Tue Jun 21 10:16:29 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.635039	85.470853	0.000000
1.146655	85.547333	0.005005
1.478418	88.404833	0.010010
1.462528	69.749492	0.015014
1.095277	83.073996	0.020019
1.083508	71.027350	0.025024
0.971048	72.269603	0.030029
0.442557	64.525002	0.035034
0.558040	44.566044	0.040038
-0.120220	43.029765	0.045043
-0.229634	46.244276	0.050048
-0.884059	39.122019	0.055053
-1.592136	41.168174	0.060058
-1.432302	34.807781	0.065062
-1.968268	43.540370	0.070067
-1.773647	36.678312	0.075072
-1.908448	30.811700	0.080077
-2.672918	36.384105	0.085082
-2.837338	31.702661	0.090086
-3.136542	47.314628	0.095091
-3.256493	42.241802	0.100096
-3.293884	34.641254	0.105101
-3.775219	35.943796	0.110106
-4.360590	33.284099	0.115110
-4.825805	38.920222	0.120115
-4.793844	36.756031	0.125120
-4.748925	35.681354	0.130125
-5.138921	39.472960	0.135130
-4.765368	30.717442	0.140134
-4.799952	37.497449	0.145139
-5.660199	41.549261	0.150144
-5.992795	37.242974	0.155149
-6.454948	43.708979	0.160154
-5.978079	37.596039	0.165158
-6.685061	28.535185	0.170163
-7.368465	43.672041	0.175168
-7.827093	36.609324	0.180173
-8.199446	40.182518	0.185178
-7.634565	34.836848	0.190182
-7.963318	37.564935	0.195187
-8.209978	30.117641	0.200192
-8.062228	38.524283	0.205197
-8.250386	32.713078	0.210202
-8.680171	30.461757	0.215206
-9.472322	40.272381	0.220211
-9.500093	32.073104	0.225216
-9.550909	28.110490	0.230221
-10.113982	38.917613	0.235226
-10.232749	34.948884	0.240230
-11.086374	38.644790	0.245235
-11.233221	30.319204	0.250240
-11.013031	37.386572	0.255245
-11.236746	39.996034	0.260250
-10.895989	27.262732	0.265254
-11.404456	42.239786	0.270259
-12.245265	29.577026	0.275264
-12.244994	32.217873	0.280269
-12.686290	36.822706	0.285274
-12.239687	28.513899	0.290278
-13.175433	25.418687	0.295283
-13.984124	27.230097	0.300288
-13.771159	28.375047	0.305293
-13.967778	32.500095	0.310298
-14.269931	29.317134	0.315302
-14.416746	32.350959	0.320307
-14.241922	30.408005	0.325312
-14.285901	31.346860	0.330317
-14.648097	36.096661	0.335322
-15.150927	34.999021	0.340326
-15.586988	37.704029	0.345331
-15.719964	38.404834	0.350336
-15.697644	38.798721	0.355341
-16.572813	29.399070	0.360346
-17.124420	34.271602	0.365350
-17.508466	28.446857	0.370355
-17.441052	29.904018	0.375360
-17.014835	30.138867	0.380365
-17.307373	33.758044	0.385370
-17.047912	25.805830	0.390374
-17.912502	31.707392	0.395379
-18.373880	36.564195	0.400384
-18.843258	30.092112	0.405389
-18.894567	34.749781	0.410394
-19.164782	25.752966	0.415398
-19.600472	44.053726	0.420403
-19.756865	38.798877	0.425408
-19.244151	39.196610	0.430413
-19.889248	38.284739	0.435418
-20.260948	39.461383	0.440422
-20.676190	37.386046	0.445427
-20.641621	34.478455	0.450432
-20.616971	31.181389	0.455437
-21.291285	44.188676	0.460442
-21.683425	37.147709	0.465446
-22.292056	37.374148	0.470451
-21.868441	40.571630	0.475456
-22.045481	27.091119	0.480461
-22.144679	44.239567	0.485466
-22.783300	29.837364	0.490470
-23.566165	36.754698	0.495475
-23.550909	40.301004	0.500480
-23.872667	30.387613	0.505485
-24.280962	38.357077	0.510490
-23.754874	28.588441	0.515494
-24.118520	36.366396	0.520499
-24.085776	34.617664	0.525504
-25.128470	30.476527	0.530509
-25.273154	39.931491	0.535514
-25.401339	27.440618	0.540518
-25.801388	34.807237	0.545523
-25.523188	31.209676	0.550528
-25.321351	32.488090	0.555533
-26.039525	37.453524	0.560538
-26.476905	34.890487	0.565542
-26.791749	36.512773	0.570547
-27.188402	38.898875	0.575552
-27.110250	28.739689	0.580557
-28.116280	35.565906	0.585562
-27.986433	28.348916	0.590566
-28.703088	35.042558	0.595571
-28.777992	40.121500	0.600576
-28.536967	29.721234	0.605581
-28.621704	34.761546	0.610586
-28.648518	31.862148	0.615590
-28.824826	35.111216	0.620595
-29.191944	40.135539	0.625600
-30.078241	35.491148	0.630605
-30.469079	38.875989	0.635610
-30.517437	42.760998	0.640614
-30.873174	42.913592	0.645619
-30.864327	34.969524	0.650624
-30.506396	35.346118	0.655629
-31.348210	42.011944	0.660634
-31.578356	33.204051	0.665638
-32.093680	40.027553	0.670643
-32.281553	28.201521	0.675648
-32.097000	34.295609	0.680653
-31.985504	41.710131	0.685658
-32.674216	25.524030	0.690662
-33.415692	41.104637	0.695667
-33.473095	33.480963	0.700672
-33.647160	30.128003	0.705677
-33.489204	32.673275	0.710682
-33.881655	27.912181	0.715686
-34.679593	34.613955	0.720691
-34.803165	39.556507	0.725696
-34.817823	31.892208	0.730701
-34.989947	36.842602	0.735706
-35.015465	36.157684	0.740710
-35.480125	39.949025	0.745715
-35.924731	33.434953	0.750720
-36.382923	33.212606	0.755725
-36.726276	40.474328	0.760730
-36.717509	32.812859	0.765734
-37.004270	34.471935	0.770739
-36.698730	26.521168	0.775744
-36.748057	36.857030	0.780749
-38.058232	36.113904	0.785754
-37.983194	29.541411	0.790758
-38.259106	35.804891	0.795763
-38.577363	33.797758	0.800768
-38.895209	33.576837	0.805773
-38.766721	38.846863	0.810778
-38.586471	32.981166	0.815782
-39.261581	30.433030	0.820787
-39.956748	35.151932	0.825792
-40.193549	30.019924	0.830797
-40.268624	27.977456	0.835802
-40.179269	30.867583	0.840806
-39.951714	31.698720	0.845811
-40.483990	34.532736	0.850816
-40.872831	34.925641	0.855821
-41.422788	42.389905	0.860826
-41.451333	33.124160	0.865830
-41.839427	36.242341	0.870835
-42.467089	39.713168	0.875840
-43.060439	37.771915	0.880845
-42.644940	42.268811	0.885850
-42.628339	30.765504	0.890854
-43.324613	42.963405	0.895859
-43.450274	32.612020	0.900864
-43.409685	37.277954	0.905869
-43.946238	38.578791	0.910874
-43.640032	37.309884	0.915878
-44.941228	44.881384	0.920883
-45.365714	32.488319	0.925888
-45.146038	37.378370	0.930893
-44.922008	29.569960	0.935898
-44.979127	36.938992	0.940902
-44.965948	38.008095	0.945907
-45.509477	39.766919	0.950912
-45.993280	38.559768	0.955917
-46.532838	41.693757	0.960922
-46.344784	31.219184	0.965926
-46.766086	33.439463	0.970931
-47.049058	35.485873	0.975936
-47.576059	39.673132	0.980941
-48.167441	46.981061	0.985946
-48.242429	29.555099	0.990950
-47.981112	35.744810	0.995955
-48.001204	32.783520	1.000960
-48.215651	29.450470	1.005965
-49.181885	41.361552	1.010970
-49.770239	40.396480	1.015974
-49.610594	43.411328	1.020979
-49.773470	40.150643	1.025984
-49.356389	25.685322	1.030989
-49.765135	47.755462	1.035994
-49.953297	33.184935	1.040998
-50.737187	38.944281	1.046003
-51.206002	34.962087	1.051008
-51.039200	39.015904	1.056013
-51.594341	50.045894	1.061018
-51.488710	32.121742	1.066022
-51.463423	46.158709	1.071027
-52.011860	36.273978	1.076032
-52.531993	32.167082	1.081037
-53.008834	39.228117	1.086042
-52.954431	39.179987	1.091046
-53.240881	44.422625	1.096051
-53.099918	41.855776	1.101056
-52.971000	44.048680	1.106061
-53.822085	41.315972	1.111066
-53.902741	34.407347	1.116070
-54.412615	43.027870	1.121075
-54.865380	45.735255	1.126080
-54.763079	36.224853	1.131085
-55.652160	41.292594	1.136090
-55.913873	37.164017	1.141094
-55.999289	48.390713	1.146099
-56.201431	46.340277	1.151104
-56.425638	35.809058	1.156109
-56.306812	40.763960	1.161114
-56.240718	30.709584	1.166118
-56.222164	31.502316	1.171123
-56.850802	33.637937	1.176128
-57.124731	36.780232	1.181133
-57.598801	32.917311	1.186138
-57.577504	30.998597	1.191142
-58.716571	38.284541	1.196147
-58.841783	30.320448	1.201152
-58.820084	30.845073	1.206157
-59.038557	35.236986	1.211162
-59.281495	35.267104	1.216166
-59.259457	37.846328	1.221171
-59.249069	31.097862	1.226176
-59.320292	29.653471	1.231181
-60.145581	33.487168	1.236186
-60.502431	41.357735	1.241190
-60.633885	49.758122	1.246195
-60.793023	25.593281	1.251200
-60.955402	22.077759	1.256205
-61.743206	31.272765	1.261210
-62.124369	22.671834	1.266214
-62.328620	32.178294	1.271219
-62.757458	33.508852	1.276224
-62.557633	32.954353	1.281229
-62.664633	30.319048	1.286234
-62.356429	27.259585	1.291238
-62.624494	29.880140	1.296243
-63.068968	33.867053	1.301248
-63.494806	25.838293	1.306253
-64.034696	34.855296	1.311258
-63.815935	32.263725	1.316262
-64.105339	25.949711	1.321267
-64.696415	27.096778	1.326272
-64.738460	28.335656	1.331277
-65.589418	33.363733	1.336282
-65.764987	25.270835	1.341286
-65.593194	25.113872	1.346291
-65.745146	24.271896	1.351296
-65.813917	24.415845	1.356301
-66.611033	29.928146	1.361306
-66.898058	26.118318	1.366310
-67.211968	31.410886	1.371315
-67.449111	34.882361	1.376320
-67.534502	38.692199	1.381325
-67.322710	37.178049	1.386330
-67.402969	28.876174	1.391334
-68.356703	30.034359	1.396339
-68.812621	27.296009	1.401344
-69.042082	33.582186	1.406349
-69.278352	32.040806	1.411354
-68.960906	26.039912	1.416358
-69.094888	32.016839	1.421363
-69.054947	33.481114	1.426368
-70.086174	28.585059	1.431373
-70.548373	35.209334	1.436378
-70.556315	29.899914	1.441382
-70.732301	30.795903	1.446387
-70.906301	26.596367	1.451392
-70.748496	27.552718	1.456397
-71.167477	29.715978	1.461402
-71.781197	26.510818	1.466406
-72.334728	26.849105	1.471411
-72.902543	41.445654	1.476416
-72.344795	33.268214	1.481421
-72.533842	40.469258	1.486426
-72.485781	29.308056	1.491430
-73.039474	34.230666	1.496435
-73.538245	37.831902	1.501440
-73.741839	29.340290	1.506445
-73.887350	46.208884	1.511450
-73.792111	38.068567	1.516454
-74.486056	42.425952	1.521459
-75.379799	36.240433	1.526464
-75.318608	36.494878	1.531469
-75.443405	33.219207	1.536474
-75.418216	33.910989	1.541478
-75.468216	37.250635	1.546483
-75.714514	32.291096	1.551488
-75.406358	30.875048	1.556493
-76.225533	29.249836	1.561498
-76.750364	31.565603	1.566502
-77.282841	35.674047	1.571507
-77.004192	38.817976	1.576512
-77.281622	33.663888	1.581517
-78.138645	41.550587	1.586522
-78.316706	37.252857	1.591526
-78.612597	39.359425	1.596531
-78.642742	33.169421	1.601536
-78.857169	28.898436	1.606541
-79.016320	37.857914	1.611546
-78.707119	27.462938	1.616550
-78.598372	30.806683	1.621555
-79.482088	32.421551	1.626560
-80.124420	35.520269	1.631565
-80.529285	34.311890	1.636570
-80.522989	31.837004	1.641574
-80.451648	31.803237	1.646579
-80.552116	30.205032	1.651584
-81.516743	28.385657	1.656589
-81.894971	32.744430	1.661594
-82.195234	32.170922	1.666598
-82.254207	36.586743	1.671603
-82.394042	33.303104	1.676608
-82.446982	31.627566	1.681613
-82.810413	37.974609	1.686618
-82.379379	24.249356	1.691622
-82.821451	36.392922	1.696627
-83.435686	36.435986	1.701632
-83.584513	27.832495	1.706637
-84.026147	33.857017	1.711642
-83.877019	30.281027	1.716646
-84.404778	33.535215	1.721651
-85.050071	31.833651	1.726656
-85.179118	24.733146	1.731661
-85.656145	31.886761	1.736666
-85.615516	25.076458	1.741670
-85.669651	35.329441	1.746675
-85.598810	29.787143	1.751680
-85.439613	39.050485	1.756685
-86.476469	33.516000	1.761690
-86.571778	30.369043	1.766694
-87.183444	29.269309	1.771699
-87.340688	37.437551	1.776704
-86.928949	33.503123	1.781709
-88.171252	44.803593	1.786714
-88.225942	22.020577	1.791718
-88.727693	32.287696	1.796723
-88.568290	36.739181	1.801728
-88.482435	27.553759	1.806733
-88.958377	34.201228	1.811738
-88.858544	34.824407	1.816742
-89.764560	38.032704	1.821747
-90.094137	38.224384	1.826752
-90.518285	29.499938	1.831757
-90.777579	35.593129	1.836762
-90.642716	27.772847	1.841766
-90.754786	34.289804	1.846771
-90.938546	33.509338	1.851776
-90.743306	28.775839	1.856781
-90.878841	23.161357	1.861786
-91.463327	30.193252	1.866790
-91.725985	36.568400	1.871795
-92.403917	32.983152	1.876800
-92.273195	24.691926	1.881805
-92.939741	42.875015	1.886810
-93.458081	29.971213	1.891814
-93.529656	45.296040	1.896819
-93.846628	40.046873	1.901824
-93.394216	31.780711	1.906829
-93.929664	39.342424	1.911834
-93.482461	41.376448	1.916838
-94.064060	30.077987	1.921843
-94.759598	37.449932	1.926848
-95.009818	31.407674	1.931853
-95.480239	43.042670	1.936858
-95.124337	33.451794	1.941862
-95.741802	33.315819	1.946867
-96.581028	34.921942	1.951872
-96.778435	28.016083	1.956877
-96.778979	38.149881	1.961882
-96.802704	31.229070	1.966886
-96.947609	30.829735	1.971891
-97.184569	30.067748	1.976896
-96.615256	32.349135	1.981901
-97.244720	35.631613	1.986906
-97.774873	28.925309	1.991910
-98.467765	32.791549	1.996915
-98.492792	35.865843	2.006912
-98.463258	37.101511	2.016909
-97.986454	37.427111	2.026906
-97.153371	39.359574	2.036902
-96.774060	34.207190	2.046899
-96.003952	38.968080	2.056896
-95.884047	35.742658	2.066893
-95.347228	39.028067	2.076890
-94.407623	36.158691	2.086886
-94.148732	39.209158	2.096883
-94.088833	34.950211	2.106880
-92.951619	32.978947	2.116877
-92.577324	33.351558	2.126874
-92.587025	35.038691	2.136870
-91.611156	38.334377	2.146867
-91.038906	35.541646	2.156864
-91.033687	42.112068	2.166861
-90.034801	36.429101	2.176858
-89.577366	31.251135	2.186854
-89.197168	34.909249	2.196851
-88.224299	34.902157	2.206848
-88.247752	38.454823	2.216845
-88.197726	41.279459	2.226842
-86.969222	38.661981	2.236838
-86.461233	35.674006	2.246835
-86.471358	34.466547	2.256832
-85.870616	39.009886	2.266829
-85.071299	32.385270	2.276826
-84.753367	32.654986	2.286822
-83.675348	31.400893	2.296819
-83.545821	25.987371	2.306816
-83.503912	33.555854	2.316813
-82.681869	37.689696	2.326810
-81.969753	35.238354	2.336806
-81.899191	34.924856	2.346803
-81.448700	32.262347	2.356800
-80.511530	36.089435	2.366797
-80.270783	35.795965	2.376794
-79.491415	40.625273	2.386790
-78.776326	33.044449	2.396787
-78.634434	34.143352	2.406784
-78.434293	37.338699	2.416781
-77.647499	34.466181	2.426778
-77.268526	35.839394	2.436774
-76.636121	40.850321	2.446771
-75.749572	37.170337	2.456768
-75.859862	43.190242	2.466765
-75.548169	39.915077	2.476762
-74.630407	33.968135	2.486758
-74.377434	30.596197	2.496755
-73.543003	42.232580	2.506752
-73.008199	33.724298	2.516749
-72.831457	36.690762	2.526746
-72.077319	32.529846	2.536742
-71.418722	36.148774	2.546739
-71.361930	33.876101	2.556736
-70.712048	37.520973	2.566733
-70.136273	39.620138	2.576730
-69.803101	37.581281	2.586726
-68.615727	38.150404	2.596723
-68.235869	35.801112	2.606720
-68.176703	30.897162	2.616717
-68.237039	38.558060	2.626714
-67.123397	34.290583	2.636710
-66.791058	32.397883	2.646707
-65.706286	32.816641	2.656704
-65.279449	36.312323	2.666701
-65.318982	38.821424	2.676698
-64.882436	40.309191	2.686694
-63.855234	35.200276	2.696691
-63.412126	35.273806	2.706688
-63.562918	36.888475	2.716685
-62.523230	39.886308	2.726682
-61.808544	39.453299	2.736678
-61.850916	39.830105	2.746675
-61.743679	41.202480	2.756672
-60.764880	35.658589	2.766669
-59.484039	38.931442	2.776666
-59.387602	42.841254	2.786662
-59.381951	45.383379	2.796659
-58.640312	34.360522	2.806656
-57.709435	40.834166	2.816653
-57.445954	40.551949	2.826650
-57.566450	39.830259	2.836646
-56.871840	31.899739	2.846643
-56.150094	40.582669	2.856640
-55.647697	35.751929	2.866637
-54.734682	43.585765	2.876634
-54.391488	37.018704	2.886630
-54.331060	38.892604	2.896627
-53.536191	39.867964	2.906624
-52.736021	41.822682	2.916621
-52.733403	43.493155	2.926618
-52.548592	43.913944	2.936614
-51.266713	40.078990	2.946611
-50.628054	39.776730	2.956608
-51.072355	33.122337	2.966605
-50.316091	36.975638	2.976602
-49.678425	30.627350	2.986598
-48.903765	33.471881	2.996595
-48.240188	30.001717	3.006592
-48.026668	35.009103	3.016589
-48.037242	40.588868	3.026586
-47.156866	36.671620	3.036582
-46.788063	33.133890	3.046579
-45.735162	33.308969	3.056576
-45.281193	35.326352	3.066573
-45.114554	40.137198	3.076570
-44.855918	34.683126	3.086566
-43.836980	26.676970	3.096563
-43.508236	32.065786	3.106560
-43.369792	33.286779	3.116557
-42.360853	43.016596	3.126554
-41.923757	41.024747	3.136550
-41.756797	36.026478	3.146547
-41.202466	36.351498	3.156544
-40.518851	32.955667	3.166541
-40.225016	36.252475	3.176538
-38.994066	34.781209	3.186534
-38.594579	33.343304	3.196531
-38.433813	35.644370	3.206528
-38.315516	38.934286	3.216525
-37.956489	29.492466	3.226522
-37.018440	37.166657	3.236518
-36.853140	31.797593	3.246515
-35.796079	29.136006	3.256512
-35.414799	30.368949	3.266509
-35.355275	29.442584	3.276506
-34.705361	35.172801	3.286502
-34.017225	30.916321	3.296499
-33.435287	29.490685	3.306496
-32.423154	28.840476	3.316493
-32.402336	31.079754	3.326490
-32.236342	29.649098	3.336486
-31.898658	34.231265	3.346483
-30.568914	32.238607	3.356480
-30.395625	31.980021	3.366477
-30.418336	27.483619	3.376474
-29.417243	27.827328	3.386470
-28.534119	23.425937	3.396467
-28.742164	28.601728	3.406464
-28.364105	31.682061	3.416461
-27.625272	29.450762	3.426458
-27.076715	24.601121	3.436454
-26.020596	30.211713	3.446451
-25.809133	34.840469	3.456448
-25.774280	31.093272	3.466445
-25.360398	32.335044	3.476442
-24.131868	30.991430	3.486438
-24.107436	31.455968	3.496435
-23.759674	31.083923	3.506432
-22.618210	31.891444	3.516429
-22.495670	28.608483	3.526426
-22.506234	34.976226	3.536422
-21.496072	36.120643	3.546419
-21.172145	31.343169	3.556416
-20.338429	37.376484	3.566413
-19.430700	34.684500	3.576410
-19.503451	32.347129	3.586406
-19.465838	30.853560	3.596403
-18.698777	23.703180	3.606400
-17.863550	31.324652	3.616397
-17.645100	38.086994	3.626394
-16.498781	35.459039	3.636390
-16.111143	32.913641	3.646387
-16.114564	27.815155	3.656384
-15.943658	30.867551	3.666381
-14.848784	35.437951	3.676378
-14.586767	29.270818	3.686374
-14.247435	26.100150	3.696371
-13.035765	30.478122	3.706368
-12.930848	26.083485	3.716365
-12.827461	30.760566	3.726362
-12.233158	28.078201	3.736358
-11.448074	30.338129	3.746355
-10.873624	32.009743	3.756352
-9.967345	35.770636	3.766349
-10.175289	35.935184	3.776346
-9.976448	33.664280	3.786342
-8.795744	35.144022	3.796339
-8.608196	28.273557	3.806336
-7.964453	31.924199	3.816333
-7.058638	34.964171	3.826330
-6.717205	28.150421	3.836326
-6.562957	32.171585	3.846323
-6.405259	34.019302	3.856320
-5.367658	34.262524	3.866317
-5.142027	37.730676	3.876314
-4.359433	44.294885	3.886310
-3.776583	45.335990	3.896307
-3.662905	36.361583	3.906304
-3.349115	48.922967	3.916301
-2.813691	52.666042	3.926298
-2.323259	67.162023	3.936294
-1.811458	78.876381	3.946291
-1.292776	84.028278	3.956288
-0.762145	94.078204	3.966285
-0.408026	107.789051	3.976282
0.000000	120.000409	3.981286
0.174554	128.769314	3.986291
0.684331	126.320563	3.991296
0.609397	127.570026	3.996301
0.289803	131.655078	4.001306
0.346624	134.234876	4.006310
0.398244	145.659975	4.011315
0.776726	151.143014	4.016320
0.794115	163.670592	4.021325
0.927887	158.892767	4.026330
1.138635	159.249536	4.031334
0.855030	159.726840	4.036339
0.952715	150.833017	4.041344
0.776539	162.511537	4.046349
1.009857	159.030506	4.051354
1.085902	158.026050	4.056358
1.050800	152.737065	4.061363
0.913528	138.079265	4.066368
0.866872	134.233745	4.071373
0.610096	143.538612	4.076378
1.219711	144.998554	4.081382
1.138291	151.096279	4.086387
1.130699	136.255389	4.091392
0.633342	143.176402	4.096397
0.851241	133.179502	4.101402
1.239389	149.400994	4.106406
0.737204	140.504287	4.111411
1.595062	144.466598	4.116416
1.022516	140.975745	4.121421
1.217119	132.702492	4.126426
0.902367	131.698219	4.131430
0.694308	133.692965	4.136435
1.398506	146.060034	4.141440
1.056993	152.831714	4.146445
1.357309	150.006788	4.151450
1.126574	144.111223	4.156454
0.880294	138.957655	4.161459
1.044160	136.935200	4.166464
1.077625	158.679689	4.171469
1.200443	158.290284	4.176474
1.457840	158.969670	4.181478
1.074105	159.354230	4.186483
1.296446	160.298525	4.191488
1.374176	161.720049	4.196493
1.496030	159.418409	4.201498
1.539445	142.632993	4.206502
0.743082	142.361652	4.211507
1.134144	145.813589	4.216512
1.312046	160.596788	4.221517
1.357549	161.691332	4.226522
1.517740	152.387748	4.231526
1.310688	161.691101	4.236531
1.763149	145.850683	4.241536
1.201879	150.170727	4.246541
1.387718	154.374560	4.251546
1.504394	149.637852	4.256550
1.382043	145.784537	4.261555
1.030786	136.155585	4.266560
1.020668	143.293502	4.271565
1.537233	147.911837	4.276570
1.770061	149.352670	4.281574
1.276107	160.754058	4.286579
1.675010	152.488210	4.291584
1.439381	152.239855	4.296589
1.649546	149.786248	4.301594
1.671287	149.776679	4.306598
1.499931	152.222974	4.311603
1.652136	154.537153	4.316608
1.653248	161.205333	4.321613
1.527115	157.459993	4.326618
1.586768	159.284512	4.331622
1.629157	154.976484	4.336627
1.983605	151.579000	4.341632
1.563231	147.236698	4.346637
0.976833	136.780372	4.351642
1.233277	145.328524	4.356646
1.531219	148.510729	4.361651
1.755842	164.151518	4.366656
1.615884	159.023949	4.371661
1.668763	158.420963	4.376666
1.802190	159.789455	4.381670
1.589098	154.469557	4.386675
1.993236	153.051028	4.391680
1.914952	157.769443	4.396685
1.634708	151.065098	4.401690
1.789903	153.185193	4.406694
1.660821	157.442555	4.411699
1.891229	155.963005	4.416704
1.797178	162.724102	4.421709
1.876123	156.361859	4.426714
2.020570	154.687760	4.431718
1.800285	171.832131	4.436723
1.892919	153.724287	4.441728
1.482619	155.482764	4.446733
1.881017	156.818431	4.451738
1.688981	153.328900	4.456742
1.558812	160.036184	4.461747
1.824447	153.858126	4.466752
1.973042	164.372060	4.471757
1.697615	162.737688	4.476762
2.110009	157.645743	4.481766
1.780306	155.197463	4.486771
1.936247	159.239893	4.491776
1.687970	158.396097	4.496781
1.704944	156.291796	4.501786
2.015470	164.985913	4.506790
2.072491	183.810289	4.511795
1.989677	178.524262	4.516800
2.315555	180.344957	4.521805
2.180075	172.768870	4.526810
2.093661	159.444522	4.531814
2.098593	157.112514	4.536819
2.203992	159.503907	4.541824
1.697324	158.680399	4.546829
1.896873	167.813814	4.551834
2.349476	167.343357	4.556838
2.004923	176.147136	4.561843
2.318124	170.990507	4.566848
2.284703	183.396470	4.571853
2.376834	186.613749	4.576858
2.205775	180.737297	4.581862
2.226891	176.052122	4.586867
2.346181	184.061779	4.591872
2.304853	175.838227	4.596877
2.323003	177.413476	4.601882
2.382800	171.951690	4.606886
2.247183	162.977892	4.611891
1.879823	156.059059	4.616896
2.028501	170.302850	4.621901
1.737667	175.787403	4.626906
2.074470	190.289359	4.631910
2.111423	180.725945	4.636915
2.266547	186.809577	4.641920
2.216875	187.373653	4.646925
2.302217	174.691996	4.651930
2.545212	179.846615	4.656934
2.250663	182.283713	4.661939
2.229159	186.913603	4.666944
2.230809	183.931316	4.671949
2.505311	182.151021	4.676954
2.545245	181.402569	4.681958
2.437491	174.227024	4.686963
2.528020	182.281108	4.691968
2.567111	181.365058	4.696973
2.298871	182.492611	4.701978
2.527522	192.031683	4.706982
2.661504	202.520238	4.711987
2.518228	180.571769	4.716992
2.451816	183.205528	4.721997
2.284201	198.294423	4.727002
2.852818	200.357120	4.732006
2.863424	213.845515	4.737011
2.751963	198.631430	4.742016
2.787964	187.779752	4.747021
2.482779	179.343745	4.752026
2.807779	175.266371	4.757030
2.482353	178.222053	4.762035
2.547852	177.774846	4.767040
2.479089	183.006348	4.772045
2.653333	200.603037	4.777050
2.782349	199.822074	4.782054
2.536528	211.960909	4.787059
2.914577	210.076636	4.792064
3.036987	208.219697	4.797069
2.741904	197.970052	4.802074
2.692786	190.624749	4.807078
2.429161	197.130170	4.812083
2.751741	204.269661	4.817088
2.505525	214.758821	4.822093
2.626247	218.189826	4.827098
2.684234	214.507128	4.832102
2.875545	214.757989	4.837107
2.928141	205.267550	4.842112
2.877903	213.274114	4.847117
2.899038	213.058427	4.852122
3.132164	214.211697	4.857126
2.754581	218.441747	4.862131
2.914824	212.594490	4.867136
2.638323	215.314942	4.872141
2.815825	217.533771	4.877146
3.217327	225.255769	4.882150
2.861617	217.548588	4.887155
2.559673	212.234305	4.892160
2.357843	218.923880	4.897165
3.046156	215.210612	4.902170
3.171088	215.316765	4.907174
3.085756	221.716895	4.912179
3.206171	213.082916	4.917184
2.826929	215.810316	4.922189
2.847677	208.630448	4.927194
3.163829	204.307268	4.932198
3.072761	208.474086	4.937203
3.033100	212.182858	4.942208
3.289570	218.768720	4.947213
2.928161	216.965055	4.952218
3.212864	226.556831	4.957222
3.157099	228.158138	4.962227
3.304641	223.403667	4.967232
3.019632	223.271629	4.972237
3.403204	226.996757	4.977242
3.196878	219.935195	4.982246
3.098633	231.122318	4.987251
3.315701	230.261059	4.992256
3.321945	233.972496	4.997261
3.480656	229.483764	5.002266
3.217258	212.510297	5.007270
3.172219	220.350043	5.012275
3.048283	218.093238	5.017280
3.156280	229.881834	5.022285
3.127553	239.994788	5.027290
3.120296	237.175388	5.032294
3.072597	239.566687	5.037299
3.260085	238.544561	5.042304
3.394587	243.106208	5.047309
3.320604	246.607940	5.052314
3.607291	235.524091	5.057318
3.588651	239.026721	5.062323
3.556669	236.560902	5.067328
3.673294	245.398865	5.072333
3.339620	238.357000	5.077338
3.920095	235.149799	5.082342
3.532724	249.067029	5.087347
3.548375	236.597948	5.092352
3.603330	243.774867	5.097357
3.772684	242.597281	5.102362
3.428734	223.335388	5.107366
2.957652	238.146004	5.112371
3.506828	229.509693	5.117376
3.484856	245.289473	5.122381
3.413710	237.906749	5.127386
3.525174	242.033528	5.132390
3.185835	236.668595	5.137395
3.721086	247.042191	5.142400
3.572002	240.800159	5.147405
3.785471	243.625179	5.152410
3.539448	237.273298	5.157414
3.359466	241.542269	5.162419
3.781080	237.749230	5.167424
3.680905	244.790808	5.172429
3.422547	241.545689	5.177434
3.720461	236.424130	5.182438
3.324497	241.352649	5.187443
3.503306	241.753387	5.192448
3.331804	245.543594	5.197453
3.558669	266.945995	5.202458
3.746861	265.339235	5.207462
3.701997	270.343422	5.212467
4.008439	277.200268	5.217472
4.057580	264.430796	5.222477
3.649384	280.181618	5.227482
4.245486	265.828314	5.232486
4.011984	269.901712	5.237491
3.668473	249.010489	5.242496
3.648005	249.179002	5.247501
3.540044	263.037940	5.252506
4.023048	260.045988	5.257510
3.820669	273.669556	5.262515
3.724978	270.384472	5.267520
3.717030	275.358077	5.272525
3.919376	266.282869	5.277530
4.038326	272.239519	5.282534
3.647387	271.320078	5.287539
3.933804	264.019429	5.292544
3.672157	277.324048	5.297549
3.805654	278.428500	5.302554
4.060240	271.968650	5.307558
4.007126	270.355471	5.312563
4.161831	276.917360	5.317568
4.029789	272.484061	5.322573
4.163655	279.937820	5.327578
4.154525	269.995395	5.332582
4.363573	275.505154	5.337587
4.371445	264.540861	5.342592
3.874772	270.733244	5.347597
3.814520	274.954968	5.352602
4.237307	272.278662	5.357606
3.976730	275.929899	5.362611
4.511607	276.913226	5.367616
3.984274	276.386971	5.372621
4.073116	278.002425	5.377626
4.335229	273.631143	5.382630
4.337726	276.916960	5.387635
4.287850	277.626511	5.392640
3.940301	269.599250	5.397645
3.930600	271.768177	5.402650
4.364225	275.963180	5.407654
4.010125	276.255216	5.412659
4.302247	283.765457	5.417664
4.394115	292.040987	5.422669
4.635612	291.598971	5.427674
4.434586	285.019587	5.432678
4.152330	278.784791	5.437683
4.147025	268.349176	5.442688
4.255064	276.380281	5.447693
4.468285	299.501635	5.452698
4.808837	288.092889	5.457702
4.241212	286.765795	5.462707
4.289082	277.368251	5.467712
4.688025	287.045343	5.472717
4.054772	288.126781	5.477722
4.328727	293.604683	5.482726
4.354665	299.445318	5.487731
4.666875	297.725664	5.492736
4.515674	308.022339	5.497741
4.513608	297.981043	5.502746
4.886460	298.515022	5.507750
4.634842	306.742649	5.512755
4.457821	288.851378	5.517760
4.479705	298.907444	5.522765
4.444601	300.528426	5.527770
4.789476	295.099117	5.532774
4.420682	300.786463	5.537779
4.527866	301.759899	5.542784
4.165404	298.816174	5.547789
4.258354	298.705618	5.552794
4.646524	294.986974	5.557798
4.334728	302.022967	5.562803
4.363437	293.545028	5.567808
4.628574	295.517682	5.572813
4.536037	295.002312	5.577818
4.375282	300.176466	5.582822
4.555321	301.285448	5.587827
4.856083	317.233670	5.592832
4.975837	324.382925	5.597837
4.593024	322.072867	5.602842
4.824742	316.367265	5.607846
4.735780	325.373506	5.612851
4.888212	325.742107	5.617856
4.787882	309.082731	5.622861
4.661317	321.892196	5.627866
4.905645	319.890732	5.632870
4.931922	326.181648	5.637875
5.145877	330.522958	5.642880
4.904928	317.604138	5.647885
4.683035	311.797031	5.652890
5.024483	307.384580	5.657894
4.446852	317.521380	5.662899
4.659199	327.028503	5.667904
4.922103	334.795411	5.672909
5.188003	336.737949	5.677914
5.317296	329.916772	5.682918
5.074138	337.372010	5.687923
5.182585	342.697757	5.692928
5.067577	319.200822	5.697933
4.476360	315.543505	5.702938
4.752993	318.572193	5.707942
4.818379	332.434458	5.712947
4.725825	327.126115	5.717952
4.876335	340.365896	5.722957
4.867363	334.040832	5.727962
4.941611	327.247321	5.732966
4.548154	336.885942	5.737971
5.023377	333.639711	5.742976
4.957604	326.629026	5.747981
4.817561	340.100641	5.752986
5.289734	352.401115	5.757990
5.155953	363.933248	5.762995
5.349728	357.887583	5.768000
5.159995	359.255927	5.773005
5.316952	370.118105	5.778010
5.555989	354.608627	5.783014
5.025613	349.691673	5.788019
5.159103	336.831804	5.793024
5.269006	351.357669	5.798029
5.210921	361.774927	5.803034
5.289167	357.918733	5.808038
5.305126	366.992087	5.813043
5.527929	359.373159	5.818048
5.094292	350.693300	5.823053
5.035728	356.856785	5.828058
5.511854	346.621820	5.833062
5.080875	361.866374	5.838067
5.244563	354.657837	5.843072
5.112888	360.750547	5.848077
4.847026	360.197371	5.853082
5.397244	358.666228	5.858086
5.311176	359.433479	5.863091
5.355568	358.035625	5.868096
5.272397	357.144547	5.873101
5.319846	355.614561	5.878106
5.366491	349.358231	5.883110
5.450846	354.560884	5.888115
5.345308	357.196218	5.893120
5.498831	359.928964	5.898125
5.399161	359.456806	5.903130
5.376319	357.599628	5.908134
5.578528	371.546231	5.913139
5.897162	374.073244	5.918144
5.212751	357.236821	5.923149
5.433994	373.186428	5.928154
5.677158	381.465765	5.933158
5.498206	391.238416	5.938163
5.572746	391.231156	5.943168
5.819360	389.303109	5.948173
5.660302	388.049254	5.953178
5.642162	380.354177	5.958182
5.693381	379.055242	5.963187
5.899240	380.082203	5.968192
5.743478	372.388605	5.973197
5.685531	356.893371	5.978202
5.850965	358.125548	5.983206
5.552651	357.903159	5.988211
5.691791	356.082702	5.993216
5.899236	374.304987	5.998221
5.541497	359.703611	6.003226
5.675053	354.454909	6.008230
5.392003	370.947226	6.013235
5.675069	373.547619	6.018240
6.073889	387.915365	6.023245
5.848012	387.017524	6.028250
6.240832	369.512127	6.033254
5.439569	362.492574	6.038259
5.628095	351.869896	6.043264
5.676561	352.493309	6.048269
5.460504	359.688910	6.053274
5.716124	354.878613	6.058278
5.496406	373.565716	6.063283
5.774653	376.560995	6.068288
6.014731	384.055037	6.073293
5.945996	383.298323	6.078298
5.643717	359.686502	6.083302
5.687493	354.403529	6.088307
5.560430	353.508272	6.093312
5.630401	352.071255	6.098317
5.487694	373.433764	6.103322
6.043554	376.530093	6.108326
5.438433	368.392295	6.113331
5.794245	372.418853	6.118336
5.657427	363.492696	6.123341
5.504383	381.399933	6.128346
5.932526	382.504149	6.133350
5.767910	383.727041	6.138355
5.743576	372.724590	6.143360
5.654063	370.518107	6.148365
5.606603	379.132892	6.153370
5.862095	383.352488	6.158374
5.604971	380.481686	6.163379
5.714032	387.930724	6.168384
5.769642	383.191821	6.173389
5.446433	395.308685	6.178394
5.910740	389.006860	6.183398
5.906677	394.039260	6.188403
5.748241	380.918856	6.193408
5.829259	360.815811	6.198413
5.403779	364.513910	6.203418
5.738313	373.470776	6.208422
5.736496	385.540926	6.213427
5.721148	381.487492	6.218432
5.551642	378.231184	6.223437
5.647354	392.572359	6.228442
5.922790	384.565811	6.233446
5.827407	397.518772	6.238451
5.611939	384.383930	6.243456
5.497572	383.851254	6.248461
5.484827	388.542310	6.253466
5.940589	396.634501	6.258470
5.863299	401.771976	6.263475
5.830254	392.401377	6.268480
5.687529	375.717770	6.273485
5.415352	382.322169	6.278490
6.079006	388.521385	6.283494
5.606145	385.613289	6.288499
5.425708	380.606412	6.293504
5.889585	386.684979	6.298509
5.856984	401.702578	6.303514
5.963922	387.467656	6.308518
5.366327	378.530366	6.313523
5.637576	382.167567	6.318528
5.996593	392.424215	6.323533
5.605804	382.434996	6.328538
5.858711	366.153979	6.333542
5.583734	370.413258	6.338547
5.531634	369.833369	6.343552
6.001385	376.328727	6.348557
5.507804	376.060525	6.353562
5.772952	378.340446	6.358566
5.639536	380.644330	6.363571
5.776837	382.092913	6.368576
5.898222	368.620308	6.373581
5.748853	370.515970	6.378586
5.849659	363.484593	6.383590
5.446745	359.015607	6.388595
5.628140	357.912390	6.393600
5.746233	366.775833	6.398605
5.471736	370.307244	6.403610
6.018111	377.173543	6.408614
5.506332	370.098553	6.413619
5.773302	373.152730	6.418624
5.628690	377.160128	6.423629
5.574026	387.051518	6.428634
5.763792	389.972253	6.433638
5.835287	397.951849	6.438643
5.679855	389.918762	6.443648
5.579949	387.716169	6.448653
5.695528	395.731286	6.453658
5.897432	388.774131	6.458662
5.517758	400.820228	6.463667
5.440375	398.708824	6.468672
5.793113	393.418685	6.473677
5.419227	395.249305	6.478682
5.910560	395.229272	6.483686
5.678634	393.214896	6.488691
5.700740	396.348894	6.493696
6.224317	397.757592	6.498701
5.829776	390.560760	6.503706
5.707961	368.861066	6.508710
5.509888	377.404290	6.513715
5.775062	379.162046	6.518720
5.979149	382.232755	6.523725
5.553660	386.424013	6.528730
5.596898	364.286922	6.533734
5.701813	384.121292	6.538739
5.732760	390.726021	6.543744
5.936401	383.547362	6.548749
5.807325	370.761727	6.553754
5.822977	367.448910	6.558758
5.593472	377.670780	6.563763
5.359504	365.578012	6.568768
5.769049	365.784254	6.573773
5.859718	379.090613	6.578778
5.814429	365.461294	6.583782
5.657639	363.180109	6.588787
5.604855	364.601556	6.593792
5.336066	375.548838	6.598797
5.564034	387.414780	6.603802
6.098825	394.643743	6.608806
5.857524	391.090878	6.613811
5.585975	376.822336	6.618816
5.702023	382.359175	6.623821
5.662035	390.255991	6.628826
5.957691	386.472722	6.633830
5.698620	380.607412	6.638835
5.451204	369.453443	6.643840
5.818219	372.410342	6.648845
5.709034	382.661035	6.653850
6.035232	379.831585	6.658854
5.677677	375.391591	6.663859
5.741987	369.037605	6.668864
5.965484	360.047643	6.673869
5.690717	359.168950	6.678874
5.509179	358.721202	6.683878
5.407472	362.461202	6.688883
5.543357	370.713303	6.693888
6.032296	374.481406	6.698893
5.641548	375.835281	6.703898
5.897214	359.551248	6.708902
5.740871	362.696632	6.713907
5.680211	357.415756	6.718912
5.962522	354.575817	6.723917
5.685199	357.731168	6.728922
5.738230	357.221294	6.733926
5.736716	362.888892	6.738931
5.718009	361.191860	6.743936
5.773556	353.977943	6.748941
5.614071	357.227450	6.753946
5.673855	351.946366	6.758950
5.790328	358.446933	6.763955
5.703776	368.138753	6.768960
5.823712	366.981378	6.773965
5.543171	364.570312	6.778970
5.771788	364.046953	6.783974
5.430682	365.529363	6.788979
5.726744	372.054072	6.793984
5.357509	365.874097	6.798989
5.436536	375.775904	6.803994
5.857928	393.213880	6.808998
5.958844	395.332340	6.814003
5.824304	392.431766	6.819008
5.672388	374.572944	6.824013
5.388049	378.558091	6.829018
6.048927	382.699509	6.834022
6.003126	364.705315	6.839027
5.682386	365.207916	6.844032
5.602792	364.197052	6.849037
5.245110	361.235552	6.854042
5.887515	369.268801	6.859046
6.019096	383.561008	6.864051
6.005956	369.895577	6.869056
5.502691	362.933242	6.874061
5.482661	360.509825	6.879066
5.475153	362.085987	6.884070
5.339172	381.610952	6.889075
5.606621	391.489068	6.894080
5.837451	388.898204	6.899085
5.441291	395.079518	6.904090
5.722939	393.886090	6.909094
5.616081	391.453365	6.914099
5.619518	402.632260	6.919104
5.875142	391.391427	6.924109
5.462419	408.209159	6.929114
5.648208	392.094140	6.934118
5.549850	397.505852	6.939123
5.841268	399.823855	6.944128
6.111787	392.360210	6.949133
5.608409	403.561062	6.954138
5.944928	389.591829	6.959142
5.797695	401.425187	6.964147
5.555629	393.569841	6.969152
5.812416	393.417947	6.974157
5.273016	397.671090	6.979162
5.867814	393.338621	6.984166
5.770703	388.345571	6.989171
5.775647	395.152935	6.994176
5.946368	382.271076	6.999181
5.651739	392.047292	7.004186
5.729729	391.632348	7.009190
5.479223	391.585371	7.014195
5.413799	394.165128	7.019200
6.205356	399.348378	7.024205
5.939225	394.860285	7.029210
6.142262	400.645978	7.034214
5.797411	382.901581	7.039219
5.611806	377.852146	7.044224
5.593480	368.832560	7.049229
5.349735	372.677977	7.054234
5.869698	379.882353	7.059238
5.927106	389.127449	7.064243
5.801118	384.192069	7.069248
5.720443	372.772101	7.074253
5.594045	369.261587	7.079258
5.615150	369.092081	7.084262
5.865641	370.286494	7.089267
5.880284	374.125832	7.094272
5.845932	366.735375	7.099277
5.809572	368.492935	7.104282
5.743676	361.667162	7.109286
5.820492	365.762216	7.114291
5.430687	368.901266	7.119296
5.563762	364.061331	7.124301
5.351405	375.610627	7.129306
5.728022	372.855910	7.134310
6.026406	386.305881	7.139315
5.610904	389.984377	7.144320
5.737035	365.464492	7.149325
5.070790	377.006852	7.154330
5.794932	384.410085	7.159334
5.527088	398.744764	7.164339
5.761219	400.951678	7.169344
6.076085	394.570796	7.174349
5.742561	399.984349	7.179354
5.680934	399.382159	7.184358
5.750692	398.429050	7.189363
5.924088	404.946654	7.194368
5.848446	392.968154	7.199373
5.365904	371.153738	7.204378
5.578034	379.386510	7.209382
5.542120	396.854430	7.214387
5.598080	396.243031	7.219392
5.785865	404.575557	7.224397
5.668369	400.268479	7.229402
5.730604	399.468173	7.234406
5.635659	391.835932	7.239411
5.524383	397.544215	7.244416
5.660009	396.710049	7.249421
5.624707	406.342690	7.254426
5.790281	401.419807	7.259430
5.638341	397.091003	7.264435
5.653295	402.224255	7.269440
5.763909	395.593616	7.274445
5.688490	398.216667	7.279450
6.088706	395.048755	7.284454
5.709945	404.745766	7.289459
5.539042	397.020720	7.294464
5.746723	397.857934	7.299469
5.625126	403.619434	7.304474
5.644229	393.792237	7.309478
5.336985	393.768075	7.314483
5.595216	402.673061	7.319488
5.889994	392.510325	7.324493
5.513382	399.593998	7.329498
5.786673	399.979687	7.334502
5.634666	393.503045	7.339507
5.444367	390.426402	7.344512
5.837414	388.321565	7.349517
5.599010	396.764323	7.354522
5.781717	395.921967	7.359526
5.706888	394.278823	7.364531
5.570256	388.283516	7.369536
5.885126	388.963066	7.374541
5.624567	396.275379	7.379546
5.969768	390.679428	7.384550
5.969144	397.408581	7.389555
5.603378	402.837736	7.394560
5.871233	391.218352	7.399565
5.484956	393.830123	7.404570
5.522849	395.693991	7.409574
5.696415	399.063597	7.414579
5.602127	403.448271	7.419584
5.808148	395.716660	7.424589
5.728248	407.700298	7.429594
5.902341	395.171306	7.434598
5.870113	392.755824	7.439603
5.624800	398.173123	7.444608
5.951626	396.803093	7.449613
5.598134	395.201355	7.454618
5.501909	398.024403	7.459622
5.486206	396.916719	7.464627
5.402651	395.643652	7.469632
5.760933	385.969083	7.474637
5.654061	396.409638	7.479642
5.838494	388.133593	7.484646
5.636590	391.233837	7.489651
5.650142	392.227322	7.494656
5.976928	396.861765	7.499661
6.131195	400.395399	7.504666
6.174368	395.063769	7.509670
6.139403	397.919692	7.514675
6.010257	391.985898	7.519680
6.111366	378.069864	7.524685
5.677307	372.915539	7.529690
5.699898	372.101670	7.534694
5.676406	368.820002	7.539699
5.560101	370.097648	7.544704
5.528529	362.994257	7.549709
5.398939	378.778376	7.554714
5.877922	387.994712	7.559718
6.092800	391.421807	7.564723
5.625200	375.561029	7.569728
5.754166	368.914930	7.574733
5.747909	375.022399	7.579738
5.841860	368.255208	7.584742
5.479973	370.540286	7.589747
5.364970	369.203161	7.594752
5.629978	376.515072	7.599757
5.616326	396.396323	7.604762
5.830725	392.356941	7.609766
5.801429	390.479515	7.614771
5.952794	404.514686	7.619776
6.210285	372.774465	7.624781
5.619954	371.944867	7.629786
5.662537	364.291840	7.634790
5.860084	352.371937	7.639795
5.643828	361.955972	7.644800
5.695882	361.964078	7.649805
5.438730	361.864328	7.654810
5.391174	361.790851	7.659814
5.768813	373.551682	7.664819
5.668185	375.976433	7.669824
5.603717	368.914995	7.674829
5.661539	381.548736	7.679834
5.607427	380.323287	7.684838
5.793136	382.643792	7.689843
6.155409	394.876261	7.694848
5.879693	365.715764	7.699853
5.457813	373.434263	7.704858
5.235562	356.922506	7.709862
5.605408	372.138069	7.714867
5.484776	388.645939	7.719872
5.979475	382.404405	7.724877
6.030779	393.988992	7.729882
5.882794	387.844994	7.734886
5.747005	382.016696	7.739891
5.576360	378.077583	7.744896
5.750935	382.167900	7.749901
5.950917	393.866204	7.754906
5.618974	372.628539	7.759910
5.573112	372.395922	7.764915
5.550837	382.370946	7.769920
5.952410	380.681283	7.774925
5.682678	382.454596	7.779930
5.888124	379.770057	7.784934
5.850977	366.334558	7.789939
5.796200	356.958699	7.794944
5.823859	360.674119	7.799949
5.382097	363.659163	7.804954
5.526127	358.605473	7.809958
5.860784	370.913538	7.814963
5.624619	369.216203	7.819968
5.581836	365.606002	7.824973
5.319056	366.323578	7.829978
5.819479	378.555853	7.834982
6.027165	392.078274	7.839987
5.272273	388.210838	7.844992
5.782535	386.339188	7.849997
5.496350	393.763491	7.855002
5.729557	391.106717	7.860006
5.859915	396.328210	7.865011
5.712695	391.594079	7.870016
5.845471	390.099691	7.875021
5.776548	382.559447	7.880026
5.594846	393.605200	7.885030
5.815215	391.283662	7.890035
5.746525	398.008299	7.895040
6.000900	389.142267	7.900045
5.658502	371.053909	7.905050
5.694011	357.575010	7.910054
5.915440	361.999553	7.915059
5.627950	359.513267	7.920064
5.471551	360.494437	7.925069
5.629130	377.002207	7.930074
6.110589	385.521127	7.935078
5.992342	369.178819	7.940083
5.606038	365.404084	7.945088
5.693488	361.740943	7.950093
5.567646	357.548926	7.955098
5.465431	358.522900	7.960102
5.632311	364.312791	7.965107
5.807837	384.793203	7.970112
5.813004	361.702953	7.975117
5.470198	359.814886	7.980122
5.824202	380.194238	7.985139
5.723934	371.389175	7.990157
5.833850	382.858100	7.995174
5.626134	358.512298	8.000192
5.620255	373.177130	8.005210
5.727565	374.653890	8.010227
5.734126	379.283331	8.015245
5.756200	388.288045	8.020262
6.184783	380.969705	8.025280
5.847419	370.711488	8.030298
5.551246	355.888321	8.035315
5.521686	360.606015	8.040333
5.632614	377.753101	8.045350
5.800926	367.561930	8.050368
5.589398	387.288422	8.055386
5.539391	379.402328	8.060403
5.782792	382.986719	8.065421
5.827033	376.512676	8.070438
6.213299	373.062293	8.075456
6.007806	382.681023	8.080474
6.036967	367.328221	8.085491
5.657913	358.226833	8.090509
5.638608	365.994972	8.095526
5.887526	370.674037	8.100544
5.892798	382.222490	8.105562
5.829963	376.148040	8.110579
6.003940	368.109518	8.115597
5.641006	369.193901	8.120614
5.507834	368.742905	8.125632
5.851645	387.955621	8.130650
5.761667	381.827006	8.135667
5.940913	383.430822	8.140685
5.715845	379.605519	8.145702
5.991030	379.898264	8.150720
5.872546	388.277283	8.155738
5.686156	390.745918	8.160755
6.273925	373.775130	8.165773
6.163165	389.519276	8.170790
6.083583	381.097763	8.175808
5.645527	382.396146	8.180826
5.933875	388.543189	8.185843
6.230990	388.458315	8.190861
5.903920	388.881688	8.195878
6.176395	376.936968	8.200896
5.675078	369.612780	8.205914
5.379487	375.860249	8.210931
5.900849	379.388771	8.215949
6.022186	383.969485	8.220966
6.065237	383.464311	8.225984
5.888095	388.903645	8.231002
6.036138	391.317690	8.236019
6.160749	385.008670	8.241037
6.085210	383.600559	8.246054
6.118480	385.096666	8.251072
5.954802	384.077140	8.256090
5.977629	400.273159	8.261107
6.220788	390.606354	8.266125
5.917234	393.053250	8.271142
6.035130	387.144919	8.276160
5.889832	388.881604	8.281178
5.927986	382.336721	8.286195
6.114877	379.888573	8.291213
6.055049	394.574169	8.296230
6.136904	384.147124	8.301248
6.001942	384.003882	8.306266
5.932075	389.063668	8.311283
6.148672	387.593799	8.316301
5.908570	386.999693	8.321318
5.805828	383.864122	8.326336
6.001345	392.862756	8.331354
6.192690	381.262546	8.336371
5.933112	378.770619	8.341389
5.817949	382.438789	8.346406
5.878145	383.837334	8.351424
6.074345	377.539886	8.356442
5.782842	377.912295	8.361459
6.063430	375.948597	8.366477
5.758845	391.335498	8.371494
5.899686	379.824551	8.376512
5.690670	390.935889	8.381530
6.117373	390.953564	8.386547
6.178012	401.133904	8.391565
5.878798	405.979720	8.396582
6.143979	409.252658	8.401600
6.222934	416.839603	8.406618
6.019690	420.646768	8.411635
6.590480	408.414849	8.416653
6.342239	409.734949	8.421670
6.395359	394.134077	8.426688
6.313118	389.580445	8.431706
5.927979	384.569920	8.436723
6.061553	367.245046	8.441741
6.167319	385.002400	8.446758
5.903370	388.813508	8.451776
6.237985	397.446419	8.456794
6.276777	407.719942	8.461811
6.576831	409.271081	8.466829
6.167115	397.592839	8.471846
5.968777	391.884103	8.476864
6.313700	389.226138	8.481882
6.355852	410.752650	8.486899
6.295964	396.207030	8.491917
5.837440	398.232572	8.496934
6.479638	406.473833	8.501952
6.654049	402.425694	8.506970
6.043934	399.869965	8.511987
6.249358	393.217268	8.517005
5.952823	387.113406	8.522022
6.545218	402.393520	8.527040
6.685871	412.319100	8.532058
6.356936	400.183415	8.537075
5.942125	383.727816	8.542093
6.138053	396.910735	8.547110
6.182334	407.040641	8.552128
6.597690	412.553714	8.557146
6.205396	410.210914	8.562163
6.596347	403.829636	8.567181
6.105863	396.594777	8.572199
6.494451	392.832413	8.577216
6.641510	402.185312	8.582234
6.393048	401.116441	8.587251
6.653194	386.703848	8.592269
6.236613	387.509144	8.597287
6.127427	382.761565	8.602304
6.683483	389.167605	8.607322
6.256160	392.789442	8.612339
6.478169	389.529432	8.617357
6.008555	390.250602	8.622375
6.368357	388.282842	8.627392
6.594214	376.949735	8.632410
6.037862	386.833439	8.637427
6.504885	391.136459	8.642445
6.660447	405.392530	8.647463
6.378660	386.074744	8.652480
6.568588	384.795105	8.657498
6.115028	378.977464	8.662515
6.484311	397.576176	8.667533
6.657421	402.068997	8.672551
6.499766	393.204925	8.677568
6.519473	383.203103	8.682586
6.127719	375.716095	8.687603
6.246977	399.630047	8.692621
6.538120	397.859861	8.697639
6.433662	408.380907	8.702656
6.602033	408.517337	8.707674
6.383543	411.227494	8.712691
6.721492	411.285847	8.717709
6.827870	416.420782	8.722727
6.257112	402.622695	8.727744
6.609778	395.602727	8.732762
6.502286	402.388706	8.737779
6.395462	387.812285	8.742797
6.602895	413.048572	8.747815
6.578595	404.348422	8.752832
6.858263	401.377070	8.757850
6.290428	398.051598	8.762867
6.351304	397.137398	8.767885
6.429040	406.090586	8.772903
6.481838	400.591426	8.777920
7.026027	405.912506	8.782938
6.683424	408.716438	8.787955
6.776311	386.382288	8.792973
6.289485	385.138730	8.797991
6.381439	402.032704	8.803008
6.838186	404.121047	8.808026
6.655298	413.459694	8.813043
6.729711	404.534355	8.818061
6.494135	391.952342	8.823079
6.546392	410.988380	8.828096
6.504301	398.478450	8.833114
6.616429	410.124183	8.838131
7.020215	404.967861	8.843149
6.666329	396.346304	8.848167
6.282533	399.233427	8.853184
6.998340	397.217148	8.858202
6.528871	408.773764	8.863219
6.556152	396.590711	8.868237
6.676277	401.886543	8.873255
6.619012	410.125327	8.878272
6.972046	412.323752	8.883290
6.742507	410.945272	8.888307
6.738685	404.226635	8.893325
6.753277	410.467045	8.898343
6.986870	418.339190	8.903360
6.887837	393.400966	8.908378
6.369563	387.088168	8.913395
6.502804	390.619546	8.918413
6.423531	399.193639	8.923431
6.553968	407.614122	8.928448
6.690308	404.846214	8.933466
6.526858	408.287757	8.938483
6.738401	403.260308	8.943501
6.409131	395.798375	8.948519
6.377431	406.962838	8.953536
6.664382	408.499810	8.958554
6.675350	410.136808	8.963571
6.932192	404.574925	8.968589
6.869877	399.314104	8.973607
6.766146	402.484161	8.978624
6.804229	404.058798	8.983642
6.417302	402.556194	8.988659
6.522527	412.642157	8.993677
7.156819	422.611979	8.998695
6.619746	423.150043	9.003712
7.057477	423.446581	9.008730
6.784791	423.826897	9.013747
6.777056	424.640475	9.018765
6.813798	421.997316	9.023783
6.951609	427.576232	9.028800
6.899533	430.836554	9.033818
6.957816	431.128605	9.038835
6.871905	418.995968	9.043853
6.611953	413.223023	9.048871
6.730758	431.895532	9.053888
6.838852	424.495997	9.058906
7.030474	433.629149	9.063923
7.250083	442.181332	9.068941
7.137205	433.892854	9.073959
6.890767	430.555885	9.078976
6.794426	413.396975	9.083994
6.735134	420.539522	9.089011
6.985128	424.393088	9.094029
7.429471	435.183688	9.099047
6.793667	420.750532	9.104064
7.170378	406.144223	9.109082
6.801814	409.344552	9.114099
6.782742	409.548630	9.119117
7.019840	430.056540	9.124135
6.978474	434.395725	9.129152
7.215042	431.672039	9.134170
6.963353	434.689645	9.139187
6.566524	439.856340	9.144205
7.066285	433.818623	9.149223
7.120375	441.584489	9.154240
7.077093	438.249507	9.159258
7.167824	438.249590	9.164275
7.220099	432.582604	9.169293
7.228921	435.068131	9.174311
6.726485	433.920257	9.179328
7.183737	431.079917	9.184346
7.362337	435.107304	9.189363
6.809530	419.104409	9.194381
6.996982	429.748776	9.199399
7.105100	438.977051	9.204416
7.325434	439.057833	9.209434
7.131003	440.246790	9.214451
7.108197	437.776077	9.219469
7.321862	444.275643	9.224487
7.109997	423.008174	9.229504
6.908147	412.523960	9.234522
6.865238	416.475430	9.239539
7.029049	432.335758	9.244557
7.318947	425.080714	9.249575
7.320978	433.209305	9.254592
7.183462	434.530561	9.259610
7.229918	427.585099	9.264627
6.885479	427.721014	9.269645
7.382421	432.204315	9.274663
7.100023	436.563531	9.279680
7.347904	428.717648	9.284698
7.063478	433.265375	9.289715
6.986783	442.100464	9.294733
7.097501	429.283926	9.299751
6.925758	444.487673	9.304768
7.159538	437.655667	9.309786
7.270361	437.178243	9.314803
7.038637	440.070505	9.319821
7.201015	424.131257	9.324839
7.094972	439.616029	9.329856
7.319483	429.203322	9.334874
7.111308	433.269163	9.339891
7.148409	443.382173	9.344909
7.508607	430.242060	9.349927
7.145939	432.361176	9.354944
7.404571	430.818599	9.359962
7.388170	432.743379	9.364979
7.224357	430.963687	9.369997
7.368711	426.470942	9.375015
7.191561	429.036078	9.380032
7.331788	429.513759	9.385050
7.377825	426.888351	9.390067
7.230681	437.029306	9.395085
7.242638	428.355224	9.400103
7.249328	432.788018	9.405120
7.199256	431.570359	9.410138
7.217224	429.812925	9.415155
7.249601	427.053370	9.420173
7.472091	425.951394	9.425191
7.182133	433.752967	9.430208
7.241150	434.535021	9.435226
7.399143	447.354013	9.440243
7.422028	456.732230	9.445261
7.744357	451.457303	9.450279
7.588914	439.721374	9.455296
7.543904	434.037821	9.460314
7.369535	440.240442	9.465331
7.441371	435.059160	9.470349
7.463564	431.868052	9.475367
7.452008	433.822540	9.480384
7.620474	429.810415	9.485402
7.334639	437.775272	9.490419
7.345819	440.693058	9.495437
7.584061	426.140561	9.500455
7.258023	436.852636	9.505472
7.421308	439.088587	9.510490
7.523011	443.135401	9.515507
7.493279	446.671732	9.520525
7.729916	445.767990	9.525543
7.241149	444.095840	9.530560
7.659693	454.238209	9.535578
7.534365	445.104205	9.540595
7.364659	444.081342	9.545613
7.839897	448.923139	9.550631
7.463171	449.105737	9.555648
7.407472	456.893529	9.560666
7.603748	447.920823	9.565683
7.600387	460.693518	9.570701
7.997548	457.086796	9.575719
7.647185	441.199953	9.580736
7.530277	434.210284	9.585754
7.317465	437.129530	9.590771
7.453261	445.923138	9.595789
7.846306	449.355215	9.600807
7.658730	453.135386	9.605824
7.662299	448.837195	9.610842
7.830553	443.545266	9.615859
7.395447	439.405143	9.620877
7.301148	441.742797	9.625895
7.519749	456.789604	9.630912
7.664644	451.477329	9.635930
8.117533	456.372235	9.640947
7.861200	459.214446	9.645965
7.545842	450.698480	9.650983
7.533593	450.498897	9.656000
7.581458	461.448073	9.661018
7.675207	460.400875	9.666035
7.664105	473.526217	9.671053
7.836316	459.673357	9.676071
7.842404	464.058429	9.681088
7.630972	463.123965	9.686106
7.929036	452.151067	9.691123
7.664036	461.876740	9.696141
7.471852	456.935415	9.701159
7.797345	457.763300	9.706176
7.605306	460.614155	9.711194
7.882955	458.940876	9.716211
7.838389	464.121489	9.721229
8.240893	467.163053	9.726247
8.005570	468.776472	9.731264
7.773844	462.056180	9.736282
8.185936	460.824781	9.741299
7.661758	447.909040	9.746317
7.830826	437.056718	9.751335
7.445841	431.644604	9.756352
7.785198	443.353517	9.761370
7.718435	454.606296	9.766387
7.775563	463.698551	9.771405
7.909186	461.844212	9.776423
8.049461	461.448912	9.781440
7.861990	457.538628	9.786458
7.832474	460.427332	9.791475
7.728688	465.120539	9.796493
7.867109	460.163640	9.801511
7.689117	463.683189	9.806528
7.617760	461.546867	9.811546
7.760325	463.288843	9.816563
7.814488	464.696465	9.821581
7.830252	461.950678	9.826599
7.659303	465.695424	9.831616
7.617639	464.076986	9.836634
7.716421	462.775230	9.841651
7.722114	471.443555	9.846669
8.051683	484.523322	9.851687
8.259101	491.678823	9.856704
8.165123	475.743980	9.861722
7.925942	467.018159	9.866739
7.850183	464.980197	9.871757
8.212163	465.326285	9.876775
8.276853	460.558552	9.881792
7.902538	465.738849	9.886810
8.129524	453.821089	9.891827
7.917228	470.539154	9.896845
7.966381	466.557799	9.901863
8.116160	457.370163	9.906880
7.937819	456.931762	9.911898
7.812383	455.971838	9.916915
8.041688	469.223697	9.921933
8.326399	481.849897	9.926951
8.212572	468.267410	9.931968
7.967937	467.805341	9.936986
8.171876	462.445493	9.942003
8.039003	462.498349	9.947021
8.024678	469.130159	9.952039
7.976801	472.436051	9.957056
8.363236	486.526417	9.962074
8.513091	481.231223	9.967091
8.159942	471.004684	9.972109
8.068927	454.907768	9.977127
8.464374	452.298706	9.982144
8.306192	458.169739	9.987162
8.207234	450.741291	9.992179
8.029305	456.248295	9.997197
8.172005	451.858566	10.002215
8.093181	457.829246	10.007232
8.111158	457.660286	10.012250
8.245722	455.183195	10.017267
7.901579	464.642466	10.022285
7.954941	484.568510	10.027303
8.448487	490.517257	10.032320
8.369415	489.011697	10.037338
8.512123	480.604893	10.042355
8.081971	469.115597	10.047373
8.176626	458.683627	10.052391
8.437086	466.874555	10.057408
8.361074	471.788151	10.062426
8.214769	467.676179	10.067443
8.052404	469.471994	10.072461
8.281864	484.089499	10.077479
8.547495	487.329310	10.082496
8.510254	493.269497	10.087514
8.612613	471.325758	10.092531
8.243489	464.473107	10.097549
8.058152	464.699599	10.102567
8.321438	472.292858	10.107584
8.195308	486.646038	10.112602
8.800219	485.700406	10.117619
8.212012	471.409509	10.122637
8.240081	468.287101	10.127655
8.244846	466.183053	10.132672
8.355287	490.322016	10.137690
8.538720	493.597879	10.142707
8.218795	502.737040	10.147725
8.425480	493.856673	10.152743
8.451931	496.392437	10.157760
8.802654	496.171134	10.162778
8.551442	485.001388	10.167795
8.381033	480.236359	10.172813
8.198236	488.470579	10.177831
8.603734	484.413680	10.182848
8.385683	494.307572	10.187866
8.531553	489.282309	10.192883
8.414431	490.306117	10.197901
8.303780	486.333109	10.202919
8.561217	489.329017	10.207936
8.243705	491.926853	10.212954
8.560170	486.405656	10.217971
8.609217	494.122386	10.222989
8.596908	490.969261	10.228007
8.488522	480.999805	10.233024
8.206168	494.103745	10.238042
8.520045	495.387662	10.243059
8.902217	496.069362	10.248077
8.580774	497.571462	10.253095
8.565875	488.888014	10.258112
8.330778	495.284560	10.263130
8.247904	488.644522	10.268147
8.379485	488.763424	10.273165
8.545757	490.481991	10.278183
8.596496	488.423867	10.283200
8.112482	496.210362	10.288218
8.674089	486.208305	10.293235
8.506732	493.962837	10.298253
8.675952	501.468739	10.303271
8.403629	495.366730	10.308288
8.844422	510.421283	10.313306
9.144270	501.236921	10.318323
8.877800	501.808717	10.323341
8.523672	485.212261	10.328359
8.790666	479.498090	10.333376
8.200972	492.134448	10.338394
8.801658	489.900228	10.343411
8.738384	501.312886	10.348429
8.917960	505.467681	10.353447
8.977896	502.134490	10.358464
8.853269	495.300983	10.363482
8.705142	488.821347	10.368499
8.643605	486.866455	10.373517
8.390710	487.221843	10.378535
8.727801	490.990339	10.383552
8.545965	508.184079	10.388570
8.955184	502.657360	10.393587
8.919524	511.007771	10.398605
8.906240	509.171256	10.403623
9.072215	506.692499	10.408640
8.847218	505.157560	10.413658
8.570974	497.143721	10.418675
8.959410	512.049869	10.423693
8.948248	508.760731	10.428711
9.145564	504.143060	10.433728
8.560801	499.853303	10.438746
8.356273	502.396214	10.443763
8.710221	501.455132	10.448781
8.616860	509.101362	10.453799
8.614331	500.262325	10.458816
8.643356	508.671311	10.463834
8.884588	501.769740	10.468851
8.619521	509.029861	10.473869
9.056204	510.603267	10.478887
8.967457	510.456308	10.483904
8.937822	516.569644	10.488922
9.003991	516.290348	10.493939
9.368059	513.638640	10.498957
8.958241	510.434803	10.503975
9.127191	511.301014	10.508992
8.813598	509.881919	10.514010
8.783747	513.437181	10.519027
9.105471	505.878226	10.524045
8.841568	507.368044	10.529063
8.969924	497.472362	10.534080
8.983308	509.229396	10.539098
8.813911	510.620106	10.544115
8.818505	520.313773	10.549133
9.065901	536.120803	10.554151
9.506077	535.449282	10.559168
9.533128	528.581589	10.564186
9.020283	515.952872	10.569203
8.808204	514.713019	10.574221
8.977033	518.486943	10.579239
9.208731	508.083622	10.584256
8.919651	505.417633	10.589274
8.963367	527.461142	10.594291
9.541275	537.470493	10.599309
9.099720	534.761640	10.604327
9.065654	516.500440	10.609344
9.165476	528.686850	10.614362
9.037630	527.852313	10.619379
9.209704	541.450697	10.624397
9.233200	543.977116	10.629415
9.421974	528.587490	10.634432
9.455624	538.161797	10.639450
9.158245	523.872691	10.644467
9.197804	507.186615	10.649485
8.994886	510.655581	10.654503
9.149627	519.430346	10.659520
9.231714	538.778314	10.664538
9.232791	536.333943	10.669555
9.472086	541.983099	10.674573
9.385078	549.776319	10.679591
9.357198	527.913117	10.684608
9.229388	525.580635	10.689626
9.499901	524.790760	10.694643
9.231692	516.458670	10.699661
9.198372	527.995120	10.704679
9.313569	535.313539	10.709696
9.674693	532.795379	10.714714
9.112378	525.736318	10.719731
9.423345	519.576296	10.724749
9.284884	539.310368	10.729767
9.384875	536.340201	10.734784
9.407907	533.959907	10.739802
9.448262	541.707626	10.744819
9.557987	534.082586	10.749837
9.269646	532.698282	10.754855
9.427058	528.933616	10.759872
9.141959	532.892543	10.764890
9.087809	534.487781	10.769907
9.459397	532.138743	10.774925
9.270564	545.832323	10.779943
9.301599	535.812582	10.784960
9.695923	539.718061	10.789978
9.377002	543.966039	10.794995
9.590208	539.470916	10.800013
9.498114	542.151112	10.805031
9.310158	539.453413	10.810048
9.414671	546.135063	10.815066
9.328447	546.010913	10.820083
9.517349	535.715441	10.825101
9.750319	534.925090	10.830119
9.386782	533.223729	10.835136
9.643767	541.713483	10.840154
9.251849	542.634379	10.845171
9.453698	539.962681	10.850189
9.061067	533.952226	10.855207
9.214714	534.770187	10.860224
9.267674	545.691219	10.865242
9.814400	551.831960	10.870259
10.054371	560.464297	10.875277
9.617291	560.746648	10.880295
9.810783	549.106392	10.885312
9.725458	537.045018	10.890330
9.260788	529.778067	10.895347
9.430989	542.689403	10.900365
9.596940	565.406384	10.905383
10.090444	567.101089	10.910400
9.856079	568.699794	10.915418
9.825472	560.902713	10.920435
9.907968	544.699616	10.925453
9.642483	542.013179	10.930471
9.761419	540.142170	10.935488
9.663634	543.112661	10.940506
9.802111	534.388043	10.945523
9.842438	527.916948	10.950541
9.587561	539.283805	10.955559
9.672429	533.107282	10.960576
9.769077	547.539765	10.965594
9.938831	558.885928	10.970611
10.093969	552.478483	10.975629
9.871841	535.216454	10.980647
9.587091	531.755303	10.985664
10.136856	538.902561	10.990682
9.598990	536.138006	10.995699
9.995950	530.761330	11.000717
9.744742	542.657471	11.005735
9.633275	542.003675	11.010752
10.124615	546.655644	11.015770
10.010713	554.016338	11.020787
10.280210	541.147828	11.025805
9.877003	544.107085	11.030823
9.699728	537.723588	11.035840
10.136177	536.612947	11.040858
9.872716	536.148088	11.045875
9.978250	536.796468	11.050893
9.967822	536.880621	11.055911
9.941578	531.285848	11.060928
10.030329	526.436163	11.065946
9.560599	538.053149	11.070963
9.917318	534.359805	11.075981
9.844591	559.293332	11.080999
10.204485	562.647071	11.086016
10.449079	552.578966	11.091034
9.835341	549.719498	11.096051
9.992943	544.545433	11.101069
10.019332	541.405573	11.106087
9.888520	532.565320	11.111104
9.926564	538.206463	11.116122
10.062842	559.413480	11.121139
10.343742	555.867717	11.126157
10.173023	554.772971	11.131175
10.050097	540.552595	11.136192
10.102397	534.848758	11.141210
10.032536	549.511164	11.146227
9.868032	544.449092	11.151245
9.945331	556.951833	11.156263
9.918919	566.031801	11.161280
10.142395	559.757911	11.166298
10.148383	567.178283	11.171315
10.539152	565.735853	11.176333
10.107090	564.503683	11.181351
10.236548	567.840858	11.186368
10.214818	557.009810	11.191386
10.005481	558.663816	11.196403
10.297504	554.928820	11.201421
10.083011	560.228738	11.206439
10.110917	566.809309	11.211456
10.502321	557.194817	11.216474
10.074304	564.254006	11.221491
9.944885	559.390832	11.226509
10.070586	558.647374	11.231527
10.162763	563.670149	11.236544
10.407657	556.351437	11.241562
9.841585	564.915681	11.246579
10.101416	558.359016	11.251597
10.065401	561.479116	11.256615
10.280686	568.417614	11.261632
10.388253	576.561678	11.266650
10.406088	592.791795	11.271667
10.618029	580.441415	11.276685
10.213627	563.417004	11.281703
10.074439	573.195925	11.286720
10.293524	582.387606	11.291738
10.585024	590.983870	11.296755
10.605148	586.441182	11.301773
10.660561	599.415664	11.306791
10.116012	579.694517	11.311808
10.819373	571.407415	11.316826
10.302767	574.885819	11.321843
10.066621	575.817142	11.326861
10.347539	576.891182	11.331879
10.400575	581.929892	11.336896
10.312359	584.342146	11.341914
10.331853	598.540222	11.346931
10.370619	589.627765	11.351949
10.671339	586.657813	11.356967
10.301288	586.650341	11.361984
10.257853	579.059300	11.367002
10.315963	588.428812	11.372019
10.311002	590.806810	11.377037
10.635381	591.247705	11.382055
10.433582	588.371198	11.387072
10.645914	583.919117	11.392090
10.537095	583.578643	11.397107
10.438828	586.316952	11.402125
10.587250	587.842434	11.407143
10.195973	603.171068	11.412160
11.008847	606.342336	11.417178
10.754404	612.882676	11.422195
10.726779	604.251268	11.427213
10.536437	601.320501	11.432231
10.627246	597.199939	11.437248
10.977497	601.227292	11.442266
10.552784	600.394667	11.447283
10.499441	589.388132	11.452301
10.581853	591.740640	11.457319
10.789538	603.624619	11.462336
10.917327	603.244178	11.467354
10.679462	613.989410	11.472371
10.869161	610.180798	11.477389
11.123861	605.793740	11.482407
10.784991	601.804951	11.487424
11.027673	593.031946	11.492442
10.499401	593.513244	11.497459
10.679570	575.461369	11.502477
10.913722	595.956996	11.507495
10.734205	605.787101	11.512512
10.849828	607.334550	11.517530
10.954082	600.469790	11.522547
11.245505	600.371685	11.527565
11.181686	577.195934	11.532583
10.917348	583.503662	11.537600
10.966334	576.732310	11.542618
10.712145	582.727352	11.547635
10.570167	580.870015	11.552653
11.024994	583.964746	11.557671
10.671749	583.009270	11.562688
11.118861	592.825366	11.567706
11.230513	593.018824	11.572723
10.982778	588.272865	11.577741
10.890539	582.840174	11.582759
10.828566	584.428445	11.587776
10.839206	590.249330	11.592794
11.169404	593.574924	11.597811
11.262097	602.462761	11.602829
11.159389	585.490726	11.607847
10.909332	586.346405	11.612864
11.417660	576.323587	11.617882
11.011717	585.346338	11.622899
11.021193	585.718911	11.627917
10.952923	585.152049	11.632935
11.022039	584.414810	11.637952
11.115817	581.885794	11.642970
11.165159	587.554610	11.647987
10.973785	582.500518	11.653005
11.021579	579.458281	11.658023
11.013962	603.326041	11.663040
11.439164	605.320626	11.668058
11.239574	599.895863	11.673075
11.031561	598.260470	11.678093
11.205531	596.170904	11.683111
10.845000	605.772729	11.688128
11.200687	599.320641	11.693146
11.399168	608.807465	11.698163
11.316297	605.364442	11.703181
11.566287	599.940822	11.708199
11.115198	606.059809	11.713216
11.346356	604.173359	11.718234
11.255477	598.120393	11.723251
11.135754	612.537980	11.728269
11.202752	602.511848	11.733287
10.835936	610.900218	11.738304
11.345599	606.385514	11.743322
11.149018	606.817008	11.748339
11.065477	608.074619	11.753357
11.445100	602.211840	11.758375
10.895633	615.416014	11.763392
11.175037	602.441094	11.768410
11.126180	613.161722	11.773427
11.259800	610.034799	11.778445
11.553244	603.830798	11.783463
11.109199	606.968078	11.788480
11.177404	614.021104	11.793498
11.273199	617.250090	11.798515
11.419906	635.636351	11.803533
11.525419	642.567864	11.808551
11.700642	645.791578	11.813568
11.758017	624.387719	11.818586
11.803516	615.207612	11.823603
11.391697	611.340736	11.828621
11.498060	607.690010	11.833639
11.302466	607.266665	11.838656
11.670601	609.036067	11.843674
11.174261	605.199329	11.848691
11.224770	615.989721	11.853709
11.450891	621.895011	11.858727
11.437259	639.814152	11.863744
11.703810	642.470018	11.868762
11.715681	637.771996	11.873779
11.727905	645.518914	11.878797
11.855972	641.673258	11.883815
11.684118	638.450463	11.888832
12.058844	624.786155	11.893850
11.629691	618.978553	11.898867
11.541431	601.747824	11.903885
11.792555	597.011773	11.908903
11.124278	600.183426	11.913920
11.298775	612.518551	11.918938
11.611516	627.232238	11.923955
11.397038	632.025513	11.928973
11.511728	627.615965	11.933991
11.417809	632.419197	11.939008
11.821817	631.915463	11.944026
11.984785	630.793410	11.949043
11.860946	634.459927	11.954061
12.203029	632.760214	11.959079
11.854312	634.553441	11.964096
11.999110	633.881222	11.969114
12.035356	635.196950	11.974131
11.597681	630.443454	11.979149
12.123762	633.585448	11.984167
11.671661	632.420760	11.989184
11.736191	636.871790	11.994202
11.714285	638.804200	11.999219
11.784048	633.401356	12.004237
11.679780	632.413312	12.009255
11.856680	642.711167	12.014272
11.843569	637.727140	12.019290
12.069345	640.630295	12.024307
11.646665	642.000754	12.029325
11.752194	638.332444	12.034343
11.640197	634.152152	12.039360
11.595500	636.484377	12.044378
11.908422	635.222145	12.049395
11.682051	653.707209	12.054413
12.200221	651.049646	12.059431
12.308401	658.107489	12.064448
12.100935	646.826843	12.069466
12.413740	638.371711	12.074483
12.017561	643.813940	12.079501
12.088311	624.579010	12.084519
12.156814	636.309298	12.089536
12.042609	632.429355	12.094554
12.503763	634.757737	12.099571
12.208476	636.518497	12.104589
12.536176	628.728977	12.109607
11.904840	629.926123	12.114624
12.228660	625.611467	12.119642
12.014023	620.710813	12.124659
11.838945	630.383514	12.129677
12.146880	625.940000	12.134695
12.188201	622.290593	12.139712
12.229004	625.675529	12.144730
12.374714	622.500148	12.149747
12.185985	632.023938	12.154765
12.209592	632.298902	12.159783
12.173186	632.004700	12.164800
12.101386	624.445497	12.169818
12.483624	627.764450	12.174835
12.091478	626.135529	12.179853
12.094588	623.334921	12.184871
12.224363	626.836221	12.189888
12.043838	629.538948	12.194906
12.308244	637.209855	12.199923
12.467582	651.842673	12.204941
12.322992	653.619424	12.209959
12.606786	655.149662	12.214976
12.411928	652.967625	12.219994
12.550911	638.512069	12.225011
12.636115	639.840949	12.230029
12.537468	627.771868	12.235047
12.567434	622.257514	12.240064
12.432633	620.579289	12.245082
12.494274	626.362611	12.250099
12.254382	626.554440	12.255117
12.029291	628.358691	12.260135
12.268921	627.418815	12.265152
12.576363	647.920878	12.270170
12.784040	645.078127	12.275187
12.278700	636.763584	12.280205
12.573948	644.334117	12.285223
12.436087	645.849531	12.290240
12.208901	655.634808	12.295258
12.699526	651.930287	12.300275
12.356548	663.294895	12.305293
12.611455	658.917236	12.310311
12.325757	664.897054	12.315328
12.596409	661.982065	12.320346
12.666031	656.154062	12.325363
12.752775	660.277422	12.330381
12.591541	659.068899	12.335399
13.055032	649.205025	12.340416
12.846738	658.568301	12.345434
13.224251	653.505810	12.350451
12.770318	645.657922	12.355469
12.739423	633.167797	12.360487
12.662581	633.729064	12.365504
12.522428	630.384491	12.370522
12.683806	638.563770	12.375539
12.500833	646.256794	12.380557
12.963683	654.188928	12.385575
12.887174	653.445092	12.390592
12.510497	662.346906	12.395610
12.795805	649.244205	12.400627
12.829039	659.610345	12.405645
12.814377	658.899572	12.410663
12.868575	654.968118	12.415680
12.519986	656.726289	12.420698
12.888923	653.760383	12.425715
12.855728	662.220698	12.430733
12.765916	654.231022	12.435751
12.700313	662.279008	12.440768
12.407515	661.550513	12.445786
12.997859	655.461494	12.450803
12.723231	662.454386	12.455821
12.827712	661.496338	12.460839
13.120525	653.209066	12.465856
12.729329	657.667850	12.470874
12.737557	655.285659	12.475891
12.472436	653.963243	12.480909
13.022281	670.618314	12.485927
13.382836	681.316471	12.490944
12.893554	678.954454	12.495962
12.951311	681.969685	12.500979
13.248257	692.898844	12.505997
12.919982	682.785362	12.511015
13.216671	683.046603	12.516032
13.214743	684.513136	12.521050
13.291563	664.574430	12.526067
12.979975	650.009622	12.531085
12.955835	658.210969	12.536103
13.135916	671.703817	12.541120
13.184473	680.965917	12.546138
13.329155	675.823474	12.551155
13.121870	683.656361	12.556173
13.202072	686.155699	12.561191
13.306049	687.243297	12.566208
13.447177	681.877830	12.571226
13.308253	668.338691	12.576243
12.978008	662.971364	12.581261
13.039022	673.872256	12.586279
13.248074	672.633126	12.591296
13.032162	679.275769	12.596314
13.173297	693.128216	12.601331
13.574381	684.241534	12.606349
13.431554	686.230585	12.611367
13.518044	681.765851	12.616384
13.160755	692.215574	12.621402
13.332997	681.691280	12.626419
13.352863	681.065335	12.631437
13.134680	686.180877	12.636455
13.533601	678.008300	12.641472
13.563252	687.073544	12.646490
13.276123	679.514932	12.651507
13.117954	683.436345	12.656525
13.091186	680.235184	12.661543
13.340096	678.376493	12.666560
13.227227	680.964095	12.671578
13.613365	682.384086	12.676595
13.090456	689.149217	12.681613
12.864283	683.455611	12.686631
13.456831	693.901201	12.691648
13.552000	700.964761	12.696666
13.720788	699.039417	12.701683
13.665139	704.824868	12.706701
13.492673	710.376920	12.711719
13.872907	702.797946	12.716736
13.646173	706.286645	12.721754
13.829199	691.281648	12.726771
13.679813	688.464944	12.731789
13.648072	675.493060	12.736807
13.660404	676.186405	12.741824
13.552923	682.306791	12.746842
13.767701	684.090966	12.751859
13.975778	692.984552	12.756877
13.666761	682.694268	12.761895
13.571967	672.957465	12.766912
13.491470	681.619313	12.771930
14.052846	685.616061	12.776947
13.916367	686.638756	12.781965
13.843186	682.612644	12.786983
13.738624	677.741381	12.792000
13.635691	683.861014	12.797018
13.623707	680.214514	12.802035
13.853252	692.955134	12.807053
13.973946	694.513957	12.812071
13.931372	678.726684	12.817088
13.714626	685.189162	12.822106
13.951090	690.011325	12.827123
13.884807	705.820078	12.832141
14.036454	698.138805	12.837159
14.163887	686.282231	12.842176
14.018143	688.042643	12.847194
13.914718	678.722993	12.852211
14.158154	677.467933	12.857229
14.179323	680.956521	12.862247
14.166191	679.209327	12.867264
14.029428	673.611938	12.872282
14.162163	668.785238	12.877299
14.348398	672.314206	12.882317
13.995218	675.255755	12.887335
14.118698	661.376731	12.892352
14.065143	676.488107	12.897370
14.405327	677.032683	12.902387
14.200365	674.453124	12.907405
13.766073	676.422722	12.912423
13.958892	669.975133	12.917440
14.042976	675.886246	12.922458
14.181764	681.759172	12.927475
14.114178	676.147572	12.932493
13.791429	675.604735	12.937511
13.935380	669.328221	12.942528
13.813801	674.696254	12.947546
13.897487	688.421602	12.952563
14.071179	692.366409	12.957581
13.902753	699.648803	12.962599
14.449561	704.568788	12.967616
14.155528	704.423931	12.972634
14.352144	694.467611	12.977651
14.302767	709.017726	12.982669
14.232231	711.561317	12.987687
14.267546	709.159279	12.992704
14.227740	714.657084	12.997722
14.273100	712.099453	13.002739
14.470810	702.570091	13.007757
14.479744	706.809492	13.012775
14.614033	706.198457	13.017792
14.088296	710.352384	13.022810
14.433867	705.618378	13.027827
14.379689	705.649542	13.032845
14.194051	710.166819	13.037863
14.040190	707.880747	13.042880
14.217592	713.255976	13.047898
14.024162	705.702307	13.052915
14.423976	715.409391	13.057933
14.196934	723.049123	13.062951
14.722949	739.123597	13.067968
14.587884	730.791785	13.072986
14.658121	734.288401	13.078003
14.941048	733.932660	13.083021
14.499879	733.819646	13.088039
14.903620	732.291200	13.093056
14.664414	724.708883	13.098074
14.310000	714.133196	13.103091
14.680179	715.221992	13.108109
14.691250	731.767532	13.113127
14.794288	730.914044	13.118144
14.557759	726.487430	13.123162
14.623670	738.941419	13.128179
14.519144	740.264324	13.133197
14.421550	733.807318	13.138215
14.569785	728.892605	13.143232
14.324122	732.055720	13.148250
15.014326	740.528572	13.153267
15.071325	729.149354	13.158285
14.755877	739.656351	13.163303
14.960394	734.235883	13.168320
14.894320	733.863525	13.173338
14.966938	737.438484	13.178355
14.792529	734.714493	13.183373
14.268030	730.421383	13.188391
14.530801	729.677267	13.193408
14.578048	739.163624	13.198426
14.638871	733.529166	13.203443
14.964530	724.674240	13.208461
14.697245	734.957521	13.213479
14.623269	731.815344	13.218496
14.757759	751.091124	13.223514
15.034445	761.154436	13.228531
15.265683	757.391663	13.233549
14.860124	771.587054	13.238567
15.141721	758.505740	13.243584
15.143770	756.030860	13.248602
15.148139	760.295834	13.253619
14.994359	753.078474	13.258637
15.054508	758.719580	13.263655
15.258484	753.318092	13.268672
15.164153	753.935012	13.273690
15.030964	755.580366	13.278707
15.048570	755.974823	13.283725
15.054932	760.425285	13.288743
14.823645	758.150845	13.293760
14.914524	762.420785	13.298778
15.114660	762.196070	13.303795
15.002537	759.964099	13.308813
14.884537	764.715457	13.313831
15.053650	752.524780	13.318848
15.192860	755.996596	13.323866
15.414377	755.746294	13.328883
15.676615	752.448841	13.333901
14.968573	765.206980	13.338919
15.336875	756.161913	13.343936
15.592058	758.584652	13.348954
15.418279	760.354438	13.353971
15.417213	749.459995	13.358989
15.392717	755.315499	13.364007
15.273264	757.621146	13.369024
15.390441	760.023432	13.374042
15.277288	748.616865	13.379059
15.646615	754.203231	13.384077
15.296225	758.520253	13.389095
15.207144	752.464568	13.394112
15.710184	756.724131	13.399130
15.523523	767.596812	13.404147
15.517032	751.460986	13.409165
15.235559	759.203051	13.414183
15.670253	751.160333	13.419200
15.661495	750.316694	13.424218
15.553486	757.075750	13.429235
15.581883	763.393737	13.434253
15.184695	763.783652	13.439271
15.629045	766.106963	13.444288
15.592029	766.095918	13.449306
15.487293	782.638248	13.454323
16.018949	783.281038	13.459341
15.639843	774.539631	13.464359
15.400575	760.319027	13.469376
15.861461	776.209058	13.474394
16.057472	778.070759	13.479411
15.805828	753.435754	13.484429
15.769239	760.948698	13.489447
15.515364	752.675521	13.494464
15.464991	769.055299	13.499482
15.452365	776.475703	13.504499
15.600245	784.760439	13.509517
15.923039	788.421539	13.514535
15.846946	783.358135	13.519552
16.160494	780.999775	13.524570
16.139767	784.029596	13.529587
16.189627	781.062959	13.534605
15.955304	768.643022	13.539623
15.697758	761.284580	13.544640
15.766152	760.042357	13.549658
15.570664	780.923922	13.554675
15.787842	780.999127	13.559693
15.807348	784.444709	13.564711
15.879521	781.803102	13.569728
16.005477	782.923681	13.574746
15.673484	778.275075	13.579763
16.383969	783.910076	13.584781
16.191993	783.604231	13.589799
15.924427	785.978105	13.594816
16.090149	776.524070	13.599834
15.902835	786.461088	13.604851
16.273993	781.745656	13.609869
16.316296	788.627073	13.614887
16.157168	787.747310	13.619904
16.362027	781.010293	13.624922
16.312700	788.753695	13.629939
16.501461	784.614897	13.634957
16.389293	788.539348	13.639975
15.955248	784.678076	13.644992
16.013552	786.384634	13.650010
16.215977	783.655715	13.655027
16.225310	780.560755	13.660045
16.203634	780.861328	13.665063
16.034346	787.684478	13.670080
16.455939	780.745833	13.675098
16.207958	780.365801	13.680115
16.498881	774.149945	13.685133
16.384871	786.153470	13.690151
16.048554	780.202488	13.695168
16.090781	779.348044	13.700186
16.158330	785.155249	13.705203
16.020689	781.205137	13.710221
16.210980	783.720905	13.715239
16.195521	799.280010	13.720256
16.639137	804.804097	13.725274
16.430224	810.290175	13.730291
16.583922	803.510441	13.735309
16.690611	805.140489	13.740327
16.685838	814.924076	13.745344
17.006145	802.487862	13.750362
16.559509	799.432180	13.755379
16.542364	797.354548	13.760397
16.561137	797.103567	13.765415
16.689586	795.248667	13.770432
16.622777	795.828750	13.775450
16.511470	807.743265	13.780467
16.793359	801.755263	13.785485
16.700315	805.869063	13.790503
16.825894	802.112359	13.795520
16.906293	795.342009	13.800538
16.563620	797.737770	13.805555
16.316966	796.468580	13.810573
16.362627	809.320056	13.815591
16.289740	805.328508	13.820608
16.664766	801.963946	13.825626
16.300779	816.943404	13.830643
16.613743	813.868238	13.835661
16.619646	808.597949	13.840679
16.378800	815.034552	13.845696
16.766637	817.738866	13.850714
16.581911	832.087108	13.855731
16.871222	833.442048	13.860749
16.829737	838.598851	13.865767
17.181146	836.085795	13.870784
17.075169	843.609874	13.875802
16.993913	834.830531	13.880819
17.031217	838.070430	13.885837
17.570060	833.601221	13.890855
17.257072	816.817288	13.895872
17.063438	812.612671	13.900890
17.121255	810.891901	13.905907
17.121304	803.915964	13.910925
17.102181	803.874791	13.915943
17.343125	805.762518	13.920960
17.337131	803.775162	13.925978
16.948243	815.459673	13.930995
16.802686	812.605699	13.936013
17.052832	812.889216	13.941031
17.021669	823.077161	13.946048
17.172523	821.248862	13.951066
17.263334	829.148994	13.956083
17.234314	834.648206	13.961101
17.333870	837.471515	13.966119
17.122653	841.639536	13.971136
17.370167	835.494621	13.976154
17.173351	844.604149	13.981171
17.335500	842.809016	13.986189
17.111674	836.435859	13.991207
16.989929	842.370882	13.996224
17.289148	832.080568	14.001242
17.272187	837.897850	14.006259
17.443171	835.054054	14.011277
17.623745	838.193068	14.016295
17.264178	845.031609	14.021312
17.852036	824.308895	14.026330
17.450776	843.036519	14.031347
17.409802	840.047905	14.036365
17.622367	840.385675	14.041383
17.246321	838.859965	14.046400
17.638208	832.706105	14.051418
17.495456	842.268078	14.056435
17.673744	835.088211	14.061453
17.052098	835.833785	14.066471
17.388405	837.936031	14.071488
17.813479	827.970929	14.076506
17.451731	836.350314	14.081523
17.371334	833.479641	14.086541
17.615592	827.141969	14.091559
17.736543	832.002988	14.096576
17.734889	827.286677	14.101594
17.541007	830.347147	14.106611
17.488346	838.494259	14.111629
17.509119	852.678970	14.116647
17.479338	858.690107	14.121664
17.681203	857.453728	14.126682
17.891643	866.139550	14.131699
17.754155	865.801847	14.136717
18.193265	861.173561	14.141735
17.791844	862.196831	14.146752
18.042350	859.533162	14.151770
17.769346	861.808740	14.156787
17.646254	853.280399	14.161805
17.955877	854.950469	14.166823
17.962435	868.078929	14.171840
17.863440	857.491558	14.176858
17.757389	867.370292	14.181875
17.981745	860.420178	14.186893
18.288893	849.816741	14.191911
17.815852	862.565967	14.196928
17.988765	853.275649	14.201946
17.984759	857.251890	14.206963
17.878561	869.917152	14.211981
17.961910	859.479108	14.216999
18.184265	864.855608	14.222016
18.369716	859.324479	14.227034
18.099030	861.452041	14.232051
17.962610	862.699532	14.237069
18.264988	866.695514	14.242087
18.004860	859.235488	14.247104
18.264611	851.700012	14.252122
18.040181	859.379534	14.257139
18.400938	862.578479	14.262157
18.683697	858.161508	14.267175
17.936913	864.860244	14.272192
18.436874	863.061140	14.277210
18.219461	860.108429	14.282227
18.388034	865.247781	14.287245
18.508713	863.789814	14.292263
18.231530	871.274542	14.297280
18.631425	857.158636	14.302298
18.616485	864.079486	14.307315
18.282196	861.298090	14.312333
18.547432	858.752056	14.317351
18.479286	860.875608	14.322368
18.628212	852.355373	14.327386
18.406855	866.756955	14.332403
18.511542	861.004955	14.337421
18.579755	855.392063	14.342439
18.597188	860.696986	14.347456
18.581345	861.454451	14.352474
18.328332	866.128986	14.357491
18.275734	862.162409	14.362509
18.556858	874.003729	14.367527
18.489685	893.241821	14.372544
18.862572	893.126290	14.377562
18.661080	892.331092	14.382579
18.985675	897.279667	14.387597
18.950606	887.907628	14.392615
18.647889	870.940446	14.397632
18.654657	883.109868	14.402650
18.735037	881.015289	14.407667
18.620274	894.800451	14.412685
18.854622	899.473823	14.417703
18.851291	898.420230	14.422720
18.907453	898.567765	14.427738
19.086063	894.268419	14.432755
18.739796	890.404003	14.437773
18.856673	895.508226	14.442791
18.947064	897.797651	14.447808
18.932724	903.168476	14.452826
18.978794	899.376097	14.457843
18.981575	898.357318	14.462861
18.980656	886.437201	14.467879
19.048828	901.559743	14.472896
18.868051	887.645466	14.477914
18.920534	899.296720	14.482931
18.572466	898.801765	14.487949
18.702495	893.274289	14.492967
18.925523	892.024955	14.497984
18.862905	892.822449	14.503002
19.211427	896.934809	14.508019
18.668350	897.371324	14.513037
18.742400	895.893910	14.518055
18.886089	917.744263	14.523072
19.166795	911.951682	14.528090
19.034197	912.215509	14.533107
19.031897	919.054372	14.538125
19.110849	915.599051	14.543143
18.934436	913.663126	14.548160
19.294929	903.642924	14.553178
19.191270	910.696591	14.558195
19.204678	908.959542	14.563213
19.182093	905.830080	14.568231
19.020069	909.013632	14.573248
19.516331	924.042872	14.578266
19.646987	936.475276	14.583283
19.464737	924.631610	14.588301
19.435095	911.522572	14.593319
19.199493	916.898544	14.598336
19.650090	929.805506	14.603354
19.408424	926.099739	14.608371
19.323562	935.441955	14.613389
19.904033	936.499490	14.618407
19.798798	936.487536	14.623424
19.494812	928.010365	14.628442
19.904529	924.977422	14.633459
19.309044	928.859107	14.638477
19.510124	923.206080	14.643495
19.685540	924.548787	14.648512
19.800215	935.714984	14.653530
19.726640	927.955146	14.658547
19.859069	933.214282	14.663565
19.822723	942.121712	14.668583
19.889590	943.035952	14.673600
19.831837	935.180975	14.678618
19.761177	919.959505	14.683635
19.694833	933.614641	14.688653
19.754499	925.728809	14.693671
19.741760	937.647575	14.698688
19.879495	933.906148	14.703706
20.033227	930.445528	14.708723
19.443376	934.603437	14.713741
19.551620	923.945093	14.718759
19.427917	939.574228	14.723776
19.611437	934.728014	14.728794
19.895116	931.324221	14.733811
19.899176	931.570932	14.738829
19.827195	926.365072	14.743847
19.793710	941.191503	14.748864
19.958084	952.856159	14.753882
20.151189	961.851588	14.758899
20.254986	953.123817	14.763917
20.438242	957.492292	14.768935
20.639382	952.391195	14.773952
19.843265	951.615320	14.778970
20.267894	943.936756	14.783987
20.196858	942.266046	14.789005
20.284314	952.368296	14.794023
20.405236	951.827572	14.799040
20.120676	945.484898	14.804058
20.515402	939.848225	14.809075
20.376292	949.496272	14.814093
20.361574	935.569022	14.819111
20.075149	938.142098	14.824128
20.141307	945.098767	14.829146
20.338422	953.786844	14.834163
19.866831	962.568330	14.839181
20.356491	953.630215	14.844199
20.321345	957.192361	14.849216
20.201941	962.302661	14.854234
20.600913	959.528175	14.859251
20.194756	965.634349	14.864269
20.242655	948.655876	14.869287
20.258500	949.156532	14.874304
20.134271	957.410435	14.879322
20.524595	962.128863	14.884339
20.907220	979.315878	14.889357
20.589595	965.380098	14.894375
20.711970	962.638025	14.899392
20.662681	959.586200	14.904410
21.089991	952.978017	14.909427
20.437050	962.980436	14.914445
20.521241	961.042691	14.919463
20.610155	968.295198	14.924480
20.992478	980.010791	14.929498
20.942430	976.826021	14.934515
20.611931	980.314640	14.939533
20.355625	982.922893	14.944551
20.756926	980.465724	14.949568
21.041495	990.940859	14.954586
20.959466	985.733100	14.959603
20.878761	985.569844	14.964621
21.210040	982.642789	14.969639
21.123534	983.417472	14.974656
21.019270	988.822901	14.979674
20.996597	982.140007	14.984691
21.004413	988.394567	14.989709
21.264265	981.033417	14.994727
21.430881	969.591385	14.999744
21.069680	951.169280	15.004762
20.960728	950.057191	15.009779
20.683607	957.440771	15.014797
20.817389	969.305380	15.019815
20.872722	980.004286	15.024832
20.610189	984.835939	15.029850
21.082346	974.538156	15.034867
21.025539	992.010932	15.039885
21.146163	983.908685	15.044903
21.259692	991.526013	15.049920
21.000751	977.773018	15.054938
21.228884	975.203189	15.059955
21.079092	982.125949	15.064973
21.474876	993.478311	15.069991
21.984022	999.894739	15.075008
21.304516	988.125093	15.080026
21.655016	972.260625	15.085043
21.202238	976.407265	15.090061
21.172316	978.465057	15.095079
21.397026	977.235909	15.100096
21.262760	985.632035	15.105114
21.294051	992.376001	15.110131
21.120970	1010.225913	15.115149
21.596508	1004.743154	15.120167
21.968275	1006.975769	15.125184
21.446028	1010.611889	15.130202
21.772322	995.047460	15.135219
21.593342	998.598787	15.140237
21.525890	1000.469888	15.145255
21.502810	996.487760	15.150272
21.485361	995.190837	15.155290
21.730233	992.258008	15.160307
21.536194	998.594419	15.165325
21.820851	995.636106	15.170343
22.178003	989.246605	15.175360
21.518607	997.644259	15.180378
22.118993	992.416808	15.185395
22.216041	995.999986	15.190413
21.407579	991.160926	15.195431
22.003924	992.697318	15.200448
21.597846	1001.082950	15.205466
22.112984	989.767835	15.210483
22.061257	988.646268	15.215501
22.072756	991.243248	15.220519
22.040047	992.075557	15.225536
22.174895	995.274536	15.230554
22.251011	994.356202	15.235571
22.252958	997.485458	15.240589
21.995521	996.194021	15.245607
22.005127	996.211475	15.250624
21.995368	996.725427	15.255642
22.205722	998.498955	15.260659
22.093033	990.387700	15.265677
21.955927	1000.523227	15.270695
22.191343	991.727579	15.275712
21.718026	1000.229853	15.280730
22.213828	991.289519	15.285747
22.032056	991.377636	15.290765
22.092305	988.860012	15.295783
22.200992	988.269740	15.300800
21.860791	999.722319	15.305818
22.366323	1004.565775	15.310835
22.372570	1024.574920	15.315853
22.461296	1031.152704	15.320871
22.683313	1017.659790	15.325888
22.423622	1012.092081	15.330906
22.353432	1002.887595	15.335923
22.272492	1007.567143	15.340941
22.480106	1016.538155	15.345959
22.543636	1009.850818	15.350976
22.554370	1022.742111	15.355994
22.569658	1013.349454	15.361011
22.677445	1017.167860	15.366029
22.420887	1024.961441	15.371047
22.578021	1014.426826	15.376064
22.307558	1027.423343	15.381082
22.139659	1025.081282	15.386099
22.398942	1017.782805	15.391117
22.363032	1021.541543	15.396135
22.619340	1022.757875	15.401152
22.506710	1033.145269	15.406170
22.797591	1037.426262	15.411187
22.801481	1051.232466	15.416205
22.922860	1059.776849	15.421223
23.085895	1053.763155	15.426240
22.846916	1051.907649	15.431258
23.195906	1049.233941	15.436275
23.141328	1048.424644	15.441293
23.116882	1035.615026	15.446311
23.094415	1021.568907	15.451328
22.756556	1022.259624	15.456346
23.003358	1014.803377	15.461363
22.920338	1016.703829	15.466381
22.983882	1030.828474	15.471399
23.218863	1040.481956	15.476416
22.980386	1046.839524	15.481434
23.183510	1040.981398	15.486451
23.195642	1046.306159	15.491469
23.047799	1045.304830	15.496487
23.581644	1037.062089	15.501504
23.216704	1036.636062	15.506522
22.995199	1028.335331	15.511539
23.285703	1037.515852	15.516557
23.299140	1051.440156	15.521575
23.424207	1050.391671	15.526592
23.220125	1052.550355	15.531610
23.113978	1052.634218	15.536627
23.320394	1049.960495	15.541645
23.091712	1053.977926	15.546663
23.405940	1048.526586	15.551680
23.267805	1052.845944	15.556698
23.428782	1053.637918	15.561715
23.625085	1054.909069	15.566733
23.145060	1055.622146	15.571751
23.425452	1055.445161	15.576768
23.345555	1050.851184	15.581786
23.483133	1043.025618	15.586803
23.562701	1046.813272	15.591821
23.266472	1058.463332	15.596839
23.284048	1053.935889	15.601856
23.559492	1074.557199	15.606874
23.687927	1076.578941	15.611891
23.898146	1079.202479	15.616909
23.926118	1093.699991	15.621927
23.963820	1083.198490	15.626944
23.877780	1068.199887	15.631962
23.743011	1058.926535	15.636979
23.626649	1050.931208	15.641997
23.418957	1071.539207	15.647015
24.019114	1065.227546	15.652032
23.909149	1085.518604	15.657050
23.806660	1091.437935	15.662067
23.825912	1085.494099	15.667085
23.804012	1081.645214	15.672103
23.991372	1083.167055	15.677120
23.674284	1084.273616	15.682138
23.812236	1086.939436	15.687155
23.941127	1091.955910	15.692173
23.614591	1097.923759	15.697191
23.900528	1084.378866	15.702208
23.793949	1091.205938	15.707226
24.328780	1104.389644	15.712243
24.453191	1104.175101	15.717261
24.213825	1109.152166	15.722279
24.194907	1116.491494	15.727296
24.012520	1110.777093	15.732314
24.398812	1115.210417	15.737331
24.812574	1104.944264	15.742349
24.299288	1102.843233	15.747367
24.261664	1100.864226	15.752384
24.483436	1103.291765	15.757402
24.279548	1105.955530	15.762419
24.429086	1100.362154	15.767437
24.090247	1116.155433	15.772455
24.422942	1100.033553	15.777472
24.339161	1101.485333	15.782490
24.374505	1105.774406	15.787507
24.681275	1094.318918	15.792525
24.563554	1105.206797	15.797543
24.522958	1100.038988	15.802560
24.659398	1096.984334	15.807578
24.867724	1106.163937	15.812595
24.886181	1102.226083	15.817613
24.932234	1101.988296	15.822631
24.629225	1109.003409	15.827648
25.104456	1101.116000	15.832666
25.059473	1104.679415	15.837683
25.026870	1099.740199	15.842701
24.687130	1090.132665	15.847719
24.839502	1090.182384	15.852736
24.631373	1097.349494	15.857754
24.728580	1094.443853	15.862771
24.810518	1107.782865	15.867789
24.746831	1098.659526	15.872807
25.013060	1094.625138	15.877824
24.781644	1104.381870	15.882842
24.766878	1098.859793	15.887859
25.070716	1089.284276	15.892877
24.568420	1104.662887	15.897895
24.717674	1094.372036	15.902912
24.632951	1095.327133	15.907930
24.680887	1103.133719	15.912947
24.921374	1104.289294	15.917965
25.016989	1120.782669	15.922983
25.270116	1125.543156	15.928000
25.761241	1121.782540	15.933018
25.645149	1125.394347	15.938035
25.449764	1111.166547	15.943053
25.352849	1096.299242	15.948071
25.589529	1097.454659	15.953088
25.476422	1086.608056	15.958106
25.436854	1092.863418	15.963123
25.664827	1089.903449	15.968141
25.287965	1088.464460	15.973159
25.309175	1080.515628	15.978176
25.518234	1090.187213	15.983194
25.143487	1093.076505	15.988211
25.335285	1089.958751	15.993229
25.296127	1100.880861	15.998247
25.582738	1116.126888	16.003264
25.370269	1118.649953	16.008282
25.397565	1134.011768	16.013299
25.637098	1126.357464	16.018317
25.534811	1129.885492	16.023335
25.704965	1117.896715	16.028352
25.659168	1120.768552	16.033370
25.528816	1127.877129	16.038387
25.895378	1113.011411	16.043405
25.620092	1119.846746	16.048423
25.883329	1119.385993	16.053440
25.886600	1121.309964	16.058458
25.680526	1127.604326	16.063475
25.930928	1119.667917	16.068493
25.490175	1123.526390	16.073511
26.015255	1120.723909	16.078528
25.751356	1126.010940	16.083546
25.687211	1120.786001	16.088563
26.212925	1122.311269	16.093581
25.849150	1144.470371	16.098599
25.807756	1144.677762	16.103616
26.486291	1138.374354	16.108634
26.172124	1144.022068	16.113651
26.354749	1140.703859	16.118669
26.093636	1152.505258	16.123687
26.358306	1147.151063	16.128704
26.328165	1136.878865	16.133722
26.118073	1130.028913	16.138739
26.507598	1137.743130	16.143757
26.066924	1143.723202	16.148775
26.279783	1149.724196	16.153792
26.159929	1139.323153	16.158810
25.857543	1145.390955	16.163827
26.731467	1132.627383	16.168845
26.389980	1144.092092	16.173863
26.347900	1141.973662	16.178880
26.634568	1136.302057	16.183898
26.630521	1138.736679	16.188915
26.677018	1136.864601	16.193933
26.819252	1142.020218	16.198951
26.488319	1133.808413	16.203968
26.655746	1134.285945	16.208986
26.625203	1143.052769	16.214003
26.655435	1138.260613	16.219021
26.744824	1140.152611	16.224039
26.565908	1133.341588	16.229056
26.699727	1136.823831	16.234074
26.729433	1141.804384	16.239091
26.816505	1142.718047	16.244109
26.811655	1151.497156	16.249127
26.452943	1146.431611	16.254144
26.543505	1144.142008	16.259162
26.499307	1144.911662	16.264179
26.841129	1136.924675	16.269197
26.590435	1143.676028	16.274215
26.567803	1144.462189	16.279232
27.091522	1153.501017	16.284250
26.909128	1174.395903	16.289267
26.936453	1170.803014	16.294285
27.022575	1169.471998	16.299303
27.296229	1170.379571	16.304320
27.422999	1169.638663	16.309338
27.229992	1173.920685	16.314355
27.470854	1165.859850	16.319373
27.417393	1171.689599	16.324391
26.892619	1166.629103	16.329408
27.440239	1163.174470	16.334426
27.125555	1169.763206	16.339443
26.998781	1166.160401	16.344461
27.325538	1164.814344	16.349479
27.312672	1170.835399	16.354496
27.581930	1160.936437	16.359514
27.280007	1170.305286	16.364531
27.396530	1166.501176	16.369549
27.605864	1160.697487	16.374567
27.384986	1173.392615	16.379584
27.417607	1164.661551	16.384602
27.227122	1165.282596	16.389619
27.611018	1156.369359	16.394637
27.566294	1167.070789	16.399655
27.580432	1173.202332	16.404672
27.792153	1170.832823	16.409690
27.920605	1174.596666	16.414707
27.470229	1168.668355	16.419725
27.338818	1170.969743	16.424743
27.204088	1177.497190	16.429760
27.376806	1170.760996	16.434778
27.498416	1194.987790	16.439795
27.852911	1193.282027	16.444813
27.589957	1194.087511	16.449831
27.571935	1197.183499	16.454848
28.060346	1196.103581	16.459866
27.748225	1198.807724	16.464883
28.028116	1186.901115	16.469901
28.303823	1195.116875	16.474919
27.963308	1196.610780	16.479936
28.025252	1193.932609	16.484954
27.510536	1200.551329	16.489971
28.027515	1220.288368	16.494989
28.339051	1211.718572	16.500007
28.007698	1225.292649	16.505024
28.482549	1212.227381	16.510042
28.023509	1217.339276	16.515059
28.467796	1214.525354	16.520077
28.679028	1217.225519	16.525095
28.670039	1212.244562	16.530112
28.763567	1183.025814	16.535130
28.437985	1190.256901	16.540147
28.494752	1183.563129	16.545165
28.297136	1186.012093	16.550183
28.425163	1183.208417	16.555200
28.669403	1178.204833	16.560218
28.653920	1179.698460	16.565235
28.535957	1175.563889	16.570253
28.568752	1173.940528	16.575271
28.612660	1184.486351	16.580288
28.529080	1170.725801	16.585306
28.179336	1172.580673	16.590323
28.749470	1176.527285	16.595341
28.743083	1181.546109	16.600359
28.596827	1191.593514	16.605376
29.002447	1193.200878	16.610394
28.788387	1194.441565	16.615411
28.395953	1200.239264	16.620429
29.148902	1196.268746	16.625447
28.460382	1201.155646	16.630464
28.708893	1206.348017	16.635482
28.931285	1204.800738	16.640499
29.090591	1198.515564	16.645517
28.908355	1204.744200	16.650535
28.756763	1207.011534	16.655552
29.070649	1202.255855	16.660570
28.893149	1212.365531	16.665587
28.963989	1204.222201	16.670605
29.146512	1206.990896	16.675623
28.767814	1215.212662	16.680640
28.907335	1212.783450	16.685658
28.898590	1217.849132	16.690675
29.113141	1238.278386	16.695693
29.122117	1224.987100	16.700711
28.974658	1245.031429	16.705728
29.428061	1236.742061	16.710746
29.402111	1238.709073	16.715763
28.869883	1234.515523	16.720781
29.380472	1235.735438	16.725799
29.267425	1238.255052	16.730816
29.884481	1238.902623	16.735834
29.455755	1234.299027	16.740851
29.646271	1241.466337	16.745869
29.890762	1224.386113	16.750887
29.538301	1238.845179	16.755904
29.576558	1234.395360	16.760922
29.895118	1231.534538	16.765939
30.057154	1233.455462	16.770957
30.046254	1226.882322	16.775975
29.748362	1221.162597	16.780992
29.652161	1223.959336	16.786010
29.737775	1227.725561	16.791027
29.885886	1234.718396	16.796045
30.149323	1216.818127	16.801063
29.536469	1228.529795	16.806080
29.539417	1217.160350	16.811098
29.684565	1222.232442	16.816115
29.652264	1214.911288	16.821133
30.106741	1227.113934	16.826151
29.870904	1247.245338	16.831168
30.332213	1248.134443	16.836186
30.307465	1246.197378	16.841203
30.129671	1230.148866	16.846221
30.226419	1218.648142	16.851239
29.877389	1225.824862	16.856256
30.168261	1239.274271	16.861274
30.580452	1239.104202	16.866291
30.648962	1240.260704	16.871309
30.458972	1224.099653	16.876327
30.368902	1218.248275	16.881344
30.033776	1210.769000	16.886362
30.189853	1223.160025	16.891379
30.170024	1239.891930	16.896397
30.653318	1239.525051	16.901415
30.469512	1255.180598	16.906432
30.467890	1250.575175	16.911450
30.691753	1253.373253	16.916467
30.735802	1252.968869	16.921485
31.049518	1232.129985	16.926503
30.600572	1227.867923	16.931520
30.857257	1213.147072	16.936538
30.581449	1213.869647	16.941555
30.281295	1221.352046	16.946573
30.910911	1227.175405	16.951591
30.818801	1238.677630	16.956608
30.752936	1249.356239	16.961626
30.855379	1247.657953	16.966643
30.811207	1245.342220	16.971661
31.115329	1247.852997	16.976679
30.748142	1243.275036	16.981696
30.869906	1237.303144	16.986714
30.889447	1245.666070	16.991731
30.794240	1245.033173	16.996749
31.148060	1236.988243	17.001767
30.817964	1246.726758	17.006784
30.736936	1242.879750	17.011802
30.880765	1245.783597	17.016819
31.154425	1242.686116	17.021837
31.198159	1235.548029	17.026855
31.207372	1244.655173	17.031872
31.270595	1242.283864	17.036890
31.014308	1248.845247	17.041907
30.912179	1248.442232	17.046925
31.446498	1257.789598	17.051943
31.437745	1258.220716	17.056960
31.578849	1269.100499	17.061978
31.550755	1262.456176	17.066995
31.463995	1271.781586	17.072013
31.799790	1269.414353	17.077031
31.582760	1267.457943	17.082048
31.835107	1261.556545	17.087066
31.771081	1261.275565	17.092083
31.164267	1249.723992	17.097101
31.793932	1250.990727	17.102119
31.469763	1257.035014	17.107136
31.600447	1263.350442	17.112154
31.533878	1257.947908	17.117171
31.469946	1258.166906	17.122189
31.570470	1256.170909	17.127207
31.637450	1255.319427	17.132224
31.830696	1265.085471	17.137242
31.855403	1254.403331	17.142259
31.832704	1266.988163	17.147277
32.121587	1250.763935	17.152295
31.713535	1251.205263	17.157312
31.815530	1271.662252	17.162330
31.996037	1281.177270	17.167347
32.139754	1288.741322	17.172365
32.183411	1280.597727	17.177383
32.150209	1291.948902	17.182400
32.320989	1295.688837	17.187418
32.422166	1291.102601	17.192435
32.144192	1289.333442	17.197453
32.255291	1292.471061	17.202471
32.347363	1293.026036	17.207488
32.153144	1290.481207	17.212506
32.451910	1286.366974	17.217523
32.152639	1288.178857	17.222541
32.377166	1283.564325	17.227559
32.572564	1292.633976	17.232576
32.431078	1284.711978	17.237594
32.374812	1284.052552	17.242611
32.256547	1290.789129	17.247629
32.686477	1282.499686	17.252647
32.497695	1290.467608	17.257664
32.450768	1281.587446	17.262682
32.171916	1287.719122	17.267699
32.292423	1302.403868	17.272717
32.866368	1305.245564	17.277735
32.980589	1302.371713	17.282752
33.215327	1308.249462	17.287770
33.252716	1302.230887	17.292787
33.062905	1297.653854	17.297805
32.778306	1278.517107	17.302823
33.137610	1292.459557	17.307840
32.699345	1297.487331	17.312858
33.123432	1297.573163	17.317875
33.463282	1294.676127	17.322893
33.145135	1297.520652	17.327911
33.120589	1293.833962	17.332928
33.087518	1300.820606	17.337946
33.213751	1298.016026	17.342963
33.217754	1299.150930	17.347981
33.580623	1290.546213	17.352999
33.657165	1288.830558	17.358016
33.187904	1272.066886	17.363034
33.387509	1264.828175	17.368051
33.202771	1277.244572	17.373069
33.507447	1285.174093	17.378087
33.462348	1294.677262	17.383104
33.534651	1296.338646	17.388122
33.798877	1289.271899	17.393139
33.254404	1296.237707	17.398157
33.856408	1292.148853	17.403175
33.278453	1298.561945	17.408192
33.188940	1291.702979	17.413210
33.383201	1283.906489	17.418227
33.406532	1293.579427	17.423245
33.562681	1288.399057	17.428263
33.596820	1294.356079	17.433280
33.494642	1311.655627	17.438298
33.586119	1318.561816	17.443315
33.611427	1327.643115	17.448333
33.664933	1330.218630	17.453351
33.725533	1327.817034	17.458368
33.554582	1330.562390	17.463386
34.117586	1323.063089	17.468403
33.511926	1332.666972	17.473421
33.960878	1327.454249	17.478439
33.994244	1319.198560	17.483456
34.448711	1345.377936	17.488474
34.822210	1332.849817	17.493491
34.434904	1327.812173	17.498509
34.429618	1324.431732	17.503527
34.409136	1333.978093	17.508544
34.496076	1318.431320	17.513562
34.857381	1316.687015	17.518579
34.254040	1317.485086	17.523597
34.482356	1311.140015	17.528615
34.366807	1308.951838	17.533632
34.060937	1321.719033	17.538650
34.263425	1321.812423	17.543667
34.272137	1321.582390	17.548685
34.513751	1317.845719	17.553703
34.590663	1334.160531	17.558720
34.667624	1343.989974	17.563738
34.876256	1343.429990	17.568755
34.610765	1349.346094	17.573773
34.619555	1347.075120	17.578791
34.952138	1340.289549	17.583808
34.756100	1346.425252	17.588826
34.841814	1338.506158	17.593843
34.777188	1340.575649	17.598861
34.890189	1343.077143	17.603879
35.064714	1345.634591	17.608896
34.586346	1347.471804	17.613914
34.893330	1339.407018	17.618931
35.145776	1344.422015	17.623949
34.804781	1343.095564	17.628967
35.255225	1340.755400	17.633984
35.043423	1346.896470	17.639002
35.414688	1339.199777	17.644019
35.172757	1341.469097	17.649037
35.050963	1347.299990	17.654055
35.223693	1343.762119	17.659072
35.204779	1340.516607	17.664090
35.089309	1338.688252	17.669107
35.020435	1354.566205	17.674125
35.200268	1363.025094	17.679143
35.464872	1371.574675	17.684160
35.500896	1369.548792	17.689178
35.971506	1358.773064	17.694195
35.742644	1375.537365	17.699213
35.939088	1364.278292	17.704231
35.819650	1363.973414	17.709248
35.533777	1374.484208	17.714266
36.205002	1361.848502	17.719283
35.986773	1374.681543	17.724301
35.735407	1359.030903	17.729319
35.858828	1352.957512	17.734336
35.485902	1360.904779	17.739354
35.965971	1360.959689	17.744371
35.899034	1363.164210	17.749389
35.949487	1357.707620	17.754407
36.056923	1361.589949	17.759424
35.898111	1363.889997	17.764442
36.236572	1359.260909	17.769459
36.109586	1361.578128	17.774477
36.172644	1362.503654	17.779495
36.057553	1355.612674	17.784512
35.845384	1365.354177	17.789530
36.015014	1361.868389	17.794547
36.091033	1365.913794	17.799565
36.214820	1370.505617	17.804583
36.250530	1366.070749	17.809600
36.268246	1387.136330	17.814618
36.735512	1386.399664	17.819635
36.732698	1385.844769	17.824653
36.781082	1382.720782	17.829671
36.747551	1367.324220	17.834688
36.247466	1374.013424	17.839706
36.563305	1373.531357	17.844723
36.340067	1386.259333	17.849741
36.735774	1389.292367	17.854759
37.035076	1390.788224	17.859776
36.872562	1391.002681	17.864794
36.852259	1381.366482	17.869811
36.704821	1386.944158	17.874829
36.977263	1386.988959	17.879847
37.175847	1385.469620	17.884864
36.942717	1382.414292	17.889882
37.239046	1379.602006	17.894899
36.990451	1386.996419	17.899917
37.089551	1389.888803	17.904935
37.097329	1383.541243	17.909952
36.977068	1389.451032	17.914970
37.255277	1381.398075	17.919987
37.219409	1379.159687	17.925005
37.344550	1379.135571	17.930023
37.547781	1373.301318	17.935040
37.078547	1375.232691	17.940058
37.205589	1377.616905	17.945075
37.427226	1382.519300	17.950093
37.199519	1374.291061	17.955111
37.265197	1368.524861	17.960128
37.285152	1376.583067	17.965146
37.528963	1371.446422	17.970163
37.536295	1379.879552	17.975181
37.164524	1383.987294	17.980199
37.112011	1378.601288	17.985216
37.573587	1389.533605	17.990234
37.446638	1405.415713	17.995251
37.721061	1406.627504	18.000269
37.491134	1412.179477	18.005287
37.586686	1411.152390	18.010304
37.570997	1410.551200	18.015322
37.666433	1407.616661	18.020339
37.512887	1404.980040	18.025357
37.591791	1408.822616	18.030375
37.790028	1415.363141	18.035392
37.857990	1435.625196	18.040410
38.091477	1426.581592	18.045427
38.253747	1427.518254	18.050445
38.472981	1431.576971	18.055463
38.806169	1421.801903	18.060480
38.393583	1428.287272	18.065498
38.685580	1424.670973	18.070515
38.491428	1403.583275	18.075533
38.543896	1393.310614	18.080551
38.518521	1390.877574	18.085568
38.459422	1399.796515	18.090586
38.129829	1394.807560	18.095603
38.625935	1388.844888	18.100621
38.370517	1402.728592	18.105639
38.248542	1407.066238	18.110656
38.354543	1417.934616	18.115674
38.736380	1422.917584	18.120691
38.765713	1416.766835	18.125709
38.383394	1424.190888	18.130727
38.277820	1419.866799	18.135744
38.809705	1420.276121	18.140762
38.942944	1416.159341	18.145779
39.169786	1414.140047	18.150797
38.851291	1417.656301	18.155815
39.060934	1407.558393	18.160832
38.740394	1416.416695	18.165850
39.054944	1416.452161	18.170867
38.965137	1415.482930	18.175885
38.764289	1418.483251	18.180903
39.204309	1426.665631	18.185920
38.936600	1446.348241	18.190938
39.214811	1445.990513	18.195955
39.981063	1442.772849	18.200973
39.579494	1446.184362	18.205991
39.508668	1417.577028	18.211008
39.090210	1419.655116	18.216026
39.220215	1433.580149	18.221043
39.769753	1431.928680	18.226061
39.407247	1443.948662	18.231079
39.765804	1436.607962	18.236096
39.490555	1444.635949	18.241114
39.868938	1446.682102	18.246131
39.656430	1430.806452	18.251149
39.050657	1433.500594	18.256167
39.633213	1433.748377	18.261184
39.531624	1435.564946	18.266202
39.731156	1438.223781	18.271219
39.587656	1441.358311	18.276237
39.572768	1442.268008	18.281255
39.859200	1436.829010	18.286272
39.788307	1435.247593	18.291290
39.846666	1438.007755	18.296307
39.966016	1440.511757	18.301325
39.982273	1464.269016	18.306343
40.143982	1464.616798	18.311360
40.153113	1476.255192	18.316378
40.244753	1465.771273	18.321395
40.562863	1464.103002	18.326413
40.154099	1472.164133	18.331431
39.992776	1466.561860	18.336448
39.833376	1467.181313	18.341466
39.918669	1468.558282	18.346483
40.287000	1468.847049	18.351501
40.049446	1462.231416	18.356519
40.853399	1475.140174	18.361536
40.525583	1490.048935	18.366554
40.198630	1494.836687	18.371571
40.603650	1488.099688	18.376589
40.850654	1489.352245	18.381607
40.848178	1486.521698	18.386624
40.995714	1491.517106	18.391642
41.201871	1488.468943	18.396659
41.056116	1489.888107	18.401677
41.084015	1482.064733	18.406695
41.578502	1461.259784	18.411712
40.963551	1454.289714	18.416730
40.743841	1447.881763	18.421747
41.316154	1446.348569	18.426765
40.915374	1450.963493	18.431783
41.215489	1445.630887	18.436800
41.445444	1450.279565	18.441818
40.832751	1446.138254	18.446835
41.274219	1455.981036	18.451853
41.425000	1471.445181	18.456871
41.383664	1477.329337	18.461888
41.392315	1483.763880	18.466906
41.239536	1481.081449	18.471923
41.717520	1477.748910	18.476941
41.450297	1480.341728	18.481959
41.524403	1483.604803	18.486976
41.505965	1483.963121	18.491994
41.551437	1480.926999	18.497011
41.374259	1475.784828	18.502029
41.433278	1483.315756	18.507047
41.484182	1484.068892	18.512064
41.592616	1482.598723	18.517082
41.522710	1484.971469	18.522099
41.915564	1487.056177	18.527117
41.753556	1497.715837	18.532135
41.969609	1499.548324	18.537152
42.173195	1507.128555	18.542170
41.819479	1510.149085	18.547187
41.845215	1511.853637	18.552205
41.925456	1511.430261	18.557223
41.921228	1498.431873	18.562240
42.068425	1508.109239	18.567258
41.678459	1513.165698	18.572275
42.066444	1507.081513	18.577293
41.944765	1511.930558	18.582311
42.605458	1529.553250	18.587328
42.389583	1535.121444	18.592346
42.618856	1531.830074	18.597363
42.790568	1526.962797	18.602381
42.658335	1514.783624	18.607399
42.279540	1508.201200	18.612416
42.296630	1512.748921	18.617434
42.461059	1524.684867	18.622451
42.783935	1531.829609	18.627469
42.727481	1532.570602	18.632487
42.643600	1528.068875	18.637504
42.781451	1526.906430	18.642522
42.547874	1532.689366	18.647539
42.874999	1526.664463	18.652557
43.074286	1530.822572	18.657575
43.393977	1522.761493	18.662592
43.150934	1518.523918	18.667610
42.709138	1512.035389	18.672627
43.111965	1522.252722	18.677645
43.110615	1517.235757	18.682663
43.199265	1519.619264	18.687680
43.184358	1516.389981	18.692698
43.267912	1526.014116	18.697715
43.124338	1516.754151	18.702733
43.150587	1526.657067	18.707751
43.523927	1530.907618	18.712768
43.537621	1534.509054	18.717786
43.433853	1544.753589	18.722803
43.708700	1548.701947	18.727821
43.681629	1545.793178	18.732839
43.631252	1543.576854	18.737856
43.742496	1538.172733	18.742874
43.564995	1546.018838	18.747891
44.202446	1542.611457	18.752909
44.125487	1546.372788	18.757927
43.981378	1539.685744	18.762944
43.972326	1530.471214	18.767962
44.332475	1540.447201	18.772979
44.192443	1516.362580	18.777997
43.920599	1500.147469	18.783015
43.860697	1504.670927	18.788032
43.925832	1522.168599	18.793050
43.872241	1529.149295	18.798067
44.196830	1531.939803	18.803085
44.128152	1533.090695	18.808103
43.872354	1540.806061	18.813120
44.440603	1533.585715	18.818138
43.920130	1541.641362	18.823155
44.222953	1530.290145	18.828173
44.445487	1542.661368	18.833191
44.221848	1552.456462	18.838208
44.695957	1559.015151	18.843226
44.611459	1565.064361	18.848243
44.639480	1564.107895	18.853261
44.959902	1567.443591	18.858279
44.918275	1569.921511	18.863296
44.773752	1553.442742	18.868314
44.524232	1571.838242	18.873331
45.242928	1565.222109	18.878349
44.906394	1559.510623	18.883367
44.800367	1567.245298	18.888384
44.907333	1570.086412	18.893402
44.754905	1567.508633	18.898419
44.826525	1569.892605	18.903437
44.906241	1565.938586	18.908455
44.641550	1565.650274	18.913472
45.104310	1568.569880	18.918490
45.132210	1572.926458	18.923507
45.055986	1580.221950	18.928525
44.914974	1581.341515	18.933543
45.092079	1583.692276	18.938560
45.564121	1576.558313	18.943578
45.117085	1586.333331	18.948595
45.382577	1583.785171	18.953613
45.378121	1584.114405	18.958631
44.989674	1583.812331	18.963648
45.633961	1599.065756	18.968666
45.685314	1601.545610	18.973683
45.538553	1605.444498	18.978701
45.581879	1613.193837	18.983719
45.815837	1615.152508	18.988736
46.105970	1608.769523	18.993754
46.503362	1608.483004	18.998771
46.390529	1614.668029	19.003789
46.436657	1604.068322	19.008807
46.130809	1597.376143	19.013824
46.327880	1570.759225	19.018842
46.250054	1569.262013	19.023859
46.308194	1567.067482	19.028877
46.314075	1563.435139	19.033895
46.337887	1569.178227	19.038912
46.225554	1563.385916	19.043930
46.334788	1592.122101	19.048947
46.653459	1600.040806	19.053965
46.148071	1598.050600	19.058983
46.402617	1597.985373	19.064000
46.661441	1596.247770	19.069018
46.724449	1594.851648	19.074035
46.899821	1599.671221	19.079053
46.684340	1592.453054	19.084071
46.345480	1600.519212	19.089088
46.707880	1597.154998	19.094106
46.466753	1594.494655	19.099123
46.759423	1593.084917	19.104141
46.453158	1596.319262	19.109159
46.281248	1608.031038	19.114176
46.665457	1615.858978	19.119194
46.971061	1621.939683	19.124211
47.201308	1623.432037	19.129229
47.162098	1620.643769	19.134247
47.484930	1619.855023	19.139264
47.454132	1617.463004	19.144282
47.387716	1628.327006	19.149299
47.462928	1622.065034	19.154317
47.467825	1622.488391	19.159335
47.157417	1629.915201	19.164352
47.509091	1619.725134	19.169370
47.396971	1619.058800	19.174387
47.501518	1621.080238	19.179405
47.374414	1628.372760	19.184423
47.347853	1649.531856	19.189440
47.899546	1647.060316	19.194458
47.910677	1648.936200	19.199475
48.025412	1647.381900	19.204493
48.195525	1643.023126	19.209511
48.017098	1647.617039	19.214528
48.296386	1638.116512	19.219546
48.105477	1641.747913	19.224563
48.328535	1647.244258	19.229581
48.636455	1637.959071	19.234599
48.152448	1634.659008	19.239616
48.277713	1611.861034	19.244634
48.134375	1608.968748	19.249651
48.377729	1607.114020	19.254669
48.183713	1620.262155	19.259687
48.254663	1632.958158	19.264704
48.782632	1636.785494	19.269722
48.517892	1641.208655	19.274739
48.626216	1643.598766	19.279757
49.150388	1638.595143	19.284775
48.615720	1628.546707	19.289792
48.648018	1604.121602	19.294810
48.591859	1608.901560	19.299827
48.471485	1625.548954	19.304845
48.685363	1633.575579	19.309863
48.549226	1644.294048	19.314880
48.501169	1637.279638	19.319898
48.427673	1643.003431	19.324915
48.381289	1635.696615	19.329933
48.443147	1652.232761	19.334951
48.558575	1656.841802	19.339968
49.095602	1662.812946	19.344986
48.991577	1669.594967	19.350003
48.874959	1663.400567	19.355021
49.112331	1678.945465	19.360039
49.365976	1695.478643	19.365056
49.509793	1690.734046	19.370074
49.856572	1683.159352	19.375091
49.555736	1678.962797	19.380109
49.548826	1684.612194	19.385127
49.502611	1684.101483	19.390144
50.164455	1679.671911	19.395162
49.868171	1685.566861	19.400179
49.677931	1687.541447	19.405197
50.004753	1680.553531	19.410215
49.596725	1684.098842	19.415232
50.041507	1686.550969	19.420250
49.783428	1685.046583	19.425267
50.101705	1681.711311	19.430285
50.147338	1680.518060	19.435303
50.063693	1677.095792	19.440320
49.962349	1673.402829	19.445338
50.039704	1685.691904	19.450355
49.906889	1686.889255	19.455373
49.938385	1683.714853	19.460391
49.643193	1692.442735	19.465408
50.193011	1704.041777	19.470426
50.432207	1709.613033	19.475443
50.152799	1701.797909	19.480461
50.830191	1703.946168	19.485479
50.712623	1703.197266	19.490496
50.862469	1692.525207	19.495514
50.831906	1696.026527	19.500531
50.953148	1703.369304	19.505549
50.950606	1689.419281	19.510567
50.922504	1699.128942	19.515584
50.920613	1693.167901	19.520602
50.796671	1703.198948	19.525619
50.997443	1693.101537	19.530637
51.112723	1693.929065	19.535655
50.829886	1701.885604	19.540672
51.311554	1698.142955	19.545690
51.143777	1705.829261	19.550707
51.128102	1715.944361	19.555725
51.409450	1712.626614	19.560743
51.350630	1730.412371	19.565760
51.668952	1726.212108	19.570778
51.239077	1728.072436	19.575795
51.299680	1731.604733	19.580813
51.336799	1729.688467	19.585831
51.310167	1728.035517	19.590848
51.600519	1725.982833	19.595866
51.626566	1728.499574	19.600883
51.431180	1723.683176	19.605901
51.504796	1728.655860	19.610919
51.350104	1738.636115	19.615936
51.489122	1745.010992	19.620954
52.053814	1751.233106	19.625971
51.886291	1756.610298	19.630989
52.036036	1748.657165	19.636007
52.206978	1753.143655	19.641024
52.129822	1741.491020	19.646042
52.495506	1734.131679	19.651059
52.279206	1745.294206	19.656077
52.627161	1737.548815	19.661095
52.515722	1740.493841	19.666112
52.663812	1740.658842	19.671130
52.599226	1738.009008	19.676147
52.442572	1733.167689	19.681165
52.720136	1733.824253	19.686183
52.707326	1732.867844	19.691200
52.691354	1725.961468	19.696218
52.622148	1741.692232	19.701235
52.945597	1740.625422	19.706253
53.318899	1730.702573	19.711271
52.537611	1737.034545	19.716288
53.031371	1732.928463	19.721306
52.893503	1728.793495	19.726323
52.912914	1734.635013	19.731341
52.974953	1731.826023	19.736359
52.740796	1747.764028	19.741376
53.150609	1750.318021	19.746394
53.256195	1762.151687	19.751411
53.243850	1767.381535	19.756429
53.199701	1766.624410	19.761447
53.283605	1762.262554	19.766464
53.340505	1763.071799	19.771482
53.406165	1756.540483	19.776499
53.327330	1769.709832	19.781517
53.500760	1761.614185	19.786535
53.612757	1779.280375	19.791552
54.097846	1789.357886	19.796570
53.820137	1787.294523	19.801587
53.770971	1787.405569	19.806605
54.267536	1786.668368	19.811623
54.344276	1787.071959	19.816640
54.420707	1773.435957	19.821658
54.571355	1758.908135	19.826675
53.969064	1762.415941	19.831693
54.120536	1752.729810	19.836711
54.184933	1761.976156	19.841728
54.237653	1766.715693	19.846746
54.316461	1775.445084	19.851763
54.257531	1785.462271	19.856781
54.471365	1774.573652	19.861799
54.446320	1782.697789	19.866816
54.317057	1778.586974	19.871834
54.550126	1787.760131	19.876851
54.699118	1780.550427	19.881869
54.462704	1779.468043	19.886887
54.489778	1779.789698	19.891904
54.573427	1777.336972	19.896922
54.613184	1799.474288	19.901939
54.317960	1811.524357	19.906957
54.795306	1816.508178	19.911975
54.890305	1807.758155	19.916992
54.625208	1818.158325	19.922010
55.159229	1812.845924	19.927027
54.836251	1814.213355	19.932045
55.373690	1828.646493	19.937063
55.508104	1836.632836	19.942080
55.656623	1836.871785	19.947098
55.629597	1814.338106	19.952115
55.387598	1815.864968	19.957133
55.339378	1814.142353	19.962151
55.545455	1830.476066	19.967168
55.523182	1827.588104	19.972186
56.006763	1825.614046	19.977203
55.915630	1834.654291	19.982221
55.823636	1823.200906	19.987239
55.765541	1820.732665	19.992256
55.802364	1828.321767	19.997274
55.453935	1827.537853	20.002291
55.947009	1828.009130	20.007309
55.831478	1822.005436	20.012327
55.794698	1826.430276	20.017344
55.759846	1824.569223	20.022362
55.924751	1843.820069	20.027379
56.232582	1850.797762	20.032397
56.912808	1849.571477	20.037415
56.509071	1854.283859	20.042432
56.540109	1848.760231	20.047450
56.658973	1844.646112	20.052467
56.769675	1853.698620	20.057485
56.779200	1845.827316	20.062503
57.019493	1853.198486	20.067520
57.116805	1856.813712	20.072538
56.932257	1839.412502	20.077555
56.955365	1845.502274	20.082573
57.188036	1843.184316	20.087591
56.993061	1847.912920	20.092608
56.946404	1849.109797	20.097626
57.261064	1847.829470	20.102643
57.193735	1850.134521	20.107661
57.316477	1847.277664	20.112679
57.358602	1848.836622	20.117696
57.276132	1856.772663	20.122714
57.428095	1850.594744	20.127731
57.000201	1842.779724	20.132749
57.312630	1838.947738	20.137767
57.122426	1844.301156	20.142784
57.032870	1843.497215	20.147802
57.472846	1843.404042	20.152819
57.267301	1866.792727	20.157837
57.568765	1873.804951	20.162855
57.475355	1877.318685	20.167872
57.312037	1879.761684	20.172890
57.754586	1892.841267	20.177907
57.675099	1904.992700	20.182925
58.161677	1905.941052	20.187943
57.946676	1908.311508	20.192960
58.150213	1911.667420	20.197978
58.216636	1903.581542	20.202995
58.044860	1901.930557	20.208013
58.190437	1902.543233	20.213031
58.394240	1896.601995	20.218048
58.422135	1907.541131	20.223066
58.881049	1910.976416	20.228083
58.682405	1921.741647	20.233101
58.748701	1909.040696	20.238119
58.835040	1903.637816	20.243136
58.739941	1917.802923	20.248154
59.116453	1909.366480	20.253171
59.216141	1909.545403	20.258189
58.932098	1901.436448	20.263207
58.998217	1893.410077	20.268224
58.827677	1901.505215	20.273242
58.849833	1900.142995	20.278259
58.652701	1912.865503	20.283277
59.113799	1909.867571	20.288295
59.176152	1920.530530	20.293312
58.691288	1928.741506	20.298330
59.177028	1914.773823	20.303347
59.354904	1939.141683	20.308365
59.571117	1941.968716	20.313383
59.845394	1943.375069	20.318400
59.694662	1952.553207	20.323418
59.964272	1942.197378	20.328435
59.759437	1947.514277	20.333453
59.993654	1943.099528	20.338471
60.055616	1936.243543	20.343488
60.039347	1933.314014	20.348506
60.031198	1926.975956	20.353523
60.133520	1940.555231	20.358541
60.188025	1936.101340	20.363559
60.342249	1933.314453	20.368576
60.427453	1932.917805	20.373594
60.714195	1933.553961	20.378611
60.341766	1910.691492	20.383629
60.350841	1915.685159	20.388647
60.430445	1921.690408	20.393664
60.520614	1930.441234	20.398682
60.583502	1928.274213	20.403699
60.288066	1925.642489	20.408717
60.495167	1929.374992	20.413735
60.744998	1919.816571	20.418752
60.364425	1934.459286	20.423770
60.831506	1927.692927	20.428787
60.865752	1934.058850	20.433805
60.880580	1959.428964	20.438823
61.087340	1955.262073	20.443840
61.078492	1953.430164	20.448858
61.399891	1953.090080	20.453875
61.284356	1963.274239	20.458893
61.080546	1955.014960	20.463911
61.504450	1958.611964	20.468928
61.348254	1959.234842	20.473946
61.300455	1945.812571	20.478963
61.260367	1951.401415	20.483981
61.464731	1952.149639	20.488999
61.404257	1955.926844	20.494016
61.624282	1968.370085	20.499034
61.643232	1978.436708	20.504051
61.746037	1978.703308	20.509069
62.121420	1981.765420	20.514087
62.059750	1986.954294	20.519104
61.892846	1980.959438	20.524122
62.180035	1972.746812	20.529139
62.162964	1979.206686	20.534157
61.864966	1981.013710	20.539175
62.218165	1974.570920	20.544192
62.311062	1988.967573	20.549210
62.084829	1989.595354	20.554227
62.346958	2012.780838	20.559245
62.596965	2006.406697	20.564263
63.065607	1997.924242	20.569280
62.657878	2005.618533	20.574298
62.994161	1998.919864	20.579315
62.945669	1999.610347	20.584333
62.564551	2005.374182	20.589351
62.860232	1997.840869	20.594368
62.852490	1997.860015	20.599386
62.988397	1992.453622	20.604403
63.039166	1986.528633	20.609421
63.143536	2000.454877	20.614439
63.022611	1986.986802	20.619456
63.044653	2001.024319	20.624474
63.533523	2011.426952	20.629491
63.344572	2028.737335	20.634509
63.439575	2030.165898	20.639527
64.030329	2023.570366	20.644544
63.536030	2029.945885	20.649562
63.898379	2020.062463	20.654579
63.963721	2016.904044	20.659597
63.909113	2017.564043	20.664615
63.841976	1999.136880	20.669632
63.946083	2009.855194	20.674650
64.057446	2024.726791	20.679667
63.847590	2020.974937	20.684685
64.049381	2018.892390	20.689703
63.982291	2027.002749	20.694720
63.731819	2023.158009	20.699738
63.799391	2021.267769	20.704755
63.987070	2026.382299	20.709773
64.130364	2044.008175	20.714791
64.320649	2050.864471	20.719808
64.074965	2053.147505	20.724826
64.408842	2051.622633	20.729843
64.353154	2053.116308	20.734861
64.183693	2061.892477	20.739879
64.344084	2073.570057	20.744896
64.540932	2083.066722	20.749914
64.473557	2081.589777	20.754931
64.852025	2080.547696	20.759949
65.234659	2085.136641	20.764967
65.340099	2095.599665	20.769984
65.415053	2091.261640	20.775002
65.614068	2089.462232	20.780019
65.784257	2068.983408	20.785037
65.437812	2069.811024	20.790055
65.748321	2058.091603	20.795072
65.816332	2072.048735	20.800090
65.803855	2061.769849	20.805107
65.857429	2061.213074	20.810125
65.747412	2065.276865	20.815143
65.874245	2059.837305	20.820160
65.655516	2065.518368	20.825178
66.066823	2065.056306	20.830195
65.789892	2067.312625	20.835213
65.702408	2083.401105	20.840231
65.995309	2089.705762	20.845248
65.918771	2095.781027	20.850266
65.870380	2089.903913	20.855283
65.978600	2085.416675	20.860301
66.246697	2101.973093	20.865319
66.706905	2115.663352	20.870336
66.309669	2125.077295	20.875354
66.216259	2127.301268	20.880371
66.511149	2126.826588	20.885389
66.002843	2131.653221	20.890407
66.333439	2122.682117	20.895424
66.407952	2148.908835	20.900442
66.659735	2146.423488	20.905459
66.784226	2148.781867	20.910477
66.844181	2152.825413	20.915495
66.877699	2149.076147	20.920512
66.958861	2151.683049	20.925530
67.195453	2161.316494	20.930547
67.290487	2167.592918	20.935565
67.324301	2172.772343	20.940583
68.039356	2169.736253	20.945600
67.919564	2173.941067	20.950618
67.645953	2163.388800	20.955635
67.861700	2137.844246	20.960653
67.526051	2143.626195	20.965671
67.637563	2140.084107	20.970688
67.635012	2162.531714	20.975706
68.037160	2167.619443	20.980723
68.110982	2159.548744	20.985741
67.900947	2159.345073	20.990759
68.089411	2154.621686	20.995776
68.243970	2162.718253	21.000794
67.966285	2171.242312	21.005811
67.912659	2155.343942	21.010829
67.713061	2164.253117	21.015847
68.314230	2169.390183	21.020864
68.357033	2184.755196	21.025882
68.617422	2190.956217	21.030899
68.674005	2184.480559	21.035917
68.831382	2191.754196	21.040935
68.891676	2185.265324	21.045952
69.109179	2184.312882	21.050970
68.948931	2181.047680	21.055987
69.103615	2183.584931	21.061005
68.969674	2187.908632	21.066023
69.127876	2171.892099	21.071040
69.255861	2179.537542	21.076058
69.110758	2178.010463	21.081075
69.408733	2173.591394	21.086093
69.360648	2184.161397	21.091111
69.415080	2171.246832	21.096128
69.272003	2183.881079	21.101146
69.540039	2207.111547	21.106163
69.434492	2205.761389	21.111181
69.664350	2204.124191	21.116199
70.010556	2204.532394	21.121216
70.032644	2204.236351	21.126234
69.612687	2209.033417	21.131251
69.763946	2205.621747	21.136269
69.728238	2207.135751	21.141287
70.114476	2229.764371	21.146304
70.090179	2232.905702	21.151322
70.209317	2240.172307	21.156339
70.529358	2230.132758	21.161357
70.494713	2232.921847	21.166375
70.631200	2213.421689	21.171392
70.712772	2233.043920	21.176410
70.832132	2227.711449	21.181427
70.809050	2226.366140	21.186445
70.595538	2222.369554	21.191463
70.516925	2225.013553	21.196480
70.801645	2227.535581	21.201498
71.009507	2246.484525	21.206515
71.439632	2261.371686	21.211533
71.332599	2257.782680	21.216551
71.149714	2259.719108	21.221568
71.119902	2258.952499	21.226586
71.254643	2260.130792	21.231603
71.405226	2249.170027	21.236621
71.373311	2265.214453	21.241639
71.427006	2257.104907	21.246656
71.267137	2257.509496	21.251674
71.296250	2261.958984	21.256691
71.405674	2269.998510	21.261709
71.368596	2279.519852	21.266727
71.600035	2270.681228	21.271744
71.518301	2276.050301	21.276762
71.660481	2304.589820	21.281779
72.258907	2300.920618	21.286797
72.281985	2303.132810	21.291815
72.477935	2301.179547	21.296832
72.648277	2299.555737	21.301850
72.402364	2301.286059	21.306867
72.738256	2298.495409	21.311885
72.679507	2298.532844	21.316903
72.746711	2292.557771	21.321920
72.632832	2299.259802	21.326938
72.784259	2301.929509	21.331955
72.795349	2290.406347	21.336973
72.702680	2295.029166	21.341991
72.956791	2285.825344	21.347008
73.227627	2299.531765	21.352026
72.775037	2296.453136	21.357043
73.411986	2294.293780	21.362061
73.099477	2297.299368	21.367079
73.658800	2313.930636	21.372096
73.630977	2317.443847	21.377114
73.649316	2327.237948	21.382131
73.888655	2319.980359	21.387149
73.624735	2321.260096	21.392167
73.870767	2323.417266	21.397184
73.809843	2318.093353	21.402202
73.909573	2320.223955	21.407219
73.591810	2305.060541	21.412237
73.749834	2313.845626	21.417255
74.011211	2314.474188	21.422272
73.862444	2310.157394	21.427290
73.798722	2323.659372	21.432307
74.314959	2332.237908	21.437325
73.791079	2333.534702	21.442343
74.352268	2339.487938	21.447360
74.262250	2341.296002	21.452378
74.185641	2345.708685	21.457395
74.661317	2343.770130	21.462413
74.512390	2368.708942	21.467431
74.479946	2370.406291	21.472448
74.711282	2366.300187	21.477466
74.826310	2364.329209	21.482483
75.330878	2364.143449	21.487501
75.248315	2362.910738	21.492519
75.134688	2362.896625	21.497536
75.523785	2366.384916	21.502554
75.318896	2379.211062	21.507571
75.828989	2374.983601	21.512589
75.666743	2379.945149	21.517607
75.900115	2377.804961	21.522624
75.870655	2362.638642	21.527642
75.649537	2365.907867	21.532659
75.736733	2362.425269	21.537677
75.814515	2383.226337	21.542695
75.717387	2377.530422	21.547712
76.122938	2385.425698	21.552730
76.197814	2383.618068	21.557747
76.555344	2380.033618	21.562765
76.528942	2387.244463	21.567783
76.072876	2389.578913	21.572800
76.527135	2377.298020	21.577818
76.205539	2384.444345	21.582835
76.371511	2379.347427	21.587853
76.278763	2394.025993	21.592871
76.452876	2410.259305	21.597888
76.604597	2407.838913	21.602906
76.848825	2412.657577	21.607923
77.190041	2406.702845	21.612941
76.927808	2407.261007	21.617959
76.990265	2409.362751	21.622976
77.209875	2409.481272	21.627994
76.968370	2417.187615	21.633011
77.122313	2424.708008	21.638029
77.478101	2434.106915	21.643047
77.390881	2431.752066	21.648064
77.856980	2432.875116	21.653082
77.772713	2441.755905	21.658099
77.629354	2429.801096	21.663117
77.669080	2434.763476	21.668135
77.435736	2432.828907	21.673152
77.832454	2427.823698	21.678170
77.548122	2428.681995	21.683187
77.892966	2442.640479	21.688205
77.928323	2455.906862	21.693223
78.250436	2460.463418	21.698240
78.294967	2458.306844	21.703258
78.223023	2457.092054	21.708275
78.124501	2457.514444	21.713293
78.533124	2455.233412	21.718311
78.665188	2472.500193	21.723328
78.993483	2480.998898	21.728346
79.193561	2477.211347	21.733363
79.665746	2452.769563	21.738381
79.452438	2443.317820	21.743399
79.472624	2437.249682	21.748416
79.544777	2438.847825	21.753434
79.220243	2444.907983	21.758451
79.270768	2435.112545	21.763469
79.530565	2432.697879	21.768487
79.016335	2435.140003	21.773504
79.392168	2429.561838	21.778522
79.280196	2448.277351	21.783539
79.685577	2456.283328	21.788557
79.902638	2463.315701	21.793575
79.834115	2468.298770	21.798592
79.894168	2466.269554	21.803610
79.679122	2469.789780	21.808627
80.196179	2455.191589	21.813645
79.940580	2460.440289	21.818663
80.072336	2461.423410	21.823680
80.336334	2472.284480	21.828698
80.323654	2481.867264	21.833715
80.185334	2495.778225	21.838733
80.380922	2491.420903	21.843751
80.417996	2502.486899	21.848768
80.610067	2493.520407	21.853786
80.279316	2498.738252	21.858803
80.727372	2511.580425	21.863821
80.986715	2519.716921	21.868839
80.838382	2524.270278	21.873856
80.966168	2524.457550	21.878874
81.048821	2523.934530	21.883891
80.865470	2528.884657	21.888909
81.218830	2537.165449	21.893927
81.270236	2541.986156	21.898944
81.163873	2559.735846	21.903962
81.474587	2551.034738	21.908979
81.768338	2548.719952	21.913997
81.870592	2545.110009	21.919015
81.372083	2553.699578	21.924032
82.017371	2557.869956	21.929050
82.301965	2574.639517	21.934067
81.898087	2572.662688	21.939085
82.214068	2574.659877	21.944103
82.225939	2575.659704	21.949120
82.427205	2571.440407	21.954138
82.363882	2572.952719	21.959155
82.500115	2570.121058	21.964173
82.766290	2566.066224	21.969191
82.694306	2572.203523	21.974208
82.843225	2571.392739	21.979226
82.928020	2576.363451	21.984243
82.992668	2566.170682	21.989261
83.135212	2567.564651	21.994279
82.805099	2569.883392	21.999296
82.881689	2560.994647	22.004314
82.865619	2577.157645	22.009331
83.148547	2593.327066	22.014349
83.084460	2591.186488	22.019367
82.738627	2604.259399	22.024384
83.231288	2595.137168	22.029402
83.349676	2616.619669	22.034419
83.600677	2621.611306	22.039437
83.626643	2613.438051	22.044455
83.969535	2621.556437	22.049472
84.144677	2616.124434	22.054490
84.070689	2621.289178	22.059507
84.254595	2613.718560	22.064525
84.503819	2611.223722	22.069543
84.235645	2613.473943	22.074560
84.517943	2609.521948	22.079578
84.595577	2613.640252	22.084595
84.475963	2619.002721	22.089613
84.712718	2623.217526	22.094631
84.874891	2628.938492	22.099648
85.076471	2631.222760	22.104666
84.919189	2634.101128	22.109683
84.915232	2630.467409	22.114701
85.249368	2633.741222	22.119719
85.033548	2637.541555	22.124736
85.454893	2626.830601	22.129754
85.295037	2626.554437	22.134771
85.324627	2623.713255	22.139789
85.314034	2624.844374	22.144807
85.326150	2636.052795	22.149824
85.536313	2647.055194	22.154842
85.656769	2654.345399	22.159859
85.710028	2657.963775	22.164877
86.070340	2650.756876	22.169895
85.978927	2657.795524	22.174912
85.974128	2646.458995	22.179930
86.043176	2652.446194	22.184947
86.205679	2657.590695	22.189965
86.537761	2671.594809	22.194983
86.559901	2673.146922	22.200000
86.622872	2667.661814	22.205018
86.819162	2663.535843	22.210035
86.826302	2676.434223	22.215053
86.934864	2668.962280	22.220071
86.717550	2673.420793	22.225088
86.728820	2669.160086	22.230106
86.658668	2673.320986	22.235123
86.949860	2673.293790	22.240141
87.170672	2681.389896	22.245159
87.109406	2694.770913	22.250176
87.231063	2691.587285	22.255194
87.553687	2699.725605	22.260211
87.444379	2703.176009	22.265229
87.870601	2698.711543	22.270247
87.647166	2701.059889	22.275264
87.235838	2700.332405	22.280282
87.959416	2719.537120	22.285299
87.699546	2727.633301	22.290317
88.345153	2725.985884	22.295335
88.106702	2729.602569	22.300352
88.229915	2727.748705	22.305370
88.241635	2729.459648	22.310387
88.271237	2723.232741	22.315405
88.447694	2722.307539	22.320423
88.216680	2742.630642	22.325440
88.432028	2746.985257	22.330458
88.957776	2759.817923	22.335475
88.868574	2759.015055	22.340493
88.917424	2755.528876	22.345511
88.703575	2762.107488	22.350528
88.981270	2758.005812	22.355546
89.235681	2747.663387	22.360563
88.907975	2759.544352	22.365581
89.616347	2765.807667	22.370599
89.359479	2788.830216	22.375616
89.636839	2777.703985	22.380634
89.686404	2783.554685	22.385651
89.947152	2777.319017	22.390669
89.911278	2769.540597	22.395687
90.065562	2780.008595	22.400704
90.103303	2772.833391	22.405722
90.080142	2768.638599	22.410739
89.968444	2779.234893	22.415757
89.897748	2784.136919	22.420775
90.030202	2808.763290	22.425792
90.549353	2809.075157	22.430810
90.493098	2803.000240	22.435827
90.533899	2809.143370	22.440845
90.678739	2792.239361	22.445863
90.597019	2809.597821	22.450880
90.415654	2813.767327	22.455898
90.994052	2823.709193	22.460915
90.618880	2821.332268	22.465933
91.031925	2824.740708	22.470951
90.944532	2825.925111	22.475968
91.032058	2839.267837	22.480986
91.371069	2840.704901	22.486003
91.601992	2851.767399	22.491021
91.742124	2846.246223	22.496039
91.803661	2855.280681	22.501056
91.860366	2847.027011	22.506074
91.966551	2841.238599	22.511091
91.972774	2857.209991	22.516109
92.112772	2865.279018	22.521127
92.110653	2872.968787	22.526144
92.151514	2879.904919	22.531162
92.781550	2877.346204	22.536179
92.542540	2879.476268	22.541197
92.668708	2872.749806	22.546215
92.623138	2880.222737	22.551232
92.930919	2882.810354	22.556250
93.166726	2870.764868	22.561267
92.589011	2872.180073	22.566285
92.921217	2883.211257	22.571303
93.113597	2900.811472	22.576320
93.248788	2899.010727	22.581338
93.207532	2905.398211	22.586355
93.380386	2903.766049	22.591373
93.430202	2906.673571	22.596391
93.454187	2901.344456	22.601408
93.456215	2904.113025	22.606426
93.913337	2922.272244	22.611443
93.856745	2931.695236	22.616461
93.693177	2923.965048	22.621479
93.706373	2920.233531	22.626496
93.819896	2920.321979	22.631514
93.935091	2930.221694	22.636531
94.201177	2948.532662	22.641549
94.504477	2940.761000	22.646567
94.495079	2954.267522	22.651584
94.778991	2956.873279	22.656602
94.892242	2950.883243	22.661619
94.687109	2956.348971	22.666637
94.837008	2940.362162	22.671655
94.683274	2944.663755	22.676672
94.865693	2949.063646	22.681690
95.316895	2966.178128	22.686707
95.470044	2969.074853	22.691725
95.543997	2968.037068	22.696743
95.472813	2977.203424	22.701760
95.503435	2974.964428	22.706778
96.009654	2970.446086	22.711795
95.503979	2969.310546	22.716813
95.823409	2968.605777	22.721831
95.504890	2975.284492	22.726848
95.771754	2972.139765	22.731866
96.039909	2974.735534	22.736883
96.133855	2996.152519	22.741901
96.111066	2991.952880	22.746919
96.387095	2991.275770	22.751936
96.358358	2994.806215	22.756954
96.789787	2990.501845	22.761971
96.460557	2998.017070	22.766989
96.722061	2987.604409	22.772007
96.738348	3008.129062	22.777024
96.660942	3013.734702	22.782042
96.812256	3017.329840	22.787059
96.646430	3018.629222	22.792077
96.973806	3032.500569	22.797095
97.272943	3032.726415	22.802112
97.495369	3035.191168	22.807130
97.641964	3029.986213	22.812147
97.502776	3040.141127	22.817165
97.701055	3037.989730	22.822183
97.739335	3043.308090	22.827200
98.079383	3068.686014	22.832218
98.301946	3062.367177	22.837235
98.201705	3070.426867	22.842253
98.564406	3059.318201	22.847271
98.574924	3064.054491	22.852288
98.542549	3058.907899	22.857306
98.971063	3055.500935	22.862323
98.768928	3049.683562	22.867341
98.818548	3047.839876	22.872359
98.867965	3050.793165	22.877376
99.168574	3048.153124	22.882394
99.125585	3044.497814	22.887411
98.774063	3057.965390	22.892429
99.064204	3067.256642	22.897447
99.518844	3076.453334	22.902464
99.628234	3082.088315	22.907482
99.557432	3082.738045	22.912499
99.404348	3085.569339	22.917517
99.437958	3073.353216	22.922535
99.920863	3093.754661	22.927552
99.906294	3102.031704	22.932570
99.889720	3105.008134	22.937587
99.775833	3112.419644	22.942605
100.014575	3104.277053	22.947623
100.314362	3106.170684	22.952640
100.449651	3120.663738	22.957658
101.139827	3124.670921	22.962675
100.944681	3128.861298	22.967693
101.184660	3139.369293	22.972711
101.005621	3126.612289	22.977728
101.175974	3124.612764	22.982746
101.457120	3131.827765	22.987763
101.242265	3134.537784	22.992781
101.686951	3128.923563	22.997799
101.515803	3127.216428	23.002816
101.317481	3133.413450	23.007834
101.612016	3119.540141	23.012851
101.618061	3130.973569	23.017869
101.466837	3129.939979	23.022887
101.790896	3118.229730	23.027904
101.631719	3122.914597	23.032922
101.865062	3124.399501	23.037939
101.593841	3140.284425	23.042957
101.686660	3146.258035	23.047975
101.736165	3149.560972	23.052992
101.868468	3156.956155	23.058010
102.438244	3172.164022	23.063027
102.393453	3186.229027	23.068045
102.393893	3181.224616	23.073063
102.662857	3192.470056	23.078080
102.497134	3206.990582	23.083098
102.788567	3206.799945	23.088115
102.975078	3217.516867	23.093133
102.986558	3212.378714	23.098151
103.375033	3218.349864	23.103168
103.437182	3235.442825	23.108186
103.948063	3232.072587	23.113203
103.555010	3243.277650	23.118221
103.823828	3241.679573	23.123239
104.192776	3240.364164	23.128256
103.753832	3239.412458	23.133274
104.251556	3232.731425	23.138291
104.249457	3235.099510	23.143309
104.520143	3231.876138	23.148327
104.856132	3225.106124	23.153344
104.442940	3229.544462	23.158362
104.726004	3235.866573	23.163379
104.861481	3250.641245	23.168397
104.941916	3248.125822	23.173415
105.119414	3254.707572	23.178432
105.167447	3247.815519	23.183450
105.130205	3249.159385	23.188467
105.107396	3252.202631	23.193485
105.196456	3248.564393	23.198503
105.348471	3246.619076	23.203520
105.221962	3268.499754	23.208538
105.640090	3271.876348	23.213555
105.505487	3274.114784	23.218573
105.620691	3283.131155	23.223591
105.640653	3294.401750	23.228608
105.578557	3315.044913	23.233626
106.415519	3305.671549	23.238643
106.524347	3306.073019	23.243661
106.671691	3307.199301	23.248679
106.545034	3309.260027	23.253696
106.399419	3306.377642	23.258714
106.454352	3311.959510	23.263731
106.354346	3332.080564	23.268749
106.452775	3334.530063	23.273767
107.271819	3336.358624	23.278784
106.924019	3334.062135	23.283802
107.497427	3344.514279	23.288819
107.382255	3356.430988	23.293837
107.740422	3365.528457	23.298855
107.903553	3355.723249	23.303872
107.582528	3362.158812	23.308890
107.934923	3353.707477	23.313907
107.782754	3359.871354	23.318925
107.879672	3355.632111	23.323943
108.159288	3348.346118	23.328960
108.143178	3367.535107	23.333978
108.466618	3377.865253	23.338995
108.489712	3386.715809	23.344013
108.826929	3378.016157	23.349031
108.733218	3380.422268	23.354048
108.724101	3381.799683	23.359066
109.024209	3378.902160	23.364083
108.837139	3384.872981	23.369101
108.812847	3379.500508	23.374119
109.166860	3373.333033	23.379136
109.251119	3380.178728	23.384154
109.386136	3390.444397	23.389171
109.282900	3403.033657	23.394189
109.306636	3400.570122	23.399207
109.568725	3396.434641	23.404224
109.411232	3400.000670	23.409242
109.842623	3410.072778	23.414259
109.852147	3424.734198	23.419277
110.096134	3427.104489	23.424295
110.516415	3432.607801	23.429312
110.029543	3431.297435	23.434330
110.256670	3424.261071	23.439347
110.250243	3449.300077	23.444365
110.422282	3461.676073	23.449383
110.945126	3456.887880	23.454400
110.568359	3456.059740	23.459418
110.728301	3471.452302	23.464435
111.220085	3485.987475	23.469453
111.286304	3488.260024	23.474471
111.691301	3483.656710	23.479488
111.305620	3488.876493	23.484506
111.580073	3484.292428	23.489523
111.891944	3479.452531	23.494541
111.823947	3480.734965	23.499559
111.934697	3488.089774	23.504576
112.049791	3498.884471	23.509594
112.457701	3512.476737	23.514611
112.467590	3505.340065	23.519629
112.237149	3504.788130	23.524647
112.632567	3501.472783	23.529664
112.490102	3506.234929	23.534682
112.531505	3508.589946	23.539699
112.903082	3516.547340	23.544717
112.629721	3533.964319	23.549735
113.120459	3524.679647	23.554752
113.046769	3520.877714	23.559770
113.123807	3523.675318	23.564787
113.600678	3538.288609	23.569805
113.358862	3557.213190	23.574823
113.648243	3553.423984	23.579840
113.721109	3560.859912	23.584858
113.808505	3544.437894	23.589875
113.955739	3550.309724	23.594893
113.887378	3565.529519	23.599911
113.859626	3579.590087	23.604928
114.093223	3588.091298	23.609946
114.277947	3578.848594	23.614963
114.077327	3587.704014	23.619981
114.208832	3606.826332	23.624999
114.685549	3603.478605	23.630016
114.867518	3608.272907	23.635034
114.897788	3612.343797	23.640051
115.029565	3623.598873	23.645069
115.288374	3630.620533	23.650087
115.576572	3623.178640	23.655104
115.337901	3632.603455	23.660122
115.853428	3630.025389	23.665139
115.914846	3633.402450	23.670157
116.282513	3623.564788	23.675175
116.328094	3616.544220	23.680192
116.286672	3622.694589	23.685210
116.328274	3618.176205	23.690227
116.465123	3623.510732	23.695245
116.679171	3617.783715	23.700263
116.280019	3620.629460	23.705280
116.481437	3631.312306	23.710298
116.686821	3635.345154	23.715315
116.767670	3649.527983	23.720333
116.839516	3657.148403	23.725351
117.283321	3646.998079	23.730368
116.894201	3657.008524	23.735386
117.182760	3650.225706	23.740403
117.279821	3659.887514	23.745421
117.176975	3672.920690	23.750439
117.454541	3681.110298	23.755456
117.532622	3684.737404	23.760474
117.533433	3682.536318	23.765491
117.896713	3701.237648	23.770509
117.422134	3705.079501	23.775527
118.068960	3713.701371	23.780544
118.323516	3713.865703	23.785562
118.478487	3732.552338	23.790579
118.628338	3738.715975	23.795597
118.476385	3740.288354	23.800615
119.039497	3726.635832	23.805632
119.101279	3733.551949	23.810650
118.963473	3733.892673	23.815667
119.069016	3734.313206	23.820685
119.380977	3745.551927	23.825703
119.610472	3746.410667	23.830720
119.446203	3755.738973	23.835738
119.658885	3755.694066	23.840755
119.712640	3752.886086	23.845773
119.525026	3748.761570	23.850791
120.061525	3767.820579	23.855808
120.021766	3782.193599	23.860826
120.206092	3785.429461	23.865843
120.401627	3775.128397	23.870861
120.119388	3781.608898	23.875879
120.356345	3788.719299	23.880896
120.755076	3798.132401	23.885914
120.412168	3800.487692	23.890931
120.945093	3803.158683	23.895949
120.527957	3820.649789	23.900967
120.954873	3824.077816	23.905984
121.239634	3833.241263	23.911002
121.252500	3834.903705	23.916019
121.564591	3848.597968	23.921037
121.742511	3866.512737	23.926055
122.166730	3855.991055	23.931072
122.022847	3854.071813	23.936090
122.053881	3858.992377	23.941107
122.636934	3855.952635	23.946125
122.064811	3854.278333	23.951143
122.493520	3865.738007	23.956160
122.720131	3877.546944	23.961178
122.613545	3882.452498	23.966195
123.023599	3877.121349	23.971213
122.946936	3884.552261	23.976231
122.816382	3882.719012	23.981248
123.069334	3885.804930	23.986266
123.420281	3898.677718	23.991283
124.165522	3902.053849	23.996301
123.516172	3902.252459	24.001319
123.741021	3896.127428	24.006336
123.911060	3902.014910	24.011354
123.859054	3900.226931	24.016371
124.022948	3902.918084	24.021389
123.985157	3907.412194	24.026407
124.240361	3920.559160	24.031424
124.689236	3926.487116	24.036442
124.217168	3941.890271	24.041459
124.485265	3930.371390	24.046477
124.403133	3931.414825	24.051495
124.528393	3924.093481	24.056512
124.698568	3941.883615	24.061530
124.868864	3952.915194	24.066547
125.709416	3946.902418	24.071565
125.320248	3956.637426	24.076583
125.227565	3953.222845	24.081600
125.332052	3968.878661	24.086618
125.485165	3971.631463	24.091635
126.009947	3981.693994	24.096653
125.784747	3979.747248	24.101671
125.823119	3990.869209	24.106688
126.281407	3998.977876	24.111706
126.592451	3997.677114	24.116723
126.844166	4005.130109	24.121741
126.619661	4006.378250	24.126759
126.593610	3996.291708	24.131776
126.559741	3999.332992	24.136794
127.052173	4024.100927	24.141811
127.276775	4031.106380	24.146829
127.284290	4037.187776	24.151847
127.284486	4032.631632	24.156864
127.582845	4029.066456	24.161882
127.606804	4036.931248	24.166899
127.989520	4053.637330	24.171917
127.806951	4057.329331	24.176935
128.124367	4056.879619	24.181952
128.219242	4047.415650	24.186970
127.986486	4058.757378	24.191987
128.157881	4066.123683	24.197005
128.719059	4076.615755	24.202023
128.441198	4085.822881	24.207040
128.480280	4087.211673	24.212058
128.564269	4104.342918	24.217075
129.282251	4103.753649	24.222093
128.988363	4121.207358	24.227111
129.226949	4108.550520	24.232128
129.345659	4124.549865	24.237146
129.384589	4132.902862	24.242163
129.920675	4132.832765	24.247181
129.806790	4138.367273	24.252199
130.063910	4138.441802	24.257216
130.327966	4136.586508	24.262234
130.392232	4163.718065	24.267251
130.649918	4160.772296	24.272269
130.958460	4166.400687	24.277287
130.744349	4173.779674	24.282304
131.322013	4168.446669	24.287322
131.169702	4177.039260	24.292339
131.116153	4168.204619	24.297357
131.164940	4164.271211	24.302375
131.251197	4157.042058	24.307392
131.271743	4165.429617	24.312410
130.926706	4179.157357	24.317427
131.589275	4191.103842	24.322445
131.598322	4192.859884	24.327463
131.736077	4206.623488	24.332480
132.276446	4220.039298	24.337498
132.080490	4221.877322	24.342515
132.322619	4225.187974	24.347533
132.361201	4231.344631	24.352551
132.046723	4235.327850	24.357568
132.522660	4247.107603	24.362586
132.617817	4246.359977	24.367603
132.751810	4242.012372	24.372621
132.936031	4257.294582	24.377639
132.954586	4276.956195	24.382656
133.293372	4270.683788	24.387674
133.233212	4278.920172	24.392691
133.860865	4278.598654	24.397709
134.174708	4283.500883	24.402727
133.834220	4301.711460	24.407744
134.105167	4292.390666	24.412762
134.036411	4309.002442	24.417779
134.162624	4296.238050	24.422797
134.523229	4298.201305	24.427815
134.250942	4296.784455	24.432832
134.484983	4309.466662	24.437850
134.437757	4319.834385	24.442867
134.625685	4323.409982	24.447885
135.112385	4339.178515	24.452903
135.152850	4349.939688	24.457920
135.307365	4349.219246	24.462938
135.486308	4350.212397	24.467955
135.589713	4347.633144	24.472973
135.859835	4368.030531	24.477991
135.773840	4379.490739	24.483008
136.587466	4371.140097	24.488026
136.239528	4381.067789	24.493043
136.597285	4372.038933	24.498061
136.648926	4376.049781	24.503079
136.862225	4362.033681	24.508096
136.911487	4361.792165	24.513114
136.744138	4394.686359	24.518131
136.940501	4393.341548	24.523149
137.107697	4402.194023	24.528167
137.174503	4401.589692	24.533184
137.489694	4399.406945	24.538202
137.373205	4426.198732	24.543219
137.465433	4422.596714	24.548237
137.516395	4416.571937	24.553255
137.917635	4433.871534	24.558272
138.168775	4443.666222	24.563290
138.197006	4454.281432	24.568307
138.527599	4454.584791	24.573325
138.499087	4456.882616	24.578343
138.450540	4474.943467	24.583360
138.947049	4480.037607	24.588378
138.759312	4480.236190	24.593395
139.434503	4484.811680	24.598413
139.476755	4481.721169	24.603431
139.359991	4491.289336	24.608448
139.657367	4497.823020	24.613466
139.797183	4517.455408	24.618483
140.098934	4514.395172	24.623501
140.219670	4513.945721	24.628519
140.030931	4517.986162	24.633536
140.383903	4511.086780	24.638554
140.133724	4515.126366	24.643571
140.330416	4527.160475	24.648589
140.580820	4547.136868	24.653607
140.647439	4535.591834	24.658624
141.164152	4538.468043	24.663642
141.191256	4560.976398	24.668659
141.451403	4573.728528	24.673677
141.380502	4570.092840	24.678695
141.311314	4581.019598	24.683712
141.383413	4574.483287	24.688730
141.409163	4588.379177	24.693747
141.636064	4598.423692	24.698765
142.079633	4593.779021	24.703783
141.427897	4601.179465	24.708800
142.067988	4607.154783	24.713818
142.349668	4629.700635	24.718835
142.366621	4636.238273	24.723853
142.785768	4632.356055	24.728871
142.579629	4632.526183	24.733888
142.874989	4642.926397	24.738906
142.976574	4649.446879	24.743923
143.477032	4646.732539	24.748941
143.649462	4641.009679	24.753959
143.429697	4647.631402	24.758976
143.630023	4660.499827	24.763994
143.627266	4675.974062	24.769011
143.739782	4674.191048	24.774029
144.076897	4666.472797	24.779047
144.037607	4704.904266	24.784064
144.093010	4701.535099	24.789082
144.220980	4699.591223	24.794099
144.507902	4716.767510	24.799117
144.904917	4724.536234	24.804135
144.847351	4732.044715	24.809152
145.246166	4721.532178	24.814170
145.116780	4742.600254	24.819187
145.474758	4752.107313	24.824205
145.656813	4756.180937	24.829223
145.553753	4751.473140	24.834240
145.998957	4760.802737	24.839258
146.336982	4774.083983	24.844275
146.502428	4787.606455	24.849293
146.449578	4781.875949	24.854311
146.284752	4781.987259	24.859328
146.554241	4778.273119	24.864346
146.735312	4792.016677	24.869363
146.810498	4803.418219	24.874381
147.047673	4797.026965	24.879399
146.656713	4804.192164	24.884416
147.121647	4822.202272	24.889434
147.325041	4835.241234	24.894451
147.399435	4835.814625	24.899469
147.703188	4852.274734	24.904487
148.005344	4860.649908	24.909504
147.625521	4864.569282	24.914522
147.900797	4875.022592	24.919539
148.224313	4886.396472	24.924557
148.244175	4892.617130	24.929575
148.477297	4893.813206	24.934592
148.585442	4911.487120	24.939610
148.693356	4917.725502	24.944627
148.821979	4928.989126	24.949645
149.502391	4941.992524	24.954663
149.553207	4955.199397	24.959680
149.884665	4950.776378	24.964698
150.028662	4948.050118	24.969715
150.073911	4946.597178	24.974733
150.151256	4949.597395	24.979751
150.617961	4966.543360	24.984768
151.122706	4965.064754	24.989786
150.990417	4966.550514	24.994803
151.063250	4969.170294	24.999821
151.195207	4963.278389	25.004839
150.987218	4968.963441	25.009856
151.154417	4966.927981	25.014874
151.510602	4962.331536	25.019891
151.430176	4966.303755	25.024909
151.499565	4971.336454	25.029927
151.536923	4988.736284	25.034944
151.785690	4989.247734	25.039962
152.022850	4989.063312	25.044979
152.172380	4998.404197	25.049997
152.211755	5008.498922	25.055015
152.088533	5028.240074	25.060032
152.423302	5027.869375	25.065050
152.713413	5031.092711	25.070067
152.734257	5040.235976	25.075085
152.813607	5049.823208	25.080103
152.974960	5060.335668	25.085120
152.956893	5063.404470	25.090138
153.514169	5070.390757	25.095155
153.488915	5074.886275	25.100173
153.907617	5070.918179	25.105191
153.619565	5071.929621	25.110208
153.953842	5088.666879	25.115226
153.950093	5100.111632	25.120243
154.599999	5102.032611	25.125261
154.671145	5103.442963	25.130279
154.399577	5108.825920	25.135296
154.715129	5125.309565	25.140314
154.907821	5131.885261	25.145331
154.885183	5141.156284	25.150349
155.140765	5152.117881	25.155367
155.043013	5168.708585	25.160384
155.179077	5165.819784	25.165402
155.689805	5181.198482	25.170419
155.971756	5195.752660	25.175437
156.442394	5193.853596	25.180455
156.046344	5196.269867	25.185472
156.434529	5208.237355	25.190490
156.668711	5218.266886	25.195507
156.548571	5228.682718	25.200525
157.141084	5228.087413	25.205543
156.912013	5240.924224	25.210560
157.156682	5245.411335	25.215578
157.685324	5248.010834	25.220595
157.636186	5245.310984	25.225613
157.642001	5257.420569	25.230631
157.777054	5271.222570	25.235648
157.941627	5278.869382	25.240666
158.008605	5276.332238	25.245683
158.438618	5287.720282	25.250701
158.545161	5299.573009	25.255719
158.484490	5304.562763	25.260736
159.033934	5299.146635	25.265754
159.059130	5326.717478	25.270771
159.304791	5333.635757	25.275789
159.780561	5331.351481	25.280807
159.631702	5330.507947	25.285824
159.409889	5335.952053	25.290842
159.989345	5334.143646	25.295859
159.791073	5364.142690	25.300877
160.090023	5355.516810	25.305895
160.179587	5357.893668	25.310912
160.292646	5359.794867	25.315930
160.709272	5372.950982	25.320947
160.458900	5387.263458	25.325965
160.895533	5390.394091	25.330983
160.824776	5406.655297	25.336000
161.022582	5411.506996	25.341018
161.450071	5417.106698	25.346035
161.290975	5419.502677	25.351053
161.759723	5431.876002	25.356071
161.730295	5446.542605	25.361088
162.021694	5441.423543	25.366106
162.319327	5447.870159	25.371123
161.934303	5475.099619	25.376141
162.545190	5478.448730	25.381159
162.602561	5489.026734	25.386176
162.759199	5488.654799	25.391194
163.212744	5499.772105	25.396211
162.845198	5505.487701	25.401229
163.274336	5508.596758	25.406247
163.568204	5509.285061	25.411264
163.412493	5499.330073	25.416282
163.667494	5523.381220	25.421299
163.694600	5518.309036	25.426317
163.973392	5527.645376	25.431335
164.106899	5539.307156	25.436352
164.352936	5543.502712	25.441370
164.536250	5552.274406	25.446387
164.504773	5559.860873	25.451405
164.543178	5571.751075	25.456423
164.855923	5582.493219	25.461440
164.719108	5588.253347	25.466458
165.038768	5601.590316	25.471475
165.073903	5617.232476	25.476493
165.310277	5627.890417	25.481511
165.698638	5634.250418	25.486528
166.076414	5645.582786	25.491546
166.288436	5654.245820	25.496563
166.360722	5671.980081	25.501581
166.947558	5665.922825	25.506599
166.986956	5668.691602	25.511616
166.953038	5671.634764	25.516634
167.335710	5681.729009	25.521651
167.298690	5697.313095	25.526669
167.642488	5687.958945	25.531687
168.020823	5694.040240	25.536704
167.904189	5704.184077	25.541722
168.091770	5692.222792	25.546739
168.034173	5708.669582	25.551757
168.215251	5718.028512	25.556775
168.540653	5728.690687	25.561792
168.554188	5717.636386	25.566810
169.021643	5735.287972	25.571827
168.649961	5742.040052	25.576845
168.846141	5750.010296	25.581863
169.326025	5767.277080	25.586880
169.168630	5773.339188	25.591898
169.853279	5780.287382	25.596915
169.580660	5783.377197	25.601933
169.635909	5799.981827	25.606951
170.063096	5804.308927	25.611968
170.154978	5816.012458	25.616986
170.228047	5833.606574	25.622003
170.715961	5847.052156	25.627021
170.715099	5835.999369	25.632039
171.152937	5850.897741	25.637056
171.214239	5858.250820	25.642074
171.734321	5853.035485	25.647091
171.500921	5869.036609	25.652109
171.862601	5871.174743	25.657127
171.876743	5889.195328	25.662144
172.333166	5892.459047	25.667162
172.498907	5887.210996	25.672180
172.460084	5894.938248	25.677197
172.705492	5887.514195	25.682215
172.743827	5907.532146	25.687232
172.798079	5914.182283	25.692250
172.955124	5918.019337	25.697268
172.935263	5934.709792	25.702285
173.641150	5941.901857	25.707303
173.553884	5944.996462	25.712320
173.367711	5956.001821	25.717338
173.950438	5962.380975	25.722356
173.734444	5975.501336	25.727373
173.936973	5974.182942	25.732391
174.018623	5985.033716	25.737408
174.285945	5999.744646	25.742426
174.822723	5996.272675	25.747444
174.868768	6001.563184	25.752461
175.046275	6022.600276	25.757479
175.096466	6029.147953	25.762496
175.121038	6033.932432	25.767514
175.513873	6033.949068	25.772532
175.543871	6060.987958	25.777549
175.937137	6063.881742	25.782567
176.153517	6068.768376	25.787584
176.176081	6082.930753	25.792602
176.535659	6088.108741	25.797620
176.644916	6102.604918	25.802637
176.700774	6110.912841	25.807655
177.058267	6115.242113	25.812672
177.043557	6126.934377	25.817690
177.319580	6130.876234	25.822708
177.630381	6147.486182	25.827725
177.728722	6145.000417	25.832743
178.038283	6155.952992	25.837760
177.909693	6157.896653	25.842778
178.267891	6174.394028	25.847796
178.460013	6187.809317	25.852813
178.707603	6175.647913	25.857831
178.889130	6191.000972	25.862848
178.684997	6202.983783	25.867866
179.057296	6210.228833	25.872884
179.496420	6225.136010	25.877901
179.207488	6233.030853	25.882919
179.507300	6239.349836	25.887936
179.370797	6248.470227	25.892954
180.003306	6265.107382	25.897972
180.171542	6277.985591	25.902989
180.536970	6286.421942	25.908007
180.854570	6290.575921	25.913024
180.866567	6302.945993	25.918042
180.903223	6297.282034	25.923060
181.403489	6317.242150	25.928077
181.482796	6318.014057	25.933095
181.358466	6317.110486	25.938112
181.345071	6332.263594	25.943130
181.991260	6351.603350	25.948148
181.720303	6353.670634	25.953165
182.217375	6376.310139	25.958183
182.421468	6381.297360	25.963200
182.519849	6391.667542	25.968218
182.929922	6396.869566	25.973236
183.344169	6417.565535	25.978253
183.494572	6419.693038	25.983271
183.457421	6412.373014	25.988288
183.710246	6411.618092	25.993306
183.880444	6425.538945	25.998324
184.051280	6439.374638	26.003341
184.322764	6449.087656	26.008359
184.490756	6433.308949	26.013376
184.572529	6435.558873	26.018394
184.748417	6460.509075	26.023412
184.755301	6453.198283	26.028429
184.850579	6465.223094	26.033447
185.389719	6477.712404	26.038464
185.139563	6494.291129	26.043482
185.617160	6490.950936	26.048500
185.657004	6510.054146	26.053517
186.033698	6521.650402	26.058535
186.337944	6516.377641	26.063552
186.118661	6527.161243	26.068570
186.496829	6534.200681	26.073588
186.640056	6546.963526	26.078605
186.620784	6551.932641	26.083623
186.753456	6556.788388	26.088640
187.034015	6581.871895	26.093658
187.268268	6568.362355	26.098676
187.401164	6582.984235	26.103693
187.614982	6603.082712	26.108711
187.674595	6606.348470	26.113728
187.510910	6609.324316	26.118746
187.386003	6635.915658	26.123764
188.053232	6647.714387	26.128781
188.023102	6666.808890	26.133799
188.576604	6676.400535	26.138816
188.837806	6696.651970	26.143834
189.395600	6699.424118	26.148852
189.536489	6710.118290	26.153869
189.673566	6723.781808	26.158887
190.143271	6718.384708	26.163904
190.211367	6722.834521	26.168922
189.962865	6732.246261	26.173940
190.337183	6756.761583	26.178957
190.626562	6755.497276	26.183975
191.240521	6765.656327	26.188992
191.086021	6781.259350	26.194010
191.242713	6785.416468	26.199028
191.652817	6787.317503	26.204045
191.424905	6784.536710	26.209063
191.827960	6796.876301	26.214080
192.060327	6820.080122	26.219098
191.803289	6815.711477	26.224116
192.023725	6839.988533	26.229133
192.154889	6855.876737	26.234151
192.706221	6862.922315	26.239168
192.999026	6885.187562	26.244186
193.442777	6881.028987	26.249204
193.797703	6882.404339	26.254221
193.705815	6897.779713	26.259239
193.998137	6907.144563	26.264256
193.934708	6907.232796	26.269274
194.460305	6906.277527	26.274292
194.374773	6910.017137	26.279309
194.254472	6926.655158	26.284327
194.662076	6927.301071	26.289344
194.349112	6946.786156	26.294362
194.917670	6949.718042	26.299380
195.378448	6967.010569	26.304397
195.096964	6986.841796	26.309415
195.625397	6989.133648	26.314432
195.799855	7000.148557	26.319450
195.932482	7018.798283	26.324468
196.243621	7017.784775	26.329485
196.090859	7029.784909	26.334503
196.557817	7041.329584	26.339520
196.826887	7055.853740	26.344538
196.965052	7066.034246	26.349556
197.306971	7080.389617	26.354573
197.479506	7079.721999	26.359591
197.890555	7089.596626	26.364608
197.876151	7102.668790	26.369626
197.846043	7116.195695	26.374644
198.153674	7125.475433	26.379661
198.135328	7135.377847	26.384679
198.481827	7131.006091	26.389696
198.816892	7161.607103	26.394714
198.940475	7175.755308	26.399732
198.892674	7176.947656	26.404749
198.945416	7189.346331	26.409767
199.612407	7193.073288	26.414784
199.774648	7204.315640	26.419802
199.920644	7209.131572	26.424820
200.426571	7220.762087	26.429837
200.373120	7230.272588	26.434855
200.700589	7226.347426	26.439872
200.837203	7234.390509	26.444890
200.869593	7242.256288	26.449908
201.207354	7246.319751	26.454925
200.989837	7249.346373	26.459943
201.371821	7267.016973	26.464960
201.585993	7282.437365	26.469978
201.284207	7290.019779	26.474996
201.998781	7302.277477	26.480013
201.917081	7332.449986	26.485031
202.576483	7339.351070	26.490048
202.901589	7347.192865	26.495066
203.036243	7352.194251	26.500084
203.389030	7367.346019	26.505101
203.456615	7384.450452	26.510119
203.724237	7370.867755	26.515136
203.786058	7380.342722	26.520154
204.011219	7400.934218	26.525172
204.292726	7392.623633	26.530189
204.407700	7405.625004	26.535207
204.624800	7420.625990	26.540224
204.545681	7432.368473	26.545242
204.546571	7440.716912	26.550260
205.043352	7453.954446	26.555277
205.120073	7478.071944	26.560295
205.651112	7484.083758	26.565312
205.766588	7493.759439	26.570330
205.817747	7508.402002	26.575348
206.331208	7521.638407	26.580365
206.224682	7535.762007	26.585383
206.696856	7541.290483	26.590400
206.847033	7547.962448	26.595418
206.990409	7569.350680	26.600436
207.463613	7570.112584	26.605453
207.418746	7573.513205	26.610471
208.008047	7594.173070	26.615488
207.966010	7611.494396	26.620506
207.997690	7607.522793	26.625524
208.433048	7625.604018	26.630541
208.489604	7625.813392	26.635559
209.008963	7627.399481	26.640576
209.356373	7648.150659	26.645594
208.970837	7670.229178	26.650612
209.332198	7674.173839	26.655629
209.499580	7686.787876	26.660647
209.699978	7693.092391	26.665664
209.999098	7695.408919	26.670682
210.243418	7714.659326	26.675700
210.725583	7721.911305	26.680717
210.792982	7737.780225	26.685735
211.147431	7746.347573	26.690752
211.398835	7757.273861	26.695770
211.544807	7750.350638	26.700788
211.687088	7762.415913	26.705805
211.662758	7780.741193	26.710823
212.118194	7779.486344	26.715840
212.316179	7781.270587	26.720858
212.260343	7805.218321	26.725876
212.734893	7814.310925	26.730893
212.613766	7825.525791	26.735911
213.098903	7827.482279	26.740928
212.916652	7843.151588	26.745946
213.289320	7851.235467	26.750964
213.540424	7861.819219	26.755981
213.458595	7872.688892	26.760999
213.825341	7879.800143	26.766016
213.935384	7891.701492	26.771034
214.165319	7913.104215	26.776052
214.620420	7911.565044	26.781069
214.676832	7932.450624	26.786087
214.705566	7940.243307	26.791104
214.885537	7948.791596	26.796122
214.837311	7973.161329	26.801140
215.245685	7981.297656	26.806157
215.471167	7998.781503	26.811175
215.812193	8021.525600	26.816192
216.028509	8033.485085	26.821210
216.174250	8055.714873	26.826228
216.926308	8056.435371	26.831245
216.748479	8074.223169	26.836263
217.116236	8083.984272	26.841280
217.368206	8100.725741	26.846298
217.517035	8119.481206	26.851316
218.138755	8117.548927	26.856333
217.840557	8130.401081	26.861351
218.210322	8143.623194	26.866368
218.923554	8148.956010	26.871386
218.912840	8166.785568	26.876404
219.215204	8179.131089	26.881421
219.214761	8192.228618	26.886439
218.989131	8194.839258	26.891456
219.806132	8205.073549	26.896474
219.671104	8221.218294	26.901492
220.046817	8234.418228	26.906509
220.156987	8248.058363	26.911527
220.266550	8259.971882	26.916544
220.676001	8281.417856	26.921562
220.749569	8296.207891	26.926580
220.991435	8302.916986	26.931597
221.306255	8319.178786	26.936615
221.404160	8336.563597	26.941632
221.907375	8330.018974	26.946650
221.904879	8349.515817	26.951668
222.678284	8349.617570	26.956685
222.924126	8367.312717	26.961703
222.738465	8376.180926	26.966720
223.369376	8380.164648	26.971738
223.361629	8386.841049	26.976756
223.830131	8408.513743	26.981773
224.002886	8414.130691	26.986791
223.894683	8417.143374	26.991808
224.320393	8417.578394	26.996826
224.687604	8438.941768	27.001844
224.555650	8440.716895	27.006861
224.748350	8451.573815	27.011879
225.131462	8476.284121	27.016896
225.530358	8477.479035	27.021914
225.291579	8495.668113	27.026932
225.500840	8505.259562	27.031949
226.050090	8516.506526	27.036967
226.459318	8538.792628	27.041984
226.384635	8538.666887	27.047002
226.260437	8550.188416	27.052020
226.614011	8555.560425	27.057037
226.837782	8576.301768	27.062055
226.992913	8603.171435	27.067072
227.674454	8600.662803	27.072090
227.372871	8629.851648	27.077108
227.816152	8625.576120	27.082125
228.112659	8645.779291	27.087143
228.149218	8667.152013	27.092160
228.319134	8664.643771	27.097178
228.491315	8691.594266	27.102196
228.624520	8697.297424	27.107213
229.299202	8713.854552	27.112231
229.388790	8735.986658	27.117248
229.812469	8726.843605	27.122266
229.790093	8747.581799	27.127284
230.132460	8749.005879	27.132301
230.473185	8761.021730	27.137319
230.623571	8788.188693	27.142336
230.902963	8797.426818	27.147354
230.868816	8797.653586	27.152372
231.259143	8804.472239	27.157389
231.527292	8818.793338	27.162407
231.205251	8847.201347	27.167424
231.739850	8852.114946	27.172442
231.746658	8875.003024	27.177460
232.147999	8885.275052	27.182477
232.312668	8907.329581	27.187495
232.583032	8922.147490	27.192512
232.998508	8933.950216	27.197530
233.412779	8946.295138	27.202548
233.604159	8962.056520	27.207565
234.172190	8965.424520	27.212583
234.106348	8992.251852	27.217600
234.863809	9001.592938	27.222618
234.872045	9009.803906	27.227636
235.295469	9013.101320	27.232653
235.612523	9020.644345	27.237671
235.889543	9033.008115	27.242688
235.780650	9023.737987	27.247706
235.703584	9039.491100	27.252724
236.243901	9046.592263	27.257741
236.487966	9057.705787	27.262759
236.501465	9068.692050	27.267776
236.947373	9089.034909	27.272794
236.917392	9105.650003	27.277812
237.118400	9118.783480	27.282829
237.379837	9128.127181	27.287847
237.107793	9145.909703	27.292864
237.942917	9152.244443	27.297882
238.044104	9172.694888	27.302900
238.558119	9184.198673	27.307917
238.709250	9206.719073	27.312935
238.869451	9211.885403	27.317952
239.201996	9218.030786	27.322970
239.273378	9243.367387	27.327988
239.552105	9246.735281	27.333005
239.783558	9273.515448	27.338023
239.943054	9282.640564	27.343040
240.469718	9292.959073	27.348058
240.279069	9301.494594	27.353076
240.599606	9320.461744	27.358093
240.644943	9332.471775	27.363111
240.931205	9354.752584	27.368128
241.472672	9367.679442	27.373146
241.521374	9399.942400	27.378164
242.059907	9398.865115	27.383181
242.255772	9412.017803	27.388199
242.171038	9428.153071	27.393216
242.500931	9450.600895	27.398234
242.819399	9463.162964	27.403252
243.128344	9485.421293	27.408269
243.372053	9494.601917	27.413287
243.158470	9516.218065	27.418304
243.684037	9527.011163	27.423322
244.133549	9554.036949	27.428340
244.588137	9559.172782	27.433357
244.885282	9571.554120	27.438375
244.722877	9587.592899	27.443392
244.893500	9593.826680	27.448410
245.305848	9605.760409	27.453428
245.599544	9626.258346	27.458445
245.873963	9630.956067	27.463463
245.932678	9646.285516	27.468480
246.635079	9660.182549	27.473498
246.778776	9664.774293	27.478516
246.973755	9675.908189	27.483533
247.490873	9685.079117	27.488551
247.550839	9693.138490	27.493568
247.668508	9700.340631	27.498586
247.762311	9715.220012	27.503604
247.970439	9734.916867	27.508621
248.289659	9744.428621	27.513639
248.407126	9754.907336	27.518656
248.595847	9779.698313	27.523674
248.703129	9792.048223	27.528692
249.020571	9803.455004	27.533709
249.529422	9823.395257	27.538727
249.779088	9844.263945	27.543744
250.090635	9849.120239	27.548762
250.400146	9870.541557	27.553780
250.558806	9876.136142	27.558797
250.931095	9899.843604	27.563815
250.789078	9905.924422	27.568832
251.355453	9922.559821	27.573850
252.013053	9932.482068	27.578868
251.821752	9945.275430	27.583885
252.040707	9961.973103	27.588903
252.274692	9973.551385	27.593920
252.432219	9994.423701	27.598938
252.698112	10006.519053	27.603956
253.182715	10028.875112	27.608973
253.398735	10035.742054	27.613991
253.283836	10057.537185	27.619008
253.578742	10063.707246	27.624026
254.165937	10089.009433	27.629044
254.319154	10112.082238	27.634061
255.044582	10123.318509	27.639079
255.137732	10134.780772	27.644096
255.158813	10147.443812	27.649114
255.326034	10158.286412	27.654132
255.916350	10175.579104	27.659149
256.153527	10191.234058	27.664167
256.073830	10202.618621	27.669184
256.616056	10209.413523	27.674202
256.655174	10231.734881	27.679220
256.730183	10250.949398	27.684237
257.798222	10249.947500	27.689255
257.808296	10281.935785	27.694272
258.019525	10281.947846	27.699290
258.271933	10289.695981	27.704308
257.863117	10302.354668	27.709325
258.609308	10305.904612	27.714343
258.501826	10334.750855	27.719360
259.314885	10341.218148	27.724378
259.450886	10357.566768	27.729396
259.530578	10370.409364	27.734413
259.861425	10379.107304	27.739431
259.996961	10407.555771	27.744448
260.308834	10410.663165	27.749466
260.782444	10431.815413	27.754484
261.053143	10436.811006	27.759501
261.007707	10454.212381	27.764519
261.043449	10479.645854	27.769536
261.465078	10490.977578	27.774554
261.608372	10503.741998	27.779572
261.858748	10529.340136	27.784589
262.202775	10532.199573	27.789607
262.622467	10552.007374	27.794624
262.804571	10559.327654	27.799642
263.024815	10574.737611	27.804660
263.425461	10587.057694	27.809677
264.043035	10584.837472	27.814695
263.840620	10598.163416	27.819712
264.264810	10616.297148	27.824730
264.474326	10623.571952	27.829748
264.629694	10653.672068	27.834765
265.285161	10648.770002	27.839783
265.188500	10670.685060	27.844800
265.355557	10685.883325	27.849818
265.603375	10694.905597	27.854836
265.842807	10709.171685	27.859853
266.669897	10730.220121	27.864871
266.909928	10743.101079	27.869888
266.833753	10758.930571	27.874906
267.306708	10772.036144	27.879924
267.201838	10786.729586	27.884941
267.934078	10795.670157	27.889959
268.008117	10813.874674	27.894976
268.381567	10825.532908	27.899994
268.574852	10840.154987	27.905012
268.919632	10853.609596	27.910029
269.273704	10869.033924	27.915047
269.326980	10882.990619	27.920064
269.679279	10895.966570	27.925082
270.389721	10903.688036	27.930100
270.138298	10931.074821	27.935117
270.276764	10936.480090	27.940135
270.470314	10950.303324	27.945152
270.668891	10963.170835	27.950170
271.300233	10977.684289	27.955188
271.419275	10996.874285	27.960205
271.552284	11019.457735	27.965223
271.725306	11034.776675	27.970240
272.343563	11061.819611	27.975258
272.465707	11071.014167	27.980276
272.805433	11092.137444	27.985293
273.130016	11099.374508	27.990311
273.429122	11118.411935	27.995328
273.876204	11139.933506	28.000346
274.274197	11152.701979	28.005364
274.203180	11162.476925	28.010381
274.906918	11168.187378	28.015399
275.172039	11183.915096	28.020416
275.131025	11210.742796	28.025434
275.589294	11214.680184	28.030452
275.636941	11225.692992	28.035469
276.225914	11236.463358	28.040487
276.630340	11254.979267	28.045504
276.833367	11269.942066	28.050522
277.055729	11274.949073	28.055540
276.880408	11282.910305	28.060557
277.052279	11294.685760	28.065575
277.358637	11315.906248	28.070592
277.290567	11332.689881	28.075610
278.139725	11344.942611	28.080628
278.006652	11373.309600	28.085645
278.397128	11393.630675	28.090663
279.103099	11407.218209	28.095680
279.323963	11418.591698	28.100698
279.940632	11439.898080	28.105716
279.930904	11452.463240	28.110733
280.250758	11447.867040	28.115751
280.663869	11470.091175	28.120768
280.966213	11482.880470	28.125786
281.459067	11481.624679	28.130804
281.065789	11496.257770	28.135821
281.350832	11498.186394	28.140839
281.843463	11512.518438	28.145856
281.875121	11523.606583	28.150874
282.189615	11543.587444	28.155892
282.342520	11569.261669	28.160909
282.415097	11576.130951	28.165927
282.820925	11598.885939	28.170944
282.864954	11616.588916	28.175962
283.518402	11634.912766	28.180980
283.384904	11656.214383	28.185997
283.957917	11667.532912	28.191015
284.246776	11690.007984	28.196032
284.382661	11709.854729	28.201050
284.969005	11724.251817	28.206068
285.034244	11747.457342	28.211085
285.762774	11768.074343	28.216103
285.798214	11774.637843	28.221120
286.126648	11794.054137	28.226138
286.329912	11808.836175	28.231156
286.550251	11827.279205	28.236173
287.099201	11848.992870	28.241191
287.631329	11864.656571	28.246208
287.599732	11880.905253	28.251226
288.290155	11893.791375	28.256244
288.589999	11915.685034	28.261261
288.637890	11924.490528	28.266279
288.699426	11945.845338	28.271296
289.037772	11957.956166	28.276314
289.345224	11976.509438	28.281332
290.070703	11996.802613	28.286349
290.027857	12016.611554	28.291367
290.546315	12020.901626	28.296384
290.666047	12030.803108	28.301402
291.070989	12042.491680	28.306420
291.497586	12072.171337	28.311437
292.160179	12068.745826	28.316455
291.853869	12088.804899	28.321472
292.159160	12103.579775	28.326490
292.352910	12112.644883	28.331508
292.573582	12133.084817	28.336525
292.411387	12153.956898	28.341543
293.227526	12175.103592	28.346560
293.388233	12195.392791	28.351578
293.946870	12213.135738	28.356596
293.933137	12244.770177	28.361613
294.414524	12257.495781	28.366631
294.894632	12271.036333	28.371648
295.351989	12288.313908	28.376666
295.503586	12284.931958	28.381684
295.732972	12314.485537	28.386701
296.066265	12328.977053	28.391719
296.403956	12348.121429	28.396736
296.396465	12361.550503	28.401754
296.922469	12378.351928	28.406772
297.074651	12389.895056	28.411789
297.114311	12410.373178	28.416807
297.620266	12425.934596	28.421824
297.969274	12452.575297	28.426842
298.345453	12457.231005	28.431860
298.183746	12488.111919	28.436877
299.010406	12509.812024	28.441895
299.180998	12527.893748	28.446912
299.218710	12549.637814	28.451930
299.628076	12550.723371	28.456948
299.788142	12578.976179	28.461965
300.297263	12593.285968	28.466983
300.396812	12616.684043	28.472000
300.580386	12628.340338	28.477018
301.093659	12646.554585	28.482036
301.371799	12662.765389	28.487053
301.393376	12694.431104	28.492071
301.832944	12705.220880	28.497088
302.146949	12718.617525	28.502106
302.464692	12738.391301	28.507124
302.736258	12761.193782	28.512141
303.225425	12781.752412	28.517159
303.551615	12798.280039	28.522176
303.569285	12824.872180	28.527194
303.816240	12834.004530	28.532212
304.092164	12853.820037	28.537229
304.546230	12872.589609	28.542247
304.926132	12894.179791	28.547264
305.128898	12926.044476	28.552282
305.566119	12943.374936	28.557300
305.910203	12963.778153	28.562317
306.195798	12972.155614	28.567335
306.674174	12988.131881	28.572352
306.955152	13011.213673	28.577370
307.607356	13033.490208	28.582388
307.645624	13045.969857	28.587405
308.159886	13074.034097	28.592423
308.410415	13076.236539	28.597440
308.725106	13102.578250	28.602458
308.884475	13116.653262	28.607476
309.359170	13134.846075	28.612493
309.501484	13161.679743	28.617511
309.884915	13169.913461	28.622528
310.104765	13201.106073	28.627546
310.588630	13205.411647	28.632564
310.841705	13225.190414	28.637581
311.364821	13243.387943	28.642599
311.593463	13258.854222	28.647616
311.704717	13277.290160	28.652634
311.930400	13300.209733	28.657652
312.456840	13309.603407	28.662669
312.442365	13324.224290	28.667687
312.788015	13345.886930	28.672704
312.773277	13369.413743	28.677722
313.502339	13380.740745	28.682740
313.725774	13407.471560	28.687757
313.741459	13428.886334	28.692775
314.539758	13449.289054	28.697792
314.711951	13486.641177	28.702810
315.054080	13502.892660	28.707828
315.588164	13521.827825	28.712845
315.972236	13539.222877	28.717863
316.644468	13543.087607	28.722880
316.455307	13560.883301	28.727898
316.979742	13583.689209	28.732916
317.254920	13593.271203	28.737933
317.484315	13612.264782	28.742951
317.900222	13615.946586	28.747968
318.044527	13649.086313	28.752986
318.303490	13667.186195	28.758004
318.968090	13681.745437	28.763021
319.087387	13696.270439	28.768039
319.522380	13706.919800	28.773056
319.969101	13730.140659	28.778074
320.073140	13742.903093	28.783092
320.569198	13757.912671	28.788109
320.109198	13774.219958	28.793127
320.596895	13798.928198	28.798144
321.049120	13819.593544	28.803162
321.279325	13836.082951	28.808180
321.531713	13849.624687	28.813197
321.603427	13872.436584	28.818215
322.171566	13893.584016	28.823232
322.603166	13911.151267	28.828250
322.760167	13936.459754	28.833268
322.709382	13954.805073	28.838285
323.078415	13979.922507	28.843303
323.989580	14008.780031	28.848320
324.090494	14018.014443	28.853338
324.579366	14047.542399	28.858356
325.034743	14057.588144	28.863373
324.983777	14086.641294	28.868391
325.620422	14100.171651	28.873408
326.061511	14127.777001	28.878426
326.687540	14139.496688	28.883444
326.802435	14158.052797	28.888461
327.109287	14170.638577	28.893479
327.296413	14184.263890	28.898496
327.625098	14207.840665	28.903514
328.177132	14222.997437	28.908532
328.617435	14244.740169	28.913549
328.748026	14269.456214	28.918567
329.191555	14268.332901	28.923584
329.361986	14293.291407	28.928602
329.729443	14307.172246	28.933620
329.838740	14334.213463	28.938637
330.195771	14349.845503	28.943655
330.591046	14359.549917	28.948672
330.476665	14383.784999	28.953690
330.933666	14401.909657	28.958708
331.261950	14439.428825	28.963725
331.216454	14455.617748	28.968743
332.437439	14481.977176	28.973760
332.587661	14510.589573	28.978778
333.258203	14535.977906	28.983796
333.636478	14553.308803	28.988813
333.758346	14575.273319	28.993831
334.319419	14579.736703	28.998848
334.364835	14607.885906	29.003866
334.900650	14613.215605	29.008884
335.346712	14632.280109	29.013901
335.550856	14648.631222	29.018919
335.828502	14663.832241	29.023936
336.233938	14680.878232	29.028954
336.766361	14712.546836	29.033972
337.301975	14718.913683	29.038989
337.533720	14746.671357	29.044007
337.604722	14739.347781	29.049024
337.805587	14766.773312	29.054042
338.459141	14783.735791	29.059060
338.862658	14797.598470	29.064077
338.655398	14811.554366	29.069095
339.455852	14833.203599	29.074112
339.546195	14846.668957	29.079130
339.853344	14863.255416	29.084148
340.422563	14883.343223	29.089165
340.202558	14903.763417	29.094183
341.148987	14914.893178	29.099200
341.096089	14933.061836	29.104218
341.455555	14951.945604	29.109236
341.907804	14969.127575	29.114253
342.161604	15002.092726	29.119271
342.535103	15022.515713	29.124288
342.886904	15031.263127	29.129306
343.164003	15059.915375	29.134324
343.714403	15061.970740	29.139341
343.840539	15096.427749	29.144359
344.407907	15089.475797	29.149376
344.232569	15119.679876	29.154394
344.767986	15140.107735	29.159412
345.465526	15155.651092	29.164429
345.402207	15166.888248	29.169447
345.973011	15186.850073	29.174464
346.106186	15202.535738	29.179482
346.409859	15225.211827	29.184500
347.134263	15247.906580	29.189517
346.960765	15270.582896	29.194535
347.657067	15284.001914	29.199552
347.917674	15311.642282	29.204570
348.145443	15327.545683	29.209588
348.638271	15349.903776	29.214605
348.433827	15373.786396	29.219623
348.926652	15394.464351	29.224640
349.298909	15417.195553	29.229658
349.510378	15442.625018	29.234676
350.087785	15464.083457	29.239693
350.213499	15493.327363	29.244711
350.725313	15512.216509	29.249728
351.246234	15536.094376	29.254746
351.419769	15571.157670	29.259764
351.954483	15587.065689	29.264781
351.933522	15620.826243	29.269799
352.161771	15643.154442	29.274816
352.889379	15672.756149	29.279834
352.990663	15702.489939	29.284852
353.787371	15724.218206	29.289869
354.110519	15754.980886	29.294887
354.721572	15783.046366	29.299904
354.974604	15802.593396	29.304922
355.144663	15828.238370	29.309940
355.890020	15843.569559	29.314957
356.427680	15862.101758	29.319975
356.598947	15894.669385	29.324992
356.868736	15908.741130	29.330010
357.027492	15926.948360	29.335028
357.438228	15948.565842	29.340045
357.929297	15959.982897	29.345063
358.161383	15979.883527	29.350080
358.299071	16015.401346	29.355098
358.483556	16043.840503	29.360116
359.466211	16069.523178	29.365133
359.778210	16095.597456	29.370151
360.124970	16113.241007	29.375168
360.677392	16131.265093	29.380186
360.723454	16154.517866	29.385204
361.138978	16174.755638	29.390221
361.464321	16202.695730	29.395239
361.769365	16223.658006	29.400256
362.081616	16249.920060	29.405274
362.329132	16272.944203	29.410292
362.625507	16294.921538	29.415309
362.697475	16327.818551	29.420327
363.397096	16357.341005	29.425344
364.215952	16381.796569	29.430362
364.420423	16403.568580	29.435380
364.774513	16415.821978	29.440397
365.172859	16444.841178	29.445415
365.428374	16462.016288	29.450432
366.073342	16476.333800	29.455450
366.361077	16504.988376	29.460468
366.674626	16524.318177	29.465485
366.961698	16545.389447	29.470503
367.290149	16563.258766	29.475520
367.397432	16590.181067	29.480538
367.831247	16610.993268	29.485556
368.087689	16621.149176	29.490573
368.491552	16653.383461	29.495591
368.784845	16680.609299	29.500608
369.502417	16698.869916	29.505626
369.231638	16724.147873	29.510644
369.985433	16754.248455	29.515661
370.494035	16781.549168	29.520679
370.479136	16795.525341	29.525696
371.021243	16819.756232	29.530714
371.341291	16842.580007	29.535732
371.703530	16874.704965	29.540749
372.280183	16899.510339	29.545767
372.589320	16925.461871	29.550784
372.903602	16938.480455	29.555802
373.053212	16981.087086	29.560820
373.579762	17000.317564	29.565837
374.301277	17035.999468	29.570855
374.457945	17057.717198	29.575872
375.102067	17080.273287	29.580890
375.250944	17106.570044	29.585908
375.900197	17135.489030	29.590925
375.857448	17148.544798	29.595943
376.113377	17179.169924	29.600960
376.931196	17194.370582	29.605978
376.845649	17243.046321	29.610996
377.508038	17260.902114	29.616013
377.814129	17290.842890	29.621031
378.070057	17316.977239	29.626048
378.968422	17347.534188	29.631066
378.839002	17368.900852	29.636084
379.622907	17394.074642	29.641101
379.874883	17424.514864	29.646119
379.977509	17446.383918	29.651136
380.633778	17463.815324	29.656154
381.134462	17502.279240	29.661172
381.622290	17526.420838	29.666189
381.771495	17545.646614	29.671207
382.382621	17572.712548	29.676224
382.743253	17588.520473	29.681242
382.598790	17620.068649	29.686260
383.381377	17640.280573	29.691277
383.728590	17666.868552	29.696295
383.851628	17700.289500	29.701312
384.896051	17729.525613	29.706330
384.794313	17751.741016	29.711348
385.246747	17773.078114	29.716365
385.729523	17801.198204	29.721383
385.946404	17837.130869	29.726400
386.704118	17864.057942	29.731418
386.987030	17885.141061	29.736436
387.208078	17904.245014	29.741453
387.652861	17933.810880	29.746471
387.712014	17969.200846	29.751488
388.529965	17987.578698	29.756506
388.642191	18020.286383	29.761524
389.213059	18050.652906	29.766541
389.501406	18071.216718	29.771559
389.628563	18107.317728	29.776576
390.529739	18131.945128	29.781594
390.600072	18158.589174	29.786612
391.297289	18176.353488	29.791629
391.704558	18199.339680	29.796647
392.040261	18219.946285	29.801664
392.479139	18247.639297	29.806682
392.870943	18278.401605	29.811700
392.904295	18301.416712	29.816717
393.569552	18324.018292	29.821735
393.943847	18355.297563	29.826752
394.504065	18363.042739	29.831770
394.635801	18396.387973	29.836788
395.046070	18409.461192	29.841805
395.498453	18433.004613	29.846823
395.509462	18457.913811	29.851840
395.968462	18470.871814	29.856858
396.133413	18512.113028	29.861876
396.497268	18537.135787	29.866893
397.274757	18568.381839	29.871911
397.435762	18594.083031	29.876928
397.699513	18618.690523	29.881946
397.661229	18651.716001	29.886964
398.420801	18681.850658	29.891981
398.923874	18719.347453	29.896999
399.193529	18757.658595	29.902016
399.807429	18780.619276	29.907034
400.134372	18825.283825	29.912052
400.359188	18858.862088	29.917069
401.213684	18890.862181	29.922087
401.351850	18923.871608	29.927104
401.463032	18956.329056	29.932122
401.911936	18994.806564	29.937140
402.593106	19028.604455	29.942157
403.319848	19061.619224	29.947175
403.606594	19105.846595	29.952192
404.260242	19115.184718	29.957210
404.481003	19159.572921	29.962228
405.125846	19176.553979	29.967245
405.327635	19200.943985	29.972263
405.839607	19226.515547	29.977280
406.228131	19251.938888	29.982298
406.816916	19278.539910	29.987316
407.274732	19311.005321	29.992333
407.762474	19328.487072	29.997351
407.659263	19367.613327	30.002368
408.428824	19390.150221	30.007386
408.718591	19422.025648	30.012404
409.033735	19455.686330	30.017421
409.772839	19477.481094	30.022439
409.634503	19510.155905	30.027456
410.343095	19536.425352	30.032474
410.365323	19578.150014	30.037492
411.247563	19611.557928	30.042509
411.617746	19631.060121	30.047527
412.097802	19659.483344	30.052544
412.616826	19691.989815	30.057562
413.025801	19716.004167	30.062580
413.113672	19749.583229	30.067597
413.982764	19768.000311	30.072615
413.875010	19796.175767	30.077632
414.453979	19819.460554	30.082650
414.508015	19854.191606	30.087668
415.162762	19876.705590	30.092685
415.669994	19915.768362	30.097703
415.632741	19951.165858	30.102720
416.641888	19979.940364	30.107738
416.977297	20013.920440	30.112756
417.093495	20048.031458	30.117773
417.694115	20084.145091	30.122791
417.899839	20115.606903	30.127808
418.227651	20142.950930	30.132826
418.405119	20182.291197	30.137844
418.674023	20222.434695	30.142861
419.354393	20260.843697	30.147879
419.579410	20300.985185	30.152896
420.426334	20331.597121	30.157914
420.804596	20364.348918	30.162932
421.385273	20399.137418	30.167949
422.067009	20419.750960	30.172967
422.368872	20453.094202	30.177984
422.518054	20476.187723	30.183002
422.715695	20506.013460	30.188020
423.482941	20536.662606	30.193037
423.840643	20569.735113	30.198055
423.988449	20610.818771	30.203072
424.286467	20636.822058	30.208090
424.758694	20675.477725	30.213108
424.990187	20711.521350	30.218125
425.592331	20747.057515	30.223143
426.107764	20783.221434	30.228160
426.657489	20820.038810	30.233178
426.926599	20850.334219	30.238196
427.447114	20891.735289	30.243213
428.037026	20922.285195	30.248231
428.273393	20961.634877	30.253248
428.657592	20992.647815	30.258266
429.120716	21033.549456	30.263284
429.670456	21066.663688	30.268301
430.361970	21099.581086	30.273319
430.319808	21143.538711	30.278336
430.640701	21175.541601	30.283354
431.104531	21212.571138	30.288372
431.621304	21258.377513	30.293389
432.089018	21291.214065	30.298407
432.489555	21345.355584	30.303424
432.974158	21372.524293	30.308442
433.694394	21415.919707	30.313460
434.155785	21456.737516	30.318477
434.498360	21474.053164	30.323495
435.113372	21524.280969	30.328512
435.385154	21559.063064	30.333530
436.089087	21596.250805	30.338548
436.076174	21633.079492	30.343565
437.060305	21647.736378	30.348583
437.359987	21694.065501	30.353600
438.196001	21731.305790	30.358618
438.493567	21758.515532	30.363636
438.848288	21795.353115	30.368653
439.288897	21824.147603	30.373671
439.510611	21860.744016	30.378688
440.096540	21897.876262	30.383706
440.720757	21924.710553	30.388724
440.995825	21960.874196	30.393741
441.499232	21992.282361	30.398759
441.412986	22021.583797	30.403776
441.606869	22061.077093	30.408794
442.410983	22094.793005	30.413812
442.796981	22143.693456	30.418829
443.431072	22177.913865	30.423847
443.609068	22216.259079	30.428864
444.149219	22259.880407	30.433882
444.896468	22294.631060	30.438900
444.966497	22337.762727	30.443917
445.590904	22366.105133	30.448935
446.212262	22415.777911	30.453952
446.378048	22447.646458	30.458970
447.096911	22482.206666	30.463988
447.066443	22534.952115	30.469005
447.704261	22572.706414	30.474023
448.229377	22612.862071	30.479040
448.416700	22643.189990	30.484058
448.905354	22689.033270	30.489076
449.236192	22732.933286	30.494093
450.088281	22759.001104	30.499111
450.248315	22806.099074	30.504128
450.500656	22852.786103	30.509146
450.779302	22885.481999	30.514164
451.088126	22924.348029	30.519181
451.869548	22957.252588	30.524199
452.202555	23014.424032	30.529216
452.801797	23047.117648	30.534234
453.401270	23084.284942	30.539252
453.326787	23132.307258	30.544269
454.549652	23167.845138	30.549287
455.006550	23204.075952	30.554304
455.227153	23241.426127	30.559322
455.596934	23268.918067	30.564340
455.772797	23316.221402	30.569357
456.279294	23359.564121	30.574375
456.965511	23401.801749	30.579392
457.207459	23447.381971	30.584410
457.964339	23492.935452	30.589428
458.331999	23536.823561	30.594445
458.918159	23577.483898	30.599463
459.551817	23616.471217	30.604480
459.668062	23661.650190	30.609498
460.140920	23704.808542	30.614516
460.565632	23755.850296	30.619533
461.038644	23787.452889	30.624551
461.766144	23834.007206	30.629568
462.054492	23886.014938	30.634586
462.472848	23927.252659	30.639604
462.861291	23975.576060	30.644621
463.630712	24013.333856	30.649639
463.881460	24074.438106	30.654656
464.203453	24112.106151	30.659674
465.098612	24154.653274	30.664692
464.954277	24204.797023	30.669709
465.679887	24254.964127	30.674727
465.976883	24298.541021	30.679744
466.459734	24335.744532	30.684762
467.508740	24381.152693	30.689780
467.649351	24433.448318	30.694797
468.360319	24454.806299	30.699815
468.766254	24505.329823	30.704832
469.019206	24550.977398	30.709850
469.842373	24599.971830	30.714868
470.072338	24643.175896	30.719885
470.838416	24688.057646	30.724903
471.210070	24727.305332	30.729920
471.560987	24772.107757	30.734938
472.477275	24812.587086	30.739956
472.300847	24862.422652	30.744973
473.129060	24902.673900	30.749991
473.425366	24950.046977	30.755008
474.118435	25001.454919	30.760026
474.599080	25042.681864	30.765044
474.836391	25077.656626	30.770061
475.422812	25120.503263	30.775079
475.929400	25169.024960	30.780096
476.272965	25213.574265	30.785114
476.795035	25251.978172	30.790132
476.838726	25307.569697	30.795149
477.759982	25353.260220	30.800167
478.168832	25398.439505	30.805184
478.413696	25450.982774	30.810202
479.109043	25492.503310	30.815220
479.303662	25555.379022	30.820237
480.341490	25605.435328	30.825255
480.644610	25635.959145	30.830272
480.890749	25692.802196	30.835290
481.285155	25726.257156	30.840308
481.469241	25776.373217	30.845325
481.907895	25825.980464	30.850343
482.614475	25873.322890	30.855360
483.136963	25919.279622	30.860378
483.715265	25954.467856	30.865396
483.999221	26010.864093	30.870413
484.481933	26063.868255	30.875431
485.131910	26095.956822	30.880448
485.562421	26155.546712	30.885466
485.895860	26197.674536	30.890484
486.450453	26249.878784	30.895501
486.657998	26294.551174	30.900519
487.583437	26338.086024	30.905536
488.102581	26383.751187	30.910554
489.075963	26426.887183	30.915572
489.095659	26475.376409	30.920589
490.083048	26519.715305	30.925607
490.422516	26555.575170	30.930624
490.837021	26603.646131	30.935642
491.110082	26641.539156	30.940660
491.599612	26695.212868	30.945677
492.150174	26738.851767	30.950695
493.050757	26783.615784	30.955712
493.459531	26831.741953	30.960730
493.972482	26863.759987	30.965748
494.504595	26909.291904	30.970765
494.718750	26944.567647	30.975783
495.373844	26999.577651	30.980800
495.641575	27045.276697	30.985818
496.167611	27081.302360	30.990836
496.426860	27145.681019	30.995853
497.013549	27189.848193	31.000871
497.626385	27240.522148	31.005888
497.915455	27294.391766	31.010906
498.652944	27348.439720	31.015924
498.878679	27403.581986	31.020941
499.236199	27457.235736	31.025959
499.948946	27506.837148	31.030976
500.238966	27556.221580	31.035994
500.917603	27614.926842	31.041012
501.205539	27682.577238	31.046029
501.877205	27739.034820	31.051047
502.527153	27787.221526	31.056064
502.988971	27848.345214	31.061082
503.513705	27895.540291	31.066100
503.887164	27945.871042	31.071117
504.571721	28005.472572	31.076135
505.449237	28058.171439	31.081152
505.521034	28110.010050	31.086170
506.388911	28153.095247	31.091188
506.694354	28199.377862	31.096205
507.371141	28253.334568	31.101223
508.131054	28305.533112	31.106240
508.129263	28353.201429	31.111258
508.572579	28401.884620	31.116276
508.933317	28460.017535	31.121293
509.787008	28513.052973	31.126311
510.870956	28553.989706	31.131328
510.764372	28609.809113	31.136346
511.221076	28650.994980	31.141364
512.151605	28703.339999	31.146381
512.211558	28751.393537	31.151399
513.046191	28803.959789	31.156416
513.677111	28853.401907	31.161434
514.180705	28895.034889	31.166452
514.447197	28938.322490	31.171469
515.025606	28990.755027	31.176487
515.818047	29039.729266	31.181504
516.297833	29094.661322	31.186522
517.203380	29133.351107	31.191540
517.166348	29173.304309	31.196557
517.720599	29212.330026	31.201575
518.129442	29249.682545	31.206592
518.441287	29302.453529	31.211610
518.833798	29344.061791	31.216628
519.063034	29390.612564	31.221645
519.677077	29432.313734	31.226663
520.230369	29483.814885	31.231680
520.622811	29541.204730	31.236698
521.298305	29590.941280	31.241716
521.198165	29652.820496	31.246733
522.194457	29711.808370	31.251751
522.799925	29769.933536	31.256768
523.105119	29825.685523	31.261786
523.818214	29882.957176	31.266804
524.296454	29936.049587	31.271821
524.692870	29985.868137	31.276839
525.385075	30049.526452	31.281856
525.675130	30112.835067	31.286874
526.600256	30164.330328	31.291892
526.945275	30228.744009	31.296909
527.765788	30283.090199	31.301927
528.118633	30342.883936	31.306944
528.527638	30402.252108	31.311962
529.020676	30460.470728	31.316980
529.713491	30518.050698	31.321997
530.091038	30580.889023	31.327015
531.003689	30635.249453	31.332032
531.388850	30689.047362	31.337050
531.608564	30746.318270	31.342068
532.618123	30805.231898	31.347085
532.798989	30863.140651	31.352103
533.678294	30919.507876	31.357120
534.131321	30981.394885	31.362138
534.502247	31033.706934	31.367156
535.320624	31092.552186	31.372173
535.737912	31160.696279	31.377191
536.700839	31205.395065	31.382208
537.020919	31265.358267	31.387226
537.670328	31308.026704	31.392244
538.554327	31361.781991	31.397261
538.786744	31413.565905	31.402279
539.573423	31469.517936	31.407296
540.011614	31518.384155	31.412314
540.695087	31562.101447	31.417332
541.165102	31620.703187	31.422349
541.722069	31661.526122	31.427367
542.229076	31714.716944	31.432384
542.782074	31770.923158	31.437402
543.013626	31812.614367	31.442420
543.534294	31873.483587	31.447437
543.994377	31924.843215	31.452455
544.674976	31977.561194	31.457472
545.134075	32038.292862	31.462490
546.148247	32075.838362	31.467508
546.121483	32135.795633	31.472525
546.874072	32205.074709	31.477543
547.362952	32250.671833	31.482560
547.628792	32312.035949	31.487578
548.379920	32371.161640	31.492596
548.966075	32417.790715	31.497613
549.637903	32481.981822	31.502631
550.460882	32515.123266	31.507648
551.524193	32569.770805	31.512666
551.834178	32608.506818	31.517684
552.350863	32655.924270	31.522701
552.641780	32707.998900	31.527719
553.247367	32751.372283	31.532736
553.833651	32793.571946	31.537754
554.268399	32829.993716	31.542772
554.684884	32878.053138	31.547789
555.396679	32922.154077	31.552807
556.076412	32976.538153	31.557824
556.497857	33017.168896	31.562842
556.870688	33056.829540	31.567860
557.434821	33100.059163	31.572877
557.838954	33153.542697	31.577895
558.341588	33200.818767	31.582912
558.953977	33260.200731	31.587930
559.222601	33314.082686	31.592948
559.716904	33366.270749	31.597965
560.029338	33432.626408	31.602983
560.703482	33495.268201	31.608000
561.302456	33555.499087	31.613018
561.284997	33618.801672	31.618036
562.297302	33688.463259	31.623053
562.909199	33748.815731	31.628071
563.424018	33803.052892	31.633088
563.968742	33878.778996	31.638106
564.334716	33946.339507	31.643124
565.193115	34011.691817	31.648141
565.444602	34076.324278	31.653159
566.374820	34145.524707	31.658176
566.957795	34210.576176	31.663194
567.656386	34278.783497	31.668212
568.413795	34326.364376	31.673229
568.769280	34393.394974	31.678247
569.753578	34453.110691	31.683264
570.390377	34512.391787	31.688282
571.094392	34567.862303	31.693300
571.529894	34622.465368	31.698317
572.272130	34680.561904	31.703335
572.757789	34734.655228	31.708352
573.218633	34791.864536	31.713370
573.723081	34856.360122	31.718388
574.157018	34895.459292	31.723405
575.066759	34966.379942	31.728423
575.554979	35011.864301	31.733440
576.109424	35082.692708	31.738458
576.594669	35141.088884	31.743476
577.079128	35196.619759	31.748493
577.489874	35265.121459	31.753511
578.274186	35333.305980	31.758528
578.540647	35393.853690	31.763546
579.238774	35461.756291	31.768564
579.821701	35522.170017	31.773581
580.256896	35596.406591	31.778599
581.034952	35655.279893	31.783616
581.658197	35722.261674	31.788634
582.317873	35793.176457	31.793652
582.779174	35842.943851	31.798669
583.443839	35906.949590	31.803687
583.949817	35968.936654	31.808704
584.793840	36046.623343	31.813722
584.987096	36103.508664	31.818740
585.671112	36160.357158	31.823757
586.100404	36238.940196	31.828775
586.989035	36291.503912	31.833792
587.832385	36364.527273	31.838810
587.956562	36427.320775	31.843828
588.628301	36478.873067	31.848845
589.093102	36549.532689	31.853863
589.928792	36616.975006	31.858880
590.271157	36688.163576	31.863898
590.956118	36754.507724	31.868916
591.841697	36801.284881	31.873933
592.284085	36867.770576	31.878951
592.437025	36919.028044	31.883968
592.919398	36975.221233	31.888986
593.653084	37042.565228	31.894004
594.480154	37101.798106	31.899021
594.961236	37165.343128	31.904039
595.333504	37230.755981	31.909056
596.040889	37292.944665	31.914074
596.559805	37363.128208	31.919092
597.380100	37428.710690	31.924109
597.867542	37495.535271	31.929127
598.118957	37551.960993	31.934144
598.967910	37613.167812	31.939162
599.905341	37687.812790	31.944180
600.580184	37748.928928	31.949197
600.713685	37821.371709	31.954215
601.544281	37880.022601	31.959232
602.192925	37950.893989	31.964250
602.721701	38024.702054	31.969268
603.539959	38086.221720	31.974285
603.862935	38150.534952	31.979303
604.875111	38209.740815	31.984320
605.572374	38269.118917	31.989338
606.112362	38340.830488	31.994356
606.589511	38402.830627	31.999373
607.330418	38463.228012	32.004391
608.103194	38535.725692	32.009408
608.808776	38595.144513	32.014426
609.121564	38662.488374	32.019444
609.825248	38719.240610	32.024461
610.461237	38784.012496	32.029479
611.123947	38846.251751	32.034496
612.235588	38905.901126	32.039514
612.545331	38975.980273	32.044532
613.172223	39029.384368	32.049549
613.445130	39094.855062	32.054567
614.181847	39160.040919	32.059584
614.875477	39227.437491	32.064602
615.331427	39300.009553	32.069620
615.994699	39351.296747	32.074637
616.396324	39429.276250	32.079655
617.093282	39503.706425	32.084672
617.323075	39557.682828	32.089690
618.429919	39629.709727	32.094708
619.213791	39695.729379	32.099725
619.646559	39766.015317	32.104743
620.358011	39828.960115	32.109760
621.511271	39892.785387	32.114778
621.695602	39955.871490	32.119796
622.253636	40018.618186	32.124813
622.913531	40087.046298	32.129831
623.218253	40149.289217	32.134848
624.155013	40210.973200	32.139866
624.441520	40290.847403	32.144884
624.899964	40361.251325	32.149901
625.268974	40449.001568	32.154919
626.166140	40507.533059	32.159936
627.419081	40581.051665	32.164954
627.812756	40660.186806	32.169972
628.455023	40715.916747	32.174989
628.965074	40783.131561	32.180007
629.637200	40859.446544	32.185024
630.202207	40922.002586	32.190042
630.797463	40996.266199	32.195060
631.406406	41061.454673	32.200077
632.150240	41136.448788	32.205095
632.873182	41199.115391	32.210112
633.582915	41259.205108	32.215130
633.526511	41326.850251	32.220148
634.185603	41386.917189	32.225165
635.193549	41456.195710	32.230183
635.656467	41518.221329	32.235200
636.284457	41585.138565	32.240218
636.629800	41652.942587	32.245236
637.247233	41722.027823	32.250253
637.641909	41799.364964	32.255271
638.260800	41873.325099	32.260288
639.423042	41952.442799	32.265306
639.705666	42031.169638	32.270324
640.327700	42098.973713	32.275341
641.110278	42180.627250	32.280359
640.988603	42250.022994	32.285376
642.042358	42331.341870	32.290394
642.581057	42424.980512	32.295412
643.495392	42504.005811	32.300429
644.313394	42587.982152	32.305447
644.983588	42670.742522	32.310464
645.621236	42740.251269	32.315482
646.116778	42824.509343	32.320500
646.769697	42894.047709	32.325517
647.929528	42981.214972	32.330535
648.535375	43056.182830	32.335552
649.425235	43126.863706	32.340570
650.095988	43201.249932	32.345588
650.658389	43280.854549	32.350605
651.218734	43352.399073	32.355623
651.943675	43423.790347	32.360640
652.431017	43488.735909	32.365658
653.100324	43565.412934	32.370676
654.159122	43634.425931	32.375693
654.586747	43711.449804	32.380711
655.290758	43791.453105	32.385728
655.461649	43868.378008	32.390746
656.113447	43949.284180	32.395764
657.192539	44013.798979	32.400781
658.087335	44096.616913	32.405799
658.543428	44178.658415	32.410816
659.672499	44253.446629	32.415834
659.888355	44333.387747	32.420852
660.887150	44399.846413	32.425869
661.514709	44469.457977	32.430887
662.343940	44554.375923	32.435904
662.954175	44616.867414	32.440922
663.615410	44691.365326	32.445940
664.236807	44757.341424	32.450957
664.991051	44815.992207	32.455975
665.536498	44903.191107	32.460992
666.465383	44968.652908	32.466010
666.897131	45046.559393	32.471028
667.294509	45111.354934	32.476045
668.131022	45192.043278	32.481063
668.670764	45252.713927	32.486080
669.631848	45334.888494	32.491098
669.704423	45413.654809	32.496116
670.700980	45481.825992	32.501133
671.302980	45550.248997	32.506151
671.954846	45639.476752	32.511168
672.537006	45716.732726	32.516186
673.206494	45802.194275	32.521204
673.582992	45869.212630	32.526221
674.400892	45944.892694	32.531239
675.035496	46032.306260	32.536256
675.838207	46104.146405	32.541274
676.673905	46178.817111	32.546292
677.393084	46252.680028	32.551309
678.022398	46326.810727	32.556327
678.737751	46402.256952	32.561344
679.266162	46468.608088	32.566362
679.974059	46544.340321	32.571380
680.597929	46610.527741	32.576397
681.335442	46674.132355	32.581415
681.978306	46753.135160	32.586432
682.515832	46820.935513	32.591450
682.964225	46891.027744	32.596468
683.670154	46970.128388	32.601485
684.630677	47045.043965	32.606503
685.211275	47130.570410	32.611520
686.158090	47204.712014	32.616538
686.731150	47284.938093	32.621556
686.873324	47357.533324	32.626573
687.698908	47434.465478	32.631591
688.143030	47515.636007	32.636608
689.187477	47597.689738	32.641626
689.492211	47691.453234	32.646644
690.229998	47788.189973	32.651661
691.089685	47871.254457	32.656679
691.538662	47960.769841	32.661696
692.414717	48046.273621	32.666714
692.955234	48135.720992	32.671732
693.626308	48223.959707	32.676749
694.575564	48318.150231	32.681767
695.251842	48407.323757	32.686784
696.259146	48487.988366	32.691802
696.675422	48585.685570	32.696820
697.318926	48672.825527	32.701837
698.325791	48753.832419	32.706855
698.996607	48840.144310	32.711872
699.827208	48926.341724	32.716890
700.934786	49016.514242	32.721908
701.107115	49103.017153	32.726925
702.075014	49170.315637	32.731943
702.919899	49266.028288	32.736960
703.592984	49345.090490	32.741978
704.164783	49431.468789	32.746996
704.790759	49516.170880	32.752013
706.152149	49603.559521	32.757031
706.413299	49696.019795	32.762048
706.842134	49779.277509	32.767066
707.775544	49867.568811	32.772084
708.264207	49951.496438	32.777101
709.135752	50032.388966	32.782119
709.498400	50114.152477	32.787136
710.517543	50199.863262	32.792154
711.485369	50291.754666	32.797172
711.577615	50385.294804	32.802189
712.782580	50464.279927	32.807207
713.348647	50559.334438	32.812224
713.921881	50653.428020	32.817242
714.766797	50736.036688	32.822260
715.586871	50826.344187	32.827277
716.423992	50917.881150	32.832295
716.626310	51002.201827	32.837312
717.560494	51090.293267	32.842330
718.460659	51183.090831	32.847348
719.445097	51277.422652	32.852365
720.195805	51347.496908	32.857383
720.783074	51439.734667	32.862400
721.638759	51514.410192	32.867418
722.370318	51596.738036	32.872436
722.914936	51679.469882	32.877453
723.631592	51761.497647	32.882471
724.105647	51847.640705	32.887488
724.928730	51939.999765	32.892506
725.726388	52009.620090	32.897524
726.233345	52098.380618	32.902541
727.055595	52172.186045	32.907559
727.761325	52260.699630	32.912576
728.265509	52340.054687	32.917594
728.931425	52412.806555	32.922612
729.249368	52514.968563	32.927629
730.225753	52605.308998	32.932647
730.786523	52692.597593	32.937664
731.341532	52780.228694	32.942682
732.170075	52880.987722	32.947700
732.880886	52973.585044	32.952717
733.633277	53054.361378	32.957735
734.316040	53160.781558	32.962752
735.193877	53267.561765	32.967770
735.826758	53353.236599	32.972788
736.661848	53450.509914	32.977805
737.432272	53538.671078	32.982823
738.216930	53640.635384	32.987840
739.012833	53741.821225	32.992858
739.671797	53845.633331	32.997876
740.477723	53943.634183	33.002893
741.275509	54037.599504	33.007911
742.045211	54145.596512	33.012928
742.517553	54249.492160	33.017946
743.650070	54336.466023	33.022964
744.144625	54441.534220	33.027981
745.230182	54530.273215	33.032999
745.723748	54641.294581	33.038016
746.547885	54733.578150	33.043034
747.490829	54833.468935	33.048052
748.392424	54929.449570	33.053069
749.364736	55019.321555	33.058087
750.235283	55115.567290	33.063104
750.817886	55208.291094	33.068122
751.558841	55302.682540	33.073140
752.183629	55402.451896	33.078157
753.262052	55497.837354	33.083175
754.043767	55602.592505	33.088192
754.513075	55687.685280	33.093210
755.463994	55775.384252	33.098228
756.115815	55865.521602	33.103245
757.149708	55961.403202	33.108263
757.801640	56059.793855	33.113280
758.368569	56151.343018	33.118298
759.598201	56234.846381	33.123316
759.955677	56327.031295	33.128333
760.850976	56423.405649	33.133351
761.491019	56526.173327	33.138368
761.980818	56619.405622	33.143386
763.276516	56708.978996	33.148404
763.799626	56799.451494	33.153421
764.558434	56893.202975	33.158439
765.031923	56999.090702	33.163456
765.593917	57096.205903	33.168474
767.064795	57184.709764	33.173492
767.604162	57291.573945	33.178509
768.432842	57382.478802	33.183527
769.229300	57481.749893	33.188544
769.984313	57582.096306	33.193562
771.272092	57672.882309	33.198580
771.922952	57779.446275	33.203597
772.443073	57853.063763	33.208615
773.139170	57947.708954	33.213632
773.628082	58039.102707	33.218650
774.391406	58135.601921	33.223668
775.591267	58240.636668	33.228685
775.940133	58333.672735	33.233703
776.988893	58420.021042	33.238720
777.688259	58503.672135	33.243738
778.703536	58585.236382	33.248756
779.082364	58687.072456	33.253773
779.828983	58769.705680	33.258791
780.647467	58857.263102	33.263808
781.387187	58944.808652	33.268826
782.302393	59030.461205	33.273844
782.662625	59136.644345	33.278861
783.628829	59223.129822	33.283879
784.283359	59315.620583	33.288896
785.256365	59418.556530	33.293914
786.158229	59512.163832	33.298932
786.695329	59612.044469	33.303949
787.903283	59703.446905	33.308967
788.187620	59795.843084	33.313984
789.153765	59905.911681	33.319002
790.026354	59991.550068	33.324020
790.794279	60101.684111	33.329037
791.909898	60189.280308	33.334055
792.643755	60289.491984	33.339072
793.086988	60393.146197	33.344090
794.137078	60487.751042	33.349108
794.503484	60587.563577	33.354125
795.617721	60684.920707	33.359143
796.335672	60789.416347	33.364160
796.750857	60902.924941	33.369178
798.014657	60999.437182	33.374196
798.817637	61095.273960	33.379213
799.647100	61209.550041	33.384231
800.172835	61328.876545	33.389248
801.022793	61420.946356	33.394266
802.076404	61519.834431	33.399284
802.836884	61632.221780	33.404301
803.747749	61741.222275	33.409319
804.378721	61848.487202	33.414336
805.013177	61951.605710	33.419354
806.260656	62051.431360	33.424372
807.071759	62154.224594	33.429389
807.663256	62260.828199	33.434407
808.677855	62375.503654	33.439424
809.127975	62481.133085	33.444442
810.314894	62582.627408	33.449460
810.888346	62685.298257	33.454477
812.167428	62794.243437	33.459495
813.440473	62898.525275	33.464512
813.873522	63003.136198	33.469530
814.356397	63101.020091	33.474548
815.298148	63209.865232	33.479565
816.189116	63306.645942	33.484583
817.431465	63403.881007	33.489600
817.526964	63514.688212	33.494618
818.536362	63618.372526	33.499636
819.417858	63721.282031	33.504653
820.142871	63829.053731	33.509671
821.173164	63927.489449	33.514688
822.055229	64035.545993	33.519706
822.942508	64132.792635	33.524724
823.390055	64243.153579	33.529741
824.158750	64348.859964	33.534759
825.216070	64455.271411	33.539776
825.878609	64565.149680	33.544794
826.966135	64672.416972	33.549812
827.533447	64780.118540	33.554829
828.435119	64879.755860	33.559847
829.339591	64984.368340	33.564864
829.846330	65089.274705	33.569882
830.888144	65196.172952	33.574900
831.575705	65294.159761	33.579917
832.650990	65391.058778	33.584935
833.506804	65491.560045	33.589952
833.935222	65579.596263	33.594970
834.820659	65676.565933	33.599988
835.300274	65783.832004	33.605005
836.060377	65877.858361	33.610023
837.163275	65982.620036	33.615040
837.649763	66098.876415	33.620058
838.825981	66199.214293	33.625076
839.759533	66314.291573	33.630093
840.603057	66419.774788	33.635111
841.892177	66528.238426	33.640128
842.226733	66626.334099	33.645146
842.998599	66725.691887	33.650164
843.996617	66841.943643	33.655181
844.850123	66957.815317	33.660199
845.959925	67059.742529	33.665216
846.359203	67178.282672	33.670234
847.352969	67274.489444	33.675252
848.056232	67395.819270	33.680269
848.797099	67502.424978	33.685287
850.162841	67622.862567	33.690304
850.671222	67739.996876	33.695322
851.784986	67844.557377	33.700340
852.668029	67959.588765	33.705357
853.196306	68075.798546	33.710375
854.246115	68184.676988	33.715392
854.808685	68307.167052	33.720410
855.530552	68421.639593	33.725428
856.403474	68545.344242	33.730445
857.452178	68665.113072	33.735463
858.498049	68777.554921	33.740480
859.406137	68908.223590	33.745498
860.386210	69017.617336	33.750516
861.579568	69142.322059	33.755533
862.129417	69259.666540	33.760551
863.661817	69364.152642	33.765568
864.078528	69476.803397	33.770586
865.307654	69586.683684	33.775604
865.561233	69698.344575	33.780621
866.791150	69818.564146	33.785639
867.381756	69934.059240	33.790656
868.142154	70046.801589	33.795674
868.964055	70159.123351	33.800692
870.138332	70274.713451	33.805709
870.938735	70397.131909	33.810727
871.959503	70509.694520	33.815744
872.704884	70623.681752	33.820762
873.640228	70746.358111	33.825780
874.406014	70855.638604	33.830797
875.470394	70971.889295	33.835815
876.458837	71087.299503	33.840832
877.006938	71218.111350	33.845850
878.114598	71328.773144	33.850868
878.860861	71446.906511	33.855885
879.813958	71565.923244	33.860903
880.850417	71669.294781	33.865920
881.786146	71781.486034	33.870938
882.859733	71904.595100	33.875956
883.735141	72012.092678	33.880973
884.359608	72130.755822	33.885991
885.746298	72241.850431	33.891008
885.989207	72360.084671	33.896026
886.958621	72470.199696	33.901044
887.927029	72580.328095	33.906061
888.266712	72710.494114	33.911079
889.155874	72822.287395	33.916096
890.233537	72940.987526	33.921114
891.150417	73047.073114	33.926132
892.207387	73149.961363	33.931149
892.631773	73265.033762	33.936167
893.573732	73358.721461	33.941184
894.203149	73486.447350	33.946202
895.349068	73603.906590	33.951220
896.245494	73721.395071	33.956237
897.121748	73840.753181	33.961255
897.914089	73951.790375	33.966272
898.694235	74077.888416	33.971290
899.312255	74191.605555	33.976308
900.498228	74317.960410	33.981325
900.903592	74450.453312	33.986343
902.017595	74567.625749	33.991360
902.798174	74699.805127	33.996378
903.977662	74835.884834	34.001396
905.076290	74961.947934	34.006413
906.097518	75098.744820	34.011431
907.150708	75203.376292	34.016448
907.721139	75339.724273	34.021466
908.543838	75468.429031	34.026484
909.478928	75594.143304	34.031501
910.344547	75722.671677	34.036519
911.275275	75860.127053	34.041536
912.016044	75993.433939	34.046554
913.062543	76128.721373	34.051572
914.325489	76260.627930	34.056589
914.851406	76391.790624	34.061607
915.917832	76532.649563	34.066624
916.970733	76668.173255	34.071642
917.732534	76800.045712	34.076660
918.826686	76923.299721	34.081677
919.513343	77073.465948	34.086695
920.632438	77207.078090	34.091712
921.738933	77348.555440	34.096730
922.713745	77475.083431	34.101748
923.599812	77609.837125	34.106765
924.436317	77751.918308	34.111783
925.401217	77876.090836	34.116800
926.286073	78014.667729	34.121818
927.173910	78151.815421	34.126836
928.437851	78283.645230	34.131853
929.286563	78428.315833	34.136871
930.140093	78548.696174	34.141888
931.046711	78693.694169	34.146906
932.273021	78823.256131	34.151924
932.915588	78956.400847	34.156941
933.957964	79090.536642	34.161959
935.084826	79230.643482	34.166976
935.584794	79358.873696	34.171994
936.693907	79492.558037	34.177012
938.139571	79632.734849	34.182029
938.785315	79761.265863	34.187047
939.781076	79889.315887	34.192064
940.660078	80034.270128	34.197082
941.376329	80168.048728	34.202100
942.402495	80301.112629	34.207117
943.494879	80442.232200	34.212135
944.381697	80576.826383	34.217152
945.552452	80719.282194	34.222170
946.430477	80846.351217	34.227188
947.480842	80974.442618	34.232205
948.138909	81112.399100	34.237223
949.365463	81233.839152	34.242240
950.072973	81374.983864	34.247258
950.792674	81504.992885	34.252276
952.363196	81632.989320	34.257293
952.858005	81765.219645	34.262311
953.807640	81880.894859	34.267328
954.899198	82009.067497	34.272346
955.768428	82134.335737	34.277364
956.769796	82249.080570	34.282381
957.250849	82386.023777	34.287399
958.417661	82512.605114	34.292416
959.069441	82641.107070	34.297434
960.018125	82778.664907	34.302452
961.297892	82902.022025	34.307469
962.182198	83061.527325	34.312487
963.259999	83189.038170	34.317504
963.689449	83323.205314	34.322522
964.741752	83454.619242	34.327540
965.706865	83601.562184	34.332557
966.536014	83748.452616	34.337575
967.594842	83884.492989	34.342592
968.797470	84021.041863	34.347610
969.564869	84176.391946	34.352628
970.485862	84321.518195	34.357645
971.197853	84481.567948	34.362663
972.399225	84616.456463	34.367680
973.237826	84760.282995	34.372698
974.467901	84925.754921	34.377716
975.472009	85074.845720	34.382733
976.659117	85217.111519	34.387751
977.829901	85364.525142	34.392768
978.973113	85504.009520	34.397786
979.769274	85657.884077	34.402804
980.740749	85797.404929	34.407821
982.087590	85939.534815	34.412839
982.818168	86079.546441	34.417856
984.157749	86235.967260	34.422874
985.299933	86368.597691	34.427892
986.207572	86505.817346	34.432909
986.856354	86653.932857	34.437927
987.865011	86788.195005	34.442944
988.875642	86936.701743	34.447962
990.059023	87084.225330	34.452980
991.213768	87221.844925	34.457997
991.873168	87370.507386	34.463015
992.903081	87509.440215	34.468032
994.215891	87655.965118	34.473050
995.092275	87804.537474	34.478068
996.172524	87941.901463	34.483085
996.912046	88093.991423	34.488103
998.008245	88234.948907	34.493120
999.283337	88378.567178	34.498138
1000.086238	88533.876909	34.503156
1000.915789	88677.646593	34.508173
1001.901599	88829.276526	34.513191
1002.676589	88973.727829	34.518208
1004.016314	89123.136777	34.523226
1004.982605	89278.158539	34.528244
1006.181483	89419.675619	34.533261
1006.847124	89572.242876	34.538279
1007.956033	89717.219362	34.543296
1008.952332	89867.613725	34.548314
1009.537402	90021.184435	34.553332
1010.745877	90169.893807	34.558349
1011.957838	90330.178938	34.563367
1012.934648	90473.049012	34.568384
1014.309586	90626.720827	34.573402
1014.950370	90774.129107	34.578420
1016.492776	90917.231073	34.583437
1017.151889	91064.707714	34.588455
1017.957074	91213.559823	34.593472
1019.570537	91356.279227	34.598490
1020.102787	91496.855450	34.603508
1021.440076	91630.976548	34.608525
1021.927492	91776.947925	34.613543
1022.869887	91917.813208	34.618560
1024.088285	92051.481593	34.623578
1025.220192	92195.633691	34.628596
1026.516904	92331.917334	34.633613
1027.237893	92476.569431	34.638631
1027.701506	92623.252377	34.643648
1028.801976	92770.381570	34.648666
1029.582692	92917.792378	34.653684
1030.580378	93072.909224	34.658701
1031.367701	93231.321565	34.663719
1032.445135	93390.642737	34.668736
1033.467868	93557.329054	34.673754
1034.645476	93724.693493	34.678772
1035.606312	93883.904219	34.683789
1036.809379	94047.582734	34.688807
1037.837335	94214.500514	34.693824
1038.721243	94375.714704	34.698842
1039.753961	94545.191202	34.703860
1040.918659	94701.075614	34.708877
1042.024251	94875.188513	34.713895
1042.800827	95043.729626	34.718912
1044.460160	95207.536623	34.723930
1045.409725	95382.425833	34.728948
1046.448932	95540.083386	34.733965
1047.617436	95706.601848	34.738983
1048.396930	95871.774093	34.744000
1049.419462	96041.427083	34.749018
1050.178683	96220.120174	34.754036
1051.515184	96387.767533	34.759053
1052.744775	96560.219496	34.764071
1053.499869	96734.188114	34.769088
1054.961500	96896.171414	34.774106
1055.875309	97066.165856	34.779124
1057.159041	97245.115063	34.784141
1057.903315	97422.451790	34.789159
1059.159147	97589.525443	34.794176
1060.410651	97757.164356	34.799194
1061.679435	97937.937881	34.804212
1062.779949	98108.566896	34.809229
1063.752907	98280.477992	34.814247
1064.837038	98449.225418	34.819264
1066.157382	98611.433037	34.824282
1066.862138	98780.631580	34.829300
1068.101817	98933.630352	34.834317
1069.272673	99115.175535	34.839335
1070.001486	99284.550725	34.844352
1071.457476	99455.636523	34.849370
1072.406387	99628.592701	34.854388
1073.933679	99788.146169	34.859405
1074.806618	99952.677568	34.864423
1075.780142	100115.262344	34.869440
1076.939274	100273.018300	34.874458
1078.067501	100453.345437	34.879476
1078.940094	100613.841707	34.884493
1080.328512	100791.247398	34.889511
1081.013697	100957.386492	34.894528
1082.134757	101123.100030	34.899546
1083.082315	101293.813629	34.904564
1084.039144	101454.079608	34.909581
1085.699292	101632.104659	34.914599
1086.566169	101808.666488	34.919616
1087.842247	101962.348493	34.924634
1088.354866	102129.486086	34.929652
1089.519249	102315.955795	34.934669
1090.973437	102480.210955	34.939687
1091.880353	102638.890548	34.944704
1093.315446	102789.131917	34.949722
1093.873838	102955.969654	34.954740
1094.673537	103113.720063	34.959757
1096.167866	103274.560626	34.964775
1096.939303	103433.381430	34.969792
1097.897601	103596.592158	34.974810
1099.068647	103782.754652	34.979828
1100.172039	103941.004414	34.984845
1101.131160	104123.886266	34.989863
1101.857552	104296.080887	34.994880
1102.999018	104467.878731	34.999898
1104.048595	104646.101296	35.004916
1104.887969	104836.758780	35.009933
1106.100169	105029.192434	35.014951
1107.245906	105213.355493	35.019968
1108.369791	105387.821906	35.024986
1109.510057	105593.848651	35.030004
1110.318807	105771.801982	35.035021
1111.884013	105963.943427	35.040039
1112.957277	106162.057074	35.045056
1114.286021	106343.284641	35.050074
1115.356635	106535.397985	35.055092
1116.233794	106724.428899	35.060109
1117.865257	106907.966101	35.065127
1118.957542	107105.589636	35.070144
1120.487379	107282.901868	35.075162
1121.152549	107475.342308	35.080180
1122.293256	107669.719450	35.085197
1123.717706	107852.841357	35.090215
1124.593246	108036.536578	35.095232
1126.213306	108227.038566	35.100250
1127.068851	108420.163610	35.105268
1128.292636	108607.934470	35.110285
1129.340827	108793.202300	35.115303
1130.497636	108989.688974	35.120320
1131.746272	109177.675011	35.125338
1132.958524	109364.224317	35.130356
1133.876712	109549.924148	35.135373
1135.345602	109737.092277	35.140391
1136.450138	109936.469894	35.145408
1137.766709	110121.449057	35.150426
1138.810682	110307.158581	35.155444
1140.050963	110493.267610	35.160461
1141.465413	110677.955667	35.165479
1142.410937	110877.404425	35.170496
1143.715761	111052.472953	35.175514
1144.877055	111240.918322	35.180532
1146.033736	111413.784081	35.185549
1147.282324	111601.710766	35.190567
1148.392578	111794.374164	35.195584
1149.556344	111977.072793	35.200602
1150.748039	112146.909632	35.205620
1151.777282	112333.294001	35.210637
1153.080997	112521.091129	35.215655
1153.818695	112703.573597	35.220672
1155.225913	112882.994782	35.225690
1156.243954	113074.301417	35.230708
1157.058143	113272.395565	35.235725
1158.434619	113457.703879	35.240743
1159.610510	113648.405579	35.245760
1160.741152	113836.088139	35.250778
1161.675597	114027.263077	35.255796
1162.826573	114226.993302	35.260813
1164.038864	114414.666229	35.265831
1165.116132	114609.254914	35.270848
1166.608527	114793.767375	35.275866
1167.733726	114992.075624	35.280884
1168.864046	115175.497493	35.285901
1169.873930	115347.398273	35.290919
1171.036089	115519.591670	35.295936
1171.852774	115697.088579	35.300954
1172.978015	115874.700301	35.305972
1173.902093	116067.018374	35.310989
1175.353078	116255.994403	35.316007
1176.279693	116452.356448	35.321024
1177.316227	116642.239782	35.326042
1178.692275	116838.314788	35.331060
1179.823067	117041.476500	35.336077
1181.244314	117228.842042	35.341095
1182.399538	117423.411732	35.346112
1183.537588	117614.247691	35.351130
1184.943720	117812.263003	35.356148
1185.737829	118004.197408	35.361165
1187.093492	118200.171026	35.366183
1188.112712	118411.964489	35.371200
1189.374709	118618.460803	35.376218
1191.321687	118817.495992	35.381236
1192.016217	119023.645492	35.386253
1193.478947	119212.106769	35.391271
1194.765701	119418.072466	35.396288
1196.071488	119614.659432	35.401306
1197.197848	119812.671271	35.406324
1198.138871	120011.374021	35.411341
1199.451245	120210.815066	35.416359
1200.528553	120419.242763	35.421376
1201.911294	120609.969210	35.426394
1203.401643	120812.641648	35.431412
1204.139706	121027.275734	35.436429
1205.546491	121222.690913	35.441447
1206.942179	121430.743650	35.446464
1208.291680	121624.194046	35.451482
1209.630977	121832.233576	35.456500
1210.665133	122035.268589	35.461517
1212.195111	122234.750685	35.466535
1213.318851	122436.430309	35.471552
1214.477216	122629.437265	35.476570
1215.791846	122833.255091	35.481588
1217.108854	123032.803067	35.486605
1218.501054	123228.183127	35.491623
1219.316600	123435.483963	35.496640
1220.798536	123644.741841	35.501658
1222.138836	123831.617885	35.506676
1222.886496	124039.162217	35.511693
1224.371755	124235.167107	35.516711
1225.576426	124446.504155	35.521728
1226.758367	124648.797331	35.526746
1228.076443	124850.461008	35.531764
1229.048273	125051.688968	35.536781
1230.636960	125254.045682	35.541799
1231.717277	125469.998410	35.546816
1232.952958	125680.882637	35.551834
1234.114601	125885.329324	35.556852
1235.761423	126093.093923	35.561869
1236.913674	126285.656239	35.566887
1238.053567	126497.360408	35.571904
1239.089491	126692.124523	35.576922
1240.502792	126899.819099	35.581940
1241.661373	127108.266965	35.586957
1242.877096	127313.195841	35.591975
1243.877206	127529.024181	35.596992
1244.966695	127724.445042	35.602010
1246.058425	127938.195045	35.607028
1247.273125	128158.770826	35.612045
1248.763155	128368.642698	35.617063
1250.238964	128573.207329	35.622080
1251.349185	128774.816954	35.627098
1252.501760	128965.697333	35.632116
1253.581648	129169.545412	35.637133
1254.999067	129355.707068	35.642151
1255.974350	129562.705892	35.647168
1257.048170	129772.072858	35.652186
1258.410536	129971.556955	35.657204
1259.718197	130183.562631	35.662221
1261.162906	130382.135706	35.667239
1261.815040	130597.028570	35.672256
1263.079408	130809.134315	35.677274
1264.535653	131022.401342	35.682292
1265.491813	131236.918687	35.687309
1266.888981	131457.804283	35.692327
1268.070735	131671.970345	35.697344
1269.327644	131894.568131	35.702362
1270.486522	132123.407990	35.707380
1271.629526	132353.709947	35.712397
1272.723705	132582.449669	35.717415
1274.350023	132819.482630	35.722432
1275.368250	133041.037550	35.727450
1276.709795	133282.164992	35.732468
1277.815139	133514.547834	35.737485
1279.289036	133750.040792	35.742503
1280.680631	133986.182932	35.747520
1282.170330	134229.498799	35.752538
1283.696101	134455.720904	35.757556
1284.668028	134694.409678	35.762573
1286.124775	134919.822332	35.767591
1287.551256	135153.735802	35.772608
1288.839773	135399.730618	35.777626
1289.951834	135638.301644	35.782644
1290.980419	135878.637789	35.787661
1292.437330	136116.166354	35.792679
1294.037388	136354.230810	35.797696
1295.142241	136600.391669	35.802714
1296.626802	136833.140959	35.807732
1297.875422	137076.251365	35.812749
1299.408371	137315.005737	35.817767
1300.639844	137562.978502	35.822784
1301.729158	137809.264921	35.827802
1303.433957	138046.778901	35.832820
1304.716002	138286.963658	35.837837
1306.274064	138517.645750	35.842855
1307.811096	138764.308908	35.847872
1308.974637	139004.784603	35.852890
1310.172943	139232.082187	35.857908
1311.638825	139481.729319	35.862925
1312.740480	139708.069712	35.867943
1314.684752	139955.625163	35.872960
1315.638442	140185.847831	35.877978
1316.870977	140423.291594	35.882996
1318.132218	140660.212366	35.888013
1319.481332	140895.053372	35.893031
1320.842709	141133.457099	35.898048
1321.727822	141377.051355	35.903066
1323.429357	141610.964025	35.908084
1324.630767	141873.783749	35.913101
1325.657463	142104.273391	35.918119
1327.210533	142346.800307	35.923136
1328.575867	142589.245802	35.928154
1329.978474	142839.510912	35.933172
1331.416020	143080.058409	35.938189
1332.879379	143323.748181	35.943207
1334.162574	143560.152394	35.948224
1335.008579	143802.565247	35.953242
1336.540574	144041.556566	35.958260
1337.770199	144275.679082	35.963277
1339.336466	144514.224063	35.968295
1340.973552	144743.120950	35.973312
1341.975598	144963.247105	35.978330
1343.500279	145189.603734	35.983348
1344.709914	145419.133576	35.988365
1345.704023	145650.032096	35.993383
1347.349525	145869.106318	35.998400
1348.104542	146106.641887	36.003418
1349.776793	146338.688259	36.008436
1350.950165	146583.830498	36.013453
1352.232185	146814.092795	36.018471
1353.683181	147057.518282	36.023488
1354.602815	147305.408651	36.028506
1356.155719	147550.570758	36.033524
1357.476584	147802.000019	36.038541
1358.765173	148051.711484	36.043559
1360.185516	148290.876147	36.048576
1361.468447	148557.028870	36.053594
1362.663605	148804.515993	36.058612
1364.148048	149064.208791	36.063629
1365.828233	149315.512862	36.068647
1367.132360	149577.407855	36.073664
1368.324834	149838.803117	36.078682
1369.899091	150096.814059	36.083700
1370.956403	150356.269334	36.088717
1372.419440	150624.208084	36.093735
1374.080830	150888.298172	36.098752
1375.129524	151154.799799	36.103770
1376.935677	151413.314137	36.108788
1378.132349	151681.152175	36.113805
1379.384809	151946.458753	36.118823
1380.658537	152216.634358	36.123840
1382.150099	152494.322973	36.128858
1383.706653	152755.868430	36.133876
1385.029470	153028.781442	36.138893
1386.710262	153288.724436	36.143911
1388.087785	153554.960093	36.148928
1389.426130	153830.172094	36.153946
1390.998759	154100.514441	36.158964
1392.097963	154370.886157	36.163981
1393.718493	154648.099552	36.168999
1395.194231	154912.641151	36.174016
1396.132158	155187.586375	36.179034
1397.556000	155458.660352	36.184052
1399.331946	155736.363135	36.189069
1400.654584	156014.929264	36.194087
1402.094446	156287.807584	36.199104
1403.666933	156566.158688	36.204122
1404.815190	156826.175015	36.209140
1406.625554	157106.469524	36.214157
1407.746662	157381.399629	36.219175
1409.013422	157650.307125	36.224192
1410.426255	157932.753557	36.229210
1412.265844	158213.139730	36.234228
1413.881413	158484.545020	36.239245
1415.281730	158757.345113	36.244263
1416.783988	159029.127966	36.249280
1418.157532	159304.321154	36.254298
1419.217505	159576.764293	36.259316
1420.701040	159844.013877	36.264333
1421.990550	160125.074933	36.269351
1423.484012	160391.463724	36.274368
1425.002763	160681.688540	36.279386
1426.711584	160939.342109	36.284404
1428.253212	161208.849143	36.289421
1429.246638	161483.421818	36.294439
1430.917251	161751.934125	36.299456
1432.299163	162020.787656	36.304474
1433.914579	162282.004629	36.309492
1435.641298	162529.172601	36.314509
1436.996550	162783.381482	36.319527
1438.563657	163020.745925	36.324544
1439.432309	163281.508810	36.329562
1441.048945	163519.578345	36.334580
1442.479819	163776.445045	36.339597
1443.625047	164037.230258	36.344615
1445.080076	164289.452289	36.349632
1446.252940	164558.978034	36.354650
1447.623175	164818.347788	36.359668
1449.095433	165087.027993	36.364685
1450.119999	165356.900387	36.369703
1451.970164	165632.170112	36.374720
1453.466040	165908.603992	36.379738
1454.565384	166193.707886	36.384756
1456.072526	166475.091945	36.389773
1457.338533	166759.588274	36.394791
1458.658507	167044.597744	36.399808
1460.249449	167337.989597	36.404826
1461.855022	167608.832893	36.409844
1463.229537	167906.058191	36.414861
1464.682712	168203.158253	36.419879
1466.539754	168481.933948	36.424896
1467.777252	168784.225232	36.429914
1469.236380	169080.213417	36.434932
1470.828403	169372.539728	36.439949
1471.923077	169666.701222	36.444967
1473.687729	169959.764120	36.449984
1475.434805	170257.666515	36.455002
1476.840475	170551.845725	36.460020
1478.618771	170852.931897	36.465037
1479.599701	171153.923349	36.470055
1481.589553	171441.476406	36.475072
1482.996224	171736.005553	36.480090
1484.206422	172048.436608	36.485108
1485.885252	172343.241836	36.490125
1487.197378	172642.309952	36.495143
1488.966620	172939.438950	36.500160
1490.538305	173238.975542	36.505178
1491.715979	173531.434386	36.510196
1493.632345	173848.126095	36.515213
1494.973793	174150.155688	36.520231
1496.877971	174447.792044	36.525248
1498.029416	174750.808577	36.530266
1500.009220	175040.935825	36.535284
1501.414099	175338.609361	36.540301
1502.846907	175645.798342	36.545319
1504.932279	175935.710387	36.550336
1506.125592	176236.660534	36.555354
1507.532342	176534.658259	36.560372
1509.263866	176824.710116	36.565389
1510.602461	177126.187364	36.570407
1511.953934	177422.156204	36.575424
1513.888870	177720.314861	36.580442
1515.308331	178017.354743	36.585460
1516.667721	178308.022376	36.590477
1518.230196	178612.822113	36.595495
1520.036120	178903.990497	36.600512
1521.414460	179199.317973	36.605530
1523.034954	179494.619828	36.610548
1524.375968	179784.943498	36.615565
1525.722656	180087.223830	36.620583
1527.508561	180378.543452	36.625600
1528.851567	180685.232049	36.630618
1530.074348	180980.963432	36.635636
1531.941963	181280.093044	36.640653
1533.495075	181579.352465	36.645671
1535.107052	181845.717463	36.650688
1536.437941	182129.316024	36.655706
1537.968270	182409.240343	36.660724
1539.598709	182684.085179	36.665741
1541.148712	182967.398118	36.670759
1542.551421	183245.101242	36.675776
1544.201136	183534.150545	36.680794
1545.433810	183809.104891	36.685812
1547.304750	184102.106260	36.690829
1548.193384	184397.975122	36.695847
1549.896617	184679.850010	36.700864
1551.639698	184982.473252	36.705882
1552.976441	185287.183517	36.710900
1554.513134	185587.394332	36.715917
1555.738102	185900.110563	36.720935
1557.657572	186187.047436	36.725952
1559.173243	186502.689274	36.730970
1560.212935	186805.095829	36.735988
1562.118686	187114.279003	36.741005
1563.557604	187443.914564	36.746023
1565.180316	187741.558421	36.751040
1566.896707	188054.243374	36.756058
1568.473663	188371.459432	36.761076
1569.951263	188686.002483	36.766093
1571.342177	189006.007344	36.771111
1573.206633	189325.085203	36.776128
1575.054280	189644.192953	36.781146
1576.087861	189962.586387	36.786164
1577.851534	190280.645101	36.791181
1579.369159	190606.337470	36.796199
1581.004417	190935.452400	36.801216
1582.709286	191261.422045	36.806234
1584.294369	191601.999457	36.811252
1586.144572	191910.163271	36.816269
1587.411112	192250.390684	36.821287
1589.097883	192568.956495	36.826304
1590.935122	192898.226347	36.831322
1592.287419	193230.218626	36.836340
1594.306475	193551.438617	36.841357
1596.048250	193879.142516	36.846375
1597.520490	194209.101614	36.851392
1599.111441	194533.266448	36.856410
1600.699701	194860.239050	36.861428
1602.691031	195194.116531	36.866445
1604.054111	195519.885532	36.871463
1605.883703	195842.900337	36.876480
1607.481609	196164.507715	36.881498
1609.149218	196495.626930	36.886516
1611.120707	196806.917616	36.891533
1612.718292	197130.065950	36.896551
1614.407814	197455.409749	36.901568
1615.965476	197775.444617	36.906586
1617.377248	198105.357205	36.911604
1619.724678	198423.601507	36.916621
1620.823279	198743.310517	36.921639
1622.443478	199055.164793	36.926656
1624.127883	199377.750896	36.931674
1625.912772	199708.764945	36.936692
1627.302085	200018.896927	36.941709
1628.848430	200335.009748	36.946727
1630.267555	200665.618986	36.951744
1632.395347	200985.930086	36.956762
1633.774830	201316.307676	36.961780
1635.688879	201628.391496	36.966797
1637.212858	201948.108343	36.971815
1638.819304	202271.685492	36.976832
1640.443687	202583.643537	36.981850
1641.894578	202906.093790	36.986868
1643.312051	203204.934706	36.991885
1644.844379	203515.032767	36.996903
1646.654675	203814.801617	37.001920
1648.050057	204110.615236	37.006938
1649.520699	204435.290851	37.011956
1651.053112	204740.340513	37.016973
1652.408687	205064.009357	37.021991
1654.166956	205378.991593	37.027008
1655.951483	205703.569970	37.032026
1657.151973	206030.734871	37.037044
1658.779788	206352.357960	37.042061
1660.071588	206692.830169	37.047079
1661.885655	207033.115996	37.052096
1663.677114	207378.562244	37.057114
1664.805054	207711.053695	37.062132
1666.898254	208056.833952	37.067149
1668.572754	208400.284970	37.072167
1669.991313	208745.608197	37.077184
1671.885377	209094.003403	37.082202
1673.558020	209441.001785	37.087220
1675.187922	209800.516185	37.092237
1676.982262	210155.433670	37.097255
1678.584493	210504.822614	37.102272
1680.428529	210865.906133	37.107290
1682.412015	211223.209471	37.112308
1684.048616	211575.797043	37.117325
1685.752899	211928.146294	37.122343
1687.249920	212283.502608	37.127360
1689.369980	212635.989185	37.132378
1690.486483	213002.306455	37.137396
1692.466553	213360.939664	37.142413
1694.235084	213724.688656	37.147431
1695.900536	214093.484770	37.152448
1698.173869	214449.737274	37.157466
1699.319894	214817.072836	37.162484
1701.349716	215179.971679	37.167501
1703.279489	215543.650371	37.172519
1704.762408	215916.115672	37.177536
1706.257790	216273.443274	37.182554
1707.829531	216640.055207	37.187572
1709.759603	217016.844716	37.192589
1711.725606	217389.083474	37.197607
1713.277217	217753.264657	37.202624
1715.036640	218115.812745	37.207642
1716.669072	218496.796914	37.212660
1718.763748	218868.943687	37.217677
1720.644171	219238.942917	37.222695
1722.296443	219613.756088	37.227712
1723.882146	219981.165162	37.232730
1725.311545	220349.896664	37.237748
1727.075203	220719.844168	37.242765
1729.009139	221097.308309	37.247783
1730.605014	221475.642360	37.252800
1732.605606	221840.246114	37.257818
1734.123965	222291.084950	37.262836
1736.148126	222671.206456	37.267853
1738.247978	223036.407264	37.272871
1739.906707	223408.539953	37.277888
1741.573765	223768.404457	37.282906
1743.008164	224146.824838	37.287924
1745.260971	224507.560028	37.292941
1746.934504	224884.419259	37.297959
1748.692594	225246.355954	37.302976
1750.456098	225609.512017	37.307994
1751.881303	225982.732631	37.313012
1753.683821	226344.309580	37.318029
1755.273724	226722.712196	37.323047
1756.934208	227093.611189	37.328064
1759.054100	227437.307807	37.333082
1760.368662	227796.149966	37.338100
1762.118685	228138.817276	37.343117
1764.098995	228498.033966	37.348135
1765.439585	228855.884024	37.353152
1767.360524	229188.543308	37.358170
1768.951271	229566.217194	37.363188
1770.639460	229919.821446	37.368205
1772.283318	230278.285456	37.373223
1773.893382	230651.869475	37.378240
1776.277322	231014.912231	37.383258
1778.058892	231382.119524	37.388276
1779.662796	231754.284867	37.393293
1781.090182	232117.513657	37.398311
1782.612395	232497.238429	37.403328
1784.813107	232872.533839	37.408346
1786.232939	233263.479319	37.413364
1788.102031	233644.165579	37.418381
1790.092473	234030.166983	37.423399
1791.813162	234426.552247	37.428416
1793.553280	234811.021886	37.433434
1795.131670	235203.317390	37.438452
1796.773646	235591.767612	37.443469
1799.021817	235983.242977	37.448487
1800.191936	236402.788406	37.453504
1802.627417	236794.437779	37.458522
1804.420008	237190.614073	37.463540
1805.923826	237595.018304	37.468557
1807.775812	237994.387075	37.473575
1809.540904	238415.642171	37.478592
1811.516845	238809.149606	37.483610
1813.340481	239221.455136	37.488628
1815.165960	239642.016880	37.493645
1817.346688	240052.359864	37.498663
1818.849401	240466.905349	37.503680
1821.011728	240875.246091	37.508698
1822.817512	241287.405986	37.513716
1824.600895	241704.549171	37.518733
1826.657310	242112.325267	37.523751
1828.447534	242526.623631	37.528768
1830.492652	242942.201501	37.533786
1832.396381	243351.757556	37.538804
1834.184135	243761.968448	37.543821
1836.479475	244164.297497	37.548839
1838.299187	244577.349395	37.553856
1840.354783	244975.959558	37.558874
1841.944515	245381.328110	37.563892
1843.806849	245791.783536	37.568909
1845.879198	246188.614279	37.573927
1847.531863	246605.151222	37.578944
1849.419679	247009.989901	37.583962
1851.344534	247413.501969	37.588980
1853.174666	247829.350552	37.593997
1854.977298	248234.738095	37.599015
1856.721211	248664.649651	37.604032
1858.635482	249071.543766	37.609050
1860.469466	249486.555095	37.614068
1862.001612	249891.379203	37.619085
1863.769791	250302.312225	37.624103
1865.962523	250724.378251	37.629120
1867.842221	251148.680976	37.634138
1869.636273	251563.776817	37.639156
1871.239255	251974.509750	37.644173
1873.123513	252401.403737	37.649191
1874.976259	252828.608036	37.654208
1876.939649	253234.023749	37.659226
1878.919997	253658.667121	37.664244
1880.328824	254076.622412	37.669261
1882.676046	254483.880577	37.674279
1884.122565	254886.588031	37.679296
1885.784450	255288.523367	37.684314
1887.541386	255685.819733	37.689332
1888.838685	256094.166326	37.694349
1890.893398	256509.272233	37.699367
1892.027860	256939.645146	37.704384
1894.260378	257356.830312	37.709402
1896.280191	257783.932532	37.714420
1897.936559	258225.066615	37.719437
1900.087208	258651.054926	37.724455
1901.609275	259086.216003	37.729472
1903.508419	259526.801895	37.734490
1905.368446	259976.132929	37.739508
1906.933811	260424.699637	37.744525
1909.004871	260878.619045	37.749543
1910.898095	261334.803182	37.754560
1912.672227	261789.965302	37.759578
1914.921680	262253.914500	37.764596
1916.604261	262719.836941	37.769613
1919.042511	263163.279526	37.774631
1920.659449	263643.488946	37.779648
1922.395234	264103.940156	37.784666
1924.818339	264569.663054	37.789684
1926.601656	265042.934397	37.794701
1929.126277	265508.106381	37.799719
1930.758368	265979.471311	37.804736
1933.032764	266441.864086	37.809754
1935.069099	266916.540035	37.814772
1936.822121	267387.121598	37.819789
1938.962639	267844.225891	37.824807
1940.962733	268312.022150	37.829824
1943.010998	268775.923269	37.834842
1944.948350	269258.310093	37.839860
1946.981062	269722.034820	37.844877
1949.177122	270182.251785	37.849895
1951.275362	270667.861729	37.854912
1953.060038	271138.763712	37.859930
1955.132170	271594.477492	37.864948
1956.969124	272064.861405	37.869965
1959.191120	272534.799960	37.874983
1961.120085	273000.721713	37.880000
1962.802623	273478.724211	37.885018
1964.995650	273951.027613	37.890036
1966.964155	274420.217327	37.895053
1969.131671	274897.222679	37.900071
1970.512876	275368.133351	37.905088
1972.675601	275849.075008	37.910106
1974.974873	276325.496923	37.915124
1976.784529	276810.229014	37.920141
1979.024504	277283.534214	37.925159
1981.031807	277762.643081	37.930176
1983.133481	278238.560019	37.935194
1985.350029	278705.515377	37.940212
1987.201125	279186.348660	37.945229
1989.056740	279654.047237	37.950247
1991.265925	280132.456679	37.955264
1993.165630	280603.473282	37.960282
1995.466402	281071.780682	37.965300
1997.069977	281551.683518	37.970317
1999.099244	282012.971618	37.975335
2001.226716	282489.432373	37.980352
2003.441866	282961.025640	37.985370
2005.224661	283422.630016	37.990388
2007.200480	283908.967470	37.995405
2009.223817	284375.076241	38.000423
2011.346710	284857.398516	38.005440
2013.392254	285324.161212	38.010458
2015.536295	285766.749881	38.015476
2017.089511	286218.223495	38.020493
2019.286667	286655.009335	38.025511
2021.076469	287106.618942	38.030528
2023.338574	287549.843121	38.035546
2025.286239	287999.264754	38.040564
2026.891238	288446.226847	38.045581
2029.181632	288896.020761	38.050599
2031.025346	289354.675424	38.055616
2032.784288	289817.584327	38.060634
2035.515242	290272.863464	38.065652
2037.363512	290737.710131	38.070669
2039.219547	291189.853824	38.075687
2040.988959	291669.162636	38.080704
2043.001126	292136.034413	38.085722
2044.729168	292610.952192	38.090740
2046.645795	293092.263038	38.095757
2048.627543	293568.201879	38.100775
2050.793971	294065.062746	38.105792
2052.759028	294551.617211	38.110810
2054.927078	295033.462628	38.115828
2057.121453	295539.049699	38.120845
2059.027901	296036.681327	38.125863
2061.055283	296530.023711	38.130880
2063.080497	297039.670124	38.135898
2065.591319	297534.909132	38.140916
2067.543235	298042.327708	38.145933
2069.550264	298545.924942	38.150951
2071.593217	299062.289030	38.155968
2073.687149	299563.098448	38.160986
2075.851857	300063.614277	38.166004
2077.741860	300587.513456	38.171021
2080.062359	301101.078086	38.176039
2082.159911	301607.616257	38.181056
2084.114331	302123.750148	38.186074
2086.328151	302637.527216	38.191092
2087.979792	303165.895962	38.196109
2090.525013	303682.329957	38.201127
2092.348096	304201.496076	38.206144
2094.651750	304734.446399	38.211162
2097.149696	305258.599639	38.216180
2099.384078	305784.190033	38.221197
2101.604373	306293.373619	38.226215
2103.691824	306823.477017	38.231232
2105.648251	307349.992500	38.236250
2108.026498	307872.778045	38.241268
2110.145410	308402.891606	38.246285
2112.253094	308915.506169	38.251303
2114.652095	309433.453175	38.256320
2116.839427	309956.586962	38.261338
2119.312385	310457.348046	38.266356
2121.079639	310982.804509	38.271373
2123.481767	311491.849319	38.276391
2125.400522	312013.058272	38.281408
2127.523183	312524.732568	38.286426
2130.033287	313033.089000	38.291444
2131.877205	313559.099092	38.296461
2134.428750	314064.978424	38.301479
2136.559710	314578.719495	38.306496
2138.252385	315101.315368	38.311514
2140.346393	315607.030948	38.316532
2142.373400	316130.249743	38.321549
2144.560175	316642.849514	38.326567
2146.946001	317168.083569	38.331584
2149.082357	317690.155392	38.336602
2151.401331	318200.918981	38.341620
2153.132051	318718.073063	38.346637
2155.489770	319223.947303	38.351655
2157.647939	319710.400690	38.356672
2159.624124	320209.068448	38.361690
2161.777578	320691.071917	38.366708
2163.841607	321196.141673	38.371725
2166.267255	321676.442514	38.376743
2168.154966	322163.430144	38.381760
2170.042427	322665.115190	38.386778
2172.244284	323158.086297	38.391796
2174.146998	323663.848736	38.396813
2176.144146	324166.316204	38.401831
2178.100869	324674.727454	38.406848
2180.070169	325198.696152	38.411866
2182.273418	325710.561862	38.416884
2184.213197	326244.936002	38.421901
2186.316400	326776.028656	38.426919
2188.860843	327315.828185	38.431936
2190.456108	327854.027670	38.436954
2193.139717	328393.616643	38.441972
2195.274166	328940.222142	38.446989
2197.537996	329486.775732	38.452007
2199.773751	330033.227200	38.457024
2201.477452	330585.727214	38.462042
2203.729948	331132.393815	38.467060
2206.007183	331700.071111	38.472077
2208.464100	332267.154458	38.477095
2210.576011	332823.576000	38.482112
2212.949090	333382.081195	38.487130
2215.219192	333947.959465	38.492148
2217.892687	334508.256612	38.497165
2219.776349	335081.954632	38.502183
2222.064194	335637.023500	38.507200
2224.330270	336215.875385	38.512218
2226.736988	336783.985532	38.517236
2229.261318	337351.740071	38.522253
2231.070261	337918.895703	38.527271
2233.568821	338491.388663	38.532288
2235.598686	339078.344742	38.537306
2237.952753	339646.787220	38.542324
2240.542872	340219.397792	38.547341
2242.682057	340799.995453	38.552359
2245.383630	341363.639902	38.557376
2247.202985	341961.612508	38.562394
2249.671482	342530.383693	38.567412
2252.007377	343109.652437	38.572429
2254.248129	343683.092354	38.577447
2256.550860	344257.022770	38.582464
2259.088112	344828.547194	38.587482
2261.458194	345404.965198	38.592500
2263.594088	345980.627998	38.597517
2265.775902	346555.134038	38.602535
2268.252910	347125.447472	38.607552
2270.073542	347709.109734	38.612570
2272.733388	348285.088708	38.617588
2275.169152	348859.117875	38.622605
2277.175567	349442.067346	38.627623
2279.446703	350025.929869	38.632640
2281.558958	350610.369241	38.637658
2283.895448	351194.713124	38.642676
2286.405041	351774.427573	38.647693
2288.555329	352361.654118	38.652711
2291.205643	352930.976584	38.657728
2293.458693	353508.629398	38.662746
2295.974918	354085.850367	38.667764
2298.402247	354662.037828	38.672781
2300.456135	355239.826898	38.677799
2302.884106	355818.891107	38.682816
2305.001631	356390.995464	38.687834
2307.432772	356946.852157	38.692852
2309.758129	357503.860607	38.697869
2311.980052	358040.580645	38.702887
2314.456855	358576.972480	38.707904
2316.711429	359132.067519	38.712922
2318.912073	359668.211402	38.717940
2320.995208	360211.065492	38.722957
2323.521920	360755.564221	38.727975
2325.841268	361301.916385	38.732992
2327.795870	361860.803246	38.738010
2330.057893	362409.635798	38.743028
2332.055192	362972.964839	38.748045
2334.591650	363532.061622	38.753063
2337.102645	364092.600543	38.758080
2339.108154	364664.757248	38.763098
2341.513186	365235.190573	38.768116
2343.710582	365821.174480	38.773133
2346.217532	366403.673698	38.778151
2348.289954	366971.802009	38.783168
2350.692767	367567.922252	38.788186
2352.978536	368149.390832	38.793204
2355.700967	368742.141951	38.798221
2357.375575	369343.883484	38.803239
2359.780417	369935.044431	38.808256
2362.357235	370539.001702	38.813274
2364.969811	371144.743848	38.818292
2367.633515	371750.112306	38.823309
2370.020566	372353.208185	38.828327
2372.575587	372939.273299	38.833344
2374.896103	373552.301949	38.838362
2377.180267	374154.978427	38.843380
2379.509591	374756.724118	38.848397
2381.797577	375377.283944	38.853415
2384.914732	375983.316594	38.858432
2387.046776	376595.536828	38.863450
2389.604639	377200.981029	38.868468
2392.343803	377809.047298	38.873485
2394.370071	378422.596349	38.878503
2396.910256	379036.328431	38.883520
2399.224222	379640.856519	38.888538
2401.813518	380257.829333	38.893556
2404.180103	380861.413834	38.898573
2406.730707	381469.368977	38.903591
2409.334410	382080.803260	38.908608
2411.634553	382695.521733	38.913626
2414.093879	383305.765310	38.918644
2416.513236	383925.917565	38.923661
2418.777679	384550.038702	38.928679
2421.529530	385168.793845	38.933696
2423.701285	385789.128586	38.938714
2426.130774	386405.225612	38.943732
2428.706866	387009.599308	38.948749
2430.930086	387637.951333	38.953767
2433.669676	388265.546483	38.958784
2436.283265	388886.457359	38.963802
2438.565635	389504.368533	38.968820
2440.896950	390121.980476	38.973837
2443.521318	390747.237737	38.978855
2446.179542	391358.332341	38.983872
2448.103020	391988.977701	38.988890
2450.469662	392603.694843	38.993908
2452.875936	393237.757864	38.998925
2455.285517	393863.620183	39.003943
2457.980301	394485.975376	39.008960
2460.225616	395120.557420	39.013978
2462.697938	395753.643817	39.018996
2465.223826	396386.276979	39.024013
2467.374958	397010.899149	39.029031
2470.016307	397631.955140	39.034048
2472.288869	398245.050552	39.039066
2474.719688	398833.043771	39.044084
2477.382255	399443.287220	39.049101
2479.566977	400051.113177	39.054119
2482.195445	400646.486962	39.059136
2484.589365	401252.909835	39.064154
2486.633074	401850.483482	39.069172
2489.289494	402458.332292	39.074189
2491.512534	403081.873132	39.079207
2494.240957	403699.793145	39.084224
2496.584313	404321.006163	39.089242
2498.717053	404951.766565	39.094260
2501.418476	405568.838755	39.099277
2503.664813	406215.259823	39.104295
2505.935603	406853.630548	39.109312
2508.451571	407501.775548	39.114330
2510.996789	408154.130982	39.119348
2513.385601	408801.860604	39.124365
2515.537960	409466.054325	39.129383
2518.255076	410141.461685	39.134400
2520.455497	410811.339088	39.139418
2522.959288	411484.822489	39.144436
2525.787943	412148.229951	39.149453
2528.324809	412841.025240	39.154471
2530.848323	413520.937652	39.159488
2533.291841	414210.546100	39.164506
2535.979610	414897.411322	39.169524
2538.806323	415582.032026	39.174541
2541.342177	416289.070457	39.179559
2543.769783	416965.970550	39.184576
2546.502264	417671.596184	39.189594
2549.043246	418368.142682	39.194612
2551.687282	419066.729520	39.199629
2554.038054	419770.840322	39.204647
2556.859290	420470.143983	39.209664
2559.420350	421170.382566	39.214682
2561.918441	421879.878998	39.219700
2565.313956	422582.244261	39.224717
2567.739227	423295.180875	39.229735
2570.209859	423996.392468	39.234752
2572.804086	424693.917912	39.239770
2575.417766	425402.711315	39.244788
2578.075607	426097.704991	39.249805
2580.372542	426815.066017	39.254823
2583.386056	427523.174330	39.259840
2586.043338	428229.649792	39.264858
2588.582755	428936.781907	39.269876
2591.280995	429649.030411	39.274893
2594.036301	430363.728552	39.279911
2596.822673	431073.742767	39.284928
2599.769891	431776.065441	39.289946
2601.888535	432481.945693	39.294964
2604.549737	433177.136231	39.299981
2606.974925	433887.630494	39.304999
2609.479204	434596.166534	39.310016
2612.571301	435306.203333	39.315034
2614.933836	436024.284221	39.320052
2617.833400	436723.528783	39.325069
2620.351733	437437.743718	39.330087
2623.000298	438137.947557	39.335104
2625.697925	438845.256651	39.340122
2628.230472	439557.023656	39.345140
2630.853482	440261.011189	39.350157
2633.313338	440981.498592	39.355175
2636.233589	441686.403881	39.360192
2638.932792	442393.650520	39.365210
2641.227385	443102.711943	39.370228
2644.231280	443788.866849	39.375245
2646.527393	444475.572244	39.380263
2649.456773	445155.321944	39.385280
2652.240524	445810.033443	39.390298
2654.424305	446500.133141	39.395316
2657.225740	447155.863118	39.400333
2659.645976	447836.472122	39.405351
2662.318997	448518.282259	39.410368
2664.898732	449198.265055	39.415386
2667.518426	449884.187647	39.420404
2669.789339	450570.246637	39.425421
2672.623140	451258.769715	39.430439
2675.001471	451954.425528	39.435456
2677.698232	452655.062778	39.440474
2680.097186	453370.390743	39.445492
2682.707327	454071.854159	39.450509
2685.664286	454789.367142	39.455527
2688.135429	455516.643587	39.460544
2690.835737	456230.507912	39.465562
2692.998087	456971.890513	39.470580
2696.119038	457696.201307	39.475597
2698.741659	458445.290825	39.480615
2701.014590	459179.193114	39.485632
2704.091076	459930.427548	39.490650
2706.580620	460690.223264	39.495668
2709.627204	461429.627827	39.500685
2712.234836	462195.614796	39.505703
2714.484358	462950.662809	39.510720
2717.719547	463721.086823	39.515738
2720.318706	464483.852664	39.520756
2722.978485	465252.542489	39.525773
2725.407928	466035.188431	39.530791
2728.152166	466808.603980	39.535808
2731.571714	467574.701466	39.540826
2733.885921	468369.652797	39.545844
2737.045053	469147.504492	39.550861
2739.678073	469937.992687	39.555879
2742.383125	470727.223623	39.560896
2745.642703	471499.405004	39.565914
2748.273017	472302.375549	39.570932
2751.386995	473078.103395	39.575949
2754.185345	473867.996004	39.580967
2756.992664	474655.782680	39.585984
2760.451357	475430.345839	39.591002
2763.119225	476206.471924	39.596020
2766.129580	476973.872016	39.601037
2768.948217	477757.888383	39.606055
2771.758268	478528.287069	39.611072
2774.830904	479309.417467	39.616090
2777.389471	480077.267205	39.621108
2779.793775	480839.151199	39.626125
2783.120082	481625.492965	39.631143
2785.901580	482399.822371	39.636160
2788.857317	483165.001256	39.641178
2791.725560	483944.248353	39.646196
2794.494187	484704.444288	39.651213
2797.546576	485479.504433	39.656231
2800.182557	486238.192526	39.661248
2802.996349	487000.251380	39.666266
2805.561762	487777.714064	39.671284
2808.680329	488531.377837	39.676301
2811.486633	489298.839968	39.681319
2814.047863	490072.769072	39.686336
2817.288410	490833.480102	39.691354
2819.911512	491608.642637	39.696372
2823.231753	492371.644737	39.701389
2825.978206	493135.060825	39.706407
2828.638805	493888.516361	39.711424
2831.351250	494633.554047	39.716442
2834.154589	495358.916748	39.721460
2836.856817	496076.898843	39.726477
2839.546881	496796.113756	39.731495
2842.165315	497528.123985	39.736512
2845.517695	498234.051345	39.741530
2848.236290	498961.442258	39.746548
2850.911380	499682.150186	39.751565
2853.668704	500410.329044	39.756583
2856.183343	501153.647557	39.761600
2859.025943	501888.354859	39.766618
2861.602392	502633.008836	39.771636
2864.262911	503378.119546	39.776653
2867.259537	504131.966113	39.781671
2869.937640	504896.873958	39.786688
2872.684773	505654.725461	39.791706
2875.448493	506436.741573	39.796724
2878.078804	507207.145324	39.801741
2880.876589	507984.643945	39.806759
2883.757582	508768.493954	39.811776
2886.596514	509553.572874	39.816794
2889.189214	510360.733399	39.821812
2891.805405	511159.431094	39.826829
2894.936224	511968.336735	39.831847
2897.639950	512778.329878	39.836864
2901.012895	513603.290955	39.841882
2903.655230	514423.339881	39.846900
2906.478928	515234.698522	39.851917
2909.550339	516076.058003	39.856935
2912.774364	516919.715091	39.861952
2915.709731	517737.223400	39.866970
2918.449575	518573.614543	39.871988
2921.631145	519409.837045	39.877005
2924.735028	520255.951272	39.882023
2926.901757	521099.855967	39.887040
2930.476139	521940.157270	39.892058
2933.621385	522789.750876	39.897076
2936.477653	523635.466223	39.902093
2939.627077	524492.619205	39.907111
2942.711909	525332.309047	39.912128
2945.816810	526169.732789	39.917146
2948.827903	527023.843099	39.922164
2951.805400	527869.601800	39.927181
2955.326780	528716.431039	39.932199
2958.032640	529568.280271	39.937216
2961.449594	530401.688212	39.942234
2964.325043	531247.220058	39.947252
2967.179458	532082.638956	39.952269
2970.352240	532929.534710	39.957287
2973.470110	533768.739743	39.962304
2976.606065	534606.081413	39.967322
2979.386125	535443.634614	39.972340
2982.518005	536294.517580	39.977357
2985.801786	537134.204287	39.982375
2988.605083	537975.631820	39.987392
2991.556384	538812.406760	39.992410
2994.870708	539659.285974	39.997428
2997.820284	540483.535858	40.002445
3001.017661	541325.153020	40.007463
3004.061077	542165.286585	40.012480
3007.045965	543000.249041	40.017498
3010.015707	543824.652239	40.022516
3012.868546	544667.081602	40.027533
3016.246791	545497.102465	40.032551
3018.689104	546335.374682	40.037568
3021.696365	547161.686117	40.042586
3024.910896	547998.322272	40.047604
3027.990408	548837.695181	40.052621
3030.799762	549658.459320	40.057639
3033.805197	550470.293927	40.062656
3036.811834	551266.697506	40.067674
3039.666539	552061.420720	40.072692
3042.348982	552847.731723	40.077709
3045.704554	553651.778961	40.082727
3048.385399	554455.688487	40.087744
3051.338522	555258.902037	40.092762
3054.093681	556075.668145	40.097780
3057.205183	556886.748027	40.102797
3059.887994	557715.083546	40.107815
3062.631811	558544.713977	40.112832
3065.958774	559373.543263	40.117850
3068.947836	560216.492681	40.122868
3071.717981	561070.776947	40.127885
3074.927339	561913.631614	40.132903
3077.859337	562783.600077	40.137920
3080.830855	563639.140317	40.142938
3083.691118	564510.612605	40.147956
3086.594874	565380.562991	40.152973
3089.791697	566263.462000	40.157991
3092.610413	567161.927906	40.163008
3095.720251	568049.539045	40.168026
3098.752327	568945.736441	40.173044
3101.594381	569857.413855	40.178061
3104.990526	570763.563874	40.183079
3107.778781	571676.324644	40.188096
3110.919808	572602.361759	40.193114
3114.285396	573524.781094	40.198132
3117.407381	574455.402678	40.203149
3120.425248	575388.832555	40.208167
3123.610524	576322.666980	40.213184
3126.694005	577264.274745	40.218202
3129.953935	578202.722066	40.223220
3133.298262	579155.079604	40.228237
3136.478092	580091.390532	40.233255
3139.734915	581044.670037	40.238272
3143.391230	581988.883000	40.243290
3146.555092	582922.623764	40.248308
3149.532061	583891.523953	40.253325
3153.013958	584832.988484	40.258343
3156.092870	585780.512692	40.263360
3159.362231	586722.316671	40.268378
3162.870564	587674.684718	40.273396
3165.883748	588629.715458	40.278413
3169.348203	589580.886947	40.283431
3172.434413	590530.942556	40.288448
3175.640874	591472.934980	40.293466
3179.318530	592429.255898	40.298484
3182.257545	593388.777809	40.303501
3185.832280	594330.181640	40.308519
3189.137769	595288.135886	40.313536
3192.653446	596222.284449	40.318554
3195.570369	597154.954525	40.323572
3198.862820	598098.706650	40.328589
3202.247238	599033.202675	40.333607
3205.140770	599977.769286	40.338624
3208.521503	600911.863944	40.343642
3211.657827	601855.185481	40.348660
3214.861392	602796.015548	40.353677
3218.257006	603742.193071	40.358695
3221.439780	604691.881170	40.363712
3224.566221	605620.878900	40.368730
3227.900149	606575.940368	40.373748
3230.871242	607518.420732	40.378765
3234.150373	608460.371402	40.383783
3237.199719	609415.790101	40.388800
3240.356170	610352.749305	40.393818
3243.715588	611280.842349	40.398836
3246.639322	612196.925134	40.403853
3249.811337	613090.034094	40.408871
3253.147198	614000.898694	40.413888
3256.465437	614901.989660	40.418906
3259.600308	615801.387192	40.423924
3262.511034	616714.798291	40.428941
3265.707918	617627.586326	40.433959
3269.147259	618551.106572	40.438976
3272.156596	619473.519892	40.443994
3275.148661	620395.408120	40.449012
3278.145235	621330.161969	40.454029
3281.386187	622275.039719	40.459047
3284.691726	623213.977671	40.464064
3287.487619	624163.610509	40.469082
3291.063497	625129.018547	40.474100
3294.470996	626086.973714	40.479117
3297.297701	627058.176106	40.484135
3300.800888	628038.668572	40.489152
3304.012678	629015.422768	40.494170
3307.200137	629998.433113	40.499188
3310.243262	630999.601634	40.504205
3313.774449	631992.056682	40.509223
3317.140217	633004.564713	40.514240
3320.340160	634022.692989	40.519258
3323.807789	635020.312704	40.524276
3326.747869	636050.365133	40.529293
3330.185859	637070.901106	40.534311
3333.771876	638086.571559	40.539328
3336.724288	639130.936045	40.544346
3340.316698	640170.499204	40.549364
3343.700448	641212.585407	40.554381
3347.050941	642263.998169	40.559399
3350.524357	643299.571806	40.564416
3353.900580	644354.405317	40.569434
3357.249818	645408.734608	40.574452
3360.392856	646473.907011	40.579469
3363.989193	647531.613504	40.584487
3367.375472	648592.284017	40.589504
3370.766730	649657.626348	40.594522
3374.311461	650720.686734	40.599540
3378.010732	651799.803706	40.604557
3381.345819	652860.078622	40.609575
3384.876430	653928.577806	40.614592
3388.041354	655004.344571	40.619610
3392.140231	656064.049814	40.624628
3396.065808	657133.779655	40.629645
3398.894674	658194.360246	40.634663
3403.053451	659255.303521	40.639680
3406.046811	660323.194001	40.644698
3410.024591	661377.163968	40.649716
3412.933951	662447.323260	40.654733
3416.423442	663498.852302	40.659751
3419.882729	664559.975944	40.664768
3423.574056	665629.005308	40.669786
3427.403774	666682.069853	40.674804
3430.594915	667740.794862	40.679821
3434.003637	668795.983439	40.684839
3437.375604	669859.566080	40.689856
3441.145296	670911.574420	40.694874
3444.371929	671966.041237	40.699892
3447.965527	673024.157953	40.704909
3451.541842	674078.180674	40.709927
3454.705965	675145.624290	40.714944
3458.174560	676196.641650	40.719962
3461.843232	677248.799393	40.724980
3465.060995	678309.558853	40.729997
3468.515829	679364.791106	40.735015
3472.290968	680401.653344	40.740020
3475.453519	681390.114803	40.745024
3478.941451	682319.851438	40.750029
3482.223613	683200.429490	40.755034
3485.115531	684004.060336	40.760039
3488.404451	684760.805247	40.765044
3491.296056	685434.564707	40.770048
3494.545841	686050.421140	40.775053
3497.102708	686590.042559	40.780058
3499.898843	687072.203110	40.785063
3502.277795	687473.527860	40.790068
3504.914586	687830.248390	40.795072
3507.141625	688111.573938	40.800077
3508.936425	688342.697396	40.805082
3510.980652	688516.692374	40.810087
3513.070194	688637.477513	40.815092
3514.856123	688713.871081	40.820096
3516.742732	688727.942039	40.825101
3518.030328	688697.472566	40.830106
3519.129291	688614.332593	40.835111
3520.639236	688510.371725	40.840116
3521.859208	688373.462113	40.845120
3523.251821	688192.776197	40.850125
3524.496337	687968.513504	40.855130
3525.928504	687720.374338	40.860135
3527.019159	687427.489933	40.865140
3527.829536	687111.547232	40.870144
3528.677873	686760.395904	40.875149
3529.348760	686399.304670	40.880154
3529.974732	686011.474736	40.885159
3530.757128	685604.436385	40.890164
3531.532455	685176.620894	40.895168
3532.443334	684719.239366	40.900173
3532.416943	684256.761395	40.905178
3532.817203	683769.094473	40.910183
3533.389301	683288.394220	40.915188
3533.459622	682784.346575	40.920192
3534.129876	682266.776034	40.925197
3533.989698	681750.704260	40.930202
3534.853639	681203.060238	40.935207
3535.479228	680667.227561	40.940212
3535.511544	680105.957716	40.945216
3536.109264	679527.723006	40.950221
3536.011652	678964.213158	40.955226
3536.417034	678361.526152	40.960231
3536.688572	677774.666157	40.965236
3536.650233	677186.624178	40.970240
3536.600678	676570.641444	40.975245
3536.833153	675977.694505	40.980250
3536.937333	675354.778626	40.985255
3537.244177	674740.011472	40.990260
3536.975816	674122.955950	40.995264
3537.229982	673499.442999	41.000269
3537.104583	672877.346914	41.005274
3536.979278	672242.646344	41.010279
3537.377134	671622.823802	41.015284
3537.119229	670993.545119	41.020288
3537.270107	670352.688353	41.025293
3536.766023	669729.050430	41.030298
3537.086699	669088.079978	41.035303
3537.029582	668450.769250	41.040308
3536.954405	667819.503769	41.045312
3536.824826	667176.533257	41.050317
3536.487376	666543.480544	41.055322
3536.380503	665911.046268	41.060327
3536.676620	665276.458235	41.065332
3536.696487	664650.106187	41.070336
3536.422765	664007.095926	41.075341
3536.118804	663371.532712	41.080346
3536.322385	662741.033910	41.085351
3536.270030	662102.101746	41.090356
3536.008100	661465.507642	41.095360
3535.803718	660826.017085	41.100365
3536.047025	660194.696799	41.105370
3535.760619	659565.020198	41.110375
3535.480654	658923.619665	41.115380
3535.369780	658302.519165	41.120384
3535.452924	657668.864690	41.125389
3535.031853	657050.381973	41.130394
3534.940936	656415.776238	41.135399
3534.687520	655799.434093	41.140404
3534.366545	655189.357186	41.145408
3534.549016	654550.840277	41.150413
3534.270890	653942.427199	41.155418
3534.168226	653328.253206	41.160423
3533.805298	652713.534465	41.165428
3533.565906	652117.941164	41.170432
3533.945603	651510.219454	41.175437
3533.751228	650897.258995	41.180442
3533.520458	650289.263541	41.185447
3533.600453	649677.781852	41.190452
3532.813713	649080.098265	41.195456
3533.015991	648476.518726	41.200461
3532.683237	647885.635786	41.205466
3532.474373	647287.100373	41.210471
3532.483891	646697.790617	41.215476
3532.098942	646109.911069	41.220480
3532.111207	645518.082525	41.225485
3531.919865	644947.450301	41.230490
3531.475355	644361.928628	41.235495
3531.416997	643780.359497	41.240500
3531.196753	643210.234309	41.245504
3531.243371	642637.532953	41.250509
3530.657373	642070.604574	41.255514
3530.353194	641507.299070	41.260519
3530.289016	640938.821614	41.265524
3530.000445	640385.654556	41.270528
3530.127013	639823.335842	41.275533
3529.638548	639279.845815	41.280538
3529.370166	638742.994064	41.285543
3529.338317	638198.021059	41.290548
3529.198921	637656.939306	41.295552
3528.819471	637109.314589	41.300557
3528.622657	636581.444559	41.305562
3528.323256	636044.707977	41.310567
3528.507305	635510.416032	41.315572
3528.053557	634990.764066	41.320576
3527.825496	634468.596796	41.325581
3527.469957	633956.584000	41.330586
3527.354455	633441.954027	41.335591
3527.247566	632931.001192	41.340596
3526.859019	632432.933886	41.345600
3526.909944	631907.189127	41.350605
3526.605684	631424.077201	41.355610
3526.304431	630923.621259	41.360615
3526.055775	630428.740070	41.365620
3525.937620	629937.819494	41.370624
3526.004406	629446.094618	41.375629
3525.827920	628975.016249	41.380634
3525.350422	628492.700074	41.385639
3525.058769	628013.786572	41.390644
3525.041161	627545.322663	41.395648
3524.756191	627074.979159	41.400653
3524.393728	626604.978248	41.405658
3524.174306	626147.153640	41.410663
3524.108731	625685.126901	41.415668
3523.717465	625237.459214	41.420672
3523.878717	624788.880337	41.425677
3523.509462	624345.579769	41.430682
3523.347177	623903.178610	41.435687
3523.694072	623454.363166	41.440692
3523.285434	623023.188132	41.445696
3523.011410	622566.121621	41.450701
3522.966578	622141.214233	41.455706
3522.461346	621711.455738	41.460711
3522.399504	621282.809693	41.465716
3521.921474	620849.555158	41.470720
3522.213265	620421.267795	41.475725
3521.727189	620015.291705	41.480730
3521.643474	619607.329817	41.485735
3522.009447	619195.519825	41.490740
3521.264720	618784.328378	41.495744
3521.479133	618366.046807	41.500749
3521.198960	617970.786697	41.505754
3521.004110	617555.448673	41.510759
3521.151956	617164.900877	41.515764
3520.439473	616765.207343	41.520768
3520.430585	616360.621037	41.525773
3520.290344	615977.648077	41.530778
3519.978232	615590.128025	41.535783
3519.904030	615203.507717	41.540788
3519.595425	614829.697295	41.545792
3519.703155	614450.089883	41.550797
3519.603578	614080.932702	41.555802
3519.151287	613709.063560	41.560807
3519.146007	613337.710011	41.565812
3518.590090	612970.045206	41.570816
3519.087188	612598.935207	41.575821
3518.852788	612250.098847	41.580826
3518.500944	611887.379456	41.585831
3518.737292	611532.274654	41.590836
3518.264237	611182.039979	41.595840
3518.301856	610823.735622	41.600845
3518.216649	610471.508919	41.605850
3517.666513	610120.350904	41.610855
3517.922845	609774.315719	41.615860
3517.844923	609444.827816	41.620864
3517.663328	609096.987985	41.625869
3517.372220	608757.683279	41.630874
3517.004875	608421.089832	41.635879
3517.165492	608088.914342	41.640884
3516.748390	607764.098653	41.645888
3516.814317	607445.214377	41.650893
3516.649421	607116.676144	41.655898
3516.634998	606794.274792	41.660903
3516.389435	606475.815913	41.665908
3515.977247	606164.550605	41.670912
3516.278106	605844.829950	41.675917
3515.804890	605546.352788	41.680922
3515.464123	605247.544890	41.685927
3515.648426	604938.506146	41.690932
3515.415631	604646.288523	41.695936
3515.020395	604334.267797	41.700941
3515.248574	604041.707817	41.705946
3514.999250	603755.191146	41.710951
3514.852309	603459.466185	41.715956
3514.580356	603183.628782	41.720960
3514.668098	602884.487684	41.725965
3514.555712	602606.251180	41.730970
3514.350038	602325.413314	41.735975
3514.265389	602044.498446	41.740980
3513.781685	601777.345573	41.745984
3513.757027	601499.971328	41.750989
3513.805282	601238.691584	41.755994
3513.433279	600973.459329	41.760999
3513.260896	600701.862988	41.766004
3513.389557	600449.587971	41.771008
3513.567794	600190.070280	41.776013
3513.867614	599928.317823	41.781018
3512.936374	599664.452930	41.786023
3513.388547	599405.977004	41.791028
3512.827014	599161.669794	41.796032
3512.819788	598907.726784	41.801037
3512.833317	598655.783121	41.806042
3512.329473	598418.178631	41.811047
3512.475089	598168.411839	41.816052
3512.062744	597938.414409	41.821056
3512.297173	597684.254228	41.826061
3512.101046	597464.053396	41.831066
3512.089900	597215.396698	41.836071
3512.086556	596985.413499	41.841076
3512.110630	596753.563255	41.846080
3511.921694	596517.876785	41.851085
3511.998499	596285.807710	41.856090
3511.587626	596053.914833	41.861095
3511.848261	595824.970148	41.866100
3511.414553	595615.872318	41.871104
3511.639183	595386.724128	41.876109
3511.309813	595159.219670	41.881114
3511.095824	594944.448690	41.886119
3511.140346	594721.946777	41.891124
3511.080900	594509.754089	41.896128
3510.774460	594296.694195	41.901133
3510.718680	594084.191875	41.906138
3510.602574	593878.828118	41.911143
3510.781197	593680.695480	41.916148
3510.518320	593461.636022	41.921152
3510.725005	593265.249852	41.926157
3510.917117	593053.893686	41.931162
3510.653143	592850.595931	41.936167
3510.447687	592639.950909	41.941172
3510.356605	592440.937734	41.946176
3510.035944	592240.251041	41.951181
3510.225678	592044.299534	41.956186
3510.097667	591853.370626	41.961191
3510.178565	591652.808776	41.966196
3509.941605	591452.848545	41.971200
3509.979595	591260.576548	41.976205
3510.034029	591066.339357	41.981210
3509.453475	590870.897356	41.986215
3509.601240	590681.813363	41.991220
3509.366076	590501.431239	41.996224
3509.220372	590324.196990	42.001229
3509.236343	590135.779223	42.006234
3509.264099	589959.013413	42.011239
3509.505555	589778.139858	42.016244
3509.171262	589603.689514	42.021248
3509.287223	589420.168154	42.026253
3509.185166	589243.362907	42.031258
3508.818070	589063.533540	42.036263
3508.890810	588889.759450	42.041268
3508.849121	588725.097003	42.046272
3509.029364	588559.591709	42.051277
3508.922782	588393.578628	42.056282
3508.688902	588216.830215	42.061287
3508.825953	588046.601240	42.066292
3508.642603	587869.688634	42.071296
3508.801288	587701.762891	42.076301
3508.406816	587531.614212	42.081306
3508.423487	587372.300923	42.086311
3508.485519	587197.046697	42.091316
3508.373267	587035.036333	42.096320
3508.065535	586884.615343	42.101325
3508.355589	586727.811647	42.106330
3508.346605	586571.959858	42.111335
3508.594860	586401.438021	42.116340
3508.013023	586255.175674	42.121344
3508.362873	586088.100657	42.126349
3507.936451	585937.184812	42.131354
3508.053376	585786.629914	42.136359
3508.054506	585630.864854	42.141364
3507.686367	585477.872886	42.146368
3507.682084	585327.030665	42.151373
3507.698776	585182.114390	42.156378
3507.728652	585036.892617	42.161383
3508.067164	584886.993754	42.166388
3507.618699	584737.021652	42.171392
3507.684790	584585.454884	42.176397
3507.836933	584441.211193	42.181402
3507.419025	584293.138765	42.186407
3507.503558	584138.547264	42.191412
3507.395353	584000.574650	42.196416
3507.374478	583868.970436	42.201421
3507.235406	583721.699707	42.206426
3506.724391	583592.737099	42.211431
3507.233636	583452.344039	42.216436
3507.070901	583315.026188	42.221440
3506.730569	583183.517488	42.226445
3506.953923	583046.786553	42.231450
3506.868353	582917.796979	42.236455
3507.078757	582781.014930	42.241460
3506.808853	582644.109396	42.246464
3506.692967	582512.858146	42.251469
3506.790709	582385.793520	42.256474
3506.745994	582255.231652	42.261479
3506.655542	582121.508436	42.266484
3506.262125	582009.453298	42.271488
3506.421206	581885.842570	42.276493
3506.530331	581762.842178	42.281498
3506.787454	581641.173717	42.286503
3506.760727	581512.209921	42.291508
3506.272056	581383.170047	42.296512
3506.517708	581267.734582	42.301517
3506.702126	581141.799255	42.306522
3506.321842	581009.519567	42.311527
3506.654513	580887.479220	42.316532
3506.387125	580767.749003	42.321536
3506.361094	580650.190332	42.326541
3506.388600	580516.430202	42.331546
3506.190152	580413.228681	42.336551
3506.346252	580292.166939	42.341556
3506.172378	580173.370952	42.346560
3506.313178	580059.098003	42.351565
3505.990185	579942.637525	42.356570
3505.859432	579824.736232	42.361575
3505.968449	579707.800054	42.366580
3505.829497	579593.468318	42.371584
3506.162402	579484.187193	42.376589
3505.532387	579373.907130	42.381594
3505.716011	579278.025621	42.386599
3505.769575	579158.226892	42.391604
3505.558963	579061.654322	42.396608
3505.589437	578949.300318	42.401613
3505.451093	578844.868809	42.406618
3505.625756	578745.514571	42.411623
3505.740121	578635.557887	42.416628
3505.721119	578530.299391	42.421632
3505.475414	578422.311256	42.426637
3505.437350	578315.444709	42.431642
3505.555041	578220.119105	42.436647
3505.696149	578104.067779	42.441652
3505.639165	577999.967806	42.446656
3505.386126	577903.091434	42.451661
3505.651659	577806.380332	42.456666
3505.275131	577698.910413	42.461671
3505.691688	577594.678719	42.466676
3505.260941	577486.411159	42.471680
3505.355539	577386.405386	42.476685
3505.414391	577283.839535	42.481690
3505.354983	577180.789348	42.486695
3505.752435	577078.618692	42.491700
3505.345186	576981.961749	42.496704
3505.505363	576866.851415	42.501709
3505.598932	576775.945037	42.506714
3505.068104	576673.421030	42.511719
3505.221108	576585.571760	42.516724
3504.813325	576485.792445	42.521728
3504.910657	576385.576990	42.526733
3505.000598	576294.265294	42.531738
3505.163452	576202.639105	42.536743
3505.096050	576103.504869	42.541748
3504.941734	576021.637924	42.546752
3505.013659	575927.459276	42.551757
3504.869183	575836.585287	42.556762
3504.721853	575751.345105	42.561767
3505.145018	575642.015360	42.566772
3504.684295	575555.567886	42.571776
3504.649012	575458.586333	42.576781
3505.008858	575379.950576	42.581786
3504.768014	575297.388879	42.586791
3505.014766	575193.064517	42.591796
3504.750142	575114.731221	42.596800
3504.972498	575023.438741	42.601805
3504.932484	574931.987604	42.606810
3504.540919	574847.636735	42.611815
3504.378816	574754.292748	42.616820
3504.540244	574671.710953	42.621824
3504.830508	574592.930808	42.626829
3504.483333	574512.796260	42.631834
3504.644983	574413.158133	42.636839
3504.592066	574328.798283	42.641844
3504.877192	574252.884482	42.646848
3504.862241	574165.096228	42.651853
3504.925173	574072.414434	42.656858
3504.867738	573992.933172	42.661863
3504.684970	573903.359565	42.666868
3504.794101	573813.133484	42.671872
3504.532673	573719.798184	42.676877
3504.804673	573637.543564	42.681882
3504.457275	573550.208300	42.686887
3504.459152	573469.053651	42.691892
3504.371685	573397.372044	42.696896
3504.658492	573309.075284	42.701901
3505.005081	573222.981858	42.706906
3504.501621	573144.575016	42.711911
3504.721599	573049.998208	42.716916
3504.643818	572975.444690	42.721920
3504.485807	572884.752843	42.726925
3504.854838	572798.753459	42.731930
3504.416537	572731.453001	42.736935
3504.608763	572624.499933	42.741940
3504.226344	572556.132696	42.746944
3504.425299	572460.951150	42.751949
3504.575620	572401.753561	42.756954
3504.439487	572322.174111	42.761959
3504.664557	572234.634781	42.766964
3504.322859	572156.698327	42.771968
3504.355967	572072.812399	42.776973
3504.264779	571991.361688	42.781978
3504.333697	571920.098801	42.786983
3504.698759	571827.652663	42.791988
3504.260340	571745.452482	42.796993
3504.462694	571671.348316	42.801997
3504.492172	571585.748889	42.807002
3504.372009	571518.037312	42.812007
3504.516697	571431.310810	42.817012
3504.336473	571362.803170	42.822017
3504.239177	571280.443121	42.827021
3504.545233	571201.337307	42.832026
3504.218041	571124.046296	42.837031
3504.316103	571036.821564	42.842036
3504.107790	570963.334484	42.847041
3504.033818	570880.716389	42.852045
3504.175234	570808.126920	42.857050
3504.148667	570744.170039	42.862055
3504.470593	570656.754843	42.867060
3504.463782	570579.256755	42.872065
3504.475462	570510.461278	42.877069
3504.466009	570425.162400	42.882074
3504.603921	570356.898866	42.887079
3504.511935	570270.757028	42.892084
3504.176446	570185.711573	42.897089
3504.245578	570107.896150	42.902093
3504.435841	570037.357608	42.907098
3504.218463	569966.130949	42.912103
3504.484242	569877.562153	42.917108
3504.240125	569802.262504	42.922113
3504.537782	569725.061344	42.927117
3504.651900	569651.211599	42.932122
3504.723297	569572.587296	42.937127
3504.593863	569488.761444	42.942132
3504.300740	569400.835053	42.947137
3504.176100	569327.777714	42.952141
3504.246129	569245.980894	42.957146
3504.218570	569172.051068	42.962151
3504.333869	569096.084075	42.967156
3504.232702	569022.215843	42.972161
3504.492709	568958.454443	42.977165
3504.566944	568860.448021	42.982170
3504.141192	568776.766992	42.987175
3504.581863	568700.895034	42.992180
3504.565204	568621.927079	42.997185
3504.442311	568545.895410	43.002189
3504.606783	568467.550975	43.007194
3504.438516	568381.912304	43.012199
3504.523983	568302.623558	43.017204
3504.167659	568226.527794	43.022209
3504.275855	568151.160373	43.027213
3504.707994	568067.232679	43.032218
3504.273706	567995.829459	43.037223
3504.794060	567914.956628	43.042228
3504.305874	567845.222495	43.047233
3504.138876	567759.629798	43.052237
3504.199121	567676.918549	43.057242
3503.940982	567613.688872	43.062247
3504.033095	567535.149332	43.067252
3503.856346	567463.348361	43.072257
3503.990176	567397.989242	43.077261
3504.309271	567326.005124	43.082266
3504.198961	567256.809573	43.087271
3504.121664	567176.936659	43.092276
3503.990402	567098.179575	43.097281
3503.956743	567023.986696	43.102285
3504.026178	566952.595352	43.107290
3503.516058	566894.135471	43.112295
3504.107551	566820.543148	43.117300
3504.046990	566756.622299	43.122305
3503.920613	566682.593751	43.127309
3504.220240	566615.844181	43.132314
3503.868760	566544.872318	43.137319
3504.182028	566469.914325	43.142324
3503.917007	566397.769580	43.147329
3503.916890	566320.949421	43.152333
3503.950556	566250.315200	43.157338
3503.876487	566191.780281	43.162343
3504.006941	566112.520981	43.167348
3504.046646	566051.751646	43.172353
3503.689548	565985.358747	43.177357
3504.076109	565909.177214	43.182362
3503.688310	565851.598616	43.187367
3504.105301	565775.209910	43.192372
3504.082497	565698.339448	43.197377
3503.989262	565633.109499	43.202381
3504.239007	565556.042251	43.207386
3503.897282	565494.880060	43.212391
3503.958096	565420.158963	43.217396
3504.157476	565346.622875	43.222401
3504.268063	565271.892722	43.227405
3504.355755	565192.181733	43.232410
3503.844927	565121.026931	43.237415
3504.215049	565048.770003	43.242420
3504.335437	564983.451238	43.247425
3504.293898	564910.707570	43.252429
3504.410106	564830.083423	43.257434
3503.863806	564772.677186	43.262439
3504.178234	564688.746951	43.267444
3504.260505	564611.349261	43.272449
3504.183082	564541.831680	43.277453
3504.327093	564463.013194	43.282458
3503.764335	564393.826536	43.287463
3504.263835	564309.460571	43.292468
3504.140479	564247.904076	43.297473
3503.987417	564178.245968	43.302477
3504.305421	564103.978412	43.307482
3504.004964	564039.630544	43.312487
3504.149634	563953.910953	43.317492
3504.079270	563882.878186	43.322497
3503.574357	563809.650861	43.327501
3503.915855	563741.419439	43.332506
3503.828076	563681.364929	43.337511
3503.833949	563607.599138	43.342516
3503.758832	563542.456410	43.347521
3503.894390	563478.084271	43.352525
3503.702644	563406.716448	43.357530
3503.786334	563342.906063	43.362535
3503.875100	563263.535549	43.367540
3503.764641	563209.978105	43.372545
3503.733406	563146.538169	43.377549
3504.140215	563083.932103	43.382554
3503.684082	563013.512058	43.387559
3503.753678	562938.271728	43.392564
3503.933473	562880.636786	43.397569
3504.210434	562809.540943	43.402573
3504.282498	562738.428123	43.407578
3503.897817	562673.181006	43.412583
3503.925564	562595.780338	43.417588
3503.716631	562529.143948	43.422593
3503.995262	562462.074386	43.427597
3504.089333	562390.402135	43.432602
3503.302229	562333.629098	43.437607
3503.748278	562260.085307	43.442612
3503.801055	562208.360055	43.447617
3503.812080	562136.297244	43.452621
3504.073934	562070.386655	43.457626
3503.678055	562006.699136	43.462631
3504.044854	561916.850622	43.467636
3503.911163	561865.054027	43.472641
3503.507774	561797.338079	43.477645
3503.792514	561729.206238	43.482650
3503.629718	561669.054131	43.487655
3504.302356	561595.116765	43.492660
3503.964239	561529.805919	43.497665
3504.022177	561460.098555	43.502669
3504.016910	561390.753756	43.507674
3503.764627	561331.118446	43.512679
3503.723680	561253.217573	43.517684
3503.679347	561185.036416	43.522689
3503.672460	561125.359735	43.527693
3503.806137	561054.328355	43.532698
3503.757099	560990.326944	43.537703
3503.891148	560925.287817	43.542708
3504.024052	560862.968103	43.547713
3503.934626	560793.936197	43.552717
3503.844890	560714.227133	43.557722
3503.937512	560651.963421	43.562727
3503.707698	560569.758428	43.567732
3503.331448	560518.298673	43.572737
3503.528858	560458.232761	43.577741
3503.693732	560387.797008	43.582746
3503.503408	560344.112315	43.587751
3503.577096	560272.834788	43.592756
3503.662731	560214.599297	43.597761
3503.523640	560150.004270	43.602765
3503.497858	560084.534051	43.607770
3503.487285	560031.753016	43.612775
3503.712508	559967.248157	43.617780
3503.800195	559895.412266	43.622785
3503.684090	559826.480423	43.627789
3503.581883	559756.488241	43.632794
3503.262511	559701.792492	43.637799
3503.573384	559644.222500	43.642804
3503.450779	559583.500212	43.647809
3503.397564	559533.695856	43.652813
3503.533862	559465.576778	43.657818
3503.589460	559415.149638	43.662823
3503.619856	559344.881589	43.667828
3503.555199	559287.170455	43.672833
3503.381298	559232.700633	43.677837
3503.882448	559153.690671	43.682842
3503.582409	559104.126845	43.687847
3503.697776	559026.086329	43.692852
3503.424796	558967.652596	43.697857
3503.564228	558921.340033	43.702861
3503.618211	558849.755867	43.707866
3503.556328	558802.267191	43.712871
3503.555745	558729.432122	43.717876
3503.484211	558666.732781	43.722881
3503.377617	558618.797483	43.727885
3503.429756	558550.334975	43.732890
3503.379782	558491.358687	43.737895
3503.561651	558433.200244	43.742900
3503.205616	558379.965838	43.747905
3503.418346	558320.290673	43.752909
3503.384565	558257.432063	43.757914
3503.310116	558210.295941	43.762919
3503.799974	558140.197658	43.767924
3503.598623	558080.438533	43.772929
3503.421643	558022.438170	43.777933
3503.657572	557955.151256	43.782938
3503.111388	557894.642151	43.787943
3503.205500	557833.725018	43.792948
3503.605298	557776.484887	43.797953
3503.011867	557728.223608	43.802957
3503.312656	557670.193354	43.807962
3503.189123	557626.287192	43.812967
3503.425121	557562.171858	43.817972
3503.774836	557508.364294	43.822977
3503.554067	557454.751269	43.827981
3503.101343	557384.753958	43.832986
3503.078542	557329.193549	43.837991
3503.393632	557274.080986	43.842996
3503.454121	557211.655282	43.848001
3503.123112	557163.449461	43.853005
3503.403737	557096.301974	43.858010
3503.135337	557051.914028	43.863015
3503.135846	556982.998577	43.868020
3503.260815	556934.011516	43.873025
3503.252850	556884.492033	43.878029
3503.443179	556825.972539	43.883034
3503.411944	556776.305357	43.888039
3503.460212	556708.791191	43.893044
3503.414910	556657.161153	43.898049
3503.373051	556601.298587	43.903053
3503.493994	556533.167020	43.908058
3503.457644	556475.842049	43.913063
3503.581059	556418.389747	43.918068
3503.546319	556354.363607	43.923073
3503.440907	556299.064419	43.928077
3503.831860	556228.670121	43.933082
3503.348276	556174.944123	43.938087
3503.333429	556112.576078	43.943092
3503.539789	556051.733077	43.948097
3503.490691	555997.330207	43.953101
3503.645976	555928.635719	43.958106
3503.268641	555894.892192	43.963111
3503.455038	555828.559961	43.968116
3503.271425	555769.795182	43.973121
3503.523191	555704.408809	43.978125
3503.528043	555649.239913	43.983130
3503.198815	555592.110564	43.988135
3503.557359	555543.936419	43.993140
3503.307026	555478.732448	43.998145
3503.381757	555424.558759	44.003149
3503.543668	555355.003739	44.008154
3503.364534	555295.681933	44.013159
3503.519459	555233.432971	44.018164
3503.748461	555176.310630	44.023169
3503.515926	555115.283788	44.028173
3503.823696	555058.147966	44.033178
3503.459118	555006.060337	44.038183
3503.266077	554934.697418	44.043188
3503.380203	554869.682353	44.048193
3503.102345	554810.122747	44.053197
3503.254223	554744.949704	44.058202
3503.213164	554707.217736	44.063207
3503.024103	554634.744093	44.068212
3503.169004	554590.632578	44.073217
3503.225311	554535.853716	44.078221
3503.371385	554477.180110	44.083226
3503.062007	554426.038473	44.088231
3503.172808	554366.060151	44.093236
3503.405972	554305.910239	44.098241
3503.245294	554261.243360	44.103245
3503.307277	554206.714158	44.108250
3503.376037	554154.047950	44.113255
3503.498283	554105.907597	44.118260
3503.456380	554049.127440	44.123265
3503.103338	553990.382798	44.128269
3503.496679	553925.216389	44.133274
3502.927218	553877.038037	44.138279
3503.145056	553824.043645	44.143284
3503.188462	553764.224918	44.148289
3503.294408	553709.636075	44.153293
3503.225957	553652.757846	44.158298
3503.290708	553603.214278	44.163303
3503.199169	553544.273433	44.168308
3503.095717	553493.547829	44.173313
3503.035608	553438.783695	44.178317
3503.522614	553371.029290	44.183322
3503.216971	553325.375395	44.188327
3503.333688	553270.531051	44.193332
3503.350794	553208.597793	44.198337
3503.171840	553161.461133	44.203341
3503.105670	553101.455966	44.208346
3502.944699	553062.479375	44.213351
3502.933942	553002.766986	44.218356
3503.128280	552953.250074	44.223361
3502.885277	552907.433270	44.228365
3502.990225	552851.077406	44.233370
3502.745007	552803.043358	44.238375
3502.935570	552758.263235	44.243380
3503.369035	552702.457329	44.248385
3503.178842	552645.141390	44.253389
3503.332978	552589.330655	44.258394
3503.236188	552539.658633	44.263399
3503.403655	552477.747649	44.268404
3503.078187	552425.089276	44.273409
3502.944739	552368.014782	44.278413
3503.290184	552313.783996	44.283418
3502.971882	552275.183824	44.288423
3502.978424	552219.093522	44.293428
3503.179925	552175.771115	44.298433
3503.032768	552129.633518	44.303437
3503.146935	552063.899420	44.308442
3503.067455	552008.981512	44.313447
3503.028383	551973.811745	44.318452
3503.198165	551911.343447	44.323457
3502.848867	551865.288657	44.328461
3503.402061	551803.462224	44.333466
3502.881183	551761.668624	44.338471
3503.141815	551697.924470	44.343476
3503.263948	551647.658748	44.348481
3502.976836	551597.863452	44.353485
3503.366626	551543.975067	44.358490
3502.966257	551492.030974	44.363495
3502.843467	551436.513123	44.368500
3502.774147	551390.460984	44.373505
3502.715343	551337.653655	44.378509
3502.988453	551294.014254	44.383514
3502.881718	551256.132291	44.388519
3502.852743	551202.714747	44.393524
3503.024234	551159.293253	44.398529
3502.949271	551112.283533	44.403533
3502.988493	551060.114157	44.408538
3502.864077	551014.271421	44.413543
3502.899605	550963.765451	44.418548
3502.789800	550909.553690	44.423553
3502.725438	550856.644614	44.428557
3502.798942	550821.705316	44.433562
3502.682698	550771.022044	44.438567
3502.715081	550722.330094	44.443572
3502.937488	550672.901054	44.448577
3502.770714	550634.523254	44.453581
3503.417654	550567.030926	44.458586
3502.870684	550531.991529	44.463591
3502.961138	550471.041723	44.468596
3503.032975	550429.448765	44.473601
3502.890753	550388.949381	44.478605
3503.158814	550329.683321	44.483610
3502.933768	550296.001511	44.488615
3502.885539	550248.480393	44.493620
3502.857795	550187.296790	44.498625
3503.142927	550147.734310	44.503629
3502.942390	550092.324603	44.508634
3503.051563	550050.875548	44.513639
3502.972308	550001.191374	44.518644
3503.122256	549946.479362	44.523649
3502.781817	549892.251165	44.528653
3503.212240	549838.097340	44.533658
3503.190482	549798.987650	44.538663
3503.156630	549736.240529	44.543668
3503.198722	549690.869949	44.548673
3502.906386	549631.945234	44.553677
3503.252553	549582.189436	44.558682
3502.822012	549525.807250	44.563687
3502.867550	549481.443499	44.568692
3502.997911	549433.134051	44.573697
3502.838362	549389.055820	44.578701
3502.921053	549345.441580	44.583706
3502.715132	549304.747862	44.588711
3502.772748	549245.360574	44.593716
3502.856869	549197.612378	44.598721
3502.896985	549162.775158	44.603725
3502.665777	549112.860772	44.608730
3502.931283	549067.300096	44.613735
3502.788408	549010.414731	44.618740
3502.819582	548965.194769	44.623745
3502.422891	548926.043559	44.628749
3502.710849	548874.984217	44.633754
3502.487770	548837.669200	44.638759
3502.790244	548789.530754	44.643764
3502.897224	548754.026186	44.648769
3502.609656	548702.960229	44.653773
3502.776219	548647.988264	44.658778
3502.992376	548611.305960	44.663783
3503.186271	548554.917700	44.668788
3502.843808	548509.001686	44.673793
3502.550450	548463.430285	44.678797
3502.992914	548421.518121	44.683802
3502.844519	548374.964777	44.688807
3502.723374	548332.691538	44.693812
3502.624782	548282.802692	44.698817
3502.552094	548248.737879	44.703821
3502.786503	548189.316897	44.708826
3502.639012	548155.163360	44.713831
3502.737936	548116.129809	44.718836
3502.964773	548059.330815	44.723841
3502.475638	548024.527514	44.728845
3502.777398	547977.797828	44.733850
3502.736084	547932.586417	44.738855
3502.620882	547887.538265	44.743860
3502.725415	547845.579216	44.748865
3502.763199	547801.160909	44.753869
3502.860856	547754.212046	44.758874
3502.419726	547715.518408	44.763879
3502.778546	547666.257710	44.768884
3502.739713	547621.548983	44.773889
3502.645535	547579.722693	44.778893
3502.585177	547525.338171	44.783898
3502.809559	547493.894365	44.788903
3502.581386	547443.973423	44.793908
3502.728964	547403.014177	44.798913
3502.411859	547364.904064	44.803917
3502.916739	547311.685867	44.808922
3502.809649	547278.935055	44.813927
3502.731199	547228.686186	44.818932
3502.901667	547194.679527	44.823937
3502.469426	547151.042364	44.828941
3502.267686	547097.788545	44.833946
3502.751617	547069.426633	44.838951
3502.832862	547019.806064	44.843956
3502.714398	546969.865330	44.848961
3502.426124	546931.345959	44.853965
3502.902260	546880.701954	44.858970
3502.604481	546842.486386	44.863975
3502.587022	546798.174787	44.868980
3502.867963	546757.746214	44.873985
3502.803266	546714.198349	44.878989
3502.794130	546671.699905	44.883994
3502.508866	546620.424193	44.888999
3502.828474	546580.089560	44.894004
3502.802860	546538.954635	44.899009
3502.678973	546494.609187	44.904013
3503.027374	546443.430063	44.909018
3502.688549	546404.463813	44.914023
3502.175749	546357.661219	44.919028
3502.438911	546314.663064	44.924033
3502.387352	546287.597784	44.929037
3502.576191	546227.722134	44.934042
3502.382881	546194.478797	44.939047
3502.379190	546153.238281	44.944052
3502.579852	546114.787318	44.949057
3502.651698	546079.079997	44.954061
3502.883882	546022.372593	44.959066
3502.710713	545994.015931	44.964071
3502.511706	545939.244684	44.969076
3502.821575	545892.355372	44.974081
3502.755550	545858.686913	44.979085
3503.046711	545809.985363	44.984090
3502.830943	545762.577214	44.989095
3502.827602	545718.511929	44.994100
3502.806333	545670.466394	44.999105
3502.805775	545639.559636	45.004109
3502.862621	545587.568286	45.009114
3502.788872	545547.245056	45.014119
3503.020028	545503.241285	45.019124
3502.851550	545451.387395	45.024129
3502.787256	545411.818503	45.029133
3502.545257	545364.161219	45.034138
3502.607415	545318.218345	45.039143
3502.541490	545276.531705	45.044148
3502.740987	545233.944059	45.049153
3502.581867	545196.759928	45.054157
3503.071920	545143.384606	45.059162
3502.792871	545105.312424	45.064167
3502.792694	545058.420974	45.069172
3502.596920	545014.486011	45.074177
3502.519693	544971.237270	45.079181
3502.439486	544920.375276	45.084186
3502.839691	544884.459516	45.089191
3502.766227	544844.033358	45.094196
3502.902058	544801.858256	45.099201
3502.468409	544753.474137	45.104205
3502.838853	544714.134155	45.109210
3502.576969	544685.789443	45.114215
3502.446744	544636.951542	45.119220
3502.964613	544594.864127	45.124225
3502.937839	544561.387751	45.129229
3502.616345	544505.673016	45.134234
3502.710414	544464.159271	45.139239
3502.678896	544421.808906	45.144244
3502.701174	544371.381830	45.149249
3502.502606	544332.336231	45.154253
3502.668498	544285.263546	45.159258
3502.529137	544240.106680	45.164263
3502.702337	544199.335465	45.169268
3502.793160	544150.610708	45.174273
3502.555509	544100.628880	45.179277
3502.639792	544067.385140	45.184282
3502.788691	544029.340348	45.189287
3502.558366	543987.929069	45.194292
3502.674290	543943.788096	45.199297
3502.286437	543902.402522	45.204301
3502.281035	543850.969630	45.209306
3502.446214	543823.662145	45.214311
3502.342109	543789.339433	45.219316
3502.687553	543749.194052	45.224321
3502.500173	543718.112120	45.229325
3502.679781	543665.992529	45.234330
3502.329979	543626.616899	45.239335
3502.329240	543590.410906	45.244340
3502.592091	543548.211091	45.249345
3502.436770	543515.761918	45.254349
3502.569956	543464.809034	45.259354
3502.536226	543420.892780	45.264359
3502.583742	543390.578239	45.269364
3502.747205	543341.284000	45.274369
3502.418027	543308.358726	45.279373
3503.013245	543255.614425	45.284378
3502.617021	543218.716233	45.289383
3502.708480	543182.141001	45.294388
3502.871111	543133.451299	45.299393
3502.695600	543086.682982	45.304397
3502.773941	543041.788943	45.309402
3502.677528	543004.336501	45.314407
3502.823714	542960.237873	45.319412
3502.489277	542916.268734	45.324417
3502.570915	542870.970177	45.329421
3503.035505	542839.778860	45.334426
3502.615730	542800.866298	45.339431
3502.829927	542741.576666	45.344436
3502.864660	542708.337869	45.349441
3502.588798	542667.081476	45.354445
3502.521197	542621.050265	45.359450
3502.717336	542580.270562	45.364455
3502.763920	542532.354346	45.369460
3502.571966	542493.453820	45.374465
3502.540285	542455.938818	45.379469
3502.816886	542409.295463	45.384474
3502.668292	542364.688808	45.389479
3502.655420	542316.378210	45.394484
3502.911715	542274.932112	45.399489
3502.577746	542236.155136	45.404493
3502.913503	542177.246543	45.409498
3502.849549	542135.197201	45.414503
3503.014779	542095.681970	45.419508
3502.858911	542037.509414	45.424513
3502.612962	542005.021251	45.429517
3502.977998	541943.383540	45.434522
3502.717767	541914.831215	45.439527
3502.374096	541874.693176	45.444532
3502.797755	541826.510692	45.449537
3502.341498	541796.981783	45.454541
3502.701923	541741.345415	45.459546
3502.428344	541710.727136	45.464551
3502.438977	541671.387490	45.469556
3502.464657	541632.196554	45.474561
3502.385208	541593.628032	45.479565
3502.611592	541559.800176	45.484570
3502.564434	541513.610676	45.489575
3502.441109	541473.334315	45.494580
3502.728148	541431.527637	45.499585
3502.362157	541384.230275	45.504589
3502.407828	541346.548271	45.509594
3502.557230	541306.428229	45.514599
3502.425067	541266.102298	45.519604
3502.587219	541216.498229	45.524609
3502.422099	541188.735714	45.529613
3502.573149	541149.068866	45.534618
3502.484147	541099.404902	45.539623
3502.411007	541064.061733	45.544628
3502.667220	541025.032864	45.549633
3502.494960	540992.025870	45.554637
3502.813557	540960.753591	45.559642
3502.852738	540910.613922	45.564647
3502.505441	540874.004127	45.569652
3502.573417	540829.407363	45.574657
3501.985119	540797.023266	45.579661
3502.173671	540749.380215	45.584666
3502.317248	540717.430132	45.589671
3502.316264	540689.135223	45.594676
3502.916227	540643.290170	45.599681
3502.546027	540594.175136	45.604685
3502.544928	540550.648049	45.609690
3502.709261	540518.391475	45.614695
3502.499185	540479.740564	45.619700
3502.617945	540443.758976	45.624705
3502.373349	540399.061052	45.629709
3502.461832	540358.141360	45.634714
3502.631293	540313.526248	45.639719
3502.777933	540278.245775	45.644724
3502.541842	540230.166575	45.649729
3502.290505	540192.732194	45.654733
3502.678546	540142.128812	45.659738
3502.747804	540122.799232	45.664743
3502.516175	540073.861312	45.669748
3502.909193	540027.846619	45.674753
3502.445334	539995.087106	45.679757
3502.689048	539945.818220	45.684762
3502.222127	539919.666559	45.689767
3502.510416	539876.291471	45.694772
3502.873158	539820.092342	45.699777
3502.565195	539792.401065	45.704781
3502.496985	539748.933016	45.709786
3502.609138	539706.897871	45.714791
3502.267438	539664.432989	45.719796
3502.363062	539630.722957	45.724801
3502.484719	539603.464918	45.729805
3502.420838	539556.716946	45.734810
3502.272699	539523.551234	45.739815
3502.197933	539471.659833	45.744820
3502.568549	539409.757974	45.749825
3502.213238	539330.220147	45.754829
3502.365518	539176.247158	45.759834
3502.142233	538976.986619	45.764839
3501.786916	538713.883755	45.769844
3501.830168	538398.601192	45.774849
3501.371847	538033.251202	45.779853
3501.173869	537595.356208	45.784858
3501.074731	537110.312123	45.789863
3500.891914	536561.596331	45.794868
3500.782048	535950.538001	45.799873
3500.280559	535282.806375	45.804877
3499.899804	534549.832267	45.809882
3499.590517	533767.256844	45.814887
3499.324031	532917.212770	45.819892
3498.983336	531986.535790	45.824897
3498.118635	531014.904077	45.829901
3497.527254	529972.045427	45.834906
3497.062620	528878.765958	45.839911
3496.170850	527713.489500	45.844916
3495.291353	526479.812541	45.849921
3494.404310	525189.738513	45.854925
3493.181627	523841.489667	45.859930
3492.643231	522433.923439	45.864935
3491.900509	520955.402991	45.869940
3491.185055	519416.578307	45.874945
3489.645195	517827.574396	45.879949
3488.402334	516164.902263	45.884954
3487.244467	514457.070773	45.889959
3486.326855	512680.897562	45.894964
3485.092342	510841.809696	45.899969
3483.813400	508947.828866	45.904973
3482.618530	507000.584253	45.909978
3481.232046	504999.901662	45.914983
3479.479646	502930.977520	45.919988
3478.277639	500820.337297	45.924993
3476.703627	498650.367712	45.929997
3475.138915	496431.961576	45.935002
3473.320925	494153.308163	45.940007
3471.739488	491825.689475	45.945012
3469.925188	489454.428846	45.950017
3467.850264	487044.577283	45.955021
3466.414321	484579.321514	45.960026
3464.491403	482069.104390	45.965031
3462.214181	479516.116932	45.970036
3460.501281	476913.661697	45.975041
3457.959837	474270.358783	45.980045
3456.047609	471594.920594	45.985050
3454.229314	468862.451612	45.990055
3451.682256	466105.140018	45.995060
3449.883433	463303.075684	46.000065
3447.635758	460458.064148	46.005069
3444.947365	457580.431863	46.010074
3442.739420	454669.258654	46.015079
3440.182147	451716.763657	46.020084
3437.898865	448732.924301	46.025089
3435.290821	445721.027906	46.030093
3432.581421	442668.909689	46.035098
3429.646604	439593.220211	46.040103
3427.234534	436484.700852	46.045108
3424.827228	433346.830957	46.050113
3421.518216	430207.364736	46.055117
3418.659239	427007.308018	46.060122
3415.977019	423794.460018	46.065127
3412.918811	420558.913034	46.070132
3410.593710	417285.834243	46.075137
3407.350186	414006.189726	46.080141
3404.181823	410698.362642	46.085146
3401.219846	407371.168644	46.090151
3398.043701	404027.397127	46.095156
3394.925754	400645.437681	46.100161
3391.645636	397262.469048	46.105165
3388.568408	393854.935301	46.110170
3385.683765	390430.565329	46.115175
3381.938634	387001.914898	46.120180
3378.728431	383537.801901	46.125185
3375.566461	380068.938922	46.130189
3371.954003	376579.501254	46.135194
3368.617030	373084.502563	46.140199
3365.031569	369582.817535	46.145204
3361.654508	366069.471167	46.150209
3358.146011	362539.745265	46.155213
3354.626854	358994.007837	46.160218
3350.920706	355463.380908	46.165223
3347.247147	351917.364843	46.170228
3343.899729	348353.781228	46.175233
3340.150295	344782.476996	46.180237
3336.175955	341213.076720	46.185242
3332.634449	337635.965819	46.190247
3328.812259	334061.477139	46.195252
3324.979851	330471.328779	46.200257
3320.942290	326891.498395	46.205261
3317.047768	323307.661481	46.210266
3313.410253	319726.148522	46.215271
3309.316048	316143.015592	46.220276
3305.514315	312550.028777	46.225281
3301.608209	308966.231308	46.230285
3297.801040	305383.352752	46.235290
3293.655702	301805.907011	46.240295
3289.565614	298231.447541	46.245300
3285.865293	294656.391197	46.250305
3281.818692	291098.110195	46.255309
3277.743323	287525.802298	46.260314
3273.690206	283969.162709	46.265319
3269.778101	280429.177189	46.270324
3265.848461	276873.514971	46.275329
3261.704336	273327.737182	46.280333
3257.505812	269796.642194	46.285338
3253.408515	266260.681609	46.290343
3248.911813	262750.510510	46.295348
3245.073589	259240.700952	46.300353
3240.898010	255747.396288	46.305357
3236.767822	252256.281632	46.310362
3232.643141	248781.330407	46.315367
3228.602525	245321.266218	46.320372
3224.352315	241855.263875	46.325377
3219.993471	238406.670435	46.330381
3215.751641	234968.505549	46.335386
3211.630415	231540.217747	46.340391
3207.061612	228128.148985	46.345396
3202.978347	224733.223512	46.350401
3198.129240	221357.056394	46.355405
3193.940308	217987.809065	46.360410
3190.048741	214645.385237	46.365415
3185.204751	211298.781632	46.370420
3180.785310	207971.064446	46.375425
3176.666101	204687.376629	46.380429
3172.299425	201405.563692	46.385434
3168.107288	198052.502767	46.390439
3163.784695	194791.154935	46.395444
3159.578687	191554.198250	46.400449
3154.836191	188348.451852	46.405453
3150.607718	185138.635027	46.410458
3146.382137	181955.788282	46.415463
3141.959148	178794.501859	46.420468
3137.820388	175648.389352	46.425473
3133.058790	172532.058161	46.430477
3128.620725	169415.801057	46.435482
3124.496119	166319.739033	46.440487
3119.823707	163256.203137	46.445492
3115.536174	160190.914250	46.450497
3111.094752	157164.641639	46.455501
3106.712434	154161.540804	46.460506
3102.576899	151163.563241	46.465511
3098.070686	148195.191460	46.470516
3093.870197	145232.156278	46.475521
3089.157282	142307.029174	46.480525
3084.893537	139391.084236	46.485530
3080.671429	136501.209240	46.490535
3076.120082	133630.512317	46.495540
3071.639513	130766.905835	46.500545
3067.187461	127952.196359	46.505549
3063.057832	125133.087400	46.510554
3059.019200	122347.549448	46.515559
3054.716171	119581.649906	46.520564
3050.496294	116814.498344	46.525569
3045.994119	114080.099794	46.530573
3041.927263	111364.526117	46.535578
3037.585785	108663.220563	46.540583
3033.414266	105980.021539	46.545588
3028.807385	103307.753069	46.550593
3023.836864	100693.593829	46.555597
3019.371460	98094.658896	46.560602
3014.954139	95502.189156	46.565607
3009.958149	92957.614059	46.570612
3005.906392	90406.833464	46.575617
3001.416449	87906.959448	46.580621
2996.976927	85409.014215	46.585626
2992.309218	82948.841224	46.590631
2987.910939	80519.906291	46.595636
2983.659724	78101.542785	46.600641
2979.148592	75708.630806	46.605645
2974.324823	73345.010316	46.610650
2970.280858	71004.231429	46.615655
2965.720959	68686.687546	46.620660
2961.580852	66386.946491	46.625665
2957.027715	64122.698279	46.630669
2952.574330	61874.395254	46.635674
2948.520773	59663.630432	46.640679
2943.406318	57464.304501	46.645684
2939.041565	55293.051122	46.650689
2934.352624	53151.383744	46.655693
2929.632206	51042.673485	46.660698
2924.535180	48968.941745	46.665703
2919.085411	46939.772162	46.670708
2912.763083	44972.606006	46.675713
2904.596069	43106.546966	46.680717
2896.890854	41300.824112	46.685722
2889.764224	39563.738435	46.690727
2882.312147	37907.823077	46.695732
2875.843799	36330.759209	46.700737
2869.022002	34828.618858	46.705741
2862.754863	33392.258789	46.710746
2856.555553	32040.466199	46.715751
2850.793207	30745.371834	46.720756
2845.056005	29521.800305	46.725761
2839.450174	28361.787159	46.730765
2834.401670	27259.297744	46.735770
2829.372812	26202.319959	46.740775
2824.446367	25201.792757	46.745780
2819.682581	24241.765784	46.750785
2814.985296	23315.260401	46.755789
2810.410618	22440.649637	46.760794
2806.356584	21599.310590	46.765799
2801.887480	20785.272174	46.770804
2797.831371	20000.900954	46.775809
2793.892199	19250.520469	46.780813
2790.119710	18520.060756	46.785818
2786.475141	17804.964466	46.790823
2782.194754	17110.224962	46.795828
2778.819380	16425.174299	46.800833
2775.152894	15759.661024	46.805837
2771.442023	15124.349714	46.810842
2768.253919	14482.975156	46.815847
2764.255137	13849.138359	46.820852
2760.832035	13217.420968	46.825857
2757.355244	12608.469463	46.830861
2754.008728	11999.514414	46.835866
2750.573594	11407.881966	46.840871
2746.873844	10819.182046	46.845876
2743.906959	10218.984724	46.850881
2740.357620	9650.738029	46.855885
2736.655968	9063.316304	46.860890
2733.440227	8483.136629	46.865895
2729.993715	7920.490979	46.870900
2726.756446	7344.442248	46.875905
2722.903940	6787.191468	46.880909
2719.340669	6221.838798	46.885914
2715.809409	5666.455233	46.890919
2712.260256	5115.478023	46.895924
2708.730531	4568.104687	46.900929
2705.084845	4032.905866	46.905933
2700.770651	3511.619306	46.910938
2695.845773	3012.212580	46.915943
2690.568454	2544.724816	46.920948
2685.828947	2101.585286	46.925953
2680.694816	1696.270106	46.930957
2675.636108	1309.879582	46.935962
2670.369862	953.302755	46.940967
2664.831508	643.897970	46.945972
2659.727469	360.427922	46.950977
2651.547946	182.059632	46.955981
2639.767121	179.541451	46.960986
2631.845802	180.002136	46.965991
2626.975257	184.543680	46.970996
2625.208091	184.317219	46.976001
2623.425351	178.385382	46.981005
2622.052704	179.826885	46.986010
2620.503769	177.943045	46.991015
2618.550046	183.184564	46.996020
2615.532157	180.161730	47.001025
2612.245869	176.109249	47.006029
2608.714765	186.793295	47.011034
2605.388430	176.798722	47.016039
2601.292657	186.363480	47.021044
2598.468809	174.974451	47.026049
2595.629869	181.788451	47.031053
2592.070352	174.883686	47.036058
2589.024423	170.650655	47.041063
2585.817175	179.446768	47.046068
2582.691804	171.444184	47.051073
2579.269807	180.166807	47.056077
2576.213404	172.719219	47.061082
2572.904297	167.255981	47.066087
2568.942136	175.078273	47.071092
2566.015339	173.460517	47.076097
2562.801267	166.447856	47.081101
2559.035480	177.366024	47.086106
2555.605730	160.996636	47.091111
2552.025956	173.335365	47.096116
2549.122486	174.699564	47.101121
2545.817684	175.450744	47.106125
2541.836180	175.292948	47.111130
2538.368709	171.744833	47.116135
2535.033824	172.914220	47.121140
2532.337110	168.677271	47.126145
2528.861679	173.045889	47.131149
2524.808095	171.073005	47.136154
2521.434857	163.936663	47.141159
2517.673710	177.482299	47.146164
2514.824982	173.686840	47.151169
2511.430500	175.875683	47.156173
2507.757816	173.232924	47.161178
2504.582595	162.684619	47.166183
2501.279838	173.351557	47.171188
2498.131433	167.269428	47.176193
2494.077741	169.834676	47.181197
2490.966570	165.308571	47.186202
2487.433853	166.891906	47.191207
2483.369446	171.047538	47.196212
2480.243895	172.936654	47.201217
2477.066557	165.617242	47.206221
2473.143290	163.812342	47.211226
2470.142014	169.259166	47.216231
2466.292990	170.591209	47.221236
2462.855840	164.623464	47.226241
2459.865181	161.384687	47.231245
2456.074318	161.660039	47.236250
2452.854104	161.621368	47.241255
2448.908586	165.611764	47.246260
2445.887293	156.043759	47.251265
2442.367907	160.951325	47.256269
2438.603758	155.443311	47.261274
2435.303425	160.688886	47.266279
2431.632690	158.381743	47.271284
2427.908106	155.247549	47.276289
2424.385868	161.220456	47.281293
2421.321156	168.533189	47.286298
2418.053195	150.558488	47.291303
2414.707690	168.620227	47.296308
2411.156620	153.699360	47.301313
2407.704286	162.596007	47.306317
2404.073791	168.937673	47.311322
2400.639681	162.614653	47.316327
2396.893264	167.577091	47.321332
2393.377645	157.852328	47.326337
2390.185745	155.519855	47.331341
2385.957564	168.723105	47.336346
2383.401326	160.252565	47.341351
2379.814463	163.810834	47.346356
2376.649235	160.941933	47.351361
2372.878136	165.105278	47.356365
2368.770616	154.693608	47.361370
2365.791795	159.115336	47.366375
2362.187259	159.675356	47.371380
2358.920375	166.131086	47.376385
2355.331346	157.866963	47.381389
2351.368568	167.380729	47.386394
2347.721994	158.011523	47.391399
2344.716871	162.257629	47.396404
2341.781508	159.140440	47.401409
2338.157546	161.007720	47.406413
2334.319704	160.209880	47.411418
2330.917787	155.926855	47.416423
2327.251126	166.507528	47.421428
2323.909146	156.512611	47.426433
2320.144878	159.994036	47.431437
2316.898008	158.821191	47.436442
2313.895280	155.925113	47.441447
2309.977626	165.351732	47.446452
2306.322236	166.767179	47.451457
2303.192287	165.757384	47.456461
2299.276563	162.337517	47.461466
2296.027717	158.500501	47.466471
2292.197679	163.394326	47.471476
2288.587749	164.094218	47.476481
2285.428123	162.288521	47.481485
2281.735719	167.623388	47.486490
2278.620168	161.656765	47.491495
2274.882116	166.581597	47.496500
2271.451988	160.909642	47.501505
2268.214078	164.135285	47.506509
2264.511971	162.222607	47.511514
2261.006902	160.605779	47.516519
2257.341729	164.407951	47.521524
2254.264569	149.972597	47.526529
2250.625375	154.281992	47.531533
2247.135064	159.464322	47.536538
2243.944042	156.975114	47.541543
2239.992269	166.720399	47.546548
2236.635622	166.089081	47.551553
2233.410612	167.879126	47.556557
2229.935200	167.861814	47.561562
2226.393977	161.806446	47.566567
2222.209431	173.425062	47.571572
2219.061874	163.251697	47.576577
2215.697777	159.497309	47.581581
2211.875236	161.268402	47.586586
2208.197936	157.203804	47.591591
2205.052868	163.600834	47.596596
2201.569569	161.342647	47.601601
2198.534775	156.884648	47.606605
2194.554344	157.310693	47.611610
2191.224601	162.780324	47.616615
2187.623655	159.685897	47.621620
2184.159493	163.855142	47.626625
2180.856364	162.106756	47.631629
2176.906287	161.627135	47.636634
2173.756375	152.071091	47.641639
2170.003192	167.032925	47.646644
2166.495339	168.308472	47.651649
2163.285231	155.615955	47.656653
2159.617629	164.253468	47.661658
2156.164857	158.909770	47.666663
2152.661821	164.966910	47.671668
2149.342521	156.511599	47.676673
2145.854955	166.293183	47.681677
2141.987524	161.285951	47.686682
2138.759924	162.058595	47.691687
2135.281664	165.504378	47.696692
2131.690888	159.133628	47.701697
2128.125198	152.070414	47.706701
2124.808296	157.193801	47.711706
2121.654750	155.075410	47.716711
2117.842325	165.929723	47.721716
2113.988521	154.445883	47.726721
2110.399626	164.022408	47.731725
2106.911784	160.818985	47.736730
2103.636040	151.901450	47.741735
2100.116750	157.697263	47.746740
2096.859152	154.444780	47.751745
2093.269055	154.461106	47.756749
2089.642221	160.035507	47.761754
2086.382073	154.251560	47.766759
2082.543303	167.890790	47.771764
2079.318207	167.668853	47.776769
2075.799173	162.857928	47.781773
2071.817187	164.737947	47.786778
2068.932847	162.185190	47.791783
2065.292358	164.118545	47.796788
2061.600817	158.056556	47.801793
2058.256894	154.023070	47.806797
2054.658624	157.596471	47.811802
2051.232177	155.159689	47.816807
2047.778711	161.589186	47.821812
2044.253474	153.564226	47.826817
2040.940656	154.671884	47.831821
2037.099226	157.459776	47.836826
2033.482623	150.098773	47.841831
2030.139464	158.313369	47.846836
2026.679795	148.397725	47.851841
2023.295178	163.081705	47.856845
2019.390688	159.136870	47.861850
2016.228160	147.077585	47.866855
2012.569644	158.338330	47.871860
2009.203013	152.640700	47.876865
2005.938054	154.254355	47.881869
2002.633377	160.261863	47.886874
1998.813729	152.962047	47.891879
1995.259647	161.415153	47.896884
1991.619414	157.104640	47.901889
1988.386959	156.526003	47.906893
1984.466245	162.480148	47.911898
1981.252473	155.047924	47.916903
1977.786695	152.307867	47.921908
1974.399826	152.375575	47.926913
1971.067474	156.317169	47.931917
1967.102101	164.708369	47.936922
1963.957409	151.607371	47.941927
1960.121972	164.683310	47.946932
1956.419762	160.786030	47.951937
1953.348043	150.226389	47.956941
1949.372003	161.855165	47.961946
1946.129774	154.265453	47.966951
1942.556934	156.566225	47.971956
1939.291623	159.284698	47.976961
1935.709785	153.657004	47.981965
1932.124633	158.994924	47.986970
1928.884846	157.400047	47.991975
1925.137855	161.710505	47.996980
1921.511479	164.224581	48.001985
1918.294405	159.654395	48.006989
1914.810046	168.279174	48.011994
1911.358626	153.387682	48.016999
1907.674994	156.365502	48.022004
1904.414872	153.416492	48.027009
1900.810951	157.397458	48.032013
1896.877901	154.225892	48.037018
1893.785285	153.398267	48.042023
1890.066138	162.166823	48.047028
1886.730223	162.353659	48.052033
1883.284327	150.085525	48.057037
1879.523133	162.979540	48.062042
1876.253612	154.545427	48.067047
1872.679828	153.425894	48.072052
1869.165191	156.595273	48.077057
1865.875903	157.443409	48.082061
1862.196381	159.247787	48.087066
1858.637844	145.645905	48.092071
1854.934516	155.818514	48.097076
1851.852453	154.792819	48.102081
1848.448540	158.566733	48.107085
1844.592208	146.905563	48.112090
1841.249496	151.774085	48.117095
1837.722466	153.011198	48.122100
1834.141158	158.051749	48.127105
1830.605453	148.454311	48.132109
1827.005035	149.064366	48.137114
1823.555459	147.082893	48.142119
1820.243899	153.008174	48.147124
1816.655626	155.791914	48.152129
1813.292355	149.715183	48.157133
1809.752657	161.029253	48.162138
1806.367304	155.659693	48.167143
1802.530801	159.045487	48.172148
1799.342452	158.753730	48.177153
1795.837324	147.116686	48.182157
1792.094613	159.096777	48.187162
1788.589014	147.078555	48.192167
1784.966066	150.090053	48.197172
1781.458580	150.052117	48.202177
1778.391555	150.094363	48.207181
1774.379985	150.799213	48.212186
1771.435552	148.724073	48.217191
1767.647007	145.064801	48.222196
1764.114516	150.467349	48.227201
1760.692179	150.942854	48.232205
1757.176373	147.236365	48.237210
1753.505337	145.752714	48.242215
1750.274046	150.535398	48.247220
1746.397334	148.591587	48.252225
1743.106645	149.487400	48.257229
1739.359547	156.133341	48.262234
1736.087730	147.674264	48.267239
1732.622871	157.225999	48.272244
1729.286869	155.861862	48.277249
1725.715567	148.572372	48.282253
1722.226905	155.310416	48.287258
1719.045426	144.449594	48.292263
1715.417684	143.021181	48.297268
1711.402472	150.033492	48.302273
1707.998191	145.987742	48.307277
1704.199020	157.661867	48.312282
1701.143593	150.606273	48.317287
1697.746313	158.687532	48.322292
1694.202010	152.084497	48.327297
1690.816043	146.374126	48.332301
1686.846331	157.787531	48.337306
1683.523792	144.130439	48.342311
1679.974282	151.817311	48.347316
1676.422319	147.675605	48.352321
1673.583003	143.941092	48.357325
1669.513649	143.775241	48.362330
1666.189430	139.933175	48.367335
1662.079710	152.452532	48.372340
1658.556982	147.481719	48.377345
1656.066383	146.541371	48.382349
1652.048951	154.028701	48.387354
1648.769523	149.812980	48.392359
1645.471420	151.528259	48.397364
1641.569638	151.331786	48.402369
1637.967372	147.661580	48.407373
1634.509344	153.614928	48.412378
1631.382610	150.615856	48.417383
1627.708600	155.853817	48.422388
1623.799851	151.204338	48.427393
1620.184924	150.616525	48.432397
1616.611946	151.645105	48.437402
1613.764454	145.528306	48.442407
1610.017702	148.694579	48.447412
1606.490874	151.643953	48.452417
1603.359613	146.803674	48.457421
1599.452624	157.994440	48.462426
1595.901595	143.620152	48.467431
1592.335899	144.518092	48.472436
1589.191437	147.556646	48.477441
1585.912379	146.776410	48.482445
1581.773310	153.159644	48.487450
1578.517711	144.173680	48.492455
1575.008186	145.450915	48.497460
1571.424657	142.934871	48.502465
1567.816623	142.163617	48.507469
1564.189167	153.345712	48.512474
1560.968224	136.622642	48.517479
1557.422013	144.316941	48.522484
1554.138259	149.299444	48.527489
1550.576871	138.217760	48.532493
1546.955348	149.659175	48.537498
1543.670852	140.890945	48.542503
1540.035872	142.948300	48.547508
1536.387088	143.911912	48.552513
1533.078804	139.631783	48.557517
1529.207820	146.172638	48.562522
1526.050959	141.882687	48.567527
1522.365290	142.524426	48.572532
1519.145751	141.442931	48.577537
1515.582258	142.490346	48.582541
1511.723466	140.415305	48.587546
1508.438783	139.583365	48.592551
1504.917085	145.075873	48.597556
1501.422715	142.304200	48.602561
1498.098768	134.257689	48.607565
1494.641481	148.460807	48.612570
1490.999271	139.738904	48.617575
1487.540461	143.244671	48.622580
1483.823160	138.694916	48.627585
1480.274993	137.938703	48.632589
1476.906765	148.476324	48.637594
1473.382900	138.302981	48.642599
1470.363458	139.049963	48.647604
1466.373690	145.321392	48.652609
1462.814914	137.005272	48.657613
1458.992044	143.513956	48.662618
1455.998223	134.452865	48.667623
1452.405718	142.804923	48.672628
1448.955694	140.467609	48.677633
1445.633309	139.067093	48.682637
1442.081742	148.842715	48.687642
1438.424530	147.795519	48.692647
1434.443555	156.177852	48.697652
1431.187919	136.690961	48.702657
1428.017344	132.592796	48.707661
1424.159762	144.434234	48.712666
1421.003759	139.648698	48.717671
1417.358560	145.549056	48.722676
1413.785710	140.696645	48.727681
1410.667331	138.504260	48.732685
1406.870460	140.817385	48.737690
1403.109203	134.938776	48.742695
1400.072180	136.023199	48.747700
1396.324754	139.667900	48.752705
1392.940651	143.261637	48.757709
1389.433624	144.686404	48.762714
1385.964094	139.982706	48.767719
1382.476322	138.977608	48.772724
1378.589362	143.326010	48.777729
1375.407366	134.973744	48.782733
1371.552325	141.441041	48.787738
1368.580696	132.917256	48.792743
1364.750058	145.433922	48.797748
1361.129999	142.249181	48.802753
1357.959498	132.872613	48.807757
1354.387574	146.135095	48.812762
1350.743292	141.676987	48.817767
1347.506372	139.088245	48.822772
1343.653562	144.499626	48.827777
1340.159465	138.651113	48.832781
1336.906269	134.054772	48.837786
1333.064588	144.538120	48.842791
1329.613800	136.969550	48.847796
1326.221003	145.686524	48.852801
1323.098355	141.892112	48.857805
1319.088664	145.537597	48.862810
1315.745787	137.322083	48.867815
1312.255663	138.623342	48.872820
1308.620936	149.005211	48.877825
1305.295463	136.953703	48.882829
1301.528301	144.162142	48.887834
1298.736553	142.876297	48.892839
1295.092062	139.688940	48.897844
1291.413917	134.733857	48.902849
1288.006855	138.565703	48.907853
1284.270561	144.833269	48.912858
1280.743192	139.062925	48.917863
1276.860142	137.931235	48.922868
1273.247750	134.238336	48.927873
1270.650231	140.254922	48.932877
1266.865200	141.742704	48.937882
1263.206874	135.424699	48.942887
1259.775291	139.496241	48.947892
1255.988877	148.469351	48.952897
1252.863314	135.662581	48.957901
1249.103335	140.623950	48.962906
1245.787403	138.368231	48.967911
1242.184113	144.846506	48.972916
1238.480540	143.564013	48.977921
1235.103701	131.128552	48.982925
1231.812576	142.209086	48.987930
1228.337479	136.743127	48.992935
1225.114594	136.316969	48.997940
1221.340393	132.052923	49.002945
1217.537506	136.272900	49.007949
1214.006727	138.471545	49.012954
1210.533611	132.327217	49.017959
1206.884308	143.447440	49.022964
1203.742098	135.280348	49.027969
1200.413832	131.145665	49.032973
1197.071242	144.193913	49.037978
1193.750361	143.967503	49.042983
1190.035322	139.806580	49.047988
1185.671277	143.530885	49.052993
1182.448875	134.799059	49.057997
1178.854482	137.816352	49.063002
1175.753115	136.274907	49.068007
1172.095248	138.482358	49.073012
1168.418125	142.202642	49.078017
1165.441081	131.344393	49.083021
1161.462052	143.578868	49.088026
1157.836045	136.177349	49.093031
1154.683270	137.716793	49.098036
1151.106385	142.704803	49.103041
1147.960823	134.700718	49.108045
1144.104886	133.014479	49.113050
1140.503359	134.866310	49.118055
1137.098288	139.653843	49.123060
1133.418049	143.406441	49.128065
1130.188144	134.566375	49.133069
1126.414380	143.348829	49.138074
1123.153772	128.393963	49.143079
1119.778343	134.256052	49.148084
1116.217288	137.209467	49.153089
1112.681786	140.020129	49.158093
1108.783850	138.504260	49.163098
1105.707746	140.302797	49.168103
1101.800010	139.552651	49.173108
1098.689278	141.139845	49.178113
1095.314368	130.078655	49.183117
1091.594848	149.105318	49.188122
1088.102262	135.805236	49.193127
1084.543301	127.718196	49.198132
1080.867523	133.906442	49.203137
1077.990235	127.320737	49.208141
1074.003134	138.905588	49.213146
1070.343971	134.960498	49.218151
1067.066910	142.392375	49.223156
1063.305313	134.521787	49.228161
1059.712902	129.826439	49.233165
1056.350862	137.894581	49.238170
1053.286520	142.882378	49.243175
1049.983170	131.906091	49.248180
1046.327932	135.803019	49.253185
1042.861797	131.227706	49.258189
1038.874278	133.358931	49.263194
1035.556821	132.434084	49.268199
1031.983963	133.769164	49.273204
1028.304731	131.177228	49.278209
1024.869561	130.786906	49.283213
1021.469989	140.839404	49.288218
1017.861998	137.232227	49.293223
1014.219410	132.839445	49.298228
1010.844821	135.039452	49.303233
1007.635741	126.121255	49.308237
1004.223564	140.182616	49.313242
1000.801060	130.993639	49.318247
996.888965	139.558702	49.323252
993.669366	135.516522	49.328257
990.562578	128.993693	49.333261
986.569674	139.418823	49.338266
982.795925	132.174700	49.343271
979.112348	139.509471	49.348276
975.860595	138.582485	49.353281
972.771959	129.047250	49.358285
968.862921	137.109404	49.363290
965.343519	135.740245	49.368295
961.904302	139.663087	49.373300
958.491494	133.801451	49.378305
955.307766	118.407582	49.383309
951.294870	134.710813	49.388314
947.593892	136.861039	49.393319
944.375837	135.842860	49.398324
940.829642	133.112567	49.403329
937.624314	136.911103	49.408333
933.934502	135.407542	49.413338
930.433191	130.761373	49.418343
927.226039	130.591736	49.423348
923.429678	135.098982	49.428353
919.837401	130.725392	49.433357
916.154879	129.752272	49.438362
912.667683	130.696954	49.443367
909.343581	125.670235	49.448372
905.977818	130.686656	49.453377
902.624714	127.144186	49.458381
898.946753	132.640271	49.463386
895.355798	129.641934	49.468391
891.971567	131.423290	49.473396
888.473013	126.429188	49.478401
885.276860	126.888258	49.483405
881.471655	124.226703	49.488410
877.839453	128.067458	49.493415
874.091031	127.652689	49.498420
870.647379	134.621658	49.503425
867.790928	128.075677	49.508429
863.857380	128.766239	49.513434
860.185806	126.672446	49.518439
856.548374	123.322476	49.523444
853.087919	129.979875	49.528449
849.976145	122.394720	49.533453
846.524156	126.459471	49.538458
843.201305	119.706876	49.543463
839.492565	131.306642	49.548468
835.564659	127.414886	49.553473
832.060925	130.806205	49.558477
828.436417	135.418109	49.563482
825.287599	125.234626	49.568487
821.916301	129.814324	49.573492
818.298893	134.040055	49.578497
814.977464	118.769134	49.583501
811.443896	125.879506	49.588506
807.958394	120.055086	49.593511
804.362563	131.224949	49.598516
800.886532	126.241996	49.603521
797.441442	129.423144	49.608525
793.743898	132.661248	49.613530
790.106672	125.077207	49.618535
786.949647	119.213275	49.623540
783.198097	125.717584	49.628545
779.946954	120.124382	49.633549
776.511491	129.748431	49.638554
772.590526	122.148191	49.643559
769.023568	120.544726	49.648564
765.686330	128.853260	49.653569
762.525678	116.337871	49.658573
758.696608	121.248095	49.663578
755.244383	125.473585	49.668583
752.049327	119.503092	49.673588
748.107752	133.239932	49.678593
744.647042	128.645615	49.683597
741.205427	129.538291	49.688602
737.747310	123.409840	49.693607
734.635931	130.756110	49.698612
730.548968	132.217711	49.703617
726.960646	125.294023	49.708621
723.800600	131.410053	49.713626
720.188138	132.733774	49.718631
716.766248	121.717398	49.723636
712.909620	136.184969	49.728641
709.596775	130.618010	49.733645
706.120787	130.521025	49.738650
702.696293	127.581156	49.743655
699.377901	123.200142	49.748660
695.471124	125.002963	49.753665
692.474323	120.927320	49.758669
688.552427	127.032645	49.763674
685.335665	124.881129	49.768679
681.625712	125.120256	49.773684
678.017175	124.848870	49.778689
674.600078	121.257572	49.783693
671.041593	132.317550	49.788698
667.600274	126.683078	49.793703
664.376912	127.917018	49.798708
660.753231	129.501945	49.803713
657.342395	126.389353	49.808717
653.709220	124.151050	49.813722
650.205678	135.738123	49.818727
646.694243	122.221350	49.823732
642.626704	137.267728	49.828737
639.716848	127.767515	49.833741
636.039317	125.172476	49.838746
632.548396	128.388957	49.843751
629.383946	123.563582	49.848756
625.801286	131.682914	49.853761
622.397124	128.198053	49.858765
618.379870	132.078046	49.863770
614.957227	133.189291	49.868775
611.716713	125.030845	49.873780
608.115507	137.920354	49.878785
604.864473	125.494836	49.883789
600.968076	134.714944	49.888794
597.499255	127.589455	49.893799
594.111049	125.034006	49.898804
590.908825	127.928850	49.903809
587.358668	126.792419	49.908813
583.547094	127.330437	49.913818
580.096138	126.039660	49.918823
576.381976	123.421528	49.923828
572.741297	124.652945	49.928833
569.559330	123.294781	49.933837
565.978415	130.756732	49.938842
562.490335	124.298307	49.943847
559.610966	123.575439	49.948852
555.632659	130.459432	49.953857
551.974285	122.673284	49.958861
548.530913	127.562687	49.963866
544.989324	116.436229	49.968871
541.913878	128.248346	49.973876
537.710509	131.733941	49.978881
534.569213	116.372893	49.983885
531.086750	117.185464	49.988890
527.413346	126.883780	49.993895
523.914488	122.373910	49.998900
520.363056	125.564178	50.003905
517.356054	108.943624	50.008909
513.761824	117.320891	50.013914
510.072655	121.712458	50.018919
506.470711	116.461293	50.023924
502.753244	117.717708	50.028929
499.511419	120.917740	50.033933
495.879999	114.733122	50.038938
492.499385	123.574128	50.043943
489.618866	112.428520	50.048948
485.379588	122.025728	50.053953
481.922345	111.754252	50.058957
478.128199	123.805309	50.063962
474.672752	123.749115	50.068967
471.516497	124.061771	50.073972
467.791004	121.738459	50.078977
464.737921	121.022100	50.083981
461.182917	126.192499	50.088986
457.439804	115.777325	50.093991
453.869110	113.531026	50.098996
450.061120	118.057349	50.104001
447.149372	121.718637	50.109005
443.775279	117.831906	50.114010
439.993542	112.133589	50.119015
436.559284	114.981884	50.124020
432.836051	115.965605	50.129025
429.290216	114.073775	50.134029
425.869321	123.393129	50.139034
422.598074	123.061796	50.144039
419.296603	121.192288	50.149044
415.392399	120.031313	50.154049
411.734155	114.589647	50.159053
408.264258	122.900439	50.164058
405.087788	117.362474	50.169063
401.145010	121.418393	50.174068
397.826799	116.767044	50.179073
394.807937	110.357022	50.184077
390.902495	115.822270	50.189082
387.346265	116.042127	50.194087
383.845976	120.639932	50.199092
380.092748	123.080868	50.204097
376.994344	118.667655	50.209101
373.602011	118.011651	50.214106
369.856880	122.192363	50.219111
366.575869	122.504232	50.224116
362.604925	129.384010	50.229121
359.131998	124.563523	50.234125
356.004710	127.520132	50.239130
352.009569	126.826365	50.244135
348.827143	120.475017	50.249140
344.903641	119.648235	50.254145
341.775497	117.596179	50.259149
338.570113	117.974882	50.264154
334.967620	118.156459	50.269159
331.449947	123.197639	50.274164
327.647050	124.575693	50.279169
324.402558	122.468707	50.284173
321.025280	125.695823	50.289178
317.362650	115.573140	50.294183
313.853954	116.145725	50.299188
310.198249	122.467791	50.304193
306.876309	125.777324	50.309197
303.435178	121.167708	50.314202
299.874776	122.851779	50.319207
296.513338	126.353946	50.324212
292.603183	128.762913	50.329217
289.611772	114.904074	50.334221
285.550197	129.418107	50.339226
281.938399	128.255427	50.344231
278.714120	120.109571	50.349236
275.203762	117.589794	50.354241
272.251974	115.094784	50.359245
268.392386	126.079371	50.364250
264.306898	122.931360	50.369255
261.319039	121.705482	50.374260
257.511602	114.603194	50.379265
254.325800	116.477888	50.384269
250.982492	122.523130	50.389274
247.221378	120.938030	50.394279
243.754701	116.719081	50.399284
239.977345	125.094109	50.404289
236.699790	116.856665	50.409293
233.250284	120.308334	50.414298
229.422265	113.691377	50.419303
226.450807	113.432327	50.424308
223.047801	123.136035	50.429313
219.496405	113.840624	50.434317
216.302548	121.548975	50.439322
212.272760	121.702914	50.444327
208.617474	118.713051	50.449332
204.745206	127.669782	50.454337
201.574104	118.427073	50.459341
198.203884	126.375388	50.464346
194.492737	123.624089	50.469351
191.466486	118.171541	50.474356
187.703548	128.972654	50.479361
184.003976	115.607652	50.484365
180.322047	127.009078	50.489370
176.973814	118.253731	50.494375
174.081848	114.578680	50.499380
169.934515	117.635013	50.504385
166.650780	119.831263	50.509389
163.231103	115.034694	50.514394
159.654584	119.164380	50.519399
156.326578	112.831569	50.524404
152.543956	120.652822	50.529409
149.471423	122.573370	50.534413
145.639620	123.696673	50.539418
142.185423	121.088578	50.544423
138.689094	120.922204	50.549428
134.910516	119.648139	50.554433
131.541957	123.853337	50.559437
128.100489	126.410611	50.564442
124.584304	124.032428	50.569447
121.228928	116.196917	50.574452
117.662734	121.074216	50.579457
114.270708	111.980049	50.584461
110.658932	117.974326	50.589466
107.298870	124.229254	50.594471
103.896661	115.191443	50.599476
99.821014	117.398476	50.604481
96.432331	108.017044	50.609485
92.853108	116.832792	50.614490
89.526661	117.590483	50.619495
86.477415	115.775582	50.624500
82.461392	117.451001	50.629505
79.214231	115.138432	50.634509
75.550919	120.099135	50.639514
71.831152	119.665714	50.644519
68.707222	114.951094	50.649524
65.345367	121.912024	50.654529
61.788808	112.364236	50.659533
57.805447	125.181031	50.664538
54.643257	123.530487	50.669543
51.132866	116.590958	50.674548
47.440896	121.257661	50.679553
43.766987	121.816379	50.684557
40.225660	118.531132	50.689562
36.809866	120.542142	50.694567
33.876754	117.918310	50.699572
29.996145	121.895588	50.704577
26.794730	115.757811	50.709581
23.287087	116.740523	50.714586
19.716458	120.876450	50.719591
16.016947	120.369078	50.724596
12.248443	120.727403	50.729601
8.970948	116.763666	50.734605
5.265664	123.577262	50.739610
2.221805	131.944892	50.744615