Mon Mar 08 20:36:09 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.485897	93.371664	0.000000
-1.900941	93.267523	0.005005
-2.309470	66.105278	0.010010
-4.930919	40.221637	0.015014
-9.518841	38.946035	0.020019
-14.155426	29.396647	0.025024
-19.417194	45.446047	0.030029
-23.643038	38.899689	0.035034
-26.890682	40.603442	0.040038
-30.342399	33.720749	0.045043
-33.742001	40.072041	0.050048
-37.968117	45.687913	0.055053
-41.818900	38.810546	0.060058
-45.723491	42.449823	0.065062
-49.238214	39.740062	0.070067
-52.490456	34.648408	0.075072
-57.053327	42.128239	0.080077
-60.987770	34.012241	0.085082
-64.614734	35.096935	0.090086
-68.664370	46.020728	0.095091
-71.766842	34.383405	0.100096
-75.271287	40.478683	0.105101
-79.069669	30.724755	0.110106
-83.101635	40.092562	0.115110
-87.283884	29.513702	0.120115
-90.524008	27.130754	0.125120
-94.588804	41.385705	0.130125
-98.181662	31.469719	0.135130
-101.835408	31.765591	0.140134
-105.818056	33.719161	0.145139
-109.378311	23.944643	0.150144
-113.744692	29.899959	0.155149
-117.165579	36.218488	0.160154
-120.966111	35.255839	0.165158
-124.516634	37.123152	0.170163
-128.106810	30.529183	0.175168
-132.257953	36.339814	0.180173
-135.995173	27.195922	0.185178
-139.666567	30.085409	0.190182
-143.819395	26.742794	0.195187
-146.910458	38.557626	0.200192
-150.862547	41.674830	0.205197
-154.475392	41.101726	0.210202
-157.903447	28.018483	0.215206
-162.401491	36.058971	0.220211
-165.958045	24.252987	0.225216
-170.211986	33.154911	0.230221
-174.056585	33.875554	0.235226
-177.616604	30.257071	0.240230
-181.548940	37.962917	0.245235
-184.880250	38.764087	0.250240
-188.568869	40.420157	0.255245
-192.268444	36.767197	0.260250
-196.064406	32.210329	0.265254
-199.824301	36.917928	0.270259
-203.816856	31.463688	0.275264
-207.380101	37.648950	0.280269
-211.187743	30.621493	0.285274
-214.708314	21.484159	0.290278
-218.747012	29.032003	0.295283
-222.357705	35.417230	0.300288
-226.390296	29.169964	0.305293
-229.959142	27.623353	0.310298
-233.680364	34.051464	0.315302
-237.345288	43.576965	0.320307
-241.190290	31.992157	0.325312
-245.175005	37.424781	0.330317
-249.110594	37.231308	0.335322
-252.665950	29.673262	0.340326
-256.352941	34.236856	0.345331
-259.910315	34.940178	0.350336
-263.860715	40.712682	0.355341
-267.660874	39.568869	0.360346
-271.509268	36.942653	0.365350
-275.298494	41.628242	0.370355
-278.650278	26.871033	0.375360
-282.731193	42.601606	0.380365
-286.423012	36.177058	0.385370
-290.130636	30.584455	0.390374
-293.969007	43.185740	0.395379
-297.674566	34.792360	0.400384
-301.584737	46.279259	0.405389
-304.878082	29.756166	0.410394
-308.939283	31.566498	0.415398
-313.039509	42.482974	0.420403
-316.238410	38.851208	0.425408
-320.409811	44.059883	0.430413
-324.165278	29.159038	0.435418
-327.812820	41.947512	0.440422
-331.594963	42.075007	0.445427
-334.906546	38.431294	0.450432
-339.133813	33.686484	0.455437
-342.741478	45.470481	0.460442
-346.694173	35.292235	0.465446
-350.336370	43.393541	0.470451
-354.035785	28.149513	0.475456
-358.286900	44.572796	0.480461
-361.943564	37.135160	0.485466
-365.187579	33.914333	0.490470
-368.993465	36.175978	0.495475
-372.672790	35.378868	0.500480
-376.922855	41.347614	0.505485
-380.602073	32.161750	0.510490
-384.143370	38.178190	0.515494
-388.107846	39.210025	0.520499
-391.499219	30.139062	0.525504
-395.853916	41.359627	0.530509
-399.284265	45.142927	0.535514
-402.821227	38.025264	0.540518
-406.703272	41.095429	0.545523
-410.249705	33.950908	0.550528
-414.763373	49.575755	0.555533
-418.529767	32.160190	0.560538
-422.194950	29.216408	0.565542
-425.751321	37.778742	0.570547
-429.133932	29.176333	0.575552
-433.235215	36.471185	0.580557
-436.743766	40.339557	0.585562
-440.544641	27.204334	0.590566
-444.309471	36.709809	0.595571
-448.240769	25.766724	0.600576
-452.313111	35.403308	0.605581
-455.580220	30.257832	0.610586
-459.370255	30.908720	0.615590
-463.561478	38.922827	0.620595
-466.937631	26.941873	0.625600
-470.796705	34.843032	0.630605
-474.513257	31.259457	0.635610
-478.243352	26.342478	0.640614
-481.968687	27.831404	0.645619
-485.675548	33.295727	0.650624
-489.759460	31.685114	0.655629
-493.350288	39.027848	0.660634
-496.753023	28.154966	0.665638
-500.983910	34.519797	0.670643
-504.501155	33.578745	0.675648
-508.503024	36.977265	0.680653
-512.059465	22.363488	0.685658
-515.725778	31.298288	0.690662
-520.002020	32.742803	0.695667
-523.250302	28.590973	0.700672
-527.399489	33.547306	0.705677
-530.994816	39.523701	0.710682
-534.608525	36.824166	0.715686
-538.509675	45.541067	0.720691
-542.156222	35.456185	0.725696
-546.041183	40.777173	0.730701
-549.788489	27.199956	0.735706
-553.799027	42.211705	0.740710
-557.600536	37.758806	0.745715
-560.749828	26.872350	0.750720
-564.564407	38.871032	0.755725
-568.309409	31.184511	0.760730
-572.102469	35.365003	0.765734
-576.172629	31.768692	0.770739
-579.670083	29.643546	0.775744
-583.958882	31.356664	0.780749
-587.506735	41.141483	0.785754
-591.259323	31.306994	0.790758
-595.223192	46.014912	0.795763
-598.893251	33.685321	0.800768
-602.233040	35.579587	0.805773
-606.022837	40.010328	0.810778
-609.809522	32.563904	0.815782
-613.823566	42.298663	0.820787
-617.404536	32.651250	0.825792
-621.371433	32.405050	0.830797
-625.189558	35.411738	0.835802
-628.409983	33.431628	0.840806
-632.372836	42.238947	0.845811
-636.128711	29.615651	0.850816
-640.218483	39.288437	0.855821
-643.926924	39.439342	0.860826
-647.482434	37.700432	0.865830
-651.474214	37.486640	0.870835
-654.745300	35.096801	0.875840
-658.763852	35.483339	0.880845
-662.322782	33.446979	0.885850
-666.109845	35.221998	0.890854
-670.152817	46.284428	0.895859
-673.990342	30.828066	0.900864
-678.151811	45.942964	0.905869
-681.659027	39.650395	0.910874
-685.025043	34.502126	0.915878
-688.981930	40.604323	0.920883
-692.390230	35.095419	0.925888
-696.941355	37.057218	0.930893
-700.321365	32.967683	0.935898
-704.062499	27.921956	0.940902
-708.218953	32.045615	0.945907
-711.235029	20.330761	0.950912
-715.091022	34.744090	0.955917
-718.693420	27.706763	0.960922
-722.249710	33.984676	0.965926
-726.611397	37.436321	0.970931
-730.270133	22.255828	0.975936
-734.243874	35.276743	0.980941
-738.115331	33.892787	0.985946
-741.694202	30.043232	0.990950
-745.533548	29.179241	0.995955
-748.804576	30.375226	1.000960
-752.560780	30.803571	1.005965
-756.746664	24.559661	1.010970
-760.291025	20.482291	1.015974
-764.560244	39.594444	1.020979
-768.126699	27.828859	1.025984
-771.920603	38.652961	1.030989
-775.339833	29.900824	1.035994
-778.806264	25.688034	1.040998
-782.879397	46.393016	1.046003
-786.627010	24.355014	1.051008
-790.614218	38.492985	1.056013
-794.246941	31.854830	1.061018
-798.274357	30.407598	1.066022
-802.098786	31.504461	1.071027
-805.523731	30.211666	1.076032
-809.510953	44.051654	1.081037
-813.098630	32.205959	1.086042
-816.661978	39.771827	1.091046
-820.659463	41.635911	1.096051
-823.899868	37.193110	1.101056
-827.917934	44.970436	1.106061
-831.972549	44.886831	1.111066
-835.699077	37.029080	1.116070
-839.592589	28.639835	1.121075
-843.286303	36.049973	1.126080
-847.121033	32.867478	1.131085
-850.587569	36.679269	1.136090
-854.189246	31.964704	1.141094
-858.171688	27.471848	1.146099
-862.131104	43.160238	1.151104
-865.933296	40.324203	1.156109
-869.564315	33.175006	1.161114
-873.133178	44.195082	1.166118
-877.241955	35.706280	1.171123
-880.513441	28.130652	1.176128
-884.495413	36.380073	1.181133
-888.285113	40.025978	1.186138
-891.900949	44.987550	1.191142
-895.957455	32.601980	1.196147
-899.786772	29.741957	1.201152
-903.519719	32.216693	1.206157
-907.242398	35.148649	1.211162
-910.573646	33.970328	1.216166
-914.764742	39.914805	1.221171
-918.426937	40.692630	1.226176
-922.540292	45.041563	1.231181
-926.155283	40.463268	1.236186
-929.318205	34.874494	1.241190
-933.052075	44.949712	1.246195
-936.867351	45.685814	1.251200
-941.087094	46.391981	1.256205
-944.750402	30.520354	1.261210
-948.582021	40.715291	1.266214
-952.389199	40.865122	1.271219
-956.013049	33.951443	1.276224
-959.818872	36.045291	1.281229
-963.410071	45.787108	1.286234
-966.994321	39.062638	1.291238
-971.151011	46.901784	1.296243
-974.697464	38.074108	1.301248
-978.877521	40.278285	1.306253
-982.564308	29.979816	1.311258
-985.912788	40.882812	1.316262
-989.825901	36.352291	1.321267
-993.300862	35.739496	1.326272
-997.262816	37.341173	1.331277
-1001.394088	28.894045	1.336282
-1004.911468	24.823777	1.341286
-1008.797955	33.230000	1.346291
-1012.487827	27.724036	1.351296
-1016.334180	37.795285	1.356301
-1019.928556	37.748783	1.361306
-1023.390117	38.803743	1.366310
-1027.466791	52.464431	1.371315
-1031.405180	38.265795	1.376320
-1034.912143	39.176658	1.381325
-1038.987476	31.887500	1.386330
-1042.384171	36.535149	1.391334
-1046.050994	42.665644	1.396339
-1049.787877	34.557618	1.401344
-1054.341085	49.470866	1.406349
-1057.961833	52.071393	1.411354
-1061.519221	31.886188	1.416358
-1065.423895	42.506115	1.421363
-1068.798042	34.775309	1.426368
-1072.330806	39.842122	1.431373
-1076.169871	36.785271	1.436378
-1079.840043	33.663571	1.441382
-1083.843173	34.850968	1.446387
-1087.800400	39.720789	1.451392
-1091.673034	32.252662	1.456397
-1095.590877	45.992117	1.461402
-1098.434636	34.376383	1.466406
-1102.588749	44.919583	1.471411
-1106.172874	40.401288	1.476416
-1110.286841	45.275720	1.481421
-1114.167498	48.588055	1.486426
-1117.773043	42.953661	1.491430
-1121.882159	47.142998	1.496435
-1125.421434	38.795348	1.501440
-1129.116403	34.066184	1.506445
-1132.757715	37.039088	1.511450
-1136.584738	30.725859	1.516454
-1140.426303	42.974122	1.521459
-1143.991749	27.623310	1.526464
-1147.795697	28.241258	1.531469
-1151.645078	35.820249	1.536474
-1155.122411	34.671957	1.541478
-1159.213298	39.873911	1.546483
-1162.915021	32.301302	1.551488
-1166.536748	27.778085	1.556493
-1170.491638	29.434111	1.561498
-1174.250198	23.333907	1.566502
-1178.172394	37.864162	1.571507
-1181.310208	28.227193	1.576512
-1185.277336	32.108514	1.581517
-1189.195106	23.430481	1.586522
-1193.089071	31.172772	1.591526
-1197.085343	46.941681	1.596531
-1200.649780	37.396643	1.601536
-1204.272861	39.024867	1.606541
-1207.921958	36.450310	1.611546
-1211.305006	29.820192	1.616550
-1215.710383	44.916634	1.621555
-1219.212549	31.820132	1.626560
-1223.136227	32.501511	1.631565
-1227.092557	32.989441	1.636570
-1230.494173	24.888002	1.641574
-1234.384012	28.337605	1.646579
-1237.956320	29.913606	1.651584
-1241.939859	35.869586	1.656589
-1245.812969	41.263902	1.661594
-1249.472121	39.971395	1.666598
-1253.244148	38.450973	1.671603
-1256.733707	24.882632	1.676608
-1260.839883	31.574140	1.681613
-1264.296555	37.791170	1.686618
-1268.055018	37.068049	1.691622
-1272.150280	38.729365	1.696627
-1275.631903	30.964043	1.701632
-1279.388939	33.462147	1.706637
-1283.113415	37.847226	1.711642
-1286.783507	29.277947	1.716646
-1291.191835	43.178187	1.721651
-1294.292181	28.510072	1.726656
-1298.082226	29.624313	1.731661
-1302.215284	31.726931	1.736666
-1305.705894	25.495764	1.741670
-1309.716352	39.081643	1.746675
-1313.308950	39.453166	1.751680
-1317.349662	37.283628	1.756685
-1320.839457	37.755394	1.761690
-1324.134843	30.559533	1.766694
-1327.978502	35.318540	1.771699
-1331.815393	33.650948	1.776704
-1336.316204	37.028211	1.781709
-1339.974092	40.308412	1.786714
-1343.605284	27.598594	1.791718
-1347.405867	28.749292	1.796723
-1350.614032	36.246463	1.801728
-1354.378607	41.473785	1.806733
-1358.552517	39.090694	1.811738
-1362.266959	30.670555	1.816742
-1366.765089	38.956071	1.821747
-1369.755523	27.033058	1.826752
-1373.225235	28.469851	1.831757
-1377.163031	36.080695	1.836762
-1380.445868	27.941553	1.841766
-1384.825738	45.069871	1.846771
-1388.489583	34.052544	1.851776
-1392.310742	39.329979	1.856781
-1396.293633	42.118293	1.861786
-1399.842428	35.797244	1.866790
-1403.608499	43.137814	1.871795
-1407.196589	38.391997	1.876800
-1410.972918	44.617837	1.881805
-1414.964983	35.509009	1.886810
-1418.489497	34.494814	1.891814
-1422.795592	45.080225	1.896819
-1426.417561	30.603038	1.901824
-1429.823508	28.891849	1.906829
-1433.583868	36.252047	1.911834
-1437.115449	33.400448	1.916838
-1441.107206	33.610589	1.921843
-1444.758878	28.542308	1.926848
-1448.928890	33.394756	1.931853
-1453.021728	33.193785	1.936858
-1456.236989	32.544837	1.941862
-1460.152180	36.628020	1.946867
-1463.696451	42.025228	1.951872
-1467.556876	44.798785	1.956877
-1471.450099	45.269145	1.961882
-1474.608780	36.075872	1.966886
-1478.623673	37.995894	1.971891
-1482.584182	46.296464	1.976896
-1486.151809	48.020317	1.981901
-1490.102226	47.463899	1.986906
-1493.811626	36.219099	1.991910
-1497.897077	45.293416	1.996915
-1501.511743	40.011460	2.006912
-1502.680516	41.390551	2.016909
-1500.159248	38.724290	2.026906
-1497.177956	37.672142	2.036902
-1495.200334	40.055205	2.046899
-1493.311582	38.639621	2.056896
-1490.801870	31.906572	2.066893
-1489.290659	42.537934	2.076890
-1487.642346	43.505419	2.086886
-1485.727838	39.692207	2.096883
-1483.576639	39.366630	2.106880
-1481.636126	32.697889	2.116877
-1480.031299	36.528448	2.126874
-1478.061142	31.200128	2.136870
-1476.028275	28.110026	2.146867
-1474.202343	38.482600	2.156864
-1472.320472	27.325165	2.166861
-1470.513015	34.181483	2.176858
-1468.324663	32.650060	2.186854
-1466.744661	23.321887	2.196851
-1464.745258	37.193802	2.206848
-1462.777566	29.895507	2.216845
-1460.995261	30.110558	2.226842
-1459.058795	39.835496	2.236838
-1457.342486	31.969602	2.246835
-1455.506618	35.002191	2.256832
-1453.399759	29.745156	2.266829
-1451.489165	33.885176	2.276826
-1449.735342	28.889914	2.286822
-1447.645809	28.159012	2.296819
-1445.622075	29.945830	2.306816
-1443.940554	31.318525	2.316813
-1442.122877	33.048344	2.326810
-1440.336444	25.032300	2.336806
-1438.178437	27.752821	2.346803
-1436.293576	31.132819	2.356800
-1434.996196	31.302376	2.366797
-1432.916157	27.102734	2.376794
-1430.770806	30.963627	2.386790
-1428.982802	29.325821	2.396787
-1427.039370	29.264069	2.406784
-1425.251651	31.786534	2.416781
-1423.514594	33.312974	2.426778
-1421.139532	32.177989	2.436774
-1419.315199	34.058328	2.446771
-1417.796154	29.299608	2.456768
-1415.593262	31.474584	2.466765
-1413.648938	34.028826	2.476762
-1412.439331	31.392653	2.486758
-1410.508292	32.267568	2.496755
-1408.296989	30.407287	2.506752
-1406.473284	28.665895	2.516749
-1404.040358	33.971196	2.526746
-1402.509740	37.494769	2.536742
-1400.784503	30.667934	2.546739
-1399.130615	29.853667	2.556736
-1396.967689	32.298725	2.566733
-1395.013310	38.301124	2.576730
-1393.107648	34.269945	2.586726
-1391.482029	37.535177	2.596723
-1389.484531	33.055121	2.606720
-1387.653615	35.401767	2.616717
-1385.919764	42.590448	2.626714
-1383.931751	34.379550	2.636710
-1381.798987	37.936213	2.646707
-1380.002931	28.824537	2.656704
-1377.888931	31.730570	2.666701
-1376.493995	29.732595	2.676698
-1374.536074	33.295148	2.686694
-1372.770245	31.228333	2.696691
-1370.458011	28.265695	2.706688
-1368.728311	32.382641	2.716685
-1367.122210	36.520953	2.726682
-1365.320399	43.337220	2.736678
-1363.208033	33.290775	2.746675
-1361.333189	36.563502	2.756672
-1359.382199	37.613675	2.766669
-1357.311010	41.461252	2.776666
-1355.642774	33.170517	2.786662
-1353.949172	36.349112	2.796659
-1352.229522	36.583749	2.806656
-1349.987652	41.079754	2.816653
-1347.935080	39.317563	2.826650
-1346.185544	34.537780	2.836646
-1344.406804	41.499852	2.846643
-1342.594793	33.364522	2.856640
-1340.728557	33.125739	2.866637
-1338.942939	41.949739	2.876634
-1337.155486	38.302233	2.886630
-1335.011989	32.908391	2.896627
-1332.843480	33.465910	2.906624
-1331.205860	38.001806	2.916621
-1329.687574	37.253499	2.926618
-1327.667149	29.964235	2.936614
-1325.384863	35.945793	2.946611
-1323.454581	32.738037	2.956608
-1321.825475	34.547077	2.966605
-1320.318015	30.911242	2.976602
-1318.103676	32.985015	2.986598
-1316.268010	33.392150	2.996595
-1314.415929	33.304064	3.006592
-1312.478685	34.407000	3.016589
-1310.625926	35.810807	3.026586
-1308.652872	36.281217	3.036582
-1306.754749	31.092448	3.046579
-1305.018799	38.045611	3.056576
-1303.125494	34.156996	3.066573
-1301.178028	30.992294	3.076570
-1299.292336	27.775907	3.086566
-1297.438399	31.344117	3.096563
-1295.516448	31.685358	3.106560
-1293.743171	38.299424	3.116557
-1291.978039	42.690218	3.126554
-1290.016077	43.381878	3.136550
-1288.315090	42.822238	3.146547
-1286.191463	29.873733	3.156544
-1284.221159	35.103213	3.166541
-1282.549442	36.417603	3.176538
-1280.604406	38.641871	3.186534
-1278.584039	37.524322	3.196531
-1276.873689	36.402705	3.206528
-1274.954343	32.655198	3.216525
-1273.059999	32.757735	3.226522
-1271.222590	33.972992	3.236518
-1269.251832	30.356199	3.246515
-1267.675254	32.506818	3.256512
-1265.707369	26.026482	3.266509
-1263.394991	29.535569	3.276506
-1261.759910	44.184369	3.286502
-1259.913595	33.376952	3.296499
-1258.182656	29.446464	3.306496
-1256.101944	34.830395	3.316493
-1254.229061	30.150932	3.326490
-1252.556205	29.136379	3.336486
-1250.783722	40.324495	3.346483
-1248.552527	28.486096	3.356480
-1246.509794	29.575366	3.366477
-1244.772171	31.627605	3.376474
-1243.405025	35.057454	3.386470
-1241.363530	24.758787	3.396467
-1239.032764	26.662438	3.406464
-1237.353594	33.436860	3.416461
-1235.668155	31.964022	3.426458
-1233.692992	31.052678	3.436454
-1231.686934	34.511346	3.446451
-1229.943918	33.577155	3.456448
-1228.207417	26.724953	3.466445
-1225.921532	34.910094	3.476442
-1224.182768	35.670679	3.486438
-1222.249443	43.637522	3.496435
-1220.339628	31.261661	3.506432
-1218.737656	23.884715	3.516429
-1217.231843	34.386102	3.526426
-1214.962291	33.531874	3.536422
-1213.254986	40.791256	3.546419
-1210.934516	34.740827	3.556416
-1209.234069	37.863178	3.566413
-1207.478246	35.051297	3.576410
-1205.649640	36.465369	3.586406
-1203.569171	30.161264	3.596403
-1201.576885	29.652968	3.606400
-1199.742961	29.231586	3.616397
-1198.000174	30.542560	3.626394
-1196.091848	36.817754	3.636390
-1194.527301	31.816641	3.646387
-1192.484638	30.706650	3.656384
-1190.361364	31.735719	3.666381
-1188.647511	34.458073	3.676378
-1186.934425	35.944323	3.686374
-1184.824251	43.567140	3.696371
-1182.853113	32.929266	3.706368
-1180.916030	25.219274	3.716365
-1179.318618	30.393250	3.726362
-1177.668993	28.349908	3.736358
-1175.467904	38.534847	3.746355
-1173.517704	20.868198	3.756352
-1171.480808	36.329037	3.766349
-1169.937484	39.591811	3.776346
-1168.257809	27.532261	3.786342
-1166.122589	23.268760	3.796339
-1164.175247	34.515810	3.806336
-1162.128773	23.515404	3.816333
-1160.326762	32.130104	3.826330
-1158.702543	33.635328	3.836326
-1156.691623	31.567356	3.846323
-1154.868537	32.732895	3.856320
-1153.062395	34.030611	3.866317
-1151.046268	37.612471	3.876314
-1149.154371	32.107470	3.886310
-1147.428463	43.012625	3.896307
-1145.298256	33.486094	3.906304
-1143.552277	27.462901	3.916301
-1141.665765	31.509155	3.926298
-1140.154209	33.512382	3.936294
-1137.813709	33.295781	3.946291
-1135.835776	31.765172	3.956288
-1134.285043	24.472257	3.966285
-1132.347682	32.105397	3.976282
-1130.623676	26.751998	3.986278
-1128.847292	31.022707	3.996275
-1126.358901	32.474974	4.006272
-1124.709910	30.019693	4.016269
-1122.932787	32.081496	4.026266
-1121.173448	29.442787	4.036262
-1119.128626	31.763329	4.046259
-1117.562083	36.170240	4.056256
-1115.469317	31.743057	4.066253
-1113.451159	33.171090	4.076250
-1111.870974	32.859833	4.086246
-1109.806556	32.531117	4.096243
-1107.832358	30.020670	4.106240
-1106.013844	36.761858	4.116237
-1104.296435	33.424127	4.126234
-1102.282171	32.495587	4.136230
-1100.407913	32.901458	4.146227
-1098.576867	25.694770	4.156224
-1096.358660	32.790424	4.166221
-1094.646866	36.942030	4.176218
-1093.057737	29.534055	4.186214
-1091.165175	26.793539	4.196211
-1089.222749	28.989970	4.206208
-1087.283646	30.171740	4.216205
-1085.326046	36.286004	4.226202
-1083.508188	34.768411	4.236198
-1081.813880	30.332362	4.246195
-1079.700081	30.295753	4.256192
-1078.158265	35.131354	4.266189
-1075.833627	35.114708	4.276186
-1073.738367	25.530676	4.286182
-1072.332899	27.391453	4.296179
-1070.638574	28.036111	4.306176
-1068.381903	33.685742	4.316173
-1066.998106	27.024261	4.326170
-1065.048498	28.662233	4.336166
-1062.944891	27.430510	4.346163
-1061.030502	25.226490	4.356160
-1058.923748	29.081284	4.366157
-1057.131884	35.833091	4.376154
-1055.664726	32.290698	4.386150
-1053.480332	30.815552	4.396147
-1051.643165	31.225815	4.406144
-1049.430370	27.062105	4.416141
-1048.004744	26.838764	4.426138
-1045.809635	28.840094	4.436134
-1044.183630	28.684175	4.446131
-1042.529531	34.768073	4.456128
-1040.754490	29.566034	4.466125
-1038.425167	28.383493	4.476122
-1036.404947	35.892952	4.486118
-1034.490107	31.183262	4.496115
-1033.027062	29.397210	4.506112
-1031.037101	30.450903	4.516109
-1029.135747	24.349260	4.526106
-1027.224380	32.386100	4.536102
-1025.333730	29.175446	4.546099
-1023.426769	20.805700	4.556096
-1021.649837	22.905503	4.566093
-1019.638800	30.106992	4.576090
-1017.657220	22.228965	4.586086
-1016.116951	14.718339	4.596083
-1014.388104	25.192102	4.606080
-1012.391076	24.525325	4.616077
-1010.013490	19.316949	4.626074
-1008.611375	28.565688	4.636070
-1006.656781	20.371482	4.646067
-1004.721756	19.918297	4.656064
-1002.735504	24.834447	4.666061
-1001.026294	23.872675	4.676058
-999.124441	17.703088	4.686054
-997.259425	25.919456	4.696051
-995.298715	18.485282	4.706048
-993.281180	17.703145	4.716045
-991.607485	18.294321	4.726042
-989.984267	20.990269	4.736038
-987.982809	26.399756	4.746035
-985.679580	18.666099	4.756032
-984.149161	19.352818	4.766029
-982.128295	12.576886	4.776026
-980.350978	27.182644	4.786022
-978.457911	23.820072	4.796019
-976.698483	27.790478	4.806016
-974.544561	34.313945	4.816013
-973.018563	28.487084	4.826010
-970.906177	24.838414	4.836006
-969.114546	24.098734	4.846003
-967.045289	22.454196	4.856000
-965.386947	23.657279	4.865997
-963.744682	28.510054	4.875994
-961.740163	28.697854	4.885990
-959.332729	24.866237	4.895987
-957.668120	21.608101	4.905984
-956.091755	15.429014	4.915981
-954.014217	22.305739	4.925978
-952.209426	25.174774	4.935974
-950.493279	25.729196	4.945971
-948.345439	28.728109	4.955968
-946.416485	21.755333	4.965965
-944.438814	21.552729	4.975962
-942.903800	22.142432	4.985958
-941.011161	23.945923	4.995955
-938.891541	15.035432	5.005952
-937.453337	20.849208	5.015949
-935.319679	22.487861	5.025946
-933.231786	17.859524	5.035942
-931.656314	23.259806	5.045939
-929.611305	20.236114	5.055936
-927.872402	27.053330	5.065933
-926.032586	28.685292	5.075930
-924.068399	26.209752	5.085926
-922.074824	20.750244	5.095923
-920.142423	21.369580	5.105920
-918.423151	20.294162	5.115917
-916.380287	25.728672	5.125914
-914.683014	29.988519	5.135910
-912.961590	25.766130	5.145907
-911.300351	21.221809	5.155904
-909.163664	25.048276	5.165901
-906.805075	29.614481	5.175898
-905.387849	27.490065	5.185894
-903.356446	22.536068	5.195891
-901.373105	26.975966	5.205888
-899.658866	26.591319	5.215885
-897.893530	29.389343	5.225882
-896.086142	21.004030	5.235878
-894.009001	31.210655	5.245875
-892.052565	21.704221	5.255872
-890.065212	22.777398	5.265869
-888.695061	20.235810	5.275866
-886.634076	24.585945	5.285862
-884.524851	24.264473	5.295859
-882.523701	29.031519	5.305856
-880.788219	18.826256	5.315853
-879.152673	18.446309	5.325850
-877.093033	23.851333	5.335846
-875.336940	26.483494	5.345843
-873.366234	22.655466	5.355840
-871.548834	22.830625	5.365837
-869.558445	27.121014	5.375834
-868.002765	28.312159	5.385830
-865.611748	23.989081	5.395827
-863.842437	23.931950	5.405824
-861.947009	22.094253	5.415821
-860.386285	19.449591	5.425818
-858.525321	21.064015	5.435814
-856.800194	31.930065	5.445811
-854.251153	26.626539	5.455808
-852.633323	25.524754	5.465805
-851.123390	26.739011	5.475802
-849.069967	23.939815	5.485798
-846.919798	27.262115	5.495795
-845.350553	24.199285	5.505792
-843.181880	22.785263	5.515789
-841.400473	30.525696	5.525786
-839.918577	29.234083	5.535782
-837.641581	25.050828	5.545779
-835.819095	20.742871	5.555776
-834.045106	22.781716	5.565773
-832.160902	30.079438	5.575770
-830.335126	31.900025	5.585766
-828.231511	30.515360	5.595763
-826.382071	28.325064	5.605760
-824.647456	32.814260	5.615757
-822.762864	26.301792	5.625754
-820.683693	31.607440	5.635750
-819.072254	31.070347	5.645747
-817.160126	33.044499	5.655744
-815.149332	27.266552	5.665741
-813.578080	30.313543	5.675738
-811.360022	37.968427	5.685734
-809.231238	30.689090	5.695731
-807.776806	27.605163	5.705728
-805.915162	25.701861	5.715725
-804.078118	29.350545	5.725722
-802.185794	28.691207	5.735718
-800.151830	28.482885	5.745715
-798.372189	19.053721	5.755712
-796.405954	29.930231	5.765709
-794.604924	29.711777	5.775706
-792.709890	26.382189	5.785702
-790.482181	29.745831	5.795699
-788.953213	30.125037	5.805696
-787.215441	30.612969	5.815693
-785.314288	30.397466	5.825690
-783.404821	35.957627	5.835686
-781.567712	22.898998	5.845683
-779.368839	32.371068	5.855680
-777.701607	25.078687	5.865677
-775.765763	27.505369	5.875674
-774.383978	26.322947	5.885670
-771.920628	25.068724	5.895667
-769.977529	31.300843	5.905664
-768.472961	27.477921	5.915661
-766.136974	32.403128	5.925658
-764.559927	28.816504	5.935654
-762.693727	34.418331	5.945651
-760.899173	33.741494	5.955648
-759.007355	36.048920	5.965645
-757.190223	35.461629	5.975642
-755.252175	31.359455	5.985638
-753.135555	31.718980	5.995635
-751.355405	27.405216	6.005632
-749.407600	30.654166	6.015629
-747.658020	39.740208	6.025626
-745.671757	36.137145	6.035622
-743.847632	31.355335	6.045619
-742.192043	30.189174	6.055616
-740.345288	31.529668	6.065613
-738.027736	23.617110	6.075610
-736.480438	25.299124	6.085606
-734.574691	29.056879	6.095603
-732.778246	27.342461	6.105600
-730.592683	25.267463	6.115597
-729.062071	34.033267	6.125594
-727.098894	32.846384	6.135590
-725.003459	25.678230	6.145587
-723.228909	31.672079	6.155584
-721.478462	32.660106	6.165581
-719.635882	34.672294	6.175578
-717.354142	33.916063	6.185574
-715.840317	31.684747	6.195571
-714.101792	33.776720	6.205568
-711.952515	37.044033	6.215565
-709.982192	35.211853	6.225562
-708.272684	32.488252	6.235558
-706.376035	31.114660	6.245555
-704.376160	29.874566	6.255552
-702.975569	40.503682	6.265549
-700.853837	31.997218	6.275546
-698.712841	37.147851	6.285542
-697.214072	23.832302	6.295539
-695.058110	27.186976	6.305536
-693.118573	27.158034	6.315533
-691.187200	23.647466	6.325530
-689.499583	37.355261	6.335526
-687.814434	31.604182	6.345523
-685.739102	24.084033	6.355520
-683.731094	31.802603	6.365517
-682.038170	30.284751	6.375514
-680.053193	32.632616	6.385510
-678.229550	32.456424	6.395507
-676.393981	28.923281	6.405504
-674.710167	35.241121	6.415501
-672.687842	28.869376	6.425498
-670.972090	28.451497	6.435494
-668.555881	28.291157	6.445491
-666.814455	40.422585	6.455488
-665.043776	32.726925	6.465485
-663.340923	33.664184	6.475482
-661.456725	36.274467	6.485478
-659.337803	35.519042	6.495475
-657.708188	32.571413	6.505472
-655.563493	32.001336	6.515469
-653.944624	40.516273	6.525466
-651.954377	41.661820	6.535462
-650.328942	39.074839	6.545459
-648.100675	41.721739	6.555456
-646.243400	32.870750	6.565453
-644.612389	36.623531	6.575450
-642.680242	31.834010	6.585446
-640.898610	26.400686	6.595443
-638.626525	39.970947	6.605440
-636.903022	27.282637	6.615437
-635.014247	32.115225	6.625434
-633.200459	40.510623	6.635430
-631.385175	40.561578	6.645427
-629.578694	36.862599	6.655424
-627.405386	30.357828	6.665421
-625.647243	37.592195	6.675418
-624.021184	33.345765	6.685414
-621.954406	25.681778	6.695411
-619.971618	41.334988	6.705408
-618.369137	30.101192	6.715405
-616.535853	23.999676	6.725402
-614.469702	38.267554	6.735398
-612.373532	40.138272	6.745395
-610.646072	28.107724	6.755392
-608.770997	17.583507	6.765389
-606.941532	26.041148	6.775386
-605.312725	31.452097	6.785382
-603.242023	37.878707	6.795379
-601.160378	31.447018	6.805376
-599.197081	31.850119	6.815373
-597.735587	35.175304	6.825370
-595.959602	33.131118	6.835366
-593.700618	28.616247	6.845363
-592.030898	32.253942	6.855360
-589.999680	33.977169	6.865357
-588.020110	28.341747	6.875354
-586.215029	30.142149	6.885350
-584.449329	30.463149	6.895347
-582.713751	32.404122	6.905344
-580.649878	32.601711	6.915341
-578.579353	33.786598	6.925338
-577.195899	34.553899	6.935334
-575.212229	30.349846	6.945331
-572.926189	30.679313	6.955328
-571.323652	31.269527	6.965325
-569.513806	31.106674	6.975322
-567.560848	32.002474	6.985318
-565.848714	30.647413	6.995315
-563.614993	26.049769	7.005312
-561.790976	29.059720	7.015309
-559.954587	28.052688	7.025306
-558.378669	27.605123	7.035302
-556.286264	29.234927	7.045299
-554.163817	25.791835	7.055296
-552.505814	27.161046	7.065293
-550.720835	29.578859	7.075290
-548.798983	32.751605	7.085286
-547.100412	33.964351	7.095283
-545.026340	26.927640	7.105280
-543.223706	27.239614	7.115277
-541.451764	28.797465	7.125274
-539.464192	35.436346	7.135270
-537.401415	33.458495	7.145267
-535.561261	35.848562	7.155264
-533.636783	37.835187	7.165261
-531.633865	36.098992	7.175258
-530.112672	37.071676	7.185254
-528.382483	29.933593	7.195251
-526.132386	34.572786	7.205248
-524.327761	29.822668	7.215245
-522.333885	33.437063	7.225242
-520.570153	33.182145	7.235238
-518.747937	37.404976	7.245235
-517.112087	33.854901	7.255232
-515.156323	32.940936	7.265229
-513.263032	32.444293	7.275226
-511.242662	39.035335	7.285222
-509.418603	38.218193	7.295219
-507.338261	28.730136	7.305216
-505.616753	33.985838	7.315213
-504.012059	27.690394	7.325210
-501.729643	34.219068	7.335206
-499.682730	33.933151	7.345203
-498.006134	29.021930	7.355200
-496.375278	26.091576	7.365197
-494.601104	28.926394	7.375194
-492.547508	32.158670	7.385190
-490.299760	30.291837	7.395187
-488.935176	35.381935	7.405184
-486.851047	31.681350	7.415181
-484.739728	22.350988	7.425178
-483.137226	38.142425	7.435174
-481.241502	31.004778	7.445171
-479.266341	35.825283	7.455168
-477.290851	31.619456	7.465165
-475.885096	37.004547	7.475162
-473.903089	40.151964	7.485158
-471.780442	32.352861	7.495155
-469.995063	39.549852	7.505152
-467.939358	35.287014	7.515149
-466.075358	27.559218	7.525146
-464.432387	37.511941	7.535142
-462.606689	32.772710	7.545139
-460.613369	36.240416	7.555136
-458.723456	28.611112	7.565133
-456.940553	32.486607	7.575130
-454.941171	35.476537	7.585126
-452.875090	35.457583	7.595123
-451.223984	30.893072	7.605120
-449.363986	36.946128	7.615117
-446.973001	43.391216	7.625114
-445.622040	42.872283	7.635110
-443.963782	36.187815	7.645107
-441.796362	37.259463	7.655104
-439.567193	36.712404	7.665101
-438.245480	45.096549	7.675098
-436.546438	36.796724	7.685094
-434.326677	46.966835	7.695091
-432.143475	43.976745	7.705088
-430.454963	40.726192	7.715085
-428.639766	44.053432	7.725082
-427.147377	47.639046	7.735078
-424.888646	35.771653	7.745075
-423.101226	44.544053	7.755072
-420.973463	37.618855	7.765069
-419.280270	33.623925	7.775066
-417.493817	42.756460	7.785062
-415.514736	29.648545	7.795059
-413.713448	44.566783	7.805056
-412.132153	38.702994	7.815053
-410.064975	38.066570	7.825050
-408.034869	43.407284	7.835046
-406.112864	37.342268	7.845043
-404.194487	45.397502	7.855040
-402.417256	35.732139	7.865037
-400.562241	40.606632	7.875034
-398.596051	40.071600	7.885030
-396.802022	38.163614	7.895027
-394.883794	42.977498	7.905024
-393.125065	45.608034	7.915021
-391.009257	47.742643	7.925018
-389.297579	54.332565	7.935014
-387.359440	52.437891	7.945011
-385.572569	37.098181	7.955008
-383.898512	35.839320	7.965005
-381.819011	36.830328	7.975002
-379.797627	37.677468	7.984998
-378.006607	38.274035	7.994995
-376.081412	46.441884	8.004992
-374.251984	29.372866	8.014989
-372.522559	31.476021	8.024986
-370.799163	39.072966	8.034982
-368.526047	37.551120	8.044979
-366.501801	38.056783	8.054976
-364.670915	34.919327	8.064973
-362.956758	37.061241	8.074970
-361.341287	31.845674	8.084966
-359.412565	41.178164	8.094963
-357.509358	37.726028	8.104960
-355.390189	40.557983	8.114957
-353.538696	44.443139	8.124954
-351.917400	41.615449	8.134950
-350.166426	43.400991	8.144947
-347.854898	43.080855	8.154944
-345.905098	44.079970	8.164941
-344.229242	45.781198	8.174938
-342.419708	46.049594	8.184934
-340.457742	42.226532	8.194931
-338.629897	44.257165	8.204928
-336.824404	47.090268	8.214925
-334.776455	44.316053	8.224922
-332.864866	40.976274	8.234918
-331.358690	42.527766	8.244915
-329.181312	37.520923	8.254912
-327.476978	41.773779	8.264909
-325.445530	45.833905	8.274906
-323.736030	41.107002	8.284902
-321.819414	42.660874	8.294899
-319.880011	36.709979	8.304896
-317.880325	40.023646	8.314893
-315.774573	37.194434	8.324890
-314.712568	43.678125	8.334886
-312.080420	39.268139	8.344883
-310.404475	35.369185	8.354880
-308.583905	40.486081	8.364877
-306.500967	38.113650	8.374874
-304.785388	41.728451	8.384870
-303.327578	38.565330	8.394867
-301.255884	38.640341	8.404864
-299.401642	41.994607	8.414861
-297.173030	32.541459	8.424858
-295.526605	36.866735	8.434854
-293.597716	36.405633	8.444851
-291.687400	38.371036	8.454848
-289.897339	37.371602	8.464845
-287.757648	34.101234	8.474842
-286.096215	36.723698	8.484838
-284.246033	34.292126	8.494835
-282.313348	35.695052	8.504832
-280.373135	31.867617	8.514829
-278.409950	37.440166	8.524826
-276.826443	38.096771	8.534822
-274.885633	46.985333	8.544819
-273.054723	37.194648	8.554816
-270.940726	47.516012	8.564813
-269.139736	43.887635	8.574810
-267.469835	42.629517	8.584807
-265.345792	47.683806	8.594803
-263.715138	47.077706	8.604800
-261.643512	43.312988	8.614797
-259.684666	38.715270	8.624794
-258.083122	36.928100	8.634791
-256.216501	34.735490	8.644787
-254.031400	33.442523	8.654784
-252.227745	39.627890	8.664781
-250.217461	33.381542	8.674778
-248.490502	30.702836	8.684775
-246.680604	27.546713	8.694771
-244.824843	33.467993	8.704768
-243.015125	28.208869	8.714765
-241.140961	30.866883	8.724762
-239.216821	35.151037	8.734759
-237.129762	25.774213	8.744755
-235.487684	30.485466	8.754752
-233.554173	31.743045	8.764749
-231.527117	33.655131	8.774746
-229.891972	29.344347	8.784743
-228.036455	34.774657	8.794739
-226.244950	36.602767	8.804736
-224.037353	32.671129	8.814733
-222.284462	30.503010	8.824730
-220.511727	37.574336	8.834727
-218.607728	34.794771	8.844723
-216.510454	37.444042	8.854720
-214.774975	33.583017	8.864717
-212.782241	32.715498	8.874714
-211.103150	34.591557	8.884711
-209.259201	32.183139	8.894707
-207.433403	41.360096	8.904704
-205.384594	33.026704	8.914701
-203.475819	36.847579	8.924698
-201.777121	32.520354	8.934695
-199.834365	27.896833	8.944691
-197.964406	32.964885	8.954688
-196.152529	27.879122	8.964685
-194.406597	31.915451	8.974682
-192.130837	28.639241	8.984679
-190.460437	37.949948	8.994675
-188.535480	22.498336	9.004672
-186.415064	26.421232	9.014669
-184.622134	34.329314	9.024666
-182.975586	23.458180	9.034663
-181.130667	32.461586	9.044659
-178.954031	29.954319	9.054656
-177.283266	34.061073	9.064653
-175.414700	34.367540	9.074650
-173.622666	29.133389	9.084647
-171.660941	30.782809	9.094643
-169.738453	30.540709	9.104640
-168.079394	18.186625	9.114637
-166.156359	33.158278	9.124634
-163.851640	30.954252	9.134631
-162.280334	33.805909	9.144627
-160.271079	27.545587	9.154624
-158.631769	40.385285	9.164621
-156.468980	31.190636	9.174618
-154.972889	36.405214	9.184615
-153.048417	39.671028	9.194611
-150.859923	37.101895	9.204608
-148.938934	34.685966	9.214605
-147.147939	31.578716	9.224602
-145.505455	38.634573	9.234599
-143.383354	39.843190	9.244595
-141.587852	37.390449	9.254592
-140.117358	37.439949	9.264589
-137.945287	33.067238	9.274586
-136.096089	36.561378	9.284583
-134.128966	34.575442	9.294579
-132.348638	33.201909	9.304576
-129.860535	46.337243	9.314573
-128.331172	33.536519	9.324570
-127.076993	42.252145	9.334567
-125.119518	34.214421	9.344563
-122.914984	36.300380	9.354560
-120.639487	40.233333	9.364557
-118.988516	25.112825	9.374554
-117.205831	36.448714	9.384551
-115.265375	35.998539	9.394547
-113.560246	35.955362	9.404544
-111.912899	35.059348	9.414541
-109.727887	35.129076	9.424538
-108.034224	34.143576	9.434535
-105.926276	31.929945	9.444531
-104.052632	31.012044	9.454528
-102.083540	36.604330	9.464525
-100.199792	32.743411	9.474522
-98.475443	38.273698	9.484519
-96.737933	32.495697	9.494515
-94.768330	48.538365	9.504512
-92.594094	39.574027	9.514509
-91.014605	37.476290	9.524506
-89.201607	44.007650	9.534503
-87.397193	41.468267	9.544499
-85.350733	37.099849	9.554496
-83.278309	35.210834	9.564493
-81.771243	27.532349	9.574490
-79.699726	40.617357	9.584487
-77.656582	32.856511	9.594483
-75.884405	31.489055	9.604480
-74.045653	27.575338	9.614477
-72.045291	36.852449	9.624474
-70.391069	49.680377	9.634471
-68.791162	31.797137	9.644467
-66.756104	45.146911	9.654464
-64.483501	41.437132	9.664461
-62.534169	36.100597	9.674458
-60.843438	42.946730	9.684455
-59.327996	32.799164	9.694451
-57.555927	43.031603	9.704448
-55.229839	27.339250	9.714445
-53.201487	33.968906	9.724442
-51.603099	37.136827	9.734439
-49.616518	38.326095	9.744435
-47.623854	42.631060	9.754432
-45.946638	29.694696	9.764429
-44.077046	36.221798	9.774426
-42.213988	35.487201	9.784423
-40.174643	39.284228	9.794419
-38.568542	38.383790	9.804416
-36.770577	41.761453	9.814413
-34.305345	35.794787	9.824410
-32.772559	37.934297	9.834407
-31.237836	45.768441	9.844403
-29.255188	34.949558	9.854400
-27.069790	45.139780	9.864397
-25.060494	29.684283	9.874394
-23.359362	32.569007	9.884391
-21.692845	41.229981	9.894387
-19.643661	39.210522	9.904384
-17.904777	44.002808	9.914381
-16.189405	41.433470	9.924378
-13.982029	40.779758	9.934375
-12.020249	38.621096	9.944371
-10.226316	42.517289	9.954368
-8.440333	42.516550	9.964365
-6.542035	39.556484	9.974362
-4.634477	37.359111	9.984359
-3.645616	54.055639	9.994355
-2.305221	99.924041	10.004352
-1.037824	156.843699	10.014349
0.000000	204.812465	10.019354
0.816745	253.637366	10.024359
0.818814	288.198720	10.029363
1.569991	320.967621	10.034368
1.791690	344.429186	10.039373
2.318431	378.397745	10.044378
2.719380	405.292064	10.049383
2.784305	406.005459	10.054387
3.262966	417.061852	10.059392
3.198945	420.388205	10.064397
3.435851	468.697636	10.069402
3.417492	447.038855	10.074407
3.094616	464.413970	10.079411
3.453744	473.642938	10.084416
4.079553	450.831205	10.089421
4.130386	508.504028	10.094426
4.177289	498.462757	10.099431
3.994699	487.448887	10.104435
4.649521	489.436941	10.109440
4.363479	484.149488	10.114445
3.865303	477.369443	10.119450
4.035587	494.022569	10.124455
4.177882	484.327201	10.129459
4.631034	493.525417	10.134464
4.467353	512.792697	10.139469
4.432726	509.642823	10.144474
4.365543	506.707868	10.149479
4.407326	514.248165	10.154483
4.841225	514.557378	10.159488
4.658439	518.571297	10.164493
4.436638	514.170838	10.169498
4.816132	506.053939	10.174503
4.845786	530.743296	10.179507
4.960754	517.026457	10.184512
4.537556	526.785494	10.189517
4.586656	525.694299	10.194522
4.844449	537.449883	10.199527
4.590507	554.736844	10.204531
4.975664	544.179563	10.209536
4.939589	543.223373	10.214541
4.838360	541.534856	10.219546
5.008975	547.865646	10.224551
4.972756	529.938946	10.229555
5.245951	562.559134	10.234560
5.338089	531.865910	10.239565
5.386882	555.796926	10.244570
5.493262	556.319219	10.249575
5.342449	557.316179	10.254579
5.675116	556.309061	10.259584
5.385267	549.418487	10.264589
5.328066	562.053777	10.269594
5.539241	559.727251	10.274599
5.279641	564.712187	10.279603
5.200284	554.438711	10.284608
5.361077	570.741792	10.289613
5.728099	577.842333	10.294618
6.002353	568.345052	10.299623
5.686565	598.299688	10.304627
6.113858	573.016884	10.309632
6.051344	576.513338	10.314637
6.034190	599.683840	10.319642
6.169621	584.430927	10.324647
6.001709	581.866824	10.329651
6.484803	597.276468	10.334656
6.428758	584.831014	10.339661
6.409311	569.730547	10.344666
6.197456	564.989452	10.349671
5.765019	585.058180	10.354675
6.368298	574.298937	10.359680
6.275804	590.068446	10.364685
6.283497	601.375132	10.369690
6.765890	589.608596	10.374695
6.452630	597.312791	10.379699
6.314337	606.349951	10.384704
6.715046	599.249872	10.389709
6.799631	603.329978	10.394714
6.979840	607.407449	10.399719
6.337431	601.823562	10.404723
6.766981	602.593927	10.409728
6.972893	604.560558	10.414733
6.853526	618.073107	10.419738
6.789786	595.186626	10.424743
6.784401	615.258245	10.429747
7.195822	602.981064	10.434752
6.920961	622.488564	10.439757
7.216817	614.641979	10.444762
7.055581	604.416219	10.449767
7.092514	618.078875	10.454771
7.298059	613.236503	10.459776
7.238297	612.561620	10.464781
6.998602	610.710682	10.469786
7.241230	623.350243	10.474791
7.462665	615.305799	10.479795
7.128243	615.780130	10.484800
7.140878	625.739373	10.489805
7.398172	611.247563	10.494810
7.271034	616.887881	10.499815
7.128350	614.158904	10.504819
7.357752	618.599105	10.509824
7.396164	649.665841	10.514829
7.531484	656.683531	10.519834
7.706062	637.370091	10.524839
7.493731	680.004061	10.529843
7.832344	640.528914	10.534848
7.689696	678.263360	10.539853
7.810787	661.412091	10.544858
7.624058	659.114318	10.549863
7.644203	655.239761	10.554867
7.850301	666.749813	10.559872
8.095666	658.056574	10.564877
8.144193	671.342128	10.569882
8.232907	694.951625	10.574887
8.422367	693.609380	10.579891
8.368410	655.899866	10.584896
8.262368	679.915703	10.589901
8.250553	654.478870	10.594906
8.639178	687.796847	10.599911
8.422480	681.793382	10.604915
8.768772	665.065459	10.609920
8.432700	687.679857	10.614925
8.360133	670.799540	10.619930
8.424469	689.600193	10.624935
8.729562	687.408474	10.629939
8.973410	676.104103	10.634944
9.023930	688.826399	10.639949
8.710986	693.588080	10.644954
9.009365	690.520670	10.649959
8.930970	692.291390	10.654963
9.348061	678.799019	10.659968
8.935365	668.941314	10.664973
8.904512	672.349165	10.669978
8.987449	671.561637	10.674983
8.992673	684.155538	10.679987
9.086329	683.088764	10.684992
8.905989	690.754464	10.689997
8.752313	689.944749	10.695002
9.312503	690.468785	10.700007
9.198712	695.528279	10.705011
9.404995	703.078708	10.710016
9.334136	689.749303	10.715021
9.234811	693.764151	10.720026
9.525123	696.781749	10.725031
9.310713	692.220788	10.730035
9.528515	690.913446	10.735040
9.438386	694.501062	10.740045
9.496723	696.607934	10.745050
9.984519	698.774043	10.750055
9.753935	717.489308	10.755059
9.872275	714.630375	10.760064
9.638599	713.475459	10.765069
9.736685	730.253910	10.770074
10.280551	728.505063	10.775079
10.124234	730.464830	10.780083
10.438914	716.211339	10.785088
10.168621	716.508292	10.790093
10.049724	707.202930	10.795098
10.374696	685.949492	10.800103
10.119215	699.411287	10.805107
10.153122	695.558177	10.810112
10.230841	703.906529	10.815117
10.403698	719.130823	10.820122
10.394407	713.196764	10.825127
10.278396	732.671194	10.830131
10.726292	731.448574	10.835136
10.571915	743.974944	10.840141
10.705748	726.238493	10.845146
10.520287	708.507257	10.850151
10.555290	726.323913	10.855155
10.609856	732.916137	10.860160
10.461625	732.447742	10.865165
10.517461	738.344347	10.870170
10.992948	722.330595	10.875175
11.028281	733.506823	10.880179
10.850073	729.343767	10.885184
10.890902	732.193010	10.890189
10.585293	740.567826	10.895194
10.997755	734.098151	10.900199
10.651646	737.532642	10.905203
10.810691	734.392830	10.910208
10.940083	725.841046	10.915213
11.013712	725.652650	10.920218
11.459047	747.959596	10.925223
11.460191	759.368372	10.930227
11.457058	750.243212	10.935232
11.404551	742.258157	10.940237
11.396710	739.039307	10.945242
11.351923	740.229099	10.950247
11.542830	750.208879	10.955251
11.647774	755.370700	10.960256
12.006954	765.787267	10.965261
11.643629	747.415737	10.970266
11.816383	724.735755	10.975271
11.343753	739.369175	10.980275
11.905996	750.306843	10.985280
12.103264	756.788012	10.990285
11.769010	759.446351	10.995290
12.139138	753.275149	11.000295
11.817423	754.124340	11.005299
11.973136	757.264341	11.010304
12.436396	772.062338	11.015309
12.067943	756.547416	11.020314
12.274177	744.534646	11.025319
11.730168	753.125683	11.030323
12.153817	766.545459	11.035328
12.300282	771.419972	11.040333
12.143132	773.411415	11.045338
12.316403	769.594405	11.050343
12.344574	769.522067	11.055347
12.481248	765.901701	11.060352
12.506415	780.203463	11.065357
12.631104	775.096395	11.070362
12.531530	765.978721	11.075367
12.312277	769.974871	11.080371
12.377741	772.334501	11.085376
12.390269	771.406813	11.090381
12.331925	786.997628	11.095386
12.517623	766.808629	11.100391
12.527083	784.034931	11.105395
13.032389	797.752365	11.110400
13.061261	811.351837	11.115405
13.016067	797.196661	11.120410
13.549454	786.787449	11.125415
12.857725	807.995374	11.130419
13.249825	793.095537	11.135424
13.103878	773.199114	11.140429
12.752229	780.106876	11.145434
13.319566	789.474726	11.150439
13.252055	798.081255	11.155443
13.337988	805.037510	11.160448
13.457421	805.439462	11.165453
13.293497	804.185106	11.170458
13.417890	793.388541	11.175463
13.224092	809.157099	11.180467
13.414054	800.926764	11.185472
13.434680	798.780399	11.190477
13.422644	801.917202	11.195482
13.598108	798.464103	11.200487
13.447620	802.638526	11.205491
13.552167	799.808584	11.210496
13.906998	798.405263	11.215501
13.648334	809.313054	11.220506
13.882291	806.869317	11.225511
14.136730	828.647026	11.230515
14.213290	824.020693	11.235520
14.223937	798.928523	11.240525
13.795270	803.421696	11.245530
14.176917	788.402108	11.250535
14.246288	805.718227	11.255539
14.203903	803.268102	11.260544
14.264746	797.896824	11.265549
14.199418	816.700976	11.270554
14.374068	814.482735	11.275559
14.056234	827.861556	11.280563
14.161140	835.540185	11.285568
14.486315	837.323828	11.290573
14.417168	839.812169	11.295578
14.397861	833.092772	11.300583
14.582104	832.301695	11.305587
14.876246	830.762973	11.310592
14.832828	832.332592	11.315597
14.741678	842.374767	11.320602
14.868350	835.493318	11.325607
14.713647	836.229147	11.330611
14.779242	843.303779	11.335616
14.761511	831.739812	11.340621
14.734963	829.851697	11.345626
15.245163	838.623152	11.350631
14.878369	848.822832	11.355635
14.910911	844.585130	11.360640
14.642276	850.951415	11.365645
14.728749	834.988544	11.370650
15.054923	835.259755	11.375655
15.159181	868.480003	11.380659
15.515935	860.484805	11.385664
15.829296	848.248287	11.390669
15.658766	841.037349	11.395674
15.595701	842.904989	11.400679
15.435441	841.006658	11.405683
15.340786	824.432454	11.410688
15.377098	839.039997	11.415693
15.132832	845.318816	11.420698
15.748760	849.842521	11.425703
15.401741	864.459187	11.430707
15.988700	872.355841	11.435712
15.857763	869.005209	11.440717
15.783868	863.951857	11.445722
15.997392	864.231574	11.450727
15.844041	865.372459	11.455731
15.974881	869.369571	11.460736
15.841821	859.411943	11.465741
15.999452	867.020680	11.470746
16.452342	864.400094	11.475751
16.327560	862.773642	11.480755
16.278866	871.109136	11.485760
16.562411	861.074027	11.490765
16.319044	858.621254	11.495770
16.180023	858.922504	11.500775
15.953710	867.467670	11.505779
16.300167	855.430869	11.510784
16.235751	855.661874	11.515789
15.914181	869.782485	11.520794
16.244126	864.346187	11.525799
16.494133	876.883871	11.530803
16.278398	873.084721	11.535808
16.571465	865.812449	11.540813
16.475987	883.637493	11.545818
16.778212	877.226336	11.550823
16.897614	876.451905	11.555827
16.888183	890.376100	11.560832
17.042890	890.138502	11.565837
16.988810	868.568363	11.570842
17.089098	885.704607	11.575847
17.078672	881.489517	11.580851
17.144206	880.064519	11.585856
17.030874	870.912704	11.590861
16.936829	882.882377	11.595866
17.323776	884.403866	11.600871
17.185738	893.037469	11.605875
17.343671	894.051441	11.610880
17.543482	884.414442	11.615885
17.179396	900.325373	11.620890
17.648667	880.259721	11.625895
17.260882	895.239306	11.630899
17.378739	884.527293	11.635904
17.445114	881.828001	11.640909
17.335573	885.350952	11.645914
17.386972	894.290230	11.650919
17.408512	896.898157	11.655923
17.170654	891.006786	11.660928
17.544570	879.120126	11.665933
17.471267	892.814816	11.670938
17.630068	913.388936	11.675943
18.064644	922.563585	11.680947
18.342543	917.405224	11.685952
17.837900	895.782324	11.690957
17.821809	912.430966	11.695962
17.983804	907.291093	11.700967
18.187902	919.402479	11.705971
18.063907	916.580579	11.710976
18.534048	908.709194	11.715981
18.333703	923.335643	11.720986
18.657962	906.875881	11.725991
18.345221	891.648390	11.730995
18.320492	889.457205	11.736000
18.474996	877.250729	11.741005
18.360703	886.743123	11.746010
18.847862	873.963209	11.751015
18.482549	879.447652	11.756019
18.470091	888.135340	11.761024
18.964884	880.980697	11.766029
18.521030	881.445679	11.771034
18.722982	871.023035	11.776039
18.804334	889.837005	11.781043
18.581951	889.965472	11.786048
18.866220	899.716004	11.791053
18.684365	913.341295	11.796058
19.260886	902.693313	11.801063
18.779957	911.443113	11.806067
18.958238	913.554542	11.811072
19.278233	913.382045	11.816077
19.136858	922.158122	11.821082
19.417084	919.617103	11.826087
19.142168	918.295283	11.831091
19.273193	912.192110	11.836096
19.491487	908.937157	11.841101
19.163171	914.849369	11.846106
19.566037	909.451887	11.851111
19.135438	926.668117	11.856115
18.993499	912.968223	11.861120
19.476721	912.296614	11.866125
19.469817	918.707917	11.871130
19.361834	908.815642	11.876135
19.619321	912.486642	11.881139
19.484749	907.269489	11.886144
19.534729	913.449371	11.891149
19.090199	922.303758	11.896154
19.493527	934.626232	11.901159
19.583773	938.737069	11.906163
19.362731	955.249714	11.911168
19.829776	934.884724	11.916173
19.747019	946.939382	11.921178
19.826614	938.947342	11.926183
20.045138	940.256004	11.931187
20.024298	934.629622	11.936192
19.931307	940.088003	11.941197
19.901678	967.424201	11.946202
20.519073	955.023989	11.951207
20.482978	966.371059	11.956211
20.891229	965.101129	11.961216
20.569705	927.561309	11.966221
20.437493	949.465520	11.971226
20.877965	922.707145	11.976231
20.629764	938.615406	11.981235
20.688403	931.676953	11.986240
20.638213	917.717996	11.991245
20.613227	933.108109	11.996250
20.834915	934.537690	12.001255
20.772316	929.556629	12.006259
20.683109	928.052228	12.011264
20.695812	920.718988	12.016269
20.519038	938.921337	12.021274
20.948562	925.067214	12.026279
20.843222	927.130839	12.031283
20.727836	921.085884	12.036288
20.945079	934.161848	12.041293
20.662096	921.727066	12.046298
20.954988	931.927249	12.051303
21.041784	920.392271	12.056307
20.936353	929.962127	12.061312
21.280870	925.796070	12.066317
20.785175	924.980964	12.071322
20.933496	924.600883	12.076327
20.643384	927.879833	12.081331
20.717528	935.514536	12.086336
20.972960	930.022290	12.091341
20.525894	923.065146	12.096346
20.654740	928.861876	12.101351
20.752831	939.507866	12.106355
20.712388	932.883256	12.111360
21.169125	923.232063	12.116365
20.927602	921.654185	12.121370
21.363122	928.187320	12.126375
21.182481	937.512134	12.131379
21.324171	932.444877	12.136384
21.180497	928.738296	12.141389
21.031952	944.690594	12.146394
21.227451	924.403618	12.151399
21.064381	916.929680	12.156403
20.719288	910.188089	12.161408
20.687615	901.326002	12.166413
20.707073	909.546571	12.171418
20.620700	908.659878	12.176423
20.776092	917.213583	12.181427
21.227912	932.204381	12.186432
21.031165	914.357997	12.191437
20.715221	916.253361	12.196442
20.892282	901.799288	12.201447
21.164555	908.858337	12.206451
20.605170	911.219874	12.211456
20.957349	915.090237	12.216461
20.936624	915.429391	12.221466
21.114720	910.458835	12.226471
20.895671	915.352268	12.231475
20.800546	908.078808	12.236480
21.112687	912.444405	12.241485
20.812092	908.275584	12.246490
20.824430	919.914512	12.251495
20.989269	914.156024	12.256499
21.146712	920.831275	12.261504
20.954487	903.501418	12.266509
20.909179	920.211498	12.271514
20.847366	911.582867	12.276519
20.935233	929.124840	12.281523
21.034653	920.565106	12.286528
21.032182	920.261113	12.291533
20.638852	922.752286	12.296538
20.933775	911.456932	12.301543
20.826804	920.904027	12.306547
20.756192	919.467623	12.311552
20.976565	925.345948	12.316557
20.741760	912.362601	12.321562
20.819744	903.126636	12.326567
20.917351	919.418113	12.331571
20.841389	929.771736	12.336576
21.338394	909.455620	12.341581
21.077929	907.106489	12.346586
20.752558	913.461349	12.351591
21.180790	922.439893	12.356595
20.830875	904.584833	12.361600
20.884325	879.720659	12.366605
20.944855	889.563637	12.371610
21.201510	885.903607	12.376615
20.854162	894.857595	12.381619
20.949827	884.620624	12.386624
20.994700	876.437040	12.391629
21.057571	885.188405	12.396634
21.142683	881.117348	12.401639
20.837702	877.452276	12.406643
20.863219	893.684259	12.411648
20.941284	900.288582	12.416653
20.846878	885.786357	12.421658
21.091177	876.288923	12.426663
20.734723	886.761365	12.431667
20.870811	891.408919	12.436672
21.176117	886.484315	12.441677
21.090628	889.169234	12.446682
21.020589	889.320712	12.451687
21.098290	884.199022	12.456691
20.494180	872.053614	12.461696
21.196587	875.749840	12.466701
20.898194	873.154455	12.471706
20.876324	871.543128	12.476711
20.458619	871.674361	12.481715
20.404588	886.865633	12.486720
20.676538	884.589287	12.491725
20.697983	888.570736	12.496730
20.709553	890.322401	12.501735
20.785219	893.194505	12.506739
20.898208	889.863311	12.511744
20.768379	890.965754	12.516749
20.558424	900.501798	12.521754
21.077795	895.412166	12.526759
20.975501	886.722197	12.531763
20.765522	891.380789	12.536768
20.760326	892.748780	12.541773
20.934226	897.820809	12.546778
20.823034	898.928165	12.551783
20.775392	899.527075	12.556787
20.859222	893.713707	12.561792
20.658693	886.510684	12.566797
20.723363	901.132691	12.571802
20.798590	902.215047	12.576807
20.696306	899.648304	12.581811
20.569635	905.790124	12.586816
20.816392	887.655425	12.591821
20.811174	903.792974	12.596826
21.260270	898.351854	12.601831
21.171528	901.053063	12.606835
20.869064	897.259853	12.611840
20.885487	897.798083	12.616845
20.785672	897.631039	12.621850
20.886831	883.980710	12.626855
21.047205	891.126981	12.631859
20.816587	891.445994	12.636864
21.373603	882.124184	12.641869
21.208410	888.917105	12.646874
21.425669	895.830383	12.651879
20.931665	886.311919	12.656883
20.742560	870.396112	12.661888
21.031925	861.380349	12.666893
20.744265	865.855782	12.671898
20.830367	862.738615	12.676903
20.674669	869.883246	12.681907
20.618281	871.454938	12.686912
20.807063	869.939324	12.691917
20.678277	884.197934	12.696922
21.079839	888.151876	12.701927
21.298537	884.288168	12.706931
21.188168	874.325334	12.711936
20.976335	864.601036	12.716941
20.808905	880.925277	12.721946
20.746768	870.331865	12.726951
20.835577	866.797955	12.731955
20.810115	866.945478	12.736960
20.838452	873.992953	12.741965
20.720421	870.726992	12.746970
20.999521	869.897131	12.751975
21.330445	878.958975	12.756979
20.983517	876.224675	12.761984
21.359799	865.681193	12.766989
21.219161	883.160207	12.771994
21.061418	867.614711	12.776999
21.349555	866.602062	12.782003
20.622564	860.129555	12.787008
20.960160	844.345816	12.792013
20.735295	853.139897	12.797018
20.614259	853.200163	12.802023
20.908575	858.785975	12.807027
20.812042	872.064888	12.812032
20.877523	868.266620	12.817037
20.476551	877.426265	12.822042
20.411379	878.799089	12.827047
20.611796	876.846385	12.832051
20.668798	879.756156	12.837056
20.732542	863.853646	12.842061
20.804408	872.483723	12.847066
21.076769	883.093994	12.852071
20.815064	877.712626	12.857075
21.003446	873.120483	12.862080
21.261246	876.321500	12.867085
20.903258	876.837441	12.872090
21.080594	882.842460	12.877095
21.145396	878.845604	12.882099
20.873470	875.443339	12.887104
20.705155	875.916416	12.892109
20.916696	886.580543	12.897114
20.817755	874.037603	12.902119
20.685634	889.665527	12.907123
20.792391	887.180563	12.912128
20.985226	869.701028	12.917133
20.819369	882.413850	12.922138
20.658852	880.895595	12.927143
20.941048	883.969722	12.932147
20.898405	876.995409	12.937152
21.047409	882.949754	12.942157
21.028338	880.781322	12.947162
20.843883	865.186474	12.952167
20.733718	869.649370	12.957171
20.607210	879.228862	12.962176
20.958845	875.328186	12.967181
20.717221	888.639715	12.972186
20.761702	890.873403	12.977191
20.800780	881.645235	12.982195
20.907610	869.225598	12.987200
20.602408	900.279867	12.992205
20.937856	893.890213	12.997210
20.967184	884.699867	13.002215
20.914947	873.843103	13.007219
21.020046	894.745880	13.012224
21.191060	891.910050	13.017229
20.866509	878.602006	13.022234
20.815990	887.245302	13.027239
20.942897	856.686190	13.032243
20.385022	864.128344	13.037248
20.773390	865.968144	13.042253
20.861318	880.961731	13.047258
21.020076	878.276090	13.052263
20.762133	894.209510	13.057267
20.742688	901.204695	13.062272
21.071987	889.397680	13.067277
20.827435	889.953878	13.072282
20.929241	891.287457	13.077287
21.193959	882.778653	13.082291
20.634685	864.096028	13.087296
20.562653	863.583937	13.092301
20.908866	877.721055	13.097306
21.021313	875.211533	13.102311
21.013120	866.385145	13.107315
20.646078	864.656982	13.112320
21.107883	854.694371	13.117325
20.677139	856.160188	13.122330
20.593454	858.568851	13.127335
20.916574	868.403052	13.132339
20.856119	882.275453	13.137344
21.164008	878.348638	13.142349
20.983674	867.561193	13.147354
20.808228	862.875693	13.152359
20.445091	857.688702	13.157363
20.391328	883.525779	13.162368
21.119422	882.684233	13.167373
20.985623	891.028581	13.172378
21.009554	888.787059	13.177383
20.750904	881.233767	13.182387
20.687487	888.543460	13.187392
21.037745	885.502429	13.192397
20.602489	886.437542	13.197402
20.788394	894.193170	13.202407
21.215043	887.151893	13.207411
20.709676	883.799472	13.212416
20.707711	893.780151	13.217421
20.818757	887.252826	13.222426
20.740927	902.892605	13.227431
21.090940	891.627905	13.232435
20.785866	902.839630	13.237440
21.017779	890.005794	13.242445
20.755966	887.243725	13.247450
20.697300	895.951403	13.252455
20.929635	897.212126	13.257459
20.651931	909.933348	13.262464
20.729040	894.656294	13.267469
21.051371	893.406380	13.272474
21.012765	891.365640	13.277479
21.186063	893.665516	13.282483
20.754183	882.117097	13.287488
20.992174	866.213603	13.292493
20.564064	863.689369	13.297498
20.918786	867.390582	13.302503
20.831861	874.708748	13.307507
20.775021	884.332324	13.312512
21.037145	867.474091	13.317517
21.019282	894.174350	13.322522
20.874010	859.733654	13.327527
20.852392	868.791793	13.332531
20.577477	867.463670	13.337536
20.614074	870.591155	13.342541
20.740976	884.246023	13.347546
21.160001	891.210698	13.352551
21.405533	882.302835	13.357555
20.912569	871.207284	13.362560
20.897182	864.685940	13.367565
20.916359	868.420167	13.372570
20.874151	857.101353	13.377575
21.054892	865.315099	13.382579
20.712835	878.532251	13.387584
21.141049	850.700497	13.392589
21.036344	868.993765	13.397594
20.884455	869.137797	13.402599
21.163448	866.015097	13.407603
20.527623	873.679420	13.412608
20.762267	855.477307	13.417613
20.720996	867.299782	13.422618
20.592110	870.657083	13.427623
21.018287	865.558669	13.432627
20.612695	862.068917	13.437632
20.937063	871.240610	13.442637
20.917582	868.465127	13.447642
21.047194	869.418961	13.452647
21.216679	868.899890	13.457651
20.620212	869.732982	13.462656
20.808115	864.637877	13.467661
20.687733	871.073566	13.472666
20.655892	877.203404	13.477671
20.780283	865.190972	13.482675
20.910525	870.101222	13.487680
20.904390	866.752763	13.492685
20.939311	868.735664	13.497690
20.774321	867.855204	13.502695
21.022548	863.456944	13.507699
20.473171	867.846386	13.512704
20.771112	864.255470	13.517709
20.790603	863.829706	13.522714
20.945533	866.944626	13.527719
20.960532	864.729763	13.532723
20.787662	863.508366	13.537728
21.041231	863.296003	13.542733
20.612008	877.192519	13.547738
20.838018	872.073989	13.552743
21.044836	860.423724	13.557747
20.798361	872.490238	13.562752
21.000989	867.187783	13.567757
20.637067	879.151610	13.572762
20.783321	868.397234	13.577767
21.192469	869.453141	13.582771
20.709545	872.617750	13.587776
21.041757	871.132877	13.592781
20.697177	875.893354	13.597786
20.535494	872.457739	13.602791
20.788497	869.418029	13.607795
20.638065	869.810984	13.612800
20.877422	872.712170	13.617805
20.918973	880.612236	13.622810
20.810830	878.328703	13.627815
21.153779	876.537768	13.632819
20.863061	874.594008	13.637824
20.985884	866.186689	13.642829
20.678083	866.795550	13.647834
20.907863	881.750746	13.652839
21.311315	868.107413	13.657843
21.216938	879.347018	13.662848
21.472295	878.883637	13.667853
21.106912	877.095285	13.672858
21.070226	861.093680	13.677863
20.951814	846.125398	13.682867
20.674031	861.421714	13.687872
20.978813	842.555583	13.692877
20.954179	840.220890	13.697882
20.414714	851.695459	13.702887
20.833785	854.905443	13.707891
20.933982	863.589342	13.712896
20.801638	853.767220	13.717901
21.079471	845.033998	13.722906
20.746748	861.299424	13.727911
20.844202	850.806729	13.732915
20.645744	853.973275	13.737920
20.975453	840.316498	13.742925
20.597255	853.036352	13.747930
20.674501	869.477674	13.752935
20.987608	866.240724	13.757939
20.847410	880.597344	13.762944
21.192377	876.978425	13.767949
20.769717	857.599094	13.772954
20.774590	853.534533	13.777959
21.010705	847.841975	13.782963
20.654319	852.071325	13.787968
20.775514	858.408558	13.792973
20.717037	869.286044	13.797978
20.429901	884.017756	13.802983
20.981748	880.069379	13.807987
20.699969	883.000064	13.812992
20.803845	876.286233	13.817997
21.051903	886.879882	13.823002
20.764864	889.185365	13.828007
21.155290	885.453540	13.833011
20.612287	887.550689	13.838016
21.107207	891.267396	13.843021
21.081658	874.355687	13.848026
20.749229	876.668407	13.853031
21.151453	863.656046	13.858035
20.749164	868.670149	13.863040
20.928799	853.999674	13.868045
20.670276	857.306685	13.873050
20.758289	851.295551	13.878055
21.328881	863.152902	13.883059
20.686617	864.608300	13.888064
20.712926	848.940432	13.893069
20.861836	856.263554	13.898074
20.497508	856.564467	13.903079
20.708452	865.676976	13.908083
20.699558	892.295377	13.913088
21.021813	885.021595	13.918093
20.943595	888.968477	13.923098
20.941449	896.768290	13.928103
20.891385	871.565828	13.933107
20.991163	894.391731	13.938112
21.097852	879.731286	13.943117
21.122583	871.366417	13.948122
20.703362	857.827488	13.953127
20.962827	848.682462	13.958131
20.943985	838.799671	13.963136
20.859567	844.773880	13.968141
20.973733	853.166968	13.973146
20.712602	859.196174	13.978151
21.154178	849.184754	13.983155
20.617123	850.867796	13.988160
20.731735	856.127458	13.993165
21.110944	860.796152	13.998170
20.734412	856.254685	14.003175
21.091134	850.787314	14.008179
20.583660	859.224354	14.013184
20.757005	850.400563	14.018189
20.811753	861.945563	14.023207
20.766120	860.905247	14.028224
21.235302	853.928470	14.033242
20.813935	857.542535	14.038259
20.729874	843.687597	14.043277
20.777747	860.198576	14.048295
20.932440	853.265664	14.053312
20.719319	863.484182	14.058330
21.087680	863.510333	14.063347
21.045452	851.188592	14.068365
21.241859	849.642522	14.073383
20.910393	866.470390	14.078400
20.980729	850.171691	14.083418
20.647219	871.322236	14.088435
21.109577	864.884476	14.093453
21.316394	884.311471	14.098471
21.257099	880.700053	14.103488
21.564497	871.438467	14.108506
20.739964	869.825573	14.113523
21.264979	873.788895	14.118541
21.172539	873.853932	14.123559
21.160387	884.551609	14.128576
21.385997	882.853025	14.133594
21.335115	888.540876	14.138611
20.900063	879.820806	14.143629
21.376399	874.252204	14.148647
21.148438	893.479584	14.153664
21.466637	894.798803	14.158682
21.237592	899.745919	14.163699
21.611533	893.770527	14.168717
21.661645	890.967436	14.173735
21.356041	893.104961	14.178752
21.576425	887.076989	14.183770
21.283915	881.624711	14.188787
21.444725	885.020103	14.193805
21.678555	895.363976	14.198823
21.578942	896.499736	14.203840
21.302483	878.974391	14.208858
21.159244	886.194827	14.213875
21.254447	897.133349	14.218893
21.420401	893.961024	14.223911
20.980625	905.870421	14.228928
21.290274	893.196818	14.233946
21.311253	890.439268	14.238963
21.422982	893.487012	14.243981
21.613547	904.468529	14.248999
21.483465	917.473623	14.254016
21.723175	915.233278	14.259034
21.400560	927.223101	14.264051
21.772399	934.232436	14.269069
21.682640	921.661830	14.274087
21.595221	936.165415	14.279104
21.984592	930.085308	14.284122
21.865711	928.569066	14.289139
21.673892	943.252891	14.294157
22.075901	935.171592	14.299175
22.135436	927.890476	14.304192
21.991541	927.528023	14.309210
21.851429	931.232521	14.314227
21.833867	930.530618	14.319245
21.801802	930.980828	14.324263
21.617568	936.620757	14.329280
21.928443	933.115446	14.334298
21.805614	931.456698	14.339315
21.855671	928.736972	14.344333
22.040854	938.074105	14.349351
21.852737	927.551386	14.354368
22.090544	925.747040	14.359386
22.096869	929.270892	14.364403
21.892447	926.305482	14.369421
22.155565	922.894300	14.374439
22.399780	930.979412	14.379456
22.269368	938.358266	14.384474
22.398562	922.293901	14.389491
22.030447	928.505808	14.394509
22.141068	919.760031	14.399527
22.064487	934.991719	14.404544
22.164998	932.990633	14.409562
22.148510	930.660592	14.414579
22.036618	930.802659	14.419597
22.213172	922.593739	14.424615
21.848526	932.123942	14.429632
22.065012	934.451894	14.434650
22.627916	941.032814	14.439667
22.772926	951.222591	14.444685
22.269185	932.659126	14.449703
22.158562	943.127176	14.454720
22.532223	952.278540	14.459738
22.505981	964.726033	14.464755
22.682925	954.703460	14.469773
22.699046	950.733955	14.474791
22.334438	946.732369	14.479808
22.663555	946.211113	14.484826
22.820877	953.669919	14.489843
22.366009	939.444621	14.494861
22.541106	944.468861	14.499879
22.622459	948.222981	14.504896
22.491600	957.505144	14.509914
22.415458	957.372541	14.514931
22.474718	949.282980	14.519949
23.015663	948.716930	14.524967
22.620419	949.486166	14.529984
22.647737	948.149511	14.535002
22.667124	951.480962	14.540019
22.600562	947.854957	14.545037
22.719651	952.002581	14.550055
22.829393	964.186158	14.555072
22.926892	953.276546	14.560090
22.908113	955.642023	14.565107
22.930825	961.285135	14.570125
22.859642	942.613349	14.575143
22.520393	957.754826	14.580160
22.867702	954.168200	14.585178
22.901287	949.459785	14.590195
22.675758	961.324048	14.595213
22.856847	957.270034	14.600231
22.780915	955.592793	14.605248
22.943661	948.710457	14.610266
22.842729	954.291493	14.615283
22.849941	971.170855	14.620301
23.239414	968.615627	14.625319
22.888956	982.366885	14.630336
23.169011	991.267379	14.635354
23.360505	989.821173	14.640371
23.280049	990.099789	14.645389
23.290872	973.335421	14.650407
23.292738	975.041701	14.655424
23.278639	966.642955	14.660442
23.628627	956.548740	14.665459
23.201084	958.485513	14.670477
23.776563	948.470165	14.675495
23.563379	942.852640	14.680512
23.399170	953.668993	14.685530
23.547218	945.785482	14.690547
23.075491	954.651704	14.695565
23.500283	946.352849	14.700583
23.069478	954.457545	14.705600
23.644950	954.249333	14.710618
23.934486	953.687202	14.715635
23.501788	958.533119	14.720653
23.790079	948.832542	14.725671
23.316008	961.247640	14.730688
23.167664	959.051874	14.735706
23.464865	946.874106	14.740723
23.577626	955.710029	14.745741
23.595071	955.858209	14.750759
23.281907	957.196333	14.755776
23.613849	957.297502	14.760794
23.394436	957.444133	14.765811
23.133646	965.166241	14.770829
23.532307	968.289355	14.775847
23.810389	985.079920	14.780864
23.591726	984.090783	14.785882
23.949914	978.721871	14.790899
23.789792	975.996333	14.795917
23.819467	975.988417	14.800935
24.009975	984.610625	14.805952
24.036173	980.071681	14.810970
24.244400	967.972575	14.815987
23.852790	963.231300	14.821005
24.051902	947.794360	14.826023
23.913611	951.187136	14.831040
23.550983	952.753357	14.836058
24.035323	958.344867	14.841075
23.865729	977.319246	14.846093
23.986543	976.404949	14.851111
24.090859	978.439361	14.856128
24.130824	971.414585	14.861146
24.486354	972.524951	14.866163
23.658907	953.251792	14.871181
23.844716	967.770032	14.876199
24.228592	977.374357	14.881216
24.060659	985.257834	14.886234
24.098921	978.363879	14.891251
24.204515	967.438809	14.896269
24.338618	980.684953	14.901287
24.301986	979.479609	14.906304
24.249986	975.837118	14.911322
24.662314	977.855439	14.916339
24.497282	980.118411	14.921357
24.270645	956.911506	14.926375
24.328307	945.121128	14.931392
24.194985	948.332226	14.936410
24.590911	951.929220	14.941427
24.275999	960.811332	14.946445
24.188630	970.338235	14.951463
24.052917	979.622759	14.956480
24.233563	977.467324	14.961498
24.486431	965.098423	14.966515
24.081810	980.069464	14.971533
24.320263	979.740406	14.976551
24.314927	980.110854	14.981568
24.297549	980.354244	14.986586
24.189477	974.704214	14.991603
24.456266	987.787641	14.996621
24.620479	998.282680	15.001639
24.723685	1003.224031	15.006656
24.676718	1010.328508	15.011674
25.191760	1000.030201	15.016691
24.764677	997.586319	15.021709
24.782930	985.487610	15.026727
24.812230	970.124916	15.031744
24.704756	979.493020	15.036762
24.821865	970.719438	15.041779
24.587519	980.014974	15.046797
24.709448	987.210474	15.051815
24.880390	998.533369	15.056832
24.950016	1005.361291	15.061850
25.222899	994.513334	15.066867
24.896210	1000.415091	15.071885
24.867098	1003.738560	15.076903
25.362974	993.083115	15.081920
24.683080	984.183393	15.086938
24.983821	986.244677	15.091955
25.136918	997.660075	15.096973
25.188434	1002.529450	15.101991
25.118855	992.450218	15.107008
24.851720	987.733125	15.112026
25.380446	988.548475	15.117043
25.126397	1000.749205	15.122061
24.864043	999.812650	15.127079
25.132222	997.317657	15.132096
25.285214	999.092641	15.137114
25.491653	992.156129	15.142131
25.322551	1005.483683	15.147149
25.297167	999.483850	15.152167
25.261695	1003.870056	15.157184
25.262832	1009.129688	15.162202
25.427229	992.402149	15.167219
25.375826	1003.776238	15.172237
25.311787	1000.001963	15.177255
25.523564	994.775937	15.182272
25.425810	1002.888888	15.187290
25.508071	996.695722	15.192307
25.484505	1008.763752	15.197325
25.621673	998.996013	15.202343
25.818956	988.784568	15.207360
25.037346	995.586230	15.212378
25.295823	1004.117392	15.217395
25.311090	1006.342176	15.222413
25.419702	1009.218993	15.227431
25.424728	992.664726	15.232448
25.409631	990.675777	15.237466
25.466999	998.927571	15.242483
25.256707	999.948865	15.247501
25.414046	998.813251	15.252519
26.147488	1011.595777	15.257536
25.727444	1014.405905	15.262554
25.645819	999.304674	15.267571
25.741769	1005.442603	15.272589
25.870093	1026.224010	15.277607
25.932200	1030.970591	15.282624
25.890507	1037.432487	15.287642
26.026505	1022.087326	15.292659
25.984343	1030.485563	15.297677
26.064807	1031.916637	15.302695
25.978941	1036.713559	15.307712
25.753783	1030.860397	15.312730
26.019390	1034.715707	15.317747
25.932388	1028.986795	15.322765
25.802091	1031.286704	15.327783
25.873219	1026.040629	15.332800
25.855717	1025.245909	15.337818
26.206390	1025.149049	15.342835
26.243078	1025.539536	15.347853
26.171074	1025.258417	15.352871
26.011442	1029.135929	15.357888
25.695876	1040.226580	15.362906
25.752539	1034.849110	15.367923
26.002055	1034.911518	15.372941
26.087275	1057.308947	15.377959
26.459557	1061.218034	15.382976
26.613000	1064.762498	15.387994
26.579432	1055.239015	15.393011
26.613407	1045.042564	15.398029
26.543775	1026.467944	15.403047
26.761619	1021.851235	15.408064
26.830217	1029.012791	15.413082
26.677026	1028.028939	15.418099
26.992763	1022.075362	15.423117
26.828217	1013.798102	15.428135
26.801584	1015.814080	15.433152
26.644243	1014.994474	15.438170
26.737558	1017.777784	15.443187
26.880299	1026.514595	15.448205
26.572381	1021.116628	15.453223
26.515155	1022.940870	15.458240
26.484494	1026.160778	15.463258
26.743616	1025.144202	15.468275
26.678275	1024.566310	15.473293
26.637742	1028.045753	15.478311
26.745608	1024.704923	15.483328
26.520023	1026.845434	15.488346
26.591486	1023.541868	15.493363
26.449722	1027.292268	15.498381
26.443680	1028.732420	15.503399
26.713357	1020.297822	15.508416
26.662436	1021.142700	15.513434
26.968110	1040.234835	15.518451
27.351617	1040.614054	15.523469
26.658858	1040.166109	15.528487
26.908059	1048.058595	15.533504
27.143242	1051.467332	15.538522
26.861717	1051.398941	15.543539
27.062372	1056.903606	15.548557
26.861784	1065.264213	15.553575
27.102020	1051.218938	15.558592
27.096679	1061.396594	15.563610
27.272726	1056.415329	15.568627
27.795482	1057.717670	15.573645
27.443015	1049.995717	15.578663
27.636960	1054.645780	15.583680
27.232315	1047.589634	15.588698
27.160728	1038.100537	15.593715
27.322358	1042.716427	15.598733
27.454661	1058.695103	15.603751
27.795639	1056.146021	15.608768
26.951576	1053.441460	15.613786
26.878179	1047.921143	15.618803
27.368317	1061.895471	15.623821
27.180963	1064.902866	15.628839
27.414358	1068.572999	15.633856
27.406978	1063.465264	15.638874
27.310581	1063.395661	15.643891
27.513337	1070.617635	15.648909
27.389914	1066.174880	15.653927
27.838812	1054.446281	15.658944
27.834725	1050.473680	15.663962
27.699324	1056.830987	15.668979
27.628422	1051.203311	15.673997
27.703856	1056.581665	15.679015
27.729668	1058.752869	15.684032
27.699986	1055.589688	15.689050
27.510963	1061.125042	15.694067
27.725590	1058.935864	15.699085
27.516918	1069.745238	15.704103
27.819739	1067.439752	15.709120
27.899641	1083.198738	15.714138
27.694950	1091.649670	15.719155
27.913242	1083.907456	15.724173
27.858310	1083.480476	15.729191
27.991854	1093.904976	15.734208
27.866690	1088.425931	15.739226
28.040433	1086.938504	15.744243
28.153346	1075.952414	15.749261
27.861895	1077.445952	15.754279
28.236284	1084.294516	15.759296
28.168957	1087.949695	15.764314
28.160778	1088.951345	15.769331
28.337369	1080.699862	15.774349
28.016027	1088.286983	15.779367
28.192909	1080.818773	15.784384
28.314046	1083.094321	15.789402
28.239539	1093.953098	15.794419
28.040313	1087.998255	15.799437
28.168158	1092.360015	15.804455
28.687990	1085.848503	15.809472
28.308787	1090.459430	15.814490
27.975215	1088.404862	15.819507
28.327347	1081.205986	15.824525
28.113631	1081.282500	15.829543
28.090781	1080.016751	15.834560
28.367231	1101.746714	15.839578
28.552043	1111.661286	15.844595
28.730791	1113.616210	15.849613
28.729473	1118.921889	15.854631
29.044930	1101.150872	15.859648
29.127681	1094.219880	15.864666
28.748413	1084.229297	15.869683
29.078109	1073.056062	15.874701
29.105109	1073.427648	15.879719
28.974392	1072.685586	15.884736
28.892461	1067.844554	15.889754
28.761185	1069.174128	15.894771
29.031725	1077.813515	15.899789
28.773626	1075.315930	15.904807
28.730680	1080.000634	15.909824
28.980444	1063.772174	15.914842
28.690613	1075.058509	15.919859
28.994365	1082.371341	15.924877
28.960478	1080.679515	15.929895
28.975644	1075.708172	15.934912
28.759821	1077.751185	15.939930
28.691479	1082.941705	15.944947
28.965426	1076.618840	15.949965
28.579874	1077.375524	15.954983
28.881811	1089.887184	15.960000
29.065062	1103.393001	15.965018
28.943545	1108.310456	15.970035
29.105612	1111.041923	15.975053
29.303162	1118.807414	15.980071
29.462737	1106.942453	15.985088
29.582542	1114.913811	15.990106
29.171338	1109.211403	15.995123
29.631435	1097.671308	16.000141
29.211773	1110.909938	16.005159
29.433311	1101.927725	16.010176
29.713277	1106.085914	16.015194
29.547246	1117.203110	16.020211
29.642102	1105.405097	16.025229
29.525911	1090.002562	16.030247
29.378975	1108.934177	16.035264
29.381535	1099.790271	16.040282
29.144440	1110.789815	16.045299
29.483134	1106.808147	16.050317
29.643117	1111.473082	16.055335
29.732745	1108.822513	16.060352
29.982914	1111.582399	16.065370
29.953720	1117.477654	16.070387
29.865696	1114.517235	16.075405
30.147260	1110.130996	16.080423
29.811062	1107.147240	16.085440
29.823895	1084.888167	16.090458
29.824126	1090.297401	16.095475
30.101102	1083.063323	16.100493
29.544584	1095.424048	16.105511
29.320771	1100.996425	16.110528
29.789490	1104.567693	16.115546
29.827762	1116.032956	16.120563
29.975549	1114.680219	16.125581
30.128725	1118.636849	16.130599
30.241166	1114.493071	16.135616
30.408493	1109.256791	16.140634
30.102613	1111.781332	16.145651
30.282924	1107.697515	16.150669
30.363755	1112.250811	16.155687
30.337176	1119.083119	16.160704
30.402411	1106.844689	16.165722
30.226716	1114.229281	16.170739
30.461332	1108.708579	16.175757
30.081662	1107.894539	16.180775
29.952960	1117.571267	16.185792
30.089974	1105.593508	16.190810
29.926129	1113.397756	16.195827
30.036540	1108.655016	16.200845
29.989460	1118.376926	16.205863
29.869196	1118.945021	16.210880
30.555688	1125.732821	16.215898
30.323910	1149.495921	16.220915
30.018086	1140.912375	16.225933
30.250138	1150.298797	16.230951
30.361177	1140.931510	16.235968
30.646774	1137.785666	16.240986
30.533418	1142.583861	16.246003
30.742902	1140.845350	16.251021
31.164493	1141.108393	16.256039
30.983124	1144.838401	16.261056
31.106172	1139.324470	16.266074
31.011358	1147.875882	16.271091
30.854081	1150.625254	16.276109
31.006580	1138.460965	16.281127
30.803395	1140.948685	16.286144
31.058294	1142.669685	16.291162
30.924417	1155.285510	16.296179
31.092390	1141.723554	16.301197
31.085316	1142.276744	16.306215
30.812986	1150.312232	16.311232
31.314562	1137.179970	16.316250
31.201358	1138.072538	16.321267
30.842444	1131.529698	16.326285
31.169960	1133.467192	16.331303
31.036949	1144.772614	16.336320
31.077729	1140.190398	16.341338
30.840891	1152.018869	16.346355
30.949943	1141.988119	16.351373
30.985656	1143.857326	16.356391
30.850953	1146.702192	16.361408
31.374090	1135.199203	16.366426
31.140798	1146.555223	16.371443
30.929896	1137.461066	16.376461
31.314030	1138.134327	16.381479
31.279824	1155.297346	16.386496
31.508271	1160.350905	16.391514
31.430359	1162.892578	16.396531
31.505979	1165.543466	16.401549
31.430349	1162.176816	16.406567
31.217064	1164.041693	16.411584
31.897488	1156.762112	16.416602
31.460208	1167.285564	16.421619
31.743599	1160.136937	16.426637
31.725673	1168.558129	16.431655
32.171907	1163.337121	16.436672
31.756998	1146.088346	16.441690
31.792460	1167.937062	16.446707
31.604087	1165.129482	16.451725
31.820999	1157.038256	16.456743
31.685712	1169.339731	16.461760
31.918341	1152.135536	16.466778
32.098795	1167.436582	16.471795
31.902085	1169.909117	16.476813
32.095209	1166.013566	16.481831
31.752062	1164.976633	16.486848
32.244214	1153.879669	16.491866
31.873424	1151.851475	16.496883
32.130546	1156.332628	16.501901
31.991258	1150.198323	16.506919
31.718477	1166.263742	16.511936
31.796051	1168.403114	16.516954
31.852783	1167.824623	16.521971
31.757750	1170.582948	16.526989
31.860620	1178.492551	16.532007
31.772421	1183.145182	16.537024
32.395637	1182.929357	16.542042
32.413687	1194.412063	16.547059
32.661462	1178.759488	16.552077
32.452143	1170.937566	16.557095
32.285859	1191.006464	16.562112
32.840325	1177.367108	16.567130
33.086479	1183.770581	16.572147
32.344634	1169.452400	16.577165
32.804916	1161.325506	16.582183
32.580772	1161.266837	16.587200
32.876803	1157.018269	16.592218
32.504743	1145.887684	16.597235
32.537906	1146.722306	16.602253
32.509349	1149.202625	16.607271
32.561126	1179.405778	16.612288
32.717543	1184.580938	16.617306
32.870550	1176.548655	16.622323
32.901254	1177.434004	16.627341
32.980174	1171.411174	16.632359
32.903894	1199.651313	16.637376
33.286302	1164.974567	16.642394
33.016329	1148.607114	16.647411
32.897438	1171.589373	16.652429
32.956185	1131.210510	16.657447
33.134290	1179.471280	16.662464
33.127566	1150.094522	16.667482
32.956198	1155.817423	16.672499
33.190080	1134.267020	16.677517
33.370694	1154.227065	16.682535
32.915879	1158.238198	16.687552
33.439280	1169.621417	16.692570
33.342864	1152.425655	16.697587
32.764611	1154.823763	16.702605
33.395144	1170.476155	16.707623
33.218629	1182.771632	16.712640
33.371179	1179.107479	16.717658
33.478230	1177.010940	16.722675
33.470785	1179.351052	16.727693
33.469999	1164.252485	16.732711
33.207050	1177.664373	16.737728
33.458105	1171.743072	16.742746
33.419620	1180.689766	16.747763
33.313194	1179.884052	16.752781
33.798542	1157.057181	16.757799
33.495630	1185.695212	16.762816
33.530185	1166.046779	16.767834
33.446265	1183.813905	16.772851
33.256189	1181.132429	16.777869
33.295171	1160.901308	16.782887
33.124995	1189.315269	16.787904
33.903537	1181.604772	16.792922
33.883943	1188.879568	16.797939
34.041102	1199.056572	16.802957
34.430273	1187.211557	16.807975
33.802279	1191.472101	16.812992
33.804400	1175.643214	16.818010
34.218323	1163.042405	16.823027
33.867694	1165.983055	16.828045
34.326211	1177.686497	16.833063
33.993835	1183.593952	16.838080
34.260803	1173.162063	16.843098
34.047782	1170.946692	16.848115
33.852642	1171.037546	16.853133
34.004126	1192.263787	16.858151
34.396652	1181.459529	16.863168
34.089027	1191.512460	16.868186
34.044030	1201.753165	16.873203
34.143766	1198.490665	16.878221
34.561907	1191.748373	16.883239
34.564657	1198.241004	16.888256
34.467349	1192.194362	16.893274
34.694677	1192.826571	16.898291
34.388288	1199.782187	16.903309
34.359942	1188.467773	16.908327
34.453414	1193.472087	16.913344
34.417137	1189.273359	16.918362
34.756327	1187.010817	16.923379
34.354271	1194.373350	16.928397
34.519996	1194.022856	16.933415
34.323473	1192.533123	16.938432
34.422568	1187.792162	16.943450
34.621888	1195.337200	16.948467
34.507960	1207.122521	16.953485
34.748855	1212.922835	16.958503
35.085651	1215.514778	16.963520
35.077971	1230.460523	16.968538
35.003239	1225.729969	16.973555
34.910460	1228.744335	16.978573
35.350085	1216.405210	16.983591
34.871302	1199.147681	16.988608
35.033920	1187.581029	16.993626
35.021908	1188.267136	16.998643
35.065582	1213.600251	17.003661
35.364795	1221.687768	17.008679
35.534899	1214.705037	17.013696
35.245790	1197.925323	17.018714
35.367532	1183.370309	17.023731
35.214546	1194.310887	17.028749
35.297710	1187.985368	17.033767
34.813136	1186.851443	17.038784
35.194152	1208.190531	17.043802
35.725841	1215.605501	17.048819
35.429997	1220.053743	17.053837
35.593283	1220.950984	17.058855
35.586487	1224.758558	17.063872
35.219380	1215.911047	17.068890
35.569982	1211.060759	17.073907
35.538933	1224.665358	17.078925
35.830731	1210.916858	17.083943
35.905630	1214.664212	17.088960
35.768234	1208.106458	17.093978
35.657790	1218.285256	17.098995
35.639367	1233.585058	17.104013
35.679960	1219.488093	17.109031
35.669151	1215.900317	17.114048
35.473409	1214.449781	17.119066
35.655239	1215.424284	17.124083
35.581393	1214.250021	17.129101
36.091341	1209.284665	17.134119
35.760545	1215.242215	17.139136
35.775122	1219.738475	17.144154
35.880626	1217.538363	17.149171
35.995053	1216.518110	17.154189
35.747255	1215.541467	17.159207
36.068781	1230.249103	17.164224
36.113972	1233.685039	17.169242
36.243279	1239.518889	17.174259
35.955081	1243.405950	17.179277
36.180844	1247.638889	17.184295
36.445872	1246.278454	17.189312
36.263937	1247.180416	17.194330
36.494922	1239.827759	17.199347
36.234430	1243.383229	17.204365
36.300780	1246.609737	17.209383
36.404687	1244.379989	17.214400
35.939742	1242.898453	17.219418
36.108215	1237.161747	17.224435
36.310690	1238.707085	17.229453
36.955982	1239.374881	17.234471
36.804630	1242.934967	17.239488
36.461760	1242.684456	17.244506
36.739662	1249.993632	17.249523
36.534688	1269.876910	17.254541
36.765459	1270.198701	17.259559
37.032653	1263.109233	17.264576
36.838931	1275.744144	17.269594
37.186397	1273.201857	17.274611
37.163544	1267.037922	17.279629
37.071755	1228.126765	17.284647
36.954967	1245.466648	17.289664
37.228432	1244.800110	17.294682
37.268861	1233.402338	17.299699
37.038326	1227.090651	17.304717
36.877543	1231.467024	17.309735
37.118842	1232.987294	17.314752
37.026902	1246.977559	17.319770
37.105549	1253.621697	17.324787
37.240292	1267.144842	17.329805
37.172469	1266.644411	17.334823
37.248538	1262.495382	17.339840
36.824530	1273.707319	17.344858
37.435154	1258.306664	17.349875
37.228159	1269.001094	17.354893
37.386975	1271.775581	17.359911
37.413003	1273.622755	17.364928
37.231980	1273.140376	17.369946
37.547124	1265.673616	17.374963
37.240610	1261.783792	17.379981
37.374324	1256.041611	17.384999
37.501602	1260.051172	17.390016
37.409181	1287.019966	17.395034
37.807534	1279.653182	17.400051
37.381391	1298.996070	17.405069
37.712563	1294.194470	17.410087
38.052117	1286.494155	17.415104
37.838902	1284.561928	17.420122
37.794791	1287.332603	17.425139
37.957628	1309.740066	17.430157
38.140092	1287.710020	17.435175
38.343173	1287.116051	17.440192
37.471844	1309.693158	17.445210
38.093609	1294.567529	17.450227
38.276750	1291.112392	17.455245
38.069324	1279.183128	17.460263
38.602450	1286.888902	17.465280
38.322035	1281.425103	17.470298
38.702413	1301.296867	17.475315
38.721003	1282.564709	17.480333
38.415740	1276.774555	17.485351
38.574111	1264.300925	17.490368
38.094980	1251.225865	17.495386
38.402162	1268.076611	17.500403
38.437266	1285.571635	17.505421
38.598543	1291.969817	17.510439
38.585265	1292.122900	17.515456
38.483623	1303.660959	17.520474
38.548130	1287.631672	17.525491
38.279406	1292.629291	17.530509
38.663785	1297.864088	17.535527
38.795833	1277.498419	17.540544
38.325139	1289.614395	17.545562
38.806859	1295.585540	17.550579
38.437579	1288.792608	17.555597
38.500220	1270.690486	17.560615
38.931033	1290.094890	17.565632
38.584343	1295.624018	17.570650
38.858293	1288.102471	17.575667
38.708104	1319.297626	17.580685
39.126410	1296.404153	17.585703
39.449091	1332.650183	17.590720
39.207627	1314.716048	17.595738
39.077825	1324.822506	17.600755
39.366604	1305.860047	17.605773
39.272694	1317.933262	17.610791
39.361119	1277.914182	17.615808
39.126512	1303.491600	17.620826
39.051469	1294.328487	17.625843
39.218892	1302.440213	17.630861
39.220913	1310.037225	17.635879
38.988515	1320.016902	17.640896
39.307030	1306.224728	17.645914
39.348724	1297.810598	17.650931
39.591230	1310.984706	17.655949
39.519795	1313.504923	17.660967
39.660938	1309.985696	17.665984
39.833717	1313.657695	17.671002
39.630139	1306.920122	17.676019
39.535729	1305.050740	17.681037
39.560853	1307.042775	17.686055
40.247669	1309.745650	17.691072
39.904139	1299.455072	17.696090
39.967797	1314.112687	17.701107
40.415179	1301.070715	17.706125
39.915067	1301.400532	17.711143
40.201122	1292.694190	17.716160
40.252263	1317.741593	17.721178
40.236808	1285.668333	17.726195
40.085756	1301.019242	17.731213
39.946881	1305.271026	17.736231
40.526468	1298.943366	17.741248
39.936898	1302.515151	17.746266
39.917865	1301.586959	17.751283
40.363929	1297.891698	17.756301
39.909230	1301.690501	17.761319
40.085066	1298.280570	17.766336
40.131725	1301.944366	17.771354
40.066410	1295.191041	17.776371
40.035380	1302.640743	17.781389
40.678552	1313.899589	17.786407
41.047737	1320.115197	17.791424
40.683992	1312.275354	17.796442
40.800573	1303.097406	17.801459
40.795642	1291.827939	17.806477
40.653777	1290.809230	17.811495
40.513196	1297.644072	17.816512
40.879757	1295.586352	17.821530
40.712060	1294.505698	17.826547
40.550930	1295.725227	17.831565
40.714339	1320.946633	17.836583
41.045397	1313.879987	17.841600
40.830579	1332.745645	17.846618
40.812251	1325.849538	17.851635
41.043583	1329.007284	17.856653
40.963389	1325.197749	17.861671
41.089959	1321.710729	17.866688
41.044134	1323.401062	17.871706
41.072346	1321.939966	17.876723
40.936103	1306.277713	17.881741
40.401856	1339.948647	17.886759
41.095591	1310.124818	17.891776
40.949974	1330.714407	17.896794
41.173129	1351.163422	17.901811
41.620089	1333.866632	17.906829
41.643816	1358.802079	17.911847
41.837489	1344.295205	17.916864
41.644507	1339.872896	17.921882
41.332778	1315.694310	17.926899
41.837859	1316.912985	17.931917
41.334263	1334.762954	17.936935
41.686420	1314.107311	17.941952
41.681219	1355.922046	17.946970
41.694310	1336.946885	17.951987
41.969189	1330.479050	17.957005
41.657842	1353.495435	17.962023
41.829280	1344.503760	17.967040
42.032389	1335.300982	17.972058
42.163812	1352.637588	17.977075
42.272029	1327.959446	17.982093
41.899490	1326.088800	17.987111
41.870999	1323.565563	17.992128
41.738519	1327.924868	17.997146
41.906329	1336.679891	18.002163
42.298462	1330.182346	18.007181
41.949837	1348.429170	18.012199
41.955203	1354.633603	18.017216
42.066122	1334.436383	18.022234
41.962279	1350.531691	18.027251
42.342046	1319.894357	18.032269
41.779572	1358.350049	18.037287
42.608823	1351.063944	18.042304
42.541650	1348.348678	18.047322
42.205030	1356.979673	18.052339
42.306107	1378.645218	18.057357
42.937773	1353.452564	18.062375
42.893199	1360.597729	18.067392
42.776220	1359.844022	18.072410
43.079079	1366.111124	18.077427
43.254086	1354.164852	18.082445
43.157987	1346.274444	18.087463
42.948326	1329.145292	18.092480
42.850097	1318.357851	18.097498
42.657589	1337.715439	18.102515
42.670503	1328.808826	18.107533
42.963427	1336.653604	18.112551
42.843102	1334.844976	18.117568
43.054157	1352.805931	18.122586
43.301301	1349.162829	18.127603
43.298819	1357.458978	18.132621
42.959284	1361.928387	18.137639
42.937902	1341.283514	18.142656
43.018315	1347.708774	18.147674
42.978485	1355.015194	18.152691
42.829446	1352.611846	18.157709
42.772272	1356.797134	18.162727
42.980369	1365.764392	18.167744
43.404330	1375.974476	18.172762
43.363020	1390.422401	18.177779
43.664300	1388.058914	18.182797
43.443884	1390.898621	18.187815
43.699035	1383.700907	18.192832
43.812460	1380.533708	18.197850
43.679523	1388.032738	18.202867
43.948031	1371.623200	18.207885
43.715305	1385.763460	18.212903
43.816397	1380.457424	18.217920
44.173528	1373.100313	18.222938
43.841090	1383.964263	18.227955
44.047023	1376.612387	18.232973
44.209749	1383.274636	18.237991
44.104020	1386.300538	18.243008
44.258416	1379.858187	18.248026
43.874663	1382.719222	18.253043
44.165419	1379.152524	18.258061
44.223507	1381.427164	18.263079
44.441574	1388.767976	18.268096
44.441768	1375.858597	18.273114
44.007728	1376.509773	18.278131
44.302819	1379.849264	18.283149
44.187575	1380.141299	18.288167
43.960436	1384.589645	18.293184
44.018780	1377.901501	18.298202
44.140444	1379.403116	18.303219
44.385968	1384.343924	18.308237
44.224077	1396.509840	18.313255
44.233398	1404.072704	18.318272
44.602929	1402.429759	18.323290
44.533859	1406.261469	18.328307
44.354140	1406.239756	18.333325
44.391696	1410.222770	18.338343
44.836658	1427.820912	18.343360
45.225098	1417.131959	18.348378
45.053067	1428.734824	18.353395
45.086216	1423.471067	18.358413
45.459744	1419.450729	18.363431
45.454191	1405.447455	18.368448
45.219501	1399.284214	18.373466
44.890838	1392.173307	18.378483
45.122281	1391.499309	18.383501
44.922489	1397.388852	18.388519
44.987388	1405.270031	18.393536
45.683685	1414.477203	18.398554
45.329564	1415.310683	18.403571
45.428244	1423.461754	18.408589
45.540945	1421.394166	18.413607
45.776397	1409.748084	18.418624
46.039205	1408.106428	18.423642
45.485557	1401.314530	18.428659
45.788828	1392.267196	18.433677
45.405174	1394.970921	18.438695
45.402295	1396.517565	18.443712
45.695559	1414.882323	18.448730
45.667940	1412.261408	18.453747
45.823955	1418.070623	18.458765
45.933759	1420.392076	18.463783
45.780917	1423.744811	18.468800
46.043177	1416.808634	18.473818
45.775058	1420.865565	18.478835
45.772040	1410.372746	18.483853
46.058536	1412.041553	18.488871
45.993900	1425.080709	18.493888
46.210869	1415.713654	18.498906
45.931251	1409.018046	18.503923
45.812037	1414.097252	18.508941
46.016646	1422.231429	18.513959
45.807916	1444.110067	18.518976
46.617487	1443.405217	18.523994
46.222398	1437.704824	18.529011
46.388566	1456.306973	18.534029
47.015021	1441.490320	18.539047
46.430520	1444.686963	18.544064
46.693564	1439.015318	18.549082
46.667783	1450.760039	18.554099
46.952875	1441.083240	18.559117
47.027879	1436.106949	18.564135
47.089797	1437.481249	18.569152
46.991510	1453.728363	18.574170
46.488812	1445.687245	18.579187
46.437577	1431.071481	18.584205
46.644980	1430.074138	18.589223
46.525416	1439.357954	18.594240
46.941357	1436.010370	18.599258
46.856181	1442.193101	18.604275
47.199841	1441.782767	18.609293
47.066655	1442.304172	18.614311
46.885391	1437.266506	18.619328
47.192205	1444.906214	18.624346
47.186501	1470.334168	18.629363
47.543433	1469.416793	18.634381
48.040377	1462.175763	18.639399
47.669689	1463.600178	18.644416
47.574866	1437.845283	18.649434
47.273081	1437.780117	18.654451
47.518340	1440.680847	18.659469
47.471471	1450.075768	18.664487
47.592909	1466.624472	18.669504
47.737428	1464.128674	18.674522
47.999023	1466.781420	18.679539
47.714062	1464.498826	18.684557
48.084576	1468.732343	18.689575
48.044018	1459.988328	18.694592
48.023839	1458.346179	18.699610
48.166381	1467.421479	18.704627
47.804106	1454.873418	18.709645
48.286648	1454.752384	18.714663
48.114018	1455.006383	18.719680
48.335150	1454.038308	18.724698
48.044866	1472.071497	18.729715
48.237804	1458.692448	18.734733
48.678966	1458.793510	18.739751
47.948142	1465.617170	18.744768
47.996450	1458.211741	18.749786
48.241640	1458.768758	18.754803
47.954839	1456.823074	18.759821
48.251676	1455.083181	18.764839
48.095910	1460.412043	18.769856
48.525885	1439.484272	18.774874
48.326767	1460.269762	18.779891
48.557815	1474.903992	18.784909
48.835713	1465.108778	18.789927
48.984030	1478.911520	18.794944
49.134290	1466.494064	18.799962
48.899074	1474.593022	18.804979
49.117392	1466.864758	18.809997
48.779197	1466.830565	18.815015
48.527747	1471.350452	18.820032
49.092804	1471.170644	18.825050
48.738308	1483.584418	18.830067
48.802531	1477.793458	18.835085
49.045594	1471.774214	18.840103
49.250993	1478.720703	18.845120
49.104121	1484.048154	18.850138
49.063698	1482.450128	18.855155
49.226175	1469.898592	18.860173
49.534512	1503.416660	18.865191
49.581338	1509.284222	18.870208
49.895688	1481.013300	18.875226
49.562537	1489.260014	18.880243
49.295446	1479.498220	18.885261
49.603754	1478.758479	18.890279
49.915187	1495.336691	18.895296
49.587556	1500.118838	18.900314
49.949588	1490.261429	18.905331
49.523982	1509.956857	18.910349
50.113463	1481.352632	18.915367
49.834572	1507.843504	18.920384
50.116062	1490.159224	18.925402
49.890720	1485.745176	18.930419
49.856401	1515.327279	18.935437
50.266347	1479.426333	18.940455
49.944448	1514.726441	18.945472
50.108117	1486.894803	18.950490
50.169267	1495.559971	18.955507
50.377963	1495.062623	18.960525
50.203728	1497.743980	18.965543
50.126457	1478.471594	18.970560
50.162346	1514.384731	18.975578
50.467677	1494.881427	18.980595
50.198251	1522.957950	18.985613
50.629185	1512.837861	18.990631
50.470678	1535.792410	18.995648
50.729023	1527.450560	19.000666
50.596292	1527.276639	19.005683
50.909419	1533.940142	19.010701
50.944025	1503.193875	19.015719
50.576108	1527.359964	19.020736
50.952443	1492.158030	19.025754
50.601463	1521.288865	19.030771
50.610405	1507.375987	19.035789
50.785216	1503.091597	19.040807
50.883582	1523.974451	19.045824
50.723789	1531.726368	19.050842
51.187300	1524.929500	19.055859
51.079204	1545.007698	19.060877
51.382927	1536.520971	19.065895
51.046693	1543.307694	19.070912
51.075973	1521.854624	19.075930
51.395649	1535.749639	19.080947
51.126114	1545.611914	19.085965
51.345824	1533.328827	19.090983
51.487925	1555.330219	19.096000
51.329799	1565.453945	19.101018
51.756880	1566.079485	19.106035
52.226671	1557.123469	19.111053
52.310893	1552.884969	19.116071
51.889518	1546.557959	19.121088
51.733750	1535.956491	19.126106
52.116492	1548.632627	19.131123
52.146406	1547.046972	19.136141
52.169449	1533.819999	19.141159
51.757541	1522.950297	19.146176
51.949475	1557.654990	19.151194
52.201035	1547.346410	19.156211
52.012297	1554.848133	19.161229
52.243147	1546.515376	19.166247
52.234565	1557.928688	19.171264
52.222599	1552.415683	19.176282
52.433554	1546.050753	19.181299
52.177434	1550.285126	19.186317
52.403835	1548.694878	19.191335
52.762611	1543.781833	19.196352
52.727195	1554.197433	19.201370
52.866742	1561.693996	19.206387
52.586932	1558.941816	19.211405
53.037162	1548.999518	19.216423
53.006551	1559.486713	19.221440
52.676297	1559.655740	19.226458
52.655016	1546.205383	19.231475
52.757272	1566.098272	19.236493
53.080495	1575.851097	19.241511
53.130833	1589.874057	19.246528
53.043822	1587.805261	19.251546
52.978967	1587.696019	19.256563
53.115571	1582.499074	19.261581
53.498325	1582.913039	19.266599
53.376572	1583.253306	19.271616
53.449986	1577.014113	19.276634
53.681898	1565.852951	19.281651
53.282490	1605.867288	19.286669
53.784399	1575.209938	19.291687
53.653121	1566.703689	19.296704
53.592855	1574.340659	19.301722
53.864230	1579.345052	19.306739
53.743457	1570.849710	19.311757
53.827971	1564.945371	19.316775
53.566717	1589.204662	19.321792
53.733018	1558.616596	19.326810
53.702565	1584.789573	19.331827
53.569325	1576.805863	19.336845
53.845005	1569.161203	19.341863
54.266572	1572.027552	19.346880
54.004651	1572.794428	19.351898
53.887349	1581.090139	19.356915
54.155345	1577.739377	19.361933
54.413123	1583.744784	19.366951
54.396884	1594.506558	19.371968
54.227174	1616.052051	19.376986
54.772502	1600.472693	19.382003
54.620734	1605.857597	19.387021
54.645036	1600.524402	19.392039
54.673637	1604.604851	19.397056
54.548114	1605.754234	19.402074
54.843247	1593.142112	19.407091
54.452953	1623.017151	19.412109
55.044701	1615.515542	19.417127
55.028339	1594.609963	19.422144
54.650184	1619.569051	19.427162
54.994378	1598.780571	19.432179
54.967571	1604.727552	19.437197
55.105272	1602.772353	19.442215
55.050551	1608.133917	19.447232
55.025198	1599.626488	19.452250
55.450806	1591.475001	19.457267
55.091945	1592.100037	19.462285
55.436511	1596.476154	19.467303
55.236413	1593.003411	19.472320
55.000108	1603.960730	19.477338
55.461451	1600.472166	19.482355
55.115347	1598.919728	19.487373
55.277930	1602.145127	19.492391
55.613932	1621.948909	19.497408
55.949731	1626.134528	19.502426
55.890393	1622.563828	19.507443
55.661509	1625.950757	19.512461
56.000973	1616.007202	19.517479
56.098554	1611.134214	19.522496
55.942209	1625.902733	19.527514
56.281880	1620.547553	19.532531
56.176417	1621.929687	19.537549
56.121584	1618.883648	19.542567
56.376337	1616.000594	19.547584
56.180924	1617.678637	19.552602
56.320789	1611.222771	19.557619
56.147555	1624.627055	19.562637
56.018844	1619.577798	19.567655
56.240208	1603.578202	19.572672
55.892455	1619.221932	19.577690
56.391753	1610.912395	19.582707
56.102782	1614.678555	19.587725
56.178851	1616.670374	19.592743
56.422171	1638.463060	19.597760
56.311784	1642.405238	19.602778
56.767044	1638.338775	19.607795
56.634196	1655.483512	19.612813
56.807786	1646.936465	19.617831
56.667561	1638.503958	19.622848
56.671383	1644.600225	19.627866
56.845566	1641.278565	19.632883
57.150759	1655.087919	19.637901
57.316137	1668.784304	19.642919
57.378886	1665.231877	19.647936
57.358256	1675.296001	19.652954
57.647600	1655.537060	19.657971
57.196813	1642.288810	19.662989
57.192123	1657.605746	19.668007
57.778004	1652.884533	19.673024
57.506015	1668.895325	19.678042
57.775688	1648.312136	19.683059
57.726251	1659.142171	19.688077
57.874994	1651.489398	19.693095
57.649481	1644.862127	19.698112
57.903048	1653.583219	19.703130
58.248297	1641.008681	19.708147
57.864029	1658.064529	19.713165
57.873688	1652.865782	19.718183
58.110321	1644.363737	19.723200
57.822097	1670.269668	19.728218
57.892560	1664.829990	19.733235
57.841005	1661.717353	19.738253
57.730522	1667.028058	19.743271
57.944511	1669.556303	19.748288
57.978270	1682.974822	19.753306
58.497208	1681.676103	19.758323
58.204225	1684.160930	19.763341
58.480443	1690.418267	19.768359
58.597264	1687.027095	19.773376
58.561506	1680.806840	19.778394
58.641155	1677.377554	19.783411
58.481466	1669.028356	19.788429
58.418995	1691.031904	19.793447
59.009650	1682.761240	19.798464
58.607645	1708.311011	19.803482
58.900426	1727.454879	19.808499
58.987399	1697.001866	19.813517
59.079870	1728.053814	19.818535
59.361213	1702.044983	19.823552
59.130845	1732.174736	19.828570
59.295215	1725.349976	19.833587
59.384395	1705.029867	19.838605
59.014644	1729.489162	19.843623
59.259590	1723.096713	19.848640
59.261276	1726.302181	19.853658
59.188394	1701.594081	19.858675
59.078944	1727.391382	19.863693
59.038832	1711.840771	19.868711
59.493358	1732.179501	19.873728
59.527876	1757.925583	19.878746
59.816985	1742.206038	19.883763
59.898940	1730.382834	19.888781
59.928709	1736.371183	19.893799
60.157854	1742.895595	19.898816
60.127377	1736.024825	19.903834
60.324063	1730.470614	19.908851
60.275536	1736.244937	19.913869
60.126460	1736.317434	19.918887
60.567675	1722.922145	19.923904
60.113168	1726.321482	19.928922
60.093860	1731.932270	19.933939
60.374612	1725.199062	19.938957
60.572369	1720.473655	19.943975
60.406440	1730.153581	19.948992
60.693667	1755.267912	19.954010
60.919569	1754.456359	19.959027
61.103338	1745.196633	19.964045
60.938488	1733.636149	19.969063
61.034444	1725.106155	19.974080
60.941624	1728.153663	19.979098
60.611093	1729.938208	19.984115
61.121186	1738.380921	19.989133
60.961767	1751.671436	19.994151
61.013677	1755.968431	19.999168
61.045357	1752.935308	20.004186
61.313205	1760.856676	20.009203
61.131042	1753.475265	20.014221
61.102166	1756.429213	20.019239
61.674831	1755.832919	20.024256
61.460091	1745.125085	20.029274
61.365959	1748.935714	20.034291
61.394001	1751.414976	20.039309
61.171345	1750.251815	20.044327
61.529396	1759.950448	20.049344
61.610921	1783.085758	20.054362
61.912394	1780.495667	20.059379
62.004752	1779.867428	20.064397
61.965974	1783.121832	20.069415
62.270135	1765.432029	20.074432
61.910648	1775.551832	20.079450
62.252843	1774.973415	20.084467
62.285575	1770.346666	20.089485
62.302715	1774.641345	20.094503
62.173210	1770.786073	20.099520
62.201851	1773.582990	20.104538
62.155437	1762.678416	20.109555
62.582246	1769.894902	20.114573
62.421168	1773.445656	20.119591
62.800985	1767.324259	20.124608
62.631227	1769.322267	20.129626
62.553515	1759.279974	20.134643
62.830245	1764.775929	20.139661
62.591331	1773.541022	20.144679
63.181771	1784.003274	20.149696
62.962659	1784.816815	20.154714
62.840928	1798.587422	20.159731
62.992415	1791.686035	20.164749
62.828069	1813.663543	20.169767
62.983040	1802.707949	20.174784
62.825414	1801.027905	20.179802
62.839241	1801.766549	20.184819
63.287594	1792.272694	20.189837
63.121375	1798.709170	20.194855
63.376592	1800.046388	20.199872
63.665757	1801.406508	20.204890
63.749503	1817.505453	20.209907
63.771974	1814.948835	20.214925
63.539072	1820.725852	20.219943
63.352403	1815.265774	20.224960
63.625687	1811.283339	20.229978
63.421259	1819.251736	20.234995
63.797948	1820.324196	20.240013
63.852504	1824.288884	20.245031
63.951296	1831.068502	20.250048
64.096668	1837.109244	20.255066
64.174037	1839.590093	20.260083
64.516061	1827.026920	20.265101
64.378015	1837.334822	20.270119
64.350804	1830.413149	20.275136
64.759970	1842.320062	20.280154
64.363111	1834.315326	20.285171
64.884646	1818.091450	20.290189
64.727959	1823.562161	20.295207
64.542240	1820.334033	20.300224
64.766443	1824.557956	20.305242
64.899201	1823.983047	20.310259
65.093410	1818.517286	20.315277
64.777885	1824.504106	20.320295
64.785006	1821.924767	20.325312
65.040978	1819.672257	20.330330
64.994913	1819.264289	20.335347
65.278571	1830.198636	20.340365
65.120850	1851.937621	20.345383
65.634852	1836.106607	20.350400
65.733881	1851.103616	20.355418
65.649606	1851.002187	20.360435
65.613384	1851.608816	20.365453
65.416398	1848.297535	20.370471
65.494141	1846.537481	20.375488
65.569243	1845.103462	20.380506
65.418899	1856.888825	20.385523
65.697002	1841.935412	20.390541
65.657408	1850.100909	20.395559
65.934671	1851.123161	20.400576
65.921602	1846.055383	20.405594
65.604209	1849.967706	20.410611
66.165367	1860.709961	20.415629
66.235190	1877.077032	20.420647
66.101437	1877.202142	20.425664
66.434171	1875.045920	20.430682
66.035168	1869.056542	20.435699
66.628579	1875.043157	20.440717
66.264096	1871.885994	20.445735
66.467328	1868.680774	20.450752
66.731028	1866.976007	20.455770
66.555675	1867.642575	20.460787
66.658713	1872.892564	20.465805
66.636714	1875.227245	20.470823
66.486936	1871.450682	20.475840
67.176103	1876.934393	20.480858
66.739300	1897.583805	20.485875
66.912394	1893.483618	20.490893
66.855528	1903.313007	20.495911
67.299265	1902.059298	20.500928
67.155634	1890.193285	20.505946
67.121610	1900.945538	20.510963
67.648138	1891.876452	20.515981
67.112716	1897.761515	20.520999
67.204724	1909.921979	20.526016
67.945587	1914.277470	20.531034
67.953970	1919.588188	20.536051
68.304089	1908.252185	20.541069
67.903383	1893.808085	20.546087
67.907099	1893.938014	20.551104
68.330533	1891.594295	20.556122
67.821344	1898.162584	20.561139
68.076087	1883.077575	20.566157
68.259112	1887.212129	20.571175
68.227856	1914.600199	20.576192
68.464236	1916.311666	20.581210
68.299470	1922.988637	20.586227
68.682507	1913.240852	20.591245
68.606398	1911.790041	20.596263
68.550947	1908.448311	20.601280
68.513195	1896.667656	20.606298
68.456486	1923.411718	20.611315
68.918102	1909.780198	20.616333
68.866652	1911.402283	20.621351
68.470537	1923.080600	20.626368
69.054190	1914.461714	20.631386
68.625980	1914.729733	20.636403
68.352988	1915.072101	20.641421
68.766233	1908.564645	20.646439
69.051979	1937.179500	20.651456
69.271851	1941.850887	20.656474
69.193744	1936.076150	20.661491
69.365676	1937.417225	20.666509
69.639990	1931.893030	20.671527
69.312227	1929.448871	20.676544
69.828930	1935.281004	20.681562
69.700765	1933.059845	20.686579
69.497903	1926.387933	20.691597
69.936274	1930.827846	20.696615
69.792203	1941.679475	20.701632
69.940440	1928.686221	20.706650
69.798130	1935.644334	20.711667
69.763727	1931.040824	20.716685
69.973257	1930.554342	20.721703
69.661182	1932.521583	20.726720
69.980979	1948.754492	20.731738
70.042899	1946.468413	20.736755
70.028870	1957.555720	20.741773
70.094418	1968.150572	20.746791
70.316312	1959.959008	20.751808
70.553704	1958.917523	20.756826
70.009315	1968.568295	20.761843
70.540322	1976.012089	20.766861
71.134725	1973.175479	20.771879
70.899226	1971.841314	20.776896
70.887666	1964.484499	20.781914
71.062916	1974.280068	20.786931
71.028718	1974.266607	20.791949
71.334681	1971.032398	20.796967
71.347474	1975.788728	20.801984
71.512378	1970.628032	20.807002
71.258980	1981.709483	20.812019
71.346324	1966.632204	20.817037
71.423020	1976.267312	20.822055
71.454946	1976.540608	20.827072
71.339415	1971.103733	20.832090
71.682164	1977.073735	20.837107
71.495198	1995.325476	20.842125
71.747260	2005.143424	20.847143
71.653046	2010.292783	20.852160
72.181204	1992.656650	20.857178
71.539945	2009.385799	20.862195
71.840260	1997.555872	20.867213
72.354863	1994.330860	20.872231
72.110929	2000.872626	20.877248
72.172543	2002.726804	20.882266
72.091690	2006.011562	20.887283
72.405001	2011.251667	20.892301
73.009908	2026.820998	20.897319
72.840092	2010.507379	20.902336
72.892989	1996.162304	20.907354
72.738950	1997.605702	20.912371
72.627242	1988.823949	20.917389
73.389539	1995.058965	20.922407
72.841383	1996.922287	20.927424
72.875526	1996.287592	20.932442
73.287534	1996.577359	20.937459
73.421616	1986.656865	20.942477
73.310347	1990.688940	20.947495
73.076970	1992.259820	20.952512
73.216895	1982.063118	20.957530
73.285735	2008.502599	20.962547
73.251873	2020.233340	20.967565
73.401912	2020.445331	20.972583
73.223966	2021.349847	20.977600
73.464167	2020.962292	20.982618
73.543702	2012.818568	20.987635
73.269489	2028.474604	20.992653
73.579862	2032.044623	20.997671
73.727351	2044.696578	21.002688
74.139916	2049.047834	21.007706
73.750949	2058.450510	21.012723
73.908221	2046.478184	21.017741
74.057839	2032.624167	21.022759
73.875055	2045.759800	21.027776
74.220938	2046.992922	21.032794
74.638647	2069.283845	21.037811
74.455166	2073.671953	21.042829
74.830089	2056.639055	21.047847
74.756407	2068.660905	21.052864
74.801031	2065.625653	21.057882
74.811806	2061.187932	21.062899
74.771020	2057.677087	21.067917
75.163743	2057.787458	21.072935
75.099672	2062.600118	21.077952
75.161092	2065.975462	21.082970
75.391604	2060.667418	21.087987
75.188366	2053.326966	21.093005
75.647167	2058.701192	21.098023
75.305568	2053.916965	21.103040
75.175022	2047.942904	21.108058
75.285766	2055.005441	21.113075
75.265289	2073.413204	21.118093
75.662061	2079.643623	21.123111
75.738344	2089.908088	21.128128
75.822173	2080.162286	21.133146
75.723862	2106.218036	21.138163
75.927843	2089.646518	21.143181
75.768083	2078.921803	21.148199
75.415122	2101.154767	21.153216
76.115463	2099.584843	21.158234
76.232302	2113.344447	21.163251
76.158539	2119.360475	21.168269
76.354265	2120.199119	21.173287
76.603374	2119.802277	21.178304
76.457713	2119.573779	21.183322
76.617269	2122.526069	21.188339
76.570175	2124.894678	21.193357
77.049702	2117.253409	21.198375
77.223767	2119.055063	21.203392
77.370729	2112.906161	21.208410
77.068971	2107.793089	21.213427
76.617963	2108.253510	21.218445
76.934987	2101.758166	21.223463
76.693287	2106.127253	21.228480
76.949953	2143.295066	21.233498
77.366560	2139.086766	21.238515
77.129406	2141.468382	21.243533
77.529714	2132.548266	21.248551
77.373009	2150.274698	21.253568
77.626527	2149.328159	21.258586
77.962309	2126.668343	21.263603
77.550932	2145.500330	21.268621
77.840423	2148.866067	21.273639
78.015170	2134.930866	21.278656
77.796483	2141.190240	21.283674
77.831596	2141.538538	21.288691
78.051619	2163.159550	21.293709
78.133588	2155.007493	21.298727
78.084810	2158.702455	21.303744
78.268481	2160.655169	21.308762
78.513701	2150.226051	21.313779
78.517485	2150.255297	21.318797
78.758581	2143.624177	21.323815
78.732377	2131.496992	21.328832
78.771528	2145.333509	21.333850
79.090114	2151.183166	21.338867
78.861406	2160.368440	21.343885
79.291137	2164.468454	21.348903
79.203131	2168.781590	21.353920
79.476497	2176.979165	21.358938
79.810070	2161.349607	21.363955
79.567283	2153.878555	21.368973
79.452262	2141.531140	21.373991
79.498407	2139.868900	21.379008
79.623002	2127.178117	21.384026
80.008824	2137.766069	21.389043
79.645180	2149.211296	21.394061
79.545826	2151.111610	21.399079
79.847277	2158.419071	21.404096
79.899374	2155.093169	21.409114
80.110554	2160.708269	21.414131
80.052221	2162.949687	21.419149
80.249564	2166.248324	21.424167
80.068902	2157.774769	21.429184
80.100067	2154.304338	21.434202
80.082722	2153.260989	21.439219
80.098815	2172.625752	21.444237
80.444935	2183.327035	21.449255
80.744624	2190.858166	21.454272
80.420266	2196.690813	21.459290
80.697090	2195.976513	21.464307
80.494740	2195.856155	21.469325
80.491455	2195.565625	21.474343
80.703130	2206.560502	21.479360
80.978544	2211.658857	21.484378
81.341168	2209.612655	21.489395
81.401364	2214.847578	21.494413
81.508608	2222.321322	21.499431
81.344087	2218.798707	21.504448
81.593816	2218.702218	21.509466
81.839792	2204.686378	21.514483
81.577469	2208.427989	21.519501
81.709242	2206.920403	21.524519
81.997919	2210.308307	21.529536
81.985360	2208.139458	21.534554
81.780032	2205.175496	21.539571
81.665632	2207.814405	21.544589
81.925692	2210.447088	21.549607
81.958338	2207.182478	21.554624
81.723340	2209.960170	21.559642
81.988910	2231.202781	21.564659
81.864293	2232.164874	21.569677
82.233573	2231.066162	21.574695
82.436427	2223.569631	21.579712
82.831516	2247.089845	21.584730
82.973755	2243.206844	21.589747
82.821671	2252.697715	21.594765
82.934039	2260.987079	21.599783
83.452985	2257.375920	21.604800
83.155657	2257.781950	21.609818
83.304272	2255.266490	21.614835
82.912377	2261.710840	21.619853
83.106618	2255.011634	21.624871
83.164958	2259.383260	21.629888
83.245738	2253.037208	21.634906
83.533555	2254.057809	21.639923
83.299062	2256.066203	21.644941
83.583499	2268.334713	21.649959
83.952844	2274.497231	21.654976
83.546788	2286.463719	21.659994
83.966245	2282.871565	21.665011
83.860481	2287.126218	21.670029
84.065812	2282.007731	21.675047
84.156220	2285.583002	21.680064
83.963085	2281.295708	21.685082
84.255736	2271.318275	21.690099
84.374678	2296.608250	21.695117
84.537220	2293.824715	21.700135
84.982233	2295.631953	21.705152
84.499034	2309.287644	21.710170
85.061961	2301.544890	21.715187
84.679288	2300.135057	21.720205
84.895708	2302.725951	21.725223
84.974399	2303.223037	21.730240
85.052107	2308.886221	21.735258
85.275136	2285.533113	21.740275
85.020105	2308.851920	21.745293
85.254170	2306.764857	21.750311
85.040793	2285.353282	21.755328
84.912738	2318.478775	21.760346
85.258555	2317.405821	21.765363
85.266938	2338.651847	21.770381
85.323941	2318.090612	21.775399
85.527640	2338.731325	21.780416
86.080749	2350.773015	21.785434
86.347390	2348.350406	21.790451
86.290046	2357.667359	21.795469
86.330845	2354.305458	21.800487
86.612322	2345.334948	21.805504
86.184148	2340.558136	21.810522
86.285084	2333.087239	21.815539
86.399550	2360.261000	21.820557
86.424954	2342.235839	21.825575
86.402634	2338.926480	21.830592
86.674715	2341.741320	21.835610
86.782098	2353.912290	21.840627
86.427907	2339.976290	21.845645
86.708524	2359.269233	21.850663
87.336864	2381.102323	21.855680
87.083515	2371.230762	21.860698
87.475387	2364.109871	21.865715
87.538685	2369.550427	21.870733
87.299606	2373.595122	21.875751
87.419054	2363.810417	21.880768
87.386348	2375.009562	21.885786
87.503443	2361.438852	21.890803
87.549287	2378.618871	21.895821
87.566188	2367.351378	21.900839
87.939230	2375.283054	21.905856
87.774800	2392.443134	21.910874
88.273775	2400.738574	21.915891
88.335722	2398.424105	21.920909
88.142320	2401.883419	21.925927
88.606250	2404.457675	21.930944
88.295871	2397.659538	21.935962
88.504541	2396.070456	21.940979
88.090257	2407.003272	21.945997
88.207280	2405.796116	21.951015
88.822121	2413.780495	21.956032
88.805781	2417.339786	21.961050
89.118950	2416.730582	21.966067
89.351051	2416.405661	21.971085
89.487792	2415.960662	21.976103
89.328401	2405.875887	21.981120
89.341885	2402.237537	21.986138
89.490973	2405.142790	21.991155
89.515282	2407.160276	21.996173
89.552744	2408.857117	22.001191
89.578830	2403.280303	22.006208
89.336458	2413.533672	22.011226
89.704560	2408.124910	22.016243
89.941377	2414.136370	22.021261
89.753614	2431.107514	22.026279
90.157038	2429.779967	22.031296
89.855239	2435.710574	22.036314
90.290742	2436.022564	22.041331
90.290879	2431.774408	22.046349
90.309299	2436.587409	22.051367
90.483949	2432.626828	22.056384
90.278830	2435.453283	22.061402
90.229685	2422.541401	22.066419
90.846669	2441.998690	22.071437
90.733546	2448.817108	22.076455
91.037432	2450.026291	22.081472
90.692105	2464.308250	22.086490
90.934386	2449.788593	22.091507
91.070848	2454.671656	22.096525
91.030011	2454.906226	22.101543
91.169991	2449.556634	22.106560
91.214284	2467.864117	22.111578
91.294930	2482.562680	22.116595
91.350372	2483.978227	22.121613
91.456152	2483.878735	22.126631
91.607305	2472.630654	22.131648
91.751458	2478.115775	22.136666
91.806240	2487.885283	22.141683
91.926583	2490.231187	22.146701
91.999208	2497.474630	22.151719
92.188282	2486.369148	22.156736
91.954554	2498.224169	22.161754
92.267659	2502.625248	22.166771
92.431707	2503.703357	22.171789
92.771652	2515.235674	22.176807
92.962772	2523.091044	22.181824
93.057567	2513.901650	22.186842
92.956445	2512.337571	22.191859
93.283303	2509.386217	22.196877
93.162218	2520.911038	22.201895
93.491184	2518.442283	22.206912
93.405770	2517.588307	22.211930
93.408242	2518.379137	22.216947
93.650734	2502.323275	22.221965
93.496801	2512.146530	22.226983
93.722627	2512.762527	22.232000
93.681269	2510.108995	22.237018
93.584047	2518.567212	22.242035
93.883990	2512.278913	22.247053
93.561847	2512.255520	22.252071
93.844045	2525.500706	22.257088
93.927244	2532.657535	22.262106
93.992501	2538.811237	22.267123
94.495880	2531.893505	22.272141
94.168049	2527.005458	22.277159
94.384087	2531.424383	22.282176
94.619586	2549.250791	22.287194
94.635698	2558.787403	22.292211
95.042122	2570.094438	22.297229
95.069078	2571.778815	22.302247
94.934340	2574.576769	22.307264
95.194950	2560.485106	22.312282
95.099318	2568.983213	22.317299
95.318521	2564.932118	22.322317
95.217155	2563.736176	22.327335
95.775503	2555.649513	22.332352
95.358388	2570.834966	22.337370
95.483757	2574.149893	22.342387
95.704968	2556.027961	22.347405
95.522079	2566.828040	22.352423
95.612130	2563.602963	22.357440
95.766042	2570.242000	22.362458
95.616222	2590.987421	22.367475
95.794093	2594.412749	22.372493
95.897374	2587.076635	22.377511
95.960083	2601.994479	22.382528
95.934443	2609.839626	22.387546
96.412999	2618.482956	22.392563
96.587066	2605.615548	22.397581
96.424175	2617.976133	22.402599
96.957899	2616.568017	22.407616
97.082723	2626.838493	22.412634
97.238751	2642.528835	22.417651
97.473403	2634.684875	22.422669
97.562257	2640.629569	22.427687
97.710611	2618.926218	22.432704
97.700181	2603.724651	22.437722
97.786325	2597.844017	22.442739
97.512371	2589.746110	22.447757
97.674230	2600.279661	22.452775
97.877269	2615.823260	22.457792
97.987407	2623.836323	22.462810
97.798601	2623.986731	22.467827
98.129984	2619.098938	22.472845
97.758862	2617.286876	22.477863
98.021718	2610.830622	22.482880
97.965304	2617.506364	22.487898
98.081888	2624.330710	22.492915
98.630260	2644.858697	22.497933
98.776304	2654.844224	22.502951
98.484670	2651.471552	22.507968
98.419850	2645.146187	22.512986
98.699004	2648.313121	22.518003
98.862064	2659.478911	22.523021
99.069641	2675.504792	22.528039
99.234739	2678.681268	22.533056
99.254429	2676.670809	22.538074
99.282614	2672.819252	22.543091
99.752099	2671.939712	22.548109
99.312821	2688.823052	22.553127
99.302461	2672.289769	22.558144
100.041735	2681.784303	22.563162
99.687364	2688.900076	22.568179
99.531595	2699.043876	22.573197
99.910581	2694.345105	22.578215
100.244646	2690.304765	22.583232
100.211480	2680.136747	22.588250
100.050488	2694.516960	22.593267
100.743985	2698.617548	22.598285
100.364130	2706.349330	22.603303
100.596795	2719.906989	22.608320
100.778528	2716.266117	22.613338
100.755073	2728.152293	22.618355
101.134710	2722.473363	22.623373
101.026497	2712.035704	22.628391
101.370050	2713.231506	22.633408
101.063423	2716.635012	22.638426
101.325576	2721.057654	22.643443
101.662949	2714.462052	22.648461
101.271066	2715.901755	22.653479
101.578965	2718.420721	22.658496
101.515427	2726.082413	22.663514
101.633943	2738.564980	22.668531
101.700656	2743.743995	22.673549
101.975492	2747.337954	22.678567
102.101331	2747.498758	22.683584
102.240078	2735.456458	22.688602
101.924311	2752.704017	22.693619
102.364494	2761.919087	22.698637
102.493595	2759.590707	22.703655
102.443017	2756.195305	22.708672
102.869954	2772.001475	22.713690
103.210877	2774.739354	22.718707
102.914558	2758.839913	22.723725
103.266502	2757.135922	22.728743
103.058650	2771.426150	22.733760
103.318833	2758.006085	22.738778
103.070356	2767.666825	22.743795
103.609845	2772.271790	22.748813
103.647734	2785.582912	22.753831
103.722829	2796.449784	22.758848
103.772849	2788.930140	22.763866
103.383020	2799.503822	22.768883
103.891841	2796.650821	22.773901
103.744363	2800.353031	22.778919
104.093873	2791.310049	22.783936
104.052942	2799.034247	22.788954
104.036740	2815.864432	22.793971
104.138459	2820.708325	22.798989
104.556923	2813.819734	22.804007
104.622725	2811.801904	22.809024
104.631844	2804.974653	22.814042
104.470224	2828.876395	22.819059
104.612808	2834.311563	22.824077
104.577174	2842.588677	22.829095
104.855583	2845.680264	22.834112
105.211008	2841.160608	22.839130
105.295527	2867.164184	22.844147
105.729149	2865.503004	22.849165
105.728186	2859.243660	22.854183
105.456827	2866.797768	22.859200
105.632616	2861.142637	22.864218
105.834035	2864.454943	22.869235
106.227612	2859.738063	22.874253
106.026962	2863.108973	22.879271
106.280216	2869.999738	22.884288
106.310374	2855.807675	22.889306
106.200389	2855.399644	22.894323
106.112357	2859.726359	22.899341
106.506478	2878.698284	22.904359
106.504925	2885.589571	22.909376
106.504761	2887.923291	22.914394
106.406066	2898.599285	22.919411
106.228691	2901.022615	22.924429
106.807349	2913.710407	22.929447
107.010542	2921.691492	22.934464
107.476465	2911.544415	22.939482
107.255072	2919.376106	22.944499
107.027286	2922.188962	22.949517
107.565216	2935.309585	22.954535
107.699027	2936.881793	22.959552
108.278571	2938.433271	22.964570
107.809472	2941.625977	22.969587
108.053673	2940.179048	22.974605
108.019799	2943.336967	22.979623
108.266093	2939.944527	22.984640
108.191166	2929.313414	22.989658
108.198331	2941.379725	22.994675
108.673786	2952.340977	22.999693
109.042286	2957.443634	23.004711
109.294108	2959.159847	23.009728
109.554342	2945.679823	23.014746
109.274737	2948.557579	23.019763
109.440976	2952.478025	23.024781
109.543746	2959.411706	23.029799
109.342371	2968.777184	23.034816
109.690742	2956.578573	23.039834
109.932557	2956.300075	23.044851
109.693151	2950.973038	23.049869
109.827719	2950.176775	23.054887
109.987927	2952.203344	23.059904
110.201564	2941.916348	23.064922
109.634577	2951.237071	23.069939
109.881421	2948.240970	23.074957
110.026055	2950.578356	23.079975
109.934941	2962.020876	23.084992
110.636501	2967.467648	23.090010
110.258414	2976.154183	23.095027
110.235345	2978.873842	23.100045
110.888243	2980.836016	23.105063
110.770746	2989.353585	23.110080
111.208686	2994.660703	23.115098
111.162331	2998.342906	23.120115
111.432211	2994.767355	23.125133
111.656106	2987.326859	23.130151
111.626307	2999.017626	23.135168
111.906972	2992.585109	23.140186
111.779711	2991.382247	23.145203
111.818562	2998.337150	23.150221
111.836337	2999.230966	23.155239
111.835921	2998.270593	23.160256
111.637736	2996.666877	23.165274
111.905364	3003.859817	23.170291
112.313939	3019.345907	23.175309
112.200289	3025.710040	23.180327
112.137443	3023.735504	23.185344
112.639834	3019.646999	23.190362
112.377512	3025.744593	23.195379
112.192255	3042.548508	23.200397
112.980814	3049.797634	23.205415
113.005156	3052.998209	23.210432
113.230313	3055.905624	23.215450
113.005640	3056.436949	23.220467
113.077824	3044.756605	23.225485
113.490803	3060.931074	23.230503
113.354697	3075.578275	23.235520
113.491643	3067.507398	23.240538
113.586201	3081.986469	23.245555
113.530101	3086.950004	23.250573
114.414768	3089.550907	23.255591
114.551804	3104.633609	23.260608
114.653445	3101.028223	23.265626
114.956273	3095.346454	23.270643
114.812540	3100.709387	23.275661
115.182125	3099.291220	23.280679
114.756706	3112.258841	23.285696
114.880840	3102.764714	23.290714
115.050379	3096.793499	23.295731
114.774801	3104.582014	23.300749
114.929880	3097.231092	23.305767
114.938185	3100.217140	23.310784
115.262827	3117.866426	23.315802
115.477416	3125.760071	23.320819
115.553547	3128.939820	23.325837
115.660418	3127.217444	23.330855
115.279083	3133.447325	23.335872
115.902389	3141.061862	23.340890
115.958495	3152.518813	23.345907
115.899503	3160.637797	23.350925
116.180920	3151.854010	23.355943
116.206203	3157.308002	23.360960
116.534362	3175.762254	23.365978
116.600506	3181.816192	23.370995
116.878033	3181.380974	23.376013
117.252307	3172.867111	23.381031
117.287901	3171.277228	23.386048
117.538692	3159.872721	23.391066
117.771878	3154.304288	23.396083
117.599881	3171.843260	23.401101
117.893643	3156.618572	23.406119
117.864215	3161.617208	23.411136
117.777656	3155.119680	23.416154
117.637248	3167.697386	23.421171
118.108724	3167.580486	23.426189
117.957233	3162.631068	23.431207
117.951216	3168.930120	23.436224
118.208035	3166.779531	23.441242
117.914029	3171.836087	23.446259
118.275739	3187.266116	23.451277
118.240575	3193.602077	23.456295
118.159623	3200.670567	23.461312
118.188312	3208.317808	23.466330
118.669911	3217.381837	23.471347
118.955495	3220.680020	23.476365
119.156700	3214.540886	23.481383
119.220423	3224.266202	23.486400
118.986355	3240.241991	23.491418
119.397796	3242.840505	23.496435
119.359220	3246.989547	23.501453
119.372361	3241.423129	23.506471
119.383518	3247.441814	23.511488
120.109421	3260.211838	23.516506
120.055536	3264.266576	23.521523
120.143427	3270.470468	23.526541
120.584445	3255.227705	23.531559
120.412442	3267.867169	23.536576
120.647344	3260.932912	23.541594
120.814144	3275.057707	23.546611
120.779866	3282.501075	23.551629
121.037248	3289.311152	23.556647
120.991371	3291.039476	23.561664
121.099389	3287.585625	23.566682
121.439465	3286.778603	23.571699
121.271653	3285.711968	23.576717
121.370396	3285.280869	23.581735
121.525551	3302.340721	23.586752
121.615669	3308.849470	23.591770
121.815677	3309.434225	23.596787
121.481278	3325.422957	23.601805
121.764642	3334.545411	23.606823
122.220645	3340.734689	23.611840
122.294567	3343.589977	23.616858
122.628691	3340.773383	23.621875
122.413913	3343.446590	23.626893
123.194020	3330.502369	23.631911
123.216939	3329.732540	23.636928
123.222781	3327.870505	23.641946
122.965462	3325.130123	23.646963
123.324424	3344.745400	23.651981
124.023373	3343.227502	23.656999
123.905921	3344.304937	23.662016
123.826168	3352.003367	23.667034
124.092794	3347.269606	23.672051
124.168436	3346.294723	23.677069
124.559715	3341.466363	23.682087
124.382968	3335.544757	23.687104
123.939750	3317.823577	23.692122
124.535108	3323.716898	23.697139
124.233211	3338.257862	23.702157
124.264104	3360.954618	23.707175
124.550415	3350.912963	23.712192
124.341655	3343.237647	23.717210
124.872170	3339.511909	23.722227
124.788075	3361.143081	23.727245
124.735692	3366.597736	23.732263
124.675980	3373.350648	23.737280
124.952578	3371.896154	23.742298
125.315523	3387.938953	23.747315
125.115784	3414.400215	23.752333
125.469640	3409.891650	23.757351
125.526910	3411.012026	23.762368
125.834147	3425.654177	23.767386
125.790018	3432.086061	23.772403
125.994713	3431.708072	23.777421
126.194970	3439.280883	23.782439
126.077364	3449.168981	23.787456
126.480743	3455.436707	23.792474
127.126998	3451.652371	23.797491
126.815797	3456.990220	23.802509
126.929651	3467.992214	23.807527
127.168442	3455.183747	23.812544
127.168124	3454.073875	23.817562
127.275752	3473.283400	23.822579
127.627572	3473.094333	23.827597
127.878251	3476.597150	23.832615
127.994160	3479.584997	23.837632
127.746715	3471.675083	23.842650
127.792496	3473.043500	23.847667
127.747372	3483.433710	23.852685
127.852140	3494.718774	23.857703
128.119706	3503.283797	23.862720
128.127453	3508.341125	23.867738
128.364508	3499.391940	23.872755
128.631871	3522.974709	23.877773
129.118025	3530.100034	23.882791
129.206023	3531.247770	23.887808
128.653949	3532.557340	23.892826
129.180235	3526.684818	23.897843
129.300292	3533.194400	23.902861
129.354535	3547.484499	23.907879
129.360100	3559.527192	23.912896
129.512464	3568.573141	23.917914
129.820640	3556.065804	23.922931
129.813602	3568.816094	23.927949
129.786440	3586.313592	23.932967
130.115497	3588.752254	23.937984
130.110977	3595.235317	23.943002
130.151928	3600.244907	23.948019
130.500007	3614.315169	23.953037
131.042250	3617.375087	23.958055
131.185008	3621.366321	23.963072
131.097571	3621.086820	23.968090
131.411003	3617.783420	23.973107
131.436272	3617.134339	23.978125
131.387771	3605.670227	23.983143
131.622021	3610.785083	23.988160
131.511216	3606.684063	23.993178
132.079891	3604.027461	23.998195
132.047471	3614.779936	24.003213
132.050789	3608.161684	24.008231
132.166696	3613.609264	24.013248
132.242121	3633.808961	24.018266
132.451347	3625.355764	24.023283
132.100893	3637.434832	24.028301
132.226856	3627.646670	24.033319
132.722699	3640.951634	24.038336
132.715750	3657.244850	24.043354
133.167799	3643.740683	24.048371
133.400268	3647.882808	24.053389
133.274366	3643.360991	24.058407
133.703799	3649.415411	24.063424
133.533802	3649.184471	24.068442
133.782411	3666.875652	24.073459
133.736570	3669.767404	24.078477
133.899106	3674.443779	24.083495
134.440448	3669.083241	24.088512
133.837266	3670.563797	24.093530
134.157156	3680.777961	24.098547
134.343495	3693.521913	24.103565
134.752219	3705.214123	24.108583
135.262395	3700.496482	24.113600
134.953015	3709.174851	24.118618
135.299920	3684.590743	24.123635
135.278580	3701.846750	24.128653
135.038853	3706.739872	24.133671
135.461117	3701.598893	24.138688
135.742895	3715.625550	24.143706
135.641544	3707.001573	24.148723
135.816184	3730.118057	24.153741
135.692228	3723.871659	24.158759
135.832062	3722.492427	24.163776
136.096985	3744.894459	24.168794
136.211044	3734.758082	24.173811
135.969578	3769.254770	24.178829
136.345056	3749.192157	24.183847
136.332182	3785.494677	24.188864
136.966801	3782.254878	24.193882
136.955900	3775.112575	24.198899
137.374791	3776.318487	24.203917
137.285902	3797.848810	24.208935
137.542670	3806.865676	24.213952
137.494860	3810.287947	24.218970
138.074355	3796.180441	24.223987
137.957958	3816.480982	24.229005
138.006396	3816.279714	24.234023
138.153135	3795.861773	24.239040
137.872974	3799.487061	24.244058
138.234638	3826.108129	24.249075
138.309233	3836.540072	24.254093
138.408004	3837.310900	24.259111
138.707796	3826.503757	24.264128
138.595209	3832.448805	24.269146
138.721107	3866.901311	24.274163
139.092292	3843.548053	24.279181
139.274656	3868.455434	24.284199
139.645266	3855.784498	24.289216
139.580212	3853.457011	24.294234
139.595339	3870.628741	24.299251
140.082954	3871.925179	24.304269
140.106403	3860.550868	24.309287
140.154596	3888.919546	24.314304
140.153532	3892.617565	24.319322
140.379618	3881.930685	24.324339
140.443101	3892.036421	24.329357
140.393658	3916.320082	24.334375
140.957097	3926.560092	24.339392
140.945708	3932.416677	24.344410
141.078432	3916.073919	24.349427
141.280490	3914.823980	24.354445
141.280039	3921.272714	24.359463
141.709128	3931.566398	24.364480
141.640194	3931.439692	24.369498
142.078493	3943.718918	24.374515
142.407034	3940.857479	24.379533
141.948266	3935.564263	24.384551
142.195953	3932.611096	24.389568
142.330491	3933.137882	24.394586
142.534955	3942.956871	24.399603
142.624737	3956.127850	24.404621
142.669119	3960.849113	24.409639
142.890731	3967.980648	24.414656
142.911751	3971.320400	24.419674
142.807189	3973.682738	24.424691
143.135711	3979.434018	24.429709
143.125364	3997.198352	24.434727
143.541422	3992.918828	24.439744
143.703825	4014.978920	24.444762
143.987286	4015.448928	24.449779
144.190700	4029.315324	24.454797
144.190134	4022.451290	24.459815
144.493858	4009.384988	24.464832
144.202517	4026.251781	24.469850
144.580558	4032.991841	24.474867
144.563671	4037.369703	24.479885
144.562358	4027.960268	24.484903
144.784595	4031.698236	24.489920
145.081314	4072.157405	24.494938
145.086355	4062.927858	24.499955
145.469558	4061.850404	24.504973
145.686925	4058.258586	24.509991
145.475631	4086.245811	24.515008
145.742134	4098.930139	24.520026
145.899319	4090.894806	24.525043
146.437491	4084.282315	24.530061
146.217986	4097.737932	24.535079
146.455722	4089.031349	24.540096
146.537320	4096.216735	24.545114
146.912049	4110.436624	24.550131
147.226322	4115.725333	24.555149
147.053697	4120.673970	24.560167
147.197116	4122.464247	24.565184
146.989624	4126.298284	24.570202
147.123952	4123.471708	24.575219
147.406254	4128.161387	24.580237
147.175732	4152.176963	24.585255
147.568897	4145.821979	24.590272
147.659410	4155.438236	24.595290
147.729980	4164.621098	24.600307
148.099658	4180.370285	24.605325
148.432604	4183.117578	24.610343
148.572779	4200.858947	24.615360
148.573554	4205.449581	24.620378
148.465537	4204.457512	24.625395
149.354203	4189.103085	24.630413
149.094402	4207.208724	24.635431
149.581503	4222.825175	24.640448
149.696820	4231.643026	24.645466
149.915682	4234.378625	24.650483
150.292060	4231.404096	24.655501
150.016677	4225.298833	24.660519
150.360782	4229.536603	24.665536
150.426058	4235.708327	24.670554
150.398814	4225.126878	24.675571
150.294026	4226.597248	24.680589
150.593564	4248.093050	24.685607
150.653890	4232.340448	24.690624
151.040412	4247.102155	24.695642
150.751829	4259.768924	24.700659
151.008810	4268.506001	24.705677
151.189833	4277.081346	24.710695
151.814007	4276.290341	24.715712
151.800087	4273.721003	24.720730
151.833414	4303.780192	24.725747
152.171844	4293.329189	24.730765
152.231584	4295.629198	24.735783
152.364939	4293.059975	24.740800
152.224425	4309.423196	24.745818
152.477285	4302.339274	24.750835
152.862569	4315.306924	24.755853
152.907947	4329.560655	24.760871
153.348946	4320.642962	24.765888
153.581202	4317.806243	24.770906
153.467382	4326.826664	24.775923
153.650152	4321.727588	24.780941
153.475690	4329.447136	24.785959
153.921694	4336.245727	24.790976
154.227554	4338.368056	24.795994
153.836970	4351.084205	24.801011
154.292788	4336.884987	24.806029
154.054929	4352.381951	24.811047
154.275182	4362.829593	24.816064
154.740919	4367.932985	24.821082
154.707513	4385.077657	24.826099
155.212108	4374.221730	24.831117
154.870831	4385.791775	24.836135
154.820418	4389.470254	24.841152
155.264888	4401.052704	24.846170
155.326252	4407.025316	24.851187
155.191640	4410.762850	24.856205
155.806725	4438.486842	24.861223
156.024568	4435.424271	24.866240
156.220951	4430.547969	24.871258
156.444322	4436.277650	24.876275
156.868204	4434.921506	24.881293
156.970410	4455.033110	24.886311
157.186673	4455.594872	24.891328
157.582469	4448.978174	24.896346
157.433686	4447.210660	24.901363
157.650263	4441.166897	24.906381
157.440173	4446.459088	24.911399
157.323201	4457.798340	24.916416
157.798432	4450.986475	24.921434
157.456894	4476.429164	24.926451
157.845991	4476.286068	24.931469
158.119417	4468.711066	24.936487
157.950219	4491.742762	24.941504
158.521012	4490.957113	24.946522
158.575607	4505.961583	24.951539
158.760501	4508.690064	24.956557
158.895492	4523.269530	24.961575
159.179794	4521.289791	24.966592
159.679065	4524.658048	24.971610
159.103691	4527.966356	24.976627
159.950204	4537.353781	24.981645
159.925765	4553.173284	24.986663
160.069431	4555.836761	24.991680
160.020716	4554.488300	24.996698
160.140701	4545.213378	25.001715
160.387116	4558.952277	25.006733
160.617848	4576.836210	25.011751
160.972994	4580.328935	25.016768
161.003696	4575.135232	25.021786
160.634949	4579.257836	25.026803
161.124758	4585.933924	25.031821
161.735295	4598.520574	25.036839
161.753590	4607.221175	25.041856
161.838351	4599.819355	25.046874
161.706061	4598.803595	25.051891
162.054692	4601.136262	25.056909
162.374351	4628.973794	25.061927
162.714256	4623.685940	25.066944
162.967016	4625.367596	25.071962
162.865928	4628.573567	25.076979
162.930502	4627.235357	25.081997
163.151928	4623.667929	25.087015
162.878409	4622.054011	25.092032
162.878208	4613.409439	25.097050
162.784840	4628.215000	25.102067
163.274693	4639.742420	25.107085
163.457457	4651.838787	25.112103
163.749384	4665.296774	25.117120
164.544567	4662.992493	25.122138
164.228918	4685.969175	25.127155
164.334196	4678.138462	25.132173
164.571506	4673.805431	25.137191
164.731034	4692.907592	25.142208
165.159659	4702.800703	25.147226
164.880660	4698.446924	25.152243
165.058351	4705.970501	25.157261
165.203613	4712.357019	25.162279
165.223203	4717.869141	25.167296
165.612565	4724.717067	25.172314
165.200491	4733.157529	25.177331
165.395634	4746.120476	25.182349
166.064517	4758.621657	25.187367
165.879788	4769.610873	25.192384
166.489208	4782.698966	25.197402
166.537117	4794.352818	25.202419
166.877254	4789.955373	25.207437
167.060442	4802.644157	25.212455
167.408718	4823.929290	25.217472
167.480852	4808.687881	25.222490
167.602475	4820.240322	25.227507
167.964623	4820.509802	25.232525
168.230105	4810.287971	25.237543
168.075453	4812.488507	25.242560
168.316696	4825.505536	25.247578
168.271388	4838.609165	25.252595
168.504004	4840.172125	25.257613
168.881504	4840.484786	25.262631
168.733453	4843.717170	25.267648
169.159280	4854.190605	25.272666
168.880496	4867.892376	25.277683
168.879506	4866.574037	25.282701
169.236124	4872.775891	25.287719
169.334397	4887.826495	25.292736
169.572533	4911.685995	25.297754
169.632409	4908.886872	25.302771
169.677005	4918.204935	25.307789
170.162237	4926.964234	25.312807
170.284619	4938.596100	25.317824
170.630433	4942.779529	25.322842
170.838673	4951.854403	25.327859
170.807382	4953.528676	25.332877
171.291409	4967.799631	25.337895
171.465260	4967.667250	25.342912
171.743691	4977.077087	25.347930
171.507533	4976.460969	25.352947
171.855902	4969.420504	25.357965
172.004021	4970.262981	25.362983
171.798161	4996.089288	25.368000
172.534703	5001.776717	25.373018
172.572713	5012.491454	25.378035
172.651862	5003.792309	25.383053
172.857599	4994.591542	25.388071
173.163554	5021.164669	25.393088
173.003344	5031.777286	25.398106
173.119946	5033.776489	25.403123
173.386713	5031.433674	25.408141
173.782992	5045.007538	25.413159
173.672269	5059.120087	25.418176
174.001375	5051.844290	25.423194
173.758116	5069.338673	25.428211
174.201339	5080.459296	25.433229
174.349681	5071.157496	25.438247
174.603087	5086.610741	25.443264
175.099948	5088.815229	25.448282
175.171816	5109.545392	25.453299
175.464550	5108.333609	25.458317
175.687476	5106.205457	25.463335
175.350040	5116.780306	25.468352
175.991558	5120.545332	25.473370
176.160293	5133.078582	25.478387
176.448306	5139.023228	25.483405
176.164281	5133.663162	25.488423
176.641128	5139.222910	25.493440
176.752652	5134.206502	25.498458
176.656673	5148.048527	25.503475
176.706722	5166.277445	25.508493
176.916187	5168.604857	25.513511
176.999622	5179.168511	25.518528
177.577093	5181.883310	25.523546
177.763578	5192.052149	25.528563
177.654951	5195.626827	25.533581
178.118365	5204.379545	25.538599
178.256958	5220.892022	25.543616
178.555778	5231.317535	25.548634
178.570055	5230.167441	25.553651
178.617263	5240.438759	25.558669
179.407626	5243.123565	25.563687
178.794442	5255.760331	25.568704
179.157025	5244.382020	25.573722
179.214023	5258.213922	25.578739
179.331835	5278.010276	25.583757
179.470043	5282.846027	25.588775
179.739123	5300.320370	25.593792
180.052561	5299.637863	25.598810
180.113356	5300.360543	25.603827
180.263322	5320.494041	25.608845
180.797707	5322.289797	25.613863
180.814653	5333.038020	25.618880
181.132344	5324.690859	25.623898
181.385999	5326.296934	25.628915
181.073459	5333.466304	25.633933
181.812455	5350.232505	25.638951
181.705230	5354.131116	25.643968
182.183346	5349.214320	25.648986
181.851235	5363.960343	25.654003
182.075690	5364.437448	25.659021
182.310033	5378.138921	25.664039
182.282023	5379.742702	25.669056
182.665234	5382.499523	25.674074
182.936516	5399.099612	25.679092
182.953505	5413.464339	25.684109
183.342609	5401.162816	25.689127
183.575967	5416.360781	25.694144
183.566695	5434.948782	25.699162
184.211023	5427.161545	25.704180
184.338516	5431.069960	25.709197
184.744308	5427.829325	25.714215
184.579474	5433.163427	25.719232
184.856690	5439.553616	25.724250
185.321658	5450.897626	25.729268
185.128709	5458.358738	25.734285
185.120652	5457.935951	25.739303
185.161116	5464.939759	25.744320
185.361039	5471.933883	25.749338
185.543370	5485.963148	25.754356
185.670542	5481.775673	25.759373
186.228218	5492.466134	25.764391
185.963703	5522.511574	25.769408
186.226264	5519.223737	25.774426
186.728718	5516.701669	25.779444
186.923549	5542.454829	25.784461
186.980543	5536.676006	25.789479
187.145184	5556.663521	25.794496
187.349540	5552.040473	25.799514
187.430110	5566.956922	25.804532
187.462668	5571.222727	25.809549
187.704684	5576.993155	25.814567
187.848373	5601.745225	25.819584
188.067229	5608.268305	25.824602
188.818547	5602.747738	25.829620
188.823307	5633.189461	25.834637
188.930996	5622.961542	25.839655
189.152783	5626.272813	25.844672
189.254635	5629.794374	25.849690
189.552752	5647.455673	25.854708
189.579553	5667.803597	25.859725
190.243032	5650.667051	25.864743
190.104055	5656.058475	25.869760
190.095890	5653.347943	25.874778
190.494228	5662.654929	25.879796
190.781689	5678.070327	25.884813
190.959289	5674.750370	25.889831
191.015619	5684.697992	25.894848
190.780192	5682.921323	25.899866
191.044090	5693.565932	25.904884
191.045290	5718.363728	25.909901
191.478946	5706.050917	25.914919
191.558350	5720.285626	25.919936
191.779225	5732.343768	25.924954
192.218307	5722.852816	25.929972
192.187469	5743.455488	25.934989
192.278170	5756.517797	25.940007
192.923551	5755.784717	25.945024
192.882841	5757.004286	25.950042
193.389658	5757.723546	25.955060
193.219683	5778.188744	25.960077
193.704722	5791.057626	25.965095
193.821559	5779.238970	25.970112
193.617329	5787.829412	25.975130
193.941914	5814.462370	25.980148
194.039565	5820.674444	25.985165
194.216594	5824.359506	25.990183
194.527802	5844.280777	25.995200
195.046556	5846.546408	26.000218
195.252325	5848.387540	26.005236
195.108293	5872.469227	26.010253
195.485764	5868.037195	26.015271
195.709236	5870.040719	26.020288
195.609108	5882.791336	26.025306
196.311333	5896.528849	26.030324
196.040257	5904.596616	26.035341
196.434583	5894.254372	26.040359
196.460151	5917.700172	26.045376
196.882606	5928.518718	26.050394
197.073441	5924.781991	26.055412
196.917651	5940.920520	26.060429
197.601293	5943.576061	26.065447
197.682607	5963.508179	26.070464
197.229806	5966.045141	26.075482
197.823873	5971.961795	26.080500
197.921497	5984.352123	26.085517
198.338589	5992.264606	26.090535
198.431945	6008.671104	26.095552
198.671946	6010.166931	26.100570
199.248814	6027.434157	26.105588
199.151853	6043.968587	26.110605
199.655841	6031.840979	26.115623
200.058472	6027.330150	26.120640
200.045511	6041.695543	26.125658
200.396406	6043.209099	26.130676
200.123892	6064.483278	26.135693
200.404667	6065.532041	26.140711
200.524234	6047.132497	26.145728
200.392702	6091.514198	26.150746
200.883013	6086.624329	26.155764
200.516494	6093.331414	26.160781
201.101820	6127.233718	26.165799
201.667534	6114.809831	26.170816
201.690030	6128.193316	26.175834
201.940754	6146.569259	26.180852
202.315750	6156.956540	26.185869
202.235979	6156.029065	26.190887
202.436194	6149.130459	26.195904
202.631001	6159.013843	26.200922
203.305800	6171.435054	26.205940
203.262698	6178.727880	26.210957
203.342982	6173.242484	26.215975
203.878334	6170.038472	26.220992
203.772712	6184.971852	26.226010
204.158538	6189.997372	26.231028
204.124087	6197.675118	26.236045
204.137384	6210.278910	26.241063
204.755564	6200.560060	26.246080
204.812516	6216.935616	26.251098
205.275452	6214.297791	26.256116
205.273852	6228.623005	26.261133
205.475163	6236.016938	26.266151
205.674322	6228.272716	26.271168
205.557876	6251.018668	26.276186
205.935292	6258.982466	26.281204
206.177314	6262.344942	26.286221
206.455888	6270.428352	26.291239
206.642627	6272.918489	26.296256
206.695105	6281.355005	26.301274
207.182934	6281.488051	26.306292
206.654627	6303.929967	26.311309
207.246060	6311.451357	26.316327
207.717536	6316.738629	26.321344
207.485154	6333.607308	26.326362
207.847711	6330.974450	26.331380
208.132832	6349.995805	26.336397
208.322372	6370.325051	26.341415
208.518145	6367.718773	26.346432
208.899952	6381.308773	26.351450
209.372182	6391.596538	26.356468
209.356658	6398.806402	26.361485
209.621003	6408.833859	26.366503
210.082665	6404.471646	26.371520
209.995742	6419.279549	26.376538
210.175696	6421.018657	26.381556
210.609893	6421.474957	26.386573
210.633473	6429.540882	26.391591
210.490133	6428.017724	26.396608
210.654469	6452.196749	26.401626
211.135068	6452.266437	26.406644
211.119731	6470.232812	26.411661
211.159712	6490.247759	26.416679
211.675173	6490.245016	26.421696
212.066627	6506.405500	26.426714
212.073113	6503.572889	26.431732
212.452568	6517.061898	26.436749
212.511437	6528.086756	26.441767
212.845072	6528.817146	26.446784
212.969465	6541.147028	26.451802
213.323300	6538.259829	26.456820
213.463328	6546.528335	26.461837
213.490177	6554.548963	26.466855
213.664927	6555.594209	26.471872
213.936397	6572.012279	26.476890
214.134054	6591.097454	26.481908
214.373579	6587.226132	26.486925
214.666377	6587.279340	26.491943
214.812697	6601.962915	26.496960
214.690068	6619.345488	26.501978
215.173984	6604.600695	26.506996
215.294895	6620.983813	26.512013
215.609776	6635.420258	26.517031
215.812220	6644.803157	26.522048
216.338092	6659.722111	26.527066
216.415176	6665.229731	26.532084
216.452249	6666.348071	26.537101
216.590749	6676.936280	26.542119
217.124968	6693.933362	26.547136
216.792754	6718.515335	26.552154
217.426675	6715.704618	26.557172
217.609486	6726.625683	26.562189
217.598372	6729.605336	26.567207
217.976957	6730.945400	26.572224
218.180422	6757.187889	26.577242
217.990300	6772.559400	26.582260
218.677962	6793.828697	26.587277
219.107123	6786.012118	26.592295
219.284091	6792.295356	26.597312
219.047559	6803.153504	26.602330
219.656954	6824.027772	26.607348
220.047048	6818.978980	26.612365
220.175133	6857.622206	26.617383
220.409169	6853.496776	26.622400
220.587322	6854.307043	26.627418
221.091210	6860.857630	26.632436
221.437385	6875.743293	26.637453
221.067581	6878.753401	26.642471
221.611336	6871.517249	26.647488
221.570905	6884.567628	26.652506
221.537781	6909.855188	26.657524
221.861638	6889.861852	26.662541
221.965606	6919.658629	26.667559
222.426378	6935.114596	26.672576
222.542569	6937.805706	26.677594
222.562102	6953.233678	26.682612
223.013345	6958.594434	26.687629
223.411403	6968.484516	26.692647
223.952813	6978.309269	26.697664
224.100671	6982.092901	26.702682
224.264659	6988.424712	26.707700
224.779256	6982.451220	26.712717
224.725770	7006.693410	26.717735
225.193145	7009.705426	26.722752
225.233765	7015.267769	26.727770
225.182813	7008.681816	26.732788
225.363207	7007.333587	26.737805
225.254216	7013.852903	26.742823
225.819028	7027.489075	26.747840
225.874013	7035.820980	26.752858
226.256144	7047.772671	26.757876
226.705646	7053.338305	26.762893
226.560234	7059.835122	26.767911
226.542416	7069.291953	26.772928
226.650211	7071.214949	26.777946
226.869964	7091.202053	26.782964
226.862279	7096.348048	26.787981
226.914961	7130.251804	26.792999
227.311963	7131.943813	26.798016
227.707623	7160.208332	26.803034
227.701336	7179.182004	26.808052
228.179608	7180.422822	26.813069
228.428765	7208.615583	26.818087
228.679888	7224.014789	26.823104
229.072149	7231.673049	26.828122
229.232333	7248.687119	26.833140
229.892268	7261.760735	26.838157
230.039842	7277.027011	26.843175
230.360386	7266.990629	26.848192
230.648939	7301.747048	26.853210
230.818225	7297.612148	26.858228
231.274993	7305.688182	26.863245
231.202010	7312.850213	26.868263
231.551078	7319.714441	26.873280
231.633026	7317.868096	26.878298
232.019142	7325.036420	26.883316
232.323113	7357.294781	26.888333
232.482399	7358.499125	26.893351
232.855557	7339.911211	26.898368
233.247034	7361.044429	26.903386
233.174874	7369.412523	26.908404
233.570374	7380.770679	26.913421
233.350184	7396.274302	26.918439
233.350060	7402.230393	26.923456
233.912894	7410.332066	26.928474
233.489657	7409.594588	26.933492
234.203845	7438.649175	26.938509
234.602708	7426.514379	26.943527
235.092093	7472.298534	26.948544
235.240810	7458.850274	26.953562
235.003195	7476.213623	26.958580
235.621789	7461.183727	26.963597
235.641923	7516.193391	26.968615
236.025067	7481.260875	26.973632
236.515641	7531.386635	26.978650
236.529760	7516.988851	26.983668
236.830683	7515.850328	26.988685
236.699196	7563.801467	26.993703
237.061105	7530.376608	26.998720
237.299470	7568.815276	27.003738
237.406534	7563.272383	27.008756
238.176924	7564.868736	27.013773
238.394117	7581.405161	27.018791
238.736791	7570.997606	27.023808
238.899453	7587.955808	27.028826
239.017172	7609.212483	27.033844
239.107811	7600.338457	27.038861
239.367763	7607.302001	27.043879
239.436699	7609.228901	27.048896
239.608223	7643.434334	27.053914
239.751958	7635.089220	27.058932
239.667622	7645.949687	27.063949
240.184275	7673.760791	27.068967
240.259997	7692.397879	27.073984
240.838278	7691.861900	27.079002
241.226382	7721.825080	27.084020
241.528908	7729.316147	27.089037
241.258060	7731.990413	27.094055
241.704121	7745.302338	27.099072
241.808247	7749.124612	27.104090
241.969383	7765.947926	27.109108
242.627148	7764.006599	27.114125
242.591880	7794.992612	27.119143
242.841714	7811.162938	27.124160
243.283933	7826.624372	27.129178
243.296707	7849.847090	27.134196
243.902805	7847.676366	27.139213
244.146343	7856.211579	27.144231
244.452660	7876.373210	27.149248
244.483821	7891.368334	27.154266
244.874150	7888.531717	27.159284
245.038923	7909.667232	27.164301
245.308560	7903.201312	27.169319
245.583977	7918.654022	27.174336
245.966841	7933.267382	27.179354
246.003862	7963.922771	27.184372
246.412253	7952.131452	27.189389
246.366091	7951.771320	27.194407
246.718315	7988.272265	27.199424
247.228810	7966.563124	27.204442
246.878790	7997.153592	27.209460
247.230057	8011.795670	27.214477
247.691163	8014.614549	27.219495
247.720849	8040.435365	27.224512
247.906586	8048.217456	27.229530
248.318440	8066.769963	27.234548
248.951503	8069.176680	27.239565
248.977814	8097.657653	27.244583
249.447595	8089.796943	27.249600
249.847427	8095.896503	27.254618
250.058767	8125.013310	27.259636
250.112927	8114.980265	27.264653
250.129795	8124.640752	27.269671
250.187700	8134.699928	27.274688
250.635656	8167.276230	27.279706
250.935466	8159.284420	27.284724
251.163451	8168.092967	27.289741
251.104594	8191.872919	27.294759
251.240111	8193.543788	27.299776
251.886340	8207.927386	27.304794
251.857767	8241.037748	27.309812
252.234879	8237.401374	27.314829
252.544498	8253.817593	27.319847
252.609812	8267.377159	27.324864
253.206389	8279.697751	27.329882
253.303631	8291.510162	27.334900
253.607757	8288.030977	27.339917
254.342286	8306.072047	27.344935
254.503169	8314.716695	27.349952
254.721987	8312.883821	27.354970
254.547767	8327.397517	27.359988
254.975342	8327.071241	27.365005
255.277044	8339.541960	27.370023
255.472082	8346.745961	27.375040
255.497744	8388.484524	27.380058
255.559611	8387.636623	27.385076
256.018338	8391.652765	27.390093
256.371382	8424.500488	27.395111
256.369797	8427.763805	27.400128
256.865106	8435.255979	27.405146
256.719561	8459.081648	27.410164
257.235173	8467.717845	27.415181
257.601222	8478.413496	27.420199
257.757749	8493.663073	27.425216
258.381007	8510.995854	27.430234
258.484295	8528.378482	27.435252
258.761294	8519.390799	27.440269
258.903896	8552.060679	27.445287
258.840260	8564.671650	27.450304
259.555041	8568.505394	27.455322
259.821393	8591.604657	27.460340
260.105290	8597.938506	27.465357
260.551401	8599.005962	27.470375
260.656732	8620.659492	27.475392
261.076334	8625.081664	27.480410
261.172452	8636.152511	27.485428
261.337282	8637.602369	27.490445
262.109135	8665.424233	27.495463
262.194049	8659.113331	27.500480
262.763084	8655.557218	27.505498
262.659233	8666.513601	27.510516
262.939826	8696.270051	27.515533
263.085205	8686.698928	27.520551
263.267308	8687.751029	27.525568
263.650634	8701.745805	27.530586
263.348936	8731.458217	27.535604
263.740348	8711.114109	27.540621
264.168396	8737.113424	27.545639
264.292587	8758.420284	27.550656
264.629659	8777.464808	27.555674
264.781553	8785.022124	27.560692
264.581681	8800.341409	27.565709
265.336772	8792.233421	27.570727
265.084487	8821.927907	27.575744
265.709991	8850.638225	27.580762
265.820246	8856.248389	27.585780
266.148811	8866.098889	27.590797
266.542909	8878.512843	27.595815
266.822966	8917.684874	27.600832
267.475374	8915.462561	27.605850
267.665340	8910.746349	27.610868
267.598514	8931.865934	27.615885
267.996928	8951.245559	27.620903
268.351582	8953.482770	27.625920
268.803256	8968.254972	27.630938
268.834529	8990.454744	27.635956
268.954629	8988.515557	27.640973
269.424394	9001.650148	27.645991
269.286873	9028.026145	27.651008
269.911059	9041.585868	27.656026
269.982671	9052.983162	27.661044
270.239820	9069.198938	27.666061
270.958631	9080.521824	27.671079
270.906786	9098.576275	27.676096
271.370079	9114.165140	27.681114
271.567114	9131.881338	27.686132
271.683405	9135.716588	27.691149
272.083197	9167.755079	27.696167
272.271178	9167.283238	27.701184
272.718412	9176.532333	27.706202
272.754060	9197.015097	27.711220
272.882040	9227.320612	27.716237
273.418113	9230.826157	27.721255
273.617216	9249.095750	27.726272
273.910907	9257.818930	27.731290
274.109378	9273.365183	27.736308
274.242369	9293.627577	27.741325
274.929130	9303.229274	27.746343
274.945569	9323.363132	27.751360
275.737651	9336.617802	27.756378
275.893037	9348.723170	27.761396
275.685688	9381.482902	27.766413
276.258524	9364.895602	27.771431
276.451872	9402.936199	27.776448
276.845538	9406.235887	27.781466
277.224738	9425.318593	27.786484
277.015571	9438.739619	27.791501
277.606160	9444.352141	27.796519
277.589896	9474.766527	27.801536
277.822293	9459.781634	27.806554
278.334938	9492.679851	27.811572
278.439214	9511.047503	27.816589
279.092902	9525.385162	27.821607
279.393257	9531.394546	27.826624
279.626140	9526.724419	27.831642
279.795294	9552.339909	27.836660
279.850707	9553.925729	27.841677
280.416188	9562.010467	27.846695
280.523362	9583.353873	27.851712
280.860351	9580.499086	27.856730
281.061759	9611.248909	27.861748
280.909021	9629.981487	27.866765
281.560076	9633.599828	27.871783
281.709634	9652.092246	27.876800
281.970624	9669.889386	27.881818
282.440660	9687.597359	27.886836
282.486650	9710.826333	27.891853
283.150999	9706.588265	27.896871
283.028419	9743.443818	27.901888
283.315207	9765.113761	27.906906
283.634854	9771.363329	27.911924
283.946411	9792.326242	27.916941
284.494022	9805.421596	27.921959
284.505308	9817.412990	27.926976
285.263191	9821.206758	27.931994
285.474650	9850.241532	27.937012
285.445779	9860.480957	27.942029
285.928114	9869.392018	27.947047
285.937178	9884.749540	27.952064
286.627502	9895.185995	27.957082
287.057541	9909.700138	27.962100
287.356768	9938.310707	27.967117
288.007942	9927.070930	27.972135
288.057866	9938.205977	27.977152
288.285956	9959.232791	27.982170
288.315128	9962.534430	27.987188
288.432575	9979.369960	27.992205
289.088805	9983.798114	27.997223
289.309820	9990.997986	28.002240
289.274378	10019.785598	28.007258
289.749891	10012.052828	28.012276
290.059419	10039.795920	28.017293
290.061507	10054.677839	28.022311
290.305220	10079.040157	28.027328
290.648558	10082.560888	28.032346
290.915647	10104.647609	28.037364
291.329834	10122.335489	28.042381
291.559006	10133.139925	28.047399
291.711550	10154.491866	28.052416
292.044836	10180.611496	28.057434
292.603186	10193.445787	28.062452
292.800286	10209.888785	28.067469
293.092010	10219.205418	28.072487
293.293497	10232.683683	28.077504
293.724956	10248.762394	28.082522
293.799929	10272.272496	28.087540
294.082398	10287.022609	28.092557
294.912649	10302.770258	28.097575
294.789523	10317.119949	28.102592
294.666598	10334.846068	28.107610
295.046533	10352.898140	28.112628
295.107925	10371.210724	28.117645
295.476283	10382.256790	28.122663
296.076012	10402.383736	28.127680
296.246601	10406.221678	28.132698
296.843726	10421.707167	28.137716
296.881805	10442.203049	28.142733
297.654434	10453.224482	28.147751
297.892608	10461.454738	28.152768
298.048232	10480.607476	28.157786
298.239622	10478.709858	28.162804
298.646311	10510.251584	28.167821
298.912675	10521.188487	28.172839
299.080134	10535.913104	28.177856
299.036613	10548.707475	28.182874
299.628663	10574.356081	28.187892
299.574451	10604.575763	28.192909
300.389861	10617.088504	28.197927
300.426627	10628.527570	28.202944
300.825657	10649.589888	28.207962
301.460789	10651.709869	28.212980
301.621157	10677.185059	28.217997
302.416036	10698.728949	28.223015
302.617101	10714.098036	28.228032
302.865559	10717.807570	28.233050
303.181420	10726.185742	28.238068
303.477920	10750.397507	28.243085
303.708992	10742.399155	28.248103
303.912071	10759.629963	28.253120
304.154437	10779.938714	28.258138
304.642865	10787.092419	28.263156
304.559841	10808.181023	28.268173
304.598897	10816.153204	28.273191
305.277134	10842.601883	28.278208
305.272362	10865.424417	28.283226
305.657168	10879.827878	28.288244
305.699915	10905.531537	28.293261
305.871266	10910.691630	28.298279
306.531100	10946.620745	28.303296
306.490438	10978.402768	28.308314
306.931265	10982.812434	28.313332
307.187882	11010.999388	28.318349
307.396548	11022.229563	28.323367
307.900383	11067.434956	28.328384
308.239274	11077.765343	28.333402
309.006328	11094.885410	28.338420
309.095093	11117.156292	28.343437
309.366919	11130.898818	28.348455
309.824405	11153.048426	28.353472
310.103496	11175.426788	28.358490
310.677184	11186.011811	28.363508
310.678087	11197.782057	28.368525
310.958846	11223.775330	28.373543
311.319302	11232.133693	28.378560
311.398039	11256.096867	28.383578
312.119741	11259.711444	28.388596
312.094900	11277.343159	28.393613
312.410579	11289.714956	28.398631
312.997070	11294.420634	28.403648
312.885285	11323.479469	28.408666
313.508736	11329.887476	28.413684
313.625115	11343.468447	28.418701
314.177536	11354.382802	28.423719
314.570621	11382.063510	28.428736
314.486318	11389.123435	28.433754
314.977844	11418.650401	28.438772
315.060956	11429.852488	28.443789
315.304598	11449.489041	28.448807
315.946256	11460.246408	28.453824
316.139069	11484.468796	28.458842
316.487017	11494.614260	28.463860
316.701198	11515.927617	28.468877
316.956649	11544.685559	28.473895
317.157478	11566.586660	28.478912
317.343394	11580.392083	28.483930
318.334884	11598.829463	28.488948
318.398842	11624.323586	28.493965
318.749952	11646.875731	28.498983
319.366509	11655.177779	28.504000
319.294264	11675.882987	28.509018
319.573216	11692.366507	28.514036
319.668331	11714.851331	28.519053
319.995996	11737.327857	28.524071
320.466026	11765.083187	28.529088
320.470164	11790.368328	28.534106
321.175484	11812.742677	28.539124
321.290399	11839.605176	28.544141
321.752770	11856.873049	28.549159
322.478513	11869.187848	28.554176
322.657126	11895.298117	28.559194
322.869951	11905.178122	28.564212
323.407061	11920.936027	28.569229
324.025251	11930.481888	28.574247
324.651135	11948.017771	28.579264
325.025212	11956.668723	28.584282
325.535895	11956.006073	28.589300
325.550296	11953.464737	28.594317
325.747636	11984.357401	28.599335
326.204094	11986.055868	28.604352
326.415038	12000.021000	28.609370
326.359431	12017.612045	28.614388
326.665134	12034.103089	28.619405
326.706915	12042.870402	28.624423
327.212632	12064.474540	28.629440
327.267794	12081.205864	28.634458
327.985750	12099.225454	28.639476
328.340783	12114.647781	28.644493
328.227012	12138.104688	28.649511
328.875675	12159.219067	28.654528
328.937235	12167.484308	28.659546
329.240110	12177.221458	28.664564
329.585721	12202.011727	28.669581
329.994639	12218.057185	28.674599
330.150977	12243.558095	28.679616
330.372488	12266.079085	28.684634
330.821469	12274.219486	28.689652
331.125411	12297.080974	28.694669
331.390369	12317.620381	28.699687
331.835065	12328.575243	28.704704
332.217585	12356.388896	28.709722
332.692386	12376.986048	28.714740
333.144652	12387.529882	28.719757
333.178258	12407.459113	28.724775
333.632761	12420.754791	28.729792
333.936145	12438.332407	28.734810
334.611484	12453.451783	28.739828
335.020646	12459.329312	28.744845
335.152455	12490.082335	28.749863
335.299199	12494.522788	28.754880
335.659394	12508.293419	28.759898
336.140582	12537.651464	28.764916
336.338754	12551.348387	28.769933
336.255705	12565.082463	28.774951
336.862541	12596.837512	28.779968
337.167460	12620.696757	28.784986
337.548352	12626.445841	28.790004
337.739164	12681.993467	28.795021
337.983395	12684.846247	28.800039
338.443983	12702.454215	28.805056
338.559060	12720.503129	28.810074
339.197379	12767.193941	28.815092
339.363012	12781.086142	28.820109
339.903349	12809.251708	28.825127
340.361327	12825.914747	28.830144
340.513726	12847.582999	28.835162
340.829702	12871.892864	28.840180
341.380247	12893.196281	28.845197
341.545188	12940.067152	28.850215
342.308249	12931.618258	28.855232
342.416662	12963.453304	28.860250
342.953165	12981.485748	28.865268
343.244861	13003.300071	28.870285
343.498546	13024.997695	28.875303
343.847411	13035.095646	28.880320
344.248035	13052.727746	28.885338
344.710907	13073.049312	28.890356
345.024123	13089.278993	28.895373
345.447183	13097.480054	28.900391
345.831921	13104.806851	28.905408
345.995811	13127.493758	28.910426
346.594591	13137.145219	28.915444
346.938822	13161.645856	28.920461
347.174435	13181.266459	28.925479
347.746942	13185.299438	28.930496
347.559129	13212.860401	28.935514
348.409918	13221.353868	28.940532
348.640837	13223.531959	28.945549
348.601219	13251.266547	28.950567
348.833578	13251.262935	28.955584
348.852251	13282.774100	28.960602
349.047713	13317.800746	28.965620
349.604052	13327.925261	28.970637
349.960926	13345.562903	28.975655
350.375787	13377.263402	28.980672
350.578736	13404.633161	28.985690
350.803688	13429.365365	28.990708
351.726279	13439.618143	28.995725
351.617624	13457.752976	29.000743
352.278242	13486.725146	29.005760
352.724979	13519.259739	29.010778
352.860960	13530.215671	29.015796
353.125548	13558.756770	29.020813
353.233019	13588.350554	29.025831
353.934678	13607.955891	29.030848
354.275627	13617.813452	29.035866
354.371800	13649.790815	29.040884
355.412507	13675.146718	29.045901
355.551860	13680.997273	29.050919
355.916397	13709.155334	29.055936
356.276486	13755.105406	29.060954
356.935475	13752.198352	29.065972
357.577240	13758.201283	29.070989
357.458147	13772.494957	29.076007
358.192843	13793.657740	29.081024
358.637974	13812.695367	29.086042
358.504172	13829.624422	29.091060
359.216297	13850.610232	29.096077
359.283625	13862.441625	29.101095
359.626573	13879.115102	29.106112
360.251617	13889.596251	29.111130
360.348013	13923.701114	29.116148
360.783639	13923.994242	29.121165
361.101077	13957.220237	29.126183
361.483474	13969.394787	29.131200
361.908010	13990.179649	29.136218
362.097880	14016.518574	29.141236
363.025706	14025.105508	29.146253
363.047684	14045.475805	29.151271
363.360264	14063.966644	29.156288
363.845485	14078.781343	29.161306
364.194782	14088.310720	29.166324
364.723522	14107.194200	29.171341
364.527769	14125.873657	29.176359
364.804609	14150.625235	29.181376
365.504882	14176.112975	29.186394
365.547539	14200.767640	29.191412
366.082246	14208.162292	29.196429
366.151524	14233.010345	29.201447
366.467346	14252.741365	29.206464
366.727659	14264.470392	29.211482
367.301610	14298.379589	29.216500
367.645566	14307.419454	29.221517
367.477206	14350.907768	29.226535
368.212886	14363.300376	29.231552
368.844876	14387.883973	29.236570
368.930514	14408.825345	29.241588
369.398444	14431.448729	29.246605
369.614047	14460.573960	29.251623
369.645924	14479.458257	29.256640
370.305245	14501.943406	29.261658
370.507152	14533.400900	29.266676
371.348148	14568.019089	29.271693
371.588876	14568.907104	29.276711
371.768600	14609.414944	29.281728
372.427396	14604.465034	29.286746
372.701039	14670.934955	29.291764
373.402311	14651.989616	29.296781
373.746260	14695.454841	29.301799
373.946264	14710.153639	29.306816
374.497322	14728.445325	29.311834
374.623216	14762.092072	29.316852
375.538965	14763.322226	29.321869
375.743348	14793.498219	29.326887
375.953128	14813.042093	29.331904
376.655501	14836.671262	29.336922
376.398979	14850.369303	29.341940
377.413792	14898.037901	29.346957
377.578740	14898.309436	29.351975
377.823272	14913.103375	29.356992
378.266814	14943.251791	29.362010
378.096305	14980.150632	29.367028
379.053712	14996.908193	29.372045
379.158579	15014.521015	29.377063
379.454922	15052.762215	29.382080
380.126624	15073.762065	29.387098
380.337028	15086.229811	29.392116
381.060936	15103.060782	29.397133
381.128383	15124.557865	29.402151
381.835683	15145.678391	29.407168
381.905066	15180.209256	29.412186
382.563247	15197.150804	29.417204
382.895833	15212.426651	29.422221
383.091349	15242.546492	29.427239
383.366643	15269.706054	29.432256
384.247613	15283.192835	29.437274
384.533817	15317.163898	29.442292
384.827385	15330.150849	29.447309
385.012914	15358.212262	29.452327
385.349096	15372.961638	29.457344
385.643499	15405.568420	29.462362
385.986149	15433.860882	29.467380
386.687371	15440.893367	29.472397
386.749108	15468.591032	29.477415
387.249968	15490.554098	29.482432
387.853335	15529.173461	29.487450
387.846043	15527.572772	29.492468
387.900291	15544.507510	29.497485
388.584217	15588.817760	29.502503
388.799012	15595.883341	29.507520
389.316260	15616.368706	29.512538
389.541614	15654.113773	29.517556
390.384750	15681.998774	29.522573
390.332012	15708.720833	29.527591
390.661501	15727.492924	29.532608
391.261455	15754.111168	29.537626
391.516059	15794.222102	29.542644
391.702899	15812.941648	29.547661
392.181191	15835.963711	29.552679
392.537053	15877.432076	29.557696
393.350935	15891.937076	29.562714
394.011455	15916.480611	29.567732
394.679066	15935.199676	29.572749
394.917890	15946.410295	29.577767
395.264906	15990.237400	29.582784
396.066326	15995.398235	29.587802
395.923943	16019.133915	29.592820
396.161000	16039.166353	29.597837
396.572329	16069.086634	29.602855
397.150536	16090.618042	29.607872
397.686785	16094.650017	29.612890
398.000680	16139.535388	29.617908
398.434575	16145.101619	29.622925
398.900905	16162.946996	29.627943
399.045976	16195.834324	29.632960
399.562346	16225.084647	29.637978
400.039294	16228.076389	29.642996
400.031003	16245.187288	29.648013
400.504426	16279.320680	29.653031
400.904309	16321.692131	29.658048
401.818354	16339.303416	29.663066
401.674960	16376.845768	29.668084
402.321325	16395.877197	29.673101
402.678787	16411.625300	29.678119
402.939945	16443.072452	29.683136
403.489985	16470.469948	29.688154
403.836947	16495.990306	29.693172
404.211395	16524.091161	29.698189
404.565299	16540.323943	29.703207
405.028559	16568.999026	29.708224
405.597342	16598.726086	29.713242
405.828122	16609.871258	29.718260
406.025794	16663.808689	29.723277
406.780310	16671.344406	29.728295
406.699184	16702.987153	29.733312
407.740516	16716.994369	29.738330
407.961365	16750.562639	29.743348
408.302286	16771.741920	29.748365
408.512235	16797.256856	29.753383
409.049829	16807.923822	29.758400
409.275781	16828.850276	29.763418
409.286382	16868.935476	29.768436
410.082252	16887.554577	29.773453
410.561266	16908.361698	29.778471
410.963240	16942.701425	29.783488
411.440102	16955.717633	29.788506
411.835854	16977.374424	29.793524
412.082751	17010.802514	29.798541
412.821449	17026.386585	29.803559
413.176337	17060.824028	29.808576
413.838423	17061.038546	29.813594
413.652577	17094.086996	29.818612
414.337226	17125.232863	29.823629
415.108158	17143.598799	29.828647
415.218849	17168.407018	29.833664
415.838447	17178.956663	29.838682
416.084927	17214.257294	29.843700
416.273002	17237.307622	29.848717
416.525570	17256.014124	29.853735
417.202510	17280.435885	29.858752
417.785628	17309.414676	29.863770
417.980010	17336.426922	29.868788
418.649554	17349.952673	29.873805
419.796389	17359.060317	29.878823
419.684128	17394.866697	29.883840
420.140845	17407.739860	29.888858
420.929187	17442.781868	29.893876
421.066625	17456.561172	29.898893
421.621732	17477.632900	29.903911
421.817936	17490.835996	29.908928
421.829397	17509.965238	29.913946
422.425355	17535.493710	29.918964
422.930121	17562.816124	29.923981
423.270314	17596.218022	29.928999
423.275732	17628.188019	29.934016
424.394628	17636.689310	29.939034
424.514549	17674.557990	29.944052
424.691212	17698.945561	29.949069
425.170221	17721.073757	29.954087
425.482441	17758.779734	29.959104
426.037307	17777.788879	29.964122
426.475692	17809.872543	29.969140
426.510451	17837.935235	29.974157
427.099241	17869.444903	29.979175
427.770034	17905.724718	29.984192
428.287410	17928.717121	29.989210
428.920541	17960.634452	29.994228
429.081779	17997.345442	29.999245
429.758069	18008.110238	30.004263
429.807839	18045.379620	30.009280
430.490760	18076.822159	30.014298
430.803896	18086.128020	30.019316
430.866449	18137.205074	30.024333
431.741976	18147.152440	30.029351
432.001640	18171.131489	30.034368
432.781493	18195.803651	30.039386
433.187158	18214.831396	30.044404
433.313435	18229.568044	30.049421
433.581107	18274.594250	30.054439
434.231783	18291.028441	30.059456
434.620735	18302.211252	30.064474
434.927231	18336.338985	30.069492
435.232079	18354.534966	30.074509
436.145398	18374.849699	30.079527
436.034403	18408.720886	30.084544
436.663447	18430.917141	30.089562
437.261433	18457.166282	30.094580
437.213869	18505.521230	30.099597
437.735774	18516.796006	30.104615
438.191454	18548.543023	30.109632
438.749723	18579.684406	30.114650
439.054351	18612.974088	30.119668
439.305990	18646.676214	30.124685
439.993709	18669.699275	30.129703
439.979260	18719.490140	30.134720
440.914619	18751.930044	30.139738
441.201068	18761.160250	30.144756
441.788807	18806.656689	30.149773
442.510324	18833.789539	30.154791
442.505027	18861.111451	30.159808
443.367113	18896.460562	30.164826
443.905199	18922.581847	30.169844
444.270085	18949.381556	30.174861
444.819153	18972.386606	30.179879
445.409610	19008.875312	30.184896
445.585770	19025.470920	30.189914
446.038361	19049.654060	30.194932
446.321601	19085.884012	30.199949
446.892515	19123.728871	30.204967
447.157257	19152.350812	30.209984
447.883950	19190.121409	30.215002
448.311723	19211.367368	30.220020
448.583485	19242.876203	30.225037
449.420646	19265.668468	30.230055
449.588144	19306.458021	30.235072
449.922877	19338.416084	30.240090
450.550685	19358.903982	30.245108
451.113315	19399.499727	30.250125
451.727172	19423.928633	30.255143
452.052543	19449.188601	30.260160
452.518797	19472.369008	30.265178
453.147182	19498.146552	30.270196
453.262648	19536.670111	30.275213
454.071625	19548.138897	30.280231
454.457299	19582.815046	30.285248
454.590319	19615.636162	30.290266
455.102728	19641.409583	30.295284
455.477425	19670.600420	30.300301
456.214221	19685.763265	30.305319
456.110266	19711.405452	30.310336
456.687560	19738.424272	30.315354
457.222739	19765.350237	30.320372
457.201453	19805.839656	30.325389
457.941190	19830.081424	30.330407
458.230289	19863.621154	30.335424
458.534882	19887.207483	30.340442
459.276050	19924.040495	30.345460
459.773309	19961.735337	30.350477
459.995566	19990.863258	30.355495
460.156388	20018.441855	30.360512
460.765969	20048.187756	30.365530
461.581065	20091.016903	30.370548
461.579711	20133.260424	30.375565
462.385927	20160.055700	30.380583
462.824652	20189.364091	30.385600
463.185495	20223.605428	30.390618
464.201461	20264.457224	30.395636
464.415901	20291.922242	30.400653
464.802957	20314.721999	30.405671
465.316099	20365.258159	30.410688
465.812490	20396.931988	30.415706
466.557804	20416.488305	30.420724
466.395458	20469.136532	30.425741
467.324395	20487.025732	30.430759
467.961442	20520.687448	30.435776
467.915745	20553.916208	30.440794
468.822839	20579.106602	30.445812
469.399736	20608.046095	30.450829
469.667581	20636.959274	30.455847
470.072333	20663.699278	30.460864
470.659748	20707.438925	30.465882
471.292796	20731.206912	30.470900
471.583045	20776.575767	30.475917
472.014569	20799.636110	30.480935
472.905459	20829.756852	30.485952
472.971890	20868.859290	30.490970
473.659265	20893.914308	30.495988
473.867223	20920.164380	30.501005
474.381299	20961.968536	30.506023
474.797405	20992.426281	30.511040
475.214042	21034.372153	30.516058
476.103944	21052.504477	30.521076
475.984404	21089.446634	30.526093
476.513236	21122.427970	30.531111
477.313921	21165.125334	30.536128
477.469029	21205.084293	30.541146
478.135856	21228.121568	30.546164
478.594154	21262.275628	30.551181
478.783707	21306.591819	30.556199
479.305907	21352.099040	30.561216
479.648530	21388.208320	30.566234
480.537518	21413.918779	30.571252
480.645135	21460.692545	30.576269
481.167421	21488.872952	30.581287
482.101637	21517.366596	30.586304
482.317675	21557.211216	30.591322
482.736092	21590.353275	30.596340
483.054940	21618.247370	30.601357
483.902899	21644.697154	30.606375
484.269219	21673.194126	30.611392
484.160604	21710.784146	30.616410
485.280842	21741.419819	30.621428
485.621737	21771.568560	30.626445
486.139247	21804.557467	30.631463
486.869761	21829.511821	30.636480
487.155668	21863.078788	30.641498
487.434540	21903.618345	30.646516
487.874591	21939.658246	30.651533
488.476990	21974.346915	30.656551
488.836610	22014.247002	30.661568
489.098567	22053.375975	30.666586
490.028575	22088.335611	30.671604
490.393072	22123.310585	30.676621
490.744575	22165.682931	30.681639
491.622896	22185.546335	30.686656
491.802648	22229.994668	30.691674
492.476073	22270.196674	30.696692
493.175600	22307.734209	30.701709
493.653844	22344.947162	30.706727
494.401305	22366.417813	30.711744
494.666802	22402.662207	30.716762
495.450442	22428.335198	30.721780
495.708039	22470.405140	30.726797
496.274110	22507.332772	30.731815
496.996492	22531.174325	30.736832
497.220357	22569.036339	30.741850
497.478957	22591.153014	30.746868
498.128397	22634.548705	30.751885
498.499769	22664.061868	30.756903
499.253849	22706.283333	30.761920
499.374193	22743.640083	30.766938
500.079744	22778.257389	30.771956
500.649506	22813.311463	30.776973
500.739737	22842.201859	30.781991
501.533812	22880.399098	30.787008
501.765441	22932.329643	30.792026
502.302820	22958.676747	30.797044
503.123269	22998.730391	30.802061
502.998409	23033.867243	30.807079
503.985046	23072.932149	30.812096
504.121733	23126.105547	30.817114
504.529716	23169.025282	30.822132
505.321048	23221.251194	30.827149
505.673468	23258.612362	30.832167
506.643875	23291.562965	30.837184
506.976534	23336.740657	30.842202
507.463922	23373.704904	30.847220
508.127295	23407.137059	30.852237
508.758938	23432.093169	30.857255
508.955033	23467.804449	30.862272
509.671948	23507.418264	30.867290
510.253327	23512.642919	30.872308
510.882601	23549.811817	30.877325
510.952378	23598.641850	30.882343
511.649898	23609.871088	30.887360
512.082404	23650.100022	30.892378
512.574250	23693.864773	30.897396
513.099873	23730.719009	30.902413
513.319084	23759.696866	30.907431
513.902831	23799.474400	30.912448
514.151337	23840.627890	30.917466
514.681414	23883.039410	30.922484
515.341035	23917.295548	30.927501
515.348319	23963.683125	30.932519
516.188073	23999.207227	30.937536
516.445292	24045.610370	30.942554
517.318556	24093.081263	30.947572
518.002320	24130.125483	30.952589
518.175930	24171.650146	30.957607
518.951036	24212.936546	30.962624
519.560963	24256.123224	30.967642
519.897234	24295.884708	30.972660
520.708602	24337.577609	30.977677
520.872674	24396.017275	30.982695
521.618180	24424.387142	30.987712
521.924301	24463.113327	30.992730
522.542506	24508.536379	30.997748
523.254689	24575.113575	31.002765
523.406553	24601.643760	31.007783
524.471156	24634.720797	31.012800
525.113372	24678.213830	31.017818
525.720829	24733.798850	31.022836
526.573806	24759.231440	31.027853
526.712787	24799.139821	31.032871
527.384150	24837.837102	31.037888
527.702658	24871.344607	31.042906
528.357491	24908.043151	31.047924
529.187025	24948.118402	31.052941
529.835386	24993.405704	31.057959
530.800576	24998.884026	31.062976
530.598745	25042.398270	31.067994
531.482019	25073.625638	31.073012
531.906241	25101.919493	31.078029
531.808638	25143.681300	31.083047
532.501479	25178.162520	31.088064
532.858097	25208.055361	31.093082
533.441753	25262.869333	31.098100
534.001134	25306.508826	31.103117
534.332692	25343.634030	31.108135
535.209110	25385.288601	31.113152
535.671279	25421.283281	31.118170
536.007530	25461.142994	31.123188
536.802590	25500.650876	31.128205
537.180198	25547.950625	31.133223
537.935074	25568.419313	31.138240
538.242634	25613.637407	31.143258
538.396510	25661.744319	31.148276
538.858965	25671.498438	31.153293
539.497692	25741.297513	31.158311
540.082657	25760.973472	31.163328
540.076599	25794.381787	31.168346
540.649953	25866.087917	31.173364
541.541245	25891.424055	31.178381
541.849947	25938.616984	31.183399
542.470115	25995.976032	31.188416
542.903008	26018.569949	31.193434
543.515401	26091.407601	31.198452
544.076524	26136.167702	31.203469
544.393151	26171.363255	31.208487
545.317081	26218.617365	31.213504
545.771226	26275.437454	31.218522
546.743310	26337.068096	31.223540
547.116420	26360.483421	31.228557
547.657452	26388.976016	31.233575
548.216966	26468.178769	31.238592
548.543186	26493.774445	31.243610
549.522765	26546.541413	31.248628
550.025758	26579.799389	31.253645
550.443233	26640.552132	31.258663
550.778971	26688.633161	31.263680
551.533583	26721.924624	31.268698
551.854069	26777.131539	31.273716
553.008881	26820.255715	31.278733
553.621983	26866.270048	31.283751
553.726080	26923.419183	31.288768
554.937362	26949.884591	31.293786
555.339175	26972.896825	31.298804
555.864061	27035.746841	31.303821
556.655748	27047.349558	31.308839
556.950390	27115.905602	31.313856
557.662364	27121.611718	31.318874
557.561975	27198.323400	31.323892
558.807789	27202.043534	31.328909
559.155177	27284.167490	31.333927
559.677519	27291.859230	31.338944
560.254783	27366.395770	31.343962
560.975033	27390.339515	31.348980
561.738921	27449.030411	31.353997
561.735777	27462.038654	31.359015
562.475314	27539.183852	31.364032
563.026860	27570.297194	31.369050
563.716716	27582.505817	31.374068
564.419008	27647.218401	31.379085
564.755448	27684.456970	31.384103
565.225430	27712.473988	31.389120
565.888012	27769.715234	31.394138
566.371359	27793.479866	31.399156
567.323348	27852.592924	31.404173
567.627382	27908.192383	31.409191
568.343105	27924.298569	31.414208
568.728733	27960.829547	31.419226
569.184852	27979.123234	31.424244
569.656857	28037.312840	31.429261
570.499664	28062.618391	31.434279
570.861837	28118.706453	31.439296
571.539247	28135.077370	31.444314
571.695983	28183.844507	31.449332
572.263446	28224.116249	31.454349
572.879624	28254.546212	31.459367
573.896450	28300.376660	31.464384
574.249732	28350.269587	31.469402
574.764587	28390.310610	31.474420
575.222456	28428.127977	31.479437
575.809968	28492.173631	31.484455
576.159733	28508.040867	31.489472
576.735927	28575.709734	31.494490
576.920358	28612.050469	31.499508
578.292062	28671.345509	31.504525
578.559765	28704.534260	31.509543
579.151690	28769.300436	31.514560
579.871250	28800.605280	31.519578
580.167202	28853.737665	31.524596
581.124706	28882.513458	31.529613
581.865159	28942.459973	31.534631
582.471627	28993.825751	31.539648
583.178226	29006.661542	31.544666
583.667838	29087.468040	31.549684
584.254628	29097.310036	31.554701
584.502650	29166.491258	31.559719
585.162883	29193.006374	31.564736
586.265527	29251.667217	31.569754
586.411582	29300.658457	31.574772
586.961913	29317.782002	31.579789
587.429313	29383.055818	31.584807
587.945849	29424.325135	31.589824
588.693928	29464.167789	31.594842
589.137448	29515.195574	31.599860
590.232150	29557.648023	31.604877
590.490781	29613.236142	31.609895
591.088285	29656.105260	31.614912
592.273899	29697.399522	31.619930
592.363861	29726.817675	31.624948
592.831727	29796.340052	31.629965
593.498690	29829.949744	31.634983
594.155846	29869.809450	31.640000
594.943429	29931.055372	31.645018
595.295208	29972.249887	31.650036
596.074696	30008.863022	31.655053
596.588351	30041.019372	31.660071
597.179392	30119.562889	31.665088
597.581185	30135.432892	31.670106
598.178479	30215.581729	31.675124
598.645062	30251.403698	31.680141
599.320462	30296.884437	31.685159
600.292892	30335.256261	31.690176
600.687506	30376.783803	31.695194
600.889625	30426.984549	31.700212
601.546480	30462.441009	31.705229
602.172536	30497.812622	31.710247
602.429929	30539.323031	31.715264
603.378080	30598.523954	31.720282
603.804726	30662.895339	31.725300
604.400161	30690.542158	31.730317
604.974315	30744.284140	31.735335
605.571218	30794.323865	31.740352
606.180413	30831.894221	31.745370
606.596254	30890.506451	31.750388
607.639401	30942.401423	31.755405
608.043487	30999.143640	31.760423
608.609720	31052.608948	31.765440
609.464381	31098.496780	31.770458
610.085204	31146.779684	31.775476
610.701136	31175.407492	31.780493
611.552029	31240.559916	31.785511
612.182964	31288.304207	31.790528
612.624576	31315.283131	31.795546
613.292768	31387.798477	31.800564
613.987807	31418.410946	31.805581
614.713313	31469.314841	31.810599
614.722996	31525.647300	31.815616
615.290972	31560.522980	31.820634
616.213244	31624.630105	31.825652
616.942347	31693.483814	31.830669
617.538081	31731.847991	31.835687
617.987599	31770.259181	31.840704
618.586419	31826.103267	31.845722
619.145331	31893.199224	31.850740
620.311706	31925.901550	31.855757
620.632413	31973.679903	31.860775
621.284251	32045.199947	31.865792
621.991923	32096.118087	31.870810
622.956050	32111.651452	31.875828
623.312171	32203.000924	31.880845
623.641598	32224.043094	31.885863
624.738533	32294.338061	31.890880
625.284439	32336.880423	31.895898
625.737019	32381.770422	31.900916
626.507222	32420.436265	31.905933
627.219189	32479.659545	31.910951
627.515879	32531.861255	31.915968
628.515476	32571.245899	31.920986
628.841261	32622.440835	31.926004
629.351722	32665.798258	31.931021
629.983216	32755.909075	31.936039
630.552201	32772.133302	31.941056
631.159003	32833.209255	31.946074
631.690970	32909.222164	31.951092
632.494259	32938.425324	31.956109
632.801768	32981.639362	31.961127
632.997796	33049.775054	31.966144
633.588009	33075.700810	31.971162
634.355054	33167.221899	31.976180
635.330761	33213.351727	31.981197
635.875746	33257.362488	31.986215
636.114730	33330.572625	31.991232
637.298119	33367.272413	31.996250
637.348539	33427.124588	32.001268
638.569448	33504.222169	32.006285
639.101242	33536.242216	32.011303
639.605539	33579.160100	32.016320
640.424763	33644.602948	32.021338
641.368717	33666.300985	32.026356
642.180103	33743.638279	32.031373
642.817320	33803.027963	32.036391
643.436733	33813.089889	32.041408
644.384524	33897.932844	32.046426
644.758232	33931.971238	32.051444
645.216151	33994.730284	32.056461
645.737762	34043.453637	32.061479
646.376906	34085.181762	32.066496
647.167623	34169.270856	32.071514
647.697119	34183.905978	32.076532
648.325168	34232.614517	32.081549
649.019388	34333.691873	32.086567
649.074921	34366.115657	32.091584
649.840897	34413.868013	32.096602
650.793101	34467.483158	32.101620
651.302113	34562.410626	32.106637
652.703447	34597.752761	32.111655
652.581374	34660.490024	32.116672
653.626398	34695.359448	32.121690
654.329594	34753.343816	32.126708
654.986188	34851.171994	32.131725
655.590035	34868.907625	32.136743
656.405440	34942.762963	32.141760
657.219826	34984.936789	32.146778
657.786731	35045.120848	32.151796
658.287736	35096.836241	32.156813
659.174991	35159.100981	32.161831
659.569147	35201.616558	32.166848
660.115805	35277.724702	32.171866
660.855907	35309.391852	32.176884
661.415045	35412.144619	32.181901
662.396911	35417.261361	32.186919
662.531616	35511.921220	32.191936
663.429231	35526.530452	32.196954
664.043432	35628.350423	32.201972
664.638636	35662.940382	32.206989
665.461282	35727.148673	32.212007
666.274068	35782.916890	32.217024
666.783138	35839.701593	32.222042
667.369291	35901.566185	32.227060
667.930679	35968.952584	32.232077
669.382417	36006.991774	32.237095
669.528773	36077.862480	32.242112
670.268075	36123.136316	32.247130
670.707836	36171.703950	32.252148
671.285698	36189.531840	32.257165
672.048689	36283.873757	32.262183
672.423592	36329.773709	32.267200
672.956159	36380.542159	32.272218
673.424362	36436.504579	32.277236
673.944020	36521.611964	32.282253
675.067848	36553.073773	32.287271
675.618419	36628.287258	32.292288
676.484872	36695.177127	32.297306
677.349855	36751.991822	32.302324
677.870552	36787.537172	32.307341
678.671423	36878.718593	32.312359
679.193607	36904.634372	32.317376
679.761735	37002.520775	32.322394
680.745314	37024.954751	32.327412
681.306588	37111.076967	32.332429
682.633637	37140.057535	32.337447
683.073301	37217.157988	32.342464
684.039980	37271.393152	32.347482
684.853132	37315.712508	32.352500
685.316882	37364.949837	32.357517
686.016017	37402.281172	32.362535
686.345914	37488.120532	32.367552
687.249712	37507.160806	32.372570
687.886501	37595.879625	32.377588
688.891003	37639.650666	32.382605
689.427524	37695.619025	32.387623
690.020535	37730.024419	32.392640
690.728068	37824.852096	32.397658
691.480604	37855.192993	32.402676
692.044889	37936.831832	32.407693
692.805839	37970.443152	32.412711
693.300145	38030.069302	32.417728
694.470683	38075.979805	32.422746
695.085801	38134.797183	32.427764
696.021953	38199.719002	32.432781
696.638532	38236.634904	32.437799
697.335858	38292.809845	32.442816
698.220906	38341.609289	32.447834
698.880233	38395.037720	32.452852
699.084227	38451.291728	32.457869
699.973542	38507.189277	32.462887
700.595621	38559.197240	32.467904
701.229542	38621.586150	32.472922
701.966882	38679.972874	32.477940
702.356243	38744.745757	32.482957
703.129005	38809.809463	32.487975
703.829123	38843.340763	32.492992
704.354382	38928.788973	32.498010
705.460507	38975.172596	32.503028
705.499059	39046.921260	32.508045
706.488219	39104.301233	32.513063
707.237508	39154.483811	32.518080
707.765931	39214.226970	32.523098
708.589775	39256.129394	32.528116
708.876933	39325.554913	32.533133
709.924053	39381.359281	32.538151
710.568220	39448.002203	32.543168
711.287575	39480.773270	32.548186
712.327905	39556.746529	32.553204
712.641495	39621.851767	32.558221
713.104598	39672.232813	32.563239
714.070131	39731.023616	32.568256
714.657400	39798.938432	32.573274
715.499458	39852.720819	32.578292
716.057644	39906.832398	32.583309
716.814471	39986.320175	32.588327
717.361631	40058.378472	32.593344
717.979258	40111.109380	32.598362
719.270730	40181.031335	32.603380
719.686792	40238.687727	32.608397
720.290021	40319.409393	32.613415
721.519271	40374.036921	32.618432
721.989631	40429.485570	32.623450
722.729846	40510.801322	32.628468
723.479459	40568.033585	32.633485
724.413862	40613.767820	32.638503
724.737459	40705.634063	32.643520
725.654321	40753.328411	32.648538
726.295227	40828.737026	32.653556
727.235108	40892.066428	32.658573
728.331689	40932.283270	32.663591
729.068442	41025.061584	32.668608
729.653003	41078.718533	32.673626
731.056303	41119.795313	32.678644
731.499417	41177.169878	32.683661
732.223651	41226.132546	32.688679
733.132304	41309.749733	32.693696
733.678516	41350.105638	32.698714
734.539777	41398.390970	32.703732
734.856868	41470.600673	32.708749
735.344505	41522.121867	32.713767
736.431743	41596.306895	32.718784
736.962677	41670.918277	32.723802
737.887687	41711.331435	32.728820
738.100660	41778.727078	32.733837
739.181789	41854.816072	32.738855
740.080812	41901.371561	32.743872
740.765794	41969.238466	32.748890
741.547568	42019.787047	32.753908
741.768211	42098.975763	32.758925
742.600169	42178.196853	32.763943
743.547975	42233.403458	32.768960
743.908489	42297.752872	32.773978
745.163587	42370.233394	32.778996
745.829236	42423.091545	32.784013
746.703718	42510.599623	32.789031
747.210745	42540.205768	32.794048
747.670915	42626.029827	32.799066
749.093128	42658.464882	32.804084
749.137727	42738.340636	32.809101
749.933185	42791.642925	32.814119
750.482400	42854.661701	32.819136
751.360796	42921.508007	32.824154
752.203743	42991.571231	32.829172
752.728990	43047.806609	32.834189
753.129359	43103.551059	32.839207
754.126032	43180.924238	32.844224
754.780386	43262.058542	32.849242
755.880514	43305.888919	32.854260
756.426475	43388.662382	32.859277
757.118112	43456.442626	32.864295
758.217207	43517.884307	32.869312
758.491536	43600.784036	32.874330
759.329740	43675.645410	32.879348
760.248951	43734.952604	32.884365
761.201418	43803.014439	32.889383
761.717935	43886.088330	32.894400
762.674476	43944.298879	32.899418
763.564221	44023.651751	32.904436
764.246767	44105.268158	32.909453
765.161929	44175.693769	32.914471
765.785740	44234.207459	32.919488
766.546006	44307.730711	32.924506
767.684573	44388.342142	32.929524
768.520669	44450.475678	32.934541
769.359308	44511.230508	32.939559
770.265256	44590.747438	32.944576
770.732983	44654.173759	32.949594
771.656222	44709.972655	32.954612
772.589442	44781.457787	32.959629
773.012577	44859.484979	32.964647
774.220736	44912.362202	32.969664
774.410132	44979.862425	32.974682
775.221984	45059.087328	32.979700
776.112006	45136.927886	32.984717
777.013769	45182.204727	32.989735
778.154566	45279.296628	32.994752
778.378283	45341.625467	32.999770
779.487659	45389.008667	33.004788
779.584904	45485.258319	33.009805
780.695656	45529.341875	33.014823
781.598915	45627.845824	33.019840
782.086097	45681.578352	33.024858
783.096560	45764.292378	33.029876
783.628714	45828.750639	33.034893
784.534649	45917.075408	33.039911
785.664153	45968.545569	33.044928
785.895663	46059.751455	33.049946
786.760085	46139.534463	33.054964
787.856694	46198.982749	33.059981
788.674040	46278.647692	33.064999
789.711221	46346.838528	33.070016
789.948053	46393.028841	33.075034
790.968393	46474.432244	33.080052
791.687306	46514.741188	33.085069
792.367136	46606.878669	33.090087
793.140854	46651.649693	33.095104
793.979177	46718.069026	33.100122
794.696398	46788.076107	33.105140
795.602091	46869.499597	33.110157
796.241840	46934.910227	33.115175
797.091198	46999.429589	33.120192
797.813931	47078.365508	33.125210
798.556774	47116.980965	33.130228
799.204362	47214.900401	33.135245
799.959309	47273.390813	33.140263
800.683627	47370.901375	33.145280
801.584552	47421.415213	33.150298
802.454435	47512.811013	33.155316
803.537529	47578.159791	33.160333
804.445135	47671.572814	33.165351
805.306238	47723.311723	33.170368
806.094706	47819.798627	33.175386
806.918817	47867.218189	33.180404
807.929499	47968.400069	33.185421
808.109623	48021.696446	33.190439
809.350191	48076.515376	33.195456
809.972005	48155.655197	33.200474
810.837060	48279.106018	33.205492
811.383931	48351.033249	33.210509
812.295935	48403.365548	33.215527
813.359477	48463.962667	33.220544
814.027973	48583.323018	33.225562
814.921733	48614.029631	33.230580
816.291922	48712.883631	33.235597
816.551289	48775.543988	33.240615
817.690604	48870.516754	33.245632
818.054091	48928.251436	33.250650
819.011307	49002.125945	33.255668
819.898001	49076.870239	33.260685
820.548065	49167.520771	33.265703
821.681849	49221.631376	33.270720
822.530855	49331.322107	33.275738
823.399808	49376.290019	33.280756
823.609121	49488.932848	33.285773
824.559128	49541.751565	33.290791
825.711979	49626.190292	33.295808
826.483657	49697.787456	33.300826
827.090879	49796.708986	33.305844
828.299966	49851.443784	33.310861
828.892357	49951.895789	33.315879
829.966642	50023.550240	33.320896
831.029509	50092.795984	33.325914
831.641177	50149.270803	33.330932
832.303276	50256.299020	33.335949
832.846741	50310.118768	33.340967
834.157084	50382.854170	33.345984
834.853843	50461.424366	33.351002
835.301599	50520.987367	33.356020
836.192777	50600.827342	33.361037
836.622262	50678.219809	33.366055
837.836229	50747.889001	33.371072
838.459851	50817.122267	33.376090
838.808844	50914.172469	33.381108
839.878127	50960.254867	33.386125
840.335418	51084.291852	33.391143
841.335990	51135.886013	33.396160
842.065299	51254.573001	33.401178
842.959751	51317.819728	33.406196
843.829447	51421.666166	33.411213
844.894478	51497.061277	33.416231
845.698602	51606.593289	33.421248
846.568176	51675.522499	33.426266
847.485435	51754.189526	33.431284
848.733461	51853.162496	33.436301
849.343317	51947.036736	33.441319
850.206133	52013.917026	33.446336
851.254821	52104.913548	33.451354
851.800556	52209.049639	33.456372
853.029239	52280.073190	33.461389
853.416798	52373.006704	33.466407
854.481853	52451.574374	33.471424
855.456619	52538.744089	33.476442
856.346109	52643.560174	33.481460
857.555814	52716.283227	33.486477
858.017529	52811.539475	33.491495
859.079340	52892.618607	33.496512
860.026513	52963.090018	33.501530
860.575129	53070.323537	33.506548
861.559023	53148.051880	33.511565
862.391188	53233.148876	33.516583
863.279953	53315.100120	33.521600
863.833655	53446.090921	33.526618
864.608543	53509.496958	33.531636
866.211302	53613.753858	33.536653
866.646612	53678.177147	33.541671
867.440766	53779.615837	33.546688
868.323041	53872.689817	33.551706
869.468754	53957.475213	33.556724
869.991994	54050.209558	33.561741
871.105761	54159.995047	33.566759
871.750028	54243.217180	33.571776
872.679707	54340.344952	33.576794
873.460431	54414.724407	33.581812
874.645310	54502.507743	33.586829
875.520151	54614.325624	33.591847
876.646532	54687.814774	33.596864
877.694680	54784.910296	33.601882
877.984277	54876.587636	33.606900
879.275482	54940.825560	33.611917
879.972239	55042.611920	33.616935
881.009117	55119.835284	33.621952
881.600253	55201.640416	33.626970
882.447688	55269.977701	33.631988
883.668152	55348.369108	33.637005
883.896632	55435.258045	33.642023
884.428212	55513.605114	33.647040
885.936379	55608.668513	33.652058
886.549741	55698.145747	33.657076
887.570393	55774.758956	33.662093
887.966764	55879.189282	33.667111
889.500225	55948.325875	33.672128
890.308872	56044.071031	33.677146
890.924628	56144.137166	33.682164
892.173394	56218.619976	33.687181
892.931745	56316.606270	33.692199
894.013556	56399.291989	33.697216
894.717134	56489.645753	33.702234
895.613366	56585.310360	33.707252
896.486981	56657.291452	33.712269
897.434899	56763.457299	33.717287
898.284446	56858.360530	33.722304
899.402505	56938.609105	33.727322
900.101114	57044.557398	33.732340
901.398109	57118.253330	33.737357
902.129423	57219.680132	33.742375
903.021811	57302.753627	33.747392
903.920249	57389.620995	33.752410
904.636935	57507.069262	33.757428
905.716057	57585.353855	33.762445
906.752037	57681.535443	33.767463
907.348991	57774.456906	33.772480
907.879262	57879.616010	33.777498
908.976564	57977.266801	33.782516
910.012530	58072.279224	33.787533
910.786991	58177.483252	33.792551
911.325752	58280.288223	33.797568
912.494862	58376.490137	33.802586
913.175263	58492.261477	33.807604
914.289480	58591.491315	33.812621
915.332497	58691.307591	33.817639
916.277218	58795.146314	33.822656
917.083533	58903.335953	33.827674
918.318124	59005.251291	33.832692
919.543822	59102.773948	33.837709
920.422703	59208.977493	33.842727
921.195884	59294.639328	33.847744
922.224247	59394.546968	33.852762
922.952569	59492.071881	33.857780
923.744362	59581.012352	33.862797
925.010086	59708.635392	33.867815
925.962606	59797.690245	33.872832
927.035250	59882.375771	33.877850
927.694086	59980.994071	33.882868
928.972841	60085.854014	33.887885
929.902032	60170.828887	33.892903
930.147850	60246.406317	33.897920
931.560809	60354.586818	33.902938
932.216194	60427.633973	33.907956
933.327484	60530.331893	33.912973
934.368133	60596.362833	33.917991
935.220171	60705.161887	33.923008
936.269937	60772.824353	33.928026
937.057002	60867.211856	33.933044
937.936822	60967.871455	33.938061
938.831311	61040.147292	33.943079
939.462704	61136.035429	33.948096
940.689551	61235.842429	33.953114
941.405758	61340.792610	33.958132
942.528324	61421.599824	33.963149
943.166998	61526.225529	33.968167
944.041857	61620.899668	33.973184
945.161664	61721.960874	33.978202
945.482479	61839.407923	33.983220
947.058982	61933.236301	33.988237
948.002375	62025.280802	33.993255
948.808405	62133.615518	33.998272
950.363740	62240.458086	34.003290
951.371285	62321.704281	34.008308
951.891624	62430.506122	34.013325
953.423392	62509.576211	34.018343
954.266581	62618.419346	34.023360
955.347913	62709.444267	34.028378
955.900726	62813.487672	34.033396
956.962287	62903.029393	34.038413
958.111480	63009.100986	34.043431
958.309540	63117.039152	34.048448
959.932671	63204.010965	34.053466
960.571854	63309.862237	34.058484
961.657929	63422.782808	34.063501
962.659226	63527.210357	34.068519
963.229746	63617.433570	34.073536
964.363769	63730.540976	34.078554
965.510022	63827.601942	34.083572
966.342669	63957.485920	34.088589
967.689415	64040.150811	34.093607
968.486822	64146.332111	34.098624
969.976969	64246.204751	34.103642
971.167574	64331.055786	34.108660
971.840254	64456.585379	34.113677
972.865691	64519.629275	34.118695
973.894758	64641.970669	34.123712
975.136957	64717.192766	34.128730
975.906499	64837.287135	34.133748
977.056059	64901.121010	34.138765
977.807984	65013.374688	34.143783
978.560525	65085.214891	34.148800
979.853714	65202.335452	34.153818
980.983018	65290.743912	34.158836
981.869326	65391.937663	34.163853
982.680061	65492.262849	34.168871
983.614594	65553.726607	34.173888
984.644566	65656.326393	34.178906
985.002676	65752.622476	34.183924
986.096483	65811.585702	34.188941
987.181732	65896.488894	34.193959
987.593590	66040.324893	34.198976
988.698389	66109.820027	34.203994
989.329111	66192.327083	34.209012
990.317296	66340.419423	34.214029
991.318737	66419.691243	34.219047
992.541285	66497.803858	34.224064
993.844677	66621.289171	34.229082
994.519952	66738.151057	34.234100
995.898634	66804.983709	34.239117
996.864485	66940.100182	34.244135
998.077215	67014.041070	34.249152
998.702344	67149.529053	34.254170
999.508453	67223.712301	34.259188
1000.826727	67344.512061	34.264205
1001.551705	67440.436072	34.269223
1002.556276	67547.812977	34.274240
1003.733121	67694.723397	34.279258
1004.322151	67780.042329	34.284276
1005.741879	67860.757006	34.289293
1006.491694	68021.540658	34.294311
1007.527708	68140.586755	34.299328
1008.382878	68223.224730	34.304346
1009.499479	68331.898985	34.309364
1010.340188	68467.327159	34.314381
1011.824677	68574.693436	34.319399
1012.616972	68682.284126	34.324416
1014.003672	68813.186769	34.329434
1015.062364	68909.080764	34.334452
1015.614557	69041.659139	34.339469
1017.030579	69124.483390	34.344487
1017.690909	69274.071785	34.349504
1018.247857	69364.286241	34.354522
1019.366511	69500.233339	34.359540
1020.432857	69616.080623	34.364557
1021.651826	69732.150707	34.369575
1022.825555	69864.939062	34.374592
1024.171941	69984.269279	34.379610
1025.060982	70115.758938	34.384628
1026.169380	70234.629432	34.389645
1027.319327	70323.894768	34.394663
1028.039432	70462.015805	34.399680
1029.202862	70577.790167	34.404698
1030.316128	70681.935448	34.409716
1031.233085	70795.273646	34.414733
1032.409391	70927.386450	34.419751
1033.072240	71054.780049	34.424768
1034.418567	71150.917294	34.429786
1035.255147	71295.962990	34.434804
1035.976991	71386.463802	34.439821
1037.382768	71531.464925	34.444839
1038.494503	71608.415254	34.449856
1039.317087	71749.403856	34.454874
1040.256757	71817.321881	34.459892
1041.303663	71964.758975	34.464909
1042.516772	72052.373017	34.469927
1043.109866	72184.921898	34.474944
1044.231147	72287.614835	34.479962
1045.126420	72395.696056	34.484980
1046.148073	72537.631673	34.489997
1047.436358	72630.562891	34.495015
1048.447903	72756.976857	34.500032
1049.286063	72866.447199	34.505050
1050.128264	72972.890833	34.510068
1051.088123	73120.236639	34.515085
1052.436762	73227.371977	34.520103
1053.196095	73397.670051	34.525120
1054.232051	73479.764312	34.530138
1055.795333	73627.226424	34.535156
1056.187014	73745.865566	34.540173
1057.791376	73881.133738	34.545191
1058.925461	74005.381370	34.550208
1059.829466	74121.394682	34.555226
1060.823824	74262.279025	34.560244
1061.745105	74405.236036	34.565261
1063.174745	74525.654711	34.570279
1064.072683	74665.110128	34.575296
1065.161234	74793.610126	34.580314
1066.626041	74914.524775	34.585332
1067.181573	75074.543760	34.590349
1068.319417	75164.831316	34.595367
1069.591623	75321.382676	34.600384
1071.022964	75438.747951	34.605402
1071.877556	75574.197377	34.610420
1073.014383	75721.047604	34.615437
1073.988910	75831.637391	34.620455
1074.536717	75992.922515	34.625472
1076.039564	76105.155050	34.630490
1077.157932	76238.045424	34.635508
1077.907742	76394.625014	34.640525
1079.797137	76505.395306	34.645543
1080.780239	76639.510605	34.650560
1081.713899	76770.127100	34.655578
1083.112266	76883.947926	34.660596
1084.137789	77024.846664	34.665613
1085.140279	77164.839958	34.670631
1085.988856	77270.041376	34.675648
1087.661920	77416.060232	34.680666
1088.466834	77524.455254	34.685684
1089.358480	77646.570833	34.690701
1090.247949	77831.896205	34.695719
1091.405028	77947.714332	34.700736
1092.462815	78060.218101	34.705754
1093.810249	78200.757783	34.710772
1094.625831	78338.753728	34.715789
1095.905918	78428.211590	34.720807
1096.685707	78592.052889	34.725824
1097.780058	78727.662229	34.730842
1099.286080	78810.815878	34.735860
1100.184206	78977.586825	34.740877
1101.116688	79057.109853	34.745895
1102.575212	79156.706104	34.750912
1103.426514	79293.173210	34.755930
1104.450951	79458.221392	34.760948
1105.097502	79583.156016	34.765965
1106.459062	79672.246083	34.770983
1107.658154	79834.583167	34.776000
1108.326998	79975.179743	34.781018
1109.741979	80070.470177	34.786036
1110.562218	80255.935954	34.791053
1111.832442	80385.915242	34.796071
1113.034058	80493.864681	34.801088
1114.238426	80632.869845	34.806106
1115.530445	80771.887292	34.811124
1116.947234	80912.744265	34.816141
1118.180234	81025.103689	34.821159
1118.874930	81176.659035	34.826176
1120.310183	81280.333856	34.831194
1121.588866	81429.155874	34.836212
1122.290344	81577.261610	34.841229
1123.426094	81705.481625	34.846247
1124.647197	81845.851385	34.851264
1125.504199	81969.603820	34.856282
1126.702847	82105.730846	34.861300
1128.144640	82265.734730	34.866317
1129.463052	82394.024769	34.871335
1130.434189	82511.073973	34.876352
1131.562240	82667.755057	34.881370
1132.855502	82781.081628	34.886388
1134.109545	82916.168372	34.891405
1135.163918	83057.894070	34.896423
1136.439719	83209.472959	34.901440
1137.431614	83326.662514	34.906458
1138.596599	83461.463490	34.911476
1139.234592	83623.755066	34.916493
1140.669205	83731.235410	34.921511
1141.759873	83901.460869	34.926528
1142.881820	84039.755883	34.931546
1143.750439	84164.644806	34.936564
1144.816719	84337.887034	34.941581
1146.321340	84458.017080	34.946599
1147.282658	84613.013234	34.951616
1148.556743	84755.651158	34.956634
1149.706736	84912.098939	34.961652
1150.831585	85038.697281	34.966669
1152.239905	85197.344244	34.971687
1153.394805	85317.990019	34.976704
1154.347277	85492.657096	34.981722
1155.894559	85603.935276	34.986740
1156.927719	85774.393632	34.991757
1157.910987	85880.818628	34.996775
1159.374026	86034.537783	35.001792
1160.416635	86143.148650	35.006810
1161.669477	86262.576579	35.011828
1162.356519	86418.723402	35.016845
1163.579713	86534.907627	35.021863
1164.696672	86649.560263	35.026880
1165.405617	86815.804221	35.031898
1166.878275	86915.542753	35.036916
1168.144897	87079.076043	35.041933
1168.860510	87217.329946	35.046951
1170.206660	87324.665569	35.051968
1171.324193	87500.954239	35.056986
1172.581847	87611.410051	35.062004
1173.224012	87794.871360	35.067021
1174.493737	87908.697083	35.072039
1175.956960	88097.670810	35.077056
1176.622170	88216.583407	35.082074
1177.936230	88399.860845	35.087092
1179.456858	88537.147913	35.092109
1180.307718	88685.033069	35.097127
1181.575592	88855.541896	35.102144
1182.891892	88999.048849	35.107162
1183.612575	89163.753505	35.112180
1185.274246	89311.785955	35.117197
1186.355113	89467.835423	35.122215
1187.896037	89653.022499	35.127232
1189.064726	89786.054310	35.132250
1190.344457	89952.339248	35.137268
1191.738998	90106.617020	35.142285
1192.456530	90265.676951	35.147303
1194.341155	90409.216721	35.152320
1195.425947	90549.558150	35.157338
1196.324703	90724.560888	35.162356
1197.287993	90866.694429	35.167373
1198.535241	91040.303572	35.172391
1200.155941	91177.174062	35.177408
1201.018002	91356.532457	35.182426
1202.812363	91489.930554	35.187444
1203.984027	91664.416781	35.192461
1205.094087	91799.987316	35.197479
1206.500107	91998.946109	35.202496
1207.200671	92128.847475	35.207514
1208.420287	92250.527381	35.212532
1209.772353	92462.065842	35.217549
1210.962681	92599.728323	35.222567
1212.374950	92763.983363	35.227584
1213.452888	92918.053013	35.232602
1214.744878	93076.675182	35.237620
1215.803660	93228.277049	35.242637
1216.987618	93400.409596	35.247655
1218.626370	93552.958766	35.252672
1219.670596	93708.740693	35.257690
1220.889766	93857.253758	35.262708
1222.249468	94023.442994	35.267725
1223.560125	94176.801302	35.272743
1225.036669	94311.898899	35.277760
1225.639995	94458.243164	35.282778
1227.149621	94591.477597	35.287796
1228.446018	94734.993652	35.292813
1229.660915	94873.425393	35.297831
1230.526601	95015.487329	35.302848
1231.683032	95162.165755	35.307866
1233.228889	95303.678617	35.312884
1234.187775	95456.038983	35.317901
1235.060455	95607.338752	35.322919
1236.547772	95758.478577	35.327936
1237.619151	95908.603867	35.332954
1238.935548	96079.489918	35.337972
1240.116693	96228.417002	35.342989
1240.930479	96381.224212	35.348007
1242.305815	96543.242075	35.353024
1243.410942	96703.526504	35.358042
1244.706949	96864.597765	35.363060
1245.883949	97040.915563	35.368077
1246.999321	97224.683867	35.373095
1248.891572	97370.937115	35.378112
1249.879026	97546.371716	35.383130
1250.964662	97704.762204	35.388148
1252.081853	97881.519908	35.393165
1253.560560	98058.392326	35.398183
1254.571211	98219.765314	35.403200
1255.978407	98392.495360	35.408218
1257.806673	98571.599996	35.413236
1258.794136	98756.413248	35.418253
1259.502244	98934.117199	35.423271
1261.375801	99092.297200	35.428288
1262.719855	99263.114302	35.433306
1263.766086	99449.853413	35.438324
1265.030703	99616.155946	35.443341
1266.328336	99788.110484	35.448359
1267.613493	99959.201533	35.453376
1268.576528	100150.236435	35.458394
1270.461101	100314.819500	35.463412
1271.769462	100484.835214	35.468429
1272.800969	100694.629244	35.473447
1274.663417	100836.556526	35.478464
1275.678800	101010.830121	35.483482
1276.989449	101195.402838	35.488500
1278.249812	101372.696189	35.493517
1279.292594	101521.584926	35.498535
1281.462225	101675.698921	35.503552
1282.309621	101890.594814	35.508570
1283.633103	102018.726713	35.513588
1284.814677	102231.389723	35.518605
1285.843735	102369.618179	35.523623
1287.506734	102570.970340	35.528640
1288.744872	102724.587634	35.533658
1289.582032	102908.072308	35.538676
1291.246408	103058.555198	35.543693
1292.176937	103252.139186	35.548711
1293.654553	103399.882461	35.553728
1294.833902	103567.827810	35.558746
1296.174851	103711.766515	35.563764
1297.093829	103898.789479	35.568781
1298.086609	104047.613690	35.573799
1299.247105	104218.831852	35.578816
1300.465116	104409.937124	35.583834
1301.630248	104572.930814	35.588852
1303.252616	104758.861639	35.593869
1304.170585	104925.852066	35.598887
1305.778372	105099.903782	35.603904
1306.763668	105310.904638	35.608922
1308.178576	105480.319617	35.613940
1309.732274	105667.122803	35.618957
1310.521659	105848.998944	35.623975
1311.545782	106056.291857	35.628992
1313.587013	106218.379224	35.634010
1314.581124	106440.874777	35.639028
1316.355902	106602.779287	35.644045
1317.351969	106819.873508	35.649063
1318.764486	106986.299839	35.654080
1320.108712	107204.253531	35.659098
1321.801156	107377.194594	35.664116
1323.251815	107560.769689	35.669133
1324.236678	107775.754208	35.674151
1325.955820	107937.410773	35.679168
1327.059500	108146.259702	35.684186
1328.180874	108320.893206	35.689204
1329.429764	108536.209623	35.694221
1331.084741	108693.729620	35.699239
1332.549205	108927.097400	35.704256
1333.789146	109096.027775	35.709274
1335.131634	109309.456429	35.714292
1336.849061	109488.180911	35.719309
1338.146910	109665.967032	35.724327
1339.349894	109886.651007	35.729344
1341.056559	110052.690955	35.734362
1342.387903	110252.812563	35.739380
1344.024999	110442.025760	35.744397
1344.812857	110640.819107	35.749415
1346.645297	110810.091287	35.754432
1347.779996	111004.427051	35.759450
1348.947792	111204.943226	35.764468
1350.253683	111393.026419	35.769485
1351.421791	111593.108955	35.774503
1352.922461	111769.536203	35.779520
1354.579634	111983.628130	35.784538
1355.446491	112190.941519	35.789556
1357.032365	112354.072805	35.794573
1358.266222	112582.125239	35.799591
1359.626493	112739.338325	35.804608
1361.072135	112966.499742	35.809626
1362.375318	113141.562865	35.814644
1364.107146	113354.762221	35.819661
1365.127092	113518.377250	35.824679
1366.682146	113729.639183	35.829696
1368.010402	113887.231776	35.834714
1369.883087	114041.244443	35.839732
1371.161918	114234.785012	35.844749
1371.778144	114439.548802	35.849767
1373.837949	114587.413466	35.854784
1374.967421	114810.501714	35.859802
1375.765985	114966.178464	35.864820
1377.429245	115123.877536	35.869837
1378.411264	115368.037455	35.874855
1380.120581	115514.811077	35.879872
1381.618968	115719.388115	35.884890
1382.914485	115912.603410	35.889908
1384.318968	116055.250217	35.894925
1385.954732	116286.976116	35.899943
1387.344826	116458.287947	35.904960
1388.632621	116628.015425	35.909978
1389.988267	116852.187362	35.914996
1391.480291	117012.742786	35.920013
1393.172062	117212.995937	35.925031
1394.034731	117407.924848	35.930048
1395.753580	117581.445933	35.935066
1397.545457	117783.637701	35.940084
1398.426830	117985.564210	35.945101
1400.066260	118138.986772	35.950119
1401.482589	118377.895765	35.955136
1402.912088	118547.353885	35.960154
1403.854924	118786.842110	35.965172
1405.563282	118939.327750	35.970189
1406.686009	119150.209673	35.975207
1407.990928	119362.413031	35.980224
1409.827193	119568.828734	35.985242
1410.731297	119768.657104	35.990260
1412.586164	119960.573015	35.995277
1413.841858	120188.025530	36.000295
1415.638446	120361.825263	36.005312
1417.345764	120617.057941	36.010330
1418.384419	120795.141170	36.015348
1420.354839	120959.514089	36.020365
1421.413997	121192.015323	36.025383
1422.973675	121375.731369	36.030400
1424.500659	121588.582474	36.035418
1425.802116	121767.947682	36.040436
1427.036854	121979.075332	36.045453
1428.504141	122152.426369	36.050471
1430.234700	122398.737639	36.055488
1431.491843	122566.704174	36.060506
1432.873741	122797.686506	36.065524
1434.258229	122985.139858	36.070541
1435.428596	123197.338695	36.075559
1437.104850	123379.948305	36.080576
1438.219815	123614.209857	36.085594
1439.394512	123817.433068	36.090612
1441.335189	124034.202491	36.095629
1441.975122	124238.970447	36.100647
1444.122929	124399.587516	36.105664
1445.259822	124611.258301	36.110682
1446.126448	124839.819680	36.115700
1448.006205	124993.617852	36.120717
1449.505861	125211.214195	36.125735
1450.478988	125419.662128	36.130752
1452.297101	125578.400686	36.135770
1453.719003	125797.458104	36.140788
1455.069422	126046.814771	36.145805
1456.613448	126240.054275	36.150823
1457.724363	126438.012727	36.155840
1459.567720	126625.557986	36.160858
1460.465671	126881.771066	36.165876
1462.152613	127066.063438	36.170893
1463.609016	127275.766264	36.175911
1465.055882	127509.856959	36.180928
1466.783699	127720.267458	36.185946
1467.882579	127938.468733	36.190964
1469.549035	128171.922162	36.195981
1470.951675	128369.696274	36.200999
1472.038438	128627.377843	36.206016
1474.062015	128819.077281	36.211034
1475.065313	129072.570498	36.216052
1476.855059	129264.322851	36.221069
1478.634097	129542.336813	36.226087
1479.573117	129740.283089	36.231104
1481.411720	129978.285097	36.236122
1482.663362	130196.923364	36.241140
1484.249368	130452.857684	36.246157
1485.559651	130654.552112	36.251175
1487.128858	130926.088795	36.256192
1488.806558	131133.632050	36.261210
1489.909180	131371.889568	36.266228
1492.093634	131617.654823	36.271245
1493.592447	131829.957294	36.276263
1494.759743	132071.276456	36.281280
1496.322644	132329.017977	36.286298
1497.931642	132530.577074	36.291316
1499.862976	132808.802014	36.296333
1501.255208	133038.386794	36.301351
1502.568988	133243.748162	36.306368
1504.580338	133449.798412	36.311386
1505.894235	133724.430744	36.316404
1507.345258	133954.887826	36.321421
1509.074634	134152.106056	36.326439
1510.330348	134419.557520	36.331456
1512.251096	134626.150150	36.336474
1513.691162	134854.740966	36.341492
1515.202356	135104.469906	36.346509
1517.155138	135305.398473	36.351527
1518.269660	135576.240917	36.356544
1519.918517	135782.923055	36.361562
1521.465729	135976.964275	36.366580
1522.645756	136223.600366	36.371597
1524.336253	136465.811161	36.376615
1525.704502	136647.289898	36.381632
1527.538439	136866.811936	36.386650
1529.036411	137105.244483	36.391668
1529.869468	137299.547359	36.396685
1531.945556	137483.808026	36.401703
1533.413521	137728.751089	36.406720
1534.744164	137915.312463	36.411738
1536.235625	138156.935287	36.416756
1537.646601	138361.886710	36.421773
1539.666932	138573.192980	36.426791
1540.653790	138805.409696	36.431808
1542.339399	139034.349105	36.436826
1543.533667	139244.245339	36.441844
1545.104834	139470.633754	36.446861
1546.491647	139722.893055	36.451879
1548.086381	139927.889485	36.456896
1549.525269	140178.775698	36.461914
1551.102671	140387.782713	36.466932
1552.907994	140659.930929	36.471949
1554.797627	140862.022774	36.476967
1555.764080	141143.953013	36.481984
1557.315964	141371.296710	36.487002
1559.300841	141592.819524	36.492020
1560.967917	141862.643283	36.497037
1562.443797	142058.345271	36.502055
1563.678862	142346.213423	36.507072
1565.643558	142554.464205	36.512090
1567.504369	142782.555218	36.517108
1568.649876	143072.928593	36.522125
1570.299744	143281.006211	36.527143
1571.958316	143525.522794	36.532160
1573.604098	143778.915524	36.537178
1575.497986	144001.091371	36.542196
1576.877017	144255.164126	36.547213
1578.731120	144506.083538	36.552231
1580.168598	144729.313090	36.557248
1582.169294	145015.474982	36.562266
1583.231058	145247.602440	36.567284
1585.026514	145456.723666	36.572301
1587.031313	145688.438458	36.577319
1588.167916	145982.072816	36.582336
1589.769104	146176.285407	36.587354
1591.154152	146449.401090	36.592372
1592.634979	146672.282769	36.597389
1594.399453	146944.683363	36.602407
1595.526651	147192.545549	36.607424
1597.481382	147417.309329	36.612442
1599.394116	147698.312570	36.617460
1600.678315	147911.739833	36.622477
1603.000885	148149.735058	36.627495
1604.424836	148419.337598	36.632512
1606.121110	148643.428568	36.637530
1607.632701	148904.933697	36.642548
1609.006248	149151.783277	36.647565
1610.825374	149367.176280	36.652583
1611.963267	149636.910580	36.657600
1614.154594	149816.131067	36.662618
1614.916605	150086.803543	36.667636
1616.732437	150293.684293	36.672653
1618.364745	150515.123615	36.677671
1619.691770	150795.448401	36.682688
1620.570074	151006.564701	36.687706
1622.575267	151235.492786	36.692724
1624.285841	151519.553477	36.697741
1626.124164	151757.069122	36.702759
1627.339626	151989.512867	36.707776
1629.228302	152227.708533	36.712794
1630.649115	152506.904787	36.717812
1632.191975	152735.168788	36.722829
1633.868002	153012.870820	36.727847
1635.230365	153244.273164	36.732864
1636.984913	153519.050972	36.737882
1638.778501	153802.940693	36.742900
1640.356275	154033.046481	36.747917
1642.331965	154296.638447	36.752935
1643.595809	154580.086409	36.757952
1645.353921	154822.365996	36.762970
1647.289098	155126.378553	36.767988
1648.464446	155369.084284	36.773005
1650.995650	155601.889560	36.778023
1652.596992	155896.401983	36.783040
1654.102129	156175.438027	36.788058
1655.984766	156395.520221	36.793076
1657.950610	156691.794834	36.798093
1659.445306	156958.844084	36.803111
1661.281971	157181.094203	36.808128
1662.704582	157457.554502	36.813146
1664.371615	157730.326386	36.818164
1666.288408	157960.937618	36.823181
1668.178293	158252.216493	36.828199
1669.888550	158521.031566	36.833216
1671.891084	158738.497638	36.838234
1673.097741	159039.617452	36.843252
1674.720257	159269.016092	36.848269
1676.956160	159520.142186	36.853287
1678.708595	159812.724045	36.858304
1679.655737	160057.363218	36.863322
1681.636560	160312.935753	36.868340
1683.479989	160550.892698	36.873357
1685.576212	160797.370842	36.878375
1686.905803	161061.979704	36.883392
1688.239451	161339.080955	36.888410
1690.067818	161636.624286	36.893428
1691.616547	161890.070278	36.898445
1693.496604	162142.882111	36.903463
1694.993473	162419.750271	36.908480
1696.484200	162671.207313	36.913498
1699.192955	162913.265707	36.918516
1700.497307	163180.988662	36.923533
1701.915331	163456.456954	36.928551
1704.046087	163668.479723	36.933568
1705.489771	163953.535394	36.938586
1706.981336	164196.480497	36.943604
1708.456261	164419.987800	36.948621
1710.791115	164632.605233	36.953639
1711.883520	164917.584719	36.958656
1713.084680	165145.781738	36.963674
1715.431562	165372.580727	36.968692
1716.703825	165645.146319	36.973709
1718.078289	165931.686916	36.978727
1720.027339	166197.896474	36.983744
1721.618307	166423.946823	36.988762
1724.112595	166656.044497	36.993780
1725.384485	166971.526961	36.998797
1727.222027	167202.058123	37.003815
1728.992977	167464.018060	37.008832
1730.507038	167768.916209	37.013850
1732.280755	168009.380975	37.018868
1733.443944	168262.539094	37.023885
1735.825300	168533.288138	37.028903
1738.122265	168790.455432	37.033920
1739.555999	169091.863587	37.038938
1741.347627	169336.430859	37.043956
1742.963033	169633.895094	37.048973
1744.565183	169880.094130	37.053991
1746.710454	170134.580155	37.059008
1747.913877	170446.804518	37.064026
1749.859651	170685.825532	37.069044
1751.555141	171019.184854	37.074061
1753.316931	171283.785534	37.079079
1754.917375	171553.893447	37.084096
1756.697146	171804.985552	37.089114
1758.767640	172079.360698	37.094132
1760.376718	172401.062743	37.099149
1762.004294	172678.632916	37.104167
1763.842862	172936.407993	37.109184
1765.593765	173273.659400	37.114202
1767.697830	173524.723691	37.119220
1769.289231	173813.800543	37.124237
1771.082824	174120.645265	37.129255
1773.053534	174382.683798	37.134272
1775.035989	174682.855563	37.139290
1777.091861	174946.964731	37.144308
1778.516890	175262.934395	37.149325
1780.527795	175530.695390	37.154343
1782.209661	175800.324504	37.159360
1783.850127	176087.392817	37.164378
1785.476986	176388.902313	37.169396
1787.392892	176668.522195	37.174413
1789.022485	176947.339442	37.179431
1790.620106	177257.245724	37.184448
1792.605357	177531.900027	37.189466
1794.259009	177845.785439	37.194484
1795.755431	178113.530803	37.199501
1798.035468	178424.796482	37.204519
1799.759131	178676.194016	37.209536
1801.643813	178958.765024	37.214554
1803.533143	179238.685580	37.219572
1805.475831	179498.667865	37.224589
1807.186623	179787.120861	37.229607
1809.045805	180029.636532	37.234624
1810.866289	180320.270668	37.239642
1812.854809	180574.339913	37.244660
1814.035932	180836.367106	37.249677
1815.954771	181125.912669	37.254695
1817.704399	181385.569190	37.259712
1819.611532	181650.087113	37.264730
1821.518161	181961.374585	37.269748
1823.325179	182211.219163	37.274765
1824.672391	182520.518605	37.279783
1826.871704	182789.095371	37.284800
1828.640931	183078.931511	37.289818
1830.507147	183361.610614	37.294836
1832.140027	183643.199299	37.299853
1834.040857	183947.434371	37.304871
1836.209573	184239.029203	37.309888
1837.400653	184524.233748	37.314906
1839.430358	184838.948045	37.319924
1841.336790	185118.726242	37.324941
1842.887260	185421.047529	37.329959
1844.796851	185715.383192	37.334976
1846.448273	186043.108805	37.339994
1848.535409	186317.637844	37.345012
1850.002433	186672.615655	37.350029
1852.167005	186962.858364	37.355047
1854.231341	187265.249968	37.360064
1856.289990	187580.042176	37.365082
1857.855284	187911.157598	37.370100
1860.146082	188189.916572	37.375117
1862.028015	188514.158973	37.380135
1864.155217	188810.408838	37.385152
1865.657191	189122.685746	37.390170
1868.330718	189406.441870	37.395188
1869.649639	189750.730982	37.400205
1871.607771	190037.421662	37.405223
1873.310293	190349.205327	37.410240
1875.228673	190657.695343	37.415258
1877.686302	190958.208294	37.420276
1879.346068	191272.771301	37.425293
1881.087833	191581.815613	37.430311
1882.980116	191879.086405	37.435328
1885.061732	192180.973808	37.440346
1887.034267	192502.779702	37.445364
1889.180347	192792.858148	37.450381
1890.906208	193095.772186	37.455399
1892.830027	193413.860634	37.460416
1894.836759	193698.966245	37.465434
1896.632048	194009.299223	37.470452
1898.901362	194314.901188	37.475469
1901.001354	194601.177473	37.480487
1902.499312	194893.554014	37.485504
1904.155332	195155.917001	37.490522
1905.994308	195451.237873	37.495540
1908.091133	195714.536450	37.500557
1909.614948	195990.872932	37.505575
1911.417200	196287.892507	37.510592
1912.926478	196548.407586	37.515610
1914.766401	196862.393601	37.520628
1916.577726	197150.760798	37.525645
1918.731585	197433.592248	37.530663
1920.514685	197744.927296	37.535680
1922.463392	198054.638699	37.540698
1924.597833	198344.674704	37.545716
1926.363087	198647.755244	37.550733
1928.206892	198954.315498	37.555751
1930.408174	199263.828943	37.560768
1931.856591	199556.011278	37.565786
1933.979221	199897.767510	37.570804
1936.362331	200186.822186	37.575821
1938.066191	200483.106895	37.580839
1940.219481	200817.121466	37.585856
1942.043195	201130.830801	37.590874
1943.928746	201428.602316	37.595892
1945.818896	201736.237301	37.600909
1947.451236	202088.874323	37.605927
1949.825960	202390.419484	37.610944
1951.401928	202725.971644	37.615962
1953.715374	203051.469835	37.620980
1955.549545	203361.471019	37.625997
1957.261896	203712.468171	37.631015
1959.243753	204006.455542	37.636032
1961.439804	204325.391724	37.641050
1963.297481	204693.229178	37.646068
1965.104265	205008.892473	37.651085
1966.834634	205371.359576	37.656103
1969.043546	205693.411356	37.661120
1971.316438	206039.840162	37.666138
1973.265856	206375.875036	37.671156
1975.212116	206704.308478	37.676173
1977.104275	207043.872570	37.681191
1979.220125	207394.041032	37.686208
1981.337538	207733.814531	37.691226
1983.293420	208057.201540	37.696244
1985.269337	208398.169158	37.701261
1987.152713	208755.021751	37.706279
1989.754870	209068.282838	37.711296
1991.356963	209403.653561	37.716314
1993.542095	209761.187775	37.721332
1995.214959	210079.590574	37.726349
1997.342053	210421.929256	37.731367
1999.460774	210752.756692	37.736384
2001.486176	211117.433325	37.741402
2003.601427	211435.595129	37.746420
2005.843313	211768.439612	37.751437
2007.535225	212112.989365	37.756455
2009.569683	212429.950215	37.761472
2011.775267	212732.755390	37.766490
2013.783805	213034.983864	37.771508
2015.347562	213359.285821	37.776525
2017.825321	213657.303979	37.781543
2019.924775	213962.518517	37.786560
2021.350307	214278.658210	37.791578
2023.293447	214601.839676	37.796596
2025.252013	214923.471364	37.801613
2027.185236	215228.184878	37.806631
2029.102986	215593.094174	37.811648
2031.299344	215886.164735	37.816666
2032.984186	216250.086138	37.821684
2034.951616	216552.311737	37.826701
2037.106723	216926.090581	37.831719
2039.506887	217232.859278	37.836736
2041.443080	217581.956598	37.841754
2043.243766	217924.881277	37.846772
2045.056498	218278.216883	37.851789
2047.382924	218629.758723	37.856807
2049.263457	218965.083213	37.861824
2051.513078	219316.767591	37.866842
2053.345273	219658.857650	37.871860
2055.542015	220022.336474	37.876877
2057.602212	220376.227208	37.881895
2059.997813	220729.736323	37.886912
2061.820048	221092.721193	37.891930
2064.038454	221448.509224	37.896948
2066.018702	221801.797295	37.901965
2068.058560	222164.384627	37.906983
2070.399711	222511.727262	37.912000
2072.352262	222887.854490	37.917018
2074.532048	223244.583985	37.922036
2077.077509	223606.793212	37.927053
2079.064388	223972.152828	37.932071
2081.076200	224336.507083	37.937088
2083.101819	224744.096268	37.942106
2085.094879	225113.320261	37.947124
2087.175011	225467.053582	37.952141
2089.157030	225835.685846	37.957159
2091.493371	226197.800365	37.962176
2093.885135	226556.301485	37.967194
2095.702151	226924.901331	37.972212
2098.018027	227293.944304	37.977229
2099.830753	227652.961031	37.982247
2102.360145	228015.446489	37.987264
2104.011969	228400.497699	37.992282
2105.865312	228758.496792	37.997300
2108.523039	229110.985705	38.002317
2110.191033	229491.594806	38.007335
2112.414010	229863.634993	38.012352
2114.782008	230232.021983	38.017370
2116.978562	230598.786881	38.022388
2119.363118	230964.634557	38.027405
2121.403050	231324.798596	38.032423
2123.572862	231660.054072	38.037440
2125.589606	232006.281334	38.042458
2127.455916	232338.311140	38.047476
2129.886619	232671.293914	38.052493
2131.703068	233022.941000	38.057511
2133.556343	233362.418007	38.062528
2135.956120	233698.863390	38.067546
2138.178489	234058.247049	38.072564
2140.099013	234395.608994	38.077581
2141.833742	234750.526284	38.082599
2143.982710	235106.725258	38.087616
2146.138837	235461.476662	38.092634
2148.150001	235814.880793	38.097652
2150.319207	236176.083828	38.102669
2152.611433	236542.119758	38.107687
2154.755828	236913.641146	38.112704
2157.060548	237267.105299	38.117722
2158.767715	237644.870517	38.122740
2161.074314	238014.287353	38.127757
2163.065253	238399.350528	38.132775
2165.410829	238772.116448	38.137792
2167.545934	239161.807491	38.142810
2169.806724	239536.748376	38.147828
2172.292872	239912.213565	38.152845
2174.482566	240287.269824	38.157863
2176.438164	240681.388702	38.162880
2178.820307	241059.566506	38.167898
2181.007918	241438.589174	38.172916
2183.465240	241825.698225	38.177933
2185.639249	242214.250452	38.182951
2187.976472	242585.404470	38.187968
2190.398864	242986.416559	38.192986
2192.376376	243355.216939	38.198004
2194.988267	243732.731678	38.203021
2197.207342	244129.944245	38.208039
2199.346098	244490.695878	38.213056
2201.602338	244879.065541	38.218074
2203.782193	245268.616889	38.223092
2205.846882	245649.576848	38.228109
2208.268527	246034.215177	38.233127
2210.326599	246415.356143	38.238144
2212.336186	246798.995126	38.243162
2214.216616	247190.860115	38.248180
2217.048675	247568.198372	38.253197
2219.328094	247954.363189	38.258215
2221.367120	248342.853242	38.263232
2224.143260	248736.637878	38.268250
2226.325472	249120.763668	38.273268
2228.568077	249490.706957	38.278285
2230.872114	249884.772637	38.283303
2233.062901	250266.690010	38.288320
2235.473411	250649.106892	38.293338
2237.198420	251029.042421	38.298356
2239.502658	251401.876164	38.303373
2241.870382	251786.385417	38.308391
2243.573251	252156.395006	38.313408
2246.208553	252510.737106	38.318426
2248.623751	252862.777864	38.323444
2250.705115	253222.797621	38.328461
2252.543993	253580.113145	38.333479
2254.937206	253930.762385	38.338496
2257.004771	254311.235022	38.343514
2258.817798	254675.466091	38.348532
2261.313680	255051.477754	38.353549
2263.502191	255423.372928	38.358567
2265.602743	255796.476645	38.363584
2267.858145	256185.559890	38.368602
2269.897392	256565.660339	38.373620
2272.463572	256945.830347	38.378637
2274.363510	257343.913700	38.383655
2276.521659	257742.236265	38.388672
2279.064658	258132.191929	38.393690
2281.155845	258544.218433	38.398708
2283.311937	258942.111570	38.403725
2285.488375	259344.142759	38.408743
2288.040206	259758.409955	38.413760
2290.281328	260151.084036	38.418778
2292.521286	260576.756987	38.423796
2294.861832	260983.489644	38.428813
2297.089606	261405.939694	38.433831
2299.586023	261817.272172	38.438848
2302.291325	262232.001505	38.443866
2304.274279	262660.284050	38.448884
2307.060650	263057.702313	38.453901
2309.146107	263476.062598	38.458919
2311.489692	263907.998490	38.463936
2314.062268	264319.118978	38.468954
2316.542750	264752.024944	38.473972
2318.615558	265153.648678	38.478989
2321.011946	265573.206927	38.484007
2323.024301	265995.468426	38.489024
2326.043090	266414.268413	38.494042
2328.489060	266841.237820	38.499060
2330.739177	267255.130638	38.504077
2333.056508	267674.500259	38.509095
2335.407176	268088.327050	38.514112
2337.581079	268516.255590	38.519130
2340.108355	268932.646174	38.524148
2342.543797	269351.693555	38.529165
2345.133879	269767.871540	38.534183
2347.345841	270181.442376	38.539200
2350.178818	270613.916709	38.544218
2352.110131	271021.918370	38.549236
2354.373332	271437.260002	38.554253
2357.192981	271860.871332	38.559271
2359.242279	272277.390390	38.564288
2361.571192	272692.544308	38.569306
2363.912772	273114.148818	38.574324
2366.526840	273519.020229	38.579341
2368.824914	273930.597518	38.584359
2371.133512	274331.910245	38.589376
2373.818092	274701.917246	38.594394
2375.697450	275101.291249	38.599412
2378.023546	275486.902036	38.604429
2380.139086	275871.606287	38.609447
2382.700127	276271.278755	38.614464
2385.312002	276659.511617	38.619482
2387.368875	277059.695814	38.624500
2389.401009	277447.512428	38.629517
2391.718888	277855.962072	38.634535
2393.631175	278274.510265	38.639552
2396.593751	278675.744606	38.644570
2398.611508	279095.571445	38.649588
2400.949290	279517.811555	38.654605
2403.390293	279930.966149	38.659623
2405.218147	280361.695263	38.664640
2408.122438	280793.650761	38.669658
2410.267152	281215.463474	38.674676
2412.864665	281650.083679	38.679693
2415.361624	282088.021987	38.684711
2417.686184	282534.548235	38.689728
2420.317010	282963.243341	38.694746
2422.883044	283415.319385	38.699764
2425.437660	283847.963401	38.704781
2427.849630	284292.772392	38.709799
2430.396848	284734.917616	38.714816
2432.827421	285174.159543	38.719834
2434.946185	285611.646827	38.724852
2437.808026	286052.851768	38.729869
2440.061262	286499.538128	38.734887
2442.691028	286953.683602	38.739904
2445.546118	287393.541727	38.744922
2447.631160	287845.028889	38.749940
2450.311633	288303.737147	38.754957
2452.991283	288734.450898	38.759975
2455.413298	289182.377237	38.764992
2457.968587	289635.667207	38.770010
2460.869728	290068.096796	38.775028
2463.729799	290505.434980	38.780045
2465.900019	290937.598034	38.785063
2468.312354	291393.727564	38.790080
2470.856707	291829.056038	38.795098
2473.544263	292259.102748	38.800116
2475.946988	292707.559892	38.805133
2478.551526	293144.959550	38.810151
2480.838050	293582.357990	38.815168
2483.375739	294014.457509	38.820186
2486.075509	294462.635610	38.825204
2488.212754	294902.315959	38.830221
2491.055491	295336.320532	38.835239
2492.789805	295792.294923	38.840256
2495.688354	296234.925525	38.845274
2498.045088	296670.096588	38.850292
2500.730478	297118.093440	38.855309
2503.297079	297543.246308	38.860327
2505.671688	297966.548901	38.865344
2508.135866	298379.091354	38.870362
2510.320243	298789.187830	38.875380
2512.967996	299202.842395	38.880397
2515.320043	299619.413227	38.885415
2517.131160	300049.506211	38.890432
2519.990862	300468.839521	38.895450
2522.513862	300892.619578	38.900468
2524.692608	301322.270006	38.905485
2527.310504	301759.165295	38.910503
2529.401566	302203.153599	38.915520
2531.867305	302645.303190	38.920538
2534.310459	303094.897610	38.925556
2536.764198	303555.386058	38.930573
2539.269722	304009.311419	38.935591
2541.511762	304475.317127	38.940608
2543.959608	304939.967871	38.945626
2546.589830	305410.049342	38.950644
2549.096766	305885.889292	38.955661
2551.667219	306367.381839	38.960679
2554.079424	306843.258832	38.965696
2556.698485	307326.848447	38.970714
2559.769632	307818.264123	38.975732
2562.060832	308300.962221	38.980749
2564.874441	308776.768497	38.985767
2567.495160	309276.327073	38.990784
2570.085472	309757.702133	38.995802
2572.924920	310244.623753	39.000820
2575.361645	310730.870590	39.005837
2578.370764	311232.035865	39.010855
2581.265911	311707.335004	39.015872
2584.057448	312186.661671	39.020890
2586.821905	312667.133554	39.025908
2589.537238	313158.405764	39.030925
2592.384199	313627.151414	39.035943
2594.904767	314105.064940	39.040960
2597.738913	314579.675615	39.045978
2600.534849	315045.426080	39.050996
2602.792530	315523.273242	39.056013
2605.771216	315992.241523	39.061031
2608.611733	316477.586042	39.066048
2611.170265	316945.371949	39.071066
2613.657799	317412.709740	39.076084
2616.247348	317872.409770	39.081101
2618.847186	318347.852650	39.086119
2621.399946	318830.970742	39.091136
2623.895602	319308.203193	39.096154
2627.023397	319777.028134	39.101172
2629.343003	320250.575642	39.106189
2631.981381	320721.809876	39.111207
2634.764873	321198.885405	39.116224
2637.168033	321679.193267	39.121242
2639.840940	322146.503465	39.126260
2642.321013	322618.565508	39.131277
2645.102132	323077.726692	39.136295
2647.846075	323539.557947	39.141312
2650.476979	323971.487857	39.146330
2653.049770	324415.919660	39.151348
2655.444839	324863.424782	39.156365
2658.159349	325307.702431	39.161383
2660.357605	325757.265576	39.166400
2663.003873	326202.590426	39.171418
2665.549062	326655.496676	39.176436
2668.139950	327108.012211	39.181453
2671.055247	327569.209721	39.186471
2673.622423	328034.700636	39.191488
2675.812209	328496.286963	39.196506
2678.837152	328961.064979	39.201524
2680.963670	329450.513574	39.206541
2683.693332	329926.480686	39.211559
2686.290786	330415.289803	39.216576
2689.113143	330900.428767	39.221594
2691.981558	331390.915370	39.226612
2694.031218	331890.263794	39.231629
2696.815607	332384.439135	39.236647
2699.632533	332890.693168	39.241664
2702.336872	333386.296333	39.246682
2705.510882	333892.613672	39.251700
2707.759016	334399.277137	39.256717
2710.821618	334903.268683	39.261735
2713.755699	335427.006813	39.266752
2716.177089	335927.181981	39.271770
2719.193157	336435.714845	39.276788
2721.590103	336953.711504	39.281805
2724.464082	337468.226129	39.286823
2727.548583	337973.460940	39.291840
2729.901331	338495.515185	39.296858
2732.917488	339021.954410	39.301876
2735.670880	339540.712148	39.306893
2738.289773	340061.949878	39.311911
2741.073775	340607.074958	39.316928
2744.162059	341112.233762	39.321946
2746.829765	341646.120384	39.326964
2749.599998	342169.881053	39.331981
2752.642396	342692.350083	39.336999
2755.440234	343202.641101	39.342016
2758.274439	343727.368475	39.347034
2761.483410	344243.018873	39.352052
2764.224933	344757.621732	39.357069
2767.373076	345279.340672	39.362087
2770.597885	345793.883363	39.367104
2772.894726	346288.105714	39.372122
2775.915398	346797.467308	39.377140
2778.547602	347318.665732	39.382157
2781.406298	347824.641915	39.387175
2784.716478	348324.906161	39.392192
2787.019821	348833.474568	39.397210
2789.999193	349334.619960	39.402228
2792.677788	349841.698104	39.407245
2795.454745	350333.118119	39.412263
2798.190216	350819.285401	39.417280
2800.763979	351286.485407	39.422298
2803.429026	351751.255302	39.427316
2806.181999	352223.699007	39.432333
2809.089096	352685.503169	39.437351
2811.737969	353165.672069	39.442368
2814.147318	353652.119141	39.447386
2816.835600	354130.952994	39.452404
2819.667289	354626.665591	39.457421
2821.961046	355119.514076	39.462439
2824.569179	355611.775015	39.467456
2827.361743	356124.486434	39.472474
2830.241746	356633.752114	39.477492
2832.486347	357159.459835	39.482509
2835.328904	357679.330912	39.487527
2838.498180	358208.790142	39.492544
2840.980249	358749.266799	39.497562
2843.666938	359268.993577	39.502580
2846.772322	359807.329358	39.507597
2849.549970	360340.304852	39.512615
2852.566416	360889.049000	39.517632
2855.179439	361438.155303	39.522650
2858.272446	361980.047411	39.527668
2861.044495	362541.323750	39.532685
2864.016409	363097.257382	39.537703
2867.150515	363634.200258	39.542720
2870.064577	364198.505141	39.547738
2872.663262	364754.274992	39.552756
2875.532820	365326.110615	39.557773
2878.630399	365885.670661	39.562791
2881.939660	366425.801548	39.567808
2884.806661	367007.488367	39.572826
2888.625132	367555.315979	39.577844
2891.304832	368100.424120	39.582861
2893.846637	368665.442670	39.587879
2897.111913	369220.874065	39.592896
2900.128233	369761.619712	39.597914
2902.968750	370334.004566	39.602932
2906.216621	370882.363015	39.607949
2909.214572	371424.359502	39.612967
2912.408396	371980.959309	39.617984
2915.450926	372538.945973	39.623002
2918.468245	373082.009305	39.628020
2921.200004	373628.815364	39.633037
2924.336343	374176.539776	39.638055
2926.875300	374727.548505	39.643072
2930.008028	375277.212628	39.648090
2933.009555	375813.442792	39.653108
2936.009539	376364.026716	39.658125
2938.765295	376927.708232	39.663143
2942.088037	377464.322411	39.668160
2944.898806	378003.750505	39.673178
2948.035095	378559.382368	39.678196
2950.995589	379111.482431	39.683213
2953.572359	379647.424112	39.688231
2956.651035	380150.983539	39.693248
2959.462368	380674.417560	39.698266
2962.122913	381180.820471	39.703284
2964.862236	381692.633166	39.708301
2967.648744	382201.970865	39.713319
2970.403014	382719.526102	39.718336
2972.953085	383254.584886	39.723354
2975.765009	383782.720168	39.728372
2978.493760	384312.281765	39.733389
2981.214961	384870.298291	39.738407
2984.420626	385407.480339	39.743424
2986.661259	385971.314537	39.748442
2990.001849	386524.870665	39.753460
2992.650070	387102.371092	39.758477
2996.082830	387665.052180	39.763495
2998.645985	388231.895088	39.768512
3001.438241	388825.223363	39.773530
3004.904337	389397.941665	39.778548
3007.756341	389984.951236	39.783565
3010.800916	390586.149040	39.788583
3013.928619	391158.664356	39.793600
3016.831393	391764.353675	39.798618
3020.197966	392353.144670	39.803636
3023.233570	392943.347596	39.808653
3026.410352	393557.331538	39.813671
3029.850963	394141.541020	39.818688
3032.476754	394751.888337	39.823706
3036.034981	395323.024328	39.828724
3038.945478	395956.077484	39.833741
3042.080180	396522.239331	39.838759
3045.177940	397154.530386	39.843776
3048.396840	397727.530548	39.848794
3051.299590	398368.400269	39.853812
3054.517383	398959.002348	39.858829
3058.176527	399545.619241	39.863847
3060.857202	400181.620620	39.868864
3063.911622	400764.330610	39.873882
3066.889158	401361.443660	39.878900
3070.249897	401985.030675	39.883917
3073.159896	402593.794464	39.888935
3076.795095	403182.428456	39.893952
3079.716790	403796.288837	39.898970
3083.320392	404382.928153	39.903988
3086.139620	405006.795370	39.909005
3089.478788	405599.918546	39.914023
3092.551923	406182.349285	39.919040
3095.332225	406824.768455	39.924058
3098.552983	407385.707154	39.929076
3101.944777	408011.882609	39.934093
3104.764872	408610.657890	39.939111
3107.993197	409216.961312	39.944128
3110.749543	409828.498251	39.949146
3113.853216	410451.424796	39.954164
3117.040370	411031.413555	39.959181
3120.334344	411655.425702	39.964199
3123.449147	412217.331236	39.969216
3126.144059	412780.103643	39.974234
3129.244051	413375.343770	39.979252
3132.323905	413917.783331	39.984269
3135.173651	414489.673265	39.989287
3138.145563	415082.339422	39.994304
3141.094603	415646.410693	39.999322
3144.525628	416224.383627	40.004340
3147.223525	416836.063951	40.009357
3150.128929	417415.768732	40.014375
3153.522329	418020.395734	40.019392
3156.296225	418651.512207	40.024410
3159.303813	419238.613792	40.029428
3162.472007	419874.885964	40.034445
3165.322311	420459.579874	40.039463
3168.449642	421104.673792	40.044480
3171.440088	421711.312598	40.049498
3174.886819	422375.988280	40.054516
3178.089601	423016.338690	40.059533
3180.863715	423657.426100	40.064551
3184.383105	424284.598507	40.069568
3187.283805	424974.480665	40.074586
3190.317685	425597.620879	40.079604
3193.782965	426246.948908	40.084621
3196.703898	426965.530177	40.089639
3200.185670	427598.939601	40.094656
3203.722383	428301.150010	40.099674
3206.611825	428950.452969	40.104692
3209.865852	429613.639108	40.109709
3213.434003	430271.794377	40.114727
3216.500412	430980.998886	40.119744
3219.385615	431666.708585	40.124762
3222.986437	432331.037529	40.129780
3226.314052	433032.192128	40.134797
3230.131249	433704.859972	40.139815
3233.126774	434407.245300	40.144832
3236.468796	435067.543210	40.149850
3240.046491	435745.716020	40.154868
3243.556411	436416.866899	40.159885
3246.847626	437084.894542	40.164903
3249.923127	437813.052501	40.169920
3253.505354	438459.853839	40.174938
3257.032794	439159.060346	40.179956
3260.491548	439795.465124	40.184973
3263.588108	440497.284623	40.189991
3266.876665	441150.088104	40.195008
3270.255992	441849.494980	40.200026
3273.909909	442486.558729	40.205044
3277.052445	443145.002980	40.210061
3280.112616	443859.288505	40.215079
3283.519189	444551.271711	40.220096
3286.549123	445217.423537	40.225114
3289.519174	445875.820385	40.230132
3293.609568	446538.932550	40.235149
3296.581638	447229.084351	40.240167
3299.540873	447842.069285	40.245184
3303.536061	448447.686231	40.250202
3306.612994	449063.506123	40.255220
3309.716670	449686.037848	40.260237
3312.544840	450322.212550	40.265255
3315.781436	450950.257315	40.270272
3318.573313	451587.617797	40.275290
3321.397748	452256.791114	40.280308
3324.872070	452947.807565	40.285325
3327.726276	453609.800437	40.290343
3330.593775	454263.067296	40.295360
3334.229020	454956.325364	40.300378
3337.133737	455663.391749	40.305396
3340.287931	456331.229075	40.310413
3343.766370	457038.212093	40.315431
3347.094638	457741.654427	40.320448
3350.429698	458445.630039	40.325466
3353.491352	459189.497332	40.330484
3357.327136	459894.157229	40.335501
3360.084997	460595.878713	40.340519
3363.912708	461296.750868	40.345536
3367.156626	462045.905924	40.350554
3370.039157	462818.009132	40.355572
3373.793192	463553.068885	40.360589
3376.702818	464293.801473	40.365607
3379.592609	465038.305423	40.370624
3383.408971	465787.492839	40.375642
3386.892415	466550.413767	40.380660
3390.906072	467275.694212	40.385677
3394.346512	468058.849517	40.390695
3397.504123	468865.891634	40.395712
3401.096423	469636.118111	40.400730
3404.506555	470373.878374	40.405748
3408.002837	471140.928950	40.410765
3411.098533	471910.340513	40.415783
3414.980288	472682.683585	40.420800
3418.912110	473447.253470	40.425818
3422.237417	474203.042357	40.430836
3426.021533	474996.245961	40.435853
3429.242241	475769.992340	40.440871
3432.776773	476503.467606	40.445888
3436.371479	477305.002787	40.450906
3440.005705	478093.356194	40.455924
3443.633527	478828.703157	40.460941
3446.927284	479593.747469	40.465959
3450.264548	480386.707341	40.470976
3453.727296	481137.461788	40.475994
3457.172100	481893.547876	40.481012
3461.294873	482643.837117	40.486029
3464.746951	483425.082376	40.491047
3468.235907	484185.823259	40.496064
3471.998860	484956.092454	40.501082
3475.202271	485717.727800	40.506100
3478.786980	486472.855371	40.511117
3481.732675	487228.270494	40.516122
3485.346051	487932.128778	40.521127
3488.860834	488581.219865	40.526132
3491.329113	489185.930868	40.531136
3494.105829	489737.086667	40.536141
3496.562760	490236.817167	40.541146
3499.199962	490665.294593	40.546151
3501.416386	491066.681875	40.551156
3503.769381	491440.943297	40.556160
3505.830665	491710.458242	40.561165
3507.461533	491959.222340	40.566170
3509.041303	492133.442971	40.571175
3510.798615	492228.528128	40.576180
3512.753819	492328.443323	40.581184
3513.671077	492406.593383	40.586189
3514.853702	492477.509823	40.591194
3515.712414	492455.799998	40.596199
3517.033047	492407.834462	40.601204
3517.620855	492339.321997	40.606208
3518.355538	492301.830753	40.611213
3518.622669	492188.751162	40.616218
3519.696190	492023.886058	40.621223
3520.256449	491934.055088	40.626228
3519.619347	491758.619998	40.631232
3520.494407	491563.952108	40.636237
3520.575130	491374.421719	40.641242
3520.533484	491226.489759	40.646247
3520.619156	491043.336726	40.651252
3520.717383	490820.978547	40.656256
3521.170297	490576.529606	40.661261
3521.069295	490357.692176	40.666266
3520.380006	490138.337379	40.671271
3521.222455	489882.067133	40.676276
3520.744508	489666.067010	40.681280
3520.669238	489456.180259	40.686285
3520.650704	489241.065047	40.691290
3520.390440	489004.306250	40.696295
3520.372107	488763.656604	40.701300
3519.830334	488505.610996	40.706304
3519.626407	488240.264858	40.711309
3519.900333	487996.418704	40.716314
3519.311032	487800.930339	40.721319
3519.760077	487566.118406	40.726324
3519.230231	487332.268802	40.731328
3518.862678	487077.063749	40.736333
3518.537904	486830.207179	40.741338
3518.542131	486580.610494	40.746343
3518.398283	486344.712103	40.751348
3517.787877	486160.406094	40.756352
3517.579000	485951.768346	40.761357
3517.322823	485721.452737	40.766362
3517.220495	485493.288523	40.771367
3517.086555	485318.068958	40.776372
3516.753511	485096.370640	40.781376
3515.673334	484885.933851	40.786381
3516.093172	484667.607410	40.791386
3516.171924	484460.883972	40.796391
3515.691963	484314.842186	40.801396
3515.101581	484102.748845	40.806400
3515.216839	483920.181373	40.811405
3514.905380	483752.828934	40.816410
3514.220614	483556.349835	40.821415
3514.995674	483357.966002	40.826420
3514.672771	483187.773123	40.831424
3514.139402	483024.908279	40.836429
3513.838943	482857.293058	40.841434
3513.315187	482688.698300	40.846439
3513.612812	482511.105059	40.851444
3513.070089	482373.773820	40.856448
3513.342773	482207.481205	40.861453
3512.749856	482037.726339	40.866458
3512.472433	481919.098250	40.871463
3512.364340	481753.926064	40.876468
3512.527397	481608.674463	40.881472
3512.243591	481487.105786	40.886477
3511.986818	481322.054809	40.891482
3511.530188	481206.288415	40.896487
3511.684605	481043.855795	40.901492
3511.125137	480951.464664	40.906496
3511.234580	480771.402406	40.911501
3511.117778	480696.372064	40.916506
3510.757723	480537.715819	40.921511
3510.940006	480396.759605	40.926516
3510.784613	480319.656246	40.931520
3510.603295	480219.397899	40.936525
3510.040264	480095.837740	40.941530
3510.070055	479977.808188	40.946535
3510.244468	479852.558993	40.951540
3509.397381	479782.252174	40.956544
3509.844359	479645.759013	40.961549
3509.347694	479577.423170	40.966554
3509.138484	479474.023461	40.971559
3509.135763	479371.198712	40.976564
3509.150423	479264.113721	40.981568
3508.995357	479208.594864	40.986573
3509.124453	479081.371511	40.991578
3508.805173	479037.534206	40.996583
3508.640998	478920.137164	41.001588
3508.673753	478820.952852	41.006592
3508.304361	478757.814037	41.011597
3508.201299	478690.983999	41.016602
3507.955202	478591.133099	41.021607
3508.280992	478550.588321	41.026612
3508.280686	478476.899528	41.031616
3508.196841	478370.230738	41.036621
3508.091456	478311.964785	41.041626
3507.565506	478224.319612	41.046631
3507.672358	478170.530293	41.051636
3507.332903	478098.616856	41.056640
3507.677549	478016.256053	41.061645
3507.040265	477970.540770	41.066650
3507.401483	477886.402963	41.071655
3507.535394	477815.579372	41.076660
3507.218869	477810.459812	41.081664
3507.169418	477712.854125	41.086669
3507.095994	477669.228365	41.091674
3506.781148	477593.457375	41.096679
3507.260372	477547.463297	41.101684
3506.604882	477483.301336	41.106688
3506.668676	477440.514997	41.111693
3506.590612	477384.370700	41.116698
3506.483188	477319.107934	41.121703
3506.534661	477314.538283	41.126708
3506.344583	477238.290082	41.131712
3506.339903	477208.438304	41.136717
3506.264629	477138.608366	41.141722
3506.222893	477122.649603	41.146727
3506.077299	477065.400048	41.151732
3506.418020	477002.853030	41.156736
3506.326890	476984.165033	41.161741
3506.171032	476912.826529	41.166746
3506.055127	476893.838259	41.171751
3506.312558	476832.621664	41.176756
3506.093236	476774.825406	41.181760
3506.034227	476744.677420	41.186765
3505.913147	476741.097916	41.191770
3505.848579	476672.075618	41.196775
3506.305208	476647.066515	41.201780
3505.867496	476628.179540	41.206784
3505.840538	476576.586543	41.211789
3506.010445	476550.862362	41.216794
3505.773971	476510.858492	41.221799
3505.739050	476477.006283	41.226804
3505.681303	476437.379501	41.231808
3505.561222	476406.429696	41.236813
3505.651235	476354.817644	41.241818
3504.947087	476313.316045	41.246823
3505.439146	476271.828045	41.251828
3505.125967	476252.819664	41.256832
3505.225819	476217.830632	41.261837
3505.658781	476172.550329	41.266842
3505.480451	476138.416101	41.271847
3506.055026	476120.737183	41.276852
3505.399210	476091.138718	41.281856
3505.521005	476035.516618	41.286861
3505.677528	476035.745273	41.291866
3505.087557	476041.971523	41.296871
3504.740139	475981.506861	41.301876
3504.453056	475961.429664	41.306880
3504.966326	475936.360043	41.311885
3505.818988	475899.680197	41.316890
3504.882294	475892.681382	41.321895
3504.823731	475902.219693	41.326900
3504.916317	475869.410732	41.331904
3504.705500	475820.176449	41.336909
3505.110791	475795.377154	41.341914
3504.967278	475772.185176	41.346919
3505.266928	475723.934407	41.351924
3504.960607	475727.328130	41.356928
3504.980991	475723.827461	41.361933
3504.889875	475722.777395	41.366938
3504.779566	475677.024287	41.371943
3504.632852	475666.251058	41.376948
3504.635529	475664.983415	41.381952
3504.670186	475622.197820	41.386957
3504.672926	475600.655212	41.391962
3504.375344	475583.873981	41.396967
3504.394351	475562.278074	41.401972
3504.512651	475544.113205	41.406976
3504.788545	475510.413002	41.411981
3504.694461	475527.104058	41.416986
3504.385748	475507.638080	41.421991
3504.324972	475478.907736	41.426996
3504.179334	475481.008912	41.432000
3504.466331	475458.863662	41.437005
3504.297326	475441.504426	41.442010
3504.814685	475402.038157	41.447015
3504.766542	475417.860348	41.452020
3504.549651	475405.577434	41.457024
3504.753520	475354.248961	41.462029
3504.772408	475382.022955	41.467034
3504.346580	475350.815727	41.472039
3504.651313	475306.212698	41.477044
3504.813572	475314.145052	41.482048
3504.355918	475285.122342	41.487053
3504.531128	475256.405073	41.492058
3504.513877	475254.430919	41.497063
3504.771370	475242.934632	41.502068
3504.512838	475235.727026	41.507072
3504.585466	475185.229880	41.512077
3504.535351	475214.130156	41.517082
3504.308954	475174.628930	41.522087
3504.601588	475160.339176	41.527092
3504.321539	475159.876514	41.532096
3504.858575	475116.452877	41.537101
3504.466334	475132.735183	41.542106
3504.212012	475083.201852	41.547111
3504.968832	475088.303135	41.552116
3504.492630	475096.843369	41.557120
3504.588445	475054.097597	41.562125
3504.645484	475037.310554	41.567130
3504.267868	475030.172384	41.572135
3504.709495	474981.846721	41.577140
3504.590623	475029.158209	41.582144
3504.282776	474978.112416	41.587149
3504.623107	474949.571372	41.592154
3504.193374	474964.643201	41.597159
3504.602683	474948.256609	41.602164
3504.551979	474925.707951	41.607168
3504.412286	474932.674395	41.612173
3504.156114	474905.494793	41.617178
3504.186982	474903.766445	41.622183
3504.354005	474873.579944	41.627188
3504.733239	474858.617331	41.632192
3504.430087	474866.674108	41.637197
3504.566297	474823.262505	41.642202
3504.046219	474833.330465	41.647207
3504.511367	474786.571989	41.652212
3504.025001	474819.343484	41.657216
3504.577005	474759.544049	41.662221
3504.324654	474794.052731	41.667226
3504.277126	474762.277913	41.672231
3504.865723	474730.909401	41.677236
3504.768333	474755.762634	41.682240
3504.157869	474709.173980	41.687245
3504.224530	474714.384438	41.692250
3504.325088	474688.415405	41.697255
3504.309306	474642.594334	41.702260
3504.218290	474689.952899	41.707264
3504.013529	474670.013479	41.712269
3504.608850	474628.455108	41.717274
3504.379314	474651.099002	41.722279
3504.859521	474591.614561	41.727284
3504.687383	474580.895462	41.732288
3504.235259	474605.298044	41.737293
3504.412409	474595.081337	41.742298
3504.057734	474568.322371	41.747303
3504.354491	474539.584879	41.752308
3504.430402	474509.969829	41.757312
3504.297785	474544.054490	41.762317
3504.282237	474535.084769	41.767322
3504.125019	474534.551989	41.772327
3504.018421	474495.790859	41.777332
3504.402781	474470.537046	41.782336
3504.363313	474465.018010	41.787341
3504.303019	474490.423297	41.792346
3504.260162	474482.471672	41.797351
3504.593790	474462.193506	41.802356
3504.102192	474432.262515	41.807360
3504.569230	474399.037164	41.812365
3504.463269	474428.048764	41.817370
3504.109677	474390.188206	41.822375
3504.793192	474339.237577	41.827380
3504.106554	474367.073775	41.832384
3503.972575	474373.583294	41.837389
3504.371374	474331.497783	41.842394
3504.555002	474305.160298	41.847399
3504.127668	474314.706947	41.852404
3504.395463	474336.157394	41.857408
3504.437498	474298.588971	41.862413
3504.464339	474248.096736	41.867418
3504.325757	474262.210633	41.872423
3504.549356	474221.977454	41.877428
3504.264831	474237.128251	41.882432
3503.896150	474259.338354	41.887437
3504.051364	474214.249655	41.892442
3504.061070	474212.423212	41.897447
3504.347825	474203.253494	41.902452
3504.269019	474206.256673	41.907456
3504.260175	474204.787997	41.912461
3504.084026	474183.120087	41.917466
3504.265427	474176.552246	41.922471
3504.401711	474141.858023	41.927476
3503.620424	474141.575939	41.932480
3504.189608	474119.435324	41.937485
3504.564840	474095.399076	41.942490
3504.334997	474093.914630	41.947495
3504.474634	474126.030695	41.952500
3504.141681	474112.396683	41.957504
3504.200059	474072.138630	41.962509
3504.002578	474061.980866	41.967514
3504.342171	474040.231292	41.972519
3504.601338	474014.844628	41.977524
3504.156269	474025.408042	41.982528
3504.172664	474003.354670	41.987533
3504.491686	473984.396314	41.992538
3503.702140	474005.456616	41.997543
3504.065767	473970.624787	42.002548
3504.082640	473992.622169	42.007552
3504.068412	474003.725797	42.012557
3504.013126	473998.209134	42.017562
3503.710443	473995.468908	42.022567
3503.818720	473971.677472	42.027572
3504.257172	473936.985835	42.032576
3503.928769	473937.899457	42.037581
3503.991723	473946.202882	42.042586
3503.975325	473937.892023	42.047591
3504.301324	473944.937277	42.052596
3503.821899	473936.294066	42.057600
3504.112408	473908.823963	42.062605
3503.936178	473886.648834	42.067610
3504.156958	473868.973190	42.072615
3504.470113	473894.218812	42.077620
3504.187074	473891.982383	42.082624
3503.959556	473866.165538	42.087629
3503.454424	473863.051757	42.092634
3503.641482	473868.091328	42.097639
3503.869924	473860.248657	42.102644
3503.865250	473872.009839	42.107648
3504.029878	473851.757778	42.112653
3504.154044	473842.360136	42.117658
3503.687358	473865.498609	42.122663
3503.925380	473860.797312	42.127668
3504.277999	473836.967101	42.132672
3503.472674	473809.416601	42.137677
3503.746657	473789.958264	42.142682
3503.253622	473795.003958	42.147687
3503.412757	473800.098650	42.152692
3503.465032	473799.988967	42.157696
3503.687295	473813.488531	42.162701
3503.815979	473807.334439	42.167706
3503.824448	473817.471435	42.172711
3504.184231	473787.202168	42.177716
3504.448401	473775.045004	42.182720
3503.985246	473813.644018	42.187725
3503.828451	473816.254046	42.192730
3504.077411	473796.242059	42.197735
3504.225909	473774.573097	42.202740
3503.974216	473790.428723	42.207744
3503.920779	473779.589058	42.212749
3504.233156	473718.354379	42.217754
3504.038206	473692.380091	42.222759
3503.862880	473684.601169	42.227764
3504.263828	473684.030839	42.232768
3504.113007	473666.869982	42.237773
3504.115924	473674.067777	42.242778
3503.772099	473702.763157	42.247783
3504.209934	473668.375315	42.252788
3503.937525	473653.818966	42.257792
3503.941450	473689.759086	42.262797
3504.246486	473686.314462	42.267802
3504.025122	473678.289353	42.272807
3503.991239	473659.893394	42.277812
3504.109670	473652.879108	42.282816
3504.125904	473639.899282	42.287821
3503.906263	473608.454021	42.292826
3503.712991	473610.208070	42.297831
3503.958127	473604.187588	42.302836
3503.854804	473604.609419	42.307840
3503.695683	473605.699070	42.312845
3503.894284	473598.925556	42.317850
3503.473026	473588.549462	42.322855
3503.483468	473569.842263	42.327860
3503.576303	473574.491258	42.332864
3503.752946	473587.744720	42.337869
3504.287089	473599.775746	42.342874
3504.154100	473598.478725	42.347879
3504.284695	473593.845038	42.352884
3504.316352	473584.613977	42.357888
3504.058776	473586.682346	42.362893
3504.338338	473566.969453	42.367898
3504.091985	473536.897001	42.372903
3504.240917	473536.011651	42.377908
3504.374853	473533.253046	42.382912
3504.395031	473515.558110	42.387917
3504.587141	473502.854555	42.392922
3504.233955	473474.471752	42.397927
3503.990175	473441.762732	42.402932
3504.097925	473432.012648	42.407936
3504.387558	473418.482543	42.412941
3504.283447	473383.520870	42.417946
3504.296897	473387.371368	42.422951
3504.215174	473360.111439	42.427956
3503.922466	473356.761233	42.432960
3503.690852	473399.582643	42.437965
3503.755258	473411.992179	42.442970
3503.809551	473410.716238	42.447975
3504.090708	473370.928523	42.452980
3503.640310	473356.146629	42.457984
3503.514160	473356.470687	42.462989
3503.475696	473349.430400	42.467994
3503.995555	473328.868212	42.472999
3503.966269	473315.489830	42.478004
3503.988342	473320.150068	42.483008
3504.048255	473316.034420	42.488013
3503.882763	473352.001910	42.493018
3503.904974	473355.192020	42.498023
3504.177081	473334.162065	42.503028
3503.888672	473303.487599	42.508032
3503.499562	473299.899154	42.513037
3504.228771	473282.497499	42.518042
3504.320158	473281.773313	42.523047
3503.927190	473276.461906	42.528052
3504.001259	473286.842263	42.533056
3503.624987	473277.675536	42.538061
3504.596664	473237.220801	42.543066
3503.838587	473258.530360	42.548071
3504.007987	473219.064173	42.553076
3504.241142	473195.252098	42.558080
3504.206639	473251.577794	42.563085
3504.240854	473207.570557	42.568090
3504.505158	473163.678941	42.573095
3504.451086	473185.333550	42.578100
3504.096429	473169.269052	42.583104
3503.885473	473161.242095	42.588109
3504.490762	473126.015782	42.593114
3504.183547	473113.745759	42.598119
3504.116341	473144.578025	42.603124
3504.328119	473114.686012	42.608128
3503.983598	473116.058459	42.613133
3504.234406	473090.722664	42.618138
3504.305280	473085.135122	42.623143
3503.873873	473072.479154	42.628148
3504.250192	473067.603738	42.633152
3504.094718	473037.313413	42.638157
3504.433562	473052.011706	42.643162
3504.149873	473024.276313	42.648167
3503.934613	473013.309736	42.653172
3504.113551	473016.779292	42.658176
3504.033305	472996.108842	42.663181
3504.080784	472985.607663	42.668186
3503.946441	472991.407963	42.673191
3504.209426	472974.738755	42.678196
3503.790529	472950.066268	42.683200
3504.066832	472954.838489	42.688205
3504.385819	472935.929864	42.693210
3503.458172	472965.073406	42.698215
3503.914092	472924.091243	42.703220
3504.088586	472890.149270	42.708224
3503.598636	472940.971446	42.713229
3503.780077	472921.729689	42.718234
3503.957171	472907.811481	42.723239
3503.683691	472932.086434	42.728244
3503.937564	472880.034117	42.733248
3503.818174	472911.736781	42.738253
3504.219323	472889.418623	42.743258
3504.129069	472885.174541	42.748263
3503.613395	472909.386410	42.753268
3503.709820	472858.778359	42.758272
3503.825678	472854.400306	42.763277
3503.354671	472865.171191	42.768282
3503.840241	472856.831251	42.773287
3503.665181	472885.855960	42.778292
3503.473319	472874.125198	42.783296
3503.780560	472857.246124	42.788301
3503.871291	472895.353769	42.793306
3503.639464	472853.364892	42.798311
3503.680238	472856.805617	42.803316
3503.721770	472831.350496	42.808321
3503.896391	472857.126238	42.813325
3504.269756	472833.392972	42.818330
3503.930925	472836.234671	42.823335
3503.829028	472838.278509	42.828340
3504.043110	472796.066956	42.833345
3503.810824	472835.493125	42.838349
3504.118363	472803.659141	42.843354
3503.397309	472828.157038	42.848359
3503.481078	472783.482034	42.853364
3503.727194	472762.100740	42.858369
3503.439542	472802.803084	42.863373
3503.807736	472781.858765	42.868378
3503.706546	472797.336510	42.873383
3504.088242	472792.510874	42.878388
3504.051679	472779.437458	42.883393
3503.465281	472786.576623	42.888397
3503.938654	472760.140663	42.893402
3503.741781	472747.802287	42.898407
3503.648395	472770.376047	42.903412
3503.440726	472754.845632	42.908417
3504.073185	472751.602576	42.913421
3503.592015	472779.661925	42.918426
3503.981169	472749.031624	42.923431
3503.942013	472760.697505	42.928436
3503.777693	472737.505359	42.933441
3503.729101	472731.936602	42.938445
3503.964961	472736.816656	42.943450
3504.109637	472717.783297	42.948455
3504.008712	472728.445067	42.953460
3504.319943	472692.909627	42.958465
3503.833335	472708.397660	42.963469
3504.204992	472692.927719	42.968474
3503.898084	472704.788033	42.973479
3503.966637	472659.202661	42.978484
3504.006165	472682.820100	42.983489
3503.715052	472654.983991	42.988493
3504.117475	472635.149398	42.993498
3504.015676	472648.396781	42.998503
3503.881493	472624.946271	43.003508
3503.455406	472657.204749	43.008513
3503.719348	472617.012737	43.013517
3503.568984	472634.475475	43.018522
3503.399448	472649.457186	43.023527
3503.618581	472631.121704	43.028532
3503.575479	472611.560282	43.033537
3503.509840	472631.189509	43.038541
3503.956960	472603.540822	43.043546
3503.841299	472630.224540	43.048551
3504.207556	472610.953282	43.053556
3504.206825	472597.823393	43.058561
3503.853705	472612.225808	43.063565
3504.099625	472574.115048	43.068570
3503.938660	472553.406215	43.073575
3503.582433	472597.110808	43.078580
3503.634739	472576.773850	43.083585
3503.538549	472575.217472	43.088589
3503.708009	472532.505481	43.093594
3503.677724	472561.000816	43.098599
3503.299402	472553.050767	43.103604
3503.677754	472552.027726	43.108609
3503.785364	472565.191371	43.113613
3504.107593	472568.486271	43.118618
3503.479668	472571.069528	43.123623
3503.778816	472533.660010	43.128628
3503.760295	472512.168197	43.133633
3503.427940	472557.542038	43.138637
3503.675348	472527.897015	43.143642
3504.024589	472529.362631	43.148647
3503.324765	472528.003043	43.153652
3503.904421	472510.168119	43.158657
3504.069644	472543.245831	43.163661
3503.421226	472528.950889	43.168666
3503.789004	472492.240179	43.173671
3503.626458	472518.069636	43.178676
3504.060854	472486.367197	43.183681
3503.756247	472513.030234	43.188685
3504.125329	472521.640719	43.193690
3504.032395	472475.421427	43.198695
3504.238051	472490.749516	43.203700
3504.158009	472458.418609	43.208705
3504.152523	472479.610025	43.213709
3503.876019	472454.863741	43.218714
3503.945249	472421.495279	43.223719
3503.948231	472434.269982	43.228724
3504.181052	472462.673174	43.233729
3504.021393	472408.454434	43.238733
3504.052229	472426.953311	43.243738
3503.963638	472386.765872	43.248743
3503.759138	472421.930029	43.253748
3503.544197	472421.203532	43.258753
3503.786938	472372.142713	43.263757
3504.075975	472356.989751	43.268762
3503.755477	472396.380007	43.273767
3504.018920	472345.592210	43.278772
3504.164637	472381.106649	43.283777
3503.543084	472390.431408	43.288781
3503.408402	472336.208530	43.293786
3503.774684	472329.509488	43.298791
3503.521514	472344.453943	43.303796
3504.012042	472305.898463	43.308801
3503.732466	472362.113245	43.313805
3503.862236	472339.178342	43.318810
3503.945930	472322.993203	43.323815
3503.550899	472328.378631	43.328820
3504.168434	472284.682789	43.333825
3503.413540	472316.943071	43.338829
3503.791987	472312.624793	43.343834
3503.326814	472326.538161	43.348839
3503.730686	472290.632516	43.353844
3503.678616	472342.046007	43.358849
3503.384338	472325.312262	43.363853
3504.303998	472284.204836	43.368858
3503.755227	472318.206886	43.373863
3503.765727	472276.077138	43.378868
3503.816789	472306.182230	43.383873
3503.910503	472275.445832	43.388877
3503.758067	472300.462833	43.393882
3503.640634	472256.680310	43.398887
3504.219882	472236.310428	43.403892
3503.785787	472278.811305	43.408897
3503.475040	472252.346536	43.413901
3503.927541	472223.479792	43.418906
3503.813624	472272.114964	43.423911
3503.258911	472253.952149	43.428916
3504.070208	472208.653954	43.433921
3503.483475	472247.833094	43.438925
3503.757859	472211.998473	43.443930
3503.809659	472235.310311	43.448935
3504.045868	472208.759040	43.453940
3503.985160	472248.666173	43.458945
3503.845551	472198.752848	43.463949
3504.169785	472194.595201	43.468954
3503.629807	472202.031405	43.473959
3503.931309	472188.802791	43.478964
3504.045764	472190.964586	43.483969
3504.321065	472160.047229	43.488973
3504.007917	472160.552947	43.493978
3504.059901	472162.775315	43.498983
3503.958873	472143.323994	43.503988
3504.204609	472126.301955	43.508993
3503.621516	472120.868207	43.513997
3504.098756	472139.651660	43.519002
3503.967014	472123.855287	43.524007
3503.946832	472075.240884	43.529012
3504.318640	472106.208105	43.534017
3503.687897	472084.052166	43.539021
3504.597531	472054.352494	43.544026
3503.989023	472086.792784	43.549031
3503.979591	472076.756401	43.554036
3504.016875	472052.061430	43.559041
3504.236886	472009.695240	43.564045
3504.266088	472007.966911	43.569050
3503.905753	472029.519053	43.574055
3503.661056	472003.246309	43.579060
3504.097585	472012.454705	43.584065
3503.857962	471972.188934	43.589069
3503.915385	471991.393750	43.594074
3504.231286	471963.917035	43.599079
3504.088160	471972.304527	43.604084
3504.093130	471972.607882	43.609089
3503.726667	471937.228944	43.614093
3503.791270	471934.835960	43.619098
3503.916202	471977.249104	43.624103
3503.556596	471932.743722	43.629108
3504.130532	471902.133655	43.634113
3503.489675	471955.212762	43.639117
3503.598576	471908.402636	43.644122
3503.758831	471932.610213	43.649127
3503.446002	471927.589967	43.654132
3503.866856	471912.618631	43.659137
3503.502742	471960.077365	43.664141
3503.725343	471914.415300	43.669146
3503.587893	471907.897130	43.674151
3503.549842	471902.123697	43.679156
3503.994310	471881.014319	43.684161
3503.720721	471907.977416	43.689165
3503.854866	471870.846257	43.694170
3503.865135	471926.813629	43.699175
3503.621505	471890.097088	43.704180
3504.231012	471837.124086	43.709185
3503.692819	471879.692933	43.714189
3503.716858	471893.985541	43.719194
3503.571217	471877.177244	43.724199
3503.648626	471863.578267	43.729204
3503.662609	471862.207209	43.734209
3503.446455	471891.696083	43.739213
3504.121328	471849.409762	43.744218
3503.755672	471868.935043	43.749223
3503.789345	471828.270921	43.754228
3503.815354	471856.606242	43.759233
3503.412121	471834.059198	43.764237
3504.038482	471841.311191	43.769242
3503.931083	471866.828566	43.774247
3503.456993	471847.588019	43.779252
3503.574319	471832.157631	43.784257
3503.398676	471845.670685	43.789261
3503.573499	471833.932071	43.794266
3503.657603	471814.603270	43.799271
3503.764124	471824.370875	43.804276
3503.771672	471815.092133	43.809281
3503.588661	471810.761095	43.814285
3503.462412	471821.325944	43.819290
3504.021335	471809.678699	43.824295
3503.494977	471812.245995	43.829300
3504.015066	471776.828057	43.834305
3503.358079	471792.546491	43.839309
3503.723342	471776.671300	43.844314
3503.523970	471775.688835	43.849319
3503.668096	471792.801560	43.854324
3504.044149	471776.975361	43.859329
3503.795775	471770.778860	43.864333
3503.553282	471773.960356	43.869338
3504.145125	471756.579129	43.874343
3503.711341	471748.789624	43.879348
3503.813443	471760.839320	43.884353
3503.864119	471760.628485	43.889357
3504.206099	471741.563041	43.894362
3503.845866	471731.429843	43.899367
3503.707221	471734.290750	43.904372
3504.057091	471715.883096	43.909377
3504.135325	471714.907449	43.914381
3503.553389	471722.857426	43.919386
3503.736242	471688.861456	43.924391
3503.362732	471686.233505	43.929396
3503.785804	471685.558235	43.934401
3503.653687	471682.942828	43.939405
3503.827136	471678.961001	43.944410
3503.566755	471699.787928	43.949415
3503.874902	471696.038300	43.954420
3504.076553	471687.793462	43.959425
3504.054614	471668.329193	43.964429
3503.774098	471643.988145	43.969434
3503.786833	471652.706013	43.974439
3503.992638	471662.762187	43.979444
3504.068107	471636.336980	43.984449
3503.816773	471623.905142	43.989453
3503.792958	471612.958256	43.994458
3503.783705	471624.721448	43.999463
3503.221362	471623.796343	44.004468
3503.946999	471618.104919	44.009473
3503.418666	471613.574931	44.014477
3503.568601	471621.257182	44.019482
3503.576473	471635.451131	44.024487
3503.975398	471600.102737	44.029492
3503.800654	471593.336875	44.034497
3503.738205	471594.259259	44.039501
3503.881070	471579.230224	44.044506
3503.904814	471587.033828	44.049511
3503.784844	471591.868999	44.054516
3503.774113	471561.097348	44.059521
3503.707917	471567.698435	44.064525
3503.863029	471549.879086	44.069530
3503.859166	471557.889853	44.074535
3503.476327	471582.639954	44.079540
3503.864520	471545.265269	44.084545
3503.368849	471578.905260	44.089549
3503.816219	471540.152383	44.094554
3503.625825	471533.135487	44.099559
3503.515649	471557.183457	44.104564
3503.703800	471517.051978	44.109569
3504.226415	471524.472573	44.114573
3503.826444	471553.737494	44.119578
3503.789450	471519.877388	44.124583
3504.200155	471528.481712	44.129588
3503.958880	471500.179887	44.134593
3503.721842	471505.185674	44.139597
3503.742058	471501.937797	44.144602
3504.029132	471501.740294	44.149607
3503.696173	471476.139898	44.154612
3503.697963	471481.260036	44.159617
3503.853539	471453.909378	44.164621
3503.481404	471479.469074	44.169626
3503.251008	471475.044059	44.174631
3503.759606	471445.052015	44.179636
3503.755351	471481.402869	44.184641
3503.492857	471470.747119	44.189645
3503.997351	471433.100362	44.194650
3503.760338	471456.357331	44.199655
3503.410336	471428.833058	44.204660
3503.633638	471449.583790	44.209665
3503.318114	471423.422898	44.214669
3503.501388	471460.048338	44.219674
3503.309078	471458.456369	44.224679
3503.338481	471430.567947	44.229684
3503.989374	471415.154314	44.234689
3503.466218	471462.690023	44.239693
3503.648810	471432.242509	44.244698
3503.784922	471466.543295	44.249703
3503.443724	471440.183692	44.254708
3503.505012	471448.488390	44.259713
3503.605423	471458.054344	44.264717
3503.673723	471455.103046	44.269722
3503.590371	471437.878965	44.274727
3503.726906	471413.522428	44.279732
3503.559600	471438.999102	44.284737
3503.587479	471414.051366	44.289741
3503.478424	471421.267647	44.294746
3503.821952	471427.601231	44.299751
3503.689737	471419.459751	44.304756
3503.611115	471417.140042	44.309761
3503.609554	471434.276090	44.314765
3503.749678	471412.048289	44.319770
3503.801123	471400.582418	44.324775
3503.476864	471403.422008	44.329780
3503.649202	471382.203039	44.334785
3503.168159	471382.329728	44.339789
3503.253429	471404.116280	44.344794
3503.564706	471394.992136	44.349799
3503.527972	471399.205822	44.354804
3503.346987	471381.084564	44.359809
3503.209666	471407.164912	44.364813
3503.499913	471393.329196	44.369818
3503.440893	471389.688242	44.374823
3503.394133	471399.632368	44.379828
3503.476963	471403.675063	44.384833
3503.823196	471402.758441	44.389837
3503.871297	471400.773586	44.394842
3503.656136	471390.921478	44.399847
3503.486906	471424.358033	44.404852
3503.422233	471397.751880	44.409857
3503.488991	471418.578083	44.414861
3503.525896	471408.331261	44.419866
3503.730680	471389.033687	44.424871
3503.481440	471362.710148	44.429876
3503.901815	471372.428363	44.434881
3503.788632	471399.772352	44.439885
3503.634708	471364.612330	44.444890
3503.947127	471394.119768	44.449895
3503.348041	471361.210104	44.454900
3503.529228	471404.781584	44.459905
3503.375905	471374.387076	44.464909
3503.592630	471405.734746	44.469914
3503.667319	471352.743636	44.474919
3503.444086	471367.734763	44.479924
3503.538234	471342.015998	44.484929
3503.399724	471390.707831	44.489933
3503.560966	471366.752916	44.494938
3503.958894	471336.068436	44.499943
3503.644950	471392.646174	44.504948
3503.695864	471354.868171	44.509953
3503.685284	471390.713206	44.514957
3503.876887	471344.091522	44.519962
3503.908648	471349.206957	44.524967
3503.965589	471326.890815	44.529972
3503.774630	471329.557253	44.534977
3503.902285	471332.528220	44.539981
3503.790476	471352.115264	44.544986
3503.431663	471310.194008	44.549991
3503.704171	471282.875341	44.554996
3503.504788	471295.784128	44.560001
3503.975596	471269.448064	44.565005
3503.713353	471309.490260	44.570010
3503.609977	471280.355171	44.575015
3503.383792	471312.432059	44.580020
3504.184440	471290.201127	44.585025
3504.074499	471288.038448	44.590029
3503.557282	471275.496329	44.595034
3503.705235	471272.938001	44.600039
3503.717054	471250.882399	44.605044
3503.717030	471281.453343	44.610049
3503.692346	471256.057442	44.615053
3503.806998	471259.182569	44.620058
3503.850598	471279.150704	44.625063
3503.140550	471243.469994	44.630068
3504.001346	471208.301424	44.635073
3503.917972	471239.037699	44.640077
3503.861424	471232.912115	44.645082
3504.198761	471218.359064	44.650087
3503.584664	471254.857401	44.655092
3503.846936	471195.752461	44.660097
3504.113330	471175.177493	44.665101
3503.811222	471186.074650	44.670106
3503.812519	471225.365580	44.675111
3503.874684	471209.639256	44.680116
3503.947413	471176.014738	44.685121
3503.570228	471161.929466	44.690125
3503.667047	471164.956030	44.695130
3503.827047	471154.233341	44.700135
3503.829314	471171.875985	44.705140
3503.684269	471161.100116	44.710145
3503.875162	471138.255616	44.715149
3504.045424	471151.714452	44.720154
3503.876360	471128.774738	44.725159
3503.791857	471096.898689	44.730164
3503.660540	471114.511797	44.735169
3503.823893	471153.574456	44.740173
3503.521448	471124.622705	44.745178
3504.185760	471088.876606	44.750183
3503.885308	471092.219462	44.755188
3503.655434	471116.641751	44.760193
3503.505086	471118.946908	44.765197
3503.569543	471104.791796	44.770202
3503.838136	471109.261476	44.775207
3503.335403	471097.477437	44.780212
3503.756384	471089.248394	44.785217
3503.495100	471085.588656	44.790221
3503.730645	471043.015236	44.795226
3503.579077	471072.393672	44.800231
3503.504202	471070.073332	44.805236
3503.792857	471039.101491	44.810241
3503.705177	471088.343685	44.815245
3503.448144	471062.477283	44.820250
3503.845534	471038.281872	44.825255
3503.574046	471074.675676	44.830260
3503.571451	471092.116363	44.835265
3503.680823	471054.683463	44.840269
3503.743437	471064.762559	44.845274
3503.790344	471040.622544	44.850279
3503.808154	471019.579724	44.855284
3503.923934	471049.372226	44.860289
3503.706085	471031.611378	44.865293
3504.143185	471002.745367	44.870298
3504.093810	470971.877550	44.875303
3503.575440	471022.252648	44.880308
3503.561671	470999.237547	44.885313
3503.823970	470972.883362	44.890317
3503.652801	471013.672219	44.895322
3503.912717	470977.685651	44.900327
3503.668322	470972.400860	44.905332
3503.725263	470986.029811	44.910337
3503.586012	471001.160026	44.915341
3503.428907	470982.172764	44.920346
3503.258612	470974.341320	44.925351
3503.296702	470968.606291	44.930356
3503.473942	470960.770613	44.935361
3503.383685	470967.882683	44.940365
3503.866430	470941.747112	44.945370
3503.620459	470944.523692	44.950375
3503.647304	470955.825268	44.955380
3503.954338	470946.194609	44.960385
3503.711799	470943.140270	44.965389
3503.505968	470967.711031	44.970394
3503.561421	470962.784438	44.975399
3503.686127	470935.539372	44.980404
3503.732708	470945.316867	44.985409
3503.720282	470965.040665	44.990413
3503.761853	470938.265033	44.995418
3503.777657	470960.620718	45.000423
3503.779421	470932.989490	45.005428
3503.901748	470910.611867	45.010433
3503.546907	470942.760359	45.015437
3503.542400	470908.235033	45.020442
3504.070193	470914.742448	45.025447
3503.813055	470916.151924	45.030452
3503.876289	470878.624601	45.035457
3503.636017	470936.459417	45.040461
3503.560365	470911.983730	45.045466
3503.944564	470868.676672	45.050471
3503.783569	470858.105962	45.055476
3503.553405	470894.949843	45.060481
3503.323804	470871.664518	45.065485
3503.741069	470858.974450	45.070490
3503.881242	470909.195041	45.075495
3503.761657	470882.546205	45.080500
3503.610282	470888.299087	45.085505
3503.510751	470864.689003	45.090509
3503.785750	470849.993450	45.095514
3503.996611	470851.126166	45.100519
3503.677765	470858.375800	45.105524
3503.998187	470842.963275	45.110529
3503.930465	470868.272813	45.115533
3503.828834	470835.232990	45.120538
3504.040262	470841.182040	45.125543
3503.967716	470818.936516	45.130548
3503.867147	470822.754815	45.135553
3503.750024	470837.780253	45.140557
3503.614121	470796.126920	45.145562
3503.629812	470812.348169	45.150567
3503.429620	470797.474186	45.155572
3503.698492	470787.646689	45.160577
3503.498489	470776.270913	45.165581
3503.493845	470773.483145	45.170586
3503.608476	470803.124085	45.175591
3503.952192	470766.921110	45.180596
3503.981727	470816.398921	45.185601
3503.462718	470776.935468	45.190605
3503.840679	470762.629175	45.195610
3503.677422	470756.114719	45.200615
3503.530651	470754.262001	45.205620
3503.596674	470760.436853	45.210625
3503.654465	470733.050000	45.215629
3503.490552	470779.871402	45.220634
3503.569122	470752.531990	45.225639
3503.536842	470784.680445	45.230644
3503.557315	470743.205088	45.235649
3503.900863	470769.058139	45.240653
3503.380746	470752.713708	45.245658
3503.862598	470750.001145	45.250663
3503.545026	470739.556520	45.255668
3503.681797	470745.111802	45.260673
3503.644904	470721.187457	45.265677
3503.497848	470750.667034	45.270682
3503.762428	470713.918781	45.275687
3503.667602	470748.764251	45.280692
3503.635929	470732.697501	45.285697
3503.629045	470727.628606	45.290701
3503.640315	470736.042895	45.295706
3503.688843	470689.898649	45.300711
3503.646634	470682.858043	45.305716
3503.741764	470713.668283	45.310721
3503.781277	470674.876854	45.315725
3503.546001	470716.943915	45.320730
3503.336872	470701.107985	45.325735
3503.663005	470685.238145	45.330740
3503.541962	470723.231174	45.335745
3503.362015	470729.394211	45.340749
3503.153617	470703.621073	45.345754
3503.945122	470676.320979	45.350759
3503.395778	470697.955077	45.355764
3503.541771	470719.175056	45.360769
3503.330225	470693.757300	45.365773
3503.627228	470670.946215	45.370778
3503.429345	470698.608713	45.375783
3503.221981	470682.620392	45.380788
3503.752769	470653.688389	45.385793
3503.667722	470651.014712	45.390797
3503.286666	470706.489537	45.395802
3503.380676	470682.240261	45.400807
3503.725292	470666.113987	45.405812
3503.685918	470652.887571	45.410817
3503.589378	470687.175719	45.415821
3503.436778	470691.002265	45.420826
3503.144349	470680.300139	45.425831
3503.733567	470664.997098	45.430836
3504.144722	470657.783431	45.435841
3503.809899	470642.575718	45.440845
3503.528507	470632.176021	45.445850
3503.867049	470610.118799	45.450855
3503.236631	470648.648769	45.455860
3503.307469	470668.968084	45.460865
3503.321250	470637.633491	45.465869
3503.447149	470658.400412	45.470874
3503.631335	470649.498827	45.475879
3503.482808	470655.352722	45.480884
3503.595526	470668.973066	45.485889
3503.589721	470659.746616	45.490893
3503.453045	470666.561928	45.495898
3503.767844	470649.578461	45.500903
3503.465228	470648.003863	45.505908
3503.322991	470670.182041	45.510913
3503.649677	470658.520159	45.515917
3503.402836	470642.436647	45.520922
3503.508477	470671.825697	45.525927
3503.609048	470667.905895	45.530932
3503.601408	470644.433135	45.535937
3503.543054	470641.045443	45.540941
3503.328647	470625.007491	45.545946
3503.409009	470640.356757	45.550951
3503.636976	470618.722618	45.555956
3503.468487	470623.920581	45.560961
3503.705173	470640.157735	45.565965
3503.526683	470633.392151	45.570970
3503.555231	470633.286201	45.575975
3503.432245	470633.863298	45.580980
3503.580995	470647.123063	45.585985
3503.844646	470645.205468	45.590989
3503.354787	470637.880701	45.595994
3503.777925	470647.193224	45.600999
3503.685199	470635.344119	45.606004
3503.621832	470626.937947	45.611009
3503.605483	470629.272679	45.616013
3503.375190	470608.927751	45.621018
3503.743409	470604.965635	45.626023
3503.588057	470625.574241	45.631028
3503.643145	470609.848581	45.636033
3503.563067	470620.457444	45.641037
3503.588205	470624.255911	45.646042
3503.868428	470610.471958	45.651047
3503.587006	470614.623077	45.656052
3503.466465	470625.998828	45.661057
3504.082191	470610.894356	45.666061
3503.769157	470587.267000	45.671066
3503.781341	470596.188199	45.676071
3503.555476	470591.204581	45.681076
3503.472931	470577.173743	45.686081
3503.602041	470582.983778	45.691085
3503.632526	470591.293689	45.696090
3503.805123	470577.881623	45.701095
3503.609128	470583.134643	45.706100
3503.529507	470581.068497	45.711105
3503.669196	470539.320392	45.716109
3503.435030	470552.590038	45.721114
3503.582932	470555.152317	45.726119
3503.506093	470547.610141	45.731124
3503.724758	470540.071957	45.736129
3503.958392	470567.869227	45.741133
3503.858489	470535.994751	45.746138
3503.696290	470567.606377	45.751143
3503.777252	470531.596620	45.756148
3503.639802	470530.756407	45.761153
3503.929154	470515.754150	45.766157
3503.674225	470523.906398	45.771162
3503.960396	470519.399534	45.776167
3503.838993	470519.469384	45.781172
3503.702759	470492.822679	45.786177
3503.824845	470487.834742	45.791181
3503.486821	470489.459830	45.796186
3503.878480	470476.469376	45.801191
3503.623348	470470.425653	45.806196
3503.594389	470484.930411	45.811201
3503.940987	470499.223702	45.816205
3503.615671	470474.026458	45.821210
3503.924026	470457.348053	45.826215
3503.555300	470468.915215	45.831220
3503.771724	470438.917198	45.836225
3503.922358	470431.034825	45.841229
3503.597263	470455.320841	45.846234
3503.790789	470436.683263	45.851239
3503.723075	470459.458290	45.856244
3503.784853	470434.858919	45.861249
3503.877094	470412.029213	45.866253
3503.840332	470409.347873	45.871258
3503.884856	470391.342207	45.876263
3503.531444	470419.435260	45.881268
3503.759477	470413.467256	45.886273
3504.084949	470391.665370	45.891277
3503.485544	470385.726735	45.896282
3503.428594	470385.887799	45.901287
3503.776720	470385.883439	45.906292
3503.738927	470377.828027	45.911297
3503.883323	470373.090037	45.916301
3503.822656	470374.468497	45.921306
3503.876557	470375.676747	45.926311
3503.593523	470363.350562	45.931316
3503.748961	470337.468765	45.936321
3503.722395	470343.303472	45.941325
3503.529288	470335.982396	45.946330
3503.654633	470332.362817	45.951335
3503.705173	470348.122616	45.956340
3503.693480	470321.963013	45.961345
3503.685718	470340.926160	45.966349
3503.348323	470354.212247	45.971354
3503.700517	470337.324016	45.976359
3503.191932	470338.823971	45.981364
3503.404607	470334.683587	45.986369
3503.554954	470327.865929	45.991373
3503.254335	470327.051497	45.996378
3503.624248	470304.127086	46.001383
3503.432792	470316.376122	46.006388
3503.490105	470318.090841	46.011393
3503.593179	470307.224612	46.016397
3503.145840	470316.826964	46.021402
3503.588230	470308.949134	46.026407
3503.223990	470323.811199	46.031412
3503.217602	470324.927580	46.036417
3503.536582	470317.373461	46.041421
3503.158409	470341.363795	46.046426
3503.180796	470325.997992	46.051431
3503.254292	470332.830896	46.056436
3503.742687	470355.518143	46.061441
3503.530445	470344.397567	46.066445
3503.107645	470334.476373	46.071450
3503.490436	470319.155004	46.076455
3503.294463	470338.249301	46.081460
3503.057790	470349.643557	46.086465
3503.754799	470349.482656	46.091469
3503.245751	470334.657157	46.096474
3503.391150	470334.076434	46.101479
3503.249655	470358.282844	46.106484
3503.292588	470373.587523	46.111489
3503.575694	470384.443306	46.116493
3503.256953	470380.184119	46.121498
3503.591665	470363.298672	46.126503
3503.274741	470363.855728	46.131508
3503.589604	470362.538417	46.136513
3503.621578	470343.368585	46.141517
3503.230221	470361.479734	46.146522
3503.342965	470351.727407	46.151527
3503.215196	470363.966349	46.156532
3503.346661	470362.424523	46.161537
3503.724044	470351.514962	46.166541
3503.226489	470365.941764	46.171546
3503.430333	470343.652047	46.176551
3503.447966	470351.254280	46.181556
3503.662973	470367.545774	46.186561
3503.476995	470359.513775	46.191565
3503.301578	470365.118500	46.196570
3503.607098	470354.625902	46.201575
3503.588342	470365.022401	46.206580
3503.721764	470361.148049	46.211585
3503.708343	470364.090752	46.216589
3503.343102	470369.117074	46.221594
3503.754232	470389.687081	46.226599
3503.567895	470363.910034	46.231604
3503.622671	470372.621796	46.236609
3503.796402	470378.931840	46.241613
3504.062565	470347.354119	46.246618
3503.741470	470344.768410	46.251623
3503.711708	470350.400819	46.256628
3503.713307	470337.522628	46.261633
3503.751010	470333.004294	46.266637
3503.445958	470348.363991	46.271642
3503.840993	470331.519684	46.276647
3503.739867	470322.308150	46.281652
3503.804869	470314.895572	46.286657
3504.020842	470320.894754	46.291661
3503.610428	470321.213084	46.296666
3503.867891	470307.229726	46.301671
3503.850089	470311.136439	46.306676
3503.933847	470296.115817	46.311681
3503.884360	470279.291025	46.316685
3503.703553	470278.559055	46.321690
3503.987519	470276.131210	46.326695
3503.689793	470265.886012	46.331700
3503.602048	470253.427495	46.336705
3503.798787	470229.921965	46.341709
3503.788728	470248.581355	46.346714
3503.979774	470224.873917	46.351719
3503.651195	470255.701103	46.356724
3503.764407	470235.149415	46.361729
3503.735577	470230.540173	46.366733
3503.966021	470231.010720	46.371738
3503.737419	470207.470989	46.376743
3503.791008	470187.080780	46.381748
3503.781274	470213.446666	46.386753
3503.785725	470199.401823	46.391757
3503.603004	470198.416650	46.396762
3503.834459	470204.920425	46.401767
3503.603143	470166.576458	46.406772
3503.476961	470187.130187	46.411777
3503.489306	470152.296736	46.416781
3503.303363	470184.571808	46.421786
3503.704529	470155.913106	46.426791
3503.797207	470162.692333	46.431796
3503.666523	470164.842384	46.436801
3503.520096	470170.036973	46.441805
3503.423054	470184.907607	46.446810
3503.649377	470146.846178	46.451815
3503.372520	470170.567192	46.456820
3503.217835	470195.840592	46.461825
3503.253997	470163.386331	46.466829
3503.181217	470197.620830	46.471834
3503.694077	470177.563629	46.476839
3503.713804	470181.363033	46.481844
3503.486472	470197.521769	46.486849
3503.531882	470183.216938	46.491853
3503.486816	470184.288739	46.496858
3503.506186	470134.396011	46.501863
3503.200355	470169.225100	46.506868
3503.429914	470134.458690	46.511873
3503.624390	470130.777450	46.516877
3503.724058	470148.405569	46.521882
3503.742460	470124.573201	46.526887
3503.950538	470157.039545	46.531892
3503.772415	470129.537081	46.536897
3504.049601	470153.778957	46.541901
3504.002666	470130.565333	46.546906
3503.659617	470100.705954	46.551911
3503.809534	470123.548353	46.556916
3503.754700	470107.890388	46.561921
3503.944689	470086.413802	46.566925
3503.621189	470132.247864	46.571930
3503.638597	470081.544105	46.576935
3503.688321	470092.234123	46.581940
3503.854234	470060.570410	46.586945
3503.994115	470067.088703	46.591949
3503.409913	470061.451777	46.596954
3503.922511	470044.943566	46.601959
3503.630311	470081.190279	46.606964
3503.761329	470053.841659	46.611969
3503.818462	470059.612516	46.616973
3503.736408	470032.855256	46.621978
3504.048160	470056.432668	46.626983
3503.770368	470029.858444	46.631988
3503.731181	470066.166597	46.636993
3503.554250	470056.409214	46.641997
3503.556031	470013.617129	46.647002
3503.582587	470011.483443	46.652007
3503.747545	470012.167150	46.657012
3503.616278	470004.481275	46.662017
3503.829130	470007.641772	46.667021
3503.900250	470007.985402	46.672026
3503.524764	470009.616447	46.677031
3503.845194	470021.936856	46.682036
3503.593040	469991.201034	46.687041
3504.000933	469988.297258	46.692045
3503.400713	469993.056600	46.697050
3503.822976	469948.828990	46.702055
3503.715243	469959.087651	46.707060
3503.203624	469987.256992	46.712065
3503.445644	469955.682494	46.717069
3503.837861	469950.043318	46.722074
3503.532466	469988.624539	46.727079
3503.639814	469949.212620	46.732084
3503.605008	469984.556897	46.737089
3503.661745	469953.721498	46.742093
3503.359415	469956.760622	46.747098
3503.794145	469939.047803	46.752103
3503.655892	469909.155781	46.757108
3503.066974	469945.348224	46.762113
3503.616580	469930.152309	46.767117
3503.433251	469926.936356	46.772122
3503.456028	469945.033113	46.777127
3503.409853	469949.045780	46.782132
3503.295891	469939.734703	46.787137
3503.511138	469958.815055	46.792141
3503.533228	469952.727365	46.797146
3503.381176	469951.940137	46.802151
3503.347106	469955.900189	46.807156
3503.226327	469938.630077	46.812161
3503.361399	469944.236543	46.817165
3503.377165	469921.874699	46.822170
3503.352802	469951.488120	46.827175
3503.066495	469963.042535	46.832180
3503.330999	469928.929377	46.837185
3503.270583	469965.241061	46.842189
3503.329770	469943.937106	46.847194
3503.472413	469975.907060	46.852199
3503.412843	469942.200053	46.857204
3503.211279	469975.441244	46.862209
3503.568644	469955.763316	46.867213
3503.984315	469941.704007	46.872218
3503.618962	469970.864280	46.877223
3503.680844	469944.844678	46.882228
3503.392751	469983.068265	46.887233
3503.610375	469962.601209	46.892237
3503.672465	469949.510413	46.897242
3503.493777	469977.728550	46.902247
3503.705762	469950.671205	46.907252
3503.631246	469966.096149	46.912257
3503.734734	469920.549927	46.917261
3503.683231	469965.428740	46.922266
3503.931350	469932.180099	46.927271
3503.978794	469907.227462	46.932276
3503.838119	469945.326416	46.937281
3503.671445	469904.892994	46.942285
3503.429964	469919.786645	46.947290
3503.250295	469887.061857	46.952295
3503.508884	469905.425587	46.957300
3502.893063	469900.402032	46.962305
3503.546896	469910.793857	46.967309
3503.201465	469937.517359	46.972314
3503.624007	469935.118274	46.977319
3503.580767	469942.882381	46.982324
3503.643351	469921.476463	46.987329
3504.010971	469886.890626	46.992333
3503.840554	469921.495920	46.997338
3503.850939	469890.262142	47.002343
3503.895578	469902.981121	47.007348
3503.649529	469889.482675	47.012353
3504.029334	469891.298564	47.017357
3504.028631	469854.793529	47.022362
3503.628866	469872.399415	47.027367
3503.488149	469862.636217	47.032372
3503.291969	469868.802074	47.037377
3503.630163	469861.143351	47.042381
3503.639948	469875.591708	47.047386
3503.251795	469861.101673	47.052391
3503.706734	469880.245617	47.057396
3503.648963	469856.424981	47.062401
3503.740061	469872.533641	47.067405
3503.449337	469854.834005	47.072410
3503.258406	469834.127186	47.077415
3503.761253	469815.997883	47.082420
3503.526290	469823.538828	47.087425
3503.849795	469852.641094	47.092429
3503.187201	469838.397225	47.097434
3503.624848	469809.326668	47.102439
3503.647587	469838.831400	47.107444
3503.316260	469844.815818	47.112449
3503.975817	469816.267915	47.117453
3503.456398	469841.751496	47.122458
3503.885054	469858.465937	47.127463
3503.434091	469815.542194	47.132468
3503.538575	469801.278466	47.137473
3503.719334	469827.209120	47.142477
3503.334528	469837.917244	47.147482
3503.210491	469829.368234	47.152487
3503.268675	469803.906759	47.157492
3503.418714	469774.222487	47.162497
3503.587596	469816.886612	47.167501
3503.595616	469821.397755	47.172506
3503.630714	469803.798685	47.177511
3503.856444	469794.383152	47.182516
3503.583503	469832.351112	47.187521
3503.513895	469808.177380	47.192525
3503.912755	469807.607285	47.197530
3503.541373	469806.804015	47.202535
3503.850114	469768.728871	47.207540
3503.612775	469789.959683	47.212545
3503.943929	469756.393428	47.217549
3503.370115	469791.772520	47.222554
3503.479866	469765.745129	47.227559
3503.299039	469771.350868	47.232564
3503.385039	469763.022143	47.237569
3503.602312	469778.401108	47.242573
3503.769108	469771.884881	47.247578
3503.662256	469772.611556	47.252583
3503.651628	469782.043727	47.257588
3503.879828	469765.732351	47.262593
3503.909323	469735.813568	47.267597
3503.683392	469751.110496	47.272602
3504.030171	469715.310825	47.277607
3503.477568	469745.667152	47.282612
3503.552018	469735.920590	47.287617
3503.764070	469718.851201	47.292621
3503.644404	469737.731179	47.297626
3503.262460	469708.790019	47.302631
3503.589076	469723.087003	47.307636
3503.465871	469704.448129	47.312641
3503.895472	469697.028408	47.317645
3503.394316	469703.039707	47.322650
3503.656987	469715.217321	47.327655
3503.393573	469696.499196	47.332660
3503.798942	469691.111382	47.337665
3503.948928	469718.263882	47.342669
3503.601099	469714.566877	47.347674
3503.771794	469687.008698	47.352679
3503.734208	469661.612887	47.357684
3503.606064	469691.445888	47.362689
3503.635327	469676.382731	47.367693
3503.897195	469649.418517	47.372698
3503.718501	469694.672930	47.377703
3503.748123	469681.587097	47.382708
3503.170091	469668.495892	47.387713
3503.639302	469640.789067	47.392717
3503.716961	469687.980359	47.397722
3503.464926	469692.380526	47.402727
3503.715187	469655.886180	47.407732
3503.968885	469662.741525	47.412737
3503.990810	469631.049217	47.417741
3503.742816	469631.848906	47.422746
3503.596129	469634.914179	47.427751
3503.694903	469635.608360	47.432756
3503.608390	469638.309207	47.437761
3503.934340	469627.762313	47.442765
3503.768995	469603.603476	47.447770
3503.574337	469602.417351	47.452775
3503.626876	469607.580632	47.457780
3503.609762	469599.724459	47.462785
3503.649923	469602.202482	47.467789
3503.698220	469611.270501	47.472794
3503.754710	469604.771656	47.477799
3504.170443	469597.556901	47.482804
3503.503934	469593.656730	47.487809
3503.388541	469553.721544	47.492813
3503.527284	469561.964054	47.497818
3503.642854	469558.650100	47.502823
3504.034190	469562.542991	47.507828
3503.531776	469560.999886	47.512833
3503.681262	469573.144769	47.517837
3503.286150	469573.612797	47.522842
3503.437501	469545.094145	47.527847
3504.009726	469583.283895	47.532852
3503.637440	469573.759970	47.537857
3503.444194	469533.228623	47.542861
3503.803711	469542.450294	47.547866
3503.571284	469568.852192	47.552871
3503.469742	469539.460861	47.557876
3503.306996	469535.328952	47.562881
3503.828795	469510.554380	47.567885
3503.668524	469553.118959	47.572890
3503.668982	469533.142126	47.577895
3503.769332	469545.953922	47.582900
3503.799293	469500.824024	47.587905
3503.608419	469518.498596	47.592909
3503.277510	469498.624805	47.597914
3503.416790	469480.197757	47.602919
3503.694421	469520.158068	47.607924
3503.405294	469508.237958	47.612929
3504.036929	469469.654914	47.617933
3503.563616	469514.195744	47.622938
3503.446693	469524.506773	47.627943
3503.707981	469496.528405	47.632948
3503.581927	469513.736415	47.637953
3503.495333	469505.840485	47.642957
3503.681270	469465.908209	47.647962
3503.755674	469490.284312	47.652967
3503.775379	469460.062467	47.657972
3503.403839	469477.157198	47.662977
3503.790810	469446.674477	47.667981
3503.456598	469474.055931	47.672986
3503.229601	469459.438740	47.677991
3503.772631	469479.431073	47.682996
3503.164943	469462.085415	47.688001
3503.545468	469482.356942	47.693005
3503.317082	469464.799230	47.698010
3503.287338	469479.862539	47.703015
3503.432355	469473.552471	47.708020
3503.593160	469476.112845	47.713025
3503.681599	469475.439697	47.718029
3503.359269	469484.819862	47.723034
3503.229577	469489.251437	47.728039
3503.552646	469458.474618	47.733044
3503.134911	469493.221116	47.738049
3503.411239	469458.851809	47.743053
3503.272436	469499.790623	47.748058
3503.934814	469489.038379	47.753063
3503.307267	469475.295746	47.758068
3503.630074	469488.427335	47.763073
3503.660822	469457.240394	47.768077
3503.733140	469462.704800	47.773082
3503.299519	469462.874701	47.778087
3503.664553	469434.727746	47.783092
3503.066968	469443.695110	47.788097
3503.097574	469455.605338	47.793101
3503.287184	469463.079309	47.798106
3503.573127	469426.122600	47.803111
3503.563220	469454.010552	47.808116
3503.414145	469434.209366	47.813121
3503.631181	469465.712022	47.818125
3503.412087	469447.950017	47.823130
3503.182140	469439.062668	47.828135
3503.764650	469427.613180	47.833140
3503.183381	469457.264618	47.838145
3503.521250	469431.809188	47.843149
3503.108596	469475.884189	47.848154
3503.254310	469435.096268	47.853159
3503.600132	469472.003738	47.858164
3503.072709	469466.104162	47.863169
3503.741595	469450.534129	47.868173
3503.688813	469453.838100	47.873178
3503.458793	469462.088229	47.878183
3503.575945	469453.855863	47.883188
3503.680363	469459.872925	47.888193
3503.854448	469439.158725	47.893197
3503.631933	469483.964197	47.898202
3503.645665	469447.658978	47.903207
3503.884096	469454.313995	47.908212
3503.542860	469420.447852	47.913217
3504.264562	469409.990408	47.918221
3503.724217	469429.342775	47.923226
3503.874972	469414.970065	47.928231
3503.797940	469425.376242	47.933236
3503.951109	469365.725623	47.938241
3503.688252	469380.217414	47.943245
3503.585725	469412.226982	47.948250
3503.408370	469384.824819	47.953255
3503.910708	469364.312178	47.958260
3503.815989	469406.562479	47.963265
3503.742518	469367.431554	47.968269
3504.087854	469365.348825	47.973274
3503.740650	469338.632582	47.978279
3504.073977	469357.897633	47.983284
3503.875667	469353.416389	47.988289
3503.884450	469323.348181	47.993293
3503.807139	469337.962784	47.998298
3503.855656	469325.887799	48.003303
3503.910396	469279.790153	48.008308
3503.690035	469327.637797	48.013313
3503.892589	469318.022902	48.018317
3504.014642	469282.815741	48.023322
3503.801357	469300.392633	48.028327
3503.571565	469274.874622	48.033332
3503.777732	469245.282135	48.038337
3503.642536	469287.691182	48.043341
3503.569068	469263.061103	48.048346
3503.602871	469299.764676	48.053351
3504.104264	469263.027142	48.058356
3503.835257	469274.224282	48.063361
3503.544093	469243.949851	48.068365
3503.774589	469227.941911	48.073370
3503.293583	469248.197722	48.078375
3503.547653	469222.958094	48.083380
3503.487681	469250.397903	48.088385
3503.565108	469221.636978	48.093389
3503.753122	469253.600869	48.098394
3502.870842	469237.363187	48.103399
3503.773296	469215.367475	48.108404
3503.049863	469257.362524	48.113409
3502.968454	469237.195536	48.118413
3503.589294	469220.010428	48.123418
3503.649520	469251.994518	48.128423
3503.685662	469225.876682	48.133428
3503.406960	469263.745179	48.138433
3503.241263	469230.662232	48.143437
3503.820723	469245.274504	48.148442
3503.457341	469232.351910	48.153447
3503.754353	469251.774908	48.158452
3503.789033	469219.674336	48.163457
3503.323730	469189.021723	48.168461
3503.431602	469217.550518	48.173466
3503.270057	469192.680760	48.178471
3503.639328	469212.345890	48.183476
3503.500260	469227.832285	48.188481
3503.262374	469203.228121	48.193485
3503.702966	469210.054077	48.198490
3503.263605	469203.785585	48.203495
3503.935182	469200.535808	48.208500
3503.618066	469198.861983	48.213505
3503.577060	469225.943903	48.218509
3503.511720	469200.349107	48.223514
3503.730787	469206.703043	48.228519
3503.595977	469223.304238	48.233524
3503.861665	469179.201154	48.238529
3503.509302	469187.420024	48.243533
3503.689079	469152.406333	48.248538
3503.397297	469182.975768	48.253543
3503.583389	469156.682037	48.258548
3502.942790	469188.574177	48.263553
3503.192224	469155.222686	48.268557
3502.930099	469190.046499	48.273562
3503.396647	469156.914213	48.278567
3503.466819	469176.981572	48.283572
3503.169668	469204.965958	48.288577
3503.344212	469161.485680	48.293581
3503.348617	469201.743300	48.298586
3503.585714	469213.570327	48.303591
3503.858478	469179.556047	48.308596
3503.557970	469180.465460	48.313601
3503.597264	469193.084309	48.318605
3503.947051	469174.167392	48.323610
3503.718900	469211.115336	48.328615
3503.678069	469190.637670	48.333620
3503.612724	469186.490298	48.338625
3503.721762	469189.920844	48.343629
3503.601023	469165.653043	48.348634
3503.245772	469176.356834	48.353639
3503.799852	469122.219511	48.358644
3503.686797	469170.811104	48.363649
3503.585593	469135.233355	48.368653
3503.552359	469168.195707	48.373658
3503.076648	469143.223435	48.378663
3503.919396	469156.830793	48.383668
3503.219788	469168.400266	48.388673
3503.349241	469150.988546	48.393677
3503.734569	469169.028674	48.398682
3503.370183	469157.627290	48.403687
3503.858602	469167.031568	48.408692
3503.586891	469155.209909	48.413697
3503.519262	469157.045878	48.418701
3503.582740	469167.075054	48.423706
3504.022186	469113.209342	48.428711
3503.451893	469136.318762	48.433716
3503.714480	469113.308602	48.438721
3503.402198	469145.301027	48.443725
3503.728431	469109.097940	48.448730
3503.305545	469156.065325	48.453735
3503.439758	469128.917802	48.458740
3503.572784	469118.705365	48.463745
3503.503092	469140.062449	48.468749
3504.109012	469103.865852	48.473754
3503.615159	469136.647538	48.478759
3503.634190	469104.295746	48.483764
3503.666695	469095.670990	48.488769
3503.565634	469081.946292	48.493773
3503.884162	469090.211276	48.498778
3503.411857	469087.192976	48.503783
3503.565559	469103.038818	48.508788
3503.894062	469080.423831	48.513793
3503.399233	469101.442520	48.518797
3503.456408	469084.447796	48.523802
3503.099739	469111.174129	48.528807
3503.606497	469072.610091	48.533812
3503.533994	469128.496673	48.538817
3503.199242	469082.916482	48.543821
3503.652150	469121.531563	48.548826
3503.371365	469104.539566	48.553831
3503.806446	469091.338578	48.558836
3503.812416	469071.208323	48.563841
3503.337269	469076.911468	48.568845
3503.287056	469058.666109	48.573850
3503.290501	469051.820551	48.578855
3503.396947	469068.637255	48.583860
3503.598395	469080.875619	48.588865
3503.188424	469069.177171	48.593869
3503.780442	469042.058587	48.598874
3503.355903	469065.043641	48.603879
3503.448134	469090.786388	48.608884
3503.197077	469076.679766	48.613889
3503.806567	469057.772401	48.618893
3503.204644	469079.619295	48.623898
3503.214990	469055.381352	48.628903
3503.629437	469078.487307	48.633908
3503.456109	469056.965680	48.638913
3503.736695	469094.340458	48.643917
3503.627990	469071.388936	48.648922
3503.836687	469061.925063	48.653927
3503.745267	469088.457391	48.658932
3503.527283	469062.075295	48.663937
3503.547179	469080.122553	48.668941
3503.468303	469064.315495	48.673946
3503.640141	469023.674754	48.678951
3503.930474	469053.848152	48.683956
3503.359778	469063.064946	48.688961
3503.427451	469028.271580	48.693965
3503.616943	469081.328182	48.698970
3503.347483	469063.573810	48.703975
3503.687977	469024.681038	48.708980
3503.405594	469078.217857	48.713985
3503.290587	469042.743538	48.718989
3503.380029	469060.729118	48.723994
3503.017288	469075.845348	48.728999
3503.475038	469034.601702	48.734004
3503.434523	469079.227163	48.739009
3502.898154	469060.399498	48.744013
3503.209025	469057.561633	48.749018
3503.519407	469031.501619	48.754023
3503.650514	469032.393524	48.759028
3503.671523	469036.142230	48.764033
3503.662936	469072.751494	48.769037
3503.455170	469093.319193	48.774042
3503.413681	469100.322784	48.779047
3503.642102	469097.548659	48.784052
3503.262675	469098.217031	48.789057
3503.366329	469088.364145	48.794061
3503.461559	469093.165882	48.799066
3503.270306	469084.931411	48.804071
3503.323100	469103.581891	48.809076
3503.554941	469088.689107	48.814081
3503.984467	469043.545774	48.819085
3504.060095	469014.987664	48.824090
3503.560972	469010.351075	48.829095
3503.912321	468997.264669	48.834100
3503.977862	468997.862716	48.839105
3503.419806	469006.215575	48.844109
3503.304854	469039.393860	48.849114
3503.407729	469063.512444	48.854119
3502.865629	469035.711140	48.859124
3503.613278	469016.832606	48.864129
3503.342793	469017.027429	48.869133
3503.498013	469057.058676	48.874138
3503.142716	469041.345993	48.879143
3504.037094	468995.013607	48.884148
3503.644083	469015.002217	48.889153
3503.472960	469056.352634	48.894157
3503.976112	469046.588699	48.899162
3503.292611	469011.052067	48.904167
3503.885634	468982.412138	48.909172
3503.700390	469029.392950	48.914177
3503.714748	469000.337469	48.919181
3503.115531	468994.753327	48.924186
3503.489013	468984.705635	48.929191
3504.006184	468979.553488	48.934196
3503.376203	468997.247197	48.939201
3503.583088	468981.699134	48.944205
3503.790733	469003.468858	48.949210
3503.767019	469002.458494	48.954215
3503.822343	468966.196571	48.959220
3503.531811	468946.315873	48.964225
3503.729227	468969.709770	48.969229
3503.762564	468961.084827	48.974234
3502.786255	468962.455985	48.979239
3503.750872	468937.712157	48.984244
3503.650892	468954.510874	48.989249
3503.433678	468977.412553	48.994253
3503.188856	468955.750009	48.999258
3503.837342	468951.540473	49.004263
3503.607581	468982.100398	49.009268
3504.031190	468938.985923	49.014273
3503.511750	468960.718496	49.019277
3504.029165	468922.406017	49.024282
3503.276138	468941.133297	49.029287
3503.593105	468917.708698	49.034292
3503.411291	468939.945673	49.039297
3503.689461	468917.287762	49.044301
3503.721196	468930.009372	49.049306
3503.375182	468936.807630	49.054311
3504.160346	468892.621840	49.059316
3503.986216	468917.088596	49.064321
3503.521898	468895.663498	49.069325
3503.683140	468871.705716	49.074330
3503.469421	468879.852090	49.079335
3503.521690	468911.280214	49.084340
3503.491445	468886.744269	49.089345
3503.465041	468903.683510	49.094349
3503.627435	468918.970374	49.099354
3503.625239	468891.032842	49.104359
3503.523518	468906.057236	49.109364
3503.660449	468888.035669	49.114369
3503.584446	468854.633729	49.119373
3503.560339	468851.696668	49.124378
3503.266819	468889.314663	49.129383
3503.443266	468884.571272	49.134388
3503.306115	468899.043527	49.139393
3503.333239	468891.636432	49.144397
3503.391095	468890.004724	49.149402
3503.257404	468885.361054	49.154407
3503.144960	468865.553541	49.159412
3502.994431	468867.504045	49.164417
3503.275541	468892.101696	49.169421
3503.294840	468934.385632	49.174426
3503.165703	468927.256765	49.179431
3503.318173	468917.852418	49.184436
3503.814925	468894.450082	49.189441
3503.670665	468888.794005	49.194445
3503.748707	468885.587285	49.199450
3503.226122	468922.176642	49.204455
3503.402631	468898.419294	49.209460
3503.559310	468885.160770	49.214465
3503.231709	468897.482858	49.219469
3503.718942	468857.603209	49.224474
3503.358959	468899.440122	49.229479
3503.394156	468867.186816	49.234484
3503.615287	468888.701008	49.239489
3503.303453	468896.051619	49.244493
3503.431961	468862.414552	49.249498
3503.337514	468902.992594	49.254503
3503.492630	468863.723191	49.259508
3503.460041	468893.187299	49.264513
3503.370933	468880.271842	49.269517
3503.814259	468881.063703	49.274522
3503.229462	468885.161704	49.279527
3503.815684	468853.581847	49.284532
3503.556403	468914.366105	49.289537
3503.631162	468891.537500	49.294541
3503.796921	468886.592983	49.299546
3503.369849	468885.037918	49.304551
3503.837312	468852.412046	49.309556
3503.503226	468882.126637	49.314561
3503.325884	468861.011074	49.319565
3504.004010	468825.765961	49.324570
3503.547373	468872.790018	49.329575
3503.419017	468846.190669	49.334580
3503.509399	468816.717284	49.339585
3503.572716	468850.324030	49.344589
3503.112316	468867.737526	49.349594
3503.118096	468839.697257	49.354599
3503.195462	468879.132700	49.359604
3503.236956	468836.078407	49.364609
3503.590455	468872.073049	49.369613
3503.534622	468846.577725	49.374618
3503.650834	468865.624026	49.379623
3503.450904	468852.878179	49.384628
3503.559065	468854.483575	49.389633
3503.678423	468868.763198	49.394637
3503.880694	468869.035414	49.399642
3503.714701	468869.822171	49.404647
3503.936252	468855.387184	49.409652
3503.711570	468830.324159	49.414657
3503.679199	468844.323555	49.419661
3503.585261	468836.834166	49.424666
3503.441771	468830.011759	49.429671
3503.503792	468832.790642	49.434676
3503.817358	468830.915698	49.439681
3503.494720	468827.518776	49.444685
3503.892799	468836.329033	49.449690
3503.358990	468833.168304	49.454695
3503.630461	468797.328263	49.459700
3503.607661	468796.824787	49.464705
3503.778323	468789.496377	49.469709
3503.841248	468770.725844	49.474714
3503.395930	468783.573646	49.479719
3503.659092	468783.024973	49.484724
3503.631521	468770.201131	49.489729
3503.793673	468798.468396	49.494733
3503.562348	468798.606327	49.499738
3503.523354	468766.516705	49.504743
3503.432553	468787.066218	49.509748
3503.224259	468761.138549	49.514753
3503.148546	468745.584272	49.519757
3503.426470	468771.855808	49.524762
3503.377037	468794.680464	49.529767
3503.709825	468780.075732	49.534772
3503.660240	468763.401846	49.539777
3503.756294	468770.738739	49.544781
3503.527142	468738.577720	49.549786
3503.439773	468763.385873	49.554791
3503.242701	468752.616979	49.559796
3503.678074	468731.404445	49.564801
3503.696200	468771.052272	49.569805
3503.462715	468744.824339	49.574810
3503.658802	468762.032755	49.579815
3503.593847	468771.169743	49.584820
3503.426171	468742.345491	49.589825
3503.298263	468766.145962	49.594829
3503.614188	468775.831201	49.599834
3503.421485	468737.630619	49.604839
3503.397457	468771.149888	49.609844
3503.263028	468773.300673	49.614849
3503.936031	468741.402706	49.619853
3503.620745	468755.244059	49.624858
3503.036402	468723.341972	49.629863
3503.476242	468710.494923	49.634868
3503.221976	468730.259058	49.639873
3503.459514	468714.300317	49.644877
3503.784264	468708.722178	49.649882
3503.532964	468697.505487	49.654887
3503.686069	468737.588383	49.659892
3503.773223	468752.735148	49.664897
3503.561897	468752.210763	49.669901
3503.576162	468751.042272	49.674906
3503.634660	468761.680880	49.679911
3503.969073	468749.661786	49.684916
3504.021348	468743.873199	49.689921
3503.552741	468705.614757	49.694925
3503.406737	468683.682792	49.699930
3503.845279	468665.866887	49.704935
3503.779191	468700.052076	49.709940
3503.737684	468687.534612	49.714945
3503.666452	468666.452786	49.719949
3503.774389	468690.469590	49.724954
3504.104807	468637.836796	49.729959
3503.931754	468663.824813	49.734964
3503.677375	468627.002799	49.739969
3503.501451	468660.495547	49.744973
3503.570563	468643.701397	49.749978
3503.706395	468640.586915	49.754983
3503.601489	468671.786717	49.759988
3503.456311	468622.119205	49.764993
3503.396279	468632.624498	49.769997
3503.785294	468607.869849	49.775002
3503.470340	468612.381594	49.780007
3503.558378	468582.046273	49.785012
3503.870141	468626.414201	49.790017
3503.668065	468598.000824	49.795021
3503.796583	468596.510040	49.800026
3503.445705	468618.875484	49.805031
3503.808173	468606.598351	49.810036
3503.706690	468589.729711	49.815041
3503.353355	468605.098316	49.820045
3503.627690	468574.378608	49.825050
3503.484361	468564.158874	49.830055
3503.582319	468569.872985	49.835060
3503.636202	468576.151812	49.840065
3503.227763	468574.745892	49.845069
3503.533180	468584.584994	49.850074
3503.487222	468558.631417	49.855079
3503.151704	468583.580412	49.860084
3503.691143	468561.083643	49.865089
3503.663890	468562.913282	49.870093
3503.668753	468570.315362	49.875098
3503.384532	468580.602591	49.880103
3503.544406	468577.636414	49.885108
3503.623697	468578.840756	49.890113
3503.596762	468585.233763	49.895117
3503.809936	468571.509770	49.900122
3503.652793	468579.698023	49.905127
3503.505367	468534.695488	49.910132
3503.530113	468571.249654	49.915137
3503.321030	468557.237457	49.920141
3503.300133	468530.519314	49.925146
3503.125610	468573.240250	49.930151
3503.440824	468536.074528	49.935156
3503.310528	468557.188260	49.940161
3503.076767	468543.991230	49.945165
3503.895880	468529.715099	49.950170
3503.634078	468572.247012	49.955175
3503.432348	468535.112287	49.960180
3503.461750	468553.259905	49.965185
3503.133487	468559.649840	49.970189
3503.404833	468566.249233	49.975194
3503.165239	468549.909437	49.980199
3503.721492	468553.015882	49.985204
3503.626658	468554.450565	49.990209
3503.159074	468554.372315	49.995213
3503.225733	468574.085873	50.000218
3503.334362	468550.389565	50.005223
3503.096773	468556.866579	50.010228
3503.290052	468577.067170	50.015233
3503.624809	468566.416943	50.020237
3503.945342	468547.047743	50.025242
3503.140540	468589.361215	50.030247
3503.306259	468561.143181	50.035252
3503.686482	468551.601264	50.040257
3503.421310	468546.268433	50.045261
3503.530294	468590.769896	50.050266
3503.634775	468557.592481	50.055271
3503.684444	468584.762308	50.060276
3503.609675	468550.751233	50.065281
3503.488439	468590.928474	50.070285
3503.393515	468579.889823	50.075290
3503.434983	468564.621119	50.080295
3503.498592	468580.126662	50.085300
3503.735659	468545.964884	50.090305
3503.170832	468603.046183	50.095309
3503.576662	468583.714241	50.100314
3503.407874	468549.008157	50.105319
3503.209327	468566.329811	50.110324
3503.510993	468542.755098	50.115329
3503.245814	468564.549303	50.120333
3503.970310	468529.042842	50.125338
3503.368182	468562.552403	50.130343
3503.437639	468537.036901	50.135348
3503.785954	468514.671698	50.140353
3503.443423	468520.607557	50.145357
3503.620243	468538.630479	50.150362
3503.415770	468530.245764	50.155367
3503.467640	468536.423512	50.160372
3503.818883	468534.846816	50.165377
3503.251295	468526.113852	50.170381
3503.539121	468548.733357	50.175386
3503.531382	468525.410346	50.180391
3503.161334	468559.795918	50.185396
3503.852921	468521.810114	50.190401
3503.274299	468576.459834	50.195405
3503.041707	468542.575099	50.200410
3503.053435	468528.223755	50.205415
3503.458028	468535.359850	50.210420
3503.285244	468540.761827	50.215425
3503.693699	468518.082894	50.220429
3503.725072	468524.415999	50.225434
3503.465073	468575.567436	50.230439
3503.282569	468564.796143	50.235444
3503.073050	468536.941611	50.240449
3503.546930	468531.796198	50.245453
3503.614298	468573.769035	50.250458
3503.286901	468559.927654	50.255463
3503.515440	468531.750356	50.260468
3503.475536	468542.658152	50.265473
3503.343721	468579.946914	50.270477
3503.828848	468547.672710	50.275482
3503.416908	468532.019301	50.280487
3503.167581	468533.579813	50.285492
3503.730750	468519.901879	50.290497
3503.440373	468523.750596	50.295501
3503.559853	468501.269433	50.300506
3503.199923	468522.216675	50.305511
3503.735426	468491.810501	50.310516
3503.083161	468511.739154	50.315521
3503.011514	468535.429586	50.320525
3503.441066	468497.180923	50.325530
3503.231470	468512.324058	50.330535
3503.318813	468555.561395	50.335540
3503.596947	468548.722963	50.340545
3503.913656	468513.078106	50.345549
3503.439280	468542.206893	50.350554
3503.355029	468530.760891	50.355559
3503.795839	468501.941547	50.360564
3503.582039	468544.263111	50.365569
3503.316765	468544.761342	50.370573
3503.581532	468497.006227	50.375578
3503.862699	468509.536555	50.380583
3503.626561	468520.120443	50.385588
3503.859586	468529.920307	50.390593
3503.468221	468550.568260	50.395597
3503.508690	468515.372705	50.400602
3503.118853	468482.628232	50.405607
3503.877503	468465.370024	50.410612
3503.773196	468486.834653	50.415617
3503.261348	468504.003056	50.420621
3503.370893	468465.044340	50.425626
3503.616076	468488.583339	50.430631
3502.819629	468497.430419	50.435636
3503.093361	468482.124946	50.440641
3503.731567	468464.480133	50.445645
3503.468442	468499.558774	50.450650
3502.975705	468497.861943	50.455655
3503.133904	468482.929664	50.460660
3503.616344	468477.427951	50.465665
3503.136955	468517.307005	50.470669
3503.268487	468485.392820	50.475674
3503.420653	468547.076505	50.480679
3503.007625	468533.704983	50.485684
3503.511986	468549.850754	50.490689
3503.215804	468527.181790	50.495693
3502.962218	468557.898213	50.500698
3503.378648	468535.116629	50.505703
3502.920783	468571.392138	50.510708
3503.209104	468535.244759	50.515713
3503.444467	468532.672282	50.520717
3503.475860	468573.028254	50.525722
3503.237482	468581.330754	50.530727
3503.077812	468563.710720	50.535732
3503.299246	468504.046859	50.540737
3503.017215	468521.736678	50.545741
3503.287072	468450.504312	50.550746
3503.200102	468435.610749	50.555751
3503.044269	468340.918149	50.560756
3503.051036	468281.743932	50.565761
3502.648125	468205.749350	50.570765
3502.996523	468088.665455	50.575770
3502.521093	468040.569940	50.580775
3502.487016	467922.835690	50.585780
3501.903881	467800.826799	50.590785
3501.937858	467681.508541	50.595789
3501.310531	467552.051288	50.600794
3500.985825	467418.742350	50.605799
3501.716355	467269.394245	50.610804
3501.113849	467142.060283	50.615809
3500.711630	466943.955510	50.620813
3500.405060	466791.370471	50.625818
3500.445853	466656.680530	50.630823
3499.657897	466457.212312	50.635828
3500.125433	466234.014217	50.640833
3499.350399	466084.337913	50.645837
3499.044973	465892.191880	50.650842
3498.228658	465675.174750	50.655847
3498.353013	465435.946937	50.660852
3497.927183	465264.809120	50.665857
3497.292071	465043.142074	50.670861
3497.431165	464799.239196	50.675866
3496.862303	464583.135421	50.680871
3496.770375	464326.686550	50.685876
3496.053251	464090.568880	50.690881
3495.585708	463827.529702	50.695885
3495.481238	463617.834466	50.700890
3494.913417	463325.135830	50.705895
3494.327316	463090.406569	50.710900
3493.743336	462813.375328	50.715905
3493.361165	462538.286687	50.720909
3492.942991	462295.052180	50.725914
3492.362989	461994.983141	50.730919
3491.738329	461744.927869	50.735924
3491.366289	461422.348701	50.740929
3490.557835	461180.279295	50.745933
3490.304126	460870.100198	50.750938
3489.509260	460612.501138	50.755943
3489.128833	460299.493470	50.760948
3488.575234	460011.161027	50.765953
3487.896336	459727.308456	50.770957
3487.332178	459439.223814	50.775962
3487.229942	459115.198463	50.780967
3486.426318	458837.492116	50.785972
3486.234539	458506.015034	50.790977
3485.315987	458217.716850	50.795981
3484.872555	457897.430834	50.800986
3484.066039	457564.870086	50.805991
3483.320101	457287.439615	50.810996
3483.043292	456953.669942	50.816001
3482.270041	456648.282559	50.821005
3482.134313	456330.259121	50.826010
3480.971075	455996.006491	50.831015
3480.306695	455704.743856	50.836020
3480.048649	455352.023342	50.841025
3478.987647	455062.134218	50.846029
3478.399838	454695.858283	50.851034
3477.668061	454415.954760	50.856039
3477.278862	454056.435940	50.861044
3476.782127	453745.739505	50.866049
3476.076113	453426.192445	50.871053
3475.433238	453070.249941	50.876058
3475.041624	452767.997257	50.881063
3474.055224	452439.550255	50.886068
3473.729567	452101.048532	50.891073
3472.654986	451771.946263	50.896077
3472.689918	451431.804652	50.901082
3472.061609	451103.637187	50.906087
3470.880448	450753.224347	50.911092
3470.240877	450420.075888	50.916097
3469.886461	450089.871658	50.921101
3469.087100	449739.738397	50.926106
3468.595775	449405.790760	50.931111
3467.647588	449069.982086	50.936116
3467.306876	448728.490056	50.941121
3466.571047	448394.972642	50.946125
3465.866637	448037.186266	50.951130
3465.320548	447701.142190	50.956135
3464.242367	447373.856206	50.961140
3464.214207	447025.945944	50.966145
3463.004395	446678.115847	50.971149
3462.172227	446362.653556	50.976154
3461.509486	446003.560955	50.981159
3460.854020	445661.820590	50.986164
3460.206641	445338.092936	50.991169
3459.408045	444995.756583	50.996173
3458.705419	444654.263070	51.001178
3458.460849	444334.214338	51.006183
3457.401170	443986.575121	51.011188
3456.893033	443632.194019	51.016193
3455.654398	443311.781244	51.021197
3455.054395	442972.430445	51.026202
3454.521350	442660.222549	51.031207
3454.022671	442311.709157	51.036212
3453.141741	441973.810212	51.041217
3452.485038	441644.755046	51.046221
3452.081564	441310.223482	51.051226
3451.412598	440976.440052	51.056231
3450.118360	440658.437989	51.061236
3449.795013	440307.152308	51.066241
3448.882093	439971.769243	51.071245
3448.362827	439644.417098	51.076250
3447.573094	439327.257365	51.081255
3446.884341	438990.099392	51.086260
3446.741635	438650.032723	51.091265
3445.727921	438331.271011	51.096269
3445.033325	437999.837791	51.101274
3444.380160	437660.472998	51.106279
3443.445707	437319.980275	51.111284
3442.864810	436999.711524	51.116289
3441.928506	436675.280533	51.121293
3441.562636	436338.061206	51.126298
3440.647460	436008.109111	51.131303
3440.045162	435687.522444	51.136308
3439.728755	435359.828404	51.141313
3438.246872	435035.818107	51.146317
3438.045602	434707.005727	51.151322
3437.362051	434392.331380	51.156327
3436.769283	434066.162423	51.161332
3435.796112	433733.397124	51.166337
3435.317291	433425.559398	51.171341
3434.504320	433088.317026	51.176346
3433.748944	432769.698530	51.181351
3433.148519	432445.084531	51.186356
3432.689022	432106.732418	51.191361
3431.451173	431791.885431	51.196365
3431.213351	431469.334886	51.201370
3430.368125	431134.382961	51.206375
3429.415741	430829.458722	51.211380
3428.638785	430505.788027	51.216385
3427.943395	430183.319360	51.221389
3427.373838	429867.454773	51.226394
3426.701452	429542.917686	51.231399
3425.854298	429236.155319	51.236404
3425.284463	428920.101683	51.241409
3424.563621	428621.743459	51.246413
3423.988896	428280.973115	51.251418
3423.357611	427983.685600	51.256423
3422.523474	427670.477878	51.261428
3422.337984	427353.760779	51.266433
3421.439887	427020.898478	51.271437
3420.541514	426735.728331	51.276442
3419.681450	426393.785404	51.281447
3419.217592	426074.760666	51.286452
3418.285390	425789.204889	51.291457
3417.657830	425457.347248	51.296461
3416.980389	425156.962586	51.301466
3416.387415	424848.331946	51.306471
3415.335785	424531.413921	51.311476
3414.713642	424246.199315	51.316481
3414.251839	423914.652284	51.321485
3413.378269	423627.286589	51.326490
3412.888133	423298.352821	51.331495
3411.761405	423020.292002	51.336500
3411.747410	422677.559124	51.341505
3410.843518	422421.047981	51.346509
3410.099953	422072.225023	51.351514
3409.539729	421784.612814	51.356519
3408.728617	421475.140602	51.361524
3407.673247	421165.271730	51.366529
3407.439904	420888.369257	51.371533
3406.409687	420569.395627	51.376538
3406.140820	420256.852062	51.381543
3405.215097	419972.378217	51.386548
3404.951268	419627.005437	51.391553
3403.612039	419383.110185	51.396557
3402.765210	419061.042001	51.401562
3402.696962	418744.461503	51.406567
3401.888276	418476.136890	51.411572
3401.353557	418142.398911	51.416577
3400.391296	417876.811297	51.421581
3399.739590	417522.506160	51.426586
3398.881617	417265.890030	51.431591
3398.250708	416960.735211	51.436596
3397.796795	416656.438404	51.441601
3396.915681	416370.016085	51.446605
3396.475520	416068.835949	51.451610
3395.670366	415753.024966	51.456615
3394.893044	415497.117186	51.461620
3394.140027	415167.851014	51.466625
3393.583350	414888.248308	51.471629
3392.900365	414573.853491	51.476634
3392.402997	414300.791148	51.481639
3391.330504	413990.669485	51.486644
3391.221721	413694.595879	51.491649
3390.247277	413404.144585	51.496653
3389.621753	413103.522249	51.501658
3388.718967	412807.209554	51.506663
3387.985284	412507.945002	51.511668
3387.553455	412211.221573	51.516673
3386.898437	411931.377718	51.521677
3386.399097	411629.856578	51.526682
3385.628488	411335.541227	51.531687
3384.881480	411036.975560	51.536692
3383.924881	410730.918226	51.541697
3383.118648	410446.510339	51.546701
3382.530837	410151.188858	51.551706
3381.931521	409873.934499	51.556711
3381.454412	409584.129882	51.561716
3380.637076	409294.528772	51.566721
3380.028591	409003.468756	51.571725
3379.604473	408692.605252	51.576730
3378.529269	408410.736770	51.581735
3377.851232	408125.549936	51.586740
3377.437378	407838.209322	51.591745
3376.965299	407542.081895	51.596749
3376.215677	407236.871695	51.601754
3375.494320	406949.317285	51.606759
3374.288288	406666.055732	51.611764
3374.147403	406368.924375	51.616769
3373.264551	406091.756984	51.621773
3372.408517	405797.274802	51.626778
3371.483168	405500.742116	51.631783
3371.001923	405219.182789	51.636788
3370.413708	404952.938525	51.641793
3369.594551	404651.119842	51.646797
3368.890021	404369.639062	51.651802
3368.316761	404068.157188	51.656807
3367.659746	403811.699774	51.661812
3367.030662	403517.338342	51.666817
3366.282977	403240.175357	51.671821
3365.749297	402942.997587	51.676826
3365.488894	402661.965262	51.681831
3364.314104	402369.967191	51.686836
3363.646421	402075.547768	51.691841
3362.963643	401792.668228	51.696845
3362.399050	401511.496025	51.701850
3361.426996	401239.892642	51.706855
3360.459705	400949.119883	51.711860
3360.199922	400664.028368	51.716865
3359.444734	400385.088075	51.721869
3358.722120	400102.149274	51.726874
3358.060975	399827.485374	51.731879
3357.125641	399552.582903	51.736884
3356.451086	399273.061144	51.741889
3356.238243	399001.268282	51.746893
3355.332971	398724.930575	51.751898
3354.545010	398439.649064	51.756903
3354.139608	398161.092213	51.761908
3353.312923	397880.337090	51.766913
3352.681041	397611.776854	51.771917
3351.984479	397337.936839	51.776922
3351.329861	397047.156526	51.781927
3350.199469	396787.007104	51.786932
3350.053821	396506.641238	51.791937
3349.328419	396229.923960	51.796941
3348.517697	395954.641619	51.801946
3347.999507	395672.573531	51.806951
3347.266969	395394.096328	51.811956
3346.814743	395116.004732	51.816961
3345.861244	394847.371672	51.821965
3345.403637	394567.369646	51.826970
3344.901648	394288.491035	51.831975
3343.946080	394011.054825	51.836980
3343.444939	393734.053025	51.841985
3342.583967	393461.301067	51.846989
3342.082183	393177.099562	51.851994
3341.363918	392904.142675	51.856999
3340.243969	392629.594481	51.862004
3339.743169	392339.512605	51.867009
3339.076188	392079.559294	51.872013
3338.264134	391816.499541	51.877018
3337.993934	391541.020216	51.882023
3336.977292	391258.613532	51.887028
3336.349398	390994.882846	51.892033
3335.792511	390724.324467	51.897037
3335.108276	390440.180487	51.902042
3334.530783	390175.037222	51.907047
3333.605378	389916.278523	51.912052
3333.324950	389624.206986	51.917057
3332.400978	389367.071477	51.922061
3331.508534	389091.773271	51.927066
3331.101473	388814.641631	51.932071
3330.368883	388541.475369	51.937076
3329.904900	388273.146930	51.942081
3328.937498	387996.224765	51.947085
3328.286149	387729.701975	51.952090
3327.876451	387460.367201	51.957095
3327.009756	387188.305435	51.962100
3326.663184	386909.598479	51.967105
3325.764283	386645.421047	51.972109
3324.843224	386374.531624	51.977114
3324.155557	386115.225028	51.982119
3323.531766	385837.850747	51.987124
3322.785521	385569.089379	51.992129
3322.126299	385317.707122	51.997133
3321.779351	385042.749930	52.002138
3321.115258	384774.834495	52.007143
3320.220493	384515.168013	52.012148
3319.678310	384214.295402	52.017153
3319.164162	383977.987664	52.022157
3318.147746	383695.522311	52.027162
3317.791556	383427.039935	52.032167
3316.921664	383154.287936	52.037172
3316.218132	382888.883141	52.042177
3315.067437	382626.700879	52.047181
3314.748799	382363.673113	52.052186
3314.175891	382096.182073	52.057191
3313.301594	381852.186380	52.062196
3312.514197	381566.566156	52.067201
3311.843473	381320.754553	52.072205
3311.401972	381066.359361	52.077210
3310.652622	380796.776192	52.082215
3310.136793	380534.759052	52.087220
3309.658666	380265.358215	52.092225
3308.969519	380001.533622	52.097229
3308.140377	379736.406784	52.102234
3307.917928	379469.961334	52.107239
3306.433114	379201.068463	52.112244
3306.029312	378934.291977	52.117249
3305.418512	378671.412609	52.122253
3304.557118	378394.759601	52.127258
3303.967834	378145.252466	52.132263
3303.398567	377888.084392	52.137268
3303.027341	377607.227779	52.142273
3302.213327	377350.730856	52.147277
3301.375249	377092.302932	52.152282
3300.802532	376824.648774	52.157287
3300.016099	376572.975485	52.162292
3299.466183	376297.225341	52.167297
3298.770985	376034.494652	52.172301
3297.971724	375772.694464	52.177306
3297.341036	375511.069435	52.182311
3296.555144	375245.397265	52.187316
3296.237000	374976.698623	52.192321
3295.391999	374748.349741	52.197325
3294.964610	374455.702478	52.202330
3294.419754	374189.959940	52.207335
3293.333413	373951.494966	52.212340
3292.904891	373666.244874	52.217345
3292.202369	373403.981886	52.222349
3291.464523	373141.112306	52.227354
3290.802669	372875.786910	52.232359
3289.675997	372627.984632	52.237364
3289.406518	372354.834946	52.242369
3288.838230	372095.061052	52.247373
3287.750130	371824.098002	52.252378
3287.560322	371569.984960	52.257383
3286.502261	371322.138748	52.262388
3286.024181	371050.972544	52.267393
3285.420237	370776.644492	52.272397
3284.513439	370525.615150	52.277402
3283.996073	370263.634183	52.282407
3283.708306	370010.672221	52.287412
3282.938074	369741.579233	52.292417
3282.187238	369468.283736	52.297421
3281.219413	369217.867048	52.302426
3280.784556	368954.898370	52.307431
3279.940218	368699.930624	52.312436
3279.351830	368434.820580	52.317441
3278.699382	368174.883759	52.322445
3278.090979	367921.858655	52.327450
3277.355929	367662.466166	52.332455
3276.340539	367410.545636	52.337460
3276.194249	367140.269473	52.342465
3275.564695	366889.735196	52.347469
3274.705660	366619.339626	52.352474
3274.201141	366350.565587	52.357479
3273.412725	366099.695828	52.362484
3272.993880	365830.777928	52.367489
3272.395103	365576.440452	52.372493
3271.157617	365307.394489	52.377498
3270.967371	365043.320915	52.382503
3269.989390	364796.494028	52.387508
3269.592374	364529.142507	52.392513
3268.554619	364272.831694	52.397517
3267.981783	364008.812680	52.402522
3267.615597	363746.998574	52.407527
3266.779926	363490.397021	52.412532
3266.091747	363219.903427	52.417537
3265.630789	362956.318741	52.422541
3265.020837	362701.992623	52.427546
3264.396702	362430.771884	52.432551
3263.352212	362179.081611	52.437556
3263.098865	361902.404818	52.442561
3261.574234	361653.866570	52.447565
3261.205224	361392.599583	52.452570
3260.770302	361124.216789	52.457575
3259.870511	360869.824896	52.462580
3259.010385	360620.794482	52.467585
3258.491700	360366.695891	52.472589
3257.962954	360102.673516	52.477594
3257.306460	359835.870801	52.482599
3256.198710	359600.844365	52.487604
3256.137308	359339.848400	52.492609
3255.182839	359091.588451	52.497613
3254.149366	358830.896197	52.502618
3254.316378	358571.819428	52.507623
3252.952163	358313.874135	52.512628
3252.508637	358054.814878	52.517633
3251.816382	357811.418341	52.522637
3251.464807	357543.308031	52.527642
3250.770569	357290.340972	52.532647
3249.875318	357042.417653	52.537652
3249.533176	356783.310315	52.542657
3248.512097	356524.690752	52.547661
3247.923164	356272.032743	52.552666
3247.740385	355998.008963	52.557671
3246.572023	355763.101229	52.562676
3245.792996	355489.525301	52.567681
3245.299467	355240.842523	52.572685
3244.675355	354969.784194	52.577690
3244.285401	354718.970257	52.582695
3243.240156	354467.469827	52.587700
3242.586704	354205.650163	52.592705
3242.156445	353949.850831	52.597709
3241.318950	353691.926002	52.602714
3240.983132	353426.438364	52.607719
3239.899600	353176.999195	52.612724
3239.487692	352924.245932	52.617729
3238.628998	352663.239984	52.622733
3238.039534	352407.076591	52.627738
3237.339412	352133.597855	52.632743
3236.318049	351895.722694	52.637748
3235.848481	351647.935317	52.642753
3235.417836	351391.512892	52.647757
3234.500749	351135.980613	52.652762
3234.004403	350878.446317	52.657767
3233.174106	350623.559620	52.662772
3232.845747	350355.001464	52.667777
3231.861335	350107.135782	52.672781
3231.117960	349851.442755	52.677786
3230.565436	349596.634606	52.682791
3229.912110	349351.741880	52.687796
3229.589222	349093.790008	52.692801
3228.978351	348839.318484	52.697805
3228.035058	348578.280889	52.702810
3227.356728	348316.563868	52.707815
3226.576337	348060.384888	52.712820
3225.976755	347800.790997	52.717825
3225.473402	347543.878648	52.722829
3224.530379	347298.208320	52.727834
3224.268061	347034.077950	52.732839
3223.249022	346786.584863	52.737844
3222.919403	346518.110354	52.742849
3222.222568	346264.353571	52.747853
3221.493064	346015.436922	52.752858
3220.937915	345756.513994	52.757863
3220.195510	345503.881040	52.762868
3219.336090	345244.851256	52.767873
3219.139506	344983.068321	52.772877
3217.843806	344732.708573	52.777882
3217.715719	344460.883775	52.782887
3216.812926	344219.164880	52.787892
3215.885852	343953.853059	52.792897
3215.339590	343702.275915	52.797901
3214.495050	343454.104847	52.802906
3214.186362	343184.797334	52.807911
3213.133003	342939.126247	52.812916
3212.610584	342686.675659	52.817921
3211.648194	342427.751800	52.822925
3211.258421	342175.634485	52.827930
3210.934977	341916.123760	52.832935
3210.136794	341668.854475	52.837940
3209.278395	341412.811759	52.842945
3208.827650	341156.219859	52.847949
3207.850854	340899.048283	52.852954
3207.788108	340644.632969	52.857959
3206.969633	340394.179938	52.862964
3206.239562	340127.420408	52.867969
3205.905715	339874.266744	52.872973
3204.750841	339613.325222	52.877978
3204.334899	339365.680963	52.882983
3203.295057	339108.486650	52.887988
3202.677774	338830.019607	52.892993
3202.076748	338608.697785	52.897997
3201.517870	338329.812059	52.903002
3201.096343	338083.105661	52.908007
3200.370392	337822.750941	52.913012
3199.498928	337550.148168	52.918017
3198.652284	337314.172419	52.923021
3197.707735	337056.089442	52.928026
3197.717919	336789.326407	52.933031
3196.661590	336538.972528	52.938036
3196.142138	336292.860479	52.943041
3195.406395	336039.220991	52.948045
3194.718388	335783.078199	52.953050
3194.236081	335517.813652	52.958055
3193.268343	335272.914402	52.963060
3192.515699	335010.949203	52.968065
3191.985422	334768.066468	52.973069
3191.331242	334515.426741	52.978074
3190.823732	334254.412753	52.983079
3189.736008	334012.735705	52.988084
3189.420152	333765.131314	52.993089
3188.842145	333491.447590	52.998093
3188.199636	333244.427667	53.003098
3187.354883	332990.005083	53.008103
3186.706511	332742.449725	53.013108
3186.233631	332490.639660	53.018113
3185.488068	332235.638625	53.023117
3184.809736	331981.924443	53.028122
3184.359430	331717.938924	53.033127
3183.744225	331470.475806	53.038132
3182.743065	331215.358883	53.043137
3182.572028	330956.545508	53.048141
3181.574337	330707.510965	53.053146
3181.160885	330443.056790	53.058151
3180.305796	330176.711188	53.063156
3179.630905	329917.210139	53.068161
3179.174176	329654.822238	53.073165
3178.442258	329403.755499	53.078170
3177.820714	329146.458347	53.083175
3177.129096	328896.605624	53.088180
3176.164969	328637.044135	53.093185
3175.989629	328362.768532	53.098189
3175.071059	328105.260299	53.103194
3174.265545	327846.893154	53.108199
3173.403096	327595.561136	53.113204
3173.431606	327328.123872	53.118209
3172.683863	327072.800267	53.123213
3171.203082	326819.475873	53.128218
3171.030008	326569.457328	53.133223
3170.284445	326315.887732	53.138228
3169.240434	326055.464751	53.143233
3169.011980	325796.923303	53.148237
3168.024354	325542.269322	53.153242
3167.472820	325290.931843	53.158247
3166.697574	325042.760674	53.163252
3166.341918	324784.541702	53.168257
3165.717883	324540.571627	53.173261
3165.102109	324283.461622	53.178266
3164.745158	324015.896274	53.183271
3163.752733	323750.340208	53.188276
3162.943692	323494.938828	53.193281
3162.111133	323237.452573	53.198285
3161.762327	322980.831091	53.203290
3160.891978	322718.995360	53.208295
3160.265848	322478.253344	53.213300
3159.785080	322217.856711	53.218305
3158.741883	321948.814904	53.223309
3157.805107	321705.293664	53.228314
3157.357390	321453.317421	53.233319
3156.431779	321206.101077	53.238324
3155.932521	320954.258897	53.243329
3155.296327	320701.775666	53.248333
3154.763178	320456.022911	53.253338
3154.514736	320194.514242	53.258343
3153.540109	319956.214048	53.263348
3152.513445	319701.829243	53.268353
3152.470007	319443.468818	53.273357
3151.467827	319201.046132	53.278362
3150.931364	318945.257666	53.283367
3150.185011	318686.828136	53.288372
3149.483824	318431.649989	53.293377
3148.914220	318188.366937	53.298381
3148.382720	317940.799482	53.303386
3147.492576	317680.836762	53.308391
3146.806121	317433.547161	53.313396
3146.191411	317172.495533	53.318401
3145.822747	316914.001527	53.323405
3144.761598	316678.660598	53.328410
3144.247148	316419.755502	53.333415
3143.757101	316167.262636	53.338420
3143.166657	315897.138898	53.343425
3142.416260	315660.014920	53.348429
3141.315812	315405.681518	53.353434
3140.830250	315140.759214	53.358439
3140.247255	314904.014432	53.363444
3139.467508	314649.781222	53.368449
3139.040227	314383.956551	53.373453
3137.884141	314136.020267	53.378458
3137.332407	313882.742230	53.383463
3136.816323	313654.667252	53.388468
3136.235625	313388.074997	53.393473
3135.670697	313146.001478	53.398477
3134.931090	312883.812950	53.403482
3134.617652	312637.904369	53.408487
3133.583692	312396.743731	53.413492
3133.101096	312117.960984	53.418497
3132.800925	311866.421000	53.423501
3131.458071	311626.224300	53.428506
3131.007792	311368.901082	53.433511
3130.158230	311118.719597	53.438516
3129.670016	310855.391611	53.443521
3129.238066	310604.888300	53.448525
3128.206270	310353.613563	53.453530
3127.651779	310100.200130	53.458535
3127.026492	309862.279948	53.463540
3126.219040	309609.949556	53.468545
3125.726915	309336.865791	53.473549
3124.766570	309099.964788	53.478554
3124.165121	308849.841144	53.483559
3123.719044	308591.238015	53.488564
3123.081234	308339.642124	53.493569
3122.317328	308089.899170	53.498573
3121.387092	307830.683522	53.503578
3121.159347	307579.479613	53.508583
3120.384863	307336.357824	53.513588
3119.503680	307082.047708	53.518593
3119.091646	306824.072247	53.523597
3118.452981	306577.591590	53.528602
3117.653241	306316.824355	53.533607
3117.074553	306077.540019	53.538612
3116.338858	305814.036863	53.543617
3115.602150	305579.105801	53.548621
3114.640489	305328.624935	53.553626
3114.344651	305070.627741	53.558631
3113.594921	304818.991933	53.563636
3112.970926	304569.194786	53.568641
3112.390986	304320.536193	53.573645
3111.445796	304070.916325	53.578650
3111.051834	303808.246639	53.583655
3110.212333	303572.615465	53.588660
3109.387096	303322.924407	53.593665
3108.787121	303063.800303	53.598669
3108.437413	302832.776216	53.603674
3107.640700	302567.545053	53.608679
3106.930456	302323.411233	53.613684
3106.312088	302082.751364	53.618689
3105.714506	301821.918537	53.623693
3105.013537	301575.693841	53.628698
3104.526211	301321.285722	53.633703
3103.685579	301071.109593	53.638708
3103.611885	300809.071694	53.643713
3102.741923	300556.836633	53.648717
3101.865133	300312.445957	53.653722
3101.442067	300045.547089	53.658727
3100.633988	299796.993740	53.663732
3099.819034	299536.242597	53.668737
3099.255843	299273.643088	53.673741
3098.540125	299030.982289	53.678746
3097.854173	298767.739313	53.683751
3097.211729	298526.568767	53.688756
3096.475129	298270.947643	53.693761
3095.904541	298020.214994	53.698765
3095.102380	297758.364149	53.703770
3094.418889	297503.370228	53.708775
3093.947437	297262.705776	53.713780
3093.322332	297007.243544	53.718785
3092.361679	296753.667696	53.723789
3091.655534	296501.604736	53.728794
3090.926658	296248.169829	53.733799
3090.297466	295999.557581	53.738804
3089.875205	295746.608335	53.743809
3089.137818	295492.893691	53.748813
3088.305508	295264.864711	53.753818
3088.268209	294984.807440	53.758823
3087.593745	294735.691498	53.763828
3086.343806	294489.416801	53.768833
3086.020936	294232.324316	53.773837
3085.062764	293980.119926	53.778842
3084.619883	293712.578747	53.783847
3083.796118	293475.429225	53.788852
3083.193858	293222.530994	53.793857
3082.489686	292963.179879	53.798861
3081.906220	292721.407425	53.803866
3081.313130	292468.456009	53.808871
3080.803050	292209.760996	53.813876
3079.824245	291956.844624	53.818881
3079.618700	291697.973558	53.823885
3078.466075	291452.062316	53.828890
3078.115264	291189.597325	53.833895
3077.379954	290946.064470	53.838900
3076.717006	290682.757007	53.843905
3075.840568	290424.347412	53.848909
3075.123439	290171.515274	53.853914
3074.323018	289926.132681	53.858919
3074.032315	289669.386989	53.863924
3073.360392	289422.226362	53.868929
3072.705023	289170.096684	53.873933
3072.066254	288915.442854	53.878938
3071.600079	288658.163780	53.883943
3070.825323	288408.497296	53.888948
3070.137425	288146.617742	53.893953
3069.420126	287895.362764	53.898957
3068.960300	287642.309568	53.903962
3068.321152	287378.842693	53.908967
3067.513741	287117.745304	53.913972
3066.839617	286867.705220	53.918977
3066.364929	286598.863469	53.923981
3065.473458	286342.006529	53.928986
3064.877165	286097.836739	53.933991
3063.962991	285826.389854	53.938996
3063.421395	285584.808843	53.944001
3063.196715	285323.592564	53.949005
3061.945454	285064.677903	53.954010
3061.345596	284811.492212	53.959015
3060.964696	284552.006564	53.964020
3060.313383	284307.054952	53.969025
3059.118724	284047.876083	53.974029
3058.557563	283793.257507	53.979034
3058.304813	283538.157039	53.984039
3057.488166	283286.150935	53.989044
3056.677779	283022.784893	53.994049
3055.997086	282772.132327	53.999053
3055.239209	282516.551027	54.004058
3055.052372	282261.490490	54.009063
3054.338135	282016.445939	54.014068
3053.370414	281752.773161	54.019073
3052.809020	281496.676468	54.024077
3051.911506	281248.528048	54.029082
3051.497029	280989.097050	54.034087
3050.629007	280745.910122	54.039092
3049.847469	280492.318360	54.044097
3049.337442	280233.182398	54.049101
3048.638668	279994.298094	54.054106
3047.871714	279736.221390	54.059111
3047.156521	279483.281037	54.064116
3047.036726	279232.844175	54.069121
3046.150869	278975.906720	54.074125
3045.498184	278732.557889	54.079130
3045.329044	278469.572784	54.084135
3044.279152	278212.431934	54.089140
3043.728982	277955.746798	54.094145
3043.297601	277701.258577	54.099149
3042.253770	277445.644768	54.104154
3041.589866	277179.757985	54.109159
3040.970983	276932.354103	54.114164
3040.226066	276670.504105	54.119169
3039.724185	276419.210481	54.124173
3038.932587	276165.288517	54.129178
3038.484291	275907.568363	54.134183
3037.429241	275647.040836	54.139188
3036.435491	275402.319481	54.144193
3036.178282	275135.247663	54.149197
3035.633774	274887.016996	54.154202
3035.007298	274636.099667	54.159207
3034.250072	274387.316924	54.164212
3033.533394	274124.214555	54.169217
3032.812345	273872.140714	54.174221
3032.203463	273629.141363	54.179226
3031.522048	273365.396799	54.184231
3030.737943	273117.178765	54.189236
3029.658872	272869.924316	54.194241
3029.443275	272610.817809	54.199245
3028.711756	272366.488247	54.204250
3028.388043	272104.750249	54.209255
3027.604568	271851.846187	54.214260
3026.650455	271611.907108	54.219265
3025.983943	271345.741128	54.224269
3025.369152	271115.528312	54.229274
3024.891233	270855.063003	54.234279
3024.409069	270594.751259	54.239284
3023.294932	270344.828814	54.244289
3023.107211	270080.573995	54.249293
3022.403572	269833.642952	54.254298
3021.626151	269576.663709	54.259303
3020.842835	269326.740208	54.264308
3020.250020	269072.075030	54.269313
3019.890876	268828.273383	54.274317
3018.962752	268575.444263	54.279322
3018.663118	268310.571193	54.284327
3017.875832	268056.650354	54.289332
3017.326694	267794.873212	54.294337
3016.708420	267524.804521	54.299341
3015.846533	267285.336331	54.304346
3015.193968	267014.483838	54.309351
3014.308512	266762.387442	54.314356
3013.721082	266503.393094	54.319361
3013.251074	266238.573586	54.324365
3012.406073	265998.059216	54.329370
3011.945035	265732.219883	54.334375
3011.051943	265480.431070	54.339380
3010.255403	265218.643664	54.344385
3009.894572	264964.275075	54.349389
3009.117433	264710.787524	54.354394
3008.210023	264442.421991	54.359399
3007.378197	264183.264102	54.364404
3006.365936	263934.373079	54.369409
3006.273602	263675.760694	54.374413
3005.489124	263444.737935	54.379418
3004.895234	263187.453239	54.384423
3004.772980	262922.682948	54.389428
3003.601209	262677.510963	54.394433
3003.343697	262401.658535	54.399437
3002.337768	262166.469566	54.404442
3001.849570	261899.160358	54.409447
3001.110652	261655.677970	54.414452
3000.475789	261392.696493	54.419457
2999.992695	261135.879896	54.424461
2998.919325	260879.844589	54.429466
2998.476690	260630.815173	54.434471
2998.030408	260370.988281	54.439476
2996.956048	260122.135731	54.444481
2996.608866	259853.456400	54.449485
2995.806782	259612.176059	54.454490
2995.307042	259343.572349	54.459495
2994.406628	259092.426664	54.464500
2993.643091	258829.187981	54.469505
2993.593154	258569.172876	54.474509
2992.506967	258315.077714	54.479514
2991.744479	258058.435788	54.484519
2991.175332	257807.748381	54.489524
2990.332594	257549.642620	54.494529
2989.566191	257293.307788	54.499533
2989.138867	257046.266081	54.504538
2988.424349	256784.168023	54.509543
2987.751533	256541.775325	54.514548
2986.922395	256295.129155	54.519553
2986.604743	256037.655170	54.524557
2985.634789	255783.366277	54.529562
2985.013653	255536.789959	54.534567
2984.714371	255267.191694	54.539572
2983.736091	255026.173423	54.544577
2983.240962	254758.847950	54.549581
2982.238706	254508.971594	54.554586
2981.912042	254241.951242	54.559591
2981.439395	253998.969669	54.564596
2980.578746	253746.779882	54.569601
2980.381513	253478.925191	54.574605
2979.496489	253228.522651	54.579610
2978.990642	252977.474705	54.584615
2978.309985	252707.507532	54.589620
2977.500011	252440.107911	54.594625
2976.916905	252182.451982	54.599629
2976.037864	251928.052074	54.604634
2975.454857	251665.863847	54.609639
2974.816027	251401.622072	54.614644
2973.941916	251146.687762	54.619649
2973.553150	250880.268047	54.624653
2973.138802	250623.733784	54.629658
2972.350322	250370.289645	54.634663
2972.031434	250107.247167	54.639668
2971.140573	249839.431599	54.644673
2970.265864	249575.408401	54.649677
2969.403572	249320.831648	54.654682
2968.902562	249048.728341	54.659687
2968.352205	248804.315000	54.664692
2967.598078	248535.919798	54.669697
2967.126281	248262.259850	54.674701
2966.121232	248011.833396	54.679706
2965.029135	247745.785060	54.684711
2964.784492	247493.965830	54.689716
2964.371401	247229.313450	54.694721
2963.787925	246969.832621	54.699725
2963.232623	246712.868918	54.704730
2962.421911	246444.893998	54.709735
2961.848509	246183.350306	54.714740
2960.632544	245921.119391	54.719745
2960.398423	245658.402506	54.724749
2959.900179	245395.371423	54.729754
2958.983993	245131.566653	54.734759
2958.603566	244855.759786	54.739764
2957.648723	244602.835917	54.744769
2957.092958	244344.119670	54.749773
2956.145301	244079.074194	54.754778
2955.723425	243811.475910	54.759783
2955.312031	243548.714906	54.764788
2954.325094	243287.344273	54.769793
2953.885566	243022.653472	54.774797
2952.871768	242754.921943	54.779802
2952.061833	242506.613935	54.784807
2951.541857	242253.982429	54.789812
2950.884121	241975.322735	54.794817
2950.209854	241724.855801	54.799821
2949.591194	241474.253265	54.804826
2948.977651	241197.701954	54.809831
2948.451092	240940.006793	54.814836
2947.451533	240674.009237	54.819841
2946.874087	240421.874547	54.824845
2945.960020	240163.198405	54.829850
2945.506158	239898.949692	54.834855
2945.050433	239648.197976	54.839860
2944.177563	239396.799851	54.844865
2943.657546	239127.979847	54.849869
2942.772095	238878.087269	54.854874
2942.280438	238607.736186	54.859879
2941.731026	238353.971989	54.864884
2940.702348	238089.512996	54.869889
2940.282754	237842.426464	54.874893
2939.697183	237571.914578	54.879898
2939.036954	237316.617068	54.884903
2938.210175	237073.289021	54.889908
2937.215938	236799.380732	54.894913
2937.098709	236538.549926	54.899917
2936.262753	236285.930954	54.904922
2935.665020	236021.332522	54.909927
2935.126930	235756.750795	54.914932
2934.219110	235500.070990	54.919937
2933.760944	235251.850846	54.924941
2932.758570	234985.944150	54.929946
2932.079179	234727.116709	54.934951
2931.736571	234473.278314	54.939956
2930.704844	234215.475583	54.944961
2930.327017	233952.248258	54.949965
2929.536275	233704.008251	54.954970
2929.257168	233441.836119	54.959975
2928.708827	233178.408722	54.964980
2927.900169	232917.798690	54.969985
2927.327477	232658.017743	54.974989
2926.574215	232385.662149	54.979994
2925.854159	232133.290107	54.984999
2924.955609	231873.359214	54.990004
2924.168976	231604.524986	54.995009
2923.981076	231355.431835	55.000013
2923.140677	231080.216628	55.005018
2922.155114	230837.947710	55.010023
2922.202027	230559.410844	55.015028
2921.476258	230306.331790	55.020033
2920.922694	230040.851720	55.025037
2919.893239	229776.007937	55.030042
2919.468594	229509.745188	55.035047
2918.685196	229244.864043	55.040052
2917.956401	228970.681584	55.045057
2917.640875	228714.181213	55.050061
2916.746674	228457.187600	55.055066
2916.180549	228176.896622	55.060071
2915.504260	227918.571593	55.065076
2914.639565	227658.316664	55.070081
2913.930926	227382.506563	55.075085
2913.301022	227115.418024	55.080090
2912.559653	226860.976602	55.085095
2912.013839	226593.876416	55.090100
2911.124847	226342.871704	55.095105
2910.740158	226075.747680	55.100109
2910.172545	225812.829025	55.105114
2909.438735	225555.755257	55.110119
2908.672920	225287.573887	55.115124
2907.902060	225025.160975	55.120129
2907.134454	224759.082126	55.125133
2906.585210	224491.582011	55.130138
2906.058899	224232.633759	55.135143
2905.700104	223961.451754	55.140148
2904.568105	223700.997156	55.145153
2904.214754	223441.654952	55.150157
2903.137948	223179.793062	55.155162
2902.562576	222913.015331	55.160167
2901.987865	222656.536820	55.165172
2901.120465	222386.128237	55.170177
2900.930992	222132.620170	55.175181
2899.954757	221873.407321	55.180186
2899.395937	221602.914479	55.185191
2898.695318	221327.047718	55.190196
2897.928760	221083.334472	55.195201
2897.730180	220807.250120	55.200205
2897.327908	220545.532391	55.205210
2896.200743	220274.128722	55.210215
2895.771781	220010.825942	55.215220
2894.974466	219739.715721	55.220225
2894.581334	219471.699372	55.225229
2893.675928	219199.373543	55.230234
2892.844566	218934.076243	55.235239
2892.324627	218659.323807	55.240244
2891.288715	218399.687139	55.245249
2890.883649	218125.936895	55.250253
2890.250343	217868.007764	55.255258
2889.445538	217603.296757	55.260263
2889.159630	217330.956375	55.265268
2888.467425	217071.944813	55.270273
2887.963475	216798.100847	55.275277
2886.736539	216531.220485	55.280282
2886.337682	216254.370787	55.285287
2885.644518	215991.824860	55.290292
2884.599757	215735.661711	55.295297
2884.486760	215456.695230	55.300301
2883.602050	215187.029311	55.305306
2882.677810	214933.981321	55.310311
2882.222119	214667.368025	55.315316
2881.206108	214407.845085	55.320321
2880.651777	214136.374583	55.325325
2879.900841	213889.909094	55.330330
2879.613768	213614.999984	55.335335
2879.024912	213351.315093	55.340340
2878.005829	213098.378235	55.345345
2877.856475	212838.138780	55.350349
2876.897579	212565.542409	55.355354
2876.318662	212291.843337	55.360359
2875.908335	212032.450308	55.365364
2875.082395	211762.305497	55.370369
2874.291907	211493.658093	55.375373
2873.847119	211227.528086	55.380378
2873.083576	210958.216847	55.385383
2872.569662	210695.841956	55.390388
2871.647180	210430.249148	55.395393
2871.287842	210162.010081	55.400397
2870.919662	209879.569762	55.405402
2869.719756	209617.206209	55.410407
2869.280733	209344.261446	55.415412
2868.385505	209072.548309	55.420417
2868.092506	208801.670111	55.425421
2866.906276	208543.725330	55.430426
2866.545558	208275.100178	55.435431
2866.304908	207999.559155	55.440436
2865.173178	207728.067666	55.445441
2864.643075	207453.911309	55.450445
2863.889050	207175.935428	55.455450
2862.874932	206923.862889	55.460455
2862.385219	206647.489390	55.465460
2861.734060	206386.796573	55.470465
2861.007509	206107.370523	55.475469
2860.333106	205844.278464	55.480474
2859.391020	205591.627540	55.485479
2858.971588	205307.269711	55.490484
2858.063300	205052.350475	55.495489
2857.648002	204793.727300	55.500493
2856.873331	204522.028668	55.505498
2856.338908	204267.664578	55.510503
2855.617913	204004.970072	55.515508
2854.951601	203741.593639	55.520513
2854.863404	203466.558916	55.525517
2853.778414	203212.248557	55.530522
2853.067744	202936.449619	55.535527
2852.665932	202666.838806	55.540532
2851.620076	202396.542276	55.545537
2851.163906	202125.262886	55.550541
2850.595709	201862.541493	55.555546
2849.673029	201608.849041	55.560551
2849.355026	201325.169679	55.565556
2848.648973	201063.122937	55.570561
2848.139656	200791.489503	55.575565
2847.257951	200524.039409	55.580570
2846.653874	200249.242350	55.585575
2846.149302	199976.708750	55.590580
2845.168893	199717.104304	55.595585
2844.768100	199434.720461	55.600589
2843.955673	199168.335046	55.605594
2843.382688	198905.412418	55.610599
2842.691997	198630.192012	55.615604
2841.785575	198363.265627	55.620609
2841.232203	198081.307617	55.625613
2840.638306	197829.400600	55.630618
2839.935337	197548.983385	55.635623
2839.351843	197276.310757	55.640628
2838.482390	197023.026117	55.645633
2838.063570	196745.431261	55.650637
2837.584618	196473.662466	55.655642
2836.637646	196208.674937	55.660647
2836.028449	195936.726019	55.665652
2835.412194	195662.934659	55.670657
2834.795452	195399.922180	55.675661
2833.956553	195124.234912	55.680666
2833.137905	194861.142687	55.685671
2832.993353	194584.406841	55.690676
2832.220779	194329.275274	55.695681
2831.325953	194046.808229	55.700685
2831.061787	193775.108966	55.705690
2830.236749	193496.654683	55.710695
2829.466731	193227.023410	55.715700
2828.530355	192963.654468	55.720705
2828.122996	192680.685419	55.725709
2827.730213	192412.004024	55.730714
2826.793833	192139.262392	55.735719
2826.210822	191874.138431	55.740724
2825.541511	191592.425873	55.745729
2824.689278	191328.912471	55.750733
2824.090829	191057.103088	55.755738
2823.023470	190794.759020	55.760743
2822.887560	190516.886945	55.765748
2822.022082	190257.172931	55.770753
2821.423298	189989.033826	55.775757
2820.728384	189717.323669	55.780762
2820.090149	189461.318479	55.785767
2819.824615	189176.082948	55.790772
2819.115956	188907.662032	55.795777
2818.057375	188629.590906	55.800781
2817.566265	188355.095587	55.805786
2817.198099	188083.050521	55.810791
2816.303777	187809.436492	55.815796
2815.222589	187538.703411	55.820801
2814.656475	187264.391805	55.825805
2814.370529	187000.711145	55.830810
2813.264434	186736.398567	55.835815
2813.132701	186461.641312	55.840820
2812.258395	186197.880343	55.845825
2811.429749	185922.002701	55.850829
2810.902711	185659.996330	55.855834
2810.299170	185385.383904	55.860839
2809.826763	185105.816489	55.865844
2809.063895	184844.411943	55.870849
2808.455148	184564.538736	55.875853
2807.746487	184288.728428	55.880858
2806.752915	184016.412356	55.885863
2806.147706	183737.472422	55.890868
2805.349219	183477.417241	55.895873
2804.880151	183202.237234	55.900877
2804.193408	182935.260143	55.905882
2803.505265	182674.174572	55.910887
2802.923806	182393.763789	55.915892
2802.059641	182138.598931	55.920897
2801.428338	181864.763236	55.925901
2800.647177	181602.337729	55.930906
2800.006273	181322.375766	55.935911
2799.333762	181059.592901	55.940916
2798.757466	180797.101687	55.945921
2798.300874	180525.014923	55.950925
2797.682656	180247.066140	55.955930
2796.788982	179983.396344	55.960935
2796.813827	179712.815780	55.965940
2795.492020	179437.120643	55.970945
2795.187847	179165.438186	55.975949
2794.729021	178899.900078	55.980954
2793.566944	178626.080163	55.985959
2793.167198	178344.382476	55.990964
2792.609180	178084.347299	55.995969
2791.767045	177798.449664	56.000973
2791.118619	177528.727505	56.005978
2790.458912	177247.269194	56.010983
2790.165000	176983.892124	56.015988
2789.044282	176707.661687	56.020993
2788.765844	176440.279192	56.025997
2788.023765	176155.152934	56.031002
2787.120158	175882.849192	56.036007
2786.668347	175611.137081	56.041012
2785.864298	175333.428580	56.046017
2785.452669	175049.109867	56.051021
2784.713860	174783.515417	56.056026
2784.456492	174494.890110	56.061031
2783.404616	174224.770373	56.066036
2782.560449	173947.090488	56.071041
2781.929742	173672.558209	56.076045
2781.684580	173394.914474	56.081050
2780.385589	173120.046716	56.086055
2779.648619	172841.696235	56.091060
2779.051801	172564.737166	56.096065
2778.572701	172298.711162	56.101069
2777.934006	172023.161456	56.106074
2777.178151	171759.039676	56.111079
2776.871224	171469.706606	56.116084
2775.771034	171198.953883	56.121089
2775.040287	170931.285643	56.126093
2774.783868	170665.095594	56.131098
2774.168131	170380.499376	56.136103
2773.233701	170097.430874	56.141108
2772.445082	169835.374764	56.146113
2771.680916	169550.693730	56.151117
2771.463463	169292.543877	56.156122
2770.674153	168970.764367	56.161127
2770.581293	168684.915278	56.166132
2769.589434	168381.115549	56.171137
2768.881133	168127.145952	56.176141
2768.648127	167821.755451	56.181146
2767.007210	167565.088954	56.186151
2767.082516	167244.433328	56.191156
2765.960693	167013.514239	56.196161
2765.681550	166710.988396	56.201165
2764.808594	166447.710229	56.206170
2763.849705	166174.262446	56.211175
2763.762781	165870.670314	56.216180
2762.639054	165606.344308	56.221185
2762.161421	165339.489264	56.226189
2761.220942	165060.121527	56.231194
2760.600653	164753.736731	56.236199
2759.557226	164523.837945	56.241204
2758.819464	164261.978022	56.246209
2758.438472	163967.170527	56.251213
2758.018400	163680.191084	56.256218
2757.541237	163438.982463	56.261223
2757.185093	163127.216685	56.266228
2755.936392	162891.931680	56.271233
2755.375442	162605.987498	56.276237
2755.358072	162287.907207	56.281242
2754.708046	162064.242492	56.286247
2753.471708	161760.764947	56.291252
2752.853770	161459.048252	56.296257
2752.552936	161214.533758	56.301261
2751.841060	160897.872646	56.306266
2750.675866	160639.552186	56.311271
2750.253277	160348.302650	56.316276
2749.728919	160067.127869	56.321281
2748.922621	159829.021532	56.326285
2748.099975	159527.341029	56.331290
2747.672060	159242.928442	56.336295
2746.753288	158973.495454	56.341300
2746.283618	158677.792304	56.346305
2745.686764	158434.437335	56.351309
2744.679439	158124.382409	56.356314
2744.305282	157873.838908	56.361319
2743.515121	157574.382185	56.366324
2743.115928	157314.159864	56.371329
2741.934503	157030.456842	56.376333
2742.040926	156736.636748	56.381338
2740.828308	156498.338000	56.386343
2740.548546	156177.481897	56.391348
2739.733634	155942.518116	56.396353
2738.982869	155631.046812	56.401357
2738.389307	155359.594925	56.406362
2737.502596	155117.529756	56.411367
2737.179657	154783.168673	56.416372
2736.248211	154546.872940	56.421377
2735.616176	154271.711512	56.426381
2734.546144	153976.627223	56.431386
2734.426670	153681.738172	56.436391
2733.866575	153446.713330	56.441396
2732.742741	153154.860685	56.446401
2732.193507	152862.042560	56.451405
2731.593486	152591.046326	56.456410
2730.962731	152324.645646	56.461415
2730.709950	152023.119490	56.466420
2729.383452	151777.131816	56.471425
2729.075771	151459.808025	56.476429
2728.269904	151220.681771	56.481434
2727.625734	150906.352660	56.486439
2727.204248	150668.122812	56.491444
2726.418182	150370.827040	56.496449
2725.876380	150083.726490	56.501453
2725.222065	149830.529694	56.506458
2724.508992	149522.274606	56.511463
2724.021561	149273.097318	56.516468
2723.090768	148974.604528	56.521473
2722.345746	148702.252926	56.526477
2721.722804	148405.318010	56.531482
2721.291489	148156.966589	56.536487
2720.227149	147862.267140	56.541492
2719.584604	147580.021540	56.546497
2718.936490	147299.329763	56.551501
2718.207885	147045.378865	56.556506
2717.558600	146740.165139	56.561511
2716.930790	146486.990678	56.566516
2716.261379	146212.284761	56.571521
2715.692268	145934.083395	56.576525
2715.059025	145630.275776	56.581530
2714.138955	145402.114450	56.586535
2713.861589	145094.087556	56.591540
2712.883565	144840.994598	56.596545
2712.322156	144548.025612	56.601549
2711.913799	144273.104811	56.606554
2710.959573	143995.261340	56.611559
2710.498130	143721.230650	56.616564
2709.882061	143445.956204	56.621569
2708.759198	143162.441574	56.626573
2708.060717	142904.936386	56.631578
2707.540975	142615.905536	56.636583
2707.272463	142342.110737	56.641588
2706.358843	142075.472590	56.646593
2705.634097	141794.525098	56.651597
2705.217104	141524.598450	56.656602
2704.455834	141257.663821	56.661607
2703.928728	140972.309091	56.666612
2703.066868	140688.051959	56.671617
2702.410367	140432.149320	56.676621
2701.888092	140129.471356	56.681626
2700.992021	139888.934127	56.686631
2700.748618	139591.540981	56.691636
2699.490430	139335.336463	56.696641
2699.095337	139041.670029	56.701645
2698.646337	138753.897405	56.706650
2697.614870	138503.089141	56.711655
2697.232344	138209.187564	56.716660
2696.494789	137951.515011	56.721665
2695.660514	137643.728318	56.726669
2695.162014	137418.456979	56.731674
2694.261224	137115.641042	56.736679
2694.340954	136852.296917	56.741684
2693.391458	136550.637906	56.746689
2692.449280	136298.030352	56.751693
2691.883496	136018.153979	56.756698
2691.192534	135715.001737	56.761703
2690.710828	135470.585761	56.766708
2689.883090	135164.246965	56.771713
2689.077065	134920.217304	56.776717
2688.660272	134597.508464	56.781722
2687.903250	134360.665733	56.786727
2687.233960	134085.473764	56.791732
2686.365556	133788.187797	56.796737
2685.560699	133514.877386	56.801741
2685.398467	133270.569223	56.806746
2684.404170	132977.427252	56.811751
2683.784486	132673.457452	56.816756
2683.282115	132438.495657	56.821761
2682.425707	132126.846317	56.826765
2681.984622	131889.847046	56.831770
2680.943923	131601.934431	56.836775
2680.513619	131300.388123	56.841780
2679.936732	131068.764657	56.846785
2678.942257	130794.138785	56.851789
2677.967265	130502.530923	56.856794
2678.035208	130208.220652	56.861799
2677.339057	129962.565086	56.866804
2676.815707	129689.932998	56.871809
2676.286243	129386.492498	56.876813
2675.579751	129098.286005	56.881818
2674.664196	128880.120836	56.886823
2674.034596	128580.007171	56.891828
2673.376061	128274.897457	56.896833
2672.778134	128033.891728	56.901837
2672.401992	127749.291930	56.906842
2671.067651	127464.973885	56.911847
2670.636514	127174.165834	56.916852
2670.237215	126924.667667	56.921857
2668.980802	126621.258534	56.926861
2668.955314	126348.923560	56.931866
2667.838711	126088.561757	56.936871
2667.610514	125799.628418	56.941876
2666.625831	125525.383719	56.946881
2666.676338	125226.202381	56.951885
2665.757902	124966.188255	56.956890
2664.780017	124684.179429	56.961895
2664.445082	124400.446301	56.966900
2663.649678	124136.890544	56.971905
2663.014534	123841.541149	56.976909
2662.063713	123572.415686	56.981914
2661.441792	123270.823073	56.986919
2660.764004	123031.969716	56.991924
2659.735987	122736.453554	56.996929
2659.788570	122438.522027	57.001933
2659.126225	122193.820222	57.006938
2658.174828	121887.432440	57.011943
2657.537713	121621.425988	57.016948
2656.955558	121349.166603	57.021953
2656.476787	121057.391309	57.026957
2655.874055	120805.049471	57.031962
2654.612347	120501.799612	57.036967
2654.549536	120222.816642	57.041972
2653.498332	119946.881656	57.046977
2653.069286	119642.405287	57.051981
2652.168745	119406.813248	57.056986
2651.254808	119109.510685	57.061991
2651.169010	118811.521715	57.066996
2650.413725	118533.053821	57.072001
2649.404738	118296.524208	57.077005
2648.708076	117998.749314	57.082010
2648.367668	117689.610007	57.087015
2647.820640	117415.558178	57.092020
2646.950317	117174.948158	57.097025
2646.105055	116858.815087	57.102029
2645.561395	116579.681075	57.107034
2644.796195	116332.581727	57.112039
2644.309549	116027.801821	57.117044
2643.164469	115781.580457	57.122049
2642.354306	115479.930396	57.127053
2642.028293	115225.403328	57.132058
2641.055749	114946.304458	57.137063
2640.628235	114696.578026	57.142068
2639.947224	114410.876256	57.147073
2639.501234	114126.549464	57.152077
2638.516876	113861.008377	57.157082
2638.042022	113561.581227	57.162087
2637.731857	113297.468820	57.167092
2636.637387	113063.571900	57.172097
2635.693100	112761.772650	57.177101
2636.062923	112465.245690	57.182106
2634.689370	112234.808737	57.187111
2634.244643	111942.980009	57.192116
2633.864562	111656.494217	57.197121
2632.847749	111418.304213	57.202125
2632.194379	111129.621347	57.207130
2631.189778	110842.279379	57.212135
2631.085319	110575.142762	57.217140
2629.935990	110294.271121	57.222145
2629.443711	110051.994404	57.227149
2629.147293	109725.794044	57.232154
2628.332132	109501.385982	57.237159
2627.897101	109211.193574	57.242164
2627.092901	108927.002383	57.247169
2626.279189	108652.226095	57.252173
2625.621016	108351.489012	57.257178
2624.803708	108111.599111	57.262183
2624.620008	107814.321429	57.267188
2623.771201	107538.294337	57.272193
2623.082548	107278.760894	57.277197
2622.688571	106980.238794	57.282202
2621.825015	106718.448621	57.287207
2621.432377	106436.061534	57.292212
2620.501791	106140.648650	57.297217
2619.622580	105886.959464	57.302221
2618.960939	105585.293163	57.307226
2617.909294	105331.256546	57.312231
2617.655733	105054.738702	57.317236
2616.997436	104768.682982	57.322241
2616.362344	104504.432038	57.327245
2615.670262	104222.010812	57.332250
2615.321793	103940.344211	57.337255
2614.434244	103678.705501	57.342260
2613.808016	103392.915117	57.347265
2612.832410	103114.504340	57.352269
2612.370025	102848.360484	57.357274
2611.555686	102557.826887	57.362279
2611.082482	102301.828150	57.367284
2610.402541	101995.440272	57.372289
2609.833855	101770.837565	57.377293
2608.952810	101461.868722	57.382298
2608.558895	101202.792957	57.387303
2607.906078	100907.909177	57.392308
2607.485996	100654.692135	57.397313
2606.272408	100369.583726	57.402317
2606.404184	100069.423045	57.407322
2605.023316	99822.501046	57.412327
2604.794779	99516.905338	57.417332
2603.896528	99234.704088	57.422337
2602.961921	98981.942155	57.427341
2602.619982	98679.204411	57.432346
2601.777151	98420.706756	57.437351
2601.027603	98119.759839	57.442356
2600.244333	97879.931070	57.447361
2599.846261	97574.648204	57.452365
2599.284373	97319.194548	57.457370
2598.247288	97035.279362	57.462375
2597.968577	96778.207733	57.467380
2597.472231	96461.013294	57.472385
2596.673051	96225.935668	57.477389
2596.137558	95918.629435	57.482394
2594.986693	95662.602912	57.487399
2594.820814	95373.516193	57.492404
2594.047966	95099.825331	57.497409
2593.208185	94840.575405	57.502413
2592.795686	94532.177918	57.507418
2592.005846	94289.889843	57.512423
2591.587043	93978.539578	57.517428
2590.467256	93726.189220	57.522433
2589.743610	93423.683954	57.527437
2589.169940	93162.401243	57.532442
2588.709522	92867.819873	57.537447
2587.812104	92604.610319	57.542452
2587.138565	92338.851119	57.547457
2586.683121	92044.260914	57.552461
2586.045118	91763.469136	57.557466
2584.946158	91504.686047	57.562471
2584.260162	91222.792840	57.567476
2583.693433	90950.420348	57.572481
2583.025581	90682.346999	57.577485
2582.634734	90406.301369	57.582490
2581.904782	90147.234921	57.587495
2581.314602	89855.979695	57.592500
2580.589347	89582.305289	57.597505
2579.593900	89312.563532	57.602509
2579.494557	89040.369073	57.607514
2578.644523	88758.679541	57.612519
2578.099684	88473.217568	57.617524
2577.296302	88220.347949	57.622529
2576.802042	87940.229313	57.627533
2576.116309	87653.653056	57.632538
2575.464097	87395.754651	57.637543
2574.957819	87082.557539	57.642548
2574.143167	86846.802928	57.647553
2573.040291	86537.841495	57.652557
2572.951908	86280.348938	57.657562
2571.544727	86006.403317	57.662567
2571.494478	85701.147616	57.667572
2570.920808	85470.701014	57.672577
2569.997287	85194.736843	57.677581
2569.476832	84891.183663	57.682586
2569.004232	84593.331940	57.687591
2568.226386	84360.698588	57.692596
2567.594548	84058.252548	57.697601
2566.803227	83782.862637	57.702605
2566.500758	83490.025794	57.707610
2565.410657	83221.903465	57.712615
2565.022403	82952.697275	57.717620
2564.576742	82660.991164	57.722625
2563.427128	82396.735967	57.727629
2562.768608	82104.114332	57.732634
2562.164559	81828.441547	57.737639
2561.589322	81563.548154	57.742644
2560.846314	81290.731090	57.747649
2560.221920	80999.608885	57.752653
2559.695904	80698.943764	57.757658
2558.640035	80468.527106	57.762663
2558.184556	80169.227352	57.767668
2557.663760	79881.317411	57.772673
2556.861982	79616.269344	57.777677
2556.342296	79327.315012	57.782682
2555.549619	79061.005260	57.787687
2554.711962	78789.041003	57.792692
2554.025415	78490.188813	57.797697
2553.332963	78246.584464	57.802701
2553.248113	77965.038600	57.807706
2552.101687	77686.142401	57.812711
2551.508816	77410.533230	57.817716
2550.641271	77127.608573	57.822721
2549.782654	76859.316683	57.827725
2549.053153	76586.819712	57.832730
2548.527032	76328.955713	57.837735
2548.256205	76041.465722	57.842740
2547.487544	75766.394597	57.847745
2546.386037	75509.614288	57.852749
2546.228832	75211.366312	57.857754
2545.243264	74967.847762	57.862759
2544.660554	74677.537601	57.867764
2544.087502	74421.390663	57.872769
2543.223549	74143.759290	57.877773
2542.748309	73879.538896	57.882778
2542.385639	73595.506766	57.887783
2541.480970	73327.674660	57.892788
2540.961645	73059.582358	57.897793
2539.928590	72781.135164	57.902797
2539.781352	72512.851884	57.907802
2538.417037	72250.960482	57.912807
2538.291574	71978.462038	57.917812
2537.650278	71688.172978	57.922817
2537.024327	71416.547069	57.927821
2536.156900	71134.270738	57.932826
2535.499523	70867.743862	57.937831
2534.746670	70608.285692	57.942836
2534.401500	70317.184422	57.947841
2533.523546	70034.007086	57.952845
2532.993989	69788.997584	57.957850
2532.289616	69496.768295	57.962855
2531.441680	69238.812752	57.967860
2530.785619	68956.584892	57.972865
2530.298975	68671.598154	57.977869
2529.564306	68418.423688	57.982874
2528.887939	68138.839286	57.987879
2528.153476	67863.479767	57.992884
2527.371514	67585.047401	57.997889
2526.654873	67330.234454	58.002893
2526.321744	67044.712094	58.007898
2525.557086	66785.740448	58.012903
2525.035714	66478.369578	58.017908
2524.284908	66252.834103	58.022913
2523.497914	65955.183848	58.027917
2523.110407	65690.160590	58.032922
2522.241584	65410.817136	58.037927
2521.334099	65143.160865	58.042932
2520.654935	64882.915807	58.047937
2519.654289	64588.831897	58.052941
2519.368010	64356.824199	58.057946
2518.833786	64052.723626	58.062951
2518.071361	63816.726449	58.067956
2517.073479	63556.641808	58.072961
2516.142115	63277.709889	58.077965
2516.554643	63005.005251	58.082970
2515.083478	62763.523596	58.087975
2514.600742	62463.999067	58.092980
2514.073236	62221.054644	58.097985
2513.323781	61934.819844	58.102989
2512.825670	61683.621593	58.107994
2512.225982	61418.115320	58.112999
2511.429504	61142.492080	58.118004
2510.866883	60883.372387	58.123009
2510.132734	60611.504511	58.128013
2509.459228	60360.946844	58.133018
2508.504287	60077.830687	58.138023
2508.203470	59809.758020	58.143028
2507.326829	59558.724189	58.148033
2506.730905	59258.806577	58.153037
2506.232858	59038.207231	58.158042
2505.031988	58756.330733	58.163047
2504.874416	58456.331257	58.168052
2504.014893	58223.176511	58.173057
2503.171971	57954.874668	58.178061
2502.842517	57667.071991	58.183066
2501.778175	57441.014251	58.188071
2501.604486	57145.440966	58.193076
2500.950475	56869.190632	58.198081
2500.252652	56650.575614	58.203085
2499.693168	56347.417516	58.208090
2498.720258	56128.564320	58.213095
2498.320076	55824.778815	58.218100
2497.453082	55574.269096	58.223105
2496.496247	55312.334033	58.228109
2496.206287	55057.274752	58.233114
2495.103418	54794.034848	58.238119
2494.789285	54509.332929	58.243124
2494.294397	54287.799545	58.248129
2493.414129	53994.933234	58.253133
2492.991333	53736.708039	58.258138
2492.103814	53484.230482	58.263143
2491.725191	53193.474581	58.268148
2491.154759	52955.756174	58.273153
2489.934330	52680.032404	58.278157
2489.894176	52397.262953	58.283162
2488.683902	52159.944372	58.288167
2488.043176	51867.457373	58.293172
2487.548853	51620.116611	58.298177
2486.681071	51367.194122	58.303181
2486.276549	51080.083207	58.308186
2485.113445	50850.756738	58.313191
2484.841975	50568.375421	58.318196
2483.962122	50309.398602	58.323201
2483.375547	50061.201825	58.328205
2482.798653	49775.838034	58.333210
2482.079865	49542.924212	58.338215
2481.297609	49274.272862	58.343220
2480.928315	48993.842724	58.348225
2479.920319	48772.784472	58.353229
2479.267495	48478.093044	58.358234
2478.564699	48241.619173	58.363239
2478.542644	47956.468706	58.368244
2477.663719	47718.052720	58.373249
2476.888972	47444.955136	58.378253
2476.440462	47184.560586	58.383258
2475.696951	46920.414639	58.388263
2475.022971	46661.575513	58.393268
2474.429002	46392.789449	58.398273
2473.433915	46127.265641	58.403277
2472.917130	45874.701101	58.408282
2472.388294	45617.271348	58.413287
2471.442727	45352.387173	58.418292
2470.980729	45088.091373	58.423297
2470.198755	44827.278655	58.428301
2470.037884	44563.695787	58.433306
2469.274831	44300.481186	58.438311
2468.230067	44032.792785	58.443316
2467.720199	43776.045029	58.448321
2466.489664	43515.436948	58.453325
2466.090270	43253.217868	58.458330
2465.643087	42998.400765	58.463335
2465.081488	42735.045179	58.468340
2464.030841	42479.461757	58.473345
2463.175402	42230.659433	58.478349
2462.775548	41964.785492	58.483354
2462.035102	41704.285174	58.488359
2461.019937	41460.619808	58.493364
2460.715173	41205.076210	58.498369
2459.859476	40947.957389	58.503373
2459.241458	40697.008467	58.508378
2458.697388	40450.909745	58.513383
2457.617936	40189.690974	58.518388
2457.382631	39928.309183	58.523393
2456.429712	39687.283495	58.528397
2455.882586	39432.713811	58.533402
2455.191366	39184.588935	58.538407
2454.424062	38929.868820	58.543412
2454.009245	38668.607547	58.548417
2453.022063	38442.042217	58.553421
2452.291821	38188.696295	58.558426
2451.517085	37949.023311	58.563431
2451.060780	37683.767217	58.568436
2450.499585	37430.563926	58.573441
2449.578611	37210.610203	58.578445
2449.000056	36961.848827	58.583450
2448.422250	36716.957147	58.588455
2447.624394	36454.861445	58.593460
2446.883712	36214.896353	58.598465
2446.161720	35975.371117	58.603469
2445.339025	35722.815047	58.608474
2444.695839	35493.897285	58.613479
2444.127535	35256.523227	58.618484
2443.416981	35009.697215	58.623489
2442.624584	34785.641042	58.628493
2441.792380	34539.411803	58.633498
2440.959107	34310.436099	58.638503
2440.310933	34080.996446	58.643508
2439.792927	33843.073518	58.648513
2439.140242	33606.106147	58.653517
2438.376724	33370.215358	58.658522
2437.645049	33141.081642	58.663527
2437.235491	32909.472787	58.668532
2436.830198	32671.405002	58.673537
2435.528300	32451.364238	58.678541
2435.048046	32215.648850	58.683546
2434.626574	31983.362751	58.688551
2434.058125	31752.552201	58.693556
2433.448465	31519.820534	58.698561
2432.586817	31290.826339	58.703565
2432.203721	31056.654298	58.708570
2431.172990	30835.151143	58.713575
2430.132962	30597.752762	58.718580
2429.690116	30377.889543	58.723585
2428.864021	30151.939206	58.728589
2428.321407	29919.529295	58.733594
2427.667377	29694.717683	58.738599
2426.774542	29477.431043	58.743604
2426.330730	29255.308019	58.748609
2425.512496	29029.986546	58.753613
2424.804696	28814.812226	58.758618
2424.127318	28590.417677	58.763623
2423.370516	28367.647054	58.768628
2422.681684	28152.500618	58.773633
2422.125672	27937.321762	58.778637
2421.427102	27725.068759	58.783642
2420.736389	27505.293903	58.788647
2419.825466	27290.510075	58.793652
2418.948365	27098.223033	58.798657
2418.166553	26878.414280	58.803661
2417.578481	26659.988419	58.808666
2416.554141	26459.008831	58.813671
2415.910045	26253.626799	58.818676
2415.413813	26066.021782	58.823681
2414.193353	25861.687830	58.828685
2413.505842	25671.499638	58.833690
2412.734466	25479.676402	58.838695
2411.931947	25288.187355	58.843700
2410.965659	25113.041001	58.848705
2409.815969	24935.257141	58.853709
2409.251591	24762.853656	58.858714
2408.281429	24599.234813	58.863719
2406.938427	24441.983357	58.868724
2406.135448	24279.994138	58.873729
2405.098923	24138.866961	58.878733
2404.340415	23984.489484	58.883738
2403.593627	23843.598534	58.888743
2402.754098	23701.412684	58.893748
2402.004460	23566.106033	58.898753
2401.087439	23435.766375	58.903757
2400.442602	23298.497304	58.908762
2399.724211	23173.970134	58.913767
2398.752598	23045.781481	58.918772
2398.367681	22923.292787	58.923777
2397.200622	22811.369479	58.928781
2396.691478	22690.318871	58.933786
2396.270058	22563.174465	58.938791
2395.219470	22458.479102	58.943796
2394.618004	22332.388429	58.948801
2393.948138	22217.480020	58.953805
2393.641341	22100.347454	58.958810
2392.591445	21992.139027	58.963815
2391.883244	21869.737380	58.968820
2391.520796	21775.713613	58.973825
2390.588728	21660.173378	58.978829
2389.977345	21554.766926	58.983834
2389.204167	21440.257968	58.988839
2388.769811	21334.007732	58.993844
2388.275303	21227.695111	58.998849
2387.432829	21126.993595	59.003853
2387.291507	21003.423176	59.008858
2386.318781	20887.691357	59.013863
2385.330883	20800.581879	59.018868
2385.043922	20691.538614	59.023873
2384.500574	20579.917544	59.028877
2383.762477	20470.404159	59.033882
2383.249843	20371.599352	59.038887
2382.697293	20260.190839	59.043892
2381.849662	20142.999897	59.048897
2380.978746	20034.861830	59.053901
2380.655529	19928.300315	59.058906
2380.083705	19824.875270	59.063911
2379.425199	19722.864384	59.068916
2379.108642	19595.598237	59.073921
2378.073527	19485.796599	59.078925
2377.587221	19382.743015	59.083930
2376.771843	19270.458769	59.088935
2376.158334	19147.145207	59.093940
2375.757954	19038.838373	59.098945
2374.568527	18935.522668	59.103949
2374.241006	18823.017847	59.108954
2373.489015	18712.792308	59.113959
2372.568066	18614.968416	59.118964
2372.260422	18504.836906	59.123969
2371.378939	18390.955136	59.128973
2370.755370	18290.421894	59.133978
2370.201994	18185.352579	59.138983
2369.488965	18088.584841	59.143988
2368.749029	17978.251291	59.148993
2368.038063	17885.240772	59.153997
2367.679907	17771.090323	59.159002
2366.819187	17658.901857	59.164007
2366.159534	17559.365185	59.169012
2365.674148	17447.499206	59.174017
2364.871633	17338.331801	59.179021
2364.252360	17238.836369	59.184026
2363.395052	17145.874803	59.189031
2362.788503	17048.347194	59.194036
2362.648006	16932.333991	59.199041
2361.469417	16835.271587	59.204045
2360.680990	16726.036018	59.209050
2360.079922	16625.847240	59.214055
2359.192807	16528.126661	59.219060
2358.594070	16430.663474	59.224065
2357.865861	16341.385352	59.229069
2357.265939	16240.105913	59.234074
2356.557245	16143.754555	59.239079
2355.802319	16054.381106	59.244084
2355.230630	15954.056768	59.249089
2354.368242	15876.381157	59.254093
2353.488816	15779.562993	59.259098
2353.317212	15688.220609	59.264103
2352.039904	15611.588945	59.269108
2351.583196	15515.690706	59.274113
2350.893499	15422.456544	59.279117
2350.283285	15333.076769	59.284122
2349.450019	15255.043435	59.289127
2348.694625	15162.696144	59.294132
2348.129400	15057.002507	59.299137
2347.388248	15011.783619	59.304141
2346.904879	14905.099402	59.309146
2346.173545	14816.288776	59.314151
2345.592393	14717.258298	59.319156
2344.908280	14650.586074	59.324161
2344.211141	14559.942414	59.329165
2343.664802	14470.003220	59.334170
2342.757725	14395.835404	59.339175
2342.012791	14307.061064	59.344180
2341.612460	14222.595929	59.349185
2340.766490	14149.533760	59.354189
2340.346628	14070.937206	59.359194
2339.851138	13978.915509	59.364199
2338.756142	13896.644948	59.369204
2338.231897	13816.979265	59.374209
2337.724285	13732.097046	59.379213
2336.946607	13653.640467	59.384218
2336.452089	13571.408747	59.389223
2335.674167	13495.830385	59.394228
2335.458289	13401.681404	59.399233
2333.996061	13324.505480	59.404237
2333.727091	13244.613502	59.409242
2333.105237	13164.258256	59.414247
2332.244476	13081.847358	59.419252
2331.818618	12991.774365	59.424257
2330.789816	12914.842311	59.429261
2330.452973	12837.893441	59.434266
2329.645153	12755.846407	59.439271
2328.814316	12682.455474	59.444276
2328.333623	12598.682919	59.449281
2327.441587	12533.111811	59.454285
2326.741560	12450.115825	59.459290
2326.432599	12376.518737	59.464295
2325.862433	12300.949075	59.469300
2325.118152	12219.455710	59.474305
2324.246152	12134.800863	59.479309
2323.787703	12063.557582	59.484314
2323.195786	11993.489430	59.489319
2322.547283	11909.260826	59.494324
2321.423078	11813.405486	59.499329
2321.124997	11763.306079	59.504333
2320.327104	11672.552074	59.509338
2319.867696	11595.915956	59.514343
2318.874327	11521.010470	59.519348
2318.092907	11448.400220	59.524353
2317.268633	11382.037265	59.529357
2316.791640	11302.718729	59.534362
2316.107334	11237.823918	59.539367
2315.056949	11176.301772	59.544372
2315.088099	11092.528174	59.549377
2314.171742	11033.979126	59.554381
2313.416271	10960.803348	59.559386
2313.065926	10873.796113	59.564391
2312.177838	10818.013068	59.569396
2311.903491	10748.843195	59.574401
2311.137023	10672.373286	59.579405
2310.562321	10594.418433	59.584410
2309.665710	10520.983133	59.589415
2308.584133	10461.848868	59.594420
2308.132852	10371.717968	59.599425
2307.022057	10309.426662	59.604429
2306.593257	10262.030791	59.609434
2306.053113	10179.818397	59.614439
2305.265103	10119.184440	59.619444
2304.957174	10052.851177	59.624449
2304.054000	9995.037631	59.629453
2303.405011	9903.581492	59.634458
2303.271139	9848.844187	59.639463
2302.369683	9791.566858	59.644468
2301.798988	9699.486523	59.649473
2301.130787	9635.908097	59.654477
2300.565872	9576.281184	59.659482
2299.653544	9488.683904	59.664487
2299.060115	9422.328486	59.669492
2298.522175	9357.426463	59.674497
2297.290303	9297.048072	59.679501
2297.239920	9220.701566	59.684506
2296.307201	9152.175580	59.689511
2295.775554	9090.866881	59.694516
2295.231810	9022.920405	59.699521
2294.272445	8949.218344	59.704525
2293.762140	8888.046729	59.709530
2293.132838	8823.649845	59.714535
2292.331731	8753.640597	59.719540
2291.914705	8679.743011	59.724545
2291.272945	8618.628058	59.729549
2290.065788	8550.868618	59.734554
2289.502624	8478.675550	59.739559
2288.809922	8421.731279	59.744564
2288.097741	8354.978950	59.749569
2287.622327	8289.045306	59.754573
2286.956590	8224.343598	59.759578
2286.426285	8154.194814	59.764583
2285.562702	8092.144909	59.769588
2285.196504	8031.155504	59.774593
2284.016404	7974.294975	59.779597
2283.574946	7919.979925	59.784602
2283.163670	7847.402156	59.789607
2282.361148	7779.007765	59.794612
2281.644851	7720.419237	59.799617
2281.207866	7652.475475	59.804621
2280.497676	7577.153119	59.809626
2279.553952	7516.120946	59.814631
2278.917014	7459.654279	59.819636
2278.609658	7380.697961	59.824641
2277.626341	7329.742295	59.829645
2277.106824	7257.664175	59.834650
2276.352589	7194.185518	59.839655
2275.813890	7154.300496	59.844660
2275.002927	7073.173598	59.849665
2274.272661	7010.222011	59.854669
2273.734189	6960.019007	59.859674
2273.295070	6899.093922	59.864679
2272.404024	6835.720533	59.869684
2271.740200	6765.120667	59.874689
2271.079986	6712.147822	59.879693
2270.250974	6654.044008	59.884698
2270.011066	6578.406813	59.889703
2269.005702	6521.009850	59.894708
2268.575353	6464.298076	59.899713
2267.949951	6402.293967	59.904718
2267.295185	6330.487110	59.909722
2266.696242	6272.091163	59.914727
2265.985486	6206.487247	59.919732
2265.519099	6131.373346	59.924737
2264.625581	6079.316877	59.929742
2263.751398	6020.440261	59.934746
2263.538397	5950.865207	59.939751
2262.577734	5891.344209	59.944756
2262.077463	5822.654554	59.949761
2261.085498	5763.146137	59.954766
2260.674462	5698.433180	59.959770
2259.781074	5668.695669	59.964775
2258.827997	5582.745555	59.969780
2258.425815	5523.351210	59.974785
2257.944797	5471.072926	59.979790
2257.101201	5403.366435	59.984794
2257.065875	5343.567586	59.989799
2255.887216	5281.161401	59.994804
2255.327135	5218.258277	59.999809
2254.602748	5170.284260	60.004814
2253.934125	5092.116739	60.009818
2253.439932	5034.864532	60.014823
2252.267172	4979.170604	60.019828
2251.880443	4907.003996	60.024833
2251.256813	4856.792458	60.029838
2250.563041	4808.645195	60.034842
2249.718647	4749.084343	60.039847
2249.371252	4689.722523	60.044852
2248.759487	4619.678311	60.049857
2247.883601	4561.048346	60.054862
2247.237856	4509.428182	60.059866
2246.999707	4441.808324	60.064871
2245.882735	4402.766178	60.069876
2245.509238	4324.934484	60.074881
2244.723723	4269.816706	60.079886
2243.817655	4210.157409	60.084890
2243.104420	4144.757073	60.089895
2242.381595	4092.646646	60.094900
2241.826135	4038.432539	60.099905
2241.207779	3982.175747	60.104910
2240.705591	3920.264269	60.109914
2240.122861	3861.204164	60.114919
2239.189331	3818.241727	60.119924
2238.867716	3749.191921	60.124929
2238.385296	3691.038510	60.129934
2237.560216	3627.293066	60.134938
2236.705198	3562.742725	60.139943
2236.095128	3513.310433	60.144948
2235.726322	3455.873357	60.149953
2234.424221	3384.861756	60.154958
2233.904218	3336.256445	60.159962
2233.387900	3263.350349	60.164967
2232.635998	3229.171229	60.169972
2232.019956	3158.242752	60.174977
2230.994606	3110.353968	60.179982
2230.218296	3063.259391	60.184986
2229.942896	2994.107237	60.189991
2229.356415	2946.419867	60.194996
2228.921699	2882.804223	60.200001
2227.825752	2852.068357	60.205006
2227.409425	2774.950374	60.210010
2226.637294	2726.548744	60.215015
2225.885833	2694.253949	60.220020
2225.677804	2625.988679	60.225025
2224.673837	2559.502046	60.230030
2224.019480	2506.754761	60.235034
2223.239356	2463.629249	60.240039
2222.673315	2405.609344	60.245044
2222.340839	2334.364677	60.250049
2221.220769	2271.629258	60.255054
2220.385774	2240.542602	60.260058
2220.146404	2176.105762	60.265063
2219.108014	2143.121983	60.270068
2218.840961	2085.693866	60.275073
2218.139066	2008.937492	60.280078
2217.302706	1983.067049	60.285082
2216.869565	1904.027554	60.290087
2215.772015	1873.997394	60.295092
2215.390907	1795.361853	60.300097
2214.610083	1763.982176	60.305102
2213.960744	1713.065578	60.310106
2213.656615	1643.828965	60.315111
2212.451905	1612.122593	60.320116
2212.192162	1544.890147	60.325121
2211.842399	1496.139379	60.330126
2210.560528	1426.025938	60.335130
2210.035159	1408.156350	60.340135
2209.143652	1325.549774	60.345140
2208.563135	1293.923290	60.350145
2208.113832	1238.169886	60.355150
2207.360365	1176.010275	60.360154
2206.719157	1137.159265	60.365159
2205.715573	1087.780278	60.370164
2205.105822	1030.600714	60.375169
2204.365468	991.642029	60.380174
2203.888014	951.741292	60.385178
2203.276581	897.746436	60.390183
2202.744885	853.946836	60.395188
2202.311845	800.409750	60.400193
2201.135476	755.236679	60.405198
2200.275708	706.353422	60.410202
2199.878037	659.749832	60.415207
2199.059224	608.089718	60.420212
2198.320558	564.129863	60.425217
2197.910680	522.306767	60.430222
2197.153170	480.709245	60.435226
2196.453730	429.108103	60.440231
2195.791396	394.899376	60.445236
2194.976406	346.218388	60.450241
2194.179136	311.241232	60.455246
2193.194099	262.596963	60.460250
2193.099554	213.980325	60.465255
2192.157945	180.016676	60.470260
2191.399188	137.862120	60.475265
2190.742873	120.147360	60.480270
2189.884484	79.880544	60.485274
2189.219383	32.447806	60.490279
2188.219805	6.515342	60.495284
2187.619470	-12.411290	60.500289
2186.623864	-12.534072	60.505294
2184.762183	-14.033261	60.510298
2178.765159	133.225755	60.515303
2178.921163	149.723614	60.520308
2180.549499	125.327821	60.525313
2180.962921	133.526669	60.530318
2181.377457	143.158737	60.535322
2181.476065	116.887869	60.540327
2180.673934	129.936094	60.545332
2179.915418	129.927081	60.550337
2179.125892	141.353853	60.555342
2177.923674	122.549338	60.560346
2177.608358	135.887756	60.565351
2177.319126	139.022726	60.570356
2176.620911	127.508632	60.575361
2175.771245	132.162745	60.580366
2174.508110	135.220413	60.585370
2174.166967	131.568806	60.590375
2173.670150	142.373581	60.595380
2173.537305	135.596649	60.600385
2172.965337	137.401426	60.605390
2172.293161	134.493012	60.610394
2171.557536	121.072094	60.615399
2169.935833	142.325590	60.620404
2169.496705	130.607974	60.625409
2168.381853	142.332354	60.630414
2168.073011	140.905343	60.635418
2168.024132	134.145053	60.640423
2167.374380	129.725579	60.645428
2166.917953	133.005340	60.650433
2166.227978	139.020209	60.655438
2165.024291	123.229369	60.660442
2164.492590	132.678817	60.665447
2163.438677	141.312291	60.670452
2162.834258	134.971282	60.675457
2162.956763	126.110198	60.680462
2162.027820	129.390808	60.685466
2162.016776	125.803526	60.690471
2161.007483	136.084074	60.695476
2159.601327	132.771733	60.700481
2159.425802	138.919445	60.705486
2158.637190	138.530451	60.710490
2158.080323	134.383236	60.715495
2157.457414	143.616936	60.720500
2156.801502	139.250476	60.725505
2156.226418	134.652007	60.730510
2154.914184	148.128095	60.735514
2154.598683	134.383487	60.740519
2154.056372	141.879284	60.745524
2153.854832	144.424781	60.750529
2152.707520	142.529999	60.755534
2152.380476	145.033909	60.760538
2151.926539	137.128407	60.765543
2150.644368	131.929365	60.770548
2150.400804	133.923310	60.775553
2149.866521	139.259073	60.780558
2148.491583	146.806549	60.785562
2148.966787	133.590906	60.790567
2147.586997	137.901797	60.795572
2146.501000	139.837014	60.800577
2146.976910	135.519643	60.805582
2145.376381	133.838689	60.810586
2145.014369	152.558565	60.815591
2144.273881	135.495801	60.820596
2143.754954	130.070022	60.825601
2143.447017	129.221590	60.830606
2141.724780	148.009035	60.835610
2141.358228	122.490029	60.840615
2140.925842	128.128154	60.845620
2140.824912	141.634405	60.850625
2140.350087	136.750385	60.855630
2138.836059	144.417698	60.860634
2138.661073	115.490617	60.865639
2137.723305	139.239051	60.870644
2137.025584	139.743931	60.875649
2136.313231	133.740162	60.880654
2135.734918	135.405610	60.885658
2135.222851	137.092086	60.890663
2134.811288	139.890092	60.895668
2133.732383	134.343432	60.900673
2132.531244	133.190453	60.905678
2132.514640	134.913434	60.910682
2132.391881	142.844120	60.915687
2131.157081	144.697301	60.920692
2130.137043	139.786249	60.925697
2130.024021	137.331582	60.930702
2129.458122	136.437349	60.935706
2128.405185	147.098560	60.940711
2127.462763	131.236322	60.945716
2127.183196	159.158457	60.950721
2127.052352	142.557187	60.955726
2125.823243	124.636873	60.960730
2125.291725	149.612341	60.965735
2124.537082	131.706624	60.970740
2124.054324	129.572384	60.975745
2123.154356	154.174250	60.980750
2122.253433	135.963744	60.985754
2122.427461	141.887270	60.990759
2121.386866	129.561806	60.995764
2120.518715	150.247938	61.000769
2120.048773	138.691331	61.005774
2118.689580	121.567494	61.010778
2119.185566	150.285884	61.015783
2117.829285	148.089972	61.020788
2117.592135	121.121785	61.025793
2117.104453	152.669072	61.030798
2115.885630	130.514755	61.035802
2115.792003	145.448507	61.040807
2115.152949	137.649653	61.045812
2114.279526	135.831278	61.050817
2114.107799	134.436134	61.055822
2112.842181	141.452211	61.060826
2111.664787	132.641262	61.065831
2111.031401	137.480266	61.070836
2111.148421	133.749668	61.075841
2110.095430	130.356091	61.080846
2109.059791	145.568612	61.085850
2108.991802	139.743298	61.090855
2107.978783	144.385506	61.095860
2107.426216	139.633672	61.100865
2106.887156	138.732032	61.105870
2106.104315	138.763168	61.110874
2105.802092	137.484920	61.115879
2105.106257	142.846324	61.120884
2104.666175	130.387741	61.125889
2104.301126	122.688920	61.130894
2103.217235	130.656986	61.135898
2102.100186	140.875805	61.140903
2101.193165	138.964997	61.145908
2100.593523	134.512360	61.150913
2100.589857	133.469004	61.155918
2099.320146	143.127024	61.160922
2099.012438	133.971516	61.165927
2098.126447	147.603909	61.170932
2097.624021	141.741876	61.175937
2097.317521	133.880802	61.180942
2096.488757	133.130784	61.185946
2096.392929	133.339908	61.190951
2095.439186	148.042720	61.195956
2094.351826	144.536333	61.200961
2093.497355	132.895678	61.205966
2092.712865	136.784145	61.210970
2092.072691	132.708511	61.215975
2091.677480	133.359360	61.220980
2091.112241	131.695511	61.225985
2090.539327	133.560376	61.230990
2090.000235	135.296877	61.235994
2089.708420	126.403772	61.240999
2088.957970	136.092934	61.246004
2088.024032	138.316270	61.251009
2086.899224	126.809978	61.256014
2086.014181	142.235137	61.261018
2085.541970	133.044237	61.266023
2085.279582	120.093869	61.271028
2084.467742	128.089732	61.276033
2083.929075	140.437039	61.281038
2083.243279	137.604924	61.286042
2082.960420	127.005783	61.291047
2082.442131	139.026594	61.296052
2081.202713	131.078600	61.301057
2080.217416	125.179661	61.306062
2079.376936	134.853149	61.311066
2079.098482	125.070140	61.316071
2078.759087	125.972320	61.321076
2077.571483	132.435157	61.326081
2077.237079	133.260855	61.331086
2076.780423	140.435577	61.336090
2076.241551	130.074170	61.341095
2075.790176	128.630368	61.346100
2075.114829	128.100430	61.351105
2074.254855	126.220013	61.356110
2073.260591	132.734171	61.361114
2073.013719	128.096262	61.366119
2072.245401	124.477766	61.371124
2071.449309	125.553336	61.376129
2070.316761	125.349827	61.381134
2069.539814	135.451610	61.386138
2069.386421	120.071314	61.391143
2068.499134	132.825579	61.396148
2067.547233	130.682220	61.401153
2067.103466	125.853214	61.406158
2066.340609	132.707530	61.411162
2066.488591	128.752833	61.416167
2065.806783	132.470477	61.421172
2065.189595	124.912594	61.426177
2064.748316	126.297701	61.431182
2063.310198	126.104838	61.436186
2062.539926	113.686062	61.441191
2061.683884	128.397011	61.446196
2061.329589	125.763027	61.451201
2060.762183	121.954965	61.456206
2060.355068	133.294262	61.461210
2059.987372	127.912315	61.466215
2059.619430	117.293573	61.471220
2057.981714	123.580268	61.476225
2057.395189	123.832568	61.481230
2056.810085	130.038962	61.486234
2056.346295	129.424998	61.491239
2055.751253	134.491306	61.496244
2055.157773	140.933990	61.501249
2054.265588	131.328793	61.506254
2053.189811	138.790988	61.511258
2052.795367	139.687715	61.516263
2052.205699	136.010913	61.521268
2051.532039	144.935728	61.526273
2051.288305	128.122181	61.531278
2050.491052	142.973621	61.536282
2049.798057	123.251056	61.541287
2048.698561	138.659788	61.546292
2047.808332	139.862263	61.551297
2047.368010	130.530703	61.556302
2046.524370	132.195696	61.561306
2046.425214	131.888131	61.566311
2045.809598	129.554226	61.571316
2045.292974	137.384989	61.576321
2045.062443	133.610199	61.581326
2043.758003	136.810092	61.586330
2042.730146	128.491094	61.591335
2042.128263	142.138329	61.596340
2041.408697	129.711502	61.601345
2041.191952	135.591376	61.606350
2040.498040	135.398693	61.611354
2040.133431	130.401018	61.616359
2038.945343	129.357971	61.621364
2038.052100	126.495717	61.626369
2037.783048	133.747896	61.631374
2037.075488	140.550870	61.636378
2036.708488	122.364504	61.641383
2036.261692	121.025634	61.646388
2034.908527	137.731401	61.651393
2034.226076	128.320004	61.656398
2033.588208	129.873502	61.661402
2033.038085	125.592793	61.666407
2032.886233	134.109957	61.671412
2031.889126	135.397204	61.676417
2031.722743	124.809554	61.681422
2030.532267	126.867046	61.686426
2029.655289	126.856376	61.691431
2028.981372	128.852393	61.696436
2028.401167	125.317595	61.701441
2028.064393	127.414644	61.706446
2027.442283	136.287123	61.711450
2026.390023	122.129648	61.716455
2025.562231	140.467698	61.721460
2024.905882	134.567037	61.726465
2024.523319	128.796388	61.731470
2023.507238	134.620194	61.736474
2023.239397	132.601672	61.741479
2022.832109	126.916946	61.746484
2022.330606	134.390510	61.751489
2021.479328	132.276929	61.756494
2020.219500	127.396099	61.761498
2019.314895	123.236301	61.766503
2018.996811	132.560404	61.771508
2018.554676	149.164186	61.776513
2018.333682	129.759365	61.781518
2017.695902	126.925959	61.786522
2017.226375	135.197085	61.791527
2016.280458	133.850699	61.796532
2015.163638	136.643953	61.801537
2014.657138	128.056157	61.806542
2014.169706	139.796121	61.811546
2013.265563	140.601863	61.816551
2012.022857	131.071235	61.821556
2011.585903	135.495900	61.826561
2011.072166	134.776335	61.831566
2010.340779	131.155151	61.836570
2010.168503	127.043130	61.841575
2009.362446	131.280377	61.846580
2009.223587	135.099516	61.851585
2008.658162	125.491369	61.856590
2007.505227	120.797002	61.861594
2006.573286	138.866164	61.866599
2006.431071	124.725113	61.871604
2005.794521	135.681374	61.876609
2004.802436	130.890517	61.881614
2003.608251	134.547572	61.886618
2003.056747	128.799008	61.891623
2002.590860	117.298579	61.896628
2002.023300	144.604074	61.901633
2001.919569	126.357010	61.906638
2001.400833	136.379982	61.911642
2000.440242	139.982621	61.916647
1999.493968	133.117198	61.921652
1998.701808	128.848102	61.926657
1998.637124	132.425243	61.931662
1997.035522	133.639713	61.936666
1996.666370	127.595717	61.941671
1995.751999	129.115840	61.946676
1995.216266	131.909915	61.951681
1994.706260	134.348262	61.956686
1993.997534	138.254691	61.961690
1993.741190	125.131501	61.966695
1993.369342	125.677735	61.971700
1992.507536	131.678907	61.976705
1991.783741	124.174235	61.981710
1990.870842	130.363281	61.986714
1990.525567	133.639617	61.991719
1990.268104	135.924348	61.996724
1988.814988	117.235475	62.001729
1988.212902	137.757955	62.006734
1987.470270	110.242465	62.011738
1986.921718	126.276509	62.016743
1986.481448	137.088087	62.021748
1985.662343	132.020636	62.026753
1984.962365	128.970038	62.031758
1984.102236	136.867941	62.036762
1983.755912	128.054468	62.041767
1983.334067	125.289297	62.046772
1982.535873	128.430945	62.051777
1981.454274	118.745469	62.056782
1980.364098	130.789239	62.061786
1980.093013	133.186514	62.066791
1979.657112	129.311871	62.071796
1978.970273	126.953020	62.076801
1978.786914	121.628562	62.081806
1978.205108	132.041572	62.086810
1977.165314	126.334246	62.091815
1976.488512	121.242640	62.096820
1975.909716	129.598914	62.101825
1975.313387	123.419101	62.106830
1973.821346	125.324216	62.111834
1973.588310	117.424709	62.116839
1972.927169	127.867654	62.121844
1971.806734	129.179227	62.126849
1971.617823	129.168173	62.131854
1970.889236	124.726579	62.136858
1970.581589	124.002696	62.141863
1970.203015	121.129741	62.146868
1969.561413	130.019510	62.151873
1968.625984	128.830743	62.156878
1967.923389	126.758234	62.161882
1967.304257	119.678490	62.166887
1966.876732	124.347653	62.171892
1965.499989	144.136847	62.176897
1965.244823	123.080168	62.181902
1964.432444	134.165261	62.186906
1963.696899	127.865626	62.191911
1963.622519	126.850842	62.196916
1962.910432	129.232962	62.201921
1961.949276	119.137312	62.206926
1961.010470	131.239060	62.211930
1960.561320	128.844064	62.216935
1960.088912	125.569705	62.221940
1959.092162	131.444077	62.226945
1958.822643	119.698035	62.231950
1957.752645	124.470751	62.236954
1957.160050	120.843326	62.241959
1956.879665	124.943535	62.246964
1955.868919	125.903405	62.251969
1955.566795	123.087700	62.256974
1954.410978	121.546006	62.261978
1953.694060	121.353844	62.266983
1953.456610	119.570195	62.271988
1952.767136	126.378193	62.276993
1952.306774	116.723433	62.281998
1951.135459	128.116219	62.287002
1950.198439	122.673280	62.292007
1950.027074	115.424704	62.297012
1949.325410	125.781047	62.302017
1949.164581	111.288176	62.307022
1947.505982	123.109949	62.312026
1946.686731	124.209731	62.317031
1946.416370	124.984280	62.322036
1945.920625	117.910188	62.327041
1945.429681	115.395681	62.332046
1944.818911	126.931297	62.337050
1944.614101	118.059109	62.342055
1944.091865	122.487852	62.347060
1942.322081	123.525631	62.352065
1941.900619	124.724693	62.357070
1941.532424	124.300571	62.362074
1941.117478	119.366101	62.367079
1940.042058	117.611388	62.372084
1939.368165	120.834236	62.377089
1938.911747	124.574475	62.382094
1938.521732	124.842915	62.387098
1937.755108	119.136403	62.392103
1936.558219	124.626250	62.397108
1935.786955	123.476090	62.402113
1935.743403	115.002490	62.407118
1934.813930	125.051234	62.412122
1934.086367	124.949072	62.417127
1933.119386	120.862286	62.422132
1932.023187	116.438059	62.427137
1932.639131	114.930519	62.432142
1931.756052	121.340337	62.437146
1930.754589	129.675403	62.442151
1930.747045	122.061793	62.447156
1929.436495	122.402239	62.452161
1928.727039	121.679067	62.457166
1927.811186	124.237036	62.462170
1927.645218	121.306687	62.467175
1927.374444	114.666802	62.472180
1926.341540	120.876487	62.477185
1925.217161	120.001568	62.482190
1924.439394	126.929238	62.487194
1923.944637	125.325201	62.492199
1923.255927	123.717259	62.497204
1922.987796	128.028405	62.502209
1922.815071	124.760099	62.507214
1921.909605	130.315653	62.512218
1920.787033	127.379462	62.517223
1920.172639	122.150240	62.522228
1919.318850	132.237439	62.527233
1919.289607	123.882984	62.532238
1918.767648	128.032581	62.537242
1917.521702	120.930930	62.542247
1917.124172	123.335665	62.547252
1916.222578	124.946821	62.552257
1915.934395	124.795418	62.557262
1915.006026	133.990904	62.562266
1913.925093	133.416585	62.567271
1913.339193	123.037470	62.572276
1912.536332	128.862155	62.577281
1912.359948	118.705031	62.582286
1911.653674	139.438008	62.587290
1911.429113	121.345765	62.592295
1910.868453	116.940612	62.597300
1909.716842	125.763119	62.602305
1909.571697	119.951655	62.607310
1908.725223	125.899952	62.612314
1907.871074	117.337419	62.617319
1906.919345	124.029367	62.622324
1905.960256	131.301202	62.627329
1905.628072	125.013249	62.632334
1905.320938	125.593375	62.637338
1904.542900	118.778561	62.642343
1903.906559	123.875100	62.647348
1902.921521	130.652760	62.652353
1902.725960	126.538141	62.657358
1902.110506	124.278362	62.662362
1901.043586	130.012509	62.667367
1900.403999	116.396701	62.672372
1899.516963	121.011088	62.677377
1899.074939	121.809738	62.682382
1898.517145	118.738175	62.687386
1898.259806	112.370541	62.692391
1897.369816	118.991190	62.697396
1896.302633	121.443887	62.702401
1896.091954	114.103794	62.707406
1895.416356	123.336419	62.712410
1894.578548	118.771847	62.717415
1893.461104	115.240373	62.722420
1892.725972	127.549486	62.727425
1892.456321	122.423234	62.732430
1891.941129	119.579864	62.737434
1891.268391	127.621493	62.742439
1891.129807	128.083405	62.747444
1889.957210	124.127043	62.752449
1889.349857	116.523506	62.757454
1888.954215	119.300088	62.762458
1887.899875	125.418577	62.767463
1886.722029	118.250942	62.772468
1886.160371	119.863335	62.777473
1885.582395	111.346854	62.782478
1885.282244	110.749520	62.787482
1884.873633	125.723765	62.792487
1884.636697	113.999379	62.797492
1883.799605	125.875267	62.802497
1882.775556	116.655349	62.807502
1882.046297	116.413129	62.812506
1881.239730	118.785036	62.817511
1880.794084	123.289936	62.822516
1879.768169	125.021761	62.827521
1878.843028	128.437468	62.832526
1878.579286	125.601488	62.837530
1878.118150	115.622035	62.842535
1877.885673	112.098306	62.847540
1876.534568	129.811415	62.852545
1876.191955	112.666718	62.857550
1875.396846	116.399233	62.862554
1874.905068	119.875445	62.867559
1874.482431	125.024792	62.872564
1873.153629	123.931625	62.877569
1872.815786	105.797475	62.882574
1871.961261	126.763696	62.887578
1871.779608	122.802984	62.892583
1871.169855	125.801210	62.897588
1870.024550	121.820026	62.902593
1869.457604	131.544744	62.907598
1869.214396	121.896529	62.912602
1868.201128	132.600387	62.917607
1867.021030	123.491975	62.922612
1866.235316	136.094545	62.927617
1866.091770	119.839140	62.932622
1865.576801	133.608194	62.937626
1865.125586	125.464231	62.942631
1864.656442	121.460856	62.947636
1863.121154	129.038634	62.952641
1862.666533	129.178577	62.957646
1862.278454	119.362561	62.962650
1861.630396	124.451507	62.967655
1861.603156	119.928566	62.972660
1860.240658	117.796860	62.977665
1859.625864	121.041881	62.982670
1858.927090	122.087870	62.987674
1857.963630	118.423160	62.992679
1857.143162	112.813533	62.997684
1856.211124	120.678720	63.002689
1856.268327	125.122714	63.007694
1855.690857	118.514186	63.012698
1855.258482	131.037004	63.017703
1855.114991	125.296242	63.022708
1853.530390	125.601391	63.027713
1852.935504	121.127571	63.032718
1852.488940	121.556383	63.037722
1851.809859	124.556157	63.042727
1850.823712	116.755739	63.047732
1849.887299	121.355903	63.052737
1849.814931	114.894258	63.057742
1849.336541	121.865871	63.062746
1848.302340	125.295747	63.067751
1847.264995	127.278546	63.072756
1846.766366	125.725599	63.077761
1846.339972	123.626622	63.082766
1846.034820	131.354445	63.087770
1845.426317	133.871530	63.092775
1844.636169	124.746949	63.097780
1843.635393	122.387519	63.102785
1843.299456	120.766168	63.107790
1842.692905	129.677197	63.112794
1841.400135	126.088429	63.117799
1840.505132	124.663066	63.122804
1839.789958	125.811008	63.127809
1839.424760	123.114139	63.132814
1839.538194	130.707699	63.137818
1839.109839	119.789536	63.142823
1837.972451	130.962518	63.147828
1836.779091	139.842147	63.152833
1836.511801	123.212170	63.157838
1836.106830	119.190730	63.162842
1835.322422	121.981736	63.167847
1834.350776	120.385626	63.172852
1833.402388	127.739356	63.177857
1833.537959	115.473312	63.182862
1833.108580	130.400398	63.187866
1831.768371	124.157390	63.192871
1831.009481	119.432085	63.197876
1830.336722	117.984056	63.202881
1830.248465	118.813278	63.207886
1829.399399	108.247337	63.212890
1828.315164	121.132252	63.217895
1827.866456	121.193994	63.222900
1827.175270	115.958071	63.227905
1826.815257	114.786803	63.232910
1825.671362	118.546324	63.237914
1824.582444	123.637467	63.242919
1824.469678	117.432962	63.247924
1823.974477	118.896049	63.252929
1823.613554	116.004549	63.257934
1822.872508	119.151356	63.262938
1821.456171	129.476117	63.267943
1821.127182	123.006333	63.272948
1820.527850	131.075742	63.277953
1820.220270	121.412527	63.282958
1819.733674	119.192233	63.287962
1818.725841	122.816619	63.292967
1818.440435	113.780642	63.297972
1817.474872	123.051433	63.302977
1816.481279	120.055391	63.307982
1815.289572	119.861385	63.312986
1814.860550	117.531030	63.317991
1814.403901	117.247122	63.322996
1813.903693	121.372780	63.328001
1814.067354	129.354158	63.333006
1812.924932	121.706295	63.338010
1812.308465	119.706886	63.343015
1811.712765	109.887587	63.348020
1810.905381	126.544603	63.353025
1809.761451	116.864383	63.358030
1808.884140	120.042291	63.363034
1808.218568	126.529568	63.368039
1808.032231	118.592714	63.373044
1807.768323	126.164184	63.378049
1807.111424	125.115748	63.383054
1806.355108	116.069390	63.388058
1805.428618	122.252757	63.393063
1805.211471	122.433847	63.398068
1803.765219	121.119679	63.403073
1802.973885	116.636068	63.408078
1802.569933	110.592914	63.413082
1801.929396	120.871764	63.418087
1801.759689	116.366718	63.423092
1801.293705	122.825457	63.428097
1800.343830	111.614821	63.433102
1799.469519	119.045099	63.438106
1798.984781	129.669784	63.443111
1798.525369	117.474561	63.448116
1797.277075	116.781792	63.453121
1796.590506	120.328368	63.458126
1795.961063	108.861862	63.463130
1795.545588	115.955946	63.468135
1795.264509	108.521400	63.473140
1793.933290	118.438430	63.478145
1793.075457	115.267885	63.483150
1792.984947	117.679076	63.488154
1792.232422	115.445822	63.493159
1792.030946	118.038628	63.498164
1790.953491	111.750774	63.503169
1790.202067	119.683490	63.508174
1789.727376	116.377995	63.513178
1788.839316	113.638009	63.518183
1788.535269	114.277579	63.523188
1787.221558	118.910864	63.528193
1786.973286	114.044575	63.533198
1786.508182	131.061969	63.538202
1785.790191	122.583515	63.543207
1784.628928	119.571534	63.548212
1783.908003	131.104162	63.553217
1783.519198	120.854638	63.558222
1783.525215	118.838392	63.563226
1782.328231	123.949864	63.568231
1781.446032	127.948535	63.573236
1780.698559	126.239583	63.578241
1780.329444	116.647649	63.583246
1779.935298	125.078700	63.588250
1779.251075	116.490815	63.593255
1778.507630	123.624367	63.598260
1777.526306	123.600389	63.603265
1777.274398	114.939128	63.608270
1776.481152	121.664291	63.613274
1775.144000	120.933606	63.618279
1775.002700	116.974384	63.623284
1774.329058	125.355203	63.628289
1773.885861	123.545900	63.633294
1773.417002	115.218697	63.638298
1772.488530	128.462081	63.643303
1771.767616	115.814828	63.648308
1771.182885	117.624862	63.653313
1770.439398	118.665359	63.658318
1769.439813	115.919436	63.663322
1768.540583	128.431236	63.668327
1768.534443	124.310207	63.673332
1768.151137	130.670673	63.678337
1767.721680	120.511184	63.683342
1766.799592	114.808922	63.688346
1765.679514	117.421447	63.693351
1765.417417	116.146334	63.698356
1764.293944	127.030135	63.703361
1763.530859	123.614329	63.708366
1762.953794	117.592363	63.713370
1762.332814	123.383470	63.718375
1762.011916	127.253593	63.723380
1761.496662	129.579276	63.728385
1760.518737	123.341856	63.733390
1760.003384	130.179009	63.738394
1759.308649	133.312173	63.743399
1758.788565	120.582570	63.748404
1757.737115	126.273310	63.753409
1756.902206	119.798726	63.758414
1756.608766	128.103406	63.763418
1755.994932	139.278433	63.768423
1755.678838	125.319580	63.773428
1754.176082	125.812055	63.778433
1753.313746	126.100336	63.783438
1753.268141	116.479113	63.788442
1752.446969	122.809766	63.793447
1752.523120	110.915851	63.798452
1751.440982	119.022511	63.803457
1750.364575	120.324028	63.808462
1749.849651	117.239387	63.813466
1749.213582	123.592684	63.818471
1749.129685	117.270067	63.823476
1747.651713	125.710813	63.828481
1747.137163	118.343307	63.833486
1746.440064	114.584309	63.838490
1746.114937	129.269343	63.843495
1745.891111	117.322140	63.848500
1744.899468	120.218617	63.853505
1744.063329	115.100352	63.858510
1743.945144	108.500923	63.863514
1742.171945	124.092392	63.868519
1741.882992	105.124237	63.873524
1740.783981	116.533984	63.878529
1740.525095	114.816838	63.883534
1740.513001	102.929060	63.888538
1739.697180	125.516482	63.893543
1738.723122	111.783555	63.898548
1738.009581	115.588303	63.903553
1737.419578	106.321611	63.908558
1737.352337	110.216102	63.913562
1736.118849	114.645867	63.918567
1735.411407	114.825980	63.923572
1734.444383	109.755314	63.928577
1734.171750	116.449844	63.933582
1733.054314	114.206754	63.938586
1732.269954	117.169659	63.943591
1731.806141	113.843527	63.948596
1731.238491	116.759403	63.953601
1730.711023	116.620791	63.958606
1730.534353	107.875059	63.963610
1730.029757	120.339957	63.968615
1729.334927	113.892025	63.973620
1728.494743	114.421212	63.978625
1727.626098	116.424569	63.983630
1726.834091	112.986564	63.988634
1726.105900	117.940032	63.993639
1725.660666	115.717920	63.998644
1724.937957	119.213483	64.003649
1723.936277	117.644263	64.008654
1723.490714	114.064511	64.013658
1722.557992	114.345057	64.018663
1722.233292	102.973683	64.023668
1722.061397	111.878764	64.028673
1721.000579	108.551257	64.033678
1720.427655	107.711848	64.038682
1719.782689	114.689426	64.043687
1719.075666	108.142516	64.048692
1717.827292	111.743638	64.053697
1717.380346	114.019056	64.058702
1716.769380	98.101281	64.063706
1716.200059	113.586711	64.068711
1715.995879	110.493727	64.073716
1715.137339	104.762476	64.078721
1714.153338	105.732379	64.083726
1713.590863	107.753345	64.088730
1713.138521	103.925528	64.093735
1712.237721	115.004196	64.098740
1711.261496	106.710286	64.103745
1710.752956	109.711389	64.108750
1710.638482	111.210219	64.113754
1710.040219	107.173775	64.118759
1709.004358	108.443639	64.123764
1708.328259	105.479220	64.128769
1707.602852	116.925831	64.133774
1707.077314	105.915922	64.138778
1706.618914	110.678319	64.143783
1706.025994	101.058884	64.148788
1704.945313	106.252829	64.153793
1704.458443	109.403449	64.158798
1703.869799	105.751814	64.163802
1702.440445	111.491547	64.168807
1702.182585	107.705380	64.173812
1701.548800	114.652801	64.178817
1701.037266	109.189703	64.183822
1701.194587	111.652991	64.188826
1699.769174	115.190780	64.193831
1699.349799	110.589788	64.198836
1698.764906	113.721286	64.203841
1697.569770	116.497139	64.208846
1697.005256	113.626958	64.213850
1696.169943	113.906234	64.218855
1695.902070	107.902992	64.223860
1695.422684	106.599323	64.228865
1694.501339	104.219457	64.233870
1693.732079	98.923447	64.238874
1692.810727	116.464271	64.243879
1692.412549	96.561056	64.248884
1691.967166	102.183936	64.253889
1691.270110	113.692273	64.258894
1690.653406	104.778329	64.263898
1689.751319	122.372868	64.268903
1689.624940	112.099042	64.273908
1688.675221	109.879795	64.278913
1687.505037	111.030659	64.283918
1687.426574	100.263553	64.288922
1685.989690	114.555893	64.293927
1686.178532	106.527940	64.298932
1685.468319	115.017074	64.303937
1684.173307	113.280003	64.308942
1683.962349	103.744981	64.313946
1683.215213	117.847354	64.318951
1683.023849	107.839308	64.323956
1681.971686	114.842143	64.328961
1680.777034	108.399502	64.333966
1680.541406	99.579573	64.338970
1680.202264	113.347496	64.343975
1679.922181	105.381407	64.348980
1678.512152	100.231326	64.353985
1677.949421	107.828174	64.358990
1677.815353	119.165102	64.363994
1676.599612	108.681120	64.368999
1675.643984	100.010240	64.374004
1675.186381	105.583026	64.379009
1674.703192	108.283655	64.384014
1674.453400	106.024205	64.389018
1673.419889	112.208835	64.394023
1673.081024	98.857591	64.399028
1672.583545	113.897973	64.404033
1671.093094	115.112327	64.409038
1670.433010	105.560336	64.414042
1669.678980	112.192562	64.419047
1669.679548	101.023417	64.424052
1669.279362	106.017833	64.429057
1668.069979	122.680367	64.434062
1667.567961	106.713761	64.439066
1666.579990	104.880626	64.444071
1666.374342	117.171893	64.449076
1665.099578	109.881008	64.454081
1664.464659	111.341084	64.459086
1664.237473	102.201286	64.464090
1663.521571	107.668452	64.469095
1663.226146	109.325328	64.474100
1662.020684	110.182200	64.479105
1661.399680	99.278933	64.484110
1661.130970	105.211207	64.489114
1659.833753	112.749688	64.494119
1658.900339	106.016419	64.499124
1658.403127	112.647278	64.504129
1657.983318	115.106043	64.509134
1657.464638	110.147114	64.514138
1657.035750	123.880418	64.519143
1656.355315	111.086446	64.524148
1655.314945	117.300557	64.529153
1654.714161	124.898730	64.534158
1654.233656	124.260688	64.539162
1653.816308	124.252827	64.544167
1653.172517	107.537651	64.549172
1652.136287	118.700922	64.554177
1651.806188	121.974877	64.559182
1651.535697	113.854308	64.564186
1649.927838	123.654499	64.569191
1649.137289	109.351604	64.574196
1648.611074	120.208373	64.579201
1648.093093	133.506428	64.584206
1648.146900	120.591094	64.589210
1647.147106	120.100189	64.594215
1646.532762	111.014001	64.599220
1645.702130	125.159609	64.604225
1645.103577	113.284568	64.609230
1644.224095	109.494651	64.614234
1643.288709	123.928121	64.619239
1642.945330	124.362653	64.624244
1642.563984	122.053141	64.629249
1641.474911	119.570631	64.634254
1640.779204	121.953381	64.639258
1639.622020	130.729561	64.644263
1639.362907	117.833975	64.649268
1639.150726	94.722255	64.654273
1638.484373	124.724060	64.659278
1638.372447	112.508387	64.664282
1637.408105	118.678890	64.669287
1636.731553	115.060157	64.674292
1635.557759	118.606894	64.679297
1634.520457	117.298822	64.684302
1634.200657	112.486494	64.689306
1633.485256	117.423760	64.694311
1633.250804	116.886980	64.699316
1632.807654	115.060351	64.704321
1631.680287	119.143737	64.709326
1631.575573	117.756912	64.714330
1630.602964	127.203908	64.719335
1630.144534	111.883214	64.724340
1628.843003	113.961672	64.729345
1628.120245	120.768707	64.734350
1627.920960	100.512235	64.739354
1627.300646	125.451267	64.744359
1626.482688	110.624481	64.749364
1625.798802	133.107390	64.754369
1625.409180	118.556316	64.759374
1624.913796	108.304850	64.764378
1623.591151	125.674486	64.769383
1622.766513	124.728433	64.774388
1622.621506	114.817103	64.779393
1622.051129	102.027747	64.784398
1621.220751	104.822956	64.789402
1620.289269	116.056323	64.794407
1619.701138	116.512391	64.799412
1619.632245	121.127777	64.804417
1618.640005	111.984937	64.809422
1617.740971	104.522439	64.814426
1617.037818	114.016509	64.819431
1616.739980	118.234622	64.824436
1616.149862	106.192685	64.829441
1614.731829	123.462362	64.834446
1614.490450	119.799737	64.839450
1613.908112	110.274835	64.844455
1613.693662	109.301239	64.849460
1612.729191	118.407913	64.854465
1611.709093	117.380955	64.859470
1611.534123	113.747204	64.864474
1610.730736	137.865403	64.869479
1610.091498	120.769479	64.874484
1609.349460	117.173771	64.879489
1608.320897	102.918172	64.884494
1608.359236	112.177764	64.889498
1607.579426	116.130258	64.894503
1606.164611	117.471399	64.899508
1605.699789	115.684486	64.904513
1604.963160	126.294005	64.909518
1605.133070	102.063502	64.914522
1604.154136	125.719159	64.919527
1603.270371	112.656324	64.924532
1602.492549	111.154089	64.929537
1601.821491	110.025959	64.934542
1601.842400	120.223412	64.939546
1600.825619	121.122875	64.944551
1600.043346	105.885180	64.949556
1599.134332	114.968854	64.954561
1598.814149	132.601860	64.959566
1598.424495	98.957991	64.964570
1597.207623	115.459308	64.969575
1596.594497	100.513279	64.974580
1596.293345	122.862836	64.979585
1595.607278	120.295826	64.984590
1594.626733	98.662290	64.989594
1593.670053	111.690992	64.994599
1593.182846	99.782524	64.999604
1593.196161	112.165148	65.004609
1592.177953	122.776822	65.009614
1591.581374	109.502801	65.014618
1590.777761	114.876691	65.019623
1590.495106	113.565442	65.024628
1589.659775	111.725434	65.029633
1588.431524	109.556782	65.034638
1587.691065	112.440214	65.039642
1587.285746	111.897469	65.044647
1587.017544	107.955274	65.049652
1586.683030	118.149266	65.054657
1585.629378	106.756538	65.059662
1585.125923	104.603625	65.064666
1584.423146	118.741541	65.069671
1583.603958	117.340495	65.074676
1582.739283	110.334576	65.079681
1582.263840	120.412193	65.084686
1581.920815	119.916319	65.089690
1580.723612	116.769804	65.094695
1580.166285	114.902980	65.099700
1579.716420	112.944970	65.104705
1579.326981	114.462257	65.109710
1578.153935	105.802305	65.114714
1577.103436	117.680610	65.119719
1576.889847	94.991737	65.124724
1576.421469	104.331821	65.129729
1575.666652	114.158941	65.134734
1575.075141	99.524863	65.139738
1574.077300	106.802938	65.144743
1573.978281	103.683804	65.149748
1573.599313	103.023339	65.154753
1572.023611	111.407151	65.159758
1571.484788	103.292965	65.164762
1570.737929	112.283078	65.169767
1570.336594	107.641404	65.174772
1570.010196	106.218842	65.179777
1568.769322	115.363131	65.184782
1568.180654	104.539908	65.189786
1567.514044	112.448151	65.194791
1567.332311	109.830988	65.199796
1566.306827	119.328973	65.204801
1565.650765	118.099126	65.209806
1565.176513	107.828554	65.214810
1564.341344	117.770941	65.219815
1563.672340	106.354961	65.224820
1563.072628	110.434963	65.229825
1562.399955	113.903692	65.234830
1561.919341	106.456739	65.239834
1561.093683	110.091691	65.244839
1560.127844	109.396740	65.249844
1559.675845	105.180989	65.254849
1559.288545	109.752344	65.259854
1558.990770	106.608020	65.264858
1557.705969	114.767438	65.269863
1557.001716	117.686125	65.274868
1556.203256	115.551702	65.279873
1555.996143	112.910189	65.284878
1555.625615	99.535624	65.289882
1553.964560	116.456013	65.294887
1553.358434	106.720458	65.299892
1552.841204	108.226512	65.304897
1552.267563	115.101328	65.309902
1552.138958	120.817397	65.314906
1551.258952	113.116946	65.319911
1550.636166	112.496798	65.324916
1550.010627	99.905459	65.329921
1549.353898	121.537255	65.334926
1548.244351	110.192847	65.339930
1547.141706	115.104927	65.344935
1547.056567	110.854546	65.349940
1546.968715	109.474508	65.354945
1545.941851	114.456546	65.359950
1546.000261	107.556284	65.364954
1544.879696	110.462273	65.369959
1544.004805	111.848545	65.374964
1543.141862	111.283901	65.379969
1541.959018	112.963516	65.384974
1541.617516	112.793820	65.389978
1540.797734	113.914306	65.394983
1540.576567	108.386193	65.399988
1540.321245	110.522387	65.404993
1539.676775	104.954302	65.409998
1539.170143	102.276806	65.415002
1538.004573	108.879832	65.420007
1537.476042	121.386390	65.425012
1536.625923	104.555823	65.430017
1535.716710	108.971995	65.435022
1535.658832	118.688395	65.440026
1534.588622	122.415826	65.445031
1533.777752	114.442635	65.450036
1533.218373	112.864716	65.455041
1532.704988	122.317616	65.460046
1532.765524	105.359709	65.465050
1531.365026	114.712290	65.470055
1530.505272	114.401020	65.475060
1530.299160	112.164607	65.480065
1529.300004	115.705716	65.485070
1528.920368	109.412768	65.490074
1527.829126	107.832628	65.495079
1527.113306	101.186265	65.500084
1526.977792	101.881083	65.505089
1526.094561	124.764642	65.510094
1525.320242	109.292338	65.515098
1524.449651	101.864784	65.520103
1523.909385	104.289090	65.525108
1523.494533	122.195727	65.530113
1523.024823	115.816169	65.535118
1522.090804	108.283579	65.540122
1521.208103	125.443003	65.545127
1521.046498	121.600566	65.550132
1520.635868	115.738298	65.555137
1519.333143	125.512150	65.560142
1518.717845	116.866102	65.565146
1518.131238	113.176346	65.570151
1517.915150	114.907359	65.575156
1516.825902	101.744767	65.580161
1515.782199	115.812285	65.585166
1515.367382	119.422972	65.590170
1515.103728	118.111867	65.595175
1514.385429	118.424645	65.600180
1513.574583	109.973668	65.605185
1512.827458	115.485252	65.610190
1512.541052	111.405618	65.615194
1511.621078	126.155195	65.620199
1510.607520	115.093582	65.625204
1510.008540	122.133275	65.630209
1509.714966	119.611153	65.635214
1509.053257	103.751981	65.640218
1508.129218	111.037273	65.645223
1507.618693	118.777234	65.650228
1507.186899	105.934358	65.655233
1506.300275	103.727234	65.660238
1505.231476	105.035524	65.665242
1504.219882	117.141043	65.670247
1504.288757	109.258304	65.675252
1503.921369	106.238585	65.680257
1503.044832	108.643791	65.685262
1502.525766	125.628750	65.690266
1501.778219	118.211607	65.695271
1500.827729	96.122372	65.700276
1500.591066	120.377565	65.705281
1499.538141	117.564539	65.710286
1498.835224	105.865405	65.715290
1498.120176	111.931684	65.720295
1497.695250	113.557116	65.725300
1497.306858	108.867671	65.730305
1496.056202	116.427207	65.735310
1495.462340	107.735190	65.740314
1495.055774	101.418148	65.745319
1494.549785	106.082481	65.750324
1494.108891	112.054738	65.755329
1492.955514	111.924172	65.760334
1492.688471	105.260123	65.765338
1491.825430	110.290260	65.770343
1491.272488	113.490833	65.775348
1490.283554	105.691031	65.780353
1489.553190	112.683794	65.785358
1489.232926	110.943317	65.790362
1488.643903	108.619527	65.795367
1487.588607	102.708330	65.800372
1487.265956	94.660744	65.805377
1486.435813	128.722212	65.810382
1486.150264	102.944654	65.815386
1484.991562	97.327421	65.820391
1484.300338	104.023817	65.825396
1483.975138	101.090433	65.830401
1483.227546	116.858082	65.835406
1482.530168	106.203542	65.840410
1481.431818	107.872910	65.845415
1480.953600	108.395118	65.850420
1480.511390	122.012274	65.855425
1480.041704	103.404069	65.860430
1479.063748	90.263246	65.865434
1478.349438	120.190653	65.870439
1477.689066	96.948364	65.875444
1477.516561	109.076659	65.880449
1476.528509	90.779489	65.885454
1475.892389	114.591969	65.890458
1475.549472	116.809893	65.895463
1474.673924	101.229134	65.900468
1474.051271	104.648933	65.905473
1472.801280	116.478545	65.910478
1472.390732	106.366603	65.915482
1471.852854	108.579239	65.920487
1471.479877	117.260815	65.925492
1470.808983	100.701413	65.930497
1469.910536	107.449665	65.935502
1469.511580	108.334575	65.940506
1469.063924	119.085838	65.945511
1467.722151	118.620963	65.950516
1467.206086	101.466129	65.955521
1466.609029	99.044281	65.960526
1466.179153	112.659468	65.965530
1465.128174	115.978611	65.970535
1464.421832	104.770444	65.975540
1463.841096	100.600404	65.980545
1463.406774	107.311171	65.985550
1462.999341	101.830017	65.990554
1462.277300	113.804381	65.995559
1461.371547	106.261019	66.000564
1460.962617	90.645550	66.005569
1459.558330	116.136473	66.010574
1458.883779	115.756375	66.015578
1458.438816	106.965019	66.020583
1458.253151	111.141661	66.025588
1458.135480	107.244947	66.030593
1456.857730	118.531802	66.035598
1455.897415	100.630750	66.040602
1455.745929	107.014312	66.045607
1454.953831	109.770373	66.050612
1453.831573	111.383631	66.055617
1452.892095	113.447213	66.060622
1452.499732	105.656699	66.065626
1451.942941	112.442123	66.070631
1451.640440	107.499353	66.075636
1451.449495	109.141223	66.080641
1450.158915	105.831428	66.085646
1449.765657	96.926213	66.090650
1448.883001	116.564473	66.095655
1447.728223	103.611018	66.100660
1447.030623	107.835901	66.105665
1446.454867	112.982814	66.110670
1446.239162	90.101951	66.115674
1445.917542	99.253147	66.120679
1445.197995	113.786380	66.125684
1444.549379	110.204266	66.130689
1443.427663	100.574342	66.135694
1443.133175	99.651327	66.140698
1441.891776	100.122945	66.145703
1441.453097	119.122979	66.150708
1441.473325	104.861640	66.155713
1440.252492	112.044315	66.160718
1439.451951	114.076361	66.165722
1439.052250	105.673613	66.170727
1438.402607	109.895607	66.175732
1437.309983	102.796673	66.180737
1436.411808	100.772751	66.185742
1436.114163	102.172970	66.190746
1435.513081	107.293948	66.195751
1435.154289	108.897842	66.200756
1434.848372	102.981112	66.205761
1433.250481	116.945922	66.210766
1433.146188	109.563769	66.215770
1432.321846	110.492635	66.220775
1431.392761	108.197673	66.225780
1430.909302	106.992470	66.230785
1429.883365	112.480576	66.235790
1429.550544	110.119238	66.240794
1429.524044	110.199101	66.245799
1428.655909	111.749908	66.250804
1427.576317	99.910407	66.255809
1426.780403	106.210312	66.260814
1426.579504	105.614607	66.265818
1425.795991	108.642109	66.270823
1424.833464	116.135384	66.275828
1424.441064	97.975372	66.280833
1423.587544	114.034235	66.285838
1423.189563	98.751326	66.290842
1422.509068	105.163769	66.295847
1421.558206	113.628119	66.300852
1421.335297	115.992548	66.305857
1420.746019	99.603116	66.310862
1419.622959	99.745294	66.315866
1418.595267	96.851031	66.320871
1417.832790	120.806596	66.325876
1418.073504	87.004323	66.330881
1417.214140	109.494588	66.335886
1416.683121	104.118235	66.340890
1416.019169	94.197970	66.345895
1415.123683	118.706077	66.350900
1414.953955	90.757730	66.355905
1413.296478	104.776159	66.360910
1413.075616	105.921341	66.365914
1412.900049	100.472730	66.370919
1411.827673	97.118817	66.375924
1411.065201	97.549026	66.380929
1410.050293	96.472444	66.385934
1409.339110	109.154677	66.390938
1409.222926	112.372578	66.395943
1408.777588	93.847272	66.400948
1408.208976	106.399617	66.405953
1406.941591	97.709029	66.410958
1406.757656	109.914826	66.415962
1406.213349	91.856238	66.420967
1405.060718	108.446735	66.425972
1404.485839	95.158310	66.430977
1403.500656	110.528506	66.435982
1403.492322	97.977894	66.440986
1402.807934	92.444585	66.445991
1401.924714	110.278993	66.450996
1401.404299	106.294913	66.456001
1400.619311	106.810701	66.461006
1399.944650	89.660614	66.466010
1399.444122	107.039978	66.471015
1398.537880	101.482006	66.476020
1398.311904	94.283200	66.481025
1397.099603	104.616696	66.486030
1396.563168	106.322941	66.491034
1396.062138	93.467462	66.496039
1395.761869	98.974273	66.501044
1395.073968	116.189473	66.506049
1394.055947	84.651397	66.511054
1393.472590	115.291220	66.516058
1392.294187	112.785176	66.521063
1391.332450	92.758773	66.526068
1391.172150	89.652549	66.531073
1390.442914	114.326605	66.536078
1390.229398	90.128724	66.541082
1389.856401	91.102553	66.546087
1388.740081	113.665204	66.551092
1388.212875	91.513500	66.556097
1387.357074	91.512294	66.561102
1386.801370	106.965608	66.566106
1385.748823	96.821702	66.571111
1385.029730	109.891530	66.576116
1384.900255	102.887108	66.581121
1384.158183	108.604485	66.586126
1383.642087	114.303294	66.591130
1382.566142	87.549198	66.596135
1381.505354	121.571611	66.601140
1381.616546	77.396791	66.606145
1381.098637	113.146297	66.611150
1380.290664	102.764831	66.616154
1379.867150	102.794262	66.621159
1378.878213	96.825265	66.626164
1378.180482	115.413905	66.631169
1377.110107	106.332488	66.636174
1376.284959	104.645469	66.641178
1376.012742	107.405648	66.646183
1375.602581	122.574085	66.651188
1375.666834	102.379872	66.656193
1374.084760	102.085698	66.661198
1373.560063	95.445282	66.666202
1373.454935	100.561552	66.671207
1371.904534	107.512798	66.676212
1371.141758	100.672115	66.681217
1370.655265	101.902095	66.686222
1370.668460	81.544149	66.691226
1369.903348	114.223364	66.696231
1368.326112	103.598339	66.701236
1367.986108	95.602420	66.706241
1367.398982	106.688068	66.711246
1367.186555	96.401176	66.716250
1366.866775	101.177847	66.721255
1365.702202	114.646479	66.726260
1365.245983	97.941047	66.731265
1363.979197	106.923955	66.736270
1362.819199	99.234981	66.741274
1362.599143	104.859927	66.746279
1361.715672	102.992959	66.751284
1361.894966	99.485846	66.756289
1361.339977	105.326447	66.761294
1360.896368	106.743568	66.766298
1360.008418	106.099388	66.771303
1359.281225	104.355806	66.776308
1358.609654	95.857533	66.781313
1357.399615	121.268733	66.786318
1356.945432	103.380320	66.791322
1356.343163	92.832140	66.796327
1355.604764	111.198594	66.801332
1355.403171	107.469761	66.806337
1354.087745	97.891177	66.811342
1353.520079	95.081507	66.816346
1353.282755	116.351758	66.821351
1352.278713	105.031691	66.826356
1351.660370	100.266872	66.831361
1351.199092	108.040015	66.836366
1350.639219	112.044342	66.841370
1349.699460	96.366631	66.846375
1348.663231	105.331819	66.851380
1348.449070	105.159253	66.856385
1347.463931	115.477165	66.861390
1347.311011	111.187114	66.866394
1346.921689	106.065785	66.871399
1345.831089	99.474329	66.876404
1345.410612	92.582403	66.881409
1343.998293	92.925126	66.886414
1343.070908	105.692192	66.891418
1342.576847	102.415108	66.896423
1342.134030	99.003729	66.901428
1341.975553	96.321396	66.906433
1341.480567	98.792151	66.911438
1340.817747	105.687476	66.916442
1340.100763	110.949892	66.921447
1339.117472	109.256486	66.926452
1339.005239	96.656172	66.931457
1337.649416	114.420645	66.936462
1336.966029	118.405188	66.941466
1336.652472	92.155946	66.946471
1336.101282	117.812480	66.951476
1335.643205	109.032701	66.956481
1334.333200	105.166267	66.961486
1333.544255	106.051691	66.966490
1333.520752	104.096916	66.971495
1332.293954	106.248786	66.976500
1331.966064	99.253837	66.981505
1331.085086	95.765463	66.986510
1330.541903	95.063335	66.991514
1330.451208	111.838267	66.996519
1329.288601	94.888768	67.001524
1328.841741	92.707994	67.006529
1328.188011	103.900421	67.011534
1327.161783	114.694778	67.016538
1326.213020	105.463176	67.021543
1325.466990	101.532327	67.026548
1325.281254	93.683774	67.031553
1324.266802	103.407134	67.036558
1324.660686	108.228050	67.041562
1323.438241	96.463354	67.046567
1322.899851	102.802766	67.051572
1322.381257	97.129591	67.056577
1321.006720	96.997991	67.061582
1320.394277	105.824861	67.066586
1320.032147	102.395929	67.071591
1319.246521	108.293701	67.076596
1318.963184	102.034376	67.081601
1317.965383	105.195315	67.086606
1317.361661	105.787962	67.091610
1316.964564	103.277597	67.096615
1316.113303	98.923533	67.101620
1315.321267	107.127707	67.106625
1314.650766	103.531766	67.111630
1314.214806	110.324806	67.116634
1313.637623	108.544776	67.121639
1312.407219	114.566871	67.126644
1311.693582	110.640335	67.131649
1311.015656	112.123097	67.136654
1310.896402	107.096031	67.141658
1310.545115	105.872995	67.146663
1309.504506	114.477793	67.151668
1308.782737	103.059264	67.156673
1308.236821	106.009606	67.161678
1307.987235	106.295236	67.166682
1306.905716	100.049267	67.171687
1306.198406	116.953763	67.176692
1306.001411	91.490209	67.181697
1304.698037	107.756207	67.186702
1304.176552	103.469564	67.191706
1303.565228	106.991670	67.196711
1302.829874	115.584212	67.201716
1302.300758	112.331630	67.206721
1301.386871	106.924714	67.211726
1300.998337	115.064749	67.216730
1300.666148	106.638688	67.221735
1299.336166	104.409086	67.226740
1298.706180	103.388045	67.231745
1298.236579	117.219278	67.236750
1297.694542	90.181675	67.241754
1296.897650	97.224467	67.246759
1295.678682	110.318585	67.251764
1295.351881	99.945814	67.256769
1294.940322	103.328936	67.261774
1294.488093	111.930081	67.266778
1293.878323	93.328463	67.271783
1292.446066	107.322188	67.276788
1292.464634	102.377288	67.281793
1292.022966	111.724190	67.286798
1291.150182	114.182481	67.291802
1290.297174	105.277854	67.296807
1289.333806	103.065665	67.301812
1289.013938	97.707818	67.306817
1288.523494	105.979162	67.311822
1287.388317	105.648686	67.316826
1286.792358	101.498460	67.321831
1285.860954	105.434135	67.326836
1285.659776	107.429283	67.331841
1285.107273	100.045873	67.336846
1284.637640	105.316282	67.341850
1283.766233	98.939155	67.346855
1282.942346	112.298457	67.351860
1282.972636	93.929384	67.356865
1281.476492	103.869677	67.361870
1281.077877	104.436032	67.366874
1280.539079	106.063830	67.371879
1279.508528	101.627902	67.376884
1278.804412	95.309335	67.381889
1278.279124	103.130503	67.386894
1277.475440	106.378860	67.391898
1277.258391	100.213079	67.396903
1276.733325	100.268133	67.401908
1275.913355	94.120942	67.406913
1275.353045	99.244925	67.411918
1274.555950	101.833103	67.416922
1273.721349	92.463543	67.421927
1272.858012	106.191793	67.426932
1272.404692	96.722191	67.431937
1272.281664	101.185328	67.436942
1271.115217	96.998080	67.441946
1270.237968	98.364314	67.446951
1269.447916	105.197883	67.451956
1269.267777	102.619920	67.456961
1268.690883	96.348934	67.461966
1267.487245	91.546316	67.466970
1267.079738	95.731421	67.471975
1265.939024	105.916397	67.476980
1265.988240	105.965301	67.481985
1265.556162	112.682040	67.486990
1265.038032	107.874504	67.491994
1264.108941	97.372007	67.496999
1263.135288	104.203229	67.502004
1262.816935	105.937901	67.507009
1262.187507	103.704168	67.512014
1261.463753	114.261229	67.517018
1260.435985	106.444056	67.522023
1259.150298	110.809786	67.527028
1258.662243	98.269237	67.532033
1258.304661	93.772056	67.537038
1257.843993	101.087815	67.542042
1257.606927	110.425842	67.547047
1257.119318	118.906469	67.552052
1256.157399	103.076215	67.557057
1255.905811	99.721179	67.562062
1254.594497	95.266828	67.567066
1253.460435	98.006352	67.572071
1252.676836	112.557675	67.577076
1252.373455	87.924726	67.582081
1251.932351	97.228957	67.587086
1251.703244	106.296071	67.592090
1251.326383	99.436651	67.597095
1249.842211	97.330935	67.602100
1249.762848	95.146938	67.607105
1248.763249	103.647463	67.612110
1247.544123	106.465167	67.617114
1247.157628	98.109255	67.622119
1246.430338	109.805375	67.627124
1246.469578	96.457212	67.632129
1245.607486	99.259149	67.637134
1244.634191	103.885858	67.642138
1244.092710	97.401102	67.647143
1243.507689	106.702991	67.652148
1243.126289	103.037453	67.657153
1241.764119	103.949393	67.662158
1241.220373	107.728835	67.667162
1240.959099	100.504127	67.672167
1239.857591	99.318388	67.677172
1239.544144	98.657019	67.682177
1238.682769	100.438610	67.687182
1237.960198	100.714299	67.692186
1237.878873	92.219990	67.697191
1237.226503	106.332573	67.702196
1236.147340	106.031058	67.707201
1235.610889	101.890307	67.712206
1235.121787	104.694441	67.717210
1233.863746	91.689737	67.722215
1233.092152	104.946115	67.727220
1232.962174	111.936504	67.732225
1232.500890	100.486053	67.737230
1231.381235	93.441985	67.742234
1230.499765	91.672514	67.747239
1229.864273	105.046017	67.752244
1229.620046	96.807830	67.757249
1228.985704	98.531249	67.762254
1228.275466	101.881450	67.767258
1227.631519	93.386717	67.772263
1226.810971	104.667180	67.777268
1226.586421	100.076314	67.782273
1225.613360	104.551613	67.787278
1224.651193	99.344787	67.792282
1224.747391	91.997019	67.797287
1223.720669	110.888695	67.802292
1222.781948	106.729910	67.807297
1222.089229	98.451078	67.812302
1221.434729	105.990041	67.817306
1221.078841	95.976711	67.822311
1220.070244	102.316789	67.827316
1219.413025	100.979994	67.832321
1219.003066	93.607057	67.837326
1218.438742	105.160578	67.842330
1218.088709	105.492148	67.847335
1216.864823	102.922464	67.852340
1216.562485	96.040166	67.857345
1216.090205	103.192205	67.862350
1215.209562	109.609708	67.867354
1214.548722	98.309260	67.872359
1213.655091	111.413172	67.877364
1212.967158	101.528328	67.882369
1211.919316	107.330631	67.887374
1211.292904	103.978432	67.892378
1210.923814	98.521198	67.897383
1210.439997	100.264840	67.902388
1210.180251	93.911906	67.907393
1209.224671	101.807809	67.912398
1208.278811	101.182352	67.917402
1207.856199	95.686324	67.922407
1206.924701	101.807577	67.927412
1206.012681	93.292403	67.932417
1205.582071	100.545044	67.937422
1205.203192	104.369235	67.942426
1204.911450	101.911520	67.947431
1203.921922	101.835450	67.952436
1203.183625	95.243238	67.957441
1202.392879	100.608868	67.962446
1201.617828	102.023526	67.967450
1201.200915	94.736849	67.972455
1200.189041	109.977298	67.977460
1199.410259	105.293224	67.982465
1199.110034	97.125444	67.987470
1198.620079	100.798573	67.992474
1197.948329	97.478819	67.997479
1196.997392	107.759790	68.002484
1196.831459	98.665534	68.007489
1196.340667	106.716182	68.012494
1195.219219	112.746228	68.017498
1194.687699	97.659662	68.022503
1194.169361	102.242427	68.027508
1193.133769	101.470403	68.032513
1192.155983	104.170912	68.037518
1191.408909	105.398208	68.042522
1191.382652	95.887527	68.047527
1190.674494	105.667871	68.052532
1189.955859	97.883578	68.057537
1188.950858	95.402099	68.062542
1188.004667	104.778772	68.067546
1187.999914	96.750080	68.072551
1187.292622	111.439079	68.077556
1187.159032	99.190675	68.082561
1185.894452	97.381221	68.087566
1185.238559	97.381409	68.092570
1184.998509	99.657117	68.097575
1183.667591	114.781160	68.102580
1182.992912	104.242970	68.107585
1182.566832	96.068402	68.112590
1181.702112	107.791115	68.117594
1181.704329	93.538998	68.122599
1180.947063	109.057490	68.127604
1179.801777	93.179181	68.132609
1179.281174	99.421171	68.137614
1178.912836	99.769849	68.142618
1177.947670	95.268381	68.147623
1177.103539	109.900296	68.152628
1176.780446	99.298319	68.157633
1176.627798	91.170155	68.162638
1175.567367	96.648057	68.167642
1175.072301	87.754376	68.172647
1173.992891	103.428163	68.177652
1173.465126	97.641375	68.182657
1172.720795	107.872153	68.187662
1171.996394	108.346837	68.192666
1171.337864	98.198728	68.197671
1170.576782	105.959642	68.202676
1169.742374	97.876816	68.207681
1169.004780	88.021971	68.212686
1168.359040	103.103276	68.217690
1168.156351	100.834821	68.222695
1167.932497	106.482452	68.227700
1167.431900	104.772276	68.232705
1166.125244	106.922730	68.237710
1165.477393	107.883532	68.242714
1164.929939	109.066477	68.247719
1163.827133	100.241054	68.252724
1163.272830	97.569648	68.257729
1162.822625	98.795470	68.262734
1162.300677	107.171180	68.267738
1161.846877	97.130860	68.272743
1160.637843	105.634757	68.277748
1160.439507	101.741437	68.282753
1159.695717	104.445744	68.287758
1158.345708	105.518211	68.292762
1157.829497	100.273608	68.297767
1157.336251	101.723884	68.302772
1156.909489	100.897630	68.307777
1156.504779	101.335670	68.312782
1155.669850	104.079701	68.317786
1155.115942	97.762518	68.322791
1154.073855	107.275870	68.327796
1153.833510	96.458902	68.332801
1152.800221	101.325404	68.337806
1152.011972	104.582379	68.342810
1151.984370	94.647740	68.347815
1151.259868	100.393910	68.352820
1150.393273	101.012632	68.357825
1149.328432	105.428440	68.362830
1148.929402	104.723926	68.367834
1148.500934	95.996266	68.372839
1147.313095	107.855523	68.377844
1146.651557	96.254032	68.382849
1146.194151	107.235501	68.387854
1145.518605	109.436977	68.392858
1145.587087	98.184563	68.397863
1144.455742	100.641442	68.402868
1143.629497	97.149166	68.407873
1143.307373	101.298632	68.412878
1142.206829	102.312511	68.417882
1141.513090	97.436750	68.422887
1140.855821	103.556986	68.427892
1140.390980	109.733350	68.432897
1140.048466	101.449311	68.437902
1138.915932	115.062719	68.442906
1138.470801	98.196342	68.447911
1137.536887	105.592109	68.452916
1137.573869	101.819055	68.457921
1136.551001	101.604819	68.462926
1135.340770	114.115739	68.467930
1135.158193	100.020738	68.472935
1134.474583	108.330704	68.477940
1133.917876	104.527495	68.482945
1133.025250	100.178503	68.487950
1132.308774	100.724473	68.492954
1132.001090	96.036462	68.497959
1131.111131	107.474634	68.502964
1130.159209	100.750849	68.507969
1129.856880	97.243060	68.512974
1129.037146	99.495854	68.517978
1128.509007	96.396118	68.522983
1128.000557	114.850596	68.527988
1127.054699	98.352426	68.532993
1126.708450	96.396952	68.537998
1125.917359	103.568168	68.543002
1125.303307	91.987520	68.548007
1124.509877	97.762002	68.553012
1123.802214	107.928613	68.558017
1123.634691	101.382837	68.563022
1122.267222	102.207378	68.568026
1122.096200	87.967059	68.573031
1121.424853	106.270825	68.578036
1120.554073	100.514952	68.583041
1119.907228	97.799930	68.588046
1118.980660	109.111471	68.593050
1118.727862	105.496461	68.598055
1118.048116	97.551477	68.603060
1117.207469	105.599430	68.608065
1116.637533	118.232440	68.613070
1115.789954	111.414795	68.618074
1115.647626	92.090822	68.623079
1114.121900	116.164626	68.628084
1113.544251	102.124578	68.633089
1113.404342	92.756557	68.638094
1112.660633	111.817696	68.643098
1112.256055	97.396909	68.648103
1110.805195	102.801323	68.653108
1110.302665	97.527751	68.658113
1110.330673	101.769757	68.663118
1109.523320	112.057879	68.668122
1108.711099	108.063515	68.673127
1107.898618	105.707558	68.678132
1107.442501	98.215838	68.683137
1107.279645	100.723688	68.688142
1105.996385	104.809995	68.693146
1105.169891	95.237377	68.698151
1104.656071	95.960846	68.703156
1104.289367	100.323975	68.708161
1103.206786	96.877214	68.713166
1102.260162	101.608531	68.718170
1101.962447	101.725227	68.723175
1101.693018	104.787740	68.728180
1101.189150	107.162183	68.733185
1099.929834	99.195851	68.738190
1099.207522	108.227875	68.743194
1098.765988	94.158307	68.748199
1098.352072	98.281377	68.753204
1097.420394	103.937517	68.758209
1096.678091	94.383050	68.763214
1096.075378	104.815229	68.768218
1095.757037	98.449557	68.773223
1094.636337	110.774369	68.778228
1094.091676	100.105156	68.783233
1093.624715	94.877968	68.788238
1092.821615	105.677893	68.793242
1091.983129	95.209952	68.798247
1091.396675	103.938107	68.803252
1090.631816	104.472862	68.808257
1090.388056	105.810933	68.813262
1089.420012	102.901016	68.818266
1088.581926	94.954422	68.823271
1087.674588	106.534130	68.828276
1087.376605	103.391488	68.833281
1087.252414	100.575998	68.838286
1086.633066	118.327492	68.843290
1085.862839	101.659488	68.848295
1085.152954	101.258304	68.853300
1084.314752	102.191058	68.858305
1083.552406	97.739367	68.863310
1082.678798	104.679304	68.868314
1082.552795	102.759763	68.873319
1081.561799	100.053763	68.878324
1080.525381	101.817517	68.883329
1080.071417	96.153050	68.888334
1079.446292	105.377764	68.893338
1079.299434	99.166158	68.898343
1078.568358	103.694474	68.903348
1077.523247	94.528782	68.908353
1077.124661	101.513004	68.913358
1076.317733	111.451000	68.918362
1075.689646	99.815829	68.923367
1074.608120	102.539187	68.928372
1074.026066	95.430188	68.933377
1073.811771	98.580121	68.938382
1073.129643	102.629169	68.943386
1072.676439	93.375639	68.948391
1071.631245	102.968350	68.953396
1071.032864	102.051144	68.958401
1070.894119	101.508657	68.963406
1069.424097	108.141366	68.968410
1068.983001	93.556104	68.973415
1068.580340	110.465768	68.978420
1067.688480	106.838882	68.983425
1066.693190	93.473962	68.988430
1065.942772	113.177959	68.993434
1065.610700	105.445753	68.998439
1065.319834	100.256788	69.003444
1064.784019	112.253623	69.008449
1063.895637	107.725795	69.013454
1063.167861	105.520374	69.018458
1062.759133	96.994588	69.023463
1061.710753	100.392308	69.028468
1060.894502	109.740464	69.033473
1060.226972	99.193304	69.038478
1059.883587	104.911987	69.043482
1059.198073	103.675925	69.048487
1058.205902	98.056075	69.053492
1057.458775	99.229803	69.058497
1057.315825	105.077444	69.063502
1056.779625	113.373439	69.068506
1055.760113	100.324591	69.073511
1055.020112	106.189938	69.078516
1054.695980	101.938194	69.083521
1054.129278	98.921876	69.088526
1052.607760	109.602714	69.093530
1052.484131	96.703084	69.098535
1051.963278	108.998719	69.103540
1051.645597	103.645296	69.108545
1050.970299	100.605254	69.113550
1049.614201	108.192777	69.118554
1049.192031	104.628372	69.123559
1048.885305	100.009604	69.128564
1047.756437	93.733454	69.133569
1047.031395	102.365395	69.138574
1046.516783	96.573396	69.143578
1046.287927	96.483613	69.148583
1045.102989	104.043909	69.153588
1044.341334	112.487726	69.158593
1043.912593	107.148816	69.163598
1043.191389	103.190459	69.168602
1043.245620	109.749438	69.173607
1041.808350	103.090283	69.178612
1041.131324	108.311717	69.183617
1040.663862	105.355304	69.188622
1040.261149	108.237186	69.193626
1039.455166	96.032699	69.198631
1038.934764	104.625782	69.203636
1038.177050	104.057187	69.208641
1037.299929	94.484769	69.213646
1036.174034	101.169976	69.218650
1035.974727	100.261831	69.223655
1035.493784	112.809727	69.228660
1034.979794	103.048658	69.233665
1034.139411	105.894513	69.238670
1033.140622	106.247314	69.243674
1032.544595	99.544226	69.248679
1032.254368	111.434190	69.253684
1031.157188	105.607139	69.258689
1030.661530	103.356920	69.263694
1029.720627	102.032190	69.268698
1029.850577	101.498998	69.273703
1028.768051	98.243064	69.278708
1028.067803	96.061660	69.283713
1027.691280	97.669999	69.288718
1026.575830	99.785373	69.293722
1026.050941	100.403391	69.298727
1025.371178	102.465225	69.303732
1024.850183	103.994051	69.308737
1024.070042	102.881857	69.313742
1023.568773	98.656721	69.318746
1022.862708	96.668621	69.323751
1021.955384	110.738214	69.328756
1021.427935	99.176936	69.333761
1021.145627	100.959512	69.338766
1019.937155	101.203757	69.343770
1019.425164	98.401083	69.348775
1018.957419	87.327030	69.353780
1018.428862	97.876719	69.358785
1017.508215	96.299628	69.363790
1016.401518	100.122933	69.368794
1016.271333	95.354670	69.373799
1015.650381	96.218194	69.378804
1014.968986	100.211948	69.383809
1014.220432	89.059572	69.388814
1013.554591	97.332034	69.393818
1013.198872	94.078749	69.398823
1012.015433	105.366525	69.403828
1011.445904	103.191136	69.408833
1011.050178	98.707953	69.413838
1010.078051	108.402597	69.418842
1009.899396	97.290433	69.423847
1008.643787	92.406337	69.428852
1007.855652	96.741907	69.433857
1007.793333	101.113388	69.438862
1007.075477	103.506121	69.443866
1006.331180	99.576681	69.448871
1005.573758	97.601487	69.453876
1004.893174	112.194800	69.458881
1004.673786	100.340103	69.463886
1003.727868	103.172796	69.468890
1002.448212	98.317757	69.473895
1002.192212	98.645435	69.478900
1001.797494	106.901579	69.483905
1001.715942	92.793698	69.488910
1000.069807	93.392992	69.493914
999.733366	96.855657	69.498919
999.281486	98.338801	69.503924
998.240748	111.921875	69.508929
997.453198	102.473983	69.513934
996.877626	102.123992	69.518938
996.459707	96.078517	69.523943
996.097212	93.881234	69.528948
994.946579	96.505237	69.533953
994.312404	95.904386	69.538958
993.869744	100.144000	69.543962
993.268195	95.884366	69.548967
992.156630	101.813569	69.553972
991.610628	108.646222	69.558977
991.431857	97.746956	69.563982
990.558060	104.004166	69.568986
989.858753	101.929850	69.573991
989.034615	96.043615	69.578996
988.603929	98.863724	69.584001
988.018851	95.657970	69.589006
986.830909	95.542593	69.594010
986.282912	101.101455	69.599015
985.833980	93.236486	69.604020
985.287995	100.081749	69.609025
984.713347	94.699842	69.614030
983.517626	98.993037	69.619034
983.206865	90.200968	69.624039
982.859371	98.105840	69.629044
981.670591	99.329355	69.634049
981.046094	95.907537	69.639054
980.317820	102.548427	69.644058
979.753674	89.324688	69.649063
979.697561	104.719032	69.654068
978.512383	104.235810	69.659073
977.792529	98.757164	69.664078
976.935595	103.094228	69.669082
976.680390	91.778223	69.674087
975.946591	96.311725	69.679092
974.974580	97.549639	69.684097
974.792720	93.838215	69.689102
973.962064	107.860926	69.694106
973.678622	90.483220	69.699111
972.578666	103.799763	69.704116
971.940121	94.518981	69.709121
971.493296	85.390618	69.714126
970.494945	103.087288	69.719130
969.505917	93.684084	69.724135
968.748985	97.461220	69.729140
968.446834	102.883206	69.734145
968.308554	99.939088	69.739150
967.580404	98.454384	69.744154
966.448962	98.952888	69.749159
965.832781	96.641440	69.754164
965.320985	98.797982	69.759169
965.043132	98.950955	69.764174
963.998495	100.282425	69.769178
963.092633	105.303753	69.774183
962.734917	103.421086	69.779188
962.576890	101.342655	69.784193
961.465875	96.306275	69.789198
960.324812	101.565286	69.794202
960.153900	93.045843	69.799207
959.837707	96.894776	69.804212
958.513423	103.397124	69.809217
958.382035	94.354181	69.814222
957.202127	101.625143	69.819226
956.713767	99.236592	69.824231
955.658011	95.252652	69.829236
954.964853	102.064569	69.834241
954.450506	93.308051	69.839246
954.015521	93.533332	69.844250
953.925781	89.405155	69.849255
953.371678	98.230674	69.854260
952.280747	105.537942	69.859265
951.799365	90.131280	69.864270
950.681503	93.746663	69.869274
949.943478	95.000970	69.874279
949.598446	103.012680	69.879284
948.964561	104.764476	69.884289
948.419665	97.815173	69.889294
947.452930	98.156599	69.894298
946.790424	92.591575	69.899303
946.503550	97.197468	69.904308
945.545235	107.058656	69.909313
944.696822	93.227334	69.914318
943.919620	93.921782	69.919322
943.931056	92.303641	69.924327
942.865714	91.247890	69.929332
941.559878	99.106564	69.934337
940.999852	96.579618	69.939342
940.549258	118.664293	69.944346
940.506608	103.787020	69.949351
940.243402	93.571369	69.954356
938.955697	99.962255	69.959361
938.442504	90.786114	69.964366
937.744339	97.896856	69.969370
937.172461	97.896354	69.974375
936.406889	92.161663	69.979380
935.505879	106.181381	69.984385
935.221077	89.754753	69.989390
933.833775	88.862192	69.994394
933.209081	96.580950	69.999399
933.187222	95.953645	70.004404
932.729972	110.233900	70.009409
932.004825	97.687033	70.014414
930.793257	95.780972	70.019418
930.438166	96.851358	70.024423
929.767900	90.806632	70.029428
928.977751	94.554372	70.034433
928.133585	97.936993	70.039438
927.320968	100.507240	70.044442
927.131961	97.214827	70.049447
926.909591	101.200213	70.054452
925.176426	98.416841	70.059457
924.772120	97.424638	70.064462
924.173681	96.334023	70.069466
923.851138	96.330118	70.074471
923.571343	85.954699	70.079476
922.337620	101.659409	70.084481
921.606340	102.818039	70.089486
921.030098	109.530941	70.094490
920.866518	93.688962	70.099495
919.832218	86.051193	70.104500
918.715039	90.883817	70.109505
918.551489	105.287634	70.114510
917.911276	97.065210	70.119514
916.823732	97.815356	70.124519
916.146052	91.361830	70.129524
915.289927	103.094266	70.134529
915.415909	98.518625	70.139534
914.950348	93.956694	70.144538
913.770305	103.235040	70.149543
912.886652	94.888940	70.154548
912.355820	100.229051	70.159553
912.238427	91.683756	70.164558
910.902168	98.487633	70.169562
910.372985	96.395731	70.174567
909.940924	95.493098	70.179572
909.481988	96.373441	70.184577
908.818076	95.692195	70.189582
907.930795	101.544741	70.194586
907.493641	92.919448	70.199591
906.804341	91.781799	70.204596
905.784012	95.897315	70.209601
905.106211	95.273469	70.214606
904.649753	97.367603	70.219610
904.147154	96.444658	70.224615
903.122529	86.703400	70.229620
902.279667	103.802941	70.234625
902.198542	93.473173	70.239630
901.532274	98.270322	70.244634
900.295455	95.480521	70.249639
899.410878	102.264565	70.254644
899.271394	102.486985	70.259649
898.718264	105.845379	70.264654
898.320646	107.818195	70.269658
897.366246	100.516201	70.274663
896.767494	92.047506	70.279668
896.139469	108.778572	70.284673
895.261374	103.309365	70.289678
894.420356	99.147787	70.294682
894.005271	111.536984	70.299687
893.822597	109.225950	70.304692
892.547412	102.252532	70.309697
891.774526	92.531137	70.314702
891.221958	93.229276	70.319706
890.802238	108.947963	70.324711
890.384641	100.437823	70.329716
889.103093	105.627761	70.334721
888.484438	98.944087	70.339726
887.694475	107.715696	70.344730
887.745304	108.204280	70.349735
887.520830	98.170121	70.354740
886.081051	97.188172	70.359745
885.760024	90.698400	70.364750
884.674785	108.738484	70.369754
883.812253	103.284150	70.374759
883.396536	96.904056	70.379764
882.687252	108.308801	70.384769
882.306169	105.691894	70.389774
881.250359	99.576078	70.394778
880.495654	99.483265	70.399783
880.084895	92.403835	70.404788
879.604399	110.653597	70.409793
879.307497	101.621232	70.414798
877.753063	114.444044	70.419802
877.454250	96.572094	70.424807
876.850576	100.638661	70.429812
876.372762	118.550557	70.434817
875.569206	107.239830	70.439822
874.760623	100.464967	70.444826
874.080299	103.280667	70.449831
873.717438	89.157660	70.454836
872.613936	107.206959	70.459841
871.871491	99.732483	70.464846
871.151359	95.532754	70.469850
870.812945	127.182174	70.474855
870.946385	92.089896	70.479860
869.369705	97.361499	70.484865
868.536884	103.886594	70.489870
868.498922	100.484999	70.494874
867.785041	99.199893	70.499879
866.945068	93.713597	70.504884
866.052869	110.519822	70.509889
866.092419	103.986856	70.514894
865.172662	90.881248	70.519898
864.269203	103.758144	70.524903
863.514912	106.888377	70.529908
862.835496	104.087153	70.534913
862.477556	98.002202	70.539918
861.511144	99.396953	70.544922
860.863883	110.914828	70.549927
860.655919	94.471257	70.554932
859.916875	101.098118	70.559937
858.960044	95.417545	70.564942
858.316991	111.700025	70.569946
857.759036	113.969585	70.574951
857.577197	88.224683	70.579956
856.244259	105.635602	70.584961
855.661416	111.646285	70.589966
855.486244	99.283144	70.594970
853.996396	108.568244	70.599975
853.370266	98.008268	70.604980
852.630757	120.228801	70.609985
852.540910	94.742046	70.614990
852.066468	103.345180	70.619994
851.273910	103.394010	70.624999
850.483992	103.157009	70.630004
849.546642	103.276189	70.635009
849.319681	104.523301	70.640014
848.081713	99.251729	70.645018
847.451167	99.131282	70.650023
847.075788	89.258340	70.655028
846.519770	109.669380	70.660033
846.101935	93.697583	70.665038
844.910261	89.993933	70.670042
844.081388	102.501015	70.675047
843.829397	107.088750	70.680052
843.619657	109.440080	70.685057
842.993862	93.504535	70.690062
841.809683	99.489502	70.695066
841.321415	97.589789	70.700071
840.293303	95.708189	70.705076
839.524461	103.788933	70.710081
839.147180	100.537531	70.715086
838.560255	94.928975	70.720090
838.111019	103.097616	70.725095
837.145962	104.556812	70.730100
836.534100	103.384781	70.735105
835.885037	84.452185	70.740110
835.383622	107.448465	70.745114
834.438523	99.698769	70.750119
833.998702	94.859963	70.755124
833.320517	106.478948	70.760129
832.762918	96.010569	70.765134
831.759046	92.092543	70.770138
831.013310	102.301525	70.775143
830.453311	106.602411	70.780148
830.051732	98.200119	70.785153
829.840396	95.587744	70.790158
828.715683	103.069156	70.795162
827.781929	101.675562	70.800167
827.463916	98.859404	70.805172
826.149349	108.646446	70.810177
825.165861	101.096817	70.815182
824.873015	99.692676	70.820186
824.377530	106.350164	70.825191
824.322013	94.977179	70.830196
823.875246	97.005132	70.835201
822.814454	116.424255	70.840206
822.314383	104.100213	70.845210
821.283058	101.127944	70.850215
821.139506	103.311053	70.855220
819.827394	103.294361	70.860225
819.556014	97.796427	70.865230
819.037085	109.120425	70.870234
817.643443	105.425277	70.875239
817.043765	100.750680	70.880244
816.368519	106.809190	70.885249
816.448369	100.345504	70.890254
815.588047	100.233253	70.895258
814.571529	97.138789	70.900263
814.260923	99.206570	70.905268
813.634004	98.770182	70.910273
812.962267	95.832142	70.915278
812.188632	107.702852	70.920282
811.269724	98.810504	70.925287
811.178772	96.664643	70.930292
809.885561	96.567682	70.935297
808.909684	104.840648	70.940302
808.605516	100.880643	70.945306
807.883122	105.559020	70.950311
807.800556	91.946473	70.955316
807.325102	102.935561	70.960321
806.436150	95.645270	70.965326
805.642422	104.663484	70.970330
804.501495	111.075223	70.975335
803.519322	109.183172	70.980340
802.785739	106.150904	70.985345
802.670447	103.838616	70.990350
802.525071	95.228406	70.995354
802.158180	103.565282	71.000359
801.781929	101.382835	71.005364
800.560373	104.019788	71.010369
799.721178	101.693421	71.015374
798.549745	96.348213	71.020378
797.489888	103.530747	71.025383
797.450182	97.863485	71.030388
796.913992	103.354270	71.035393
796.408157	96.203264	71.040398
795.571663	97.235181	71.045402
794.793538	98.765557	71.050407
794.569212	96.158407	71.055412
793.999818	101.334374	71.060417
792.954088	95.813052	71.065422
792.136716	101.250828	71.070426
791.548468	100.426690	71.075431
790.868281	103.048434	71.080436
789.976894	109.491417	71.085441
789.607181	94.984767	71.090446
788.862895	102.109188	71.095450
788.516170	100.943850	71.100455
788.352038	94.839105	71.105460
787.240378	96.648064	71.110465
786.400710	95.163821	71.115470
785.598598	101.005999	71.120474
784.542967	100.704087	71.125479
784.115809	99.155760	71.130484
783.410906	96.055861	71.135489
783.357281	95.428884	71.140494
782.782533	85.324361	71.145498
781.855924	103.224101	71.150503
781.170002	92.378800	71.155508
780.394661	98.461131	71.160513
779.790050	99.041429	71.165518
779.206978	90.456744	71.170522
778.483464	99.539473	71.175527
778.091489	94.111203	71.180532
776.749198	104.637492	71.185537
776.165692	89.319686	71.190542
775.811237	97.446435	71.195546
775.235765	90.956189	71.200551
774.997327	93.726802	71.205556
773.784809	105.263702	71.210561
773.358134	95.624431	71.215566
772.518531	99.112021	71.220570
771.255090	106.334856	71.225575
770.985240	92.493522	71.230580
770.105849	100.716448	71.235585
769.761409	89.987096	71.240590
769.574806	89.562626	71.245594
768.388382	97.448094	71.250599
767.952958	98.622746	71.255604
767.312410	98.168040	71.260609
766.860681	98.120068	71.265614
765.784624	104.289694	71.270618
764.903860	101.061685	71.275623
764.665969	91.915886	71.280628
764.321414	107.315117	71.285633
763.057739	100.188566	71.290638
762.495458	100.962391	71.295642
761.825622	102.937559	71.300647
761.590673	96.752632	71.305652
760.109297	120.690200	71.310657
759.351591	101.469001	71.315662
759.064390	102.840820	71.320666
758.588002	103.153144	71.325671
758.385290	97.522872	71.330676
757.358634	103.033394	71.335681
756.457576	98.532940	71.340686
755.903838	97.515670	71.345690
755.348298	101.703902	71.350695
755.210086	95.900946	71.355700
754.097803	102.770161	71.360705
753.522990	97.892941	71.365710
752.857379	97.238813	71.370714
751.747787	91.417037	71.375719
751.298926	96.979075	71.380724
750.632863	100.730766	71.385729
750.171592	91.764023	71.390734
749.351033	95.013635	71.395738
748.637533	99.040943	71.400743
748.007512	95.121784	71.405748
747.489754	108.785660	71.410753
746.628990	90.252631	71.415758
745.804570	95.678924	71.420762
744.849721	93.777819	71.425767
744.623028	98.587020	71.430772
744.377249	105.152730	71.435777
743.688040	94.639106	71.440782
742.745680	94.826928	71.445786
742.218016	101.306630	71.450791
741.643902	97.916281	71.455796
740.528320	93.902544	71.460801
739.772254	109.405131	71.465806
739.135474	91.096630	71.470810
738.483984	101.255934	71.475815
738.417443	106.645158	71.480820
737.623410	94.503558	71.485825
736.677175	96.921678	71.490830
736.302208	106.652212	71.495834
735.925045	108.598140	71.500839
735.070928	101.094187	71.505844
733.889069	101.285449	71.510849
733.283551	99.850676	71.515854
733.066328	94.044533	71.520858
732.071546	103.402256	71.525863
731.511344	96.281999	71.530868
730.810311	102.549621	71.535873
730.443260	107.717042	71.540878
729.780890	96.152114	71.545882
728.660054	103.949893	71.550887
728.259699	105.267194	71.555892
728.019966	108.889523	71.560897
726.653213	107.848735	71.565902
726.552965	107.530362	71.570906
725.806873	103.099860	71.575911
724.996371	101.210472	71.580916
723.980569	111.643814	71.585921
723.190676	106.938027	71.590926
723.115150	103.731641	71.595930
722.542646	99.259315	71.600935
721.685414	96.604708	71.605940
720.822210	96.833550	71.610945
720.189779	101.701040	71.615950
719.844776	115.476185	71.620954
718.867076	106.504930	71.625959
717.963933	95.678465	71.630964
717.537660	99.280030	71.635969
717.274416	103.989404	71.640974
716.514313	102.349024	71.645978
715.225849	106.305461	71.650983
714.742630	96.216342	71.655988
714.311926	105.312391	71.660993
714.082385	98.467483	71.665998
713.316461	101.970168	71.671002
712.081123	106.947838	71.676007
711.754010	101.053541	71.681012
711.121282	103.967352	71.686017
710.441235	98.346852	71.691022
709.679657	95.296998	71.696026
708.846503	106.891790	71.701031
708.875090	101.478573	71.706036
707.731668	101.793030	71.711041
706.904302	104.635334	71.716046
706.396086	89.264571	71.721050
706.070292	98.673477	71.726055
705.557055	97.086833	71.731060
704.455911	101.273633	71.736065
703.686879	104.631745	71.741070
703.082849	99.915299	71.746074
702.131949	104.831919	71.751079
701.493913	98.575566	71.756084
700.984861	107.953734	71.761089
700.540150	98.842448	71.766094
700.388941	102.945817	71.771098
699.425958	101.512774	71.776103
698.920321	102.026874	71.781108
697.844759	105.794891	71.786113
696.797611	109.723955	71.791118
696.229491	96.311724	71.796122
695.642865	104.770318	71.801127
695.602543	107.490474	71.806132
694.623487	107.013992	71.811137
693.585072	98.982768	71.816142
693.130679	103.344130	71.821146
692.398991	102.054027	71.826151
692.071442	99.362404	71.831156
691.240494	99.138293	71.836161
690.339565	108.689234	71.841166
690.099231	94.808529	71.846170
689.599170	96.800835	71.851175
688.727320	93.161455	71.856180
687.958942	99.367272	71.861185
687.683364	106.806577	71.866190
686.538989	103.901249	71.871194
685.608184	113.102158	71.876199
685.370327	99.184787	71.881204
684.678145	103.509897	71.886209
684.011166	112.848563	71.891214
683.117857	103.521713	71.896218
682.011845	104.252824	71.901223
681.909217	98.953535	71.906228
681.802258	102.682451	71.911233
681.038117	101.293446	71.916238
680.154561	88.325666	71.921242
679.215236	104.333644	71.926247
678.928156	90.969713	71.931252
677.750410	95.547164	71.936257
676.822638	107.649007	71.941262
676.668328	99.213691	71.946266
676.116577	99.385075	71.951271
675.962879	91.257154	71.956276
674.684200	108.123366	71.961281
674.150700	97.930307	71.966286
673.817963	90.825890	71.971290
672.574850	113.066683	71.976295
671.835134	100.662586	71.981300
671.350853	104.762221	71.986305
670.796115	100.854749	71.991310
670.599601	98.377218	71.996314
669.359838	97.076561	72.001319
668.599417	96.328749	72.006324
668.021495	96.715601	72.011329
667.417506	93.413602	72.016334
667.064468	94.882640	72.021338
665.956626	98.588002	72.026343
665.893027	90.932986	72.031348
664.453254	91.662056	72.036353
663.486518	95.072155	72.041358
663.274005	105.746591	72.046362
662.570903	104.578094	72.051367
662.418648	102.926098	72.056372
661.996001	93.894886	72.061377
660.909192	91.705762	72.066382
660.112710	92.609933	72.071386
659.477944	102.679860	72.076391
659.108179	98.676711	72.081396
658.114344	100.017560	72.086401
657.431081	97.209128	72.091406
657.092138	89.700451	72.096410
656.219471	108.596087	72.101415
655.539074	94.056952	72.106420
654.433648	96.711747	72.111425
653.911120	100.863202	72.116430
653.981785	94.605979	72.121434
653.061697	97.778433	72.126439
652.324774	89.945220	72.131444
651.306206	95.522293	72.136449
650.964815	96.681991	72.141454
650.578958	97.356789	72.146458
649.252109	102.435783	72.151463
648.660863	91.058251	72.156468
648.554063	94.586879	72.161473
648.181257	95.237524	72.166478
647.086609	96.458819	72.171482
645.995798	96.815386	72.176487
645.684421	99.402092	72.181492
645.312916	91.925408	72.186497
643.832679	90.142693	72.191502
643.589579	97.855927	72.196506
642.813952	93.226745	72.201511
642.364091	95.912768	72.206516
642.252588	97.937824	72.211521
641.102249	97.252108	72.216526
640.417520	93.095702	72.221530
639.735544	98.343234	72.226535
638.972394	97.048697	72.231540
638.194134	95.214126	72.236545
637.306885	104.310342	72.241550
636.972015	95.643604	72.246554
636.637136	99.328392	72.251559
636.563736	90.508066	72.256564
635.086644	96.443569	72.261569
634.398294	102.753343	72.266574
633.661278	89.047935	72.271578
632.631596	98.108484	72.276583
632.321490	98.816952	72.281588
631.457546	89.931710	72.286593
631.041755	94.100861	72.291598
631.075064	98.781938	72.296602
629.869836	99.987736	72.301607
629.300492	93.797736	72.306612
628.782483	97.418651	72.311617
627.533529	97.057709	72.316622
627.032571	90.889935	72.321626
626.201607	96.233729	72.326631
626.030818	93.119789	72.331636
625.453202	88.386548	72.336641
624.594691	98.474760	72.341646
623.827057	99.170935	72.346650
623.189793	107.112511	72.351655
622.998894	98.701952	72.356660
621.769747	90.615992	72.361665
620.946798	106.067743	72.366670
621.003170	88.136172	72.371674
620.062809	91.527894	72.376679
619.288192	85.574003	72.381684
618.405807	110.925267	72.386689
618.024866	98.123462	72.391694
617.425524	83.188270	72.396698
615.682368	111.418758	72.401703
615.607544	69.003744	72.406708
615.076274	103.897396	72.411713
614.363645	83.008688	72.416718
614.731150	96.919495	72.421722
613.525596	100.074347	72.426727
612.767804	72.383979	72.431732
611.999290	94.251157	72.436737
611.073498	96.632951	72.441742
610.494856	96.018626	72.446746
609.415178	91.057854	72.451751
609.227857	98.224498	72.456756
609.265250	105.341169	72.461761
608.111857	82.575235	72.466766
607.118697	98.265385	72.471770
606.474005	86.745004	72.476775
606.303078	109.781680	72.481780
605.722218	95.291365	72.486785
604.447274	90.232388	72.491790
604.004638	95.733531	72.496794
603.520555	93.732285	72.501799
602.810203	80.588743	72.506804
601.648799	95.946161	72.511809
601.198518	90.844164	72.516814
600.975306	91.972433	72.521818
600.362526	99.982645	72.526823
599.500520	93.407202	72.531828
598.803682	98.053173	72.536833
598.063592	97.937619	72.541838
597.800182	87.214332	72.546842
596.677371	100.895721	72.551847
596.022124	94.345696	72.556852
595.720452	92.269674	72.561857
594.933302	96.884299	72.566862
594.293946	94.636563	72.571866
593.293520	104.222293	72.576871
593.300992	92.536557	72.581876
592.301441	104.507932	72.586881
591.231309	97.637648	72.591886
590.704202	95.531300	72.596890
590.048104	100.181824	72.601895
589.387656	102.795743	72.606900
588.759138	101.430898	72.611905
587.949234	107.286985	72.616910
587.682153	93.524099	72.621914
587.240903	95.775124	72.626919
586.317975	99.007973	72.631924
585.556329	100.827505	72.636929
584.669313	105.161591	72.641934
584.683483	85.792348	72.646938
583.401621	92.753279	72.651943
582.688439	102.558178	72.656948
582.069738	101.164964	72.661953
581.434301	105.403796	72.666958
581.202834	105.525770	72.671962
580.063587	103.622559	72.676967
579.980700	95.663135	72.681972
579.244464	93.564864	72.686977
577.787776	95.433591	72.691982
577.628140	86.614393	72.696986
577.004592	95.066263	72.701991
576.731103	98.446408	72.706996
575.598285	94.258889	72.712001
574.675978	101.605661	72.717006
574.327616	96.358135	72.722010
573.664267	102.250804	72.727015
573.463232	96.975083	72.732020
572.582068	96.262300	72.737025
571.400335	99.656212	72.742030
571.391960	91.017915	72.747034
569.808858	97.124867	72.752039
569.409068	85.969173	72.757044
568.794559	88.183141	72.762049
568.440616	93.879884	72.767054
568.252188	99.108749	72.772058
567.062950	91.737087	72.777063
566.238889	99.511311	72.782068
565.782505	92.740403	72.787073
565.047638	101.016054	72.792078
564.945863	84.699155	72.797082
563.570534	102.861195	72.802087
563.022962	92.471734	72.807092
562.802771	100.216012	72.812097
561.168986	98.192889	72.817102
560.728219	89.979827	72.822106
559.993233	94.778529	72.827111
559.761932	95.938050	72.832116
559.735990	92.958733	72.837121
558.355287	100.848419	72.842126
558.025139	91.495017	72.847130
557.287910	94.783450	72.852135
556.887242	91.181036	72.857140
555.872091	91.440442	72.862145
554.885976	93.336730	72.867150
554.711545	84.783228	72.872154
553.950840	91.613862	72.877159
553.304543	91.548034	72.882164
552.566631	100.842821	72.887169
552.019444	97.336278	72.892174
551.470947	92.119055	72.897178
550.029294	88.923698	72.902183
549.777929	97.084499	72.907188
549.493001	91.987715	72.912193
548.672940	96.330067	72.917198
547.932589	97.029804	72.922202
546.957754	97.949802	72.927207
546.728545	84.877874	72.932212
546.291069	93.941893	72.937217
545.108114	98.305777	72.942222
544.319220	96.148100	72.947226
543.890367	90.927593	72.952231
543.451933	95.292738	72.957236
542.732054	98.304039	72.962241
541.714469	97.483693	72.967246
541.302692	95.989729	72.972250
540.806247	98.268474	72.977255
539.949893	104.671255	72.982260
539.159022	90.761589	72.987265
538.481829	94.469370	72.992270
538.054965	97.358314	72.997274
537.162854	101.256435	73.002279
536.470090	94.054857	73.007284
536.060174	92.231036	73.012289
535.197782	100.429239	73.017294
534.962414	96.720080	73.022298
534.319261	96.961243	73.027303
533.441237	100.510213	73.032308
532.808241	92.767717	73.037313
532.251091	98.317069	73.042318
531.684942	97.779616	73.047322
530.598622	105.078414	73.052327
530.148269	96.751773	73.057332
529.721649	96.844915	73.062337
528.038930	99.312608	73.067342
527.793544	97.241822	73.072346
527.010158	96.756316	73.077351
526.866823	91.684290	73.082356
526.488407	87.786620	73.087361
525.343195	95.627772	73.092366
524.618090	95.610772	73.097370
524.156620	95.529704	73.102375
523.744013	92.910002	73.107380
522.723575	90.467534	73.112385
521.650353	91.589282	73.117390
521.659367	89.892689	73.122394
521.031112	92.310695	73.127399
520.135947	92.379127	73.132404
519.460924	94.176995	73.137409
518.876060	96.193878	73.142414
518.772350	95.191710	73.147418
517.406945	97.796514	73.152423
517.035539	90.714058	73.157428
516.506270	93.560972	73.162433
515.408311	101.424565	73.167438
514.582416	84.106604	73.172442
513.533649	103.739888	73.177447
513.342610	101.945857	73.182452
513.327135	85.586839	73.187457
512.695515	96.859421	73.192462
511.717645	81.814267	73.197466
510.764781	92.983484	73.202471
510.238602	88.719870	73.207476
509.783775	87.276922	73.212481
508.827989	99.195615	73.217486
508.343383	96.044945	73.222490
507.537573	98.894912	73.227495
507.528074	103.062439	73.232500
506.494972	92.881213	73.237505
505.463181	93.048678	73.242510
505.189136	87.630069	73.247514
504.046917	89.980145	73.252519
503.062401	87.565079	73.257524
502.860998	92.870122	73.262529
502.253205	93.996583	73.267534
502.199006	82.085740	73.272538
500.860783	88.130069	73.277543
500.216942	92.125839	73.282548
499.940970	90.876740	73.287553
499.252274	91.360118	73.292558
498.502056	90.170792	73.297562
497.713684	92.570157	73.302567
496.969258	88.778100	73.307572
496.586770	82.552073	73.312577
495.244174	94.075092	73.317582
494.530900	98.561290	73.322586
494.268291	89.405291	73.327591
493.558511	88.606893	73.332596
493.386298	108.859027	73.337601
492.650977	92.540559	73.342606
491.788160	87.017055	73.347610
490.996396	89.686603	73.352615
490.789004	95.467234	73.357620
489.807590	93.430123	73.362625
488.702460	91.540446	73.367630
488.877595	92.001334	73.372634
488.255663	96.162342	73.377639
487.328708	89.275616	73.382644
486.431405	81.833848	73.387649
486.009402	88.698846	73.392654
484.864214	88.400290	73.397658
483.798655	89.462489	73.402663
483.452567	84.828019	73.407668
483.125920	77.847250	73.412673
482.615447	93.082087	73.417678
482.232208	86.824645	73.422682
480.996587	95.441835	73.427687
480.586381	89.385794	73.432692
480.284517	86.764229	73.437697
479.180441	82.163778	73.442702
478.520215	90.195753	73.447706
477.602482	97.779928	73.452711
477.216612	91.835121	73.457716
477.061175	81.769559	73.462721
475.721779	94.900467	73.467726
475.437179	85.852050	73.472730
474.659781	92.776819	73.477735
473.703010	99.173537	73.482740
472.868898	92.237334	73.487745
472.003176	101.166168	73.492750
472.085353	94.579133	73.497754
471.564915	100.332369	73.502759
471.157797	94.570707	73.507764
470.258435	91.646957	73.512769
469.280780	102.626188	73.517774
468.940638	95.199737	73.522778
467.566557	95.704002	73.527783
466.942832	95.336575	73.532788
466.766611	84.747655	73.537793
466.092426	91.843630	73.542798
465.485517	90.650407	73.547802
464.414236	95.688774	73.552807
463.907745	95.138680	73.557812
463.528795	98.482020	73.562817
462.580934	117.372328	73.567822
461.818784	96.378035	73.572826
461.004422	96.592878	73.577831
460.515557	97.695673	73.582836
460.690478	105.816954	73.587841
459.653145	101.365136	73.592846
458.879193	95.814871	73.597850
458.183111	104.114327	73.602855
457.362622	103.790863	73.607860
456.653427	86.384957	73.612865
455.339965	112.274811	73.617870
455.305034	97.074726	73.622874
455.107315	95.672825	73.627879
454.530724	97.901279	73.632884
453.291836	98.302018	73.637889
452.232096	98.321003	73.642894
452.202856	92.980089	73.647898
451.788732	104.084003	73.652903
450.940654	106.198023	73.657908
450.070243	96.574343	73.662913
449.474908	98.898818	73.667918
449.247146	106.071908	73.672922
447.848628	105.717537	73.677927
446.665518	90.687762	73.682932
446.815312	96.198616	73.687937
446.318150	100.095344	73.692942
445.980267	99.191983	73.697946
444.785973	93.741803	73.702951
444.232872	104.795323	73.707956
443.851328	101.065310	73.712961
443.128525	104.389321	73.717966
442.359133	101.930545	73.722970
441.880387	97.659390	73.727975
440.762847	105.317986	73.732980
439.730123	94.119664	73.737985
439.016173	97.614141	73.742990
438.585270	92.318296	73.747994
438.214540	94.403576	73.752999
437.998823	91.976436	73.758004
437.511261	89.999434	73.763009
436.264238	89.415945	73.768014
435.697398	101.629062	73.773018
435.410242	85.499411	73.778023
433.986766	91.152103	73.783028
433.725502	89.996857	73.788033
432.482213	94.895493	73.793038
432.630638	91.369617	73.798042
431.587394	98.669469	73.803047
430.796462	93.227569	73.808052
430.598707	96.862147	73.813057
429.689715	95.395382	73.818062
428.941963	89.828341	73.823066
428.160739	88.177229	73.828071
427.339636	89.063319	73.833076
427.326141	95.596756	73.838081
426.370317	103.532348	73.843086
425.635900	91.340397	73.848090
425.154638	100.826117	73.853095
424.398582	91.867010	73.858100
424.392935	96.363480	73.863105
423.051489	101.079077	73.868110
422.659469	91.144245	73.873114
421.661732	98.586651	73.878119
420.488946	110.148887	73.883124
420.258542	88.141143	73.888129
419.645227	90.813819	73.893134
419.511393	104.780796	73.898138
418.744145	90.657702	73.903143
417.195832	99.747336	73.908148
416.970777	80.730044	73.913153
415.940535	114.085332	73.918158
416.153274	89.449326	73.923162
415.444080	99.475953	73.928167
414.465474	65.697980	73.933172
413.870443	109.678120	73.938177
413.069473	99.898320	73.943182
412.996210	89.840171	73.948186
412.039044	85.184809	73.953191
411.224502	100.912775	73.958196
410.837311	104.651649	73.963201
409.573851	99.792787	73.968206
409.055859	103.437391	73.973210
408.527380	100.806210	73.978215
407.922503	95.700505	73.983220
407.142166	95.354892	73.988225
406.406031	93.316582	73.993230
405.843605	96.567743	73.998234
405.371678	90.784887	74.003239
404.517281	104.150775	74.008244
404.054673	91.644308	74.013249
402.783042	104.188905	74.018254
402.593487	91.768235	74.023258
402.298293	90.392909	74.028263
401.235374	105.693706	74.033268
400.736643	91.288156	74.038273
399.824721	93.336674	74.043278
399.574309	110.322979	74.048282
398.745012	85.714246	74.053287
397.799901	88.811928	74.058292
397.198874	105.040434	74.063297
396.993819	82.866251	74.068302
395.830057	90.934318	74.073306
394.678589	111.175319	74.078311
394.468875	97.299268	74.083316
394.463122	88.409852	74.088321
393.637183	93.243585	74.093326
392.786998	89.257116	74.098330
392.212205	86.705857	74.103335
391.520951	100.528267	74.108340
390.622955	74.184928	74.113345
389.601683	99.178296	74.118350
389.098278	96.845882	74.123354
388.735738	90.422745	74.128359
388.189303	89.260905	74.133364
387.288906	101.068309	74.138369
386.586632	94.685110	74.143374
386.360373	78.805958	74.148378
385.763683	93.464794	74.153383
384.375437	99.490347	74.158388
384.065963	91.491363	74.163393
383.521584	84.780256	74.168398
383.115275	86.823905	74.173402
382.104642	100.708243	74.178407
380.795652	90.137411	74.183412
380.842137	96.913584	74.188417
380.521134	90.387642	74.193422
379.241168	102.354870	74.198426
378.763552	94.254952	74.203431
378.112442	100.303395	74.208436
377.989154	89.729706	74.213441
376.976233	105.908734	74.218446
376.348217	95.448578	74.223450
375.898830	113.543579	74.228455
374.513381	98.248058	74.233460
373.768762	85.944226	74.238465
373.113924	87.828794	74.243470
372.695712	95.642468	74.248474
372.578769	87.776803	74.253479
371.450383	101.665716	74.258484
370.837555	97.783349	74.263489
369.940298	80.385383	74.268494
369.397586	92.167327	74.273498
369.170557	99.663552	74.278503
368.372942	98.754615	74.283508
367.851158	86.224479	74.288513
367.362515	99.819078	74.293518
366.302296	91.748924	74.298522
365.442219	85.780363	74.303527
364.880883	87.642150	74.308532
364.444979	93.982710	74.313537
363.753431	77.687305	74.318542
362.790474	97.119292	74.323546
362.058805	91.149192	74.328551
361.348975	90.260960	74.333556
361.256548	83.432115	74.338561
360.114303	95.071490	74.343566
359.343258	94.615610	74.348570
358.855827	97.801217	74.353575
358.700539	98.808302	74.358580
358.163431	91.088432	74.363585
356.964254	101.620474	74.368590
356.404103	104.202698	74.373594
355.825310	103.025522	74.378599
355.098082	89.154686	74.383604
354.398087	91.886917	74.388609
353.735100	96.414017	74.393614
353.162901	95.111220	74.398618
352.057166	90.932113	74.403623
351.115368	100.590567	74.408628
351.006542	91.536240	74.413633
350.043433	102.719753	74.418638
349.848617	89.770112	74.423642
349.736196	99.706386	74.428647
348.403564	93.434686	74.433652
347.734616	95.958558	74.438657
347.326214	105.032157	74.443662
346.373187	99.748572	74.448666
345.655345	101.278936	74.453671
345.034606	96.022823	74.458676
344.853978	89.901847	74.463681
343.837012	105.201643	74.468686
342.691160	91.757042	74.473690
342.227586	92.124169	74.478695
341.646790	102.693287	74.483700
341.688572	90.723015	74.488705
340.471773	104.791598	74.493710
339.873976	91.891982	74.498714
339.162487	88.772776	74.503719
338.630268	100.846352	74.508724
338.061678	92.945435	74.513729
336.886162	98.673777	74.518734
336.546335	99.905800	74.523738
336.346754	84.361428	74.528743
334.986818	90.122310	74.533748
334.628704	87.066635	74.538753
333.988655	93.914361	74.543758
333.526908	96.482484	74.548762
332.873456	96.566078	74.553767
331.940561	94.171240	74.558772
331.596054	82.819162	74.563777
330.239224	86.409803	74.568782
329.695135	93.136589	74.573786
329.243625	91.294205	74.578791
328.669750	91.461306	74.583796
328.135266	91.029235	74.588801
327.032526	96.167278	74.593806
326.432166	94.629294	74.598810
326.194750	92.125206	74.603815
325.613300	98.865833	74.608820
324.706880	83.511371	74.613825
323.860894	102.142614	74.618830
323.390156	97.463383	74.623834
322.908079	92.737079	74.628839
321.558354	102.927297	74.633844
321.089544	96.569990	74.638849
320.517681	94.972276	74.643854
320.333470	95.562953	74.648858
319.574807	95.157147	74.653863
318.686865	104.791261	74.658868
318.329311	99.723434	74.663873
317.731009	102.512005	74.668878
316.598369	106.316073	74.673882
315.473985	100.086892	74.678887
314.970268	94.961941	74.683892
314.443486	102.635240	74.688897
314.034317	98.253685	74.693902
313.679478	100.167727	74.698906
313.049702	86.678749	74.703911
311.987988	92.611299	74.708916
311.884845	93.457122	74.713921
310.876257	92.750548	74.718926
309.875795	90.819044	74.723930
309.633229	87.547853	74.728935
308.860676	100.895983	74.733940
307.942063	89.424101	74.738945
307.018025	88.642558	74.743950
306.561145	99.977201	74.748954
306.455269	91.433311	74.753959
305.620733	94.120768	74.758964
305.207327	87.585916	74.763969
304.336862	100.419829	74.768974
303.630446	102.211717	74.773978
302.616700	84.802387	74.778983
301.562564	95.375982	74.783988
301.354096	94.611280	74.788993
300.755869	98.631363	74.793998
300.300941	97.196356	74.799002
299.840992	88.603247	74.804007
298.896077	103.543086	74.809012
298.602837	86.018931	74.814017
298.055612	92.769874	74.819022
296.709799	96.183748	74.824026
296.345741	88.754843	74.829031
295.690983	91.095128	74.834036
295.030892	94.136385	74.839041
293.863394	88.292536	74.844046
293.290522	93.324069	74.849050
292.837806	99.649973	74.854055
292.148582	105.017001	74.859060
292.229838	89.822090	74.864065
291.165812	98.277979	74.869070
290.226671	92.255819	74.874074
290.079480	94.652400	74.879079
289.003906	96.022186	74.884084
288.042587	92.863970	74.889089
287.694793	98.974468	74.894094
287.090594	91.219584	74.899098
286.560068	87.503889	74.904103
285.279913	85.126572	74.909108
284.962302	93.502921	74.914113
284.246567	99.725674	74.919118
283.858248	102.039268	74.924122
283.059673	93.519052	74.929127
282.092486	100.549807	74.934132
281.878014	81.858853	74.939137
281.543011	90.759911	74.944142
280.244423	94.237225	74.949146
279.644135	85.529305	74.954151
278.864912	94.480664	74.959156
278.532508	93.303660	74.964161
277.625685	95.048652	74.969166
276.559168	100.073718	74.974170
276.517246	91.866546	74.979175
275.767323	92.131099	74.984180
275.383347	94.054519	74.989185
274.496524	107.360952	74.994190
273.777759	94.884313	74.999194
273.534003	92.286631	75.004199
272.416918	100.159665	75.009204
271.577427	108.217104	75.014209
271.008040	100.732620	75.019214
270.810210	103.605598	75.024218
270.314394	96.612407	75.029223
268.796057	104.721273	75.034228
268.344354	87.493600	75.039233
267.943222	88.377457	75.044238
267.138822	98.671579	75.049242
266.289760	91.753614	75.054247
265.243234	107.226866	75.059252
265.292569	87.473641	75.064257
265.012302	88.549532	75.069262
263.996569	94.287126	75.074266
263.494173	84.999097	75.079271
262.578430	93.033993	75.084276
262.184639	90.201622	75.089281
261.045141	92.813128	75.094286
260.173905	91.256838	75.099290
260.285669	83.939749	75.104295
259.592028	92.565255	75.109300
258.802241	94.326291	75.114305
258.050772	95.855730	75.119310
257.548617	92.387816	75.124314
256.260411	92.793360	75.129319
254.973951	95.491367	75.134324
255.246000	95.034832	75.139329
254.645770	91.333408	75.144334
253.967233	93.108251	75.149338
254.036315	91.406818	75.154343
252.447198	107.400190	75.159348
252.305520	90.435322	75.164353
251.322732	94.377945	75.169358
250.389976	92.643819	75.174362
249.979826	92.512048	75.179367
249.177761	93.281628	75.184372
248.764577	82.990700	75.189377
247.953664	95.947584	75.194382
247.380701	97.726100	75.199386
246.512484	90.502135	75.204391
246.035504	98.161195	75.209396
245.702958	83.792294	75.214401
244.863513	89.575907	75.219406
244.223381	100.890881	75.224410
243.803463	94.677179	75.229415
242.823253	92.349840	75.234420
241.898279	99.826435	75.239425
241.088572	91.337972	75.244430
240.378650	84.191277	75.249434
240.473019	90.906189	75.254439
239.388668	102.493807	75.259444
238.710362	90.507446	75.264449
238.179624	91.099750	75.269454
237.781019	114.122194	75.274458
237.155447	98.508547	75.279463
235.747969	105.272053	75.284468
235.479041	95.412259	75.289473
234.911931	90.863524	75.294478
234.210858	106.027846	75.299482
233.323058	90.479660	75.304487
232.300198	101.234362	75.309492
232.323188	94.324056	75.314497
231.908917	101.750787	75.319502
230.948931	87.365213	75.324506
230.660639	89.640792	75.329511
229.824677	102.589063	75.334516
228.915060	88.163923	75.339521
227.858454	98.443065	75.344526
227.423212	83.549681	75.349530
227.062005	94.232027	75.354535
225.929106	94.680636	75.359540
225.052748	96.318296	75.364545
224.440790	95.835523	75.369550
224.324879	89.073508	75.374554
223.882447	83.861550	75.379559
223.265914	98.928817	75.384564
222.501863	92.769976	75.389569
221.931997	97.402102	75.394574
221.143054	101.914619	75.399578
220.163811	98.377690	75.404583
219.469784	102.983881	75.409588
219.042649	90.607430	75.414593
218.394789	89.222116	75.419598
217.135133	99.828500	75.424602
216.836248	88.683627	75.429607
216.010454	93.736569	75.434612
215.780341	93.997124	75.439617
215.585560	97.293790	75.444622
214.439091	100.005770	75.449626
213.878347	81.031012	75.454631
213.300463	89.259628	75.459636
212.177884	87.778112	75.464641
211.328039	89.963447	75.469646
210.951039	95.126188	75.474650
210.805290	96.697849	75.479655
209.895254	97.864674	75.484660
208.765433	86.495893	75.489665
208.226717	93.207648	75.494670
207.721468	95.946717	75.499674
207.555835	91.989961	75.504679
206.153385	105.137343	75.509684
205.323610	90.499226	75.514689
205.357325	93.158688	75.519694
204.585799	93.565470	75.524698
204.303750	86.467267	75.529703
202.895877	95.588237	75.534708
202.954333	92.731090	75.539713
201.732529	104.001610	75.544718
200.790088	91.650542	75.549722
200.434472	95.198336	75.554727
199.806746	100.336398	75.559732
199.289230	99.575242	75.564737
198.883477	99.169983	75.569742
197.751035	94.373931	75.574746
197.192049	91.288804	75.579751
196.621061	95.326640	75.584756
195.583422	88.323658	75.589761
194.818915	90.478049	75.594766
194.181025	93.840621	75.599770
193.896882	102.246335	75.604775
193.833755	99.162580	75.609780
192.741192	99.177448	75.614785
191.814037	96.961513	75.619790
191.548477	94.431967	75.624794
190.927861	93.778706	75.629799
189.714393	104.882333	75.634804
189.201063	92.921727	75.639809
188.833309	91.546958	75.644814
187.717184	95.357906	75.649818
187.175929	86.374119	75.654823
186.096852	91.858504	75.659828
185.911611	90.602864	75.664833
185.447401	92.766152	75.669838
184.701662	100.999462	75.674842
184.014976	103.370095	75.679847
183.125029	96.509140	75.684852
182.811631	89.031187	75.689857
182.357428	93.260129	75.694862
180.955902	94.346054	75.699866
180.910888	87.187992	75.704871
180.219064	99.832613	75.709876
179.292556	90.621679	75.714881
178.624035	91.330571	75.719886
178.056981	87.068830	75.724890
177.657350	86.093357	75.729895
176.483486	89.009979	75.734900
175.403564	97.137303	75.739905
175.170055	96.502752	75.744910
174.759862	88.184003	75.749914
174.348106	93.300252	75.754919
173.028261	99.843250	75.759924
172.571309	95.992858	75.764929
172.186365	92.458973	75.769934
171.588240	97.205992	75.774938
170.997049	80.386930	75.779943
169.914481	92.592402	75.784948
169.355934	89.021543	75.789953
169.218179	83.467732	75.794958
168.369983	94.637698	75.799962
167.635557	84.645570	75.804967
166.947029	87.483246	75.809972
166.281217	94.016586	75.814977
165.128227	85.130332	75.819982
164.319339	83.494757	75.824986
164.461847	78.651578	75.829991
163.586373	85.711894	75.834996
162.766961	91.432416	75.840001
162.323826	75.308802	75.845006
161.391535	83.656998	75.850010
161.350591	76.488834	75.855015
159.782418	80.866987	75.860020
159.224011	83.296015	75.865025
159.078017	79.178451	75.870030
158.406855	80.357670	75.875034
157.756811	92.566724	75.880039
156.584986	82.828827	75.885044
156.250034	85.980694	75.890049
156.111583	83.960711	75.895054
154.942307	88.822441	75.900058
154.293181	83.687604	75.905063
153.861385	83.614490	75.910068
152.856061	79.790037	75.915073
151.486515	88.209526	75.920078
150.997551	85.039137	75.925082
150.827602	77.897847	75.930087
150.359063	84.347700	75.935092
150.002888	82.802370	75.940097
149.206604	86.795713	75.945102
148.345801	93.905734	75.950106
148.218985	89.020340	75.955111
146.764266	92.587262	75.960116
145.689825	91.547504	75.965121
145.346113	92.032743	75.970126
144.857243	89.983479	75.975130
145.018331	86.457156	75.980135
143.909682	91.791741	75.985140
142.872386	92.275605	75.990145
142.351319	89.859338	75.995150
141.783964	96.124691	76.000154
140.599107	90.370419	76.005159
139.905737	95.842210	76.010164
139.684951	85.858082	76.015169
139.212549	87.158571	76.020174
138.541308	93.525637	76.025178
137.971182	90.494338	76.030183
137.110148	94.378169	76.035188
136.754165	88.909612	76.040193
136.068834	83.458876	76.045198
134.859100	89.667385	76.050202
134.527178	80.935652	76.055207
133.837934	86.348440	76.060212
132.714528	92.062249	76.065217
132.270602	88.353285	76.070222
131.374068	101.837899	76.075226
131.424219	96.769758	76.080231
130.887530	89.824123	76.085236
129.926394	88.137145	76.090241
129.342613	77.584892	76.095246
128.363262	87.536371	76.100250
127.852236	87.199946	76.105255
126.734165	91.052226	76.110260
126.376381	83.439448	76.115265
126.088002	87.419622	76.120270
125.374600	85.261092	76.125274
124.570525	80.390651	76.130279
123.417176	84.893486	76.135284
123.084538	88.350897	76.140289
122.910021	83.271276	76.145294
121.828512	88.320862	76.150298
120.731233	77.951403	76.155303
120.201771	81.016022	76.160308
119.886506	80.282558	76.165313
119.758180	75.271265	76.170318
118.560708	80.329877	76.175322
117.854054	81.525803	76.180327
117.186189	86.629278	76.185332
116.927974	83.031049	76.190337
116.159224	88.617356	76.195342
115.105805	85.598472	76.200346
114.492695	79.032437	76.205351
114.161331	85.510882	76.210356
113.299669	86.893940	76.215361
112.847879	80.455138	76.220366
111.833321	97.239988	76.225370
111.508850	88.368305	76.230375
110.169659	83.395546	76.235380
109.620178	86.133800	76.240385
109.199275	78.381292	76.245390
108.614324	83.260250	76.250394
108.378984	81.892766	76.255399
107.586997	82.212960	76.260404
106.536243	88.776151	76.265409
106.342994	77.705928	76.270414
105.254302	91.386746	76.275418
104.796272	79.699618	76.280423
103.585921	99.563734	76.285428
103.241638	88.793533	76.290433
103.189328	79.217764	76.295438
102.131897	83.662738	76.300442
101.379406	86.862266	76.305447
100.757985	88.072990	76.310452
100.114099	91.378195	76.315457
99.491234	81.268968	76.320462
98.574127	80.798616	76.325466
98.221231	84.327063	76.330471
97.927387	85.622740	76.335476
96.670942	88.183583	76.340481
96.180878	89.447475	76.345486
95.513234	88.237227	76.350490
94.954228	93.214549	76.355495
93.876956	92.191034	76.360500
93.159976	94.489253	76.365505
92.566352	86.814746	76.370510
92.156474	89.472400	76.375514
91.843621	83.959132	76.380519
90.792696	92.200123	76.385524
90.071771	99.272089	76.390529
89.953550	86.365486	76.395534
88.809643	85.620664	76.400538
87.941233	92.566344	76.405543
87.046378	97.816404	76.410548
86.827638	93.470763	76.415553
86.853834	80.444950	76.420558
85.503237	88.221249	76.425562
84.806346	87.178083	76.430567
84.153096	92.504726	76.435572
83.546517	89.778855	76.440577
82.552758	82.759474	76.445582
81.596403	91.564090	76.450586
81.455976	81.601853	76.455591
81.027315	96.798434	76.460596
80.776594	91.784580	76.465601
79.755816	93.793801	76.470606
78.889201	88.282110	76.475610
78.580354	92.718107	76.480615
77.683650	102.093498	76.485620
76.810434	93.091718	76.490625
76.255681	85.601816	76.495630
75.610323	87.633170	76.500634
75.441492	91.234764	76.505639
73.877390	71.338360	76.510644
73.209609	97.533721	76.515649
73.255527	68.135534	76.520654
72.590173	110.315009	76.525658
72.306222	78.280876	76.530663
70.991727	93.003739	76.535668
70.324184	94.292784	76.540673
69.704583	91.739293	76.545678
68.680333	94.225279	76.550682
68.026385	87.217944	76.555687
67.984432	95.140365	76.560692
67.320132	91.537515	76.565697
66.659603	65.030392	76.570702
65.755356	121.581509	76.575706
65.481371	80.612934	76.580711
64.271036	89.938992	76.585716
63.074167	107.132956	76.590721
63.029963	69.333505	76.595726
62.130644	96.343170	76.600730
62.165118	78.139255	76.605735
61.595513	76.050849	76.610740
60.076219	103.979354	76.615745
59.670144	86.287199	76.620750
58.930325	81.709291	76.625754
58.552065	93.119710	76.630759
58.142138	87.412207	76.635764
57.060136	94.015092	76.640769
56.375103	108.399494	76.645774
55.782123	87.719057	76.650778
55.339238	92.655792	76.655783
54.412349	108.701338	76.660788
53.795376	101.052635	76.665793
53.573851	94.870415	76.670798
52.037174	94.003753	76.675802
52.075603	88.227906	76.680807
51.521071	85.476400	76.685812
50.383981	94.562143	76.690817
49.777568	95.507153	76.695822
48.870947	112.836180	76.700826
48.580651	80.672186	76.705831
48.003058	99.374194	76.710836
47.275151	114.922846	76.715841
46.746813	77.426076	76.720846
45.608993	109.789346	76.725850
45.610748	96.939298	76.730855
45.024580	91.807069	76.735860
43.643851	109.041399	76.740865
43.590718	94.610644	76.745870
42.381252	85.731889	76.750874
41.944657	95.943749	76.755879
41.108011	77.336325	76.760884
40.245400	115.272440	76.765889
40.419066	91.267166	76.770894
39.385431	103.408117	76.775898
38.584584	93.218485	76.780903
37.883293	97.993021	76.785908
37.504395	96.952768	76.790913
37.096786	100.114661	76.795918
35.548194	94.259190	76.800922
35.159108	91.471841	76.805927
34.834333	105.458191	76.810932
34.452825	113.297585	76.815937
33.848962	93.296931	76.820942
32.913245	88.557896	76.825946
32.277811	110.261996	76.830951
31.226381	102.794542	76.835956
30.135538	82.600350	76.840961
29.696933	100.830793	76.845966
29.280248	96.904632	76.850970
28.693754	102.201721	76.855975
28.395270	94.797108	76.860980
27.243591	88.222378	76.865985
27.014703	104.317445	76.870990
26.421775	100.957095	76.875994
25.520822	85.379587	76.880999
24.770594	105.462069	76.886004
24.398870	97.293326	76.891009
23.655349	85.118776	76.896014
22.443112	112.645125	76.901018
21.650926	96.861039	76.906023
21.334546	90.809063	76.911028
20.915420	91.848782	76.916033
20.593484	86.851028	76.921038
19.323778	110.624187	76.926042
18.787964	104.282372	76.931047
18.111938	100.407033	76.936052
17.431174	100.031474	76.941057
16.835825	99.177122	76.946062
15.771873	94.907946	76.951066
15.545318	102.585437	76.956071
15.010725	105.467985	76.961076
14.473539	98.776332	76.966081
13.756818	92.742477	76.971086
12.863501	93.969780	76.976090
12.433579	99.129944	76.981095
11.277262	89.971511	76.986100
10.533858	93.696281	76.991105
10.166444	93.794262	76.996110
9.650500	95.465970	77.001114
9.616025	96.994663	77.006119
8.553900	97.413162	77.011124
7.639423	98.831487	77.016129
7.194593	89.769303	77.021134
6.071653	98.868576	77.026139
5.591532	97.857088	77.031143
5.285188	87.710025	77.036148
4.519299	97.313709	77.041153
3.283840	93.988040	77.046158