504.142457	460367.427760	47.838145
3503.915510	460317.246746	47.843149
3504.310440	460322.053835	47.848154
3504.087421	460306.263134	47.853159
3504.268619	460315.314116	47.858164
3504.348755	460299.729113	47.863169
3503.914474	460329.826468	47.868173
3503.923614	460308.977381	47.873178
3504.342371	460311.092323	47.878183
3504.078732	460324.068654	47.883188
3504.311709	460289.336466	47.888193
3503.888009	460298.990312	47.893197
3504.197329	460277.180710	47.898202
3504.092438	460267.103151	47.903207
3504.116812	460283.686129	47.908212
3504.443484	460255.127436	47.913217
3504.053119	460312.608990	47.918221
3504.060398	460286.383410	47.923226
3503.960554	460271.181905	47.928231
3504.329842	460248.652657	47.933236
3504.101354	460270.145150	47.938241
3504.158518	460272.976667	47.943245
3504.014283	460232.369273	47.948250
3503.939409	460263.170774	47.953255
3504.253962	460239.737131	47.958260
3504.247636	460258.709025	47.963265
3503.633841	460258.856763	47.968269
3504.251911	460245.164940	47.973274
3504.212352	460254.605912	47.978279
3503.950015	460262.458916	47.983284
3503.879884	460241.317949	47.988289
3504.121087	460274.808588	47.993293
3504.464332	460221.138700	47.998298
3504.020501	460241.752220	48.003303
3504.244436	460191.093854	48.008308
3504.088451	460211.154660	48.013313
3503.539947	460224.581872	48.018317
3503.979379	460207.976247	48.023322
3504.025933	460234.447018	48.028327
3504.107022	460204.811142	48.033332
3503.905765	460229.799356	48.038337
3504.026974	460206.193341	48.043341
3504.388069	460193.556594	48.048346
3503.918228	460256.731995	48.053351
3503.968269	460224.970632	48.058356
3504.383973	460185.694927	48.063361
3504.056767	460217.449418	48.068365
3504.150607	460174.166615	48.073370
3504.306639	460201.178091	48.078375
3504.213902	460172.685586	48.083380
3504.210661	460194.548345	48.088385
3503.894569	460193.076567	48.093389
3504.500870	460162.546024	48.098394
3503.845287	460131.454032	48.103399
3503.918805	460170.652490	48.108404
3503.926793	460137.680260	48.113409
3504.074356	460137.809102	48.118413
3504.012596	460168.913011	48.123418
3504.113977	460142.570937	48.128423
3503.898727	460166.699116	48.133428
3504.020968	460147.201561	48.138433
3504.033962	460132.489369	48.143437
3504.240440	460154.927714	48.148442
3504.046661	460144.001830	48.153447
3504.324201	460124.327533	48.158452
3504.287405	460168.666619	48.163457
3504.017460	460146.441205	48.168461
3504.449381	460114.112074	48.173466
3504.096920	460143.790953	48.178471
3504.099268	460123.145661	48.183476
3504.405523	460097.785643	48.188481
3504.099561	460136.435449	48.193485
3504.659360	460149.890420	48.198490
3503.851330	460104.568878	48.203495
3503.932261	460068.237186	48.208500
3504.175806	460120.242217	48.213505
3503.596457	460100.348271	48.218509
3504.186085	460068.602842	48.223514
3504.176596	460118.213086	48.228519
3504.454157	460075.814093	48.233524
3504.257965	460099.432086	48.238529
3504.159828	460081.643221	48.243533
3504.272421	460091.263112	48.248538
3504.435066	460064.759087	48.253543
3504.115129	460059.027028	48.258548
3504.546567	460022.386233	48.263553
3504.044511	460070.704871	48.268557
3504.046999	460048.588470	48.273562
3504.466537	460029.348166	48.278567
3504.147823	460029.956510	48.283572
3504.316847	460015.219578	48.288577
3504.145497	460018.848121	48.293581
3504.161964	460001.396150	48.298586
3504.236068	460005.036623	48.303591
3503.921216	460035.724201	48.308596
3503.919155	460019.238944	48.313601
3503.961465	460011.166994	48.318605
3504.112972	459985.780582	48.323610
3504.082140	460019.821859	48.328615
3504.456637	459984.356673	48.333620
3504.663255	459996.497990	48.338625
3504.047245	459988.022841	48.343629
3504.222675	459956.647070	48.348634
3504.580542	459939.445436	48.353639
3504.359675	459982.799491	48.358644
3504.336648	459960.889934	48.363649
3504.095757	459944.442373	48.368653
3504.070306	459907.924330	48.373658
3504.222497	459938.233870	48.378663
3504.112238	459952.048501	48.383668
3504.339044	459938.012533	48.388673
3504.016289	459946.636075	48.393677
3504.025998	459929.337291	48.398682
3503.945581	459899.827982	48.403687
3504.112383	459917.453952	48.408692
3504.081464	459904.980454	48.413697
3504.089422	459892.855879	48.418701
3504.107132	459881.084833	48.423706
3504.043797	459867.297583	48.428711
3503.990982	459865.936343	48.433716
3503.652287	459882.323387	48.438721
3503.340958	459893.177052	48.443725
3503.465435	459898.026984	48.448730
3503.831219	459903.498199	48.453735
3503.961578	459919.608173	48.458740
3504.176776	459916.226294	48.463745
3503.949468	459899.370751	48.468749
3504.232881	459880.253284	48.473754
3504.305655	459878.973644	48.478759
3504.522126	459873.664000	48.483764
3504.978596	459854.569882	48.488769
3504.384345	459857.250793	48.493773
3504.220125	459872.139234	48.498778
3504.224038	459903.334587	48.503783
3504.045205	459896.870030	48.508788
3503.843121	459868.901666	48.513793
3503.819064	459863.680764	48.518797
3504.518948	459842.011898	48.523802
3504.281019	459817.295551	48.528807
3504.490244	459809.095693	48.533812
3504.708615	459790.191331	48.538817
3504.228508	459813.448705	48.543821
3503.714888	459826.972095	48.548826
3504.479800	459800.068202	48.553831
3503.989229	459822.160537	48.558836
3504.621583	459768.545299	48.563841
3504.256303	459811.973242	48.568845
3504.231870	459783.367984	48.573850
3504.555796	459763.381680	48.578855
3504.209653	459734.319956	48.583860
3504.586928	459716.709277	48.588865
3503.873369	459722.401871	48.593869
3503.823509	459740.518759	48.598874
3503.918040	459772.460857	48.603879
3503.783843	459757.619505	48.608884
3503.574082	459748.217714	48.613889
3503.741924	459737.792449	48.618893
3504.217177	459767.138100	48.623898
3503.851962	459789.667182	48.628903
3503.301670	459762.311702	48.633908
3503.271362	459759.628036	48.638913
3503.317702	459772.555694	48.643917
3503.683326	459793.396764	48.648922
3503.862247	459801.484536	48.653927
3504.373155	459778.070090	48.658932
3504.131731	459787.644621	48.663937
3503.872572	459817.157016	48.668941
3504.082924	459775.731850	48.673946
3504.180401	459769.172854	48.678951
3503.933487	459773.827890	48.683956
3504.662643	459727.349535	48.688961
3504.269761	459738.216166	48.693965
3504.043324	459771.730765	48.698970
3504.114132	459784.147294	48.703975
3504.062613	459783.343824	48.708980
3503.898814	459754.101127	48.713985
3503.961798	459749.373694	48.718989
3503.654021	459723.958127	48.723994
3504.260433	459729.188448	48.728999
3504.213696	459731.224850	48.734004
3504.286952	459756.322387	48.739009
3503.880888	459737.364505	48.744013
3504.338623	459717.610636	48.749018
3504.218524	459758.311475	48.754023
3503.887724	459729.957477	48.759028
3504.302883	459732.478849	48.764033
3504.138484	459767.809766	48.769037
3504.041492	459733.788290	48.774042
3503.966595	459697.176263	48.779047
3503.733856	459720.698989	48.784052
3503.941219	459677.498716	48.789057
3503.878280	459720.473244	48.794061
3504.106270	459684.472752	48.799066
3504.117793	459701.616182	48.804071
3503.647120	459713.103829	48.809076
3503.873425	459677.763025	48.814081
3503.740444	459701.422179	48.819085
3504.246770	459726.552747	48.824090
3504.161770	459720.377659	48.829095
3504.027433	459720.246710	48.834100
3504.485639	459724.993203	48.839105
3504.088406	459729.215479	48.844109
3503.925452	459713.820662	48.849114
3503.680329	459707.569429	48.854119
3503.926309	459680.240160	48.859124
3504.428495	459691.472590	48.864129
3503.846387	459717.992628	48.869133
3503.457802	459672.553168	48.874138
3504.357479	459657.041071	48.879143
3503.731303	459704.314892	48.884148
3504.216742	459652.041458	48.889153
3504.105213	459688.581562	48.894157
3504.133474	459663.975145	48.899162
3503.731856	459674.843188	48.904167
3504.524440	459645.094095	48.909172
3504.376813	459690.314000	48.914177
3503.803466	459676.455069	48.919181
3504.084634	459665.149520	48.924186
3503.954227	459672.931154	48.929191
3504.069933	459686.659509	48.934196
3504.270834	459648.837117	48.939201
3503.812394	459668.895499	48.944205
3504.439021	459628.368044	48.949210
3503.965457	459651.168024	48.954215
3503.895704	459648.997836	48.959220
3504.089316	459619.698467	48.964225
3503.776517	459644.755701	48.969229
3504.156774	459630.188025	48.974234
3504.276921	459614.494761	48.979239
3504.059157	459664.494030	48.984244
3504.010866	459625.392119	48.989249
3504.043565	459649.532398	48.994253
3504.181982	459630.741989	48.999258
3503.963761	459613.986242	49.004263
3504.012125	459615.652542	49.009268
3504.249879	459589.440427	49.014273
3503.744348	459632.941618	49.019277
3504.146152	459607.160126	49.024282
3504.030774	459597.844804	49.029287
3504.002821	459618.697525	49.034292
3504.119504	459620.860283	49.039297
3504.249425	459612.419258	49.044301
3504.323701	459614.537994	49.049306
3504.217481	459603.953083	49.054311
3504.245396	459595.629627	49.059316
3504.242138	459596.086667	49.064321
3504.252191	459580.157151	49.069325
3504.179387	459570.632185	49.074330
3504.190637	459589.449701	49.079335
3504.096259	459576.681692	49.084340
3504.345617	459588.359947	49.089345
3504.342940	459567.765655	49.094349
3504.118068	459527.676964	49.099354
3504.196072	459560.078516	49.104359
3504.006959	459526.324911	49.109364
3504.357055	459542.958413	49.114369
3503.765301	459524.841315	49.119373
3504.029000	459550.720599	49.124378
3504.288811	459527.649933	49.129383
3504.222782	459534.964906	49.134388
3504.338835	459519.170769	49.139393
3503.937639	459511.118013	49.144397
3504.169126	459504.487030	49.149402
3503.947701	459494.478263	49.154407
3503.885636	459500.828824	49.159412
3504.327244	459489.751456	49.164417
3504.108929	459501.503680	49.169421
3503.724028	459493.346890	49.174426
3503.748425	459508.002858	49.179431
3503.845486	459501.443848	49.184436
3503.841965	459496.625422	49.189441
3503.905930	459492.303588	49.194445
3503.901307	459514.370145	49.199450
3503.900499	459496.616149	49.204455
3503.802506	459527.777416	49.209460
3504.431982	459499.322059	49.214465
3503.970898	459505.735691	49.219469
3503.705481	459513.843077	49.224474
3504.054041	459493.091745	49.229479
3503.735269	459513.331095	49.234484
3504.063981	459499.329466	49.239489
3504.004174	459498.476570	49.244493
3504.334789	459491.677736	49.249498
3504.278107	459474.744171	49.254503
3503.812450	459488.716721	49.259508
3504.302534	459470.377849	49.264513
3504.225631	459457.607009	49.269517
3503.843455	459502.052756	49.274522
3503.580109	459465.419405	49.279527
3503.850087	459494.392058	49.284532
3503.989450	459471.644729	49.289537
3503.948870	459465.614727	49.294541
3503.852055	459480.492777	49.299546
3504.045540	459475.338849	49.304551
3503.595873	459482.105766	49.309556
3503.873779	459479.525526	49.314561
3503.750899	459494.813496	49.319565
3504.187766	459487.135523	49.324570
3503.915813	459476.779651	49.329575
3503.837900	459484.451602	49.334580
3504.042555	459495.781888	49.339585
3504.167321	459486.327109	49.344589
3503.977979	459494.523930	49.349594
3504.022731	459466.363860	49.354599
3503.755056	459486.087896	49.359604
3504.072071	459449.464236	49.364609
3504.033311	459463.369324	49.369613
3504.112804	459429.218029	49.374618
3503.935540	459464.500740	49.379623
3503.996388	459448.512373	49.384628
3503.962353	459462.822524	49.389633
3504.106826	459427.291349	49.394637
3504.141953	459460.359267	49.399642
3504.332427	459446.531634	49.404647
3503.935557	459464.703599	49.409652
3504.297450	459443.290673	49.414657
3504.027146	459441.152165	49.419661
3503.905702	459455.526864	49.424666
3504.355524	459407.418025	49.429671
3503.995236	459421.221784	49.434676
3504.097898	459399.241075	49.439681
3503.903669	459406.018365	49.444685
3503.613531	459424.477851	49.449690
3504.134105	459384.524701	49.454695
3503.601934	459439.393178	49.459700
3503.843334	459400.092899	49.464705
3503.950059	459403.474684	49.469709
3503.979071	459416.811099	49.474714
3504.221932	459404.294042	49.479719
3504.091560	459403.198665	49.484724
3504.411685	459414.815099	49.489729
3503.831081	459427.081164	49.494733
3504.107337	459416.283527	49.499738
3504.132116	459401.366080	49.504743
3504.155538	459409.935112	49.509748
3503.932186	459399.064259	49.514753
3503.866638	459376.653579	49.519757
3503.928809	459380.093136	49.524762
3504.063233	459390.673683	49.529767
3503.931001	459384.201609	49.534772
3504.090096	459371.900679	49.539777
3503.938909	459386.584482	49.544781
3504.165804	459388.171853	49.549786
3504.139037	459364.994137	49.554791
3503.860136	459399.836479	49.559796
3504.131749	459384.727825	49.564801
3503.969818	459375.977757	49.569805
3504.088297	459391.176922	49.574810
3504.251520	459374.512878	49.579815
3504.033254	459377.996763	49.584820
3504.165840	459360.475204	49.589825
3504.157242	459338.765653	49.594829
3503.847580	459366.003944	49.599834
3504.356436	459343.806796	49.604839
3504.003694	459360.044268	49.609844
3504.213866	459352.300628	49.614849
3503.887962	459340.482155	49.619853
3503.735530	459367.137601	49.624858
3503.847045	459336.785579	49.629863
3503.655780	459360.505038	49.634868
3504.020892	459337.366803	49.639873
3503.742885	459368.962560	49.644877
3504.233639	459340.782558	49.649882
3503.879189	459368.433737	49.654887
3503.803803	459346.430393	49.659892
3503.868455	459362.500434	49.664897
3504.064848	459358.614179	49.669901
3503.920158	459341.390064	49.674906
3504.128965	459355.256088	49.679911
3503.843734	459365.649349	49.684916
3504.284974	459341.890369	49.689921
3503.777244	459330.100630	49.694925
3503.964129	459331.795782	49.699930
3504.144702	459321.621941	49.704935
3504.003344	459316.368724	49.709940
3503.906619	459338.044204	49.714945
3504.130159	459320.761868	49.719949
3504.016139	459317.584116	49.724954
3503.722323	459331.529603	49.729959
3503.694331	459319.664028	49.734964
3504.088169	459322.340998	49.739969
3503.686188	459323.672693	49.744973
3503.796885	459350.032936	49.749978
3504.032097	459301.196892	49.754983
3503.994605	459348.479876	49.759988
3504.116375	459317.720396	49.764993
3503.925740	459346.157333	49.769997
3504.158326	459309.496059	49.775002
3503.730496	459349.992661	49.780007
3504.064560	459324.728811	49.785012
3503.927322	459356.099430	49.790017
3503.928951	459315.112202	49.795021
3504.039275	459343.298665	49.800026
3504.259501	459322.212373	49.805031
3503.931501	459323.025108	49.810036
3503.868413	459284.280017	49.815041
3503.714193	459304.189189	49.820045
3503.943526	459269.303791	49.825050
3503.825881	459299.352502	49.830055
3504.013108	459277.206125	49.835060
3504.033067	459299.218286	49.840065
3503.985375	459294.508250	49.845069
3503.521916	459295.697484	49.850074
3503.811387	459280.636663	49.855079
3503.765714	459308.797101	49.860084
3503.907139	459282.295490	49.865089
3503.845743	459300.871102	49.870093
3503.977209	459293.241335	49.875098
3504.335816	459278.068131	49.880103
3504.036167	459319.761965	49.885108
3503.917367	459287.265041	49.890113
3504.046319	459305.506202	49.895117
3504.038617	459276.136744	49.900122
3504.409826	459307.427064	49.905127
3504.119261	459281.145914	49.910132
3503.852598	459314.464658	49.915137
3504.370349	459290.135538	49.920141
3504.044919	459271.925407	49.925146
3503.960072	459269.301029	49.930151
3504.099468	459250.915954	49.935156
3503.791940	459273.030632	49.940161
3503.953098	459248.149111	49.945165
3503.701051	459276.342212	49.950170
3504.398726	459240.368208	49.955175
3503.969415	459267.980618	49.960180
3504.064502	459242.348636	49.965185
3504.001030	459259.656444	49.970189
3503.623272	459272.194891	49.975194
3504.103784	459262.683785	49.980199
3503.897891	459268.854241	49.985204
3503.777520	459263.952781	49.990209
3504.086553	459272.831806	49.995213
3503.887338	459265.102120	50.000218
3504.316136	459265.237241	50.005223
3503.775943	459290.026461	50.010228
3503.873030	459259.473707	50.015233
3503.624950	459273.462728	50.020237
3503.887962	459274.537132	50.025242
3503.998604	459271.983307	50.030247
3503.678358	459264.830744	50.035252
3503.928404	459270.421865	50.040257
3504.295398	459277.211938	50.045261
3504.207648	459263.225262	50.050266
3503.886260	459245.826096	50.055271
3503.868965	459248.010069	50.060276
3504.035307	459220.946452	50.065281
3504.110505	459229.862457	50.070285
3503.984918	459247.991720	50.075290
3504.422506	459213.377675	50.080295
3503.902671	459241.359515	50.085300
3504.074018	459236.969931	50.090305
3504.166631	459231.476804	50.095309
3503.982402	459238.861285	50.100314
3503.997603	459251.692717	50.105319
3503.918338	459238.719217	50.110324
3503.861754	459248.112585	50.115329
3504.189699	459247.249115	50.120333
3503.603159	459228.167141	50.125338
3503.879135	459242.377705	50.130343
3504.057785	459234.486827	50.135348
3504.004721	459246.111613	50.140353
3504.321795	459207.509203	50.145357
3504.011207	459211.565701	50.150362
3504.127523	459201.046874	50.155367
3504.320610	459208.473177	50.160372
3504.169717	459194.344258	50.165377
3503.984342	459231.201153	50.170381
3503.826497	459203.022044	50.175386
3504.306486	459216.997471	50.180391
3504.180123	459199.110901	50.185396
3504.015904	459205.173334	50.190401
3503.766658	459163.566032	50.195405
3503.732895	459185.028803	50.200410
3504.361811	459154.899108	50.205415
3503.870040	459147.925799	50.210420
3503.669107	459192.597155	50.215425
3503.907589	459154.565069	50.220429
3503.700067	459181.483082	50.225434
3504.480139	459154.931096	50.230439
3503.674316	459176.870999	50.235444
3503.900527	459178.864308	50.240449
3503.707036	459171.285864	50.245453
3504.203705	459154.315314	50.250458
3504.028827	459187.873376	50.255463
3503.936507	459163.792728	50.260468
3503.831312	459189.477112	50.265473
3503.969046	459157.852530	50.270477
3503.655027	459188.541154	50.275482
3504.325516	459167.282089	50.280487
3503.844261	459165.176899	50.285492
3503.868395	459187.797232	50.290497
3504.161586	459174.663368	50.295501
3503.751562	459173.054188	50.300506
3504.044011	459175.544295	50.305511
3503.798350	459192.170778	50.310516
3503.886729	459188.047933	50.315521
3504.204512	459181.149579	50.320525
3503.819290	459182.935174	50.325530
3503.860466	459184.146101	50.330535
3503.712874	459207.250100	50.335540
3503.700234	459193.555868	50.340545
3503.853408	459184.553010	50.345549
3503.753025	459196.641842	50.350554
3503.580004	459185.154207	50.355559
3503.288393	459210.259311	50.360564
3503.888697	459193.221683	50.365569
3503.992643	459191.987803	50.370573
3503.791724	459198.816941	50.375578
3504.227447	459198.545153	50.380583
3503.859785	459203.980297	50.385588
3504.046739	459183.507852	50.390593
3503.889407	459194.895512	50.395597
3503.867055	459209.153254	50.400602
3504.048589	459200.044466	50.405607
3504.075806	459195.931289	50.410612
3503.868081	459202.355688	50.415617
3504.089279	459205.009234	50.420621
3503.447366	459212.466068	50.425626
3504.166208	459211.236448	50.430631
3503.913359	459184.543408	50.435636
3503.929031	459217.462584	50.440641
3503.534820	459198.198003	50.445645
3503.557161	459210.926876	50.450650
3504.126805	459194.959357	50.455655
3504.084485	459221.191760	50.460660
3503.872194	459220.667315	50.465665
3504.482644	459201.497568	50.470669
3503.920389	459185.962591	50.475674
3504.070080	459186.649098	50.480679
3504.287646	459173.375007	50.485684
3504.066311	459161.337000	50.490689
3504.095286	459171.579233	50.495693
3504.005349	459176.666123	50.500698
3504.223220	459174.906966	50.505703
3503.913667	459174.245714	50.510708
3503.996660	459181.435795	50.515713
3503.934354	459168.611753	50.520717
3504.038467	459180.363910	50.525722
3504.223197	459158.217809	50.530727
3504.139924	459148.795769	50.535732
3504.118721	459111.514833	50.540737
3503.812714	459089.091143	50.545741
3503.817534	459049.574002	50.550746
3504.205637	458968.907145	50.555751
3503.680057	458942.561285	50.560756
3503.545000	458849.599213	50.565761
3503.833097	458764.128300	50.570765
3503.273471	458672.754427	50.575770
3503.357994	458578.031756	50.580775
3503.346867	458483.881811	50.585780
3502.701234	458345.697829	50.590785
3502.741767	458226.224984	50.595789
3502.402864	458097.325102	50.600794
3502.250436	457953.784875	50.605799
3501.923068	457808.039256	50.610804
3501.542616	457648.806819	50.615809
3501.429492	457482.276501	50.620813
3500.942975	457324.276047	50.625818
3500.868268	457148.707040	50.630823
3500.257369	456978.091665	50.635828
3499.814461	456791.214120	50.640833
3499.597436	456598.059190	50.645837
3499.283196	456394.619136	50.650842
3499.370856	456194.918729	50.655847
3498.836998	455989.531108	50.660852
3498.303271	455777.647571	50.665857
3498.084808	455563.987214	50.670861
3497.689773	455329.804856	50.675866
3497.208192	455102.584590	50.680871
3496.751772	454864.348223	50.685876
3496.153188	454625.320027	50.690881
3496.065254	454392.905960	50.695885
3495.587893	454146.699546	50.700890
3495.515387	453882.718641	50.705895
3494.805284	453631.773995	50.710900
3494.102152	453367.125706	50.715905
3493.803688	453088.761177	50.720909
3493.056915	452840.452134	50.725914
3492.566801	452566.323053	50.730919
3492.236922	452290.186415	50.735924
3491.498964	452011.523073	50.740929
3491.006153	451725.104583	50.745933
3490.584373	451454.604976	50.750938
3490.242479	451158.869414	50.755943
3489.247427	450876.477876	50.760948
3488.609892	450591.286091	50.765953
3488.439425	450304.951287	50.770957
3487.751833	450014.939398	50.775962
3487.187247	449711.253248	50.780967
3486.627240	449416.392679	50.785972
3486.097093	449117.260729	50.790977
3485.499214	448809.203673	50.795981
3484.514880	448515.058566	50.800986
3484.158396	448203.656611	50.805991
3483.262470	447906.038818	50.810996
3482.841144	447596.466147	50.816001
3482.348052	447295.427299	50.821005
3481.640582	446989.596892	50.826010
3481.247052	446682.038009	50.831015
3480.583801	446370.355854	50.836020
3479.944650	446058.716558	50.841025
3479.468370	445736.642353	50.846029
3478.320270	445424.770684	50.851034
3478.008980	445099.768650	50.856039
3477.408899	444794.502175	50.861044
3476.809324	444467.049970	50.866049
3476.413983	444143.368013	50.871053
3475.759380	443826.829173	50.876058
3475.136049	443491.905666	50.881063
3474.270147	443179.807981	50.886068
3473.975848	442844.214359	50.891073
3473.162529	442516.109591	50.896077
3472.528999	442202.338182	50.901082
3472.025135	441867.931795	50.906087
3471.075254	441540.698486	50.911092
3470.376080	441215.502575	50.916097
3469.528573	440871.186754	50.921101
3468.794517	440566.091368	50.926106
3468.362788	440244.673266	50.931111
3467.661946	439909.433668	50.936116
3467.063330	439574.960290	50.941121
3466.456338	439254.445486	50.946125
3465.543903	438927.273097	50.951130
3465.112536	438595.882487	50.956135
3464.364985	438270.960121	50.961140
3463.587727	437939.386998	50.966145
3462.930470	437596.138015	50.971149
3462.363964	437272.925754	50.976154
3461.421567	436947.103088	50.981159
3460.818502	436628.889643	50.986164
3459.941108	436295.965119	50.991169
3459.211311	435969.410742	50.996173
3458.726059	435643.473603	51.001178
3458.123662	435327.427119	51.006183
3457.326352	435006.151936	51.011188
3456.275529	434678.971608	51.016193
3455.887744	434352.824819	51.021197
3455.378010	434032.507528	51.026202
3454.757210	433687.041709	51.031207
3453.932995	433375.703438	51.036212
3453.056741	433053.121315	51.041217
3452.640463	432722.286360	51.046221
3451.701706	432417.556447	51.051226
3450.933548	432080.547917	51.056231
3450.291795	431763.727470	51.061236
3449.516056	431449.565203	51.066241
3449.158776	431126.394619	51.071245
3448.148966	430805.253102	51.076250
3447.682511	430481.177648	51.081255
3446.868468	430169.012168	51.086260
3446.167631	429847.251415	51.091265
3445.553877	429517.041936	51.096269
3444.530274	429206.142523	51.101274
3444.207833	428886.925934	51.106279
3443.752142	428586.900232	51.111284
3442.958391	428261.681099	51.116289
3442.172854	427929.066404	51.121293
3441.506827	427612.580848	51.126298
3441.179544	427282.450705	51.131303
3440.312315	426974.725922	51.136308
3439.379119	426655.452229	51.141313
3439.007711	426324.783952	51.146317
3437.914036	426011.801240	51.151322
3437.444252	425687.820396	51.156327
3436.940305	425364.577641	51.161332
3435.563037	425056.708454	51.166337
3435.001146	424754.497888	51.171341
3434.185902	424440.538675	51.176346
3433.730739	424122.785161	51.181351
3432.907124	423806.407017	51.186356
3432.113601	423500.510814	51.191361
3431.944322	423189.330787	51.196365
3430.986794	422878.068664	51.201370
3430.549820	422557.982719	51.206375
3429.476329	422250.465844	51.211380
3428.723891	421939.059133	51.216385
3428.339173	421635.567043	51.221389
3427.288911	421325.648473	51.226394
3427.043454	421017.783846	51.231399
3426.440414	420709.972368	51.236404
3425.427738	420396.049305	51.241409
3424.841785	420077.482645	51.246413
3423.798021	419780.450928	51.251418
3423.190347	419474.023867	51.256423
3422.709035	419166.379508	51.261428
3422.020777	418866.157256	51.266433
3421.405023	418550.575851	51.271437
3420.455974	418261.896842	51.276442
3419.890182	417942.439231	51.281447
3419.336207	417646.654249	51.286452
3418.381167	417351.336121	51.291457
3417.970481	417043.174993	51.296461
3417.310609	416746.609895	51.301466
3416.697348	416443.047536	51.306471
3415.544885	416133.215497	51.311476
3414.799958	415830.124851	51.316481
3414.464536	415537.078480	51.321485
3413.398521	415241.171963	51.326490
3412.984322	414944.041433	51.331495
3412.134525	414649.339723	51.336500
3411.215963	414350.504330	51.341505
3410.674583	414052.724243	51.346509
3409.947186	413752.734558	51.351514
3409.430464	413466.734440	51.356519
3408.895304	413172.146045	51.361524
3408.184493	412868.460373	51.366529
3407.687986	412568.854139	51.371533
3406.612496	412285.522796	51.376538
3406.212855	411978.983707	51.381543
3405.461738	411686.015599	51.386548
3404.569518	411389.560206	51.391553
3404.451340	411091.149883	51.396557
3403.309436	410809.619270	51.401562
3402.764412	410501.690436	51.406567
3402.207228	410210.303639	51.411572
3401.543539	409919.693245	51.416577
3400.834957	409620.904324	51.421581
3399.635314	409328.670373	51.426586
3399.281079	409038.409229	51.431591
3398.630015	408743.185842	51.436596
3397.475966	408456.222292	51.441601
3396.968392	408156.472369	51.446605
3396.089915	407870.171353	51.451610
3395.581447	407591.941727	51.456615
3395.342798	407305.432643	51.461620
3394.447788	407017.753954	51.466625
3393.930068	406711.993741	51.471629
3393.101293	406445.520755	51.476634
3392.500484	406142.233351	51.481639
3391.639022	405866.738111	51.486644
3390.481363	405576.546072	51.491649
3389.884444	405285.652696	51.496653
3389.418576	405018.500183	51.501658
3388.626778	404737.621169	51.506663
3388.369063	404457.366877	51.511668
3387.571696	404164.156503	51.516673
3386.856244	403875.937664	51.521677
3385.983609	403607.998788	51.526682
3385.489175	403315.520624	51.531687
3384.802666	403031.330977	51.536692
3384.004339	402752.214696	51.541697
3383.846148	402451.541659	51.546701
3382.622043	402186.594982	51.551706
3382.249872	401882.696884	51.556711
3381.420261	401604.414412	51.561716
3380.641612	401327.011162	51.566721
3380.019610	401036.438892	51.571725
3379.034295	400766.155565	51.576730
3378.595548	400476.261068	51.581735
3378.142631	400193.356781	51.586740
3377.255179	399922.796795	51.591745
3376.763574	399641.851230	51.596749
3376.080123	399352.493894	51.601754
3375.569533	399075.766352	51.606759
3374.826024	398798.081893	51.611764
3374.069223	398504.025794	51.616769
3373.775639	398218.384682	51.621773
3372.722669	397948.699030	51.626778
3371.890733	397657.062400	51.631783
3371.203320	397378.797932	51.636788
3370.277952	397106.593916	51.641793
3369.921074	396825.577803	51.646797
3369.019359	396550.924963	51.651802
3368.241399	396273.885963	51.656807
3367.869912	395991.721170	51.661812
3366.497151	395742.000276	51.666817
3366.652111	395451.739326	51.671821
3365.412641	395169.450715	51.676826
3365.333459	394906.552907	51.681831
3364.652744	394622.620545	51.686836
3364.042968	394354.615828	51.691841
3363.158693	394066.210900	51.696845
3362.449890	393795.268207	51.701850
3361.906379	393510.618494	51.706855
3361.152254	393240.365097	51.711860
3360.518395	392971.107600	51.716865
3359.926991	392681.602366	51.721869
3359.226920	392409.427025	51.726874
3358.341889	392133.566585	51.731879
3357.843037	391852.430490	51.736884
3356.748105	391575.429234	51.741889
3355.892424	391306.753383	51.746893
3355.472683	391056.237701	51.751898
3355.035930	390762.878133	51.756903
3354.285242	390508.901957	51.761908
3353.423733	390238.388143	51.766913
3353.264668	389949.249775	51.771917
3352.520575	389675.229514	51.776922
3351.327919	389412.288481	51.781927
3350.898325	389142.740623	51.786932
3350.078186	388870.023079	51.791937
3349.264557	388599.413025	51.796941
3348.389903	388323.699380	51.801946
3348.098863	388062.055361	51.806951
3347.502356	387796.770514	51.811956
3346.615581	387532.521384	51.816961
3346.456083	387261.696194	51.821965
3345.609378	387004.735221	51.826970
3344.791199	386725.338645	51.831975
3344.213711	386453.302079	51.836980
3343.289629	386188.337107	51.841985
3342.975065	385909.490459	51.846989
3342.580860	385640.521451	51.851994
3341.775876	385371.386576	51.856999
3341.104611	385091.649244	51.862004
3340.143061	384830.622328	51.867009
3339.633304	384551.058854	51.872013
3338.735714	384286.305022	51.877018
3337.960653	384021.606243	51.882023
3337.545161	383744.641344	51.887028
3337.109578	383467.906482	51.892033
3336.165944	383201.194027	51.897037
3335.327898	382929.986857	51.902042
3334.675663	382658.621205	51.907047
3333.959358	382396.216163	51.912052
3332.757835	382136.327638	51.917057
3332.463620	381868.256932	51.922061
3331.949941	381607.289578	51.927066
3331.257989	381340.117399	51.932071
3330.607980	381074.233864	51.937076
3330.027686	380819.172372	51.942081
3329.203593	380553.338229	51.947085
3328.419962	380286.631102	51.952090
3328.185116	380016.121919	51.957095
3327.576846	379765.076609	51.962100
3326.540956	379500.438790	51.967105
3325.801021	379219.168728	51.972109
3325.118452	378961.135391	51.977114
3324.237956	378700.257470	51.982119
3323.665248	378443.831250	51.987124
3323.303110	378189.354059	51.992129
3322.615393	377931.594631	51.997133
3321.672777	377662.910910	52.002138
3321.201192	377401.196727	52.007143
3320.583018	377138.791801	52.012148
3319.965377	376876.842937	52.017153
3319.396591	376610.738459	52.022157
3318.490681	376350.052731	52.027162
3317.913963	376081.504089	52.032167
3316.877148	375820.301483	52.037172
3315.943250	375556.740687	52.042177
3315.630098	375296.692150	52.047181
3314.758721	375041.003782	52.052186
3314.471502	374787.612595	52.057191
3313.909191	374538.180810	52.062196
3312.491236	374276.163756	52.067201
3312.341374	374013.537477	52.072205
3311.641081	373766.768454	52.077210
3310.874613	373512.656666	52.082215
3310.318619	373244.874848	52.087220
3309.696822	372988.065915	52.092225
3309.269630	372722.117429	52.097229
3308.317422	372468.155878	52.102234
3307.553576	372206.963649	52.107239
3307.339375	371936.117591	52.112244
3306.207203	371688.030923	52.117249
3305.516584	371426.669669	52.122253
3305.086868	371174.016926	52.127258
3304.230400	370918.530002	52.132263
3303.537974	370666.221095	52.137268
3303.004963	370417.803330	52.142273
3302.706152	370160.646393	52.147277
3302.007642	369894.290690	52.152282
3301.076229	369630.946778	52.157287
3300.388888	369375.373088	52.162292
3299.705849	369118.321627	52.167297
3299.069145	368848.337088	52.172301
3298.389737	368593.978763	52.177306
3297.461362	368329.227240	52.182311
3297.148378	368086.027821	52.187316
3296.491908	367827.768841	52.192321
3295.943581	367567.379554	52.197325
3294.979725	367317.409478	52.202330
3294.392720	367040.129537	52.207335
3293.604948	366785.777974	52.212340
3292.626806	366534.202893	52.217345
3292.063240	366276.174669	52.222349
3291.589844	366014.924885	52.227354
3290.654987	365777.077969	52.232359
3290.319179	365524.454270	52.237364
3289.454777	365269.851852	52.242369
3289.210148	365012.478409	52.247373
3288.103476	364771.981839	52.252378
3287.303979	364506.525875	52.257383
3287.120824	364240.334794	52.262388
3286.160432	364002.228243	52.267393
3285.871315	363742.437536	52.272397
3285.137674	363491.112346	52.277402
3284.278253	363237.210346	52.282407
3283.743143	362976.411041	52.287412
3282.832750	362720.478717	52.292417
3282.450239	362458.761827	52.297421
3281.251755	362205.849332	52.302426
3280.614893	361957.681252	52.307431
3280.425223	361705.166314	52.312436
3279.177714	361451.697745	52.317441
3278.751763	361199.828189	52.322445
3278.259437	360952.268145	52.327450
3277.682440	360696.475730	52.332455
3276.895761	360443.183389	52.337460
3276.081725	360192.973034	52.342465
3275.613212	359935.149171	52.347469
3274.738518	359695.073479	52.352474
3274.196166	359432.118439	52.357479
3273.737783	359180.981433	52.362484
3272.943153	358934.120501	52.367489
3272.377009	358666.966380	52.372493
3271.893230	358424.125240	52.377498
3270.674129	358164.883945	52.382503
3270.219919	357904.935019	52.387508
3269.470069	357662.615731	52.392513
3269.358581	357405.561900	52.397517
3268.339828	357157.989586	52.402522
3267.660821	356906.494230	52.407527
3267.005917	356648.682694	52.412532
3266.415308	356394.117035	52.417537
3265.813844	356145.939333	52.422541
3264.878352	355883.613041	52.427546
3264.154928	355625.221827	52.432551
3263.683516	355376.918014	52.437556
3262.995131	355120.809092	52.442561
3262.525551	354872.884286	52.447565
3261.500082	354604.763331	52.452570
3260.750897	354365.940180	52.457575
3260.382776	354098.297961	52.462580
3259.296271	353855.377588	52.467585
3258.874003	353618.204410	52.472589
3258.258360	353350.063074	52.477594
3257.572492	353096.488756	52.482599
3256.652637	352844.553575	52.487604
3255.785484	352602.101718	52.492609
3255.357318	352345.581740	52.497613
3255.011716	352097.955061	52.502618
3253.748578	351852.890155	52.507623
3253.804136	351609.498877	52.512628
3252.734595	351362.365072	52.517633
3252.431443	351103.274323	52.522637
3251.733789	350853.152535	52.527642
3251.095827	350603.172859	52.532647
3250.348589	350355.856236	52.537652
3249.591566	350107.649253	52.542657
3249.072650	349848.408517	52.547661
3248.412248	349601.634692	52.552666
3247.435409	349344.958268	52.557671
3246.861005	349088.038837	52.562676
3246.207698	348847.521645	52.567681
3245.541219	348590.487229	52.572685
3244.733187	348337.851771	52.577690
3244.528536	348076.745987	52.582695
3243.794249	347839.444256	52.587700
3242.832598	347585.608026	52.592705
3242.343788	347330.499601	52.597709
3241.763074	347076.269962	52.602714
3241.074639	346828.648477	52.607719
3240.636284	346570.067121	52.612724
3239.360924	346327.423259	52.617729
3239.300435	346068.678075	52.622733
3238.330008	345820.027850	52.627738
3237.699081	345567.072170	52.632743
3237.115772	345309.271729	52.637748
3236.056202	345081.249670	52.642753
3235.252987	344824.576389	52.647757
3234.595684	344558.155614	52.652762
3233.962477	344324.412477	52.657767
3233.469044	344073.235866	52.662772
3232.871729	343835.437971	52.667777
3232.270503	343577.785571	52.672781
3232.015025	343334.000816	52.677786
3231.396220	343091.672540	52.682791
3230.836319	342821.105053	52.687796
3229.372769	342570.075649	52.692801
3229.124124	342314.067562	52.697805
3228.630112	342058.148131	52.702810
3227.380765	341812.783602	52.707815
3227.048936	341565.847481	52.712820
3226.123031	341302.738594	52.717825
3225.838314	341051.720175	52.722829
3224.813116	340815.811018	52.727834
3224.219695	340567.792303	52.732839
3223.516461	340302.531202	52.737844
3222.583365	340065.459173	52.742849
3221.772528	339822.384847	52.747853
3221.508511	339576.499329	52.752858
3221.067188	339321.935025	52.757863
3220.419824	339077.075558	52.762868
3219.728450	338832.247580	52.767873
3219.281403	338576.306615	52.772877
3218.397270	338329.878045	52.777882
3217.676599	338079.782434	52.782887
3217.260849	337814.796544	52.787892
3216.122940	337568.685280	52.792897
3215.632286	337322.878012	52.797901
3215.371205	337078.866400	52.802906
3214.113851	336815.053374	52.807911
3213.686010	336559.610686	52.812916
3213.026060	336320.063449	52.817921
3212.712800	336070.863199	52.822925
3211.693042	335815.587706	52.827930
3211.011589	335561.479685	52.832935
3210.628809	335303.810354	52.837940
3209.785029	335056.090479	52.842945
3208.841800	334801.231875	52.847949
3208.621131	334562.678203	52.852954
3207.783389	334309.608597	52.857959
3207.034812	334053.494487	52.862964
3206.381872	333807.165609	52.867969
3205.831020	333560.845177	52.872973
3205.007366	333311.613905	52.877978
3203.923945	333057.967674	52.882983
3203.273820	332811.176641	52.887988
3202.782569	332567.007294	52.892993
3202.147327	332320.314054	52.897997
3201.531572	332078.683136	52.903002
3200.695801	331834.031188	52.908007
3200.276582	331587.632245	52.913012
3199.565729	331346.752248	52.918017
3198.851506	331092.124207	52.923021
3198.248684	330849.163325	52.928026
3197.464166	330601.087667	52.933031
3197.038707	330356.620493	52.938036
3196.076759	330118.984085	52.943041
3195.500278	329864.431895	52.948045
3194.875062	329618.339071	52.953050
3194.590070	329377.970919	52.958055
3194.032280	329114.604287	52.963060
3192.890985	328870.856596	52.968065
3192.124400	328619.563699	52.973069
3191.556454	328372.235747	52.978074
3190.728471	328140.427743	52.983079
3190.421271	327881.549123	52.988084
3189.686233	327650.386922	52.993089
3188.958609	327396.054181	52.998093
3188.630933	327137.405497	53.003098
3187.743461	326898.321639	53.008103
3186.935625	326646.723441	53.013108
3186.014348	326406.701432	53.018113
3185.668861	326151.795067	53.023117
3185.121998	325903.386748	53.028122
3184.251893	325665.696824	53.033127
3183.841304	325408.226909	53.038132
3182.941314	325166.797543	53.043137
3182.234913	324928.163003	53.048141
3181.767416	324675.206386	53.053146
3181.124874	324424.695496	53.058151
3180.454439	324181.877526	53.063156
3179.556204	323932.805988	53.068161
3178.898415	323691.588666	53.073165
3177.978648	323438.699901	53.078170
3177.334098	323207.612725	53.083175
3177.158426	322949.436134	53.088180
3176.477997	322710.485712	53.093185
3176.026964	322465.947710	53.098189
3175.351163	322214.340777	53.103194
3174.343370	321960.977866	53.108199
3173.660153	321712.451549	53.113204
3172.919024	321479.389072	53.118209
3172.441278	321220.033031	53.123213
3171.642548	320979.339778	53.128218
3170.982777	320728.006200	53.133223
3170.427851	320478.743239	53.138228
3169.701347	320242.416102	53.143233
3168.745005	319989.752457	53.148237
3168.512475	319741.073046	53.153242
3167.527112	319497.197172	53.158247
3167.434742	319250.505811	53.163252
3166.563275	318992.478908	53.168257
3166.049103	318735.566053	53.173261
3165.299283	318501.300681	53.178266
3164.729732	318259.163679	53.183271
3164.112257	317992.843947	53.188276
3163.154602	317757.336506	53.193281
3162.297803	317504.166698	53.198285
3161.984033	317249.127905	53.203290
3161.217355	317008.393987	53.208295
3160.760782	316756.024680	53.213300
3159.656669	316514.935547	53.218305
3159.301875	316255.444632	53.223309
3158.756699	316006.601395	53.228314
3157.844200	315773.144644	53.233319
3157.172505	315507.336106	53.238324
3156.598059	315255.720154	53.243329
3155.952246	315011.677573	53.248333
3155.255351	314762.702552	53.253338
3154.433154	314511.887914	53.258343
3154.110028	314264.787820	53.263348
3153.271549	314009.747581	53.268353
3152.622813	313756.968464	53.273357
3152.099471	313509.669129	53.278362
3151.104893	313274.335489	53.283367
3150.856187	313001.858556	53.288372
3149.736351	312772.807821	53.293377
3148.968053	312517.702051	53.298381
3148.293465	312264.541615	53.303386
3147.852104	312021.274786	53.308391
3147.220580	311772.639076	53.313396
3146.377765	311543.109102	53.318401
3145.706652	311295.395335	53.323405
3145.494035	311035.512838	53.328410
3144.846577	310795.331756	53.333415
3144.133533	310547.062804	53.338420
3143.449949	310286.845729	53.343425
3142.614387	310039.460895	53.348429
3141.729152	309786.277435	53.353434
3140.864954	309557.791015	53.358439
3140.580586	309298.552684	53.363444
3140.001823	309048.604162	53.368449
3139.320886	308816.471334	53.373453
3138.460568	308557.628153	53.378458
3137.839310	308319.296946	53.383463
3137.044279	308074.040798	53.388468
3136.512838	307824.693500	53.393473
3135.556764	307580.887934	53.398477
3135.255424	307339.855885	53.403482
3134.232952	307101.152978	53.408487
3133.924694	306841.073023	53.413492
3132.914417	306604.022533	53.418497
3132.606261	306365.790970	53.423501
3132.056399	306110.458927	53.428506
3131.055232	305869.687727	53.433511
3130.584613	305632.550131	53.438516
3129.990130	305377.605757	53.443521
3129.645304	305127.714551	53.448525
3128.589867	304872.434737	53.453530
3127.779075	304630.434364	53.458535
3126.972373	304380.360257	53.463540
3126.120230	304138.823978	53.468545
3125.581807	303898.892938	53.473549
3125.037209	303653.869285	53.478554
3124.336635	303423.996718	53.483559
3124.010639	303173.258754	53.488564
3123.009325	302920.258881	53.493569
3122.645074	302685.391536	53.498573
3122.008716	302433.020685	53.503578
3121.193082	302195.295401	53.508583
3120.973531	301934.097399	53.513588
3119.769887	301711.865331	53.518593
3119.126834	301457.100125	53.523597
3118.983284	301194.488225	53.528602
3117.963691	300958.576000	53.533607
3117.419008	300715.635940	53.538612
3116.493691	300471.991758	53.543617
3115.831074	300218.628364	53.548621
3115.230606	299978.548303	53.553626
3114.416115	299737.916038	53.558631
3113.724002	299494.080737	53.563636
3113.125760	299249.389837	53.568641
3112.665218	299019.116432	53.573645
3112.072183	298762.149072	53.578650
3111.408545	298513.520153	53.583655
3110.725601	298269.019571	53.588660
3110.113666	298023.743417	53.593665
3109.404991	297778.660514	53.598669
3108.922274	297523.583965	53.603674
3107.987090	297284.953923	53.608679
3107.546142	297026.915929	53.613684
3106.740082	296779.886185	53.618689
3105.946571	296536.470465	53.623693
3105.506778	296284.237792	53.628698
3104.704053	296048.513991	53.633703
3104.005655	295782.263763	53.638708
3102.972522	295550.752458	53.643713
3102.571736	295304.777324	53.648717
3102.047528	295056.707651	53.653722
3101.267853	294832.591878	53.658727
3100.894119	294572.655553	53.663732
3100.158968	294341.401383	53.668737
3099.270180	294083.481501	53.673741
3098.729561	293827.008799	53.678746
3098.090289	293595.000132	53.683751
3097.365952	293345.508564	53.688756
3096.582452	293105.882000	53.693761
3096.464364	292871.370727	53.698765
3095.541653	292606.476476	53.703770
3094.722911	292362.474334	53.708775
3093.892722	292104.415667	53.713780
3093.302943	291864.680822	53.718785
3092.375083	291624.591772	53.723789
3091.998942	291380.926122	53.728794
3091.446567	291131.023091	53.733799
3090.630212	290894.761344	53.738804
3090.250219	290654.431907	53.743809
3089.516243	290404.556945	53.748813
3088.967302	290143.191990	53.753818
3087.873677	289908.705091	53.758823
3087.347040	289669.467669	53.763828
3086.893304	289412.747596	53.768833
3086.166037	289175.986438	53.773837
3085.530448	288923.445986	53.778842
3084.868792	288676.486920	53.783847
3084.282804	288425.440824	53.788852
3083.361190	288186.061017	53.793857
3082.816588	287946.443097	53.798861
3082.444936	287699.182720	53.803866
3081.363842	287448.952813	53.808871
3081.009084	287197.461722	53.813876
3080.252861	286956.272127	53.818881
3079.952562	286700.162364	53.823885
3079.077302	286440.858040	53.828890
3078.305877	286204.509296	53.833895
3077.643572	285950.442831	53.838900
3076.751047	285700.996896	53.843905
3075.985131	285458.840120	53.848909
3075.708284	285204.279237	53.853914
3075.031021	284963.483430	53.858919
3074.349533	284719.046216	53.863924
3073.715717	284458.912943	53.868929
3072.812285	284212.855158	53.873933
3072.126050	283966.839280	53.878938
3071.444262	283728.539442	53.883943
3070.904283	283473.229756	53.888948
3069.994986	283242.376951	53.893953
3069.403692	282990.717114	53.898957
3069.457541	282735.083892	53.903962
3067.892602	282505.302345	53.908967
3067.708178	282253.323119	53.913972
3067.329583	281990.932531	53.918977
3066.625981	281751.820349	53.923981
3065.710905	281500.262089	53.928986
3065.124497	281245.009760	53.933991
3064.428268	280993.493097	53.938996
3063.618620	280744.260984	53.944001
3063.189292	280499.731182	53.949005
3062.514494	280249.051356	53.954010
3061.761239	279999.810106	53.959015
3061.243691	279751.422881	53.964020
3060.204787	279512.337650	53.969025
3059.591833	279251.511386	53.974029
3059.370546	278998.900294	53.979034
3058.238476	278754.048339	53.984039
3057.891171	278496.439828	53.989044
3057.206571	278255.642846	53.994049
3056.468622	278009.022015	53.999053
3056.057499	277752.034731	54.004058
3055.249071	277509.219780	54.009063
3054.285371	277249.849460	54.014068
3053.772869	276998.277439	54.019073
3052.661725	276752.581470	54.024077
3052.109397	276505.472688	54.029082
3051.186503	276278.517105	54.034087
3050.864412	276019.172508	54.039092
3050.263664	275781.392801	54.044097
3049.814460	275540.074472	54.049101
3049.535169	275286.224274	54.054106
3048.625390	275034.409470	54.059111
3047.741834	274778.668396	54.064116
3047.077824	274533.156350	54.069121
3046.545157	274286.451991	54.074125
3045.790020	274033.339363	54.079130
3044.902571	273783.533126	54.084135
3044.438884	273535.315295	54.089140
3043.860651	273287.344844	54.094145
3042.870280	273046.570803	54.099149
3042.440859	272799.824827	54.104154
3041.779592	272550.212197	54.109159
3041.005513	272301.992764	54.114164
3040.579331	272062.912394	54.119169
3039.773478	271809.477087	54.124173
3039.145531	271547.711008	54.129178
3038.150453	271327.949446	54.134183
3037.843887	271066.514660	54.139188
3036.936976	270820.557835	54.144193
3036.293782	270581.919685	54.149197
3036.111471	270333.785391	54.154202
3035.132873	270077.168930	54.159207
3034.548811	269827.442957	54.164212
3033.773202	269584.139928	54.169217
3032.857172	269333.218737	54.174221
3032.654274	269093.059717	54.179226
3031.946030	268841.265386	54.184231
3031.568211	268589.877291	54.189236
3030.613385	268336.237560	54.194241
3029.635055	268086.829389	54.199245
3029.285611	267824.485828	54.204250
3028.394720	267593.299280	54.209255
3028.162785	267353.833260	54.214260
3027.649836	267100.022328	54.219265
3026.746777	266845.229086	54.224269
3026.329908	266594.026443	54.229274
3025.453695	266345.035969	54.234279
3024.863448	266080.286560	54.239284
3024.014482	265827.701074	54.244289
3023.034927	265588.405277	54.249293
3022.903650	265321.393458	54.254298
3022.121647	265076.616541	54.259303
3021.395114	264828.163606	54.264308
3020.564251	264582.095875	54.269313
3019.940199	264330.316216	54.274317
3019.413144	264075.974586	54.279322
3018.469907	263828.804573	54.284327
3017.680778	263576.669569	54.289332
3017.100905	263338.967405	54.294337
3016.224075	263102.331132	54.299341
3015.806216	262843.287064	54.304346
3015.225121	262595.525836	54.309351
3014.386402	262335.071671	54.314356
3013.901437	262094.222881	54.319361
3013.175654	261853.514275	54.324365
3012.710244	261588.697617	54.329370
3011.777902	261354.618272	54.334375
3011.718829	261089.992437	54.339380
3010.706148	260842.683023	54.344385
3009.732935	260597.736080	54.349389
3009.415094	260359.205341	54.354394
3008.713236	260106.779344	54.359399
3007.806967	259849.572572	54.364404
3007.435613	259613.037461	54.369409
3006.273132	259366.771855	54.374413
3006.073178	259112.229996	54.379418
3005.203457	258864.339565	54.384423
3004.769349	258620.582570	54.389428
3004.145741	258367.662072	54.394433
3003.295810	258124.964639	54.399437
3002.828337	257875.279792	54.404442
3002.186558	257626.055754	54.409447
3001.696743	257368.174512	54.414452
3000.829464	257125.429964	54.419457
3000.063296	256878.263841	54.424461
2999.415398	256608.209694	54.429466
2998.680855	256369.010400	54.434471
2997.538448	256128.882721	54.439476
2997.457838	255864.291579	54.444481
2996.484405	255631.166666	54.449485
2995.789677	255384.398476	54.454490
2995.149625	255141.416529	54.459495
2994.918268	254891.825160	54.464500
2993.777185	254649.126867	54.469505
2993.007278	254403.314089	54.474509
2992.801759	254154.127055	54.479514
2991.927924	253902.601317	54.484519
2991.372633	253657.392211	54.489524
2990.926392	253412.038835	54.494529
2989.747395	253164.713504	54.499533
2989.568488	252918.529006	54.504538
2988.697283	252675.612310	54.509543
2987.929622	252417.043010	54.514548
2987.524428	252180.445370	54.519553
2986.508212	251928.180940	54.524557
2986.221940	251673.967741	54.529562
2985.311959	251442.773542	54.534567
2984.564854	251191.384406	54.539572
2983.952016	250936.154427	54.544577
2983.260300	250700.648346	54.549581
2982.443711	250452.887572	54.554586
2981.464736	250212.054266	54.559591
2981.185671	249963.266904	54.564596
2980.714022	249718.203029	54.569601
2980.104361	249478.280098	54.574605
2979.455343	249228.330087	54.579610
2979.033315	248990.313642	54.584615
2978.487829	248741.035624	54.589620
2977.765445	248488.042509	54.594625
2977.258951	248239.319405	54.599629
2976.466799	247982.849347	54.604634
2975.846830	247742.268692	54.609639
2974.993652	247481.632761	54.614644
2974.532258	247231.121620	54.619649
2973.523856	246980.391921	54.624653
2973.120310	246723.200476	54.629658
2972.374691	246474.721994	54.634663
2971.570591	246218.842706	54.639668
2971.056049	245964.165868	54.644673
2970.257954	245708.617631	54.649677
2969.747112	245464.662147	54.654682
2969.191042	245215.188255	54.659687
2968.343395	244958.808925	54.664692
2967.915050	244705.343164	54.669697
2966.779402	244459.247481	54.674701
2966.463899	244196.724648	54.679706
2965.782654	243964.996783	54.684711
2964.901663	243715.882769	54.689716
2964.376203	243450.822717	54.694721
2963.365117	243203.054493	54.699725
2962.955295	242955.446226	54.704730
2962.235389	242716.443773	54.709735
2961.703978	242458.542430	54.714740
2961.069343	242203.306317	54.719745
2960.194803	241957.658028	54.724749
2959.672157	241705.944846	54.729754
2959.120670	241450.875415	54.734759
2958.270326	241204.359040	54.739764
2957.943839	240964.177331	54.744769
2957.086426	240707.680989	54.749773
2956.509926	240446.608061	54.754778
2955.916852	240200.613296	54.759783
2955.299011	239944.462689	54.764788
2954.716023	239692.610611	54.769793
2953.399996	239445.204070	54.774797
2953.431328	239184.954520	54.779802
2952.541310	238935.877417	54.784807
2951.969622	238690.773806	54.789812
2951.279664	238432.244451	54.794817
2950.306633	238179.719093	54.799821
2949.889745	237919.696276	54.804826
2949.368708	237670.028901	54.809831
2948.548624	237416.691737	54.814836
2947.953849	237164.567230	54.819841
2946.804941	236904.382674	54.824845
2946.513813	236659.010108	54.829850
2945.934745	236411.341055	54.834855
2945.293956	236156.807222	54.839860
2944.532334	235913.446131	54.844865
2943.750803	235649.437976	54.849869
2943.230315	235397.738882	54.854874
2942.198943	235157.808925	54.859879
2942.025702	234902.618554	54.864884
2941.613435	234639.420332	54.869889
2940.345340	234398.689395	54.874893
2939.748227	234139.519466	54.879898
2939.354925	233884.621189	54.884903
2938.633354	233632.092669	54.889908
2938.206747	233376.844517	54.894913
2937.481699	233130.225226	54.899917
2936.764705	232866.392543	54.904922
2935.720368	232616.718686	54.909927
2935.389395	232367.161712	54.914932
2934.800375	232101.426677	54.919937
2933.808808	231854.012649	54.924941
2933.005460	231596.842881	54.929946
2932.336911	231355.642772	54.934951
2931.729942	231101.447840	54.939956
2931.124684	230845.292763	54.944961
2930.672621	230598.560565	54.949965
2929.729060	230356.260851	54.954970
2929.174295	230105.803355	54.959975
2928.626228	229851.475304	54.964980
2928.054841	229597.355367	54.969985
2926.986002	229351.691808	54.974989
2926.960653	229096.442936	54.979994
2926.173486	228843.072267	54.984999
2925.673150	228587.339932	54.990004
2924.689555	228332.372322	54.995009
2923.921545	228088.268771	55.000013
2923.386063	227818.056809	55.005018
2922.521825	227567.961135	55.010023
2922.192658	227328.296906	55.015028
2921.560116	227062.138303	55.020033
2920.827350	226818.618435	55.025037
2920.377344	226560.694596	55.030042
2919.594478	226299.005147	55.035047
2918.765435	226043.307097	55.040052
2918.078641	225786.619821	55.045057
2917.048988	225536.938357	55.050061
2916.799483	225281.991132	55.055066
2915.825128	225031.971484	55.060071
2915.332646	224781.990890	55.065076
2914.890121	224525.319864	55.070081
2914.258226	224273.937163	55.075085
2913.813532	224014.289297	55.080090
2912.884601	223758.843468	55.085095
2912.196026	223492.374481	55.090100
2911.770833	223246.474397	55.095105
2910.684033	222995.664283	55.100109
2910.153127	222742.475601	55.105114
2909.155349	222485.389985	55.110119
2908.373399	222234.992355	55.115124
2908.006577	221974.066020	55.120129
2907.084164	221732.030229	55.125133
2906.751320	221489.252657	55.130138
2906.214256	221237.903020	55.135143
2905.760266	220979.858079	55.140148
2905.051104	220715.807936	55.145153
2904.227801	220467.904988	55.150157
2903.892837	220202.015311	55.155162
2902.747714	219948.755080	55.160167
2902.413404	219703.208592	55.165172
2901.843477	219435.207656	55.170177
2900.615527	219188.938813	55.175181
2900.050545	218926.005205	55.180186
2899.553799	218679.482310	55.185191
2898.727898	218428.684499	55.190196
2898.265092	218169.632590	55.195201
2897.239593	217922.114073	55.200205
2896.832727	217659.847472	55.205210
2896.286357	217410.141890	55.210215
2895.548495	217165.851819	55.215220
2895.133477	216906.542424	55.220225
2894.354593	216644.771322	55.225229
2893.434321	216395.917771	55.230234
2892.802353	216131.694175	55.235239
2892.155560	215883.041027	55.240244
2891.655228	215630.101530	55.245249
2890.590770	215383.387441	55.250253
2890.554835	215122.319161	55.255258
2889.768831	214868.256731	55.260263
2888.910903	214617.821508	55.265268
2888.693015	214355.881310	55.270273
2888.101404	214107.696934	55.275277
2887.743622	213843.247986	55.280282
2886.592275	213577.742034	55.285287
2885.856829	213313.596851	55.290292
2885.335790	213045.053062	55.295297
2884.484245	212798.174877	55.300301
2884.022905	212532.627565	55.305306
2883.066474	212277.876639	55.310311
2882.259094	212013.022659	55.315316
2881.691218	211761.546959	55.320321
2881.366630	211501.404309	55.325325
2880.919104	211240.034875	55.330330
2879.847206	210986.580166	55.335335
2879.351703	210726.429584	55.340340
2878.425239	210462.084594	55.345345
2877.345888	210211.179709	55.350349
2877.106440	209955.000954	55.355354
2876.623743	209696.163568	55.360359
2875.758122	209448.778869	55.365364
2875.003232	209183.495795	55.370369
2874.423070	208932.517063	55.375373
2873.877523	208671.110323	55.380378
2873.439636	208417.769381	55.385383
2872.606232	208149.830546	55.390388
2872.414618	207897.700039	55.395393
2871.245667	207633.418380	55.400397
2870.785397	207372.627382	55.405402
2870.191755	207103.866186	55.410407
2869.438630	206846.636475	55.415412
2868.870235	206585.407889	55.420417
2868.323055	206320.257285	55.425421
2867.766279	206056.483872	55.430426
2867.025088	205794.993451	55.435431
2866.264120	205525.858706	55.440436
2865.660264	205263.839866	55.445441
2864.549143	205003.595147	55.450445
2864.132078	204735.707712	55.455450
2863.617204	204468.676949	55.460455
2862.994917	204220.817389	55.465460
2862.495997	203954.702789	55.470465
2861.563565	203676.441034	55.475469
2861.001859	203410.797069	55.480474
2860.213594	203158.641586	55.485479
2859.384170	202887.977545	55.490484
2858.985324	202624.500365	55.495489
2857.996951	202367.098908	55.500493
2857.143781	202099.840241	55.505498
2856.897293	201836.253592	55.510503
2856.112170	201569.355758	55.515508
2855.278288	201311.769320	55.520513
2854.390780	201060.211744	55.525517
2854.174714	200790.669767	55.530522
2853.431117	200537.373881	55.535527
2852.611527	200272.587533	55.540532
2851.969123	200007.672623	55.545537
2851.047603	199757.538981	55.550541
2850.485808	199492.753820	55.555546
2850.018891	199242.830545	55.560551
2849.414656	198987.191210	55.565556
2848.694888	198719.788105	55.570561
2847.989726	198469.129976	55.575565
2847.643459	198191.897689	55.580570
2846.849387	197938.673028	55.585575
2846.212172	197682.256304	55.590580
2845.750661	197416.027778	55.595585
2844.781558	197162.223819	55.600589
2843.879344	196889.209244	55.605594
2843.151598	196633.957234	55.610599
2842.872685	196378.826277	55.615604
2842.079550	196116.092539	55.620609
2841.468164	195868.231452	55.625613
2840.495838	195607.462791	55.630618
2840.156619	195349.063685	55.635623
2839.234867	195092.552237	55.640628
2839.140978	194825.400979	55.645633
2838.122151	194573.691759	55.650637
2837.560868	194299.479195	55.655642
2836.977434	194043.161275	55.660647
2835.980585	193780.751864	55.665652
2835.635255	193524.118985	55.670657
2834.466261	193273.699748	55.675661
2834.018270	193010.902126	55.680666
2833.306854	192754.840158	55.685671
2832.666208	192505.015499	55.690676
2831.975926	192241.395175	55.695681
2831.237931	191979.870443	55.700685
2830.691893	191728.380754	55.705690
2829.964195	191475.089008	55.710695
2829.575416	191211.617368	55.715700
2829.246402	190947.857797	55.720705
2828.416011	190695.985935	55.725709
2827.723527	190418.825995	55.730714
2826.981465	190167.273722	55.735719
2826.345482	189906.062170	55.740724
2825.962334	189643.488860	55.745729
2825.192400	189376.525366	55.750733
2824.118243	189123.619021	55.755738
2823.600566	188855.549840	55.760743
2822.965170	188592.856941	55.765748
2822.319306	188329.734618	55.770753
2821.518988	188085.034550	55.775757
2821.087217	187813.433693	55.780762
2820.483629	187552.713556	55.785767
2819.469814	187294.947750	55.790772
2819.095884	187027.858656	55.795777
2818.604680	186759.835549	55.800781
2818.014755	186491.600653	55.805786
2817.056353	186238.284630	55.810791
2816.567671	185978.992791	55.815796
2815.854178	185702.462172	55.820801
2815.305922	185448.207816	55.825805
2814.261731	185182.647780	55.830810
2813.833235	184929.331489	55.835815
2813.003135	184657.787067	55.840820
2812.357514	184388.135975	55.845825
2811.769680	184138.729353	55.850829
2811.222384	183873.658122	55.855834
2810.550935	183609.943837	55.860839
2809.689981	183341.948760	55.865844
2809.321846	183079.309043	55.870849
2808.335536	182823.281810	55.875853
2807.867328	182549.962979	55.880858
2807.183899	182283.129270	55.885863
2806.465804	182023.706010	55.890868
2805.850221	181756.241481	55.895873
2805.334334	181499.409735	55.900877
2804.644936	181235.381886	55.905882
2803.903767	180970.842325	55.910887
2802.770144	180715.003502	55.915892
2802.429655	180436.844141	55.920897
2801.413439	180189.257883	55.925901
2800.991241	179932.764108	55.930906
2800.628810	179671.568809	55.935911
2799.424595	179417.466127	55.940916
2798.562738	179148.479648	55.945921
2798.279579	178901.293595	55.950925
2797.995052	178642.394561	55.955930
2797.363604	178368.975633	55.960935
2796.898058	178110.515576	55.965940
2796.562388	177844.519476	55.970945
2795.414526	177580.930444	55.975949
2794.718238	177312.412877	55.980954
2794.004135	177043.950749	55.985959
2793.435650	176781.699573	55.990964
2792.627439	176508.587996	55.995969
2792.066782	176252.660215	56.000973
2791.412542	175989.397463	56.005978
2790.435968	175718.886992	56.010983
2789.651082	175459.972671	56.015988
2789.436618	175185.198811	56.020993
2788.365200	174934.981750	56.025997
2788.069150	174671.670807	56.031002
2787.556195	174399.277007	56.036007
2786.770782	174143.703366	56.041012
2786.368151	173873.966457	56.046017
2785.728530	173606.787051	56.051021
2785.100693	173334.291514	56.056026
2784.407465	173069.400696	56.061031
2783.765995	172796.898287	56.066036
2783.194394	172509.392673	56.071041
2782.535230	172192.284032	56.076045
2781.888535	171923.959810	56.081050
2781.090948	171643.045771	56.086055
2780.399482	171376.156729	56.091060
2779.570454	171101.546579	56.096065
2778.780960	170839.725432	56.101069
2778.246783	170565.110522	56.106074
2777.935649	170302.161731	56.111079
2777.053671	170039.521332	56.116084
2776.545094	169751.822603	56.121089
2775.659297	169485.587774	56.126093
2775.172024	169215.743771	56.131098
2774.593711	168937.866612	56.136103
2773.891823	168665.542645	56.141108
2773.109672	168387.027828	56.146113
2772.519937	168112.693615	56.151117
2771.615363	167849.906553	56.156122
2771.182054	167574.139994	56.161127
2770.195567	167303.918173	56.166132
2769.314657	167039.136636	56.171137
2768.792659	166774.974052	56.176141
2767.952223	166514.042670	56.181146
2767.618905	166242.796819	56.186151
2766.833263	165979.673440	56.191156
2765.900717	165701.711005	56.196161
2765.469865	165439.806793	56.201165
2765.094565	165174.551562	56.206170
2764.102963	164911.544703	56.211175
2763.565912	164639.541842	56.216180
2763.079134	164367.800048	56.221185
2762.325058	164102.637995	56.226189
2761.861972	163835.728013	56.231194
2761.380125	163551.518445	56.236199
2760.307146	163290.964635	56.241204
2759.912717	163035.937686	56.246209
2758.924282	162764.452633	56.251213
2757.911578	162484.022686	56.256218
2757.449120	162211.187074	56.261223
2756.798903	161962.247442	56.266228
2756.310790	161687.576354	56.271233
2755.513684	161424.424174	56.276237
2754.875738	161166.308785	56.281242
2754.723786	160885.322776	56.286247
2753.551058	160617.532038	56.291252
2753.008401	160356.000235	56.296257
2752.041080	160088.333537	56.301261
2751.542643	159821.827785	56.306266
2751.393763	159551.861565	56.311271
2750.293935	159295.193338	56.316276
2749.759349	159008.307795	56.321281
2748.591499	158753.256160	56.326285
2747.750246	158490.069355	56.331290
2747.705986	158226.338781	56.336295
2746.856163	157964.873528	56.341300
2746.088818	157699.341917	56.346305
2745.711154	157442.191628	56.351309
2744.934709	157171.669571	56.356314
2744.426981	156906.776703	56.361319
2743.324708	156652.048019	56.366324
2743.136706	156371.866884	56.371329
2742.191022	156095.990274	56.376333
2741.350364	155850.149868	56.381338
2740.633094	155596.499443	56.386343
2740.211368	155322.846932	56.391348
2739.519362	155068.510040	56.396353
2738.747761	154803.878749	56.401357
2738.443600	154541.260143	56.406362
2738.075969	154265.205225	56.411367
2737.003100	154004.860778	56.416372
2736.250013	153741.645868	56.421377
2735.725441	153480.430576	56.426381
2734.858055	153213.793299	56.431386
2734.320943	152954.681402	56.436391
2733.545918	152695.926984	56.441396
2733.012607	152418.540888	56.446401
2732.229399	152159.677575	56.451405
2731.476355	151887.059017	56.456410
2731.060542	151637.712439	56.461415
2730.232540	151372.215015	56.466420
2729.552160	151103.506163	56.471425
2728.992019	150841.758183	56.476429
2728.483253	150587.973183	56.481434
2727.742645	150327.872066	56.486439
2727.204399	150058.018174	56.491444
2726.779921	149777.993669	56.496449
2725.856926	149524.968926	56.501453
2725.090383	149260.355985	56.506458
2724.728314	148982.857640	56.511463
2723.765063	148721.343199	56.516468
2723.095014	148456.467421	56.521473
2722.749341	148190.462204	56.526477
2722.084401	147916.604972	56.531482
2721.284233	147650.383965	56.536487
2720.460535	147375.361940	56.541492
2720.585096	147108.287314	56.546497
2719.261104	146841.088589	56.551501
2718.814705	146564.908225	56.556506
2718.415624	146293.437471	56.561511
2717.201823	146030.904731	56.566516
2716.753750	145749.762994	56.571521
2715.941181	145483.613091	56.576525
2715.278921	145215.789656	56.581530
2714.669413	144948.824277	56.586535
2713.726804	144678.724406	56.591540
2713.329293	144401.780262	56.596545
2712.539687	144148.472503	56.601549
2711.854424	143889.864153	56.606554
2711.747608	143601.419360	56.611559
2710.713588	143350.266234	56.616564
2710.021679	143073.571260	56.621569
2709.334960	142812.189435	56.626573
2708.665870	142529.739665	56.631578
2707.970749	142264.196128	56.636583
2707.474042	142000.465883	56.641588
2706.750436	141728.629218	56.646593
2706.084401	141463.494666	56.651597
2705.053041	141216.538995	56.656602
2704.885004	140920.696273	56.661607
2704.031081	140659.753347	56.666612
2703.040886	140383.015798	56.671617
2702.263302	140125.394286	56.676621
2701.532201	139855.583166	56.681626
2701.145510	139601.156814	56.686631
2700.411601	139336.864909	56.691636
2700.020484	139070.996437	56.696641
2699.107367	138807.766731	56.701645
2698.455184	138546.772184	56.706650
2698.263930	138279.875453	56.711655
2697.456242	138018.465537	56.716660
2696.688664	137744.499560	56.721665
2696.284136	137487.083212	56.726669
2695.482391	137204.171107	56.731674
2694.704156	136941.368631	56.736679
2694.129301	136683.465449	56.741684
2693.514751	136403.694723	56.746689
2692.727676	136141.790112	56.751693
2692.050863	135883.122528	56.756698
2691.631666	135599.758849	56.761703
2690.527411	135337.009795	56.766708
2690.073820	135071.962371	56.771713
2689.278192	134811.163621	56.776717
2688.479769	134525.812632	56.781722
2687.961780	134278.846471	56.786727
2687.146247	134011.922592	56.791732
2686.679579	133729.778880	56.796737
2686.046514	133462.488240	56.801741
2685.107555	133214.823094	56.806746
2684.525800	132953.067384	56.811751
2683.875820	132681.379028	56.816756
2683.372673	132421.355969	56.821761
2682.359036	132176.696704	56.826765
2682.134362	131904.173591	56.831770
2681.554957	131632.001450	56.836775
2680.670706	131368.491959	56.841780
2679.771477	131098.890571	56.846785
2679.220275	130835.968384	56.851789
2678.621827	130590.799870	56.856794
2678.295483	130309.582524	56.861799
2677.480009	130045.198197	56.866804
2676.619795	129769.113205	56.871809
2676.035094	129510.654130	56.876813
2675.625552	129247.216436	56.881818
2675.235022	128980.641191	56.886823
2674.198809	128718.984287	56.891828
2673.687121	128440.063213	56.896833
2673.163160	128172.856488	56.901837
2672.187716	127917.433364	56.906842
2671.999393	127644.971557	56.911847
2670.828752	127367.334166	56.916852
2670.180350	127095.280917	56.921857
2669.225918	126831.851080	56.926861
2668.320230	126574.702298	56.931866
2668.030799	126305.851111	56.936871
2667.249110	126051.125907	56.941876
2666.780193	125778.193838	56.946881
2666.114610	125521.575751	56.951885
2665.541030	125254.507074	56.956890
2664.938250	124984.740841	56.961895
2664.296669	124738.094897	56.966900
2663.541271	124461.107197	56.971905
2662.803655	124187.230631	56.976909
2662.156357	123927.361381	56.981914
2661.961660	123660.223128	56.986919
2660.704433	123397.535113	56.991924
2660.487242	123123.802857	56.996929
2659.969646	122855.834980	57.001933
2658.566922	122597.076124	57.006938
2658.140363	122332.641734	57.011943
2657.492221	122067.216612	57.016948
2656.792376	121791.885840	57.021953
2656.140428	121534.745249	57.026957
2655.536564	121266.718272	57.031962
2655.244071	121003.837689	57.036967
2654.375268	120746.701081	57.041972
2653.616933	120484.299467	57.046977
2653.049546	120202.336776	57.051981
2652.118354	119944.627563	57.056986
2651.565296	119683.528241	57.061991
2650.661252	119415.999476	57.066996
2650.006441	119150.744634	57.072001
2649.202883	118901.214415	57.077005
2648.782758	118634.613661	57.082010
2648.171055	118357.261167	57.087015
2647.263089	118113.245919	57.092020
2646.869430	117840.980681	57.097025
2646.191878	117574.552292	57.102029
2645.631680	117314.937987	57.107034
2644.950728	117062.435539	57.112039
2644.397114	116800.368953	57.117044
2643.757961	116513.335610	57.122049
2643.176649	116268.213494	57.127053
2642.275495	115997.051169	57.132058
2642.202050	115713.383730	57.137063
2641.055764	115454.439797	57.142068
2640.429566	115185.362499	57.147073
2639.902902	114923.806072	57.152077
2638.998226	114659.278466	57.157082
2638.737938	114390.881550	57.162087
2637.772194	114133.166546	57.167092
2637.336849	113865.310721	57.172097
2636.504510	113583.831114	57.177101
2635.753827	113325.696854	57.182106
2635.504974	113046.250577	57.187111
2634.537771	112779.531480	57.192116
2633.969042	112502.293409	57.197121
2633.637772	112235.720536	57.202125
2632.636873	111961.888750	57.207130
2632.252086	111690.684835	57.212135
2631.167555	111424.696973	57.217140
2630.714727	111151.472690	57.222145
2629.633625	110884.068627	57.227149
2629.191004	110617.917957	57.232154
2628.664489	110349.981274	57.237159
2627.815868	110074.515487	57.242164
2627.019578	109801.741387	57.247169
2626.509768	109534.794550	57.252173
2625.366468	109283.484705	57.257178
2624.916022	109004.820545	57.262183
2624.109005	108756.470572	57.267188
2623.473074	108496.059074	57.272193
2623.134666	108228.483927	57.277197
2622.123019	107977.978924	57.282202
2621.836643	107705.407710	57.287207
2621.199441	107445.071183	57.292212
2620.694908	107170.180256	57.297217
2620.050162	106925.040266	57.302221
2619.108317	106640.777225	57.307226
2618.606928	106381.788478	57.312231
2617.983189	106117.980969	57.317236
2617.074360	105852.546585	57.322241
2616.625572	105587.080323	57.327245
2615.491335	105335.347108	57.332250
2615.445951	105059.931848	57.337255
2614.555232	104788.993221	57.342260
2614.020031	104521.839598	57.347265
2613.535644	104252.777698	57.352269
2612.723481	103987.342509	57.357274
2612.181747	103706.331027	57.362279
2611.458510	103451.951689	57.367284
2610.867862	103180.622367	57.372289
2610.140404	102905.752661	57.377293
2609.399623	102646.696784	57.382298
2609.194198	102360.408220	57.387303
2608.295697	102098.845956	57.392308
2607.446482	101838.319147	57.397313
2606.682184	101557.996712	57.402317
2605.891038	101287.082723	57.407322
2605.401922	101036.517607	57.412327
2604.008189	100765.882809	57.417332
2603.808186	100492.676996	57.422337
2603.607885	100233.061246	57.427341
2602.548435	99966.455070	57.432346
2601.859411	99701.011114	57.437351
2600.933627	99438.347840	57.442356
2600.350865	99173.318106	57.447361
2600.097909	98904.668244	57.452365
2599.222770	98649.122464	57.457370
2598.731694	98384.068306	57.462375
2597.924525	98126.272347	57.467380
2597.306096	97855.885130	57.472385
2597.069426	97581.343494	57.477389
2595.894392	97324.198410	57.482394
2595.319750	97047.541400	57.487399
2594.628220	96784.725688	57.492404
2593.855023	96530.557449	57.497409
2593.310778	96262.910874	57.502413
2592.475415	95998.484542	57.507418
2592.033310	95729.350461	57.512423
2590.910493	95479.498480	57.517428
2590.870531	95209.076605	57.522433
2590.108014	94933.769004	57.527437
2589.033333	94674.818223	57.532442
2588.611389	94415.196271	57.537447
2588.101196	94137.290218	57.542452
2587.374652	93881.946074	57.547457
2586.799984	93619.174280	57.552461
2585.813007	93353.744257	57.557466
2585.264806	93089.040503	57.562471
2584.136585	92834.355440	57.567476
2583.805894	92567.860656	57.572481
2583.380022	92309.227755	57.577485
2582.644927	92060.639900	57.582490
2582.154293	91793.184322	57.587495
2581.164073	91526.483273	57.592500
2580.605348	91260.256022	57.597505
2580.246695	91004.252779	57.602509
2579.327606	90746.768938	57.607514
2578.869199	90466.789528	57.612519
2577.965427	90234.277342	57.617524
2577.459117	89944.954063	57.622529
2577.183006	89678.992927	57.627533
2576.285167	89415.625188	57.632538
2575.492223	89152.199640	57.637543
2575.051060	88889.279445	57.642548
2574.199325	88618.629626	57.647553
2573.819390	88353.639480	57.652557
2572.679990	88091.695500	57.657562
2572.511025	87818.525780	57.662567
2571.764842	87554.345225	57.667572
2571.117182	87280.364345	57.672577
2570.674979	87009.676177	57.677581
2569.527554	86750.564453	57.682586
2568.650890	86481.485903	57.687591
2567.937475	86215.858659	57.692596
2567.438041	85958.111826	57.697601
2566.904228	85683.664275	57.702605
2566.338810	85438.973254	57.707610
2565.991282	85154.956765	57.712615
2564.859616	84892.061919	57.717620
2564.333446	84632.326053	57.722625
2563.566785	84357.995936	57.727629
2562.901301	84097.350627	57.732634
2562.090082	83829.265092	57.737639
2561.452304	83566.054940	57.742644
2560.821380	83296.844756	57.747649
2560.085785	83036.147639	57.752653
2559.417660	82772.039560	57.757658
2558.648662	82526.324444	57.762663
2558.240292	82255.127604	57.767668
2557.333928	81988.056705	57.772673
2557.150156	81716.755205	57.777677
2556.215047	81473.867383	57.782682
2555.657355	81197.561825	57.787687
2554.827050	80932.222560	57.792692
2554.038950	80675.486139	57.797697
2553.725230	80411.617977	57.802701
2552.738048	80157.631889	57.807706
2552.460581	79890.120741	57.812711
2551.247775	79626.582543	57.817716
2550.553661	79362.553605	57.822721
2550.027272	79095.149260	57.827725
2549.195823	78849.126416	57.832730
2548.340387	78585.056994	57.837735
2548.003593	78333.049779	57.842740
2547.376707	78081.623915	57.847745
2547.142042	77821.825506	57.852749
2546.053291	77565.511394	57.857754
2545.711893	77287.354800	57.862759
2545.071463	77047.095757	57.867764
2544.484762	76782.962698	57.872769
2543.652270	76507.327696	57.877773
2542.911944	76250.252631	57.882778
2542.278576	75991.193407	57.887783
2541.753580	75722.382149	57.892788
2540.881984	75460.389648	57.897793
2540.379481	75187.520733	57.902797
2539.409600	74932.532575	57.907802
2539.119511	74671.718944	57.912807
2538.506671	74404.732139	57.917812
2537.941625	74140.991337	57.922817
2537.323215	73871.826820	57.927821
2536.501284	73617.801218	57.932826
2535.814209	73347.026513	57.937831
2535.124946	73089.578329	57.942836
2534.461407	72821.296687	57.947841
2533.903205	72547.224601	57.952845
2533.014938	72294.968456	57.957850
2532.803897	72018.834185	57.962855
2532.079966	71768.934179	57.967860
2531.221362	71498.642594	57.972865
2530.696295	71226.914604	57.977869
2529.630017	70971.206955	57.982874
2528.879891	70693.510712	57.987879
2528.203446	70435.474237	57.992884
2527.671199	70169.025653	57.997889
2526.911492	69919.623479	58.002893
2526.038150	69661.729724	58.007898
2525.836466	69404.587967	58.012903
2525.137709	69147.883068	58.017908
2523.703764	68881.062896	58.022913
2523.410839	68624.015542	58.027917
2522.758229	68369.935659	58.032922
2521.985390	68108.607409	58.037927
2521.088190	67853.794031	58.042932
2520.678257	67596.506467	58.047937
2520.312888	67343.591456	58.052941
2519.318267	67096.381089	58.057946
2518.604975	66840.516429	58.062951
2517.949145	66588.866928	58.067956
2517.118981	66333.185841	58.072961
2516.596587	66080.039950	58.077965
2515.769808	65826.749326	58.082970
2515.699425	65572.629727	58.087975
2514.840337	65327.671799	58.092980
2513.988979	65076.639834	58.097985
2513.592609	64818.234709	58.102989
2512.657057	64581.641275	58.107994
2512.223256	64307.446890	58.112999
2511.449639	64054.927966	58.118004
2510.413410	63807.133351	58.123009
2509.931651	63553.112130	58.128013
2509.307049	63303.622030	58.133018
2508.814308	63050.622357	58.138023
2508.198230	62814.481462	58.143028
2507.439020	62560.185099	58.148033
2506.985384	62297.334207	58.153037
2505.946756	62049.493297	58.158042
2505.547398	61785.672218	58.163047
2504.883948	61536.331876	58.168052
2503.951977	61286.936103	58.173057
2503.585737	61036.083288	58.178061
2502.976860	60790.333895	58.183066
2502.449305	60530.134078	58.188071
2501.517711	60276.453005	58.193076
2500.753026	60021.156739	58.198081
2500.666011	59766.031918	58.203085
2499.277654	59520.656995	58.208090
2499.070511	59259.414352	58.213095
2498.145226	59014.972895	58.218100
2497.447690	58763.604868	58.223105
2496.715198	58504.583078	58.228109
2495.764439	58263.770089	58.233114
2495.308885	58002.043274	58.238119
2494.381038	57765.911015	58.243124
2493.849385	57523.873339	58.248129
2493.763447	57258.389156	58.253133
2492.597587	57021.031868	58.258138
2491.885122	56769.221739	58.263143
2491.517441	56528.133238	58.268148
2490.717422	56281.495894	58.273153
2489.914700	56025.839806	58.278157
2488.993466	55785.386802	58.283162
2488.488063	55540.497572	58.288167
2488.034054	55308.989510	58.293172
2487.336327	55057.399910	58.298177
2487.064011	54802.467956	58.303181
2485.926994	54557.147746	58.308186
2485.020716	54312.838507	58.313191
2484.392949	54072.772908	58.318196
2483.792565	53834.345242	58.323201
2483.091713	53580.662796	58.328205
2482.394002	53345.351621	58.333210
2482.002910	53098.553270	58.338215
2481.295551	52869.749001	58.343220
2480.500038	52620.160922	58.348225
2480.023446	52379.185708	58.353229
2479.235077	52150.036376	58.358234
2478.495858	51903.917029	58.363239
2477.942493	51657.423554	58.368244
2476.882904	51416.797265	58.373249
2476.329267	51176.353428	58.378253
2475.395755	50948.444681	58.383258
2475.091551	50705.651722	58.388263
2474.375379	50469.653395	58.393268
2473.580534	50247.258586	58.398273
2473.221219	49999.868162	58.403277
2472.502933	49763.971243	58.408282
2471.845951	49527.055396	58.413287
2471.533464	49285.586439	58.418292
2470.376368	49049.075755	58.423297
2470.235647	48797.314479	58.428301
2469.300283	48576.047878	58.433306
2468.599494	48319.308137	58.438311
2468.010244	48082.910121	58.443316
2467.080646	47854.812617	58.448321
2466.744020	47602.457247	58.453325
2465.962481	47365.618510	58.458330
2465.195265	47130.207246	58.463335
2464.495144	46895.620379	58.468340
2463.766060	46654.936600	58.473345
2463.194542	46420.462207	58.478349
2462.126003	46194.252263	58.483354
2461.305900	45962.787073	58.488359
2460.889322	45735.385333	58.493364
2460.081657	45506.960540	58.498369
2459.962461	45266.986673	58.503373
2459.143827	45034.575216	58.508378
2458.064629	44803.334083	58.513383
2457.563247	44579.484073	58.518388
2457.132380	44343.769154	58.523393
2456.482584	44096.751198	58.528397
2455.577343	43882.515630	58.533402
2454.964395	43636.538849	58.538407
2454.373927	43410.864810	58.543412
2453.402724	43192.884929	58.548417
2452.983901	42947.073746	58.553421
2452.322677	42729.284580	58.558426
2451.631109	42499.998640	58.563431
2450.809078	42274.085229	58.568436
2450.058790	42040.068216	58.573441
2449.413996	41828.653301	58.578445
2448.590766	41612.706358	58.583450
2447.818873	41379.587150	58.588455
2447.180854	41157.928016	58.593460
2446.163779	40942.703235	58.598465
2445.586906	40712.755777	58.603469
2444.852456	40515.402373	58.608474
2444.122107	40304.969964	58.613479
2443.353251	40097.287555	58.618484
2442.500084	39888.038567	58.623489
2441.639485	39671.943403	58.628493
2440.626298	39477.145563	58.633498
2440.398805	39282.005649	58.638503
2439.140819	39088.928338	58.643508
2437.967790	38902.083919	58.648513
2437.201695	38721.520728	58.653517
2436.572410	38532.958055	58.658522
2435.161736	38362.638348	58.663527
2434.118933	38200.932366	58.668532
2433.269115	38044.189252	58.673537
2432.724116	37875.379573	58.678541
2431.743320	37729.075422	58.683546
2430.617986	37588.141311	58.688551
2429.843536	37442.801175	58.693556
2429.190386	37290.462904	58.698561
2428.548460	37150.481653	58.703565
2427.851714	37021.732695	58.708570
2426.912521	36891.161201	58.713575
2425.907827	36757.401971	58.718580
2425.387252	36632.846684	58.723585
2424.736811	36504.551137	58.728589
2423.749602	36391.175187	58.733594
2423.035535	36258.729977	58.738599
2422.465822	36140.562090	58.743604
2421.589172	36030.224662	58.748609
2420.973684	35904.592942	58.753613
2420.483561	35795.147251	58.758618
2419.687933	35670.754939	58.763623
2418.964793	35567.710770	58.768628
2418.170276	35466.009318	58.773633
2417.749065	35343.363403	58.778637
2417.079185	35237.714537	58.783642
2416.022788	35138.071689	58.788647
2415.406002	35024.445557	58.793652
2414.945143	34930.658291	58.798657
2414.397790	34808.652673	58.803661
2413.678386	34706.240659	58.808666
2412.815880	34598.304770	58.813671
2412.360849	34497.574754	58.818676
2411.593199	34383.340020	58.823681
2410.930526	34285.561587	58.828685
2410.090821	34186.827236	58.833690
2409.429133	34078.824951	58.838695
2409.195576	33987.312687	58.843700
2408.278988	33906.405786	58.848705
2407.559006	33794.931541	58.853709
2407.241407	33697.730823	58.858714
2406.498063	33591.061060	58.863719
2405.736148	33490.676586	58.868724
2404.938302	33398.523789	58.873729
2404.625830	33288.568618	58.878733
2403.657664	33192.178822	58.883738
2403.128927	33095.759418	58.888743
2402.441732	32983.370471	58.893748
2401.343823	32901.221980	58.898753
2401.146906	32796.689347	58.903757
2400.205047	32716.689842	58.908762
2399.575591	32617.391081	58.913767
2399.134660	32521.607410	58.918772
2398.292305	32438.252939	58.923777
2397.894295	32338.647363	58.928781
2397.082837	32251.583411	58.933786
2396.273111	32156.282248	58.938791
2395.879424	32066.375103	58.943796
2395.038675	31971.252167	58.948801
2394.236048	31883.326003	58.953805
2393.645412	31786.457928	58.958810
2393.090974	31694.699531	58.963815
2392.511661	31610.033970	58.968820
2391.284730	31531.163071	58.973825
2390.976284	31433.903125	58.978829
2390.537873	31354.334468	58.983834
2389.567558	31265.736643	58.988839
2389.178846	31177.069196	58.993844
2388.600003	31081.105632	58.998849
2388.092380	30995.261050	59.003853
2387.195842	30896.073497	59.008858
2386.677986	30812.628421	59.013863
2385.966509	30716.566361	59.018868
2385.190769	30631.703156	59.023873
2384.830701	30532.753481	59.028877
2383.993408	30442.500552	59.033882
2383.333969	30365.654585	59.038887
2382.829790	30262.762036	59.043892
2382.175618	30167.953359	59.048897
2381.438529	30085.136089	59.053901
2380.548579	29996.646156	59.058906
2379.918554	29910.853537	59.063911
2379.244540	29815.536571	59.068916
2378.423080	29733.195810	59.073921
2378.284890	29650.276302	59.078925
2377.592125	29557.158333	59.083930
2377.020780	29462.406981	59.088935
2376.777071	29370.149437	59.093940
2375.663762	29284.823824	59.098945
2375.136742	29183.494737	59.103949
2374.333459	29098.631241	59.108954
2373.675486	29009.027683	59.113959
2373.140593	28927.133738	59.118964
2372.013092	28830.265627	59.123969
2371.677814	28740.024680	59.128973
2371.027883	28646.375892	59.133978
2370.209738	28556.598013	59.138983
2369.519379	28464.898278	59.143988
2369.231470	28381.569791	59.148993
2368.707634	28272.963007	59.153997
2367.722745	28194.842405	59.159002
2367.122976	28107.015013	59.164007
2366.339638	27997.629745	59.169012
2365.504892	27919.316051	59.174017
2364.637776	27831.989097	59.179021
2364.432826	27740.364988	59.184026
2363.687953	27657.637164	59.189031
2363.303700	27571.712093	59.194036
2362.067229	27482.122624	59.199041
2361.634627	27385.173509	59.204045
2360.903038	27311.065003	59.209050
2360.225231	27210.417474	59.214055
2359.653311	27136.016696	59.219060
2358.407451	27051.966302	59.224065
2358.037252	26959.756755	59.229069
2357.882022	26877.102135	59.234074
2356.739323	26794.104574	59.239079
2356.120441	26713.467283	59.244084
2355.523947	26635.747579	59.249089
2354.897902	26548.491238	59.254093
2354.064024	26468.353678	59.259098
2353.537147	26382.561818	59.264103
2353.188962	26285.114679	59.269108
2352.361800	26213.548209	59.274113
2351.559515	26128.643300	59.279117
2351.261125	26043.160576	59.284122
2350.423776	25959.578695	59.289127
2349.747210	25873.370227	59.294132
2348.887595	25790.451433	59.299137
2348.243594	25711.101012	59.304141
2347.620853	25622.640833	59.309146
2346.702179	25550.569013	59.314151
2346.381355	25459.767598	59.319156
2345.552714	25378.023556	59.324161
2344.997831	25290.397908	59.329165
2344.474243	25206.550651	59.334170
2343.650849	25129.983819	59.339175
2342.917718	25057.121911	59.344180
2342.014834	24967.420932	59.349185
2341.793825	24890.206907	59.354189
2341.146338	24817.442283	59.359194
2340.194002	24733.396207	59.364199
2339.871836	24642.158983	59.369204
2338.876286	24566.798044	59.374209
2338.084477	24499.859776	59.379213
2337.800116	24413.776245	59.384218
2337.176328	24337.594578	59.389223
2336.630842	24242.032750	59.394228
2335.402496	24181.725061	59.399233
2335.005711	24084.340885	59.404237
2334.472328	24009.780316	59.409242
2333.411605	23933.978642	59.414247
2332.911019	23861.547286	59.419252
2332.105786	23771.935474	59.424257
2331.489301	23699.090498	59.429261
2330.842248	23622.003881	59.434266
2330.126722	23543.179396	59.439271
2329.783971	23471.316244	59.444276
2328.574362	23392.703527	59.449281
2328.394313	23304.654268	59.454285
2327.866083	23244.177521	59.459290
2326.985723	23165.452912	59.464295
2326.799445	23085.599195	59.469300
2325.712824	23002.319516	59.474305
2325.044567	22917.458625	59.479309
2324.521176	22850.295233	59.484314
2323.722481	22772.082363	59.489319
2323.085307	22680.713684	59.494324
2322.392042	22615.663613	59.499329
2321.830236	22539.312560	59.504333
2320.774746	22451.996718	59.509338
2320.162010	22377.300858	59.514343
2320.098835	22305.679752	59.519348
2319.191039	22236.151913	59.524353
2318.109991	22142.030778	59.529357
2317.609382	22083.459375	59.534362
2317.049106	22004.823224	59.539367
2316.415267	21923.432439	59.544372
2315.380565	21857.737706	59.549377
2315.215238	21783.618783	59.554381
2314.444051	21704.383552	59.559386
2313.563663	21635.206167	59.564391
2313.288045	21553.443864	59.569396
2312.622376	21475.998777	59.574401
2311.655702	21404.638749	59.579405
2311.020304	21336.887656	59.584410
2310.243465	21250.028542	59.589415
2310.071923	21174.727567	59.594420
2309.040370	21110.579805	59.599425
2308.585700	21026.771353	59.604429
2307.936936	20950.585879	59.609434
2307.066009	20878.373784	59.614439
2306.589948	20808.888393	59.619444
2305.802144	20745.548652	59.624449
2305.188156	20655.387717	59.629453
2304.583524	20581.011349	59.634458
2303.928344	20510.834861	59.639463
2303.286938	20437.890465	59.644468
2302.480163	20364.635125	59.649473
2301.850674	20286.751202	59.654477
2301.624716	20199.063273	59.659482
2300.524581	20134.711300	59.664487
2299.558124	20055.050355	59.669492
2298.960666	19983.573499	59.674497
2298.396793	19905.523565	59.679501
2297.994736	19855.012142	59.684506
2297.085804	19778.083367	59.689511
2296.603986	19690.544654	59.694516
2295.635226	19638.129616	59.699521
2294.976593	19562.023120	59.704525
2294.456866	19489.499631	59.709530
2293.753430	19426.370533	59.714535
2293.186433	19345.602637	59.719540
2292.515528	19273.755032	59.724545
2292.036302	19209.774170	59.729549
2291.104574	19133.752154	59.734554
2290.505751	19062.533142	59.739559
2290.070809	18987.629438	59.744564
2289.543650	18922.030732	59.749569
2288.589551	18848.106439	59.754573
2288.223648	18767.824742	59.759578
2287.268521	18701.713434	59.764583
2286.418345	18616.994244	59.769588
2285.888298	18556.419794	59.774593
2285.138652	18476.018903	59.779597
2284.193394	18413.707464	59.784602
2283.605760	18361.778600	59.789607
2283.271408	18283.009657	59.794612
2282.351877	18209.817453	59.799617
2281.650477	18141.832945	59.804621
2281.351103	18073.721423	59.809626
2280.434525	18011.053014	59.814631
2279.815510	17926.828232	59.819636
2279.006082	17862.808586	59.824641
2278.568352	17797.807076	59.829645
2278.079520	17724.750928	59.834650
2277.542812	17658.723930	59.839655
2276.957332	17581.738534	59.844660
2276.078630	17521.628960	59.849665
2275.401905	17434.404799	59.854669
2274.658685	17363.704696	59.859674
2273.868194	17297.872033	59.864679
2273.321973	17231.310031	59.869684
2272.523397	17157.150682	59.874689
2271.932990	17083.923437	59.879693
2271.682982	17020.290569	59.884698
2270.660452	16956.039314	59.889703
2270.458780	16866.592276	59.894708
2269.420084	16815.619650	59.899713
2268.799460	16732.044527	59.904718
2268.395379	16661.036331	59.909722
2267.273573	16601.248910	59.914727
2266.695048	16520.038563	59.919732
2265.904880	16460.030373	59.924737
2265.636573	16383.589259	59.929742
2264.879101	16317.100422	59.934746
2264.065559	16244.485977	59.939751
2263.601347	16164.785468	59.944756
2262.607796	16107.882236	59.949761
2261.915242	16030.403290	59.954766
2261.460771	15957.792932	59.959770
2260.625063	15901.327057	59.964775
2260.397346	15834.526893	59.969780
2259.753778	15758.959378	59.974785
2259.160207	15687.498843	59.979790
2258.157501	15618.939455	59.984794
2257.350090	15548.328301	59.989799
2256.927081	15476.734846	59.994804
2256.388413	15405.705147	59.999809
2255.494741	15337.920845	60.004814
2254.827150	15266.973306	60.009818
2253.947618	15195.871578	60.014823
2253.564547	15122.425138	60.019828
2252.809014	15065.584600	60.024833
2252.002351	14987.654191	60.029838
2251.237498	14927.482136	60.034842
2250.575049	14876.225324	60.039847
2249.959335	14802.198371	60.044852
2249.351236	14738.471940	60.049857
2248.512381	14683.773963	60.054862
2247.910824	14609.521263	60.059866
2247.224726	14554.822503	60.064871
2246.525774	14492.781050	60.069876
2246.106529	14423.027310	60.074881
2245.470331	14355.741890	60.079886
2245.116090	14293.549100	60.084890
2243.992657	14226.549094	60.089895
2244.104139	14143.031440	60.094900
2243.206663	14080.515212	60.099905
2242.063121	14019.057301	60.104910
2241.441608	13941.404790	60.109914
2240.472792	13887.826939	60.114919
2240.153447	13823.310458	60.119924
2238.995264	13754.758147	60.124929
2238.458213	13697.613215	60.129934
2237.898843	13633.121309	60.134938
2237.308824	13572.029094	60.139943
2237.075938	13511.261239	60.144948
2236.310170	13447.619238	60.149953
2235.463294	13374.637797	60.154958
2234.913027	13311.342352	60.159962
2233.787657	13246.162787	60.164967
2233.695234	13175.302992	60.169972
2232.809108	13126.886901	60.174977
2232.432178	13047.357446	60.179982
2232.163508	12976.578220	60.184986
2230.929362	12925.926356	60.189991
2230.621239	12853.801600	60.194996
2230.000821	12779.565930	60.200001
2228.845205	12713.498988	60.205006
2228.363445	12656.848998	60.210010
2227.588373	12593.037460	60.215015
2227.296107	12512.494418	60.220020
2226.286561	12449.684370	60.225025
2225.965008	12378.590813	60.230030
2225.295479	12310.193287	60.235034
2224.284789	12241.654890	60.240039
2223.758074	12168.321503	60.245044
2223.080872	12105.329569	60.250049
2222.030758	12041.042602	60.255054
2221.756252	11981.012823	60.260058
2221.134968	11913.144428	60.265063
2220.527503	11845.549727	60.270068
2219.530692	11784.729262	60.275073
2219.039738	11727.096297	60.280078
2218.525502	11651.105089	60.285082
2217.610583	11595.331041	60.290087
2216.961951	11522.778007	60.295092
2216.363980	11454.549546	60.300097
2215.785185	11400.928280	60.305102
2215.016716	11338.453483	60.310106
2214.250464	11272.627157	60.315111
2213.849713	11207.450899	60.320116
2213.277091	11136.386039	60.325121
2212.709345	11076.647415	60.330126
2212.335052	11006.316271	60.335130
2211.347743	10948.032804	60.340135
2210.691570	10870.117977	60.345140
2209.945000	10810.056285	60.350145
2208.974434	10747.637300	60.355150
2208.522130	10673.288244	60.360154
2207.613353	10603.325839	60.365159
2207.056514	10546.432532	60.370164
2206.305971	10489.928768	60.375169
2205.571163	10421.439887	60.380174
2205.092464	10355.922655	60.385178
2204.261031	10296.649290	60.390183
2203.984995	10227.775678	60.395188
2203.232148	10169.177158	60.400193
2202.772576	10092.779196	60.405198
2201.921532	10039.546015	60.410202
2200.935160	9982.457100	60.415207
2200.296570	9906.044700	60.420212
2199.899931	9861.523622	60.425217
2199.169542	9789.512226	60.430222
2198.628108	9714.947330	60.435226
2197.899473	9663.363129	60.440231
2197.347259	9583.937093	60.445236
2196.710068	9530.376332	60.450241
2195.750954	9460.731770	60.455246
2195.277355	9390.663374	60.460250
2194.290060	9351.261477	60.465255
2194.094550	9269.539542	60.470260
2193.223389	9215.070309	60.475265
2192.267991	9144.824279	60.480270
2191.863502	9082.927126	60.485274
2191.166583	9030.112907	60.490279
2190.368517	8975.294110	60.495284
2189.846996	8902.415617	60.500289
2189.428177	8832.312346	60.505294
2188.858686	8776.003662	60.510298
2187.726468	8711.829166	60.515303
2187.530587	8645.651301	60.520308
2186.546174	8587.630974	60.525313
2185.789850	8525.725677	60.530318
2185.580866	8451.348235	60.535322
2184.747386	8402.226236	60.540327
2184.312465	8333.476855	60.545332
2183.505868	8271.070971	60.550337
2182.780949	8199.022579	60.555342
2182.095615	8132.470638	60.560346
2181.351075	8067.093547	60.565351
2181.007957	8005.166665	60.570356
2180.212024	7941.599259	60.575361
2179.515312	7875.474679	60.580366
2178.891133	7807.320993	60.585370
2178.441604	7744.526585	60.590375
2177.730667	7682.511093	60.595380
2176.714182	7618.330048	60.600385
2176.263578	7540.963942	60.605390
2175.431708	7480.765458	60.610394
2174.560088	7429.053502	60.615399
2173.806171	7349.893003	60.620404
2173.446006	7286.397306	60.625409
2172.722887	7242.881237	60.630414
2171.993900	7179.582556	60.635418
2171.426244	7115.000382	60.640423
2170.884028	7049.284870	60.645428
2170.157902	6983.538877	60.650433
2169.571019	6929.397332	60.655438
2169.116812	6861.896232	60.660442
2168.233232	6798.444644	60.665447
2167.566345	6720.895466	60.670452
2166.947083	6672.813230	60.675457
2165.695482	6602.779216	60.680462
2165.632173	6539.658459	60.685466
2164.615332	6481.149046	60.690471
2164.050853	6411.803591	60.695476
2163.258337	6357.557934	60.700481
2162.621882	6292.540653	60.705486
2162.294185	6232.268036	60.710490
2161.036853	6179.712184	60.715495
2160.819439	6120.049598	60.720500
2160.150349	6060.859605	60.725505
2159.186877	5998.854937	60.730510
2158.731670	5944.147914	60.735514
2157.946368	5884.630013	60.740519
2157.415664	5815.276472	60.745524
2157.142526	5762.128988	60.750529
2156.196624	5701.589850	60.755534
2155.530953	5634.138937	60.760538
2154.685217	5575.826811	60.765543
2154.222408	5512.091559	60.770548
2154.014341	5449.507147	60.775553
2152.765574	5396.561519	60.780558
2151.886519	5330.786402	60.785562
2151.665578	5280.233581	60.790567
2151.066767	5207.515608	60.795572
2150.004473	5166.307312	60.800577
2149.756856	5099.452669	60.805582
2149.250357	5029.631272	60.810586
2148.015205	4973.579866	60.815591
2147.646238	4907.328200	60.820596
2147.614091	4843.764903	60.825601
2146.496074	4789.162594	60.830606
2145.798464	4719.066977	60.835610
2144.975804	4662.665804	60.840615
2144.313848	4579.703274	60.845620
2143.473389	4535.324957	60.850625
2142.659087	4477.501965	60.855630
2142.583054	4399.402752	60.860634
2141.393398	4353.677340	60.865639
2141.036053	4300.389961	60.870644
2140.484071	4240.321163	60.875649
2139.582139	4180.663035	60.880654
2138.778501	4109.835552	60.885658
2138.185957	4050.154890	60.890663
2137.916601	3997.577056	60.895668
2136.952076	3944.899142	60.900673
2136.256641	3877.198383	60.905678
2135.847543	3805.734844	60.910682
2134.951610	3749.502592	60.915687
2134.173738	3688.297612	60.920692
2133.591223	3634.646172	60.925697
2132.770667	3575.798562	60.930702
2132.262323	3517.603527	60.935706
2131.216312	3459.433312	60.940711
2130.883533	3405.742296	60.945716
2130.223624	3369.030286	60.950721
2129.702438	3301.638913	60.955726
2129.172501	3250.626342	60.960730
2128.233455	3191.227336	60.965735
2127.766700	3122.399979	60.970740
2127.088972	3066.589179	60.975745
2126.073120	2992.078571	60.980750
2125.525985	2945.955949	60.985754
2124.750559	2893.596436	60.990759
2124.547785	2826.812836	60.995764
2124.020062	2786.190416	61.000769
2122.870540	2726.028650	61.005774
2122.660689	2656.885928	61.010778
2121.461260	2598.193059	61.015783
2120.623004	2554.437862	61.020788
2120.205682	2496.139398	61.025793
2119.459014	2439.518666	61.030798
2118.856217	2395.509729	61.035802
2118.431827	2336.086953	61.040807
2117.826750	2280.582267	61.045812
2117.031965	2223.970796	61.050817
2116.368662	2173.188177	61.055822
2115.582237	2111.401324	61.060826
2114.827949	2047.046856	61.065831
2114.418859	2000.609613	61.070836
2113.517908	1937.870972	61.075841
2112.977316	1894.378848	61.080846
2112.378062	1833.207713	61.085850
2111.456552	1790.421366	61.090855
2110.902293	1721.534859	61.095860
2110.185714	1677.986147	61.100865
2109.532535	1615.031375	61.105870
2108.938042	1574.713897	61.110874
2108.392456	1515.760791	61.115879
2107.674576	1472.332756	61.120884
2106.895708	1422.234241	61.125889
2105.915471	1359.433404	61.130894
2105.397166	1307.772113	61.135898
2104.544331	1263.828356	61.140903
2104.517726	1200.004800	61.145908
2103.578941	1157.928770	61.150913
2102.725806	1105.110197	61.155918
2102.114807	1059.313566	61.160922
2101.427541	1009.433759	61.165927
2101.082018	958.974761	61.170932
2100.256577	908.462782	61.175937
2099.723059	853.090178	61.180942
2098.751538	805.206887	61.185946
2097.968531	757.721196	61.190951
2097.368246	703.203432	61.195956
2096.438941	659.924924	61.200961
2095.604103	623.694672	61.205966
2095.434762	568.648563	61.210970
2094.582739	526.687548	61.215975
2093.909101	466.812868	61.220980
2093.034156	436.542338	61.225985
2092.351379	389.281644	61.230990
2092.080117	342.862527	61.235994
2090.900219	311.077935	61.240999
2090.785183	253.517125	61.246004
2089.863855	221.899849	61.251009
2089.170066	179.509471	61.256014
2088.506188	132.927835	61.261018
2087.618700	100.531205	61.266023
2086.884078	67.064919	61.271028
2086.239760	35.104489	61.276033
2085.539260	-3.942882	61.281038
2084.577224	-34.887692	61.286042
2083.207027	-56.126704	61.291047
2078.460424	26.639599	61.296052
2075.660130	104.469353	61.301057
2076.866449	91.530388	61.306062
2078.682343	93.304776	61.311066
2079.299606	87.567883	61.316071
2079.552515	70.655111	61.321076
2078.529666	76.462654	61.326081
2076.450294	85.618433	61.331086
2076.203368	83.995577	61.336090
2075.776284	92.420821	61.341095
2075.216546	86.895939	61.346100
2074.258867	89.329658	61.351105
2072.892866	91.165884	61.356110
2073.285010	85.691787	61.361114
2072.525912	82.573329	61.366119
2071.580152	86.911606	61.371124
2070.929378	89.137357	61.376129
2070.803957	90.953322	61.381134
2070.151940	91.329587	61.386138
2069.667161	91.258285	61.391143
2068.804546	92.377569	61.396148
2068.311501	91.131224	61.401153
2067.235431	94.217641	61.406158
2066.950107	90.989305	61.411162
2065.865021	99.030142	61.416167
2064.912523	95.578116	61.421172
2063.960531	97.599370	61.426177
2063.083540	98.749321	61.431182
2063.262487	89.820989	61.436186
2062.403073	99.855462	61.441191
2061.986873	96.837122	61.446196
2061.702893	92.834324	61.451201
2060.539633	106.001403	61.456206
2059.972638	100.349944	61.461210
2060.234236	98.255320	61.466215
2059.219206	104.884773	61.471220
2058.169987	96.670141	61.476225
2057.288597	99.555363	61.481230
2057.150393	94.594339	61.486234
2056.365113	98.883504	61.491239
2055.170174	92.838139	61.496244
2055.469839	96.592439	61.501249
2054.336305	97.188621	61.506254
2053.276381	99.641729	61.511258
2053.024811	105.115586	61.516263
2052.390934	99.309171	61.521268
2052.208772	96.797715	61.526273
2050.791219	104.181726	61.531278
2050.482471	97.251433	61.536282
2049.762081	103.566058	61.541287
2048.836728	104.621191	61.546292
2048.375847	102.709031	61.551297
2047.399076	106.935554	61.556302
2046.914518	101.662082	61.561306
2046.376066	106.416681	61.566311
2045.404621	93.249339	61.571316
2044.736597	95.630791	61.576321
2043.954394	91.623492	61.581326
2043.670860	87.623781	61.586330
2042.914926	98.636847	61.591335
2042.747806	97.646273	61.596340
2041.961821	94.401208	61.601345
2040.737938	96.266933	61.606350
2040.397766	97.741685	61.611354
2040.109819	93.588139	61.616359
2039.367067	94.622179	61.621364
2038.451362	101.715246	61.626369
2037.287146	97.308125	61.631374
2037.788520	95.604357	61.636378
2036.772196	106.303957	61.641383
2035.834390	91.473978	61.646388
2035.242486	100.668099	61.651393
2034.126129	102.888907	61.656398
2033.727595	93.159710	61.661402
2033.612975	96.099857	61.666407
2032.673126	104.328959	61.671412
2032.015494	86.694975	61.676417
2031.206461	96.663112	61.681422
2030.804912	92.760976	61.686426
2030.075921	90.457730	61.691431
2029.544692	106.162633	61.696436
2028.701344	91.536853	61.701441
2027.758404	113.217260	61.706446
2027.272314	101.026247	61.711450
2027.012705	103.800181	61.716455
2026.279028	93.056627	61.721460
2025.918119	101.091348	61.726465
2025.026660	95.245403	61.731470
2024.370699	99.422592	61.736474
2022.718485	95.944446	61.741479
2022.175596	105.067717	61.746484
2022.439299	89.091462	61.751489
2021.772150	100.897805	61.756494
2020.814317	90.405864	61.761498
2019.669464	90.510293	61.766503
2019.225594	100.958196	61.771508
2019.343785	94.945700	61.776513
2017.738383	99.721415	61.781518
2017.290375	101.500277	61.786522
2016.401756	98.284124	61.791527
2016.536942	102.017218	61.796532
2015.806831	97.162757	61.801537
2014.422006	108.441222	61.806542
2014.320686	93.120536	61.811546
2013.575133	97.980545	61.816551
2012.798241	94.904349	61.821556
2012.265606	98.511634	61.826561
2011.723415	98.540914	61.831566
2011.143088	91.590661	61.836570
2010.629629	99.780475	61.841575
2009.747599	94.738827	61.846580
2009.382375	96.296402	61.851585
2007.628373	92.247823	61.856590
2007.536368	93.959143	61.861594
2007.057046	105.245270	61.866599
2005.971327	99.986803	61.871604
2005.656606	90.425654	61.876609
2004.890534	107.760483	61.881614
2004.470164	90.144040	61.886618
2003.610142	93.536795	61.891623
2002.989794	95.589006	61.896628
2002.664876	89.033437	61.901633
2001.904990	104.492369	61.906638
2001.467242	95.783338	61.911642
2001.006451	92.723205	61.916647
1999.918729	96.174179	61.921652
1999.208853	93.793794	61.926657
1998.064099	94.011753	61.931662
1997.658532	85.130472	61.936666
1997.018497	107.089210	61.941671
1996.480169	95.748559	61.946676
1995.967915	82.889973	61.951681
1994.990990	98.477961	61.956686
1995.060896	89.630015	61.961690
1994.032651	98.302066	61.966695
1992.657661	99.356050	61.971700
1992.189883	86.999735	61.976705
1991.589912	94.367534	61.981710
1991.252731	96.469415	61.986714
1990.276843	87.495740	61.991719
1989.731145	101.682822	61.996724
1989.187696	86.936928	62.001729
1988.191003	102.660518	62.006734
1988.029562	91.294743	62.011738
1987.732797	86.341551	62.016743
1986.921168	96.885670	62.021748
1986.412885	87.402557	62.026753
1984.896277	98.917976	62.031758
1984.284242	85.386132	62.036762
1983.918933	93.396319	62.041767
1983.109839	90.793580	62.046772
1982.506021	82.255995	62.051777
1981.766070	99.425829	62.056782
1981.462695	90.187722	62.061786
1981.075683	86.264367	62.066791
1980.209298	95.155146	62.071796
1979.894722	90.441313	62.076801
1978.823747	88.685929	62.081806
1977.927333	93.910496	62.086810
1977.249419	96.812328	62.091815
1976.369093	96.352840	62.096820
1976.083208	90.518022	62.101825
1975.542656	96.990185	62.106830
1975.132376	98.461881	62.111834
1974.536750	94.372951	62.116839
1972.970111	92.232644	62.121844
1972.549622	99.223467	62.126849
1971.509051	95.687691	62.131854
1971.245970	92.047426	62.136858
1970.936175	91.327076	62.141863
1970.181435	97.375943	62.146868
1969.707304	87.912643	62.151873
1969.013331	93.415724	62.156878
1968.485713	94.027723	62.161882
1967.877102	85.998657	62.166887
1967.061639	83.846346	62.171892
1966.552229	91.742218	62.176897
1965.455912	87.448931	62.181902
1965.130686	94.564974	62.186906
1964.230855	83.306956	62.191911
1963.067692	97.525820	62.196916
1962.435027	84.891351	62.201921
1961.415497	99.390179	62.206926
1961.697094	86.019253	62.211930
1961.048853	80.808061	62.216935
1960.125678	94.376999	62.221940
1959.832981	80.860707	62.226945
1958.948955	93.018430	62.231950
1958.565004	82.684576	62.236954
1957.985440	89.226006	62.241959
1956.846781	84.447459	62.246964
1956.067350	86.933343	62.251969
1955.356954	78.204539	62.256974
1955.054969	86.245671	62.261978
1954.298689	92.887691	62.266983
1953.714057	82.234050	62.271988
1953.633677	84.437088	62.276993
1951.959549	88.641876	62.281998
1951.299930	77.083976	62.287002
1950.684722	84.143549	62.292007
1950.117193	86.816560	62.297012
1949.888239	80.081777	62.302017
1949.178199	80.820503	62.307022
1948.565372	79.929073	62.312026
1947.992107	90.682927	62.317031
1947.075797	88.374750	62.322036
1946.429666	86.916200	62.327041
1945.555038	91.184881	62.332046
1944.659057	84.865050	62.337050
1944.516506	85.415926	62.342055
1943.838658	89.703831	62.347060
1943.735137	92.741559	62.352065
1942.607248	91.113491	62.357070
1941.741851	86.411416	62.362074
1940.773540	80.170876	62.367079
1939.919444	89.483889	62.372084
1939.781878	83.111473	62.377089
1939.455661	90.571432	62.382094
1939.181950	78.852931	62.387098
1938.277152	89.066507	62.392103
1936.627669	92.305496	62.397108
1936.474344	91.142438	62.402113
1935.563393	91.410037	62.407118
1935.187205	90.572503	62.412122
1934.694514	93.848622	62.417127
1934.285159	95.342252	62.422132
1933.157950	87.818126	62.427137
1932.402358	101.685310	62.432142
1931.878038	87.546652	62.437146
1931.225842	97.871517	62.442151
1930.681768	95.620943	62.447156
1930.523710	88.568989	62.452161
1929.295153	91.499899	62.457166
1928.668852	91.236634	62.462170
1928.140031	80.828020	62.467175
1927.137806	104.952539	62.472180
1926.776562	87.730423	62.477185
1925.886294	97.208452	62.482190
1924.901876	96.864849	62.487194
1924.339725	91.545384	62.492199
1923.677043	92.293945	62.497204
1923.295273	96.850230	62.502209
1922.868079	99.283361	62.507214
1922.180482	88.002704	62.512218
1921.905149	90.619874	62.517223
1920.311935	97.263887	62.522228
1919.743873	85.368196	62.527233
1919.010404	98.183242	62.532238
1918.532786	91.776504	62.537242
1918.370024	85.026484	62.542247
1917.673196	93.989702	62.547252
1917.282602	88.914228	62.552257
1915.976354	87.756014	62.557262
1915.452579	79.730846	62.562266
1914.647076	92.815932	62.567271
1914.004724	102.035423	62.572276
1914.096464	88.054424	62.577281
1912.733602	97.419834	62.582286
1911.661266	86.671749	62.587290
1911.279365	87.741573	62.592295
1910.601945	98.466242	62.597300
1910.162940	88.981614	62.602305
1909.806154	86.852694	62.607310
1909.079287	86.630628	62.612314
1907.666340	87.946135	62.617319
1907.039065	102.994535	62.622324
1906.953314	79.771243	62.627329
1906.290482	100.159866	62.632334
1905.635805	92.018287	62.637338
1905.598313	85.284650	62.642343
1904.587179	92.654660	62.647348
1903.678397	89.944776	62.652353
1902.728305	82.630658	62.657358
1902.554623	89.965482	62.662362
1901.291480	78.462415	62.667367
1900.531263	99.590284	62.672372
1899.722654	83.907280	62.677377
1899.210285	92.916906	62.682382
1898.625627	87.006539	62.687386
1898.544853	92.964191	62.692391
1897.688818	95.642018	62.697396
1897.443636	85.625176	62.702401
1896.535472	90.138881	62.707406
1895.487799	88.878127	62.712410
1895.153216	87.387474	62.717415
1894.328025	99.363995	62.722420
1893.940085	80.409991	62.727425
1892.768286	93.646271	62.732430
1892.151140	97.178687	62.737434
1891.274212	87.394600	62.742439
1890.896523	98.342909	62.747444
1890.552400	80.212966	62.752449
1889.745745	94.010988	62.757454
1889.551267	82.478604	62.762458
1888.284704	88.777470	62.767463
1887.240451	91.761135	62.772468
1887.109303	90.676557	62.777473
1886.420990	86.346915	62.782478
1885.625057	83.934499	62.787482
1885.447349	85.579007	62.792487
1884.428812	80.115982	62.797492
1883.723465	88.550724	62.802497
1882.961058	84.516685	62.807502
1882.689002	89.126512	62.812506
1882.103295	77.444945	62.817511
1880.895213	102.873112	62.822516
1880.269551	84.546603	62.827521
1879.700178	91.061198	62.832526
1879.203252	90.468335	62.837530
1878.903491	83.560309	62.842535
1877.845817	88.939809	62.847540
1876.915417	89.382396	62.852545
1875.813930	87.753320	62.857550
1875.338047	87.649104	62.862554
1875.067017	85.128123	62.867559
1874.241204	94.488701	62.872564
1874.090380	87.151769	62.877569
1874.021444	83.280433	62.882574
1872.988931	92.274877	62.887578
1872.261049	74.590635	62.892583
1871.370432	93.823295	62.897588
1870.502813	95.014395	62.902593
1869.630368	90.463268	62.907598
1868.984676	90.740811	62.912602
1868.241931	90.631660	62.917607
1867.586330	85.402740	62.922612
1867.490202	91.630897	62.927617
1867.195313	94.798354	62.932622
1866.247885	98.750628	62.937626
1865.234476	85.728813	62.942631
1864.680738	89.796766	62.947636
1864.479495	91.058676	62.952641
1862.952028	99.218699	62.957646
1862.124612	95.563976	62.962650
1862.046810	90.205472	62.967655
1861.175042	96.525245	62.972660
1861.094482	87.880963	62.977665
1860.135825	90.868393	62.982670
1858.785443	87.708272	62.987674
1858.547229	92.121926	62.992679
1857.896048	97.060021	62.997684
1857.674765	80.801263	63.002689
1857.067024	95.819750	63.007694
1856.190860	92.051350	63.012698
1855.289928	91.606213	63.017703
1854.141808	88.730933	63.022708
1854.032611	94.245263	63.027713
1853.500894	86.163026	63.032718
1853.225559	84.008568	63.037722
1852.022026	86.738427	63.042727
1850.817697	93.180387	63.047732
1850.653844	86.339090	63.052737
1850.313707	87.203605	63.057742
1849.873724	88.818798	63.062746
1849.127867	92.333813	63.067751
1847.971660	101.164992	63.072756
1847.309329	96.323478	63.077761
1847.050649	82.014952	63.082766
1846.331669	102.054542	63.087770
1845.548393	89.514987	63.092775
1844.566345	98.868844	63.097780
1844.308175	93.124260	63.102785
1843.586175	100.344309	63.107790
1842.902682	89.034648	63.112794
1842.301282	84.588723	63.117799
1841.245313	93.396099	63.122804
1840.897070	90.406434	63.127809
1840.160443	87.470554	63.132814
1839.738553	100.906313	63.137818
1838.854275	89.691609	63.142823
1837.722466	84.696000	63.147828
1837.393239	76.542199	63.152833
1836.907342	83.721599	63.157838
1836.411121	90.374387	63.162842
1836.027744	80.303814	63.167847
1834.648538	91.931513	63.172852
1833.991875	94.147214	63.177857
1833.255739	93.010475	63.182862
1833.052118	95.455424	63.187866
1832.772720	88.943121	63.192871
1831.911989	97.471932	63.197876
1830.969948	86.778891	63.202881
1830.055059	91.552292	63.207886
1829.511055	86.677807	63.212890
1829.289697	86.772869	63.217895
1828.344189	86.956110	63.222900
1827.370351	92.757535	63.227905
1826.536070	94.224040	63.232910
1826.008631	88.525371	63.237914
1825.747633	83.386764	63.242919
1825.188563	85.815617	63.247924
1824.895547	91.874772	63.252929
1823.656980	94.567633	63.257934
1822.901339	90.726494	63.262938
1822.255374	88.632468	63.267943
1821.898522	93.159574	63.272948
1821.216236	91.375652	63.277953
1820.476119	92.018268	63.282958
1819.415745	95.308856	63.287962
1819.243483	92.557743	63.292967
1818.630081	95.255410	63.297972
1817.960513	95.992475	63.302977
1817.142547	85.260818	63.307982
1816.241075	84.766897	63.312986
1815.909742	87.344084	63.317991
1815.336688	101.068762	63.322996
1814.398561	93.320713	63.328001
1813.302486	89.828512	63.333006
1812.712040	87.634214	63.338010
1812.761806	91.764032	63.343015
1811.878444	100.562935	63.348020
1811.539427	96.141580	63.353025
1810.792510	99.702504	63.358030
1810.007553	86.903049	63.363034
1809.556959	86.752254	63.368039
1808.315290	94.348126	63.373044
1807.564836	96.452576	63.378049
1807.005569	89.961065	63.383054
1806.624944	84.549735	63.388058
1806.567958	76.926694	63.393063
1805.031853	93.525982	63.398068
1804.280561	88.220817	63.403073
1803.783931	86.959326	63.408078
1803.168387	91.139601	63.413082
1803.147644	82.703440	63.418087
1801.853261	86.931589	63.423092
1801.012927	86.602999	63.428097
1800.199599	83.296131	63.433102
1799.591432	77.566140	63.438106
1799.454073	78.554570	63.443111
1799.016791	91.861885	63.448116
1798.146477	87.862355	63.453121
1797.336525	80.707372	63.458126
1796.615949	91.106183	63.463130
1796.152334	79.659134	63.468135
1794.928937	88.351190	63.473140
1793.941922	92.082701	63.478145
1793.326630	85.995889	63.483150
1793.097261	86.500638	63.488154
1792.859685	87.005114	63.493159
1792.044189	95.137261	63.498164
1791.712328	90.516088	63.503169
1791.244970	93.469676	63.508174
1790.168613	103.276898	63.513178
1789.786481	91.514141	63.518183
1788.971841	100.240638	63.523188
1788.110929	91.415948	63.528193
1787.347076	88.492291	63.533198
1786.659076	94.998932	63.538202
1786.084117	90.648165	63.543207
1785.424645	90.622003	63.548212
1784.448955	95.324653	63.553217
1784.027940	87.163358	63.558222
1783.259090	87.493595	63.563226
1783.128580	85.588946	63.568231
1782.434631	91.812693	63.573236
1781.493158	84.494106	63.578241
1780.699577	94.959707	63.583246
1779.669205	85.573758	63.588250
1779.910949	79.208933	63.593255
1778.783970	79.425741	63.598260
1777.833068	83.321823	63.603265
1777.362911	84.990702	63.608270
1776.645249	89.262888	63.613274
1776.357483	82.543778	63.618279
1775.962816	96.670614	63.623284
1774.629383	87.080495	63.628289
1774.084147	86.884814	63.633294
1773.258737	89.685540	63.638298
1773.104961	90.096289	63.643303
1772.280447	92.169933	63.648308
1771.536752	86.811536	63.653313
1770.639107	84.691265	63.658318
1770.146367	87.663077	63.663322
1769.699974	78.852994	63.668327
1769.106128	92.656659	63.673332
1768.454402	92.205091	63.678337
1767.531509	86.094600	63.683342
1766.755327	83.992886	63.688346
1766.687183	82.734315	63.693351
1765.297339	92.853084	63.698356
1764.500630	90.787743	63.703361
1763.871235	93.212008	63.708366
1763.195261	90.372169	63.713370
1762.940840	81.662479	63.718375
1762.713041	89.188812	63.723380
1762.166032	74.963949	63.728385
1761.374922	84.957668	63.733390
1760.078738	95.600859	63.738394
1759.789974	90.447747	63.743399
1759.351064	88.377622	63.748404
1758.434270	83.064068	63.753409
1757.870595	84.791954	63.758414
1757.128422	85.324532	63.763418
1756.135779	85.549975	63.768423
1755.345385	88.914398	63.773428
1754.432433	85.900897	63.778433
1754.267299	83.039855	63.783438
1753.695592	93.232115	63.788442
1753.498885	85.374234	63.793447
1752.930908	86.191370	63.798452
1752.002750	89.456253	63.803457
1751.367392	82.350826	63.808462
1750.178694	91.892056	63.813466
1749.491240	79.196993	63.818471
1748.523190	85.752844	63.823476
1747.960796	81.248715	63.828481
1747.628443	94.315452	63.833486
1747.289767	92.100106	63.838490
1747.193305	80.304616	63.843495
1745.902524	93.526721	63.848500
1744.897782	82.369043	63.853505
1744.155432	92.596289	63.858510
1743.695217	95.531404	63.863514
1743.737683	92.035024	63.868519
1742.393062	94.266970	63.873524
1741.579256	82.875552	63.878529
1741.237667	91.310893	63.883534
1740.642317	97.004929	63.888538
1740.281953	78.573280	63.893543
1738.999268	89.569127	63.898548
1738.533551	79.733997	63.903553
1738.032208	86.586295	63.908558
1737.293149	89.395394	63.913562
1736.590356	86.985580	63.918567
1735.420311	90.205310	63.923572
1735.142313	89.328560	63.928577
1734.490796	86.934256	63.933582
1733.720408	86.274473	63.938586
1733.527660	74.945268	63.943591
1732.575877	83.124297	63.948596
1731.699087	96.397347	63.953601
1731.088841	93.646422	63.958606
1730.685301	86.598793	63.963610
1730.657561	82.571121	63.968615
1729.324944	89.799863	63.973620
1728.398579	90.584042	63.978625
1728.237886	83.527807	63.983630
1726.895631	87.370951	63.988634
1726.491711	80.296581	63.993639
1725.659223	85.542601	63.998644
1725.033675	79.293446	64.003649
1725.166163	83.577266	64.008654
1724.161064	91.830999	64.013658
1723.521336	81.594599	64.018663
1722.421731	89.495929	64.023668
1721.859017	94.959291	64.028673
1721.621992	73.680726	64.033678
1720.689042	82.033376	64.038682
1719.829077	85.460894	64.043687
1718.862417	87.112451	64.048692
1718.425635	77.662221	64.053697
1718.286118	90.739326	64.058702
1717.702726	92.134478	64.063706
1717.404745	76.220665	64.068711
1715.944362	85.197957	64.073716
1715.325544	80.625532	64.078721
1715.120116	86.683394	64.083726
1714.222472	89.459342	64.088730
1713.115121	88.077261	64.093735
1712.270147	87.505021	64.098740
1712.305611	77.203963	64.103745
1711.741364	86.914091	64.108750
1710.734531	85.511316	64.113754
1709.953990	83.033439	64.118759
1709.111890	94.911755	64.123764
1708.510348	75.394115	64.128769
1708.285903	84.804278	64.133774
1707.740355	87.335079	64.138778
1707.670009	88.834816	64.143783
1706.872839	84.856818	64.148788
1705.954295	85.201392	64.153793
1704.890002	83.304723	64.158798
1703.854422	89.491288	64.163802
1703.671869	76.451135	64.168807
1702.780039	94.140250	64.173812
1701.574349	90.898888	64.178817
1700.770616	82.624949	64.183822
1700.492298	92.899917	64.188826
1700.277639	86.259091	64.193831
1699.889299	84.278712	64.198836
1699.433756	93.403904	64.203841
1698.729771	81.902027	64.208846
1697.582930	87.101796	64.213850
1697.199875	86.446730	64.218855
1696.249128	94.669763	64.223860
1695.096594	93.613396	64.228865
1694.434673	82.410752	64.233870
1693.435436	89.569211	64.238874
1693.446693	83.630480	64.243879
1693.407920	90.117589	64.248884
1692.813110	90.950038	64.253889
1692.259838	82.905966	64.258894
1691.106625	92.247625	64.263898
1690.858847	85.481180	64.268903
1689.821964	81.992251	64.273908
1688.501933	87.512831	64.278913
1687.931556	84.287254	64.283918
1687.699748	83.776892	64.288922
1687.289733	86.109558	64.293927
1686.790545	75.060838	64.298932
1685.638521	78.941589	64.303937
1685.055342	78.354581	64.308942
1684.467004	81.239094	64.313946
1683.853139	86.768928	64.318951
1682.622575	83.563066	64.323956
1681.852061	87.875206	64.328961
1681.894838	77.667601	64.333966
1680.940916	90.858295	64.338970
1680.578133	86.272016	64.343975
1679.893686	90.043809	64.348980
1679.081132	89.734499	64.353985
1678.709267	79.655832	64.358990
1677.908281	92.271906	64.363994
1677.138153	78.021014	64.368999
1675.955571	89.182324	64.374004
1675.369685	72.877465	64.379009
1675.317214	92.669261	64.384014
1674.649103	79.184295	64.389018
1674.282301	76.364757	64.394023
1672.988561	75.818085	64.399028
1672.376569	78.586515	64.404033
1672.183387	73.639003	64.409038
1671.278693	80.676796	64.414042
1670.411103	80.584378	64.419047
1669.868356	71.638252	64.424052
1668.906592	78.815990	64.429057
1668.872894	78.244200	64.434062
1667.836058	87.356077	64.439066
1667.239298	79.503416	64.444071
1666.336378	87.009263	64.449076
1666.032502	79.576833	64.454081
1665.551768	77.336762	64.459086
1664.259716	93.611925	64.464090
1663.566350	79.337807	64.469095
1663.091143	86.750482	64.474100
1662.586628	81.420361	64.479105
1662.608505	85.478907	64.484110
1661.681718	85.704963	64.489114
1660.870791	83.711298	64.494119
1660.244137	95.107568	64.499124
1659.425741	83.943985	64.504129
1658.721609	87.881327	64.509134
1658.032303	84.267816	64.514138
1657.498148	78.529264	64.519143
1656.239266	96.216773	64.524148
1655.413143	75.055460	64.529153
1655.258719	80.370395	64.534158
1654.630079	89.223479	64.539162
1654.587531	85.914063	64.544167
1653.729756	86.636913	64.549172
1652.375528	79.882245	64.554177
1651.978972	84.962845	64.559182
1651.483761	91.063589	64.564186
1650.693715	78.640317	64.569191
1649.916436	77.939079	64.574196
1649.082938	82.294345	64.579201
1648.847027	91.204887	64.584206
1647.929248	74.815571	64.589210
1647.657234	88.115554	64.594215
1646.543761	85.006221	64.599220
1645.788647	84.296732	64.604225
1645.364423	86.603277	64.609230
1644.791958	86.807745	64.614234
1644.433672	78.657024	64.619239
1643.226432	83.494265	64.624244
1642.646503	83.840261	64.629249
1642.363789	78.586869	64.634254
1641.510896	83.203825	64.639258
1640.901612	76.486936	64.644263
1640.059589	88.871425	64.649268
1639.350041	80.664547	64.654273
1639.111090	76.813929	64.659278
1638.254337	88.552663	64.664282
1637.453404	77.832575	64.669287
1636.232112	72.997933	64.674292
1636.104402	77.617953	64.679297
1635.989562	80.129226	64.684302
1635.130010	81.232391	64.689306
1634.127447	67.362212	64.694311
1633.437781	80.004751	64.699316
1632.829016	75.660978	64.704321
1632.759470	73.519587	64.709326
1631.560085	86.481214	64.714330
1631.078664	81.114317	64.719335
1630.475360	77.204893	64.724340
1629.002817	78.023837	64.729345
1628.316369	82.724737	64.734350
1627.404824	82.560473	64.739354
1627.363357	71.416983	64.744359
1627.191062	75.287186	64.749364
1626.754014	75.993667	64.754369
1626.263176	72.498442	64.759374
1624.813618	81.410980	64.764378
1624.347411	64.205666	64.769383
1623.729294	77.817652	64.774388
1623.118282	75.699206	64.779393
1622.360778	73.212969	64.784398
1621.384947	76.734611	64.789402
1621.138091	73.728879	64.794407
1620.618644	76.348582	64.799412
1619.671991	81.015131	64.804417
1619.182656	80.868946	64.809422
1618.174360	74.617557	64.814426
1617.679538	72.236240	64.819431
1616.843512	81.954860	64.824436
1615.842120	77.687658	64.829441
1615.515254	68.618949	64.834446
1614.854901	77.972207	64.839450
1614.471525	66.968193	64.844455
1614.454315	74.347528	64.849460
1613.239472	74.948930	64.854465
1612.761793	69.597217	64.859470
1611.935832	80.255631	64.864474
1611.105841	76.535183	64.869479
1610.657752	74.174825	64.874484
1610.065866	82.906961	64.879489
1609.409603	77.408584	64.884494
1608.319423	77.346819	64.889498
1607.530092	79.116892	64.894503
1607.070407	72.611203	64.899508
1606.322969	81.707078	64.904513
1606.104835	80.554341	64.909518
1605.056763	66.407572	64.914522
1604.374135	71.707077	64.919527
1604.069558	69.891596	64.924532
1602.997227	77.621478	64.929537
1602.245791	72.937700	64.934542
1601.304413	77.250195	64.939546
1600.877704	74.211541	64.944551
1600.863583	71.323371	64.949556
1600.305122	75.423652	64.954561
1599.654537	70.704930	64.959566
1598.464756	67.058995	64.964570
1597.951715	75.002781	64.969575
1597.080382	80.027934	64.974580
1595.899387	82.350643	64.979585
1595.518337	72.869519	64.984590
1594.961735	74.184749	64.989594
1594.613980	72.626852	64.994599
1594.302077	73.250380	64.999604
1593.450343	73.450344	65.004609
1592.724641	73.316488	65.009614
1591.688460	82.284785	65.014618
1591.193938	74.004344	65.019623
1590.856763	75.056066	65.024628
1590.454723	78.152260	65.029633
1589.488399	76.298421	65.034638
1588.730406	84.142365	65.039642
1588.282933	78.475210	65.044647
1587.077506	83.782095	65.049652
1586.517752	84.955909	65.054657
1586.112333	68.355928	65.059662
1585.327066	88.371353	65.064666
1584.237428	77.839075	65.069671
1583.691891	79.220355	65.074676
1583.137071	76.664083	65.079681
1582.780338	73.232712	65.084686
1582.231766	73.632083	65.089690
1581.489130	81.861498	65.094695
1581.049456	78.692450	65.099700
1580.147873	86.250143	65.104705
1579.381523	70.825509	65.109710
1578.494218	85.945189	65.114714
1577.805380	72.291683	65.119719
1577.314520	64.745492	65.124724
1576.563042	80.201536	65.129729
1576.709885	65.000807	65.134734
1575.555460	82.580268	65.139738
1574.831438	77.559422	65.144743
1574.152120	78.686007	65.149748
1573.531805	87.889421	65.154753
1572.610853	70.236003	65.159758
1571.708065	79.701901	65.164762
1571.295817	77.239667	65.169767
1571.055100	80.587761	65.174772
1570.321423	77.815494	65.179777
1569.743877	79.354819	65.184782
1568.976748	83.199694	65.189786
1568.453249	73.007964	65.194791
1567.546249	72.134983	65.199796
1566.377189	79.101273	65.204801
1565.662182	68.561525	65.209806
1565.204768	76.829197	65.214810
1565.002865	74.770337	65.219815
1564.839730	70.463007	65.224820
1563.759834	77.694236	65.229825
1563.240857	73.716243	65.234830
1562.827033	64.990930	65.239834
1561.452002	71.851180	65.244839
1560.709848	74.548854	65.249844
1559.793172	71.031424	65.254849
1559.753824	62.921515	65.259854
1558.716433	79.678177	65.264858
1558.034785	77.006451	65.269863
1557.554244	68.209742	65.274868
1556.792018	74.037541	65.279873
1556.823778	71.164159	65.284878
1555.688958	69.838552	65.289882
1554.644112	73.727553	65.294887
1554.179951	74.890916	65.299892
1553.535724	73.280788	65.304897
1553.280510	72.570741	65.309902
1551.941272	79.964602	65.314906
1551.243784	72.168985	65.319911
1550.878903	84.308947	65.324916
1550.313883	72.578486	65.329921
1550.553096	75.665829	65.334926
1549.091019	73.075535	65.339930
1548.305165	72.566492	65.344935
1548.063364	75.134207	65.349940
1546.861817	80.051003	65.354945
1545.989221	65.125795	65.359950
1545.449929	73.409630	65.364954
1545.029955	76.565445	65.369959
1545.006548	75.342352	65.374964
1543.726912	80.686274	65.379969
1543.094856	66.916537	65.384974
1542.196756	78.876307	65.389978
1541.970799	79.798405	65.394983
1541.246744	73.850376	65.399988
1540.372630	81.760086	65.404993
1540.074468	76.023490	65.409998
1539.238603	77.507678	65.415002
1538.402367	75.215317	65.420007
1537.470748	79.666624	65.425012
1536.653020	83.484856	65.430017
1536.511309	82.766236	65.435022
1535.869110	81.310324	65.440026
1535.619166	74.525332	65.445031
1534.659492	65.654961	65.450036
1533.597644	80.647845	65.455041
1533.412330	64.695696	65.460046
1532.251129	81.908834	65.465050
1531.422730	70.289613	65.470055
1530.796137	70.669855	65.475060
1530.281177	66.998723	65.480065
1530.345162	68.043475	65.485070
1529.395217	76.137113	65.490074
1528.398399	75.202729	65.495079
1527.976862	75.838955	65.500084
1527.111556	82.320200	65.505089
1527.041019	75.557162	65.510094
1525.750213	79.456875	65.515098
1525.045062	76.645398	65.520103
1524.593793	74.559939	65.525108
1523.663282	77.470471	65.530113
1523.289950	78.941087	65.535118
1522.338055	81.374072	65.540122
1521.464264	78.423822	65.545127
1521.233571	71.057063	65.550132
1520.698841	80.639522	65.555137
1520.706803	67.887671	65.560142
1519.503089	70.860538	65.565146
1518.824083	68.820731	65.570151
1518.462058	73.036459	65.575156
1517.147077	77.072474	65.580161
1517.176828	75.366296	65.585166
1516.203304	84.570652	65.590170
1514.792627	75.391925	65.595175
1514.497344	69.099820	65.600180
1513.942810	72.114604	65.605185
1513.617619	70.184145	65.610190
1512.673105	70.222270	65.615194
1511.855315	70.631322	65.620199
1511.275356	73.090357	65.625204
1510.588823	67.002345	65.630209
1510.400998	78.483419	65.635214
1509.346202	78.726717	65.640218
1508.612651	66.947365	65.645223
1508.125913	70.902229	65.650228
1507.339916	70.960895	65.655233
1507.093947	73.745306	65.660238
1506.203453	69.564605	65.665242
1505.386896	77.471482	65.670247
1504.840781	68.404525	65.675252
1503.995968	78.181330	65.680257
1503.195837	79.212019	65.685262
1502.282231	77.203188	65.690266
1501.795146	71.168634	65.695271
1501.334891	77.848854	65.700276
1500.941553	80.558920	65.705281
1500.610008	65.964049	65.710286
1499.849994	72.635135	65.715290
1498.908396	71.498033	65.720295
1498.546083	73.745875	65.725300
1497.300428	76.025287	65.730305
1496.783428	75.634377	65.735310
1495.875118	73.730357	65.740314
1495.521270	76.194463	65.745319
1495.036936	81.541326	65.750324
1493.941589	83.836276	65.755329
1493.480597	73.678789	65.760334
1492.960572	79.753530	65.765338
1492.397709	75.662685	65.770343
1491.699771	70.864794	65.775348
1490.518857	76.276623	65.780353
1489.959550	78.601501	65.785358
1489.443303	74.008113	65.790362
1488.972394	81.380698	65.795367
1488.446911	77.756975	65.800372
1487.400516	92.823117	65.805377
1486.959217	74.574725	65.810382
1486.729617	80.530778	65.815386
1485.835872	81.475429	65.820391
1484.834200	70.375750	65.825396
1484.157162	82.981612	65.830401
1483.775464	79.295618	65.835406
1482.461341	81.286313	65.840410
1481.801290	70.033003	65.845415
1481.528702	77.233729	65.850420
1480.662933	84.232274	65.855425
1480.529598	77.113385	65.860430
1480.425703	79.984025	65.865434
1479.095773	73.711278	65.870439
1478.641267	73.032911	65.875444
1477.918592	74.182179	65.880449
1477.059000	78.059115	65.885454
1475.923348	78.979139	65.890458
1475.411059	77.152532	65.895463
1474.983801	72.431470	65.900468
1474.730406	85.933478	65.905473
1474.102930	70.666587	65.910478
1473.280167	78.954484	65.915482
1472.549845	76.842423	65.920487
1472.020860	74.277342	65.925492
1470.639251	70.124244	65.930497
1470.049809	74.183740	65.935502
1469.855858	68.971464	65.940506
1469.495695	70.558259	65.945511
1468.669450	74.857229	65.950516
1467.720896	83.959864	65.955521
1467.304901	67.172381	65.960526
1466.625013	68.715375	65.965530
1465.669291	75.053316	65.970535
1465.052003	76.671514	65.975540
1464.297216	72.612757	65.980545
1464.156171	78.439624	65.985550
1462.470945	74.155019	65.990554
1462.111453	69.790602	65.995559
1461.638224	72.133342	66.000564
1461.044583	65.863435	66.005569
1460.961627	72.387506	66.010574
1459.947485	77.353396	66.015578
1458.918332	82.124565	66.020583
1458.385568	73.577441	66.025588
1457.592133	72.926136	66.030593
1457.347630	69.899553	66.035598
1457.123323	80.314152	66.040602
1455.946150	84.843934	66.045607
1455.516160	68.224249	66.050612
1454.565950	70.046739	66.055617
1453.600427	64.687448	66.060622
1453.045005	75.616690	66.065626
1452.538186	81.137434	66.070631
1452.239564	71.424062	66.075636
1451.074171	77.396383	66.080641
1450.295107	77.982216	66.085646
1449.792604	76.359053	66.090650
1449.441274	72.704509	66.095655
1449.239082	70.719820	66.100660
1448.166578	73.064771	66.105665
1447.289866	74.006728	66.110670
1446.533517	73.702751	66.115674
1446.135790	80.194854	66.120679
1445.269809	63.657086	66.125684
1444.474625	83.134803	66.130689
1444.119506	67.253814	66.135694
1443.730747	78.776281	66.140698
1442.743995	83.367261	66.145703
1442.034808	68.083412	66.150708
1441.221451	80.390838	66.155713
1440.991405	71.008751	66.160718
1439.892949	78.660842	66.165722
1438.779785	73.876924	66.170727
1438.732150	74.660307	66.175732
1437.871042	79.338546	66.180737
1437.696868	64.078474	66.185742
1436.447948	76.470894	66.190746
1435.665739	81.947105	66.195751
1435.564443	67.284119	66.200756
1434.778288	82.468165	66.205761
1434.454043	75.665039	66.210766
1433.523209	72.534664	66.215770
1432.665220	68.195870	66.220775
1432.262023	78.694090	66.225780
1431.672263	76.659044	66.230785
1430.715360	69.024545	66.235790
1429.790960	74.789846	66.240794
1429.003166	69.558425	66.245799
1429.313477	72.513033	66.250804
1428.343995	70.937289	66.255809
1427.345433	66.922022	66.260814
1426.814742	67.203471	66.265818
1426.430612	80.466067	66.270823
1425.827338	74.137778	66.275828
1424.922832	70.274709	66.280833
1424.383163	73.009617	66.285838
1424.125888	75.161930	66.290842
1422.755649	68.767898	66.295847
1422.163409	62.489898	66.300852
1421.390676	75.434229	66.305857
1421.138966	71.642438	66.310862
1420.275101	67.640455	66.315866
1419.403794	73.684309	66.320871
1418.884783	71.817785	66.325876
1418.300185	73.210036	66.330881
1417.590408	75.754376	66.335886
1417.137589	69.725435	66.340890
1416.054680	83.250479	66.345895
1415.983168	68.133355	66.350900
1414.872357	78.059686	66.355905
1413.890383	87.503523	66.360910
1413.397321	78.596880	66.365914
1412.950189	78.854013	66.370919
1412.708874	62.436161	66.375924
1411.270189	78.069256	66.380929
1410.720322	64.092556	66.385934
1410.124021	72.106362	66.390938
1409.275806	71.780730	66.395943
1408.968419	75.492648	66.400948
1408.732475	85.051282	66.405953
1408.163927	71.490685	66.410958
1407.183170	63.661306	66.415962
1406.388233	71.929023	66.420967
1405.620211	66.085799	66.425972
1404.801881	80.046580	66.430977
1404.222001	70.040475	66.435982
1403.981107	68.509774	66.440986
1402.959132	77.292950	66.445991
1402.646160	65.924584	66.450996
1401.558182	74.898013	66.456001
1401.537848	69.677072	66.461006
1400.613924	75.014975	66.466010
1399.601903	69.372952	66.471015
1399.080783	63.375375	66.476020
1398.457783	69.135350	66.481025
1397.803427	65.366565	66.486030
1396.772113	72.866078	66.491034
1395.791370	62.037499	66.496039
1395.907091	72.022748	66.501044
1395.419364	78.071869	66.506049
1394.557201	71.114572	66.511054
1394.016551	65.596313	66.516058
1393.164028	75.667664	66.521063
1392.905813	57.629911	66.526068
1391.786659	67.455072	66.531073
1391.111611	68.424913	66.536078
1390.185372	78.615211	66.541082
1390.295157	74.026410	66.546087
1389.310507	70.426817	66.551092
1387.995918	69.516194	66.556097
1387.421310	70.228809	66.561102
1387.322059	71.126048	66.566106
1386.879573	66.331739	66.571111
1386.080856	61.283413	66.576116
1385.167064	76.222834	66.581121
1384.642995	68.576322	66.586126
1383.964201	75.895233	66.591130
1382.985854	70.254172	66.596135
1382.420852	59.542434	66.601140
1381.561343	77.827225	66.606145
1381.330119	77.822974	66.611150
1381.237928	62.450543	66.616154
1379.997578	71.303126	66.621159
1379.765069	62.711458	66.626164
1378.912123	66.737166	66.631169
1377.986921	63.698955	66.636174
1377.140678	71.843954	66.641178
1376.342283	67.631319	66.646183
1376.135973	68.329545	66.651188
1375.262173	65.549655	66.656193
1374.539804	70.147510	66.661198
1373.667013	67.714371	66.666202
1373.258912	72.880404	66.671207
1373.168405	67.982840	66.676212
1371.998174	70.510503	66.681217
1371.235723	69.534196	66.686222
1370.814719	70.085210	66.691226
1370.186070	75.917050	66.696231
1369.092571	75.663537	66.701236
1368.341929	70.457770	66.706241
1367.831052	67.716380	66.711246
1367.622459	78.090632	66.716250
1366.816594	74.741733	66.721255
1366.303444	69.253800	66.726260
1365.161267	72.134955	66.731265
1364.912600	65.127456	66.736270
1364.206338	68.339841	66.741274
1362.808225	83.384646	66.746279
1362.422116	62.095224	66.751284
1361.782228	68.897045	66.756289
1361.525298	61.403610	66.761294
1361.622562	70.172869	66.766298
1360.441909	78.721100	66.771303
1359.707295	66.036857	66.776308
1359.217162	71.584918	66.781313
1358.047729	67.502231	66.786318
1357.404960	74.980990	66.791322
1356.681351	71.682094	66.796327
1356.412596	74.679860	66.801332
1355.384478	79.662200	66.806337
1354.312048	64.398293	66.811342
1353.821019	77.531231	66.816346
1353.168198	76.715688	66.821351
1353.473710	73.666334	66.826356
1352.733335	75.346699	66.831361
1351.581601	74.902189	66.836366
1351.027031	80.192430	66.841370
1350.530085	74.414933	66.846375
1349.295695	80.850824	66.851380
1348.524201	70.832623	66.856385
1348.129025	76.360861	66.861390
1347.926581	68.164941	66.866394
1346.760593	78.223061	66.871399
1345.983843	78.669793	66.876404
1345.372651	74.335948	66.881409
1345.053295	74.702083	66.886414
1344.811866	84.674728	66.891418
1343.742631	72.133564	66.896423
1342.964685	78.137369	66.901428
1342.550224	68.284752	66.906433
1341.691771	82.859018	66.911438
1340.860805	76.246846	66.916442
1339.726618	74.156455	66.921447
1339.854356	60.901497	66.926452
1339.243370	76.748369	66.931457
1338.446523	64.326330	66.936462
1337.702968	66.609567	66.941466
1336.730167	82.810417	66.946471
1336.482638	66.101849	66.951476
1335.684761	81.294077	66.956481
1335.111010	76.079121	66.961486
1334.633295	72.857829	66.966490
1333.764249	75.667193	66.971495
1333.004900	68.452317	66.976500
1332.196372	85.558983	66.981505
1331.537692	73.324698	66.986510
1331.072910	73.456924	66.991514
1330.604123	82.757698	66.996519
1329.931848	73.162099	67.001524
1328.931105	72.288340	67.006529
1328.304906	75.314550	67.011534
1328.037511	68.280073	67.016538
1326.744360	78.530295	67.021543
1326.131340	69.660099	67.026548
1325.465930	67.047360	67.031553
1324.992252	78.829321	67.036558
1324.732775	68.483740	67.041562
1323.700253	66.241584	67.046567
1323.079242	71.357896	67.051572
1322.655911	76.275634	67.056577
1322.344608	80.631544	67.061582
1321.320660	69.762560	67.066586
1320.362840	82.029902	67.071591
1319.874880	78.297758	67.076596
1319.413681	81.116400	67.081601
1318.747533	69.135609	67.086606
1317.928754	69.675758	67.091610
1317.150994	75.616464	67.096615
1316.479147	64.852349	67.101620
1315.421911	74.123676	67.106625
1314.907471	65.923752	67.111630
1314.562191	67.255900	67.116634
1313.928228	71.611069	67.121639
1313.838302	56.599401	67.126644
1312.765066	70.315301	67.131649
1311.663851	73.765523	67.136654
1311.420356	59.691273	67.141658
1310.426862	74.682800	67.146663
1309.619050	65.496671	67.151668
1309.088496	69.351301	67.156673
1308.464907	75.996011	67.161678
1308.480409	66.691602	67.166682
1307.519900	73.252689	67.171687
1306.660477	80.329112	67.176692
1305.675068	76.925204	67.181697
1305.531586	69.953027	67.186702
1304.585091	72.661178	67.191706
1303.474831	76.902852	67.196711
1303.352667	74.191133	67.201716
1303.100077	73.920642	67.206721
1302.127151	74.567301	67.211726
1300.993978	76.379513	67.216730
1300.151910	82.625325	67.221735
1300.273000	81.248382	67.226740
1299.778175	76.252687	67.231745
1298.655568	80.054804	67.236750
1297.997900	77.683677	67.241754
1297.248540	74.841455	67.246759
1297.049725	69.937464	67.251764
1296.150087	77.324617	67.256769
1295.327613	81.187821	67.261774
1294.746937	77.426272	67.266778
1294.170678	72.553908	67.271783
1293.753358	72.213420	67.276788
1292.432359	71.860499	67.281793
1292.107510	69.583109	67.286798
1291.679605	79.094991	67.291802
1290.839585	84.801191	67.296807
1290.562951	66.474666	67.301812
1289.925223	75.460119	67.306817
1288.477333	73.504779	67.311822
1287.966270	65.917727	67.316826
1287.030422	68.783454	67.321831
1286.655057	64.383751	67.326836
1286.590514	71.038920	67.331841
1285.825557	69.618361	67.336846
1285.166089	57.677530	67.341850
1284.228074	70.050525	67.346855
1283.587933	71.585668	67.351860
1282.397730	74.545453	67.356865
1281.631071	68.304686	67.361870
1281.512739	60.437588	67.366874
1280.557107	75.378949	67.371879
1280.673068	66.880118	67.376884
1279.776601	58.472882	67.381889
1278.761810	65.807384	67.386894
1278.339698	64.125747	67.391898
1277.754083	71.054566	67.396903
1276.842920	68.217578	67.401908
1275.896397	60.734460	67.406913
1275.343100	69.509379	67.411918
1275.266183	70.139733	67.416922
1274.401425	65.778423	67.421927
1273.672118	59.385075	67.426932
1272.769138	68.969335	67.431937
1272.472861	69.931018	67.436942
1271.981098	68.501718	67.441946
1270.580127	65.122904	67.446951
1269.872849	53.875620	67.451956
1269.431658	68.135971	67.456961
1268.898587	74.799408	67.461966
1269.151339	74.596796	67.466970
1267.577588	70.403409	67.471975
1267.141645	61.855147	67.476980
1266.421403	77.093381	67.481985
1265.958240	70.768094	67.486990
1265.111753	55.537706	67.491994
1264.392967	81.593007	67.496999
1263.776000	64.260420	67.502004
1262.594956	69.707049	67.507009
1261.595593	69.340848	67.512014
1261.506864	69.298182	67.517018
1260.943586	67.886563	67.522023
1261.072699	70.406357	67.527028
1259.827906	69.035296	67.532033
1258.677078	67.154159	67.537038
1258.449394	63.957781	67.542042
1257.485518	76.144098	67.547047
1257.272498	68.076025	67.552052
1256.502919	62.136915	67.557057
1255.407422	74.326815	67.562062
1255.327726	80.423031	67.567066
1254.615744	69.611704	67.572071
1253.603926	61.571307	67.577076
1252.773543	68.510664	67.582081
1252.444614	59.549598	67.587086
1252.241972	59.923992	67.592090
1251.294423	67.258850	67.597095
1250.237100	63.169430	67.602100
1249.680508	67.181166	67.607105
1249.255009	66.432001	67.612110
1248.908526	71.693898	67.617114
1247.781578	71.549828	67.622119
1247.033178	72.003119	67.627124
1246.786383	71.779019	67.632129
1245.796662	72.461483	67.637134
1245.398261	67.213943	67.642138
1244.371746	75.351372	67.647143
1244.068324	67.412788	67.652148
1243.665883	67.055750	67.657153
1242.274304	61.650766	67.662158
1241.875912	60.739605	67.667162
1241.340782	75.019632	67.672167
1240.804445	66.976166	67.677172
1239.845887	63.859740	67.682177
1238.965444	68.118506	67.687182
1238.850090	65.087185	67.692186
1238.325546	63.962709	67.697191
1237.398836	65.879303	67.702196
1236.570454	56.308573	67.707201
1235.802216	68.331323	67.712206
1235.610634	56.320842	67.717210
1234.095491	73.525677	67.722215
1233.542879	61.077466	67.727220
1233.100206	58.557063	67.732225
1232.648536	68.432246	67.737230
1232.598949	67.943411	67.742234
1231.644598	71.545342	67.747239
1230.531070	65.525323	67.752244
1230.177386	66.286416	67.757249
1229.257335	68.723897	67.762254
1228.605636	71.437233	67.767258
1227.692727	67.403701	67.772263
1227.628919	68.648526	67.777268
1227.084244	62.173798	67.782273
1225.715894	76.942695	67.787278
1225.248314	57.703599	67.792282
1224.426614	76.513799	67.797287
1224.554208	63.325101	67.802292
1223.537227	66.541200	67.807297
1222.377375	68.264651	67.812302
1221.952033	71.121756	67.817306
1221.483907	65.733930	67.822311
1221.157881	66.731886	67.827316
1220.015382	62.629218	67.832321
1219.081467	66.360359	67.837326
1218.865243	67.572654	67.842330
1218.335065	68.908987	67.847335
1217.564682	61.423115	67.852340
1216.447464	72.313989	67.857345
1215.881475	72.812394	67.862350
1215.668784	64.345331	67.867354
1215.149805	62.973984	67.872359
1213.906227	59.772015	67.877364
1213.761113	65.329878	67.882369
1212.902436	68.441963	67.887374
1212.347922	55.912070	67.892378
1211.378406	72.175485	67.897383
1210.636710	60.913193	67.902388
1210.207181	52.830683	67.907393
1209.768457	65.493278	67.912398
1208.890469	58.893375	67.917402
1208.000460	62.466158	67.922407
1207.364407	66.392772	67.927412
1207.318704	56.937272	67.932417
1205.999746	71.466517	67.937422
1205.449682	61.523549	67.942426
1204.840812	67.621914	67.947431
1204.190513	62.196835	67.952436
1203.924128	59.574290	67.957441
1202.791726	70.729341	67.962446
1202.229244	65.381754	67.967450
1201.328234	68.350774	67.972455
1201.342271	71.163238	67.977460
1200.497348	58.506074	67.982465
1199.485611	76.952283	67.987470
1199.332878	65.596331	67.992474
1198.351264	65.657816	67.997479
1197.443424	74.061799	68.002484
1196.864472	68.936016	68.007489
1196.262335	79.131588	68.012494
1196.048749	62.160638	68.017498
1194.799559	75.773676	68.022503
1194.118638	54.906509	68.027508
1193.614373	69.129587	68.032513
1193.102560	70.647497	68.037518
1192.759892	62.912275	68.042522
1191.587105	62.960014	68.047527
1190.940012	67.631090	68.052532
1190.578492	64.941678	68.057537
1189.568757	72.417326	68.062542
1189.119494	63.380797	68.067546
1188.641836	70.749751	68.072551
1187.926081	61.228932	68.077556
1187.165784	70.915095	68.082561
1185.979883	71.094224	68.087566
1185.803921	71.431267	68.092570
1185.118396	68.752384	68.097575
1184.861972	66.571356	68.102580
1183.791779	75.329151	68.107585
1183.012026	72.430301	68.112590
1182.890757	67.290079	68.117594
1181.492904	74.182517	68.122599
1180.612048	71.583583	68.127604
1180.329850	63.895513	68.132609
1179.401039	78.872055	68.137614
1179.158775	62.679910	68.142618
1178.664750	67.660941	68.147623
1178.317395	62.749055	68.152628
1177.583900	64.713784	68.157633
1176.700469	66.673976	68.162638
1175.747061	63.242962	68.167642
1174.521905	72.908447	68.172647
1174.114319	62.703146	68.177652
1173.987420	61.152765	68.182657
1173.346325	69.861239	68.187662
1172.861308	58.748943	68.192666
1171.669559	67.355768	68.197671
1170.938611	71.087760	68.202676
1170.432068	61.033810	68.207681
1170.150201	60.922521	68.212686
1169.449894	54.761130	68.217690
1168.434939	59.856545	68.222695
1168.160233	71.803972	68.227700
1167.638835	59.514815	68.232705
1166.332001	69.245328	68.237710
1165.831496	66.781440	68.242714
1165.287586	64.474258	68.247719
1164.873469	62.967980	68.252724
1164.012194	70.478367	68.257729
1163.059467	69.863528	68.262734
1162.804587	64.785557	68.267738
1162.057635	61.887807	68.272743
1161.468060	60.087756	68.277748
1160.477795	65.001063	68.282753
1159.651094	68.445528	68.287758
1159.397304	58.013935	68.292762
1158.708348	69.399653	68.297767
1157.992619	60.697234	68.302772
1157.561598	69.364415	68.307777
1156.788258	64.403595	68.312782
1156.495266	63.240733	68.317786
1155.097421	73.622780	68.322791
1154.775588	69.124706	68.327796
1154.333654	66.489089	68.332801
1153.280654	73.074393	68.337806
1152.474165	67.623711	68.342810
1152.149531	71.712107	68.347815
1151.553931	68.583718	68.352820
1151.234687	68.841055	68.357825
1149.962384	71.049175	68.362830
1149.319831	57.379041	68.367834
1148.958974	73.037914	68.372839
1148.318003	69.975086	68.377844
1147.157473	67.497913	68.382849
1146.079909	73.013283	68.387854
1146.365191	67.122468	68.392858
1145.840089	70.474816	68.397863
1144.878432	69.965477	68.402868
1144.258007	64.269175	68.407873
1143.437418	72.217772	68.412878
1143.094153	61.245356	68.417882
1141.894662	75.165879	68.422887
1141.022442	66.676000	68.427892
1140.973145	63.323539	68.432897
1140.233014	77.502145	68.437902
1139.946469	69.720160	68.442906
1138.810095	69.740055	68.447911
1138.240335	70.248538	68.452916
1137.732955	59.792631	68.457921
1136.451107	72.319691	68.462926
1135.936220	60.251847	68.467930
1135.204430	67.402619	68.472935
1134.521937	65.464397	68.477940
1134.756429	69.038110	68.482945
1134.003611	74.642174	68.487950
1133.259543	65.136915	68.492954
1132.480508	69.631882	68.497959
1131.710498	66.647927	68.502964
1130.696537	74.371834	68.507969
1129.816411	72.400394	68.512974
1129.766397	69.521105	68.517978
1129.460869	71.971257	68.522983
1128.612879	73.919521	68.527988
1127.783365	69.541623	68.532993
1126.912038	75.306456	68.537998
1126.307181	59.142042	68.543002
1125.503567	73.091060	68.548007
1124.878432	74.666430	68.553012
1124.319709	65.965855	68.558017
1123.927079	67.363902	68.563022
1123.004271	71.342453	68.568026
1122.022216	70.423228	68.573031
1121.478140	69.249847	68.578036
1121.193872	74.785695	68.583041
1120.646349	73.270682	68.588046
1119.362493	71.756103	68.593050
1118.440878	81.400140	68.598055
1118.020427	74.237088	68.603060
1118.016892	67.151219	68.608065
1117.640980	70.471957	68.613070
1116.249334	66.489389	68.618074
1115.811671	63.140358	68.623079
1115.376192	67.621681	68.628084
1114.715736	66.476275	68.633089
1113.507601	71.592979	68.638094
1112.754382	61.892078	68.643098
1112.518394	67.934301	68.648103
1111.954857	84.547889	68.653108
1111.119592	73.568579	68.658113
1110.388307	73.347443	68.663118
1110.140344	71.552986	68.668122
1109.300187	63.671422	68.673127
1108.173890	72.939607	68.678132
1107.579133	68.822402	68.683137
1107.062150	75.565299	68.688142
1106.916237	73.839760	68.693146
1105.717609	73.935801	68.698151
1104.837909	75.274139	68.703156
1104.891860	67.709222	68.708161
1103.959283	81.114247	68.713166
1103.129004	77.504411	68.718170
1102.329168	71.702623	68.723175
1101.866427	71.771492	68.728180
1101.707631	61.731630	68.733185
1100.593726	70.878002	68.738190
1099.636361	69.297308	68.743194
1098.981222	75.677428	68.748199
1098.701095	69.441334	68.753204
1098.345754	65.803260	68.758209
1097.058530	70.327037	68.763214
1096.365132	70.970307	68.768218
1095.890827	74.361890	68.773223
1095.476751	76.824582	68.778228
1094.631039	72.548615	68.783233
1093.836575	76.005318	68.788238
1093.507240	78.145466	68.793242
1092.857302	73.597097	68.798247
1091.494065	80.775793	68.803252
1091.145317	73.363235	68.808257
1090.275761	77.415324	68.813262
1090.229991	63.796925	68.818266
1089.958294	75.128898	68.823271
1088.675362	76.980791	68.828276
1088.104044	77.691371	68.833281
1087.419238	76.521461	68.838286
1086.747382	73.676440	68.843290
1085.823870	61.159555	68.848295
1085.129926	73.853299	68.853300
1084.595933	74.945851	68.858305
1084.177713	79.408667	68.863310
1083.625451	73.545427	68.868314
1082.719183	73.907191	68.873319
1081.904353	66.880999	68.878324
1081.714365	68.257854	68.883329
1080.342288	71.678718	68.888334
1079.940906	71.062933	68.893338
1079.494688	74.047951	68.898343
1078.792026	75.873770	68.903348
1078.703911	66.418719	68.908353
1077.767698	74.466146	68.913358
1076.944450	69.723014	68.918362
1075.905900	70.777567	68.923367
1074.851473	66.826529	68.928372
1074.473106	71.571570	68.933377
1074.065759	75.072347	68.938382
1074.035026	72.702473	68.943386
1073.174001	74.509334	68.948391
1071.951723	68.205513	68.953396
1071.641803	63.276654	68.958401
1070.862775	66.434456	68.963406
1070.220778	71.667687	68.968410
1069.394206	61.514875	68.973415
1068.815595	69.067047	68.978420
1068.496560	64.352515	68.983425
1067.479720	70.340772	68.988430
1066.724465	69.060657	68.993434
1066.162078	68.749591	68.998439
1065.671333	66.281020	69.003444
1065.330215	69.056942	69.008449
1064.136856	64.815793	69.013454
1063.656591	67.509778	69.018458
1063.148720	61.313077	69.023463
1061.768605	69.771724	69.028468
1061.229074	60.219768	69.033473
1060.674025	63.669928	69.038478
1060.421829	62.858536	69.043482
1060.050599	64.272109	69.048487
1059.201902	62.377694	69.053492
1058.653947	58.801809	69.058497
1057.548581	72.857185	69.063502
1056.740868	73.212740	69.068506
1055.992670	65.040618	69.073511
1055.263368	68.447543	69.078516
1055.052078	71.232773	69.083521
1054.246811	74.706974	69.088526
1054.056826	72.427087	69.093530
1053.145556	57.781087	69.098535
1051.985458	73.193389	69.103540
1051.745286	57.280057	69.108545
1051.138867	73.063142	69.113550
1050.423833	73.444954	69.118554
1049.919174	70.497656	69.123559
1049.204203	85.635742	69.128564
1048.501351	62.627591	69.133569
1047.199399	69.768169	69.138574
1046.886400	72.063408	69.143578
1046.459816	62.780474	69.148583
1045.761514	69.388229	69.153588
1045.474895	67.588891	69.158593
1044.307908	67.561662	69.163598
1043.932431	62.490282	69.168602
1043.525791	65.055869	69.173607
1042.352238	73.147371	69.178612
1041.780493	76.035677	69.183617
1040.974745	72.317889	69.188622
1040.494823	70.285968	69.193626
1039.325937	76.292118	69.198631
1038.198049	78.945646	69.203636
1038.181466	71.846088	69.208641
1037.649378	75.896541	69.213646
1037.417493	61.073079	69.218650
1037.211557	67.537852	69.223655
1036.236311	74.552349	69.228660
1035.332838	72.392281	69.233665
1034.757463	78.969448	69.238670
1033.850189	65.885485	69.243674
1032.922000	64.095184	69.248679
1032.439716	73.104826	69.253684
1032.213015	67.137773	69.258689
1031.153784	70.978794	69.263694
1030.109160	64.448050	69.268698
1029.849229	61.838693	69.273703
1029.260862	62.782220	69.278708
1028.820425	58.495418	69.283713
1027.544857	68.610496	69.288718
1027.111715	63.173000	69.293722
1027.083039	65.123402	69.298727
1026.124041	69.271734	69.303732
1025.247894	66.003522	69.308737
1024.399605	66.909559	69.313742
1024.257136	60.099680	69.318746
1023.466620	66.851412	69.323751
1022.548871	69.135640	69.328756
1022.165530	68.031321	69.333761
1021.465011	73.857312	69.338766
1020.493467	66.157528	69.343770
1019.917486	68.800520	69.348775
1018.805429	73.679641	69.353780
1018.700484	66.909518	69.358785
1018.290880	67.277436	69.363790
1017.157217	68.432295	69.368794
1016.381918	60.846364	69.373799
1015.798277	63.373887	69.378804
1015.661705	68.665479	69.383809
1014.597194	72.661879	69.388814
1013.746614	64.774129	69.393818
1013.585153	57.697631	69.398823
1012.907457	64.251651	69.403828
1012.286911	62.743553	69.408833
1011.325230	74.205800	69.413838
1010.485111	65.337156	69.418842
1010.265192	68.317715	69.423847
1009.376261	70.971079	69.428852
1008.758110	76.369254	69.433857
1007.754845	75.445565	69.438862
1007.307969	62.471284	69.443866
1007.205035	70.599028	69.448871
1006.202239	81.347198	69.453876
1005.445986	68.491517	69.458881
1004.860358	75.954937	69.463886
1004.353204	73.334456	69.468890
1003.255693	74.295922	69.473895
1002.222956	68.627418	69.478900
1002.256735	56.330409	69.483905
1001.695835	61.587015	69.488910
1000.868264	65.328113	69.493914
999.870834	77.289611	69.498919
999.332342	76.430741	69.503924
999.226639	62.795088	69.508929
998.735826	65.123352	69.513934
997.507042	70.309619	69.518938
996.919480	62.208151	69.523943
996.199576	75.344405	69.528948
995.433193	66.177046	69.533953
994.426863	70.664061	69.538958
993.722625	66.266282	69.543962
993.671132	62.614575	69.548967
993.099855	68.811067	69.553972
992.675165	60.007215	69.558977
991.747070	70.245207	69.563982
990.875609	75.049791	69.568986
990.701270	71.453896	69.573991
989.769180	76.637112	69.578996
988.849298	63.332843	69.584001
988.380164	77.380047	69.589006
987.263325	71.348060	69.594010
986.735779	74.379146	69.599015
985.927172	73.634216	69.604020
985.656960	66.948737	69.609025
985.146508	68.816532	69.614030
984.596964	71.191990	69.619034
983.607871	68.845305	69.624039
982.757249	65.025876	69.629044
982.319952	61.773004	69.634049
981.943465	63.438145	69.639054
980.935947	75.439096	69.644058
980.249265	66.181795	69.649063
979.698217	70.247887	69.654068
979.505051	74.801054	69.659073
978.311168	75.583911	69.664078
977.941678	69.134989	69.669082
977.676215	63.314454	69.674087
976.156205	73.640328	69.679092
975.746502	70.644824	69.684097
975.155737	70.011884	69.689102
974.420581	67.487610	69.694106
973.299840	66.305101	69.699111
972.763545	65.986752	69.704116
972.402356	66.145135	69.709121
971.975881	70.653427	69.714126
971.329078	68.416276	69.719130
970.763537	63.591183	69.724135
969.840851	73.274845	69.729140
969.210363	61.168683	69.734145
968.086688	62.023947	69.739150
967.222627	71.296180	69.744154
967.136421	66.483120	69.749159
966.213760	74.930521	69.754164
966.139657	70.323680	69.759169
965.622180	73.056716	69.764174
964.461799	69.619300	69.769178
963.659560	61.279207	69.774183
963.003123	71.226414	69.779188
962.724022	60.155530	69.784193
961.580853	72.088188	69.789198
961.096289	66.389245	69.794202
960.989275	64.678028	69.799207
960.074629	66.606990	69.804212
959.279008	68.674698	69.809217
958.248638	58.691553	69.814222
957.796585	59.995005	69.819226
957.617911	64.886465	69.824231
956.270086	63.732214	69.829236
955.863768	60.025013	69.834241
955.253001	58.310382	69.839246
954.756875	72.636251	69.844250
953.859625	64.339662	69.849255
953.012209	64.595917	69.854260
952.503229	61.329229	69.859265
952.146553	67.092633	69.864270
951.527984	67.334551	69.869274
950.590846	67.594046	69.874279
950.057103	64.779126	69.879284
949.669220	69.631342	69.884289
948.354016	64.903470	69.889294
947.411504	65.922292	69.894298
947.064346	60.993074	69.899303
946.568977	72.362211	69.904308
946.622653	68.215981	69.909313
945.317081	71.187962	69.914318
944.445390	65.665738	69.919322
944.280550	64.454126	69.924327
943.555657	69.498735	69.929332
942.891998	58.399170	69.934337
941.946303	70.478594	69.939342
941.229672	64.878083	69.944346
940.913225	67.821970	69.949351
939.569971	64.937185	69.954356
939.159752	63.509171	69.959361
938.719352	66.408131	69.964366
938.209000	68.389452	69.969370
937.935312	59.701926	69.974375
936.607822	71.290206	69.979380
936.468405	57.527479	69.984385
936.080203	64.156865	69.989390
934.286237	69.452019	69.994394
934.035572	72.238791	69.999399
933.551556	77.599867	70.004404
933.482038	58.040515	70.009409
932.170587	62.694368	70.014414
931.453875	64.093554	70.019418
930.957325	75.483382	70.024423
929.886107	66.544320	70.029428
929.168784	70.739377	70.034433
928.331313	72.227163	70.039438
927.871090	74.936904	70.044442
928.074409	62.789528	70.049447
926.972961	64.467546	70.054452
925.942736	63.907706	70.059457
925.616895	60.129361	70.064462
924.864543	64.293724	70.069466
924.634287	58.428175	70.074471
923.525025	73.223756	70.079476
922.914749	61.098628	70.084481
922.106525	73.941458	70.089486
921.639250	74.392681	70.094490
920.581709	65.232266	70.099495
919.737611	68.808871	70.104500
919.371067	66.173919	70.109505
918.923657	69.905003	70.114510
918.777016	70.823988	70.119514
917.934464	57.865402	70.124519
916.795370	82.107973	70.129524
916.446632	62.391215	70.134529
915.563770	67.279630	70.139534
914.638629	55.297651	70.144538
914.148963	54.495683	70.149543
913.576654	68.936168	70.154548
913.300713	58.796719	70.159553
912.593383	66.519198	70.164558
911.723865	67.289887	70.169562
911.457044	66.815133	70.174567
909.891375	71.446381	70.179572
908.863546	56.330181	70.184577
908.344762	61.991660	70.189582
907.980630	63.161287	70.194586
908.054277	67.657800	70.199591
907.572371	65.637262	70.204596
907.025998	63.682174	70.209601
906.025732	68.001107	70.214606
905.049731	71.398447	70.219610
904.031103	64.021584	70.224615
903.364785	64.042467	70.229620
902.749726	74.131325	70.234625
902.430947	65.298024	70.239630
901.867041	68.315987	70.244634
901.636486	61.728287	70.249639
900.293963	78.095285	70.254644
899.790513	66.131345	70.259649
899.378642	64.918053	70.264654
898.273774	70.895147	70.269658
897.667584	68.815546	70.274663
896.893243	69.463867	70.279668
896.420496	70.307027	70.284673
896.098174	65.629316	70.289678
894.876063	61.489020	70.294682
894.472568	53.784049	70.299687
893.745258	74.629177	70.304692
893.384783	58.582078	70.309697
892.479467	64.976817	70.314702
891.290504	69.965992	70.319706
891.327869	63.939590	70.324711
890.532404	65.762881	70.329716
890.112712	59.145365	70.334721
889.278109	68.389274	70.339726
888.747867	64.960413	70.344730
888.543646	61.747733	70.349735
887.141898	66.737658	70.354740
886.473342	59.156867	70.359745
886.124856	66.978350	70.364750
885.214291	69.047029	70.369754
884.545951	63.623345	70.374759
883.391067	64.027901	70.379764
882.878715	60.706575	70.384769
882.887554	62.072298	70.389774
882.309066	62.599571	70.394778
881.347772	51.384989	70.399783
880.449827	59.087348	70.404788
880.372722	70.837748	70.409793
879.570617	65.523659	70.414798
878.426138	68.757022	70.419802
878.388438	60.337860	70.424807
877.206736	68.099577	70.429812
876.329810	68.704311	70.434817
875.849666	73.449801	70.439822
875.166225	60.093771	70.444826
874.943606	60.081889	70.449831
873.890474	59.620328	70.454836
873.112562	58.474760	70.459841
872.553993	61.001475	70.464846
872.017491	64.686823	70.469850
871.943330	71.983707	70.474855
870.531569	75.109813	70.479860
869.895518	60.404335	70.484865
870.106876	52.626741	70.489870
868.773924	69.785377	70.494874
867.910755	61.980114	70.499879
867.050669	70.512192	70.504884
866.631759	65.291651	70.509889
866.496422	66.462713	70.514894
865.254380	66.985222	70.519898
864.670125	60.307175	70.524903
863.873650	66.367652	70.529908
863.747288	60.119746	70.534913
863.160742	61.862487	70.539918
861.691887	70.109858	70.544922
861.741607	65.115911	70.549927
860.822720	66.454260	70.554932
860.246738	62.091302	70.559937
859.345759	61.014209	70.564942
858.538751	64.553390	70.569946
858.342224	63.340522	70.574951
857.375183	69.738791	70.579956
856.509849	69.029739	70.584961
856.196446	60.865760	70.589966
855.403842	62.371657	70.594970
855.316994	56.790782	70.599975
854.520784	68.707669	70.604980
853.700072	60.941385	70.609985
853.136039	61.986727	70.614990
851.778593	64.632715	70.619994
851.166351	70.804214	70.624999
850.570635	67.996028	70.630004
850.423907	66.688506	70.635009
849.680752	66.194963	70.640014
848.887561	62.472094	70.645018
848.456681	55.711299	70.650023
847.627131	58.921354	70.655028
846.985124	63.285779	70.660033
846.232298	73.767133	70.665038
845.481452	67.670660	70.670042
844.969843	59.736916	70.675047
844.620576	67.665752	70.680052
843.733823	69.894648	70.685057
843.048991	65.069654	70.690062
842.069441	72.061242	70.695066
841.559505	72.727415	70.700071
841.382436	65.535158	70.705076
840.172842	61.703539	70.710081
839.851382	65.805647	70.715086
839.101656	66.710248	70.720090
838.189454	58.151183	70.725095
837.048527	65.177916	70.730100
836.766697	56.174760	70.735105
836.500918	66.077147	70.740110
836.035434	72.288364	70.745114
835.251885	60.252346	70.750119
834.083519	59.492196	70.755124
833.794801	55.994947	70.760129
833.434836	60.416976	70.765134
832.210747	62.601804	70.770138
831.292099	61.410846	70.775143
830.904443	58.402402	70.780148
830.559041	67.939018	70.785153
830.503708	61.559968	70.790158
829.369005	79.011904	70.795162
828.916308	59.710675	70.800167
827.436001	56.232797	70.805172
826.425138	63.912148	70.810177
825.864531	72.287764	70.815182
825.655406	69.241441	70.820186
825.517177	52.627593	70.825191
824.685732	68.799722	70.830196
824.309555	59.541943	70.835201
823.443074	59.657782	70.840206
822.621692	66.775575	70.845210
821.425485	63.908449	70.850215
820.461559	65.985643	70.855220
820.143097	64.380627	70.860225
819.622955	63.348577	70.865230
819.162286	72.230226	70.870234
819.464658	62.266806	70.875239
818.080748	61.066339	70.880244
817.298462	67.034688	70.885249
816.749829	59.794356	70.890254
815.670510	67.593412	70.895258
815.019689	65.784274	70.900263
814.575869	70.151851	70.905268
814.060308	70.855193	70.910273
812.981059	71.170475	70.915278
812.240658	72.988178	70.920282
811.878997	60.311039	70.925287
811.153760	73.735154	70.930292
810.766783	63.611822	70.935297
810.173959	59.163256	70.940302
809.335269	69.166303	70.945306
808.674081	57.183358	70.950311
808.180799	66.144308	70.955316
807.030566	64.192332	70.960321
806.357578	58.993330	70.965326
805.724331	71.369959	70.970330
805.738454	61.017212	70.975335
804.935457	62.666695	70.980340
804.048743	62.758956	70.985345
803.560312	61.926853	70.990350
803.069996	67.657929	70.995354
802.104124	67.940976	71.000359
801.447405	60.352023	71.005364
800.818453	56.379115	71.010369
799.823746	62.103754	71.015374
798.979788	69.075346	71.020378
798.520912	54.355892	71.025383
797.943753	54.649598	71.030388
797.753562	63.724716	71.035393
796.801832	56.220572	71.040398
795.890076	61.001662	71.045402
795.394446	63.713904	71.050407
795.250824	61.496046	71.055412
794.074979	56.541090	71.060417
793.689564	52.767523	71.065422
792.622788	64.062055	71.070426
792.341401	61.938663	71.075431
790.845406	70.491569	71.080436
790.478405	65.992867	71.085441
790.136527	60.468364	71.090446
789.532375	73.319729	71.095450
789.462517	59.347274	71.100455
787.866409	65.317456	71.105460
787.193025	68.269296	71.110465
787.012877	72.025658	71.115470
786.131259	68.279042	71.120474
785.226623	61.147427	71.125479
784.496921	67.971532	71.130484
784.111247	62.163859	71.135489
783.837084	58.998594	71.140494
782.686777	73.521644	71.145498
782.404207	69.518827	71.150503
781.555749	72.361352	71.155508
781.291327	64.320469	71.160513
780.261335	64.468661	71.165518
779.025857	77.232887	71.170522
778.745780	69.464137	71.175527
778.157927	66.337770	71.180532
777.756168	68.880540	71.185537
777.045808	58.803970	71.190542
775.887088	67.645368	71.195546
775.595380	61.461639	71.200551
775.374784	63.570316	71.205556
774.553704	64.500487	71.210561
773.871246	60.315344	71.215566
772.766259	69.255416	71.220570
772.424042	54.436979	71.225575
771.273327	73.428907	71.230580
770.648013	59.220049	71.235585
770.377877	68.509734	71.240590
769.710271	65.307762	71.245594
768.885758	65.319174	71.250599
767.844870	67.307721	71.255604
767.399299	69.624092	71.260609
767.371226	56.546954	71.265614
766.596766	69.614653	71.270618
766.122988	69.004138	71.275623
765.241953	58.410729	71.280628
764.559461	67.926899	71.285633
763.828558	55.756388	71.290638
762.844684	77.571141	71.295642
762.154608	59.099313	71.300647
761.779465	59.651007	71.305652
761.155179	69.872229	71.310657
760.159806	49.892659	71.315662
759.303940	62.937046	71.320666
759.387945	68.892068	71.325671
758.867728	58.454094	71.330676
757.634576	70.456331	71.335681
757.033947	64.611926	71.340686
756.329954	73.442438	71.345690
756.380653	60.740664	71.350695
755.039419	57.573406	71.355700
753.963339	63.675270	71.360705
753.857476	66.025864	71.365710
753.360626	70.819759	71.370714
752.504976	62.619134	71.375719
751.725427	60.076771	71.380724
751.042102	57.381904	71.385729
750.897402	56.868803	71.390734
749.846018	67.566425	71.395738
748.946497	67.864159	71.400743
748.771517	58.930736	71.405748
747.973552	71.980107	71.410753
746.912087	60.961296	71.415758
745.750037	71.536202	71.420762
745.378405	60.666170	71.425767
744.974909	63.519860	71.430772
744.603340	58.728601	71.435777
744.792230	61.254604	71.440782
743.678323	60.619859	71.445786
742.851761	66.445474	71.450791
742.049643	68.563163	71.455796
740.888272	73.235791	71.460801
740.174577	69.743139	71.465806
739.420541	66.909729	71.470810
739.403973	63.561541	71.475815
739.251744	65.835943	71.480820
738.161950	68.226502	71.485825
737.350250	63.924760	71.490830
736.832038	74.028181	71.495834
736.296187	73.837537	71.500839
734.975730	72.811505	71.505844
734.241697	69.331554	71.510849
734.226685	56.222381	71.515854
733.447232	67.269351	71.520858
732.766051	56.530606	71.525863
732.188991	62.037395	71.530868
731.484569	60.607376	71.535873
730.149530	59.536364	71.540878
729.216878	68.275558	71.545882
728.770621	50.846661	71.550887
728.584121	61.874910	71.555892
727.904657	64.614856	71.560897
727.795454	58.482499	71.565902
727.059820	58.721033	71.570906
726.364027	60.299858	71.575911
725.774084	68.091989	71.580916
724.689591	66.317232	71.585921
724.141524	56.328379	71.590926
723.495673	72.338523	71.595930
723.302870	62.078650	71.600935
722.126724	61.001266	71.605940
721.186245	63.175681	71.610945
720.920126	64.058509	71.615950
720.235712	63.251319	71.620954
719.478016	66.131448	71.625959
718.858343	52.383738	71.630964
717.888525	69.430994	71.635969
717.429236	60.700529	71.640974
716.842005	69.378422	71.645978
715.645701	60.678576	71.650983
715.370865	62.445831	71.655988
714.685477	63.157310	71.660993
714.868702	53.227058	71.665998
713.848014	54.854462	71.671002
713.237434	60.681962	71.676007
712.736470	65.765080	71.681012
711.471866	60.665036	71.686017
710.922480	52.756272	71.691022
710.064834	61.563944	71.696026
709.461533	50.219915	71.701031
708.521108	58.616593	71.706036
707.891698	57.229827	71.711041
707.717642	56.849129	71.716046
707.076319	55.013280	71.721050
706.428849	61.259791	71.726055
705.365510	56.047286	71.731060
704.716366	62.376061	71.736065
704.349276	54.670070	71.741070
703.610104	70.333972	71.746074
702.724072	59.298291	71.751079
702.227463	60.310854	71.756084
701.432599	65.374542	71.761089
701.463491	53.046496	71.766094
700.309016	62.604711	71.771098
699.342164	59.321107	71.776103
699.050748	56.650580	71.781108
698.630755	64.970706	71.786113
697.850881	62.158770	71.791118
696.726345	63.413234	71.796122
696.328318	61.901325	71.801127
695.988407	63.631638	71.806132
694.815671	61.449925	71.811137
694.410464	58.490031	71.816142
693.898635	61.635350	71.821146
693.119942	59.543851	71.826151
692.383989	58.087327	71.831156
691.233635	68.920569	71.836161
691.131397	59.682278	71.841166
690.419967	66.730559	71.846170
689.815265	56.410135	71.851175
688.778479	53.109289	71.856180
687.830398	60.986831	71.861185
687.752675	59.020247	71.866190
687.214898	60.810450	71.871194
686.848588	61.863766	71.876199
685.914584	55.834365	71.881204
684.944455	55.205136	71.886209
684.886342	49.435213	71.891214
683.452771	60.193707	71.896218
682.858934	54.431821	71.901223
682.202199	62.556268	71.906228
681.791215	59.772327	71.911233
681.398463	57.737642	71.916238
680.111558	68.370294	71.921242
679.296550	62.213142	71.926247
678.946124	67.603435	71.931252
678.768553	60.270944	71.936257
678.463573	53.548488	71.941262
677.479399	42.209936	71.946266
676.364875	60.623710	71.951271
676.169894	48.836231	71.956276
675.043734	67.627158	71.961281
674.514698	48.850639	71.966286
673.878529	56.713206	71.971290
673.376544	51.229993	71.976295
672.540140	62.751211	71.981300
671.695437	59.717811	71.986305
671.292639	61.847623	71.991310
670.640849	62.564801	71.996314
670.261899	68.036903	72.001319
669.288720	52.465894	72.006324
668.608170	68.404296	72.011329
668.502604	55.602849	72.016334
667.337201	61.176529	72.021338
666.169245	55.832477	72.026343
665.959955	63.281743	72.031348
665.360072	64.331257	72.036353
664.836571	63.127899	72.041358
663.777597	69.069388	72.046362
663.334430	75.663402	72.051367
662.877559	57.387863	72.056372
661.764390	66.531111	72.061377
661.249101	57.839541	72.066382
660.538229	63.045973	72.071386
660.183971	49.650239	72.076391
659.508795	62.448266	72.081396
658.478247	74.717881	72.086401
658.012504	62.511493	72.091406
657.349090	62.437367	72.096410
656.771746	62.694867	72.101415
656.073253	55.349148	72.106420
655.099878	72.297644	72.111425
654.493884	67.879601	72.116430
654.168949	71.744173	72.121434
653.477992	57.933724	72.126439
652.521746	63.757938	72.131444
651.685253	69.441666	72.136449
651.777683	53.891772	72.141454
650.917844	70.290788	72.146458
649.629949	63.131960	72.151463
648.992686	53.097418	72.156468
648.628373	56.216098	72.161473
648.639975	59.535098	72.166478
647.726360	63.715749	72.171482
646.882565	63.243024	72.176487
646.551875	61.056546	72.181492
645.931720	62.120331	72.186497
644.927940	52.487912	72.191502
644.104947	66.153100	72.196506
643.114843	59.251189	72.201511
642.758934	63.226341	72.206516
642.077638	64.463857	72.211521
641.560230	60.332892	72.216526
641.099435	61.683518	72.221530
640.421886	62.190353	72.226535
639.422061	57.726232	72.231540
638.340178	62.919217	72.236545
638.082245	55.345659	72.241550
637.625156	54.798740	72.246554
637.033202	64.989596	72.251559
636.269680	63.841813	72.256564
635.606093	70.360549	72.261569
635.176689	69.806068	72.266574
634.193077	65.498627	72.271578
633.506190	58.010725	72.276583
632.888497	57.902519	72.281588
632.287337	61.109380	72.286593
632.152081	61.279137	72.291598
631.160749	57.603671	72.296602
630.106152	62.248299	72.301607
629.817845	50.163474	72.306612
628.201740	53.535121	72.311617
627.745718	45.256726	72.316622
627.199820	59.715092	72.321626
626.657665	54.941563	72.326631
627.007147	50.641012	72.331636
626.064611	53.239960	72.336641
625.316909	52.879665	72.341646
624.683595	65.398237	72.346650
624.146453	57.977949	72.351655
623.221185	45.540435	72.356660
622.434956	50.557035	72.361665
621.731967	52.761467	72.366670
620.535098	58.537282	72.371674
619.774907	52.484962	72.376679
619.692112	52.099197	72.381684
618.942085	66.411894	72.386689
619.033114	51.721616	72.391694
618.336558	60.234013	72.396698
616.912393	55.347081	72.401703
616.713497	55.793462	72.406708
615.261705	58.268527	72.411713
614.311841	52.367833	72.416718
613.996557	63.949565	72.421722
613.525910	60.643739	72.426727
613.188909	49.651549	72.431732
612.495167	71.207232	72.436737
612.691359	62.386595	72.441742
611.635302	69.461396	72.446746
611.008038	58.114907	72.451751
609.912892	64.022752	72.456756
608.837529	67.095420	72.461761
608.519727	65.250648	72.466766
607.678441	57.651737	72.471770
606.651323	64.089610	72.476775
606.031197	48.129697	72.481780
605.487450	64.391644	72.486785
605.262567	53.689083	72.491790
605.135772	60.806685	72.496794
604.349922	60.477701	72.501799
603.473712	57.752100	72.506804
602.743158	62.422395	72.511809
601.385400	50.864271	72.516814
600.559435	57.106114	72.521818
600.091642	58.177181	72.526823
599.778608	59.002841	72.531828
599.293674	61.393310	72.536833
599.260567	49.848131	72.541838
597.832852	56.811823	72.546842
596.955319	61.087662	72.551847
596.858434	53.717107	72.556852
596.234539	64.494914	72.561857
595.298504	56.338701	72.566862
594.594610	50.266386	72.571866
593.810246	66.271787	72.576871
593.573631	47.488152	72.581876
592.206524	56.402220	72.586881
591.771189	61.347177	72.591886
591.214108	58.450913	72.596890
590.766079	53.047431	72.601895
590.372162	59.346614	72.606900
589.236574	57.753512	72.611905
589.150663	55.953807	72.616910
588.375781	53.942157	72.621914
587.555359	54.370843	72.626919
586.535212	55.410045	72.631924
585.787755	66.106615	72.636929
585.683864	53.339609	72.641934
584.844379	55.557907	72.646938
583.817647	51.813989	72.651943
583.654535	48.654720	72.656948
582.646494	60.982257	72.661953
581.905324	47.392722	72.666958
581.228080	52.820879	72.671962
580.661384	62.094720	72.676967
580.912653	48.643564	72.681972
579.606900	60.936523	72.686977
578.789909	53.783160	72.691982
578.416711	52.163246	72.696986
576.880015	68.044066	72.701991
576.381421	55.511802	72.706996
575.551219	59.776956	72.712001
575.309724	59.531579	72.717006
574.929491	51.329428	72.722010
574.334615	56.501634	72.727015
573.858599	56.612135	72.732020
572.708926	56.850433	72.737025
572.282530	50.812770	72.742030
571.657543	57.252830	72.747034
570.741192	55.277909	72.752039
570.320118	52.277993	72.757044
569.720140	63.979182	72.762049
569.143929	49.533952	72.767054
568.011345	60.917873	72.772058
567.762522	58.239005	72.777063
567.077438	49.770042	72.782068
565.688339	50.508496	72.787073
565.105388	56.162897	72.792078
564.719217	53.304069	72.797082
564.261331	56.808223	72.802087
564.048342	52.843244	72.807092
562.367752	54.057032	72.812097
561.902990	58.133103	72.817102
561.574825	53.672416	72.822106
561.218961	40.650688	72.827111
560.674332	46.196487	72.832116
559.634961	60.651462	72.837121
558.990018	48.120446	72.842126
558.645175	59.080872	72.847130
557.707322	54.080249	72.852135
556.882935	43.547308	72.857140
556.171484	51.699409	72.862145
555.843012	53.886778	72.867150
554.931284	50.001562	72.872154
554.081433	63.289443	72.877159
553.527979	44.043815	72.882164
553.007743	57.042662	72.887169
552.428294	52.543159	72.892174
551.520584	63.555400	72.897178
550.752198	59.426591	72.902183
550.385045	47.532531	72.907188
549.737794	52.123340	72.912193
549.380002	56.858842	72.917198
548.667506	58.028817	72.922202
548.027224	55.768673	72.927207
547.371908	40.553942	72.932212
545.691031	57.309229	72.937217
545.256451	49.014826	72.942222
545.139779	54.432541	72.947226
544.542137	57.832812	72.952231
544.119223	51.584879	72.957236
542.817695	55.552980	72.962241
542.452381	53.230117	72.967246
542.332144	49.266137	72.972250
541.113693	59.239847	72.977255
540.658136	45.783022	72.982260
539.433278	61.790786	72.987265
539.192679	47.965426	72.992270
538.789323	58.935173	72.997274
537.710778	52.905210	73.002279
537.364309	44.230946	73.007284
536.821634	58.051754	73.012289
535.632355	58.403604	73.017294
534.910884	47.404873	73.022298
534.362699	52.337850	73.027303
534.037851	55.276803	73.032308
532.985771	49.868638	73.037313
532.080555	54.837988	73.042318
532.022022	48.577746	73.047322
531.405965	49.164695	73.052327
531.236162	48.847983	73.057332
529.774495	57.832333	73.062337
529.398124	61.227321	73.067342
528.983184	49.132734	73.072346
527.683390	59.321243	73.077351
527.254050	59.195675	73.082356
526.352278	45.450412	73.087361
526.267764	55.150461	73.092366
525.130037	52.695193	73.097370
523.858645	63.030560	73.102375
523.815744	40.485267	73.107380
523.071571	51.660677	73.112385
523.027466	56.814537	73.117390
522.190647	51.892448	73.122394
520.967567	62.995931	73.127399
520.671095	59.952521	73.132404
519.972631	53.645992	73.137409
519.417383	58.283650	73.142414
518.592129	60.513894	73.147418
517.763574	54.201282	73.152423
517.471959	59.826628	73.157428
516.923089	59.745332	73.162433
516.321368	59.661417	73.167438
515.324998	58.763640	73.172442
514.889858	62.557474	73.177447
514.352067	67.881439	73.182452
513.105340	66.873743	73.187457
512.585512	56.080999	73.192462
512.209134	54.630325	73.197466
510.908463	67.627359	73.202471
510.306688	62.738786	73.207476
509.705250	62.270076	73.212481
508.912522	64.589752	73.217486
509.253608	54.068270	73.222490
508.480399	67.471680	73.227495
507.736027	55.669254	73.232500
506.815431	71.879290	73.237505
506.372989	62.140168	73.242510
505.578333	53.858981	73.247514
504.361222	67.235341	73.252519
504.216320	50.185849	73.257524
503.742305	61.195238	73.262529
502.877436	57.070779	73.267534
501.980972	52.782632	73.272538
501.030428	57.760791	73.277543
501.086039	44.884826	73.282548
500.458925	61.208936	73.287553
499.473648	65.856762	73.292558
498.849420	48.254469	73.297562
498.038050	61.670262	73.302567
497.910610	47.738582	73.307572
496.653313	62.980449	73.312577
496.045574	47.515319	73.317582
495.670137	48.406122	73.322586
494.903366	57.101602	73.327591
494.362032	54.365271	73.332596
492.939302	54.237124	73.337601
492.726996	61.729444	73.342606
492.378337	59.016030	73.347610
491.644251	65.025663	73.352615
491.151346	49.291520	73.357620
489.893225	60.949339	73.362625
489.641972	57.245914	73.367630
489.394642	51.296431	73.372634
488.034730	64.466901	73.377639
487.782207	60.230702	73.382644
487.174093	65.105434	73.387649
486.359110	59.465563	73.392654
485.762500	54.309689	73.397658
484.464945	66.669188	73.402663
484.321547	57.229342	73.407668
483.746551	58.755872	73.412673
482.910729	62.550470	73.417678
482.332540	56.606390	73.422682
481.895916	67.737553	73.427687
481.581077	54.472773	73.432692
480.159147	54.571573	73.437697
479.508671	68.256614	73.442702
479.449199	57.297504	73.447706
478.122810	66.632469	73.452711
477.295515	61.257897	73.457716
476.802130	54.953402	73.462721
476.350256	64.584255	73.467726
476.094417	61.712562	73.472730
474.951933	57.260205	73.477735
474.225718	61.341675	73.482740
473.622914	55.800463	73.487745
473.424857	52.834417	73.492750
472.501434	55.208038	73.497754
471.322697	66.320246	73.502759
471.153717	52.557601	73.507764
470.592180	64.566470	73.512769
469.820171	62.940729	73.517774
468.741179	57.204164	73.522778
468.061796	67.970331	73.527783
467.830182	56.743778	73.532788
467.344864	60.439963	73.537793
466.825353	70.378044	73.542798
465.872674	61.726255	73.547802
464.961163	55.983509	73.552807
464.763363	52.646863	73.557812
464.154516	66.180201	73.562817
462.778028	61.749362	73.567822
462.509487	53.531020	73.572826
461.657096	61.696138	73.577831
461.269723	53.725372	73.582836
460.310508	52.574132	73.587841
459.549837	59.721761	73.592846
459.081506	48.808878	73.597850
458.777186	57.867476	73.602855
458.504098	65.170799	73.607860
457.148824	63.168087	73.612865
456.688422	55.032349	73.617870
456.294790	51.641755	73.622874
455.095950	52.789898	73.627879
454.656052	54.236567	73.632884
454.126122	46.785227	73.637889
452.963197	56.351179	73.642894
452.417751	53.946652	73.647898
451.724110	66.738190	73.652903
451.388210	51.013736	73.657908
450.809426	59.725005	73.662913
450.096201	61.563707	73.667918
449.361363	56.749967	73.672922
448.642788	61.781067	73.677927
448.469041	63.905954	73.682932
447.017004	60.900019	73.687937
446.334594	61.642632	73.692942
446.067375	53.934982	73.697946
445.289871	63.313386	73.702951
444.865247	71.219560	73.707956
444.018356	61.371442	73.712961
443.222001	58.694677	73.717966
443.134923	60.039405	73.722970
441.719936	65.015896	73.727975
440.842879	61.500489	73.732980
440.435295	63.312573	73.737985
440.086522	65.906865	73.742990
439.961037	55.259459	73.747994
438.671190	59.074372	73.752999
437.769050	61.580224	73.758004
437.392824	61.452516	73.763009
437.106008	60.069581	73.768014
436.359949	56.359852	73.773018
435.071491	56.891544	73.778023
434.705147	54.116308	73.783028
434.053256	76.433264	73.788033
433.665316	60.825899	73.793038
433.053107	55.038632	73.798042
432.452458	63.754967	73.803047
431.749675	49.921277	73.808052
430.800014	58.012019	73.813057
429.957057	63.271086	73.818062
429.571860	64.456748	73.823066
428.980364	64.252961	73.828071
428.111621	58.118664	73.833076
427.075406	68.112270	73.838081
426.728266	60.898293	73.843086
426.509763	63.161190	73.848090
425.249009	61.260124	73.853095
424.440936	62.965722	73.858100
423.789850	61.976698	73.863105
423.549707	67.486626	73.868110
423.226698	59.428345	73.873114
422.503747	57.760113	73.878119
421.843013	61.553636	73.883124
421.001206	61.462270	73.888129
420.291034	61.378313	73.893134
419.568280	59.435679	73.898138
418.567424	70.126930	73.903143
418.707098	61.570752	73.908148
417.833854	64.819435	73.913153
416.358828	57.758371	73.918158
416.311461	60.515937	73.923162
415.515549	66.038731	73.928167
415.435776	55.109674	73.933172
414.231802	48.592015	73.938177
413.359144	63.309029	73.943182
413.372049	57.231363	73.948186
412.252304	57.308858	73.953191
411.448254	53.037559	73.958196
410.663399	59.085258	73.963201
410.073748	64.830637	73.968206
410.161614	65.819506	73.973210
409.293749	54.848879	73.978215
408.350627	58.198578	73.983220
407.800747	64.021192	73.988225
406.978497	55.359691	73.993230
406.760024	51.472873	73.998234
405.487962	65.758402	74.003239
405.103234	52.799652	74.008244
404.954796	47.438360	74.013249
403.581265	51.768060	74.018254
403.126848	50.851777	74.023258
402.563230	68.905050	74.028263
401.931556	53.439036	74.033268
400.715050	61.170212	74.038273
400.002888	61.804045	74.043278
399.587793	57.951711	74.048282
399.055101	61.176093	74.053287
398.927310	54.084859	74.058292
397.444235	57.075929	74.063297
396.431370	60.362634	74.068302
396.495379	53.171456	74.073306
395.911608	62.411773	74.078311
395.418616	59.666186	74.083316
394.522709	59.328000	74.088321
393.788324	59.217949	74.093326
393.757712	51.373266	74.098330
392.121983	55.568147	74.103335
391.535043	56.098455	74.108340
390.969089	62.994313	74.113345
390.533091	58.853594	74.118350
390.417702	47.755191	74.123354
389.198127	59.064729	74.128359
388.471289	61.104299	74.133364
388.225694	57.739010	74.138369
387.125053	57.501256	74.143374
386.297063	52.809609	74.148378
385.486323	62.608033	74.153383
385.318145	52.725906	74.158388
384.917045	54.817642	74.163393
383.891432	62.794355	74.168398
383.514276	50.769479	74.173402
382.555875	62.775368	74.178407
382.341060	60.791225	74.183412
381.106869	50.049290	74.188417
380.199664	63.281694	74.193422
380.187652	49.415216	74.198426
379.291327	59.711369	74.203431
378.323486	55.297460	74.208436
377.719703	51.902526	74.213441
377.450610	48.477911	74.218446
377.313187	52.320506	74.223450
376.008353	63.763479	74.228455
375.045080	58.618761	74.233460
374.619950	50.398585	74.238465
374.049506	60.513507	74.243470
373.697221	46.538842	74.248474
372.471182	56.797657	74.253479
371.960713	65.896997	74.258484
371.523580	58.646915	74.263489
370.457345	65.564158	74.268494
370.134525	59.879017	74.273498
369.388038	67.234130	74.278503
369.200957	62.643767	74.283508
368.371126	65.833511	74.288513
367.486110	57.885302	74.293518
367.224168	54.733919	74.298522
365.803509	53.528529	74.303527
365.150479	55.920595	74.308532
364.823586	62.579678	74.313537
364.035698	65.024774	74.318542
364.047596	56.775950	74.323546
362.569590	58.829585	74.328551
361.872598	68.784921	74.333556
361.506520	60.992119	74.338561
360.558285	55.371957	74.343566
359.883658	63.453584	74.348570
359.312326	63.934107	74.353575
359.172028	59.855074	74.358580
358.838549	61.748393	74.363585
357.413615	63.465589	74.368590
356.908836	59.108772	74.373594
356.444315	71.281957	74.378599
355.747053	58.314680	74.383604
354.784076	50.484554	74.388609
353.920430	59.515604	74.393614
353.709047	63.477215	74.398618
352.547106	67.956140	74.403623
351.729398	65.240233	74.408628
351.257202	54.616560	74.413633
350.471198	49.405761	74.418638
350.809129	54.136056	74.423642
350.024007	69.742672	74.428647
349.003263	74.441934	74.433652
348.144619	63.646467	74.438657
347.487119	59.407025	74.443662
346.843238	67.761282	74.448666
345.808327	63.200388	74.453671
345.494910	70.431301	74.458676
344.809848	53.832181	74.463681
344.607565	67.406387	74.468686
343.936122	64.632483	74.473690
342.756924	69.547797	74.478695
342.200702	74.316524	74.483700
341.887510	60.300934	74.488705
340.742898	64.518499	74.493710
340.207994	54.224923	74.498714
339.694677	61.673758	74.503719
339.076974	64.872279	74.508724
338.563234	66.816405	74.513729
337.392486	66.383279	74.518734
336.775494	62.369180	74.523738
336.553651	68.685118	74.528743
336.336071	67.313237	74.533748
335.444643	62.023054	74.538753
334.594641	65.335863	74.543758
333.795888	62.367800	74.548762
332.821679	68.106677	74.553767
332.252718	63.941431	74.558772
332.156978	64.984788	74.563777
330.863730	66.925424	74.568782
329.939364	66.074590	74.573786
329.521466	69.264923	74.578791
329.082703	62.240600	74.583796
328.855605	60.543830	74.588801
327.763147	65.878958	74.593806
326.933015	63.767397	74.598810
326.055846	67.726317	74.603815
325.456299	63.195388	74.608820
325.344893	63.378706	74.613825
324.443068	61.650709	74.618830
323.754608	56.520559	74.623834
323.242849	61.703218	74.628839
322.667973	62.871820	74.633844
322.103228	63.456950	74.638849
320.884056	57.878410	74.643854
320.392041	60.229057	74.648858
319.747958	64.166597	74.653863
319.105077	61.366073	74.658868
318.612552	63.268977	74.663873
317.711149	63.433133	74.668878
317.442891	47.857205	74.673882
316.891174	58.260865	74.678887
315.361415	57.102852	74.683892
314.988289	56.495307	74.688897
314.481596	55.284619	74.693902
314.279856	50.881094	74.698906
313.343012	54.351241	74.703911
312.350301	55.137038	74.708916
311.927472	47.428989	74.713921
311.424934	57.162535	74.718926
310.748162	63.949921	74.723930
309.697342	56.859164	74.728935
309.017879	44.363713	74.733940
308.978943	54.084865	74.738945
308.043706	58.868273	74.743950
307.564548	62.721186	74.748954
306.958026	57.816086	74.753959
305.775829	59.163485	74.758964
304.997733	59.602863	74.763969
304.045979	66.082441	74.768974
303.849128	53.065394	74.773978
303.110576	51.420185	74.778983
302.873554	61.138222	74.783988
302.941685	55.018649	74.788993
301.388662	65.982428	74.793998
300.899163	64.630238	74.799002
300.128080	58.177674	74.804007
298.973792	62.841469	74.809012
298.802320	55.664175	74.814017
298.086658	55.051308	74.819022
297.780565	47.663679	74.824026
296.900971	61.738466	74.829031
296.054660	62.294368	74.834036
295.556909	59.945351	74.839041
294.459382	59.845904	74.844046
293.730387	54.870450	74.849050
293.029437	52.918074	74.854055
292.555830	58.283876	74.859060
292.283817	57.087823	74.864065
291.431804	60.177053	74.869070
290.791913	62.896605	74.874074
290.052663	69.799604	74.879079
289.560657	72.309519	74.884084
289.128528	64.044745	74.889089
287.862408	57.497637	74.894094
287.534588	53.547844	74.899098
287.046016	58.247449	74.904103
286.124695	60.628685	74.909108
285.635187	58.145901	74.914113
284.520056	61.477332	74.919118
284.162467	53.448249	74.924122
283.614797	62.848396	74.929127
282.730235	57.535066	74.934132
282.141477	62.785194	74.939137
281.169408	57.246132	74.944142
281.111984	58.095738	74.949146
280.586420	57.387925	74.954151
279.346670	61.433033	74.959156
279.013610	54.387148	74.964161
278.347083	63.118736	74.969166
277.560698	57.914330	74.974170
276.666169	68.993922	74.979175
276.122286	50.565267	74.984180
275.965255	59.677658	74.989185
274.637153	67.297375	74.994190
274.341486	55.264267	74.999194
273.567014	54.182997	75.004199
273.055705	68.815639	75.009204
272.858875	59.529413	75.014209
271.557657	63.355681	75.019214
270.902535	58.551373	75.024218
270.569469	52.776430	75.029223
269.623272	67.197712	75.034228
268.933756	59.182117	75.039233
267.951940	66.101709	75.044238
267.743467	62.170737	75.049242
267.538199	65.680398	75.054247
266.278336	58.575678	75.059252
265.827277	58.204476	75.064257
264.901627	66.138489	75.069262
264.026495	59.024480	75.074266
263.322573	63.044106	75.079271
262.800202	63.753374	75.084276
262.432598	74.679600	75.089281
262.008863	63.669779	75.094286
261.515419	63.598627	75.099290
260.671020	66.517931	75.104295
260.008740	57.887759	75.109300
259.219936	57.745424	75.114305
258.049933	69.543823	75.119310
257.495209	54.134986	75.124314
257.193130	56.794389	75.129319
256.281692	61.731706	75.134324
255.640503	58.066819	75.139329
254.713951	62.555568	75.144334
254.294144	57.929783	75.149338
253.894943	57.744269	75.154343
253.433373	54.919594	75.159348
252.662796	53.041402	75.164353
252.018388	66.575699	75.169358
251.351565	58.747292	75.174362
250.290292	68.213549	75.179367
249.260137	61.283519	75.184372
249.109321	62.255238	75.189377
248.334105	61.297088	75.194382
248.377619	56.777209	75.199386
247.371925	70.596167	75.204391
246.467473	66.279434	75.209396
245.968991	53.026649	75.214401
245.312285	63.112765	75.219406
244.443121	54.531348	75.224410
244.002955	62.359592	75.229415
243.263179	60.618409	75.234420
242.816150	57.949102	75.239425
241.522056	60.036564	75.244430
241.236459	59.910207	75.249434
240.609282	59.715308	75.254439
239.984571	58.249077	75.259444
239.327396	61.714091	75.264449
238.447583	64.408827	75.269454
237.995662	59.341917	75.274458
237.644041	59.677064	75.279463
236.360825	60.111836	75.284468
235.662370	59.759578	75.289473
235.038202	66.111268	75.294478
234.792018	61.613917	75.299482
234.465926	60.166312	75.304487
233.307074	65.236112	75.309492
232.925787	62.591017	75.314497
232.274174	67.516884	75.319502
231.282614	60.106080	75.324506
230.590277	59.129993	75.329511
229.894069	66.483429	75.334516
229.847654	53.144392	75.339521
228.627471	65.144749	75.344526
227.923579	55.881023	75.349530
227.507760	57.636106	75.354535
226.505066	67.149798	75.359540
226.023415	62.932820	75.364545
224.793824	67.113521	75.369550
224.652986	62.843788	75.374554
224.525751	60.093545	75.379559
223.419912	56.274099	75.384564
222.792115	53.458585	75.389569
222.099217	47.253772	75.394574
221.694575	56.689465	75.399578
221.147370	69.460847	75.404583
219.685657	65.226655	75.409588
219.693699	59.121393	75.414593
218.833527	60.531028	75.419598
218.235563	58.030859	75.424602
217.225602	62.681140	75.429607
216.232322	61.735689	75.434612
216.118353	49.960621	75.439617
215.526381	59.298455	75.444622
214.922761	75.224644	75.449626
214.012332	45.884329	75.454631
213.449626	58.834780	75.459636
213.132206	57.847812	75.464641
212.472898	43.849609	75.469646
211.303741	72.200036	75.474650
211.231918	60.493930	75.479655
210.397877	56.810920	75.484660
209.423259	47.334917	75.489665
208.376736	68.150547	75.494670
207.951953	60.226801	75.499674
207.904557	52.074174	75.504679
206.956825	78.099734	75.509684
206.270353	51.223014	75.514689
205.390811	63.675239	75.519694
205.256352	66.981240	75.524698
204.693151	50.007971	75.529703
203.313587	75.225645	75.534708
202.817485	62.306779	75.539713
202.532192	63.076028	75.544718
201.694446	51.570880	75.549722
200.556507	69.638455	75.554727
199.819877	57.355566	75.559732
199.585958	44.208851	75.564737
198.791765	65.069399	75.569742
198.720878	61.788238	75.574746
197.639351	46.043979	75.579751
196.832706	56.291188	75.584756
196.484452	77.503254	75.589761
196.105663	56.487503	75.594766
194.790335	58.256697	75.599770
194.044884	56.929568	75.604775
193.610922	72.817671	75.609780
193.564685	54.314437	75.614785
192.296217	50.260756	75.619790
191.806374	54.960577	75.624794
191.051464	75.365477	75.629799
190.356608	63.779201	75.634804
189.217068	48.777426	75.639809
188.876578	57.024991	75.644814
187.991469	65.797752	75.649818
188.003237	55.273576	75.654823
187.575607	60.367154	75.659828
187.045045	69.026625	75.664833
185.913513	59.142011	75.669838
185.139750	67.606882	75.674842
184.358325	59.419903	75.679847
183.527600	60.804357	75.684852
183.380241	40.675768	75.689857
182.602500	60.106645	75.694862
181.679846	72.983620	75.699866
181.065921	58.055726	75.704871
180.161749	62.610312	75.709876
180.194733	42.061912	75.714881
179.096336	64.398005	75.719886
178.516206	62.188296	75.724890
177.540981	42.932815	75.729895
177.219911	58.667294	75.734900
176.631713	67.465256	75.739905
175.687347	58.003362	75.744910
175.125291	57.924245	75.749914
174.802958	64.522693	75.754919
173.728126	54.909727	75.759924
172.887106	49.873336	75.764929
172.134941	67.510427	75.769934
171.618341	55.107322	75.774938
171.487886	46.255210	75.779943
171.210939	55.372522	75.784948
170.151998	54.904305	75.789953
169.382530	65.602884	75.794958
168.841178	55.084903	75.799962
167.868900	44.990427	75.804967
166.782258	59.501921	75.809972
166.785796	50.387187	75.814977
166.150780	55.236306	75.819982
165.415167	47.850959	75.824986
164.655537	57.201339	75.829991
163.724618	55.757145	75.834996
163.628763	49.786719	75.840001
162.532741	60.132112	75.845006
161.764202	62.116896	75.850010
161.320542	54.763840	75.855015
160.756216	50.845472	75.860020
160.095044	46.218775	75.865025
158.966638	62.668567	75.870030
158.318203	44.899992	75.875034
157.809867	64.294229	75.880039
157.486617	46.541608	75.885044
157.347798	46.697766	75.890049
156.435713	64.715144	75.895054
155.640012	56.303389	75.900058
154.976038	54.733063	75.905063
153.743056	46.624411	75.910068
153.473212	62.237192	75.915073
152.669039	65.460755	75.920078
151.761521	58.176929	75.925082
150.984650	54.451713	75.930087
150.552744	58.833242	75.935092
150.043670	43.759356	75.940097
149.491254	58.728108	75.945102
149.189137	67.962974	75.950106
148.350187	56.344507	75.955111
147.378676	50.233025	75.960116
147.217999	62.636868	75.965121
146.016657	49.701181	75.970126
145.375124	51.060210	75.975130
144.864484	51.904816	75.980135
144.450589	67.113246	75.985140
143.343065	54.583615	75.990145
142.511800	52.264160	75.995150
142.208149	67.532277	76.000154
142.087716	49.682668	76.005159
140.799332	43.388345	76.010164
140.266233	64.774930	76.015169
139.655375	56.554467	76.020174
138.787510	53.212747	76.025178
138.096349	56.107653	76.030183
137.196597	70.381223	76.035188
136.976032	48.233333	76.040193
135.984574	72.472991	76.045198
135.901026	52.800971	76.050202
134.760455	48.684355	76.055207
133.903798	73.862819	76.060212
133.681557	45.663266	76.065217
133.367300	52.462259	76.070222
132.040848	69.579114	76.075226
131.627049	46.620004	76.080231
130.877222	61.066766	76.085236
130.758572	67.558628	76.090241
129.550320	67.779665	76.095246
128.639240	53.853171	76.100250
128.271870	49.010913	76.105255
127.768798	56.915423	76.110260
127.026838	66.846432	76.115265
126.054632	44.831019	76.120270
125.437270	58.851408	76.125274
125.158678	60.777000	76.130279
124.389243	54.623843	76.135284
123.488072	55.220089	76.140289
123.063709	65.505703	76.145294
122.357581	62.950272	76.150298
122.249310	58.642244	76.155303
120.964101	65.029982	76.160308
120.463757	59.016831	76.165313
119.973933	60.405289	76.170318
118.829228	62.762284	76.175322
118.371598	59.601142	76.180327
117.408501	69.332467	76.185332
117.257415	52.515851	76.190337
116.606179	61.420058	76.195342
115.828403	61.838945	76.200346
114.974944	50.419918	76.205351
114.202490	62.441952	76.210356
114.009884	55.725341	76.215361
112.697050	45.133303	76.220366
112.142827	66.758209	76.225370
111.593996	66.705380	76.230375
110.807989	63.673868	76.235380
110.878397	36.764840	76.240385
109.837810	74.324044	76.245390
109.394556	51.886838	76.250394
108.740884	65.767956	76.255399
107.654647	65.662063	76.260404
106.997257	42.200957	76.265409
106.112570	57.304691	76.270414
105.839502	60.749481	76.275418
105.683583	47.593501	76.280423
104.594879	62.316642	76.285428
104.073304	60.318373	76.290433
103.592640	50.377327	76.295438
102.513541	60.399942	76.300442
101.825999	47.046484	76.305447
100.909717	53.577231	76.310452
100.800914	58.700395	76.315457
100.370129	59.175909	76.320462
99.240949	56.691103	76.325466
98.605572	55.209266	76.330471
98.086455	58.119323	76.335476
97.175807	59.838225	76.340481
96.510700	60.433103	76.345486
96.170164	54.370823	76.350490
95.407690	48.982917	76.355495
94.265598	59.985338	76.360500
93.769859	55.746988	76.365505
93.267007	52.463763	76.370510
92.685607	47.841711	76.375514
92.118325	51.306613	76.380519
91.124161	56.820106	76.385524
90.576216	42.048889	76.390529
90.366538	55.111771	76.395534
89.216016	59.303576	76.400538
88.706150	45.797220	76.405543
87.705291	61.493459	76.410548
87.377055	51.567530	76.415553
87.112801	57.680511	76.420558
86.038956	63.630886	76.425562
85.518210	53.119110	76.430567
84.564624	61.082858	76.435572
84.366261	53.331184	76.440577
83.220358	56.744871	76.445582
82.415088	62.281857	76.450586
81.960797	59.167496	76.455591
81.470825	60.999078	76.460596
80.798391	53.166899	76.465601
80.040021	56.433636	76.470606
79.225211	54.349683	76.475610
78.924830	56.283484	76.480615
78.013561	59.144126	76.485620
77.232124	53.177394	76.490625
76.902192	53.230003	76.495630
76.355244	60.372019	76.500634
75.645279	54.187322	76.505639
74.492499	63.225134	76.510644
73.807580	49.806617	76.515649
73.500478	58.258582	76.520654
73.037313	63.725246	76.525658
72.096209	49.229603	76.530663
71.058256	52.555120	76.535668
70.807803	57.453309	76.540673
70.404574	59.302595	76.545678
69.712390	61.836586	76.550682
69.050266	50.756048	76.555687
68.216391	58.016357	76.560692
67.654156	57.678691	76.565697
66.573114	60.039747	76.570702
65.695584	64.709962	76.575706
65.476693	56.181026	76.580711
65.028933	60.451562	76.585716
64.491573	65.419163	76.590721
63.782780	48.962726	76.595726
62.657833	55.276046	76.600730
62.445348	62.834623	76.605735
61.928555	57.528961	76.610740
60.874463	62.101187	76.615745
60.117011	66.607184	76.620750
59.225297	59.681977	76.625754
59.212204	54.896762	76.630759
58.540077	62.736788	76.635764
57.574952	51.646234	76.640769
57.038598	50.224306	76.645774
56.083692	69.095300	76.650778
55.904082	55.096336	76.655783
54.931290	55.651993	76.660788
54.203258	74.565654	76.665793
54.003483	57.974417	76.670798
52.469991	59.737481	76.675802
52.396427	43.447809	76.680807
51.039853	69.376159	76.685812
51.166279	60.684924	76.690817
50.914574	51.576218	76.695822
49.570937	60.381144	76.700826
48.886647	47.438746	76.705831
48.310406	54.943378	76.710836
47.944699	47.924828	76.715841
47.172258	49.471905	76.720846
46.078075	54.813720	76.725850
45.952585	49.683760	76.730855
45.507841	54.395332	76.735860
44.658786	52.963359	76.740865
43.925869	57.265185	76.745870
43.368408	60.900407	76.750874
42.064832	48.409995	76.755879
41.050390	55.757452	76.760884
40.521559	61.453773	76.765889
40.428501	64.891935	76.770894
40.090763	56.041361	76.775898
40.052791	47.217094	76.780903
38.982198	53.733050	76.785908
38.163540	50.503361	76.790913
36.844458	46.853629	76.795918
35.824729	57.363500	76.800922
35.577195	44.436601	76.805927
34.873446	56.178046	76.810932
34.835734	55.554894	76.815937
34.213381	61.821181	76.820942
33.218858	64.859110	76.825946
32.608986	62.047098	76.830951
32.110235	47.996554	76.835956
30.845503	45.563363	76.840961
30.360171	52.928927	76.845966
29.769463	66.517757	76.850970
29.630202	46.679629	76.855975
28.589911	55.286379	76.860980
27.653687	54.752924	76.865985
27.237172	58.521776	76.870990
26.495845	54.846125	76.875994
26.365869	51.632745	76.880999
25.251486	57.155974	76.886004
24.587833	56.101262	76.891009
24.304984	59.891370	76.896014
22.880562	54.038251	76.901018
22.191563	61.945625	76.906023
22.013879	52.467175	76.911028
21.359970	56.313312	76.916033
21.267516	50.263517	76.921038
19.938875	61.355639	76.926042
19.228516	55.008610	76.931047
18.906372	58.210516	76.936052
18.078809	56.390375	76.941057
17.118601	51.808264	76.946062
16.076330	66.017861	76.951066
16.177853	59.415188	76.956071
15.761728	52.828855	76.961076
14.757306	67.395090	76.966081
14.019230	66.265524	76.971086
13.698962	67.871368	76.976090
13.098436	43.672739	76.981095
11.756314	71.634499	76.986100
11.504762	41.547467	76.991105
11.179052	52.635724	76.996110
10.035778	55.490820	77.001114
9.168046	59.388411	77.006119
8.524044	54.457845	77.011124
8.110082	49.541047	77.016129
7.461722	52.446504	77.021134
6.206732	73.661259	77.026139
6.024728	51.125662	77.031143
5.399686	57.991581	77.036148
5.163356	61.315410	77.041153
4.039761	57.751199	77.046158