Tue Jun 21 10:19:14 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.473935	100.936925	0.000000
-0.344052	103.137045	0.005005
-0.184968	108.360651	0.010010
0.100744	103.583010	0.015014
0.010444	112.369378	0.020019
0.149038	99.128470	0.025024
-0.225856	87.275415	0.030029
-0.474942	73.072381	0.035034
-0.878024	60.188199	0.040038
-1.086832	58.983919	0.045043
-1.357861	42.139263	0.050048
-1.339772	29.943922	0.055053
-2.141626	25.542152	0.060058
-2.313463	12.866583	0.065062
-2.428712	6.902487	0.070067
-3.114893	1.090950	0.075072
-3.077957	-10.500478	0.080077
-3.620704	-4.351029	0.085082
-4.141943	-14.604449	0.090086
-4.685293	-5.133165	0.095091
-4.764252	-4.394869	0.100096
-4.503004	-14.896656	0.105101
-4.704766	-10.747025	0.110106
-5.506237	-11.699239	0.115110
-5.688971	-14.427702	0.120115
-5.858051	-6.280548	0.125120
-6.158925	-11.219924	0.130125
-6.839045	-7.927828	0.135130
-6.430880	-15.924111	0.140134
-6.469762	-9.895001	0.145139
-7.336554	-10.560722	0.150144
-7.707464	-13.843714	0.155149
-8.173137	-2.043521	0.160154
-7.770476	-12.280025	0.165158
-8.017401	-14.679756	0.170163
-8.149700	-10.827171	0.175168
-7.982671	-5.796531	0.180173
-8.968284	-4.581116	0.185178
-9.056468	-15.498052	0.190182
-9.153292	-15.885354	0.195187
-9.458316	-7.479085	0.200192
-9.519178	-6.438508	0.205197
-10.756640	-11.348494	0.210202
-10.856234	-8.819520	0.215206
-10.910358	-8.695100	0.220211
-11.166417	-6.220532	0.225216
-11.049505	-10.495201	0.230221
-10.902749	-7.916247	0.235226
-11.145317	-9.860658	0.240230
-11.784128	-10.809219	0.245235
-12.140394	-7.907995	0.250240
-12.591635	-9.305177	0.255245
-12.724933	-3.613462	0.260250
-12.996952	-9.957114	0.265254
-12.855264	-10.757269	0.270259
-13.146012	-15.479870	0.275264
-13.625122	-14.378915	0.280269
-14.320443	-4.993565	0.285274
-14.173121	-11.607543	0.290278
-14.050827	-7.057703	0.295283
-14.108715	-5.873959	0.300288
-14.987381	-15.245894	0.305293
-15.602907	-4.029073	0.310298
-15.840197	-9.153816	0.315302
-15.849997	-7.132653	0.320307
-15.895435	-6.227634	0.325312
-15.717929	-9.071794	0.330317
-16.122152	-7.675200	0.335322
-16.038172	-13.165325	0.340326
-16.823564	-0.589153	0.345331
-17.339390	-2.161726	0.350336
-17.351380	-10.278470	0.355341
-17.466621	-2.781963	0.360346
-17.632723	-6.500249	0.365350
-18.289987	-11.334628	0.370355
-19.193366	-1.012806	0.375360
-19.042091	-9.457719	0.380365
-18.816720	-11.292347	0.385370
-19.303267	-14.440354	0.390374
-19.168224	-5.982636	0.395379
-19.248231	-0.280604	0.400384
-19.125934	-17.207885	0.405389
-20.253578	-2.883093	0.410394
-20.328436	-4.021537	0.415398
-20.481992	-9.761819	0.420403
-20.862228	-3.999021	0.425408
-21.498891	-7.986694	0.430413
-22.033841	-13.884240	0.435418
-22.015029	-11.637131	0.440422
-21.810616	-11.201703	0.445427
-22.169461	-11.411428	0.450432
-21.886666	-18.232739	0.455437
-22.221421	-10.564513	0.460442
-22.877581	-11.598802	0.465446
-23.526464	-3.948214	0.470451
-23.919811	-10.992834	0.475456
-23.572519	-15.571856	0.480461
-23.952496	-5.226399	0.485466
-24.124250	-8.701027	0.490470
-23.631514	-18.334194	0.495475
-24.772251	-7.036323	0.500480
-25.132546	-15.291931	0.505485
-25.394370	1.716308	0.510490
-25.347091	-10.012005	0.515494
-25.538437	-4.785663	0.520499
-25.729853	-3.940930	0.525504
-25.837369	-18.392477	0.530509
-26.651111	-2.686423	0.535514
-26.832319	-9.615409	0.540518
-27.056308	-10.358759	0.545523
-27.395035	-11.556121	0.550528
-26.996441	-12.172674	0.555533
-27.479744	-14.594630	0.560538
-27.760191	-7.012159	0.565542
-28.483194	-13.270273	0.570547
-28.959001	-5.576911	0.575552
-28.782672	-12.585230	0.580557
-29.002089	-16.085510	0.585562
-28.785499	-14.568731	0.590566
-28.947230	-3.424491	0.595571
-29.469628	-0.110951	0.600576
-29.656458	-16.138502	0.605581
-30.212471	1.424616	0.610586
-30.174532	-6.565814	0.615590
-30.971594	-1.204239	0.620595
-31.884628	-0.024123	0.625600
-31.100117	-5.459562	0.630605
-31.260035	-7.952633	0.635610
-31.601591	-1.327769	0.640614
-31.886270	-8.307700	0.645619
-32.303087	-3.792117	0.650624
-31.812749	-12.229239	0.655629
-32.521237	-8.575267	0.660634
-33.058335	-9.724781	0.665638
-33.495026	-10.976960	0.670643
-33.913884	-5.766224	0.675648
-33.592844	-13.532789	0.680653
-33.975734	-9.311723	0.685658
-34.001311	-12.220525	0.690662
-34.162770	-11.413708	0.695667
-34.875565	-12.111830	0.700672
-35.060344	-16.180644	0.705677
-35.124814	-9.980551	0.710682
-35.276528	-12.883462	0.715686
-35.519304	-18.304872	0.720691
-35.817402	-13.274174	0.725696
-35.962082	-10.014503	0.730701
-36.679036	-9.366903	0.735706
-36.467996	-3.779769	0.740710
-36.447542	-1.940033	0.745715
-37.005380	-9.772996	0.750720
-37.608477	-7.980173	0.755725
-38.037813	-9.464846	0.760730
-38.280636	-19.615569	0.765734
-37.902830	-16.806702	0.770739
-38.244100	-4.667963	0.775744
-38.203140	-18.200835	0.780749
-39.325699	-12.513236	0.785754
-39.316371	-10.477876	0.790758
-39.562306	-15.269858	0.795763
-39.956611	-5.908899	0.800768
-39.451191	-12.240590	0.805773
-39.992070	-11.633395	0.810778
-40.962692	-14.433453	0.815782
-41.004980	-20.694569	0.820787
-41.197384	-12.078045	0.825792
-41.295472	-14.849333	0.830797
-41.523938	-9.260855	0.835802
-41.638048	-19.792633	0.840806
-41.452936	-9.852744	0.845811
-42.046855	-10.247711	0.850816
-42.429620	-16.120923	0.855821
-42.993740	-13.124697	0.860826
-42.949269	-16.438780	0.865830
-42.708334	-15.632690	0.870835
-43.369300	-5.741537	0.875840
-43.883349	-12.768532	0.880845
-44.801633	-12.340968	0.885850
-44.451150	-12.847731	0.890854
-44.476228	-11.863598	0.895859
-44.768557	-7.060196	0.900864
-44.409824	-14.781103	0.905869
-44.817989	-5.227421	0.910874
-45.173420	-14.862017	0.915878
-45.543345	-14.069024	0.920883
-46.218912	-15.197578	0.925888
-46.050981	-18.958941	0.930893
-46.525073	-7.062835	0.935898
-46.556409	-9.251793	0.940902
-46.956518	-11.095915	0.945907
-48.037662	-2.718394	0.950912
-48.193279	-11.705276	0.955917
-47.539537	-10.857236	0.960922
-47.685053	-20.572175	0.965926
-47.832487	-15.047043	0.970931
-48.081444	-7.392630	0.975936
-48.488550	-17.530750	0.980941
-49.042159	-16.974727	0.985946
-49.272651	-8.462204	0.990950
-49.101997	-17.154818	0.995955
-49.558249	-7.448133	1.000960
-49.822428	-17.090931	1.005965
-50.655474	-9.289275	1.010970
-51.039212	-14.299578	1.015974
-51.078790	-18.895639	1.020979
-51.101448	-9.082763	1.025984
-51.068715	-12.235260	1.030989
-51.387009	-15.648715	1.035994
-51.381473	-11.392122	1.040998
-51.673596	-15.053225	1.046003
-52.016562	-10.875080	1.051008
-52.401142	-17.008274	1.056013
-52.726919	-17.248139	1.061018
-52.890205	-23.577818	1.066022
-53.146435	-22.351954	1.071027
-54.179599	-17.737068	1.076032
-54.494219	-21.742739	1.081037
-54.152308	-6.408037	1.086042
-54.231133	-9.202447	1.091046
-54.230706	-14.022991	1.096051
-54.590992	-13.388672	1.101056
-54.483532	-19.404040	1.106061
-55.177505	-10.210920	1.111066
-55.791405	-16.619900	1.116070
-55.994039	-20.509534	1.121075
-56.257564	-17.353715	1.126080
-55.894523	-20.586563	1.131085
-56.052615	-13.157953	1.136090
-56.460795	-10.587349	1.141094
-57.122695	-15.860810	1.146099
-57.831501	-14.932565	1.151104
-57.823280	-25.315677	1.156109
-58.007914	-16.591712	1.161114
-57.838588	-12.231805	1.166118
-57.926095	-10.998954	1.171123
-58.000048	-9.477475	1.176128
-58.504858	-14.900679	1.181133
-59.098525	-17.991276	1.186138
-59.395234	-12.920551	1.191142
-59.441795	-19.587467	1.196147
-59.588931	-15.298685	1.201152
-59.835300	-11.700519	1.206157
-60.596283	-13.865930	1.211162
-60.939952	-20.610727	1.216166
-60.646076	-17.407108	1.221171
-61.050319	-24.469249	1.226176
-60.995670	-33.281369	1.231181
-61.168263	-18.770793	1.236186
-61.696381	-6.962829	1.241190
-61.897202	-15.671872	1.246195
-62.350843	-12.593299	1.251200
-61.975689	-13.536311	1.256205
-62.469387	-18.798355	1.261210
-63.403275	-16.521153	1.266214
-63.846692	-17.395305	1.271219
-64.226621	-12.595157	1.276224
-63.434004	-20.283919	1.281229
-63.801701	-17.201030	1.286234
-64.007120	-17.017811	1.291238
-64.192051	-12.958781	1.296243
-65.024143	-6.497971	1.301248
-65.145894	-12.155109	1.306253
-65.474598	-7.284509	1.311258
-65.781964	-15.360816	1.316262
-65.585610	-18.649928	1.321267
-65.952266	-12.653961	1.326272
-65.445137	-18.486480	1.331277
-66.703469	-18.074033	1.336282
-67.221732	-17.328697	1.341286
-66.981371	-17.145103	1.346291
-67.389596	-15.589778	1.351296
-67.498176	-13.972581	1.356301
-67.358852	-11.738524	1.361306
-67.684926	-7.321638	1.366310
-68.356227	-9.656610	1.371315
-68.692340	-11.329582	1.376320
-68.597982	-9.837556	1.381325
-68.919207	-7.479079	1.386330
-69.171240	-6.489724	1.391334
-69.107518	-25.528833	1.396339
-70.039424	-16.429711	1.401344
-70.276189	-19.992234	1.406349
-71.040950	-9.637720	1.411354
-70.665094	-22.722446	1.416358
-70.871614	-9.326906	1.421363
-71.230315	-7.838587	1.426368
-71.220795	-28.518827	1.431373
-70.937963	-7.166698	1.436378
-71.230330	-11.528297	1.441382
-71.628130	-12.940438	1.446387
-72.199484	-14.854273	1.451392
-72.390000	-20.259863	1.456397
-73.374021	-19.137840	1.461402
-73.595005	-16.494438	1.466406
-73.758429	-11.373364	1.471411
-73.968272	-10.075063	1.476416
-73.448893	-12.720883	1.481421
-73.864809	-9.259807	1.486426
-73.843470	-18.858124	1.491430
-73.952931	-19.743377	1.496435
-75.008593	-4.716545	1.501440
-75.152181	-18.917414	1.506445
-75.444540	-13.350521	1.511450
-75.825205	-3.392318	1.516454
-75.587723	-9.435338	1.521459
-75.566897	-3.682915	1.526464
-76.051549	-16.186662	1.531469
-76.649884	-5.546142	1.536474
-76.808367	-13.192840	1.541478
-76.618433	-21.506801	1.546483
-77.270676	-13.107760	1.551488
-77.501061	-21.676530	1.556493
-78.247452	-12.521103	1.561498
-78.718389	-9.757767	1.566502
-78.808171	-14.030567	1.571507
-78.753055	-8.502274	1.576512
-78.727989	-14.460189	1.581517
-78.709741	-16.654200	1.586522
-78.847266	-14.572025	1.591526
-78.973970	-17.193531	1.596531
-80.176402	-11.002912	1.601536
-80.202005	-11.937967	1.606541
-80.181786	-12.313670	1.611546
-80.374808	-14.707323	1.616550
-80.267226	-18.208472	1.621555
-81.488084	-12.431768	1.626560
-81.789501	-11.861660	1.631565
-81.630998	-21.409677	1.636570
-82.180382	-5.792792	1.641574
-81.928375	-19.603724	1.646579
-82.085874	-13.198393	1.651584
-81.820633	-16.150421	1.656589
-82.398192	-19.021482	1.661594
-83.057199	-6.426183	1.666598
-83.081829	-22.928330	1.671603
-83.573780	-18.413526	1.676608
-83.593952	-17.327395	1.681613
-84.673931	-18.857243	1.686618
-85.139914	-11.561954	1.691622
-84.321089	-13.942815	1.696627
-84.875883	-8.213269	1.701632
-84.941600	-16.432008	1.706637
-84.892990	-15.943746	1.711642
-85.388691	-16.630057	1.716646
-85.556297	-18.288703	1.721651
-86.460565	-21.624646	1.726656
-86.375096	-20.131939	1.731661
-86.739911	-11.893570	1.736666
-87.128547	-17.527422	1.741670
-86.801910	-21.591139	1.746675
-87.042089	-17.864350	1.751680
-87.165835	-16.630430	1.756685
-88.130962	-14.702067	1.761690
-88.309594	-20.950268	1.766694
-88.189382	-15.888009	1.771699
-88.272437	-12.248216	1.776704
-88.504605	-22.417861	1.781709
-89.554183	-15.994837	1.786714
-89.969855	-18.608150	1.791718
-89.792190	-14.441832	1.796723
-90.119136	-12.482997	1.801728
-89.952961	-9.003077	1.806733
-89.856567	-12.375290	1.811738
-90.062037	-9.984874	1.816742
-90.568931	-20.593874	1.821747
-91.351296	-13.376825	1.826752
-91.360087	-12.557993	1.831757
-91.515416	-12.471868	1.836762
-91.602779	-15.913894	1.841766
-91.899254	-19.762922	1.846771
-93.037098	-6.563413	1.851776
-93.139403	-23.558067	1.856781
-92.672633	-13.681212	1.861786
-93.134790	-13.430608	1.866790
-93.257742	-14.995615	1.871795
-93.367611	-19.887873	1.876800
-93.300232	-18.537013	1.881805
-93.973227	-22.317962	1.886810
-94.318631	-8.554877	1.891814
-94.494507	-14.964758	1.896819
-95.027997	-7.195735	1.901824
-94.572673	-22.581518	1.906829
-95.555849	-8.776550	1.911834
-96.152674	-16.816951	1.916838
-96.374670	-25.887348	1.921843
-96.478281	-9.031822	1.926848
-95.682794	-16.488210	1.931853
-96.227324	-9.280947	1.936858
-96.729395	-7.632129	1.941862
-96.526069	-11.609319	1.946867
-97.482167	-7.428494	1.951872
-98.015732	-10.901211	1.956877
-98.085047	-6.774303	1.961882
-98.301096	-8.038744	1.966886
-98.444546	-10.566900	1.971891
-98.136274	-7.974444	1.976896
-98.631055	-12.719091	1.981901
-99.288880	-8.387171	1.986906
-99.803355	-9.229818	1.991910
-99.854669	-24.209051	1.996915
-99.996940	-17.306462	2.006912
-99.129544	-14.527768	2.016909
-98.838084	-14.414378	2.026906
-98.685089	-15.674801	2.036902
-98.594598	-15.871337	2.046899
-97.751436	-11.477701	2.056896
-97.020073	-13.420149	2.066893
-96.032077	-16.486098	2.076890
-95.715104	-19.264867	2.086886
-96.079203	-14.232057	2.096883
-95.238232	-15.318533	2.106880
-94.481244	-13.901106	2.116877
-94.125947	-16.536648	2.126874
-93.392740	-10.988280	2.136870
-92.782404	-17.294748	2.146867
-92.741587	-15.662687	2.156864
-92.229570	-11.698099	2.166861
-91.262195	-12.341573	2.176858
-90.943500	-17.234809	2.186854
-90.882585	-18.472671	2.196851
-89.832298	-15.166080	2.206848
-89.479954	-18.123200	2.216845
-89.277413	-14.265429	2.226842
-88.383515	-19.328218	2.236838
-88.236773	-18.636431	2.246835
-87.648879	-14.003524	2.256832
-87.140800	-15.595026	2.266829
-86.664187	-22.264839	2.276826
-85.670738	-22.598861	2.286822
-85.414449	-19.032344	2.296819
-85.323435	-15.359815	2.306816
-84.290963	-17.240096	2.316813
-83.802254	-16.408541	2.326810
-83.290607	-13.126949	2.336806
-83.372475	-13.379705	2.346803
-82.617309	-14.894959	2.356800
-82.238979	-14.227298	2.366797
-81.418630	-13.792293	2.376794
-80.835828	-15.040514	2.386790
-80.700718	-13.552697	2.396787
-79.470886	-15.994010	2.406784
-79.501471	-12.327621	2.416781
-78.997264	-8.819547	2.426778
-78.872076	-15.707389	2.436774
-77.916719	-15.026024	2.446771
-77.543416	-9.933553	2.456768
-77.028196	-15.404874	2.466765
-75.951745	-18.417498	2.476762
-75.643646	-14.268378	2.486758
-75.642412	-15.838577	2.496755
-75.552103	-11.891482	2.506752
-74.569778	-13.395747	2.516749
-74.016919	-11.415767	2.526746
-73.163577	-18.253678	2.536742
-72.734503	-14.577858	2.546739
-72.747288	-12.545697	2.556736
-72.264372	-12.348028	2.566733
-71.194723	-14.953483	2.576730
-71.137542	-19.824749	2.586726
-70.922115	-17.496065	2.596723
-69.932479	-14.001398	2.606720
-69.246465	-10.239695	2.616717
-68.824995	-15.074671	2.626714
-68.308461	-21.534143	2.636710
-68.293037	-14.614199	2.646707
-67.375349	-10.975232	2.656704
-66.699574	-13.655745	2.666701
-66.500501	-12.522125	2.676698
-66.091822	-10.474007	2.686694
-64.970116	-13.632632	2.696691
-64.791919	-6.524467	2.706688
-64.765394	-7.122379	2.716685
-64.464676	-12.608563	2.726682
-63.586239	-15.061230	2.736678
-62.646243	-11.985128	2.746675
-61.931938	-19.612886	2.756672
-62.098217	-17.078924	2.766669
-61.848329	-15.627897	2.776666
-61.169909	-13.463811	2.786662
-60.486378	-15.671003	2.796659
-59.767423	-6.754169	2.806656
-59.147238	-6.154419	2.816653
-58.873262	-2.381579	2.826650
-58.602987	-7.595585	2.836646
-58.175601	-8.684298	2.846643
-57.516771	-5.683148	2.856640
-57.122274	-11.464646	2.866637
-56.215731	-8.330246	2.876634
-55.727473	-11.185591	2.886630
-55.586093	-10.026609	2.896627
-54.722305	-8.015327	2.906624
-53.961423	-4.691028	2.916621
-53.863358	-5.100632	2.926618
-53.941550	-6.934499	2.936614
-53.161848	-9.666404	2.946611
-52.405464	-3.042639	2.956608
-51.841124	-1.670162	2.966605
-51.122975	-3.827169	2.976602
-50.473253	-5.431258	2.986598
-50.333838	-10.268528	2.996595
-50.347784	-5.839637	3.006592
-49.742808	-3.635328	3.016589
-48.997113	-8.381537	3.026586
-48.017464	-11.535404	3.036582
-47.755665	-10.137721	3.046579
-47.824441	-9.081655	3.056576
-47.047907	-7.291447	3.066573
-46.055768	-4.492100	3.076570
-45.732641	-12.447885	3.086566
-45.482940	-16.129352	3.096563
-45.086568	-10.115989	3.106560
-44.414373	-8.203385	3.116557
-44.087022	-16.297585	3.126554
-42.915300	-13.060685	3.136550
-42.590411	-12.609420	3.146547
-42.637269	-13.168901	3.156544
-42.208664	-12.034167	3.166541
-41.269709	-8.488024	3.176538
-41.074411	-7.363261	3.186534
-40.329911	-13.611131	3.196531
-39.374926	-12.683896	3.206528
-39.131690	-10.246793	3.216525
-39.269916	-14.000752	3.226522
-38.919038	-10.410967	3.236518
-38.079523	-11.435543	3.246515
-37.470572	-10.056225	3.256512
-36.833073	-10.385628	3.266509
-36.510297	-5.753064	3.276506
-35.841124	-4.504247	3.286502
-34.993546	-11.628296	3.296499
-34.851160	-9.561764	3.306496
-34.742855	-8.145972	3.316493
-33.782834	-6.302566	3.326490
-33.241965	-11.139531	3.336486
-33.103160	-17.920957	3.346483
-32.084666	-14.511081	3.356480
-31.711211	-17.516349	3.366477
-31.577312	-18.305326	3.376474
-31.224011	-12.909007	3.386470
-30.391873	-26.119934	3.396467
-29.770358	-12.778593	3.406464
-28.824681	-10.011066	3.416461
-28.880621	-16.545268	3.426458
-28.582522	-10.270620	3.436454
-27.889195	-10.603932	3.446451
-26.926888	-15.212919	3.456448
-26.708005	-13.706174	3.466445
-26.676084	-14.290357	3.476442
-26.265367	-18.235198	3.486438
-25.494907	-14.473837	3.496435
-24.670436	-14.422230	3.506432
-23.809761	-14.840158	3.516429
-23.893746	-7.276207	3.526426
-23.668438	-4.109407	3.536422
-22.932321	-11.338292	3.546419
-22.239838	-10.998480	3.556416
-22.196319	-12.472345	3.566413
-20.909006	-9.297059	3.576410
-20.458839	-11.555109	3.586406
-20.095009	-12.292457	3.596403
-20.339075	-13.393470	3.606400
-19.604842	-12.772291	3.616397
-18.704423	-12.732864	3.626394
-18.419739	-10.328705	3.636390
-17.504590	-14.791966	3.646387
-17.190236	-16.914308	3.656384
-16.984445	-9.347958	3.666381
-16.691506	-13.831875	3.676378
-15.818977	-11.296648	3.686374
-15.513376	-15.070952	3.696371
-14.297479	-13.983006	3.706368
-13.997522	-11.768886	3.716365
-14.080732	-14.209504	3.726362
-13.895759	-15.521257	3.736358
-12.888301	-26.019889	3.746355
-12.289824	-15.535199	3.756352
-11.416169	-15.473161	3.766349
-11.127636	-20.967795	3.776346
-10.856319	-17.061538	3.786342
-10.751749	-18.788149	3.796339
-9.728034	-16.993025	3.806336
-9.541945	-18.545426	3.816333
-8.900140	-18.505259	3.826330
-8.182864	-16.341473	3.836326
-7.754665	-15.425793	3.846323
-7.458088	-15.452543	3.856320
-6.688641	-19.172654	3.866317
-6.737387	-9.024169	3.876314
-5.611985	-12.066421	3.886310
-5.063739	-18.163037	3.896307
-4.888121	-14.430813	3.906304
-4.572388	-13.474972	3.916301
-3.735791	-0.521131	3.926298
-3.552183	1.856300	3.936294
-3.107072	9.733156	3.946291
-2.830220	23.241469	3.956288
-2.504764	39.793096	3.966285
-1.758418	62.604590	3.976282
-1.440457	79.767259	3.986278
-1.028983	97.547339	3.996275
-0.344080	131.162004	4.006272
0.000000	143.987852	4.011277
0.340549	144.730099	4.016282
0.568437	151.776966	4.021286
0.331295	158.892553	4.026291
0.708453	172.103395	4.031296
0.515519	175.846875	4.036301
0.729029	174.556275	4.041306
0.669993	176.349994	4.046310
0.920994	178.341612	4.051315
0.990620	180.030553	4.056320
1.023433	185.743771	4.061325
1.082222	176.292258	4.066330
1.188301	186.041320	4.071334
0.813297	191.014763	4.076339
1.092643	190.918202	4.081344
1.086941	189.773225	4.086349
1.029776	186.007646	4.091354
0.976805	188.226019	4.096358
0.686258	184.124737	4.101363
1.097371	176.654363	4.106368
1.050827	183.714719	4.111373
1.145898	182.582459	4.116378
1.387650	182.726165	4.121382
1.178218	181.342007	4.126387
1.307989	183.392772	4.131392
1.190344	188.426214	4.136397
0.998321	189.665337	4.141402
1.204617	182.322414	4.146406
0.956542	190.138004	4.151411
1.199084	183.155336	4.156416
1.077150	190.039327	4.161421
1.359005	190.308411	4.166426
1.110385	197.185756	4.171430
1.288210	212.792756	4.176435
1.648421	204.416928	4.181440
1.104184	216.326991	4.186445
1.360469	207.107978	4.191450
1.272098	198.870963	4.196454
1.184622	198.570316	4.201459
1.275279	207.970290	4.206464
1.252526	214.556071	4.211469
1.241668	218.179031	4.216474
1.366175	222.919202	4.221478
1.203500	223.114287	4.226483
1.589103	215.361190	4.231488
1.477324	223.522854	4.236493
1.571361	217.067382	4.241498
1.628765	226.700010	4.246502
1.607315	226.663716	4.251507
1.422951	226.713797	4.256512
1.457032	225.378509	4.261517
1.741566	217.262074	4.266522
1.694848	215.773021	4.271526
1.327455	210.015375	4.276531
1.606769	209.006330	4.281536
1.561178	220.550647	4.286541
1.507495	219.841835	4.291546
1.570992	222.325291	4.296550
1.683785	231.515791	4.301555
1.817706	222.152057	4.306560
1.453345	216.606045	4.311565
1.638843	218.022224	4.316570
1.744369	223.963181	4.321574
1.245003	226.048865	4.326579
1.718904	224.712578	4.331584
1.584240	231.176392	4.336589
1.849754	226.241623	4.341594
1.728407	228.070334	4.346598
1.621262	232.094049	4.351603
1.624082	219.959893	4.356608
1.591696	231.686739	4.361613
1.591980	225.317830	4.366618
1.563535	220.338201	4.371622
1.483117	235.139631	4.376627
1.669446	227.606799	4.381632
1.420656	231.537935	4.386637
1.572492	226.916220	4.391642
1.765205	224.291899	4.396646
1.714388	224.687507	4.401651
1.693409	224.898597	4.406656
1.480126	235.116955	4.411661
1.875550	245.813909	4.416666
2.307492	255.979510	4.421670
1.944391	244.836573	4.426675
2.059317	224.838286	4.431680
1.895090	236.677940	4.436685
1.815320	229.187789	4.441690
2.266468	239.415517	4.446694
1.654736	233.414156	4.451699
2.101901	234.775365	4.456704
1.756937	245.663988	4.461709
1.987788	256.076801	4.466714
2.392339	252.143777	4.471718
2.196686	251.352108	4.476723
2.104339	235.197149	4.481728
1.882051	227.974903	4.486733
1.875966	225.647341	4.491738
2.132276	238.665522	4.496742
1.834360	247.969231	4.501747
2.117478	238.634852	4.506752
2.314674	263.827545	4.511757
2.244574	258.670093	4.516762
1.987663	251.670443	4.521766
1.830628	261.745907	4.526771
2.393979	259.635250	4.531776
2.170245	266.940281	4.536781
2.138375	260.580431	4.541786
2.592647	264.954609	4.546790
2.343156	263.376778	4.551795
2.119551	231.870326	4.556800
2.323259	243.352066	4.561805
2.032003	243.364790	4.566810
2.622297	248.822915	4.571814
2.033387	242.209970	4.576819
2.111462	245.359004	4.581824
2.056666	254.507806	4.586829
2.209508	258.135636	4.591834
2.258713	258.721296	4.596838
2.120767	268.074305	4.601843
2.471860	253.968074	4.606848
2.502268	263.645846	4.611853
2.262436	266.019101	4.616858
2.457946	253.390253	4.621862
2.200489	269.329677	4.626867
2.285844	267.215485	4.631872
2.230540	272.648108	4.636877
2.086778	269.341254	4.641882
2.281316	263.471594	4.646886
2.345303	266.335049	4.651891
2.683538	256.971799	4.656896
2.346022	265.867271	4.661901
2.435939	264.693628	4.666906
2.659745	248.768694	4.671910
2.433824	257.784412	4.676915
2.724340	260.795458	4.681920
2.726990	262.699942	4.686925
2.410232	254.244175	4.691930
2.582596	257.135070	4.696934
2.191567	267.798280	4.701939
2.676016	264.424304	4.706944
2.369032	266.476558	4.711949
2.436109	264.979510	4.716954
3.074783	272.924579	4.721958
2.614848	272.943725	4.726963
2.992339	266.590878	4.731968
2.488387	272.575153	4.736973
2.521010	264.156052	4.741978
2.861712	265.956210	4.746982
2.363080	271.089471	4.751987
2.817613	262.251219	4.756992
2.628098	282.922036	4.761997
2.988831	283.694890	4.767002
3.182846	278.457978	4.772006
2.829044	273.412423	4.777011
2.610245	261.383014	4.782016
2.739560	268.133081	4.787021
2.898832	261.539702	4.792026
2.907674	263.835863	4.797030
2.447897	263.134896	4.802035
2.717094	274.732703	4.807040
2.972660	279.425733	4.812045
2.913590	278.065213	4.817050
3.212616	280.201434	4.822054
2.901649	271.783772	4.827059
3.080523	262.249371	4.832064
2.674683	266.509239	4.837069
3.174461	275.482352	4.842074
2.705369	264.860757	4.847078
2.620476	282.435971	4.852083
3.102025	287.464157	4.857088
2.823576	290.343669	4.862093
3.086031	291.488204	4.867098
3.122155	300.037263	4.872102
2.886893	302.535471	4.877107
3.276334	293.619572	4.882112
2.961229	299.963711	4.887117
2.983686	297.812964	4.892122
3.359477	291.154711	4.897126
3.178665	299.278511	4.902131
3.302109	295.696914	4.907136
3.135779	290.211622	4.912141
3.039848	281.408860	4.917146
3.017565	283.275441	4.922150
3.079033	283.065967	4.927155
3.257073	285.531650	4.932160
3.292202	295.746803	4.937165
2.810336	292.300368	4.942170
3.355180	293.079835	4.947174
2.945662	293.137599	4.952179
2.926521	287.680032	4.957184
3.081667	291.984953	4.962189
2.911084	290.059564	4.967194
3.125098	286.408901	4.972198
2.828922	298.682099	4.977203
3.114517	291.204828	4.982208
2.839976	296.974506	4.987213
3.134610	307.688785	4.992218
3.498921	311.373177	4.997222
3.317517	309.017406	5.002227
3.526421	318.396880	5.007232
3.533308	320.450647	5.012237
3.429791	313.368340	5.017242
3.398121	308.948278	5.022246
3.459625	324.386390	5.027251
3.372945	310.059747	5.032256
3.333444	311.255074	5.037261
3.504947	315.293845	5.042266
3.637158	312.368522	5.047270
3.304331	314.477159	5.052275
3.553373	312.232649	5.057280
3.549083	328.656712	5.062285
3.667740	317.907562	5.067290
3.590702	292.497579	5.072294
3.109690	303.618738	5.077299
3.553763	309.188912	5.082304
3.503284	315.801824	5.087309
3.415377	314.550270	5.092314
3.575179	316.449064	5.097318
3.482102	331.843910	5.102323
3.276097	320.454872	5.107328
3.245336	321.066996	5.112333
3.494800	325.552463	5.117338
3.723551	319.923001	5.122342
3.683280	324.208390	5.127347
3.407331	320.254039	5.132352
3.339659	318.626164	5.137357
3.425252	317.756346	5.142362
3.437722	310.709695	5.147366
3.414287	338.035767	5.152371
4.063839	335.434450	5.157376
4.213220	344.950687	5.162381
4.089569	332.802455	5.167386
3.986820	325.036828	5.172390
3.784071	322.815227	5.177395
3.855759	317.215721	5.182400
3.649948	324.279820	5.187405
3.710535	319.317188	5.192410
3.787073	325.758304	5.197414
3.560964	328.005367	5.202419
3.491298	322.190091	5.207424
3.586033	336.149577	5.212429
3.839765	348.270779	5.217434
4.195604	338.034693	5.222438
3.843014	342.686362	5.227443
4.194706	346.426725	5.232448
4.013523	345.176604	5.237453
3.909840	333.860007	5.242458
4.076360	325.098618	5.247462
3.759542	333.554385	5.252467
4.044523	329.893341	5.257472
4.010870	347.064478	5.262477
4.030118	358.269591	5.267482
4.163583	340.627277	5.272486
3.571071	338.662423	5.277491
3.953762	339.657597	5.282496
4.067405	340.832106	5.287501
4.149480	342.087225	5.292506
3.962676	348.233915	5.297510
3.906135	345.764121	5.302515
4.177059	340.810659	5.307520
3.877889	350.566149	5.312525
3.881440	351.746654	5.317530
4.280328	349.671704	5.322534
4.023106	356.278413	5.327539
4.364192	350.770252	5.332544
4.265171	344.887010	5.337549
4.012370	346.237444	5.342554
4.192919	354.835633	5.347558
3.925712	354.459366	5.352563
4.412471	343.427633	5.357568
4.146941	351.724742	5.362573
3.964625	348.828011	5.367578
4.099369	348.796243	5.372582
3.951398	351.544045	5.377587
4.022067	344.925637	5.382592
4.145536	359.413597	5.387597
4.326177	368.513811	5.392602
4.497642	376.456770	5.397606
4.658900	381.277339	5.402611
4.475829	356.609834	5.407616
3.867146	353.187345	5.412621
4.308972	371.139385	5.417626
4.685890	366.141131	5.422630
4.137641	381.551209	5.427635
4.407112	377.837664	5.432640
4.607349	379.680040	5.437645
4.309889	375.308509	5.442650
4.622327	371.387749	5.447654
4.477148	374.070759	5.452659
4.784995	377.107376	5.457664
4.334339	362.900156	5.462669
4.407522	371.539814	5.467674
4.678717	374.027580	5.472678
4.404495	364.249244	5.477683
4.970556	367.820320	5.482688
4.698777	356.101341	5.487693
4.270945	351.376263	5.492698
4.706998	347.150674	5.497702
4.117823	359.675697	5.502707
4.883643	357.651879	5.507712
4.806669	377.487991	5.512717
4.509916	364.193043	5.517722
4.663762	352.684798	5.522726
4.395496	376.342881	5.527731
4.579790	375.903493	5.532736
4.794011	376.908806	5.537741
4.718052	375.820048	5.542746
5.041380	374.307988	5.547750
4.829331	385.054321	5.552755
4.722599	375.630885	5.557760
4.547271	373.041237	5.562765
4.672023	381.098497	5.567770
4.861604	376.334126	5.572774
4.598570	380.369485	5.577779
4.952434	381.621636	5.582784
4.988289	383.686993	5.587789
4.993412	384.727721	5.592794
5.172348	374.943409	5.597798
4.738295	365.060110	5.602803
4.626689	356.933223	5.607808
4.762307	371.280256	5.612813
4.775495	378.208065	5.617818
5.277374	378.399081	5.622822
4.743284	376.519665	5.627827
5.062302	371.604013	5.632832
4.903276	368.828929	5.637837
5.104443	376.153639	5.642842
5.142020	356.863217	5.647846
4.994149	361.862449	5.652851
4.732813	339.769398	5.657856
4.847976	362.035283	5.662861
4.460636	369.184914	5.667866
4.701573	377.299897	5.672870
4.723698	384.625249	5.677875
5.364568	369.708605	5.682880
5.120100	378.939999	5.687885
4.802401	387.606897	5.692890
5.242051	377.773689	5.697894
4.921436	380.441941	5.702899
5.210284	375.251259	5.707904
5.068723	381.264962	5.712909
4.921737	378.034199	5.717914
5.058945	377.153660	5.722918
4.907010	388.150530	5.727923
5.287804	377.922521	5.732928
5.362087	378.327413	5.737933
5.351098	381.026686	5.742938
5.336662	375.009838	5.747942
4.955485	381.791797	5.752947
5.312145	376.564428	5.757952
5.173255	376.608558	5.762957
4.828642	381.668792	5.767962
4.884849	381.100635	5.772966
4.852503	382.510277	5.777971
5.534025	393.647389	5.782976
5.643807	398.590747	5.787981
5.474852	389.387378	5.792986
5.218012	382.113157	5.797990
5.240523	377.798560	5.802995
5.108725	382.960903	5.808000
5.505292	401.071043	5.813005
5.560642	398.275256	5.818010
5.683725	392.680631	5.823014
5.307407	385.850277	5.828019
5.587877	378.933073	5.833024
5.205975	374.314839	5.838029
4.952419	379.209818	5.843034
5.757197	388.986186	5.848038
5.366506	404.093526	5.853043
5.755172	395.239070	5.858048
5.464620	406.996563	5.863053
5.353490	392.379067	5.868058
5.830463	395.218759	5.873062
5.452849	411.502652	5.878067
5.803816	397.597598	5.883072
5.434059	381.147024	5.888077
5.471350	387.606900	5.893082
5.528558	387.925028	5.898086
5.449955	401.256924	5.903091
6.274671	400.536645	5.908096
5.491455	399.247084	5.913101
5.503165	385.501229	5.918106
5.832042	383.434711	5.923110
5.647052	388.592445	5.928115
5.467228	385.121035	5.933120
5.452510	398.118516	5.938125
5.784783	403.404715	5.943130
5.938753	399.881187	5.948134
6.036242	409.350406	5.953139
5.759297	390.075121	5.958144
5.649067	389.315082	5.963149
5.428080	382.999126	5.968154
5.853907	391.066727	5.973158
5.762988	390.211924	5.978163
5.790516	400.728362	5.983168
5.919117	397.347963	5.988173
5.544320	402.312558	5.993178
5.925532	397.703329	5.998182
5.607264	408.190597	6.003187
5.803961	396.331062	6.008192
6.082233	397.874771	6.013197
5.864029	397.754231	6.018202
5.905904	399.191842	6.023206
5.885642	400.719073	6.028211
5.853582	404.100096	6.033216
5.685520	406.041548	6.038221
5.686121	402.878499	6.043226
6.072554	394.524473	6.048230
5.996713	403.509898	6.053235
6.052179	393.650112	6.058240
6.176613	398.025270	6.063245
5.980980	394.311577	6.068250
5.901604	387.182219	6.073254
5.811691	383.519697	6.078259
5.822462	393.629425	6.083264
6.016997	386.968584	6.088269
5.812246	396.269189	6.093274
5.860133	391.162408	6.098278
5.638087	400.549158	6.103283
5.976146	401.235589	6.108288
6.100750	405.353981	6.113293
5.693408	393.611442	6.118298
5.876670	398.584863	6.123302
5.700166	402.421189	6.128307
6.098445	399.032248	6.133312
5.997710	401.832819	6.138317
5.470258	388.930079	6.143322
5.805812	387.803766	6.148326
5.694212	400.016091	6.153331
5.851443	396.359609	6.158336
5.895021	395.858270	6.163341
6.118943	404.118169	6.168346
5.950233	399.190126	6.173350
5.763396	402.979617	6.178355
5.696330	398.831997	6.183360
5.884085	400.680783	6.188365
5.464558	400.993983	6.193370
5.870856	403.720859	6.198374
5.814883	406.799373	6.203379
5.813284	399.117800	6.208384
5.768600	399.832877	6.213389
5.603192	395.030191	6.218394
6.282890	400.442978	6.223398
5.749821	407.907439	6.228403
6.126145	397.725349	6.233408
6.085192	400.799204	6.238413
5.890603	397.266298	6.243418
6.370030	396.231013	6.248422
5.721546	402.949102	6.253427
5.992283	398.923743	6.258432
6.017706	404.137416	6.263437
5.761018	407.367965	6.268442
6.097528	394.698683	6.273446
5.879127	389.429777	6.278451
5.629389	382.449403	6.283456
5.752530	388.942425	6.288461
5.844045	399.130352	6.293466
6.238259	394.531404	6.298470
5.464860	399.839264	6.303475
5.802925	395.709218	6.308480
6.203110	398.405530	6.313485
5.923565	407.265040	6.318490
5.937369	390.986172	6.323494
5.764114	393.905906	6.328499
5.980897	394.716219	6.333504
5.869085	391.387077	6.338509
5.563833	391.447112	6.343514
6.023329	393.046851	6.348518
5.829494	400.709902	6.353523
6.052507	405.381523	6.358528
5.841041	391.527178	6.363533
5.852338	396.833372	6.368538
5.996601	392.155437	6.373542
5.641027	391.869382	6.378547
5.769781	396.428337	6.383552
5.932745	392.256047	6.388557
5.677971	400.597183	6.393562
6.179455	397.385730	6.398566
5.932984	410.772072	6.403571
5.857590	398.090281	6.408576
5.863740	396.293684	6.413581
5.762398	401.456317	6.418586
6.308517	395.031094	6.423590
5.596582	387.647519	6.428595
5.781351	384.728280	6.433600
6.023088	385.864412	6.438605
5.834139	386.766380	6.443610
5.939307	380.113235	6.448614
5.657321	386.101253	6.453619
5.904760	390.295011	6.458624
6.056197	397.821359	6.463629
5.661315	394.120334	6.468634
5.994777	397.125875	6.473638
5.690589	386.920312	6.478643
5.677621	398.387330	6.483648
5.681498	397.310807	6.488653
5.807180	403.960103	6.493658
6.120823	403.985541	6.498662
5.889554	410.201583	6.503667
5.857843	406.484425	6.508672
5.749055	403.539987	6.513677
5.585105	405.019771	6.518682
6.053043	400.239493	6.523686
5.548207	409.470999	6.528691
5.437930	395.964776	6.533696
5.680386	394.890979	6.538701
5.833373	396.862347	6.543706
5.800181	395.869320	6.548710
5.842577	400.043358	6.553715
5.855731	405.260049	6.558720
5.998358	404.501949	6.563725
5.732254	399.405520	6.568730
6.104228	394.693034	6.573734
5.980435	401.825286	6.578739
5.994845	394.242103	6.583744
5.809239	401.934971	6.588749
5.506529	398.784851	6.593754
5.895862	399.817016	6.598758
5.900071	405.928350	6.603763
5.750355	393.852666	6.608768
5.831047	394.161380	6.613773
5.604990	399.049838	6.618778
5.856657	391.871187	6.623782
5.782413	405.168422	6.628787
5.707110	406.448817	6.633792
5.894311	403.530553	6.638797
5.809906	405.783171	6.643802
6.145492	388.907153	6.648806
5.774948	404.892280	6.653811
5.671220	397.006401	6.658816
6.085290	400.136338	6.663821
5.783995	398.525827	6.668826
6.009165	399.608660	6.673830
5.689519	397.761814	6.678835
5.788297	409.924116	6.683840
5.859564	407.367828	6.688845
5.718010	400.391437	6.693850
6.151453	393.235572	6.698854
5.497112	402.422366	6.703859
5.903377	411.608779	6.708864
6.323005	419.617429	6.713869
5.892107	414.403041	6.718874
6.253803	401.870483	6.723878
5.807158	405.454743	6.728883
5.954977	400.996052	6.733888
6.088459	401.757011	6.738893
5.701683	398.432746	6.743898
5.956539	399.881267	6.748902
5.511450	405.115426	6.753907
6.011771	403.183716	6.758912
5.895768	409.889414	6.763917
5.608371	407.892577	6.768922
5.849129	406.507657	6.773926
5.522918	396.822765	6.778931
6.022414	397.904179	6.783936
5.931507	398.953309	6.788941
5.924628	400.874583	6.793946
5.990643	400.987992	6.798950
5.723044	402.643206	6.803955
5.688065	392.338595	6.808960
5.770112	401.650521	6.813965
5.546720	409.711572	6.818970
5.822260	419.719061	6.823974
5.797883	440.140340	6.828979
6.099185	431.785196	6.833984
6.046746	437.841589	6.838989
5.869430	420.796687	6.843994
6.032522	402.010152	6.848998
5.853536	410.408603	6.854003
5.831347	400.114499	6.859008
6.031740	400.442268	6.864013
6.155480	402.503139	6.869018
5.816998	403.879803	6.874022
5.695842	400.287179	6.879027
6.101874	401.334537	6.884032
5.908608	405.412224	6.889037
5.687967	402.094193	6.894042
5.943491	394.680067	6.899046
5.796907	410.546613	6.904051
5.855613	405.070786	6.909056
5.813673	400.987679	6.914061
5.810302	402.559474	6.919066
6.022876	392.282546	6.924070
5.680467	401.692384	6.929075
6.030923	407.150220	6.934080
5.792956	408.453012	6.939085
5.886044	404.240192	6.944090
5.800439	395.332841	6.949094
5.700606	405.900170	6.954099
5.872914	405.037103	6.959104
6.421828	404.951160	6.964109
5.924429	411.567074	6.969114
6.368451	402.805275	6.974118
5.898747	408.157376	6.979123
5.913353	402.842975	6.984128
5.970008	396.467226	6.989133
5.851458	408.634531	6.994138
5.794756	392.468769	6.999142
5.855836	411.595913	7.004147
5.899411	398.600781	7.009152
6.241205	395.550948	7.014157
5.898144	407.550590	7.019162
5.936078	408.070039	7.024166
5.898498	410.199854	7.029171
6.074242	403.970543	7.034176
5.905165	399.277789	7.039181
5.663773	400.962211	7.044186
5.854980	402.549346	7.049190
6.007036	399.523432	7.054195
6.063087	400.311815	7.059200
5.956852	407.761248	7.064205
5.948028	398.528397	7.069210
6.165547	397.262968	7.074214
6.366064	404.613453	7.079219
5.832984	387.577373	7.084224
5.592034	390.996338	7.089229
5.444466	389.927725	7.094234
5.701855	393.627868	7.099238
5.796979	403.155295	7.104243
6.042502	399.196471	7.109248
5.908016	411.634207	7.114253
5.809376	410.619258	7.119258
6.567929	406.958714	7.124262
5.462079	398.423760	7.129267
5.810221	391.844242	7.134272
5.786970	406.233796	7.139277
5.761530	407.754386	7.144282
5.926327	404.170652	7.149286
5.811780	411.555748	7.154291
5.685249	406.012121	7.159296
6.111902	404.017621	7.164301
5.640112	409.647133	7.169306
6.091264	402.419065	7.174310
5.848275	406.363887	7.179315
6.053209	406.861406	7.184320
6.039789	392.414610	7.189325
5.790082	409.101996	7.194330
5.873488	411.385832	7.199334
6.116599	407.878130	7.204339
5.688960	396.765701	7.209344
5.941616	395.780596	7.214349
5.667687	411.032203	7.219354
5.621759	392.962101	7.224358
5.885996	413.526382	7.229363
5.769255	406.289139	7.234368
5.844215	405.988627	7.239373
5.748641	408.819920	7.244378
5.771428	405.531240	7.249382
5.751786	414.291476	7.254387
5.691677	402.325272	7.259392
5.754132	410.717093	7.264397
5.657754	417.811067	7.269402
5.978056	402.459650	7.274406
5.871419	406.511941	7.279411
5.850376	406.660092	7.284416
5.797115	406.751219	7.289421
5.472290	408.907483	7.294426
6.052236	398.174249	7.299430
5.858815	402.646838	7.304435
5.777679	401.870338	7.309440
5.871965	400.488557	7.314445
5.668312	404.279452	7.319450
5.957630	395.015390	7.324454
6.162885	394.545297	7.329459
5.784640	395.920849	7.334464
5.965953	398.077171	7.339469
5.542444	403.301046	7.344474
5.791841	392.992169	7.349478
5.466363	401.265880	7.354483
5.641935	394.495100	7.359488
5.872376	402.491062	7.364493
5.812819	422.376642	7.369498
6.160014	414.028511	7.374502
6.076614	400.819764	7.379507
5.689605	406.820642	7.384512
6.182694	397.100924	7.389517
5.706339	403.559031	7.394522
6.221209	394.806817	7.399526
6.011250	405.909807	7.404531
5.934362	399.176488	7.409536
6.019614	399.145613	7.414541
5.612845	404.162273	7.419546
6.064879	397.040033	7.424550
5.455655	392.505810	7.429555
5.713424	396.751536	7.434560
5.631024	399.973747	7.439565
5.557086	398.865905	7.444570
6.145168	413.140817	7.449574
5.930275	417.458699	7.454579
6.131213	401.096932	7.459584
6.077431	396.369103	7.464589
5.780651	401.699080	7.469594
6.173611	390.506029	7.474598
5.984236	396.058185	7.479603
5.613047	392.993407	7.484608
5.832532	400.123676	7.489613
5.601763	394.367215	7.494618
5.869596	393.299082	7.499622
5.841521	396.089200	7.504627
6.059418	396.173908	7.509632
5.845034	393.791812	7.514637
5.540276	403.678900	7.519642
5.962091	391.708484	7.524646
6.025282	397.702498	7.529651
5.835259	399.750400	7.534656
5.961673	390.548837	7.539661
5.828035	399.619806	7.544666
6.047237	392.599665	7.549670
5.782299	397.752682	7.554675
5.992123	403.980933	7.559680
5.845592	401.340137	7.564685
5.861205	408.758737	7.569690
5.916979	392.662758	7.574694
5.724104	398.391521	7.579699
5.852364	398.410951	7.584704
5.967981	393.230594	7.589709
5.886307	398.237032	7.594714
5.835099	387.205152	7.599718
5.792594	403.687918	7.604723
5.658503	398.383143	7.609728
5.808139	399.023220	7.614733
5.776627	406.539411	7.619738
5.706892	395.860082	7.624742
5.722279	406.024703	7.629747
6.150371	419.155295	7.634752
6.515041	407.724780	7.639757
5.809554	404.030586	7.644762
5.929816	399.664670	7.649766
6.058528	396.115922	7.654771
6.104635	398.191029	7.659776
6.171631	399.542584	7.664781
5.782766	394.576600	7.669786
5.934533	392.468366	7.674790
5.957602	395.640945	7.679795
6.001905	396.924623	7.684800
6.141842	400.884972	7.689805
5.776878	402.325815	7.694810
6.141844	391.567403	7.699814
5.895465	394.880112	7.704819
6.031109	399.736108	7.709824
6.298512	392.589779	7.714829
5.545238	392.882663	7.719834
6.246262	389.216848	7.724838
6.335961	395.587140	7.729843
6.086901	377.163314	7.734848
6.003282	370.215035	7.739853
5.449595	369.983494	7.744858
5.740120	365.777458	7.749862
5.641671	370.563868	7.754867
5.672693	369.217431	7.759872
5.643304	381.368174	7.764877
6.084489	404.303977	7.769882
6.228787	385.151549	7.774886
5.958106	370.965631	7.779891
6.017329	363.905491	7.784896
6.135272	372.986488	7.789901
5.715704	365.509715	7.794906
5.640463	361.730510	7.799910
5.573108	372.280005	7.804915
5.819587	380.812234	7.809920
5.780175	389.403649	7.814925
5.642771	399.853463	7.819930
6.113009	392.228546	7.824934
6.288614	396.304944	7.829939
5.713299	391.667620	7.834944
5.738502	377.185829	7.839949
5.548874	377.353410	7.844954
5.887125	382.716365	7.849958
5.900089	396.552492	7.854963
5.840079	402.863905	7.859968
6.190217	395.984690	7.864973
5.826877	388.877093	7.869978
5.614198	381.188053	7.874982
5.720678	398.345713	7.879987
5.673311	393.671880	7.884992
6.201393	405.921357	7.889997
5.843868	404.423958	7.895002
5.892249	403.214557	7.900006
6.046292	399.902171	7.905011
5.906398	401.306140	7.910016
6.231088	385.395146	7.915021
5.733336	385.977051	7.920026
5.631469	376.392371	7.925030
5.771897	382.652036	7.930035
5.939791	401.936719	7.935040
6.107633	399.506921	7.940045
5.871715	390.014091	7.945050
5.679858	372.247413	7.950054
5.705912	388.684276	7.955059
5.904628	388.827414	7.960064
6.182320	390.769055	7.965069
5.849808	391.430951	7.970074
6.053064	370.917395	7.975078
5.784038	372.169677	7.980083
5.727520	376.555651	7.985088
5.830458	375.524888	7.990093
5.888118	395.828329	7.995098
5.915214	394.340652	8.000102
5.845720	391.949169	8.005107
6.104536	386.276420	8.010112
5.887578	372.409387	8.015130
5.925604	383.190128	8.020147
5.495559	371.492318	8.025165
5.911937	376.388778	8.030182
6.115806	391.772636	8.035200
6.051908	381.495580	8.040218
5.805482	373.517686	8.045235
6.022277	364.202161	8.050253
5.981217	375.101102	8.055270
5.944903	372.415987	8.060288
5.810264	362.879739	8.065306
5.771571	371.472351	8.070323
6.022155	364.980750	8.075341
5.753717	370.376601	8.080358
5.822020	380.992495	8.085376
6.164429	385.608314	8.090394
5.844916	381.285172	8.095411
5.993718	382.609271	8.100429
6.207329	385.629210	8.105446
5.700012	375.616318	8.110464
5.867411	378.810824	8.115482
5.928844	390.725801	8.120499
6.219327	385.475332	8.125517
6.131857	388.058153	8.130534
5.773050	374.387071	8.135552
6.264385	372.477710	8.140570
5.658229	374.291952	8.145587
6.003590	383.065249	8.150605
5.948644	385.914712	8.155622
6.025100	395.206133	8.160640
5.858088	387.252481	8.165658
5.843945	395.086173	8.170675
5.821611	392.637109	8.175693
5.851836	393.821603	8.180710
5.850051	398.594019	8.185728
6.020190	392.683011	8.190746
5.851288	394.784274	8.195763
6.108392	387.045019	8.200781
6.247657	386.357061	8.205798
5.697133	394.342166	8.210816
6.057561	396.748074	8.215834
5.645885	405.005840	8.220851
5.790904	400.874848	8.225869
5.614811	399.168122	8.230886
6.107375	412.176604	8.235904
6.549520	415.913772	8.240922
6.204802	417.174526	8.245939
6.233209	398.257972	8.250957
5.970387	395.304476	8.255974
5.625012	397.722539	8.260992
6.234036	404.649167	8.266010
6.483445	414.483180	8.271027
6.151169	410.477870	8.276045
6.069991	400.811297	8.281062
6.117287	407.136896	8.286080
6.321490	408.589216	8.291098
6.009572	405.383827	8.296115
6.379012	413.954153	8.301133
6.242205	400.191566	8.306150
6.052040	405.421132	8.311168
6.317803	400.385366	8.316186
6.216490	390.858738	8.321203
6.233780	398.376226	8.326221
6.056585	392.264679	8.331238
6.082298	398.686756	8.336256
6.273016	406.505821	8.341274
6.088322	416.551865	8.346291
6.423257	416.829468	8.351309
6.328702	405.535103	8.356326
6.235984	403.444321	8.361344
6.287641	396.288649	8.366362
5.833768	397.677902	8.371379
6.222272	409.968626	8.376397
6.346637	436.012395	8.381414
6.141804	420.633409	8.386432
6.211099	418.239439	8.391450
6.577279	425.037402	8.396467
6.213631	412.946310	8.401485
6.058327	410.107872	8.406502
6.198936	423.845463	8.411520
6.173679	421.829132	8.416538
6.337719	413.012239	8.421555
6.477971	425.534227	8.426573
6.278797	422.037743	8.431590
6.241144	430.971138	8.436608
6.344343	421.000812	8.441626
6.540419	429.013083	8.446643
6.219482	419.494067	8.451661
6.425362	420.961857	8.456678
6.246020	419.382823	8.461696
6.517750	421.928217	8.466714
6.720886	421.801886	8.471731
6.538910	404.234441	8.476749
6.361838	395.379561	8.481766
6.318616	382.863806	8.486784
6.131895	383.833256	8.491802
5.944229	398.222581	8.496819
6.370224	407.409873	8.501837
6.755760	409.334887	8.506854
6.585160	413.688442	8.511872
6.540041	394.935827	8.516890
6.082678	402.732294	8.521907
6.506796	400.378383	8.526925
6.621158	400.344109	8.531942
6.373687	403.378398	8.536960
5.893768	386.854530	8.541978
5.892200	402.325759	8.546995
6.210835	417.870351	8.552013
6.603966	416.278210	8.557030
6.475896	422.201190	8.562048
6.751142	417.181760	8.567066
6.583541	413.794412	8.572083
6.503612	430.524228	8.577101
6.860159	421.073724	8.582119
6.251018	434.119979	8.587136
6.462876	425.730958	8.592154
6.731289	428.029085	8.597171
6.646370	424.349912	8.602189
6.769265	420.017671	8.607207
6.547998	402.526217	8.612224
6.382293	394.509160	8.617242
6.494273	394.727429	8.622259
6.186969	398.756200	8.627277
6.525991	416.975573	8.632295
6.808945	422.812778	8.637312
6.621915	416.419996	8.642330
6.633423	413.199039	8.647347
6.304061	403.180282	8.652365
6.527711	401.857528	8.657383
6.710058	417.565622	8.662400
6.719133	415.794180	8.667418
6.442566	406.972893	8.672435
6.338603	409.613761	8.677453
6.761182	412.789443	8.682471
6.346943	427.965671	8.687488
6.830098	421.669968	8.692506
6.742954	424.877305	8.697523
6.520107	425.124247	8.702541
6.647450	422.843884	8.707559
6.596411	421.691605	8.712576
6.791465	420.704074	8.717594
6.797092	400.822064	8.722611
6.413378	396.277872	8.727629
6.590924	393.050094	8.732647
6.632627	415.521156	8.737664
6.310102	412.723202	8.742682
6.856911	412.910214	8.747699
6.744835	415.376060	8.752717
6.906793	415.147303	8.757735
6.357094	407.814057	8.762752
6.447679	406.886539	8.767770
6.880202	420.408085	8.772787
6.771262	412.208994	8.777805
7.082498	410.517036	8.782823
6.717200	409.395931	8.787840
6.734878	394.588745	8.792858
6.753120	388.197021	8.797875
6.619972	387.269350	8.802893
6.443234	390.213779	8.807911
6.615041	417.417885	8.812928
6.879009	418.778622	8.817946
7.206740	412.872414	8.822963
6.669700	408.732125	8.827981
6.738973	390.868974	8.832999
6.684825	398.583121	8.838016
7.097874	397.500639	8.843034
6.946929	393.649940	8.848051
6.478359	389.655394	8.853069
6.886484	382.767647	8.858087
6.754173	391.278928	8.863104
6.570367	384.474828	8.868122
6.922418	397.499479	8.873139
6.538218	411.272587	8.878157
7.008242	414.644730	8.883175
6.741345	422.497850	8.888192
6.654582	420.013193	8.893210
6.861311	419.716791	8.898227
6.573838	411.118750	8.903245
6.747232	418.495642	8.908263
6.644466	414.847575	8.913280
6.881957	414.609855	8.918298
7.041591	415.027895	8.923315
6.791811	420.279738	8.928333
6.686296	416.800028	8.933351
6.668139	419.689268	8.938368
6.755531	418.644767	8.943386
6.826806	416.767559	8.948403
6.772179	424.248152	8.953421
6.640078	417.737817	8.958439
6.892725	421.389247	8.963456
7.047636	422.569041	8.968474
6.971175	413.905547	8.973491
6.925706	419.657182	8.978509
6.842391	418.501784	8.983527
6.693078	423.047867	8.988544
6.832419	422.885843	8.993562
6.996661	413.603792	8.998579
6.874395	410.251848	9.003597
7.118807	417.429986	9.008615
6.977120	421.447085	9.013632
7.166364	424.308676	9.018650
7.253681	412.351163	9.023667
7.185389	418.319948	9.028685
7.163571	419.882722	9.033703
6.821830	418.390615	9.038720
6.948049	419.409619	9.043738
7.223298	417.424428	9.048755
7.122906	416.891697	9.053773
7.308592	420.349898	9.058791
7.206361	412.532740	9.063808
7.273146	416.180499	9.068826
7.241030	407.294917	9.073843
7.188780	417.727663	9.078861
7.245072	406.746090	9.083879
6.883499	421.715967	9.088896
7.134960	409.423226	9.093914
7.258074	410.513015	9.098931
7.228906	418.417313	9.103949
7.111743	411.808844	9.108967
7.319358	423.595710	9.113984
6.915413	418.538560	9.119002
7.150457	411.300746	9.124019
7.046504	417.601988	9.129037
7.253076	417.383166	9.134055
7.303693	417.718084	9.139072
7.234225	408.048190	9.144090
7.258404	384.350403	9.149107
6.692425	389.536296	9.154125
6.853646	391.224062	9.159143
7.324193	403.393723	9.164160
7.063734	410.122030	9.169178
7.069453	404.804345	9.174195
6.987800	410.401745	9.179213
7.034302	402.266874	9.184231
7.176915	412.650028	9.189248
7.029869	411.681549	9.194266
7.526897	409.782461	9.199283
6.789806	412.910818	9.204301
7.024262	410.561542	9.209319
7.119433	409.077989	9.214336
7.148438	414.027975	9.219354
7.206837	415.677458	9.224371
7.365660	412.848811	9.229389
7.424162	408.109352	9.234407
7.505923	402.651723	9.239424
6.952641	415.926295	9.244442
7.663119	404.196285	9.249459
7.450809	404.139141	9.254477
7.567618	408.869287	9.259495
7.267766	413.431436	9.264512
7.498319	415.556117	9.269530
7.155166	413.005263	9.274547
7.348837	409.959247	9.279565
7.539197	405.855979	9.284583
7.487053	411.652612	9.289600
7.255931	408.773189	9.294618
7.465858	408.746318	9.299635
7.295156	408.778143	9.304653
7.247056	412.123884	9.309671
7.242181	418.063272	9.314688
7.057808	421.067826	9.319706
7.290282	412.451202	9.324723
7.187867	417.700097	9.329741
7.133183	410.563602	9.334759
7.274681	409.051512	9.339776
7.252885	415.215142	9.344794
7.668929	414.231960	9.349811
7.130886	414.966498	9.354829
7.342008	403.379015	9.359847
7.442748	406.884544	9.364864
7.300562	415.653756	9.369882
7.502257	407.162105	9.374899
7.230020	407.762083	9.379917
7.473568	400.107737	9.384935
7.264416	405.174711	9.389952
7.170199	419.258641	9.394970
7.771946	414.684719	9.399987
7.563994	420.171745	9.405005
7.588575	406.093473	9.410023
7.652259	409.324056	9.415040
7.556006	411.149727	9.420058
7.730853	414.090270	9.425075
7.367547	407.390680	9.430093
7.438743	404.514935	9.435111
7.565283	413.040645	9.440128
7.259963	413.900612	9.445146
7.521363	406.208270	9.450163
7.488910	411.577263	9.455181
7.356251	406.071482	9.460199
7.519504	412.673531	9.465216
7.624539	418.620899	9.470234
7.463215	413.872959	9.475251
7.459536	423.592992	9.480269
7.519679	433.628621	9.485287
7.923178	429.118622	9.490304
7.645498	436.366096	9.495322
7.328972	413.447270	9.500339
7.351784	429.700262	9.505357
7.874471	429.199977	9.510375
7.808290	432.450691	9.515392
7.611961	438.067286	9.520410
7.633137	428.828993	9.525427
7.605927	428.811863	9.530445
7.796618	430.441213	9.535463
7.592070	413.348132	9.540480
7.397251	420.672619	9.545498
7.815514	422.082015	9.550515
7.665242	433.991139	9.555533
7.690286	438.231208	9.560551
7.644981	436.063677	9.565568
7.600816	442.236337	9.570586
8.004743	434.042067	9.575603
7.784421	442.447289	9.580621
7.749593	430.317481	9.585639
7.961351	426.240387	9.590656
7.687610	417.608771	9.595674
7.527039	406.286559	9.600691
7.747249	420.568605	9.605709
7.706929	423.792202	9.610727
7.887060	423.362419	9.615744
7.874647	422.182289	9.620762
7.793771	406.142481	9.625779
7.712091	401.551228	9.630797
7.730529	402.374117	9.635815
7.892101	403.851801	9.640832
7.673557	413.080081	9.645850
7.632088	416.447361	9.650867
7.797813	433.527421	9.655885
8.048338	434.961640	9.660903
7.845054	437.530775	9.665920
7.759986	442.227238	9.670938
8.278268	421.393244	9.675955
7.620134	412.448536	9.680973
7.822730	413.461389	9.685991
7.976036	422.507833	9.691008
7.481153	428.650009	9.696026
7.589372	424.658757	9.701043
7.701662	424.888981	9.706061
7.981500	431.294974	9.711079
8.274212	430.982562	9.716096
7.862927	432.726749	9.721114
8.237068	438.656531	9.726131
8.153119	438.620255	9.731149
7.735635	425.623758	9.736167
7.466892	425.402742	9.741184
7.852790	437.331740	9.746202
7.867526	431.617894	9.751219
8.043280	424.873127	9.756237
8.042049	428.486879	9.761255
8.076713	431.256949	9.766272
8.011146	432.458096	9.771290
7.983041	433.158191	9.776307
8.107638	436.637338	9.781325
7.922766	441.994771	9.786343
8.378844	430.542087	9.791360
8.188756	430.696800	9.796378
7.966796	416.012143	9.801395
7.869342	416.620382	9.806413
7.922590	424.475802	9.811431
8.049755	431.576124	9.816448
8.106839	436.815739	9.821466
8.289546	432.163573	9.826483
8.051822	420.426203	9.831501
7.685697	417.837028	9.836519
8.108457	423.780012	9.841536
8.011548	432.671845	9.846554
8.016815	424.842785	9.851571
7.842756	435.553570	9.856589
7.624025	441.389806	9.861607
7.997602	435.706690	9.866624
7.444202	433.016643	9.871642
7.743767	437.981871	9.876659
7.792592	446.784821	9.881677
8.067459	455.609397	9.886695
8.253919	460.613439	9.891712
7.816933	466.297255	9.896730
8.339809	466.791753	9.901747
8.567865	468.227728	9.906765
8.364273	461.193224	9.911783
8.328734	444.067989	9.916800
7.927610	434.891352	9.921818
7.963540	445.013079	9.926835
8.304280	449.765799	9.931853
8.158084	450.065595	9.936871
8.418621	457.747544	9.941888
8.148641	458.921718	9.946906
8.172127	467.280284	9.951923
8.033418	461.670177	9.956941
8.324648	472.073247	9.961959
8.554745	463.864442	9.966976
8.320823	472.577030	9.971994
8.407876	464.214954	9.977011
8.450658	442.538470	9.982029
8.010467	442.207664	9.987047
8.117586	444.678357	9.992064
8.239673	465.067424	9.997082
8.281020	458.511029	10.002099
8.431238	465.524680	10.007117
8.458901	463.078939	10.012135
8.422540	461.263247	10.017152
8.282213	462.420480	10.022170
8.484965	461.120472	10.027187
8.547061	448.058716	10.032205
8.540407	445.185421	10.037223
8.248249	434.410730	10.042240
8.323022	439.062222	10.047258
8.311752	432.313579	10.052275
8.369494	449.184190	10.057293
8.100898	461.526681	10.062311
8.636579	456.047015	10.067328
8.504074	464.050726	10.072346
8.367591	461.940413	10.077363
8.209281	457.100432	10.082381
8.061653	464.844459	10.087399
8.542020	461.502157	10.092416
8.948890	472.665162	10.097434
8.571252	461.464675	10.102451
8.580807	439.465963	10.107469
8.347894	449.686734	10.112487
8.758267	441.156967	10.117504
8.244780	439.202581	10.122522
8.307648	442.232927	10.127539
8.648687	456.282807	10.132557
8.606651	469.620397	10.137575
8.788265	448.403167	10.142592
8.555202	446.063786	10.147610
8.472377	440.809370	10.152627
8.607304	429.755511	10.157645
8.017965	432.130125	10.162663
8.462717	436.558355	10.167680
8.692231	453.846954	10.172698
8.540053	458.413992	10.177715
8.847586	451.629676	10.182733
8.572677	465.545157	10.187751
8.679335	452.092777	10.192768
8.402527	455.459273	10.197786
8.615274	455.957884	10.202803
8.756689	447.380726	10.207821
8.432629	460.648283	10.212839
8.458696	460.780589	10.217856
8.431429	468.362178	10.222874
8.604645	469.299983	10.227891
8.631559	455.043339	10.232909
8.647902	458.081785	10.237927
8.779331	459.041273	10.242944
8.636852	463.618123	10.247962
8.396373	457.811301	10.252979
8.576735	462.466770	10.257997
8.410046	466.006164	10.263015
8.728338	456.185816	10.268032
8.695508	459.409165	10.273050
8.433481	455.723881	10.278067
8.589221	464.759712	10.283085
8.602001	464.087184	10.288103
8.727802	462.706026	10.293120
8.832170	464.870309	10.298138
8.686838	465.777797	10.303155
8.837349	457.964037	10.308173
8.805391	468.817446	10.313191
8.768716	460.444956	10.318208
8.768081	465.873261	10.323226
8.596782	472.241382	10.328243
8.997069	477.397018	10.333261
8.744496	480.803402	10.338279
9.027740	491.322367	10.343296
8.969161	475.382923	10.348314
8.500863	470.328144	10.353331
8.605795	466.843297	10.358349
9.067942	485.194912	10.363367
9.053241	488.280234	10.368384
9.231282	479.351741	10.373402
9.046517	474.636206	10.378419
9.115337	460.017326	10.383437
8.771716	460.887180	10.388455
8.917535	456.506451	10.393472
8.716128	461.344223	10.398490
8.640102	461.929822	10.403507
9.294317	464.174502	10.408525
8.866076	465.233160	10.413543
8.837385	457.870896	10.418560
8.949440	458.457436	10.423578
9.052460	466.979788	10.428595
8.705017	449.346389	10.433613
8.781559	479.927572	10.438631
8.898985	482.444987	10.443648
9.258398	481.763482	10.448666
9.235214	486.355623	10.453683
9.259429	472.033075	10.458701
9.085713	464.800918	10.463719
8.955977	455.503155	10.468736
9.020154	460.547129	10.473754
8.896337	463.697756	10.478771
9.247242	473.031764	10.483789
9.274383	481.126363	10.488807
9.046380	464.566011	10.493824
8.933231	457.148250	10.498842
8.710598	462.980219	10.503859
9.360217	466.594664	10.508877
9.412156	470.840918	10.513895
8.950713	463.070224	10.518912
8.910112	469.116525	10.523930
9.146998	478.112943	10.528947
9.440157	479.043289	10.533965
9.298897	468.346534	10.538983
9.151468	461.563146	10.544000
9.139317	454.872116	10.549018
8.789413	454.873580	10.554035
9.074619	471.529003	10.559053
9.115113	480.968743	10.564071
9.499790	484.204847	10.569088
9.394000	479.860460	10.574106
9.464505	471.799132	10.579123
9.434434	464.129831	10.584141
8.963623	456.168972	10.589159
9.047100	450.029198	10.594176
9.285119	470.094961	10.599194
9.306844	483.679468	10.604211
9.091816	481.664043	10.609229
8.991242	482.682223	10.614247
9.353060	480.595293	10.619264
9.667750	474.637091	10.624282
9.050655	482.937771	10.629299
9.263876	484.796059	10.634317
9.264415	488.925246	10.639335
9.312361	483.079513	10.644352
9.652779	481.132732	10.649370
9.140039	481.397955	10.654387
8.998612	484.699523	10.659405
9.437306	470.022537	10.664423
9.246442	480.781606	10.669440
9.308974	478.886745	10.674458
9.222809	487.002471	10.679475
9.468739	479.419735	10.684493
8.998767	488.086385	10.689511
9.253834	487.916615	10.694528
9.333848	484.307552	10.699546
9.136251	491.681939	10.704563
9.332396	485.210523	10.709581
9.095200	492.328886	10.714599
9.510896	500.190268	10.719616
9.763673	501.412521	10.724634
9.666823	488.797102	10.729651
9.734664	482.855561	10.734669
9.978666	480.111412	10.739687
9.979955	482.944889	10.744704
9.695737	480.753532	10.749722
9.533469	484.786063	10.754739
9.657281	476.989115	10.759757
9.533505	486.150962	10.764775
9.012355	483.816171	10.769792
9.624247	480.343038	10.774810
9.226580	484.623984	10.779827
9.135660	476.610642	10.784845
9.357607	481.390718	10.789863
9.313355	480.023742	10.794880
9.807842	476.548595	10.799898
9.540035	480.980270	10.804915
9.593540	476.300471	10.809933
9.289779	486.460365	10.814951
9.321258	497.732395	10.819968
9.877101	495.752697	10.824986
9.707671	510.955787	10.830003
9.922036	512.520599	10.835021
9.818548	493.339763	10.840039
9.570016	491.102340	10.845056
9.790853	472.951809	10.850074
9.464693	480.606715	10.855091
9.394621	496.464554	10.860109
9.601662	508.326773	10.865127
9.853317	505.016822	10.870144
10.406868	499.160190	10.875162
9.597335	488.164262	10.880179
9.832730	480.241167	10.885197
9.579007	478.037477	10.890215
9.675164	489.286390	10.895232
10.101794	496.247593	10.900250
9.742272	491.317699	10.905267
9.719592	482.199227	10.910285
9.800400	482.343333	10.915303
9.849447	494.007701	10.920320
9.757876	482.183883	10.925338
9.533711	489.056795	10.930355
9.978652	496.561781	10.935373
10.139741	512.359707	10.940391
9.926201	499.937213	10.945408
10.017241	492.088405	10.950426
9.648304	484.962969	10.955443
9.658961	493.261866	10.960461
9.461281	499.643028	10.965479
9.942332	508.855317	10.970496
10.146529	500.893678	10.975514
9.812550	502.974459	10.980531
9.903468	507.138289	10.985549
9.852195	506.658637	10.990567
9.847539	503.795434	10.995584
9.989658	501.026029	11.000602
10.131999	510.547932	11.005619
9.758905	506.843432	11.010637
9.980613	508.629455	11.015655
9.801862	515.419274	11.020672
9.943647	509.959147	11.025690
9.918521	514.297303	11.030707
10.084536	502.012338	11.035725
10.222365	502.388326	11.040743
10.179388	501.486068	11.045760
10.378634	506.780312	11.050778
10.084800	507.330920	11.055795
10.181849	504.123337	11.060813
10.268948	506.082034	11.065831
9.925834	511.614503	11.070848
10.091209	505.414692	11.075866
10.129756	512.371664	11.080883
10.152823	500.427280	11.085901
10.298556	506.887004	11.090919
9.609159	501.826703	11.095936
10.159707	498.601897	11.100954
10.043152	508.010773	11.105971
10.157605	508.640222	11.110989
10.179391	509.185808	11.116007
10.067580	509.329135	11.121024
10.218788	505.736229	11.126042
10.145321	502.284064	11.131059
10.086653	510.131880	11.136077
10.420554	499.202496	11.141095
10.250719	505.587710	11.146112
10.751426	499.885095	11.151130
10.356740	511.313524	11.156147
10.397136	504.919067	11.161165
10.272783	509.361442	11.166183
10.330630	504.495888	11.171200
10.522353	498.013782	11.176218
10.129555	493.476380	11.181235
9.971407	500.534417	11.186253
10.055623	499.828800	11.191271
9.992348	508.265530	11.196288
10.394860	497.267702	11.201306
10.411722	505.433303	11.206323
10.437368	513.397466	11.211341
10.669970	498.839416	11.216359
10.371704	504.026289	11.221376
10.287703	505.825535	11.226394
10.337375	509.032476	11.231411
10.211366	505.434297	11.236429
10.347721	498.772788	11.241447
10.326320	513.288025	11.246464
10.380867	503.834725	11.251482
10.250481	503.511078	11.256499
10.405446	507.811538	11.261517
10.517740	511.553352	11.266535
10.369168	508.097481	11.271552
10.329863	506.267509	11.276570
10.342745	505.280021	11.281587
10.200264	500.108686	11.286605
10.412274	505.242559	11.291623
10.368127	504.834557	11.296640
10.500706	503.575298	11.301658
10.631962	507.036823	11.306675
10.694300	506.396242	11.311693
10.850254	504.243011	11.316711
10.558906	510.615673	11.321728
10.250162	511.380548	11.326746
10.317918	497.095844	11.331763
10.358742	518.342477	11.336781
10.956115	524.249106	11.341799
10.749835	528.154693	11.346816
10.646112	509.970269	11.351834
10.626103	510.709773	11.356851
10.494454	508.304971	11.361869
10.823798	498.205816	11.366887
10.718867	500.870676	11.371904
10.681823	500.089082	11.376922
10.788297	501.302491	11.381939
10.914161	502.066656	11.386957
10.873236	494.059789	11.391975
10.595351	504.966936	11.396992
10.501472	495.681123	11.402010
10.401172	496.603596	11.407027
10.379173	503.713887	11.412045
11.052566	511.433792	11.417063
10.939482	528.048738	11.422080
10.945410	506.112143	11.427098
10.970416	492.669114	11.432115
10.573444	500.846549	11.437133
10.977683	492.507718	11.442151
10.687111	501.700145	11.447168
10.558357	498.106358	11.452186
10.777126	488.364474	11.457203
10.880694	505.328930	11.462221
10.968622	497.081054	11.467239
10.798223	499.046564	11.472256
10.869350	496.916041	11.477274
10.657483	494.103685	11.482291
10.680566	510.745275	11.487309
11.184693	507.376195	11.492327
11.025336	523.616540	11.497344
11.041490	510.640287	11.502362
11.017865	498.157608	11.507379
10.654518	502.857651	11.512397
10.686540	492.849069	11.517415
11.039463	511.118217	11.522432
11.239150	516.223821	11.527450
10.955811	511.739938	11.532467
10.577035	517.760961	11.537485
11.172864	516.896616	11.542503
10.888260	515.926894	11.547520
10.990044	519.931457	11.552538
11.151093	523.164445	11.557555
10.955693	524.491225	11.562573
11.476513	530.032997	11.567591
11.010848	528.171265	11.572608
10.855569	530.722034	11.577626
10.890019	533.816942	11.582643
10.901597	524.575851	11.587661
11.333932	519.062098	11.592679
11.353702	536.727035	11.597696
11.089525	529.261418	11.602714
11.107495	520.565693	11.607731
11.196685	533.900505	11.612749
11.477678	522.743658	11.617767
11.514822	522.235587	11.622784
11.217210	509.168386	11.627802
10.799719	504.801988	11.632819
10.865561	507.642890	11.637837
11.538217	510.727777	11.642855
11.308687	513.099512	11.647872
10.862386	513.544667	11.652890
11.568730	515.294533	11.657907
11.458086	517.024181	11.662925
11.186449	494.009224	11.667943
10.735508	510.915515	11.672960
11.103909	518.679234	11.677978
11.219596	521.277253	11.682995
11.637807	523.418511	11.688013
11.689325	526.704674	11.693031
11.206251	532.039473	11.698048
11.477514	536.104555	11.703066
11.504299	519.485813	11.708083
11.081656	509.498967	11.713101
11.344734	510.140417	11.718119
11.426067	517.480833	11.723136
11.271540	526.563746	11.728154
11.520656	524.706089	11.733171
11.455608	515.209598	11.738189
11.600922	508.880439	11.743207
11.695121	506.955135	11.748224
11.377355	501.088461	11.753242
11.442289	486.764472	11.758259
10.939951	497.314712	11.763277
11.466582	502.682688	11.768295
11.607522	518.005247	11.773312
11.269739	514.177188	11.778330
11.556228	519.465651	11.783347
11.210885	518.942180	11.788365
11.510710	514.573136	11.793383
11.733401	517.910868	11.798400
11.362806	523.042406	11.803418
11.569335	514.905976	11.808435
11.548452	518.567882	11.813453
11.669166	512.749455	11.818471
11.560012	519.094314	11.823488
11.488495	524.194437	11.828506
11.681895	519.807977	11.833523
11.401652	523.258122	11.838541
11.532962	523.123410	11.843559
11.848373	518.155758	11.848576
11.566705	524.402815	11.853594
11.753758	513.170985	11.858611
11.191233	527.485306	11.863629
11.835326	519.506719	11.868647
11.744154	519.225001	11.873664
11.180312	518.432217	11.878682
11.675044	515.553244	11.883699
11.170293	525.762979	11.888717
11.364944	514.205501	11.893735
11.225215	535.549767	11.898752
11.511592	547.720513	11.903770
11.793897	548.161156	11.908787
11.868088	549.701549	11.913805
11.905336	555.270257	11.918823
11.754916	548.060186	11.923840
11.909440	547.275607	11.928858
12.185545	550.238776	11.933875
12.021292	552.799302	11.938893
11.882789	544.954227	11.943911
12.076430	553.149238	11.948928
11.710402	530.900205	11.953946
11.922167	528.257444	11.958963
11.822320	540.959038	11.963981
11.961900	542.518129	11.968999
11.648237	545.138431	11.974016
12.094960	552.029801	11.979034
12.221484	546.361178	11.984051
11.932449	535.960088	11.989069
11.741440	530.630647	11.994087
11.784827	539.684732	11.999104
11.931323	542.114277	12.004122
12.065813	535.722730	12.009139
12.150681	550.494010	12.014157
12.142007	549.722282	12.019175
12.190666	551.427129	12.024192
12.064017	546.718089	12.029210
11.914093	527.568126	12.034227
11.574335	543.195490	12.039245
12.130824	542.166015	12.044263
12.109457	541.126720	12.049280
12.157232	545.610283	12.054298
11.896109	544.862248	12.059315
11.759630	544.979346	12.064333
12.055576	534.821922	12.069351
12.234201	542.753290	12.074368
11.913988	540.592291	12.079386
11.837769	543.866540	12.084403
12.144434	546.078238	12.089421
12.081510	543.271916	12.094439
12.096177	541.818805	12.099456
11.830528	546.809752	12.104474
12.601083	542.379681	12.109491
12.304033	544.759845	12.114509
12.307179	546.058474	12.119527
12.412238	534.072536	12.124544
12.271252	545.174353	12.129562
12.229742	543.006966	12.134579
12.038746	550.126367	12.139597
12.097839	537.461072	12.144615
12.563170	543.490748	12.149632
12.247656	541.882087	12.154650
12.409286	540.719976	12.159667
12.523883	543.372901	12.164685
12.433922	541.095434	12.169703
12.380674	542.169163	12.174720
12.104794	545.878811	12.179738
12.328794	531.251294	12.184755
11.989192	545.842084	12.189773
12.007153	541.314600	12.194791
12.571010	549.582944	12.199808
12.483885	561.228576	12.204826
12.648213	540.635305	12.209843
12.427305	546.563667	12.214861
12.252407	548.949588	12.219879
12.654772	543.936035	12.224896
12.316895	553.034363	12.229914
12.674279	557.517448	12.234931
12.331286	553.268613	12.239949
12.419210	557.335714	12.244967
12.535017	562.950469	12.249984
12.841778	572.689658	12.255002
12.691435	556.091940	12.260019
12.506680	552.954631	12.265037
12.485627	550.159484	12.270055
12.687264	567.498690	12.275072
12.722882	558.755142	12.280090
12.613682	548.706920	12.285107
11.934094	540.436120	12.290125
11.984695	559.977360	12.295143
12.427179	560.665872	12.300160
12.561703	559.977117	12.305178
12.906987	564.732664	12.310195
12.889684	566.326395	12.315213
12.835905	566.606954	12.320231
13.107262	562.700851	12.325248
12.803913	567.751587	12.330266
13.131708	558.088451	12.335283
12.979574	572.493903	12.340301
13.024635	559.512428	12.345319
12.771760	548.982515	12.350336
12.933038	543.240820	12.355354
12.618691	538.424682	12.360371
12.665287	534.305425	12.365389
12.704645	557.454600	12.370407
13.297261	556.995092	12.375424
12.747762	554.921661	12.380442
12.774675	544.343060	12.385459
13.071823	544.674164	12.390477
12.724526	549.822324	12.395495
12.843263	549.559387	12.400512
13.110260	565.045360	12.405530
12.991832	544.523706	12.410547
12.971634	544.910508	12.415565
12.522806	536.391277	12.420583
12.865643	546.772862	12.425600
13.038901	553.567003	12.430618
13.254597	553.280925	12.435635
13.323930	563.940473	12.440653
13.044900	551.642554	12.445671
13.010694	526.422223	12.450688
12.914352	533.971978	12.455706
12.591753	539.420750	12.460723
12.460725	555.571009	12.465741
13.040804	552.209422	12.470759
13.295814	567.957603	12.475776
13.237792	567.792828	12.480794
13.225780	562.328625	12.485811
13.028044	555.203546	12.490829
12.917113	558.165848	12.495847
12.883622	553.918911	12.500864
12.958833	557.430670	12.505882
12.918004	561.424610	12.510899
13.137828	551.047511	12.515917
12.862265	560.668957	12.520935
13.124274	557.820245	12.525952
13.201828	557.621604	12.530970
12.650625	555.252805	12.535987
13.205245	566.970512	12.541005
13.373696	576.733394	12.546023
13.534873	568.109199	12.551040
13.272440	561.511335	12.556058
13.046747	554.229478	12.561075
13.353701	556.486402	12.566093
13.024396	557.390109	12.571111
13.683804	574.806269	12.576128
13.286467	566.905623	12.581146
13.205290	563.944062	12.586163
13.250340	571.758200	12.591181
13.219970	582.920856	12.596199
13.544683	577.768979	12.601216
13.180546	591.010805	12.606234
13.293810	585.773078	12.611251
13.684816	587.744845	12.616269
13.462757	580.550164	12.621287
13.513150	578.830126	12.626304
13.463601	591.561620	12.631322
13.704599	583.626915	12.636339
14.011468	574.825844	12.641357
13.295903	566.076765	12.646375
13.072059	554.714924	12.651392
13.462911	561.233683	12.656410
13.636234	574.643570	12.661427
13.766701	570.513565	12.666445
13.819678	575.746231	12.671463
13.794790	561.820882	12.676480
13.376041	545.605395	12.681498
13.342143	542.454918	12.686515
13.726258	555.506282	12.691533
13.187341	563.450182	12.696551
13.676509	572.846588	12.701568
13.636744	575.867578	12.706586
13.921195	571.783724	12.711603
13.960982	573.825456	12.716621
13.887665	567.905287	12.721639
14.024125	549.101159	12.726656
13.585683	550.096555	12.731674
13.546188	541.519382	12.736691
13.672083	547.353706	12.741709
13.928542	561.386785	12.746727
13.574234	550.464636	12.751744
13.615839	555.825943	12.756762
13.796323	578.524641	12.761779
13.926649	575.408378	12.766797
13.860534	572.480540	12.771815
14.059249	573.950712	12.776832
13.944477	559.397373	12.781850
13.877188	559.208544	12.786867
13.751722	540.398194	12.791885
13.544799	550.548787	12.796903
13.765585	564.768867	12.801920
13.935204	572.282475	12.806938
14.003895	569.050048	12.811955
14.115881	573.583220	12.816973
13.733896	575.505040	12.821991
13.899189	573.910062	12.827008
13.986455	572.422881	12.832026
13.815610	571.383140	12.837043
13.956878	570.387381	12.842061
13.659792	571.221584	12.847079
13.865412	571.499345	12.852096
14.153523	569.860410	12.857114
13.995041	576.621704	12.862131
14.313304	573.252680	12.867149
13.891903	573.520495	12.872167
14.037703	568.535246	12.877184
13.963338	575.711719	12.882202
13.874062	576.391046	12.887219
14.031934	573.893020	12.892237
13.647349	579.435135	12.897255
13.997509	574.408565	12.902272
13.974397	578.090538	12.907290
13.962679	595.995389	12.912307
14.655829	601.132690	12.917325
14.216099	598.961947	12.922343
14.245106	576.579329	12.927360
14.206374	585.068726	12.932378
14.380770	590.778901	12.937395
14.518613	584.425359	12.942413
14.006394	581.162356	12.947431
14.276955	573.191267	12.952448
14.591312	582.454430	12.957466
14.301985	578.722656	12.962483
14.179766	572.735390	12.967501
14.347344	579.346637	12.972519
14.321635	580.090237	12.977536
14.396004	592.709880	12.982554
14.491853	593.882145	12.987571
14.569109	585.664334	12.992589
14.367233	578.895027	12.997607
14.473218	570.463030	13.002624
14.458228	579.901192	13.007642
14.224860	573.696912	13.012659
14.850529	576.708890	13.017677
14.317996	586.322907	13.022695
14.396397	572.852857	13.027712
14.644621	594.570342	13.032730
14.470963	584.046577	13.037747
14.626715	590.834580	13.042765
14.540692	585.945189	13.047783
14.845102	591.261022	13.052800
14.527122	580.435980	13.057818
14.193501	577.166632	13.062835
14.658844	579.190258	13.067853
14.446281	598.843623	13.072871
14.581977	596.061880	13.077888
14.745352	604.727258	13.082906
14.707412	599.068527	13.087923
14.873669	595.854977	13.092941
14.857465	605.053999	13.097959
14.891812	602.392968	13.102976
14.633714	591.301718	13.107994
14.487599	602.339468	13.113011
14.925889	591.331713	13.118029
14.917603	600.360927	13.123047
14.738259	590.298703	13.128064
14.831726	600.035436	13.133082
14.618152	595.486435	13.138099
14.682517	596.571400	13.143117
14.599962	601.611176	13.148135
14.943172	602.481867	13.153152
15.055475	598.863101	13.158170
14.726105	597.463016	13.163187
14.847154	599.132655	13.168205
14.730576	599.141345	13.173223
14.497445	599.929528	13.178240
14.920511	588.812491	13.183258
14.898108	598.133001	13.188275
14.902101	596.869437	13.193293
14.563339	596.753117	13.198311
14.583348	597.114760	13.203328
14.882079	591.376663	13.208346
14.746338	599.641594	13.213363
14.965215	587.826127	13.218381
14.886590	605.451534	13.223399
15.070963	616.507006	13.228416
15.284606	625.569168	13.233434
15.076050	617.731325	13.238451
15.332226	612.857305	13.243469
15.147590	603.301038	13.248487
15.150449	593.366507	13.253504
14.886488	592.117787	13.258522
14.852793	606.239501	13.263539
15.367892	617.592159	13.268557
15.347713	624.981323	13.273575
15.498460	620.974318	13.278592
15.678244	599.183201	13.283610
15.359163	603.928697	13.288627
15.327177	592.765755	13.293645
15.120377	584.185555	13.298663
15.493782	586.620052	13.303680
15.237912	591.170836	13.308698
15.370729	592.112977	13.313715
15.360901	587.176325	13.318733
15.423572	594.344682	13.323751
15.194937	591.516975	13.328768
15.216924	585.045617	13.333786
15.214677	595.474534	13.338803
15.058993	595.116887	13.343821
15.066478	600.068922	13.348839
15.282842	613.639029	13.353856
15.652349	626.775152	13.358874
15.537509	622.231053	13.363891
15.638095	618.944125	13.368909
15.441650	620.567525	13.373927
15.523072	615.947232	13.378944
15.687633	616.744363	13.383962
15.428376	611.083300	13.388979
15.429282	619.610638	13.393997
15.549125	624.707453	13.399015
15.499499	632.919562	13.404032
15.643852	623.574540	13.409050
15.721717	632.976100	13.414067
15.718442	619.867941	13.419085
15.720802	615.163894	13.424103
15.455449	621.616544	13.429120
15.688256	611.872652	13.434138
15.920894	627.639559	13.439155
15.431001	609.403221	13.444173
15.727698	615.858858	13.449191
15.576232	624.773614	13.454208
16.015883	623.854421	13.459226
15.761124	623.206897	13.464243
15.712370	618.908535	13.469261
15.693113	622.182816	13.474279
15.485502	625.220979	13.479296
15.828160	615.902965	13.484314
15.751365	624.521120	13.489331
15.981847	611.907695	13.494349
15.872740	617.377439	13.499367
15.754693	620.091339	13.504384
15.758209	618.590464	13.509402
15.531574	618.006783	13.514419
15.533431	619.338701	13.519437
15.692236	619.585634	13.524455
15.478355	618.056981	13.529472
15.760206	618.556359	13.534490
15.879028	611.454817	13.539507
16.077856	612.276980	13.544525
15.996974	616.698802	13.549543
15.936174	610.832840	13.554560
15.970733	606.572651	13.559578
16.059271	619.461214	13.564595
16.280761	616.956584	13.569613
16.046922	612.101502	13.574631
16.175051	623.184796	13.579648
16.144629	615.885536	13.584666
15.872663	625.003699	13.589683
16.115174	625.171421	13.594701
16.273422	626.264069	13.599719
16.134151	630.286138	13.604736
16.152200	622.109605	13.609754
16.123280	633.792895	13.614771
16.203970	639.712688	13.619789
16.584815	638.229247	13.624807
16.108056	638.451508	13.629824
16.428140	618.743316	13.634842
15.532285	617.342154	13.639859
16.269185	628.285673	13.644877
16.483668	632.402306	13.649895
16.010297	639.638580	13.654912
16.446549	638.277060	13.659930
16.323959	647.073667	13.664947
16.703092	631.401919	13.669965
16.674577	634.798202	13.674983
16.540703	640.393701	13.680000
16.576926	637.766210	13.685018
16.520697	629.449226	13.690035
16.447452	618.144286	13.695053
16.329218	609.952533	13.700071
16.673630	632.023414	13.705088
16.571229	617.742365	13.710106
16.397554	619.548993	13.715123
16.529290	615.576630	13.720141
16.576337	620.046558	13.725159
16.308018	615.966039	13.730176
16.472274	621.061797	13.735194
16.538538	629.179522	13.740211
16.572310	632.025757	13.745229
16.872113	632.498148	13.750247
16.669265	633.431310	13.755264
16.376679	633.194357	13.760282
16.694605	633.540920	13.765299
16.336297	630.907503	13.770317
16.733777	627.555665	13.775335
16.466888	637.612313	13.780352
16.969645	635.383528	13.785370
16.785856	629.176921	13.790387
16.975486	634.348006	13.795405
16.722802	630.393627	13.800423
16.502865	630.526120	13.805440
16.596245	633.043998	13.810458
16.405489	631.319399	13.815475
16.658768	639.468757	13.820493
17.020587	627.975241	13.825511
16.472782	629.869803	13.830528
17.040140	626.781551	13.835546
16.799736	628.995270	13.840563
17.118020	631.037743	13.845581
16.771793	624.002964	13.850599
16.827667	632.679860	13.855616
17.272343	633.743190	13.860634
17.221334	635.738945	13.865651
16.985436	622.651979	13.870669
16.725707	630.971314	13.875687
16.867343	634.055973	13.880704
16.785424	631.898021	13.885722
17.101046	629.341583	13.890739
16.959498	638.571223	13.895757
17.058624	648.685375	13.900775
16.921310	656.455741	13.905792
17.373210	649.929703	13.910810
17.164349	663.648214	13.915827
17.152290	659.533912	13.920845
17.294659	660.870518	13.925863
17.118263	658.485699	13.930880
17.388399	651.165786	13.935898
17.098361	656.495433	13.940915
17.478676	660.612960	13.945933
17.389677	647.283551	13.950951
16.956425	639.282914	13.955968
17.385747	641.552657	13.960986
17.493519	644.801579	13.966003
17.143236	649.506195	13.971021
17.283774	648.980999	13.976039
17.333371	653.583577	13.981056
17.814292	656.793547	13.986074
17.753469	642.328829	13.991091
17.112576	625.428033	13.996109
17.332328	627.955298	14.001127
17.129458	642.187731	14.006144
17.565730	647.353804	14.011162
17.366810	657.358267	14.016179
17.135553	661.535725	14.021197
17.519454	654.465856	14.026215
17.526953	654.923661	14.031232
17.276338	652.787734	14.036250
17.435683	656.534391	14.041267
17.477514	657.238072	14.046285
17.781424	654.688294	14.051303
17.542257	661.579120	14.056320
17.849564	644.932296	14.061338
17.991041	656.731475	14.066355
17.376603	661.121586	14.071373
17.538655	653.095592	14.076391
17.500473	654.036526	14.081408
17.315841	661.093903	14.086426
17.701190	657.744461	14.091443
17.682824	656.312162	14.096461
17.907540	652.918063	14.101479
17.645501	653.546478	14.106496
17.755640	654.806534	14.111514
17.685820	659.089142	14.116531
17.729366	661.512133	14.121549
17.864826	650.939893	14.126567
17.932332	661.653352	14.131584
17.751382	659.773984	14.136602
17.922515	667.399193	14.141619
17.807403	685.161827	14.146637
17.894128	694.248194	14.151655
17.961619	687.721229	14.156672
18.078001	687.035080	14.161690
18.219274	677.087418	14.166707
18.180591	681.343617	14.171725
18.193970	660.584247	14.176743
17.824572	655.888993	14.181760
18.120326	652.750046	14.186778
18.191845	649.072670	14.191795
17.958225	645.959180	14.196813
17.909704	648.179709	14.201831
17.742792	656.519906	14.206848
17.873381	667.233553	14.211866
18.308917	670.162079	14.216883
18.377872	682.835052	14.221901
18.416091	679.261996	14.226919
18.347885	685.576128	14.231936
18.181993	683.098232	14.236954
18.286891	673.440439	14.241971
18.228127	679.032176	14.246989
18.525044	683.244617	14.252007
18.100470	670.880943	14.257024
18.481698	675.217208	14.262042
18.470380	667.741147	14.267059
18.070699	666.092081	14.272077
18.255741	670.224622	14.277095
18.258272	687.319782	14.282112
18.080348	688.207877	14.287130
18.472241	681.819708	14.292147
18.221387	684.998107	14.297165
18.560621	682.154301	14.302183
18.254322	691.341571	14.307200
18.036035	684.656820	14.312218
18.347519	685.336718	14.317235
18.075680	688.344979	14.322253
18.208872	674.016994	14.327271
18.399209	693.942724	14.332288
18.380580	705.216510	14.337306
18.993724	716.039647	14.342323
18.854492	703.697199	14.347341
18.813526	691.912869	14.352359
18.593787	682.951311	14.357376
18.152286	676.414936	14.362394
18.729139	694.432274	14.367411
18.775100	706.942547	14.372429
18.702189	705.997598	14.377447
18.599459	711.554504	14.382464
18.786589	712.043980	14.387482
18.959674	703.126415	14.392499
18.719795	715.569465	14.397517
19.034480	711.562060	14.402535
18.906918	705.831127	14.407552
19.035445	709.602583	14.412570
18.939164	700.111543	14.417587
18.660368	700.071902	14.422605
18.915753	702.477931	14.427623
18.539960	704.592825	14.432640
19.165181	703.352364	14.437658
19.166245	700.773201	14.442675
19.128163	705.717068	14.447693
18.926897	707.765664	14.452711
19.133433	704.267483	14.457728
19.298828	704.764102	14.462746
19.110254	696.053663	14.467763
18.843133	674.328568	14.472781
19.042962	685.787809	14.477799
19.251014	702.528892	14.482816
19.293768	692.086142	14.487834
19.239078	675.042164	14.492851
18.631311	677.310814	14.497869
19.089421	690.952765	14.502887
19.574782	689.839395	14.507904
19.268370	704.948435	14.512922
19.472655	701.026239	14.517939
19.047769	696.164185	14.522957
19.096173	694.263370	14.527975
19.348671	703.122304	14.532992
19.195537	705.608576	14.538010
19.629352	705.074184	14.543027
19.065742	703.572331	14.548045
19.070405	699.534379	14.553063
19.405633	705.960448	14.558080
19.192562	705.594978	14.563098
19.375418	713.840284	14.568115
18.958928	705.529372	14.573133
19.283153	707.526386	14.578151
19.441853	708.097338	14.583168
19.163973	705.550978	14.588186
19.472416	697.575127	14.593203
19.183112	707.861505	14.598221
19.337706	698.830080	14.603239
19.568687	713.119472	14.608256
19.297319	731.873340	14.613274
19.529887	727.614187	14.618291
19.399542	733.292202	14.623309
19.622653	736.170094	14.628327
19.823592	731.083935	14.633344
19.528314	738.113213	14.638362
19.591167	727.586013	14.643379
19.770578	736.255896	14.648397
19.955445	733.624641	14.653415
19.746484	730.547993	14.658432
19.563110	736.015116	14.663450
19.910552	724.895151	14.668467
19.915226	728.672160	14.673485
19.586786	726.647924	14.678503
19.823092	722.160212	14.683520
19.776121	730.662076	14.688538
19.937071	727.345839	14.693555
19.700638	726.093337	14.698573
19.932522	725.749066	14.703591
20.381761	732.058241	14.708608
20.079963	728.825320	14.713626
19.960418	728.688446	14.718643
19.949135	730.270569	14.723661
19.868476	725.561732	14.728679
19.768578	729.542662	14.733696
20.103490	727.978241	14.738714
20.181118	727.192213	14.743731
19.731225	724.893220	14.748749
19.887180	730.902549	14.753767
20.023473	726.583358	14.758784
19.790305	730.773355	14.763802
20.721294	729.787365	14.768819
20.144526	728.075887	14.773837
20.065441	727.533514	14.778855
20.227218	727.919321	14.783872
20.162904	735.527254	14.788890
20.382590	738.001008	14.793907
20.435701	743.033718	14.798925
20.436711	738.137741	14.803943
20.245065	723.850113	14.808960
20.210594	732.593204	14.813978
20.513159	728.892905	14.818995
20.591353	738.118893	14.824013
20.460797	730.688922	14.829031
20.752139	725.131913	14.834048
20.151600	725.870708	14.839066
20.470172	719.814334	14.844083
20.317870	721.676879	14.849101
20.378133	727.862281	14.854119
20.405830	723.769724	14.859136
20.213679	743.812786	14.864154
20.680511	742.807594	14.869171
20.562058	758.757962	14.874189
20.536033	764.613981	14.879207
20.691028	762.328990	14.884224
20.449496	767.522303	14.889242
20.715628	762.121809	14.894259
20.597522	756.926667	14.899277
20.528180	759.204988	14.904295
20.781450	765.139952	14.909312
20.271441	762.496593	14.914330
20.922209	759.799997	14.919347
20.768713	762.513493	14.924365
20.824835	760.427543	14.929383
21.071601	762.949570	14.934400
20.768568	756.311890	14.939418
20.830746	754.960730	14.944435
20.783600	758.453427	14.949453
20.355454	761.084060	14.954471
20.938360	750.921104	14.959488
20.414711	757.755540	14.964506
20.779414	756.607817	14.969523
20.823059	771.827847	14.974541
20.888266	784.588133	14.979559
20.888043	781.080472	14.984576
21.382767	786.408560	14.989594
21.372878	785.718119	14.994611
21.184752	787.194890	14.999629
21.082882	784.411902	15.004647
21.400212	784.235363	15.009664
20.827927	772.850353	15.014682
20.991884	767.056953	15.019699
20.879247	786.503074	15.024717
21.126534	784.880325	15.029735
21.377415	786.283616	15.034752
21.026065	784.122620	15.039770
21.309451	785.187079	15.044787
21.319298	785.761817	15.049805
21.231018	783.647020	15.054823
21.204678	771.439361	15.059840
20.961872	785.275800	15.064858
20.847797	778.449349	15.069875
20.906548	784.367712	15.074893
21.082369	798.320269	15.079911
21.823643	801.074973	15.084928
21.413187	804.232188	15.089946
21.727751	797.857957	15.094963
21.755342	789.609681	15.099981
21.533712	783.667533	15.104999
21.470275	776.678768	15.110016
21.558232	779.904622	15.115034
21.355129	786.490727	15.120051
21.679044	787.685870	15.125069
21.695539	801.366006	15.130087
21.901550	794.511742	15.135104
21.549471	787.539666	15.140122
21.942387	790.321343	15.145139
21.991935	776.138998	15.150157
21.526366	775.527555	15.155175
22.020012	768.904008	15.160192
21.661832	769.577084	15.165210
21.480200	778.315042	15.170227
21.758201	776.511232	15.175245
21.724230	795.685295	15.180263
22.326989	789.496014	15.185280
21.960228	792.140109	15.190298
21.664414	775.680017	15.195315
21.626280	779.263742	15.200333
21.723398	795.941803	15.205351
22.143147	800.106773	15.210368
21.988576	812.279092	15.215386
22.121287	810.353674	15.220403
22.255140	811.012599	15.225421
21.930735	798.072024	15.230439
21.864557	794.757557	15.235456
22.032605	805.622963	15.240474
22.078557	802.483226	15.245491
22.252007	808.201906	15.250509
22.025330	811.504668	15.255527
21.877038	806.969597	15.260544
22.173558	804.759586	15.265562
22.153716	800.607954	15.270579
22.339647	803.720351	15.275597
22.259643	799.775129	15.280615
22.363135	794.488165	15.285632
22.286311	810.179735	15.290650
22.512123	805.772868	15.295667
22.374677	803.346933	15.300685
22.258268	807.567220	15.305703
22.264593	805.647376	15.310720
22.251713	805.172775	15.315738
22.079411	797.696537	15.320755
21.957497	800.029630	15.325773
22.218563	805.983396	15.330791
22.239478	798.419655	15.335808
22.412417	798.839834	15.340826
22.304464	819.178881	15.345843
22.697861	822.034497	15.350861
22.654080	833.375531	15.355879
22.480648	825.213275	15.360896
22.732615	825.773513	15.365914
22.634942	828.938387	15.370931
22.602796	818.974469	15.375949
22.612403	822.790447	15.380967
22.905365	825.174920	15.385984
22.793175	820.764176	15.391002
22.941500	825.870514	15.396019
23.061916	809.967815	15.401037
22.794333	810.671165	15.406055
22.856647	804.637506	15.411072
22.910457	799.661904	15.416090
22.605722	811.102822	15.421107
22.823802	815.694872	15.426125
22.743267	822.624067	15.431143
22.831713	815.677848	15.436160
22.686411	821.317823	15.441178
22.924538	822.548827	15.446195
23.286681	825.608429	15.451213
22.926894	829.031657	15.456231
23.134042	826.691566	15.461248
23.071441	825.627191	15.466266
22.846759	823.188139	15.471283
23.185511	819.809372	15.476301
23.225892	814.561197	15.481319
23.350411	817.695970	15.486336
23.054256	827.163911	15.491354
23.255549	818.990789	15.496371
23.447943	812.311600	15.501389
22.897792	817.570598	15.506407
23.341632	824.879087	15.511424
23.115594	821.456444	15.516442
22.668566	824.235483	15.521459
23.011617	812.903593	15.526477
23.109436	827.562763	15.531495
23.363143	824.048477	15.536512
23.452133	829.067795	15.541530
23.459260	835.362821	15.546547
23.621463	825.037205	15.551565
23.627490	827.405807	15.556583
23.365659	811.241218	15.561600
23.601425	812.213962	15.566618
23.070841	823.789132	15.571635
23.994569	820.882769	15.576653
23.649692	816.098763	15.581671
23.457179	816.705041	15.586688
23.542718	820.239953	15.591706
23.597517	835.023964	15.596723
23.999427	836.973488	15.601741
23.767989	836.616568	15.606759
23.611616	819.229834	15.611776
23.659381	825.331127	15.616794
23.619059	837.663675	15.621811
23.496869	841.212517	15.626829
23.511992	839.069568	15.631847
23.841857	848.358669	15.636864
23.868066	844.763156	15.641882
23.832644	846.474872	15.646899
23.885352	845.407938	15.651917
23.662827	849.608014	15.656935
23.571667	846.580338	15.661952
23.678192	842.932551	15.666970
23.605415	847.857013	15.671987
23.885355	847.595724	15.677005
23.867771	857.925393	15.682023
24.236985	867.217439	15.687040
24.314259	868.248712	15.692058
23.897851	870.344370	15.697075
24.091245	861.991832	15.702093
24.471347	868.373926	15.707111
24.385965	861.226558	15.712128
24.634876	845.482853	15.717146
24.341514	849.596238	15.722163
24.319814	841.227361	15.727181
24.392796	843.648262	15.732199
24.299134	835.939702	15.737216
24.146888	840.429307	15.742234
24.312671	839.066495	15.747251
24.432506	833.476038	15.752269
23.911824	850.663131	15.757287
24.327942	853.785059	15.762304
24.329763	852.934809	15.767322
24.388147	863.566851	15.772339
24.708320	860.210048	15.777357
24.627157	859.458575	15.782375
24.591861	875.204749	15.787392
24.891964	866.933747	15.792410
24.318108	865.424519	15.797427
24.778066	863.182319	15.802445
24.647014	871.843847	15.807463
24.792571	865.163335	15.812480
24.744697	845.941750	15.817498
24.464145	851.744676	15.822515
24.831683	852.708989	15.827533
24.831987	868.863025	15.832551
24.680705	867.897186	15.837568
24.755452	864.606611	15.842586
24.610321	870.464283	15.847603
24.718906	870.410100	15.852621
24.652148	868.610613	15.857639
24.731422	871.248185	15.862656
24.944149	862.856226	15.867674
24.462495	867.101577	15.872691
24.840228	859.652337	15.877709
24.791341	877.130221	15.882727
24.747399	863.779386	15.887744
24.774409	870.477810	15.892762
24.795048	884.593143	15.897779
25.040574	888.045676	15.902797
25.121066	902.104265	15.907815
25.149585	907.317473	15.912832
25.466802	899.810915	15.917850
25.190045	900.182729	15.922867
25.338048	889.475578	15.927885
25.007914	886.326053	15.932903
25.326387	902.011707	15.937920
25.269037	894.428990	15.942938
25.214448	904.402627	15.947955
25.280296	905.644842	15.952973
25.318893	900.702828	15.957991
25.446600	908.599116	15.963008
25.591969	903.483127	15.968026
25.489337	904.888668	15.973043
25.916248	904.929014	15.978061
25.564855	888.753191	15.983079
25.074019	877.336506	15.988096
25.078627	889.686852	15.993114
25.235701	906.477147	15.998131
25.606468	896.476777	16.003149
25.439135	896.491510	16.008167
25.389460	905.413587	16.013184
25.690656	911.472162	16.018202
25.392389	912.145559	16.023219
25.765613	902.420753	16.028237
25.595251	903.347764	16.033255
25.669270	911.231290	16.038272
25.709245	902.122667	16.043290
25.666398	903.256902	16.048307
25.774724	905.354255	16.053325
25.458965	902.479895	16.058343
25.877158	924.202376	16.063360
26.301660	925.816686	16.068378
25.913823	922.018858	16.073395
25.899620	921.150392	16.078413
26.044833	916.591491	16.083431
26.034117	925.624840	16.088448
26.382408	922.669260	16.093466
25.887803	911.205932	16.098483
26.059990	911.173107	16.103501
26.135479	911.872801	16.108519
26.219522	917.996470	16.113536
26.423399	921.576374	16.118554
26.236912	910.650195	16.123571
26.277206	891.468676	16.128589
26.181541	893.666339	16.133607
26.014111	895.586133	16.138624
26.417913	902.349735	16.143642
26.269262	911.941723	16.148659
26.355583	917.969348	16.153677
26.422338	912.882121	16.158695
26.478565	911.918532	16.163712
26.658837	912.262306	16.168730
26.510591	904.935571	16.173747
26.334515	898.695295	16.178765
26.544820	905.324015	16.183783
26.451366	918.237057	16.188800
26.728902	910.595731	16.193818
26.584445	911.913319	16.198835
26.536469	904.993193	16.203853
26.693543	903.242069	16.208871
26.476571	908.615213	16.213888
26.892551	914.832337	16.218906
26.462658	916.410173	16.223923
26.543101	912.321824	16.228941
26.610013	915.309075	16.233959
26.245536	915.278108	16.238976
26.480117	909.901291	16.243994
26.894201	914.036129	16.249011
26.627393	914.195674	16.254029
26.654152	925.111725	16.259047
26.611578	921.676003	16.264064
26.791729	916.928253	16.269082
26.426244	923.059037	16.274099
26.907812	928.843667	16.279117
26.873206	938.110106	16.284135
26.662027	950.049789	16.289152
26.949107	934.822491	16.294170
27.064243	942.107514	16.299187
27.134538	943.165538	16.304205
27.130728	946.531421	16.309223
27.141164	944.937246	16.314240
27.370367	931.565532	16.319258
26.878815	936.253076	16.324275
27.212389	939.933158	16.329293
27.684397	940.385314	16.334311
27.357477	940.350490	16.339328
27.381298	932.541722	16.344346
27.654333	939.554544	16.349363
27.663075	937.648457	16.354381
27.659859	932.282662	16.359399
27.646049	939.131571	16.364416
27.827720	929.366028	16.369434
27.656468	910.219515	16.374451
27.334439	898.298502	16.379469
27.462378	913.519674	16.384487
27.469739	934.805885	16.389504
27.493333	924.303554	16.394522
27.503352	927.976188	16.399539
27.705486	934.040546	16.404557
27.768974	935.503226	16.409575
27.462176	933.912370	16.414592
27.561984	929.415312	16.419610
27.541246	937.651144	16.424627
27.500634	934.118248	16.429645
27.386027	922.655373	16.434663
27.525262	938.025481	16.439680
27.788991	931.804490	16.444698
27.885083	925.905737	16.449715
27.733299	926.655663	16.454733
27.940757	938.080759	16.459751
28.047246	958.468336	16.464768
27.919301	955.065640	16.469786
28.125453	952.806008	16.474803
28.042428	955.031112	16.479821
28.244358	949.577014	16.484839
28.128470	960.035624	16.489856
28.361643	956.315661	16.494874
28.442956	938.443782	16.499891
28.022101	934.793933	16.504909
28.208250	934.228500	16.509927
28.077391	948.188668	16.514944
28.111890	950.255734	16.519962
28.121781	956.520038	16.524979
28.252109	952.937574	16.529997
28.616158	948.810522	16.535015
28.200961	960.562743	16.540032
28.268200	955.702580	16.545050
28.309793	951.817497	16.550067
28.169434	950.599459	16.555085
28.544622	962.203878	16.560103
27.997586	963.357825	16.565120
28.340482	945.243812	16.570138
28.404156	955.696308	16.575155
28.406810	960.457139	16.580173
28.579963	951.130379	16.585191
28.500051	956.791464	16.590208
28.620570	970.149024	16.595226
28.562144	982.418151	16.600243
28.493878	987.697410	16.605261
29.002790	982.110976	16.610279
29.007815	984.399456	16.615296
28.995038	982.010722	16.620314
29.014743	979.478424	16.625331
28.678273	979.044407	16.630349
29.015180	977.679231	16.635367
29.079889	978.091354	16.640384
29.017333	973.440466	16.645402
29.273505	977.075502	16.650419
28.629181	962.109090	16.655437
29.192950	966.756934	16.660455
29.003781	968.361449	16.665472
28.789980	975.158453	16.670490
29.226612	974.710593	16.675507
29.302324	974.916176	16.680525
29.297962	967.289216	16.685543
29.306615	979.424798	16.690560
29.338097	973.436729	16.695578
29.265316	978.682088	16.700595
29.372309	972.413414	16.705613
29.381814	968.552931	16.710631
29.520700	976.140326	16.715648
29.192418	971.450764	16.720666
29.493080	965.700400	16.725683
29.532417	967.152121	16.730701
29.308215	970.045859	16.735719
29.501015	976.509798	16.740736
29.510345	969.076627	16.745754
29.590436	969.042123	16.750771
29.427475	967.702239	16.755789
29.802825	968.034579	16.760807
29.463844	976.358166	16.765824
29.592587	970.861063	16.770842
29.793390	973.032087	16.775859
29.594061	972.286001	16.780877
29.618136	968.729000	16.785895
29.910578	967.123559	16.790912
29.709913	969.999620	16.795930
29.620652	978.156272	16.800947
29.362153	973.392558	16.805965
29.552101	968.832140	16.810983
29.731524	972.067298	16.816000
29.743550	978.611957	16.821018
29.884205	976.327341	16.826035
29.789401	988.887133	16.831053
29.960949	981.994007	16.836071
30.417926	987.329203	16.841088
29.915426	990.049348	16.846106
30.280317	983.532067	16.851123
29.795967	988.324336	16.856141
30.104696	979.464070	16.861159
30.030512	990.193345	16.866176
30.014704	987.441343	16.871194
30.215527	979.031608	16.876211
30.033960	990.535725	16.881229
30.378861	1005.036045	16.886247
30.442913	1011.400454	16.891264
30.608755	1014.912272	16.896282
30.698735	987.106532	16.901299
30.347336	991.863008	16.906317
30.380921	980.290122	16.911335
30.585731	989.019326	16.916352
30.764845	996.239452	16.921370
30.584113	976.906243	16.926387
30.353085	994.296706	16.931405
30.651241	986.592481	16.936423
30.811987	1002.942130	16.941440
30.691298	1009.322562	16.946458
30.911835	1009.568337	16.951475
30.670418	1001.777863	16.956493
30.753179	1000.255956	16.961511
30.819794	1010.728473	16.966528
31.140667	1009.368312	16.971546
31.163359	998.154686	16.976563
30.764258	987.908912	16.981581
30.684697	981.847890	16.986599
31.000404	996.465631	16.991616
31.270755	1002.438802	16.996634
31.191888	995.484775	17.001651
30.868522	987.977554	17.006669
31.193915	992.236151	17.011687
31.182712	1003.446329	17.016704
31.137670	1002.308563	17.021722
31.491552	1009.918642	17.026739
31.337323	1000.941328	17.031757
31.001391	983.379423	17.036775
31.189916	986.411903	17.041792
30.809452	1005.792807	17.046810
31.318140	1005.353093	17.051827
30.978038	1016.168935	17.056845
31.066155	1011.167112	17.061863
31.339064	1013.425018	17.066880
31.069722	1014.057411	17.071898
31.277207	1001.149455	17.076915
31.444529	1009.774646	17.081933
31.438360	1020.711176	17.086951
31.662464	1035.214204	17.091968
31.819384	1035.463032	17.096986
31.945132	1033.388350	17.102003
31.809248	1021.550196	17.107021
31.502629	1007.047886	17.112039
31.500589	1013.807086	17.117056
31.313847	1024.038896	17.122074
31.676879	1024.340207	17.127091
31.824912	1033.736692	17.132109
31.790771	1031.427863	17.137127
32.039420	1031.601268	17.142144
31.891264	1020.934010	17.147162
32.285938	1027.802720	17.152179
31.864392	1025.505284	17.157197
32.345980	1018.814340	17.162215
32.418135	1028.727702	17.167232
32.200865	1021.431630	17.172250
32.259297	1017.130369	17.177267
32.179815	1021.818602	17.182285
32.251445	1019.738316	17.187303
32.503637	1019.659567	17.192320
32.083265	1023.414512	17.197338
32.476903	1018.747126	17.202355
32.342288	1028.482526	17.207373
32.362701	1032.073151	17.212391
32.714802	1021.284477	17.217408
32.167428	1013.658828	17.222426
32.707987	1014.327976	17.227443
32.543565	1006.566088	17.232461
32.375529	995.806078	17.237479
32.156459	996.034883	17.242496
31.991125	1013.152686	17.247514
32.242679	1009.244240	17.252531
32.385586	1018.577000	17.257549
32.156668	1023.175807	17.262567
32.582739	1026.913034	17.267584
32.139156	1029.549809	17.272602
32.510669	1028.831636	17.277619
32.506915	1051.934756	17.282637
32.939077	1057.153617	17.287655
32.809488	1050.642203	17.292672
32.622334	1060.377268	17.297690
33.178991	1060.476840	17.302707
33.189387	1053.188330	17.307725
32.981114	1058.315997	17.312743
33.091995	1050.473857	17.317760
33.044129	1046.261054	17.322778
33.049702	1046.440063	17.327795
33.405923	1054.508425	17.332813
33.261016	1049.786900	17.337831
33.543173	1044.590343	17.342848
33.403826	1046.949193	17.347866
33.170352	1026.479018	17.352883
33.215818	1029.674167	17.357901
33.252437	1040.999284	17.362919
33.517151	1037.616196	17.367936
33.173928	1040.846180	17.372954
33.519792	1039.031105	17.377971
33.184556	1038.952382	17.382989
33.076418	1045.496101	17.388007
33.365940	1048.163848	17.393024
32.800517	1049.978306	17.398042
33.137819	1044.190745	17.403059
33.271556	1045.518184	17.408077
33.493084	1056.575695	17.413095
33.732185	1064.666211	17.418112
33.454607	1072.176553	17.423130
33.768325	1073.192312	17.428147
33.639683	1077.393045	17.433165
33.881518	1071.110665	17.438183
33.927619	1069.188533	17.443200
33.771015	1067.161387	17.448218
34.043489	1064.010072	17.453235
33.972095	1067.471422	17.458253
34.207838	1070.579956	17.463271
34.697095	1064.428260	17.468288
33.912257	1070.349412	17.473306
34.261300	1058.765571	17.478323
34.307724	1048.201110	17.483341
33.963381	1049.768731	17.488359
34.026854	1044.863101	17.493376
34.009693	1062.863486	17.498394
34.345051	1057.148287	17.503411
34.260021	1064.325571	17.508429
34.048998	1070.100924	17.513447
34.384629	1056.619357	17.518464
33.906583	1059.514592	17.523482
34.174957	1054.104179	17.528499
34.263259	1061.292130	17.533517
33.837286	1070.809666	17.538535
34.243460	1061.540316	17.543552
34.398752	1074.969372	17.548570
34.715144	1081.366042	17.553587
34.948568	1088.310296	17.558605
34.713696	1078.427022	17.563623
34.774939	1056.119472	17.568640
34.733849	1056.185740	17.573658
34.777499	1047.586645	17.578675
34.411531	1055.063585	17.583693
34.348646	1065.933556	17.588711
34.593592	1073.641230	17.593728
34.746002	1083.763773	17.598746
34.796721	1086.514375	17.603763
35.008558	1083.326248	17.608781
34.797120	1082.055403	17.613799
34.953596	1074.348611	17.618816
35.030062	1086.523834	17.623834
34.897455	1079.466466	17.628851
35.116466	1080.593573	17.633869
34.879515	1085.050031	17.638887
35.401885	1083.400602	17.643904
35.085897	1078.928650	17.648922
35.141840	1073.922685	17.653939
35.300894	1086.767680	17.658957
35.130751	1071.684457	17.663975
35.151150	1083.767390	17.668992
35.067512	1082.761203	17.674010
35.413267	1091.187214	17.679027
35.522639	1100.821238	17.684045
35.107807	1112.636503	17.689063
35.628737	1103.098921	17.694080
35.204654	1109.267039	17.699098
35.419436	1104.175317	17.704115
35.820017	1102.585814	17.709133
35.383203	1103.747108	17.714151
35.884307	1095.635613	17.719168
35.789937	1101.936530	17.724186
35.998063	1094.621166	17.729203
36.145791	1100.490667	17.734221
35.940037	1102.115264	17.739239
36.184533	1090.367612	17.744256
36.247864	1087.916654	17.749274
36.375513	1098.791319	17.754291
35.895304	1073.624655	17.759309
35.759072	1081.811579	17.764327
36.231583	1080.098360	17.769344
36.181585	1089.344604	17.774362
35.916663	1095.736356	17.779379
36.031583	1098.242870	17.784397
35.787615	1097.664401	17.789415
36.330031	1095.058132	17.794432
35.988099	1096.962751	17.799450
36.193726	1095.672058	17.804467
36.107280	1085.172092	17.809485
36.416650	1092.622657	17.814503
36.393562	1093.865835	17.819520
36.037987	1087.028842	17.824538
36.075214	1087.203399	17.829555
36.186802	1109.306035	17.834573
36.507022	1121.257464	17.839591
37.151012	1119.014678	17.844608
36.975790	1128.566712	17.849626
36.554249	1097.150283	17.854643
36.634194	1092.706466	17.859661
36.380082	1102.219974	17.864679
36.640278	1106.648055	17.869696
36.657961	1119.810967	17.874714
36.750182	1124.899923	17.879731
36.966115	1125.578342	17.884749
36.896208	1120.871541	17.889767
37.133369	1115.442653	17.894784
36.871580	1116.285998	17.899802
36.771836	1121.617364	17.904819
37.098734	1114.182326	17.909837
37.046100	1127.262007	17.914855
37.148444	1116.054398	17.919872
37.007122	1117.245503	17.924890
36.943239	1123.231546	17.929907
36.962015	1118.911627	17.934925
36.942921	1113.943664	17.939943
37.007024	1113.200801	17.944960
36.989754	1120.175950	17.949978
37.498428	1135.290205	17.954995
37.856607	1126.500013	17.960013
37.678809	1127.646373	17.965031
37.531834	1121.255128	17.970048
37.531960	1112.742336	17.975066
37.813007	1109.559672	17.980083
37.753960	1095.909963	17.985101
37.497436	1104.599876	17.990119
37.589382	1100.834761	17.995136
37.452863	1104.658469	18.000154
37.777014	1111.935735	18.005171
38.007309	1112.756653	18.010189
37.349673	1121.106703	18.015207
37.917330	1117.989964	18.020224
38.451946	1130.249199	18.025242
38.097701	1123.948178	18.030259
38.145545	1103.720288	18.035277
38.110332	1107.829184	18.040295
38.075745	1094.524236	18.045312
38.121854	1106.499389	18.050330
38.008147	1104.532455	18.055347
38.039591	1093.327940	18.060365
38.230081	1108.900356	18.065383
38.279346	1101.546728	18.070400
38.469380	1115.412575	18.075418
37.990067	1105.185121	18.080435
38.187719	1098.077390	18.085453
37.961776	1117.179311	18.090471
38.354135	1107.914977	18.095488
38.282905	1121.356779	18.100506
38.178843	1124.437340	18.105523
38.380326	1112.485381	18.110541
38.463588	1117.082524	18.115559
38.448880	1125.291474	18.120576
38.462625	1121.081440	18.125594
38.206340	1125.731658	18.130611
38.519511	1139.737370	18.135629
38.557498	1155.545316	18.140647
38.885791	1149.997392	18.145664
39.390360	1150.398103	18.150682
39.300610	1141.705692	18.155699
39.116821	1134.981175	18.160717
39.024886	1128.159957	18.165735
39.134062	1113.955618	18.170752
38.968616	1110.452406	18.175770
38.864155	1113.978296	18.180787
39.193617	1110.176607	18.185805
38.880152	1134.641336	18.190823
39.200749	1130.363562	18.195840
39.346822	1140.503727	18.200858
39.154696	1142.094970	18.205875
39.149151	1136.579887	18.210893
39.092356	1145.893036	18.215911
39.301460	1134.064600	18.220928
39.474498	1141.554299	18.225946
39.265523	1132.706441	18.230963
39.628391	1144.471698	18.235981
39.504764	1135.633328	18.240999
39.599428	1138.462094	18.246016
39.394684	1135.033886	18.251034
39.436221	1136.352585	18.256051
39.495668	1138.189173	18.261069
39.514541	1132.124392	18.266087
39.459617	1139.242002	18.271104
39.650425	1148.101565	18.276122
39.449501	1151.513124	18.281139
39.887984	1152.937354	18.286157
39.993408	1156.407241	18.291175
39.805435	1162.416208	18.296192
40.076490	1157.433652	18.301210
39.619928	1157.007702	18.306227
39.933816	1162.098943	18.311245
39.874060	1162.469476	18.316263
40.062731	1158.262750	18.321280
40.281250	1158.867122	18.326298
39.898932	1167.280268	18.331315
40.099472	1156.759110	18.336333
39.896050	1161.876954	18.341351
39.855958	1182.649327	18.346368
40.280232	1187.378998	18.351386
40.455538	1193.192001	18.356403
40.513083	1188.798715	18.361421
40.723681	1190.055961	18.366439
40.437922	1187.564366	18.371456
40.787595	1184.477016	18.376474
40.957326	1183.869805	18.381491
40.997335	1182.068744	18.386509
40.785354	1184.328620	18.391527
40.876452	1181.530537	18.396544
40.868553	1184.378655	18.401562
40.527396	1187.653602	18.406579
40.976428	1183.807294	18.411597
40.663984	1184.820837	18.416615
40.829970	1176.940376	18.421632
40.690266	1186.703489	18.426650
40.397400	1186.827981	18.431667
40.574105	1185.886158	18.436685
40.791378	1186.619475	18.441703
41.132773	1210.462122	18.446720
41.145261	1210.875812	18.451738
41.225295	1214.131809	18.456755
41.280503	1207.046040	18.461773
41.242602	1218.743463	18.466791
41.293810	1206.208058	18.471808
41.518023	1204.741841	18.476826
41.525924	1209.066849	18.481843
41.770311	1205.807954	18.486861
41.699797	1213.206521	18.491879
41.798391	1211.201272	18.496896
41.945113	1198.460691	18.501914
41.593844	1210.499360	18.506931
41.797862	1209.099478	18.511949
41.660866	1210.123341	18.516967
41.471756	1206.981106	18.521984
41.714501	1201.734331	18.527002
41.659313	1204.935947	18.532019
41.913074	1204.898670	18.537037
42.033716	1204.337775	18.542055
41.535501	1206.587176	18.547072
41.686663	1199.588276	18.552090
41.726785	1208.326370	18.557107
41.659645	1201.819906	18.562125
41.969442	1221.747010	18.567143
42.027077	1224.892941	18.572160
42.247317	1229.766250	18.577178
42.349477	1236.426406	18.582195
42.584352	1235.433217	18.587213
42.350010	1227.607599	18.592231
42.541024	1221.932777	18.597248
43.007251	1214.742727	18.602266
42.569153	1212.225566	18.607283
42.667883	1187.475837	18.612301
42.541401	1195.428928	18.617319
42.268093	1193.091173	18.622336
42.294078	1190.477881	18.627354
42.470278	1210.765669	18.632371
42.902540	1207.078428	18.637389
42.766145	1216.622907	18.642407
42.819408	1227.991074	18.647424
43.118247	1221.521639	18.652442
42.770511	1226.126400	18.657459
42.993501	1210.528741	18.662477
42.964535	1213.644128	18.667495
42.696547	1222.427736	18.672512
43.073084	1208.857376	18.677530
42.922204	1224.681704	18.682547
43.069979	1221.056920	18.687565
43.220770	1228.368852	18.692583
43.152323	1221.125601	18.697600
43.351575	1214.319909	18.702618
43.284316	1221.421489	18.707635
43.353658	1212.264121	18.712653
43.358613	1214.659338	18.717671
42.982515	1222.269922	18.722688
43.149024	1218.556212	18.727706
43.141078	1227.069603	18.732723
43.362978	1233.426078	18.737741
43.307185	1243.137932	18.742759
43.468434	1249.472173	18.747776
43.686459	1254.507665	18.752794
43.555821	1252.770284	18.757811
43.432090	1245.683811	18.762829
43.650433	1251.836161	18.767847
43.517751	1250.637300	18.772864
43.658277	1250.484129	18.777882
43.873402	1257.516529	18.782899
43.802465	1260.279431	18.787917
44.161533	1264.707723	18.792935
44.011283	1275.579316	18.797952
44.280143	1277.928483	18.802970
44.348810	1277.628157	18.807987
44.731141	1258.961588	18.813005
44.494163	1252.408422	18.818023
44.245599	1245.505215	18.823040
44.334804	1236.147303	18.828058
44.150677	1243.835952	18.833075
44.563663	1252.417453	18.838093
44.938235	1259.254163	18.843111
44.419917	1250.068095	18.848128
44.631986	1234.235216	18.853146
44.317873	1240.325728	18.858163
44.438611	1258.644053	18.863181
44.846025	1263.199771	18.868199
44.830784	1268.698689	18.873216
45.166296	1266.937270	18.878234
44.789449	1265.126877	18.883251
45.100961	1263.441085	18.888269
44.980345	1260.423716	18.893287
44.816025	1271.191337	18.898304
45.063780	1264.275626	18.903322
44.937064	1264.587171	18.908339
45.002345	1254.070627	18.913357
45.174358	1253.690593	18.918375
44.954689	1255.600969	18.923392
45.217518	1256.699576	18.928410
45.459956	1256.720866	18.933427
45.152207	1258.280872	18.938445
45.418398	1256.364793	18.943463
44.919148	1264.483971	18.948480
45.091543	1264.483789	18.953498
45.126162	1259.339959	18.958515
44.842991	1257.873106	18.963533
45.374758	1266.488489	18.968551
45.244037	1272.868328	18.973568
45.570999	1275.910621	18.978586
45.655470	1275.484452	18.983603
45.521090	1280.373582	18.988621
45.839495	1269.843462	18.993639
45.599169	1278.432760	18.998656
45.818600	1277.665744	19.003674
45.908400	1280.675260	19.008691
45.447423	1277.643379	19.013709
46.040321	1282.843185	19.018727
46.105725	1297.879030	19.023744
46.432527	1294.290727	19.028762
46.098302	1284.968251	19.033779
46.013341	1273.328555	19.038797
46.237594	1290.994355	19.043815
46.179833	1299.210526	19.048832
46.589975	1300.437892	19.053850
46.584386	1300.423873	19.058867
46.817938	1298.726577	19.063885
46.525985	1284.661728	19.068903
46.214795	1279.123975	19.073920
46.706873	1292.888790	19.078938
46.696357	1299.540465	19.083955
46.293362	1298.975721	19.088973
46.549185	1299.342822	19.093991
46.588172	1304.046956	19.099008
46.727371	1298.553518	19.104026
47.024674	1299.857834	19.109043
46.877278	1299.368089	19.114061
46.718206	1297.226361	19.119079
46.577296	1299.698105	19.124096
46.657721	1291.654983	19.129114
46.695115	1305.648637	19.134131
46.820846	1319.602086	19.139149
47.018879	1325.040514	19.144167
47.106266	1322.915453	19.149184
47.123965	1324.545986	19.154202
47.477850	1329.324364	19.159219
47.383491	1326.488460	19.164237
47.523874	1318.881848	19.169255
47.516703	1328.459722	19.174272
47.694777	1315.221733	19.179290
47.382308	1320.410439	19.184307
47.609019	1313.731652	19.189325
47.819516	1313.077137	19.194343
47.650827	1311.756675	19.199360
47.331324	1316.252851	19.204378
47.653028	1322.151110	19.209395
47.494068	1324.314038	19.214413
47.968816	1319.900454	19.219431
47.574323	1338.902210	19.224448
47.982646	1341.131839	19.229466
48.178589	1353.735911	19.234483
47.891308	1353.531923	19.239501
48.434404	1334.765810	19.244519
48.382332	1345.072381	19.249536
48.335156	1339.487348	19.254554
48.450227	1335.864410	19.259571
48.368718	1335.458635	19.264589
48.703248	1334.716653	19.269607
48.223809	1329.111466	19.274624
48.514775	1337.463221	19.279642
48.781374	1329.021147	19.284659
48.265830	1333.198217	19.289677
48.481287	1321.352445	19.294695
48.555232	1336.556597	19.299712
48.644010	1333.923829	19.304730
48.602402	1333.331922	19.309747
48.631273	1342.173529	19.314765
48.827052	1334.565218	19.319783
48.775874	1330.566662	19.324800
48.724446	1337.658588	19.329818
48.410178	1328.465063	19.334835
48.534854	1336.345932	19.339853
48.518346	1336.250651	19.344871
48.928684	1353.815633	19.349888
48.977172	1364.268557	19.354906
49.304269	1362.801433	19.359923
48.939206	1371.897652	19.364941
48.821037	1357.975613	19.369959
48.728534	1350.887858	19.374976
49.052413	1369.001026	19.379994
49.499562	1378.434021	19.385011
49.390515	1387.300064	19.390029
49.809340	1383.376821	19.395047
49.910406	1383.547504	19.400064
50.206293	1375.974958	19.405082
49.888145	1358.428184	19.410099
49.803776	1347.967852	19.415117
49.829705	1338.886888	19.420135
49.766700	1346.092938	19.425152
49.805149	1341.544111	19.430170
50.024751	1346.439610	19.435187
49.808519	1375.265745	19.440205
49.836955	1373.258706	19.445223
50.125567	1382.942755	19.450240
49.961013	1378.710599	19.455258
50.526212	1372.506051	19.460275
50.216686	1378.504913	19.465293
50.199105	1374.758261	19.470311
50.116012	1375.793289	19.475328
50.157154	1375.954208	19.480346
50.453078	1373.122963	19.485363
50.141504	1378.386343	19.490381
50.700211	1370.349420	19.495399
50.308649	1374.349674	19.500416
50.266115	1374.359095	19.505434
50.657072	1381.330548	19.510451
50.569203	1394.875735	19.515469
50.899859	1396.971777	19.520487
50.865556	1395.861338	19.525504
51.038381	1396.498483	19.530522
50.760900	1395.666103	19.535539
50.961703	1397.234042	19.540557
51.458789	1396.558449	19.545575
51.264842	1403.126762	19.550592
50.969695	1400.286294	19.555610
51.157391	1398.372566	19.560627
51.112215	1401.266660	19.565645
51.245867	1392.833573	19.570663
50.952640	1398.273841	19.575680
51.327418	1398.265346	19.580698
51.542010	1393.651512	19.585715
51.542633	1392.378204	19.590733
51.579188	1388.299359	19.595751
51.643627	1383.538737	19.600768
51.547758	1388.421918	19.605786
51.991613	1382.872494	19.610803
51.805985	1392.663813	19.615821
51.515615	1386.898560	19.620839
51.285285	1386.404433	19.625856
51.570986	1397.625972	19.630874
51.879958	1417.073154	19.635891
52.123576	1417.239918	19.640909
52.239898	1418.758856	19.645927
52.131139	1426.065433	19.650944
52.288215	1418.113097	19.655962
52.684718	1415.088420	19.660979
52.343307	1410.879633	19.665997
52.371642	1411.422986	19.671015
52.366013	1408.111353	19.676032
52.077300	1415.022919	19.681050
52.760508	1406.362611	19.686067
52.706140	1413.110965	19.691085
52.762961	1413.978735	19.696103
52.816502	1407.504564	19.701120
52.663314	1410.987801	19.706138
53.004302	1406.227839	19.711155
52.502948	1396.560529	19.716173
52.629692	1400.353317	19.721191
52.570563	1401.526503	19.726208
52.684261	1404.463189	19.731226
52.896251	1400.756078	19.736243
53.224702	1411.954801	19.741261
52.983788	1403.354594	19.746279
52.858604	1400.696219	19.751296
52.765184	1406.184903	19.756314
53.394053	1404.401274	19.761331
52.808926	1409.113898	19.766349
53.147706	1412.975518	19.771367
53.407015	1424.062470	19.776384
53.050657	1429.869106	19.781402
53.438727	1428.114323	19.786419
53.393401	1417.326220	19.791437
53.790694	1419.822647	19.796455
53.798760	1418.142989	19.801472
53.683075	1420.116876	19.806490
53.772213	1418.700565	19.811507
53.671999	1427.127769	19.816525
53.662041	1423.821967	19.821543
53.826334	1422.201874	19.826560
53.544289	1434.993030	19.831578
53.931962	1448.068975	19.836595
54.231757	1454.569337	19.841613
54.195973	1451.385916	19.846631
54.191542	1451.854775	19.851648
54.336393	1442.123353	19.856666
54.751490	1442.267630	19.861683
54.427510	1448.731115	19.866701
54.359995	1446.623025	19.871719
54.305430	1437.842732	19.876736
54.212585	1451.891153	19.881754
54.783957	1450.902865	19.886771
54.248578	1447.857284	19.891789
54.700064	1446.741602	19.896807
54.435308	1442.129170	19.901824
54.441124	1444.338454	19.906842
54.844986	1450.154655	19.911859
54.717020	1468.656928	19.916877
54.824764	1465.268637	19.921895
55.248782	1465.807107	19.926912
55.138101	1456.840032	19.931930
55.542733	1469.006889	19.936947
55.475839	1463.077832	19.941965
55.266513	1462.726289	19.946983
55.689807	1460.686142	19.952000
55.401369	1451.026063	19.957018
55.222196	1440.638058	19.962035
55.530970	1440.091675	19.967053
55.429114	1452.604586	19.972071
55.699139	1454.814612	19.977088
55.385683	1467.553122	19.982106
55.599277	1461.099278	19.987123
55.511130	1463.072548	19.992141
55.290298	1467.045343	19.997159
55.607991	1454.103804	20.002176
55.544897	1462.403228	20.007194
55.835049	1463.055201	20.012211
55.805265	1462.769204	20.017229
55.853114	1466.520741	20.022247
55.964806	1475.057767	20.027264
55.910432	1494.763633	20.032282
55.645002	1495.165079	20.037299
55.495670	1493.441395	20.042317
55.701630	1485.605340	20.047335
56.166310	1492.802827	20.052352
56.491681	1513.635211	20.057370
56.861862	1507.501090	20.062387
56.785477	1510.518089	20.067405
56.680421	1520.524101	20.072423
56.738756	1511.264442	20.077440
56.902868	1511.042009	20.082458
56.786049	1507.536954	20.087475
57.079629	1508.113164	20.092493
56.729515	1516.597543	20.097511
57.152354	1500.544061	20.102528
56.968869	1517.150859	20.107546
57.299605	1505.555151	20.112563
57.625989	1513.984603	20.117581
57.131789	1494.096741	20.122599
57.206110	1472.286820	20.127616
56.801549	1479.493187	20.132634
57.338710	1491.824733	20.137651
57.466168	1494.859946	20.142669
57.362889	1497.536907	20.147687
57.704009	1497.707607	20.152704
57.235644	1499.266277	20.157722
57.666503	1491.527627	20.162739
57.566602	1491.484342	20.167757
57.798058	1496.980290	20.172775
57.955100	1493.722412	20.177792
57.713312	1499.864829	20.182810
57.825511	1500.122252	20.187827
57.891656	1493.258951	20.192845
57.814117	1486.832828	20.197863
57.739406	1500.420024	20.202880
57.967483	1520.150809	20.207898
58.071587	1527.876126	20.212915
58.608191	1526.828236	20.217933
57.981514	1533.876523	20.222951
58.129020	1525.563117	20.227968
58.044940	1533.361721	20.232986
58.115208	1527.926466	20.238003
58.374804	1529.157913	20.243021
58.347094	1546.033831	20.248039
58.730271	1548.992462	20.253056
58.563899	1551.978305	20.258074
58.596191	1553.242665	20.263091
58.636279	1548.449804	20.268109
58.649136	1563.013897	20.273127
59.113819	1549.595576	20.278144
58.897850	1558.023513	20.283162
58.607867	1552.773096	20.288179
58.982418	1555.532368	20.293197
58.838548	1573.985037	20.298215
58.893872	1574.884953	20.303232
59.287598	1582.165884	20.308250
59.248842	1581.245540	20.313267
59.625469	1584.859204	20.318285
59.163229	1585.921982	20.323303
59.521366	1574.544522	20.328320
59.509128	1574.371761	20.333338
59.450085	1575.411087	20.338355
59.606432	1580.243118	20.343373
59.270230	1584.747648	20.348391
59.656724	1571.492649	20.353408
59.759525	1593.665543	20.358426
59.785921	1596.828534	20.363443
59.867109	1598.189133	20.368461
59.928376	1604.474327	20.373479
60.239030	1590.380288	20.378496
60.140677	1592.786369	20.383514
60.304452	1597.714814	20.388531
60.448464	1592.300791	20.393549
60.114217	1597.037679	20.398567
60.761971	1583.949255	20.403584
60.376304	1591.293097	20.408602
60.121603	1599.568807	20.413619
60.301471	1600.099282	20.418637
60.240285	1601.666527	20.423655
60.704415	1608.438566	20.428672
60.503142	1622.094855	20.433690
60.282900	1631.237718	20.438707
60.750107	1611.604697	20.443725
60.559354	1621.951737	20.448743
61.013342	1614.354081	20.453760
60.769628	1617.971251	20.458778
61.072937	1632.915275	20.463795
61.320436	1634.575902	20.468813
61.452857	1644.166292	20.473831
61.894059	1634.362059	20.478848
61.490420	1624.326060	20.483866
61.581288	1611.023124	20.488883
61.953380	1606.326456	20.493901
61.497977	1609.491270	20.498919
61.653283	1603.432848	20.503936
61.743051	1604.905808	20.508954
61.846409	1604.973751	20.513971
61.905957	1593.558707	20.518989
61.605485	1600.996716	20.524007
62.195511	1616.227898	20.529024
62.151784	1622.037960	20.534042
62.102952	1625.991372	20.539059
62.241453	1624.771989	20.544077
62.004887	1631.786435	20.549095
62.183299	1628.769482	20.554112
62.198131	1635.066707	20.559130
62.110804	1632.594152	20.564147
62.561813	1626.958024	20.569165
62.211784	1634.497168	20.574183
62.509325	1626.688005	20.579200
62.193959	1630.309956	20.584218
62.335671	1632.379047	20.589235
62.445120	1626.895931	20.594253
62.425778	1651.716322	20.599271
62.536052	1654.735120	20.604288
62.444757	1654.917183	20.609306
62.620457	1656.809783	20.614323
63.151625	1659.225028	20.619341
62.639525	1677.942730	20.624359
63.311081	1676.928393	20.629376
63.268764	1685.078431	20.634394
63.401564	1677.950071	20.639411
63.629678	1682.286781	20.644429
63.559891	1686.492894	20.649447
63.598543	1679.880916	20.654464
63.972057	1678.473402	20.659482
63.674596	1674.306871	20.664499
64.161187	1658.891892	20.669517
63.453724	1651.615265	20.674535
63.662852	1644.430582	20.679552
63.920400	1652.135279	20.684570
63.660699	1663.502042	20.689587
63.989817	1667.807063	20.694605
63.983977	1675.528611	20.699623
63.765693	1673.864355	20.704640
64.152411	1675.313351	20.709658
64.083197	1674.653560	20.714675
63.829398	1684.273670	20.719693
64.023738	1669.438179	20.724711
64.183892	1656.517044	20.729728
64.602009	1679.941018	20.734746
64.220518	1702.847019	20.739763
64.752118	1696.780982	20.744781
64.627771	1707.549767	20.749799
64.642062	1701.395363	20.754816
64.961117	1700.646479	20.759834
64.748259	1702.111681	20.764851
64.937639	1696.071597	20.769869
64.802549	1690.821470	20.774887
64.629175	1688.899774	20.779904
64.990366	1699.771628	20.784922
64.855195	1695.604599	20.789939
65.116107	1715.801857	20.794957
65.165325	1719.880399	20.799975
65.183015	1718.649121	20.804992
65.546830	1721.390123	20.810010
65.301507	1726.637137	20.815027
65.753622	1719.337776	20.820045
65.528018	1723.005516	20.825063
66.102305	1717.979269	20.830080
65.821531	1707.709877	20.835098
65.744368	1720.532305	20.840115
66.042160	1710.913583	20.845133
65.626150	1711.932100	20.850151
65.979756	1712.875945	20.855168
65.977602	1727.001726	20.860186
66.142015	1742.804694	20.865203
66.611473	1738.809987	20.870221
66.360173	1743.518224	20.875239
66.314893	1745.763176	20.880256
66.643464	1742.272119	20.885274
66.509868	1742.431266	20.890291
67.046835	1740.234860	20.895309
67.117871	1747.230710	20.900327
66.870122	1740.161394	20.905344
67.023573	1729.086615	20.910362
66.754250	1718.253106	20.915379
66.666943	1722.142833	20.920397
66.660323	1730.245645	20.925415
66.877856	1737.991263	20.930432
67.053891	1728.511196	20.935450
67.105006	1738.830472	20.940467
66.941476	1728.225113	20.945485
66.950437	1736.223772	20.950503
66.863153	1743.594265	20.955520
67.318912	1749.007494	20.960538
67.467431	1764.431612	20.965555
67.612324	1758.810296	20.970573
67.713116	1757.654627	20.975591
67.644671	1759.025055	20.980608
67.846909	1765.324769	20.985626
67.867674	1758.314925	20.990643
67.999280	1750.761525	20.995661
67.857283	1751.337030	21.000679
67.454620	1764.424417	21.005696
68.232097	1753.081334	21.010714
67.652369	1766.163393	21.015731
67.668862	1766.585883	21.020749
67.905818	1780.239044	21.025767
67.888639	1784.994357	21.030784
68.316539	1789.452746	21.035802
67.751549	1800.190615	21.040819
68.357164	1799.030100	21.045837
68.255326	1812.143703	21.050855
68.093481	1814.172921	21.055872
68.690483	1811.835066	21.060890
68.328488	1816.700632	21.065907
69.088935	1800.468894	21.070925
69.040905	1810.719199	21.075943
68.896929	1805.817756	21.080960
69.306072	1814.238000	21.085978
69.479606	1826.298520	21.090995
69.484184	1815.834561	21.096013
69.538993	1805.689859	21.101031
69.287949	1800.729371	21.106048
69.603127	1791.638834	21.111066
69.535413	1810.286659	21.116083
69.811836	1809.552704	21.121101
69.776028	1812.314218	21.126119
69.441343	1817.527632	21.131136
69.756460	1829.474159	21.136154
69.500261	1832.803675	21.141171
69.832912	1825.058287	21.146189
70.119744	1837.332738	21.151207
70.033845	1826.615243	21.156224
70.165132	1826.583286	21.161242
69.899674	1838.344444	21.166259
70.263561	1824.843756	21.171277
70.250063	1826.740143	21.176295
70.140463	1846.177246	21.181312
70.644802	1843.709451	21.186330
70.533541	1855.429343	21.191347
70.660869	1851.803862	21.196365
71.009946	1849.551147	21.201383
70.793863	1841.821802	21.206400
70.927377	1843.691881	21.211418
70.897368	1853.816393	21.216435
71.021657	1848.079949	21.221453
71.218195	1845.274525	21.226471
70.951561	1851.621198	21.231488
71.261926	1850.465863	21.236506
70.908201	1847.430674	21.241523
71.144076	1847.538096	21.246541
71.294708	1851.293575	21.251559
71.214931	1871.589966	21.256576
71.478119	1871.245611	21.261594
71.530577	1877.294967	21.266611
71.490182	1870.697570	21.271629
71.719449	1870.906483	21.276647
71.452987	1880.349672	21.281664
71.681183	1871.788858	21.286682
71.781008	1879.296550	21.291699
71.883166	1889.185416	21.296717
72.090990	1893.103488	21.301735
72.016412	1900.726289	21.306752
72.467352	1887.399720	21.311770
72.337574	1905.590601	21.316787
72.661379	1895.906826	21.321805
72.817193	1890.534054	21.326823
72.418056	1889.305635	21.331840
72.819700	1891.193926	21.336858
72.719953	1893.780603	21.341875
73.166164	1879.627637	21.346893
72.979931	1890.780427	21.351911
72.799957	1888.294429	21.356928
73.357843	1890.406069	21.361946
73.081239	1893.785829	21.366963
73.336696	1882.296797	21.371981
73.220981	1884.934149	21.376999
72.956293	1887.689478	21.382016
73.319386	1879.237036	21.387034
73.362606	1886.971039	21.392051
73.132453	1883.926406	21.397069
73.285736	1881.268693	21.402087
73.210768	1889.641572	21.407104
73.449558	1893.333251	21.412122
73.690173	1905.610684	21.417139
73.744335	1911.316849	21.422157
73.896640	1911.100698	21.427175
73.708292	1917.462388	21.432192
73.581498	1911.465123	21.437210
73.861173	1913.487393	21.442227
73.999246	1926.361758	21.447245
74.319637	1928.411149	21.452263
74.162288	1929.535674	21.457280
74.727153	1917.561516	21.462298
74.719085	1933.933409	21.467315
75.219797	1917.635891	21.472333
74.695053	1924.759207	21.477351
74.634228	1918.898264	21.482368
74.841375	1913.296113	21.487386
74.884839	1915.384266	21.492403
74.895826	1917.595123	21.497421
75.032170	1915.822123	21.502439
74.795050	1918.853215	21.507456
75.064342	1904.633060	21.512474
75.040791	1908.648501	21.517491
75.129436	1925.423675	21.522509
75.288006	1944.018052	21.527527
75.373847	1950.493024	21.532544
75.733729	1935.242851	21.537562
75.745754	1945.633700	21.542579
75.564106	1941.841633	21.547597
75.764333	1944.807010	21.552615
75.529383	1940.391073	21.557632
75.569796	1940.547395	21.562650
75.711521	1949.169870	21.567667
75.484528	1966.913518	21.572685
75.634351	1975.257886	21.577703
75.782437	1971.364365	21.582720
75.958440	1975.857823	21.587738
76.363493	1999.933678	21.592755
76.687291	2002.104566	21.597773
76.927686	1995.536218	21.602791
76.696156	2004.163436	21.607808
77.150239	1990.729956	21.612826
77.280037	1997.279169	21.617843
77.037322	1976.164755	21.622861
77.033818	1974.749559	21.627879
76.896194	1960.693186	21.632896
76.830237	1980.513795	21.637914
76.833293	1990.584494	21.642931
76.739330	1994.957297	21.647949
77.028765	1984.277551	21.652967
76.965682	1988.871231	21.657984
76.984602	1991.054012	21.663002
77.174493	2009.203897	21.668019
77.356126	2013.163345	21.673037
77.720077	2011.419974	21.678055
77.567827	2022.721567	21.683072
77.579406	2013.962674	21.688090
77.693204	2011.976066	21.693107
77.705469	2026.321393	21.698125
78.171827	2025.632362	21.703143
78.000768	2036.011456	21.708160
78.276217	2036.612346	21.713178
78.796585	2037.716404	21.718195
78.764908	2031.019461	21.723213
79.108623	2026.203347	21.728231
78.524442	2010.642071	21.733248
78.354357	1996.041417	21.738266
78.656716	2001.919519	21.743283
78.624896	2021.662085	21.748301
79.106013	2012.365199	21.753319
79.024552	2018.419853	21.758336
79.194886	2016.798306	21.763354
79.342164	2014.611659	21.768371
79.512070	2020.833758	21.773389
79.759407	2015.426103	21.778407
79.392020	2007.799681	21.783424
79.276806	2001.518170	21.788442
79.384910	2019.993431	21.793459
79.088495	2011.963903	21.798477
79.728459	2012.544204	21.803495
79.472041	2025.776498	21.808512
79.514381	2019.018878	21.813530
79.599229	2013.729075	21.818547
79.886940	2018.780054	21.823565
80.093986	2038.923659	21.828583
79.928310	2043.062277	21.833600
80.181188	2043.331459	21.838618
80.192869	2039.213646	21.843635
80.145552	2044.221676	21.848653
80.128765	2041.025932	21.853671
79.900711	2050.776655	21.858688
80.512683	2052.841568	21.863706
80.505544	2073.881735	21.868723
80.412588	2077.686262	21.873741
80.637167	2073.983208	21.878759
80.414736	2078.569832	21.883776
80.584455	2075.163273	21.888794
80.564503	2094.031491	21.893811
80.959940	2101.195453	21.898829
81.267208	2100.444174	21.903847
81.172225	2095.645554	21.908864
81.562221	2092.188740	21.913882
81.382904	2101.003436	21.918899
81.266116	2101.102714	21.923917
81.458643	2101.033844	21.928935
81.557572	2124.299127	21.933952
81.839288	2121.490969	21.938970
81.853624	2122.785515	21.943987
82.073998	2129.453651	21.949005
82.113593	2123.016532	21.954023
82.368428	2120.004943	21.959040
82.129740	2130.192927	21.964058
82.510824	2118.655361	21.969075
82.326601	2124.030586	21.974093
82.613718	2114.799226	21.979111
82.159796	2114.677934	21.984128
82.540906	2116.692493	21.989146
82.501426	2116.060438	21.994163
82.489698	2122.148076	21.999181
83.169744	2138.448382	22.004199
83.171813	2140.101668	22.009216
83.051378	2148.762542	22.014234
83.421440	2143.054591	22.019251
83.511940	2145.515319	22.024269
83.425093	2132.864616	22.029287
83.462975	2127.904612	22.034304
83.569641	2129.376006	22.039322
83.743558	2121.372490	22.044339
83.527115	2128.393669	22.049357
83.263551	2131.498474	22.054375
83.432347	2141.485922	22.059392
83.502468	2137.407622	22.064410
83.516662	2136.839517	22.069427
83.249151	2138.409873	22.074445
83.905303	2149.025326	22.079463
84.092819	2155.274485	22.084480
84.040179	2163.068200	22.089498
84.263074	2165.281803	22.094515
84.250730	2164.788566	22.099533
84.359100	2156.002937	22.104551
84.597141	2163.251652	22.109568
84.645336	2186.158089	22.114586
84.674757	2186.822555	22.119603
84.715163	2193.708713	22.124621
84.859923	2183.674074	22.129639
85.178382	2185.963594	22.134656
84.873238	2175.633749	22.139674
85.010723	2172.943561	22.144691
84.951914	2182.409640	22.149709
85.278944	2173.311014	22.154727
85.566788	2191.287407	22.159744
85.332164	2206.024974	22.164762
85.821384	2202.227678	22.169779
85.534395	2205.802539	22.174797
85.794210	2202.767668	22.179815
86.032694	2204.231024	22.184832
85.810854	2205.514285	22.189850
86.050191	2202.486741	22.194867
85.957411	2211.776171	22.199885
85.995691	2198.218830	22.204903
86.160063	2202.602070	22.209920
85.940707	2225.865082	22.214938
86.367029	2225.906723	22.219955
86.314722	2235.594603	22.224973
86.791522	2233.829768	22.229991
86.624190	2229.275774	22.235008
86.517566	2229.478492	22.240026
86.881791	2219.035428	22.245043
86.914553	2244.061141	22.250061
87.207703	2254.641488	22.255079
87.056960	2251.015496	22.260096
87.146526	2252.494851	22.265114
87.359823	2250.229128	22.270131
87.512290	2251.064572	22.275149
87.538677	2246.253685	22.280167
87.545980	2243.654728	22.285184
87.318731	2243.055725	22.290202
87.301244	2242.998397	22.295219
87.563801	2261.877134	22.300237
87.976611	2255.375806	22.305255
88.180881	2255.914471	22.310272
88.017167	2261.387533	22.315290
88.286981	2260.797967	22.320307
88.421234	2256.931864	22.325325
88.605038	2253.303239	22.330343
88.560406	2248.321817	22.335360
88.317540	2244.839825	22.340378
88.680026	2240.076054	22.345395
88.663558	2254.624784	22.350413
88.519493	2256.228652	22.355431
88.899161	2267.324632	22.360448
88.819327	2278.584498	22.365466
89.280253	2266.342230	22.370483
89.192337	2274.656040	22.375501
88.977707	2288.193857	22.380519
89.565403	2282.796298	22.385536
89.561857	2285.281281	22.390554
89.798958	2273.817049	22.395571
89.538946	2279.522607	22.400589
89.548258	2270.361169	22.405607
89.944972	2275.142598	22.410624
89.567556	2279.799824	22.415642
89.531820	2273.652295	22.420659
89.586863	2280.749465	22.425677
89.956066	2299.231831	22.430695
90.126868	2297.555450	22.435712
89.979928	2303.195050	22.440730
90.199825	2292.532120	22.445747
89.935884	2308.666049	22.450765
90.104061	2318.482838	22.455783
90.542042	2323.582664	22.460800
90.629553	2332.815936	22.465818
90.996752	2327.633618	22.470835
90.705456	2323.489512	22.475853
91.234512	2318.841846	22.480871
91.153132	2324.127273	22.485888
91.287721	2329.350565	22.490906
91.694801	2332.502648	22.495923
91.895101	2334.906248	22.500941
91.652306	2314.200070	22.505959
91.678555	2308.160381	22.510976
91.833818	2313.080229	22.515994
91.791357	2325.916309	22.521011
91.754059	2345.162528	22.526029
91.516951	2335.667420	22.531047
92.022729	2336.870774	22.536064
91.894897	2347.295677	22.541082
92.333424	2335.424801	22.546099
92.243643	2347.840758	22.551117
92.304594	2350.624933	22.556135
92.262567	2347.132107	22.561152
92.310960	2367.505961	22.566170
92.602815	2369.989295	22.571187
92.607125	2375.761368	22.576205
92.724879	2369.396251	22.581223
92.889896	2366.415236	22.586240
92.943697	2364.682231	22.591258
93.111779	2381.204968	22.596275
93.184490	2389.997392	22.601293
93.216341	2394.338057	22.606311
93.822365	2383.579637	22.611328
93.277062	2392.985439	22.616346
93.542374	2384.038650	22.621363
93.453719	2387.392120	22.626381
93.642418	2387.547126	22.631399
93.897397	2400.174169	22.636416
93.652265	2412.905285	22.641434
94.209629	2408.396617	22.646451
94.241029	2407.664226	22.651469
94.151369	2413.978674	22.656487
94.615392	2416.895743	22.661504
94.345065	2414.871102	22.666522
94.547205	2414.171469	22.671539
94.674492	2405.676286	22.676557
94.464512	2407.841509	22.681575
94.785907	2415.464360	22.686592
94.885571	2430.593276	22.691610
95.252344	2435.184818	22.696627
95.493683	2431.063526	22.701645
95.155799	2443.445829	22.706663
95.427369	2430.778457	22.711680
95.188414	2431.749590	22.716698
95.473559	2433.853707	22.721715
95.416923	2423.711699	22.726733
95.357395	2427.705276	22.731751
95.580575	2419.916299	22.736768
95.121631	2428.950716	22.741786
95.580787	2447.559713	22.746803
95.890111	2455.085757	22.751821
95.505714	2465.504396	22.756839
96.350975	2454.151165	22.761856
96.153978	2466.704660	22.766874
95.953923	2478.615718	22.771891
96.405651	2484.017277	22.776909
96.451547	2491.385366	22.781927
96.891140	2479.196075	22.786944
96.515360	2486.148513	22.791962
96.567586	2474.171402	22.796979
96.560071	2489.705546	22.801997
96.946845	2505.894550	22.807015
97.498487	2503.194795	22.812032
97.489213	2512.439867	22.817050
97.479746	2513.822251	22.822067
97.747341	2510.540347	22.827085
97.389738	2508.979386	22.832103
97.954750	2491.620951	22.837120
97.999176	2510.331761	22.842138
97.712270	2497.279211	22.847155
98.134894	2498.810934	22.852173
97.728387	2506.582301	22.857191
98.110901	2505.722870	22.862208
98.139520	2518.799326	22.867226
98.277881	2521.034065	22.872243
98.568787	2516.976202	22.877261
98.017163	2521.704077	22.882279
98.881753	2521.701114	22.887296
98.617914	2528.386201	22.892314
98.943255	2531.480201	22.897331
99.196561	2541.697632	22.902349
99.324717	2546.123190	22.907367
99.596482	2549.480018	22.912384
99.178114	2552.988907	22.917402
99.419020	2547.451812	22.922419
99.473382	2540.395104	22.927437
99.503871	2546.322366	22.932455
99.629665	2545.051076	22.937472
99.269300	2547.030179	22.942490
99.330303	2550.858546	22.947507
99.612180	2552.966766	22.952525
99.477127	2566.648352	22.957543
99.818623	2575.492449	22.962560
99.924037	2578.236230	22.967578
100.301771	2596.780141	22.972595
100.394647	2607.326167	22.977613
100.189640	2612.500260	22.982631
100.794431	2601.408408	22.987648
100.852243	2600.158606	22.992666
100.675920	2605.687423	22.997683
100.921296	2609.532920	23.002701
101.206390	2609.649133	23.007719
101.080559	2613.995099	23.012736
101.501898	2618.126054	23.017754
101.374407	2619.227966	23.022771
101.397471	2614.497049	23.027789
101.611560	2613.937566	23.032807
101.739983	2607.246941	23.037824
101.505451	2615.256049	23.042842
101.539140	2618.414103	23.047859
101.801395	2610.439022	23.052877
101.736955	2609.398844	23.057895
101.933034	2617.096878	23.062912
102.569751	2630.402692	23.067930
102.280685	2642.040401	23.072947
102.743968	2633.797361	23.077965
102.537812	2645.345355	23.082983
102.843310	2634.060495	23.088000
102.608484	2638.834780	23.093018
102.511194	2636.394423	23.098035
102.753876	2633.132369	23.103053
102.826800	2635.372446	23.108071
102.954358	2642.947575	23.113088
102.820844	2667.725100	23.118106
102.797094	2660.684814	23.123123
103.252464	2661.554784	23.128141
103.281100	2678.446227	23.133159
103.512512	2689.701318	23.138176
103.600093	2691.163720	23.143194
103.809931	2696.728642	23.148211
103.906196	2686.151666	23.153229
103.954407	2690.335363	23.158247
104.015333	2698.441276	23.163264
104.541170	2712.006089	23.168282
104.337220	2720.529519	23.173299
104.751643	2716.761810	23.178317
104.719023	2720.600602	23.183335
105.116741	2707.922358	23.188352
104.956470	2703.355636	23.193370
104.528711	2711.319614	23.198387
104.831164	2701.295151	23.203405
104.708539	2706.375708	23.208423
104.908480	2718.301831	23.213440
105.420002	2735.009440	23.218458
105.192165	2738.144671	23.223475
105.615381	2736.889877	23.228493
105.289070	2735.707206	23.233511
105.757446	2738.790166	23.238528
106.094297	2747.974528	23.243546
106.233680	2756.346245	23.248563
106.399412	2759.817926	23.253581
106.389612	2761.064549	23.258599
106.491266	2750.321664	23.263616
106.653165	2757.362380	23.268634
106.752476	2757.524709	23.273651
107.122454	2748.343831	23.278669
106.820286	2755.673995	23.283687
107.060502	2747.360340	23.288704
107.169704	2742.293049	23.293722
106.956581	2753.674152	23.298739
106.949427	2748.193412	23.303757
106.779565	2750.799320	23.308775
106.805919	2752.279739	23.313792
107.326964	2768.640111	23.318810
107.108875	2768.196275	23.323827
107.325358	2776.652883	23.328845
107.539885	2793.030955	23.333863
107.544118	2791.086407	23.338880
108.100167	2808.946664	23.343898
107.918688	2811.402918	23.348915
108.291284	2804.495389	23.353933
108.094828	2809.172813	23.358951
108.034773	2802.605050	23.363968
108.600012	2826.693468	23.368986
108.222269	2832.585268	23.374003
109.117518	2832.584320	23.379021
109.110402	2831.842931	23.384039
108.899189	2824.815103	23.389056
108.983155	2830.319804	23.394074
108.908106	2827.278045	23.399091
109.353762	2822.102657	23.404109
109.271198	2830.128450	23.409127
109.273749	2844.004839	23.414144
109.775234	2845.075471	23.419162
109.578412	2857.181574	23.424179
109.795893	2849.258277	23.429197
109.715848	2849.629057	23.434215
110.006540	2840.646308	23.439232
109.880276	2846.276379	23.444250
110.158022	2864.746606	23.449267
110.391771	2869.117369	23.454285
110.268195	2883.309189	23.459303
110.600804	2879.903049	23.464320
110.603965	2875.424977	23.469338
110.775992	2875.442579	23.474355
110.843467	2865.953810	23.479373
110.791743	2876.187315	23.484391
110.732423	2891.052817	23.489408
111.011241	2898.464039	23.494426
111.047409	2905.385468	23.499443
111.379206	2901.293964	23.504461
111.537006	2911.353026	23.509479
111.455838	2929.737070	23.514496
111.951248	2929.947218	23.519514
111.795113	2937.654901	23.524531
111.991857	2928.210840	23.529549
111.995096	2929.851811	23.534567
112.120748	2927.371347	23.539584
112.485894	2945.998870	23.544602
112.317091	2957.547997	23.549619
112.824297	2959.719370	23.554637
112.627780	2956.645330	23.559655
112.661402	2962.147387	23.564672
113.124004	2953.060514	23.569690
113.023668	2960.343183	23.574707
113.452821	2963.555923	23.579725
113.453363	2972.639785	23.584743
113.502096	2973.797592	23.589760
113.795400	2978.619593	23.594778
113.714705	2980.452042	23.599795
113.913058	2980.407406	23.604813
113.814895	2979.759438	23.609831
114.060747	2967.559715	23.614848
113.837268	2971.430167	23.619866
113.857981	2977.461583	23.624883
114.144979	2979.523341	23.629901
114.382544	2989.635002	23.634919
114.409579	2988.966305	23.639936
114.390064	2980.302577	23.644954
114.046731	2989.051218	23.649971
114.591771	3001.555917	23.654989
114.839353	3013.764565	23.660007
114.879927	3008.253782	23.665024
114.982228	3016.208114	23.670042
115.002335	3021.716762	23.675059
115.417812	3032.544738	23.680077
115.345810	3047.752679	23.685095
115.122563	3047.590424	23.690112
115.481808	3040.625942	23.695130
115.446479	3070.955335	23.700147
115.870479	3065.672026	23.705165
116.181695	3072.626346	23.710183
116.408300	3068.642775	23.715200
116.772225	3066.905204	23.720218
116.325665	3072.603741	23.725235
116.519980	3064.928684	23.730253
116.569566	3062.556472	23.735271
116.722569	3070.937128	23.740288
116.995811	3079.456165	23.745306
117.052372	3094.503483	23.750323
117.158914	3092.195860	23.755341
117.184502	3087.960496	23.760359
117.257635	3089.894274	23.765376
117.493519	3089.445746	23.770394
117.325327	3081.030222	23.775411
117.589729	3091.269803	23.780429
117.759704	3107.360670	23.785447
117.801263	3110.114330	23.790464
118.276957	3105.041369	23.795482
117.977858	3115.366779	23.800499
117.854212	3109.985915	23.805517
118.142366	3128.219668	23.810535
118.019398	3136.683061	23.815552
118.718268	3131.397140	23.820570
118.754857	3134.165014	23.825587
118.859074	3131.703029	23.830605
119.422909	3155.097234	23.835623
119.327390	3156.835690	23.840640
119.757784	3156.272665	23.845658
119.617743	3154.779563	23.850675
119.883509	3146.483516	23.855693
120.228423	3146.693386	23.860711
119.871479	3153.177988	23.865728
120.470438	3142.549764	23.870746
120.174495	3145.530979	23.875763
120.424379	3142.108950	23.880781
120.647169	3146.152830	23.885799
120.224432	3149.166850	23.890816
120.623715	3145.846477	23.895834
120.515939	3149.202488	23.900851
120.287646	3145.000479	23.905869
120.419253	3151.898736	23.910887
120.628069	3170.718570	23.915904
120.838820	3179.249977	23.920922
120.872902	3183.738541	23.925939
120.846405	3182.613294	23.930957
121.045211	3200.447312	23.935975
121.346117	3211.683401	23.940992
121.681112	3204.374398	23.946010
121.583305	3217.255023	23.951027
121.567485	3223.462680	23.956045
121.858509	3230.160938	23.961063
121.916970	3238.173435	23.966080
122.280204	3242.298824	23.971098
122.279965	3253.847430	23.976115
122.487250	3260.435928	23.981133
122.893388	3258.411789	23.986151
122.982077	3265.727091	23.991168
123.060216	3262.318114	23.996186
123.007473	3260.497127	24.001203
122.988931	3263.151696	24.006221
123.248310	3261.023493	24.011239
123.505908	3278.067462	24.016256
123.842171	3274.601572	24.021274
123.680824	3278.196034	24.026291
123.640873	3280.502536	24.031309
123.996067	3280.342160	24.036327
123.892472	3282.957658	24.041344
123.838245	3281.304256	24.046362
124.026269	3288.931902	24.051379
124.206522	3304.334970	24.056397
124.382883	3307.562468	24.061415
124.132859	3313.729005	24.066432
124.634691	3305.384342	24.071450
124.609211	3309.115390	24.076467
124.985097	3330.063914	24.081485
125.160992	3332.079539	24.086503
125.222179	3338.523341	24.091520
125.273254	3335.978773	24.096538
125.176891	3330.194450	24.101555
125.268544	3331.581033	24.106573
125.722256	3337.132978	24.111591
125.942625	3355.892455	24.116608
126.266169	3357.791502	24.121626
126.201957	3355.592435	24.126643
126.311394	3355.463690	24.131661
126.660638	3347.693546	24.136679
126.226337	3347.254774	24.141696
126.417001	3341.129191	24.146714
126.518197	3340.532857	24.151731
126.953177	3355.280345	24.156749
127.281341	3359.137523	24.161767
127.538195	3367.401921	24.166784
127.292973	3357.009391	24.171802
127.351128	3366.928140	24.176819
127.525861	3356.794862	24.181837
127.493494	3349.367063	24.186855
127.248262	3372.417141	24.191872
127.496614	3382.847389	24.196890
127.908567	3384.026993	24.201907
128.213895	3388.900288	24.206925
127.856951	3393.439869	24.211943
128.073239	3412.628882	24.216960
128.385306	3408.412545	24.221978
128.746093	3409.228135	24.226995
128.607852	3414.273312	24.232013
128.793143	3415.812531	24.237031
129.118938	3436.700192	24.242048
129.478385	3436.830487	24.247066
129.537038	3440.079075	24.252083
129.430836	3441.840593	24.257101
129.519940	3426.940139	24.262119
129.665247	3438.203335	24.267136
129.713502	3428.736307	24.272154
129.826633	3439.488624	24.277171
129.853893	3459.113765	24.282189
130.113002	3455.490903	24.287207
130.068528	3466.248070	24.292224
130.374285	3463.120303	24.297242
130.436401	3482.713321	24.302259
130.168653	3489.971190	24.307277
130.385467	3490.613744	24.312295
130.571882	3509.806641	24.317312
131.279154	3514.579568	24.322330
131.367969	3522.189890	24.327347
131.416246	3513.810744	24.332365
131.611546	3517.303295	24.337383
131.554722	3521.501848	24.342400
131.668074	3527.442145	24.347418
132.244758	3540.870116	24.352435
132.184588	3553.815662	24.357453
132.422145	3535.350295	24.362471
132.408147	3551.751249	24.367488
132.390447	3544.013015	24.372506
132.403001	3539.377665	24.377523
132.457577	3540.007707	24.382541
132.940463	3554.007591	24.387559
133.030640	3567.553144	24.392576
133.314738	3569.100826	24.397594
133.003874	3569.703170	24.402611
133.112589	3566.197321	24.407629
133.380941	3574.007896	24.412647
133.345285	3577.002405	24.417664
133.388141	3583.874597	24.422682
133.698031	3597.205429	24.427699
133.482537	3596.776099	24.432717
133.744800	3593.821672	24.437735
134.138160	3614.556633	24.442752
134.411982	3616.642710	24.447770
134.431912	3622.423289	24.452787
134.035799	3625.992515	24.457805
134.671125	3624.475737	24.462823
134.791747	3650.913764	24.467840
134.741667	3659.605956	24.472858
134.891352	3658.484582	24.477875
134.866719	3658.370550	24.482893
135.242712	3670.876215	24.487911
135.398576	3675.427446	24.492928
135.849061	3671.996505	24.497946
135.868685	3684.479280	24.502963
135.894806	3688.878349	24.507981
136.386270	3701.733083	24.512999
136.088560	3712.146856	24.518016
136.314905	3708.756559	24.523034
136.541801	3709.811293	24.528051
136.419598	3707.340635	24.533069
136.866802	3721.840349	24.538087
136.952821	3733.051752	24.543104
137.314106	3734.579979	24.548122
137.399944	3729.592628	24.553139
137.030386	3730.823681	24.558157
137.427874	3735.879494	24.563175
137.600320	3751.779250	24.568192
137.663757	3750.181920	24.573210
137.936944	3744.920598	24.578227
138.197998	3759.162541	24.583245
138.534475	3749.977965	24.588263
138.434305	3750.910446	24.593280
138.530269	3756.332767	24.598298
139.045970	3767.824685	24.603315
138.981174	3762.664595	24.608333
139.272022	3762.795225	24.613351
139.301193	3764.333945	24.618368
139.443029	3765.033420	24.623386
139.523730	3751.356275	24.628403
139.461256	3766.348738	24.633421
139.506450	3762.964401	24.638439
139.944799	3767.858713	24.643456
139.774094	3784.969026	24.648474
140.048061	3783.809349	24.653491
139.932494	3795.753093	24.658509
140.200739	3783.268281	24.663527
139.885497	3801.362524	24.668544
140.105830	3815.247033	24.673562
140.204838	3814.459677	24.678579
140.505686	3831.112387	24.683597
140.950013	3836.711349	24.688615
140.960480	3842.756214	24.693632
141.180691	3842.592983	24.698650
141.505860	3852.469014	24.703667
141.848546	3866.518380	24.708685
141.839979	3863.334290	24.713703
141.781972	3870.919081	24.718720
141.976125	3873.447976	24.723738
142.058001	3868.388784	24.728755
141.913710	3863.389876	24.733773
142.359639	3879.203534	24.738791
142.505581	3898.318556	24.743808
142.314649	3898.565963	24.748826
142.704911	3883.719564	24.753843
142.691825	3894.899846	24.758861
143.028505	3908.295024	24.763879
143.182268	3917.639545	24.768896
143.384081	3928.561404	24.773914
143.599010	3928.247054	24.778931
142.979701	3931.018523	24.783949
143.766283	3934.708600	24.788967
143.407174	3955.756415	24.793984
143.727079	3953.301515	24.799002
144.186289	3957.797096	24.804019
144.223550	3972.191656	24.809037
144.161397	3979.978793	24.814055
144.702067	3985.175971	24.819072
144.782080	3980.542317	24.824090
144.847095	3982.157814	24.829107
145.010182	4003.290134	24.834125
145.308169	4002.059524	24.839143
145.688744	4004.778085	24.844160
145.451947	4001.253738	24.849178
145.632711	3995.445733	24.854195
145.382014	4008.822474	24.859213
145.856754	4024.984323	24.864231
145.647198	4031.050723	24.869248
145.803178	4042.320462	24.874266
146.210455	4050.330754	24.879283
146.288544	4059.489431	24.884301
146.472094	4058.579387	24.889319
146.947225	4068.074765	24.894336
147.088510	4084.655720	24.899354
147.345294	4075.955881	24.904371
147.499796	4084.187596	24.909389
147.584648	4085.020950	24.914407
147.824519	4074.276327	24.919424
147.836785	4089.433526	24.924442
148.091398	4092.183982	24.929459
148.400728	4105.124725	24.934477
148.368767	4110.833353	24.939495
148.687456	4102.398100	24.944512
148.621714	4101.383631	24.949530
148.814733	4101.644655	24.954547
149.067822	4112.465225	24.959565
148.554013	4107.638456	24.964583
148.934884	4120.317719	24.969600
148.747741	4131.289938	24.974618
148.913316	4132.344616	24.979635
149.207096	4150.933811	24.984653
149.229552	4167.767637	24.989671
149.602720	4162.527821	24.994688
149.755648	4178.426516	24.999706
149.900687	4175.725682	25.004723
150.085008	4184.208463	25.009741
150.470008	4181.999488	25.014759
150.661628	4200.059891	25.019776
150.645309	4217.898002	25.024794
150.848850	4213.418663	25.029811
151.006155	4214.529056	25.034829
150.900682	4219.326110	25.039847
151.224484	4235.302105	25.044864
150.984822	4245.544384	25.049882
151.563321	4235.848510	25.054899
151.556035	4250.238099	25.059917
151.813378	4265.815606	25.064935
152.092385	4272.244601	25.069952
152.147675	4276.281856	25.074970
152.228135	4268.576629	25.079987
152.352840	4275.892742	25.085005
152.691569	4290.851967	25.090023
152.848182	4297.972223	25.095040
153.056104	4298.215032	25.100058
153.013642	4297.117943	25.105075
153.342163	4294.432389	25.110093
153.626904	4295.216912	25.115111
153.617628	4292.626659	25.120128
153.580548	4320.165344	25.125146
153.486546	4317.018145	25.130163
153.869735	4315.005551	25.135181
153.737965	4324.131396	25.140199
154.023251	4345.845631	25.145216
154.313031	4351.473517	25.150234
154.588979	4345.748068	25.155251
154.669767	4363.461587	25.160269
154.573513	4376.042062	25.165287
154.985908	4376.970840	25.170304
155.338357	4391.625473	25.175322
155.649231	4400.168537	25.180339
155.610208	4403.937134	25.185357
155.315995	4408.842671	25.190375
155.977512	4399.116415	25.195392
155.996272	4405.235728	25.200410
156.241846	4417.700580	25.205427
156.152807	4437.264686	25.210445
156.244853	4430.722249	25.215463
156.458854	4434.238688	25.220480
156.638221	4454.717616	25.225498
156.635440	4459.722982	25.230515
157.072608	4449.199033	25.235533
156.968958	4470.104435	25.240551
157.236743	4489.069272	25.245568
157.425666	4494.751709	25.250586
157.772508	4484.477381	25.255603
158.047331	4494.221182	25.260621
158.372301	4509.249050	25.265639
158.288900	4505.071512	25.270656
158.169867	4507.852398	25.275674
158.593621	4508.699761	25.280691
159.094689	4520.860930	25.285709
158.971271	4532.844336	25.290727
159.027597	4529.715522	25.295744
159.045342	4541.372356	25.300762
159.376268	4529.622392	25.305779
159.665032	4549.922673	25.310797
159.724598	4563.480848	25.315815
160.347588	4554.405885	25.320832
159.744190	4568.171475	25.325850
159.977901	4565.985133	25.330867
160.393542	4572.574346	25.335885
160.692157	4592.666711	25.340903
161.099039	4589.334152	25.345920
160.831860	4591.817468	25.350938
160.984709	4589.294833	25.355955
161.284979	4588.645808	25.360973
161.295956	4596.959833	25.365991
161.573159	4607.106541	25.371008
161.501760	4615.456265	25.376026
161.532948	4614.743890	25.381043
161.765655	4618.721934	25.386061
161.909000	4628.201702	25.391079
162.069722	4627.669497	25.396096
162.243104	4637.231717	25.401114
162.484446	4636.286084	25.406131
162.875101	4654.506225	25.411149
162.959336	4661.723685	25.416167
163.380157	4657.435855	25.421184
162.909035	4659.374086	25.426202
163.057882	4657.959415	25.431219
163.552625	4666.606071	25.436237
163.495191	4682.911045	25.441255
163.842908	4679.326004	25.446272
164.041499	4686.048856	25.451290
163.895623	4683.103123	25.456307
164.315480	4691.796056	25.461325
164.389086	4706.481396	25.466343
164.570513	4697.937815	25.471360
164.885572	4705.925122	25.476378
164.917054	4719.645593	25.481395
165.158110	4729.058842	25.486413
164.836964	4735.393643	25.491431
165.288030	4732.319150	25.496448
165.191988	4757.527718	25.501466
165.624133	4760.405629	25.506483
165.815632	4757.240216	25.511501
165.399408	4773.893718	25.516519
166.313382	4786.931031	25.521536
166.259282	4795.463065	25.526554
166.409930	4813.560097	25.531571
166.730190	4818.791684	25.536589
166.587385	4820.947292	25.541607
166.949673	4826.010472	25.546624
167.317850	4846.468893	25.551642
167.079621	4855.147214	25.556659
167.598762	4854.840767	25.561677
167.601086	4875.467690	25.566695
168.219059	4867.636956	25.571712
167.828702	4869.405902	25.576730
168.129922	4883.652063	25.581747
168.571403	4886.635563	25.586765
168.812580	4900.671947	25.591783
168.957359	4896.949551	25.596800
169.152201	4900.242446	25.601818
169.529665	4904.237552	25.606835
170.001210	4913.826975	25.611853
169.952073	4917.397324	25.616871
170.161829	4917.613064	25.621888
170.247931	4921.848578	25.626906
170.337200	4909.286971	25.631923
170.355626	4913.835328	25.636941
170.514281	4922.525952	25.641959
170.933327	4908.477153	25.646976
170.646307	4906.123373	25.651994
170.714278	4926.311842	25.657011
171.311633	4932.140255	25.662029
171.060229	4947.173390	25.667047
170.975661	4948.594017	25.672064
171.322832	4961.539443	25.677082
171.370225	4970.831320	25.682100
171.779417	4973.955645	25.687117
171.677707	4993.669029	25.692135
171.817452	5008.137355	25.697152
172.106231	5012.769359	25.702170
172.092380	5022.226558	25.707188
172.486266	5027.267246	25.712205
172.382076	5048.977624	25.717223
172.990930	5048.272772	25.722240
173.261920	5056.023403	25.727258
173.614862	5069.668910	25.732276
173.640140	5079.354365	25.737293
173.963131	5083.189206	25.742311
174.197767	5075.312359	25.747328
174.454691	5067.421587	25.752346
174.464407	5080.848271	25.757364
174.638083	5085.983715	25.762381
174.742167	5098.974223	25.767399
175.104963	5102.334654	25.772416
175.281748	5094.441384	25.777434
174.981990	5097.138880	25.782452
175.310357	5094.271288	25.787469
175.776168	5102.814291	25.792487
175.646503	5111.766186	25.797504
176.015993	5120.025862	25.802522
175.687209	5128.464146	25.807540
176.167245	5118.814753	25.812557
176.545656	5140.276033	25.817575
176.384680	5145.633866	25.822592
176.558506	5145.906751	25.827610
176.840908	5145.813549	25.832628
177.232497	5151.950978	25.837645
177.226448	5171.825954	25.842663
177.411923	5174.447859	25.847680
177.407054	5176.056147	25.852698
177.629592	5189.875351	25.857716
177.980865	5199.825099	25.862733
177.614245	5210.390666	25.867751
178.134381	5220.304596	25.872768
178.342649	5230.309540	25.877786
178.343231	5240.297679	25.882804
178.944517	5249.809911	25.887821
178.699877	5274.416982	25.892839
179.217019	5267.754206	25.897856
179.158461	5278.076648	25.902874
179.324641	5290.097746	25.907892
179.534022	5291.378380	25.912909
179.655331	5305.951631	25.917927
180.228912	5311.372213	25.922944
180.280177	5324.402367	25.927962
180.228053	5335.374333	25.932980
180.415066	5339.350675	25.937997
180.472434	5357.852060	25.943015
180.763748	5357.866070	25.948032
181.103368	5366.602591	25.953050
180.816453	5380.863083	25.958068
181.624657	5399.255182	25.963085
181.773907	5417.414572	25.968103
181.911850	5411.427265	25.973120
182.069535	5416.325247	25.978138
182.407470	5431.619635	25.983156
182.847700	5436.553547	25.988173
182.861298	5438.979484	25.993191
183.124310	5436.923641	25.998208
183.359679	5433.074284	26.003226
183.204950	5448.156473	26.008244
183.776355	5449.051910	26.013261
183.798799	5447.834518	26.018279
184.065904	5446.938919	26.023296
184.401565	5443.287184	26.028314
184.138901	5443.674077	26.033332
184.660541	5455.979851	26.038349
184.509230	5476.440031	26.043367
184.672407	5476.380742	26.048384
185.148501	5473.061748	26.053402
184.939001	5482.972192	26.058420
185.395038	5488.124820	26.063437
185.483264	5498.432557	26.068455
185.794957	5499.580494	26.073472
186.107034	5491.507109	26.078490
185.760565	5520.952339	26.083508
186.085743	5530.468708	26.088525
186.050976	5531.138431	26.093543
186.654004	5537.413495	26.098560
186.722431	5558.521833	26.103578
186.770433	5565.460592	26.108596
186.954601	5561.277859	26.113613
186.912413	5567.111573	26.118631
187.224044	5587.237711	26.123648
187.716060	5588.444803	26.128666
187.534291	5602.731405	26.133684
187.902666	5607.280312	26.138701
187.817685	5618.913206	26.143719
187.825716	5624.336159	26.148736
188.190087	5639.591719	26.153754
188.215179	5648.763245	26.158772
188.738064	5647.202293	26.163789
188.887303	5667.787027	26.168807
189.098991	5679.190490	26.173824
189.655550	5695.250732	26.178842
189.421104	5701.030473	26.183860
190.081089	5702.304282	26.188877
189.686135	5716.881466	26.193895
189.768224	5733.931564	26.198912
190.319055	5732.595174	26.203930
190.168094	5751.397721	26.208948
190.765304	5756.430979	26.213965
190.931698	5774.385525	26.218983
191.548174	5777.431593	26.224000
191.734388	5784.078203	26.229018
191.827562	5790.574030	26.234036
192.244506	5786.828425	26.239053
192.097960	5788.059331	26.244071
192.035443	5797.173773	26.249088
192.316694	5803.343902	26.254106
192.373233	5814.309239	26.259124
192.670431	5808.797919	26.264141
192.844464	5828.461969	26.269159
193.043791	5838.281327	26.274176
193.491718	5842.155533	26.279194
193.355962	5862.237153	26.284212
193.570474	5870.170814	26.289229
193.826514	5872.622843	26.294247
193.631430	5891.074492	26.299264
194.009575	5894.760994	26.304282
194.084276	5919.329592	26.309300
194.751858	5927.039417	26.314317
195.230382	5932.562593	26.319335
194.694204	5947.335856	26.324352
195.320238	5957.360318	26.329370
195.741445	5959.488084	26.334388
195.360041	5959.594558	26.339405
196.076481	5982.567617	26.344423
196.029814	5982.064976	26.349440
196.554541	5984.949846	26.354458
196.615320	5994.292881	26.359476
196.555818	6010.997320	26.364493
196.994955	6011.723296	26.369511
196.953323	6024.230667	26.374528
197.433283	6036.067280	26.379546
197.708699	6045.652847	26.384564
197.401748	6049.748948	26.389581
197.973387	6053.083679	26.394599
198.100786	6065.491426	26.399616
198.181745	6071.301002	26.404634
198.410000	6082.421616	26.409652
198.653099	6098.252190	26.414669
199.001002	6099.454827	26.419687
198.671626	6105.044069	26.424704
199.261881	6107.540050	26.429722
199.312607	6126.197022	26.434740
199.490707	6124.828577	26.439757
199.503561	6131.745048	26.444775
199.436945	6154.105247	26.449792
200.307238	6155.682965	26.454810
200.145352	6163.825584	26.459828
200.664646	6175.282452	26.464845
200.505808	6183.126849	26.469863
201.037820	6181.554887	26.474880
201.389723	6193.345081	26.479898
201.292376	6211.064172	26.484916
201.509670	6209.197745	26.489933
202.054707	6202.777284	26.494951
201.938186	6218.826614	26.499968
202.389167	6222.269571	26.504986
202.328666	6236.004224	26.510004
201.974548	6242.269467	26.515021
202.667020	6251.196176	26.520039
202.537716	6263.733214	26.525056
203.039493	6272.938823	26.530074
203.249738	6291.997273	26.535092
203.606168	6294.534357	26.540109
203.724415	6316.495565	26.545127
204.046012	6334.210815	26.550144
204.381126	6329.205009	26.555162
204.558108	6331.460685	26.560180
204.387867	6341.534507	26.565197
204.869307	6348.121457	26.570215
205.057122	6355.884925	26.575232
205.228375	6370.979401	26.580250
205.206414	6379.923634	26.585268
205.436313	6380.088018	26.590285
205.834136	6403.122312	26.595303
205.955230	6397.410736	26.600320
206.393301	6418.989906	26.605338
206.061620	6435.090037	26.610356
206.290879	6442.146466	26.615373
206.910621	6448.968912	26.620391
206.946432	6463.666081	26.625408
207.364662	6470.988185	26.630426
207.258619	6487.798499	26.635444
207.656151	6498.159655	26.640461
208.366829	6506.261187	26.645479
208.375626	6523.165949	26.650496
208.707584	6521.194651	26.655514
209.011719	6525.057387	26.660532
208.783101	6532.848921	26.665549
209.194588	6535.672300	26.670567
209.404577	6550.810159	26.675584
209.327530	6552.807822	26.680602
209.525176	6565.524909	26.685620
209.934678	6572.158518	26.690637
210.500357	6581.868070	26.695655
210.109858	6587.544001	26.700672
210.527823	6600.720869	26.705690
210.704968	6606.417836	26.710708
210.683306	6612.826678	26.715725
211.153379	6625.781485	26.720743
211.448616	6638.653398	26.725760
211.489432	6640.488994	26.730778
211.488068	6664.308883	26.735796
211.685061	6669.218077	26.740813
212.340831	6674.129305	26.745831
212.337695	6689.751544	26.750848
212.651227	6694.588681	26.755866
212.826100	6698.931278	26.760884
213.055426	6717.901227	26.765901
213.307031	6717.997434	26.770919
213.518041	6731.275621	26.775936
213.602025	6730.753692	26.780954
214.049708	6750.122323	26.785972
213.754346	6755.336745	26.790989
214.377336	6757.760465	26.796007
214.428075	6775.925908	26.801024
214.744665	6778.216037	26.806042
214.958498	6794.580678	26.811060
214.409573	6798.010486	26.816077
215.057841	6802.303103	26.821095
215.353053	6811.701544	26.826112
215.419819	6820.465927	26.831130
215.754679	6837.323349	26.836148
215.660935	6844.292435	26.841165
216.259839	6861.617371	26.846183
216.245747	6872.877907	26.851200
216.371201	6889.694433	26.856218
216.835323	6897.608558	26.861236
217.258783	6910.486247	26.866253
217.337195	6919.048687	26.871271
217.231820	6933.397880	26.876288
217.720264	6942.709275	26.881306
218.093993	6962.770173	26.886324
218.086046	6966.160875	26.891341
218.544063	6974.689650	26.896359
218.626793	6993.673956	26.901376
218.909379	7007.970809	26.906394
219.369520	7014.086595	26.911412
219.284860	7023.931646	26.916429
219.447346	7032.170671	26.921447
219.595507	7053.152799	26.926464
219.938846	7060.856999	26.931482
220.181038	7078.590165	26.936500
220.233356	7083.165830	26.941517
220.425469	7103.805197	26.946535
220.927397	7114.464550	26.951552
221.060524	7123.822268	26.956570
221.658500	7137.142288	26.961588
221.642326	7149.957466	26.966605
221.982016	7156.473699	26.971623
221.893741	7160.592958	26.976640
222.314145	7172.678955	26.981658
222.879838	7181.789447	26.986676
223.059120	7202.672099	26.991693
223.469077	7179.221754	26.996711
223.508048	7196.819340	27.001728
223.762410	7214.045736	27.006746
223.709582	7218.385997	27.011764
223.877061	7225.627871	27.016781
224.029003	7235.285800	27.021799
224.151615	7254.658448	27.026816
224.698502	7266.668441	27.031834
224.763048	7271.601322	27.036852
224.755591	7276.649313	27.041869
225.039742	7288.270371	27.046887
225.213507	7306.954049	27.051904
225.345649	7317.169842	27.056922
225.558633	7326.200958	27.061940
225.940207	7348.324015	27.066957
226.478772	7356.468659	27.071975
226.359348	7370.011607	27.076992
226.670545	7385.307590	27.082010
227.327195	7391.214550	27.087028
227.270853	7402.796745	27.092045
227.692153	7409.225530	27.097063
227.860565	7423.221065	27.102080
228.270788	7426.750596	27.107098
228.131868	7432.063796	27.112116
228.379003	7449.368050	27.117133
228.537129	7450.144557	27.122151
228.912500	7467.274002	27.127168
228.705090	7477.938381	27.132186
228.825314	7480.291053	27.137204
228.962723	7506.695736	27.142221
229.497269	7511.980976	27.147239
229.734664	7529.804452	27.152256
230.029046	7541.941525	27.157274
230.115074	7545.695680	27.162292
230.311270	7563.208567	27.167309
230.732800	7572.180095	27.172327
230.906107	7592.367127	27.177344
230.970383	7611.635649	27.182362
231.564317	7607.608261	27.187380
231.845898	7633.864831	27.192397
232.221679	7625.419056	27.197415
232.569627	7634.338995	27.202432
232.302443	7658.425720	27.207450
233.055933	7656.231693	27.212468
232.902534	7661.551304	27.217485
233.406214	7674.734572	27.222503
233.300702	7689.116763	27.227520
233.633912	7697.005699	27.232538
233.770942	7712.308771	27.237556
233.510011	7728.518225	27.242573
234.278066	7740.113077	27.247591
234.669737	7747.768650	27.252608
234.513224	7762.925797	27.257626
235.239179	7777.498909	27.262644
235.287086	7785.563514	27.267661
235.766612	7799.664635	27.272679
235.478006	7819.232863	27.277696
235.858857	7831.125042	27.282714
236.335321	7836.104132	27.287732
236.202798	7850.279831	27.292749
236.450792	7863.581989	27.297767
236.898036	7880.188752	27.302784
237.203122	7894.850545	27.307802
237.450179	7904.613658	27.312820
237.481338	7924.290565	27.317837
237.648019	7931.962202	27.322855
238.143614	7955.337042	27.327872
238.375041	7977.419661	27.332890
238.554942	7975.626179	27.337908
238.809992	8000.487169	27.342925
239.018560	7999.271069	27.347943
239.393440	8022.461969	27.352960
239.797031	8027.600488	27.357978
240.178791	8024.366703	27.362996
239.947493	8045.917887	27.368013
240.355916	8049.978787	27.373031
240.402216	8060.960761	27.378048
240.763301	8091.614640	27.383066
241.330432	8093.998982	27.388084
241.279755	8099.873628	27.393101
241.451637	8111.834482	27.398119
241.792168	8124.340109	27.403136
242.025653	8145.393053	27.408154
242.554892	8147.419742	27.413172
243.029872	8164.279800	27.418189
243.037623	8176.213517	27.423207
242.967133	8182.338034	27.428224
242.995014	8195.141244	27.433242
243.715262	8208.493919	27.438260
243.427912	8214.614959	27.443277
243.769431	8232.032054	27.448295
244.089779	8231.752174	27.453312
244.109458	8254.422433	27.458330
244.642386	8260.473090	27.463348
244.668581	8275.030941	27.468365
244.913576	8294.495666	27.473383
245.103719	8301.841412	27.478400
245.098408	8320.121875	27.483418
245.748985	8329.577404	27.488436
245.544986	8343.686596	27.493453
246.011583	8353.094607	27.498471
246.332950	8370.322980	27.503488
246.161433	8386.111032	27.508506
246.705602	8405.229390	27.513524
247.078203	8421.177912	27.518541
247.794319	8438.897166	27.523559
247.957979	8455.643638	27.528576
247.912555	8462.198950	27.533594
248.324232	8472.722125	27.538612
248.508981	8483.285233	27.543629
248.740572	8493.939063	27.548647
249.073425	8506.736942	27.553664
249.034234	8516.011354	27.558682
249.575584	8532.692237	27.563700
249.586435	8546.652606	27.568717
250.019903	8563.697991	27.573735
250.498002	8568.183121	27.578752
250.616229	8583.667386	27.583770
250.770036	8586.377820	27.588788
250.927182	8602.755279	27.593805
251.119895	8621.583097	27.598823
251.649302	8628.199301	27.603840
251.808763	8648.593204	27.608858
252.320411	8654.911436	27.613876
252.468900	8666.641825	27.618893
252.627224	8680.596807	27.623911
253.191684	8688.369182	27.628928
253.230949	8702.013030	27.633946
253.333026	8711.880201	27.638964
253.827005	8721.928288	27.643981
253.865108	8744.856941	27.648999
254.510976	8750.613376	27.654016
254.308377	8761.785918	27.659034
254.977612	8771.515918	27.664052
254.856971	8786.714572	27.669069
255.113622	8789.823170	27.674087
255.656613	8799.245585	27.679104
255.507125	8824.859390	27.684122
255.873426	8826.694142	27.689140
255.985303	8844.923508	27.694157
256.105248	8866.615382	27.699175
256.954860	8874.199638	27.704192
256.890925	8899.834850	27.709210
257.219328	8904.354309	27.714228
257.411841	8919.975492	27.719245
257.538695	8930.880920	27.724263
258.169453	8943.227286	27.729280
258.250639	8962.663221	27.734298
258.556831	8963.705985	27.739316
258.789772	8993.303555	27.744333
258.790791	9004.554426	27.749351
259.006524	9020.691009	27.754368
258.857091	9039.334892	27.759386
259.462722	9054.065383	27.764404
260.072455	9072.830218	27.769421
260.146474	9085.519365	27.774439
260.265148	9102.578831	27.779456
260.433591	9137.548986	27.784474
260.976682	9136.281369	27.789492
261.228778	9155.589987	27.794509
261.342250	9164.686673	27.799527
261.861521	9183.668285	27.804544
261.519783	9194.678241	27.809562
262.628617	9205.065232	27.814580
262.314061	9206.901652	27.819597
262.591478	9228.985478	27.824615
262.963345	9245.939377	27.829632
263.228530	9255.984709	27.834650
263.490677	9270.474472	27.839668
263.846466	9282.659428	27.844685
263.817418	9302.013183	27.849703
264.403872	9310.612556	27.854720
264.600952	9324.289108	27.859738
264.710683	9325.770918	27.864756
265.079596	9358.253609	27.869773
265.290852	9373.501869	27.874791
265.586194	9386.041176	27.879808
265.777945	9405.393171	27.884826
266.177667	9426.094136	27.889844
266.356920	9432.528360	27.894861
266.762646	9459.181762	27.899879
266.905378	9467.808976	27.904896
266.917592	9493.152861	27.909914
267.232129	9508.788296	27.914932
267.665312	9525.535390	27.919949
268.120035	9543.423615	27.924967
268.347849	9564.484091	27.929984
268.392425	9578.412991	27.935002
268.717400	9597.124737	27.940020
269.392005	9611.130575	27.945037
269.348730	9631.069269	27.950055
269.861438	9637.783199	27.955072
269.788529	9657.960811	27.960090
270.053979	9677.546731	27.965108
270.523461	9690.851564	27.970125
270.715658	9710.336992	27.975143
271.103757	9717.292169	27.980160
271.398039	9749.380706	27.985178
271.642822	9750.661367	27.990196
272.197904	9766.016954	27.995213
272.412070	9778.150888	28.000231
272.476219	9788.516596	28.005248
272.812499	9807.400824	28.010266
273.364170	9819.766477	28.015284
273.589188	9836.430181	28.020301
273.435400	9845.806261	28.025319
273.910256	9864.749552	28.030336
274.283645	9870.313579	28.035354
274.443262	9904.592007	28.040372
274.801093	9904.595820	28.045389
274.859356	9932.684633	28.050407
275.051799	9939.160208	28.055424
275.217728	9965.797421	28.060442
275.409413	9980.624072	28.065460
276.126583	10002.214686	28.070477
276.060580	10019.769724	28.075495
276.556358	10032.156611	28.080512
276.792011	10058.326284	28.085530
276.859266	10072.474025	28.090548
277.560423	10085.039672	28.095565
277.725547	10102.175233	28.100583
278.221822	10111.736152	28.105600
278.243135	10136.582422	28.110618
278.609642	10156.269585	28.115636
279.306248	10158.933773	28.120653
279.156237	10175.386526	28.125671
279.558334	10186.615167	28.130688
279.525520	10207.669204	28.135706
279.651707	10217.690090	28.140724
280.228367	10230.649105	28.145741
280.103443	10251.671176	28.150759
280.792229	10256.268453	28.155776
280.647568	10278.220323	28.160794
280.983682	10294.498980	28.165812
281.654375	10302.182083	28.170829
281.611182	10320.552239	28.175847
282.133419	10332.734868	28.180864
282.214476	10350.625968	28.185882
282.672312	10370.583476	28.190900
283.165440	10378.529996	28.195917
283.458189	10402.731411	28.200935
283.587570	10403.114964	28.205952
283.693670	10430.289129	28.210970
283.743900	10443.020313	28.215988
284.054816	10456.986248	28.221005
284.163954	10483.400513	28.226023
284.817047	10503.040665	28.231040
284.930099	10517.121339	28.236058
285.246127	10545.436423	28.241076
285.773197	10567.123868	28.246093
285.761305	10589.135333	28.251111
286.071060	10602.945591	28.256128
286.308912	10632.688755	28.261146
286.600918	10650.660298	28.266164
286.995189	10661.607726	28.271181
287.289847	10692.050669	28.276199
287.616022	10700.357461	28.281216
287.814905	10726.873873	28.286234
288.208651	10738.300460	28.291252
288.745192	10764.382871	28.296269
288.857903	10778.983819	28.301287
289.310729	10791.350828	28.306304
289.722624	10807.942849	28.311322
290.002729	10836.592142	28.316340
290.568391	10846.896792	28.321357
290.530084	10864.264590	28.326375
290.855696	10877.435862	28.331392
291.049074	10900.452185	28.336410
291.104376	10914.629430	28.341428
291.550048	10932.400945	28.346445
291.688256	10958.964023	28.351463
291.843090	10975.223738	28.356480
291.946577	10999.800888	28.361498
292.368105	11025.502519	28.366516
293.144695	11050.508816	28.371533
293.090522	11070.463697	28.376551
293.906924	11094.068929	28.381568
294.388874	11106.355724	28.386586
294.346751	11110.453382	28.391604
294.623400	11123.538415	28.396621
295.121904	11143.406634	28.401639
295.519519	11155.721608	28.406656
295.579183	11178.820338	28.411674
295.702631	11200.375321	28.416692
296.195167	11216.642414	28.421709
296.059724	11238.859577	28.426727
296.657180	11247.610239	28.431744
296.988243	11259.745639	28.436762
296.940302	11284.984899	28.441780
297.634253	11300.752309	28.446797
297.841905	11327.290316	28.451815
297.884689	11339.783920	28.456832
298.337516	11361.952732	28.461850
298.457142	11387.060413	28.466868
298.779782	11400.755765	28.471885
299.324337	11434.121224	28.476903
299.531538	11442.132934	28.481920
300.160161	11462.758451	28.486938
300.085558	11472.359522	28.491956
300.387568	11494.261956	28.496973
300.955820	11501.496947	28.501991
301.219004	11518.029221	28.507008
301.389375	11532.696944	28.512026
301.312471	11543.700900	28.517044
301.996817	11554.835718	28.522061
302.133403	11569.301061	28.527079
302.454519	11588.679175	28.532096
303.102331	11599.779101	28.537114
302.934334	11627.284289	28.542132
303.636919	11637.532117	28.547149
303.563436	11660.002761	28.552167
303.739263	11673.610763	28.557184
304.041818	11689.736439	28.562202
304.396996	11712.586889	28.567220
304.960858	11738.021843	28.572237
304.751297	11763.655763	28.577255
305.074075	11775.079075	28.582272
305.755992	11802.246906	28.587290
306.177937	11825.609638	28.592308
306.800671	11842.867495	28.597325
306.531260	11863.757200	28.602343
307.040180	11881.506686	28.607360
307.181585	11901.644531	28.612378
307.397853	11930.837384	28.617396
307.975550	11942.530637	28.622413
308.237983	11972.387232	28.627431
308.639849	11990.956661	28.632448
309.036630	12015.152726	28.637466
309.369418	12030.476359	28.642484
309.925615	12047.215963	28.647501
310.272432	12067.223888	28.652519
310.373298	12078.179871	28.657536
310.798113	12088.886837	28.662554
311.015218	12118.579435	28.667572
311.102054	12117.972556	28.672589
311.361697	12147.259474	28.677607
311.501220	12169.134560	28.682624
312.164323	12184.821270	28.687642
312.036205	12213.373525	28.692660
312.505803	12234.527475	28.697677
313.110863	12263.390253	28.702695
313.404390	12282.972324	28.707712
313.944254	12294.859624	28.712730
313.847828	12319.103107	28.717748
314.299541	12328.296090	28.722765
314.617206	12348.135840	28.727783
314.712892	12374.470317	28.732800
315.225826	12395.623608	28.737818
315.207954	12420.131595	28.742836
315.871414	12443.464700	28.747853
316.011582	12466.129598	28.752871
316.196209	12499.251102	28.757888
316.768363	12510.102581	28.762906
317.024348	12542.704924	28.767924
317.293942	12554.848319	28.772941
317.679902	12581.700835	28.777959
317.900804	12608.858074	28.782976
318.107769	12624.308679	28.787994
318.422555	12652.044568	28.793012
318.849844	12680.969031	28.798029
319.441848	12694.263163	28.803047
319.398741	12721.618727	28.808064
320.120847	12740.183288	28.813082
320.203083	12760.803189	28.818100
320.229943	12782.384139	28.823117
320.823646	12814.247179	28.828135
321.019129	12832.528667	28.833152
321.818960	12846.225058	28.838170
321.781043	12866.036042	28.843188
322.331328	12885.713448	28.848205
322.909038	12896.184469	28.853223
322.779213	12914.502556	28.858240
323.323517	12916.666069	28.863258
323.322526	12949.381100	28.868276
323.757581	12957.113153	28.873293
324.200146	12970.760043	28.878311
324.307917	13000.891547	28.883328
324.852882	13016.472543	28.888346
324.631418	13037.048503	28.893364
324.851421	13059.819210	28.898381
325.708102	13085.242484	28.903399
325.798662	13122.238750	28.908416
326.402213	13128.962754	28.913434
326.383391	13162.915137	28.918452
326.602378	13178.101093	28.923469
326.901060	13205.763368	28.928487
327.125769	13234.218036	28.933504
327.573611	13257.978838	28.938522
327.763043	13295.529632	28.943540
328.251789	13312.560655	28.948557
328.690079	13341.990358	28.953575
329.002175	13377.997072	28.958592
329.413898	13389.717268	28.963610
329.654454	13418.987569	28.968628
330.107462	13440.694277	28.973645
330.979269	13466.301611	28.978663
331.114554	13491.742481	28.983680
331.118470	13512.541774	28.988698
331.514449	13542.038729	28.993716
331.961998	13550.889530	28.998733
332.594244	13576.141112	29.003751
332.674561	13597.917595	29.008768
333.128393	13620.792223	29.013786
333.350355	13646.535764	29.018804
333.408305	13660.248467	29.023821
334.369731	13682.044710	29.028839
334.539623	13711.262613	29.033856
335.190123	13724.406069	29.038874
335.048201	13755.595243	29.043892
335.506325	13772.937563	29.048909
335.948378	13785.806669	29.053927
335.925321	13813.045690	29.058944
336.338163	13829.021275	29.063962
336.867815	13851.048385	29.068980
336.999362	13875.916799	29.073997
337.446102	13896.744154	29.079015
337.656774	13922.628689	29.084032
338.265373	13939.385214	29.089050
338.539906	13955.147408	29.094068
338.631471	13980.865777	29.099085
339.389376	14004.727649	29.104103
339.505643	14030.170928	29.109120
339.503775	14045.802440	29.114138
339.650800	14074.605549	29.119156
340.035538	14101.309470	29.124173
340.619871	14126.661245	29.129191
340.671119	14151.812872	29.134208
341.212420	14177.671457	29.139226
341.990682	14204.977087	29.144244
342.272482	14226.873937	29.149261
342.656848	14248.706558	29.154279
342.936708	14286.996442	29.159296
343.702838	14293.621527	29.164314
343.892897	14312.157740	29.169332
343.964892	14324.453364	29.174349
344.363539	14341.468853	29.179367
344.321295	14371.194289	29.184384
344.933850	14387.118453	29.189402
345.061430	14409.679382	29.194420
345.509479	14431.760185	29.199437
345.749052	14448.464832	29.204455
345.801878	14474.431527	29.209472
346.108451	14495.315941	29.214490
346.529859	14525.417255	29.219508
346.936782	14542.232996	29.224525
347.521747	14565.222788	29.229543
347.528218	14597.367753	29.234560
348.120844	14624.126381	29.239578
348.664569	14654.196654	29.244596
348.512529	14670.753569	29.249613
349.147160	14695.852030	29.254631
349.245029	14727.242929	29.259648
349.886808	14751.443487	29.264666
350.020929	14781.236617	29.269684
350.268198	14811.594237	29.274701
351.009923	14826.101012	29.279719
351.019395	14860.105813	29.284736
351.764355	14877.723362	29.289754
352.299709	14906.561379	29.294772
352.411131	14940.803230	29.299789
352.879484	14958.573823	29.304807
353.020523	14984.616562	29.309824
353.536327	15003.044478	29.314842
353.921296	15039.537689	29.319860
353.720419	15058.336464	29.324877
354.515100	15079.112466	29.329895
354.330426	15114.519592	29.334912
355.001728	15145.428650	29.339930
355.270236	15179.331344	29.344948
355.687201	15213.157525	29.349965
356.617962	15240.130718	29.354983
356.457192	15270.547261	29.360000
357.154633	15296.618195	29.365018
357.750727	15322.660236	29.370036
357.934188	15347.695663	29.375053
358.592585	15371.593339	29.380071
358.821172	15392.961501	29.385088
359.418930	15410.725353	29.390106
359.702097	15434.921649	29.395124
359.702618	15468.237245	29.400141
360.542029	15479.262416	29.405159
360.522108	15509.115458	29.410176
361.247487	15521.390530	29.415194
361.013578	15544.580269	29.420212
361.586804	15563.010345	29.425229
361.937873	15578.504514	29.430247
361.960175	15609.728339	29.435264
362.513187	15629.321913	29.440282
362.516351	15662.957431	29.445300
363.014171	15696.186453	29.450317
363.173508	15724.148722	29.455335
363.944412	15754.593225	29.460352
363.986817	15783.708240	29.465370
364.710546	15811.640297	29.470388
364.881440	15842.114911	29.475405
365.398172	15863.837930	29.480423
365.737944	15892.617050	29.485440
366.109467	15916.856175	29.490458
366.716464	15938.600607	29.495476
366.802330	15977.144049	29.500493
367.514624	15995.672964	29.505511
367.791230	16022.144131	29.510528
368.150428	16044.082608	29.515546
368.362179	16056.863943	29.520564
368.658790	16090.986110	29.525581
369.451145	16101.942256	29.530599
369.139412	16126.427173	29.535616
369.657241	16144.427298	29.540634
369.946576	16157.063466	29.545652
370.252830	16190.834317	29.550669
370.614818	16220.565539	29.555687
370.953196	16252.915727	29.560704
371.238930	16279.661641	29.565722
371.982976	16306.650151	29.570740
372.323076	16330.149513	29.575757
372.773599	16346.832210	29.580775
373.202966	16376.672358	29.585792
373.161920	16419.473262	29.590810
373.724490	16441.618202	29.595828
373.764630	16470.487325	29.600845
374.370988	16492.281459	29.605863
374.646519	16540.421148	29.610880
374.868454	16555.084840	29.615898
375.907869	16587.379560	29.620916
376.380879	16624.786988	29.625933
376.867756	16644.547191	29.630951
377.385552	16654.786224	29.635968
377.404734	16676.967816	29.640986
377.811201	16703.882014	29.646004
378.072657	16728.668606	29.651021
378.612241	16749.947648	29.656039
378.798565	16783.657590	29.661056
378.972713	16810.506373	29.666074
379.672789	16829.047707	29.671092
379.726052	16864.784900	29.676109
380.110213	16889.464728	29.681127
380.484919	16926.709408	29.686144
380.732797	16957.819626	29.691162
381.224482	16989.376637	29.696180
381.692406	17025.382883	29.701197
382.131875	17052.607451	29.706215
382.292835	17078.301825	29.711232
382.744015	17124.785790	29.716250
383.358855	17148.034344	29.721268
383.681733	17193.018567	29.726285
384.161619	17200.179310	29.731303
384.569734	17232.151005	29.736320
385.050144	17255.822352	29.741338
385.371006	17288.648790	29.746356
385.526165	17321.855821	29.751373
386.370285	17333.471024	29.756391
386.900496	17364.347693	29.761408
387.265643	17394.636956	29.766426
387.661224	17419.340905	29.771444
387.853695	17449.840128	29.776461
388.410028	17470.299189	29.781479
388.486728	17495.041838	29.786496
389.026363	17520.459839	29.791514
389.603435	17551.792556	29.796532
389.654797	17573.437204	29.801549
389.974931	17598.571646	29.806567
390.774340	17622.379889	29.811584
390.772073	17656.080250	29.816602
391.378894	17678.230559	29.821620
391.334667	17707.106336	29.826637
392.071236	17737.552297	29.831655
392.601172	17766.151868	29.836672
393.076047	17781.104252	29.841690
393.554861	17799.861429	29.846708
393.714089	17831.241755	29.851725
394.331314	17846.613609	29.856743
394.666322	17864.603302	29.861760
394.770787	17884.927997	29.866778
395.315004	17896.066711	29.871796
395.436601	17922.311188	29.876813
395.716499	17943.388821	29.881831
396.258246	17968.367340	29.886848
396.425253	17990.367002	29.891866
396.894683	18025.440352	29.896884
397.106985	18061.473809	29.901901
397.605329	18089.744964	29.906919
397.988946	18121.400834	29.911936
398.170785	18155.855223	29.916954
398.576842	18182.828639	29.921972
398.837079	18223.451404	29.926989
399.434878	18250.183530	29.932007
399.662307	18285.409405	29.937024
399.958804	18321.396384	29.942042
400.629901	18361.070252	29.947060
401.143378	18394.625271	29.952077
401.624173	18420.990804	29.957095
402.181709	18454.917003	29.962112
402.640980	18485.222627	29.967130
402.927773	18511.730762	29.972148
403.467846	18538.961611	29.977165
403.935981	18571.063101	29.982183
404.262414	18603.356786	29.987200
404.535894	18633.379708	29.992218
404.771276	18667.140522	29.997236
405.265486	18703.473960	30.002253
405.646853	18728.954685	30.007271
406.160338	18762.682280	30.012288
406.139036	18802.637319	30.017306
406.905116	18831.886994	30.022324
407.181182	18882.029215	30.027341
407.731068	18901.783258	30.032359
408.390485	18935.012523	30.037376
408.295363	18964.420718	30.042394
408.819540	18995.096465	30.047412
409.258212	19032.931193	30.052429
409.802267	19071.142696	30.057447
410.607534	19099.839304	30.062464
410.791561	19134.205486	30.067482
411.359829	19169.701582	30.072500
411.498146	19206.999941	30.077517
412.367483	19232.515766	30.082535
412.688172	19261.042176	30.087552
412.909059	19291.150655	30.092570
413.447877	19318.091324	30.097588
413.906919	19339.180487	30.102605
414.319636	19379.834429	30.107623
414.955238	19392.152475	30.112640
414.954534	19435.665464	30.117658
415.482103	19458.832373	30.122676
416.117702	19493.110371	30.127693
416.071380	19520.509233	30.132711
416.694641	19547.690123	30.137728
417.063275	19583.212252	30.142746
417.463360	19611.456526	30.147764
417.712511	19653.544502	30.152781
417.914694	19681.241464	30.157799
418.510866	19713.268778	30.162816
419.148169	19750.430587	30.167834
419.653927	19780.871184	30.172852
420.139804	19812.675723	30.177869
420.291467	19842.903857	30.182887
420.717629	19875.390026	30.187904
420.971927	19915.775083	30.192922
421.759412	19937.851203	30.197940
421.989516	19976.764712	30.202957
422.082175	20000.425297	30.207975
422.742668	20020.096142	30.212992
423.052622	20053.063832	30.218010
423.409437	20082.804383	30.223028
424.006396	20116.393187	30.228045
424.201739	20138.124534	30.233063
424.758327	20168.639407	30.238080
424.796120	20204.775725	30.243098
425.450947	20240.417428	30.248116
426.045145	20273.236031	30.253133
426.215673	20313.662710	30.258151
426.862439	20349.830999	30.263168
427.068316	20382.685698	30.268186
427.760767	20409.883341	30.273204
428.285800	20449.772380	30.278221
428.537453	20480.245259	30.283239
429.125140	20510.446583	30.288256
429.679638	20557.291936	30.293274
430.248646	20586.161056	30.298292
430.484969	20612.305620	30.303309
430.773092	20654.501594	30.308327
431.065401	20671.287340	30.313344
431.607820	20719.459547	30.318362
431.785604	20752.267585	30.323380
432.333698	20790.884390	30.328397
432.862253	20825.301075	30.333415
433.341705	20862.335375	30.338432
433.791742	20908.369654	30.343450
434.056886	20939.244763	30.348468
434.941068	20982.024050	30.353485
435.023870	21022.074346	30.358503
435.425274	21052.553435	30.363520
435.854471	21090.276113	30.368538
436.274473	21132.637510	30.373556
436.948280	21173.881692	30.378573
437.549621	21204.113535	30.383591
438.346159	21230.218381	30.388608
438.315045	21264.692315	30.393626
438.801042	21293.437633	30.398644
439.258286	21326.011331	30.403661
439.681401	21369.118601	30.408679
440.611944	21395.540526	30.413696
440.744464	21428.846157	30.418714
441.146238	21464.555981	30.423732
441.477617	21500.848312	30.428749
441.937506	21541.766141	30.433767
442.522993	21569.125267	30.438784
442.884435	21611.309922	30.443802
443.131251	21642.257150	30.448820
443.688294	21684.838498	30.453837
444.080084	21715.016058	30.458855
444.811944	21750.714435	30.463872
445.109055	21781.254671	30.468890
445.271991	21812.547213	30.473908
445.750061	21849.970218	30.478925
445.945562	21888.488628	30.483943
446.606347	21920.361233	30.488960
447.212937	21970.254546	30.493978
447.489502	21995.877404	30.498996
448.088088	22034.988542	30.504013
448.502120	22079.715342	30.509031
448.895808	22107.996397	30.514048
449.340199	22153.519384	30.519066
449.623910	22191.875665	30.524084
450.176980	22230.737768	30.529101
450.337878	22274.581380	30.534119
451.016128	22309.665387	30.539136
451.663723	22340.721019	30.544154
451.950017	22368.441585	30.549172
452.543298	22400.712588	30.554189
452.692965	22430.009043	30.559207
453.255775	22456.051970	30.564224
453.742903	22500.297885	30.569242
454.232054	22524.173913	30.574260
454.726217	22565.298262	30.579277
454.894757	22617.922956	30.584295
455.451396	22640.185898	30.589312
455.868445	22680.692546	30.594330
456.153548	22717.118132	30.599348
456.645462	22761.338706	30.604365
457.169917	22793.754303	30.609383
458.224981	22831.170720	30.614400
458.639925	22872.953863	30.619418
458.740618	22913.322614	30.624436
459.209842	22943.536853	30.629453
459.359254	22987.493007	30.634471
460.050963	23021.149177	30.639488
460.667984	23070.060018	30.644506
460.712015	23103.334692	30.649524
461.150256	23150.373611	30.654541
461.965089	23202.618782	30.659559
462.222755	23230.153107	30.664576
462.480282	23288.027288	30.669594
463.315819	23319.488839	30.674612
463.937347	23366.718793	30.679629
464.377767	23407.745264	30.684647
464.960078	23450.937130	30.689664
465.474812	23487.064594	30.694682
466.247165	23533.352278	30.699700
466.775123	23556.341827	30.704717
466.954610	23602.179030	30.709735
467.415631	23631.396065	30.714752
467.877102	23671.632792	30.719770
468.349734	23697.684661	30.724788
468.947195	23739.419225	30.729805
469.295735	23784.897782	30.734823
469.820907	23812.123852	30.739840
470.267066	23853.934196	30.744858
470.802102	23890.418703	30.749876
471.522419	23925.998985	30.754893
471.571408	23962.346453	30.759911
472.137408	23996.315517	30.764928
472.595165	24039.956847	30.769946
472.883435	24078.523205	30.774964
473.523953	24112.902803	30.779981
474.015471	24155.078548	30.784999
474.398525	24192.355268	30.790016
474.901354	24237.591872	30.795034
475.380283	24279.296905	30.800052
475.846368	24312.576634	30.805069
476.298313	24352.699842	30.810087
477.087322	24389.695342	30.815104
477.615484	24424.929978	30.820122
477.429334	24475.535845	30.825140
478.175547	24502.215483	30.830157
478.413243	24554.278007	30.835175
478.780965	24593.803828	30.840192
479.645903	24639.505149	30.845210
479.787318	24691.123525	30.850228
480.694728	24719.120468	30.855245
480.930804	24760.500984	30.860263
481.504266	24791.388840	30.865280
481.899024	24836.443045	30.870298
482.136639	24870.685819	30.875316
482.900667	24906.147360	30.880333
483.343504	24946.797051	30.885351
484.129899	24986.043170	30.890368
484.437268	25024.394014	30.895386
484.605844	25064.997897	30.900404
485.418795	25087.097036	30.905421
485.597544	25138.735811	30.910439
486.253903	25177.398286	30.915456
486.879743	25211.978079	30.920474
487.167126	25249.042672	30.925492
487.909684	25284.533783	30.930509
488.002986	25327.800265	30.935527
489.049265	25360.235321	30.940544
489.185714	25400.640289	30.945562
489.972912	25436.947578	30.950580
490.491066	25475.147843	30.955597
490.662944	25523.101615	30.960615
490.907321	25560.905779	30.965632
491.513010	25598.716477	30.970650
491.781477	25640.573198	30.975668
492.363645	25677.160954	30.980685
492.552615	25735.685591	30.985703
493.200991	25782.239595	30.990720
494.099981	25824.068130	30.995738
494.335786	25877.753123	31.000756
495.011581	25925.649864	31.005773
495.396897	25959.094402	31.010791
495.988961	26005.793964	31.015808
496.571349	26049.684741	31.020826
496.879887	26092.233034	31.025844
497.812570	26141.147726	31.030861
497.966663	26186.727904	31.035879
498.940647	26233.263946	31.040896
499.176083	26266.923144	31.045914
499.692366	26316.579117	31.050932
500.279103	26353.580778	31.055949
500.786196	26393.522977	31.060967
501.305328	26439.992893	31.065984
501.567310	26476.953923	31.071002
502.474638	26527.940048	31.076020
503.261315	26553.833886	31.081037
503.381310	26600.755119	31.086055
503.763745	26632.425492	31.091072
504.276643	26674.408303	31.096090
504.866128	26718.252289	31.101108
505.557814	26760.653658	31.106125
506.036663	26798.693017	31.111143
506.593675	26836.044467	31.116160
507.152922	26870.733245	31.121178
507.493385	26920.164531	31.126196
508.323473	26960.631867	31.131213
508.790694	26997.626293	31.136231
509.390535	27029.731441	31.141248
509.657920	27069.588685	31.146266
509.836629	27121.974706	31.151284
510.708261	27151.132940	31.156301
510.623586	27188.767984	31.161319
511.295495	27232.637490	31.166336
511.771726	27278.996884	31.171354
512.102813	27325.418274	31.176372
512.870999	27374.029293	31.181389
513.301477	27416.298833	31.186407
513.759650	27464.220074	31.191424
514.155352	27505.400942	31.196442
514.707672	27557.679137	31.201460
515.428731	27592.831551	31.206477
516.127225	27650.795692	31.211495
516.651265	27695.835966	31.216512
516.945684	27729.860491	31.221530
517.278905	27769.938737	31.226548
518.176209	27803.380988	31.231565
518.255159	27847.186120	31.236583
518.588367	27891.135416	31.241600
519.436928	27923.336715	31.246618
519.654580	27977.416083	31.251636
520.389372	28023.775693	31.256653
520.610478	28072.942931	31.261671
521.265241	28113.038167	31.266688
521.673823	28163.909730	31.271706
521.705423	28214.134005	31.276724
522.862466	28263.992384	31.281741
523.206176	28319.698728	31.286759
523.550176	28366.070281	31.291776
524.218394	28408.640453	31.296794
524.726176	28459.117892	31.301812
525.365413	28514.103991	31.306829
526.025857	28567.503050	31.311847
526.477601	28616.964911	31.316864
527.197231	28663.820882	31.321882
527.586178	28714.567953	31.326900
528.024212	28758.035176	31.331917
528.790962	28818.957447	31.336935
529.207695	28868.652962	31.341952
529.971923	28918.575058	31.346970
530.584041	28963.941604	31.351988
530.911551	29020.652955	31.357005
531.485504	29064.051126	31.362023
532.003448	29108.704853	31.367040
532.521766	29160.170055	31.372058
532.915553	29219.076355	31.377076
533.636296	29267.334541	31.382093
534.180149	29308.255380	31.387111
534.781896	29372.967553	31.392128
535.414667	29417.451632	31.397146
535.737554	29476.534586	31.402164
536.114483	29509.851682	31.407181
536.897319	29567.221414	31.412199
537.186611	29612.999570	31.417216
537.842409	29658.843403	31.422234
538.335446	29723.470743	31.427252
539.198132	29766.012046	31.432269
539.418364	29808.931084	31.437287
539.860583	29877.933941	31.442304
540.679947	29919.028317	31.447322
541.124325	29985.166467	31.452340
541.369534	30026.160481	31.457357
542.031646	30096.052240	31.462375
542.850266	30147.268726	31.467392
543.830167	30188.535942	31.472410
544.210443	30232.682101	31.477428
544.947924	30276.901783	31.482445
545.306340	30333.893067	31.487463
545.561033	30373.996581	31.492480
546.497285	30409.911000	31.497498
546.852349	30465.171101	31.502516
547.322866	30517.948108	31.507533
548.164141	30570.714410	31.512551
548.593643	30622.466782	31.517568
549.218320	30658.212400	31.522586
549.581348	30708.871716	31.527604
549.901796	30756.383040	31.532621
550.550297	30806.948076	31.537639
550.787722	30861.443241	31.542656
551.626083	30903.341354	31.547674
552.048423	30960.267292	31.552692
552.513320	31007.872135	31.557709
553.077634	31057.814465	31.562727
553.499468	31113.589319	31.567744
554.093195	31156.733816	31.572762
554.468213	31212.974242	31.577780
555.271573	31255.901290	31.582797
556.261695	31296.866511	31.587815
556.290090	31349.078634	31.592832
557.174305	31397.788918	31.597850
557.314016	31446.578344	31.602868
557.772862	31496.400531	31.607885
558.397015	31551.755189	31.612903
559.139656	31605.332894	31.617920
559.818861	31655.292612	31.622938
560.060361	31704.999891	31.627956
560.864158	31765.585468	31.632973
561.121963	31825.466436	31.637991
561.379031	31881.334080	31.643008
562.467373	31938.380160	31.648026
562.776525	31996.634493	31.653044
563.330296	32049.938719	31.658061
563.990702	32113.095630	31.663079
564.174434	32181.228871	31.668096
564.804732	32226.108571	31.673114
565.365563	32287.648057	31.678132
566.109595	32358.330390	31.683149
566.307529	32413.527910	31.688167
566.842388	32483.238751	31.693184
567.722938	32541.599127	31.698202
568.264017	32616.967277	31.703220
568.933643	32689.196816	31.708237
569.488058	32735.705990	31.713255
570.029590	32807.752095	31.718272
570.701603	32865.071995	31.723290
571.295091	32939.464083	31.728308
572.138163	32997.958381	31.733325
572.386077	33062.594302	31.738343
572.994780	33138.960107	31.743360
573.930098	33191.683954	31.748378
574.501205	33256.308127	31.753396
575.138118	33320.012823	31.758413
575.573514	33364.952890	31.763431
576.312107	33429.676206	31.768448
577.134934	33486.490338	31.773466
577.737122	33543.650411	31.778484
578.237655	33604.090469	31.783501
578.817689	33651.923185	31.788519
579.166276	33717.273786	31.793536
579.767816	33777.751366	31.798554
580.396404	33836.220787	31.803572
580.714251	33898.598127	31.808589
581.556956	33957.161904	31.813607
582.058221	34013.305091	31.818624
582.940787	34063.925885	31.823642
583.698247	34135.477725	31.828660
583.830812	34179.901904	31.833677
584.511750	34232.128118	31.838695
584.828324	34300.294804	31.843712
585.834773	34354.244240	31.848730
586.477189	34424.194175	31.853748
586.946406	34477.999337	31.858765
587.541613	34525.023982	31.863783
588.088446	34586.488504	31.868800
588.896293	34651.577176	31.873818
589.585398	34690.419321	31.878836
589.748911	34753.876079	31.883853
590.827891	34796.529385	31.888871
591.132675	34862.052356	31.893888
591.685561	34913.001505	31.898906
592.215733	34967.173603	31.903924
592.490002	35016.868900	31.908941
593.434443	35067.810513	31.913959
593.479201	35119.390294	31.918976
594.293894	35173.828381	31.923994
594.956119	35229.134504	31.929012
595.411095	35285.068411	31.934029
595.945594	35331.341463	31.939047
596.549741	35395.024242	31.944064
597.525658	35446.024841	31.949082
597.870999	35508.179144	31.954100
598.557422	35574.720928	31.959117
599.166828	35631.091140	31.964135
599.509363	35690.686985	31.969152
600.097897	35743.482036	31.974170
600.740201	35806.954813	31.979188
601.266111	35873.647343	31.984205
602.112209	35931.083964	31.989223
602.839327	35993.173619	31.994240
603.123108	36057.596616	31.999258
603.733930	36114.015444	32.004276
604.472045	36179.342108	32.009293
605.154399	36239.820917	32.014311
605.341498	36308.871941	32.019328
606.128850	36369.860893	32.024346
606.718907	36440.998264	32.029364
607.192600	36508.484509	32.034381
608.221515	36579.931720	32.039399
608.653036	36640.507022	32.044416
609.159470	36706.192697	32.049434
610.047049	36761.554607	32.054452
610.304433	36837.284094	32.059469
611.125605	36896.631129	32.064487
611.607895	36974.290330	32.069504
612.285727	37042.148791	32.074522
613.195801	37106.200459	32.079540
613.893725	37169.211149	32.084557
614.534976	37229.794753	32.089575
615.172574	37295.514519	32.094592
615.883168	37360.676398	32.099610
616.615912	37417.385280	32.104628
616.741475	37486.100607	32.109645
617.588851	37534.988352	32.114663
618.179667	37614.986993	32.119680
618.590120	37680.578441	32.124698
619.437495	37744.721644	32.129716
620.114539	37810.537750	32.134733
620.535704	37869.370204	32.139751
621.289192	37937.509882	32.144768
621.897272	37994.099147	32.149786
622.375436	38055.924562	32.154804
622.860763	38137.619033	32.159821
623.524902	38203.760655	32.164839
624.371388	38280.440324	32.169856
624.888133	38343.816488	32.174874
625.619900	38406.238749	32.179892
626.014496	38486.261048	32.184909
626.851936	38544.262926	32.189927
627.519934	38609.076470	32.194944
627.742975	38673.124209	32.199962
628.578799	38742.572719	32.204980
629.144546	38819.632538	32.209997
629.831504	38878.992458	32.215015
630.435069	38955.547848	32.220032
630.888638	39020.830782	32.225050
631.566395	39084.760540	32.230068
632.153400	39166.202877	32.235085
632.922261	39235.358139	32.240103
633.710209	39292.363600	32.245120
634.119518	39353.816521	32.250138
635.004830	39411.298688	32.255156
635.388504	39476.064480	32.260173
635.878067	39537.687829	32.265191
636.490303	39618.547163	32.270208
636.817784	39673.568639	32.275226
637.832940	39739.042171	32.280244
638.158566	39816.770940	32.285261
639.263581	39881.908125	32.290279
639.910362	39947.424402	32.295296
640.069145	40014.773671	32.300314
640.991094	40091.394769	32.305332
641.530235	40164.717493	32.310349
641.907961	40232.905779	32.315367
642.803008	40310.356174	32.320384
643.482210	40381.800362	32.325402
643.734465	40454.966506	32.330420
644.725308	40533.762606	32.335437
645.802399	40598.761733	32.340455
646.458200	40677.364480	32.345472
646.561311	40751.187853	32.350490
647.556646	40811.892049	32.355508
648.180878	40892.856012	32.360525
649.115940	40953.450682	32.365543
649.582583	41037.914010	32.370560
649.998062	41119.443872	32.375578
650.820415	41193.437309	32.380596
651.378144	41259.506511	32.385613
651.835063	41328.954859	32.390631
652.792473	41409.869122	32.395648
653.361948	41489.518796	32.400666
654.173756	41562.590436	32.405684
654.527751	41642.396383	32.410701
655.414914	41716.018121	32.415719
655.898979	41800.106346	32.420736
656.398529	41881.755092	32.425754
657.230664	41947.475108	32.430772
658.062284	42025.375706	32.435789
658.843741	42099.625783	32.440807
659.548001	42179.818095	32.445824
659.970078	42258.131551	32.450842
661.015015	42327.322183	32.455860
661.613573	42407.637151	32.460877
662.238391	42482.505068	32.465895
663.012371	42553.193688	32.470912
663.399642	42627.700517	32.475930
664.219724	42697.539073	32.480948
664.883847	42778.413099	32.485965
665.553897	42843.894729	32.490983
666.190377	42920.530555	32.496000
666.807236	43001.549131	32.501018
667.901760	43069.963936	32.506036
668.166142	43152.020245	32.511053
668.954838	43228.777392	32.516071
669.749685	43291.966658	32.521088
670.286801	43369.716368	32.526106
671.238865	43436.116421	32.531124
671.475973	43507.197421	32.536141
672.110811	43589.248037	32.541159
672.923365	43664.945296	32.546176
673.544081	43743.850976	32.551194
674.259762	43811.895445	32.556212
674.489891	43900.458725	32.561229
675.593196	43967.924970	32.566247
676.345255	44034.941209	32.571264
676.774246	44112.560329	32.576282
678.205847	44184.560891	32.581300
678.697600	44255.829942	32.586317
679.091776	44314.722089	32.591335
679.749135	44373.608774	32.596352
680.267959	44445.508732	32.601370
681.180957	44511.656984	32.606388
681.577746	44579.678050	32.611405
682.339860	44648.993534	32.616423
682.713578	44715.547472	32.621440
683.147031	44799.752285	32.626458
683.832962	44876.031114	32.631476
684.563165	44958.248762	32.636493
684.938000	45033.471361	32.641511
685.939138	45121.129742	32.646528
686.663294	45201.852719	32.651546
687.756586	45275.792249	32.656564
688.140125	45347.146485	32.661581
688.723496	45435.469085	32.666599
689.548277	45509.861296	32.671616
690.059655	45604.568899	32.676634
690.842100	45669.299722	32.681652
691.599677	45754.945638	32.686669
692.378416	45839.745312	32.691687
693.285039	45909.881494	32.696704
693.544281	45996.027767	32.701722
694.601402	46083.681355	32.706740
695.220710	46169.667802	32.711757
696.125854	46250.333737	32.716775
696.986582	46332.106301	32.721792
697.190054	46414.338468	32.726810
698.243231	46487.863061	32.731828
698.543034	46577.883158	32.736845
699.007726	46662.170037	32.741863
700.163642	46746.630317	32.746880
700.761356	46835.680236	32.751898
701.287653	46915.865343	32.756916
702.231177	47005.357810	32.761933
702.755903	47089.936660	32.766951
703.824538	47174.681711	32.771968
704.510295	47270.862516	32.776986
704.925546	47342.380065	32.782004
705.871613	47425.804344	32.787021
706.458900	47521.939543	32.792039
707.238204	47595.646363	32.797056
708.024942	47696.691841	32.802074
708.568320	47763.635802	32.807092
709.492718	47856.893576	32.812109
709.809167	47945.003550	32.817127
710.864209	48022.970945	32.822144
711.171112	48123.381153	32.827162
712.139529	48205.901907	32.832180
712.899942	48294.230600	32.837197
713.839570	48391.496209	32.842215
714.407182	48475.038202	32.847232
715.062379	48557.005903	32.852250
715.689135	48637.772207	32.857268
716.597544	48730.203102	32.862285
717.153842	48818.062651	32.867303
718.261387	48890.305250	32.872320
718.791155	48985.547722	32.877338
719.710900	49070.540570	32.882356
720.510267	49148.618006	32.887373
720.973644	49236.766455	32.892391
722.267058	49316.661016	32.897408
722.634159	49397.167102	32.902426
723.621421	49462.957087	32.907444
724.331805	49549.325838	32.912461
724.810822	49630.569243	32.917479
725.782332	49702.429963	32.922496
726.256319	49792.584798	32.927514
727.027581	49846.763507	32.932532
727.226170	49912.950798	32.937549
728.224747	50000.644668	32.942567
729.260766	50077.925533	32.947584
729.426863	50159.879891	32.952602
730.320375	50226.528152	32.957620
730.870147	50311.830878	32.962637
731.277172	50390.385691	32.967655
732.039919	50480.859202	32.972672
732.804466	50575.672707	32.977690
733.855523	50651.563608	32.982708
734.392839	50737.862066	32.987725
735.026168	50818.339506	32.992743
736.321847	50911.910751	32.997760
736.885354	50988.395316	33.002778
737.623472	51083.961116	33.007796
738.104708	51162.468876	33.012813
739.293614	51248.181705	33.017831
740.122298	51319.633003	33.022848
740.983317	51408.957460	33.027866
741.971418	51476.377733	33.032884
742.603144	51559.170687	33.037901
743.205880	51640.060909	33.042919
743.867270	51717.486091	33.047936
744.433662	51805.294361	33.052954
745.228418	51883.885839	33.057972
745.934362	51973.200631	33.062989
746.580903	52067.522892	33.068007
747.413876	52146.980940	33.073024
747.390249	52239.197390	33.078042
748.591345	52340.498716	33.083060
749.427726	52429.016939	33.088077
750.101017	52534.443607	33.093095
751.226344	52613.722523	33.098112
751.641108	52721.732715	33.103130
752.372867	52806.333945	33.108148
753.302638	52898.667466	33.113165
753.828115	52989.684673	33.118183
754.739703	53074.023550	33.123200
755.865842	53173.553612	33.128218
756.622716	53264.198965	33.133236
757.414055	53352.558226	33.138253
758.243835	53443.925241	33.143271
759.266867	53518.302971	33.148288
759.447117	53614.112421	33.153306
760.524479	53698.015882	33.158324
761.054758	53786.129639	33.163341
761.447171	53887.591679	33.168359
762.725571	53974.116710	33.173376
763.393267	54079.280913	33.178394
764.231626	54161.229311	33.183412
765.397989	54249.366293	33.188429
766.204579	54339.730371	33.193447
767.194556	54417.952207	33.198464
767.694534	54492.047350	33.203482
768.215516	54586.579394	33.208500
768.942664	54677.400447	33.213517
769.740071	54773.840066	33.218535
770.814981	54851.449314	33.223552
771.169202	54926.448467	33.228570
772.013934	55010.686645	33.233588
772.976885	55104.623619	33.238605
773.420610	55197.187318	33.243623
774.802440	55282.241377	33.248640
775.122138	55381.385208	33.253658
775.615441	55465.152677	33.258676
776.840522	55547.377746	33.263693
777.465818	55630.176269	33.268711
778.166376	55710.214018	33.273728
778.841817	55790.660647	33.278746
779.424821	55868.348923	33.283764
780.322341	55955.842902	33.288781
780.418808	56044.733540	33.293799
781.438429	56131.241304	33.298816
782.083344	56236.123730	33.303834
782.560502	56323.353948	33.308852
783.895018	56410.531205	33.313869
784.401708	56512.834519	33.318887
785.293601	56598.461816	33.323904
786.051982	56704.945619	33.328922
786.927397	56805.116779	33.333940
787.602893	56900.310412	33.338957
788.602305	56997.997557	33.343975
789.395947	57086.486832	33.348992
790.206491	57194.493866	33.354010
790.849060	57296.646010	33.359028
791.503053	57386.391969	33.364045
792.201542	57492.302172	33.369063
793.042016	57597.374249	33.374080
793.651078	57697.404344	33.379098
794.563566	57802.888986	33.384116
795.781974	57903.956826	33.389133
796.337770	58008.838001	33.394151
796.949878	58110.133548	33.399168
797.936383	58208.119420	33.404186
798.750054	58323.178330	33.409204
799.913008	58417.748729	33.414221
799.978708	58527.832574	33.419239
801.383198	58620.493353	33.424256
802.253619	58731.494279	33.429274
802.974030	58843.607627	33.434292
803.982894	58938.686260	33.439309
804.772094	59047.755860	33.444327
805.886070	59148.594424	33.449344
806.706130	59257.009102	33.454362
807.561267	59355.401468	33.459380
808.194696	59438.113247	33.464397
808.909288	59543.589164	33.469415
809.810518	59640.654415	33.474432
810.766001	59742.647116	33.479450
811.291583	59848.345480	33.484468
812.260240	59947.815321	33.489485
812.995271	60061.778465	33.494503
813.848894	60150.713678	33.499520
814.866669	60246.770283	33.504538
815.362107	60356.969945	33.509556
816.163104	60452.671521	33.514573
816.836026	60567.058585	33.519591
817.829072	60664.960463	33.524608
818.554475	60774.119412	33.529626
819.275466	60877.844127	33.534644
820.219307	60983.030455	33.539661
821.102584	61097.600596	33.544679
821.904461	61198.437748	33.549696
822.868654	61309.108585	33.554714
823.478318	61407.286009	33.559732
824.401323	61508.104653	33.564749
825.261557	61622.371836	33.569767
825.901937	61734.975758	33.574784
826.758870	61848.315608	33.579802
827.467215	61948.533532	33.584820
828.358739	62053.000805	33.589837
829.039174	62157.775317	33.594855
830.121101	62264.310679	33.599872
831.123280	62366.972454	33.604890
831.573235	62474.618445	33.609908
832.549010	62564.138115	33.614925
833.350952	62668.661259	33.619943
833.959191	62761.674853	33.624960
835.000157	62862.063450	33.629978
835.641092	62958.871454	33.634996
836.879678	63054.342138	33.640013
837.454799	63153.304784	33.645031
838.270802	63257.442998	33.650048
838.757711	63368.399813	33.655066
839.671610	63472.554526	33.660084
840.441014	63584.432922	33.665101
841.104213	63686.974013	33.670119
841.958965	63798.687740	33.675136
843.024953	63915.133419	33.680154
843.518769	64035.808558	33.685172
845.041324	64134.884698	33.690189
845.605406	64257.850496	33.695207
846.173904	64370.272072	33.700224
847.331881	64481.749682	33.705242
847.949224	64599.202658	33.710260
848.981585	64714.457286	33.715277
849.459189	64832.901892	33.720295
850.746918	64948.128223	33.725312
851.660578	65072.349595	33.730330
852.214760	65185.536540	33.735348
853.352063	65300.777054	33.740365
854.084574	65421.673613	33.745383
854.697369	65540.599294	33.750400
855.913936	65666.929849	33.755418
856.483623	65788.133616	33.760436
857.580488	65904.452546	33.765453
858.141707	66030.786206	33.770471
859.284719	66157.201424	33.775488
860.396240	66276.725257	33.780506
860.879478	66398.338812	33.785524
861.819871	66512.670247	33.790541
862.513029	66633.415924	33.795559
863.300625	66755.980110	33.800576
864.624213	66877.931622	33.805594
865.363946	67012.308820	33.810612
866.567360	67126.163852	33.815629
867.278106	67251.139780	33.820647
868.380773	67366.093889	33.825664
869.225092	67488.064969	33.830682
870.146926	67599.667766	33.835700
871.239439	67722.888932	33.840717
872.076647	67835.012765	33.845735
873.024867	67953.011448	33.850752
873.907645	68055.145606	33.855770
874.659618	68178.918906	33.860788
875.727671	68296.514003	33.865805
876.395689	68405.406345	33.870823
877.138766	68512.794670	33.875840
878.077727	68640.371301	33.880858
878.752397	68771.653303	33.885876
879.710168	68871.869503	33.890893
880.581705	68998.966254	33.895911
880.961748	69126.581325	33.900928
882.061368	69241.318475	33.905946
882.947969	69374.933920	33.910964
883.838046	69492.122448	33.915981
884.941462	69618.090658	33.920999
885.575607	69743.662987	33.926016
886.408096	69858.238967	33.931034
887.294960	69992.939482	33.936052
888.228300	70117.800593	33.941069
889.060735	70224.044574	33.946087
889.842218	70353.832670	33.951104
890.832790	70473.703659	33.956122
891.593800	70588.010811	33.961140
892.330586	70706.571876	33.966157
893.321713	70824.421253	33.971175
894.113432	70935.038629	33.976192
894.851566	71056.073858	33.981210
895.790453	71182.242870	33.986228
896.876277	71309.045968	33.991245
897.944534	71429.137078	33.996263
898.718709	71549.581023	34.001280
899.666746	71673.089150	34.006298
900.652793	71802.320955	34.011316
901.608912	71918.101604	34.016333
902.391227	72043.352979	34.021351
903.475776	72169.427780	34.026368
904.391516	72288.246181	34.031386
905.585426	72416.517673	34.036404
906.454254	72535.693000	34.041421
906.975542	72656.172269	34.046439
907.958901	72782.760634	34.051456
909.290705	72906.054221	34.056474
909.953943	73034.227397	34.061492
910.525392	73164.490804	34.066509
911.901379	73292.623520	34.071527
912.658491	73425.330512	34.076544
913.677424	73541.621678	34.081562
914.542067	73681.028732	34.086580
915.629008	73803.286443	34.091597
916.577757	73926.396174	34.096615
917.136359	74055.275668	34.101632
918.210746	74177.619763	34.106650
918.908720	74325.014541	34.111668
919.997506	74447.136404	34.116685
921.022148	74584.378757	34.121703
921.704843	74712.760929	34.126720
922.727552	74833.264137	34.131738
923.489074	74975.605769	34.136756
924.500295	75112.328693	34.141773
925.533296	75250.370723	34.146791
926.401262	75386.132384	34.151808
927.301013	75519.302798	34.156826
928.258191	75658.156836	34.161844
929.231041	75797.742836	34.166861
930.303035	75937.060326	34.171879
931.065997	76072.135178	34.176896
932.207405	76197.502717	34.181914
932.913509	76342.645295	34.186932
934.001474	76478.775753	34.191949
934.954320	76612.608089	34.196967
935.781924	76751.066621	34.201984
936.534885	76882.896953	34.207002
937.516661	77021.293720	34.212020
938.590416	77159.758366	34.217037
939.665121	77294.586687	34.222055
940.127913	77434.248339	34.227072
941.377203	77573.451886	34.232090
942.500134	77713.069371	34.237108
943.186150	77853.968133	34.242125
944.399032	77987.177453	34.247143
945.078780	78132.083018	34.252160
946.283026	78262.328743	34.257178
947.164048	78412.041869	34.262196
948.269768	78540.350898	34.267213
949.784679	78675.639772	34.272231
950.055254	78801.690972	34.277248
951.254166	78939.595593	34.282266
951.967013	79071.888246	34.287284
952.666512	79204.481196	34.292301
954.286649	79320.639984	34.297319
954.614346	79443.857679	34.302336
955.967214	79559.872120	34.307354
956.527502	79687.031671	34.312372
957.364374	79820.389937	34.317389
958.466947	79950.042291	34.322407
959.568925	80079.885269	34.327424
960.356867	80204.827597	34.332442
961.204615	80351.516246	34.337460
962.195568	80472.112062	34.342477
963.422180	80609.459261	34.347495
964.052970	80742.882332	34.352512
965.020529	80880.185436	34.357530
965.952688	81014.110648	34.362548
966.756090	81156.547892	34.367565
967.714395	81300.061202	34.372583
968.435471	81446.088274	34.377600
969.754121	81582.141855	34.382618
970.630822	81740.380456	34.387636
971.431335	81885.384956	34.392653
972.666248	82024.814413	34.397671
973.607252	82180.976632	34.402688
974.502062	82320.211058	34.407706
975.344911	82476.897654	34.412724
976.301325	82626.012397	34.417741
977.275022	82775.555470	34.422759
978.085567	82939.254315	34.427776
979.076304	83092.535789	34.432794
980.390060	83252.256291	34.437812
981.234003	83405.367982	34.442829
982.426423	83552.070752	34.447847
983.348206	83712.852592	34.452864
984.179612	83867.823242	34.457882
985.636849	84022.862278	34.462900
986.252579	84175.675133	34.467917
987.718885	84323.514356	34.472935
988.791610	84482.606190	34.477952
989.788449	84631.531035	34.482970
990.991260	84786.224946	34.487988
991.758146	84932.589204	34.493005
993.031950	85073.992120	34.498023
993.943283	85224.782501	34.503040
994.789729	85375.021438	34.508058
995.849984	85518.639018	34.513076
996.773917	85680.630003	34.518093
997.951002	85823.299980	34.523111
998.547442	85977.886907	34.528128
999.837726	86137.814607	34.533146
1000.895742	86284.474550	34.538164
1001.608786	86425.516427	34.543181
1002.754869	86581.452848	34.548199
1003.820212	86739.953783	34.553216
1004.933387	86895.290249	34.558234
1005.933090	87050.368070	34.563252
1007.044958	87196.815969	34.568269
1007.833118	87343.191739	34.573287
1008.468615	87507.078115	34.578304
1010.040700	87658.686095	34.583322
1010.938315	87805.217483	34.588340
1011.616813	87961.936427	34.593357
1012.851825	88118.830174	34.598375
1013.978400	88277.078153	34.603392
1014.940104	88425.305077	34.608410
1015.802316	88582.269851	34.613428
1016.808967	88748.799305	34.618445
1017.835237	88896.265403	34.623463
1018.788166	89044.200190	34.628480
1020.027632	89193.347890	34.633498
1021.229665	89338.768861	34.638516
1021.798563	89479.922341	34.643533
1022.797512	89611.550568	34.648551
1023.652843	89761.322243	34.653568
1024.416335	89920.767650	34.658586
1025.556160	90066.950113	34.663604
1026.234327	90223.753562	34.668621
1027.418564	90369.639397	34.673639
1028.066933	90541.696001	34.678656
1029.193962	90694.523383	34.683674
1030.242112	90869.149050	34.688692
1031.261228	91021.040668	34.693709
1032.321704	91184.249059	34.698727
1033.732783	91345.792993	34.703744
1034.800324	91515.850523	34.708762
1035.906801	91670.706464	34.713780
1037.042603	91841.729685	34.718797
1038.306774	92003.764325	34.723815
1038.819054	92167.987715	34.728832
1040.111793	92320.089069	34.733850
1041.324794	92489.376168	34.738868
1042.337351	92653.570748	34.743885
1043.174688	92812.484979	34.748903
1044.346130	92989.536015	34.753920
1045.378378	93147.647997	34.758938
1046.479256	93328.232381	34.763956
1047.666991	93490.245218	34.768973
1048.632469	93651.498332	34.773991
1049.763843	93823.827415	34.779008
1050.718023	93983.723684	34.784026
1051.994079	94153.695471	34.789044
1052.830328	94316.632720	34.794061
1053.870740	94475.492486	34.799079
1055.306661	94660.208982	34.804096
1056.473368	94819.448865	34.809114
1057.540403	94990.157268	34.814132
1058.235221	95160.801785	34.819149
1059.570171	95318.757378	34.824167
1060.508085	95491.009803	34.829184
1061.578207	95659.095283	34.834202
1062.676012	95825.860632	34.839220
1063.484355	96002.664142	34.844237
1065.019347	96157.559784	34.849255
1065.897725	96333.056340	34.854272
1067.036970	96503.066844	34.859290
1068.196565	96665.377310	34.864308
1068.953948	96839.580689	34.869325
1070.643658	96998.950618	34.874343
1071.820826	97173.561705	34.879360
1072.414774	97343.376859	34.884378
1073.875369	97503.079078	34.889396
1074.657520	97677.037274	34.894413
1075.972788	97835.031014	34.899431
1077.003767	98002.353679	34.904448
1077.742694	98174.955005	34.909466
1079.139312	98345.169657	34.914484
1079.999291	98512.682243	34.919501
1081.319651	98679.518382	34.924519
1082.343151	98854.489385	34.929536
1083.393568	99017.801694	34.934554
1084.778190	99184.674847	34.939572
1085.398518	99351.200621	34.944589
1086.765136	99515.299556	34.949607
1087.869031	99684.697885	34.954624
1089.036246	99847.287109	34.959642
1090.112829	100018.199003	34.964660
1090.861426	100175.889465	34.969677
1092.253076	100323.730611	34.974695
1093.447673	100481.038979	34.979712
1094.136482	100632.258777	34.984730
1095.655665	100789.205132	34.989748
1096.292022	100934.211535	34.994765
1097.483733	101092.119287	34.999783
1098.611440	101253.831213	35.004800
1099.523110	101413.015559	35.009818
1100.657953	101569.447703	35.014836
1101.592481	101735.322835	35.019853
1102.887855	101894.529025	35.024871
1103.608471	102071.990795	35.029888
1104.799698	102246.444335	35.034906
1105.941037	102416.683934	35.039924
1106.735805	102585.424293	35.044941
1108.094831	102752.445147	35.049959
1109.110857	102920.638212	35.054976
1110.230827	103095.894402	35.059994
1111.595725	103271.662168	35.065012
1112.614039	103441.232274	35.070029
1113.825096	103603.666923	35.075047
1115.016538	103778.922211	35.080064
1116.087321	103963.228409	35.085082
1117.284674	104132.672077	35.090100
1118.525690	104315.534172	35.095117
1119.713749	104491.807952	35.100135
1120.812297	104667.502464	35.105152
1121.856671	104840.661453	35.110170
1123.223963	105013.844182	35.115188
1123.904013	105196.108550	35.120205
1125.130287	105371.001391	35.125223
1126.164471	105550.132012	35.130240
1127.354222	105737.951888	35.135258
1128.623279	105909.890184	35.140276
1129.419047	106094.459369	35.145293
1130.426909	106278.399487	35.150311
1131.715984	106461.661100	35.155328
1133.019052	106659.297331	35.160346
1134.307150	106843.207682	35.165364
1135.720744	107027.985168	35.170381
1136.660495	107208.447144	35.175399
1137.987622	107390.834878	35.180416
1138.786026	107566.661491	35.185434
1140.198450	107753.939419	35.190452
1141.319598	107942.204117	35.195469
1142.460058	108119.244433	35.200487
1143.411069	108305.158494	35.205504
1144.561488	108490.546869	35.210522
1146.048021	108671.523592	35.215540
1147.186642	108859.690463	35.220557
1148.460412	109033.750692	35.225575
1149.427422	109226.419897	35.230592
1150.567390	109410.676263	35.235610
1151.608988	109593.607419	35.240628
1153.095748	109774.705464	35.245645
1153.834074	109960.640687	35.250663
1154.811117	110146.651719	35.255680
1156.208053	110335.976829	35.260698
1157.696290	110525.326158	35.265716
1158.656083	110707.961606	35.270733
1159.887973	110888.893810	35.275751
1160.995549	111079.842692	35.280768
1162.143557	111265.529019	35.285786
1163.557997	111449.335690	35.290804
1164.699920	111629.565556	35.295821
1165.843569	111814.977603	35.300839
1166.639907	111994.430875	35.305856
1167.706836	112184.798710	35.310874
1169.119892	112350.825226	35.315892
1169.989342	112525.227808	35.320909
1171.006835	112699.885720	35.325927
1172.148640	112875.309636	35.330944
1173.021264	113053.198888	35.335962
1174.311192	113236.543903	35.340980
1175.193943	113426.469259	35.345997
1176.544055	113607.336317	35.351015
1178.052338	113809.386462	35.356032
1178.681212	113995.797628	35.361050
1179.813930	114178.439985	35.366068
1181.015054	114378.264531	35.371085
1182.097763	114576.146305	35.376103
1183.466550	114770.155979	35.381120
1184.599108	114973.518207	35.386138
1185.999655	115163.623089	35.391156
1187.075211	115377.247436	35.396173
1188.096275	115569.850376	35.401191
1189.396184	115767.159768	35.406208
1190.735283	115981.378593	35.411226
1192.028375	116173.357829	35.416244
1192.998827	116383.522814	35.421261
1194.458859	116582.369823	35.426279
1195.520901	116784.109509	35.431296
1196.657608	116995.087752	35.436314
1197.922236	117198.963528	35.441332
1199.420306	117397.493140	35.446349
1200.429500	117605.595354	35.451367
1201.893493	117805.793288	35.456384
1202.648662	118016.576000	35.461402
1204.236732	118215.400471	35.466420
1205.659898	118432.500020	35.471437
1206.404120	118639.335676	35.476455
1208.109887	118835.800769	35.481472
1209.115384	119058.308669	35.486490
1210.358717	119255.993468	35.491508
1211.640625	119468.334273	35.496525
1212.547532	119677.101832	35.501543
1214.014061	119883.978982	35.506560
1215.062997	120101.102136	35.511578
1216.604236	120300.607519	35.516596
1217.742204	120523.826968	35.521613
1218.977078	120733.472889	35.526631
1220.264877	120934.545122	35.531648
1221.519505	121148.220496	35.536666
1222.591935	121359.874599	35.541684
1224.151512	121576.024467	35.546701
1225.130561	121784.680983	35.551719
1226.680078	121984.335770	35.556736
1227.436042	122201.041218	35.561754
1229.059077	122412.345679	35.566772
1230.158169	122607.846362	35.571789
1231.245121	122830.217166	35.576807
1232.691571	123041.225763	35.581824
1233.663202	123253.290169	35.586842
1235.280905	123472.270294	35.591860
1236.537426	123678.068010	35.596877
1237.187365	123896.564841	35.601895
1238.857437	124104.058723	35.606912
1240.078840	124333.325513	35.611930
1241.446127	124535.055184	35.616948
1242.786018	124752.962553	35.621965
1243.986649	124975.178295	35.626983
1245.551757	125171.518421	35.632000
1246.376392	125384.192389	35.637018
1247.522552	125589.514355	35.642036
1249.278029	125805.218618	35.647053
1250.059704	126011.212026	35.652071
1251.245417	126204.452906	35.657088
1252.309656	126405.662012	35.662106
1253.710109	126600.885141	35.667124
1255.256243	126800.128657	35.672141
1256.104383	127009.248410	35.677159
1257.516351	127194.853239	35.682176
1258.768268	127401.006359	35.687194
1260.276237	127606.522803	35.692212
1261.496207	127808.146251	35.697229
1262.422334	128006.156446	35.702247
1263.774070	128205.707312	35.707264
1264.750410	128414.878717	35.712282
1266.082485	128619.568997	35.717300
1267.137402	128841.938078	35.722317
1268.229850	129051.373408	35.727335
1269.632990	129271.685233	35.732352
1270.844007	129496.733074	35.737370
1271.855449	129707.605850	35.742388
1273.400218	129921.180596	35.747405
1274.575870	130152.019194	35.752423
1276.190796	130359.336010	35.757440
1277.487322	130599.601611	35.762458
1278.847969	130825.420098	35.767476
1280.068523	131035.075569	35.772493
1281.698225	131266.252859	35.777511
1283.217483	131484.000220	35.782528
1284.214320	131701.112840	35.787546
1285.463311	131915.396368	35.792564
1286.536591	132139.902546	35.797581
1288.020402	132372.379612	35.802599
1289.407801	132594.884797	35.807616
1290.367446	132827.337683	35.812634
1291.684926	133054.053709	35.817652
1293.505894	133273.069056	35.822669
1294.687981	133508.494578	35.827687
1296.032817	133733.042994	35.832704
1297.203427	133964.416921	35.837722
1298.523528	134184.852330	35.842740
1299.976895	134403.644451	35.847757
1301.089039	134636.161110	35.852775
1302.701498	134866.492194	35.857792
1304.101327	135091.725448	35.862810
1305.175911	135309.571967	35.867828
1306.831254	135540.851535	35.872845
1307.789893	135773.718546	35.877863
1309.423011	135998.386938	35.882880
1310.422380	136223.732124	35.887898
1311.838295	136459.596547	35.892916
1313.092627	136685.574681	35.897933
1314.492101	136920.063111	35.902951
1316.050707	137142.139723	35.907968
1317.252113	137369.601963	35.912986
1318.398382	137601.246229	35.918004
1320.114217	137826.014675	35.923021
1321.234876	138061.165749	35.928039
1322.551849	138290.428223	35.933056
1324.029647	138517.560909	35.938074
1325.401586	138744.205438	35.943092
1326.763358	138961.990221	35.948109
1328.170416	139188.441716	35.953127
1329.684491	139423.068066	35.958144
1330.786563	139638.414885	35.963162
1332.270195	139869.194699	35.968180
1333.623290	140086.163899	35.973197
1334.657408	140318.770848	35.978215
1336.453770	140530.851214	35.983232
1337.568565	140757.044373	35.988250
1339.014502	140976.882227	35.993268
1340.564939	141176.555252	35.998285
1341.576014	141382.405132	36.003303
1343.229932	141577.637923	36.008320
1344.271254	141789.102638	36.013338
1345.313212	141989.282824	36.018356
1346.956209	142200.054605	36.023373
1347.933452	142421.767020	36.028391
1349.496422	142625.909895	36.033408
1350.601689	142842.138386	36.038426
1351.695771	143063.848226	36.043444
1353.261773	143272.014213	36.048461
1354.164414	143503.243863	36.053479
1355.538994	143722.781056	36.058496
1356.674911	143954.672566	36.063514
1358.145864	144195.171587	36.068532
1359.515825	144426.152478	36.073549
1360.955808	144656.818937	36.078567
1362.249191	144881.309808	36.083584
1363.780184	145112.915288	36.088602
1364.866437	145356.364442	36.093620
1366.458217	145586.808890	36.098637
1367.739959	145836.138724	36.103655
1369.127247	146069.460805	36.108672
1370.677589	146317.861830	36.113690
1371.774617	146566.897487	36.118708
1373.470535	146798.651391	36.123725
1374.823571	147037.603602	36.128743
1376.325393	147277.445923	36.133760
1377.686284	147522.906101	36.138778
1379.143049	147770.508121	36.143796
1380.655565	148000.537066	36.148813
1381.857833	148259.801782	36.153831
1383.520118	148489.263667	36.158848
1384.946055	148729.495799	36.163866
1386.173565	148975.304761	36.168884
1387.500995	149213.565070	36.173901
1388.894174	149471.639863	36.178919
1390.023984	149702.097739	36.183936
1391.923227	149946.191317	36.188954
1393.353634	150202.172244	36.193972
1394.933890	150447.146219	36.198989
1396.187022	150701.904171	36.204007
1397.739151	150929.445971	36.209024
1399.407364	151181.918921	36.214042
1400.514442	151422.766403	36.219060
1402.075799	151659.139016	36.224077
1402.911376	151915.331299	36.229095
1404.361200	152153.780218	36.234112
1405.957899	152408.708460	36.239130
1407.190574	152664.002974	36.244148
1408.813811	152909.188642	36.249165
1410.099791	153174.295410	36.254183
1411.486248	153416.162052	36.259200
1413.073442	153666.647921	36.264218
1414.432274	153937.519360	36.269236
1415.999421	154174.566059	36.274253
1417.349423	154428.191104	36.279271
1418.677854	154678.193472	36.284288
1420.092082	154932.825964	36.289306
1421.397222	155183.862884	36.294324
1423.272989	155425.572312	36.299341
1424.493368	155684.909835	36.304359
1426.151363	155930.806412	36.309376
1427.329461	156177.697162	36.314394
1428.711418	156439.017203	36.319412
1430.353064	156688.054474	36.324429
1431.509799	156937.744280	36.329447
1432.645586	157176.148815	36.334464
1434.186731	157426.805683	36.339482
1435.599254	157660.651216	36.344500
1437.265154	157901.002180	36.349517
1438.515764	158144.556642	36.354535
1439.758839	158374.032249	36.359552
1441.397618	158611.575593	36.364570
1442.363344	158861.118544	36.369588
1443.806392	159110.634889	36.374605
1445.158256	159360.776768	36.379623
1446.800547	159617.088551	36.384640
1447.925511	159872.878458	36.389658
1449.421305	160129.813903	36.394676
1450.689348	160381.409410	36.399693
1451.849944	160655.200704	36.404711
1453.368950	160922.248590	36.409728
1455.154133	161188.949714	36.414746
1456.439918	161462.789050	36.419764
1457.910369	161730.040418	36.424781
1459.274977	161995.128774	36.429799
1460.510815	162277.634332	36.434816
1462.012747	162549.123234	36.439834
1463.218535	162835.113807	36.444852
1465.090743	163105.568144	36.449869
1466.627135	163390.213683	36.454887
1468.300620	163672.859179	36.459904
1470.042865	163949.823737	36.464922
1471.315566	164231.435290	36.469940
1472.730676	164504.118211	36.474957
1474.198970	164782.985814	36.479975
1475.685039	165067.232023	36.484992
1477.280360	165344.749983	36.490010
1478.174925	165633.957191	36.495028
1480.016426	165922.476927	36.500045
1481.840365	166218.411503	36.505063
1483.511714	166499.997183	36.510080
1485.059946	166788.964384	36.515098
1486.648352	167068.968617	36.520116
1487.872473	167350.595518	36.525133
1489.523832	167635.198920	36.530151
1491.044622	167929.075927	36.535168
1492.868403	168212.753585	36.540186
1493.833621	168501.777412	36.545204
1495.598259	168781.750512	36.550221
1496.864766	169076.717504	36.555239
1498.252481	169355.804721	36.560256
1499.855680	169651.950660	36.565274
1501.163920	169948.692895	36.570292
1502.792360	170241.234648	36.575309
1504.334520	170535.277198	36.580327
1505.910763	170827.856663	36.585344
1507.999690	171115.708792	36.590362
1509.029786	171413.838793	36.595380
1511.155893	171700.901612	36.600397
1512.604429	171991.580591	36.605415
1513.695398	172270.226759	36.610432
1515.509883	172557.117862	36.615450
1516.998622	172853.556844	36.620468
1518.345164	173137.901883	36.625485
1520.281280	173432.798468	36.630503
1521.522733	173725.172020	36.635520
1523.227148	174007.775253	36.640538
1524.533393	174289.354533	36.645556
1525.723903	174587.477898	36.650573
1527.458146	174874.599162	36.655591
1529.026467	175164.516142	36.660608
1530.601025	175460.411250	36.665626
1532.076105	175760.842584	36.670644
1533.441008	176040.404390	36.675661
1534.872579	176322.203099	36.680679
1536.457812	176596.172903	36.685696
1538.060495	176875.382845	36.690714
1539.324687	177136.844260	36.695732
1540.905753	177426.835836	36.700749
1542.643216	177708.134931	36.705767
1543.680279	177990.896623	36.710784
1545.105199	178265.181235	36.715802
1546.482324	178550.161665	36.720820
1548.264823	178842.082592	36.725837
1549.940754	179132.537839	36.730855
1551.229326	179427.868978	36.735872
1552.820325	179725.347562	36.740890
1554.148065	180023.480571	36.745908
1555.633168	180327.478458	36.750925
1557.057312	180634.813558	36.755943
1558.650650	180948.405206	36.760960
1560.321275	181255.627063	36.765978
1561.809860	181576.626733	36.770996
1563.318869	181878.763841	36.776013
1564.804713	182195.655317	36.781031
1566.497053	182514.367689	36.786048
1568.103472	182819.426033	36.791066
1569.839887	183154.419741	36.796084
1571.532368	183463.084963	36.801101
1573.210544	183780.867870	36.806119
1574.654663	184099.985989	36.811136
1576.628788	184414.144235	36.816154
1578.257909	184747.007606	36.821172
1579.985016	185077.813171	36.826189
1581.887494	185374.624287	36.831207
1583.478851	185697.878028	36.836224
1584.889103	186003.684596	36.841242
1586.617353	186325.332643	36.846260
1588.322351	186641.299608	36.851277
1589.947733	186949.411380	36.856295
1591.432804	187261.876578	36.861312
1593.121409	187574.487569	36.866330
1594.638833	187893.691297	36.871348
1596.498346	188202.431198	36.876365
1598.130959	188511.946482	36.881383
1599.615824	188841.430294	36.886400
1601.712067	189138.228949	36.891418
1602.922107	189453.772599	36.896436
1604.529777	189766.776847	36.901453
1606.593600	190079.275778	36.906471
1607.844220	190397.420088	36.911488
1609.769052	190701.439944	36.916506
1610.903328	191021.180898	36.921524
1612.530903	191335.142144	36.926541
1614.238201	191647.352665	36.931559
1615.909515	191970.945259	36.936576
1617.623766	192289.784590	36.941594
1619.141443	192607.134654	36.946612
1620.807325	192921.935557	36.951629
1622.728408	193236.810148	36.956647
1624.221982	193555.781301	36.961664
1625.736663	193861.636465	36.966682
1627.068690	194178.339630	36.971700
1628.788271	194494.142460	36.976717
1630.599228	194804.955176	36.981735
1632.293616	195130.464571	36.986752
1633.917965	195446.363998	36.991770
1635.753409	195767.943093	36.996788
1637.485984	196077.848109	37.001805
1639.410938	196387.341944	37.006823
1640.305785	196706.503815	37.011840
1642.058552	197017.006623	37.016858
1643.861703	197311.404218	37.021876
1645.327541	197591.702899	37.026893
1647.295117	197884.869747	37.031911
1648.745289	198181.449699	37.036928
1649.967583	198466.769092	37.041946
1651.654661	198774.637396	37.046964
1653.150834	199074.705077	37.051981
1654.584893	199383.036884	37.056999
1656.068658	199690.892093	37.062016
1657.723311	200004.332224	37.067034
1659.188397	200328.431973	37.072052
1660.333660	200650.859329	37.077069
1662.312171	200976.908684	37.082087
1663.809875	201303.394466	37.087104
1665.572885	201631.082186	37.092122
1667.011955	201964.373370	37.097140
1668.566505	202309.328037	37.102157
1670.364882	202639.693505	37.107175
1671.895574	202987.918405	37.112192
1673.481336	203330.701566	37.117210
1675.244507	203678.662776	37.122228
1676.788982	204035.384617	37.127245
1678.512497	204371.166426	37.132263
1680.236758	204739.187732	37.137280
1682.033055	205089.549761	37.142298
1683.788484	205440.275670	37.147316
1685.320534	205805.629334	37.152333
1687.123336	206156.401458	37.157351
1688.802789	206522.965790	37.162368
1690.856057	206876.861437	37.167386
1692.563446	207239.831086	37.172404
1694.234276	207595.659654	37.177421
1696.072929	207953.227058	37.182439
1697.912786	208314.897219	37.187456
1699.721018	208664.054172	37.192474
1701.675949	209034.050969	37.197492
1703.135172	209389.427113	37.202509
1704.967680	209737.098935	37.207527
1706.384660	210105.589411	37.212544
1708.030409	210462.767810	37.217562
1709.958967	210824.370737	37.222580
1711.712388	211201.495910	37.227597
1713.630038	211561.452972	37.232615
1715.343616	211925.381702	37.237632
1717.180376	212283.069404	37.242650
1718.649045	212645.771728	37.247668
1720.314377	213006.512880	37.252685
1722.213588	213376.410563	37.257703
1724.010420	213734.897969	37.262720
1725.584989	214095.506067	37.267738
1727.491788	214466.041841	37.272756
1728.771995	214837.342924	37.277773
1730.795688	215205.398780	37.282791
1732.480932	215573.486577	37.287808
1734.271740	215940.161486	37.292826
1736.370816	216313.136328	37.297844
1737.698484	216686.697183	37.302861
1739.339236	217053.197905	37.307879
1741.333486	217433.381966	37.312896
1743.168008	217797.135839	37.317914
1745.067164	218164.740891	37.322932
1746.755249	218538.223763	37.327949
1748.702064	218893.606961	37.332967
1750.202683	219271.542792	37.337984
1751.728905	219631.950706	37.343002
1753.800516	219999.914787	37.348020
1755.417665	220366.761463	37.353037
1757.130235	220735.955729	37.358055
1758.554956	221084.549427	37.363072
1760.129134	221437.361194	37.368090
1761.953347	221784.951366	37.373108
1763.391719	222218.811328	37.378125
1765.207053	222570.951868	37.383143
1766.947035	222937.151809	37.388160
1768.495169	223299.117490	37.393178
1770.500960	223648.766124	37.398196
1772.023290	224031.794568	37.403213
1774.035014	224400.875172	37.408231
1775.233909	224770.116562	37.413248
1776.966611	225135.333931	37.418266
1778.779333	225520.198727	37.423284
1780.463703	225911.461322	37.428301
1782.337104	226297.258293	37.433319
1784.133674	226681.900718	37.438336
1785.792277	227077.971794	37.443354
1787.616387	227461.824579	37.448372
1789.039953	227868.528801	37.453389
1790.886370	228261.778367	37.458407
1792.665642	228664.311368	37.463424
1794.416030	229074.292705	37.468442
1796.301731	229489.790257	37.473460
1797.794172	229893.568021	37.478477
1800.256218	230299.320456	37.483495
1801.861737	230710.676687	37.488512
1803.849339	231124.358655	37.493530
1805.801973	231532.738721	37.498548
1807.607857	231949.678902	37.503565
1809.529576	232351.741379	37.508583
1811.203203	232774.776503	37.513600
1813.604415	233184.255282	37.518618
1815.448998	233594.411260	37.523636
1816.955906	234005.741694	37.528653
1819.563386	234422.428906	37.533671
1820.992986	234816.932880	37.538688
1822.646172	235234.465513	37.543706
1825.030549	235641.616093	37.548724
1826.761558	236053.930452	37.553741
1828.713958	236454.244926	37.558759
1830.557040	236864.383437	37.563776
1832.535940	237269.140600	37.568794
1834.196359	237671.233199	37.573812
1836.047982	238088.815678	37.578829
1838.138988	238497.138538	37.583847
1839.854903	238910.020334	37.588864
1841.815588	239322.125857	37.593882
1843.614590	239718.992142	37.598900
1845.312851	240127.128989	37.603917
1847.161115	240535.394224	37.608935
1848.965097	240953.904653	37.613952
1851.138993	241376.139700	37.618970
1853.034200	241782.722802	37.623988
1854.607338	242191.849211	37.629005
1856.611490	242615.892597	37.634023
1857.941038	243023.739636	37.639040
1859.514831	243438.100839	37.644058
1862.084408	243854.838489	37.649076
1863.683401	244291.855973	37.654093
1865.638188	244698.357495	37.659111
1867.500114	245117.754105	37.664128
1869.584782	245539.756395	37.669146
1871.386275	245966.022879	37.674164
1873.171761	246385.382984	37.679181
1875.267751	246794.556578	37.684199
1876.565824	247225.556509	37.689216
1878.634429	247641.950022	37.694234
1880.882380	248051.328559	37.699252
1882.314251	248457.082645	37.704269
1884.323352	248848.185877	37.709287
1886.134885	249249.661134	37.714304
1888.038541	249652.544111	37.719322
1889.665742	250050.341666	37.724340
1891.339491	250447.877827	37.729357
1893.263752	250855.610389	37.734375
1895.358414	251262.705445	37.739392
1896.894801	251673.271603	37.744410
1898.909488	252088.382435	37.749428
1900.764214	252513.198567	37.754445
1902.420639	252927.479971	37.759463
1904.371371	253349.969054	37.764480
1906.137809	253771.574275	37.769498
1908.266292	254192.611847	37.774516
1909.777597	254626.199118	37.779533
1911.729278	255052.575524	37.784551
1913.778823	255494.965389	37.789568
1915.461465	255931.674839	37.794586
1917.991384	256362.833592	37.799604
1919.923645	256800.289535	37.804621
1921.716501	257247.879088	37.809639
1923.473034	257685.059342	37.814656
1925.630698	258133.325443	37.819674
1927.867534	258571.544179	37.824692
1929.678435	259018.622786	37.829709
1931.891279	259458.039404	37.834727
1933.572851	259904.859850	37.839744
1935.169998	260354.158285	37.844762
1937.404929	260794.434754	37.849780
1939.268812	261251.970402	37.854797
1941.050864	261695.928666	37.859815
1943.513266	262153.644611	37.864832
1945.598444	262612.743623	37.869850
1947.541197	263064.778433	37.874868
1949.426590	263517.736998	37.879885
1951.040299	263967.361540	37.884903
1953.608814	264427.878538	37.889920
1955.282086	264886.942648	37.894938
1957.557001	265335.263158	37.899956
1959.337099	265791.260570	37.904973
1961.232310	266246.882955	37.909991
1963.174210	266709.508487	37.915008
1965.152316	267170.196973	37.920026
1967.554489	267622.990846	37.925044
1969.148842	268089.889301	37.930061
1971.096715	268543.951165	37.935079
1973.141455	269009.453258	37.940096
1975.130037	269478.495068	37.945114
1977.350267	269935.177630	37.950132
1979.056278	270400.784706	37.955149
1981.153941	270858.324587	37.960167
1983.285484	271321.345240	37.965184
1984.826201	271790.534026	37.970202
1987.502150	272253.895247	37.975220
1989.068375	272716.854710	37.980237
1990.646064	273185.196887	37.985255
1993.407416	273656.721376	37.990272
1995.122128	274125.293337	37.995290
1997.341050	274581.105359	38.000308
1999.188684	275053.210026	38.005325
2000.853904	275523.845162	38.010343
2003.220275	275993.677739	38.015360
2005.183374	276459.663997	38.020378
2007.254338	276919.814374	38.025396
2009.105588	277397.070338	38.030413
2011.463232	277862.937685	38.035431
2013.487933	278302.974258	38.040448
2015.412116	278764.643603	38.045466
2017.470714	279197.001232	38.050484
2019.592061	279630.338224	38.055501
2021.216236	280067.922230	38.060519
2023.542512	280498.378406	38.065536
2025.390453	280933.002235	38.070554
2027.147269	281380.594917	38.075572
2028.885387	281832.203013	38.080589
2030.995427	282277.423551	38.085607
2032.809453	282737.856481	38.090624
2034.152905	283197.680003	38.095642
2036.630579	283663.335093	38.100660
2038.708653	284135.074913	38.105677
2040.517156	284605.968798	38.110695
2042.845531	285074.235319	38.115712
2044.307742	285557.325200	38.120730
2046.329073	286032.853346	38.125748
2048.523999	286528.875188	38.130765
2050.522692	287015.656456	38.135783
2052.791014	287501.858136	38.140800
2054.613456	287999.638211	38.145818
2056.416560	288487.919899	38.150836
2058.669355	288989.537000	38.155853
2060.618153	289499.381303	38.160871
2062.676908	290007.554461	38.165888
2064.586671	290522.582846	38.170906
2067.016090	291025.559954	38.175924
2068.767751	291538.629094	38.180941
2070.674466	292054.032681	38.185959
2073.144101	292576.173659	38.190976
2075.045316	293100.971554	38.195994
2077.351959	293618.054941	38.201012
2079.534754	294134.470688	38.206029
2081.209275	294652.187176	38.211047
2083.769277	295178.314599	38.216064
2086.026760	295708.273920	38.221082
2088.182352	296227.427584	38.226100
2090.359538	296753.890023	38.231117
2092.498607	297281.346697	38.236135
2094.994497	297795.991779	38.241152
2097.123505	298325.527512	38.246170
2099.269045	298843.171408	38.251188
2101.605694	299366.038505	38.256205
2103.702993	299882.262711	38.261223
2106.139632	300395.685225	38.266240
2108.084523	300916.653129	38.271258
2110.515989	301431.874228	38.276276
2112.468503	301940.898436	38.281293
2114.518897	302462.069018	38.286311
2116.830970	302968.158368	38.291328
2118.723939	303491.457079	38.296346
2120.869395	304002.114251	38.301364
2122.947063	304516.462223	38.306381
2125.194622	305038.271142	38.311399
2127.593910	305551.366337	38.316416
2129.575315	306078.165259	38.321434
2131.705428	306590.460622	38.326452
2134.123833	307107.454337	38.331469
2136.166277	307627.706794	38.336487
2138.303533	308131.433185	38.341504
2140.526309	308650.684390	38.346522
2142.284355	309164.066494	38.351540
2144.909458	309681.898709	38.356557
2146.605159	310195.766993	38.361575
2148.819701	310705.508506	38.366592
2151.063958	311224.840957	38.371610
2153.120344	311748.949694	38.376628
2155.112042	312250.820124	38.381645
2157.173377	312751.329847	38.386663
2159.558776	313246.602373	38.391680
2161.421829	313738.224942	38.396698
2163.346864	314231.662344	38.401716
2165.512091	314724.548898	38.406733
2167.566402	315221.030860	38.411751
2169.894020	315713.756884	38.416768
2172.020437	316223.170464	38.421786
2173.752325	316731.452035	38.426804
2176.030323	317240.731647	38.431821
2178.005590	317749.524252	38.436839
2180.464060	318259.122057	38.441856
2182.457194	318786.440288	38.446874
2184.172152	319316.847336	38.451892
2186.522210	319846.256646	38.456909
2188.351617	320377.575857	38.461927
2190.656651	320918.790996	38.466944
2192.671623	321469.596522	38.471962
2194.842629	322006.863737	38.476980
2197.091477	322555.310821	38.481997
2198.990691	323110.793218	38.487015
2201.379295	323664.438028	38.492032
2203.522102	324223.094915	38.497050
2205.705648	324796.516794	38.502068
2208.071808	325357.614727	38.507085
2209.742563	325928.597094	38.512103
2212.376209	326507.717297	38.517120
2214.631389	327089.585567	38.522138
2216.663519	327663.995379	38.527156
2219.141191	328242.997467	38.532173
2221.164291	328816.610451	38.537191
2223.468619	329403.753723	38.542208
2225.851591	329991.334987	38.547226
2227.700559	330579.328366	38.552244
2230.020596	331165.511570	38.557261
2232.199089	331764.709936	38.562279
2234.690676	332347.983727	38.567296
2236.803345	332964.899610	38.572314
2238.807114	333561.390991	38.577332
2241.812275	334166.113121	38.582349
2243.404241	334776.113359	38.587367
2245.925010	335373.463967	38.592384
2248.137520	335963.294109	38.597402
2250.297880	336585.212009	38.602420
2252.778445	337197.169885	38.607437
2254.697909	337807.537812	38.612455
2257.214829	338420.744349	38.617472
2259.579446	339031.328804	38.622490
2261.922209	339658.560599	38.627508
2264.432194	340256.059470	38.632525
2266.769790	340868.885071	38.637543
2268.942644	341474.420296	38.642560
2271.107840	342097.767149	38.647578
2273.183350	342702.973268	38.652596
2275.779041	343315.928655	38.657613
2277.898348	343942.051210	38.662631
2280.499899	344558.086140	38.667648
2283.077538	345171.858186	38.672666
2285.078196	345793.204411	38.677684
2287.473726	346405.137636	38.682701
2289.762256	347009.923590	38.687719
2292.136144	347619.281024	38.692736
2294.645072	348237.338149	38.697754
2296.707923	348837.467568	38.702772
2299.249658	349452.609591	38.707789
2301.479244	350063.379049	38.712807
2304.011984	350666.350151	38.717824
2306.488443	351276.554609	38.722842
2308.634652	351845.289719	38.727860
2310.924466	352415.592388	38.732877
2312.853942	352999.878163	38.737895
2314.949448	353568.928906	38.742912
2317.611742	354153.103425	38.747930
2319.811445	354735.367061	38.752948
2322.225930	355311.852689	38.757965
2324.139948	355900.998385	38.762983
2326.532204	356489.397143	38.768000
2329.049650	357073.910204	38.773018
2331.103275	357673.233053	38.778036
2333.404483	358259.236583	38.783053
2335.351194	358862.619223	38.788071
2337.649413	359468.979461	38.793088
2339.692707	360083.339189	38.798106
2341.992155	360699.778368	38.803124
2344.529139	361323.018800	38.808141
2346.358326	361955.423299	38.813159
2349.028768	362586.486432	38.818176
2351.336028	363224.550455	38.823194
2353.694851	363855.060982	38.828212
2356.090721	364489.639398	38.833229
2358.323462	365131.692401	38.838247
2360.803232	365782.572439	38.843264
2363.037302	366427.266936	38.848282
2365.028581	367083.075665	38.853300
2367.906690	367736.570448	38.858317
2369.948504	368395.518562	38.863335
2372.502711	369058.758573	38.868352
2374.977907	369717.434009	38.873370
2377.328030	370385.401556	38.878388
2379.711621	371046.655256	38.883405
2382.075559	371725.426184	38.888423
2384.398043	372397.190973	38.893440
2386.963581	373068.142144	38.898458
2388.857372	373756.107882	38.903476
2391.881914	374425.993812	38.908493
2394.175117	375103.621273	38.913511
2396.904402	375786.007452	38.918528
2399.107846	376465.018019	38.923546
2401.705056	377154.220805	38.928564
2404.401121	377827.975188	38.933581
2406.838614	378506.526300	38.938599
2409.252223	379184.357740	38.943616
2411.776212	379864.464851	38.948634
2414.369809	380545.713084	38.953652
2416.986644	381222.632964	38.958669
2419.124757	381895.713203	38.963687
2421.965459	382575.585760	38.968704
2424.536276	383254.170290	38.973722
2426.658841	383931.851189	38.978740
2429.471121	384596.955414	38.983757
2432.083443	385287.787071	38.988775
2434.064019	385953.406116	38.993792
2436.669753	386630.671506	38.998810
2439.187041	387314.705902	39.003828
2441.775458	387982.996077	39.008845
2444.228153	388658.316505	39.013863
2446.977246	389333.395965	39.018880
2449.422529	390010.513481	39.023898
2451.591085	390676.837855	39.028916
2454.553364	391350.925487	39.033933
2456.559091	392031.163505	39.038951
2459.009046	392692.860270	39.043968
2461.508258	393364.825171	39.048986
2464.049040	394043.459576	39.054004
2466.488779	394713.858002	39.059021
2468.761509	395372.635596	39.064039
2471.459099	396015.513580	39.069056
2474.088952	396649.493061	39.074074
2476.128632	397276.941649	39.079092
2478.686121	397919.142184	39.084109
2480.969874	398550.324536	39.089127
2483.188117	399201.169045	39.094144
2485.656898	399849.322068	39.099162
2487.994824	400496.747181	39.104180
2490.844530	401138.929191	39.109197
2493.110091	401804.302537	39.114215
2495.362325	402454.231178	39.119232
2497.642925	403113.641955	39.124250
2499.925102	403794.244479	39.129268
2502.650539	404466.396110	39.134285
2504.959625	405148.050615	39.139303
2507.094761	405827.234136	39.144320
2509.912345	406507.301713	39.149338
2512.247391	407204.000718	39.154356
2514.646163	407894.743327	39.159373
2517.416341	408595.590988	39.164391
2519.486309	409302.413123	39.169408
2522.419439	409999.904181	39.174426
2524.800936	410713.679976	39.179444
2527.650915	411422.597243	39.184461
2530.102383	412146.353864	39.189479
2532.494417	412849.558607	39.194496
2535.155428	413561.362448	39.199514
2537.579734	414288.990422	39.204532
2540.316636	415003.933666	39.209549
2543.012909	415740.593793	39.214567
2545.407465	416459.301539	39.219584
2548.196751	417185.825376	39.224602
2550.396116	417924.353514	39.229620
2553.266269	418651.683239	39.234637
2555.910557	419385.689170	39.239655
2558.206049	420118.338556	39.244672
2561.503338	420852.649705	39.249690
2563.977613	421591.936538	39.254708
2566.740945	422318.898990	39.259725
2569.050165	423061.536740	39.264743
2571.722699	423799.129806	39.269760
2574.809944	424517.948048	39.274778
2576.766457	425264.577388	39.279796
2579.904560	426001.621998	39.284813
2582.497514	426737.063284	39.289831
2584.918885	427481.269148	39.294848
2587.748296	428214.246658	39.299866
2589.918946	428954.397887	39.304884
2593.005841	429698.526058	39.309901
2595.692118	430435.306060	39.314919
2598.163427	431176.603711	39.319936
2601.314745	431910.729696	39.324954
2603.446650	432651.631651	39.329972
2606.328285	433377.960797	39.334989
2609.239956	434115.852857	39.340007
2611.850406	434851.746477	39.345024
2614.508391	435577.385235	39.350042
2616.989504	436313.101401	39.355060
2620.099379	437036.442980	39.360077
2622.231601	437769.031855	39.365095
2624.793940	438503.499576	39.370112
2627.700239	439235.002193	39.375130
2629.957833	439983.539306	39.380148
2632.361858	440709.662162	39.385165
2635.346564	441439.510913	39.390183
2637.859439	442178.166535	39.395200
2640.891080	442913.069000	39.400218
2643.430065	443640.894524	39.405236
2645.911435	444333.645655	39.410253
2648.754042	445036.938941	39.415271
2650.994806	445729.331111	39.420288
2653.935782	446422.091437	39.425306
2656.370092	447121.792538	39.430324
2658.902056	447810.984007	39.435341
2661.578262	448516.366045	39.440359
2663.844147	449224.928311	39.445376
2666.478922	449938.008627	39.450394
2669.072967	450658.303969	39.455412
2671.812371	451381.585128	39.460429
2674.353117	452092.483762	39.465447
2676.632374	452824.792842	39.470464
2679.334356	453547.499389	39.475482
2681.972412	454293.401701	39.480500
2684.477709	455031.815239	39.485517
2687.294486	455787.747042	39.490535
2689.673093	456536.341175	39.495552
2692.314693	457292.600125	39.500570
2694.824623	458068.620839	39.505588
2697.434854	458836.657935	39.510605
2700.140009	459616.075345	39.515623
2702.700025	460398.620665	39.520640
2705.738512	461178.832224	39.525658
2708.231133	461961.630660	39.530676
2710.680166	462754.009176	39.535693
2714.098945	463540.181201	39.540711
2716.273975	464344.823215	39.545728
2719.051781	465140.134489	39.550746
2721.874507	465948.697444	39.555764
2724.602784	466750.824300	39.560781
2727.483305	467567.193879	39.565799
2730.083362	468384.232081	39.570816
2732.936633	469199.981069	39.575834
2735.844927	470023.922156	39.580852
2738.572591	470840.228130	39.585869
2741.497191	471664.499670	39.590887
2743.808887	472491.362407	39.595904
2747.063897	473307.020233	39.600922
2749.823608	474132.625481	39.605940
2752.800653	474957.249157	39.610957
2755.847182	475782.633031	39.615975
2758.509578	476611.326641	39.620992
2761.306788	477435.869748	39.626010
2763.976908	478259.033230	39.631028
2766.836908	479092.936012	39.636045
2770.043880	479911.643849	39.641063
2772.594052	480741.128765	39.646080
2775.504413	481555.872505	39.651098
2778.245072	482392.673143	39.656116
2781.052170	483216.649608	39.661133
2784.089855	484033.279739	39.666151
2786.667376	484866.255555	39.671168
2789.721315	485684.119965	39.676186
2792.657386	486512.617722	39.681204
2795.548009	487346.031064	39.686221
2798.706109	488159.472804	39.691239
2801.316835	488990.986527	39.696256
2803.604215	489796.268334	39.701274
2806.650192	490624.149723	39.706292
2809.560570	491450.499884	39.711309
2812.596253	492276.941212	39.716327
2815.493330	493093.071283	39.721344
2818.051053	493920.521566	39.726362
2820.852604	494744.359490	39.731380
2823.867783	495553.792938	39.736397
2826.565408	496373.683889	39.741415
2829.172252	497193.348217	39.746432
2832.024186	497969.799010	39.751450
2834.729542	498757.083907	39.756468
2837.288875	499546.222224	39.761485
2840.320950	500325.056099	39.766503
2843.284927	501113.195846	39.771520
2845.721429	501901.385049	39.776538
2848.827325	502686.349734	39.781556
2851.557237	503480.164457	39.786573
2854.588974	504271.672071	39.791591
2857.176015	505077.586236	39.796608
2860.122453	505879.821121	39.801626
2862.736331	506682.625811	39.806644
2865.287111	507492.005943	39.811661
2868.292253	508303.438403	39.816679
2871.157939	509131.136560	39.821696
2873.802987	509952.073180	39.826714
2876.793857	510784.101253	39.831732
2879.413596	511623.707881	39.836749
2882.256006	512451.892534	39.841767
2884.851481	513305.980421	39.846784
2887.861079	514156.173811	39.851802
2890.439752	515001.403032	39.856820
2893.359010	515877.420930	39.861837
2896.387078	516739.262519	39.866855
2899.238676	517615.848656	39.871872
2901.752244	518485.235941	39.876890
2905.008255	519370.523295	39.881908
2907.830964	520254.067816	39.886925
2911.135978	521145.340309	39.891943
2913.708284	522037.638587	39.896960
2916.715608	522931.575653	39.901978
2919.874477	523821.758203	39.906996
2922.746421	524720.950562	39.912013
2925.830896	525616.377793	39.917031
2928.513618	526520.076333	39.922048
2931.351851	527428.327111	39.927066
2934.536497	528331.681961	39.932084
2937.812887	529254.904429	39.937101
2940.870781	530150.113482	39.942119
2943.677622	531069.221837	39.947136
2946.727536	531978.668188	39.952154
2949.923032	532892.463473	39.957172
2952.477497	533805.099155	39.962189
2955.994886	534711.630179	39.967207
2958.794281	535629.797753	39.972224
2961.608022	536540.959947	39.977242
2964.815658	537460.302140	39.982260
2968.033165	538376.514374	39.987277
2970.970356	539295.833405	39.992295
2974.023041	540215.325509	39.997312
2976.664575	541130.147234	40.002330
2979.796409	542050.965870	40.007348
2982.954834	542973.580979	40.012365
2985.897380	543892.750824	40.017383
2989.421459	544813.172567	40.022400
2992.214812	545736.319354	40.027418
2994.990816	546652.317210	40.032436
2998.150475	547587.248581	40.037453
3001.412279	548502.591117	40.042471
3004.229859	549422.923332	40.047488
3007.421911	550338.707946	40.052506
3010.804730	551258.169933	40.057524
3013.574300	552177.972513	40.062541
3016.571600	553088.074946	40.067559
3019.690905	554006.439120	40.072576
3022.176131	554924.091421	40.077594
3025.538065	555831.787460	40.082612
3028.579929	556742.791201	40.087629
3031.316308	557615.445394	40.092647
3034.837832	558499.117062	40.097664
3037.602006	559366.627376	40.102682
3040.528266	560230.838951	40.107700
3043.299272	561099.239048	40.112717
3046.281199	561963.930479	40.117735
3049.047853	562847.887232	40.122752
3052.089963	563742.034447	40.127770
3054.843807	564633.204872	40.132788
3057.795655	565534.073595	40.137805
3060.887257	566438.170606	40.142823
3063.601066	567358.684838	40.147840
3066.777074	568264.346899	40.152858
3069.681998	569185.250994	40.157876
3072.552197	570114.577944	40.162893
3075.576320	571031.865518	40.167911
3078.358454	571980.847250	40.172928
3081.445412	572918.716715	40.177946
3084.667488	573864.924999	40.182964
3087.778471	574832.707723	40.187981
3090.779799	575787.639145	40.192999
3093.963797	576758.973966	40.198016
3096.675041	577730.612038	40.203034
3099.662093	578704.536522	40.208052
3102.766754	579687.293453	40.213069
3106.174263	580659.088593	40.218087
3109.529020	581659.151376	40.223104
3112.396986	582651.740875	40.228122
3115.534932	583635.630742	40.233140
3118.549840	584643.528373	40.238157
3122.056809	585637.173251	40.243175
3124.950300	586654.349183	40.248192
3127.982585	587653.170324	40.253210
3131.334936	588670.701889	40.258228
3134.338511	589699.230622	40.263245
3137.765257	590701.992775	40.268263
3140.917610	591735.934160	40.273280
3144.095498	592754.098282	40.278298
3147.671364	593770.055042	40.283316
3150.769783	594795.821960	40.288333
3154.085059	595813.999857	40.293351
3157.567206	596842.680446	40.298368
3160.423498	597864.261724	40.303386
3163.984484	598872.766828	40.308404
3167.270008	599899.356818	40.313421
3170.701846	600917.770245	40.318439
3173.950246	601922.656189	40.323456
3177.109317	602947.994305	40.328474
3180.774941	603960.192366	40.333492
3183.863938	604978.552265	40.338509
3187.174762	605992.930813	40.343527
3190.522696	607004.310055	40.348544
3193.607787	608019.795494	40.353562
3197.159713	609020.802609	40.358580
3200.286729	610034.898620	40.363597
3203.329701	611029.806881	40.368615
3206.693503	612048.684022	40.373632
3209.755961	613054.363253	40.378650
3213.277024	614058.425498	40.383668
3216.563900	615071.686744	40.388685
3219.875094	616069.400018	40.393703
3223.108875	617070.135543	40.398720
3226.169133	618083.606902	40.403738
3229.527974	619078.888998	40.408756
3232.824304	620090.135738	40.413773
3235.710779	621090.860172	40.418791
3239.129286	622091.254648	40.423808
3242.187460	623082.671141	40.428826
3245.359275	624046.396227	40.433844
3248.257379	625013.277602	40.438861
3251.581337	625968.011760	40.443879
3254.743511	626927.432850	40.448896
3257.797409	627893.578440	40.453914
3261.214006	628863.771730	40.458932
3264.176334	629841.741629	40.463949
3267.212310	630814.815160	40.468967
3270.529680	631800.085220	40.473984
3273.192101	632789.414812	40.479002
3276.250517	633783.228371	40.484020
3279.694568	634789.762156	40.489037
3282.827358	635803.137718	40.494055
3285.958279	636805.435379	40.499072
3288.871260	637833.221446	40.504090
3292.288171	638859.824264	40.509108
3295.416934	639894.404722	40.514125
3298.682361	640937.538613	40.519143
3302.209224	641985.710758	40.524160
3305.143973	643036.466392	40.529178
3308.319084	644109.515754	40.534196
3311.597312	645163.386043	40.539213
3314.908553	646245.611277	40.544231
3318.559349	647325.420952	40.549248
3321.771170	648403.641664	40.554266
3325.684269	649484.123033	40.559284
3328.550983	650558.180993	40.564301
3331.831104	651654.579699	40.569319
3335.557213	652750.734069	40.574336
3338.820549	653849.334482	40.579354
3342.173765	654948.844000	40.584372
3346.009829	656048.400187	40.589389
3349.062072	657146.617594	40.594407
3352.602375	658262.111054	40.599424
3355.858151	659358.751450	40.604442
3359.455070	660474.828643	40.609460
3362.732486	661583.611517	40.614477
3366.003214	662705.907216	40.619495
3369.671387	663828.255582	40.624512
3373.041464	664950.969845	40.629530
3376.517346	666065.175481	40.634548
3379.942041	667193.787636	40.639565
3383.185320	668309.361476	40.644583
3386.618168	669445.117426	40.649600
3389.817064	670577.940679	40.654618
3393.497891	671702.939827	40.659636
3396.952221	672838.830748	40.664653
3399.970442	673973.363293	40.669671
3404.123022	675110.205989	40.674688
3407.277922	676258.109110	40.679706
3411.402858	677375.493195	40.684724
3414.569569	678509.995060	40.689741
3418.087436	679651.554137	40.694759
3421.651946	680774.780646	40.699776
3425.153563	681909.255795	40.704794
3428.731175	683029.869161	40.709812
3432.038394	684156.349106	40.714829
3435.509744	685287.479335	40.719847
3439.273963	686415.193037	40.724864
3442.652701	687533.546183	40.729882
3446.144431	688658.344019	40.734900
3449.619159	689778.686035	40.739917
3452.878049	690905.722472	40.744935
3456.901105	692030.307732	40.749952
3460.041020	693147.603520	40.754970
3463.991857	694258.225997	40.759988
3467.115547	695373.260165	40.765005
3470.452864	696477.016159	40.770010
3474.100997	697528.563365	40.775015
3477.169934	698533.750578	40.780020
3481.082037	699468.649901	40.785024
3483.961392	700335.580632	40.790029
3487.241209	701132.835815	40.795034
3490.167712	701855.539766	40.800039
3493.156246	702535.392757	40.805044
3495.656385	703128.028437	40.810048
3498.344288	703658.442091	40.815053
3500.670777	704130.759516	40.820058
3503.267436	704528.244722	40.825063
3505.604962	704878.564266	40.830068
3508.006523	705155.145672	40.835072
3510.019884	705376.200477	40.840077
3511.578157	705544.873189	40.845082
3513.652460	705654.996880	40.850087
3515.413588	705732.041628	40.855092
3516.950453	705743.063263	40.860096
3518.670274	705709.601024	40.865101
3519.839621	705636.990543	40.870106
3521.351365	705518.874945	40.875111
3522.401693	705375.253235	40.880116
3523.730199	705179.676087	40.885120
3524.817551	704968.189126	40.890125
3525.847561	704721.834834	40.895130
3526.844748	704439.463639	40.900135
3527.427142	704137.181002	40.905140
3528.278923	703809.357631	40.910144
3529.107871	703449.033622	40.915149
3529.657486	703081.536477	40.920154
3530.455755	702677.363956	40.925159
3530.706244	702265.908957	40.930164
3531.272011	701834.009145	40.935168
3531.464907	701403.441391	40.940173
3532.038737	700951.469910	40.945178
3532.596469	700473.485121	40.950183
3532.921078	699994.568269	40.955188
3533.388345	699500.143589	40.960192
3533.605195	698995.641663	40.965197
3533.670595	698482.983179	40.970202
3534.170709	697953.519476	40.975207
3534.259928	697436.520674	40.980212
3534.340392	696885.982172	40.985216
3534.651499	696347.006340	40.990221
3534.445985	695799.032699	40.995226
3534.713114	695242.244712	41.000231
3534.692709	694689.397895	41.005236
3535.008297	694122.684691	41.010240
3534.956730	693559.775908	41.015245
3535.024956	692986.216871	41.020250
3535.194670	692415.340113	41.025255
3535.133383	691833.122411	41.030260
3534.745236	691253.557406	41.035264
3535.105780	690681.244841	41.040269
3535.050139	690090.802872	41.045274
3535.481340	689509.298256	41.050279
3535.040859	688920.335536	41.055284
3534.738462	688331.958478	41.060288
3534.846018	687749.547430	41.065293
3534.612874	687160.983020	41.070298
3534.836915	686572.603613	41.075303
3534.597071	685989.937324	41.080308
3534.617603	685401.266482	41.085312
3534.370908	684815.240189	41.090317
3534.215159	684233.791579	41.095322
3534.294441	683644.150892	41.100327
3534.219278	683056.140811	41.105332
3534.015745	682469.857007	41.110336
3533.829132	681893.941546	41.115341
3533.610111	681311.819343	41.120346
3533.541881	680725.750290	41.125351
3533.251376	680146.554528	41.130356
3533.334515	679552.714771	41.135360
3533.343143	678990.931947	41.140365
3532.781331	678409.778682	41.145370
3533.089778	677833.926170	41.150375
3532.670094	677263.589020	41.155380
3532.662952	676692.650516	41.160384
3532.699821	676126.702854	41.165389
3532.328891	675564.326351	41.170394
3532.518944	674979.345825	41.175399
3531.950714	674419.723810	41.180404
3531.767039	673852.478224	41.185408
3531.821490	673298.518450	41.190413
3531.423330	672736.175605	41.195418
3531.461312	672177.715568	41.200423
3531.089361	671638.834018	41.205428
3530.655743	671088.663360	41.210432
3530.649542	670551.005547	41.215437
3530.386875	669997.751318	41.220442
3530.089521	669463.021669	41.225447
3530.034921	668924.082472	41.230452
3530.234888	668388.561920	41.235456
3530.045350	667844.296941	41.240461
3529.565059	667322.644439	41.245466
3529.128058	666781.551780	41.250471
3529.352595	666255.933651	41.255476
3529.071445	665737.903075	41.260480
3528.747119	665226.387286	41.265485
3528.589730	664709.677614	41.270490
3528.425802	664188.151123	41.275495
3528.000726	663683.006257	41.280500
3528.194582	663170.497123	41.285504
3527.777522	662662.702492	41.290509
3527.625903	662169.659748	41.295514
3527.788624	661665.709680	41.300519
3527.517916	661172.785431	41.305524
3527.420499	660670.273843	41.310528
3527.179800	660185.230840	41.315533
3526.603705	659695.226904	41.320538
3526.833235	659198.375948	41.325543
3526.056233	658731.670222	41.330548
3526.047791	658247.840314	41.335552
3526.175965	657781.838679	41.340557
3526.005872	657299.785911	41.345562
3525.734242	656836.751108	41.350567
3525.562431	656362.542100	41.355572
3525.591478	655895.218610	41.360576
3525.141259	655423.307309	41.365581
3524.977410	654977.946221	41.370586
3524.833337	654514.731004	41.375591
3524.438921	654075.760234	41.380596
3524.028597	653622.936262	41.385600
3524.192326	653184.882902	41.390605
3523.657729	652741.679949	41.395610
3523.854470	652304.331535	41.400615
3523.491844	651877.747331	41.405620
3523.345079	651436.620385	41.410624
3523.081871	651022.373557	41.415629
3522.996083	650591.941308	41.420634
3522.828932	650169.598694	41.425639
3522.727938	649746.827548	41.430644
3522.342486	649334.879373	41.435648
3522.626600	648916.007414	41.440653
3522.288169	648505.466611	41.445658
3522.184798	648099.718161	41.450663
3521.731235	647697.059813	41.455668
3521.354208	647289.374488	41.460672
3521.355453	646894.956121	41.465677
3520.823489	646506.708491	41.470682
3520.799130	646111.163974	41.475687
3520.733521	645728.708160	41.480692
3520.663707	645347.388381	41.485696
3520.759588	644972.876079	41.490701
3520.163048	644595.764259	41.495706
3520.310274	644225.265514	41.500711
3519.787038	643857.513685	41.505716
3519.951169	643477.435004	41.510720
3519.543349	643106.936936	41.515725
3519.340486	642751.493046	41.520730
3519.499044	642386.075921	41.525735
3519.178589	642020.974682	41.530740
3519.066586	641657.776433	41.535744
3519.027246	641317.008604	41.540749
3518.742015	640972.168845	41.545754
3518.830188	640614.902208	41.550759
3518.425804	640279.461619	41.555764
3518.034527	639933.654081	41.560768
3518.379602	639595.516711	41.565773
3517.889719	639265.609333	41.570778
3518.155082	638925.212094	41.575783
3517.863072	638582.144076	41.580788
3517.553934	638257.177123	41.585792
3517.568412	637930.095457	41.590797
3517.326888	637603.796067	41.595802
3517.180661	637266.613865	41.600807
3517.083757	636954.829313	41.605812
3516.886157	636646.404277	41.610816
3516.848915	636318.829911	41.615821
3516.856388	636011.853300	41.620826
3516.843605	635694.012499	41.625831
3516.224017	635390.823758	41.630836
3516.064609	635076.891417	41.635840
3516.480803	634778.568410	41.640845
3516.222855	634482.399794	41.645850
3516.034209	634172.848993	41.650855
3515.472698	633880.166503	41.655860
3515.210273	633589.478545	41.660864
3515.448186	633298.850215	41.665869
3515.518831	633020.504088	41.670874
3515.418954	632724.359729	41.675879
3514.826081	632433.393816	41.680884
3514.967182	632158.567082	41.685888
3515.196618	631877.511506	41.690893
3514.916737	631604.441600	41.695898
3514.771138	631318.677324	41.700903
3514.305385	631052.381810	41.705908
3514.002111	630783.349419	41.710912
3514.177991	630516.033504	41.715917
3513.784891	630250.256462	41.720922
3513.951829	629988.636081	41.725927
3513.676981	629741.651651	41.730932
3513.385359	629476.238964	41.735936
3513.708354	629221.934003	41.740941
3513.099160	628976.989619	41.745946
3513.319403	628725.894235	41.750951
3513.230743	628476.896821	41.755956
3513.028817	628223.806117	41.760960
3512.917268	627983.313580	41.765965
3512.704589	627745.536417	41.770970
3512.757505	627499.948089	41.775975
3512.403573	627277.908231	41.780980
3512.539579	627031.744549	41.785984
3512.607639	626800.510613	41.790989
3512.274540	626570.139086	41.795994
3512.302275	626345.362557	41.800999
3512.178050	626110.339020	41.806004
3512.110736	625882.663521	41.811008
3512.028522	625654.334506	41.816013
3511.730953	625441.463112	41.821018
3511.837548	625215.648102	41.826023
3511.618006	624998.747959	41.831028
3511.632783	624777.246563	41.836032
3511.391357	624562.094374	41.841037
3511.477314	624356.752197	41.846042
3511.631240	624141.676722	41.851047
3511.379086	623930.020207	41.856052
3511.358396	623725.284683	41.861056
3510.996070	623508.778758	41.866061
3510.837767	623300.200387	41.871066
3511.242508	623098.388706	41.876071
3510.872453	622898.504504	41.881076
3510.849154	622694.451227	41.886080
3510.682467	622489.415694	41.891085
3510.466329	622296.158461	41.896090
3510.594276	622084.453194	41.901095
3510.606119	621900.119798	41.906100
3510.407030	621700.335576	41.911104
3510.157846	621502.510055	41.916109
3510.366581	621314.326194	41.921114
3510.348460	621128.932374	41.926119
3509.979839	620937.680332	41.931124
3510.084620	620745.044067	41.936128
3510.110057	620551.565586	41.941133
3509.715004	620379.750869	41.946138
3510.180311	620182.034106	41.951143
3509.922964	620009.338942	41.956148
3509.496349	619818.928689	41.961152
3509.821113	619631.297938	41.966157
3509.346739	619468.753103	41.971162
3509.541177	619286.199537	41.976167
3509.303963	619114.739780	41.981172
3509.708501	618935.804271	41.986176
3509.379794	618760.645314	41.991181
3509.248313	618589.961792	41.996186
3509.055597	618424.047107	42.001191
3508.761322	618255.941322	42.006196
3508.868759	618080.549237	42.011200
3508.965678	617909.967836	42.016205
3508.558248	617754.954960	42.021210
3508.603620	617589.840495	42.026215
3508.519455	617439.080541	42.031220
3508.675756	617275.045801	42.036224
3508.370709	617105.269999	42.041229
3508.464868	616960.138336	42.046234
3508.508998	616799.523600	42.051239
3508.260849	616651.837639	42.056244
3508.280242	616489.768736	42.061248
3508.421012	616341.412973	42.066253
3508.197857	616188.904233	42.071258
3508.326472	616028.865890	42.076263
3508.157227	615888.576077	42.081268
3507.992760	615732.542128	42.086272
3507.970392	615586.960371	42.091277
3507.700459	615438.259062	42.096282
3507.725579	615295.322719	42.101287
3507.450122	615154.990943	42.106292
3507.415929	615020.784313	42.111296
3507.910403	614883.230081	42.116301
3507.717430	614736.361681	42.121306
3507.554369	614598.811989	42.126311
3507.249387	614466.899446	42.131316
3507.271134	614326.458041	42.136320
3507.268868	614195.244461	42.141325
3507.068934	614071.031352	42.146330
3507.560433	613924.239948	42.151335
3507.290267	613794.870835	42.156340
3507.158600	613665.377106	42.161344
3507.198918	613534.750394	42.166349
3507.127957	613399.978615	42.171354
3507.112405	613267.302101	42.176359
3506.841802	613146.449904	42.181364
3506.873092	613017.724075	42.186368
3507.147341	612890.260498	42.191373
3506.720262	612766.020069	42.196378
3507.032534	612630.022452	42.201383
3506.741196	612512.777327	42.206388
3506.516673	612395.068629	42.211392
3506.612180	612275.049290	42.216397
3506.580266	612159.312284	42.221402
3506.387018	612030.862787	42.226407
3506.536626	611914.591838	42.231412
3506.332121	611801.888541	42.236416
3506.347413	611682.026489	42.241421
3506.268889	611579.982287	42.246426
3506.364055	611460.806815	42.251431
3506.439264	611345.695690	42.256436
3506.309158	611234.779889	42.261440
3506.211928	611117.237343	42.266445
3506.076226	610999.750055	42.271450
3506.403446	610892.466877	42.276455
3506.232801	610785.064092	42.281460
3506.255259	610665.139801	42.286464
3506.123670	610557.126530	42.291469
3505.779900	610458.476237	42.296474
3506.234999	610335.417597	42.301479
3505.958926	610237.255768	42.306484
3505.960818	610129.517323	42.311488
3505.900927	610020.182962	42.316493
3506.039327	609922.200868	42.321498
3506.249513	609811.315212	42.326503
3505.858424	609714.020460	42.331508
3505.759537	609593.101510	42.336512
3506.115120	609492.571877	42.341517
3505.588722	609392.537807	42.346522
3505.827227	609278.331601	42.351527
3505.760266	609176.765220	42.356532
3505.624048	609066.932540	42.361536
3505.748185	608976.820051	42.366541
3505.772067	608878.295939	42.371546
3505.837671	608776.102139	42.376551
3505.415894	608680.157914	42.381556
3505.542852	608572.684923	42.386560
3505.468660	608466.698841	42.391565
3505.373829	608379.878390	42.396570
3505.108601	608281.647527	42.401575
3505.235629	608182.247512	42.406580
3505.557898	608090.640466	42.411584
3505.483210	607992.275352	42.416589
3504.825959	607900.426832	42.421594
3505.296172	607815.314961	42.426599
3505.370042	607722.842841	42.431604
3505.113251	607636.695549	42.436608
3505.112209	607538.966546	42.441613
3505.189873	607456.124102	42.446618
3505.579834	607362.392878	42.451623
3505.041959	607262.743148	42.456628
3505.123697	607181.252621	42.461632
3505.293604	607096.385512	42.466637
3504.941050	607010.399742	42.471642
3505.073366	606910.184927	42.476647
3504.753825	606833.725049	42.481652
3505.041047	606741.560959	42.486656
3505.496708	606646.759361	42.491661
3505.046411	606567.860750	42.496666
3505.202567	606475.364881	42.501671
3505.045589	606374.089171	42.506676
3505.162159	606297.403289	42.511680
3505.388418	606204.692963	42.516685
3505.269197	606117.859169	42.521690
3505.265687	606019.615713	42.526695
3504.815534	605928.068284	42.531700
3504.768139	605838.410642	42.536704
3504.767061	605758.729905	42.541709
3504.979619	605674.999209	42.546714
3504.824322	605597.349852	42.551719
3504.583918	605516.151339	42.556724
3504.461296	605437.742834	42.561728
3504.837309	605359.251623	42.566733
3504.894125	605279.859064	42.571738
3504.820830	605187.239984	42.576743
3504.581062	605107.694379	42.581748
3504.802786	605029.376859	42.586752
3504.755781	604941.418215	42.591757
3504.675603	604861.844594	42.596762
3505.066813	604780.938207	42.601767
3504.894579	604695.908825	42.606772
3505.079034	604603.393072	42.611776
3504.989570	604531.346000	42.616781
3504.853787	604448.014967	42.621786
3504.720845	604356.452806	42.626791
3504.993097	604273.555095	42.631796
3504.599999	604197.641626	42.636800
3504.496000	604108.029877	42.641805
3504.318702	604038.854677	42.646810
3504.747075	603958.237447	42.651815
3505.105747	603877.882062	42.656820
3504.669649	603787.619931	42.661824
3504.862335	603706.186604	42.666829
3504.620263	603642.239033	42.671834
3504.804292	603558.547695	42.676839
3504.982748	603479.373505	42.681844
3504.710538	603403.836339	42.686848
3504.676984	603309.238165	42.691853
3504.815042	603230.420226	42.696858
3505.088080	603147.965927	42.701863
3505.032039	603064.210160	42.706868
3504.824406	602973.602826	42.711872
3504.662218	602889.712708	42.716877
3504.545286	602826.241855	42.721882
3504.805427	602739.771548	42.726887
3504.610667	602665.973416	42.731892
3504.578497	602580.403318	42.736896
3504.823359	602504.323298	42.741901
3504.907770	602428.269215	42.746906
3504.832897	602344.912834	42.751911
3504.474666	602262.305235	42.756916
3504.716727	602171.165731	42.761920
3504.762039	602096.772260	42.766925
3504.403994	602033.186174	42.771930
3504.372519	601944.599619	42.776935
3504.632544	601865.501245	42.781940
3504.309835	601803.012334	42.786945
3504.518948	601724.824882	42.791949
3504.405111	601652.412358	42.796954
3504.522443	601563.446984	42.801959
3504.736342	601494.693929	42.806964
3504.613617	601412.192002	42.811969
3504.885911	601327.917710	42.816973
3504.148161	601253.045464	42.821978
3504.459190	601176.493993	42.826983
3504.183995	601105.811326	42.831988
3504.401919	601029.976990	42.836993
3504.435945	600958.288706	42.841997
3504.445158	600879.375488	42.847002
3504.707983	600803.231074	42.852007
3504.323366	600729.853398	42.857012
3504.101509	600657.201427	42.862017
3504.408580	600576.831475	42.867021
3504.245913	600515.263003	42.872026
3504.187318	600444.540593	42.877031
3504.146279	600381.897160	42.882036
3504.201866	600308.293665	42.887041
3504.283841	600239.856082	42.892045
3503.854986	600163.168811	42.897050
3504.059172	600095.061644	42.902055
3504.222074	600043.376976	42.907060
3503.890747	599967.776784	42.912065
3504.127068	599894.492291	42.917069
3503.897950	599837.097984	42.922074
3504.140178	599769.585070	42.927079
3503.839800	599704.018707	42.932084
3503.924585	599635.577088	42.937089
3503.877635	599563.240848	42.942093
3503.808103	599495.677303	42.947098
3503.947300	599432.798215	42.952103
3503.967596	599371.444530	42.957108
3504.116413	599309.366468	42.962113
3504.175122	599232.341661	42.967117
3504.116401	599172.606524	42.972122
3503.948136	599107.416662	42.977127
3504.137030	599041.213657	42.982132
3504.151561	598968.311304	42.987137
3504.045052	598899.846660	42.992141
3503.949168	598837.203912	42.997146
3504.119734	598767.035986	43.002151
3504.107635	598702.420607	43.007156
3504.072992	598636.302338	43.012161
3504.227182	598556.596281	43.017165
3504.041797	598493.464343	43.022170
3504.219319	598420.280649	43.027175
3504.015444	598355.393689	43.032180
3503.925043	598292.295215	43.037185
3503.773299	598230.210706	43.042189
3503.795793	598180.248018	43.047194
3504.226849	598103.405423	43.052199
3504.010287	598040.728058	43.057204
3504.033636	597984.236988	43.062209
3504.237312	597903.815353	43.067213
3503.881646	597839.904545	43.072218
3503.802538	597773.437219	43.077223
3504.005000	597712.848153	43.082228
3504.027093	597639.283467	43.087233
3504.248119	597573.468519	43.092237
3503.917066	597504.982454	43.097242
3503.995053	597439.642239	43.102247
3504.025565	597373.606490	43.107252
3503.919470	597321.200841	43.112257
3504.162314	597249.153948	43.117261
3503.690644	597188.271531	43.122266
3503.856785	597120.554925	43.127271
3504.177886	597060.143781	43.132276
3503.772118	596991.014215	43.137281
3504.008854	596932.474278	43.142285
3503.916192	596864.296678	43.147290
3504.056112	596790.506365	43.152295
3503.972928	596728.251912	43.157300
3503.889596	596666.549536	43.162305
3503.695659	596599.692714	43.167309
3503.494387	596548.203185	43.172314
3503.720311	596490.014336	43.177319
3503.683312	596431.065040	43.182324
3503.640261	596378.996300	43.187329
3503.452373	596312.789674	43.192333
3503.516966	596263.163371	43.197338
3503.513149	596198.432318	43.202343
3503.610864	596148.348103	43.207348
3503.453390	596080.226832	43.212353
3503.714002	596024.440475	43.217357
3503.235912	595975.906769	43.222362
3503.824475	595906.757601	43.227367
3503.526973	595852.217452	43.232372
3503.407335	595803.322642	43.237377
3503.591931	595732.832847	43.242381
3503.368329	595687.369691	43.247386
3503.367883	595631.925811	43.252391
3503.386095	595579.290989	43.257396
3503.424463	595531.122328	43.262401
3503.871201	595461.592138	43.267405
3503.485387	595412.287563	43.272410
3503.468435	595348.156646	43.277415
3503.508348	595299.936559	43.282420
3503.461283	595237.919348	43.287425
3503.871777	595180.446931	43.292429
3503.528471	595130.531491	43.297434
3503.412744	595061.644077	43.302439
3503.617092	595013.897956	43.307444
3503.398921	594966.422161	43.312449
3503.499211	594890.517016	43.317453
3503.338102	594844.588279	43.322458
3503.564848	594788.751411	43.327463
3503.620389	594736.809811	43.332468
3503.711302	594689.834441	43.337473
3503.577698	594630.038189	43.342477
3503.211745	594573.544587	43.347482
3503.598165	594523.757451	43.352487
3503.589992	594463.989912	43.357492
3503.502709	594409.257740	43.362497
3503.711859	594349.654715	43.367501
3503.557638	594286.746068	43.372506
3503.533913	594234.513952	43.377511
3503.561506	594175.844054	43.382516
3503.397759	594118.209944	43.387521
3503.358287	594066.281044	43.392525
3503.425440	594013.430240	43.397530
3503.441684	593951.345589	43.402535
3503.831724	593899.998147	43.407540
3503.447505	593845.663887	43.412545
3503.798301	593787.692230	43.417549
3503.538816	593735.094921	43.422554
3502.948063	593672.757222	43.427559
3503.234849	593621.475814	43.432564
3503.458700	593572.967199	43.437569
3503.482104	593522.281290	43.442573
3503.590836	593469.571891	43.447578
3503.516792	593413.426466	43.452583
3503.459471	593365.314945	43.457588
3503.463032	593307.398151	43.462593
3503.683288	593239.800959	43.467597
3503.054800	593192.435860	43.472602
3503.336739	593143.262901	43.477607
3503.624698	593085.298155	43.482612
3503.202513	593033.528241	43.487617
3503.626272	592968.055946	43.492621
3503.075078	592934.440762	43.497626
3503.534397	592878.556535	43.502631
3503.226118	592829.228366	43.507636
3503.338075	592777.520012	43.512641
3503.403043	592714.566869	43.517645
3503.363084	592668.609695	43.522650
3503.612144	592613.311437	43.527655
3503.704057	592551.407900	43.532660
3503.550186	592496.476899	43.537665
3503.595172	592434.027903	43.542669
3502.984211	592385.300342	43.547674
3503.390637	592325.152254	43.552679
3503.134225	592280.334416	43.557684
3503.149580	592233.010083	43.562689
3503.421599	592178.911670	43.567693
3502.981442	592138.343380	43.572698
3503.224102	592078.020083	43.577703
3503.229580	592035.519266	43.582708
3503.422491	591989.068957	43.587713
3503.667430	591930.854474	43.592717
3503.476606	591879.242334	43.597722
3503.500279	591827.494150	43.602727
3503.447747	591765.911741	43.607732
3503.456862	591708.739781	43.612737
3503.643178	591661.485473	43.617741
3503.337342	591596.025359	43.622746
3503.509076	591536.514813	43.627751
3503.047592	591494.892826	43.632756
3503.352191	591444.754560	43.637761
3503.699494	591392.398524	43.642765
3503.296819	591341.823741	43.647770
3503.268561	591283.701347	43.652775
3503.491351	591232.872315	43.657780
3503.521837	591181.924035	43.662785
3503.514094	591123.797480	43.667789
3503.527929	591080.739229	43.672794
3503.459182	591015.588534	43.677799
3503.288200	590967.285051	43.682804
3503.308085	590926.837775	43.687809
3503.674390	590858.449340	43.692813
3503.198998	590810.748039	43.697818
3503.235442	590754.370855	43.702823
3503.585023	590702.815283	43.707828
3503.530547	590652.029462	43.712833
3503.522589	590593.247205	43.717837
3503.378544	590540.114269	43.722842
3503.846038	590481.655056	43.727847
3503.715181	590426.861424	43.732852
3503.243164	590365.541866	43.737857
3503.393194	590307.837524	43.742861
3502.975532	590264.596210	43.747866
3503.186563	590212.609158	43.752871
3503.269656	590174.208921	43.757876
3503.046610	590119.077357	43.762881
3502.996167	590063.816606	43.767885
3503.147318	590027.967166	43.772890
3502.986011	589969.257348	43.777895
3503.061173	589938.293937	43.782900
3502.807093	589891.909110	43.787905
3503.457383	589828.341787	43.792909
3503.374050	589786.601266	43.797914
3503.494657	589738.797462	43.802919
3503.389637	589687.714391	43.807924
3503.092530	589635.858810	43.812929
3503.424457	589585.858971	43.817933
3503.229270	589530.720100	43.822938
3503.314425	589478.398869	43.827943
3503.425192	589423.912550	43.832948
3503.178903	589376.519490	43.837953
3503.408031	589330.153352	43.842957
3503.242024	589285.108347	43.847962
3502.939489	589235.915070	43.852967
3503.145007	589183.773710	43.857972
3503.191551	589137.939400	43.862977
3503.198203	589083.518937	43.867981
3503.127127	589038.256365	43.872986
3503.208920	588993.973415	43.877991
3503.434520	588940.521209	43.882996
3503.181812	588901.217483	43.888001
3503.414856	588834.196172	43.893005
3503.066170	588792.445659	43.898010
3503.123481	588733.241501	43.903015
3503.327551	588693.108067	43.908020
3503.249094	588642.016157	43.913025
3503.332196	588576.776891	43.918029
3503.202136	588530.919111	43.923034
3503.656697	588491.396991	43.928039
3503.392610	588434.656385	43.933044
3503.146316	588379.420133	43.938049
3503.010203	588325.723282	43.943053
3503.004529	588283.763719	43.948058
3503.472407	588240.419412	43.953063
3503.378681	588183.348031	43.958068
3503.320914	588123.154775	43.963073
3503.415203	588081.529802	43.968077
3503.177657	588035.285817	43.973082
3503.656021	587979.325273	43.978087
3503.239515	587919.943916	43.983092
3503.287986	587871.189735	43.988097
3503.437051	587805.784652	43.993101
3503.440714	587764.726313	43.998106
3503.331576	587708.760814	44.003111
3503.438575	587651.804597	44.008116
3503.380759	587608.042093	44.013121
3503.586594	587553.129578	44.018125
3503.242745	587510.268191	44.023130
3503.249964	587453.025943	44.028135
3503.201507	587398.355649	44.033140
3503.003421	587360.042994	44.038145
3503.152066	587305.088516	44.043149
3503.268329	587259.939141	44.048154
3503.385718	587209.814001	44.053159
3503.178095	587151.600590	44.058164
3502.989691	587110.069100	44.063169
3503.265386	587049.413468	44.068173
3503.145076	587016.263409	44.073178
3502.896430	586961.322575	44.078183
3503.259180	586917.287228	44.083188
3503.370644	586871.885902	44.088193
3503.158359	586817.792810	44.093197
3503.274321	586769.173824	44.098202
3503.160690	586717.727728	44.103207
3503.144809	586681.745052	44.108212
3503.148644	586625.705647	44.113217
3503.050597	586577.472969	44.118221
3503.049079	586535.757927	44.123226
3502.699946	586486.510811	44.128231
3503.036310	586450.720700	44.133236
3502.893270	586407.520740	44.138241
3502.740548	586348.892328	44.143245
3502.871593	586317.005696	44.148250
3502.787252	586270.578907	44.153255
3503.525100	586223.513848	44.158260
3503.282513	586180.329480	44.163265
3503.522463	586118.217497	44.168269
3502.908053	586079.969379	44.173274
3503.207965	586033.980977	44.178279
3503.302626	585975.108941	44.183284
3503.369239	585924.383693	44.188289
3502.949911	585875.497487	44.193293
3502.999390	585833.721358	44.198298
3502.752874	585777.518226	44.203303
3502.575576	585743.368812	44.208308
3502.880622	585717.734775	44.213313
3503.131123	585658.936047	44.218317
3502.737877	585610.446577	44.223322
3502.839184	585572.581546	44.228327
3502.922866	585532.306646	44.233332
3502.722971	585489.866732	44.238337
3502.914698	585441.933622	44.243341
3503.052659	585415.924369	44.248346
3503.193403	585361.816852	44.253351
3503.210072	585314.464993	44.258356
3502.786710	585263.516131	44.263361
3503.124108	585212.089838	44.268365
3502.887622	585170.459076	44.273370
3503.148266	585121.809632	44.278375
3503.096113	585087.788543	44.283380
3503.099410	585038.779050	44.288385
3503.190095	584988.548577	44.293389
3503.062102	584938.906858	44.298394
3503.215180	584894.245252	44.303399
3503.334568	584844.361316	44.308404
3503.016782	584791.131079	44.313409
3503.071063	584748.948288	44.318413
3503.010282	584704.120156	44.323418
3503.066499	584652.134624	44.328423
3503.151562	584612.710990	44.333428
3502.746128	584565.023624	44.338433
3502.872484	584524.537278	44.343437
3502.827715	584479.655412	44.348442
3502.739087	584445.286658	44.353447
3502.920707	584385.186142	44.358452
3502.350458	584348.081445	44.363457
3502.851658	584303.963528	44.368461
3502.816269	584272.350293	44.373466
3503.009159	584221.345775	44.378471
3502.947435	584180.889279	44.383476
3503.113013	584144.768632	44.388481
3503.296884	584095.323423	44.393485
3502.824946	584049.605509	44.398490
3502.969223	584005.846948	44.403495
3503.214812	583969.209895	44.408500
3502.930308	583925.421162	44.413505
3503.025895	583875.939342	44.418509
3502.894738	583831.421214	44.423514
3503.036088	583782.283367	44.428519
3503.104564	583749.998138	44.433524
3503.056191	583702.399364	44.438529
3503.084418	583644.079963	44.443533
3502.670409	583607.751603	44.448538
3502.802305	583554.944569	44.453543
3503.043738	583512.173663	44.458548
3502.808031	583483.104990	44.463553
3503.181532	583438.150360	44.468557
3502.834620	583389.795203	44.473562
3502.962849	583341.562649	44.478567
3503.248595	583293.153129	44.483572
3503.249206	583243.634121	44.488577
3503.142649	583197.500885	44.493581
3503.020451	583158.056426	44.498586
3502.981461	583106.381628	44.503591
3503.075842	583061.019143	44.508596
3502.576956	583025.054949	44.513601
3503.086059	582973.540642	44.518605
3503.246207	582937.467591	44.523610
3503.049764	582879.332382	44.528615
3502.837766	582833.315694	44.533620
3502.860125	582789.120389	44.538625
3503.159706	582738.393744	44.543629
3503.137569	582698.478835	44.548634
3502.976197	582647.727221	44.553639
3503.519959	582607.819316	44.558644
3503.364433	582556.714431	44.563649
3503.222891	582502.741287	44.568653
3502.901534	582459.506402	44.573658
3502.969451	582408.766290	44.578663
3502.871403	582364.790400	44.583668
3502.908783	582325.970556	44.588673
3503.215527	582279.112149	44.593677
3503.043979	582236.254005	44.598682
3502.915850	582192.383007	44.603687
3503.040153	582155.006344	44.608692
3502.827146	582112.154598	44.613697
3502.938617	582062.160039	44.618701
3502.942895	582026.059711	44.623706
3502.739020	581976.569271	44.628711
3502.681787	581935.853206	44.633716
3502.746423	581895.318038	44.638721
3502.772898	581841.615965	44.643725
3503.144589	581794.493610	44.648730
3503.069732	581753.980962	44.653735
3503.140261	581705.500074	44.658740
3502.841038	581671.912408	44.663745
3503.263920	581621.814460	44.668749
3502.956706	581586.920603	44.673754
3503.241209	581538.102115	44.678759
3503.301041	581489.471296	44.683764
3502.646487	581449.907935	44.688769
3503.273157	581392.987606	44.693773
3502.959109	581345.222318	44.698778
3502.663553	581305.096522	44.703783
3502.940452	581260.602356	44.708788
3502.626393	581221.032429	44.713793
3502.785210	581178.468118	44.718797
3502.783010	581139.751608	44.723802
3502.615704	581101.916975	44.728807
3503.022531	581062.076898	44.733812
3502.907400	581026.646974	44.738817
3502.841304	580966.319075	44.743821
3502.856451	580937.303580	44.748826
3502.643045	580887.206927	44.753831
3502.799272	580843.988210	44.758836
3502.717809	580806.289370	44.763841
3502.974710	580763.305196	44.768845
3502.872315	580720.028095	44.773850
3502.828074	580679.909127	44.778855
3502.996236	580623.513351	44.783860
3502.826926	580593.622333	44.788865
3503.208782	580541.565674	44.793869
3502.882784	580505.364450	44.798874
3502.896809	580458.748479	44.803879
3502.888712	580416.862740	44.808884
3502.783779	580378.412187	44.813889
3502.901239	580335.700924	44.818893
3502.668970	580293.248285	44.823898
3502.742964	580256.527849	44.828903
3502.907428	580210.640430	44.833908
3502.691877	580180.152601	44.838913
3502.907074	580143.106845	44.843917
3502.841853	580096.502563	44.848922
3502.630497	580054.749660	44.853927
3503.011543	580008.172077	44.858932
3502.802031	579965.915706	44.863937
3502.993289	579920.324511	44.868941
3502.740261	579883.153986	44.873946
3502.755947	579832.713571	44.878951
3503.040855	579791.129434	44.883956
3502.654381	579752.673037	44.888961
3503.122255	579719.456503	44.893965
3502.942458	579673.724393	44.898970
3502.859881	579628.227533	44.903975
3503.200557	579566.920572	44.908980
3502.582626	579538.609566	44.913985
3503.012137	579486.641185	44.918989
3502.863293	579455.185090	44.923994
3502.850926	579405.703038	44.928999
3503.028338	579371.929972	44.934004
3502.759346	579327.870815	44.939009
3503.017843	579281.813583	44.944013
3502.582382	579233.506928	44.949018
3502.819943	579205.758237	44.954023
3503.028011	579160.211760	44.959028
3502.742096	579119.876097	44.964033
3502.810590	579073.497371	44.969037
3502.917485	579025.201109	44.974042
3503.154940	578985.181085	44.979047
3503.432088	578932.782874	44.984052
3503.069203	578895.225152	44.989057
3503.253018	578842.590485	44.994061
3503.218065	578797.887380	44.999066
3503.189687	578748.455631	45.004071
3503.039128	578706.839029	45.009076
3502.845713	578658.188490	45.014081
3502.906564	578607.685346	45.019085
3502.528617	578571.034379	45.024090
3502.654735	578531.232406	45.029095
3502.930976	578492.964636	45.034100
3502.822893	578456.017397	45.039105
3502.914989	578407.570289	45.044109
3503.005446	578367.823961	45.049114
3502.860221	578327.613412	45.054119
3503.211989	578288.427288	45.059124
3502.874271	578250.360529	45.064129
3502.864199	578201.979748	45.069133
3503.096552	578153.005598	45.074138
3503.101731	578109.651334	45.079143
3503.250073	578066.273328	45.084148
3502.615065	578021.314245	45.089153
3502.840271	577961.577502	45.094157
3502.819642	577925.921935	45.099162
3503.033083	577890.881528	45.104167
3502.967853	577849.851529	45.109172
3502.966551	577797.997364	45.114177
3503.191082	577749.425276	45.119181
3503.048269	577711.777407	45.124186
3503.005628	577667.272679	45.129191
3503.004944	577622.660285	45.134196
3502.806168	577577.225339	45.139201
3502.828889	577532.809951	45.144205
3502.916819	577484.460524	45.149210
3502.857701	577440.058292	45.154215
3503.103384	577408.179911	45.159220
3502.950035	577357.053121	45.164225
3503.102863	577314.074130	45.169229
3502.948771	577272.905978	45.174234
3503.236305	577222.762232	45.179239
3503.300202	577179.093262	45.184244
3502.975722	577131.766085	45.189249
3503.183726	577080.427718	45.194253
3503.059498	577035.229999	45.199258
3503.114908	576989.700723	45.204263
3502.950399	576941.742878	45.209268
3502.754250	576894.946940	45.214273
3502.693941	576858.892462	45.219277
3502.873728	576815.957610	45.224282
3502.883811	576775.314052	45.229287
3503.073449	576734.791673	45.234292
3502.894162	576694.832954	45.239297
3503.050215	576654.164948	45.244301
3502.835827	576605.560130	45.249306
3502.842106	576562.502098	45.254311
3502.829780	576512.958216	45.259316
3502.459017	576482.436565	45.264321
3502.800736	576441.787573	45.269325
3502.711595	576408.201284	45.274330
3502.415041	576364.035548	45.279335
3502.928141	576319.535030	45.284340
3502.390514	576288.637991	45.289345
3502.669993	576239.246143	45.294349
3502.614753	576208.269414	45.299354
3502.885031	576159.079973	45.304359
3502.975455	576110.221789	45.309364
3502.613412	576076.629277	45.314369
3502.510716	576038.064298	45.319373
3502.645624	575995.083718	45.324378
3502.350071	575958.562379	45.329383
3502.889235	575923.965802	45.334388
3502.541862	575896.607946	45.339393
3502.941069	575857.506976	45.344397
3502.602596	575820.589881	45.349402
3502.357119	575777.218506	45.354407
3502.412087	575741.192108	45.359412
3502.624320	575714.848319	45.364417
3502.941739	575670.126221	45.369421
3502.728772	575638.017081	45.374426
3502.823963	575585.534170	45.379431
3502.903829	575549.402510	45.384436
3502.822529	575513.096085	45.389441
3502.476264	575468.029891	45.394445
3502.749488	575438.254748	45.399450
3502.673467	575393.294667	45.404455
3502.528133	575348.999814	45.409460
3502.372588	575317.886494	45.414465
3502.828620	575284.609793	45.419469
3502.427544	575242.117396	45.424474
3502.356193	575201.532448	45.429479
3502.574749	575156.774505	45.434484
3502.346989	575139.557088	45.439489
3502.465271	575090.690336	45.444493
3502.566416	575058.628560	45.449498
3502.850202	575019.393079	45.454503
3502.860720	574976.127664	45.459508
3502.843686	574944.839673	45.464513
3502.872692	574905.293672	45.469517
3502.638329	574856.534427	45.474522
3502.669597	574824.030802	45.479527
3502.868292	574789.738743	45.484532
3502.587673	574751.853120	45.489537
3502.747301	574715.253144	45.494541
3502.654690	574672.858910	45.499546
3502.858817	574643.093268	45.504551
3502.588061	574587.648003	45.509556
3502.780944	574558.236171	45.514561
3502.609634	574510.773210	45.519565
3502.796969	574479.299456	45.524570
3503.035361	574441.126134	45.529575
3502.823172	574386.575889	45.534580
3502.997285	574350.274319	45.539585
3503.145947	574294.959885	45.544589
3502.724276	574247.688114	45.549594
3502.904436	574217.271389	45.554599
3503.021292	574171.218643	45.559604
3502.507205	574123.307604	45.564609
3502.756410	574085.433282	45.569613
3502.923249	574053.609669	45.574618
3502.851370	574019.712271	45.579623
3502.842058	573973.126175	45.584628
3502.684008	573940.903018	45.589633
3502.674992	573880.128860	45.594637
3502.593166	573857.049544	45.599642
3502.278767	573819.971655	45.604647
3502.729132	573772.705333	45.609652
3502.443719	573743.068545	45.614657
3502.618810	573697.759145	45.619661
3502.737379	573658.596960	45.624666
3502.475567	573619.698585	45.629671
3502.648534	573585.457797	45.634676
3502.761111	573560.937160	45.639681
3502.988622	573510.134399	45.644685
3502.939631	573464.458587	45.649690
3502.805431	573424.230447	45.654695
3502.772137	573383.884924	45.659700
3502.573510	573347.390323	45.664705
3502.982534	573299.625910	45.669709
3502.941617	573263.960407	45.674714
3502.999444	573219.020807	45.679719
3503.155053	573170.844843	45.684724
3503.071151	573138.154589	45.689729
3502.864349	573085.258183	45.694733
3502.661220	573048.713144	45.699738
3502.713070	573012.830387	45.704743
3502.841538	572960.632929	45.709748
3502.859969	572928.931565	45.714753
3502.961629	572876.788493	45.719757
3502.742754	572832.044058	45.724762
3502.631014	572796.388905	45.729767
3502.929370	572760.263548	45.734772
3502.573332	572720.522561	45.739777
3502.834332	572681.786718	45.744781
3502.735166	572648.342974	45.749786
3502.641397	572603.778379	45.754791
3502.940699	572561.966570	45.759796
3502.524702	572531.945922	45.764801
3502.831062	572480.421598	45.769805
3503.078543	572441.234397	45.774810
3502.878402	572379.880709	45.779815
3502.549233	572281.765969	45.784820
3502.314785	572135.983760	45.789825
3502.109116	571925.334254	45.794829
3502.198916	571673.621921	45.799834
3501.976252	571356.236845	45.804839
3501.794418	570984.841062	45.809844
3501.507568	570555.025346	45.814849
3501.210730	570063.798890	45.819853
3501.152437	569520.927710	45.824858
3500.726264	568908.033809	45.829863
3500.540540	568241.264635	45.834868
3500.171132	567524.708662	45.839873
3500.056820	566725.212440	45.844877
3499.286822	565880.919512	45.849882
3498.743051	564976.823804	45.854887
3498.475693	563995.433315	45.859892
3497.251218	562972.937168	45.864897
3496.764274	561875.155721	45.869901
3496.034279	560713.211060	45.874906
3495.136614	559499.162298	45.879911
3494.159403	558228.699389	45.884916
3493.670392	556903.174040	45.889921
3492.816686	555506.790212	45.894925
3492.324865	554049.484261	45.899930
3490.790002	552525.673512	45.904935
3490.175190	550941.413583	45.909940
3489.016877	549304.083207	45.914945
3487.833683	547603.093398	45.919949
3486.887549	545854.663699	45.924954
3485.389802	544032.787662	45.929959
3484.464836	542161.106775	45.934964
3482.779487	540242.546246	45.939969
3481.381947	538250.028818	45.944973
3480.281208	536220.606570	45.949978
3478.683705	534122.355011	45.954983
3477.356673	531980.000421	45.959988
3475.520222	529787.042320	45.964993
3473.910980	527541.623007	45.969997
3472.082433	525250.510389	45.975002
3470.329370	522912.476581	45.980007
3468.638500	520521.495141	45.985012
3466.899923	518093.979804	45.990017
3465.290663	515612.862003	45.995021
3463.539166	513088.018143	46.000026
3461.572139	510512.469123	46.005031
3459.702392	507900.801580	46.010036
3457.575143	505244.820561	46.015041
3455.414511	502541.438406	46.020045
3453.215236	499794.379933	46.025050
3450.465807	497012.261101	46.030055
3448.617567	494197.866108	46.035060
3446.090511	491352.102903	46.040065
3444.008210	488467.540122	46.045069
3441.428826	485546.040792	46.050074
3439.116531	482593.693486	46.055079
3436.514924	479609.062367	46.060084
3433.970079	476590.562107	46.065089
3431.687104	473532.426191	46.070093
3428.583993	470452.600726	46.075098
3425.862207	467346.020856	46.080103
3423.398113	464204.492903	46.085108
3420.787093	461035.017700	46.090113
3417.867835	457844.712800	46.095117
3415.081342	454628.637097	46.100122
3411.889996	451389.765626	46.105127
3408.936296	448124.744932	46.110132
3405.860804	444834.949710	46.115137
3402.883122	441518.413821	46.120141
3400.132099	438189.724641	46.125146
3396.661830	434832.956845	46.130151
3393.829728	431459.200866	46.135156
3390.421813	428074.749911	46.140161
3387.172118	424660.604076	46.145165
3384.280313	421246.225684	46.150170
3380.813395	417804.155452	46.155175
3377.533667	414351.228606	46.160180
3373.971874	410887.401499	46.165185
3370.536587	407391.277855	46.170189
3367.341564	403908.738650	46.175194
3363.670403	400406.509859	46.180199
3360.557016	396885.694868	46.185204
3357.024070	393364.373922	46.190209
3353.459340	389821.552439	46.195213
3349.876321	386276.320077	46.200218
3346.502267	382721.811687	46.205223
3342.999853	379145.125422	46.210228
3339.075242	375575.324244	46.215233
3335.307650	371988.398434	46.220237
3331.658726	368410.096149	46.225242
3327.995919	364824.354153	46.230247
3324.208716	361220.288248	46.235252
3320.561220	357629.861745	46.240257
3316.900516	354026.403300	46.245261
3313.108302	350430.115941	46.250266
3309.097670	346817.568062	46.255271
3305.337551	343205.560628	46.260276
3301.596190	339604.602573	46.265281
3297.572580	335990.733201	46.270285
3293.622534	332388.488538	46.275290
3289.726694	328783.759337	46.280295
3286.137006	325175.522388	46.285300
3281.706180	321584.622374	46.290305
3277.775374	317977.936438	46.295309
3273.836188	314369.228544	46.300314
3269.912407	310772.737949	46.305319
3265.986923	307176.514058	46.310324
3261.665138	303601.257474	46.315329
3257.719391	300024.269129	46.320333
3253.675719	296462.113210	46.325338
3249.345542	292885.854794	46.330343
3245.423578	289322.713422	46.335348
3241.228943	285799.272636	46.340353
3237.186410	282250.995011	46.345357
3232.899272	278715.595397	46.350362
3228.591413	275203.108051	46.355367
3224.718912	271685.022049	46.360372
3220.408907	268182.299065	46.365377
3216.106052	264695.182377	46.370381
3212.143426	261211.759557	46.375386
3207.591300	257747.602587	46.380391
3203.681678	254283.035365	46.385396
3199.258074	250851.596497	46.390401
3195.019483	247418.823921	46.395405
3190.963795	243984.294956	46.400410
3186.463358	240586.731498	46.405415
3182.396475	237191.973069	46.410420
3177.888269	233808.475408	46.415425
3174.007867	230451.503404	46.420429
3169.673916	227083.885349	46.425434
3165.365431	223757.601997	46.430439
3161.445334	220417.291737	46.435444
3157.070150	217118.969881	46.440449
3152.524414	213818.111915	46.445453
3148.504229	210533.147891	46.450458
3143.632208	207267.430722	46.455463
3139.498094	204013.830580	46.460468
3135.236029	200757.731504	46.465473
3131.231481	197486.490342	46.470477
3126.729458	194290.304058	46.475482
3122.436034	191103.521240	46.480487
3118.280666	187926.032758	46.485492
3113.890895	184788.995426	46.490497
3109.219898	181639.799903	46.495501
3105.223484	178539.005787	46.500506
3100.764671	175447.852699	46.505511
3096.686746	172358.649817	46.510516
3091.790705	169297.096298	46.515521
3087.456692	166251.250190	46.520525
3083.431114	163232.948612	46.525530
3078.658417	160240.458827	46.530535
3074.399529	157260.677728	46.535540
3069.630421	154298.623246	46.540545
3064.971844	151363.720057	46.545549
3061.111167	148455.931169	46.550554
3056.468966	145565.612336	46.555559
3051.813242	142693.503291	46.560564
3046.642407	139854.180288	46.565569
3042.083107	137042.307145	46.570573
3037.745195	134260.654170	46.575578
3032.867203	131505.010893	46.580583
3028.718857	128764.097815	46.585588
3024.059098	126064.119279	46.590593
3019.450964	123373.733097	46.595597
3014.866590	120724.885738	46.600602
3010.170265	118094.612461	46.605607
3005.449636	115494.635372	46.610612
3000.743918	112920.117714	46.615617
2996.136652	110375.615041	46.620621
2991.599738	107859.540488	46.625626
2986.599305	105375.901827	46.630631
2981.966018	102908.883020	46.635636
2977.524685	100482.309476	46.640641
2972.805186	98081.678079	46.645645
2968.294020	95709.037183	46.650650
2963.833157	93369.586533	46.655655
2959.924478	91030.907977	46.660660
2954.704078	88750.318775	46.665665
2950.293575	86477.413479	46.670669
2946.139950	84250.706376	46.675674
2941.102949	82035.159596	46.680679
2936.939995	79845.583742	46.685684
2932.354660	77676.784736	46.690689
2928.274480	75552.156811	46.695693
2923.599334	73428.781628	46.700698
2919.676291	71331.792004	46.705703
2915.447975	69257.128796	46.710708
2911.063758	67211.982869	46.715713
2906.788125	65181.169154	46.720717
2902.935429	63165.888584	46.725722
2898.420823	61191.557025	46.730727
2894.536097	59210.918276	46.735732
2890.170186	57261.342698	46.740737
2885.998558	55325.474434	46.745741
2882.017392	53416.728080	46.750746
2877.603846	51525.712418	46.755751
2873.829684	49650.309346	46.760756
2869.500928	47787.872856	46.765761
2865.185777	45945.588803	46.770765
2861.143415	44124.306084	46.775770
2856.834496	42331.142529	46.780775
2852.396516	40546.594451	46.785780
2847.406798	38805.194478	46.790785
2842.289074	37087.318322	46.795789
2836.576513	35424.951242	46.800794
2829.555039	33839.771430	46.805799
2822.763152	32301.347218	46.810804
2816.219318	30839.418749	46.815809
2809.709563	29413.012852	46.820813
2803.439538	28053.184711	46.825818
2797.372204	26763.616365	46.830823
2791.672779	25518.128481	46.835828
2785.661030	24341.583972	46.840833
2780.255168	23224.613230	46.845837
2774.834902	22154.323561	46.850842
2769.690661	21140.943167	46.855847
2764.806606	20147.103511	46.860852
2759.672049	19232.611866	46.865857
2754.637828	18347.225499	46.870861
2750.078880	17498.312516	46.875866
2745.132918	16699.894874	46.880871
2740.628174	15936.473093	46.885876
2736.241652	15211.897767	46.890881
2731.645480	14512.898846	46.895885
2727.521950	13840.065319	46.900890
2722.586406	13235.737577	46.905895
2717.850894	12640.465044	46.910900
2713.344477	12085.317465	46.915905
2708.826197	11553.531768	46.920909
2704.519101	11057.912859	46.925914
2700.222868	10578.684841	46.930919
2696.074808	10128.619466	46.935924
2691.690813	9704.478518	46.940929
2687.776222	9302.437729	46.945933
2683.848715	8922.541083	46.950938
2679.821938	8550.761980	46.955943
2676.224548	8193.515615	46.960948
2672.279533	7863.145171	46.965953
2668.357108	7537.539166	46.970957
2665.273212	7220.395994	46.975962
2661.665836	6910.444194	46.980967
2658.380210	6612.034082	46.985972
2654.547938	6326.367272	46.990977
2651.236418	6044.310567	46.995981
2648.216453	5753.176367	47.000986
2644.300754	5485.009516	47.005991
2641.332996	5204.199727	47.010996
2638.010002	4933.892975	47.016001
2634.648739	4667.211151	47.021005
2631.722654	4397.471081	47.026010
2627.561313	4131.606234	47.031015
2624.668157	3867.741049	47.036020
2621.141838	3597.158386	47.041025
2618.055319	3334.516404	47.046029
2614.585027	3070.590105	47.051034
2611.010679	2819.450121	47.056039
2608.046061	2545.958592	47.061044
2604.709450	2287.000396	47.066049
2601.188521	2022.185538	47.071053
2597.876209	1769.513685	47.076058
2593.952170	1520.873944	47.081063
2590.429486	1255.792154	47.086068
2586.491590	1014.583398	47.091073
2582.866846	771.759358	47.096077
2578.851167	543.191714	47.101082
2574.590043	332.889949	47.106087
2570.351659	126.144976	47.111092
2559.516454	119.661391	47.116097
2550.325312	138.712111	47.121101
2544.860618	133.135665	47.126106
2541.064175	143.100072	47.131111
2539.714366	134.809129	47.136116
2537.759797	135.784929	47.141121
2535.082103	140.509589	47.146125
2532.656156	133.943022	47.151130
2529.637422	135.792257	47.156135
2526.740405	129.559592	47.161140
2523.170557	133.339803	47.166145
2519.472773	132.871442	47.171149
2516.443954	134.393577	47.176154
2512.888041	136.190972	47.181159
2509.910916	133.130588	47.186164
2506.002223	144.294833	47.191169
2502.700321	137.886274	47.196173
2499.462061	131.133709	47.201178
2496.184185	132.672097	47.206183
2492.722146	130.378508	47.211188
2489.410387	131.778038	47.216193
2486.034764	133.707910	47.221197
2482.767763	126.911556	47.226202
2478.768790	121.396785	47.231207
2475.923589	126.327513	47.236212
2473.204119	133.441406	47.241217
2469.079178	135.729013	47.246221
2465.203287	129.950020	47.251226
2461.627577	132.803339	47.256231
2459.053159	135.300760	47.261236
2455.095615	122.976010	47.266241
2451.838105	134.098715	47.271245
2448.333365	129.991531	47.276250
2444.927654	136.702067	47.281255
2441.709515	131.137378	47.286260
2438.730186	131.295652	47.291265
2434.778776	127.847522	47.296269
2431.045661	118.525605	47.301274
2427.892882	124.047843	47.306279
2424.885355	124.710843	47.311284
2420.784445	124.952036	47.316289
2417.262959	114.926214	47.321293
2414.278134	115.378660	47.326298
2410.422174	125.071951	47.331303
2407.243257	122.001528	47.336308
2403.458503	120.131882	47.341313
2400.132413	124.623810	47.346317
2396.588211	123.289515	47.351322
2392.907574	128.441074	47.356327
2390.022754	113.335990	47.361332
2386.319586	119.860030	47.366337
2382.866561	118.913272	47.371341
2379.546355	113.079732	47.376346
2375.571947	123.755229	47.381351
2372.487476	118.059202	47.386356
2368.739425	116.320086	47.391361
2365.140551	116.241248	47.396365
2362.282033	115.159267	47.401370
2358.603558	116.729533	47.406375
2355.366563	105.405267	47.411380
2351.723493	116.185137	47.416385
2348.268878	124.270192	47.421389
2344.735576	118.257539	47.426394
2341.200584	125.454412	47.431399
2337.739956	112.911979	47.436404
2334.091192	117.407088	47.441409
2330.512090	121.624290	47.446413
2327.199878	122.741802	47.451418
2323.287315	123.793052	47.456423
2319.922132	123.242702	47.461428
2316.753957	125.639686	47.466433
2313.487034	123.408741	47.471437
2310.430849	120.020927	47.476442
2306.475359	123.994008	47.481447
2302.706008	119.484630	47.486452
2298.829239	126.773869	47.491457
2295.638296	121.034690	47.496461
2292.310380	116.516383	47.501466
2288.932632	128.527718	47.506471
2285.377830	115.538305	47.511476
2282.026100	121.249371	47.516481
2278.359373	127.635254	47.521485
2275.180342	124.482844	47.526490
2271.224026	120.264848	47.531495
2268.155953	118.227655	47.536500
2264.694685	117.581906	47.541505
2261.256696	122.316573	47.546509
2258.076469	111.836900	47.551514
2254.075981	118.302960	47.556519
2250.445764	112.683701	47.561524
2246.707814	120.508926	47.566529
2243.001439	126.023210	47.571533
2240.112485	112.662826	47.576538
2236.513772	120.542230	47.581543
2233.568922	115.620704	47.586548
2229.634733	125.735333	47.591553
2226.060469	117.307568	47.596557
2222.480034	115.572467	47.601562
2218.635062	115.100218	47.606567
2215.557900	123.167437	47.611572
2212.134879	122.862336	47.616577
2208.702185	114.924892	47.621581
2205.709934	108.761255	47.626586
2201.856542	111.665532	47.631591
2198.395037	116.767228	47.636596
2194.488985	115.269635	47.641601
2190.941970	118.935591	47.646605
2187.738832	110.162020	47.651610
2183.910875	124.133930	47.656615
2180.631862	120.148936	47.661620
2177.445208	112.364880	47.666625
2173.864720	110.634167	47.671629
2170.401275	115.229035	47.676634
2166.345047	118.369895	47.681639
2162.948395	108.883136	47.686644
2159.848963	116.541222	47.691649
2156.266706	116.939727	47.696653
2152.815211	112.749189	47.701658
2149.037908	112.971315	47.706663
2145.901063	109.887220	47.711668
2142.376605	113.496991	47.716673
2138.681912	110.381279	47.721677
2135.170650	106.602410	47.726682
2131.354219	112.895886	47.731687
2128.433198	110.891930	47.736692
2124.667270	119.497999	47.741697
2120.948182	116.903163	47.746701
2117.557386	117.200223	47.751706
2114.091875	112.130507	47.756711
2110.929212	112.889765	47.761716
2107.410504	121.413584	47.766721
2104.015928	117.024827	47.771725
2100.427007	109.986304	47.776730
2096.674668	118.293545	47.781735
2093.053094	117.418242	47.786740
2089.985259	113.451528	47.791745
2086.275508	114.435532	47.796749
2082.837892	113.188066	47.801754
2079.443561	115.739367	47.806759
2075.946799	117.016386	47.811764
2072.307943	119.748973	47.816769
2068.571986	121.742178	47.821773
2065.322189	118.563908	47.826778
2061.619533	121.277043	47.831783
2058.256768	114.336583	47.836788
2055.108082	108.617835	47.841793
2051.283728	114.280793	47.846797
2047.987127	114.081625	47.851802
2044.004813	115.331693	47.856807
2040.964737	109.564432	47.861812
2037.467829	109.058727	47.866817
2034.022034	107.691875	47.871821
2030.531559	108.651944	47.876826
2026.785328	109.393566	47.881831
2023.259780	110.389626	47.886836
2019.874732	114.508293	47.891841
2016.086682	120.521088	47.896845
2012.919703	112.474600	47.901850
2009.261310	118.209839	47.906855
2005.791391	115.692548	47.911860
2002.421671	109.939890	47.916865
1998.673402	112.426163	47.921869
1995.459055	106.848153	47.926874
1991.943004	114.509027	47.931879
1988.382372	108.006836	47.936884
1984.877426	104.711709	47.941889
1981.030348	114.070316	47.946893
1977.911050	114.046753	47.951898
1974.537910	115.931957	47.956903
1970.903033	109.272131	47.961908
1967.566897	106.465971	47.966913
1963.612247	118.986584	47.971917
1960.637785	118.781437	47.976922
1956.747565	113.671869	47.981927
1953.765263	109.961084	47.986932
1950.364999	108.245966	47.991937
1946.038130	112.088450	47.996941
1942.928195	102.722652	48.001946
1939.103389	107.486288	48.006951
1935.807435	114.049748	48.011956
1932.441271	114.603161	48.016961
1928.992519	108.958929	48.021965
1925.810538	102.783999	48.026970
1921.925659	108.648072	48.031975
1918.432633	105.924695	48.036980
1914.636805	108.262592	48.041985
1910.910013	116.151129	48.046989
1907.843008	108.849942	48.051994
1903.993182	111.795498	48.056999
1900.467010	108.712331	48.062004
1897.415785	110.470414	48.067009
1893.983373	108.649347	48.072013
1890.796113	101.816396	48.077018
1886.693741	101.692017	48.082023
1883.285660	109.121998	48.087028
1879.664966	103.964036	48.092033
1876.425864	98.011115	48.097037
1873.144861	105.358344	48.102042
1869.381154	111.327951	48.107047
1865.913139	108.048718	48.112052
1862.307126	104.223746	48.117057
1858.577345	109.549756	48.122061
1855.409602	94.130696	48.127066
1851.765531	110.636473	48.132071
1848.298617	100.841493	48.137076
1845.172774	103.786699	48.142081
1841.408909	108.256567	48.147085
1837.981790	110.892384	48.152090
1834.275259	107.862939	48.157095
1830.681061	105.591080	48.162100
1827.220299	112.316811	48.167105
1823.481657	108.086339	48.172109
1820.256334	109.026638	48.177114
1816.743009	109.982743	48.182119
1813.373190	109.107706	48.187124
1810.141272	102.502029	48.192129
1806.095600	105.967835	48.197133
1802.801658	98.366174	48.202138
1798.956654	105.439761	48.207143
1795.922731	100.231117	48.212148
1792.614112	102.354434	48.217153
1788.643277	102.805167	48.222157
1785.264184	94.012038	48.227162
1781.510537	100.355581	48.232167
1778.229409	101.261121	48.237172
1774.686231	100.906325	48.242177
1771.221280	108.747557	48.247181
1768.175042	105.283872	48.252186
1764.549015	102.675728	48.257191
1761.313602	98.802049	48.262196
1757.554712	104.148924	48.267201
1753.360725	107.701635	48.272205
1750.156846	97.558396	48.277210
1746.607643	108.515744	48.282215
1743.459593	105.168355	48.287220
1740.192148	100.874122	48.292225
1736.055673	106.290496	48.297229
1733.001921	92.916489	48.302234
1729.078435	98.527580	48.307239
1725.425814	106.305121	48.312244
1722.138776	103.258761	48.317249
1718.495215	102.487627	48.322253
1715.504285	97.408892	48.327258
1711.848081	97.590438	48.332263
1708.134184	98.347489	48.337268
1704.954522	99.682304	48.342273
1700.800842	104.365866	48.347277
1697.737236	95.436421	48.352282
1694.396024	107.602285	48.357287
1691.203742	99.863142	48.362292
1687.520405	102.816485	48.367297
1683.648864	102.820700	48.372301
1680.306191	99.548532	48.377306
1676.824533	105.999760	48.382311
1673.043827	92.716896	48.387316
1670.077553	99.095803	48.392321
1666.384475	107.333556	48.397325
1662.593631	103.264190	48.402330
1659.012745	101.230431	48.407335
1655.526355	100.737874	48.412340
1652.501547	106.962871	48.417345
1648.931005	104.832094	48.422349
1645.430141	96.194966	48.427354
1641.516533	101.636953	48.432359
1638.030929	102.430144	48.437364
1635.004343	104.059207	48.442369
1631.153793	109.163004	48.447373
1627.633645	103.008450	48.452378
1624.324600	97.845581	48.457383
1620.682956	96.422790	48.462388
1617.205564	97.896843	48.467393
1613.633627	106.545409	48.472397
1610.190335	101.173844	48.477402
1606.516224	107.370383	48.482407
1603.250324	103.568358	48.487412
1599.826677	99.925014	48.492417
1596.408364	104.138852	48.497421
1593.050742	89.236649	48.502426
1588.795763	98.141160	48.507431
1585.213328	97.618546	48.512436
1582.019178	97.211552	48.517441
1578.064468	107.344432	48.522445
1575.541230	102.922418	48.527450
1571.875850	104.322779	48.532455
1568.212911	98.658380	48.537460
1564.979514	91.971439	48.542465
1561.039540	99.359664	48.547469
1557.960621	94.660853	48.552474
1554.029202	100.625643	48.557479
1550.761031	103.363271	48.562484
1547.240582	91.856794	48.567489
1543.246223	97.490595	48.572493
1540.168118	98.712830	48.577498
1536.807808	101.815576	48.582503
1533.164612	98.237769	48.587508
1529.857275	98.134473	48.592513
1525.858605	102.605291	48.597517
1522.649129	92.631294	48.602522
1518.926354	101.317279	48.607527
1515.817551	101.511334	48.612532
1512.600093	99.311268	48.617537
1508.545722	109.807197	48.622541
1505.048233	99.129336	48.627546
1501.551311	96.841663	48.632551
1498.124303	102.573559	48.637556
1494.879523	92.714349	48.642561
1490.940331	98.753092	48.647565
1487.570430	89.143876	48.652570
1483.993649	95.525700	48.657575
1480.321954	94.195606	48.662580
1477.290430	97.149334	48.667585
1473.531575	93.952217	48.672589
1470.146614	78.604718	48.677594
1466.734372	95.258093	48.682599
1463.040798	89.130959	48.687604
1459.506577	93.595128	48.692609
1455.919333	99.105279	48.697613
1452.642471	92.398177	48.702618
1449.191174	93.299112	48.707623
1445.696444	95.168662	48.712628
1442.020386	89.106536	48.717633
1438.455215	103.098241	48.722637
1435.286204	94.951695	48.727642
1431.564151	100.292724	48.732647
1427.919541	93.898815	48.737652
1424.365464	97.671461	48.742657
1420.834496	94.595189	48.747661
1417.840237	93.704353	48.752666
1414.399792	86.993140	48.757671
1410.761598	95.224364	48.762676
1407.228599	94.067167	48.767681
1403.244128	98.447724	48.772685
1399.953002	94.164371	48.777690
1396.506790	98.919127	48.782695
1393.272920	93.066943	48.787700
1389.770725	96.108581	48.792705
1385.720363	104.211795	48.797709
1382.074926	88.558716	48.802714
1378.723358	101.486622	48.807719
1375.530901	92.500572	48.812724
1372.079107	96.979993	48.817729
1368.671896	93.636634	48.822733
1365.248053	95.250617	48.827738
1361.716183	89.823446	48.832743
1358.166554	96.744145	48.837748
1354.559670	91.948628	48.842753
1350.771565	96.590411	48.847757
1347.604872	86.024377	48.852762
1343.773066	102.858476	48.857767
1340.374785	91.765740	48.862772
1337.294509	90.087585	48.867777
1333.497781	99.452338	48.872781
1330.064303	93.216613	48.877786
1326.196906	88.871882	48.882791
1322.961322	95.386079	48.887796
1319.559506	93.897247	48.892801
1315.796461	105.745484	48.897805
1312.631430	102.789177	48.902810
1308.814708	90.487274	48.907815
1305.280395	93.615783	48.912820
1301.983487	95.287963	48.917825
1298.177974	94.152610	48.922829
1295.058183	94.670687	48.927834
1291.315210	99.100022	48.932839
1288.095200	96.345031	48.937844
1284.452435	95.961683	48.942849
1280.877102	101.384347	48.947853
1277.637020	86.109958	48.952858
1273.847583	93.275390	48.957863
1270.550759	92.571225	48.962868
1267.122203	98.529879	48.967873
1263.207731	86.342062	48.972877
1259.894223	87.567872	48.977882
1256.327233	92.774665	48.982887
1253.036181	85.115344	48.987892
1249.806469	82.632341	48.992897
1245.715057	97.405784	48.997901
1242.312463	85.364849	49.002906
1238.951160	89.353619	49.007911
1235.312513	98.514706	49.012916
1231.768490	89.695623	49.017921
1228.319695	97.673859	49.022925
1225.046407	86.774084	49.027930
1221.278452	94.662606	49.032935
1218.222022	88.749651	49.037940
1214.574665	86.384458	49.042945
1210.468164	95.771698	49.047949
1207.410384	82.317484	49.052954
1203.535411	90.420258	49.057959
1200.428168	98.288766	49.062964
1197.211220	82.836179	49.067969
1193.228308	90.357685	49.072973
1189.838290	82.422914	49.077978
1186.240438	89.787032	49.082983
1182.476736	96.214772	49.087988
1179.273885	90.027478	49.092993
1175.976852	91.905394	49.097997
1172.478640	92.401260	49.103002
1168.872267	88.940218	49.108007
1165.661645	91.946051	49.113012
1161.774676	88.945224	49.118017
1158.475243	97.035568	49.123021
1155.069006	94.075052	49.128026
1151.219534	91.610123	49.133031
1147.561090	96.404483	49.138036
1144.380627	94.196397	49.143041
1140.444689	90.729479	49.148045
1137.326212	88.363148	49.153050
1133.767365	89.497394	49.158055
1130.271333	85.702203	49.163060
1126.861606	86.895669	49.168065
1123.415033	91.446627	49.173069
1119.945786	87.923684	49.178074
1116.087514	90.972100	49.183079
1112.762245	90.445424	49.188084
1109.470741	74.688126	49.193089
1105.730207	86.386744	49.198093
1102.320689	76.109710	49.203098
1098.992377	79.066173	49.208103
1095.245161	79.892961	49.213108
1091.855922	80.301013	49.218113
1087.836819	89.016366	49.223117
1084.520298	81.542748	49.228122
1081.322318	85.986720	49.233127
1077.564796	80.051262	49.238132
1074.341486	81.389772	49.243137
1070.666208	92.834903	49.248141
1067.539740	73.201667	49.253146
1064.023882	77.886075	49.258151
1060.341533	82.389627	49.263156
1056.636527	82.609559	49.268161
1053.011979	82.248252	49.273165
1050.045730	82.641649	49.278170
1046.222382	74.555464	49.283175
1042.808247	81.474300	49.288180
1039.092212	81.180624	49.293185
1035.308436	88.348456	49.298189
1032.174602	81.890762	49.303194
1028.576197	82.910070	49.308199
1025.556988	78.015095	49.313204
1022.010443	73.863273	49.318209
1018.272292	83.309337	49.323213
1014.440494	87.916179	49.328218
1010.934578	85.704583	49.333223
1007.849763	86.912688	49.338228
1004.602620	71.575784	49.343233
1000.616404	83.586045	49.348237
997.421966	79.065604	49.353242
993.687450	80.470549	49.358247
989.761515	82.797935	49.363252
986.471302	80.966876	49.368257
982.847205	83.099311	49.373261
979.863354	81.817700	49.378266
976.548700	86.599934	49.383271
972.765916	83.409772	49.388276
969.179596	84.182824	49.393281
965.301681	82.063370	49.398285
962.119989	80.564855	49.403290
958.773972	88.010825	49.408295
955.271380	82.883450	49.413300
951.758037	79.530347	49.418305
947.983151	87.513951	49.423309
944.732920	84.653508	49.428314
940.786055	85.027989	49.433319
937.390515	81.929715	49.438324
934.339377	76.741514	49.443329
930.623159	86.385696	49.448333
927.103294	82.126528	49.453338
923.556136	90.815864	49.458343
920.174897	83.533252	49.463348
916.736502	79.274236	49.468353
912.998157	87.963819	49.473357
909.422988	83.064965	49.478362
905.872267	98.725671	49.483367
902.414546	88.572216	49.488372
899.169222	83.870820	49.493377
895.663972	84.408123	49.498381
892.265451	81.961396	49.503386
888.635145	81.434621	49.508391
884.463708	82.302538	49.513396
881.465344	84.664473	49.518401
878.219718	85.744352	49.523405
874.980160	78.524388	49.528410
871.056387	85.920730	49.533415
867.729153	92.021759	49.538420
864.038552	85.381189	49.543425
860.553888	85.310866	49.548429
857.188711	78.593394	49.553434
853.535192	82.593073	49.558439
849.854169	78.225844	49.563444
846.461973	86.668583	49.568449
842.789815	99.033744	49.573453
839.266960	88.548146	49.578458
836.225369	88.082306	49.583463
832.500498	78.406264	49.588468
829.337056	83.240353	49.593473
825.760239	92.377094	49.598477
821.849271	82.159363	49.603482
818.128412	85.449926	49.608487
814.968874	91.755520	49.613492
811.708618	79.156248	49.618497
807.915976	87.061396	49.623501
804.619258	74.693327	49.628506
800.812423	83.406752	49.633511
797.310791	79.761555	49.638516
794.172673	74.206195	49.643521
790.472194	83.058525	49.648525
787.328601	79.220516	49.653530
783.781834	77.489275	49.658535
779.606859	81.053505	49.663540
776.355869	66.496930	49.668545
772.776093	90.084824	49.673549
769.599492	72.760321	49.678554
765.936675	77.295995	49.683559
762.553507	77.199291	49.688564
758.853452	81.408815	49.693569
755.105497	81.955986	49.698573
751.838059	75.457661	49.703578
748.645957	78.726724	49.708583
744.872721	70.595239	49.713588
741.860667	70.364937	49.718593
737.880608	73.646737	49.723597
734.527826	67.734431	49.728602
730.843154	74.052742	49.733607
727.391736	71.297184	49.738612
724.016723	66.303816	49.743617
720.133210	68.220859	49.748621
716.826396	58.725808	49.753626
713.376189	72.726559	49.758631
710.192621	68.045489	49.763636
706.401555	68.053406	49.768641
702.719217	70.427173	49.773645
699.107210	64.642043	49.778650
695.600046	67.895772	49.783655
692.312316	63.231358	49.788660
689.061503	67.068045	49.793665
685.579675	78.397564	49.798669
682.222892	64.998002	49.803674
678.537106	74.075311	49.808679
674.844008	72.311535	49.813684
671.252602	70.751168	49.818689
667.613632	67.460921	49.823693
664.414412	63.449478	49.828698
661.047921	63.515857	49.833703
657.554943	63.698479	49.838708
653.753480	64.188874	49.843713
650.089951	69.384058	49.848717
646.920585	69.907034	49.853722
643.400895	70.536910	49.858727
639.871133	69.085957	49.863732
636.580087	66.423330	49.868737
632.851940	69.956787	49.873741
629.418319	55.656125	49.878746
625.642675	59.584815	49.883751
621.999982	69.057799	49.888756
619.028315	62.557225	49.893761
615.123410	61.922384	49.898765
611.990590	62.525970	49.903770
608.341003	66.307722	49.908775
604.561868	67.682284	49.913780
601.295726	64.773433	49.918785
597.722095	71.330407	49.923789
594.387632	58.463994	49.928794
590.481063	65.995252	49.933799
587.309625	64.758565	49.938804
584.087460	71.820400	49.943809
580.202670	66.711198	49.948813
577.016224	61.726022	49.953818
573.563234	69.409383	49.958823
569.596997	65.241940	49.963828
566.451022	64.086305	49.968833
562.493374	61.934627	49.973837
559.050479	61.662861	49.978842
555.463782	67.523257	49.983847
551.789505	76.801423	49.988852
548.788146	67.406340	49.993857
545.421495	65.489204	49.998861
541.960574	61.771382	50.003866
538.252391	66.111679	50.008871
534.435132	72.546801	50.013876
531.518897	65.925624	50.018881
527.686886	75.887828	50.023885
524.300283	69.293770	50.028890
520.821585	72.325063	50.033895
516.953897	73.940107	50.038900
513.649070	66.285655	50.043905
510.065101	75.270860	50.048909
506.710375	68.776131	50.053914
503.319366	72.680943	50.058919
499.428798	77.966900	50.063924
496.147797	61.543609	50.068929
492.958046	74.866767	50.073933
489.634054	68.331446	50.078938
485.780042	66.244979	50.083943
482.095762	67.240258	50.088948
478.577122	65.452125	50.093953
475.085465	74.137519	50.098957
471.724002	66.084580	50.103962
468.322319	70.550831	50.108967
464.537919	73.261960	50.113972
461.246029	67.415187	50.118977
457.684149	72.491480	50.123981
454.323896	73.229707	50.128986
450.525077	73.022847	50.133991
447.193561	68.015009	50.138996
443.505925	74.352189	50.144001
439.666093	73.509992	50.149005
436.494912	69.233994	50.154010
433.107648	76.974267	50.159015
429.224807	77.634023	50.164020
426.478813	74.945690	50.169025
422.507589	70.245218	50.174029
419.226962	59.124180	50.179034
415.685412	66.322453	50.184039
411.860061	72.083334	50.189044
408.773461	70.822280	50.194049
404.955685	76.574810	50.199053
401.635541	64.637429	50.204058
398.092902	72.415278	50.209063
394.614247	70.073975	50.214068
391.450335	65.809242	50.219073
387.706567	73.851073	50.224077
384.144886	77.504990	50.229082
380.403267	72.248944	50.234087
376.815634	72.574738	50.239092
373.861517	59.541777	50.244097
370.082247	71.683635	50.249101
366.263386	70.074144	50.254106
362.921237	63.846426	50.259111
359.416941	72.188853	50.264116
356.369108	71.865676	50.269121
352.503338	74.833289	50.274125
349.385134	70.215289	50.279130
345.544356	78.413123	50.284135
341.920989	69.260668	50.289140
338.460815	68.056563	50.294145
334.844186	74.441868	50.299149
331.576862	71.333718	50.304154
328.301859	65.663639	50.309159
324.645092	71.379125	50.314164
321.257207	63.093690	50.319169
317.775799	76.059109	50.324173
314.210782	65.886662	50.329178
310.432498	66.757338	50.334183
306.829831	60.568449	50.339188
303.557910	63.931149	50.344193
299.924513	70.169280	50.349197
296.536286	63.286393	50.354202
292.970686	67.493964	50.359207
288.948682	65.505537	50.364212
285.883021	69.333766	50.369217
282.605344	66.443453	50.374221
279.036114	67.912806	50.379226
275.428672	65.444325	50.384231
271.715339	69.951257	50.389236
268.491580	62.958091	50.394241
264.764303	65.546859	50.399245
261.525416	58.240665	50.404250
257.916893	71.757602	50.409255
254.335823	64.328871	50.414260
251.114562	62.701472	50.419265
247.567148	70.277558	50.424269
244.181593	64.735568	50.429274
240.710230	62.390424	50.434279
236.947893	72.949510	50.439284
233.452254	59.792985	50.444289
229.770312	70.230429	50.449293
226.292411	62.983759	50.454298
222.673744	71.470722	50.459303
219.419818	68.400503	50.464308
216.006330	63.014519	50.469313
212.137280	67.461434	50.474317
208.760601	67.478543	50.479322
205.603317	68.204675	50.484327
202.362587	68.080685	50.489332
198.549485	64.891506	50.494337
194.822770	59.586402	50.499341
191.523204	60.208224	50.504346
187.992694	57.477653	50.509351
184.275525	65.158059	50.514356
180.673223	58.668286	50.519361
176.729185	62.920443	50.524365
174.176776	58.887160	50.529370
170.260568	63.215031	50.534375
166.806353	64.061586	50.539380
163.618107	60.725976	50.544385
159.972558	67.486997	50.549389
156.363636	69.223702	50.554394
152.867272	74.531517	50.559399
149.053241	73.108300	50.564404
145.860073	62.810318	50.569409
142.301005	72.680866	50.574413
139.011312	67.868037	50.579418
135.190847	75.211172	50.584423
131.563024	76.378950	50.589428
128.564194	67.313335	50.594433
124.737573	61.561688	50.599437
121.573245	68.212678	50.604442
117.777685	69.984854	50.609447
114.329240	70.881409	50.614452
110.574366	63.194857	50.619457
107.351423	71.828330	50.624461
103.875783	68.551004	50.629466
100.307460	70.656959	50.634471
96.715144	74.278483	50.639476
93.622006	70.024367	50.644481
90.242801	72.703064	50.649485
86.529560	69.573626	50.654490
82.625603	65.700832	50.659495
78.908180	68.034352	50.664500
75.802649	65.887482	50.669505
72.037623	62.505558	50.674509
68.749463	71.333574	50.679514
65.278574	70.202903	50.684519
61.597390	68.520968	50.689524
58.280873	70.765432	50.694529
54.741461	73.441477	50.699533
51.382542	63.037622	50.704538
47.558194	66.199529	50.709543
44.321538	70.132999	50.714548
40.861865	63.648153	50.719553
37.441655	61.420216	50.724557
33.639768	64.348716	50.729562
30.063185	72.665662	50.734567
26.499240	69.316788	50.739572
23.330001	61.438234	50.744577
19.700734	70.098789	50.749581
16.259543	64.239419	50.754586
12.870199	69.981518	50.759591
9.648463	72.160793	50.764596
5.821034	63.440083	50.769601
2.119664	68.941011	50.774605