Number of Data Points = 25
        
File	hc(nm)	Pmax(N)	S(N/nm)	A(nm^2)	hmax(nm)	heff(nm)	Er(GPa)	H(GPa)	A	hf(nm)	m	X(mm)	Y(mm)	Drift(nm/s)
3885_Position 113_00000.hld	3190.740164	539556.716946	1259.923476	247823368.641919	3537.377134	3511.924383	70.910063	2.177183	0.302232	2606.483526	2.114303	-132.079000	-53.018500	0.296573
3885_Position 113_00001.hld	3169.786187	572531.945922	1252.161247	244574815.511909	3535.481340	3512.712436	70.939679	2.340928	0.385053	2564.663184	2.073440	-132.029000	-53.018500	-0.019834
3885_Position 113_00002.hld	3138.091867	588096.977994	1168.917707	239701988.407690	3532.024123	3515.426158	66.893350	2.453451	0.704028	2521.438263	1.975678	-131.979000	-53.018500	-0.042701
3885_Position 113_00003.hld	3109.652239	607942.806773	1116.436039	235371399.026272	3531.049759	3518.056383	64.475071	2.582909	2.686895	2542.613891	1.791318	-131.929000	-53.018500	-0.102232
3885_Position 113_00004.hld	3079.548973	624103.420403	1064.041608	230830604.645025	3530.082964	3519.454294	62.050708	2.703729	10.452241	2577.516266	1.605922	-131.879000	-53.018500	-0.106126
3885_Position 113_00005.hld	3105.475392	647499.249130	1192.094643	234738711.358593	3528.134436	3512.846099	68.937131	2.758383	23.991003	2687.614723	1.519313	-132.079000	-52.968500	-0.102064
3885_Position 113_00006.hld	3082.823498	675619.878452	1174.477056	231322386.379090	3527.259061	3514.262245	68.418025	2.920685	23.313882	2641.464304	1.517245	-132.029000	-52.968500	-0.112067
3885_Position 113_00007.hld	3083.640519	657091.090838	1142.871254	231445171.739080	3527.799660	3514.851223	66.559197	2.839079	34.308479	2673.166233	1.463933	-131.979000	-52.968500	-0.083761
3885_Position 113_00008.hld	3070.604082	665982.010474	1122.529964	229489898.314870	3527.516191	3515.569048	65.652457	2.902010	43.977892	2668.522605	1.427719	-131.929000	-52.968500	-0.105890
3885_Position 113_00009.hld	3048.908830	690340.241740	1108.841270	226254367.348263	3527.922273	3515.842371	65.313916	3.051169	41.487648	2624.945551	1.430980	-131.879000	-52.968500	-0.079730
3885_Position 113_00010.hld	3087.536593	725735.147590	1283.431348	232031139.580903	3527.773999	3511.635133	74.650777	3.127749	36.383237	2679.072904	1.472350	-132.079000	-52.918500	-0.146968
3885_Position 113_00011.hld	3087.513177	692805.372427	1225.850866	232027615.600984	3526.131324	3511.385317	71.302150	2.985875	48.628805	2703.882526	1.428797	-132.029000	-52.918500	-0.105717
3885_Position 113_00012.hld	3086.394709	680137.668831	1201.813068	231859323.795101	3524.586431	3510.839463	69.929346	2.933407	55.962114	2714.085719	1.407875	-131.979000	-52.918500	-0.081915
3885_Position 113_00013.hld	3062.615461	720154.905413	1199.691600	228295832.644339	3526.476657	3512.827981	70.348599	3.154481	42.579185	2648.535065	1.439808	-131.929000	-52.918500	-0.075266
3885_Position 113_00014.hld	3073.490015	692042.210998	1180.319811	229922028.935004	3526.976886	3513.228172	68.967460	3.009900	38.568686	2662.000838	1.451820	-131.879000	-52.918500	-0.055143
3885_Position 113_00015.hld	3111.949210	718887.966176	1359.211556	235719696.588756	3526.082851	3508.624748	78.437537	3.049758	43.827540	2736.615553	1.459649	-132.079000	-52.868500	-0.110958
3885_Position 113_00016.hld	3101.130868	721665.305942	1326.915812	234081530.553033	3525.996197	3509.030883	76.841286	3.082966	42.079485	2714.905387	1.460147	-132.029000	-52.868500	-0.083468
3885_Position 113_00017.hld	3090.774040	725999.185387	1299.735930	232518615.314851	3525.952654	3509.704822	75.519845	3.122327	48.092214	2706.190231	1.438510	-131.979000	-52.868500	-0.058458
3885_Position 113_00018.hld	3099.381854	699051.396361	1278.401422	233817224.126437	3525.656262	3509.494467	74.073663	2.989734	42.651588	2714.851930	1.453215	-131.929000	-52.868500	-0.048723
3885_Position 113_00019.hld	3090.584828	706192.434839	1259.865041	232490110.725908	3527.127498	3510.982497	73.207675	3.037516	38.827626	2691.457610	1.462053	-131.879000	-52.868500	-0.049140
3885_Position 113_00020.hld	3139.251810	697062.180230	1422.043519	239879456.618981	3525.130222	3506.889388	81.348807	2.905885	54.828934	2800.711207	1.440641	-132.079000	-52.818500	-0.046859
3885_Position 113_00021.hld	3120.519580	731456.477120	1418.127014	237021529.736437	3525.157021	3507.362474	81.612383	3.086034	50.942457	2761.019560	1.446988	-132.029000	-52.818500	-0.047065
3885_Position 113_00022.hld	3120.769535	717798.266706	1390.667814	237059551.702629	3526.756108	3507.884772	80.025704	3.027924	48.971656	2759.689066	1.449560	-131.979000	-52.818500	-0.047409
3885_Position 113_00023.hld	3120.183277	717931.715876	1385.820480	236970377.810381	3526.023733	3508.724791	79.761768	3.029626	42.914717	2749.154212	1.466196	-131.929000	-52.818500	-0.047810
3885_Position 113_00024.hld	3127.553269	708326.261469	1392.389314	238092627.690654	3526.654460	3509.087867	79.950749	2.975003	47.418423	2769.002700	1.454819	-131.879000	-52.818500	-0.064015