Tue Jun 21 10:21:58 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.060733	81.909437	0.000000
0.594184	86.161956	0.005005
0.871581	95.233358	0.010010
0.980474	98.664395	0.015014
1.187409	88.025344	0.020019
0.632583	90.913106	0.025024
0.979016	76.230249	0.030029
0.426358	76.794814	0.035034
0.248134	64.113990	0.040038
-0.144696	48.885991	0.045043
-0.429348	47.935239	0.050048
-0.536497	39.150099	0.055053
-1.199030	25.937372	0.060058
-1.374673	19.433922	0.065062
-1.138831	11.256229	0.070067
-1.983601	4.094576	0.075072
-2.171252	-0.222383	0.080077
-2.033271	-8.689137	0.085082
-2.524881	-13.518557	0.090086
-2.727678	-20.340924	0.095091
-3.326255	-6.855200	0.100096
-3.560821	-22.852891	0.105101
-4.528743	-13.094629	0.110106
-5.064466	-6.944756	0.115110
-4.551344	-15.343190	0.120115
-5.022911	-4.425489	0.125120
-4.713206	-13.742377	0.130125
-5.158308	-3.860525	0.135130
-5.439807	-13.738412	0.140134
-5.221582	-18.283997	0.145139
-5.585466	-15.555350	0.150144
-6.241449	-14.168158	0.155149
-6.320129	-7.651940	0.160154
-6.694145	-11.821016	0.165158
-6.631837	-7.131583	0.170163
-7.285699	-7.351044	0.175168
-7.705254	-8.312407	0.180173
-8.055974	-7.913300	0.185178
-8.252060	-15.927890	0.190182
-8.097647	-8.318165	0.195187
-8.486293	-1.039423	0.200192
-8.033209	-6.052119	0.205197
-8.611735	-3.067306	0.210202
-9.625910	-0.987749	0.215206
-9.677334	-9.833592	0.220211
-10.166332	2.064791	0.225216
-9.801696	-10.294424	0.230221
-9.854395	-15.127456	0.235226
-10.058660	-0.181629	0.240230
-10.319681	-16.421809	0.245235
-11.172039	-7.376705	0.250240
-11.602297	-4.592072	0.255245
-11.590999	-17.705985	0.260250
-11.652426	-12.194492	0.265254
-11.263006	-13.285476	0.270259
-12.792525	-4.179739	0.275264
-13.181445	-9.276778	0.280269
-12.690828	-5.704144	0.285274
-13.084623	-4.535403	0.290278
-12.878998	-15.296118	0.295283
-13.091753	-13.414987	0.300288
-13.388180	-14.260380	0.305293
-13.950427	-4.860162	0.310298
-14.680699	-3.719174	0.315302
-14.635602	-9.935535	0.320307
-15.084259	-6.633603	0.325312
-14.660359	-14.516625	0.330317
-15.001836	-10.972750	0.335322
-15.170276	-6.277469	0.340326
-15.881247	-10.041463	0.345331
-16.644882	-10.044226	0.350336
-16.505626	-7.173540	0.355341
-16.431819	-9.505984	0.360346
-16.606367	-5.158974	0.365350
-16.542046	-14.089496	0.370355
-16.777494	-1.348651	0.375360
-17.269161	-8.588697	0.380365
-17.352740	-9.050200	0.385370
-17.961485	-0.251647	0.390374
-18.081703	-17.551541	0.395379
-19.326149	-6.485529	0.400384
-18.618927	-8.740924	0.405389
-19.220044	-18.695921	0.410394
-19.522861	-0.558864	0.415398
-19.558879	-12.734117	0.420403
-19.930174	-6.734609	0.425408
-19.730382	-14.431334	0.430413
-19.716409	-5.185145	0.435418
-20.304715	-8.614249	0.440422
-20.707867	-9.729288	0.445427
-20.830124	-1.846416	0.450432
-20.786318	-11.550843	0.455437
-20.995538	-4.766143	0.460442
-22.103383	-14.637623	0.465446
-22.289205	-11.448678	0.470451
-22.684451	-6.126401	0.475456
-22.740502	-11.477276	0.480461
-22.591747	-10.039627	0.485466
-22.756649	-3.331332	0.490470
-22.984758	-6.980715	0.495475
-23.356711	-5.736065	0.500480
-23.770908	-10.753534	0.505485
-24.120556	-18.490300	0.510490
-24.021608	-9.459664	0.515494
-24.243056	-16.155410	0.520499
-24.729601	-12.395506	0.525504
-25.313260	-20.117199	0.530509
-25.365507	-8.980439	0.535514
-25.860595	-3.315433	0.540518
-25.444531	-16.653452	0.545523
-25.980625	-9.843039	0.550528
-25.848343	-15.786122	0.555533
-26.529708	-8.478050	0.560538
-27.100506	-9.265378	0.565542
-26.994820	-11.248097	0.570547
-27.482606	-8.636669	0.575552
-27.677425	-8.933130	0.580557
-27.534554	-10.112344	0.585562
-27.713333	-8.300971	0.590566
-27.617651	-12.253008	0.595571
-28.735741	-9.738680	0.600576
-29.044200	-18.403423	0.605581
-28.924911	-10.745459	0.610586
-29.079479	-15.683573	0.615590
-29.390136	-11.252456	0.620595
-30.053172	-10.725851	0.625600
-30.133393	-10.823038	0.630605
-30.349848	-11.466777	0.635610
-30.674055	-12.592322	0.640614
-30.567252	-22.832280	0.645619
-30.826772	-1.922945	0.650624
-30.954050	-15.074095	0.655629
-31.509220	-20.150306	0.660634
-31.961520	-7.582138	0.665638
-31.990819	-19.367972	0.670643
-32.518964	-17.848619	0.675648
-31.941731	-18.987480	0.680653
-32.564468	-11.318721	0.685658
-33.250425	-12.379624	0.690662
-33.514053	-14.048595	0.695667
-33.955629	-10.678176	0.700672
-33.937946	-13.139065	0.705677
-33.717550	-10.622416	0.710682
-34.235397	-13.014946	0.715686
-33.938591	-22.234380	0.720691
-35.064676	-14.746103	0.725696
-35.313094	-14.648294	0.730701
-35.229553	-13.975568	0.735706
-35.419371	-8.710793	0.740710
-35.399182	-15.128846	0.745715
-35.796410	-5.317280	0.750720
-36.583395	-3.898720	0.755725
-37.056570	-9.459746	0.760730
-37.521136	-13.816879	0.765734
-37.262977	-12.025570	0.770739
-37.237609	-5.482381	0.775744
-37.283749	-21.999277	0.780749
-37.016617	-14.436246	0.785754
-37.875643	-7.732984	0.790758
-38.432690	-20.175174	0.795763
-38.935914	-4.526472	0.800768
-39.042062	-8.549278	0.805773
-39.044655	-11.978878	0.810778
-39.112171	-8.752692	0.815782
-38.851372	-17.366861	0.820787
-39.654450	-5.468765	0.825792
-40.170547	-10.644195	0.830797
-40.241974	-9.973037	0.835802
-40.717006	-0.060178	0.840806
-40.476762	-8.904789	0.845811
-40.763036	-7.617100	0.850816
-41.473855	-1.687064	0.855821
-41.745693	-12.986169	0.860826
-42.149159	-0.264071	0.865830
-42.011634	-6.325637	0.870835
-42.135974	-2.627882	0.875840
-42.224091	-3.717142	0.880845
-42.823839	-8.578772	0.885850
-43.222052	-8.773272	0.890854
-43.022550	-5.668659	0.895859
-43.964593	0.584225	0.900864
-43.763750	-4.104908	0.905869
-43.737182	-11.546407	0.910874
-43.980633	-13.833810	0.915878
-44.481129	-16.218555	0.920883
-44.924360	-10.617984	0.925888
-45.175256	-8.505376	0.930893
-45.167381	-5.868877	0.935898
-45.521273	-11.270278	0.940902
-45.582280	-15.501050	0.945907
-46.007747	-10.883185	0.950912
-46.291046	-17.609139	0.955917
-46.753472	-8.685833	0.960922
-46.905677	-7.416399	0.965926
-46.868507	-8.035440	0.970931
-47.189720	-9.168583	0.975936
-47.582205	-13.386493	0.980941
-48.056909	-13.542278	0.985946
-48.213580	-9.025561	0.990950
-48.055329	-23.770692	0.995955
-48.338785	-14.409149	1.000960
-48.407489	-16.099546	1.005965
-49.279860	-8.614405	1.010970
-49.794162	-5.583984	1.015974
-49.723757	-12.066594	1.020979
-49.860135	-5.644818	1.025984
-49.942016	-6.892978	1.030989
-50.018873	-9.192578	1.035994
-50.268561	-7.138383	1.040998
-50.983726	-16.170301	1.046003
-51.310777	-11.327592	1.051008
-51.409416	-16.152224	1.056013
-51.103356	-23.113121	1.061018
-51.609401	-6.976935	1.066022
-51.887402	-9.552644	1.071027
-52.899715	-12.786216	1.076032
-53.025485	-11.230092	1.081037
-53.010192	-16.313945	1.086042
-53.313866	-10.714976	1.091046
-53.102331	-8.896412	1.096051
-53.219305	-15.226628	1.101056
-53.231579	-13.270754	1.106061
-54.014689	-14.720691	1.111066
-54.468401	-2.645622	1.116070
-54.375872	-13.524951	1.121075
-54.768227	-8.790616	1.126080
-54.732175	-6.597853	1.131085
-55.667880	-13.531499	1.136090
-56.333926	-9.410344	1.141094
-55.858580	-19.536102	1.146099
-56.224741	-6.953981	1.151104
-56.457543	-11.906369	1.156109
-56.501543	-3.969959	1.161114
-56.578000	-7.831526	1.166118
-56.495041	-16.854326	1.171123
-57.335010	-7.830015	1.176128
-57.752797	-14.005236	1.181133
-58.180093	-14.092896	1.186138
-58.340761	-8.147016	1.191142
-58.208983	-14.482117	1.196147
-58.220943	-10.121186	1.201152
-58.181270	-6.053558	1.206157
-58.794750	-10.187113	1.211162
-59.467787	-9.698117	1.216166
-59.163569	-14.688922	1.221171
-59.942379	-8.371509	1.226176
-60.629125	-8.229524	1.231181
-60.878351	-2.530049	1.236186
-60.725421	-6.189054	1.241190
-60.719413	-10.327718	1.246195
-61.282461	-12.282767	1.251200
-61.297804	-10.637186	1.256205
-61.415070	-9.955476	1.261210
-61.451745	-8.794173	1.266214
-61.959368	-13.586594	1.271219
-62.496897	-2.191470	1.276224
-62.950932	-7.036379	1.281229
-62.965782	-9.177132	1.286234
-63.424222	-9.746458	1.291238
-63.171218	-10.926940	1.296243
-63.258283	-5.591368	1.301248
-63.565278	-16.538520	1.306253
-64.120001	-17.330872	1.311258
-64.658169	-8.637151	1.316262
-64.617854	-15.626660	1.321267
-64.866605	-10.157358	1.326272
-64.737003	-5.203002	1.331277
-65.262473	-13.665253	1.336282
-66.035755	-4.798208	1.341286
-66.266153	-12.252009	1.346291
-66.604729	-7.346216	1.351296
-66.616955	-8.822584	1.356301
-66.200076	-13.299442	1.361306
-66.632035	-5.328778	1.366310
-66.418159	-10.282719	1.371315
-67.308864	-5.286869	1.376320
-67.744945	-14.271664	1.381325
-68.000196	-11.270330	1.386330
-68.143409	-8.873041	1.391334
-67.933499	-16.781403	1.396339
-68.365509	-5.528077	1.401344
-69.094459	-19.162697	1.406349
-69.409042	-20.996288	1.411354
-70.027838	-6.453649	1.416358
-69.756185	-18.140530	1.421363
-70.165766	-10.458328	1.426368
-69.555748	-15.375061	1.431373
-69.710321	-7.447771	1.436378
-70.244189	-3.961225	1.441382
-70.764085	-21.803294	1.446387
-71.314126	-5.171222	1.451392
-71.351849	-12.341590	1.456397
-71.403531	-14.843481	1.461402
-71.758895	0.151241	1.466406
-72.269193	-18.144712	1.471411
-72.855418	-6.047700	1.476416
-72.711165	-16.579995	1.481421
-72.574715	-5.686424	1.486426
-72.719442	-2.750950	1.491430
-73.013461	-17.170372	1.496435
-73.931339	-8.716675	1.501440
-74.143523	-7.266021	1.506445
-74.055523	-15.137420	1.511450
-74.406187	-5.335934	1.516454
-74.456674	-17.968963	1.521459
-74.337601	-10.033713	1.526464
-74.945420	-13.055040	1.531469
-75.340235	-10.605033	1.536474
-75.739657	-6.132375	1.541478
-75.716064	-11.793030	1.546483
-76.228877	-11.696226	1.551488
-76.635173	-4.488562	1.556493
-76.975889	-14.072074	1.561498
-77.317083	-11.248710	1.566502
-77.299117	-12.382375	1.571507
-77.591396	-8.783103	1.576512
-77.271231	-13.501071	1.581517
-77.263741	-8.525311	1.586522
-77.883435	-3.938818	1.591526
-78.430332	-10.437792	1.596531
-79.161853	-2.989193	1.601536
-79.057190	-9.069585	1.606541
-78.693532	-12.643509	1.611546
-79.008541	-7.244139	1.616550
-79.207388	-6.630221	1.621555
-79.999564	-4.244250	1.626560
-80.512060	-2.850223	1.631565
-80.712401	-6.850126	1.636570
-80.967857	-5.109526	1.641574
-80.611323	-14.376742	1.646579
-80.990494	-2.325661	1.651584
-81.003661	-1.573179	1.656589
-81.853215	-8.409002	1.661594
-82.709181	-10.321654	1.666598
-82.431162	-3.842412	1.671603
-82.712581	-3.083590	1.676608
-82.694802	-3.134057	1.681613
-82.592835	-7.053785	1.686618
-82.757479	-1.770485	1.691622
-82.489274	-12.422766	1.696627
-83.347389	-1.635026	1.701632
-83.709222	-7.365248	1.706637
-83.786825	-18.910419	1.711642
-84.453453	-9.102390	1.716646
-84.897787	-13.995865	1.721651
-85.502958	-9.453021	1.726656
-85.649905	-11.457244	1.731661
-85.750708	-9.131705	1.736666
-85.917728	-13.045166	1.741670
-85.732625	-12.361240	1.746675
-85.799816	-18.561365	1.751680
-85.729477	-17.283006	1.756685
-86.738367	-14.198892	1.761690
-86.829110	-20.074645	1.766694
-87.115109	-16.205870	1.771699
-87.350074	-16.856012	1.776704
-87.466569	-15.394368	1.781709
-87.939026	-17.347444	1.786714
-88.891834	-8.331083	1.791718
-88.784980	-13.420232	1.796723
-88.851198	-9.730330	1.801728
-89.148932	-14.797662	1.806733
-88.720191	-10.609175	1.811738
-89.316622	-4.885745	1.816742
-88.677260	-17.884622	1.821747
-89.894886	-15.481273	1.826752
-90.346125	-12.611663	1.831757
-90.313788	-21.281923	1.836762
-90.669967	-13.154500	1.841766
-90.620743	-10.929584	1.846771
-91.353219	-14.116349	1.851776
-91.873469	-9.561323	1.856781
-92.219787	-12.050924	1.861786
-92.280815	-8.701888	1.866790
-92.154794	-19.794549	1.871795
-92.341097	-15.761921	1.876800
-92.608578	-2.655051	1.881805
-92.153946	-8.907660	1.886810
-93.087266	-9.382153	1.891814
-93.694236	-21.270036	1.896819
-94.056748	-9.616190	1.901824
-94.391559	-15.132631	1.906829
-94.086762	-12.774809	1.911834
-94.209856	-12.027408	1.916838
-93.966767	-13.933624	1.921843
-94.726626	-14.168865	1.926848
-95.236116	-22.061877	1.931853
-95.516980	-15.712082	1.936858
-95.427036	-2.065497	1.941862
-95.392003	-18.822171	1.946867
-96.173520	-16.312461	1.951872
-96.688842	-13.122619	1.956877
-96.749581	-14.850643	1.961882
-97.159889	-15.569623	1.966886
-97.161546	-18.655815	1.971891
-97.250548	-16.280332	1.976896
-97.735274	-10.483249	1.981901
-98.085968	-7.764476	1.986906
-98.718208	-7.255788	1.991910
-98.284775	-18.052251	1.996915
-98.635553	-12.796602	2.006912
-98.510623	-18.644253	2.016909
-97.887174	-11.805423	2.026906
-97.366697	-15.397927	2.036902
-96.880808	-17.366268	2.046899
-95.912536	-14.070569	2.056896
-95.961948	-13.853664	2.066893
-95.619389	-11.564378	2.076890
-95.035723	-11.719655	2.086886
-94.642299	-9.435632	2.096883
-93.558186	-11.175253	2.106880
-92.935649	-11.417188	2.116877
-92.769890	-16.640707	2.126874
-92.691263	-18.011869	2.136870
-92.203911	-12.726450	2.146867
-91.710424	-13.047979	2.156864
-90.462338	-15.836872	2.166861
-89.995221	-19.292303	2.176858
-90.049296	-15.218720	2.186854
-89.496724	-12.770580	2.196851
-88.495983	-14.067629	2.206848
-88.460278	-9.040935	2.216845
-88.250497	-17.352123	2.226842
-87.257506	-10.900707	2.236838
-86.884687	-14.379249	2.246835
-86.437353	-16.205463	2.256832
-85.488955	-16.994145	2.266829
-85.453406	-17.497288	2.276826
-85.230649	-16.304724	2.286822
-84.050738	-17.624528	2.296819
-83.694529	-13.872002	2.306816
-83.573746	-8.293311	2.316813
-83.027036	-14.717824	2.326810
-82.455750	-17.038971	2.336806
-81.741850	-12.411887	2.346803
-81.054210	-13.336990	2.356800
-80.625822	-16.715469	2.366797
-80.602194	-15.819106	2.376794
-80.074819	-16.004971	2.386790
-79.494319	-19.132414	2.396787
-78.881627	-13.513873	2.406784
-77.991475	-10.906071	2.416781
-77.689903	-11.671011	2.426778
-77.634744	-13.845825	2.436774
-76.594075	-7.278413	2.446771
-76.123601	-13.842838	2.456768
-76.138246	-13.597310	2.466765
-75.330331	-11.341226	2.476762
-74.797713	-12.716642	2.486758
-74.544460	-15.730218	2.496755
-73.595112	-12.890966	2.506752
-73.188143	-16.955080	2.516749
-73.162106	-15.702274	2.526746
-72.423447	-10.556473	2.536742
-71.761845	-10.748167	2.546739
-71.369342	-9.391263	2.556736
-70.400055	-12.221115	2.566733
-70.371598	-12.069664	2.576730
-70.070844	-12.537099	2.586726
-69.274133	-9.444749	2.596723
-68.744021	-13.724671	2.606720
-68.626999	-12.366207	2.616717
-67.363045	-20.997202	2.626714
-66.805109	-14.548222	2.636710
-66.938120	-11.701422	2.646707
-66.855810	-14.789829	2.656704
-65.901713	-13.152492	2.666701
-65.382041	-14.737970	2.676698
-64.415555	-18.719287	2.686694
-63.852854	-12.907325	2.696691
-63.968091	-16.482670	2.706688
-63.687748	-12.285256	2.716685
-62.502749	-13.399420	2.726682
-62.324223	-13.246344	2.736678
-61.995528	-16.448464	2.746675
-61.307836	-17.010210	2.756672
-60.618785	-16.102728	2.766669
-60.352773	-16.624476	2.776666
-59.734067	-19.211719	2.786662
-59.042703	-18.113553	2.796659
-58.965081	-18.741623	2.806656
-58.463509	-19.951453	2.816653
-57.566874	-10.178839	2.826650
-57.329761	-8.569766	2.836646
-56.789479	-10.896841	2.846643
-55.973931	-7.247646	2.856640
-55.545661	-12.115910	2.866637
-55.584995	-14.368336	2.876634
-54.723156	-13.064458	2.886630
-54.130274	-15.914563	2.896627
-54.154365	-16.585459	2.906624
-53.205252	-9.852515	2.916621
-52.492834	-15.456030	2.926618
-52.271935	-17.793440	2.936614
-52.007007	-18.255535	2.946611
-50.796226	-14.882816	2.956608
-50.868790	-9.412390	2.966605
-50.685262	-16.179042	2.976602
-49.546885	-17.988100	2.986598
-49.257008	-13.297704	2.996595
-49.019786	-16.323642	3.006592
-48.058649	-14.305531	3.016589
-47.771483	-14.316660	3.026586
-47.685342	-24.319658	3.036582
-46.575398	-19.876510	3.046579
-46.583846	-18.929390	3.056576
-45.664508	-14.294629	3.066573
-44.947426	-20.666538	3.076570
-45.077521	-12.487353	3.086566
-44.141749	-11.907622	3.096563
-43.724752	-14.233445	3.106560
-43.485960	-15.458835	3.116557
-42.315346	-12.674593	3.126554
-41.969966	-8.407528	3.136550
-42.010071	-18.310392	3.146547
-41.343310	-8.351711	3.156544
-40.357050	-9.076115	3.166541
-40.110468	-13.605264	3.176538
-40.051255	-13.251044	3.186534
-39.028577	-12.250419	3.196531
-38.721401	-12.589497	3.206528
-38.539857	-1.746674	3.216525
-37.693874	-9.464162	3.226522
-36.713769	-15.095210	3.236518
-36.550785	-10.743603	3.246515
-36.640584	-11.222432	3.256512
-35.614333	-13.362252	3.266509
-35.206553	-14.192791	3.276506
-35.073761	-16.179910	3.286502
-33.914289	-22.228522	3.296499
-33.760391	-16.288395	3.306496
-33.341011	-15.616033	3.316493
-32.397259	-12.606709	3.326490
-31.924031	-13.062989	3.336486
-31.983116	-14.726695	3.346483
-31.555518	-10.313199	3.356480
-30.695739	-11.155362	3.366477
-30.191891	-11.041340	3.376474
-29.300866	-18.827731	3.386470
-29.033914	-15.730829	3.396467
-28.886718	-13.251905	3.406464
-28.716520	-14.370501	3.416461
-27.567743	-10.080582	3.426458
-27.326625	-17.040923	3.436454
-26.256392	-18.421584	3.446451
-25.833698	-17.453192	3.456448
-25.628874	-14.295814	3.466445
-25.748032	-6.520525	3.476442
-24.718829	-14.957731	3.486438
-23.993413	-12.189463	3.496435
-23.880310	-12.699718	3.506432
-23.296359	-18.206477	3.516429
-22.925716	-11.768162	3.526426
-21.836605	-9.655845	3.536422
-21.292051	-11.715894	3.546419
-21.378364	-17.488259	3.556416
-21.225562	-13.073318	3.566413
-20.270397	-12.189743	3.576410
-19.641636	-11.682065	3.586406
-18.943811	-13.237369	3.596403
-18.222419	-12.187637	3.606400
-18.114288	-7.083820	3.616397
-17.868697	-7.338011	3.626394
-17.468403	-7.660498	3.636390
-16.594368	-8.198561	3.646387
-16.423349	-6.214980	3.656384
-15.356784	-10.270953	3.666381
-14.905986	-12.574907	3.676378
-14.931750	-11.840091	3.686374
-14.274218	-13.223737	3.696371
-13.269820	-5.772221	3.706368
-13.107972	-12.649294	3.716365
-13.087635	-11.721166	3.726362
-12.180558	-15.003848	3.736358
-11.452347	-14.786097	3.746355
-11.281434	-9.429491	3.756352
-10.110559	-12.959569	3.766349
-10.325191	-12.654250	3.776346
-9.837451	-10.964173	3.786342
-9.429365	-16.493971	3.796339
-8.539588	-16.136014	3.806336
-8.401436	-15.154091	3.816333
-7.363417	-19.321317	3.826330
-6.735579	-12.856435	3.836326
-6.789449	-4.321168	3.846323
-6.388012	-7.458867	3.856320
-5.389727	-7.666193	3.866317
-4.884177	-7.935768	3.876314
-5.016085	-8.272475	3.886310
-4.195513	-3.368235	3.896307
-3.754728	-0.075062	3.906304
-3.521340	5.848555	3.916301
-3.052613	11.850767	3.926298
-2.437112	24.047939	3.936294
-1.931875	33.243648	3.946291
-1.480805	57.188184	3.956288
-1.230512	70.042387	3.966285
-0.853744	84.425144	3.976282
-0.449499	109.913369	3.986278
0.000000	128.992016	3.991283
0.579538	122.764457	3.996288
0.727790	141.644156	4.001293
0.751916	153.280082	4.006298
0.769667	161.929200	4.011302
1.093414	162.248196	4.016307
1.442266	156.710034	4.021312
1.135379	162.228886	4.026317
1.263132	155.015048	4.031322
1.069177	155.120610	4.036326
1.165406	167.013576	4.041331
1.174962	161.502786	4.046336
1.083630	170.854927	4.051341
1.101037	156.331068	4.056346
0.944706	166.668615	4.061350
1.295652	157.797091	4.066355
1.372277	156.647977	4.071360
0.809770	167.812332	4.076365
1.504879	160.181699	4.081370
1.410829	166.125891	4.086374
1.465450	157.653708	4.091379
1.387251	167.437418	4.096384
1.550742	169.631996	4.101389
1.444223	161.969922	4.106394
1.522060	171.792522	4.111398
1.367105	173.642003	4.116403
1.358729	162.162775	4.121408
1.212466	168.452862	4.126413
1.419840	172.036923	4.131418
1.289552	165.809474	4.136422
1.137971	170.872022	4.141427
1.348706	156.395676	4.146432
1.428229	171.828077	4.151437
1.728213	158.685549	4.156442
1.477747	178.935516	4.161446
1.203982	171.890971	4.166451
1.388232	168.887816	4.171456
1.141467	168.002219	4.176461
1.441560	162.858711	4.181466
1.282962	169.107032	4.186470
1.342832	169.491038	4.191475
1.487169	170.928647	4.196480
1.410625	169.239724	4.201485
1.518034	168.675942	4.206490
1.439075	169.045837	4.211494
1.197854	178.490293	4.216499
1.392662	167.174752	4.221504
1.609816	183.476533	4.226509
2.031814	191.504210	4.231514
1.859707	186.041056	4.236518
1.204078	176.443649	4.241523
1.553445	173.326718	4.246528
1.460733	192.772284	4.251533
1.750803	189.848692	4.256538
1.780729	187.734635	4.261542
1.872191	197.085531	4.266547
2.017266	186.519804	4.271552
1.679833	184.048028	4.276557
1.768496	179.548508	4.281562
1.837430	178.207078	4.286566
1.563315	180.496224	4.291571
1.777843	175.643351	4.296576
1.731223	185.287259	4.301581
2.071181	191.946769	4.306586
1.699472	189.856989	4.311590
1.757775	194.536688	4.316595
2.121098	193.650704	4.321600
1.991632	196.742150	4.326605
1.960008	174.860199	4.331610
1.641778	177.552507	4.336614
1.647885	183.192206	4.341619
2.059083	193.014872	4.346624
1.838236	184.076991	4.351629
2.008162	194.291067	4.356634
2.050738	191.101008	4.361638
2.064925	195.225404	4.366643
2.009688	193.911245	4.371648
1.770148	199.207609	4.376653
1.957059	186.569230	4.381658
1.970719	199.335296	4.386662
2.083919	197.682044	4.391667
2.031098	188.865720	4.396672
1.847144	207.757295	4.401677
1.996046	190.431938	4.406682
1.885262	200.598570	4.411686
2.113260	195.189140	4.416691
2.147301	183.638343	4.421696
1.897211	199.314797	4.426701
2.193369	189.409598	4.431706
2.328090	190.208838	4.436710
2.352171	190.388607	4.441715
2.175191	190.546810	4.446720
2.059247	195.404155	4.451725
2.082859	191.970366	4.456730
2.252052	194.972888	4.461734
2.543952	196.002047	4.466739
2.213800	191.141089	4.471744
2.157349	191.506863	4.476749
1.949004	189.240253	4.481754
1.858734	196.501647	4.486758
2.004225	188.187860	4.491763
2.031871	193.209883	4.496768
2.112967	187.208498	4.501773
1.901408	189.012297	4.506778
2.204255	206.753496	4.511782
2.059698	218.622043	4.516787
2.567335	218.565644	4.521792
2.347921	217.380495	4.526797
2.421718	220.998724	4.531802
2.562667	218.605991	4.536806
2.408743	227.857035	4.541811
2.622409	220.788981	4.546816
2.145789	232.450856	4.551821
2.828873	221.274649	4.556826
2.550856	228.353825	4.561830
2.407966	223.289573	4.566835
2.865242	216.290505	4.571840
2.491383	209.132473	4.576845
2.361803	192.865962	4.581850
2.415548	202.529966	4.586854
2.747237	218.676853	4.591859
2.663585	203.422763	4.596864
2.075162	200.055788	4.601869
2.667769	207.497152	4.606874
2.550259	217.768709	4.611878
2.531155	222.863605	4.616883
3.013367	220.829755	4.621888
2.684614	221.052164	4.626893
2.907696	210.283862	4.631898
2.252067	201.479931	4.636902
2.234103	205.328646	4.641907
2.777720	214.795307	4.646912
2.558553	232.607191	4.651917
2.658403	220.442997	4.656922
2.854443	221.831596	4.661926
2.743344	218.545813	4.666931
2.779796	220.952852	4.671936
2.560006	225.140077	4.676941
2.693464	227.693660	4.681946
2.848217	224.398978	4.686950
2.671383	230.739541	4.691955
3.121810	217.149748	4.696960
2.553464	225.945290	4.701965
2.955788	223.122295	4.706970
2.755939	223.509447	4.711974
2.959878	223.816316	4.716979
2.996827	218.585925	4.721984
2.741993	233.284405	4.726989
2.811752	220.766435	4.731994
2.651452	231.353919	4.736998
2.792109	232.766687	4.742003
3.121287	227.104278	4.747008
3.030221	233.168970	4.752013
3.042415	224.942949	4.757018
2.671252	237.872426	4.762022
2.977251	233.230339	4.767027
3.103379	227.039931	4.772032
2.799211	232.916327	4.777037
2.866756	228.876731	4.782042
2.792251	225.219616	4.787046
2.721057	229.831375	4.792051
3.031341	231.825235	4.797056
2.798784	233.582392	4.802061
2.975691	226.177646	4.807066
2.894007	224.111470	4.812070
2.878135	226.069549	4.817075
3.704700	233.002127	4.822080
3.192967	234.784399	4.827085
2.926345	227.959663	4.832090
2.964758	236.520940	4.837094
2.752209	231.017107	4.842099
3.418230	236.091699	4.847104
3.199166	257.268396	4.852109
3.260416	251.079052	4.857114
3.358311	261.570323	4.862118
3.000694	252.854559	4.867123
3.233815	255.053603	4.872128
3.052757	260.429501	4.877133
3.758509	256.058264	4.882138
3.438072	248.641932	4.887142
3.074359	243.078862	4.892147
3.397263	236.037705	4.897152
3.118673	237.900562	4.902157
3.432465	242.423314	4.907162
3.452552	242.890476	4.912166
3.422219	233.461025	4.917171
3.100288	224.467041	4.922176
3.123738	248.655193	4.927181
3.542495	243.348150	4.932186
3.503760	256.414407	4.937190
3.561355	256.084429	4.942195
3.380605	251.067286	4.947200
3.640943	250.771619	4.952205
3.585204	243.174307	4.957210
3.292268	239.236040	4.962214
2.979153	238.177112	4.967219
3.510936	242.525236	4.972224
3.493018	251.267139	4.977229
3.480374	256.339269	4.982234
3.511873	254.243887	4.987238
3.762436	261.555631	4.992243
3.763862	246.910405	4.997248
3.670051	264.658548	5.002253
3.577243	253.351696	5.007258
3.679342	255.872785	5.012262
3.437132	237.353719	5.017267
3.649625	253.037495	5.022272
3.609794	258.317977	5.027277
3.626657	247.340086	5.032282
3.835478	253.218963	5.037286
3.595481	259.523030	5.042291
3.797743	257.088563	5.047296
3.473893	257.404883	5.052301
3.773869	252.284059	5.057306
3.587541	252.997343	5.062310
3.556267	261.162868	5.067315
3.728039	256.095636	5.072320
3.911560	265.567295	5.077325
3.446899	256.382224	5.082330
3.677550	257.360553	5.087334
3.544248	259.059441	5.092339
3.534127	255.665758	5.097344
3.449026	261.979303	5.102349
3.496910	259.071333	5.107354
3.419381	256.793115	5.112358
3.549175	266.340174	5.117363
3.663432	272.052969	5.122368
3.602064	291.234956	5.127373
4.064911	289.247718	5.132378
4.083712	287.661989	5.137382
4.092954	294.955495	5.142387
3.963570	289.756373	5.147392
3.612529	288.685172	5.152397
3.608037	288.130247	5.157402
3.899120	285.758029	5.162406
3.862489	291.633560	5.167411
3.916414	286.778040	5.172416
3.929850	294.600310	5.177421
4.320594	283.872670	5.182426
4.032478	283.195789	5.187430
3.868515	288.765810	5.192435
4.124532	291.335419	5.197440
3.933510	293.236668	5.202445
4.016973	283.969696	5.207450
3.937928	290.871106	5.212454
4.253176	291.269659	5.217459
4.053808	287.245041	5.222464
3.681305	290.195791	5.227469
4.204878	291.456946	5.232474
4.283441	290.255602	5.237478
4.288079	292.196874	5.242483
4.479616	290.004339	5.247488
3.869386	293.733093	5.252493
4.042909	288.895064	5.257498
4.210233	290.888530	5.262502
3.987066	288.663038	5.267507
4.080953	292.740715	5.272512
4.027655	292.650513	5.277517
4.084289	293.296530	5.282522
3.738185	304.436199	5.287526
3.980180	309.680095	5.292531
4.397772	309.983950	5.297536
4.418607	321.484976	5.302541
4.432656	315.892479	5.307546
4.443823	322.350345	5.312550
4.541576	315.927202	5.317555
4.469783	321.926970	5.322560
4.395812	316.818319	5.327565
4.772370	314.137712	5.332570
4.202543	303.395858	5.337574
4.512799	315.200611	5.342579
4.416113	308.486625	5.347584
4.596142	309.322376	5.352589
4.407536	302.117639	5.357594
4.492596	297.956327	5.362598
4.445413	307.172377	5.367603
4.297067	305.568541	5.372608
4.366190	315.628890	5.377613
4.626440	321.391530	5.382618
4.377465	328.970341	5.387622
4.345181	328.740494	5.392627
4.498348	320.485751	5.397632
4.417579	330.959688	5.402637
4.389576	328.565117	5.407642
4.657910	326.883596	5.412646
4.506912	322.093573	5.417651
4.609093	321.128082	5.422656
4.642711	327.669259	5.427661
4.728018	327.618069	5.432666
4.908521	320.370357	5.437670
4.431488	331.366948	5.442675
4.507112	311.886220	5.447680
4.354789	326.873688	5.452685
4.639493	316.557473	5.457690
4.648207	320.968950	5.462694
4.448873	327.137252	5.467699
4.472900	321.794904	5.472704
4.344832	329.010719	5.477709
4.632897	329.931591	5.482714
5.100516	342.492162	5.487718
4.544295	336.588361	5.492723
5.010593	335.780830	5.497728
4.561727	344.123888	5.502733
4.827219	352.512253	5.507738
4.764767	357.005777	5.512742
4.850777	360.050325	5.517747
5.137258	356.169216	5.522752
4.909347	357.447662	5.527757
5.012058	346.073437	5.532762
4.963150	339.812510	5.537766
4.407155	335.168680	5.542771
5.059748	345.230902	5.547776
5.094219	354.962723	5.552781
5.005074	355.073427	5.557786
4.966710	359.571449	5.562790
4.555471	363.895200	5.567795
4.818470	358.129640	5.572800
4.874017	358.022203	5.577805
4.910708	356.864886	5.582810
4.960467	350.798177	5.587814
4.952317	360.749199	5.592819
5.088090	359.798665	5.597824
4.808888	361.462918	5.602829
5.233588	350.360585	5.607834
5.130734	354.912502	5.612838
4.666101	355.765217	5.617843
5.336829	354.041530	5.622848
4.741117	360.102416	5.627853
4.934669	355.657702	5.632858
5.092503	353.301619	5.637862
4.777981	353.888921	5.642867
5.175457	363.380860	5.647872
5.139402	369.985098	5.652877
5.409513	380.021482	5.657882
5.323064	368.683299	5.662886
5.072399	365.532290	5.667891
5.117523	356.241627	5.672896
4.924796	372.410787	5.677901
5.490602	373.406837	5.682906
5.620939	381.333327	5.687910
5.065383	379.062022	5.692915
5.486256	391.049210	5.697920
5.382974	388.885155	5.702925
5.101407	374.921313	5.707930
5.519527	380.352549	5.712934
5.295497	379.752079	5.717939
5.504668	378.059432	5.722944
5.130469	381.173285	5.727949
5.167440	380.713318	5.732954
5.152810	382.871906	5.737958
5.616510	389.044500	5.742963
5.967902	379.510505	5.747968
5.688484	384.383533	5.752973
5.666843	364.343601	5.757978
5.567690	371.773299	5.762982
5.463979	357.612480	5.767987
5.323180	350.175627	5.772992
5.084906	355.306464	5.777997
5.496615	363.728640	5.783002
5.644353	381.312003	5.788006
5.638141	384.324071	5.793011
5.557991	379.930790	5.798016
5.300939	380.692891	5.803021
5.870147	384.061976	5.808026
5.426838	383.181284	5.813030
5.256519	387.331745	5.818035
5.575474	387.399933	5.823040
5.251671	388.120003	5.828045
5.097944	375.776264	5.833050
5.402974	383.014319	5.838054
5.314282	378.275926	5.843059
5.722718	375.007089	5.848064
5.674753	385.888465	5.853069
5.807256	389.412748	5.858074
5.305550	390.080777	5.863078
5.397997	392.977839	5.868083
5.547095	405.940103	5.873088
5.417163	418.218623	5.878093
5.525291	418.811520	5.883098
5.901902	419.095326	5.888102
5.792295	419.951021	5.893107
6.146555	416.639444	5.898112
5.689525	422.937680	5.903117
6.027420	415.123545	5.908122
6.066898	419.191123	5.913126
5.961303	427.255375	5.918131
6.152140	418.600846	5.923136
5.968417	416.323810	5.928141
5.837660	409.199826	5.933146
5.836833	407.574708	5.938150
6.123919	409.823844	5.943155
5.970942	388.178168	5.948160
5.578198	397.614300	5.953165
5.901941	401.476140	5.958170
5.972402	407.749776	5.963174
5.951856	418.230770	5.968179
5.974824	406.968178	5.973184
5.735959	413.154505	5.978189
6.144711	420.774621	5.983194
6.067750	419.394576	5.988198
6.025376	417.322061	5.993203
6.156542	408.943432	5.998208
5.778260	414.399008	6.003213
5.881355	410.930303	6.008218
6.028609	416.440347	6.013222
5.602173	414.487870	6.018227
5.939844	412.615674	6.023232
5.808466	417.800663	6.028237
6.031733	408.678994	6.033242
5.893966	411.856121	6.038246
5.503448	410.397360	6.043251
5.890122	406.641140	6.048256
5.625125	416.079020	6.053261
5.894458	424.414098	6.058266
6.019952	432.315170	6.063270
5.870692	434.334042	6.068275
6.392672	436.898313	6.073280
6.003525	442.485153	6.078285
6.262626	446.632802	6.083290
6.248121	441.556098	6.088294
6.068891	431.349982	6.093299
6.267847	413.596345	6.098304
5.660107	411.942273	6.103309
6.091034	417.502633	6.108314
5.787142	414.789838	6.113318
6.307056	430.089186	6.118323
6.072954	417.050470	6.123328
6.003920	422.712368	6.128333
6.084186	420.531728	6.133338
6.101396	412.391608	6.138342
5.868174	419.311501	6.143347
5.973205	404.104510	6.148352
6.067066	417.509288	6.153357
6.454523	419.292264	6.158362
6.718653	419.662186	6.163366
6.121723	416.676055	6.168371
6.494749	410.867589	6.173376
6.013142	414.538958	6.178381
6.238932	417.604575	6.183386
6.476447	415.874078	6.188390
6.179439	417.137527	6.193395
6.577621	413.559966	6.198400
6.239337	397.954748	6.203405
6.005877	387.464986	6.208410
5.914870	379.989877	6.213414
6.005972	382.204367	6.218419
5.981567	381.402510	6.223424
5.818620	383.668343	6.228429
5.709228	385.638377	6.233434
6.067173	398.036392	6.238438
6.191076	409.308473	6.243443
6.386863	405.482824	6.248448
5.897981	395.042457	6.253453
5.926101	388.141610	6.258458
5.893361	388.281258	6.263462
5.890800	409.936184	6.268467
6.234219	409.281215	6.273472
5.968745	408.393965	6.278477
6.403712	407.836123	6.283482
5.939759	397.406624	6.288486
6.031328	386.266285	6.293491
6.017036	376.386327	6.298496
6.046419	392.706990	6.303501
6.190665	383.881603	6.308506
5.897236	381.164912	6.313510
5.716481	391.040142	6.318515
6.120020	390.389624	6.323520
5.997340	408.011481	6.328525
6.047433	412.485201	6.333530
6.219597	406.668359	6.338534
5.747580	414.541673	6.343539
6.147966	402.978989	6.348544
5.898286	417.546151	6.353549
5.739021	410.871296	6.358554
5.993954	417.488939	6.363558
5.988291	412.304612	6.368563
6.470149	419.466831	6.373568
6.128891	414.130869	6.378573
6.230218	401.014322	6.383578
6.220610	398.124924	6.388582
6.017017	399.216807	6.393587
5.928201	381.538488	6.398592
5.959948	385.792442	6.403597
5.987290	393.197454	6.408602
5.965359	389.127245	6.413606
6.156392	405.472265	6.418611
6.255772	399.788052	6.423616
6.258951	395.135084	6.428621
5.736121	380.737770	6.433626
5.894275	378.057600	6.438630
5.806055	398.698557	6.443635
6.129972	403.738092	6.448640
5.955873	410.412963	6.453645
5.758922	413.769208	6.458650
6.104472	413.408514	6.463654
5.851577	412.034712	6.468659
6.210882	406.681611	6.473664
5.865014	409.452932	6.478669
6.163638	416.153722	6.483674
6.369610	410.823840	6.488678
6.008262	417.356653	6.493683
6.210933	408.383440	6.498688
5.705149	414.747369	6.503693
6.247447	407.179218	6.508698
6.126710	418.014254	6.513702
6.267776	411.766438	6.518707
6.626358	400.305993	6.523712
5.694411	392.612158	6.528717
5.709194	376.622295	6.533722
6.232544	387.676659	6.538726
5.600984	389.932473	6.543731
6.108156	398.442265	6.548736
5.924094	413.488947	6.553741
5.954007	419.240629	6.558746
6.142776	413.720201	6.563750
6.365575	414.754109	6.568755
6.212751	394.316513	6.573760
6.028228	397.413366	6.578765
5.823238	378.849683	6.583770
6.035000	392.443306	6.588774
6.093607	402.428490	6.593779
6.131270	390.673087	6.598784
5.636754	386.049846	6.603789
5.860790	402.818808	6.608794
6.442841	398.418287	6.613798
5.910304	412.176421	6.618803
6.570246	405.188111	6.623808
6.264658	396.558570	6.628813
6.168446	380.959659	6.633818
6.141884	380.384309	6.638822
5.929635	380.822656	6.643827
5.934127	374.982085	6.648832
5.717115	381.196750	6.653837
5.695158	383.730312	6.658842
5.960615	391.693042	6.663846
5.873993	405.911727	6.668851
6.204945	406.536005	6.673856
6.353726	416.776819	6.678861
5.957158	404.629562	6.683866
6.017670	389.634796	6.688870
5.544371	391.287580	6.693875
5.959624	401.545236	6.698880
6.154292	400.375176	6.703885
6.130399	414.485995	6.708890
6.354177	417.239162	6.713894
6.023127	420.772723	6.718899
6.413991	385.214529	6.723904
5.995387	393.807763	6.728909
5.817529	380.403369	6.733914
6.160195	378.968641	6.738918
5.838351	385.364655	6.743923
6.003270	379.637431	6.748928
5.915328	386.410508	6.753933
5.886194	403.019515	6.758938
6.385490	407.774258	6.763942
5.967504	398.301348	6.768947
6.072441	388.520438	6.773952
5.939152	386.193219	6.778957
6.184702	389.417574	6.783962
5.959904	380.373867	6.788966
5.771255	391.963903	6.793971
5.993904	387.940615	6.798976
6.260032	411.697906	6.803981
6.091162	411.891276	6.808986
6.297258	398.528074	6.813990
5.593129	392.426539	6.818995
5.789073	401.489704	6.824000
6.009793	407.434752	6.829005
6.059573	415.104244	6.834010
6.395482	409.019532	6.839014
6.288319	414.496124	6.844019
6.031574	395.581044	6.849024
5.886420	397.943589	6.854029
6.010559	395.089667	6.859034
6.130608	381.942409	6.864038
5.531231	394.352914	6.869043
6.116969	394.929278	6.874048
6.125905	416.135533	6.879053
6.115946	413.937668	6.884058
6.222680	412.640478	6.889062
6.097796	419.832521	6.894067
5.962557	408.772547	6.899072
6.102471	402.349097	6.904077
6.182506	405.163361	6.909082
6.033573	388.275665	6.914086
5.631263	390.754597	6.919091
6.043625	405.552925	6.924096
6.155302	409.092699	6.929101
6.137052	413.054194	6.934106
6.158743	400.525094	6.939110
6.050092	395.768885	6.944115
6.173301	392.882359	6.949120
5.867009	393.164987	6.954125
6.171287	384.094448	6.959130
5.965190	385.938214	6.964134
5.833387	391.286266	6.969139
6.194377	396.349458	6.974144
5.962027	407.072330	6.979149
6.194278	399.388378	6.984154
6.132429	388.399148	6.989158
5.653026	386.170881	6.994163
5.951574	392.826679	6.999168
6.190870	408.087617	7.004173
6.285534	411.309532	7.009178
5.785809	392.804703	7.014182
5.929701	403.567096	7.019187
5.991057	407.466073	7.024192
6.020569	415.266995	7.029197
6.583424	416.897194	7.034202
6.325298	395.589794	7.039206
5.846196	397.228937	7.044211
5.917130	393.339110	7.049216
5.797585	386.678211	7.054221
5.782669	387.509147	7.059226
6.213580	396.935777	7.064230
6.252543	407.387176	7.069235
6.141335	392.416698	7.074240
6.013573	386.518298	7.079245
5.954620	387.952097	7.084250
5.603725	384.572585	7.089254
6.118366	407.540605	7.094259
6.332954	413.010884	7.099264
6.124991	404.715253	7.104269
5.928610	386.715316	7.109274
5.669662	386.506821	7.114278
5.942182	413.227094	7.119283
6.250203	413.373858	7.124288
5.873431	412.538980	7.129293
6.076664	421.445052	7.134298
6.263115	420.556969	7.139302
6.149710	420.442381	7.144307
6.142738	407.955713	7.149312
5.812734	402.700971	7.154317
5.626258	403.794165	7.159322
6.146889	414.965824	7.164326
6.085391	429.860797	7.169331
6.207947	418.038626	7.174336
5.972286	423.371524	7.179341
6.229907	423.836063	7.184346
5.982480	415.138270	7.189350
5.940687	416.347025	7.194355
6.183251	420.093648	7.199360
5.859546	424.025804	7.204365
6.207999	420.226180	7.209370
6.408778	409.476431	7.214374
6.137281	406.188159	7.219379
6.250655	388.426622	7.224384
5.963675	386.344097	7.229389
6.103362	389.069939	7.234394
6.005077	391.182390	7.239398
5.828162	395.239025	7.244403
5.791269	387.422830	7.249408
5.559422	395.783261	7.254413
5.865868	413.205793	7.259418
6.175577	417.198430	7.264422
5.882470	430.964492	7.269427
5.875560	420.944948	7.274432
5.985389	426.964608	7.279437
6.001416	419.174761	7.284442
5.931771	419.517465	7.289446
6.276636	425.798556	7.294451
6.376407	413.117193	7.299456
6.000423	425.656892	7.304461
5.762928	428.005921	7.309466
5.989202	417.529997	7.314470
5.920900	421.762442	7.319475
6.378835	421.624288	7.324480
6.321774	426.114177	7.329485
6.401739	418.468259	7.334490
6.227785	401.068056	7.339494
5.981482	394.347827	7.344499
5.911413	384.126033	7.349504
5.733636	399.256911	7.354509
6.055414	405.775861	7.359514
5.930687	405.205123	7.364518
6.354843	418.784122	7.369523
6.347287	402.859698	7.374528
6.055026	394.210586	7.379533
5.863512	387.248031	7.384538
5.723744	388.654363	7.389542
5.747656	399.656064	7.394547
5.978208	407.193001	7.399552
6.187037	419.787411	7.404557
6.418502	419.059612	7.409562
6.329140	402.366875	7.414566
5.908219	397.022205	7.419571
5.770550	390.605652	7.424576
5.679704	398.415642	7.429581
5.895470	402.901195	7.434586
6.018125	416.063410	7.439590
5.955301	423.681694	7.444595
6.176537	415.877798	7.449600
6.263722	416.822863	7.454605
6.166073	424.055194	7.459610
6.325331	413.938280	7.464614
5.856649	395.466393	7.469619
6.013585	398.312126	7.474624
6.217161	402.055926	7.479629
5.574427	401.712064	7.484634
5.891142	407.257193	7.489638
5.858560	419.644509	7.494643
5.714929	415.217330	7.499648
6.129951	416.700521	7.504653
5.996096	409.467525	7.509658
6.446385	413.710198	7.514662
6.091628	419.062026	7.519667
6.064189	419.975947	7.524672
5.781438	422.212487	7.529677
5.926155	428.684594	7.534682
6.449572	416.263424	7.539686
6.059134	420.925736	7.544691
6.258321	417.870923	7.549696
6.225084	416.361879	7.554701
6.084938	408.575598	7.559706
5.742172	401.203542	7.564710
5.910496	407.448342	7.569715
6.134107	414.936505	7.574720
5.956982	427.636274	7.579725
6.011446	425.166856	7.584730
6.101163	414.912071	7.589734
5.741639	418.843447	7.594739
6.177335	413.816527	7.599744
6.408159	422.704218	7.604749
6.176133	414.523273	7.609754
5.864934	399.987492	7.614758
5.796673	405.437905	7.619763
6.382672	413.625620	7.624768
6.052550	415.112613	7.629773
6.130753	404.692396	7.634778
6.117754	393.493195	7.639782
5.673720	395.630536	7.644787
6.179746	412.761109	7.649792
6.074855	415.595341	7.654797
6.163684	411.328193	7.659802
6.082302	396.475517	7.664806
5.828596	392.647934	7.669811
6.117302	398.044562	7.674816
5.843247	404.716248	7.679821
5.883271	410.197672	7.684826
6.031857	419.772894	7.689830
5.931794	425.378164	7.694835
6.272344	414.022918	7.699840
6.101621	425.188294	7.704845
5.893758	430.348458	7.709850
6.073667	419.039937	7.714854
5.680585	425.627936	7.719859
5.759514	424.513152	7.724864
5.652368	424.842135	7.729869
5.589334	421.251945	7.734874
6.060950	420.395182	7.739878
5.971793	413.319759	7.744883
6.118393	417.739413	7.749888
6.113442	423.803338	7.754893
5.733189	414.474543	7.759898
5.891300	412.178595	7.764902
5.774551	423.855615	7.769907
5.596521	415.354327	7.774912
6.069588	426.548276	7.779917
6.095923	437.240173	7.784922
6.508352	439.931517	7.789926
6.561744	428.840293	7.794931
6.129188	421.431392	7.799936
5.892094	427.814377	7.804941
6.103672	415.431821	7.809946
5.761744	420.879406	7.814950
5.864701	424.984034	7.819955
6.150357	422.033897	7.824960
6.075484	421.013059	7.829965
5.935374	419.735037	7.834970
5.990935	416.885362	7.839974
6.100471	422.548081	7.844979
6.047534	418.709348	7.849984
6.067109	420.432668	7.854989
5.853779	420.909083	7.859994
6.069261	423.422476	7.864998
6.049195	423.570879	7.870003
6.062314	408.820355	7.875008
6.160474	409.947522	7.880013
6.110195	415.048433	7.885018
6.191611	413.687550	7.890022
5.815384	419.551676	7.895027
6.193346	416.670322	7.900032
6.048253	420.700974	7.905037
5.865480	422.586862	7.910042
5.767929	414.621839	7.915046
5.825432	419.074205	7.920051
6.306026	414.063137	7.925056
6.020583	419.736992	7.930061
6.089606	424.667580	7.935066
6.410280	417.170263	7.940070
6.182295	438.889593	7.945075
6.373166	410.012651	7.950080
6.239841	418.306063	7.955085
6.178374	423.228461	7.960090
6.573567	417.774493	7.965094
6.252018	422.761666	7.970099
6.398050	422.598592	7.975104
5.716867	415.990031	7.980109
5.837487	414.145489	7.985114
6.116459	409.636293	7.990118
6.084319	421.631126	7.995136
5.942533	422.960059	8.000154
6.155795	423.529658	8.005171
5.947404	420.062088	8.010189
6.160038	414.715086	8.015206
6.390118	418.866881	8.020224
6.154166	400.947038	8.025242
6.079066	406.312077	8.030259
6.302008	400.198271	8.035277
6.142803	388.477491	8.040294
5.699469	392.705361	8.045312
5.581005	396.384983	8.050330
6.054364	410.390462	8.055347
6.115707	415.181768	8.060365
6.300960	407.567615	8.065382
5.761065	423.321881	8.070400
6.123904	418.107474	8.075418
6.115682	421.148026	8.080435
5.976215	421.040260	8.085453
6.457467	419.894734	8.090470
6.378442	421.465226	8.095488
6.330286	412.834480	8.100506
6.190364	416.927474	8.105523
5.695444	416.756923	8.110541
5.890427	408.611471	8.115558
5.919512	419.960998	8.120576
6.218576	414.924268	8.125594
5.928266	416.767130	8.130611
5.654348	422.838868	8.135629
6.075147	424.023071	8.140646
6.199822	424.676429	8.145664
6.091231	416.430466	8.150682
5.962974	428.560331	8.155699
6.213461	424.307965	8.160717
6.227411	423.615778	8.165734
6.083879	427.751102	8.170752
6.365816	414.650652	8.175770
6.448806	417.942615	8.180787
6.308827	429.308335	8.185805
6.520865	427.580071	8.190822
6.315953	428.262614	8.195840
6.694398	417.289337	8.200858
6.147962	417.722157	8.205875
5.951629	418.341670	8.210893
6.433608	416.095118	8.215910
6.166905	420.814970	8.220928
6.129428	422.510461	8.225946
6.104347	422.511894	8.230963
5.673727	426.159362	8.235981
6.251791	425.240898	8.240998
6.312796	447.310784	8.246016
6.558742	453.611781	8.251034
6.226845	435.107434	8.256051
6.145177	432.859341	8.261069
6.540223	436.973392	8.266086
6.208801	440.106636	8.271104
6.246684	438.125143	8.276122
6.581166	448.411592	8.281139
6.353205	433.874603	8.286157
6.543654	423.018667	8.291174
6.550651	425.357930	8.296192
6.581769	427.239097	8.301210
6.584984	418.539412	8.306227
6.362185	424.446792	8.311245
6.639216	419.579247	8.316262
6.332103	424.684111	8.321280
6.357231	409.771597	8.326298
6.417542	409.578194	8.331315
6.368837	418.546286	8.336333
6.569464	413.507943	8.341350
6.417361	422.643936	8.346368
6.337726	417.473274	8.351386
6.311352	424.223261	8.356403
6.250669	424.192403	8.361421
6.237727	418.256420	8.366438
6.170894	428.181782	8.371456
6.524091	426.239999	8.376474
6.370853	412.344351	8.381491
6.030010	426.398652	8.386509
6.539988	417.500690	8.391526
6.529261	418.748083	8.396544
6.300244	420.661696	8.401562
6.522583	423.286930	8.406579
6.493205	424.209482	8.411597
6.646558	413.669319	8.416614
6.344954	417.614296	8.421632
6.341398	413.904555	8.426650
6.540876	424.979431	8.431667
6.557951	433.128034	8.436685
6.521688	430.748021	8.441702
6.609847	425.728496	8.446720
6.549406	421.018992	8.451738
6.480509	413.950625	8.456755
6.304202	423.670505	8.461773
6.656385	421.987337	8.466790
6.700284	427.338976	8.471808
6.350150	429.760605	8.476826
6.790003	428.743776	8.481843
6.584420	439.545407	8.486861
6.552622	419.542076	8.491878
6.623070	422.673530	8.496896
6.576923	415.149853	8.501914
6.589415	415.390125	8.506931
6.278985	421.368900	8.511949
6.495704	424.046242	8.516966
6.706888	441.338438	8.521984
6.525125	443.675499	8.527002
6.964693	446.764337	8.532019
6.324909	435.490005	8.537037
6.766208	446.655947	8.542054
6.792958	447.969965	8.547072
6.492072	432.620898	8.552090
6.531919	430.538890	8.557107
6.580822	450.026123	8.562125
6.810277	444.744431	8.567143
7.043887	437.959992	8.572160
6.573230	442.860857	8.577178
6.645004	428.813375	8.582195
6.465800	431.264175	8.587213
6.873162	427.099995	8.592231
6.456296	424.276745	8.597248
6.447647	428.762739	8.602266
6.871568	443.902930	8.607283
6.683478	449.916178	8.612301
6.831984	441.290053	8.617319
6.975722	429.031316	8.622336
6.403518	431.935749	8.627354
6.679474	420.392671	8.632371
6.510021	434.737278	8.637389
6.904088	437.782471	8.642407
6.905754	447.718942	8.647424
6.582721	436.384678	8.652442
6.908453	431.823611	8.657459
6.456609	437.444536	8.662477
7.005138	439.601221	8.667495
6.911124	424.598587	8.672512
6.700292	434.728690	8.677530
6.876287	418.627291	8.682547
6.678782	421.498806	8.687565
6.496995	426.745505	8.692583
6.780797	433.497476	8.697600
6.833289	446.748723	8.702618
7.008398	438.535685	8.707635
6.638344	458.681830	8.712653
6.834416	453.998536	8.717671
7.124706	456.190505	8.722688
6.635322	442.517804	8.727706
7.234950	444.702443	8.732723
6.759722	437.205715	8.737741
6.768438	428.316939	8.742759
6.897272	428.258635	8.747776
6.476206	424.134203	8.752794
6.994877	432.886705	8.757811
6.947999	442.917819	8.762829
6.828643	437.247858	8.767847
6.911936	429.380911	8.772864
6.676697	449.344692	8.777882
7.063672	438.383570	8.782899
6.764843	445.148370	8.787917
6.992672	453.030801	8.792935
7.108783	454.524891	8.797952
6.645525	447.257066	8.802970
6.976967	442.349601	8.807987
6.792228	448.236712	8.813005
6.768696	450.201926	8.818023
6.880703	448.331770	8.823040
6.952322	450.807963	8.828058
7.081496	442.570248	8.833075
7.178517	454.943126	8.838093
7.063727	449.063363	8.843111
7.202868	444.886512	8.848128
6.689866	440.329102	8.853146
7.122639	438.864264	8.858163
6.939645	449.771406	8.863181
6.933159	447.786826	8.868199
7.114062	450.758273	8.873216
6.726169	449.227178	8.878234
6.969153	448.199841	8.883251
7.180615	449.741523	8.888269
6.914813	454.690353	8.893287
7.255495	451.273379	8.898304
6.984340	453.474269	8.903322
7.016785	448.075997	8.908339
7.010495	451.863230	8.913357
6.663177	458.000873	8.918375
6.905773	447.340208	8.923392
6.912839	454.524798	8.928410
6.902362	449.006280	8.933427
7.015117	455.105332	8.938445
7.195386	457.280484	8.943463
6.921082	454.831822	8.948480
6.720464	453.158305	8.953498
7.002834	449.304955	8.958515
6.765385	446.427583	8.963533
6.915358	451.069785	8.968551
7.508281	443.453259	8.973568
6.990528	452.641944	8.978586
6.990865	452.296279	8.983603
7.232015	450.374228	8.988621
6.937319	439.540156	8.993639
7.221400	441.557376	8.998656
7.145043	448.985880	9.003674
7.209464	436.817628	9.008691
7.111619	444.865591	9.013709
6.852582	442.759260	9.018727
7.317998	462.098015	9.023744
7.170548	462.267339	9.028762
7.380300	456.977489	9.033779
7.291222	452.061512	9.038797
7.553072	454.229059	9.043815
7.359632	455.253578	9.048832
6.930928	451.520928	9.053850
7.284094	447.073415	9.058867
7.152642	451.108720	9.063885
6.937492	447.020652	9.068903
7.264103	450.871058	9.073920
7.199316	454.342213	9.078938
7.319754	442.733342	9.083955
7.237530	446.435517	9.088973
7.091230	449.812893	9.093991
7.442596	459.270627	9.099008
7.110989	459.487373	9.104026
7.008061	456.712912	9.109043
7.467861	469.712098	9.114061
7.506631	470.378503	9.119079
7.468404	455.485294	9.124096
7.225101	458.921842	9.129114
7.308753	447.317484	9.134131
7.536127	448.544348	9.139149
7.456664	445.827810	9.144167
7.186204	440.268887	9.149184
6.975323	447.757852	9.154202
7.079930	465.245664	9.159219
7.617891	473.516090	9.164237
7.421614	472.930362	9.169255
7.653844	480.852824	9.174272
6.943462	465.876630	9.179290
7.153571	471.225760	9.184307
7.129374	475.156309	9.189325
7.533562	473.567470	9.194343
7.684729	462.987284	9.199360
7.259368	479.739304	9.204378
7.765371	473.675834	9.209395
7.819529	480.410739	9.214413
7.468091	465.321568	9.219431
7.382460	452.786839	9.224448
7.029120	460.862551	9.229466
7.520807	468.982381	9.234483
7.457836	472.416824	9.239501
7.599111	472.832216	9.244519
7.706216	471.044950	9.249536
7.682550	463.312422	9.254554
7.386437	452.067383	9.259571
7.575479	446.219981	9.264589
7.188050	441.749251	9.269607
7.401770	447.695568	9.274624
7.521052	460.035237	9.279642
7.534629	464.221124	9.284659
7.618305	467.431691	9.289677
7.358729	466.299987	9.294695
7.619150	469.675564	9.299712
7.674006	470.083220	9.304730
7.513266	449.187091	9.309747
7.783036	458.518188	9.314765
7.644106	461.266633	9.319783
8.060848	445.449531	9.324800
7.530740	442.853676	9.329818
7.680391	436.167584	9.334835
7.649590	437.809023	9.339853
7.321420	440.801384	9.344871
7.721790	441.645492	9.349888
7.500915	441.599824	9.354906
7.135047	454.284375	9.359923
7.428239	447.128870	9.364941
7.356100	468.446675	9.369959
7.812094	471.402689	9.374976
7.916299	473.532174	9.379994
7.572518	460.573879	9.385011
7.561971	445.739084	9.390029
7.614475	459.452512	9.395047
7.624951	469.772944	9.400064
7.579833	479.693759	9.405082
7.582711	470.227224	9.410099
8.065389	470.920508	9.415117
7.370739	468.994962	9.420135
7.801411	469.757483	9.425152
7.691097	471.945718	9.430170
7.767014	470.943288	9.435187
8.016433	473.901426	9.440205
7.375848	466.550168	9.445223
7.317495	458.037810	9.450240
7.300993	473.623179	9.455258
7.515167	473.133253	9.460275
7.719326	474.403133	9.465293
7.505782	483.689680	9.470311
7.877148	476.261589	9.475328
7.819464	473.281220	9.480346
7.868873	476.832283	9.485363
7.719595	469.231175	9.490381
7.651718	477.702902	9.495399
7.808455	470.661315	9.500416
7.465889	478.539400	9.505434
7.439823	475.720713	9.510451
7.530091	476.927569	9.515469
7.414283	480.094011	9.520487
7.919989	495.878934	9.525504
8.165183	504.919463	9.530522
7.718380	502.418458	9.535539
8.164915	496.712244	9.540557
7.983580	486.101675	9.545575
7.682234	483.584065	9.550592
7.796464	478.826527	9.555610
7.749571	486.484603	9.560627
7.889726	484.764496	9.565645
7.794220	491.184054	9.570663
8.031032	496.316777	9.575680
8.187092	501.958510	9.580698
7.784171	489.977833	9.585715
8.104071	477.330659	9.590733
7.690806	479.265735	9.595751
7.908110	477.866689	9.600768
7.859457	486.434051	9.605786
7.918451	495.264675	9.610803
8.100468	502.935638	9.615821
7.767576	501.745604	9.620839
7.694561	503.151536	9.625856
8.042531	503.864372	9.630874
8.024895	496.895936	9.635891
8.067395	495.744325	9.640909
8.016345	501.557156	9.645927
8.338244	510.632818	9.650944
8.033715	507.027614	9.655962
8.062290	496.952516	9.660979
8.008008	488.500290	9.665997
7.856345	500.799824	9.671015
8.237684	493.909998	9.676032
8.138295	491.680971	9.681050
7.772880	486.591071	9.686067
7.911576	493.150380	9.691085
7.800342	496.891226	9.696103
8.171487	505.767011	9.701120
8.080017	497.926804	9.706138
8.019167	503.417067	9.711155
8.262196	500.248915	9.716173
8.112559	509.318806	9.721191
8.160292	507.424643	9.726208
8.352521	504.574724	9.731226
7.918463	504.001599	9.736243
7.878423	493.769963	9.741261
8.359507	510.133940	9.746279
8.383434	494.166888	9.751296
8.389162	507.211181	9.756314
8.067443	504.102099	9.761331
8.451460	494.592513	9.766349
7.614812	483.768433	9.771367
8.179424	496.534749	9.776384
8.073683	501.693688	9.781402
7.805440	500.280955	9.786419
8.379172	504.819342	9.791437
8.352392	514.420628	9.796455
8.361868	513.640798	9.801472
8.253911	501.398684	9.806490
8.015840	513.833199	9.811507
8.228557	507.567314	9.816525
8.320390	506.883289	9.821543
8.307381	501.208094	9.826560
8.319416	514.597586	9.831578
8.279144	509.349513	9.836595
8.610759	500.191098	9.841613
8.259146	505.805293	9.846631
8.156284	513.948013	9.851648
8.642132	501.057803	9.856666
7.873518	505.799772	9.861683
8.347424	499.664644	9.866701
8.313142	504.502519	9.871719
8.274452	504.204257	9.876736
8.263745	505.420946	9.881754
8.225021	504.055437	9.886771
8.395064	494.259848	9.891789
7.928644	510.940556	9.896807
8.203847	503.416769	9.901824
8.530072	498.911699	9.906842
8.270696	507.536602	9.911859
8.364909	497.817146	9.916877
8.181520	499.739157	9.921895
8.299891	498.288977	9.926912
8.441010	503.892243	9.931930
8.296659	504.634442	9.936947
8.430576	506.777908	9.941965
8.005486	508.264974	9.946983
8.251779	504.462661	9.952000
8.257143	505.761920	9.957018
8.346886	499.301061	9.962035
8.641847	493.780961	9.967053
8.450203	499.428108	9.972071
8.433268	500.339943	9.977088
8.592775	502.994886	9.982106
8.433674	496.701211	9.987123
8.761009	492.111909	9.992141
8.650664	491.950307	9.997159
8.549492	499.450066	10.002176
8.612779	494.589548	10.007194
8.441525	501.439343	10.012211
8.647054	497.122359	10.017229
8.619543	502.400618	10.022247
8.298638	494.224414	10.027264
8.536319	495.327536	10.032282
8.160618	495.919277	10.037299
8.375122	494.290590	10.042317
8.618062	511.377817	10.047335
8.649799	528.930913	10.052352
8.838745	522.431178	10.057370
8.116777	522.448410	10.062387
8.501283	519.863677	10.067405
8.629457	530.549675	10.072423
8.474639	530.063175	10.077440
8.880291	525.142018	10.082458
8.962461	533.510982	10.087475
9.039911	515.335185	10.092493
8.400292	509.548606	10.097511
8.525610	502.524214	10.102528
8.761677	494.095160	10.107546
8.990651	498.490648	10.112563
8.877205	493.605266	10.117581
8.545649	496.775353	10.122599
8.772602	498.482967	10.127616
8.681813	493.761932	10.132634
8.491500	497.552092	10.137651
8.429772	493.035483	10.142669
8.542262	501.454720	10.147687
8.520559	514.380734	10.152704
8.937707	529.251282	10.157722
8.579583	536.106250	10.162739
8.718570	528.971125	10.167757
8.829307	530.305493	10.172775
8.962882	531.211303	10.177792
8.981948	531.870344	10.182810
8.789383	528.373358	10.187827
8.810044	532.205554	10.192845
8.981504	535.273457	10.197863
8.628936	516.144129	10.202880
9.206923	523.662924	10.207898
8.503688	504.555657	10.212915
8.663362	518.454527	10.217933
8.991336	520.244228	10.222951
8.885099	532.382732	10.227968
8.959402	531.750425	10.232986
8.960819	532.163979	10.238003
8.873691	519.022199	10.243021
8.675832	519.074682	10.248039
8.809394	532.135620	10.253056
8.937022	532.949901	10.258074
8.792566	541.355216	10.263091
8.904218	537.948788	10.268109
9.069628	534.535033	10.273127
8.630289	538.766217	10.278144
8.990127	534.114832	10.283162
8.794317	543.678579	10.288179
9.035071	543.318689	10.293197
9.048524	541.145767	10.298215
8.695924	537.235150	10.303232
9.017930	531.139729	10.308250
8.668070	544.955882	10.313267
8.625173	540.491649	10.318285
8.793934	547.649507	10.323303
8.784890	542.992671	10.328320
8.731143	535.005656	10.333338
8.796944	545.179979	10.338355
8.905144	539.179797	10.343373
8.796673	540.331975	10.348391
9.067954	556.956516	10.353408
9.185618	559.294008	10.358426
9.211023	559.132366	10.363443
9.617771	553.353198	10.368461
9.186127	545.124442	10.373479
9.340496	541.831405	10.378496
9.277478	531.284278	10.383514
9.064722	530.751076	10.388531
8.815382	527.361911	10.393549
9.108304	531.958420	10.398567
9.246441	538.088340	10.403584
9.462039	532.409725	10.408602
9.337338	540.585405	10.413619
9.056682	536.417614	10.418637
9.138634	537.131592	10.423655
9.115515	536.074500	10.428672
9.328258	532.166325	10.433690
9.052678	531.165997	10.438707
9.141569	537.015901	10.443725
9.179542	532.664649	10.448743
8.899729	535.523439	10.453760
9.202153	527.000707	10.458778
9.036193	538.284594	10.463795
9.222318	530.791685	10.468813
9.260448	525.882177	10.473831
9.107446	534.300319	10.478848
9.040753	530.438810	10.483866
9.011048	541.915478	10.488883
9.434977	549.548373	10.493901
9.493284	551.274866	10.498919
9.173064	562.338660	10.503936
9.615002	554.820700	10.508954
9.177842	545.687796	10.513971
9.291484	541.184257	10.518989
9.408851	548.282913	10.524007
9.373754	559.306578	10.529024
9.440067	549.862755	10.534042
8.973266	546.835953	10.539059
9.050136	561.796736	10.544077
9.234429	551.809392	10.549095
9.507491	556.954439	10.554112
9.313149	556.787456	10.559130
9.261712	565.581292	10.564147
9.279238	564.102926	10.569165
9.160440	557.267152	10.574183
9.257021	560.407298	10.579200
9.415745	556.585223	10.584218
9.248029	556.316198	10.589235
9.172980	554.575227	10.594253
9.255478	548.394270	10.599271
9.306359	562.969619	10.604288
9.797298	560.735736	10.609306
9.387848	555.767665	10.614323
9.274344	565.342597	10.619341
9.396724	570.595666	10.624359
9.286678	561.356620	10.629376
9.467247	571.544236	10.634394
9.728859	579.826035	10.639411
9.747882	576.558945	10.644429
9.882926	558.312541	10.649447
9.518935	565.271243	10.654464
9.768265	560.223608	10.659482
9.487926	558.130040	10.664499
9.885099	555.360145	10.669517
9.792840	550.470645	10.674535
9.398562	560.840841	10.679552
9.684458	548.617521	10.684570
9.529534	551.005661	10.689587
9.497421	549.204040	10.694605
9.910875	552.588152	10.699623
9.328149	553.374796	10.704640
9.553947	550.926174	10.709658
9.421677	559.230274	10.714675
9.165762	562.449656	10.719693
9.569447	574.245502	10.724711
9.569240	589.735973	10.729728
10.054216	586.316138	10.734746
9.767610	582.220182	10.739763
9.796262	568.036810	10.744781
9.887290	558.352683	10.749799
9.371458	557.911397	10.754816
9.836284	569.851831	10.759834
9.702339	566.162857	10.764851
9.792321	574.672273	10.769869
9.652332	564.331952	10.774887
9.633907	572.452256	10.779904
9.840145	575.526219	10.784922
10.233925	579.975340	10.789939
9.477520	570.679157	10.794957
9.816056	560.939478	10.799975
9.687188	576.066618	10.804992
10.011255	580.424928	10.810010
10.076322	574.145672	10.815027
9.584212	567.145347	10.820045
9.878777	566.219494	10.825063
9.511859	580.486900	10.830080
9.479663	587.755215	10.835098
9.965090	588.922824	10.840115
10.017956	590.430156	10.845133
10.165272	579.619834	10.850151
9.701462	583.875159	10.855168
10.125081	581.279216	10.860186
10.232845	579.774489	10.865203
10.005931	584.242933	10.870221
10.006407	560.371121	10.875239
9.845535	564.425499	10.880256
9.854518	562.158045	10.885274
9.716260	575.063649	10.890291
10.011653	583.583542	10.895309
10.460178	575.671592	10.900327
10.077599	568.472825	10.905344
9.903104	557.077263	10.910362
9.920965	549.662205	10.915379
9.518717	568.754048	10.920397
9.895270	574.231548	10.925415
10.129016	579.702778	10.930432
10.117966	582.876105	10.935450
9.960790	583.724559	10.940467
9.958344	587.117315	10.945485
10.201100	585.004048	10.950503
9.928259	593.107835	10.955520
10.154745	587.060884	10.960538
10.028014	587.612188	10.965555
9.792424	587.502426	10.970573
10.061632	581.879479	10.975591
10.071261	586.457959	10.980608
10.458575	578.668735	10.985626
10.355282	581.554205	10.990643
9.838654	590.302260	10.995661
10.054223	578.440147	11.000679
10.107568	579.860396	11.005696
9.923893	591.635414	11.010714
10.047473	582.295075	11.015731
10.123666	582.952531	11.020749
10.530376	576.276171	11.025767
10.000731	582.548576	11.030784
10.153771	583.505493	11.035802
10.187524	589.380688	11.040819
10.197926	582.568387	11.045837
10.350738	575.087666	11.050855
10.645197	583.586848	11.055872
10.129038	576.452320	11.060890
10.487232	589.628462	11.065907
10.671076	580.643083	11.070925
10.428192	582.000581	11.075943
10.250869	582.233904	11.080960
10.185329	582.053466	11.085978
10.281549	579.036175	11.090995
10.049860	585.948964	11.096013
10.625298	579.130496	11.101031
9.984987	589.395397	11.106048
10.234566	583.970964	11.111066
10.268063	580.971933	11.116083
10.329712	582.426632	11.121101
10.300434	580.961132	11.126119
9.913085	581.947694	11.131136
10.109838	585.820819	11.136154
10.250739	597.185817	11.141171
10.440904	610.720096	11.146189
10.696133	608.874037	11.151207
10.730652	607.040117	11.156224
10.170178	594.070351	11.161242
10.133016	596.725202	11.166259
10.239128	610.976901	11.171277
10.600312	604.611987	11.176295
10.563976	616.235074	11.181312
10.770534	610.681150	11.186330
10.685892	613.254500	11.191347
10.757677	608.773226	11.196365
10.659250	594.545128	11.201383
10.642436	588.566810	11.206400
10.372276	594.682478	11.211418
10.541884	583.950739	11.216435
10.240079	589.467351	11.221453
10.655699	588.773798	11.226471
10.763022	608.377730	11.231488
10.341076	608.445668	11.236506
10.850202	598.941087	11.241523
10.540241	608.349377	11.246541
10.733803	601.407925	11.251559
10.640976	612.549842	11.256576
10.645039	614.861668	11.261594
10.844021	604.658485	11.266611
10.337738	598.529339	11.271629
10.552266	601.021259	11.276647
10.628184	603.532196	11.281664
10.600098	608.085433	11.286682
10.823080	601.920166	11.291699
10.216163	609.015171	11.296717
10.522698	608.638482	11.301735
10.632765	596.138747	11.306752
10.626745	602.071316	11.311770
10.481987	605.501814	11.316787
10.621678	610.237887	11.321805
10.538796	607.429765	11.326823
10.731977	602.981537	11.331840
10.367288	614.188157	11.336858
11.038102	616.966707	11.341875
10.879098	618.028051	11.346893
10.975441	614.824130	11.351911
10.834805	606.101903	11.356928
10.787240	607.750663	11.361946
10.965340	599.963004	11.366963
10.901204	603.085287	11.371981
11.053846	597.141106	11.376999
11.021743	613.369516	11.382016
10.549728	610.570716	11.387034
10.931286	603.997716	11.392051
10.758195	608.039169	11.397069
10.830322	603.518472	11.402087
10.679777	604.859894	11.407104
10.993696	624.756783	11.412122
11.241304	626.951908	11.417139
11.209640	624.310883	11.422157
11.225675	608.963488	11.427175
10.813967	605.813777	11.432192
10.809471	618.220130	11.437210
11.009959	601.105292	11.442227
10.868487	603.230598	11.447245
10.844499	599.497426	11.452263
11.081335	601.246326	11.457280
11.021873	626.670865	11.462298
11.009313	625.904127	11.467315
11.231723	635.458121	11.472333
11.248927	625.845229	11.477351
11.020033	606.962617	11.482368
10.834189	619.787560	11.487386
10.935608	625.340558	11.492403
10.993540	634.982021	11.497421
10.750593	644.418997	11.502439
11.228066	638.480457	11.507456
11.385236	647.235466	11.512474
11.002180	636.125943	11.517491
11.245376	640.695288	11.522509
11.268621	642.529165	11.527527
11.362885	643.912331	11.532544
11.300694	642.171583	11.537562
11.490911	638.223019	11.542579
11.506715	635.042666	11.547597
11.180433	613.286574	11.552615
11.481258	601.603228	11.557632
10.964828	614.677386	11.562650
10.892010	615.303223	11.567667
10.858844	637.774385	11.572685
11.117961	635.307636	11.577703
11.607486	630.751276	11.582720
11.293790	641.985296	11.587738
11.590906	637.198606	11.592755
11.179629	640.262244	11.597773
11.443883	633.206716	11.602791
11.777938	635.850887	11.607808
11.490821	632.683296	11.612826
11.313980	608.230964	11.617843
11.103048	619.623532	11.622861
11.292437	635.134619	11.627879
11.595517	627.858897	11.632896
11.474678	639.602681	11.637914
11.466839	613.000037	11.642931
11.129127	618.461978	11.647949
11.302372	621.066244	11.652967
11.326778	635.512588	11.657984
11.289425	633.825992	11.663002
11.515278	629.540053	11.668019
11.367166	639.329411	11.673037
11.333794	629.695365	11.678055
11.837561	637.895366	11.683072
11.408786	638.565975	11.688090
11.651331	633.900914	11.693107
11.383681	638.606422	11.698125
11.485963	637.743112	11.703143
11.503187	638.001698	11.708160
11.471725	641.122120	11.713178
11.630134	631.070906	11.718195
11.549334	642.035272	11.723213
11.261581	635.838823	11.728231
11.602394	627.126620	11.733248
11.432348	639.807633	11.738266
11.579636	629.519692	11.743283
11.626409	623.492644	11.748301
11.615680	628.096159	11.753319
11.708882	621.348867	11.758336
11.319811	634.361403	11.763354
11.647504	629.398401	11.768371
11.516406	630.496461	11.773389
11.264226	629.967816	11.778407
11.646755	631.187505	11.783424
11.353143	646.005399	11.788442
11.757988	648.706744	11.793459
11.425366	656.357891	11.798477
11.592656	660.318586	11.803495
11.716942	661.727095	11.808512
11.732693	668.687918	11.813530
11.901745	662.794141	11.818547
12.175291	663.219720	11.823565
11.935024	666.199537	11.828583
12.046816	663.222563	11.833600
12.051099	666.160703	11.838618
12.029011	660.667456	11.843635
11.741543	648.448849	11.848653
11.515672	647.980803	11.853671
11.857606	647.471093	11.858688
11.859561	669.745552	11.863706
11.786379	666.451588	11.868723
12.107709	668.895521	11.873741
11.686694	676.651467	11.878759
11.957004	658.664815	11.883776
12.079243	666.848485	11.888794
12.205343	669.501115	11.893811
12.244763	655.611139	11.898829
11.680759	647.662105	11.903847
11.877762	641.736544	11.908864
11.748616	656.963804	11.913882
11.848674	654.519847	11.918899
11.872969	668.018261	11.923917
12.153156	665.409050	11.928935
11.957226	656.464074	11.933952
11.959387	657.666047	11.938970
12.222018	657.223403	11.943987
12.195912	661.970805	11.949005
12.031033	661.712332	11.954023
12.325368	660.342835	11.959040
11.973492	664.107626	11.964058
11.910044	653.730556	11.969075
11.984794	659.290344	11.974093
11.815082	659.647598	11.979111
12.220846	660.319772	11.984128
11.798073	660.357139	11.989146
11.756356	661.610076	11.994163
11.863394	663.759984	11.999181
11.802270	665.033851	12.004199
12.368250	668.242739	12.009216
12.603710	670.961901	12.014234
12.362978	664.903710	12.019251
12.285177	670.684028	12.024269
12.323836	667.847502	12.029287
12.252981	662.305640	12.034304
12.390284	659.641747	12.039322
12.256605	662.733827	12.044339
12.378143	655.051958	12.049357
12.208490	663.942193	12.054375
12.390276	662.390557	12.059392
12.356813	667.104535	12.064410
12.126261	653.606884	12.069427
12.332848	667.973487	12.074445
12.117925	664.330575	12.079463
12.362944	650.330578	12.084480
12.359144	656.891899	12.089498
12.282345	654.926810	12.094515
12.543561	661.419054	12.099533
12.080862	660.628433	12.104551
12.548228	680.068905	12.109568
12.207437	693.707320	12.114586
12.176644	689.905177	12.119603
12.614546	692.028252	12.124621
12.420748	692.786718	12.129639
12.499680	696.801421	12.134656
12.579601	694.047817	12.139674
12.487252	696.638598	12.144691
12.448519	705.506391	12.149709
12.204462	701.291158	12.154727
12.802806	695.390846	12.159744
12.802862	696.587659	12.164762
12.544323	695.949834	12.169779
12.799241	696.814302	12.174797
12.452424	696.267862	12.179815
12.670787	700.617333	12.184832
12.911900	698.605500	12.189850
12.563693	687.867314	12.194867
12.720643	680.508291	12.199885
12.578842	678.018951	12.204903
12.817756	666.244240	12.209920
12.643565	668.435599	12.214938
12.704646	657.976491	12.219955
12.856781	653.122470	12.224973
12.619510	656.830095	12.229991
12.587111	658.495245	12.235008
12.794455	667.723821	12.240026
12.971684	667.487433	12.245043
12.885613	651.303408	12.250061
12.499792	665.138614	12.255079
12.279084	652.215680	12.260096
12.543930	671.094040	12.265114
12.745991	688.806899	12.270131
12.878145	682.766083	12.275149
12.341075	697.403486	12.280167
12.714404	692.446293	12.285184
12.914154	689.386642	12.290202
12.799121	694.886930	12.295219
13.064484	686.633620	12.300237
12.769146	688.253342	12.305255
12.980605	683.423345	12.310272
12.807737	696.385565	12.315290
12.853625	693.774991	12.320307
12.985390	679.702388	12.325325
12.637982	683.082999	12.330343
12.842214	688.563880	12.335360
13.128850	684.170622	12.340378
12.782950	686.064056	12.345395
12.865842	682.163961	12.350413
12.779852	691.088780	12.355431
12.900761	679.409973	12.360448
12.864715	684.684984	12.365466
12.739590	690.465666	12.370483
12.909141	693.877206	12.375501
12.958467	719.274827	12.380519
13.175799	714.967442	12.385536
13.225339	718.003605	12.390554
13.415345	716.613586	12.395571
13.296257	714.364168	12.400589
13.164625	705.729366	12.405607
12.865485	699.215502	12.410624
13.136167	701.109196	12.415642
13.306020	713.804848	12.420659
13.208584	691.525343	12.425677
13.061111	695.394082	12.430695
13.128819	709.388860	12.435712
13.606757	709.941610	12.440730
13.475879	698.247005	12.445747
13.238465	701.531851	12.450765
13.073274	695.356420	12.455783
13.352903	689.923038	12.460800
13.294127	687.317985	12.465818
13.097079	695.075040	12.470835
13.240131	687.215980	12.475853
13.079281	694.904839	12.480871
13.069080	708.290109	12.485888
13.173015	718.497205	12.490906
13.386124	723.303829	12.495923
13.378591	715.081521	12.500941
13.221146	723.040289	12.505959
13.279843	723.059737	12.510976
13.161231	715.458941	12.515994
13.004010	718.447455	12.521011
13.599467	712.133857	12.526029
13.162589	726.351961	12.531047
13.425474	723.450738	12.536064
13.172778	721.145101	12.541082
13.165335	723.004934	12.546099
13.393147	722.621989	12.551117
13.554333	724.017701	12.556135
13.434738	720.299544	12.561152
13.836897	718.614565	12.566170
13.677066	722.362135	12.571187
13.893175	719.111984	12.576205
13.734301	726.520625	12.581223
13.623322	721.246002	12.586240
13.914585	718.307405	12.591258
13.786774	722.885850	12.596275
14.180418	724.521009	12.601293
13.713503	724.521987	12.606311
13.883636	712.522028	12.611328
13.878431	703.166328	12.616346
13.571928	698.864198	12.621363
13.679158	686.352656	12.626381
13.366549	689.706248	12.631399
13.439883	701.563981	12.636416
13.948441	713.694912	12.641434
13.374770	715.432770	12.646451
13.738133	712.003520	12.651469
13.819257	717.649671	12.656487
13.587402	718.098708	12.661504
13.851569	717.090089	12.666522
13.340174	713.900567	12.671539
13.664303	712.905247	12.676557
13.647495	717.457042	12.681575
13.826147	711.872271	12.686592
13.717615	719.817820	12.691610
13.362010	709.746952	12.696627
13.855921	710.213203	12.701645
13.645636	712.634156	12.706663
13.900523	719.778226	12.711680
13.843494	711.491285	12.716698
13.620115	723.531626	12.721715
13.931295	719.640567	12.726733
13.852888	726.337494	12.731751
13.792905	742.009660	12.736768
14.112800	737.530175	12.741786
13.926429	753.543738	12.746803
14.035072	749.433073	12.751821
14.091456	750.563085	12.756839
13.886147	745.445012	12.761856
14.406778	735.451067	12.766874
13.925270	729.774435	12.771891
14.093024	723.136007	12.776909
14.150347	720.766041	12.781927
14.074497	719.916477	12.786944
13.960316	712.147634	12.791962
13.664117	729.282451	12.796979
14.024203	733.055342	12.801997
13.732983	749.992910	12.807015
14.250079	753.179204	12.812032
14.234295	749.153707	12.817050
14.134146	755.895977	12.822067
14.401565	746.925402	12.827085
14.189719	749.317092	12.832103
14.121060	742.521750	12.837120
14.465591	741.916731	12.842138
14.124776	751.274706	12.847155
14.362636	745.730510	12.852173
14.158347	749.765750	12.857191
14.172547	740.393036	12.862208
14.514299	747.832562	12.867226
14.126286	749.651092	12.872243
14.124991	737.406286	12.877261
14.417094	734.314012	12.882279
14.072909	745.424028	12.887296
14.331780	733.436523	12.892314
14.247434	749.291462	12.897331
14.208398	731.948046	12.902349
14.549730	742.578029	12.907367
14.200788	749.078437	12.912384
14.205294	742.416248	12.917402
14.174645	751.170135	12.922419
14.210951	742.637419	12.927437
14.259715	740.621606	12.932455
14.314474	748.046454	12.937472
14.473448	752.793944	12.942490
14.621792	768.538328	12.947507
14.528107	772.513528	12.952525
14.348308	763.078047	12.957543
14.476132	771.106132	12.962560
14.823870	758.776348	12.967578
14.527605	772.017320	12.972595
14.657513	768.104694	12.977613
14.368637	767.914780	12.982631
14.026589	769.877662	12.987648
14.885439	767.243869	12.992666
15.114615	770.545951	12.997683
14.920262	772.461150	13.002701
14.854650	765.041701	13.007719
14.452475	764.044605	13.012736
15.005266	753.076079	13.017754
14.755538	746.748492	13.022771
14.840659	743.143273	13.027789
14.745069	738.985725	13.032807
14.475258	737.855301	13.037824
14.894949	751.448936	13.042842
14.402208	753.209221	13.047859
14.816433	764.385783	13.052877
15.077544	760.982509	13.057895
14.742640	769.047453	13.062912
15.223831	761.484708	13.067930
14.679200	753.071410	13.072947
14.754730	752.980202	13.077965
14.806723	751.980733	13.082983
14.825097	764.390108	13.088000
14.903101	753.842704	13.093018
14.740596	765.473411	13.098035
14.756063	770.630084	13.103053
14.900259	766.628482	13.108071
14.628104	762.341511	13.113088
14.907837	766.494627	13.118106
14.999491	766.886159	13.123123
15.081303	763.983811	13.128141
15.074962	763.695541	13.133159
15.128956	764.135038	13.138176
15.183663	758.704627	13.143194
14.873380	775.936310	13.148211
14.925765	773.383699	13.153229
15.248085	764.754793	13.158247
14.992509	769.043400	13.163264
15.098662	761.678577	13.168282
14.938458	768.546146	13.173299
14.969583	765.787618	13.178317
15.098760	764.420266	13.183335
14.836876	769.004391	13.188352
15.187718	757.403587	13.193370
14.873645	763.130942	13.198387
14.545284	758.726908	13.203405
15.136913	770.518160	13.208423
14.987184	788.662202	13.213440
15.076474	790.080062	13.218458
15.039821	801.383277	13.223475
15.044093	798.429986	13.228493
15.203676	791.077561	13.233511
15.148756	797.639140	13.238528
15.265572	800.949205	13.243546
15.273796	797.755901	13.248563
15.073492	808.048866	13.253581
15.657550	791.389571	13.258599
15.202109	807.376095	13.263616
15.361714	806.219438	13.268634
15.173100	801.035593	13.273651
14.989127	803.192766	13.278669
15.429949	802.978867	13.283687
15.083103	824.664485	13.288704
14.840626	811.980445	13.293722
15.180015	831.467102	13.298739
15.507480	818.076897	13.303757
15.761266	823.059484	13.308775
15.529243	832.383746	13.313792
15.798771	824.853264	13.318810
16.141915	820.766344	13.323827
16.071021	813.363888	13.328845
16.054493	810.624266	13.333863
15.871742	801.985671	13.338880
15.688152	787.432144	13.343898
15.879501	798.383837	13.348915
15.591729	794.122277	13.353933
15.921366	790.856461	13.358951
15.712717	790.317452	13.363968
15.873636	790.364066	13.368986
15.774005	790.250684	13.374003
15.727384	791.106037	13.379021
15.806327	786.163312	13.384039
15.693999	792.513933	13.389056
15.950029	787.548575	13.394074
15.880475	789.295086	13.399091
16.255840	790.206541	13.404109
16.103380	784.061248	13.409127
15.635746	794.246904	13.414144
15.667459	793.312204	13.419162
15.662536	782.091931	13.424179
15.685182	787.869438	13.429197
16.192330	785.216719	13.434215
15.808849	795.336475	13.439232
16.010372	783.527317	13.444250
15.926144	787.864324	13.449267
15.756945	791.270958	13.454285
15.863526	787.251171	13.459303
15.767723	789.803171	13.464320
15.938343	788.725791	13.469338
16.154951	791.748869	13.474355
15.709697	791.659256	13.479373
16.039007	784.577927	13.484391
15.829677	786.187748	13.489408
15.999070	786.011315	13.494426
15.902687	785.769449	13.499443
15.714133	787.360870	13.504461
15.981572	780.281127	13.509479
15.736977	800.667558	13.514496
16.088025	808.879555	13.519514
16.374931	809.514334	13.524531
16.146183	822.657952	13.529549
16.299335	809.880056	13.534567
16.111814	816.452577	13.539584
16.380883	823.033743	13.544602
16.520536	827.356128	13.549619
16.221678	817.530898	13.554637
16.265285	803.846780	13.559655
15.837869	799.247335	13.564672
16.165946	808.246956	13.569690
16.296074	808.634480	13.574707
15.747933	818.311460	13.579725
16.061898	804.935311	13.584743
16.373081	815.259721	13.589760
16.060538	813.394275	13.594778
16.225151	808.643252	13.599795
16.058505	809.619265	13.604813
16.368105	806.530771	13.609831
16.166346	809.125122	13.614848
16.689868	817.917984	13.619866
16.531886	815.985607	13.624883
16.286933	810.884707	13.629901
16.385186	815.011197	13.634919
16.160666	823.986196	13.639936
16.391681	832.809393	13.644954
16.733910	840.331165	13.649971
16.447530	847.212183	13.654989
16.841819	845.004501	13.660007
17.017506	849.028419	13.665024
16.788313	832.981284	13.670042
16.905470	815.333182	13.675059
16.298343	824.470746	13.680077
16.536968	807.870208	13.685095
16.524002	820.653698	13.690112
16.564571	838.241508	13.695130
16.754322	838.680181	13.700147
16.470034	842.232256	13.705165
17.134448	835.899710	13.710183
16.863134	832.730248	13.715200
16.527869	822.650819	13.720218
16.698753	824.368542	13.725235
16.560618	829.895143	13.730253
16.609080	825.622383	13.735271
16.950972	845.472406	13.740288
16.633704	843.419164	13.745306
16.632753	830.811645	13.750323
16.535232	841.235244	13.755341
16.843643	837.556022	13.760359
17.004569	841.744580	13.765376
16.600169	826.224474	13.770394
16.900234	831.357268	13.775411
17.000824	832.901601	13.780429
16.913707	848.482309	13.785447
16.859345	845.416283	13.790464
16.884612	845.944395	13.795482
16.766127	841.820137	13.800499
16.768732	840.432794	13.805517
16.895499	842.400727	13.810535
16.977656	866.764065	13.815552
17.477526	880.575236	13.820570
17.468045	859.332850	13.825587
16.953678	852.645909	13.830605
17.021609	846.342054	13.835623
17.054126	846.905972	13.840640
16.869056	845.452859	13.845658
17.222089	846.985705	13.850675
17.073933	876.637757	13.855693
17.057813	864.336646	13.860711
17.223700	868.995235	13.865728
17.310145	871.052523	13.870746
17.361028	875.567173	13.875763
17.365074	873.115459	13.880781
17.468440	873.968815	13.885799
17.269578	863.868347	13.890816
17.078296	863.681168	13.895834
17.464973	856.240716	13.900851
17.375695	860.882897	13.905869
17.499087	868.602330	13.910887
17.421923	860.319037	13.915904
17.341963	864.256556	13.920922
17.318003	853.454327	13.925939
17.324540	872.459955	13.930957
17.571835	870.193544	13.935975
17.457229	869.772811	13.940992
17.350986	865.943357	13.946010
17.394059	873.987498	13.951027
17.207904	875.935208	13.956045
17.064017	870.691966	13.961063
17.310086	872.837778	13.966080
17.406087	873.510865	13.971098
17.592247	861.825840	13.976115
17.292806	871.247899	13.981133
17.672977	873.825423	13.986151
17.425802	863.144004	13.991168
17.317093	872.154576	13.996186
17.706990	867.342216	14.001203
17.414166	894.364431	14.006221
17.653120	901.382489	14.011239
18.033585	898.725140	14.016256
17.810832	891.444639	14.021274
17.833687	875.984044	14.026291
17.570520	874.201749	14.031309
17.728623	886.982556	14.036327
18.021211	891.787882	14.041344
17.840142	899.443184	14.046362
18.012370	886.350268	14.051379
17.612153	871.674665	14.056397
17.699445	884.904186	14.061415
17.830346	890.830728	14.066432
17.712323	902.613220	14.071450
18.015043	893.824109	14.076467
17.895507	898.636265	14.081485
18.116203	890.839438	14.086503
18.080974	898.228474	14.091520
17.925279	900.973867	14.096538
18.162152	901.883854	14.101555
18.108084	901.564903	14.106573
17.868149	903.868358	14.111591
18.069515	899.646240	14.116608
17.907214	908.727910	14.121626
18.178333	902.145908	14.126643
17.968350	903.783407	14.131661
17.689257	901.537622	14.136679
17.704876	904.547944	14.141696
17.849458	902.040278	14.146714
18.042181	899.257330	14.151731
17.934768	905.504038	14.156749
18.089710	902.152958	14.161767
18.162888	895.407287	14.166784
18.173404	899.121968	14.171802
18.534636	891.431392	14.176819
18.228986	902.113503	14.181837
18.160049	896.374790	14.186855
18.288591	895.974421	14.191872
17.990943	899.802333	14.196890
18.174391	908.037411	14.201907
18.209702	923.691619	14.206925
18.338120	925.555357	14.211943
18.689265	925.961796	14.216960
18.529097	926.541088	14.221978
18.543659	915.341507	14.226995
18.727592	927.633444	14.232013
18.664349	911.033178	14.237031
18.437269	895.774573	14.242048
18.289920	900.565352	14.247066
18.422310	901.202494	14.252083
18.315922	913.720834	14.257101
18.610010	916.096486	14.262119
18.569262	922.904187	14.267136
18.531990	932.269879	14.272154
18.718924	927.080495	14.277171
18.533938	922.302292	14.282189
18.568632	935.378367	14.287207
18.582115	932.681390	14.292224
18.444962	930.647915	14.297242
18.628591	927.270427	14.302259
18.508756	931.736594	14.307277
18.607399	928.888119	14.312295
18.700721	934.899245	14.317312
18.521237	934.082576	14.322330
19.107889	922.293788	14.327347
19.004086	926.264404	14.332365
18.626935	929.656686	14.337383
18.799168	926.779098	14.342400
18.582657	929.841641	14.347418
19.038088	924.433789	14.352435
18.814577	921.812276	14.357453
18.720680	929.298833	14.362471
19.352944	924.899061	14.367488
18.855460	922.167016	14.372506
19.005374	921.485166	14.377523
19.106839	922.665204	14.382541
18.803436	917.963695	14.387559
19.038718	920.327040	14.392576
19.170382	914.558646	14.397594
19.138611	913.992705	14.402611
19.173701	913.851896	14.407629
19.089974	920.621045	14.412647
19.326668	920.527558	14.417664
18.856578	922.762439	14.422682
19.092355	927.570096	14.427699
18.898449	923.530349	14.432717
19.014706	925.295317	14.437735
19.108864	915.188419	14.442752
19.098555	925.862978	14.447770
19.090404	917.616256	14.452787
19.331867	925.627966	14.457805
19.350556	935.164701	14.462823
19.420489	922.157195	14.467840
19.094490	923.583601	14.472858
19.496106	926.254430	14.477875
19.256315	933.766329	14.482893
18.812694	940.931289	14.487911
19.011016	943.241310	14.492928
19.068698	955.341585	14.497946
19.690093	954.477728	14.502963
19.877114	962.091793	14.507981
19.403072	967.278016	14.512999
19.901237	949.827686	14.518016
19.563528	956.538124	14.523034
19.693137	952.446373	14.528051
19.439752	942.545426	14.533069
19.196877	952.654205	14.538087
19.543943	957.966260	14.543104
19.747779	962.781974	14.548122
19.566475	960.728248	14.553139
19.521062	955.919442	14.558157
19.601180	959.099796	14.563175
19.758996	960.340189	14.568192
19.567249	959.577122	14.573210
19.564428	959.224488	14.578227
19.851075	963.455644	14.583245
19.278084	961.578190	14.588263
19.757676	954.062072	14.593280
19.657021	954.379945	14.598298
19.387966	960.076690	14.603315
19.517857	961.147698	14.608333
19.261500	959.742597	14.613351
19.655654	953.437435	14.618368
19.566874	972.014496	14.623386
20.015572	980.326552	14.628403
20.311698	979.300028	14.633421
19.924834	993.890395	14.638439
20.088576	969.384246	14.643456
19.765098	968.744957	14.648474
19.897924	973.353936	14.653491
20.134884	980.044813	14.658509
19.604119	985.574281	14.663527
19.990064	982.125879	14.668544
19.925845	982.654641	14.673562
20.224792	978.629328	14.678579
20.237434	978.804036	14.683597
20.057425	972.233323	14.688615
20.062346	974.683639	14.693632
19.925632	983.002873	14.698650
19.937624	980.330150	14.703667
20.439058	984.757233	14.708685
20.283159	981.421389	14.713703
20.325987	971.792623	14.718720
20.185385	981.210886	14.723738
19.989153	985.645232	14.728755
19.856827	978.533175	14.733773
19.916359	979.847716	14.738791
20.261768	968.029158	14.743808
19.790003	984.615395	14.748826
20.411685	996.893954	14.753843
20.668333	997.390844	14.758861
20.165058	1007.579390	14.763879
20.543593	996.996230	14.768896
20.500895	1008.513975	14.773914
20.037480	1010.531628	14.778931
20.405076	1013.167950	14.783949
20.389915	1010.911514	14.788967
20.691018	996.434612	14.793984
20.684055	1012.100634	14.799002
20.579675	1007.840535	14.804019
20.463413	1002.099777	14.809037
20.427498	1006.534353	14.814055
20.566721	1003.688200	14.819072
20.699038	1010.824750	14.824090
20.745959	1010.804418	14.829107
20.871328	1004.035885	14.834125
20.442410	1015.428225	14.839143
20.645314	1009.838939	14.844160
20.757357	1012.241601	14.849178
20.582209	1013.954443	14.854195
20.633659	1011.064557	14.859213
20.708298	1010.091241	14.864231
20.925808	998.343050	14.869248
20.603795	1008.258677	14.874266
20.755351	1002.375937	14.879283
21.091253	1003.368742	14.884301
20.559832	1008.608966	14.889319
20.966627	1007.270816	14.894336
20.957856	1008.267547	14.899354
20.894566	1001.798356	14.904371
21.049970	1010.528274	14.909389
20.845839	1008.881458	14.914407
21.269120	1009.396029	14.919424
21.308504	1005.144802	14.924442
20.921483	1005.917168	14.929459
20.927881	1000.699782	14.934477
20.763261	1007.063480	14.939495
20.863876	1005.220931	14.944512
21.018281	1006.520552	14.949530
20.513285	1017.398737	14.954547
21.123865	1027.337109	14.959565
21.056569	1036.679490	14.964583
21.326436	1033.119594	14.969600
21.185191	1043.991107	14.974618
21.188153	1031.363879	14.979635
21.296528	1040.760636	14.984653
21.125908	1039.446052	14.989671
21.459216	1040.855024	14.994688
21.518662	1032.717516	14.999706
21.330318	1032.384577	15.004723
21.636844	1029.178050	15.009741
21.358104	1032.936329	15.014759
21.415472	1024.593665	15.019776
21.516225	1032.923996	15.024794
21.270915	1035.059075	15.029811
21.574490	1030.733385	15.034829
21.671631	1035.592379	15.039847
21.546729	1036.553225	15.044864
21.648358	1034.293195	15.049882
21.248849	1033.223593	15.054899
21.407764	1034.877577	15.059917
21.583706	1036.444885	15.064935
21.216227	1032.838956	15.069952
21.489035	1030.573809	15.074970
21.390522	1027.484350	15.079987
21.442986	1027.850096	15.085005
21.290168	1040.604959	15.090023
21.383072	1055.397427	15.095040
21.921959	1053.232307	15.100058
21.607996	1061.009691	15.105075
22.004222	1068.821444	15.110093
21.854309	1074.778022	15.115111
22.060502	1059.896710	15.120128
21.907238	1069.973404	15.125146
22.025916	1073.982018	15.130163
22.008413	1064.892302	15.135181
21.958495	1066.428118	15.140199
22.062842	1060.529158	15.145216
21.890058	1049.715216	15.150234
21.685913	1059.747968	15.155251
22.031237	1060.041993	15.160269
21.437674	1076.228036	15.165287
21.656938	1071.086399	15.170304
21.822439	1074.418775	15.175322
21.735425	1075.785936	15.180339
21.975327	1060.775423	15.185357
21.763448	1069.910670	15.190375
21.864076	1064.055630	15.195392
22.263314	1069.221687	15.200410
22.427824	1090.985202	15.205427
21.977820	1071.718174	15.210445
21.773316	1074.148460	15.215463
21.717370	1085.457833	15.220480
22.349652	1093.823407	15.225498
21.898585	1090.699010	15.230515
22.097392	1081.738028	15.235533
22.288215	1088.708632	15.240551
22.171532	1093.345577	15.245568
22.638679	1087.130240	15.250586
22.295790	1097.368662	15.255603
22.677496	1096.360242	15.260621
22.315688	1093.581684	15.265639
22.195398	1091.866253	15.270656
22.470328	1088.623608	15.275674
22.105126	1094.661904	15.280691
22.389498	1083.660037	15.285709
22.594448	1104.840119	15.290727
22.452214	1116.409859	15.295744
23.094154	1114.299712	15.300762
22.820422	1105.834669	15.305779
23.019767	1089.352144	15.310797
22.827121	1091.382843	15.315815
22.817099	1087.567321	15.320832
23.046899	1079.881094	15.325850
22.753838	1096.070546	15.330867
22.906534	1081.756324	15.335885
22.795315	1087.535638	15.340903
22.539471	1085.825331	15.345920
22.748125	1079.035101	15.350938
22.477533	1089.769407	15.355955
22.899819	1081.895011	15.360973
22.726613	1088.487323	15.365991
22.727669	1098.551080	15.371008
22.754773	1091.347612	15.376026
22.305899	1104.701535	15.381043
22.816807	1103.249684	15.386061
22.777785	1121.815536	15.391079
22.722806	1114.409120	15.396096
23.184715	1111.980762	15.401114
23.036229	1117.690669	15.406131
23.132159	1116.240605	15.411149
23.109002	1119.871547	15.416167
22.966918	1123.866267	15.421184
22.986841	1115.884470	15.426202
23.007354	1123.617129	15.431219
23.219966	1119.454112	15.436237
23.011812	1114.477722	15.441255
22.937253	1120.288772	15.446272
23.239379	1117.525857	15.451290
23.344831	1120.653625	15.456307
23.332454	1125.198113	15.461325
23.398358	1121.011752	15.466343
23.245780	1122.220880	15.471360
23.631792	1111.657270	15.476378
23.136124	1114.139713	15.481395
23.595550	1107.170154	15.486413
23.239759	1117.470567	15.491431
22.918169	1114.282206	15.496448
23.409298	1133.379167	15.501466
23.494743	1141.746343	15.506483
23.761610	1144.335589	15.511501
23.741498	1146.386543	15.516519
23.842875	1152.814519	15.521536
23.767390	1141.981646	15.526554
23.445379	1126.494051	15.531571
23.637369	1123.711184	15.536589
23.769147	1123.843725	15.541607
23.574130	1130.264474	15.546624
23.531946	1127.107795	15.551642
23.871405	1139.328873	15.556659
23.945547	1143.901559	15.561677
23.774606	1135.562782	15.566695
23.682888	1122.495264	15.571712
23.897236	1124.965648	15.576730
23.737236	1139.975267	15.581747
23.806923	1138.521673	15.586765
23.566673	1141.129932	15.591783
23.664341	1141.838974	15.596800
24.039907	1139.757578	15.601818
23.524258	1138.175323	15.606835
23.415145	1144.438550	15.611853
23.794820	1138.524677	15.616871
23.505726	1138.960763	15.621888
23.910146	1148.578242	15.626906
23.838547	1169.708145	15.631923
24.116476	1170.230256	15.636941
24.200238	1169.010150	15.641959
24.152593	1165.824447	15.646976
24.600172	1174.572610	15.651994
24.355115	1177.116712	15.657011
24.578231	1162.151793	15.662029
24.196808	1141.973736	15.667047
23.837134	1142.983306	15.672064
24.463339	1143.959938	15.677082
24.596966	1144.326420	15.682099
23.949257	1148.632426	15.687117
24.219018	1140.128942	15.692135
24.118627	1165.914676	15.697152
24.380232	1167.374902	15.702170
24.578530	1167.814926	15.707187
24.556174	1169.432012	15.712205
24.432272	1162.006278	15.717223
24.393786	1177.204075	15.722240
24.382104	1167.440516	15.727258
24.094700	1162.438258	15.732275
24.332258	1160.567109	15.737293
24.568861	1165.891622	15.742311
24.646667	1164.593764	15.747328
24.548979	1169.354749	15.752346
24.708878	1168.085422	15.757363
24.535035	1160.627801	15.762381
24.917242	1162.381829	15.767399
24.220055	1165.791722	15.772416
24.511529	1168.949720	15.777434
24.793736	1161.872871	15.782451
24.445750	1165.615483	15.787469
24.598841	1166.834235	15.792487
24.595137	1190.019412	15.797504
25.010060	1187.400008	15.802522
25.038267	1190.662233	15.807539
25.099818	1194.988992	15.812557
25.034178	1186.008356	15.817575
24.751066	1192.709066	15.822592
25.231285	1190.494195	15.827610
25.083586	1189.738783	15.832627
25.363645	1193.903379	15.837645
25.489379	1192.815688	15.842663
24.965191	1181.166554	15.847680
24.997192	1167.023024	15.852698
24.946218	1176.545459	15.857715
24.801267	1182.328032	15.862733
25.176165	1186.852110	15.867751
24.977450	1191.206218	15.872768
25.312195	1188.534344	15.877786
24.943053	1193.185171	15.882803
24.898315	1186.872670	15.887821
25.352805	1197.609818	15.892839
24.867015	1200.448504	15.897856
25.166871	1188.832595	15.902874
25.392623	1187.601573	15.907891
25.369289	1189.423544	15.912909
25.357176	1190.533042	15.917927
24.940792	1199.368377	15.922944
24.966824	1196.982262	15.927962
25.488394	1219.155720	15.932979
25.173325	1217.579218	15.937997
25.747124	1220.668036	15.943015
25.432580	1222.287449	15.948032
25.375856	1222.794899	15.953050
25.478115	1220.541824	15.958067
25.632601	1216.296282	15.963085
25.836050	1215.799646	15.968103
25.184468	1225.486524	15.973120
25.689341	1215.305516	15.978138
25.636527	1228.095547	15.983155
25.545615	1216.041184	15.988173
25.954924	1215.223851	15.993191
25.546562	1227.233402	15.998208
26.025931	1225.511177	16.003226
25.795119	1218.766886	16.008243
25.833769	1227.926881	16.013261
26.217455	1232.714080	16.018279
25.774102	1240.564946	16.023296
26.109339	1237.947706	16.028314
26.037149	1237.452617	16.033331
25.558219	1243.630273	16.038349
26.049113	1246.806445	16.043367
26.276453	1255.150186	16.048384
26.283957	1244.423576	16.053402
26.442027	1236.664112	16.058419
25.984811	1234.056048	16.063437
26.341671	1227.744352	16.068455
26.123742	1249.550945	16.073472
26.325001	1240.555215	16.078490
26.468213	1231.830515	16.083507
26.358559	1238.271818	16.088525
26.279732	1217.329002	16.093543
26.030535	1222.787126	16.098560
26.361317	1241.295429	16.103578
26.634026	1237.595255	16.108595
26.362932	1245.406576	16.113613
26.593793	1242.985355	16.118631
26.576513	1239.308003	16.123648
26.556151	1216.981910	16.128666
26.452469	1213.734217	16.133683
26.060213	1220.025068	16.138701
26.395572	1220.258149	16.143719
26.324796	1233.752720	16.148736
26.340299	1241.571306	16.153754
26.718018	1242.624130	16.158771
26.612522	1242.444788	16.163789
26.746570	1240.099440	16.168807
26.697694	1247.560585	16.173824
26.697794	1243.102809	16.178842
26.888196	1245.607492	16.183859
26.562906	1246.896015	16.188877
26.800779	1242.635871	16.193895
26.566570	1244.389618	16.198912
26.512534	1239.706166	16.203930
26.557595	1241.548313	16.208947
26.547378	1243.937399	16.213965
26.952357	1247.608498	16.218983
26.965641	1268.211497	16.224000
27.255745	1273.611832	16.229018
27.118366	1264.404845	16.234035
27.002258	1263.535144	16.239053
27.291518	1252.965413	16.244071
27.206705	1244.925302	16.249088
27.150929	1240.321270	16.254106
27.219940	1233.027334	16.259123
27.130835	1239.634130	16.264141
26.861390	1236.802063	16.269159
27.558362	1247.319962	16.274176
27.344584	1246.384154	16.279194
27.453411	1243.763853	16.284211
27.033792	1240.243279	16.289229
27.058589	1229.668537	16.294247
26.903922	1257.833839	16.299264
27.037912	1266.756026	16.304282
27.101842	1266.841538	16.309299
27.196693	1275.334785	16.314317
27.654938	1270.968065	16.319335
26.825006	1276.175131	16.324352
26.969937	1280.658577	16.329370
27.226617	1279.365736	16.334387
27.354916	1292.119924	16.339405
27.793401	1294.376845	16.344423
27.634711	1295.738571	16.349440
27.758433	1301.532210	16.354458
27.849624	1292.893254	16.359475
27.602818	1297.441178	16.364493
28.289343	1288.976082	16.369511
28.004805	1285.211479	16.374528
27.841451	1283.577172	16.379546
27.587470	1271.047807	16.384563
27.926658	1287.203630	16.389581
28.030109	1286.340879	16.394599
27.858272	1292.129125	16.399616
27.898034	1299.925613	16.404634
28.383045	1295.255639	16.409651
27.729064	1276.780388	16.414669
27.712864	1268.431271	16.419687
27.930446	1285.494615	16.424704
27.912138	1285.769332	16.429722
27.989204	1289.267577	16.434739
27.831419	1291.014974	16.439757
28.140520	1291.909876	16.444775
28.354749	1289.777224	16.449792
28.239145	1291.815664	16.454810
28.577941	1275.667718	16.459827
28.098182	1289.000536	16.464845
28.279190	1278.751069	16.469863
28.261648	1286.009410	16.474880
27.949587	1290.568532	16.479898
28.068762	1277.219509	16.484915
28.043719	1281.630316	16.489933
28.154780	1284.249716	16.494951
28.233629	1294.790475	16.499968
28.359724	1305.613965	16.504986
28.777581	1314.054930	16.510003
28.464819	1315.841377	16.515021
28.386649	1317.698820	16.520039
28.720466	1323.948223	16.525056
28.556810	1326.443831	16.530074
28.668145	1320.823140	16.535091
28.386991	1322.791753	16.540109
28.639507	1316.791391	16.545127
28.883411	1319.207306	16.550144
28.695155	1320.007009	16.555162
28.911128	1303.096706	16.560179
28.732281	1321.899333	16.565197
28.625683	1312.847847	16.570215
28.883683	1317.544468	16.575232
28.845381	1319.843730	16.580250
29.135531	1310.806469	16.585267
28.881960	1321.767640	16.590285
28.919138	1314.474213	16.595303
28.781073	1311.892814	16.600320
28.700938	1318.963506	16.605338
29.162782	1311.066697	16.610355
28.980197	1319.563390	16.615373
28.926613	1307.165771	16.620391
29.120832	1312.037123	16.625408
28.890710	1310.148518	16.630426
28.963734	1313.225003	16.635443
29.075082	1313.334158	16.640461
29.031356	1311.713896	16.645479
29.301710	1313.344733	16.650496
29.003200	1320.686228	16.655514
29.395925	1327.122333	16.660531
29.282832	1338.131513	16.665549
29.605990	1338.014259	16.670567
29.671663	1336.258559	16.675584
29.740555	1337.290087	16.680602
29.686225	1319.155249	16.685619
29.326422	1314.913739	16.690637
29.486447	1308.189729	16.695655
29.579658	1307.990474	16.700672
29.373725	1307.142731	16.705690
29.612129	1320.768856	16.710707
29.920007	1332.465796	16.715725
29.678557	1331.289292	16.720743
29.732670	1322.612365	16.725760
29.847839	1336.736857	16.730778
30.077170	1317.636163	16.735795
29.531535	1316.102161	16.740813
29.662051	1319.591168	16.745831
29.753729	1329.220783	16.750848
29.844131	1344.139137	16.755866
30.145244	1338.296466	16.760883
30.184056	1343.539620	16.765901
29.870335	1343.261293	16.770919
30.245885	1336.113398	16.775936
30.030857	1327.323556	16.780954
29.979314	1310.557147	16.785971
30.119250	1320.057114	16.790989
29.998605	1332.126188	16.796007
30.391101	1330.767153	16.801024
29.741754	1341.034039	16.806042
29.947950	1343.091640	16.811059
29.829972	1338.502603	16.816077
30.056581	1338.060395	16.821095
30.497094	1333.102113	16.826112
30.113988	1349.471696	16.831130
30.140169	1333.606162	16.836147
29.969907	1343.392938	16.841165
30.333433	1340.091083	16.846183
30.250263	1333.870319	16.851200
30.159048	1346.227834	16.856218
30.196396	1363.112056	16.861235
30.270714	1375.249273	16.866253
30.444597	1370.207966	16.871271
30.334912	1368.225789	16.876288
30.552550	1371.633848	16.881306
30.984761	1363.765541	16.886323
30.582199	1364.892855	16.891341
30.908489	1365.145945	16.896359
30.827482	1365.229866	16.901376
30.712261	1361.254926	16.906394
30.904864	1359.953397	16.911411
30.907883	1371.515022	16.916429
30.798570	1370.087109	16.921447
30.770413	1367.237505	16.926464
30.636785	1372.465128	16.931482
31.050297	1358.590530	16.936499
30.610210	1362.113009	16.941517
31.071041	1368.696119	16.946535
30.878008	1359.479786	16.951552
31.089972	1363.500194	16.956570
31.179454	1363.842102	16.961587
30.816468	1361.861712	16.966605
30.704918	1361.108967	16.971623
30.954733	1362.240853	16.976640
31.143419	1371.983957	16.981658
31.255534	1385.627508	16.986675
31.002133	1379.079011	16.991693
31.096292	1383.992545	16.996711
31.618796	1382.898983	17.001728
31.418679	1388.887222	17.006746
31.668946	1382.149024	17.011763
31.660701	1387.459040	17.016781
31.357034	1385.838507	17.021799
31.461747	1377.317342	17.026816
31.068349	1385.480084	17.031834
31.378994	1371.906364	17.036851
31.543053	1377.758706	17.041869
31.481021	1380.876465	17.046887
31.715446	1375.301513	17.051904
31.778221	1386.881601	17.056922
31.697708	1376.313961	17.061939
31.720559	1376.194465	17.066957
31.358936	1382.369679	17.071975
31.519881	1387.190266	17.076992
31.487274	1382.776842	17.082010
31.464192	1378.146883	17.087027
31.506831	1386.216952	17.092045
31.601708	1403.778300	17.097063
32.124063	1408.024092	17.102080
32.149393	1408.780164	17.107098
32.202095	1411.664366	17.112115
32.310084	1419.900795	17.117133
32.031462	1419.141853	17.122151
32.239715	1402.594529	17.127168
32.035578	1410.519254	17.132186
32.016220	1414.141761	17.137203
31.935559	1404.118611	17.142221
31.619107	1409.409984	17.147239
32.101073	1408.251481	17.152256
31.993340	1407.943373	17.157274
32.273423	1405.221460	17.162291
32.264869	1400.458381	17.167309
32.212301	1400.895464	17.172327
32.425285	1403.531866	17.177344
32.550764	1418.808654	17.182362
32.393212	1415.724168	17.187379
32.645855	1417.844954	17.192397
32.482464	1429.036935	17.197415
32.738562	1425.923323	17.202432
32.622423	1432.281922	17.207450
32.673112	1418.252784	17.212467
32.701729	1404.924552	17.217485
32.534153	1400.577566	17.222503
32.380265	1410.626631	17.227520
32.456709	1416.030113	17.232538
32.590133	1431.405991	17.237555
32.880874	1431.224026	17.242573
33.050168	1425.153939	17.247591
33.374317	1423.387319	17.252608
33.187550	1423.999379	17.257626
33.006851	1423.084066	17.262643
33.068038	1417.744870	17.267661
33.125702	1411.833822	17.272679
33.026607	1392.526792	17.277696
32.809284	1401.265106	17.282714
32.642093	1407.034515	17.287731
33.181624	1411.931790	17.292749
32.842048	1416.960068	17.297767
33.118386	1420.394244	17.302784
33.083337	1424.791001	17.307802
33.286966	1419.084913	17.312819
33.573092	1418.550566	17.317837
33.000385	1422.082419	17.322855
33.499807	1420.993464	17.327872
33.187651	1422.327857	17.332890
33.200574	1421.439145	17.337907
33.356021	1417.024099	17.342925
33.258488	1417.390282	17.347943
33.309131	1414.132347	17.352960
33.576873	1434.265483	17.357978
33.741765	1443.969659	17.362995
33.901857	1450.086858	17.368013
33.716004	1444.680292	17.373031
34.009678	1424.565274	17.378048
33.763546	1426.001727	17.383066
33.571175	1419.132478	17.388083
33.560466	1414.919748	17.393101
33.657761	1436.964562	17.398119
34.073546	1444.731930	17.403136
33.900763	1442.203109	17.408154
33.810823	1451.029019	17.413171
33.758462	1446.678689	17.418189
33.839384	1453.123563	17.423207
34.099408	1453.648257	17.428224
34.193200	1445.224139	17.433242
33.859661	1448.610096	17.438259
34.065354	1441.533980	17.443277
34.070594	1451.807902	17.448295
34.329790	1430.587568	17.453312
34.293129	1447.648703	17.458330
34.026775	1446.503084	17.463347
34.266964	1440.347237	17.468365
34.182363	1445.873852	17.473383
34.224052	1437.336712	17.478400
34.240462	1442.664318	17.483418
34.133418	1437.955725	17.488435
34.261801	1437.973084	17.493453
33.883351	1458.456951	17.498471
34.671000	1462.435208	17.503488
34.909271	1476.115036	17.508506
34.358134	1477.943728	17.513523
34.607479	1472.927687	17.518541
34.357168	1475.105778	17.523559
34.518564	1470.941700	17.528576
34.533294	1469.710954	17.533594
34.681994	1461.945449	17.538611
34.853434	1459.014746	17.543629
34.401356	1471.746681	17.548647
34.970413	1468.810372	17.553664
35.320341	1466.800896	17.558682
34.907047	1469.001249	17.563699
35.099205	1459.596666	17.568717
34.950477	1469.489797	17.573735
34.903347	1460.089402	17.578752
34.860716	1475.494082	17.583770
35.040642	1472.643861	17.588787
35.072447	1466.464240	17.593805
34.694579	1472.965801	17.598823
34.855230	1482.868341	17.603840
35.166800	1493.458102	17.608858
34.873060	1504.417391	17.613875
35.396912	1502.896828	17.618893
35.178849	1497.736915	17.623911
35.443602	1488.703757	17.628928
35.425004	1491.652929	17.633946
35.602203	1493.574407	17.638963
35.496908	1490.046215	17.643981
35.533128	1489.157184	17.648999
35.533500	1481.252452	17.654016
35.619972	1484.559420	17.659034
35.499870	1486.538394	17.664051
35.698803	1483.319669	17.669069
35.768752	1481.476237	17.674087
35.902328	1475.064801	17.679104
35.685903	1481.478609	17.684122
35.414774	1482.614088	17.689139
35.542369	1474.883568	17.694157
35.577322	1489.488803	17.699175
35.662143	1476.931910	17.704192
35.887135	1500.831256	17.709210
36.128348	1513.570867	17.714227
36.191923	1505.253294	17.719245
36.242636	1508.279969	17.724263
36.168518	1492.811982	17.729280
36.386744	1492.465254	17.734298
36.332677	1484.947879	17.739315
36.356889	1484.683670	17.744333
35.945774	1481.182497	17.749351
36.332883	1482.894413	17.754368
36.328611	1477.714460	17.759386
36.154030	1480.140642	17.764403
36.087816	1476.175274	17.769421
36.183444	1494.359434	17.774439
36.485145	1502.018163	17.779456
36.443670	1507.206557	17.784474
36.309610	1515.158707	17.789491
36.442815	1499.408352	17.794509
36.240331	1503.545061	17.799527
36.460414	1503.738181	17.804544
36.725418	1505.348665	17.809562
36.443453	1506.448932	17.814579
36.870148	1500.251942	17.819597
36.499674	1501.772769	17.824615
36.416441	1505.066505	17.829632
36.679937	1500.495355	17.834650
36.343971	1511.063610	17.839667
36.767031	1523.789654	17.844685
36.763508	1537.278077	17.849703
36.571622	1536.057522	17.854720
36.755229	1536.097234	17.859738
36.875198	1546.630175	17.864755
37.107581	1536.975182	17.869773
36.902989	1540.629966	17.874791
37.005511	1539.265779	17.879808
37.523379	1535.161555	17.884826
36.684390	1542.359972	17.889843
37.113557	1537.369252	17.894861
37.199623	1556.627117	17.899879
37.449266	1566.018911	17.904896
37.656631	1560.249949	17.909914
37.453838	1550.317399	17.914931
37.632731	1540.092521	17.919949
37.516207	1533.133891	17.924967
37.606632	1533.966986	17.929984
37.165041	1522.173994	17.935002
37.368775	1535.002506	17.940019
37.399006	1550.055825	17.945037
37.259097	1554.890455	17.950055
37.702099	1564.875823	17.955072
38.236489	1561.935789	17.960090
37.921303	1556.667922	17.965107
37.705597	1549.849330	17.970125
37.785964	1556.339615	17.975143
37.647986	1551.699889	17.980160
37.977684	1551.281551	17.985178
37.824907	1553.891141	17.990195
37.745747	1551.331838	17.995213
37.973793	1556.234281	18.000231
38.032964	1553.633174	18.005248
38.070552	1556.421874	18.010266
38.090977	1554.387814	18.015283
38.151035	1552.040105	18.020301
38.305766	1550.953493	18.025319
38.181479	1558.790662	18.030336
38.397336	1542.391930	18.035354
37.826777	1553.824257	18.040371
38.207189	1547.003415	18.045389
38.235454	1548.904286	18.050407
38.287713	1563.004755	18.055424
38.177161	1571.752257	18.060442
38.430131	1579.300983	18.065459
38.506113	1579.978203	18.070477
38.510447	1581.562173	18.075495
38.545337	1579.973748	18.080512
38.628146	1574.459264	18.085530
38.696799	1581.449138	18.090547
38.632715	1586.872406	18.095565
38.435212	1580.264567	18.100583
38.734923	1582.318526	18.105600
38.697677	1570.236890	18.110618
38.722934	1581.966644	18.115635
38.591508	1571.710451	18.120653
38.882815	1587.776092	18.125671
39.002891	1604.059474	18.130688
39.560371	1602.077819	18.135706
39.334363	1593.934528	18.140723
39.188150	1580.688245	18.145741
39.204287	1582.915932	18.150759
38.920135	1579.976393	18.155776
39.169276	1584.703304	18.160794
39.221938	1595.477738	18.165811
39.368315	1609.126443	18.170829
39.633661	1605.593546	18.175847
39.540111	1605.030722	18.180864
39.578080	1580.089708	18.185882
39.333055	1583.510644	18.190899
39.373153	1582.656005	18.195917
39.429693	1586.437246	18.200935
39.605340	1604.931121	18.205952
39.698319	1597.744857	18.210970
39.722338	1596.655084	18.215987
39.740949	1601.523716	18.221005
39.495649	1603.923830	18.226023
39.746900	1601.462171	18.231040
39.927770	1594.153874	18.236058
39.688761	1600.598636	18.241075
39.432659	1599.080440	18.246093
39.576216	1596.077950	18.251111
39.810462	1604.528612	18.256128
39.703059	1594.927091	18.261146
39.423036	1596.911298	18.266163
39.657856	1612.157180	18.271181
39.987331	1629.651198	18.276199
39.691545	1638.108540	18.281216
39.820342	1637.185668	18.286234
39.809749	1629.762600	18.291251
39.703265	1629.311367	18.296269
39.955751	1640.471645	18.301287
39.885915	1650.456159	18.306304
40.700641	1656.895755	18.311322
40.155465	1654.933683	18.316339
40.546612	1654.376427	18.321357
40.761555	1655.977893	18.326375
40.869740	1656.578131	18.331392
41.285371	1644.481685	18.336410
40.981351	1647.521849	18.341427
41.113412	1636.384969	18.346445
41.111970	1614.457536	18.351463
40.676822	1615.726483	18.356480
40.964661	1601.914605	18.361498
41.022703	1605.017644	18.366515
40.788993	1614.451315	18.371533
40.964053	1609.239655	18.376551
40.915118	1615.188774	18.381568
41.121039	1614.009036	18.386586
41.062469	1613.312860	18.391603
41.120073	1608.455691	18.396621
41.295029	1605.318078	18.401639
40.943869	1613.020004	18.406656
41.216368	1607.916227	18.411674
41.067560	1615.528743	18.416691
41.257493	1610.782340	18.421709
41.152336	1611.671840	18.426727
41.094160	1626.671368	18.431744
41.400055	1622.236864	18.436762
41.346138	1629.025401	18.441779
41.650805	1634.758889	18.446797
41.816995	1633.404624	18.451815
41.652162	1643.575338	18.456832
41.808459	1633.570677	18.461850
41.925336	1631.225752	18.466867
41.924359	1615.780177	18.471885
41.418907	1608.250083	18.476903
41.076894	1620.779267	18.481920
41.219842	1621.577685	18.486938
41.661867	1624.594312	18.491955
41.403458	1639.345116	18.496973
42.022090	1632.726920	18.501991
41.532471	1635.547418	18.507008
42.014310	1646.761852	18.512026
41.932054	1669.974139	18.517043
41.981996	1676.246675	18.522061
42.024891	1665.565095	18.527079
41.938591	1677.814579	18.532096
42.352565	1674.460207	18.537114
42.344086	1676.930176	18.542131
42.318543	1670.915483	18.547149
42.329562	1667.801853	18.552167
42.434592	1666.795512	18.557184
42.442383	1665.057627	18.562202
42.311019	1662.371121	18.567219
42.512544	1666.736254	18.572237
42.838711	1658.905044	18.577255
42.337583	1663.026678	18.582272
42.731973	1654.207787	18.587290
42.606990	1661.018342	18.592307
42.528568	1664.366039	18.597325
42.741681	1658.362228	18.602343
42.769628	1658.189131	18.607360
42.829909	1656.783503	18.612378
42.864180	1665.877553	18.617395
42.898804	1664.054122	18.622413
42.854180	1657.879994	18.627431
42.811781	1655.521675	18.632448
42.860645	1657.358911	18.637466
43.212734	1659.127041	18.642483
42.901781	1654.298994	18.647501
42.958516	1656.508159	18.652519
43.025757	1667.716848	18.657536
43.357309	1680.477859	18.662554
43.507489	1679.265220	18.667571
43.277332	1689.700326	18.672589
43.758422	1674.425267	18.677607
43.648156	1682.415295	18.682624
43.614108	1665.166861	18.687642
43.561880	1657.575475	18.692659
43.287037	1656.652901	18.697677
43.644315	1662.061543	18.702695
43.600538	1673.769332	18.707712
43.540174	1676.108914	18.712730
43.386369	1677.074978	18.717747
43.614502	1674.828948	18.722765
43.654049	1674.491330	18.727783
43.376225	1681.917758	18.732800
43.419071	1681.054391	18.737818
43.679110	1690.043748	18.742835
43.587714	1694.358965	18.747853
44.054124	1704.203145	18.752871
44.214190	1714.048450	18.757888
44.112893	1706.850997	18.762906
44.174975	1713.898319	18.767923
43.781672	1720.436002	18.772941
44.458214	1707.068337	18.777959
44.198707	1705.429039	18.782976
44.318468	1707.181706	18.787994
44.449816	1707.350546	18.793011
44.267967	1707.679121	18.798029
44.547318	1706.097055	18.803047
44.250644	1707.421821	18.808064
44.209407	1714.484283	18.813082
44.446783	1703.345666	18.818099
44.435064	1706.413426	18.823117
44.651743	1707.788230	18.828135
44.706486	1722.281352	18.833152
44.975810	1721.037564	18.838170
45.268982	1718.802019	18.843187
44.935135	1718.308114	18.848205
45.130369	1697.710219	18.853223
44.910576	1701.381729	18.858240
44.729017	1700.313390	18.863258
44.833878	1703.239404	18.868275
44.786941	1709.832724	18.873293
45.081981	1713.391037	18.878311
45.133928	1718.224264	18.883328
45.135260	1725.474960	18.888346
45.144464	1715.048534	18.893363
45.083931	1719.240929	18.898381
45.223815	1718.617008	18.903399
44.815908	1723.958669	18.908416
45.153581	1719.144463	18.913434
45.312611	1725.449744	18.918451
45.379419	1750.094968	18.923469
45.481080	1744.293047	18.928487
45.300798	1747.836371	18.933504
45.580522	1751.442111	18.938522
45.854025	1743.549894	18.943539
45.236285	1751.360597	18.948557
45.820274	1749.975726	18.953575
45.606191	1756.175082	18.958592
45.681063	1744.802709	18.963610
46.221879	1740.469039	18.968627
45.827571	1740.057193	18.973645
45.647742	1740.677958	18.978663
45.823764	1738.649213	18.983680
45.880213	1752.155058	18.988698
46.309792	1756.638362	18.993715
46.516115	1777.541182	18.998733
46.114243	1754.726295	19.003751
45.934233	1758.656197	19.008768
46.260752	1764.835728	19.013786
46.445424	1771.902149	19.018803
46.207633	1765.465470	19.023821
46.710586	1770.744909	19.028839
46.245279	1772.965333	19.033856
46.435958	1772.049530	19.038874
46.404622	1762.032547	19.043891
46.160241	1763.824256	19.048909
46.489001	1769.483331	19.053927
46.410095	1769.249184	19.058944
46.300045	1788.568945	19.063962
46.482954	1789.841866	19.068979
46.568905	1798.580580	19.073997
46.662440	1801.737232	19.079015
46.553176	1795.109177	19.084032
46.554175	1802.704853	19.089050
46.443240	1804.518960	19.094067
46.938333	1812.125742	19.099085
47.334495	1823.319057	19.104103
47.408410	1820.106397	19.109120
47.682632	1828.858443	19.114138
47.788924	1812.848443	19.119155
47.659513	1820.133037	19.124173
47.610561	1793.519033	19.129191
47.551289	1791.806805	19.134208
47.493485	1784.676132	19.139226
47.593401	1775.130329	19.144243
47.450031	1783.120379	19.149261
47.900548	1779.685130	19.154279
47.660929	1788.153726	19.159296
47.904068	1792.411608	19.164314
47.718868	1790.784407	19.169331
47.748900	1792.405876	19.174349
47.858365	1796.663845	19.179367
48.201704	1803.241402	19.184384
47.957893	1807.679133	19.189402
48.128938	1790.831252	19.194419
47.937471	1787.838530	19.199437
48.174511	1792.550973	19.204455
48.141722	1796.874624	19.209472
48.014783	1812.392026	19.214490
48.527595	1807.214928	19.219507
48.180524	1816.045825	19.224525
48.185924	1811.064163	19.229543
48.599564	1805.205049	19.234560
48.076342	1809.074074	19.239578
48.175291	1807.223439	19.244595
47.962231	1818.258567	19.249613
48.386224	1808.372464	19.254631
48.500651	1813.898144	19.259648
48.341358	1807.200021	19.264666
48.670549	1808.539668	19.269683
48.430630	1828.642020	19.274701
48.756385	1838.223350	19.279719
48.403780	1841.382622	19.284736
48.646785	1847.280733	19.289754
48.635618	1834.816612	19.294771
48.784558	1839.962170	19.299789
48.939500	1843.840174	19.304807
48.782039	1841.072917	19.309824
48.965113	1836.509475	19.314842
49.153527	1833.438881	19.319859
49.224939	1850.311694	19.324877
48.973703	1855.775493	19.329895
49.433419	1863.484617	19.334912
49.346763	1881.380116	19.339930
49.846213	1861.792285	19.344947
49.385645	1862.250087	19.349965
49.498432	1868.346544	19.354983
49.625436	1858.971012	19.360000
49.734549	1860.569551	19.365018
49.912470	1851.196617	19.370035
49.960207	1846.439435	19.375053
49.756190	1859.262896	19.380071
50.027077	1844.642963	19.385088
49.815010	1861.995807	19.390106
49.895370	1857.644253	19.395123
49.632482	1856.163375	19.400141
49.887165	1852.037294	19.405159
49.770146	1855.718989	19.410176
49.881745	1865.210990	19.415194
49.964547	1849.014287	19.420211
49.992268	1854.936630	19.425229
50.035601	1854.934215	19.430247
50.200811	1852.841496	19.435264
49.776227	1859.633240	19.440282
50.299200	1877.243928	19.445299
50.123612	1889.641044	19.450317
50.456735	1888.382742	19.455335
50.466271	1891.988371	19.460352
50.507976	1886.307351	19.465370
50.709663	1889.643361	19.470387
50.552508	1882.896425	19.475405
50.513389	1886.427430	19.480423
50.850013	1884.338214	19.485440
50.599825	1892.042850	19.490458
50.677122	1895.207722	19.495475
50.882502	1906.047245	19.500493
50.905348	1906.258857	19.505511
51.329778	1909.778075	19.510528
50.829340	1915.212683	19.515546
51.395336	1906.296337	19.520563
51.231906	1913.207859	19.525581
51.388568	1918.477364	19.530599
51.397774	1906.451556	19.535616
51.551192	1909.129012	19.540634
51.634402	1904.932881	19.545651
51.579962	1898.293736	19.550669
51.616587	1909.413179	19.555687
51.673305	1894.243214	19.560704
51.694400	1910.045264	19.565722
51.755919	1898.782078	19.570739
51.888353	1898.113713	19.575757
51.631757	1903.704797	19.580775
51.911116	1899.414377	19.585792
51.950731	1897.858603	19.590810
51.859579	1900.041501	19.595827
51.607309	1901.794373	19.600845
51.551261	1897.270901	19.605863
51.576126	1905.124886	19.610880
51.622249	1906.167704	19.615898
52.027602	1913.994520	19.620915
52.209358	1931.879098	19.625933
51.981207	1928.234924	19.630951
52.231618	1927.873015	19.635968
52.192062	1930.308011	19.640986
52.643730	1929.779703	19.646003
52.497705	1937.153720	19.651021
52.047104	1934.319627	19.656039
52.237010	1929.632189	19.661056
52.189355	1926.129787	19.666074
52.133231	1930.666400	19.671091
52.992719	1941.892535	19.676109
52.776275	1954.850025	19.681127
53.049181	1953.630037	19.686144
53.150549	1948.439916	19.691162
53.075633	1958.127035	19.696179
53.422356	1954.960124	19.701197
52.826966	1940.527636	19.706215
52.668133	1930.887571	19.711232
53.077750	1948.072609	19.716250
53.210879	1945.713529	19.721267
53.450258	1953.442647	19.726285
53.100889	1950.565016	19.731303
53.730448	1939.275463	19.736320
53.155549	1952.895472	19.741338
53.409244	1945.802124	19.746355
53.480332	1944.161604	19.751373
53.699679	1943.587510	19.756391
53.618555	1942.715127	19.761408
53.629470	1944.231113	19.766426
53.798287	1944.985107	19.771443
53.846156	1934.597408	19.776461
53.501516	1942.923630	19.781479
53.791388	1943.313475	19.786496
53.765326	1938.241705	19.791514
53.614662	1937.787147	19.796531
53.931755	1961.146348	19.801549
54.037076	1966.259406	19.806567
54.310825	1961.209641	19.811584
54.024164	1973.853567	19.816602
54.359712	1970.529050	19.821619
54.088978	1971.020777	19.826637
54.164910	1975.617823	19.831655
54.550269	1971.259831	19.836672
54.630417	1968.990624	19.841690
54.282158	1971.296028	19.846707
54.343880	1965.317954	19.851725
54.095830	1968.657582	19.856743
54.630071	1980.237216	19.861760
54.455323	1996.786369	19.866778
54.690327	2003.000048	19.871795
54.876572	1990.606267	19.876813
54.627368	1988.506950	19.881831
54.582333	1986.303746	19.886848
54.768501	1989.999446	19.891866
54.706662	1985.464308	19.896883
54.968008	2004.001165	19.901901
54.949661	2009.760324	19.906919
55.303630	2015.268068	19.911936
55.410518	2021.362018	19.916954
55.380890	2019.136572	19.921971
55.376545	2014.384419	19.926989
55.557640	2020.816881	19.932007
56.094614	2009.573711	19.937024
55.753226	2022.070041	19.942042
55.745289	2005.827567	19.947059
55.997704	2008.028398	19.952077
55.761338	1996.695958	19.957095
55.600323	1984.928596	19.962112
55.650563	1992.673696	19.967130
55.947969	2004.016570	19.972147
55.960994	2009.204769	19.977165
55.736182	2009.919610	19.982183
55.568089	2016.702417	19.987200
56.043997	2007.093822	19.992218
55.979410	2008.957366	19.997235
55.907982	2009.685393	20.002253
55.880761	2017.390180	20.007271
56.398122	2010.466144	20.012288
56.167359	2019.396799	20.017306
56.128564	2032.019417	20.022323
56.340940	2037.380922	20.027341
56.095575	2038.404689	20.032359
56.650715	2043.088555	20.037376
56.592707	2049.519673	20.042394
56.786672	2040.766037	20.047411
56.508956	2044.004684	20.052429
56.720440	2045.446523	20.057447
56.649869	2041.360468	20.062464
57.037170	2037.741924	20.067482
57.076505	2041.884405	20.072499
57.220479	2033.320946	20.077517
56.985539	2041.390072	20.082535
57.190374	2039.808501	20.087552
57.314653	2056.774363	20.092570
57.135939	2061.756524	20.097587
57.894508	2067.948893	20.102605
57.138692	2058.233969	20.107623
57.770913	2054.274858	20.112640
57.488315	2061.713280	20.117658
57.419870	2062.553024	20.122675
57.555815	2057.369741	20.127693
57.480162	2063.699058	20.132711
57.505896	2063.209776	20.137728
57.948143	2059.564413	20.142746
57.953217	2062.264883	20.147763
58.151516	2054.616072	20.152781
57.820732	2065.734649	20.157799
58.018441	2067.445317	20.162816
57.886211	2058.224404	20.167834
57.722763	2068.669191	20.172851
57.701936	2063.649663	20.177869
57.888141	2082.469932	20.182887
57.975765	2077.661191	20.187904
57.969373	2083.039251	20.192922
58.091223	2084.516802	20.197939
57.980559	2081.275201	20.202957
57.781723	2095.820108	20.207975
58.187118	2097.216852	20.212992
58.545874	2102.829350	20.218010
58.628934	2108.769006	20.223027
59.056422	2106.565107	20.228045
58.896667	2107.897943	20.233063
58.805507	2108.491048	20.238080
59.225052	2102.189491	20.243098
59.171165	2109.243202	20.248115
59.286075	2104.305128	20.253133
59.308834	2106.246743	20.258151
59.112913	2104.072837	20.263168
59.242472	2098.024030	20.268186
59.184332	2110.724720	20.273203
59.070510	2093.737453	20.278221
59.304874	2098.854386	20.283239
59.499000	2087.146651	20.288256
59.284397	2096.027034	20.293274
59.417947	2117.636875	20.298291
59.878015	2127.731994	20.303309
59.657833	2131.645017	20.308327
59.715457	2126.447512	20.313344
60.243880	2126.103349	20.318362
59.749361	2127.960139	20.323379
59.769373	2125.438652	20.328397
59.512874	2131.825108	20.333415
60.089286	2118.511077	20.338432
60.070503	2116.305476	20.343450
60.202923	2119.662062	20.348467
60.555456	2116.020516	20.353485
60.460358	2120.021885	20.358503
60.235886	2113.181658	20.363520
60.272997	2110.471509	20.368538
59.983934	2111.085177	20.373555
60.354843	2113.784533	20.378573
60.345573	2105.471221	20.383591
60.750654	2111.825293	20.388608
60.547841	2106.033492	20.393626
60.540662	2137.682005	20.398643
60.463894	2135.796251	20.403661
60.679925	2153.997864	20.408679
60.551925	2147.310160	20.413696
60.791079	2143.574778	20.418714
60.660060	2146.413157	20.423731
61.027211	2151.134089	20.428749
61.108900	2166.342484	20.433767
61.391339	2158.046594	20.438784
61.751699	2162.836374	20.443802
61.373717	2167.824790	20.448819
61.918306	2158.968936	20.453837
61.418336	2151.506172	20.458855
61.740826	2141.791790	20.463872
61.999730	2132.895455	20.468890
61.275021	2135.924657	20.473907
61.468885	2147.140287	20.478925
61.679775	2159.715367	20.483943
61.868078	2166.578209	20.488960
61.835900	2166.617039	20.493978
61.946982	2170.995715	20.498995
62.406649	2163.817769	20.504013
62.020658	2165.604229	20.509031
61.986999	2157.503991	20.514048
61.949816	2160.813075	20.519066
61.577599	2161.058608	20.524083
61.952535	2163.732108	20.529101
62.141358	2188.337351	20.534119
62.451079	2187.428586	20.539136
62.589447	2187.365945	20.544154
62.320385	2191.693787	20.549171
62.534299	2184.992368	20.554189
62.104864	2186.310019	20.559207
62.280941	2188.536115	20.564224
62.976197	2204.591026	20.569242
62.679764	2218.281303	20.574259
63.176118	2213.346967	20.579277
63.182425	2213.061300	20.584295
63.402101	2207.695197	20.589312
63.615932	2211.184393	20.594330
63.129864	2212.203929	20.599347
63.505692	2204.904800	20.604365
63.489448	2205.241399	20.609383
63.428671	2204.363663	20.614400
63.799244	2197.998914	20.619418
63.600605	2206.643241	20.624435
63.651241	2201.810664	20.629453
63.911168	2198.877771	20.634471
63.621463	2189.433238	20.639488
63.748255	2180.871756	20.644506
63.509360	2192.525625	20.649523
63.677712	2196.712535	20.654541
63.704604	2205.013206	20.659559
63.835866	2204.856462	20.664576
63.752659	2200.103530	20.669594
63.624418	2207.355827	20.674611
63.652769	2204.340011	20.679629
64.033217	2218.476110	20.684647
63.995670	2226.968573	20.689664
64.154131	2225.218670	20.694682
64.085321	2236.031380	20.699699
64.412361	2230.931758	20.704717
64.543065	2236.573010	20.709735
64.287411	2233.521139	20.714752
64.751977	2241.294222	20.719770
64.869662	2256.916056	20.724787
64.926235	2266.093383	20.729805
64.739756	2262.861541	20.734823
64.629963	2261.489138	20.739840
64.852531	2254.777988	20.744858
65.057902	2260.066712	20.749875
65.265079	2250.959180	20.754893
65.265226	2252.019871	20.759911
65.284842	2261.919096	20.764928
65.504071	2256.915667	20.769946
65.155150	2260.670502	20.774963
65.381814	2245.838214	20.779981
65.416602	2263.262447	20.784999
65.495429	2276.739058	20.790016
65.281331	2283.244545	20.795034
65.121823	2297.133489	20.800051
65.706262	2290.377368	20.805069
65.742840	2278.571948	20.810087
65.389615	2287.249790	20.815104
65.980387	2295.179964	20.820122
65.877430	2311.403375	20.825139
66.100924	2317.189931	20.830157
66.071026	2307.862945	20.835175
66.395937	2308.551740	20.840192
66.505015	2293.127429	20.845210
66.262400	2302.103122	20.850227
66.199311	2297.219264	20.855245
66.303250	2303.000412	20.860263
66.237509	2308.682485	20.865280
66.838420	2332.086202	20.870298
66.803217	2344.214751	20.875315
66.651399	2335.268585	20.880333
66.897071	2339.083264	20.885351
66.935535	2337.199666	20.890368
67.485236	2333.244701	20.895386
66.966313	2339.299083	20.900403
67.093270	2330.173289	20.905421
67.509633	2331.439887	20.910439
67.076211	2339.896773	20.915456
67.497626	2320.568547	20.920474
67.483306	2330.768333	20.925491
67.557777	2328.163777	20.930509
67.451439	2333.534061	20.935527
67.545864	2332.326667	20.940544
67.523462	2323.622085	20.945562
67.759041	2331.868978	20.950579
67.397248	2336.748462	20.955597
67.716286	2326.210872	20.960615
67.897850	2339.939439	20.965632
68.041598	2342.115789	20.970650
67.814869	2352.578723	20.975667
68.006359	2354.304233	20.980685
68.233197	2353.271774	20.985703
67.994258	2361.307079	20.990720
68.236033	2344.991800	20.995738
68.100756	2357.785784	21.000755
68.154010	2355.060320	21.005773
68.330343	2354.830360	21.010791
67.900256	2357.911219	21.015808
68.243788	2379.114589	21.020826
68.417362	2387.219013	21.025843
68.307240	2389.376378	21.030861
68.630177	2380.281889	21.035879
68.694383	2381.089842	21.040896
68.828302	2397.840295	21.045914
69.154107	2412.197441	21.050931
69.195764	2413.145359	21.055949
69.286340	2408.983309	21.060967
69.341806	2410.094697	21.065984
69.376777	2401.364035	21.071002
69.551257	2404.743249	21.076019
69.981660	2404.712966	21.081037
70.012236	2400.085630	21.086055
69.950808	2397.634280	21.091072
70.021051	2396.963986	21.096090
69.578228	2377.961081	21.101107
69.809295	2387.616703	21.106125
70.021206	2384.443287	21.111143
70.112571	2403.209565	21.116160
70.207664	2382.620259	21.121178
70.227128	2389.077668	21.126195
70.341327	2390.658490	21.131213
70.597088	2391.815851	21.136231
70.283749	2390.206652	21.141248
70.251738	2391.108101	21.146266
70.622323	2391.936590	21.151283
70.436756	2384.596860	21.156301
70.377995	2393.760287	21.161319
70.431229	2389.466622	21.166336
70.647717	2391.181697	21.171354
70.470068	2388.140897	21.176371
70.315468	2389.314232	21.181389
70.623964	2406.259423	21.186407
70.669759	2422.663844	21.191424
70.817858	2417.770966	21.196442
70.908523	2420.025805	21.201459
70.713057	2419.538097	21.206477
71.278343	2427.611544	21.211495
71.116667	2433.914308	21.216512
71.260757	2442.606354	21.221530
71.143415	2444.038107	21.226547
70.895438	2444.833971	21.231565
71.512908	2454.356753	21.236583
71.667425	2459.070466	21.241600
71.505658	2461.358447	21.246618
72.136186	2466.434317	21.251635
72.221463	2470.624426	21.256653
72.354576	2456.330689	21.261671
72.300186	2468.933407	21.266688
72.318710	2452.533321	21.271706
71.945813	2467.034161	21.276723
72.445016	2462.617025	21.281741
72.419305	2457.965130	21.286759
72.316708	2459.581462	21.291776
72.544198	2456.610189	21.296794
72.483601	2455.294982	21.301811
72.232300	2450.741469	21.306829
72.748642	2455.500789	21.311847
72.541166	2458.030998	21.316864
72.761114	2449.075182	21.321882
72.711113	2455.187799	21.326899
72.657913	2473.975737	21.331917
73.098266	2479.011836	21.336935
72.925685	2488.575684	21.341952
73.112218	2481.364860	21.346970
73.190798	2480.845948	21.351987
72.837056	2494.118369	21.357005
73.038539	2478.314773	21.362023
73.079234	2490.146599	21.367040
73.461546	2496.538855	21.372058
73.589671	2506.578548	21.377075
73.505567	2512.283028	21.382093
73.676649	2512.669330	21.387111
73.503806	2515.920237	21.392128
73.775396	2508.117329	21.397146
74.232647	2507.523511	21.402163
73.895842	2510.785423	21.407181
74.374880	2505.139252	21.412199
74.083043	2519.823582	21.417216
74.243047	2527.889773	21.422234
74.350496	2533.153857	21.427251
74.402417	2546.827296	21.432269
74.371589	2533.475260	21.437287
74.265424	2538.737705	21.442304
74.274018	2530.514127	21.447322
74.508294	2534.358302	21.452339
74.542845	2551.986454	21.457357
74.992841	2552.163179	21.462375
74.785179	2557.206987	21.467392
74.803970	2559.732426	21.472410
74.915237	2557.453651	21.477427
75.132465	2568.120405	21.482445
75.609776	2554.231824	21.487463
75.380554	2556.955818	21.492480
75.275402	2552.055221	21.497498
75.663444	2558.880441	21.502515
75.585324	2564.942242	21.507533
75.543845	2552.390826	21.512551
75.616655	2571.318657	21.517568
75.731120	2580.489340	21.522586
76.147082	2580.957941	21.527603
75.987214	2587.071084	21.532621
76.160824	2576.601503	21.537639
76.446791	2588.079386	21.542656
76.015573	2589.328067	21.547674
76.639636	2574.991124	21.552691
76.324562	2581.904425	21.557709
76.807298	2569.225644	21.562727
76.411094	2578.129282	21.567744
76.277530	2569.947727	21.572762
76.872502	2573.329406	21.577779
76.426828	2579.866665	21.582797
76.670472	2580.225993	21.587815
76.678480	2573.849072	21.592832
76.656057	2570.924669	21.597850
76.718439	2584.564911	21.602867
76.792135	2604.708074	21.607885
77.183778	2605.123217	21.612903
77.281774	2611.611419	21.617920
77.027740	2618.696926	21.622938
76.940861	2602.722036	21.627955
77.017131	2620.561877	21.632973
77.254147	2627.450719	21.637991
77.424907	2639.034730	21.643008
77.284245	2642.405147	21.648026
77.713432	2637.539680	21.653043
77.609429	2644.316084	21.658061
77.655954	2633.416294	21.663079
77.752812	2639.394423	21.668096
77.516011	2658.068090	21.673114
78.175943	2663.838816	21.678131
77.911300	2665.268598	21.683149
78.096743	2662.914136	21.688167
78.686779	2658.927609	21.693184
78.366427	2660.091791	21.698202
78.857972	2651.809053	21.703219
78.579531	2658.327711	21.708237
78.698427	2654.238865	21.713255
78.512087	2657.323914	21.718272
78.505177	2658.372021	21.723290
79.247232	2659.377226	21.728307
79.101117	2679.795087	21.733325
78.838596	2678.007745	21.738343
79.063439	2679.060790	21.743360
79.308732	2679.803341	21.748378
79.789868	2673.077943	21.753395
79.413555	2676.114916	21.758413
79.623003	2670.301104	21.763431
79.616344	2665.059729	21.768448
79.384429	2669.778037	21.773466
79.750267	2663.610355	21.778483
79.871477	2675.507738	21.783501
79.794393	2667.535693	21.788519
79.687337	2665.356442	21.793536
79.277594	2678.467019	21.798554
79.773510	2682.577382	21.803571
79.944574	2697.378555	21.808589
79.729501	2696.866916	21.813607
80.230860	2702.157181	21.818624
80.113562	2706.230096	21.823642
80.879097	2722.952704	21.828659
80.668333	2738.276228	21.833677
80.397552	2727.433635	21.838695
80.575975	2733.002201	21.843712
80.616187	2736.941950	21.848730
80.892509	2723.106184	21.853747
80.511386	2731.030564	21.858765
80.670121	2732.402457	21.863783
80.871949	2748.680985	21.868800
80.830119	2758.385565	21.873818
81.271530	2747.632534	21.878835
81.159045	2753.358732	21.883853
81.315799	2742.714259	21.888871
81.617128	2752.497461	21.893888
81.723101	2767.353183	21.898906
82.051772	2764.306827	21.903923
82.105002	2774.882757	21.908941
81.927503	2772.395444	21.913959
81.755584	2774.871779	21.918976
81.649470	2778.292022	21.923994
82.265011	2772.425107	21.929011
82.175036	2776.793935	21.934029
82.375542	2772.871875	21.939047
82.467672	2776.111250	21.944064
82.340889	2778.097003	21.949082
82.371201	2777.227382	21.954099
82.674947	2777.280283	21.959117
82.666073	2769.163418	21.964135
82.601464	2782.547277	21.969152
82.803604	2797.718628	21.974170
82.920661	2801.053495	21.979187
83.077286	2813.771959	21.984205
83.437029	2804.551041	21.989223
83.204450	2796.368043	21.994240
83.207519	2799.551690	21.999258
83.444677	2801.605544	22.004275
83.134448	2807.229846	22.009293
83.155632	2802.776401	22.014311
83.654357	2803.605747	22.019328
83.647694	2807.155997	22.024346
83.356135	2795.834079	22.029363
83.603257	2810.110520	22.034381
83.685222	2816.132132	22.039399
84.105185	2813.123018	22.044416
83.545385	2825.598271	22.049434
83.837151	2812.652464	22.054451
83.994024	2817.169424	22.059469
83.931643	2815.036696	22.064487
84.395322	2835.099443	22.069504
84.529085	2842.200769	22.074522
84.363300	2845.125351	22.079539
84.365111	2850.055034	22.084557
84.418410	2843.912257	22.089575
84.556783	2838.597200	22.094592
84.931516	2847.406416	22.099610
84.599917	2860.801869	22.104627
84.439465	2874.019377	22.109645
84.754909	2870.252294	22.114663
85.048761	2866.291132	22.119680
85.113515	2882.573989	22.124698
85.572506	2892.170531	22.129715
85.486661	2890.599601	22.134733
85.670125	2890.616508	22.139751
86.095162	2889.993365	22.144768
85.745689	2897.716113	22.149786
86.066766	2894.045738	22.154803
86.072416	2888.365204	22.159821
85.995273	2885.910866	22.164839
86.321722	2891.035652	22.169856
86.164927	2886.407303	22.174874
86.244819	2881.991362	22.179891
86.193716	2888.330335	22.184909
86.144205	2892.897631	22.189927
86.626434	2891.574012	22.194944
86.356094	2903.052498	22.199962
86.768805	2906.728627	22.204979
86.921708	2918.224455	22.209997
86.712805	2911.865199	22.215015
86.585242	2912.632092	22.220032
86.586540	2912.747671	22.225050
87.090913	2915.738093	22.230067
87.005648	2935.653649	22.235085
87.040726	2940.825514	22.240103
87.193571	2941.064833	22.245120
87.196233	2948.859630	22.250138
87.314187	2939.655831	22.255155
87.346854	2942.728691	22.260173
87.253206	2957.771991	22.265191
88.046938	2956.744854	22.270208
87.787090	2967.661361	22.275226
88.096050	2956.313132	22.280243
88.085680	2959.090338	22.285261
88.077581	2962.738508	22.290279
88.529219	2953.613322	22.295296
88.316300	2959.567268	22.300314
88.678594	2957.839841	22.305331
88.655978	2958.561404	22.310349
88.262065	2970.500990	22.315367
88.737010	2980.224092	22.320384
88.750322	2995.526515	22.325402
89.426175	2983.950968	22.330419
89.084456	2995.093668	22.335437
88.931700	2994.086614	22.340455
89.417585	2982.443299	22.345472
89.107427	2988.263735	22.350490
89.251976	2983.660666	22.355507
89.325714	2985.376214	22.360525
89.148552	2984.921679	22.365543
89.494182	2980.326660	22.370560
89.681434	2984.036988	22.375578
89.781542	2984.300396	22.380595
89.635783	2984.674598	22.385613
89.650117	3000.347759	22.390631
89.931182	3001.872667	22.395648
89.730882	3013.948356	22.400666
90.059546	3005.823123	22.405683
90.054156	3014.952483	22.410701
89.869300	3025.835353	22.415719
90.205136	3028.893077	22.420736
90.204656	3044.961686	22.425754
90.406310	3046.504078	22.430771
90.511512	3040.329794	22.435789
90.632474	3045.424868	22.440807
90.934010	3055.878372	22.445824
91.170309	3060.208613	22.450842
91.260223	3055.948853	22.455859
91.297834	3060.638401	22.460877
91.250155	3066.900494	22.465895
91.544775	3061.153152	22.470912
91.332509	3066.430979	22.475930
91.637358	3061.163094	22.480947
91.603492	3064.070205	22.485965
91.517469	3061.006226	22.490983
91.624810	3059.898617	22.496000
91.742569	3078.316028	22.501018
92.011930	3084.000386	22.506035
92.202325	3093.657275	22.511053
91.923165	3086.852840	22.516071
92.209165	3088.576173	22.521088
92.161961	3096.993535	22.526106
92.046127	3086.373487	22.531123
92.327616	3095.410903	22.536141
92.154863	3121.183899	22.541159
92.759147	3123.643594	22.546176
92.507802	3120.867239	22.551194
92.719358	3124.184954	22.556211
93.209974	3129.994916	22.561229
92.624408	3144.238255	22.566247
93.296619	3143.156025	22.571264
93.402698	3149.235983	22.576282
93.772722	3145.878740	22.581299
93.646863	3151.404914	22.586317
93.546894	3144.385727	22.591335
93.430141	3139.311256	22.596352
93.497946	3147.142220	22.601370
93.734590	3144.724086	22.606387
94.164989	3158.215698	22.611405
93.904733	3167.499956	22.616423
94.293846	3164.139942	22.621440
94.334331	3169.587788	22.626458
94.341440	3154.188173	22.631475
94.664087	3157.430803	22.636493
94.355679	3163.779022	22.641511
94.524402	3158.026503	22.646528
94.653522	3161.950063	22.651546
94.642473	3148.338688	22.656563
94.802731	3173.145908	22.661581
94.785969	3190.239912	22.666599
95.214102	3184.800376	22.671616
95.045045	3192.506784	22.676634
95.134001	3195.133713	22.681651
95.320184	3184.337201	22.686669
95.086735	3193.583569	22.691687
95.539421	3182.738601	22.696704
95.577605	3189.437756	22.701722
95.531609	3187.395975	22.706739
95.414926	3195.153956	22.711757
95.454255	3209.543916	22.716775
95.818685	3199.331334	22.721792
95.958785	3209.306892	22.726810
95.537918	3211.573305	22.731827
96.055471	3231.543383	22.736845
95.759376	3236.967444	22.741863
95.978120	3234.993647	22.746880
96.243190	3243.354265	22.751898
96.670633	3255.103345	22.756915
96.682735	3259.140410	22.761933
96.768087	3266.590140	22.766951
97.021342	3260.580253	22.771968
97.133016	3265.854911	22.776986
96.983271	3261.873386	22.782003
97.538941	3260.685627	22.787021
97.311002	3263.496153	22.792039
96.955742	3260.141636	22.797056
97.377924	3284.177237	22.802074
97.545921	3285.759876	22.807091
97.702257	3281.044520	22.812109
97.812217	3291.473596	22.817127
98.168374	3289.968042	22.822144
98.165542	3292.027048	22.827162
98.096049	3288.358250	22.832179
98.258614	3277.241532	22.837197
98.364627	3297.644835	22.842215
98.894490	3288.911275	22.847232
98.800558	3305.493714	22.852250
98.680359	3319.535342	22.857267
98.827307	3306.038238	22.862285
98.813841	3311.427341	22.867303
99.233051	3301.627325	22.872320
99.182243	3297.927475	22.877338
99.092095	3296.793093	22.882355
99.351701	3294.428227	22.887373
99.419400	3304.500095	22.892391
99.412726	3296.243599	22.897408
99.161731	3300.271473	22.902426
99.261370	3294.066117	22.907443
99.358761	3305.805307	22.912461
99.231692	3325.302248	22.917479
99.623342	3331.696849	22.922496
99.665640	3333.761382	22.927514
99.518274	3345.184786	22.932531
99.720257	3348.482872	22.937549
100.123598	3356.978157	22.942567
100.176668	3353.106746	22.947584
100.387291	3374.311035	22.952602
100.645050	3390.883372	22.957619
100.822860	3383.034920	22.962637
100.760967	3395.810514	22.967655
100.701676	3389.944463	22.972672
100.674713	3384.466810	22.977690
100.992529	3396.164848	22.982707
101.157738	3401.976816	22.987725
101.285268	3414.548601	22.992743
101.497311	3409.955495	22.997760
101.499940	3409.492441	23.002778
101.507194	3410.490215	23.007795
101.890096	3403.466169	23.012813
102.071448	3412.141957	23.017831
102.046349	3407.034898	23.022848
102.189426	3398.129463	23.027866
101.946070	3401.441445	23.032883
102.159093	3398.561773	23.037901
102.123011	3408.338648	23.042919
102.265086	3409.578306	23.047936
102.199060	3428.775469	23.052954
102.203023	3426.449761	23.057971
102.595283	3430.654271	23.062989
102.696755	3436.692580	23.068007
102.722583	3424.087188	23.073024
103.124202	3428.172810	23.078042
102.999470	3445.881500	23.083059
103.030658	3456.792685	23.088077
102.954240	3463.292794	23.093095
103.403217	3464.489518	23.098112
103.533150	3454.089584	23.103130
103.528067	3462.116656	23.108147
103.573624	3457.805857	23.113165
103.699719	3479.425516	23.118183
103.590614	3480.008254	23.123200
104.032281	3487.010070	23.128218
103.898729	3486.286060	23.133235
104.249050	3483.256065	23.138253
104.254991	3497.907757	23.143271
104.175796	3504.940300	23.148288
104.406831	3513.440575	23.153306
104.396772	3514.145909	23.158323
104.521265	3511.031236	23.163341
104.525345	3520.192792	23.168359
104.505187	3526.294193	23.173376
104.611878	3535.930959	23.178394
104.911173	3542.309045	23.183411
104.898080	3546.174348	23.188429
104.952870	3563.985354	23.193447
104.850014	3568.520335	23.198464
105.022532	3574.608754	23.203482
105.744447	3590.646124	23.208499
105.906183	3592.779511	23.213517
106.156000	3599.989150	23.218535
106.404772	3595.200514	23.223552
106.371595	3592.745085	23.228570
106.394381	3597.532931	23.233587
106.688211	3593.660974	23.238605
107.125616	3588.758026	23.243623
106.881272	3582.053135	23.248640
107.278748	3583.641911	23.253658
106.817344	3595.197816	23.258675
107.168246	3578.993519	23.263693
107.429035	3581.084516	23.268711
107.550452	3583.752600	23.273728
107.836946	3587.163927	23.278746
107.491119	3587.377146	23.283763
107.457647	3578.657947	23.288781
107.687836	3583.653607	23.293799
107.498817	3565.822741	23.298816
107.806326	3580.374967	23.303834
107.392192	3575.750825	23.308851
107.627968	3567.806452	23.313869
107.383519	3586.186388	23.318887
107.621998	3597.475216	23.323904
108.024568	3603.333011	23.328922
107.980762	3612.347805	23.333939
108.121407	3629.983233	23.338957
108.372872	3629.106482	23.343975
108.031028	3643.578064	23.348992
108.448495	3645.719911	23.354010
108.105351	3658.005598	23.359027
108.437189	3665.417071	23.364045
108.678754	3670.754624	23.369063
108.676719	3689.342216	23.374080
109.066353	3689.237971	23.379098
108.829775	3700.001900	23.384115
109.260046	3688.340892	23.389133
109.539935	3707.356304	23.394151
109.668907	3720.949499	23.399168
109.859340	3718.436553	23.404186
109.791761	3726.080745	23.409203
109.956757	3715.611438	23.414221
110.124542	3727.280620	23.419239
109.748195	3720.361665	23.424256
110.557039	3731.749097	23.429274
110.601960	3747.739640	23.434291
110.832088	3745.324070	23.439309
110.746556	3743.578173	23.444327
110.791419	3746.394412	23.449344
111.110070	3749.028293	23.454362
110.967189	3746.770950	23.459379
111.098860	3743.174266	23.464397
111.439228	3755.247634	23.469415
111.687000	3768.123464	23.474432
111.655152	3764.451471	23.479450
111.485290	3772.394944	23.484467
111.781833	3763.787168	23.489485
112.001002	3769.668698	23.494503
111.912422	3772.860630	23.499520
112.116462	3771.625922	23.504538
111.866584	3778.567145	23.509555
112.036200	3791.460265	23.514573
112.393420	3800.053207	23.519591
112.275669	3803.500798	23.524608
112.603615	3798.765537	23.529626
112.476727	3801.995712	23.534643
112.590807	3806.038084	23.539661
112.882417	3828.076555	23.544679
113.235614	3825.031057	23.549696
113.211287	3822.107916	23.554714
112.948321	3826.506464	23.559731
113.453003	3821.639557	23.564749
113.236007	3835.482288	23.569767
113.238108	3849.240716	23.574784
113.495184	3852.499469	23.579802
113.569489	3858.164430	23.584819
113.759153	3867.849483	23.589837
114.080766	3879.425583	23.594855
113.952185	3886.816527	23.599872
114.459631	3872.332731	23.604890
114.503025	3877.376738	23.609907
114.518667	3875.413258	23.614925
115.042914	3877.500052	23.619943
114.693495	3897.515299	23.624960
115.067707	3899.707264	23.629978
114.931951	3908.700438	23.634995
115.136061	3905.447290	23.640013
115.474165	3905.463799	23.645031
115.223096	3897.904243	23.650048
115.337560	3895.773981	23.655066
115.504719	3903.286861	23.660083
115.530030	3914.318254	23.665101
115.938047	3917.385075	23.670119
115.990655	3934.034874	23.675136
116.393649	3929.054829	23.680154
116.153270	3926.547814	23.685171
116.078986	3929.487372	23.690189
116.270817	3927.582129	23.695207
116.049307	3939.790800	23.700224
116.445617	3946.375859	23.705242
116.217476	3950.573369	23.710259
116.233081	3958.732724	23.715277
116.737085	3958.103559	23.720295
117.104944	3977.437070	23.725312
117.352676	3986.073837	23.730330
117.462985	3984.489220	23.735347
117.575888	3981.371648	23.740365
117.721070	3987.990428	23.745383
117.196542	3989.521630	23.750400
117.508325	3975.414284	23.755418
117.320071	3988.365636	23.760435
117.648057	4006.755241	23.765453
117.632563	4005.308004	23.770471
117.877668	4010.415523	23.775488
118.144541	4024.246822	23.780506
118.270212	4032.305302	23.785523
118.287251	4041.648905	23.790541
118.669086	4032.781940	23.795559
118.381326	4045.012687	23.800576
118.701813	4056.550516	23.805594
119.086553	4060.062237	23.810611
119.070612	4063.287484	23.815629
119.181363	4060.076537	23.820647
119.249476	4067.458626	23.825664
119.828699	4072.719543	23.830682
119.823723	4083.779695	23.835699
119.820808	4083.087973	23.840717
120.029646	4076.196403	23.845735
120.020114	4076.900493	23.850752
120.025069	4081.862727	23.855770
120.209224	4080.249336	23.860787
120.398480	4091.362389	23.865805
120.715004	4099.483021	23.870823
120.616458	4108.659156	23.875840
120.836464	4118.244837	23.880858
120.628260	4109.324312	23.885875
120.661932	4113.600586	23.890893
121.537008	4113.244681	23.895911
121.123759	4125.445865	23.900928
121.136913	4126.134389	23.905946
121.420937	4134.121814	23.910963
121.242097	4136.158882	23.915981
121.420277	4139.766247	23.920999
121.463828	4159.595484	23.926016
121.563479	4158.663905	23.931034
121.734289	4167.367060	23.936051
122.038266	4173.887174	23.941069
122.542656	4182.926514	23.946087
122.408950	4188.166112	23.951104
122.691466	4187.895713	23.956122
122.958373	4191.619919	23.961139
122.643610	4188.665255	23.966157
122.979043	4177.410206	23.971175
123.011573	4191.887643	23.976192
123.362852	4206.641509	23.981210
123.473569	4215.311325	23.986227
123.384056	4216.871329	23.991245
123.842154	4210.084126	23.996263
123.478405	4223.979846	24.001280
123.716373	4214.186041	24.006298
124.029319	4215.912523	24.011315
123.936717	4217.358059	24.016333
124.338900	4228.015410	24.021351
124.358386	4242.281629	24.026368
124.288072	4244.474002	24.031386
124.509746	4244.668085	24.036403
124.619852	4251.868475	24.041421
124.936029	4237.675113	24.046439
124.621532	4239.904762	24.051456
124.890415	4235.047632	24.056474
125.022582	4246.853042	24.061491
124.989296	4265.331904	24.066509
125.098414	4266.837764	24.071527
125.290612	4267.269839	24.076544
125.606720	4254.301886	24.081562
125.683696	4271.909595	24.086579
125.602126	4284.123715	24.091597
126.150957	4276.821374	24.096615
125.892407	4301.825334	24.101632
126.026224	4283.328281	24.106650
126.038693	4292.725556	24.111667
126.200039	4313.377366	24.116685
126.432670	4319.984171	24.121703
126.524991	4322.971034	24.126720
126.637611	4324.606264	24.131738
126.870927	4332.254880	24.136755
127.043156	4337.697466	24.141773
127.131666	4344.700650	24.146791
127.195686	4349.660277	24.151808
127.188271	4349.074032	24.156826
127.618064	4357.543041	24.161843
127.989198	4368.756911	24.166861
127.806627	4366.528494	24.171879
128.302340	4376.275811	24.176896
128.377782	4364.887264	24.181914
128.586401	4369.048801	24.186931
128.278829	4368.446096	24.191949
128.656101	4369.242881	24.196967
128.780223	4389.088995	24.201984
128.834138	4399.611175	24.207002
128.964384	4389.564180	24.212019
128.825960	4397.631133	24.217037
128.741226	4389.548432	24.222055
128.931829	4407.743104	24.227072
129.460857	4416.238243	24.232090
129.288874	4431.045090	24.237107
129.143108	4435.532296	24.242125
129.934727	4425.699461	24.247143
129.923298	4446.377689	24.252160
129.994531	4443.125954	24.257178
130.050979	4438.624466	24.262195
129.814506	4451.743266	24.267213
130.302854	4460.513719	24.272231
130.071086	4473.534103	24.277248
130.254937	4472.558639	24.282266
130.621265	4487.068501	24.287283
130.569796	4499.855867	24.292301
131.131701	4493.861748	24.297319
130.922986	4502.635012	24.302336
131.028575	4522.918304	24.307354
131.375928	4521.114039	24.312371
131.327721	4535.830399	24.317389
131.946658	4543.946873	24.322407
132.095926	4548.550650	24.327424
132.307465	4545.577298	24.332442
132.523150	4552.146054	24.337459
132.465404	4554.626996	24.342477
132.726251	4544.225932	24.347495
132.984743	4536.114683	24.352512
132.947280	4537.748006	24.357530
133.200705	4536.994923	24.362547
133.132054	4527.553322	24.367565
133.390069	4532.150116	24.372583
133.429168	4539.714430	24.377600
133.321242	4534.166693	24.382618
133.377336	4535.956214	24.387635
133.388712	4544.774181	24.392653
133.758528	4552.890952	24.397671
134.017717	4556.030583	24.402688
133.538091	4566.160801	24.407706
133.790750	4561.614979	24.412723
133.985273	4572.283320	24.417741
134.076969	4579.738927	24.422759
134.290148	4595.220887	24.427776
133.987816	4596.570445	24.432794
134.765831	4605.626946	24.437811
134.577984	4624.485432	24.442829
134.869752	4628.285171	24.447847
134.938338	4637.997048	24.452864
134.806030	4650.372638	24.457882
135.506958	4654.457469	24.462899
135.579699	4660.910538	24.467917
135.634661	4658.823104	24.472935
135.412535	4677.680241	24.477952
135.307319	4685.123607	24.482970
135.941521	4685.315554	24.487987
135.944586	4699.214752	24.493005
136.334323	4711.355899	24.498023
136.800089	4711.060667	24.503040
136.957660	4717.153188	24.508058
136.662181	4705.715546	24.513075
136.724591	4729.899174	24.518093
137.303273	4741.026970	24.523111
137.232473	4742.509897	24.528128
137.169697	4740.623872	24.533146
137.748702	4743.912996	24.538163
137.486441	4746.546750	24.543181
137.979032	4768.420171	24.548199
138.215822	4766.033272	24.553216
138.188078	4767.322419	24.558234
138.643362	4765.497896	24.563251
138.324394	4762.956501	24.568269
138.548206	4765.373534	24.573287
138.855971	4767.160005	24.578304
138.443364	4775.128420	24.583322
138.776884	4783.280460	24.588339
138.690559	4790.066281	24.593357
138.886515	4787.704253	24.598375
138.900942	4809.159155	24.603392
138.573339	4826.411543	24.608410
139.193686	4822.524609	24.613427
139.541517	4852.943602	24.618445
139.875177	4840.269964	24.623463
139.930596	4851.715229	24.628480
140.151501	4854.703746	24.633498
140.295867	4860.352744	24.638515
140.733409	4878.705546	24.643533
140.482164	4879.504820	24.648551
140.872919	4870.781612	24.653568
140.582367	4876.160028	24.658586
141.315825	4881.974553	24.663603
141.575181	4902.618787	24.668621
141.303767	4902.970911	24.673639
141.623059	4895.291240	24.678656
141.460420	4903.433341	24.683674
141.632475	4895.259037	24.688691
141.715881	4894.345857	24.693709
141.924682	4906.567515	24.698727
142.231114	4918.854140	24.703744
142.485065	4928.193700	24.708762
142.555444	4929.280748	24.713779
142.551906	4926.335846	24.718797
142.572920	4925.825205	24.723815
142.497022	4924.320153	24.728832
143.033891	4935.543220	24.733850
143.251700	4946.744298	24.738867
143.140479	4948.737196	24.743885
143.576060	4947.538886	24.748903
143.384167	4945.823851	24.753920
143.260386	4946.550046	24.758938
143.499877	4958.780841	24.763955
143.583517	4971.739177	24.768973
143.596932	4977.309088	24.773991
143.857621	4987.629676	24.779008
144.147013	5003.845255	24.784026
144.464728	5005.754544	24.789043
144.350557	5013.652405	24.794061
144.669679	5027.975264	24.799079
144.692552	5030.083010	24.804096
144.534058	5028.903503	24.809114
144.786082	5046.920205	24.814131
145.187703	5061.863438	24.819149
145.341227	5068.346618	24.824167
145.552767	5068.274614	24.829184
145.433280	5089.660709	24.834202
145.785328	5098.687999	24.839219
145.955102	5100.047646	24.844237
146.053459	5104.135487	24.849255
146.228957	5119.357212	24.854272
146.336617	5132.203804	24.859290
146.848030	5133.430497	24.864307
146.636514	5132.034512	24.869325
147.229838	5146.120700	24.874343
147.508462	5161.239545	24.879360
147.282801	5164.973864	24.884378
147.543395	5162.341177	24.889395
147.450909	5156.558326	24.894413
147.708299	5161.498796	24.899431
148.018865	5164.980521	24.904448
147.936619	5179.164409	24.909466
147.866413	5175.742982	24.914483
148.139658	5180.634366	24.919501
148.108985	5210.492947	24.924519
148.570235	5210.216571	24.929536
148.390119	5220.696925	24.934554
148.654646	5218.660569	24.939571
148.787091	5235.030748	24.944589
148.744287	5234.522787	24.949607
149.555225	5247.818529	24.954624
149.476125	5270.499279	24.959642
149.477383	5266.041346	24.964659
149.933306	5267.130746	24.969677
150.033498	5266.682594	24.974695
150.602880	5276.468685	24.979712
150.187560	5296.176062	24.984730
150.633705	5296.420422	24.989747
151.033579	5288.779202	24.994765
150.905315	5295.488698	24.999783
151.166017	5295.577888	25.004800
150.967231	5294.385341	25.009818
151.173554	5288.163901	25.014835
151.624230	5293.214180	25.019853
151.414384	5308.459717	25.024871
151.799456	5302.789921	25.029888
151.521871	5313.426665	25.034906
151.820801	5303.224360	25.039923
152.018014	5306.970611	25.044941
152.028718	5327.038309	25.049959
152.242316	5333.451008	25.054976
152.309760	5336.753283	25.059994
152.501700	5339.220576	25.065011
152.603031	5350.953950	25.070029
152.683444	5363.535098	25.075047
153.092045	5359.939849	25.080064
152.903250	5358.630655	25.085082
153.015588	5383.095279	25.090099
153.584581	5386.452359	25.095117
153.410166	5398.035308	25.100135
153.862997	5387.683817	25.105152
153.698262	5405.855775	25.110170
153.810972	5413.935225	25.115187
154.277634	5416.831182	25.120205
154.061747	5423.963215	25.125223
154.398502	5437.009195	25.130240
154.179350	5447.169307	25.135258
154.617139	5453.377968	25.140275
154.744767	5462.989217	25.145293
154.914618	5481.667428	25.150311
155.044266	5481.505806	25.155328
155.273562	5505.055753	25.160346
155.645734	5511.113842	25.165363
155.820025	5505.645842	25.170381
155.942485	5530.440599	25.175399
156.243128	5524.047506	25.180416
156.235035	5528.163319	25.185434
156.581695	5519.016238	25.190451
156.707335	5532.761198	25.195469
156.741977	5553.161526	25.200487
156.958999	5558.869632	25.205504
156.825364	5563.960816	25.210522
157.290702	5559.605543	25.215539
157.234395	5569.325281	25.220557
157.577780	5574.892756	25.225575
157.822282	5581.801357	25.230592
157.776479	5585.674546	25.235610
158.155154	5602.665930	25.240627
158.470002	5605.284616	25.245645
158.554500	5613.279052	25.250663
158.532517	5603.117869	25.255680
158.619378	5601.458214	25.260698
159.339366	5628.600508	25.265715
159.478256	5624.829323	25.270733
159.216296	5633.350541	25.275751
159.509481	5630.113800	25.280768
159.310192	5632.544308	25.285786
159.667794	5624.571254	25.290803
160.010774	5635.076333	25.295821
159.652374	5662.649253	25.300839
160.076999	5655.258946	25.305856
160.177259	5670.700801	25.310874
160.180393	5683.858139	25.315891
160.566760	5688.405672	25.320909
160.506789	5710.386850	25.325927
160.760510	5704.773313	25.330944
161.117675	5731.669471	25.335962
160.993928	5733.122662	25.340979
161.406709	5729.458905	25.345997
161.138157	5743.487478	25.351015
161.630388	5742.357708	25.356032
161.636216	5754.469495	25.361050
161.875744	5771.002079	25.366067
162.219338	5774.670651	25.371085
162.216820	5787.120944	25.376103
162.393799	5787.820225	25.381120
162.455366	5805.947300	25.386138
162.582710	5816.956832	25.391155
162.885912	5811.179118	25.396173
163.240489	5820.266265	25.401191
163.793924	5838.299344	25.406208
163.653519	5850.923739	25.411226
163.474729	5837.311815	25.416243
163.969295	5836.651861	25.421261
163.665106	5845.848873	25.426279
163.921651	5851.307955	25.431296
164.028573	5860.175424	25.436314
164.422237	5863.589990	25.441331
164.869417	5863.281282	25.446349
164.774358	5874.011051	25.451367
164.752434	5877.504662	25.456384
165.096306	5891.468207	25.461402
165.261113	5891.433869	25.466419
165.612578	5889.099493	25.471437
165.597844	5894.966596	25.476455
165.909092	5910.091786	25.481472
166.044345	5923.508632	25.486490
165.742991	5928.245702	25.491507
166.230852	5926.085646	25.496525
166.396103	5946.317573	25.501543
166.649098	5947.410690	25.506560
166.617109	5951.769220	25.511578
166.927171	5956.227860	25.516595
167.063305	5970.548005	25.521613
167.081930	5976.538786	25.526631
167.178889	5974.292214	25.531648
167.417140	5983.181329	25.536666
167.505381	6001.015941	25.541683
168.005166	6000.457509	25.546701
167.819625	6013.851140	25.551719
168.382173	6030.087141	25.556736
168.570658	6022.313590	25.561754
168.454872	6031.355860	25.566771
168.875644	6037.829064	25.571789
169.044543	6063.089545	25.576807
169.246284	6055.052290	25.581824
169.479227	6055.363469	25.586842
169.439027	6069.124537	25.591859
169.928180	6074.773601	25.596877
169.748005	6078.276127	25.601895
169.991865	6077.233925	25.606912
170.420373	6079.184080	25.611930
170.282523	6097.999025	25.616947
170.735221	6104.060553	25.621965
170.671983	6118.999050	25.626983
170.834937	6114.266792	25.632000
171.186582	6111.678737	25.637018
171.344158	6138.432201	25.642035
171.319619	6133.259972	25.647053
171.612251	6143.040440	25.652071
171.783964	6136.867718	25.657088
172.119837	6157.699413	25.662106
171.748257	6172.597642	25.667123
172.203324	6166.442585	25.672141
172.210540	6175.654393	25.677159
172.426681	6181.770079	25.682176
172.521781	6197.210153	25.687194
172.928540	6200.154770	25.692212
172.990417	6194.161675	25.697229
172.721922	6214.150699	25.702247
172.583024	6219.844718	25.707264
173.292449	6231.114186	25.712282
173.077936	6254.350419	25.717300
173.755848	6267.973871	25.722317
173.669242	6295.459573	25.727335
173.852979	6287.216457	25.732352
174.625581	6309.229975	25.737370
174.444093	6314.394695	25.742388
174.529999	6303.004596	25.747405
174.626548	6311.774792	25.752423
174.963812	6326.032819	25.757440
174.927296	6337.725948	25.762458
175.101396	6343.925846	25.767476
175.775398	6346.222914	25.772493
175.753288	6379.888179	25.777511
175.769228	6374.763517	25.782528
176.092502	6372.496751	25.787546
176.135750	6387.698274	25.792564
176.853172	6395.345729	25.797581
176.728675	6403.993467	25.802599
177.036008	6395.670760	25.807616
177.038778	6395.953889	25.812634
177.045389	6423.507871	25.817652
177.458366	6425.999393	25.822669
177.706007	6430.593739	25.827687
177.725497	6433.838808	25.832704
178.019893	6439.205976	25.837722
178.045751	6451.184230	25.842740
178.148687	6455.235432	25.847757
178.289013	6469.773514	25.852775
178.266786	6493.545372	25.857792
178.549823	6480.158109	25.862810
178.461261	6515.719510	25.867828
179.112592	6512.583982	25.872845
178.875006	6520.255701	25.877863
179.416525	6546.990401	25.882880
179.662472	6545.204279	25.887898
179.939974	6549.799230	25.892916
180.030790	6568.060175	25.897933
180.124632	6578.379497	25.902951
180.286435	6576.204022	25.907968
180.379006	6592.286050	25.912986
180.621763	6604.447481	25.918004
181.010564	6603.460017	25.923021
180.964122	6626.834377	25.928039
181.033451	6625.220052	25.933056
181.944526	6626.744607	25.938074
181.403078	6636.984827	25.943092
181.928761	6648.722953	25.948109
182.243554	6645.896740	25.953127
181.919377	6657.515640	25.958144
182.222193	6675.714044	25.963162
182.353846	6686.613196	25.968180
182.989743	6682.746091	25.973197
183.210347	6701.144023	25.978215
183.180275	6715.701088	25.983232
183.570867	6716.643881	25.988250
183.368565	6723.597809	25.993268
183.625190	6732.816699	25.998285
184.236870	6742.791259	26.003303
184.116660	6736.781632	26.008320
184.506264	6736.346967	26.013338
184.778419	6761.204725	26.018356
184.494983	6760.803502	26.023373
184.643559	6763.008819	26.028391
184.783600	6771.273479	26.033408
185.216111	6780.644442	26.038426
185.186739	6792.381619	26.043444
185.400339	6788.944365	26.048461
185.451094	6811.160003	26.053479
185.623816	6823.460798	26.058496
186.152449	6836.981855	26.063514
186.120640	6854.490728	26.068532
186.447523	6856.217568	26.073549
186.665861	6858.553130	26.078567
186.745339	6872.098163	26.083584
187.209512	6880.662884	26.088602
187.145371	6887.050518	26.093620
187.197155	6883.088662	26.098637
187.752735	6898.153084	26.103655
187.687824	6914.660071	26.108672
188.292829	6912.229227	26.113690
188.136336	6915.149864	26.118708
188.185607	6912.918933	26.123725
188.356061	6925.302889	26.128743
188.315219	6945.305552	26.133760
188.994695	6936.032462	26.138778
188.968341	6951.669027	26.143796
189.272795	6962.449179	26.148813
189.000650	6971.305196	26.153831
189.132312	6986.675395	26.158848
189.608472	6990.835873	26.163866
189.597800	7003.814639	26.168884
190.047854	7021.952833	26.173901
190.531040	7038.013182	26.178919
190.201924	7039.827375	26.183936
190.856202	7059.789936	26.188954
190.922483	7058.484054	26.193972
190.817347	7067.514909	26.198989
191.243934	7084.287285	26.204007
191.534125	7096.382953	26.209024
191.388570	7093.595852	26.214042
191.901392	7115.116303	26.219060
192.136959	7118.693589	26.224077
192.652631	7124.708068	26.229095
192.151349	7149.815778	26.234112
192.531993	7154.352872	26.239130
192.703643	7150.224597	26.244148
193.061105	7170.865008	26.249165
193.086744	7174.387263	26.254183
193.297863	7195.186626	26.259200
193.488815	7197.144745	26.264218
193.627175	7213.242664	26.269236
194.067318	7220.358266	26.274253
194.414467	7233.286647	26.279271
194.479413	7241.040171	26.284288
194.449194	7237.432084	26.289306
194.691573	7253.555360	26.294324
194.737658	7265.905820	26.299341
195.375483	7275.015446	26.304359
195.370574	7293.329305	26.309376
195.331513	7292.728497	26.314394
195.581390	7317.955516	26.319412
195.921049	7328.009351	26.324429
196.028846	7323.594643	26.329447
195.804637	7351.088407	26.334464
196.435056	7357.677112	26.339482
196.537373	7375.154900	26.344500
196.945844	7389.182331	26.349517
197.390042	7390.966217	26.354535
197.505065	7409.655779	26.359552
197.910396	7409.739163	26.364570
197.774677	7426.733384	26.369588
198.263343	7414.540893	26.374605
198.501157	7421.922452	26.379623
198.693074	7439.053858	26.384640
198.816680	7440.103124	26.389658
198.828867	7441.626913	26.394676
198.834758	7449.492716	26.399693
199.174469	7459.478884	26.404711
199.119000	7472.384315	26.409728
199.302941	7477.301441	26.414746
199.831310	7493.848661	26.419764
199.634783	7504.172543	26.424781
199.840982	7498.228322	26.429799
200.260905	7533.446303	26.434816
200.601683	7524.233672	26.439834
200.533218	7537.805339	26.444852
200.478127	7547.260630	26.449869
201.128508	7556.724383	26.454887
200.808408	7563.391759	26.459904
201.364363	7575.877822	26.464922
201.854631	7588.771773	26.469940
201.852416	7591.972622	26.474957
202.211558	7604.023392	26.479975
202.341245	7612.810090	26.484992
202.481866	7611.904615	26.490010
202.577745	7627.791792	26.495028
202.648397	7650.245558	26.500045
202.814489	7650.557600	26.505063
203.023373	7669.647051	26.510080
203.901189	7680.655736	26.515098
203.692648	7680.719440	26.520116
203.861184	7686.601763	26.525133
204.076382	7707.158506	26.530151
204.065114	7717.362058	26.535168
204.338301	7723.279847	26.540186
204.500721	7742.428279	26.545204
204.743699	7749.672861	26.550221
204.843736	7765.496470	26.555239
204.990008	7783.050927	26.560256
205.777573	7792.047053	26.565274
205.855695	7810.539963	26.570292
205.775236	7814.943262	26.575309
206.105435	7823.534613	26.580327
206.569445	7846.816808	26.585344
206.542347	7839.437263	26.590362
206.777964	7860.077471	26.595380
206.960305	7875.745775	26.600397
207.181624	7875.043550	26.605415
207.155626	7886.459585	26.610432
207.827362	7896.701426	26.615450
207.801532	7906.106397	26.620468
207.920941	7926.795863	26.625485
208.487597	7926.941559	26.630503
208.457717	7944.719923	26.635520
208.490092	7951.630020	26.640538
208.824307	7952.706686	26.645556
208.907804	7973.449421	26.650573
209.089009	7980.449900	26.655591
209.413445	8002.260328	26.660608
209.621092	8006.290654	26.665626
210.217511	8013.790362	26.670644
210.397774	8035.490788	26.675661
210.653780	8039.476882	26.680679
210.620924	8040.019587	26.685696
210.639956	8040.766388	26.690714
211.147835	8068.428502	26.695732
210.977875	8062.462844	26.700749
211.276304	8076.838371	26.705767
211.315309	8088.892879	26.710784
212.004078	8102.130923	26.715802
212.271425	8124.751303	26.720820
212.089877	8129.147002	26.725837
212.361200	8141.746013	26.730855
212.451605	8157.142291	26.735872
212.431104	8154.634426	26.740890
212.710445	8172.034156	26.745908
212.800689	8180.958461	26.750925
213.415810	8209.544410	26.755943
213.342976	8233.726622	26.760960
213.508282	8240.202064	26.765978
213.933742	8247.738850	26.770996
214.053718	8263.259523	26.776013
214.367590	8273.750696	26.781031
214.583689	8286.409379	26.786048
214.585413	8287.959401	26.791066
214.969892	8300.992756	26.796084
215.096429	8310.251429	26.801101
215.732331	8328.468272	26.806119
215.728196	8346.090785	26.811136
215.944233	8341.897352	26.816154
216.301100	8359.358501	26.821172
216.428521	8375.753234	26.826189
216.926819	8365.676674	26.831207
216.808234	8397.299070	26.836224
217.509821	8402.024446	26.841242
217.572622	8405.206818	26.846260
217.381198	8416.563176	26.851277
217.852666	8430.033616	26.856295
217.611935	8442.548265	26.861312
218.273821	8459.624237	26.866330
218.677328	8459.351086	26.871348
218.493054	8467.067688	26.876365
218.921349	8487.915501	26.881383
218.938630	8497.232544	26.886400
219.063202	8515.390089	26.891418
219.729207	8518.238666	26.896436
219.339430	8543.283622	26.901453
219.942160	8546.551522	26.906471
220.094891	8560.577422	26.911488
220.542097	8576.923363	26.916506
220.865180	8587.067394	26.921524
220.614630	8597.985436	26.926541
221.170661	8605.499990	26.931559
221.100347	8613.868965	26.936576
221.340648	8633.521553	26.941594
221.231200	8644.420207	26.946612
221.364906	8658.334330	26.951629
222.046530	8667.752616	26.956647
221.892108	8695.148906	26.961664
222.636378	8706.066981	26.966682
222.981343	8716.160994	26.971700
222.715040	8743.107169	26.976717
223.212399	8740.396109	26.981735
223.634337	8764.500369	26.986752
223.759023	8773.215273	26.991770
224.383565	8783.432417	26.996788
224.369670	8795.376474	27.001805
224.790952	8791.538104	27.006823
224.963175	8806.897830	27.011840
224.756065	8824.419762	27.016858
225.009572	8824.870974	27.021876
225.050224	8843.229484	27.026893
225.292389	8863.583947	27.031911
225.665337	8877.338127	27.036928
225.654902	8889.476261	27.041946
226.286408	8897.787499	27.046964
226.400151	8925.164999	27.051981
226.905888	8929.603909	27.056999
226.994242	8934.850057	27.062016
227.345963	8954.548405	27.067034
227.508592	8966.539781	27.072052
227.763660	8963.512721	27.077069
228.228758	8972.448678	27.082087
228.380650	8983.760421	27.087104
228.422506	8985.425972	27.092122
228.654379	8994.039749	27.097140
228.680132	9021.862104	27.102157
229.070993	9016.003347	27.107175
229.108856	9026.916475	27.112192
229.038743	9039.612106	27.117210
229.503862	9042.286063	27.122228
229.635432	9055.927526	27.127245
229.771011	9063.975901	27.132263
230.259143	9078.476120	27.137280
230.139779	9089.999851	27.142298
230.542318	9099.711957	27.147316
230.650987	9124.227845	27.152333
231.065470	9137.590150	27.157351
231.226813	9147.699078	27.162368
231.414772	9171.366076	27.167386
231.739372	9173.329103	27.172404
231.441559	9203.225211	27.177421
231.904681	9220.607478	27.182439
232.472270	9231.934876	27.187456
232.729138	9250.976521	27.192474
233.270411	9265.404303	27.197492
233.171311	9274.366077	27.202509
233.623314	9283.498173	27.207527
233.640904	9293.469492	27.212544
233.428200	9310.976336	27.217562
233.911774	9321.365267	27.222580
234.120863	9349.001858	27.227597
234.475785	9356.358628	27.232615
234.643346	9372.081264	27.237632
235.076626	9388.800605	27.242650
235.451976	9403.426142	27.247668
235.560180	9413.302181	27.252685
235.599983	9436.630134	27.257703
236.077107	9441.130648	27.262720
235.865744	9464.596330	27.267738
236.741298	9478.656213	27.272756
236.815955	9485.154256	27.277773
237.098135	9504.073843	27.282791
237.405677	9514.467618	27.287808
237.702016	9524.888464	27.292826
238.529621	9537.573747	27.297844
238.134835	9547.438596	27.302861
238.407766	9558.787430	27.307879
238.723934	9566.509950	27.312896
238.535881	9570.643992	27.317914
239.328607	9582.454321	27.322932
239.082626	9603.839046	27.327949
239.558077	9610.248735	27.332967
239.611491	9626.708207	27.337984
239.756038	9641.489551	27.343002
240.311556	9661.233025	27.348020
240.331656	9670.280853	27.353037
240.041344	9692.788570	27.358055
240.883812	9699.763061	27.363072
240.591732	9730.704622	27.368090
241.162716	9732.616693	27.373108
241.354538	9765.480832	27.378125
241.672645	9773.473350	27.383143
241.954484	9786.364197	27.388160
241.980457	9802.185535	27.393178
242.505532	9821.212608	27.398196
242.509279	9835.369854	27.403213
242.690899	9854.590901	27.408231
243.456727	9865.288770	27.413248
243.418824	9877.785926	27.418266
243.896170	9888.860872	27.423284
244.431376	9900.861389	27.428301
244.264489	9917.692449	27.433319
244.750004	9926.467211	27.438336
244.816674	9943.953706	27.443354
245.126537	9944.297147	27.448372
245.540048	9947.993729	27.453389
245.667846	9948.821093	27.458407
245.982861	9975.582502	27.463424
245.730366	9982.035636	27.468442
246.200687	9988.410875	27.473460
246.473044	10005.927203	27.478477
246.449340	10007.945629	27.483495
247.016686	10024.194381	27.488512
246.990209	10037.449233	27.493530
247.232610	10050.620984	27.498548
247.593612	10068.798661	27.503565
247.566187	10081.251698	27.508583
247.766086	10094.213867	27.513600
247.900245	10122.028059	27.518618
248.226834	10134.138917	27.523636
248.345317	10159.797113	27.528653
248.547342	10175.458107	27.533671
249.074303	10198.695494	27.538688
249.038312	10220.288927	27.543706
249.751240	10234.422094	27.548724
250.279818	10252.016815	27.553741
250.345065	10275.820777	27.558759
250.558045	10285.441293	27.563776
250.738485	10305.985067	27.568794
250.934943	10325.446875	27.573812
251.058556	10337.579668	27.578829
251.584468	10358.739925	27.583847
252.107050	10361.919846	27.588864
252.203066	10389.481614	27.593882
252.489608	10390.636465	27.598900
252.669654	10414.659557	27.603917
252.469300	10428.133382	27.608935
253.464733	10438.844052	27.613952
253.328666	10458.542270	27.618970
253.908252	10466.996073	27.623988
254.177915	10491.171468	27.629005
254.615922	10493.610658	27.634023
254.663037	10502.031293	27.639040
255.012023	10519.887665	27.644058
255.175916	10518.172998	27.649076
255.809823	10531.330758	27.654093
255.683274	10546.680153	27.659111
255.959607	10544.921659	27.664128
255.768205	10571.373174	27.669146
256.184126	10578.815741	27.674164
256.376933	10603.820242	27.679181
256.398813	10613.373318	27.684199
257.060099	10636.712009	27.689216
256.752585	10647.498262	27.694234
257.115785	10664.775731	27.699252
257.577885	10691.653433	27.704269
257.915278	10711.092378	27.709287
258.280372	10724.704480	27.714304
258.629411	10741.694444	27.719322
258.950178	10756.741514	27.724340
259.137814	10766.875471	27.729357
259.662887	10775.273858	27.734375
259.990749	10792.688099	27.739392
260.080829	10809.899057	27.744410
260.598076	10811.606649	27.749428
260.754834	10820.710500	27.754445
260.928687	10827.422722	27.759463
261.282125	10836.475116	27.764480
261.110420	10850.667810	27.769498
261.854221	10847.048177	27.774516
262.160200	10863.879946	27.779533
262.171287	10877.153693	27.784551
262.275302	10875.811319	27.789568
262.555021	10893.088670	27.794586
262.670379	10915.824812	27.799604
262.938191	10920.276094	27.804621
262.978173	10938.388925	27.809639
263.639836	10942.644233	27.814656
263.757500	10968.604030	27.819674
264.025346	10978.285212	27.824692
264.094083	10992.652531	27.829709
264.459107	11019.026853	27.834727
264.779069	11022.675355	27.839744
264.905390	11031.362063	27.844762
265.139116	11052.279298	27.849780
265.492132	11060.225712	27.854797
265.833988	11074.207532	27.859815
266.329251	11085.581310	27.864832
266.597798	11113.558541	27.869850
266.626163	11126.243450	27.874868
266.896740	11136.272518	27.879885
266.943361	11145.607510	27.884903
267.684989	11170.269921	27.889920
267.730691	11184.516738	27.894938
267.787007	11207.151183	27.899956
268.121126	11226.944263	27.904973
267.803789	11242.828568	27.909991
268.661664	11258.819328	27.915008
268.559184	11282.309019	27.920026
269.278845	11303.481782	27.925044
269.295218	11321.222340	27.930061
269.545914	11339.308619	27.935079
270.036752	11364.600605	27.940096
270.097353	11385.702932	27.945114
270.643010	11408.707332	27.950132
271.056984	11414.037482	27.955149
271.300579	11434.409932	27.960167
271.963504	11442.081475	27.965184
271.953082	11463.474573	27.970202
271.970979	11470.271182	27.975220
272.795013	11482.868787	27.980237
272.747989	11506.299197	27.985255
273.071357	11511.050304	27.990272
273.166398	11535.311320	27.995290
273.660984	11542.626281	28.000308
274.531544	11550.159504	28.005325
274.316309	11565.349629	28.010343
274.608337	11569.286525	28.015360
274.669525	11584.864258	28.020378
274.793733	11600.601761	28.025396
275.560695	11621.641050	28.030413
275.181660	11633.421520	28.035431
275.523437	11653.470712	28.040448
275.776052	11668.184812	28.045466
276.193927	11687.777072	28.050484
276.649948	11699.794409	28.055501
276.623091	11722.738018	28.060519
276.985200	11730.380702	28.065536
277.211049	11751.903683	28.070554
277.434451	11770.897907	28.075572
277.899310	11778.967988	28.080589
277.932652	11810.827208	28.085607
278.179217	11820.958377	28.090624
278.382119	11837.746766	28.095642
278.223874	11863.028787	28.100660
279.038163	11881.641684	28.105677
279.158230	11901.420595	28.110695
279.768927	11915.815635	28.115712
279.941326	11938.996035	28.120730
280.224223	11951.024882	28.125748
280.519565	11972.189969	28.130765
280.708838	11980.521657	28.135783
281.325815	11996.127551	28.140800
281.510840	12017.295199	28.145818
282.160264	12032.528586	28.150836
282.324550	12044.811936	28.155853
282.085687	12059.480101	28.160871
282.822315	12061.751918	28.165888
283.091782	12075.421963	28.170906
282.946020	12075.227083	28.175924
283.442454	12094.341956	28.180941
283.405281	12117.399716	28.185959
283.588402	12128.499698	28.190976
283.843792	12149.425796	28.195994
284.122386	12165.105199	28.201012
284.646513	12190.730202	28.206029
284.883124	12213.559980	28.211047
285.071618	12235.876142	28.216064
285.448100	12252.800119	28.221082
285.850300	12268.347276	28.226100
286.341132	12290.364482	28.231117
286.314253	12317.978239	28.236135
286.691178	12330.396804	28.241152
287.016731	12354.271044	28.246170
287.210089	12372.100069	28.251188
287.595335	12389.348945	28.256205
288.157557	12396.780747	28.261223
288.156532	12423.772659	28.266240
288.415506	12437.838717	28.271258
288.722915	12460.256848	28.276276
289.253171	12477.899426	28.281293
289.440503	12497.984683	28.286311
289.758450	12506.679861	28.291328
290.187241	12524.181694	28.296346
290.139888	12559.464395	28.301364
290.588624	12558.264964	28.306381
290.960542	12583.083708	28.311399
291.144568	12586.427283	28.316416
291.319571	12613.199688	28.321434
291.446725	12627.052920	28.326452
292.382743	12643.840564	28.331469
292.317322	12674.665119	28.336487
292.696412	12678.706071	28.341504
292.956141	12702.197741	28.346522
293.227745	12718.253902	28.351540
293.836308	12732.442005	28.356557
294.145619	12749.275184	28.361575
294.262077	12751.826261	28.366592
294.827743	12775.349345	28.371610
294.995418	12789.716062	28.376628
295.204944	12806.737593	28.381645
295.291677	12822.014434	28.386663
296.028745	12833.785954	28.391680
295.943247	12853.918386	28.396698
296.166267	12883.928118	28.401716
296.870747	12886.374005	28.406733
296.806194	12903.404757	28.411751
296.891235	12920.926096	28.416768
297.233342	12944.065655	28.421786
297.632142	12963.528661	28.426804
298.310331	12972.065177	28.431821
298.110091	13001.604639	28.436839
298.720622	13017.956431	28.441856
298.942383	13033.564131	28.446874
298.961542	13043.732130	28.451892
299.821740	13061.087491	28.456909
299.828307	13076.896326	28.461927
300.136678	13086.852582	28.466944
300.233714	13101.719810	28.471962
300.400361	13117.973397	28.476980
301.055902	13126.450706	28.481997
301.103346	13150.710980	28.487015
301.124785	13162.383711	28.492032
301.757775	13173.677857	28.497050
301.773436	13193.786084	28.502068
302.517928	13212.747749	28.507085
302.651543	13225.944822	28.512103
303.065280	13256.549329	28.517120
303.142744	13276.598574	28.522138
303.310075	13286.860396	28.527156
303.906764	13309.178232	28.532173
304.014763	13332.554090	28.537191
304.428656	13359.248780	28.542208
304.597909	13362.602840	28.547226
304.679663	13398.868305	28.552244
304.991018	13417.115489	28.557261
305.452649	13447.789651	28.562279
305.770743	13468.626693	28.567296
306.011989	13488.160532	28.572314
306.354672	13516.854586	28.577332
306.955553	13532.198285	28.582349
307.289946	13570.096014	28.587367
307.488343	13582.088049	28.592384
307.899552	13602.304667	28.597402
307.969717	13618.218547	28.602420
308.585445	13630.753029	28.607437
308.814442	13664.052319	28.612455
309.140175	13675.403977	28.617472
309.625463	13696.809365	28.622490
309.839223	13698.326386	28.627508
310.262715	13724.098121	28.632525
310.531627	13745.397547	28.637543
310.808998	13759.959723	28.642560
311.237323	13778.093390	28.647578
311.101797	13799.945242	28.652596
311.573194	13817.929983	28.657613
311.660463	13843.767014	28.662631
312.182030	13863.007469	28.667648
312.792332	13879.946448	28.672666
312.554291	13907.063571	28.677684
313.186662	13923.842916	28.682701
313.626729	13945.951145	28.687719
313.836930	13958.307142	28.692736
314.403404	13981.508751	28.697754
314.713020	13999.060268	28.702772
314.818760	14018.831512	28.707789
315.291340	14034.239475	28.712807
315.428872	14053.835287	28.717824
316.201283	14069.144798	28.722842
315.831106	14096.964955	28.727860
316.343538	14116.308088	28.732877
316.354788	14135.582897	28.737895
316.929294	14153.506812	28.742912
317.628401	14175.425904	28.747930
317.768661	14196.971013	28.752948
317.990237	14210.499478	28.757965
317.966651	14236.640743	28.762983
318.210954	14255.251424	28.768000
318.582032	14282.719100	28.773018
318.916138	14300.771227	28.778036
319.293495	14315.848483	28.783053
319.712868	14354.938079	28.788071
319.941220	14380.760485	28.793088
320.420528	14393.036019	28.798106
320.707242	14417.786551	28.803124
321.122107	14439.874403	28.808141
321.435408	14457.301291	28.813159
321.193710	14482.421500	28.818176
321.965691	14491.865306	28.823194
321.916832	14529.422062	28.828212
322.266775	14538.529119	28.833229
322.717980	14563.317264	28.838247
323.158978	14588.214311	28.843264
323.632722	14603.334194	28.848282
324.088196	14624.060133	28.853300
324.257178	14651.533508	28.858317
324.467320	14666.561535	28.863335
324.493957	14687.163097	28.868352
325.128089	14704.062739	28.873370
325.527718	14734.853601	28.878388
325.971278	14755.559613	28.883405
326.453772	14765.915201	28.888423
326.356613	14796.815199	28.893440
326.751438	14809.770149	28.898458
327.491844	14833.655007	28.903476
327.663739	14849.680910	28.908493
327.733684	14859.702931	28.913511
328.125366	14883.344542	28.918528
328.655205	14906.931798	28.923546
328.716235	14933.022339	28.928564
329.020659	14954.000658	28.933581
329.764993	14986.348892	28.938599
329.598798	15006.011874	28.943616
329.947916	15029.353394	28.948634
330.283979	15056.315918	28.953652
330.604094	15076.885154	28.958669
330.828695	15099.936886	28.963687
331.149846	15123.417141	28.968704
331.907742	15150.751320	28.973722
331.815179	15181.085442	28.978740
332.168467	15202.914992	28.983757
332.918642	15224.355771	28.988775
333.196017	15244.410584	28.993792
333.733852	15254.467311	28.998810
334.007908	15280.672878	29.003828
334.099956	15301.850714	29.008845
334.529783	15328.199224	29.013863
334.641337	15356.622674	29.018880
335.246501	15370.433788	29.023898
335.450324	15402.895948	29.028916
335.728832	15434.360702	29.033933
335.987320	15442.879727	29.038951
336.246301	15485.212379	29.043968
336.711539	15499.198074	29.048986
336.880501	15532.323525	29.054004
337.474292	15563.537744	29.059021
337.873257	15583.380551	29.064039
338.158865	15604.575601	29.069056
338.748045	15630.942354	29.074074
339.272779	15652.556559	29.079092
338.970456	15679.895295	29.084109
339.669542	15700.867565	29.089127
339.835325	15721.534080	29.094144
340.380117	15748.603473	29.099162
340.544329	15762.371262	29.104180
340.699592	15783.298094	29.109197
341.694149	15808.296091	29.114215
341.646159	15832.531987	29.119232
341.536192	15851.466339	29.124250
342.008820	15874.279500	29.129268
342.426121	15899.319587	29.134285
342.860749	15927.067942	29.139303
343.272230	15947.489166	29.144320
343.669931	15970.068971	29.149338
344.015805	15990.851029	29.154356
344.479806	16006.424621	29.159373
344.677629	16028.637226	29.164391
344.948391	16046.261989	29.169408
345.361969	16058.712005	29.174426
345.755105	16091.576074	29.179444
346.083037	16113.789327	29.184461
346.343019	16126.789704	29.189479
346.271039	16156.969315	29.194496
346.778247	16180.212219	29.199514
347.212771	16205.097024	29.204532
347.504731	16231.093074	29.209549
348.283825	16251.546831	29.214567
348.286199	16281.717515	29.219584
348.684891	16302.494377	29.224602
349.175511	16320.158704	29.229620
349.300074	16348.091492	29.234637
349.896853	16367.007189	29.239655
349.750607	16380.257846	29.244672
350.821363	16409.418093	29.249690
350.930339	16435.685920	29.254708
351.178168	16457.509368	29.259725
351.513570	16479.302588	29.264743
351.909296	16511.145639	29.269760
352.360903	16535.610402	29.274778
352.776159	16554.988259	29.279796
353.014087	16583.657719	29.284813
353.355896	16603.590030	29.289831
354.065217	16633.150972	29.294848
354.004791	16658.462010	29.299866
354.488358	16678.036775	29.304884
354.991682	16700.002682	29.309901
355.216338	16715.503066	29.314919
355.725297	16749.736414	29.319936
356.050991	16763.530329	29.324954
356.764877	16786.191328	29.329972
356.624440	16811.755441	29.334989
357.112114	16829.119727	29.340007
357.451093	16863.433462	29.345024
357.518246	16880.746026	29.350042
357.985250	16901.428791	29.355060
358.147134	16932.193750	29.360077
358.558533	16955.357448	29.365095
359.136726	16981.521684	29.370112
359.487315	17018.414254	29.375130
359.725045	17047.719809	29.380148
359.837611	17078.959795	29.385165
360.419466	17098.142048	29.390183
360.765513	17134.400366	29.395200
361.086135	17160.694213	29.400218
361.444691	17186.802121	29.405236
361.676306	17215.295592	29.410253
362.269055	17243.905893	29.415271
362.494977	17270.305439	29.420288
362.905397	17294.809670	29.425306
363.489570	17327.780143	29.430324
363.387612	17358.085125	29.435341
364.398822	17376.302846	29.440359
364.512934	17402.806231	29.445376
364.852865	17427.060648	29.450394
365.051913	17454.495875	29.455412
365.207203	17484.540973	29.460429
365.988708	17506.269594	29.465447
366.270720	17535.868192	29.470464
366.715093	17566.874473	29.475482
367.710524	17575.584755	29.480500
367.814596	17618.903785	29.485517
368.433140	17616.947625	29.490535
368.945412	17644.145313	29.495552
369.091495	17655.819513	29.500570
369.411944	17665.596845	29.505588
369.353955	17693.930986	29.510605
369.617385	17703.684674	29.515623
369.894794	17729.705978	29.520640
370.219461	17750.058673	29.525658
370.315359	17776.478966	29.530676
370.495563	17803.831187	29.535693
370.893638	17831.707017	29.540711
371.275206	17864.431489	29.545728
371.857824	17899.162622	29.550746
372.213040	17923.006944	29.555764
372.567801	17959.063839	29.560781
373.165408	17985.335220	29.565799
373.442534	18005.073411	29.570816
373.584761	18041.961752	29.575834
374.190136	18063.989824	29.580852
374.451797	18103.002468	29.585869
374.760420	18124.792825	29.590887
375.512711	18164.607212	29.595904
375.530248	18196.134593	29.600922
376.330069	18232.916098	29.605940
376.505960	18256.571452	29.610957
377.016337	18281.077935	29.615975
377.490678	18306.093305	29.620992
377.672344	18336.204938	29.626010
378.597454	18362.097963	29.631028
378.401556	18394.528089	29.636045
378.637394	18414.741807	29.641063
379.251517	18445.470975	29.646080
379.335668	18478.655756	29.651098
380.134951	18504.438982	29.656116
380.550982	18541.795463	29.661133
380.717051	18550.411788	29.666151
381.309383	18589.842208	29.671168
381.614631	18619.326956	29.676186
381.975142	18640.783070	29.681204
382.299259	18674.969002	29.686221
382.695877	18702.376739	29.691239
383.337479	18731.826513	29.696256
383.520292	18765.972958	29.701274
383.853030	18800.706338	29.706292
384.290579	18823.400095	29.711309
384.701316	18853.750635	29.716327
385.415442	18891.121623	29.721344
385.277306	18923.570014	29.726362
386.156621	18937.769134	29.731380
386.343864	18981.052710	29.736397
386.694645	19001.262303	29.741415
386.976276	19021.732453	29.746432
387.244359	19060.650104	29.751450
387.894054	19074.023412	29.756468
387.772173	19117.691146	29.761485
388.362195	19134.733487	29.766503
388.643005	19171.658141	29.771520
388.922440	19211.785036	29.776538
389.530585	19237.547430	29.781556
389.701926	19276.122142	29.786573
390.133371	19308.729259	29.791591
390.504115	19344.159037	29.796608
391.205708	19383.752974	29.801626
391.713500	19411.606980	29.806644
392.100127	19446.504626	29.811661
392.704931	19473.666339	29.816679
392.927773	19502.237690	29.821696
393.253995	19531.829359	29.826714
394.086985	19550.819957	29.831732
394.378266	19574.295692	29.836749
394.488839	19594.031796	29.841767
395.162309	19621.202879	29.846784
395.036123	19638.416294	29.851802
395.353534	19651.592808	29.856820
395.590382	19692.082631	29.861837
396.019280	19718.007862	29.866855
396.425503	19751.081952	29.871872
396.699365	19785.109774	29.876890
397.170002	19815.664984	29.881908
397.146809	19851.131075	29.886925
397.480523	19891.952198	29.891943
398.172285	19920.399358	29.896960
398.366890	19960.715511	29.901978
399.405684	20001.809632	29.906996
399.372375	20045.720528	29.912013
399.751204	20075.815270	29.917031
400.341496	20110.601761	29.922048
400.717600	20148.351552	29.927066
401.437061	20171.505000	29.932084
402.219862	20200.495694	29.937101
402.796895	20226.092907	29.942119
403.318673	20259.861510	29.947136
403.194450	20282.415300	29.952154
403.933043	20300.287201	29.957172
404.084558	20338.834526	29.962189
404.481855	20363.375391	29.967207
404.728415	20391.252186	29.972224
405.209531	20420.372020	29.977242
405.767101	20438.018610	29.982260
406.170248	20475.469828	29.987277
406.646929	20503.951997	29.992295
407.005954	20529.185283	29.997312
407.453104	20560.157243	30.002330
408.380238	20574.114928	30.007348
408.527569	20615.167311	30.012365
408.812077	20633.256617	30.017383
409.299099	20650.565087	30.022400
409.275519	20698.461885	30.027418
410.259913	20722.841470	30.032436
410.156593	20750.854021	30.037453
410.530069	20772.290223	30.042471
411.406812	20811.560553	30.047488
411.328819	20834.652962	30.052506
411.760452	20860.659916	30.057524
411.965076	20894.146446	30.062541
412.545751	20928.524707	30.067559
412.961308	20959.206211	30.072576
412.911005	20997.649693	30.077594
413.244371	21036.808657	30.082612
413.987361	21075.300773	30.087629
414.155582	21119.447575	30.092647
414.945391	21145.115037	30.097664
415.078248	21194.661819	30.102682
415.767248	21227.406628	30.107700
416.061345	21274.208695	30.112717
416.452821	21312.256551	30.117735
416.967503	21329.471269	30.122752
417.598379	21364.171646	30.127770
417.606798	21395.761721	30.132788
418.221005	21427.388777	30.137805
418.838452	21463.715622	30.142823
419.266467	21493.475219	30.147840
419.676670	21536.777347	30.152858
420.332629	21564.384927	30.157876
420.828903	21596.862766	30.162893
421.037283	21622.595645	30.167911
421.163288	21647.154896	30.172928
421.682571	21684.315222	30.177946
422.281007	21709.444429	30.182964
422.951996	21732.546559	30.187981
423.230061	21755.155571	30.192999
423.518133	21778.291175	30.198016
423.770208	21813.865625	30.203034
424.602916	21842.322673	30.208052
424.616043	21868.381518	30.213069
425.315033	21901.900182	30.218087
425.342326	21921.545571	30.223104
425.491971	21963.439693	30.228122
426.277781	21980.042564	30.233140
426.595958	22016.164683	30.238157
426.873074	22055.109832	30.243175
427.323797	22084.593926	30.248192
427.432533	22127.162209	30.253210
428.084403	22157.652255	30.258228
428.354913	22199.244709	30.263245
428.980439	22249.164009	30.268263
429.660127	22276.576455	30.273280
429.694116	22321.458170	30.278298
430.351223	22345.787050	30.283316
430.809176	22394.428900	30.288333
431.178235	22429.196868	30.293351
431.816144	22463.411097	30.298368
432.135000	22502.525394	30.303386
432.537196	22530.794668	30.308404
433.128109	22573.467187	30.313421
433.236311	22623.414856	30.318439
433.848278	22643.476798	30.323456
434.631887	22691.171530	30.328474
434.728633	22727.420111	30.333492
435.138786	22762.054234	30.338509
435.871242	22809.775110	30.343527
436.549612	22847.234916	30.348544
436.863005	22878.469789	30.353562
437.232519	22894.797119	30.358580
437.800919	22945.670892	30.363597
437.942772	22984.503367	30.368615
438.813335	23009.507474	30.373632
438.947069	23045.433657	30.378650
439.506609	23078.520428	30.383668
439.728874	23102.786744	30.388685
439.935502	23146.743235	30.393703
440.738338	23179.600713	30.398720
441.025868	23215.452919	30.403738
441.153484	23250.724555	30.408756
441.981631	23292.150130	30.413773
442.376888	23339.136686	30.418791
442.815579	23363.383326	30.423808
443.458353	23418.634766	30.428826
443.306781	23446.563551	30.433844
443.894863	23482.379196	30.438861
444.277201	23535.657222	30.443879
444.987083	23564.970112	30.448896
444.664820	23615.043961	30.453914
445.586119	23650.647122	30.458932
446.295770	23696.809932	30.463949
446.366844	23744.270719	30.468967
446.928654	23783.885493	30.473984
447.465005	23824.450747	30.479002
447.841592	23870.766917	30.484020
448.544832	23918.013183	30.489037
448.728671	23960.012212	30.494055
449.543438	23990.388704	30.499072
449.710774	24035.298592	30.504090
450.391236	24072.077914	30.509108
450.937092	24100.502643	30.514125
451.114210	24136.838689	30.519143
451.703574	24176.680054	30.524160
452.118777	24208.532888	30.529178
452.811946	24243.206765	30.534196
453.613059	24256.034007	30.539213
453.578983	24290.055597	30.544231
454.481998	24315.813218	30.549248
454.451699	24339.627908	30.554266
455.053850	24377.565755	30.559284
455.801823	24412.962641	30.564301
456.080787	24444.545136	30.569319
456.508804	24477.654810	30.574336
456.480756	24513.110934	30.579354
457.179101	24550.538061	30.584372
457.355306	24585.547353	30.589389
458.113789	24633.697979	30.594407
458.469002	24665.202026	30.599424
458.479187	24708.698272	30.604442
459.381135	24747.801651	30.609460
459.833215	24789.140121	30.614477
460.141482	24833.656595	30.619495
460.544501	24874.716366	30.624512
460.694689	24920.009902	30.629530
461.261828	24960.273113	30.634548
461.933144	25007.300573	30.639565
462.353189	25050.272508	30.644583
463.100864	25100.583669	30.649600
463.482129	25134.424650	30.654618
463.643620	25184.053982	30.659636
464.369330	25213.371814	30.664653
464.613679	25261.076227	30.669671
465.186387	25302.209873	30.674688
465.714802	25358.096833	30.679706
466.279755	25399.298234	30.684724
466.936356	25449.757966	30.689741
467.261991	25482.233598	30.694759
467.799390	25520.676749	30.699776
468.124068	25571.258003	30.704794
468.754070	25617.514873	30.709812
469.534133	25654.028771	30.714829
469.521631	25699.556305	30.719847
469.949319	25735.942587	30.724864
470.465022	25781.651043	30.729882
470.871695	25817.214553	30.734900
471.630068	25864.028076	30.739917
472.110069	25915.638172	30.744935
472.726075	25947.738584	30.749952
473.344976	25991.947996	30.754970
473.621889	26031.488934	30.759988
474.312868	26056.489376	30.765005
474.574208	26101.373332	30.770023
475.521566	26136.024746	30.775040
475.974454	26170.764362	30.780058
475.935617	26207.673603	30.785076
476.404826	26245.871000	30.790093
476.956119	26291.171159	30.795111
477.582437	26328.812807	30.800128
477.886568	26365.719255	30.805146
478.206331	26408.887819	30.810164
478.778421	26449.431282	30.815181
479.144079	26503.774843	30.820199
479.716597	26531.984688	30.825216
480.197932	26579.208755	30.830234
480.684233	26627.078788	30.835252
481.366895	26663.926389	30.840269
481.497865	26704.742176	30.845287
481.817246	26738.252711	30.850304
482.209101	26782.060094	30.855322
482.715191	26828.782341	30.860340
483.356543	26864.015807	30.865357
484.015409	26905.867707	30.870375
484.450747	26938.889424	30.875392
485.429908	26970.120941	30.880410
485.545078	27011.981050	30.885428
486.469293	27047.521387	30.890445
486.398398	27083.838441	30.895463
487.054396	27113.559054	30.900480
487.381627	27153.608418	30.905498
488.295973	27185.381010	30.910516
488.685287	27226.177357	30.915533
488.847638	27267.500312	30.920551
489.697831	27296.233275	30.925568
489.978926	27330.924787	30.930586
490.213160	27376.721893	30.935604
490.957567	27411.523018	30.940621
491.168257	27457.122339	30.945639
491.250770	27493.058395	30.950656
491.645464	27544.611756	30.955674
492.362699	27592.086616	30.960692
493.023342	27640.750798	30.965709
492.964381	27691.972719	30.970727
493.745087	27742.743537	30.975744
494.424467	27795.537625	30.980762
495.016508	27841.816192	30.985780
495.489484	27877.593791	30.990797
495.784710	27936.694948	30.995815
496.439215	27977.704705	31.000832
497.435593	28021.875768	31.005850
497.466138	28068.490762	31.010868
498.428203	28109.727550	31.015885
498.815042	28164.883565	31.020903
499.389638	28202.222371	31.025920
500.222312	28248.774520	31.030938
500.482332	28283.234813	31.035956
500.946690	28321.844547	31.040973
501.267290	28374.068811	31.045991
501.743074	28415.389947	31.051008
502.574873	28464.567576	31.056026
502.807690	28506.455977	31.061044
503.454590	28542.215627	31.066061
504.059317	28597.030939	31.071079
504.861077	28630.717686	31.076096
504.930436	28671.220183	31.081114
505.286700	28713.145440	31.086132
505.540663	28764.804569	31.091149
505.993056	28818.522668	31.096167
506.895596	28864.017496	31.101184
506.693080	28909.474460	31.106202
507.693825	28969.068100	31.111220
508.537967	29009.682944	31.116237
508.627959	29055.284331	31.121255
509.234235	29108.905297	31.126272
509.926218	29141.904504	31.131290
510.762603	29188.521646	31.136308
511.182131	29233.437989	31.141325
511.410097	29279.332619	31.146343
512.100651	29315.152883	31.151360
512.691196	29356.267959	31.156378
513.311480	29416.077516	31.161396
513.857336	29443.864278	31.166413
513.959722	29498.402721	31.171431
514.383268	29538.205004	31.176448
515.006686	29581.422684	31.181466
515.556947	29631.855384	31.186484
515.822094	29679.729390	31.191501
516.417765	29712.941221	31.196519
517.363339	29765.078842	31.201536
517.784374	29796.685439	31.206554
518.344208	29838.876278	31.211572
518.694691	29867.021006	31.216589
519.126382	29901.869389	31.221607
519.460882	29949.268865	31.226624
520.087030	29986.618732	31.231642
520.641044	30035.717391	31.236660
521.348349	30079.853158	31.241677
521.819027	30114.906901	31.246695
522.106483	30160.071481	31.251712
523.153543	30191.764507	31.256730
523.133098	30246.934527	31.261748
523.790197	30295.234393	31.266765
524.261341	30338.403412	31.271783
524.400050	30382.132362	31.276800
525.039132	30422.819124	31.281818
525.581439	30474.785794	31.286836
526.289765	30522.374214	31.291853
526.925451	30573.344477	31.296871
527.580384	30621.266979	31.301888
527.632567	30663.786745	31.306906
527.976656	30717.509648	31.311924
528.600438	30766.983735	31.316941
529.122298	30819.513273	31.321959
529.884444	30878.969887	31.326976
530.753285	30920.140389	31.331994
530.798953	30972.373706	31.337012
531.575711	31015.790407	31.342029
532.278388	31070.215459	31.347047
532.568350	31128.753992	31.352064
533.458891	31170.227547	31.357082
533.830885	31222.540128	31.362100
534.609199	31270.188404	31.367117
535.047135	31323.033078	31.372135
535.731179	31368.548473	31.377152
536.160749	31413.408771	31.382170
536.360091	31464.125658	31.387188
536.998510	31510.216922	31.392205
537.723423	31560.944938	31.397223
538.380253	31612.627808	31.402240
538.915359	31651.384617	31.407258
539.442446	31700.852079	31.412276
539.727080	31753.067092	31.417293
540.311429	31795.075550	31.422311
540.672957	31853.658280	31.427328
541.009282	31897.885229	31.432346
541.224146	31952.967994	31.437364
542.273996	32011.058705	31.442381
542.836519	32071.091935	31.447399
543.369711	32138.725325	31.452416
544.257336	32182.464180	31.457434
544.665271	32227.459493	31.462452
545.332212	32282.610474	31.467469
545.628511	32320.373274	31.472487
546.534702	32379.896299	31.477504
547.209713	32426.678097	31.482522
547.549010	32469.145223	31.487540
548.636063	32521.554742	31.492557
548.767852	32568.275332	31.497575
548.947639	32617.247448	31.502592
549.683919	32656.922978	31.507610
550.218618	32723.589602	31.512628
551.040411	32770.846594	31.517645
551.682755	32807.395090	31.522663
552.162399	32856.236204	31.527680
552.403508	32897.534112	31.532698
553.138229	32947.765896	31.537716
553.678436	32983.675296	31.542733
554.100712	33028.768088	31.547751
554.301488	33085.361905	31.552768
554.887301	33117.382652	31.557786
555.285906	33168.226057	31.562804
555.909417	33226.605872	31.567821
556.424190	33277.834288	31.572839
556.733674	33323.848998	31.577856
557.848572	33370.371158	31.582874
557.983261	33429.053412	31.587892
558.422039	33473.191591	31.592909
559.194342	33532.933125	31.597927
559.103290	33589.826124	31.602944
560.264657	33646.395318	31.607962
560.389803	33704.319533	31.612980
561.031254	33770.956632	31.617997
561.773956	33825.819001	31.623015
562.438266	33896.122890	31.628032
563.088147	33940.546024	31.633050
563.823306	34007.654485	31.638068
564.247319	34060.089881	31.643085
565.217084	34107.726719	31.648103
565.441202	34167.270745	31.653120
566.301422	34215.866420	31.658138
566.547419	34281.677763	31.663156
567.325979	34322.145270	31.668173
567.950261	34381.832082	31.673191
568.117154	34445.732065	31.678208
569.111158	34489.525264	31.683226
569.289883	34557.289591	31.688244
569.756937	34611.669795	31.693261
570.356532	34671.443708	31.698279
571.218324	34727.472589	31.703296
571.891850	34789.800396	31.708314
572.413479	34847.545934	31.713332
572.874529	34896.136914	31.718349
573.626425	34957.022707	31.723367
574.094874	35020.044831	31.728384
574.911345	35074.589540	31.733402
575.417010	35134.746625	31.738420
575.684620	35199.882382	31.743437
576.941256	35245.278232	31.748455
577.257685	35309.835079	31.753472
577.930233	35354.138039	31.758490
578.264622	35415.040810	31.763508
578.841490	35472.444679	31.768525
579.549692	35522.183119	31.773543
579.972477	35582.475342	31.778560
580.860106	35636.770125	31.783578
581.172843	35700.685149	31.788596
581.667391	35760.732547	31.793613
582.643049	35810.976688	31.798631
582.893112	35872.112723	31.803648
583.678245	35926.456898	31.808666
584.272768	35984.061464	31.813684
584.676883	36035.164570	31.818701
585.369351	36087.308973	31.823719
585.671960	36151.842713	31.828736
586.587681	36198.714480	31.833754
586.649320	36270.856935	31.838772
587.691303	36328.338067	31.843789
588.622156	36385.310689	31.848807
588.788676	36445.648194	31.853824
589.603852	36493.777743	31.858842
589.964281	36560.133962	31.863860
590.496616	36607.360593	31.868877
591.040984	36666.803079	31.873895
591.742686	36733.523246	31.878912
592.633432	36767.971389	31.883930
592.984982	36817.185346	31.888948
593.775799	36868.441450	31.893965
594.071130	36921.111621	31.898983
594.689552	36974.296618	31.904000
595.133612	37019.724073	31.909018
595.682830	37080.495907	31.914036
596.376247	37140.890582	31.919053
596.693340	37183.833350	31.924071
596.914309	37252.711817	31.929088
597.343173	37312.358595	31.934106
598.200277	37373.468699	31.939124
598.596095	37447.293369	31.944141
599.680848	37508.839717	31.949159
599.700302	37576.161940	31.954176
600.816808	37634.960571	31.959194
601.217245	37708.368893	31.964212
601.645319	37777.726417	31.969229
602.612565	37834.009475	31.974247
603.112537	37905.814444	31.979264
603.896627	37972.307737	31.984282
604.303007	38032.238361	31.989300
604.764329	38112.932811	31.994317
605.743423	38170.363904	31.999335
605.984964	38245.113771	32.004352
606.989862	38301.120585	32.009370
607.710225	38368.844278	32.014388
608.268159	38437.472610	32.019405
609.504951	38487.355849	32.024423
609.760017	38564.702615	32.029440
610.652806	38608.064853	32.034458
611.100465	38678.719906	32.039476
611.396661	38742.793569	32.044493
612.084585	38803.762850	32.049511
612.742071	38868.225414	32.054528
613.424670	38929.899918	32.059546
613.862712	38995.586123	32.064564
614.516930	39061.003206	32.069581
615.446708	39124.490416	32.074599
615.952544	39190.200824	32.079616
616.295365	39248.715986	32.084634
616.940013	39314.864748	32.089652
617.715175	39391.305062	32.094669
618.221598	39447.801919	32.099687
618.866527	39521.552716	32.104704
619.356631	39584.991151	32.109722
619.835557	39656.392941	32.114740
620.463955	39735.166542	32.119757
621.323029	39788.512488	32.124775
621.823937	39864.924385	32.129792
622.323062	39934.903367	32.134810
623.070126	40000.744075	32.139828
623.513808	40063.216391	32.144845
624.472908	40145.185388	32.149863
624.858929	40214.729564	32.154880
625.508878	40290.853396	32.159898
626.055675	40349.527723	32.164916
626.811883	40425.584023	32.169933
627.824654	40472.905323	32.174951
628.484802	40550.584880	32.179968
629.138673	40610.852339	32.184986
629.910517	40673.256645	32.190004
630.414500	40740.084128	32.195021
631.420962	40791.309247	32.200039
631.510577	40865.106787	32.205056
632.069913	40928.617318	32.210074
632.696816	40989.455568	32.215092
633.297590	41059.352547	32.220109
633.760952	41121.064356	32.225127
634.591003	41177.939170	32.230144
634.707682	41230.531316	32.235162
635.365349	41292.217864	32.240180
635.945523	41362.406683	32.245197
636.783190	41420.022883	32.250215
637.260767	41493.954479	32.255232
637.920934	41565.494679	32.260250
638.524430	41631.778532	32.265268
639.077190	41704.811392	32.270285
639.930704	41770.981767	32.275303
640.182596	41847.291516	32.280320
640.881459	41917.046060	32.285338
641.398134	41980.327314	32.290356
642.512294	42063.639891	32.295373
643.154351	42127.870148	32.300391
643.322944	42198.875311	32.305408
644.336239	42271.209088	32.310426
644.955638	42344.053477	32.315444
645.651698	42431.632785	32.320461
646.381386	42496.718051	32.325479
647.020519	42564.682134	32.330496
647.546514	42643.207220	32.335514
648.545783	42703.171760	32.340532
649.024888	42788.389125	32.345549
649.709932	42852.611614	32.350567
650.270093	42926.996206	32.355584
650.671763	43011.804323	32.360602
651.495657	43087.601442	32.365620
652.101014	43158.762172	32.370637
653.134712	43233.050698	32.375655
653.599570	43308.377677	32.380672
654.197324	43389.145224	32.385690
654.957333	43456.284271	32.390708
655.620541	43537.439460	32.395725
656.336346	43614.573232	32.400743
656.882354	43686.232028	32.405760
657.394300	43767.580582	32.410778
658.387837	43840.971985	32.415796
658.951278	43914.523238	32.420813
659.498747	43985.024147	32.425831
660.097854	44066.261695	32.430848
660.744560	44139.831631	32.435866
661.681346	44215.797779	32.440884
662.201047	44296.402170	32.445901
663.089520	44364.944106	32.450919
664.168264	44438.102723	32.455936
664.611292	44513.532881	32.460954
665.547324	44582.339293	32.465972
665.645291	44655.228423	32.470989
666.559850	44725.156695	32.476007
667.211115	44798.270603	32.481024
667.706680	44876.677464	32.486042
668.611891	44952.771804	32.491060
668.695193	45037.543857	32.496077
669.713794	45108.419423	32.501095
670.317903	45181.498412	32.506112
670.939727	45268.462252	32.511130
671.558951	45329.710627	32.516148
672.218272	45414.780635	32.521165
672.791069	45485.696635	32.526183
673.381217	45566.241122	32.531200
674.023255	45651.536096	32.536218
674.741610	45723.894106	32.541236
675.163690	45819.406852	32.546253
675.939079	45887.606733	32.551271
676.848884	45975.170371	32.556288
677.263138	46062.427982	32.561306
678.425939	46124.855294	32.566324
678.855289	46201.674428	32.571341
679.658536	46274.749961	32.576359
680.140332	46332.875939	32.581376
680.668997	46429.899376	32.586394
681.699227	46483.030901	32.591412
682.103344	46561.939874	32.596429
682.914061	46636.790307	32.601447
683.595778	46710.288677	32.606464
684.293881	46791.913156	32.611482
684.884379	46859.487111	32.616500
685.408059	46952.304491	32.621517
686.262761	47022.266951	32.626535
686.838416	47101.920332	32.631552
687.710330	47183.817748	32.636570
688.763209	47255.854673	32.641588
688.872067	47335.523092	32.646605
689.627364	47409.896241	32.651623
690.435119	47484.564175	32.656640
690.891342	47574.433489	32.661658
691.890098	47652.023277	32.666676
692.611729	47735.978573	32.671693
693.258830	47813.005044	32.676711
694.160935	47894.831041	32.681728
694.562331	47974.226344	32.686746
695.560590	48056.772973	32.691764
696.101190	48149.425994	32.696781
696.897834	48231.438261	32.701799
697.768940	48302.138557	32.706816
698.497126	48387.908432	32.711834
699.332718	48464.805283	32.716852
699.607153	48548.253851	32.721869
700.055664	48624.195267	32.726887
701.051582	48706.574541	32.731904
701.470309	48793.493336	32.736922
702.178079	48876.069443	32.741940
702.977429	48965.414778	32.746957
703.691506	49053.678701	32.751975
704.676056	49134.476220	32.756992
705.259182	49223.842733	32.762010
706.070811	49303.987368	32.767028
706.840592	49390.939224	32.772045
707.141560	49476.544595	32.777063
708.190011	49560.299052	32.782080
708.650473	49655.455091	32.787098
709.699867	49725.527879	32.792116
710.371803	49819.316889	32.797133
710.907284	49900.965728	32.802151
711.867798	49986.979087	32.807168
712.460533	50080.270794	32.812186
713.314599	50153.185338	32.817204
714.097249	50254.450091	32.822221
714.829988	50335.685956	32.827239
715.745438	50413.518623	32.832256
716.195985	50500.480908	32.837274
716.889954	50576.967425	32.842292
717.694818	50650.296279	32.847309
718.312539	50755.400175	32.852327
719.141256	50825.074414	32.857344
719.509070	50918.811669	32.862362
720.432626	51000.682068	32.867380
720.874402	51093.498245	32.872397
721.829004	51178.377606	32.877415
722.675105	51253.736097	32.882432
723.114242	51343.022508	32.887450
723.720337	51419.267870	32.892468
724.648860	51506.799969	32.897485
725.237645	51598.697165	32.902503
726.252557	51682.210497	32.907520
726.315474	51762.899802	32.912538
727.761519	51837.194733	32.917556
728.429143	51917.993129	32.922573
728.831192	52001.192249	32.927591
729.939131	52073.459209	32.932608
730.539420	52149.961095	32.937626
731.006193	52228.285900	32.942644
731.849288	52317.655260	32.947661
732.312645	52395.147364	32.952679
733.121348	52475.210827	32.957696
733.609574	52571.564291	32.962714
734.396489	52663.477950	32.967732
735.344158	52754.657853	32.972749
735.800816	52843.038459	32.977767
736.617856	52923.247687	32.982784
736.951963	53022.092835	32.987802
737.919738	53115.791940	32.992820
738.545419	53213.774807	32.997837
739.354667	53312.068970	33.002855
740.327915	53400.385588	33.007872
740.982349	53488.660569	33.012890
742.184180	53581.836693	33.017908
742.836787	53677.062728	33.022925
743.204910	53771.306421	33.027943
744.495897	53861.107864	33.032960
744.980856	53958.940812	33.037978
745.995348	54047.935884	33.042996
746.698436	54128.775437	33.048013
747.405739	54223.843428	33.053031
748.121884	54318.752458	33.058048
748.899147	54407.680984	33.063066
750.048616	54498.639729	33.068084
750.731370	54579.358123	33.073101
751.235503	54667.258868	33.078119
752.442589	54754.595114	33.083136
752.942749	54850.850349	33.088154
753.700862	54936.909508	33.093172
754.358628	55026.960010	33.098189
755.036313	55122.365788	33.103207
756.060506	55211.680430	33.108224
756.447331	55308.759101	33.113242
757.322695	55389.790146	33.118260
758.429167	55478.618482	33.123277
758.945333	55572.227036	33.128295
759.691493	55652.541236	33.133312
760.222627	55761.414323	33.138330
761.169625	55846.631061	33.143348
762.314189	55944.036133	33.148365
762.977278	56027.202750	33.153383
763.873668	56115.973903	33.158400
764.677867	56205.917066	33.163418
765.199600	56297.942062	33.168436
766.067139	56390.744389	33.173453
766.504111	56476.130333	33.178471
767.904951	56569.338162	33.183488
768.196185	56652.486749	33.188506
769.142397	56748.513093	33.193524
769.896335	56841.740731	33.198541
770.296109	56928.480736	33.203559
771.159937	57008.098467	33.208576
771.689780	57114.742161	33.213594
772.242723	57208.364949	33.218612
773.282804	57303.695954	33.223629
773.732490	57411.081200	33.228647
774.546618	57509.964097	33.233664
775.351090	57610.808085	33.238682
776.280849	57698.702357	33.243700
777.190509	57797.002121	33.248717
777.750609	57892.326844	33.253735
778.717271	57974.863637	33.258752
779.231913	58069.444700	33.263770
779.880322	58165.982099	33.268788
780.442857	58260.278076	33.273805
781.304108	58345.089914	33.278823
781.967993	58439.047665	33.283840
782.734412	58541.217096	33.288858
783.140718	58646.511663	33.293876
784.649533	58748.812138	33.298893
784.979412	58855.523416	33.303911
786.068566	58951.795764	33.308928
786.820404	59053.306620	33.313946
787.666162	59147.528297	33.318964
788.754662	59247.707834	33.323981
789.142832	59355.960483	33.328999
790.305020	59462.670014	33.334016
791.042726	59565.569847	33.339034
791.884374	59655.945700	33.344052
792.822548	59761.322414	33.349069
793.541356	59855.410382	33.354087
794.102020	59951.016488	33.359104
795.058685	60059.602305	33.364122
795.381460	60167.971222	33.369140
796.550022	60257.954394	33.374157
797.290965	60377.656905	33.379175
798.385261	60476.937761	33.384192
799.068846	60592.504927	33.389210
799.638863	60686.646631	33.394228
800.648665	60785.614309	33.399245
801.419246	60900.473591	33.404263
802.294523	61006.088370	33.409280
803.303454	61108.970109	33.414298
803.876569	61209.914533	33.419316
805.149729	61303.411859	33.424333
805.681369	61406.797517	33.429351
806.670723	61508.325585	33.434368
807.559218	61611.368826	33.439386
808.133705	61723.016363	33.444404
809.455225	61809.883963	33.449421
810.187679	61910.211341	33.454439
811.210447	62003.677433	33.459456
811.931325	62108.400609	33.464474
812.779371	62207.547300	33.469492
813.814140	62295.772793	33.474509
814.006544	62406.697140	33.479527
815.048944	62493.803429	33.484544
815.780398	62593.521182	33.489562
816.582920	62692.917937	33.494580
817.444242	62791.325693	33.499597
817.682417	62898.458848	33.504615
818.916395	63002.950005	33.509632
819.623293	63109.975127	33.514650
820.555104	63219.713287	33.519668
821.338492	63317.327340	33.524685
821.830828	63420.900290	33.529703
822.807109	63530.436788	33.534720
823.415925	63634.933403	33.539738
824.593484	63734.791485	33.544756
825.448567	63849.539480	33.549773
825.858909	63969.045782	33.554791
826.536057	64068.400352	33.559808
827.401082	64175.164614	33.564826
828.351407	64295.436873	33.569844
829.478627	64399.807349	33.574861
830.235824	64510.055334	33.579879
830.885195	64614.695568	33.584896
832.114257	64711.306883	33.589914
832.454485	64808.691494	33.594932
833.939600	64908.377922	33.599949
834.290752	65014.011407	33.604967
835.068736	65104.997021	33.609984
835.717584	65198.185381	33.615002
836.631801	65303.354222	33.620020
838.065535	65397.899269	33.625037
838.524051	65502.967476	33.630055
839.278455	65605.237273	33.635072
840.068567	65697.544726	33.640090
841.037057	65806.304263	33.645108
841.911875	65909.428053	33.650125
843.013395	66011.800475	33.655143
843.690548	66113.510233	33.660160
844.551862	66208.709955	33.665178
845.107423	66321.327348	33.670196
846.308139	66414.031557	33.675213
847.151801	66527.171392	33.680231
847.897928	66628.486587	33.685248
848.720748	66734.859971	33.690266
849.637337	66850.113733	33.695284
850.839470	66954.927131	33.700301
851.193958	67065.602900	33.705319
852.320822	67170.682712	33.710336
853.153835	67274.167838	33.715354
853.619630	67394.923701	33.720372
854.494583	67514.082560	33.725389
855.239821	67624.342576	33.730407
856.380737	67733.216329	33.735424
857.112641	67844.832709	33.740442
858.100204	67952.221872	33.745460
859.195026	68068.047122	33.750477
859.863070	68185.675984	33.755495
860.279447	68293.142373	33.760512
861.349461	68413.835726	33.765530
862.002645	68536.097187	33.770548
863.268492	68643.955968	33.775565
863.810958	68775.398776	33.780583
864.642970	68895.103610	33.785600
865.792070	69010.861796	33.790618
866.219382	69138.304552	33.795636
867.224487	69253.474550	33.800653
868.246044	69378.639053	33.805671
869.239393	69492.939719	33.810688
870.349601	69613.102091	33.815706
871.309571	69738.911193	33.820724
872.543392	69853.110786	33.825741
873.423437	69963.436506	33.830759
873.881251	70079.131441	33.835776
874.970984	70173.381686	33.840794
875.566013	70296.042233	33.845812
876.601755	70404.453827	33.850829
877.182937	70531.651792	33.855847
878.447278	70647.678006	33.860864
879.527272	70764.196941	33.865882
879.916519	70880.109877	33.870900
880.977668	70986.269072	33.875917
881.750204	71102.884953	33.880935
882.595972	71221.240965	33.885952
883.692532	71335.098055	33.890970
884.305487	71454.170466	33.895988
885.162395	71564.097194	33.901005
886.158844	71694.976922	33.906023
886.939240	71815.617191	33.911040
888.176043	71928.777584	33.916058
888.773342	72054.584321	33.921076
889.707669	72162.673724	33.926093
890.505542	72275.402616	33.931111
891.249753	72376.011834	33.936128
892.426686	72487.224655	33.941146
892.857136	72608.110601	33.946164
894.124081	72704.170211	33.951181
894.399977	72826.050491	33.956199
895.524249	72938.102769	33.961216
896.426364	73048.744160	33.966234
897.500045	73160.730064	33.971252
898.023494	73287.150610	33.976269
899.044405	73406.621599	33.981287
899.977309	73524.267463	33.986304
900.919523	73628.618935	33.991322
901.429812	73763.999495	33.996340
902.608460	73880.759188	34.001357
903.595238	74016.030885	34.006375
904.588732	74135.276393	34.011392
905.734982	74261.182165	34.016410
906.446124	74381.101819	34.021428
907.532993	74484.370946	34.026445
908.365696	74617.363408	34.031463
909.126377	74745.410156	34.036480
910.246006	74863.456074	34.041498
910.847699	74987.318365	34.046516
912.080921	75113.979919	34.051533
912.955350	75232.839974	34.056551
913.603079	75369.656047	34.061568
914.837910	75483.878767	34.066586
915.653897	75617.613703	34.071604
916.500936	75743.805133	34.076621
917.548905	75869.110200	34.081639
918.432334	76008.421189	34.086656
919.506001	76124.033721	34.091674
920.109936	76254.271940	34.096692
921.288615	76390.146324	34.101709
922.195821	76513.536541	34.106727
923.020402	76640.413569	34.111744
924.499746	76764.507524	34.116762
925.232029	76891.951536	34.121780
926.128345	77011.646111	34.126797
927.435357	77143.266012	34.131815
928.065021	77265.321075	34.136832
928.967005	77393.151031	34.141850
929.924365	77518.821954	34.146868
930.927905	77648.957973	34.151885
931.775745	77760.416321	34.156903
932.363584	77894.164728	34.161920
933.622266	78026.670739	34.166938
934.434884	78154.747546	34.171956
935.426668	78291.259021	34.176973
936.290085	78412.396111	34.181991
937.233250	78546.715882	34.187008
938.028849	78672.426354	34.192026
938.802946	78814.581530	34.197044
939.947553	78943.284781	34.202061
941.028726	79073.365622	34.207079
941.988302	79205.668698	34.212096
942.882918	79336.680171	34.217114
943.991097	79464.336010	34.222132
944.706204	79603.418893	34.227149
945.763908	79733.779436	34.232167
946.190117	79862.948334	34.237184
947.361493	79992.608366	34.242202
948.348021	80139.702677	34.247220
949.595466	80270.964868	34.252237
950.778292	80406.280901	34.257255
951.818060	80528.469302	34.262272
952.520908	80647.399148	34.267290
953.280682	80772.266858	34.272308
954.141477	80895.524330	34.277325
955.337038	81006.137780	34.282343
955.819546	81127.137309	34.287360
957.028741	81245.619622	34.292378
958.099281	81383.402011	34.297396
958.741541	81502.713272	34.302413
959.569089	81622.348798	34.307431
960.352734	81747.559530	34.312448
961.307876	81890.621382	34.317466
962.280661	82009.773080	34.322484
963.085945	82155.221177	34.327501
964.273511	82290.579238	34.332519
965.028549	82432.671625	34.337536
966.107969	82567.846751	34.342554
966.777178	82709.499517	34.347572
968.030354	82848.045032	34.352589
968.921545	82992.351723	34.357607
969.514127	83132.716433	34.362624
971.118036	83270.959745	34.367642
971.959278	83419.579674	34.372660
972.705952	83557.941150	34.377677
973.871491	83708.799687	34.382695
974.731719	83851.003632	34.387712
975.790780	83991.751970	34.392730
976.545957	84152.114983	34.397748
977.590686	84282.794621	34.402765
978.931840	84435.065119	34.407783
979.715800	84588.947299	34.412800
980.566522	84737.333670	34.417818
981.593024	84891.013230	34.422836
982.674991	85035.598484	34.427853
983.906090	85185.544625	34.432871
984.692028	85336.470171	34.437888
985.874558	85479.554589	34.442906
986.877722	85629.617202	34.447924
987.859556	85787.511549	34.452941
989.056191	85914.802605	34.457959
989.885346	86078.760726	34.462976
990.816564	86220.125802	34.467994
991.773087	86377.053833	34.473012
992.395746	86525.324733	34.478029
993.345193	86678.370674	34.483047
994.679642	86839.725739	34.488064
996.020623	86993.449348	34.493082
997.197691	87157.313159	34.498100
997.972620	87294.344226	34.503117
999.039862	87439.250466	34.508135
1000.361838	87585.602572	34.513152
1001.334208	87733.070189	34.518170
1002.662460	87878.056191	34.523188
1003.525521	88025.860112	34.528205
1004.648091	88155.510620	34.533223
1005.560171	88296.695114	34.538240
1006.489240	88436.966360	34.543258
1007.672863	88579.132818	34.548276
1008.548216	88728.919850	34.553293
1009.812486	88868.524358	34.558311
1010.663156	89017.494589	34.563328
1011.566027	89149.711897	34.568346
1012.691597	89296.676578	34.573364
1013.358476	89440.420818	34.578381
1014.730747	89590.681673	34.583399
1015.523941	89734.640951	34.588416
1016.803226	89867.407535	34.593434
1017.578914	90014.611676	34.598452
1018.355523	90167.012486	34.603469
1019.596035	90295.984261	34.608487
1020.517468	90441.932802	34.613504
1021.774465	90573.105774	34.618522
1022.421247	90707.196723	34.623540
1023.473479	90837.911338	34.628557
1024.565995	90974.278109	34.633575
1024.852201	91118.721887	34.638592
1026.117730	91263.852693	34.643610
1027.189053	91400.465875	34.648628
1028.423063	91550.242835	34.653645
1029.275896	91684.045634	34.658663
1029.786223	91837.431395	34.663680
1030.711186	91999.737097	34.668698
1032.117597	92148.799356	34.673716
1033.155805	92295.562571	34.678733
1033.984002	92452.273179	34.683751
1034.896095	92615.642118	34.688768
1036.248133	92774.116367	34.693786
1037.220623	92931.477115	34.698804
1038.044662	93086.249325	34.703821
1039.457660	93241.621386	34.708839
1039.976410	93404.877075	34.713856
1041.157476	93558.542520	34.718874
1042.184488	93725.900206	34.723892
1043.289391	93897.373143	34.728909
1044.520817	94062.952317	34.733927
1045.396912	94235.085756	34.738944
1046.792534	94403.551791	34.743962
1047.728303	94565.113118	34.748980
1048.752027	94728.521964	34.753997
1049.598238	94891.499151	34.759015
1050.729750	95063.032758	34.764032
1052.234960	95224.137094	34.769050
1053.494144	95394.050372	34.774068
1054.365104	95555.565574	34.779085
1055.450511	95715.375194	34.784103
1056.401171	95886.558250	34.789120
1057.611292	96046.051852	34.794138
1058.853292	96206.756626	34.799156
1059.499884	96375.094020	34.804173
1060.827437	96539.217850	34.809191
1061.964802	96701.449746	34.814208
1062.888421	96865.737461	34.819226
1064.110666	97034.984333	34.824244
1064.993163	97194.343182	34.829261
1066.160965	97359.201491	34.834279
1067.174840	97540.577707	34.839296
1067.971876	97702.087336	34.844314
1069.272857	97875.125270	34.849332
1070.400689	98037.595276	34.854349
1071.629599	98206.196853	34.859367
1072.694457	98369.768311	34.864384
1073.650166	98538.816121	34.869402
1074.882832	98712.776407	34.874420
1075.983887	98882.612841	34.879437
1077.154572	99044.639057	34.884455
1078.075429	99210.082077	34.889472
1079.411014	99372.127435	34.894490
1080.433052	99540.309911	34.899508
1081.376372	99707.309915	34.904525
1082.396762	99864.991338	34.909543
1083.721774	100041.788171	34.914560
1084.894178	100209.899548	34.919578
1086.134312	100367.541409	34.924596
1086.721925	100522.765891	34.929613
1088.207039	100685.921851	34.934631
1089.471407	100858.321329	34.939648
1090.648433	101016.724729	34.944666
1091.763924	101153.732257	34.949684
1092.863932	101303.361948	34.954701
1093.929894	101446.362584	34.959719
1094.929212	101585.949598	34.964736
1095.825070	101740.092064	34.969754
1097.219736	101881.128588	34.974772
1097.994162	102035.191582	34.979789
1099.256598	102177.327985	34.984807
1100.104423	102335.167050	34.989824
1101.058393	102491.203933	34.994842
1102.394251	102640.238826	34.999860
1102.924725	102796.543848	35.004877
1104.326655	102947.367855	35.009895
1105.176783	103106.705574	35.014912
1106.204321	103289.367645	35.019930
1107.236137	103454.186359	35.024948
1108.156505	103616.073750	35.029965
1109.130655	103785.298605	35.034983
1110.141151	103963.763620	35.040000
1111.197553	104142.450222	35.045018
1112.636212	104324.025709	35.050036
1113.350603	104505.354914	35.055053
1114.582198	104674.479611	35.060071
1115.756521	104857.609597	35.065088
1116.831819	105052.219060	35.070106
1118.119463	105231.191443	35.075124
1119.252251	105420.386114	35.080141
1120.368628	105586.432728	35.085159
1121.929227	105777.585667	35.090176
1122.790438	105956.418137	35.095194
1124.102671	106127.590593	35.100212
1125.083019	106326.810030	35.105229
1126.212831	106503.473945	35.110247
1127.617952	106678.725610	35.115264
1128.727104	106859.271028	35.120282
1129.880172	107038.239826	35.125300
1130.786085	107234.945149	35.130317
1132.009932	107408.065666	35.135335
1133.545572	107593.042000	35.140352
1134.213205	107776.123832	35.145370
1135.609788	107954.336502	35.150388
1136.436168	108151.378338	35.155405
1138.004953	108335.442309	35.160423
1139.130351	108511.385510	35.165440
1140.306516	108685.788790	35.170458
1141.606561	108869.267487	35.175476
1142.704137	109052.476894	35.180493
1144.011401	109225.772622	35.185511
1145.191024	109411.314278	35.190528
1146.224546	109594.297253	35.195546
1147.674705	109769.764243	35.200564
1148.938071	109957.943232	35.205581
1150.047078	110120.256858	35.210599
1151.194098	110310.205609	35.215616
1152.208422	110483.709772	35.220634
1153.337832	110661.173649	35.225652
1154.434447	110838.010709	35.230669
1155.761091	111009.110364	35.235687
1156.765226	111193.236322	35.240704
1157.681483	111382.242543	35.245722
1159.405695	111553.609227	35.250740
1160.287166	111728.334001	35.255757
1161.584183	111902.953179	35.260775
1162.864203	112087.140838	35.265792
1163.728327	112267.154564	35.270810
1165.278923	112446.637916	35.275828
1166.139001	112622.030622	35.280845
1167.062776	112797.806631	35.285863
1168.124237	112970.571173	35.290880
1169.342698	113151.507536	35.295898
1170.741310	113309.687347	35.300916
1171.546782	113486.855491	35.305933
1172.613773	113651.008451	35.310951
1174.109586	113815.636254	35.315968
1175.065226	113995.151908	35.320986
1175.985018	114163.538366	35.326004
1176.965853	114347.435664	35.331021
1178.131867	114518.089359	35.336039
1179.180409	114700.938882	35.341056
1180.396215	114888.284975	35.346074
1181.420207	115066.744584	35.351092
1182.738577	115262.235457	35.356109
1183.608330	115449.300388	35.361127
1185.238871	115641.004672	35.366144
1186.332690	115830.797117	35.371162
1187.784732	116025.460271	35.376180
1188.570948	116209.553875	35.381197
1189.661117	116418.102678	35.386215
1191.037231	116608.639192	35.391232
1191.985521	116809.954206	35.396250
1193.404374	116999.497964	35.401268
1194.752514	117205.412405	35.406285
1195.873300	117407.729417	35.411303
1197.061475	117600.799716	35.416320
1198.269996	117804.029977	35.421338
1199.408017	117995.514682	35.426356
1200.576571	118211.640775	35.431373
1201.904162	118414.247435	35.436391
1203.097665	118623.403356	35.441408
1204.143566	118824.437530	35.446426
1205.546783	119025.059229	35.451444
1206.440056	119230.860545	35.456461
1208.124309	119438.103837	35.461479
1209.245619	119639.460631	35.466496
1210.277929	119852.428178	35.471514
1211.499911	120056.216847	35.476532
1213.021504	120271.856353	35.481549
1214.523730	120477.210958	35.486567
1215.447481	120681.154638	35.491584
1216.779742	120885.893912	35.496602
1218.059158	121092.341429	35.501620
1219.309800	121295.994549	35.506637
1220.677069	121505.091626	35.511655
1222.184695	121705.879126	35.516672
1223.560978	121919.172247	35.521690
1224.740800	122117.190716	35.526708
1225.786236	122307.299537	35.531725
1226.495871	122518.945630	35.536743
1228.143219	122720.426561	35.541760
1229.227313	122933.762565	35.546778
1230.530429	123129.397501	35.551796
1231.848364	123344.586075	35.556813
1233.052910	123547.070906	35.561831
1234.465920	123750.397107	35.566848
1235.355478	123963.671191	35.571866
1237.094588	124168.479802	35.576884
1238.169275	124368.900474	35.581901
1239.412300	124581.093918	35.586919
1240.710413	124777.766949	35.591936
1241.570388	124993.651314	35.596954
1242.958485	125185.255208	35.601972
1244.358578	125390.597047	35.606989
1245.518610	125598.882338	35.612007
1246.961200	125808.186983	35.617024
1247.962099	126013.446900	35.622042
1248.752361	126212.709974	35.627060
1250.273580	126418.545667	35.632077
1251.367829	126621.512803	35.637095
1253.072022	126816.230632	35.642112
1253.807508	127011.185859	35.647130
1255.102944	127210.055012	35.652148
1256.385601	127399.079136	35.657165
1257.402767	127604.790583	35.662183
1258.859342	127795.271352	35.667200
1259.855714	128011.255752	35.672218
1261.320477	128206.985213	35.677236
1262.347690	128417.960608	35.682253
1263.441007	128628.711019	35.687271
1264.935451	128822.804304	35.692288
1266.104725	129041.771346	35.697306
1267.020688	129256.167836	35.702324
1268.469851	129471.757907	35.707341
1269.552327	129706.525260	35.712359
1271.211968	129915.010444	35.717376
1272.423189	130122.772534	35.722394
1273.724313	130337.163411	35.727412
1274.870641	130568.795609	35.732429
1275.950992	130789.538784	35.737447
1277.342103	131003.526320	35.742464
1278.865748	131236.216532	35.747482
1280.016823	131462.327501	35.752500
1281.237050	131685.500332	35.757517
1282.256129	131913.943457	35.762535
1284.131871	132138.963315	35.767552
1285.299751	132375.320821	35.772570
1286.693961	132605.063282	35.777588
1287.746272	132831.732643	35.782605
1288.925672	133069.246941	35.787623
1290.584103	133280.771439	35.792640
1291.788943	133524.293894	35.797658
1293.272843	133758.365369	35.802676
1294.604992	133982.575118	35.807693
1296.042129	134207.859331	35.812711
1297.347216	134435.994054	35.817728
1298.244146	134671.728449	35.822746
1299.374931	134909.745940	35.827764
1301.219351	135128.528786	35.832781
1302.289616	135375.573701	35.837799
1304.356937	135602.487540	35.842816
1305.658209	135835.386908	35.847834
1306.971689	136058.498208	35.852852
1308.273434	136280.053500	35.857869
1309.538715	136509.274119	35.862887
1310.951760	136731.866339	35.867904
1312.290105	136959.784761	35.872922
1313.596017	137188.014387	35.877940
1315.190049	137408.856887	35.882957
1316.055066	137639.317859	35.887975
1317.653431	137859.148286	35.892992
1319.019265	138084.660786	35.898010
1319.892531	138313.565473	35.903028
1321.352116	138538.989433	35.908045
1322.724207	138767.649914	35.913063
1324.003938	138988.339144	35.918080
1325.485777	139227.267616	35.923098
1326.527078	139450.344961	35.928116
1327.840455	139677.474340	35.933133
1328.996339	139911.414946	35.938151
1330.657391	140150.700646	35.943168
1331.792623	140378.460065	35.948186
1332.931585	140609.999030	35.953204
1334.337506	140841.127703	35.958221
1335.385146	141083.412331	35.963239
1336.831030	141322.158429	35.968256
1338.183086	141550.726637	35.973274
1339.263465	141776.551542	35.978292
1340.699005	142005.070895	35.983309
1341.784983	142236.223686	35.988327
1343.378837	142449.921474	35.993344
1344.760279	142679.734928	35.998362
1345.739194	142900.334004	36.003380
1347.758523	143130.159108	36.008397
1348.569088	143362.594883	36.013415
1349.849143	143593.724525	36.018432
1351.266456	143827.115610	36.023450
1352.576713	144065.243367	36.028468
1354.269387	144292.048449	36.033485
1355.042220	144537.800930	36.038503
1356.659500	144769.567284	36.043520
1357.466021	145013.985906	36.048538
1359.105341	145263.151025	36.053556
1360.668753	145510.593008	36.058573
1361.896445	145754.668063	36.063591
1363.331343	146000.853780	36.068608
1364.432096	146245.067264	36.073626
1365.667358	146501.790135	36.078644
1367.148127	146755.671469	36.083661
1368.930775	147011.673364	36.088679
1369.977489	147281.115230	36.093696
1371.370690	147519.543787	36.098714
1372.787889	147782.079553	36.103732
1374.011514	148030.127502	36.108749
1375.007635	148298.836916	36.113767
1377.180126	148559.972443	36.118784
1378.563210	148823.421742	36.123802
1379.664526	149085.105801	36.128820
1381.395148	149341.956890	36.133837
1383.070391	149596.700802	36.138855
1384.152595	149855.070419	36.143872
1385.890889	150118.761886	36.148890
1387.498456	150380.422085	36.153908
1388.693056	150635.227117	36.158925
1390.508756	150893.888529	36.163943
1391.835158	151142.929506	36.168960
1393.193622	151391.814614	36.173978
1394.243980	151653.233240	36.178996
1395.809040	151912.526476	36.184013
1397.192106	152172.346228	36.189031
1398.703648	152419.842866	36.194048
1400.435614	152680.737298	36.199066
1401.684954	152944.744815	36.204084
1403.167813	153192.403377	36.209101
1404.333752	153462.745061	36.214119
1405.676374	153708.387893	36.219136
1407.268732	153973.347823	36.224154
1408.664867	154224.566330	36.229172
1410.461241	154476.176967	36.234189
1411.983988	154747.293118	36.239207
1413.386613	154997.614886	36.244224
1414.605160	155237.211711	36.249242
1415.848895	155502.277648	36.254260
1417.657129	155755.695808	36.259277
1418.417094	156010.531983	36.264295
1420.031345	156268.298488	36.269312
1421.554469	156531.143236	36.274330
1423.037694	156791.725588	36.279348
1424.429972	157046.857145	36.284365
1425.235321	157306.603439	36.289383
1427.114171	157562.558551	36.294400
1428.802692	157829.862570	36.299418
1429.985485	158097.619821	36.304436
1431.454303	158354.662585	36.309453
1432.827883	158610.390666	36.314471
1433.977525	158842.548284	36.319488
1435.872924	159087.282971	36.324506
1436.896709	159331.287795	36.329524
1438.508214	159569.627596	36.334541
1439.909426	159811.898291	36.339559
1441.291997	160060.224997	36.344576
1442.635788	160310.627531	36.349594
1443.778736	160561.280440	36.354612
1445.373973	160809.069017	36.359629
1446.798687	161069.599527	36.364647
1448.353941	161329.450366	36.369664
1449.515316	161581.920596	36.374682
1450.958150	161840.067733	36.379700
1452.345060	162099.887718	36.384717
1453.522916	162368.434645	36.389735
1454.500739	162631.497318	36.394752
1456.249146	162911.625792	36.399770
1457.733752	163189.071877	36.404788
1459.607859	163472.761151	36.409805
1460.798714	163746.884483	36.414823
1462.493227	164020.964401	36.419840
1464.057468	164304.723058	36.424858
1465.240968	164574.056847	36.429876
1467.117479	164852.666939	36.434893
1468.269956	165131.969420	36.439911
1469.706163	165409.831104	36.444928
1471.584821	165688.192413	36.449946
1472.704408	165976.653966	36.454964
1474.577462	166256.212504	36.459981
1476.150163	166544.526768	36.464999
1477.674083	166827.712085	36.470016
1479.307028	167107.328360	36.475034
1480.581787	167378.301085	36.480052
1482.146776	167660.977359	36.485069
1483.473280	167945.725048	36.490087
1484.906393	168233.083545	36.495104
1486.468858	168520.219472	36.500122
1488.141133	168807.097982	36.505140
1490.118110	169083.586226	36.510157
1491.486157	169371.622529	36.515175
1492.781294	169648.861328	36.520192
1494.407763	169935.944843	36.525210
1495.654836	170227.013911	36.530228
1496.995432	170503.006768	36.535245
1498.342120	170794.481705	36.540263
1499.747265	171093.803790	36.545280
1501.573415	171383.045925	36.550298
1503.034790	171686.309065	36.555316
1504.212488	171978.288839	36.560333
1505.920331	172271.667568	36.565351
1507.374828	172566.866605	36.570368
1509.278636	172857.069416	36.575386
1510.790494	173159.013876	36.580404
1512.509439	173451.903136	36.585421
1513.895386	173739.569961	36.590439
1515.231953	174038.642801	36.595456
1517.331172	174326.398326	36.600474
1518.304360	174616.752853	36.605492
1520.113740	174894.483201	36.610509
1521.524037	175194.883522	36.615527
1522.669336	175489.390104	36.620544
1524.494002	175784.915703	36.625562
1525.957402	176086.467586	36.630580
1527.573230	176386.485871	36.635597
1528.823797	176675.220334	36.640615
1530.403487	176974.055156	36.645632
1532.420119	177270.116300	36.650650
1533.488987	177561.398799	36.655668
1535.253260	177825.052796	36.660685
1536.654076	178102.208645	36.665703
1538.222128	178385.341545	36.670720
1539.859780	178649.033441	36.675738
1540.990648	178924.410756	36.680756
1542.448190	179207.249177	36.685773
1543.968159	179487.032769	36.690791
1545.600577	179768.258882	36.695808
1546.817974	180057.322659	36.700826
1547.961535	180356.972822	36.705844
1549.678161	180647.645450	36.710861
1551.207923	180957.452504	36.715879
1552.900656	181256.458615	36.720896
1554.262577	181557.805719	36.725914
1555.459589	181864.309568	36.730932
1557.069097	182170.912033	36.735949
1558.697411	182485.839551	36.740967
1560.206542	182786.572720	36.745984
1561.966145	183103.360693	36.751002
1563.514666	183421.010434	36.756020
1565.289821	183728.520978	36.761037
1566.938517	184056.109169	36.766055
1567.990138	184373.745008	36.771072
1569.891313	184701.676130	36.776090
1571.324749	185025.066124	36.781108
1572.862633	185343.388793	36.786125
1574.441909	185673.460547	36.791143
1576.336379	186001.641615	36.796160
1577.893778	186322.276839	36.801178
1579.468875	186647.277571	36.806196
1581.440183	186973.395218	36.811213
1583.262580	187288.267253	36.816231
1584.516395	187619.153050	36.821248
1586.264108	187938.699636	36.826266
1587.792460	188255.986616	36.831284
1589.467517	188584.510729	36.836301
1591.376578	188901.154401	36.841319
1593.249641	189219.938359	36.846336
1594.825089	189528.414685	36.851354
1596.436859	189857.502227	36.856372
1597.662270	190174.164121	36.861389
1599.326555	190494.068446	36.866407
1601.195021	190826.419483	36.871424
1603.146894	191132.036411	36.876442
1604.405811	191461.064097	36.881460
1606.319719	191777.265214	36.886477
1607.985563	192097.698238	36.891495
1609.506366	192416.735068	36.896512
1611.147829	192735.182339	36.901530
1613.052167	193057.992985	36.906548
1614.424333	193364.719698	36.911565
1616.421405	193681.450001	36.916583
1617.600772	194005.654813	36.921600
1619.498001	194310.014253	36.926618
1621.161971	194630.854129	36.931636
1622.423835	194952.193689	36.936653
1624.304469	195257.563321	36.941671
1625.596167	195585.426573	36.946688
1627.362445	195914.876200	36.951706
1628.816452	196231.213702	36.956724
1630.275843	196553.645776	36.961741
1632.119557	196878.821702	36.966759
1633.752547	197197.914648	36.971776
1635.463990	197514.723601	36.976794
1637.365846	197842.294150	36.981812
1639.183097	198148.995342	36.986829
1640.791532	198460.658494	36.991847
1642.311027	198768.490843	36.996864
1644.623023	199061.453401	37.001882
1645.527927	199351.462905	37.006900
1647.243969	199639.536758	37.011917
1649.225463	199924.368480	37.016935
1650.449674	200228.142511	37.021952
1652.066507	200522.470330	37.026970
1653.422380	200819.165946	37.031988
1655.020438	201125.700713	37.037005
1656.510199	201419.494605	37.042023
1657.909297	201731.003817	37.047040
1659.807579	202042.368432	37.052058
1661.305069	202373.518675	37.057076
1662.831175	202687.182172	37.062093
1664.710688	203004.902421	37.067111
1666.101574	203331.998916	37.072128
1667.679558	203648.794085	37.077146
1669.363258	203984.606007	37.082164
1670.836269	204311.985272	37.087181
1672.684339	204643.989253	37.092199
1674.272791	204978.907145	37.097216
1675.964123	205313.593659	37.102234
1677.702832	205646.978679	37.107252
1679.484241	205983.811771	37.112269
1681.463264	206310.900144	37.117287
1682.761323	206659.154802	37.122304
1684.292691	207000.718948	37.127322
1686.460000	207346.141165	37.132340
1688.067619	207685.841807	37.137357
1689.879747	208034.398496	37.142375
1691.261104	208378.926468	37.147392
1693.046020	208720.011616	37.152410
1694.823886	209067.981589	37.157428
1696.305949	209412.573453	37.162445
1698.420754	209769.772893	37.167463
1699.816441	210114.978728	37.172480
1701.605612	210469.822307	37.177498
1703.065769	210829.521609	37.182516
1704.596909	211180.271173	37.187533
1706.880834	211540.192923	37.192551
1708.413082	211894.932443	37.197568
1710.465054	212258.171626	37.202586
1712.226904	212609.472947	37.207604
1713.835816	212970.883478	37.212621
1715.760600	213312.636819	37.217639
1717.404224	213671.733304	37.222656
1719.048474	214024.100849	37.227674
1721.092467	214385.978487	37.232692
1722.885168	214741.194143	37.237709
1724.718760	215092.696366	37.242727
1726.184582	215446.190864	37.247744
1728.096087	215799.917834	37.252762
1729.894855	216148.813763	37.257780
1731.417109	216512.614366	37.262797
1733.590853	216867.317847	37.267815
1734.756188	217220.538306	37.272832
1736.666323	217579.859539	37.277850
1738.652026	217931.143750	37.282868
1740.185139	218297.311151	37.287885
1741.970499	218642.865512	37.292903
1743.189240	219009.519166	37.297920
1745.411753	219368.617339	37.302938
1747.100346	219733.519634	37.307956
1748.631491	220092.963071	37.312973
1750.954774	220444.301651	37.317991
1752.230103	220807.116989	37.323008
1753.763096	221174.132612	37.328026
1755.556204	221530.794478	37.333044
1757.332206	221933.178807	37.338061
1758.931635	222298.307649	37.343079
1760.651860	222657.525074	37.348096
1762.513358	222993.530641	37.353114
1764.421466	223341.543442	37.358132
1765.608224	223690.260622	37.363149
1767.805066	224027.432967	37.368167
1769.442901	224381.030611	37.373184
1771.101578	224728.377511	37.378202
1772.484246	225082.857553	37.383220
1774.485229	225444.729473	37.388237
1775.964157	225793.429882	37.393255
1777.352654	226166.428664	37.398272
1779.340369	226521.549475	37.403290
1781.417965	226893.141166	37.408308
1782.495095	227275.059283	37.413325
1784.924394	227642.226174	37.418343
1786.512694	228030.132738	37.423360
1788.360611	228404.281271	37.428378
1790.085431	228776.114312	37.433396
1791.914355	229164.339980	37.438413
1794.105364	229541.686222	37.443431
1795.725242	229928.957905	37.448448
1797.562147	230313.349895	37.453466
1799.594790	230692.503388	37.458484
1801.265752	231079.795107	37.463501
1803.182119	231458.512548	37.468519
1804.514066	231855.692463	37.473536
1806.402522	232245.770768	37.478554
1808.533021	232632.711123	37.483572
1810.550480	233036.715367	37.488589
1812.453921	233411.553293	37.493607
1814.434455	233815.565581	37.498624
1815.952848	234196.235013	37.503642
1817.859720	234588.906876	37.508660
1819.608322	234981.910600	37.513677
1821.897204	235373.682906	37.518695
1823.480221	235777.486060	37.523712
1825.294129	236165.934721	37.528730
1827.233132	236557.335559	37.533748
1828.942433	236955.405044	37.538765
1830.809291	237347.124262	37.543783
1832.667673	237745.424785	37.548800
1834.797351	238149.041135	37.553818
1837.113625	238542.212626	37.558836
1838.650370	238945.903083	37.563853
1840.610949	239329.990050	37.568871
1842.255434	239724.621027	37.573888
1844.061688	240121.308987	37.578906
1845.759993	240516.161114	37.583924
1847.830517	240921.850062	37.588941
1849.733800	241314.942346	37.593959
1851.799840	241722.665606	37.598976
1853.469835	242121.310061	37.603994
1855.308684	242512.992378	37.609012
1857.004693	242913.462766	37.614029
1858.815292	243311.196762	37.619047
1860.356093	243724.446104	37.624064
1862.212103	244125.222100	37.629082
1864.422867	244532.112931	37.634100
1866.006767	244933.849484	37.639117
1868.045748	245332.615500	37.644135
1869.827867	245742.220639	37.649152
1871.562796	246158.921485	37.654170
1873.673707	246565.425017	37.659188
1875.218745	246974.359548	37.664205
1877.406570	247387.151253	37.669223
1878.959266	247798.676548	37.674240
1880.624766	248204.213955	37.679258
1882.710362	248589.918860	37.684276
1884.255583	248992.428556	37.689293
1886.476127	249380.321961	37.694311
1888.266751	249777.711238	37.699328
1889.923723	250173.319302	37.704346
1892.053887	250559.856838	37.709364
1893.659252	250963.704652	37.714381
1895.655124	251362.229825	37.719399
1897.705344	251758.891868	37.724416
1899.096582	252164.782734	37.729434
1900.919015	252570.831277	37.734452
1902.518487	252985.376146	37.739469
1905.025598	253398.729827	37.744487
1906.569028	253820.397300	37.749504
1908.346776	254242.280313	37.754522
1910.636200	254659.303199	37.759540
1912.387446	255077.075604	37.764557
1914.131080	255507.220808	37.769575
1915.786173	255935.856569	37.774592
1917.824719	256366.791628	37.779610
1919.783564	256801.245598	37.784628
1921.544922	257245.385511	37.789645
1923.369984	257677.448393	37.794663
1925.229413	258128.075452	37.799680
1927.059523	258579.139224	37.804698
1929.115960	259026.101087	37.809716
1930.785535	259474.422373	37.814733
1932.764871	259927.214245	37.819751
1935.083972	260386.935844	37.824768
1937.239920	260845.185490	37.829786
1939.403304	261301.426926	37.834804
1941.148291	261762.665541	37.839821
1943.228225	262220.622459	37.844839
1945.378076	262671.734165	37.849856
1947.214757	263125.031245	37.854874
1949.411738	263584.238352	37.859892
1950.977471	264048.884104	37.864909
1953.029585	264505.904497	37.869927
1955.116551	264962.436166	37.874944
1956.865678	265426.669637	37.879962
1958.928592	265887.573922	37.884980
1961.355451	266360.789039	37.889997
1963.089945	266818.952405	37.895015
1965.059507	267298.059456	37.900032
1966.894602	267758.593191	37.905050
1968.775919	268226.130040	37.910068
1970.750549	268687.579646	37.915085
1973.132152	269157.268282	37.920103
1975.244963	269625.908398	37.925120
1977.293032	270089.909876	37.930138
1979.237929	270556.671283	37.935156
1980.830336	271027.072044	37.940173
1982.658875	271502.539092	37.945191
1984.857925	271964.684010	37.950208
1987.059994	272447.759545	37.955226
1989.058551	272907.522844	37.960244
1990.891476	273388.142886	37.965261
1993.128831	273857.492773	37.970279
1995.357111	274330.704510	37.975296
1996.987997	274810.161414	37.980314
1999.238716	275269.345529	37.985332
2001.226226	275751.358165	37.990349
2003.284285	276208.870329	37.995367
2005.486406	276670.879401	38.000384
2007.074979	277146.985448	38.005402
2009.389818	277607.449820	38.010420
2011.208282	278077.571749	38.015437
2013.254739	278538.332419	38.020455
2015.396045	278984.902073	38.025472
2017.538435	279430.200448	38.030490
2019.470356	279857.649633	38.035508
2021.425996	280309.657503	38.040525
2022.848593	280748.492573	38.045543
2025.325178	281183.062895	38.050560
2027.030379	281645.752128	38.055578
2029.192392	282088.170477	38.060596
2031.130666	282547.211814	38.065613
2033.202916	283007.474456	38.070631
2035.157230	283467.272671	38.075648
2036.896916	283928.171881	38.080666
2039.210936	284384.047104	38.085684
2041.164517	284853.163708	38.090701
2043.024811	285319.779587	38.095719
2045.146410	285791.862903	38.100736
2047.055203	286257.909046	38.105754
2049.272260	286732.412089	38.110772
2050.958313	287209.439713	38.115789
2053.128761	287694.590168	38.120807
2054.936279	288174.312337	38.125824
2057.327020	288661.429678	38.130842
2059.488204	289155.669867	38.135860
2061.832296	289639.768710	38.140877
2063.483574	290128.729981	38.145895
2066.006399	290619.501312	38.150912
2067.739637	291110.477304	38.155930
2069.813253	291593.241809	38.160948
2072.410408	292096.872810	38.165965
2074.053340	292590.829584	38.170983
2076.475635	293081.226706	38.176000
2078.626395	293575.527335	38.181018
2080.700188	294078.474352	38.186036
2082.689794	294574.321270	38.191053
2085.178282	295076.789022	38.196071
2087.260449	295563.472602	38.201088
2089.141432	296070.734957	38.206106
2091.424500	296565.305363	38.211124
2093.699622	297063.963983	38.216141
2095.874390	297559.233413	38.221159
2097.995439	298051.283762	38.226176
2099.948306	298563.703568	38.231194
2102.090498	299060.037892	38.236212
2104.305513	299559.938867	38.241229
2106.134190	300063.913978	38.246247
2108.742600	300563.033786	38.251264
2110.663499	301069.934616	38.256282
2113.090470	301567.352133	38.261300
2115.436859	302068.691538	38.266317
2117.612284	302566.780235	38.271335
2120.043786	303064.138254	38.276352
2121.941086	303552.438846	38.281370
2124.109684	304046.787258	38.286388
2126.254415	304548.959062	38.291405
2128.405114	305040.358895	38.296423
2130.734674	305524.869413	38.301440
2132.830589	306018.660036	38.306458
2135.048707	306508.186492	38.311476
2137.209934	307001.706685	38.316493
2139.289314	307484.215704	38.321511
2141.594306	307972.728853	38.326528
2143.648104	308469.991238	38.331546
2145.596124	308952.614926	38.336564
2147.734078	309447.343291	38.341581
2149.756851	309937.795847	38.346599
2151.940923	310422.276334	38.351616
2153.996662	310913.910940	38.356634
2156.008624	311411.415814	38.361652
2158.167990	311885.504881	38.366669
2160.226683	312351.202122	38.371687
2162.834303	312802.737543	38.376704
2164.955473	313270.297956	38.381722
2166.941204	313732.951393	38.386740
2168.917289	314206.700542	38.391757
2170.922843	314679.527595	38.396775
2173.106761	315149.757400	38.401792
2174.741235	315634.802850	38.406810
2177.096307	316114.545887	38.411828
2179.356754	316601.639808	38.416845
2181.012026	317090.074482	38.421863
2183.448357	317581.957130	38.426880
2185.482111	318079.514411	38.431898
2187.421356	318585.361486	38.436916
2189.762216	319093.906208	38.441933
2191.529947	319603.074918	38.446951
2193.895455	320111.430105	38.451968
2195.799390	320638.266256	38.456986
2197.955086	321157.490079	38.462004
2200.246148	321674.427626	38.467021
2202.339286	322199.696450	38.472039
2204.806731	322731.069056	38.477056
2206.468012	323270.898282	38.482074
2208.550255	323802.782486	38.487092
2211.081335	324359.114615	38.492109
2213.193609	324900.784925	38.497127
2215.607334	325445.701310	38.502144
2217.630096	325997.024631	38.507162
2219.918298	326551.625048	38.512180
2222.498516	327094.823403	38.517197
2224.676901	327663.471530	38.522215
2227.268928	328209.298098	38.527232
2229.089578	328777.232838	38.532250
2231.412929	329326.926853	38.537268
2233.970283	329881.121343	38.542285
2235.473007	330451.478456	38.547303
2238.330150	331007.516523	38.552320
2240.781534	331573.059906	38.557338
2243.077268	332127.656312	38.562356
2245.210378	332694.002411	38.567373
2247.512809	333262.193278	38.572391
2250.198735	333814.804302	38.577408
2252.414254	334371.218975	38.582426
2254.319818	334932.248363	38.587444
2256.910926	335496.458725	38.592461
2259.052890	336079.978704	38.597479
2261.457468	336628.266236	38.602496
2263.888519	337194.134761	38.607514
2265.994758	337757.639257	38.612532
2268.591800	338327.097832	38.617549
2270.912202	338896.316497	38.622567
2273.397088	339454.358531	38.627584
2275.459818	340022.642480	38.632602
2277.680067	340573.786285	38.637620
2280.360080	341139.112793	38.642637
2282.155109	341701.279255	38.647655
2284.602661	342258.382182	38.652672
2286.991513	342818.838730	38.657690
2288.652450	343396.008001	38.662708
2291.289541	343955.598157	38.667725
2293.786816	344526.651317	38.672743
2296.528032	345078.064002	38.677760
2298.504862	345641.651719	38.682778
2300.415349	346207.680008	38.687796
2303.281237	346773.112273	38.692813
2305.096209	347344.218236	38.697831
2307.597100	347896.068559	38.702848
2309.940433	348436.365782	38.707866
2311.947966	348973.641263	38.712884
2314.459403	349510.015087	38.717901
2316.185498	350044.355032	38.722919
2318.415615	350580.863919	38.727936
2320.697659	351133.319600	38.732954
2322.785872	351684.455386	38.737972
2325.461485	352237.466601	38.742989
2327.367849	352793.947311	38.748007
2329.849786	353347.407702	38.753024
2332.101492	353920.031668	38.758042
2334.113815	354481.624128	38.763060
2336.399102	355048.010591	38.768077
2338.538175	355634.027622	38.773095
2340.876168	356205.692939	38.778112
2343.216686	356793.512738	38.783130
2345.168509	357379.637614	38.788148
2347.920212	357970.722012	38.793165
2349.917719	358569.686207	38.798183
2352.183154	359169.130174	38.803200
2354.785387	359781.017753	38.808218
2357.091873	360382.847177	38.813236
2359.285033	360995.595590	38.818253
2361.027971	361601.812600	38.823271
2363.973345	362223.880949	38.828288
2366.445168	362853.882097	38.833306
2368.693867	363476.172350	38.838324
2371.239622	364105.405319	38.843341
2373.369950	364743.550056	38.848359
2375.816102	365373.818782	38.853376
2378.176818	366009.671983	38.858394
2380.350606	366643.693568	38.863412
2383.131678	367274.890043	38.868429
2385.288332	367927.537098	38.873447
2387.580593	368576.954259	38.878464
2390.041614	369218.443608	38.883482
2392.459173	369879.028531	38.888500
2395.219901	370524.072707	38.893517
2397.580532	371186.799264	38.898535
2400.022684	371850.337190	38.903552
2402.367489	372496.175662	38.908570
2404.797782	373161.770982	38.913588
2407.307070	373810.627296	38.918605
2409.895556	374477.439849	38.923623
2412.795498	375124.001024	38.928640
2415.072445	375780.619678	38.933658
2417.160682	376434.797123	38.938676
2420.104104	377079.869133	38.943693
2422.570595	377754.119863	38.948711
2424.975533	378397.734330	38.953728
2427.710928	379049.219120	38.958746
2429.906427	379705.649065	38.963764
2432.200482	380351.197085	38.968781
2434.851290	381016.806854	38.973799
2437.375345	381672.459262	38.978816
2440.235663	382320.259006	38.983834
2442.130398	382971.146483	38.988852
2444.845213	383617.524688	38.993869
2447.508384	384273.026006	38.998887
2450.080507	384927.337435	39.003904
2452.848153	385566.340776	39.008922
2454.849281	386223.229931	39.013940
2457.720457	386857.373354	39.018957
2459.798089	387507.048707	39.023975
2462.434784	388141.661357	39.028992
2465.277033	388785.175942	39.034010
2467.837255	389446.012412	39.039028
2470.243762	390062.650877	39.044045
2473.155304	390674.833689	39.049063
2475.617481	391264.315604	39.054080
2478.050766	391871.863979	39.059098
2480.319637	392460.315432	39.064116
2482.975340	393049.350657	39.069133
2485.357412	393654.767968	39.074151
2487.866325	394240.863929	39.079168
2490.293976	394836.187542	39.084186
2492.518047	395437.210104	39.089204
2494.919068	396044.958235	39.094221
2497.254519	396652.577957	39.099239
2499.348267	397267.549218	39.104256
2502.020891	397876.380461	39.109274
2504.083050	398513.708355	39.114292
2506.794260	399147.215269	39.119309
2509.180788	399786.691672	39.124327
2511.445633	400417.988924	39.129344
2514.183440	401052.589768	39.134362
2516.467048	401711.678604	39.139380
2518.958839	402349.509173	39.144397
2521.487526	403003.814438	39.149415
2524.031620	403659.976906	39.154432
2526.704143	404315.215989	39.159450
2528.996492	404977.748597	39.164468
2531.625140	405654.043244	39.169485
2533.489792	406325.532328	39.174503
2536.170437	406995.654299	39.179520
2538.893488	407677.001120	39.184538
2541.247052	408367.410496	39.189556
2543.727099	409039.263211	39.194573
2546.059461	409730.299902	39.199591
2548.584547	410426.150621	39.204608
2551.340717	411127.897798	39.209626
2553.781204	411837.581501	39.214644
2556.550594	412544.101719	39.219661
2559.138509	413258.079549	39.224679
2561.937203	413956.198490	39.229696
2564.387227	414657.066294	39.234714
2566.573240	415371.863055	39.239732
2569.397609	416088.231572	39.244749
2572.129858	416815.485175	39.249767
2574.523010	417527.376787	39.254784
2577.405853	418241.674787	39.259802
2580.181549	418973.240679	39.264820
2582.916208	419686.939920	39.269837
2585.185734	420409.304987	39.274855
2587.963577	421126.982275	39.279872
2590.943227	421846.352690	39.284890
2593.237067	422567.764981	39.289908
2595.958868	423286.730966	39.294925
2598.677336	424015.044107	39.299943
2601.450316	424741.301215	39.304960
2603.682644	425455.929693	39.309978
2606.373811	426189.498807	39.314996
2609.015362	426911.206465	39.320013
2611.589136	427641.105427	39.325031
2614.152301	428374.983402	39.330048
2616.685005	429089.707508	39.335066
2618.928876	429835.085031	39.340084
2622.167530	430564.379635	39.345101
2625.003350	431297.362762	39.350119
2627.151498	432030.284547	39.355136
2630.062590	432758.400665	39.360154
2632.704670	433494.586230	39.365172
2635.353004	434216.018644	39.370189
2637.716708	434952.608550	39.375207
2640.464061	435696.956194	39.380224
2642.847010	436411.986364	39.385242
2645.279179	437125.518318	39.390260
2648.032771	437827.537810	39.395277
2650.651153	438537.350854	39.400295
2653.162643	439241.896413	39.405312
2655.442876	439949.645828	39.410330
2657.818210	440666.869827	39.415348
2660.505486	441380.325550	39.420365
2663.093523	442100.605141	39.425383
2665.543480	442839.654592	39.430400
2668.137997	443568.435522	39.435418
2670.652710	444303.630406	39.440436
2673.345311	445054.504463	39.445453
2676.135807	445798.810535	39.450471
2678.599010	446554.982064	39.455488
2681.323886	447305.064308	39.460506
2683.826469	448066.790912	39.465524
2686.596824	448823.590394	39.470541
2689.427541	449600.028113	39.475559
2691.786933	450370.698724	39.480576
2694.882079	451142.838178	39.485594
2697.446895	451920.043436	39.490612
2700.058008	452710.765258	39.495629
2702.791703	453490.159832	39.500647
2705.589175	454277.049124	39.505664
2708.098503	455061.528790	39.510682
2710.846996	455854.939384	39.515700
2713.591169	456662.932240	39.520717
2716.487908	457463.536754	39.525735
2718.717078	458262.753631	39.530752
2721.800452	459075.700804	39.535770
2724.789864	459893.129906	39.540788
2727.551052	460704.497142	39.545805
2730.309822	461517.499932	39.550823
2733.131908	462330.762318	39.555840
2736.151660	463152.753572	39.560858
2738.820723	463975.627637	39.565876
2741.704523	464781.854347	39.570893
2744.713843	465595.254191	39.575911
2747.385139	466419.541242	39.580928
2750.179651	467241.498893	39.585946
2753.227452	468064.087259	39.590964
2755.872738	468877.864043	39.595981
2758.607266	469695.330652	39.600999
2761.443197	470523.558108	39.606016
2764.379603	471341.880776	39.611034
2767.208079	472161.448934	39.616052
2769.808211	472991.274599	39.621069
2772.540496	473818.566487	39.626087
2775.423381	474649.484566	39.631104
2778.010735	475470.816943	39.636122
2781.016568	476301.236885	39.641140
2783.656603	477127.841259	39.646157
2786.513728	477964.524441	39.651175
2789.174458	478798.424181	39.656192
2792.269514	479627.517635	39.661210
2794.600502	480472.354052	39.666228
2797.343089	481310.771172	39.671245
2800.318999	482140.223920	39.676263
2802.846778	482976.528779	39.681280
2805.830917	483822.766805	39.686298
2808.655356	484672.474700	39.691316
2811.278738	485515.864590	39.696333
2814.269276	486352.843510	39.701351
2817.034287	487206.932666	39.706368
2820.176792	488045.471986	39.711386
2822.752084	488900.822460	39.716404
2825.621087	489734.379371	39.721421
2828.692125	490557.062385	39.726439
2831.158876	491384.297645	39.731456
2833.924342	492177.783542	39.736474
2836.497237	492978.682697	39.741492
2839.304124	493794.694555	39.746509
2842.656578	494595.137200	39.751527
2845.066140	495410.632684	39.756544
2848.096086	496211.254217	39.761562
2850.946091	497034.419181	39.766580
2853.519214	497844.876515	39.771597
2856.444703	498667.242822	39.776615
2858.987997	499505.017066	39.781632
2862.020269	500327.586650	39.786650
2864.666653	501158.148446	39.791668
2867.735579	501992.633774	39.796685
2870.418058	502840.001163	39.801703
2873.294409	503684.872203	39.806720
2876.294706	504546.118842	39.811738
2879.059815	505395.609625	39.816756
2881.838080	506254.987184	39.821773
2885.119691	507102.689889	39.826791
2887.739646	507968.607546	39.831808
2890.667403	508827.621810	39.836826
2893.801905	509705.309280	39.841844
2896.577177	510580.235228	39.846861
2899.588803	511447.664313	39.851879
2902.386015	512322.188244	39.856896
2905.479830	513207.803892	39.861914
2908.381106	514079.390752	39.866932
2911.027381	514959.740038	39.871949
2914.529354	515840.100204	39.876967
2917.314653	516737.358938	39.881984
2919.964492	517621.185249	39.887002
2923.063945	518521.765508	39.892020
2926.052525	519416.366458	39.897037
2929.249551	520311.535819	39.902055
2932.259118	521208.346082	39.907072
2935.173736	522106.731146	39.912090
2938.098892	523002.895467	39.917108
2940.975332	523917.700574	39.922125
2944.200946	524813.959755	39.927143
2946.890823	525717.404946	39.932160
2950.053925	526618.854400	39.937178
2953.219249	527523.219914	39.942196
2955.946194	528433.846219	39.947213
2959.085278	529338.508274	39.952231
2961.877682	530258.728564	39.957248
2964.793839	531162.560265	39.962266
2967.919199	532083.114783	39.967284
2970.778854	532997.312888	39.972301
2974.326478	533908.118913	39.977319
2977.429504	534822.514423	39.982336
2980.237614	535731.213940	39.987354
2983.286531	536644.546779	39.992372
2986.375659	537557.865226	39.997389
2989.295787	538465.568175	40.002407
2992.332755	539381.696981	40.007424
2995.304824	540292.193081	40.012442
2998.524501	541207.469567	40.017460
3001.945459	542119.685648	40.022477
3004.816034	543028.814747	40.027495
3007.543965	543938.210221	40.032512
3010.489804	544852.841707	40.037530
3013.646900	545755.811607	40.042548
3016.737116	546680.859987	40.047565
3019.661110	547589.531845	40.052583
3022.635469	548505.576995	40.057600
3025.734852	549406.306646	40.062618
3028.829668	550301.699129	40.067636
3031.530042	551192.422824	40.072653
3034.760967	552056.459828	40.077671
3037.597874	552930.459019	40.082688
3040.413111	553791.840198	40.087706
3043.405456	554669.923120	40.092724
3045.820270	555545.480974	40.097741
3048.882683	556421.025635	40.102759
3051.709916	557317.605368	40.107776
3054.780569	558209.813897	40.112794
3057.569023	559111.002079	40.117812
3060.098502	560024.027580	40.122829
3063.560811	560929.853653	40.127847
3066.465529	561853.289830	40.132864
3069.176564	562782.669875	40.137882
3072.385026	563719.786844	40.142900
3075.032317	564657.431120	40.147917
3078.069367	565605.237664	40.152935
3081.280699	566564.996949	40.157952
3084.247590	567525.277428	40.162970
3087.226887	568485.082524	40.167988
3090.286738	569454.390798	40.173005
3093.686762	570422.515316	40.178023
3096.845708	571400.042252	40.183040
3099.786635	572383.251398	40.188058
3102.916169	573366.503591	40.193076
3105.717547	574368.701707	40.198093
3108.954548	575347.164791	40.203111
3112.242609	576354.794041	40.208128
3114.955564	577363.038795	40.213146
3118.292214	578367.888462	40.218164
3121.065267	579392.011434	40.223181
3124.493120	580404.054429	40.228199
3127.846566	581430.019130	40.233216
3130.900962	582446.720054	40.238234
3133.705086	583476.565704	40.243252
3136.742036	584522.832206	40.248269
3140.124255	585547.644039	40.253287
3143.137641	586608.674971	40.258304
3146.837596	587648.045108	40.263322
3150.050242	588686.353185	40.268340
3152.963297	589743.164500	40.273357
3156.337274	590783.018224	40.278375
3159.602154	591831.067196	40.283392
3162.385240	592881.007035	40.288410
3165.989634	593923.353515	40.293428
3168.934336	594985.805133	40.298445
3172.499118	596035.034660	40.303463
3175.469744	597104.002432	40.308480
3178.600399	598162.078200	40.313498
3181.630155	599221.426471	40.318516
3185.040776	600303.198236	40.323533
3188.061185	601361.300664	40.328551
3191.724650	602432.366726	40.333568
3194.534144	603498.017139	40.338586
3197.997996	604555.952237	40.343604
3201.267388	605636.443843	40.348621
3204.369419	606699.394528	40.353639
3207.421206	607778.016533	40.358656
3211.050905	608844.031376	40.363674
3214.328615	609919.559176	40.368692
3217.382789	610987.416716	40.373709
3220.816977	612050.457636	40.378727
3223.991070	613124.743789	40.383744
3227.111947	614185.331607	40.388762
3230.575352	615261.463587	40.393780
3233.728234	616323.941238	40.398797
3237.191399	617389.614960	40.403815
3240.272657	618443.599821	40.408832
3243.464584	619465.822577	40.413850
3246.650469	620490.799487	40.418868
3249.514498	621511.084764	40.423885
3252.929448	622524.686557	40.428903
3256.046695	623557.580286	40.433920
3259.328870	624574.559058	40.438938
3262.656813	625606.022097	40.443956
3265.589773	626633.454455	40.448973
3269.105488	627672.180281	40.453991
3272.552127	628712.763904	40.459008
3275.778226	629755.029665	40.464026
3279.085115	630794.882353	40.469044
3282.076374	631835.832873	40.474061
3284.771934	632890.658136	40.479079
3288.372738	633948.772338	40.484096
3291.377208	635017.908830	40.489114
3295.099609	636081.327154	40.494132
3298.035112	637162.332665	40.499149
3301.337089	638231.288809	40.504167
3304.986393	639317.889199	40.509184
3307.932919	640418.359724	40.514202
3311.811513	641504.491382	40.519220
3314.515637	642597.434745	40.524237
3317.965324	643693.429637	40.529255
3321.336583	644806.722935	40.534272
3324.241077	645906.906953	40.539290
3327.835388	647020.717502	40.544308
3331.209324	648148.897853	40.549325
3334.656374	649262.882922	40.554343
3338.242778	650389.081190	40.559360
3341.036055	651512.990586	40.564378
3344.666484	652636.286139	40.569396
3347.949578	653778.244917	40.574413
3351.738583	654919.988288	40.579431
3354.892496	656060.757499	40.584448
3357.980197	657212.661039	40.589466
3361.737733	658353.611701	40.594484
3364.980475	659506.165421	40.599501
3368.215762	660656.442878	40.604519
3371.965954	661815.459679	40.609536
3375.242050	662974.564889	40.614554
3378.700255	664130.365102	40.619572
3382.072025	665288.180261	40.624589
3385.316162	666451.747804	40.629607
3389.134070	667607.964414	40.634624
3392.181175	668781.827154	40.639642
3396.066371	669942.325011	40.644660
3399.244349	671120.253284	40.649677
3402.640548	672286.163323	40.654695
3406.202840	673457.768335	40.659712
3409.609010	674646.652574	40.664730
3413.292622	675801.637475	40.669748
3416.750586	676974.259860	40.674765
3419.957278	678139.420453	40.679783
3423.908734	679315.789819	40.684800
3427.054398	680484.987484	40.689818
3430.722196	681651.267847	40.694836
3434.140020	682831.249364	40.699853
3437.774752	683991.177085	40.704871
3441.035685	685163.929702	40.709888
3444.376440	686337.163175	40.714906
3448.159004	687502.427188	40.719924
3451.308353	688678.317361	40.724941
3454.509563	689843.572978	40.729959
3458.306283	691013.243919	40.734976
3461.536033	692199.428055	40.739994
3465.274063	693368.303984	40.745012
3468.527629	694522.427122	40.750016
3471.964861	695629.889638	40.755021
3475.541446	696687.867634	40.760026
3478.578063	697683.216550	40.765031
3481.650863	698611.090271	40.770036
3484.540828	699489.091845	40.775040
3487.841003	700289.455319	40.780045
3490.358171	701008.820322	40.785050
3492.852670	701678.884687	40.790055
3495.849859	702289.138467	40.795060
3498.285376	702822.081402	40.800064
3500.504767	703302.214238	40.805069
3503.100917	703712.556585	40.810074
3505.044431	704058.752614	40.815079
3507.213773	704355.518723	40.820084
3508.967549	704591.589949	40.825088
3510.907516	704789.225691	40.830093
3512.300854	704919.341187	40.835098
3513.589059	705020.711293	40.840103
3515.515329	705072.053927	40.845108
3516.823110	705079.041048	40.850112
3518.231214	705042.945173	40.855117
3519.407011	704958.853218	40.860122
3519.983675	704867.110012	40.865127
3521.134903	704726.391195	40.870132
3522.333129	704569.418377	40.875136
3522.979001	704370.209071	40.880141
3524.099308	704151.095430	40.885146
3524.944299	703894.513542	40.890151
3525.711941	703627.901209	40.895156
3526.066162	703337.153280	40.900160
3527.079168	703011.458134	40.905165
3527.418633	702678.309395	40.910170
3527.672056	702331.944901	40.915175
3528.233481	701960.123935	40.920180
3528.561791	701588.275812	40.925184
3528.745343	701201.576864	40.930189
3529.748408	700793.157100	40.935194
3529.838021	700378.059890	40.940199
3529.981976	699947.675450	40.945204
3530.318314	699514.603796	40.950208
3530.567553	699064.028163	40.955213
3531.050688	698597.583123	40.960218
3530.885031	698148.321291	40.965223
3531.452675	697681.714280	40.970228
3531.482442	697192.450157	40.975232
3531.594551	696716.122353	40.980237
3532.024123	696219.628339	40.985242
3531.586758	695729.713656	40.990247
3531.895037	695230.896691	40.995252
3531.632808	694729.758514	41.000256
3531.465748	694225.393319	41.005261
3531.548979	693728.717240	41.010266
3531.350222	693222.012378	41.015271
3531.703910	692707.377995	41.020276
3531.796561	692210.167937	41.025280
3531.163886	691696.980905	41.030285
3531.399372	691190.387532	41.035290
3531.298199	690677.452405	41.040295
3531.339311	690150.731488	41.045300
3530.952525	689645.695771	41.050304
3531.121159	689133.772392	41.055309
3531.410547	688622.695762	41.060314
3531.135572	688111.782663	41.065319
3531.251505	687583.555317	41.070324
3530.913361	687069.258911	41.075328
3530.765081	686564.260043	41.080333
3530.488337	686040.337839	41.085338
3530.722949	685541.939177	41.090343
3530.345765	685013.543566	41.095348
3530.260820	684518.228094	41.100352
3530.170780	683999.235787	41.105357
3530.215581	683491.793675	41.110362
3529.847689	682993.155547	41.115367
3529.771057	682483.287171	41.120372
3529.472989	681983.188076	41.125376
3529.342747	681481.290859	41.130381
3529.514239	680977.473589	41.135386
3529.003589	680484.201232	41.140391
3529.327105	679992.060100	41.145396
3528.687803	679494.222909	41.150400
3528.518453	678997.626489	41.155405
3528.194022	678508.053656	41.160410
3528.141661	678023.890648	41.165415
3528.163177	677529.176842	41.170420
3527.708771	677058.632149	41.175424
3527.808587	676577.408060	41.180429
3527.483969	676106.444914	41.185434
3527.577554	675624.524704	41.190439
3527.502260	675134.234456	41.195444
3526.970767	674680.427722	41.200448
3526.855781	674207.440110	41.205453
3526.689353	673731.944730	41.210458
3526.406002	673287.749561	41.215463
3526.674094	672825.296640	41.220468
3526.426515	672363.205031	41.225472
3526.480388	671898.947067	41.230477
3526.175102	671444.497663	41.235482
3525.725464	670994.886631	41.240487
3525.630379	670531.981950	41.245492
3525.355772	670101.696358	41.250496
3525.315810	669652.402684	41.255501
3525.364850	669212.149427	41.260506
3525.029355	668769.146212	41.265511
3524.868592	668326.293018	41.270516
3524.342203	667902.732052	41.275520
3524.350111	667463.651415	41.280525
3523.756940	667029.438229	41.285530
3523.617021	666624.013407	41.290535
3523.650225	666193.699552	41.295540
3523.758992	665775.127526	41.300544
3523.169684	665358.947176	41.305549
3523.571815	664947.175492	41.310554
3522.936770	664539.798086	41.315559
3523.027467	664135.527094	41.320564
3523.048970	663728.506049	41.325568
3522.554382	663329.387291	41.330573
3522.456738	662924.996649	41.335578
3521.806395	662528.714855	41.340583
3522.009786	662145.002448	41.345588
3521.869750	661758.736112	41.350592
3521.607388	661369.779298	41.355597
3521.538825	660974.635592	41.360602
3521.512208	660594.094025	41.365607
3521.606365	660214.016800	41.370612
3521.606445	659835.537614	41.375616
3521.568382	659447.814580	41.380621
3521.287550	659070.500094	41.385626
3520.806608	658694.551936	41.390631
3520.695966	658322.622264	41.395636
3520.467774	657953.194226	41.400640
3520.013219	657594.175081	41.405645
3520.379300	657215.434009	41.410650
3520.067599	656875.089609	41.415655
3520.293351	656514.071184	41.420660
3520.113870	656157.500784	41.425664
3519.597464	655798.026508	41.430669
3519.589709	655443.199710	41.435674
3519.536919	655099.055402	41.440679
3519.491106	654746.956657	41.445684
3519.527880	654403.472525	41.450688
3519.071729	654058.659100	41.455693
3518.946887	653712.180631	41.460698
3518.356128	653390.493017	41.465703
3518.478292	653043.201128	41.470708
3518.313257	652717.075505	41.475712
3517.963882	652383.475981	41.480717
3518.031724	652057.340244	41.485722
3517.451366	651745.739116	41.490727
3517.339609	651426.856501	41.495732
3517.490077	651115.814670	41.500736
3517.363400	650795.015661	41.505741
3517.556141	650481.398844	41.510746
3517.130778	650177.268019	41.515751
3517.247024	649870.989925	41.520756
3517.298539	649567.961234	41.525760
3517.124718	649260.063173	41.530765
3517.079421	648954.283350	41.535770
3516.717103	648650.445507	41.540775
3516.723543	648342.139695	41.545780
3516.516107	648040.706740	41.550784
3516.328376	647745.059194	41.555789
3516.268581	647450.131594	41.560794
3516.207922	647157.494713	41.565799
3515.976116	646870.425812	41.570804
3515.972032	646581.011852	41.575808
3515.524240	646302.709912	41.580813
3515.808099	646018.780970	41.585818
3515.536013	645745.333607	41.590823
3515.390049	645448.212069	41.595828
3515.231724	645179.629834	41.600832
3515.176529	644908.473771	41.605837
3515.054080	644636.871573	41.610842
3514.539172	644370.676438	41.615847
3515.014743	644094.811439	41.620852
3514.671661	643839.673669	41.625856
3514.595807	643569.085208	41.630861
3514.503843	643303.942438	41.635866
3514.221255	643047.724781	41.640871
3514.140377	642791.617453	41.645876
3514.599311	642538.015046	41.650880
3513.897934	642293.098746	41.655885
3513.829539	642028.869051	41.660890
3513.640172	641782.805959	41.665895
3513.540750	641533.871504	41.670900
3513.552629	641292.214406	41.675904
3512.964679	641053.001062	41.680909
3513.012060	640806.275311	41.685914
3513.028644	640584.956582	41.690919
3512.726914	640341.078029	41.695924
3513.010942	640112.802746	41.700928
3512.683285	639868.317019	41.705933
3513.110339	639646.660332	41.710938
3512.754365	639432.981209	41.715943
3512.525163	639190.714093	41.720948
3512.136738	638971.928472	41.725952
3511.892775	638753.664666	41.730957
3512.196881	638539.107858	41.735962
3511.974777	638313.227263	41.740967
3511.781351	638101.444771	41.745972
3511.836897	637895.320164	41.750976
3511.721359	637679.313787	41.755981
3512.070280	637476.634561	41.760986
3511.537548	637262.989640	41.765991
3511.638579	637052.688125	41.770996
3511.238071	636847.968683	41.776000
3510.942747	636631.019418	41.781005
3511.203921	636441.943824	41.786010
3510.721879	636252.536927	41.791015
3510.741701	636054.437443	41.796020
3510.866463	635860.169843	41.801024
3510.730798	635667.142470	41.806029
3510.899949	635470.358310	41.811034
3510.572031	635284.160979	41.816039
3510.373547	635089.531926	41.821044
3510.312251	634905.785997	41.826048
3510.166069	634720.849764	41.831053
3510.414044	634525.285862	41.836058
3510.078398	634357.339567	41.841063
3510.328638	634167.173504	41.846068
3510.187298	633987.978831	41.851072
3509.811147	633818.629221	41.856077
3509.917340	633628.627241	41.861082
3509.825335	633460.676434	41.866087
3509.952603	633276.670574	41.871092
3510.025185	633101.629730	41.876096
3509.872732	632931.428074	41.881101
3510.031487	632753.664390	41.886106
3509.590638	632584.255420	41.891111
3509.541843	632406.419944	41.896116
3509.801508	632238.591828	41.901120
3509.468157	632073.061236	41.906125
3509.430646	631896.767024	41.911130
3509.254585	631737.162042	41.916135
3509.376708	631568.144495	41.921140
3509.650416	631412.715483	41.926144
3509.120608	631240.446105	41.931149
3509.273403	631082.829491	41.936154
3508.836220	630910.489391	41.941159
3509.001994	630756.420161	41.946164
3509.237099	630592.124302	41.951168
3508.770509	630437.203406	41.956173
3509.131280	630275.084735	41.961178
3508.636360	630116.008396	41.966183
3508.610820	629959.505841	41.971188
3508.694187	629808.340220	41.976192
3508.460288	629673.596928	41.981197
3508.556138	629521.173451	41.986202
3508.557371	629366.610390	41.991207
3508.522594	629210.699116	41.996212
3508.320414	629060.921769	42.001216
3508.325474	628923.776233	42.006221
3508.374567	628783.016479	42.011226
3508.229008	628635.727400	42.016231
3508.310784	628486.646245	42.021236
3508.360216	628346.681825	42.026240
3507.795250	628205.464784	42.031245
3507.831623	628055.533788	42.036250
3507.421317	627930.762441	42.041255
3507.734927	627784.838110	42.046260
3507.786412	627652.225495	42.051264
3507.662225	627514.081513	42.056269
3507.820695	627377.291365	42.061274
3507.670283	627251.417574	42.066279
3507.176915	627121.392097	42.071284
3507.414808	626996.352745	42.076288
3507.291496	626865.712285	42.081293
3507.565679	626734.403744	42.086298
3507.098675	626608.574533	42.091303
3507.124190	626476.402313	42.096308
3507.516255	626348.925994	42.101312
3507.064972	626233.607310	42.106317
3507.219753	626103.713048	42.111322
3507.200700	625989.372282	42.116327
3507.230565	625861.398900	42.121332
3507.311195	625732.363808	42.126336
3506.838637	625611.682672	42.131341
3507.083310	625491.082338	42.136346
3506.908115	625383.472560	42.141351
3506.779978	625261.779052	42.146356
3506.972129	625141.634239	42.151360
3506.786723	625026.609359	42.156365
3506.910637	624903.267379	42.161370
3506.528390	624786.018291	42.166375
3506.538949	624672.910869	42.171380
3506.732978	624563.979742	42.176384
3506.611473	624454.798951	42.181389
3506.605447	624340.338267	42.186394
3506.460229	624221.641355	42.191399
3506.438539	624103.123154	42.196404
3506.568898	623990.940602	42.201408
3506.595270	623891.147491	42.206413
3506.705631	623774.607712	42.211418
3506.499999	623677.806491	42.216423
3506.280448	623553.052835	42.221428
3506.419750	623456.092589	42.226432
3506.299470	623348.653768	42.231437
3506.441449	623234.557718	42.236442
3505.937963	623129.033482	42.241447
3506.241250	623019.667940	42.246452
3506.220294	622918.019952	42.251456
3505.763099	622826.713388	42.256461
3506.348202	622717.348446	42.261466
3505.935157	622616.363433	42.266471
3505.772562	622512.881236	42.271476
3505.792687	622407.514168	42.276480
3505.451225	622318.388717	42.281485
3505.942143	622211.138474	42.286490
3505.745797	622131.657409	42.291495
3506.150485	622027.876680	42.296500
3505.802117	621938.097885	42.301504
3505.649060	621829.647274	42.306509
3505.696217	621731.384016	42.311514
3505.571066	621629.039609	42.316519
3505.244706	621542.210128	42.321524
3505.843723	621451.319171	42.326528
3505.744764	621359.640547	42.331533
3505.759665	621253.361188	42.336538
3505.600433	621163.093837	42.341543
3505.734508	621075.032266	42.346548
3505.720582	620977.774407	42.351552
3505.503006	620889.268190	42.356557
3505.759630	620788.807193	42.361562
3505.772713	620690.840782	42.366567
3505.322617	620603.823739	42.371572
3505.860845	620512.183291	42.376576
3505.472280	620421.847347	42.381581
3505.921288	620319.897095	42.386586
3505.637803	620241.669326	42.391591
3505.631317	620136.735590	42.396596
3505.490883	620039.239618	42.401600
3505.302843	619950.119532	42.406605
3505.293968	619844.882697	42.411610
3505.506843	619766.569721	42.416615
3505.197055	619676.866092	42.421620
3505.429572	619592.985920	42.426624
3505.247867	619506.366905	42.431629
3505.534577	619412.303005	42.436634
3505.283973	619336.569100	42.441639
3505.237588	619246.317363	42.446644
3505.312992	619152.336159	42.451648
3505.128562	619077.692125	42.456653
3505.507027	618984.210824	42.461658
3505.254871	618903.963580	42.466663
3505.306078	618805.121923	42.471668
3505.313885	618717.112215	42.476672
3504.762240	618635.859854	42.481677
3504.971213	618555.283465	42.486682
3504.939780	618475.397657	42.491687
3504.879875	618393.861986	42.496692
3504.966835	618313.103437	42.501696
3505.182339	618234.728925	42.506701
3505.420992	618152.340319	42.511706
3505.420644	618068.186089	42.516711
3505.077619	617986.343183	42.521716
3505.219753	617888.029603	42.526720
3505.144595	617806.391825	42.531725
3505.308696	617716.644132	42.536730
3504.916830	617639.819032	42.541735
3504.671463	617555.500745	42.546740
3504.887054	617477.972920	42.551744
3504.988440	617402.167614	42.556749
3505.006853	617324.570948	42.561754
3504.800976	617245.807678	42.566759
3505.172747	617161.484919	42.571764
3505.253658	617082.372462	42.576768
3504.910372	617007.138968	42.581773
3504.934850	616916.756097	42.586778
3504.779338	616836.878796	42.591783
3504.764065	616763.895450	42.596788
3505.246182	616680.102223	42.601792
3504.628930	616599.196461	42.606797
3504.735354	616525.239034	42.611802
3504.866890	616442.003054	42.616807
3504.899575	616367.956463	42.621812
3504.951280	616291.901040	42.626816
3504.808141	616213.220291	42.631821
3505.199616	616126.831013	42.636826
3504.837869	616048.185108	42.641831
3504.859528	615979.401486	42.646836
3504.928728	615901.686150	42.651840
3504.719190	615830.433107	42.656845
3504.692026	615745.062333	42.661850
3504.568793	615673.493259	42.666855
3504.909594	615597.184872	42.671860
3504.744216	615526.373786	42.676864
3504.419640	615447.316399	42.681869
3504.385669	615376.181892	42.686874
3504.351699	615305.046926	42.691879
3504.777709	615228.120335	42.696884
3504.762697	615157.031427	42.701888
3504.174906	615099.171933	42.706893
3504.428228	615023.976982	42.711898
3504.290493	614953.458480	42.716903
3504.446146	614881.086272	42.721908
3504.237686	614806.567574	42.726912
3504.348153	614741.521860	42.731917
3504.547391	614665.230369	42.736922
3504.799323	614599.007347	42.741927
3504.624319	614534.609111	42.746932
3504.595628	614454.493101	42.751936
3504.456358	614386.628570	42.756941
3504.536364	614305.290242	42.761946
3504.776656	614244.933285	42.766951
3504.512525	614171.723106	42.771956
3504.576617	614100.764795	42.776960
3504.409101	614043.983739	42.781965
3504.622133	613966.080674	42.786970
3504.551243	613891.382724	42.791975
3504.377981	613825.325427	42.796980
3504.409493	613748.152720	42.801985
3504.173100	613681.302703	42.806989
3504.474600	613613.210378	42.811994
3504.404316	613542.170352	42.816999
3504.217283	613470.497254	42.822004
3504.307409	613408.154780	42.827009
3504.015720	613347.930749	42.832013
3504.217951	613279.852739	42.837018
3504.181893	613222.343804	42.842023
3504.180397	613156.605229	42.847028
3504.030156	613086.728783	42.852033
3504.169731	613031.195697	42.857037
3504.410116	612957.292631	42.862042
3504.120746	612893.555597	42.867047
3504.165464	612827.105424	42.872052
3504.420221	612751.042355	42.877057
3504.492025	612698.477392	42.882061
3504.592056	612623.742753	42.887066
3504.246769	612546.974823	42.892071
3504.401394	612487.274346	42.897076
3504.513018	612415.244348	42.902081
3504.194818	612361.187486	42.907085
3504.269497	612283.997503	42.912090
3504.211043	612223.478208	42.917095
3504.260092	612154.716482	42.922100
3504.325607	612093.373673	42.927105
3504.210162	612022.431682	42.932109
3504.146032	611953.185871	42.937114
3504.121267	611887.393488	42.942119
3504.270673	611823.176823	42.947124
3504.504356	611748.965949	42.952129
3504.109785	611687.696724	42.957133
3504.213514	611625.993993	42.962138
3503.919879	611568.067601	42.967143
3504.044077	611498.888240	42.972148
3504.428776	611435.834216	42.977153
3504.185530	611381.659949	42.982157
3504.154778	611308.593073	42.987162
3504.327252	611248.983337	42.992167
3504.154372	611176.139627	42.997172
3504.268677	611115.084323	43.002177
3503.775277	611055.131899	43.007181
3504.104056	610977.088552	43.012186
3503.982128	610924.797931	43.017191
3503.921084	610861.011652	43.022196
3503.795153	610798.439417	43.027201
3503.680548	610764.804412	43.032205
3504.091037	610697.980360	43.037210
3503.784422	610629.318011	43.042215
3504.031065	610577.316120	43.047220
3504.065722	610514.013652	43.052225
3504.016252	610460.806114	43.057229
3504.067565	610391.230667	43.062234
3504.117730	610338.758480	43.067239
3503.923957	610275.993878	43.072244
3503.933520	610205.922589	43.077249
3504.052988	610152.083857	43.082253
3503.920112	610074.862668	43.087258
3504.112327	610015.092641	43.092263
3503.830645	609962.924171	43.097268
3503.822498	609902.032912	43.102273
3503.545820	609853.725337	43.107277
3503.709432	609792.504226	43.112282
3504.078795	609747.450409	43.117287
3503.893984	609691.051313	43.122292
3504.155734	609620.082094	43.127297
3503.701251	609569.495232	43.132301
3503.875457	609490.915255	43.137306
3503.761713	609454.667824	43.142311
3503.651686	609388.924972	43.147316
3503.984146	609333.090934	43.152321
3503.815681	609273.175751	43.157325
3504.205057	609214.472533	43.162330
3503.802465	609152.939947	43.167335
3503.626808	609099.345452	43.172340
3504.225474	609030.524141	43.177345
3504.111278	608981.885066	43.182349
3503.832115	608924.594739	43.187354
3504.002113	608859.254115	43.192359
3504.098031	608806.115108	43.197364
3503.808254	608744.310877	43.202369
3503.560160	608692.582449	43.207373
3504.004474	608629.101528	43.212378
3504.020737	608570.456439	43.217383
3503.796895	608518.271731	43.222388
3503.931013	608447.466649	43.227393
3503.704752	608397.639550	43.232397
3503.790483	608327.243010	43.237402
3503.755266	608284.808472	43.242407
3503.579170	608225.340464	43.247412
3503.881338	608159.823510	43.252417
3503.470891	608121.965182	43.257421
3503.634117	608055.768185	43.262426
3503.706383	608002.829958	43.267431
3503.650435	607951.267134	43.272436
3503.732372	607893.811726	43.277441
3503.662210	607839.591842	43.282445
3503.554211	607781.565146	43.287450
3503.799351	607720.720691	43.292455
3503.403673	607678.794790	43.297460
3503.872392	607616.257362	43.302465
3503.383839	607574.145701	43.307469
3503.431941	607504.201755	43.312474
3503.618837	607465.239400	43.317479
3503.377768	607412.350040	43.322484
3503.641854	607354.510687	43.327489
3503.367213	607316.526937	43.332493
3503.441902	607251.744592	43.337498
3503.497113	607213.204434	43.342503
3503.614816	607171.192051	43.347508
3503.501747	607116.925601	43.352513
3503.307509	607065.331352	43.357517
3503.661702	607008.930358	43.362522
3504.006049	606960.909415	43.367527
3503.699344	606906.774210	43.372532
3504.047144	606848.617446	43.377537
3503.859317	606788.290879	43.382541
3504.118292	606719.561654	43.387546
3503.792806	606670.997615	43.392551
3503.877836	606614.739360	43.397556
3504.025948	606550.191772	43.402561
3503.682094	606505.593773	43.407565
3503.524180	606444.407489	43.412570
3503.462816	606386.667001	43.417575
3503.719437	606340.464169	43.422580
3503.609238	606283.483824	43.427585
3503.690572	606230.535817	43.432589
3503.599425	606170.190029	43.437594
3503.827960	606124.041120	43.442599
3503.536400	606071.153817	43.447604
3503.790316	606014.011767	43.452609
3503.452825	605971.869248	43.457613
3503.531354	605907.480001	43.462618
3503.432415	605863.190352	43.467623
3503.559869	605802.806590	43.472628
3503.462830	605752.695662	43.477633
3503.268195	605698.435865	43.482637
3503.486032	605646.265482	43.487642
3503.464753	605606.578385	43.492647
3503.421848	605547.024183	43.497652
3503.605298	605499.876609	43.502657
3503.861218	605460.293858	43.507661
3503.900310	605408.252196	43.512666
3503.588045	605349.795103	43.517671
3503.502716	605293.056588	43.522676
3503.716892	605223.874088	43.527681
3503.545239	605184.160118	43.532685
3503.529976	605115.416205	43.537690
3503.695505	605082.671523	43.542695
3503.728502	605038.557644	43.547700
3503.616663	604981.119418	43.552705
3503.235007	604928.743452	43.557709
3503.391983	604871.360737	43.562714
3503.494103	604817.650013	43.567719
3503.350824	604769.599813	43.572724
3503.541169	604713.967162	43.577729
3503.260630	604678.384280	43.582733
3503.428522	604627.020372	43.587738
3503.615991	604579.667602	43.592743
3503.403488	604529.269222	43.597748
3503.413206	604479.887840	43.602753
3503.666542	604432.122141	43.607757
3503.388412	604374.908995	43.612762
3503.748817	604328.379802	43.617767
3503.686295	604268.470867	43.622772
3503.786874	604214.807745	43.627777
3503.746696	604155.045085	43.632781
3503.598932	604092.539692	43.637786
3503.718439	604053.024725	43.642791
3503.361917	604000.489799	43.647796
3503.566220	603942.341843	43.652801
3503.247541	603897.528727	43.657805
3503.547580	603843.078210	43.662810
3503.835858	603794.350562	43.667815
3503.619852	603741.741105	43.672820
3503.627880	603681.516352	43.677825
3503.529293	603646.502504	43.682829
3503.713537	603594.227905	43.687834
3503.624134	603551.182372	43.692839
3503.154829	603492.340140	43.697844
3503.511260	603451.830500	43.702849
3502.976161	603396.561919	43.707853
3503.637802	603340.844925	43.712858
3503.582514	603299.398835	43.717863
3503.485842	603244.810095	43.722868
3503.718992	603194.934652	43.727873
3503.416383	603149.312939	43.732877
3503.402995	603097.018451	43.737882
3503.699679	603052.552320	43.742887
3503.467285	602994.371136	43.747892
3503.795464	602941.417380	43.752897
3503.616610	602887.442755	43.757901
3503.222215	602836.063088	43.762906
3503.626910	602789.118826	43.767911
3503.189271	602747.683556	43.772916
3503.385330	602691.237086	43.777921
3503.271028	602646.034055	43.782925
3503.444213	602589.590855	43.787930
3503.594627	602547.054134	43.792935
3503.083406	602494.838936	43.797940
3503.427044	602444.942028	43.802945
3503.282288	602403.708210	43.807949
3503.204133	602353.428682	43.812954
3503.269340	602296.801069	43.817959
3503.146912	602256.717469	43.822964
3503.666757	602209.551095	43.827969
3503.126012	602160.551580	43.832973
3503.402603	602109.258859	43.837978
3503.512138	602058.043633	43.842983
3503.279433	602024.201382	43.847988
3503.430195	601968.712507	43.852993
3503.499782	601934.217851	43.857997
3503.595351	601878.336083	43.863002
3503.532338	601829.306624	43.868007
3503.474765	601775.959318	43.873012
3503.361226	601728.293011	43.878017
3503.240779	601678.670036	43.883021
3503.237824	601629.529439	43.888026
3503.464423	601581.404911	43.893031
3503.195274	601540.339081	43.898036
3503.583058	601483.051958	43.903041
3503.407777	601440.665210	43.908045
3503.441876	601394.228095	43.913050
3503.604196	601340.842537	43.918055
3503.263134	601295.621368	43.923060
3503.774824	601244.135465	43.928065
3503.184489	601199.005190	43.933069
3503.198489	601141.828164	43.938074
3503.338350	601100.241589	43.943079
3503.051549	601052.902224	43.948084
3503.321393	601006.274105	43.953089
3502.944701	600966.980884	43.958093
3503.039211	600911.395792	43.963098
3503.060635	600882.528150	43.968103
3502.898865	600837.978419	43.973108
3502.997058	600793.486076	43.978113
3502.753756	600750.857004	43.983117
3503.087424	600704.618744	43.988122
3502.973013	600672.660601	43.993127
3502.661078	600634.309365	43.998132
3503.299562	600589.476205	44.003137
3503.141329	600545.125560	44.008141
3503.049781	600505.331977	44.013146
3503.026022	600462.213860	44.018151
3502.981737	600426.327847	44.023156
3502.949726	600381.654572	44.028161
3502.983806	600344.399971	44.033165
3503.130900	600299.044250	44.038170
3502.960676	600262.074056	44.043175
3502.911472	600233.969452	44.048180
3503.252936	600181.151431	44.053185
3503.091865	600149.601143	44.058189
3502.916339	600107.259737	44.063194
3502.843840	600060.182198	44.068199
3502.790468	600016.816289	44.073204
3503.386066	599976.154617	44.078209
3503.131152	599938.695320	44.083213
3503.145822	599896.522612	44.088218
3503.156614	599845.514651	44.093223
3503.171590	599808.763505	44.098228
3503.368986	599753.557519	44.103233
3503.141922	599712.478248	44.108237
3503.195108	599674.063658	44.113242
3503.041789	599627.499715	44.118247
3503.101593	599585.268233	44.123252
3503.107753	599533.104962	44.128257
3502.986116	599495.421450	44.133261
3502.877262	599457.986732	44.138266
3502.818849	599418.334564	44.143271
3502.715339	599379.995025	44.148276
3503.141374	599338.304755	44.153281
3503.108521	599309.944186	44.158285
3503.044724	599264.066907	44.163290
3503.336785	599221.042742	44.168295
3503.280600	599183.247017	44.173300
3503.011708	599128.064687	44.178305
3503.101776	599088.035479	44.183309
3503.141366	599047.663006	44.188314
3503.470227	598989.419328	44.193319
3503.308247	598958.920289	44.198324
3503.520133	598900.394200	44.203329
3502.908040	598862.739245	44.208333
3503.151627	598816.006224	44.213338
3503.310019	598761.705684	44.218343
3502.916161	598727.830118	44.223348
3503.307092	598673.942720	44.228353
3503.148042	598635.409041	44.233357
3503.217431	598582.578371	44.238362
3503.120851	598535.699445	44.243367
3503.172680	598499.339749	44.248372
3503.016447	598455.884537	44.253377
3503.022694	598419.281056	44.258381
3503.038921	598370.826389	44.263386
3503.499814	598342.030629	44.268391
3503.123755	598296.552452	44.273396
3503.234365	598246.977101	44.278401
3502.892155	598203.501382	44.283405
3502.598348	598159.917102	44.288410
3503.258266	598116.928657	44.293415
3503.005457	598086.090819	44.298420
3503.211948	598025.603001	44.303425
3502.581791	597995.379426	44.308429
3502.748741	597948.053016	44.313434
3502.938591	597909.509649	44.318439
3503.028315	597870.982653	44.323444
3502.864800	597831.041119	44.328449
3502.962298	597797.081870	44.333453
3502.592758	597760.036122	44.338458
3503.021117	597716.783088	44.343463
3502.596721	597683.411632	44.348468
3502.679770	597642.575210	44.353473
3502.671516	597625.654947	44.358477
3502.357110	597579.611467	44.363482
3502.753786	597556.900109	44.368487
3502.474330	597519.035342	44.373492
3503.095683	597487.399097	44.378497
3502.640140	597446.952022	44.383501
3502.674626	597411.043708	44.388506
3503.007592	597370.114936	44.393511
3502.668479	597347.122708	44.398516
3502.989739	597287.315144	44.403521
3502.930054	597263.322636	44.408525
3502.807576	597209.262002	44.413530
3502.963604	597176.195161	44.418535
3502.579521	597135.032223	44.423540
3503.099397	597097.285441	44.428545
3502.793542	597068.361818	44.433549
3502.856385	597021.199451	44.438554
3502.906524	596984.785095	44.443559
3502.741228	596952.774881	44.448564
3503.130279	596907.617139	44.453569
3502.760610	596872.075062	44.458573
3502.855758	596826.965441	44.463578
3502.945870	596792.753408	44.468583
3502.533971	596753.853440	44.473588
3502.923504	596725.617839	44.478593
3502.774566	596685.167814	44.483597
3502.731956	596654.592850	44.488602
3503.027773	596612.412128	44.493607
3502.648000	596579.431893	44.498612
3502.776429	596534.566746	44.503617
3502.648174	596509.529425	44.508621
3502.518042	596467.719676	44.513626
3502.626082	596433.804945	44.518631
3502.451166	596407.218342	44.523636
3503.069107	596367.343897	44.528641
3502.630498	596325.433819	44.533645
3502.557408	596289.389132	44.538650
3502.867387	596266.287812	44.543655
3502.428556	596233.868737	44.548660
3502.748107	596188.418364	44.553665
3502.563593	596158.719209	44.558669
3502.578599	596128.133376	44.563674
3502.796004	596087.068504	44.568679
3502.958940	596055.303060	44.573684
3502.962868	596017.637824	44.578689
3502.890864	595972.100477	44.583693
3502.983489	595942.907524	44.588698
3503.087397	595891.716247	44.593703
3502.933435	595853.976063	44.598708
3503.319375	595817.452520	44.603713
3502.844177	595785.540400	44.608717
3502.716599	595739.207777	44.613722
3502.865028	595707.192677	44.618727
3502.638596	595670.066494	44.623732
3503.077459	595621.681443	44.628737
3502.735482	595585.377572	44.633741
3502.616315	595551.146179	44.638746
3502.624907	595511.971903	44.643751
3502.702082	595485.592775	44.648756
3502.880305	595452.567635	44.653761
3502.771935	595407.536309	44.658765
3502.687695	595374.654644	44.663770
3502.952715	595341.866001	44.668775
3502.905949	595301.896587	44.673780
3502.957132	595260.303766	44.678785
3502.880348	595230.182723	44.683789
3502.580944	595189.199875	44.688794
3502.794857	595158.327621	44.693799
3502.194654	595124.576038	44.698804
3503.047588	595085.311426	44.703809
3502.562540	595060.480474	44.708813
3502.701687	595024.547597	44.713818
3502.775794	594983.201137	44.718823
3502.328822	594954.948455	44.723828
3502.879777	594923.065785	44.728833
3502.924179	594888.805507	44.733837
3502.590278	594859.881046	44.738842
3502.924448	594806.989688	44.743847
3502.676271	594784.831256	44.748852
3502.899543	594732.259186	44.753857
3502.699667	594708.184097	44.758861
3502.639297	594673.789783	44.763866
3502.709498	594625.612063	44.768871
3502.769794	594600.941401	44.773876
3502.735547	594562.926211	44.778881
3502.678050	594529.736421	44.783885
3502.813863	594495.911970	44.788890
3502.873799	594458.383183	44.793895
3502.507414	594428.006450	44.798900
3502.801461	594388.178675	44.803905
3502.624882	594354.957789	44.808909
3502.781690	594317.111229	44.813914
3502.948163	594283.582477	44.818919
3502.532504	594243.519574	44.823924
3502.858766	594200.973591	44.828929
3502.713066	594171.966196	44.833933
3502.881690	594130.601168	44.838938
3503.225109	594098.348650	44.843943
3502.739518	594057.342309	44.848948
3502.870963	594019.348290	44.853953
3502.784728	593979.682257	44.858957
3502.860750	593942.299862	44.863962
3503.047592	593892.291701	44.868967
3502.719277	593869.943836	44.873972
3502.924772	593833.845710	44.878977
3502.965165	593806.313616	44.883981
3502.868456	593765.844927	44.888986
3502.795201	593725.472692	44.893991
3502.403583	593689.522750	44.898996
3502.869321	593639.969857	44.904001
3502.876219	593614.150645	44.909005
3502.689135	593580.175859	44.914010
3503.003328	593533.359911	44.919015
3502.791011	593497.078455	44.924020
3503.008375	593460.324237	44.929025
3502.806151	593424.442739	44.934029
3502.974515	593388.700986	44.939034
3503.104945	593345.380500	44.944039
3502.840949	593320.710369	44.949044
3502.528406	593260.735605	44.954049
3502.439769	593243.671578	44.959053
3502.866612	593208.589927	44.964058
3502.777823	593169.524372	44.969063
3502.300715	593143.783891	44.974068
3502.954299	593109.066436	44.979073
3502.686352	593082.537875	44.984077
3502.250991	593036.697424	44.989082
3502.938308	593007.097805	44.994087
3502.799445	592972.962628	44.999092
3502.735677	592920.831655	45.004097
3502.647664	592895.629308	45.009101
3502.759341	592856.529685	45.014106
3502.802775	592811.312724	45.019111
3502.661638	592796.316266	45.024116
3502.665471	592755.526148	45.029121
3502.575477	592723.190603	45.034125
3502.466078	592689.853492	45.039130
3502.746738	592657.557156	45.044135
3502.704544	592619.486785	45.049140
3502.770792	592582.202169	45.054145
3502.523656	592548.334781	45.059149
3502.385517	592503.950317	45.064154
3502.865318	592478.201402	45.069159
3502.564971	592450.420895	45.074164
3502.685410	592407.852147	45.079169
3502.506767	592381.357532	45.084173
3502.456947	592353.535513	45.089178
3502.545334	592310.167934	45.094183
3502.720462	592282.811035	45.099188
3502.485449	592256.074250	45.104193
3502.586399	592232.245950	45.109197
3502.990218	592193.146233	45.114202
3502.761995	592145.660648	45.119207
3502.741423	592119.290106	45.124212
3502.890389	592089.073609	45.129217
3502.429622	592047.403125	45.134221
3502.466165	592017.858047	45.139226
3502.581813	591981.568135	45.144231
3502.438359	591954.062030	45.149236
3502.752542	591912.162894	45.154241
3502.893978	591889.432450	45.159245
3502.748775	591853.134893	45.164250
3502.833264	591812.730140	45.169255
3502.628852	591773.628798	45.174260
3503.074848	591734.369910	45.179265
3502.618513	591692.195069	45.184269
3502.516611	591670.056922	45.189274
3503.118883	591627.104548	45.194279
3502.927698	591585.940639	45.199284
3503.033407	591552.615123	45.204289
3502.904701	591512.897584	45.209293
3502.629439	591487.321190	45.214298
3502.866537	591444.528811	45.219303
3502.838896	591418.409073	45.224308
3502.971308	591380.908825	45.229313
3503.050523	591343.919620	45.234317
3502.773128	591307.190024	45.239322
3502.877318	591262.760986	45.244327
3502.474006	591226.554288	45.249332
3502.756819	591186.416165	45.254337
3502.624371	591156.947035	45.259341
3502.516426	591131.543264	45.264346
3502.661500	591088.262365	45.269351
3502.599282	591059.936954	45.274356
3502.523814	591024.881393	45.279361
3502.729446	590989.226755	45.284365
3502.727474	590948.079699	45.289370
3502.759864	590911.750002	45.294375
3502.215306	590887.522967	45.299380
3502.826958	590847.681205	45.304385
3502.778000	590815.283460	45.309389
3502.478500	590781.319175	45.314394
3502.833506	590747.849842	45.319399
3502.484538	590708.417123	45.324404
3502.603032	590680.563452	45.329409
3502.504976	590648.022616	45.334413
3502.519861	590620.236120	45.339418
3502.834932	590589.737233	45.344423
3502.474067	590554.928289	45.349428
3502.813737	590523.118865	45.354433
3502.647791	590489.483439	45.359437
3502.691377	590463.651328	45.364442
3502.776736	590429.773350	45.369447
3502.510683	590395.802453	45.374452
3502.930223	590358.050698	45.379457
3502.857878	590324.801333	45.384461
3502.644414	590296.147323	45.389466
3502.610823	590255.505526	45.394471
3502.301628	590216.617310	45.399476
3502.580085	590189.941995	45.404481
3502.440404	590162.933570	45.409485
3502.404530	590133.596727	45.414490
3502.789128	590094.191827	45.419495
3502.613010	590063.873029	45.424500
3502.798341	590024.651471	45.429505
3502.825225	589992.088257	45.434509
3502.801799	589962.196246	45.439514
3502.767881	589927.934537	45.444519
3502.534838	589883.505687	45.449524
3502.572115	589854.809299	45.454529
3502.512835	589822.360313	45.459533
3502.181418	589786.740338	45.464538
3502.382095	589760.880821	45.469543
3502.347600	589733.703352	45.474548
3502.415599	589699.976904	45.479553
3502.272179	589665.883227	45.484557
3502.153048	589637.815050	45.489562
3502.481726	589626.254435	45.494567
3502.469689	589598.068024	45.499572
3502.117726	589566.118794	45.504577
3502.360326	589533.619278	45.509581
3502.303498	589518.052071	45.514586
3502.597868	589482.629551	45.519591
3502.143749	589465.218346	45.524596
3502.919059	589416.702301	45.529601
3502.658463	589399.962577	45.534605
3502.515410	589366.621701	45.539610
3502.426910	589320.257523	45.544615
3502.239315	589301.445464	45.549620
3502.619896	589260.933026	45.554625
3502.371418	589242.834383	45.559629
3502.522544	589210.650555	45.564634
3502.725806	589177.603823	45.569639
3502.489047	589159.402625	45.574644
3502.627869	589120.035021	45.579649
3502.723224	589087.357564	45.584653
3502.469822	589050.566814	45.589658
3503.035449	589014.746468	45.594663
3502.555796	588988.947146	45.599668
3502.630166	588948.835860	45.604673
3502.644771	588920.492715	45.609677
3502.289648	588875.024994	45.614682
3502.572055	588846.285793	45.619687
3502.451401	588823.793703	45.624692
3502.321474	588780.700517	45.629697
3502.536837	588747.952109	45.634701
3502.400553	588734.758745	45.639706
3502.511575	588697.957109	45.644711
3502.440820	588680.280583	45.649716
3502.609105	588640.404043	45.654721
3502.306227	588608.946676	45.659725
3502.342261	588580.498694	45.664730
3502.771779	588544.297367	45.669735
3502.545260	588523.982963	45.674740
3502.460154	588487.514509	45.679745
3502.405048	588464.106416	45.684749
3502.265147	588423.375413	45.689754
3502.302462	588398.544914	45.694759
3502.455635	588374.700310	45.699764
3502.436727	588343.195451	45.704769
3502.201262	588321.726380	45.709773
3502.670570	588292.904806	45.714778
3502.734173	588260.933863	45.719783
3502.324248	588223.312075	45.724788
3502.240070	588184.128908	45.729793
3502.757830	588154.796491	45.734797
3502.443286	588127.611276	45.739802
3502.620574	588096.977994	45.744807
3502.405542	588074.952331	45.749812
3502.859014	588043.318589	45.754817
3502.548803	587986.030558	45.759821
3502.205893	587893.620177	45.764826
3502.445453	587754.577491	45.769831
3502.172113	587570.488540	45.774836
3501.856476	587304.033756	45.779841
3502.174838	586997.865607	45.784845
3501.936365	586633.129091	45.789850
3501.685644	586210.131251	45.794855
3501.290036	585718.332618	45.799860
3501.113042	585176.765748	45.804865
3500.835115	584583.164362	45.809869
3500.528011	583926.550113	45.814874
3500.124980	583206.069231	45.819879
3499.768014	582433.451824	45.824884
3499.148742	581593.101876	45.829889
3499.037288	580691.063601	45.834893
3498.025330	579747.469608	45.839898
3497.707566	578718.042566	45.844903
3497.022378	577646.140734	45.849908
3496.447377	576509.944853	45.854913
3495.938656	575313.217889	45.859917
3494.623658	574055.130830	45.864922
3494.230692	572727.179453	45.869927
3492.970109	571347.803300	45.874932
3492.104147	569913.808949	45.879937
3491.477225	568409.550890	45.884941
3490.146274	566859.373750	45.889946
3489.290362	565241.570191	45.894951
3487.788551	563562.040835	45.899956
3486.633077	561825.534621	45.904961
3485.450263	560028.515944	45.909965
3484.113524	558195.110787	45.914970
3483.373333	556285.130387	45.919975
3481.800261	554341.860087	45.924980
3480.120314	552338.660357	45.929985
3478.958415	550290.221869	45.934989
3477.310682	548171.991304	45.939994
3475.825464	546009.242440	45.944999
3473.875300	543811.439648	45.950004
3472.140500	541543.304866	45.955009
3470.425157	539251.649467	45.960013
3468.446799	536913.153472	45.965018
3466.512631	534523.154936	45.970023
3464.648929	532102.621736	45.975028
3462.841805	529628.477522	45.980033
3461.078642	527108.728232	45.985037
3458.754406	524553.957000	45.990042
3456.987174	521954.623296	45.995047
3454.816750	519317.988964	46.000052
3452.821972	516632.627938	46.005057
3450.806156	513921.087558	46.010061
3447.838513	511163.197282	46.015066
3445.731038	508369.254081	46.020071
3443.067850	505548.982296	46.025076
3440.899850	502685.919578	46.030081
3438.196128	499802.875582	46.035085
3435.643788	496880.765212	46.040090
3433.010827	493935.902480	46.045095
3430.226132	490960.400632	46.050100
3427.762884	487957.664454	46.055105
3424.621901	484920.259296	46.060109
3422.095295	481866.186131	46.065114
3419.624147	478774.624731	46.070119
3416.459014	475674.400610	46.075124
3413.407819	472544.161710	46.080129
3410.652578	469390.000471	46.085133
3407.619790	466214.287561	46.090138
3404.979617	463002.417132	46.095143
3401.171761	459786.770006	46.100148
3398.470488	456550.604761	46.105153
3395.378451	453300.200261	46.110157
3392.317413	450032.750800	46.115162
3389.177720	446723.678725	46.120167
3385.699404	443405.377665	46.125172
3382.351803	440073.767598	46.130177
3379.350258	436725.518447	46.135181
3375.491497	433376.003442	46.140186
3372.499939	429999.672544	46.145191
3368.806355	426634.192431	46.150196
3365.381355	423233.270408	46.155201
3362.191192	419824.502610	46.160205
3358.288233	416428.643475	46.165210
3354.901093	412981.539091	46.170215
3351.219903	409561.992450	46.175220
3347.571222	406123.488290	46.180225
3343.914926	402682.421295	46.185229
3340.051745	399234.184210	46.190234
3336.908064	395781.477806	46.195239
3332.986906	392323.363208	46.200244
3329.199278	388855.479743	46.205249
3325.583642	385384.487653	46.210253
3321.632865	381914.979381	46.215258
3318.379656	378438.177057	46.220263
3313.835325	374964.154801	46.225268
3310.092840	371475.287533	46.230273
3306.615622	368008.061285	46.235277
3302.126602	364533.760263	46.240282
3298.791443	361047.966187	46.245287
3294.499540	357575.530795	46.250292
3290.560746	354106.177818	46.255297
3286.937359	350630.740125	46.260301
3282.408315	347163.854474	46.265306
3279.148398	343702.095654	46.270311
3274.660697	340227.691866	46.275316
3271.001567	336768.051184	46.280321
3266.871368	333319.659846	46.285325
3262.340059	329868.265301	46.290330
3258.798615	326416.473143	46.295335
3254.436109	322993.127299	46.300340
3250.416147	319557.065463	46.305345
3246.214401	316130.224855	46.310349
3242.011976	312712.230449	46.315354
3237.786754	309294.516861	46.320359
3233.832198	305895.937751	46.325364
3229.905295	302511.198115	46.330369
3225.803579	299122.212709	46.335373
3221.318298	295758.945117	46.340378
3217.436122	292393.106030	46.345383
3213.372862	289037.108147	46.350388
3208.994321	285686.246966	46.355393
3204.923923	282356.676879	46.360397
3200.911734	279036.709215	46.365402
3196.756967	275722.413653	46.370407
3192.094245	272416.355437	46.375412
3188.003538	269125.624004	46.380417
3184.094598	265847.032963	46.385421
3179.604869	262582.423306	46.390426
3175.809539	259331.160520	46.395431
3171.317643	256085.791030	46.400436
3167.005398	252850.228151	46.405441
3162.847832	249641.089364	46.410445
3158.761453	246440.441250	46.415450
3154.606411	243243.068359	46.420455
3150.167240	240074.252162	46.425460
3146.142972	236901.974091	46.430465
3141.805044	233753.789577	46.435469
3137.441732	230618.630706	46.440474
3133.552686	227494.944859	46.445479
3128.884906	224389.871744	46.450484
3124.795343	221291.276400	46.455489
3120.654537	218221.396985	46.460493
3116.182430	215160.067047	46.465498
3112.317221	212106.297875	46.470503
3107.553072	209088.236263	46.475508
3103.373895	206055.039111	46.480513
3099.409062	203063.778324	46.485517
3095.243412	200050.408629	46.490522
3090.963260	197011.412270	46.495527
3086.681194	194059.841313	46.500532
3082.224280	191111.706896	46.505537
3078.015726	188180.486034	46.510541
3073.864515	185284.513694	46.515546
3069.714582	182381.183076	46.520551
3065.391967	179525.423504	46.525556
3061.190545	176661.098084	46.530561
3057.278598	173805.375116	46.535565
3052.834886	170980.047597	46.540570
3048.836616	168153.214357	46.545575
3044.676394	165356.732278	46.550580
3040.539832	162566.529850	46.555585
3036.601558	159794.690953	46.560589
3032.157701	157037.632303	46.565594
3027.892116	154289.863897	46.570599
3023.683556	151566.541468	46.575604
3019.424328	148855.297712	46.580609
3015.457804	146157.718514	46.585613
3011.013722	143484.345222	46.590618
3007.072507	140812.768327	46.595623
3002.723757	138168.095306	46.600628
2998.502134	135537.360440	46.605633
2994.786544	132917.858862	46.610637
2990.409885	130322.315554	46.615642
2986.320481	127722.717618	46.620647
2982.049166	125146.365193	46.625652
2978.190739	122592.713934	46.630657
2973.901966	120051.318571	46.635661
2969.854364	117524.521047	46.640666
2965.923277	115004.873277	46.645671
2961.503536	112506.295911	46.650676
2957.645335	110011.964478	46.655681
2953.368211	107535.618356	46.660685
2949.225766	105092.110180	46.665690
2945.350788	102647.849764	46.670695
2941.006623	100216.743122	46.675700
2936.724555	97806.058719	46.680705
2932.895302	95410.900227	46.685709
2928.563392	93030.846784	46.690714
2924.734542	90656.702379	46.695719
2920.808647	88309.415804	46.700724
2916.486858	85965.394297	46.705729
2912.631023	83641.783454	46.710733
2908.484537	81337.392218	46.715738
2904.591761	79031.979551	46.720743
2900.474945	76748.031716	46.725748
2896.330284	74482.279065	46.730753
2892.393366	72220.370574	46.735757
2887.805878	69993.899394	46.740762
2883.460099	67765.051651	46.745767
2879.396365	65566.047096	46.750772
2875.417618	63384.090978	46.755777
2871.052748	61218.592957	46.760781
2866.654984	59072.615894	46.765786
2862.375346	56944.560056	46.770791
2857.751453	54840.022436	46.775796
2852.698480	52760.392835	46.780801
2847.852008	50718.994089	46.785805
2841.811041	48732.370304	46.790810
2834.675106	46819.040346	46.795815
2827.205615	44980.406597	46.800820
2820.112555	43200.466505	46.805825
2813.529931	41477.720451	46.810829
2805.942692	39842.407145	46.815834
2799.674300	38267.389614	46.820839
2792.877531	36779.810969	46.825844
2786.862853	35357.067285	46.830849
2780.742313	33999.021598	46.835853
2774.791631	32704.564118	46.840858
2769.409284	31481.435907	46.845863
2763.951404	30315.507053	46.850868
2758.838050	29195.149133	46.855873
2753.955298	28120.467494	46.860877
2749.046854	27105.598625	46.865882
2744.187519	26119.771234	46.870887
2739.665239	25186.640914	46.875892
2735.471437	24294.130856	46.880897
2731.351700	23421.543774	46.885901
2726.726156	22589.555975	46.890906
2722.528383	21771.700900	46.895911
2718.531011	20998.306366	46.900916
2714.886620	20226.019092	46.905921
2710.827025	19479.446488	46.910925
2706.916342	18752.127273	46.915930
2703.181024	18050.436700	46.920935
2699.374883	17366.824637	46.925940
2695.671206	16691.888812	46.930945
2692.321160	16035.341986	46.935949
2688.397886	15397.840663	46.940954
2684.777441	14759.830422	46.945959
2681.409048	14131.930241	46.950964
2677.427712	13522.052486	46.955969
2673.644813	12929.765873	46.960973
2669.533082	12350.091830	46.965978
2665.807682	11779.327867	46.970983
2661.589464	11223.215525	46.975988
2657.520130	10691.369451	46.980993
2653.358545	10174.043796	46.985997
2648.433112	9677.138369	46.991002
2644.540457	9199.875432	46.996007
2640.066784	8738.938626	47.001012
2635.732779	8297.048473	47.006017
2631.656854	7873.120084	47.011021
2627.618569	7470.596131	47.016026
2623.638404	7073.385933	47.021031
2619.714740	6698.876894	47.026036
2615.949440	6328.013850	47.031041
2612.136516	5974.052611	47.036045
2608.479921	5644.666905	47.041050
2604.941313	5302.605331	47.046055
2601.172631	4971.301757	47.051060
2597.493035	4649.025754	47.056065
2593.716220	4342.957156	47.061069
2590.043858	4032.371231	47.066074
2586.863967	3724.166448	47.071079
2583.184093	3435.738010	47.076084
2580.104642	3146.205202	47.081089
2576.741212	2850.398311	47.086093
2573.132195	2563.725744	47.091098
2569.756902	2271.973143	47.096103
2566.272047	1990.289167	47.101108
2562.799187	1709.370114	47.106113
2558.985824	1434.009139	47.111117
2555.667135	1164.715444	47.116122
2552.305096	884.081534	47.121127
2548.414110	626.346284	47.126132
2544.603622	382.495495	47.131137
2540.381275	144.753206	47.136141
2528.890081	120.918819	47.141146
2518.479216	127.206369	47.146151
2511.841736	132.000479	47.151156
2508.294784	131.158760	47.156161
2506.841728	129.639914	47.161165
2504.968564	130.339850	47.166170
2503.222736	130.476081	47.171175
2501.197919	131.337609	47.176180
2497.919995	131.218363	47.181185
2494.824049	136.084321	47.186189
2490.965422	132.408529	47.191194
2487.786573	129.322289	47.196199
2484.400983	133.304212	47.201204
2480.950980	131.267199	47.206209
2478.212165	131.164364	47.211213
2474.749466	129.544657	47.216218
2471.185171	123.724932	47.221223
2467.812240	134.287295	47.226228
2464.342571	127.285273	47.231233
2461.679960	120.807586	47.236237
2457.850408	129.912769	47.241242
2454.106411	125.526999	47.246247
2451.120066	122.478474	47.251252
2447.693764	130.873771	47.256257
2444.196244	125.245912	47.261261
2440.710465	127.561867	47.266266
2437.352926	118.210761	47.271271
2434.437391	124.931579	47.276276
2430.755393	131.956130	47.281281
2427.725760	124.956493	47.286285
2423.277385	136.868608	47.291290
2419.924483	130.851812	47.296295
2416.814036	129.095854	47.301300
2413.345459	128.330860	47.306305
2410.156994	129.273994	47.311309
2406.622825	130.735975	47.316314
2403.374786	126.560443	47.321319
2400.054072	118.700712	47.326324
2396.093349	131.801251	47.331329
2392.741398	116.469030	47.336333
2389.018754	124.974848	47.341338
2385.939074	129.598214	47.346343
2382.909144	129.479154	47.351348
2379.022987	139.954210	47.356353
2376.203480	116.715645	47.361357
2372.187071	131.727563	47.366362
2368.762136	131.106954	47.371367
2364.962121	128.522755	47.376372
2361.283243	123.274981	47.381377
2358.540596	133.845845	47.386381
2354.974329	132.351463	47.391386
2351.455306	131.062414	47.396391
2347.863618	121.333836	47.401396
2344.332928	130.379301	47.406401
2340.991541	116.235939	47.411405
2337.808450	127.327480	47.416410
2334.413820	124.782554	47.421415
2330.527609	133.833043	47.426420
2327.042319	129.062673	47.431425
2323.851338	122.380823	47.436429
2320.244962	126.455541	47.441434
2316.458561	125.869383	47.446439
2313.223736	130.350467	47.451444
2309.692609	116.545714	47.456449
2306.213442	121.723888	47.461453
2302.558189	122.126081	47.466458
2299.318692	119.937030	47.471463
2295.862509	109.629237	47.476468
2292.193166	122.762643	47.481473
2288.900841	114.955146	47.486477
2285.348012	125.313261	47.491482
2282.085248	117.318742	47.496487
2278.837307	117.346645	47.501492
2274.976859	120.367505	47.506497
2271.333633	121.209384	47.511501
2267.866246	125.649164	47.516506
2264.266123	125.422435	47.521511
2260.895492	117.845948	47.526516
2257.180219	126.942462	47.531521
2254.166984	117.276534	47.536525
2250.517870	123.266246	47.541530
2247.382024	125.929503	47.546535
2243.645842	123.423864	47.551540
2240.185516	124.577561	47.556545
2236.550431	113.284427	47.561549
2232.754525	125.494690	47.566554
2229.634681	128.426067	47.571559
2226.277895	123.738361	47.576564
2222.480479	125.338263	47.581569
2219.415600	116.313364	47.586573
2215.967328	123.374061	47.591578
2212.518318	121.922589	47.596583
2208.419518	119.192285	47.601588
2205.026688	123.985863	47.606593
2201.768169	122.998075	47.611597
2198.170322	128.273472	47.616602
2194.747467	117.905984	47.621607
2191.432281	123.317649	47.626612
2187.497697	129.549119	47.631617
2184.448657	117.317802	47.636621
2180.598977	129.050338	47.641626
2177.066717	125.083321	47.646631
2173.929170	120.903918	47.651636
2170.150453	120.552625	47.656641
2167.211373	112.995140	47.661645
2163.095961	117.479628	47.666650
2159.909887	116.778878	47.671655
2156.465192	111.472675	47.676660
2152.423579	126.489486	47.681665
2149.590197	113.356659	47.686669
2145.633653	115.620896	47.691674
2141.982872	119.362656	47.696679
2138.769256	111.439266	47.701684
2135.288330	117.711306	47.706689
2132.169441	112.233905	47.711693
2128.187863	124.306562	47.716698
2124.991420	121.580267	47.721703
2121.259056	119.786298	47.726708
2117.708475	119.504530	47.731713
2114.286696	120.005265	47.736717
2110.424589	123.247941	47.741722
2107.342806	119.268952	47.746727
2103.783337	122.484352	47.751732
2100.215349	118.059545	47.756737
2096.930999	110.599580	47.761741
2093.083159	121.109539	47.766746
2090.158344	119.348797	47.771751
2086.955476	119.721440	47.776756
2082.963438	127.466999	47.781761
2079.618029	124.066749	47.786765
2076.159860	112.408864	47.791770
2072.648833	116.805261	47.796775
2069.087994	112.642947	47.801780
2065.192483	121.020444	47.806785
2061.873967	121.964755	47.811789
2058.147841	117.146156	47.816794
2054.516242	118.759850	47.821799
2051.552181	106.285103	47.826804
2047.806876	123.225465	47.831809
2044.676757	111.051459	47.836813
2040.956753	123.461254	47.841818
2037.426346	122.836196	47.846823
2034.234099	112.686119	47.851828
2030.624135	114.276325	47.856833
2027.049876	108.260672	47.861837
2023.583057	108.422971	47.866842
2019.915914	116.817447	47.871847
2016.164253	112.285101	47.876852
2012.544005	113.307495	47.881857
2009.504526	106.427794	47.886861
2006.014162	110.702024	47.891866
2002.581512	113.185138	47.896871
1998.915035	104.840929	47.901876
1995.559562	112.885371	47.906881
1991.889343	113.656137	47.911885
1988.351705	113.811607	47.916890
1984.886613	111.227463	47.921895
1981.497417	103.408973	47.926900
1978.095039	110.722330	47.931905
1974.757745	109.347700	47.936909
1971.249853	110.405246	47.941914
1967.528591	111.058754	47.946919
1963.943224	108.074946	47.951924
1960.547878	109.260535	47.956929
1956.914209	110.071468	47.961933
1953.528461	109.046057	47.966938
1949.994934	108.438947	47.971943
1946.497120	101.078888	47.976948
1942.980141	112.416802	47.981953
1939.562333	109.858234	47.986957
1935.885319	111.743754	47.991962
1932.582625	111.839148	47.996967
1929.047971	106.175994	48.001972
1925.394992	114.192064	48.006977
1922.076283	110.516575	48.011981
1918.296017	116.289395	48.016986
1915.244539	107.254814	48.021991
1911.795666	104.960111	48.026996
1907.865965	112.356467	48.032001
1904.582404	105.207135	48.037005
1900.960257	104.443802	48.042010
1897.505330	111.439688	48.047015
1893.990389	112.183894	48.052020
1890.427348	109.178694	48.057025
1886.774648	115.973408	48.062029
1883.601196	101.301858	48.067034
1880.155959	113.716093	48.072039
1876.503153	112.724982	48.077044
1873.207436	104.729317	48.082049
1869.474664	101.916162	48.087053
1865.772001	109.404698	48.092058
1862.242999	105.223477	48.097063
1859.028981	107.559671	48.102068
1855.589818	116.027111	48.107073
1851.816772	105.415632	48.112077
1848.650212	110.402950	48.117082
1845.304542	114.424081	48.122087
1841.605203	111.860781	48.127092
1837.933960	112.653146	48.132097
1834.346643	110.651329	48.137101
1830.519470	114.573415	48.142106
1827.255279	108.523478	48.147111
1823.977644	111.933076	48.152116
1820.812162	111.474249	48.157121
1817.209963	109.311901	48.162125
1813.670873	112.834752	48.167130
1809.934989	113.874229	48.172135
1806.333521	109.388488	48.177140
1802.707200	110.726602	48.182145
1799.594852	104.937154	48.187149
1796.265202	105.667399	48.192154
1792.567572	108.985369	48.197159
1788.954159	100.713486	48.202164
1785.162020	109.721575	48.207169
1781.899175	100.696558	48.212173
1778.631841	102.805988	48.217178
1774.993447	96.979731	48.222183
1771.370991	98.560747	48.227188
1768.108025	110.176692	48.232193
1764.430670	102.458866	48.237197
1760.822281	98.073768	48.242202
1757.279928	110.711719	48.247207
1754.151130	107.155156	48.252212
1750.361952	112.469374	48.257217
1746.976546	106.542733	48.262221
1743.459116	110.147897	48.267226
1739.924055	111.065252	48.272231
1736.465300	110.881477	48.277236
1733.194878	104.451777	48.282241
1729.825786	100.630634	48.287245
1725.851749	102.290489	48.292250
1722.329299	108.451254	48.297255
1718.885180	106.468890	48.302260
1714.780055	113.180202	48.307265
1711.910978	103.981646	48.312269
1708.147948	101.167306	48.317274
1705.200247	115.166176	48.322279
1701.730657	105.509355	48.327284
1697.925609	108.124854	48.332289
1694.339391	100.695934	48.337293
1690.862767	107.056356	48.342298
1687.227758	105.015962	48.347303
1684.059072	100.619849	48.352308
1680.206879	109.970846	48.357313
1677.162640	105.872879	48.362317
1673.514990	113.029616	48.367322
1669.794863	103.619844	48.372327
1666.526872	104.241125	48.377332
1663.116125	104.351994	48.382337
1659.626789	100.644508	48.387341
1655.509125	107.598888	48.392346
1652.335538	109.332573	48.397351
1649.134288	106.629707	48.402356
1645.135156	113.913805	48.407361
1641.898949	99.110149	48.412365
1638.179850	107.304483	48.417370
1634.586956	103.185702	48.422375
1631.621931	103.074747	48.427380
1627.666257	107.510778	48.432385
1624.441282	98.629213	48.437389
1621.275162	104.458644	48.442394
1617.734282	100.523097	48.447399
1614.334616	97.123677	48.452404
1610.282994	104.004031	48.457409
1606.777026	107.018933	48.462413
1603.308378	100.778775	48.467418
1599.667876	100.301694	48.472423
1596.419142	100.399260	48.477428
1593.012692	100.525455	48.482433
1589.365033	95.935636	48.487437
1585.505479	104.849033	48.492442
1582.207359	102.511711	48.497447
1578.896714	100.334332	48.502452
1575.030874	108.271159	48.507457
1572.051681	98.634456	48.512461
1568.467421	98.922465	48.517466
1565.063720	103.972034	48.522471
1561.425464	97.078723	48.527476
1558.074008	102.856527	48.532481
1554.399591	96.820519	48.537485
1550.587476	97.119751	48.542490
1547.103844	95.001964	48.547495
1543.873299	92.723560	48.552500
1540.186255	102.061177	48.557505
1536.841006	95.034614	48.562509
1533.198226	100.908726	48.567514
1529.552977	101.126329	48.572519
1526.868707	85.348287	48.577524
1522.494460	94.812301	48.582529
1519.426353	89.605795	48.587533
1515.995594	100.451567	48.592538
1512.548018	95.612070	48.597543
1509.065719	89.351950	48.602548
1505.048600	100.019538	48.607553
1501.615501	80.569257	48.612557
1498.141127	93.704860	48.617562
1494.819049	89.546772	48.622567
1491.331769	85.678448	48.627572
1487.826746	93.130637	48.632577
1484.224535	92.866958	48.637581
1480.539774	92.323283	48.642586
1477.280797	89.478726	48.647591
1473.884719	86.564672	48.652596
1470.615156	95.740393	48.657601
1466.892155	90.788975	48.662605
1462.957330	93.955564	48.667610
1459.441697	94.248102	48.672615
1456.274707	93.333723	48.677620
1452.981811	92.902124	48.682625
1449.453716	83.183172	48.687629
1445.991564	99.424086	48.692634
1442.134793	90.439288	48.697639
1438.803182	87.075922	48.702644
1435.264372	92.150668	48.707649
1431.471109	88.917676	48.712653
1428.080925	91.080404	48.717658
1424.527376	97.315974	48.722663
1421.318955	94.260434	48.727668
1417.524166	96.279086	48.732673
1414.437442	101.521463	48.737677
1410.935650	99.994655	48.742682
1407.471184	92.219857	48.747687
1403.855849	84.282530	48.752692
1400.225550	96.744994	48.757697
1396.901850	97.216615	48.762701
1393.093741	90.051768	48.767706
1389.461749	91.951970	48.772711
1386.040183	90.786866	48.777716
1382.326880	91.318155	48.782721
1378.989935	87.243521	48.787725
1375.655125	85.691709	48.792730
1372.017195	98.747864	48.797735
1369.313467	87.072669	48.802740
1365.223691	96.362316	48.807745
1361.920267	101.903991	48.812749
1358.139806	101.142188	48.817754
1354.560808	95.627342	48.822759
1351.515761	90.082459	48.827764
1347.606012	96.722499	48.832769
1344.190155	82.632982	48.837773
1340.359180	88.231278	48.842778
1337.080376	88.142776	48.847783
1333.615396	86.217636	48.852788
1329.973801	90.467403	48.857793
1326.810992	88.927255	48.862797
1323.205275	96.402516	48.867802
1319.779152	89.087569	48.872807
1316.146271	89.463535	48.877812
1312.453290	88.475568	48.882817
1309.224240	97.727376	48.887821
1305.576713	94.246027	48.892826
1301.709280	96.158772	48.897831
1298.827609	84.948372	48.902836
1295.220650	87.604458	48.907841
1291.606211	85.453436	48.912845
1288.312078	83.856879	48.917850
1284.515961	98.811586	48.922855
1281.038907	93.657853	48.927860
1277.497360	93.481399	48.932865
1274.402014	101.279439	48.937869
1270.798830	88.428265	48.942874
1267.034078	94.141575	48.947879
1264.086347	92.838244	48.952884
1259.780259	92.315562	48.957889
1256.436206	87.338191	48.962893
1253.137966	93.575879	48.967898
1249.714015	96.258384	48.972903
1246.265722	92.369601	48.977908
1242.405948	95.915287	48.982913
1238.603894	79.155194	48.987917
1235.224721	81.593499	48.992922
1231.868682	96.955218	48.997927
1228.768916	93.403706	49.002932
1225.201203	97.582336	49.007937
1221.891703	89.860617	49.012941
1218.148701	87.892727	49.017946
1214.342007	93.483951	49.022951
1211.143544	89.092124	49.027956
1207.370099	97.197472	49.032961
1204.170349	92.927817	49.037965
1200.770116	91.940484	49.042970
1196.808473	88.830845	49.047975
1193.682117	84.529728	49.052980
1189.919763	93.948710	49.057985
1186.471330	88.915240	49.062989
1183.005796	91.357205	49.067994
1179.637554	89.560051	49.072999
1176.304448	83.615556	49.078004
1172.563382	90.334997	49.083009
1168.839859	88.961862	49.088013
1165.387702	87.923939	49.093018
1162.028288	84.126107	49.098023
1158.753409	88.024695	49.103028
1155.182706	90.602470	49.108033
1151.671750	80.149217	49.113037
1147.594796	90.717441	49.118042
1144.069405	87.817325	49.123047
1140.979200	84.343628	49.128052
1137.345917	92.323829	49.133057
1133.903330	89.056993	49.138061
1130.778499	90.297907	49.143066
1127.103736	87.081897	49.148071
1124.006874	85.354372	49.153076
1119.723856	83.238454	49.158081
1116.322287	83.862078	49.163085
1112.822561	85.975852	49.168090
1109.732342	90.221646	49.173095
1105.776633	82.473866	49.178100
1102.540265	91.063754	49.183105
1099.142871	83.717800	49.188109
1095.119333	81.595904	49.193114
1091.705095	87.578971	49.198119
1088.451879	84.224619	49.203124
1084.844055	93.769090	49.208129
1081.846572	88.180428	49.213133
1078.170051	83.220480	49.218138
1074.321345	84.044366	49.223143
1070.994031	78.996887	49.228148
1067.521257	83.523823	49.233153
1063.832090	80.610203	49.238157
1060.215968	71.906658	49.243162
1056.886449	83.721079	49.248167
1053.607487	82.079957	49.253172
1049.462126	80.954477	49.258177
1046.462557	76.038519	49.263181
1043.239963	75.354645	49.268186
1039.123432	81.395463	49.273191
1035.957344	80.484586	49.278196
1032.281856	89.147919	49.283201
1029.119240	77.038937	49.288205
1025.536981	83.704402	49.293210
1021.607050	89.581967	49.298215
1018.452334	76.496051	49.303220
1014.642822	82.344432	49.308225
1011.595368	83.075933	49.313229
1007.814753	83.843622	49.318234
1004.465217	80.439550	49.323239
1001.026073	73.308975	49.328244
997.340513	84.871109	49.333249
993.811754	76.155740	49.338253
990.341246	79.908398	49.343258
986.672192	89.733611	49.348263
983.438483	70.247712	49.353268
979.944112	92.268710	49.358273
976.432811	73.074603	49.363277
972.982954	81.221328	49.368282
969.257068	86.740572	49.373287
965.660426	81.511172	49.378292
962.109160	85.951313	49.383297
958.893170	77.877693	49.388301
955.686770	85.461622	49.393306
951.634361	89.374085	49.398311
948.269005	84.570193	49.403316
944.641984	90.115929	49.408321
941.516264	84.726379	49.413325
937.864704	77.362803	49.418330
934.226259	94.580980	49.423335
930.608622	87.143912	49.428340
927.138014	88.635344	49.433345
923.537841	86.578961	49.438349
920.170924	93.550878	49.443354
916.510102	90.501267	49.448359
913.412323	85.202036	49.453364
910.080515	86.496671	49.458369
906.232539	73.006313	49.463373
903.098593	81.580566	49.468378
899.278036	83.818209	49.473383
895.760433	75.371434	49.478388
892.003460	76.522683	49.483393
888.558190	75.594347	49.488397
885.541062	79.804119	49.493402
881.626888	79.324334	49.498407
878.627048	80.203354	49.503412
874.672237	81.352213	49.508417
871.346938	79.189041	49.513421
867.512145	84.558639	49.518426
863.833501	89.876958	49.523431
860.614232	81.810865	49.528436
857.485976	76.458703	49.533441
854.078259	91.068447	49.538445
849.913462	79.168195	49.543450
846.194547	91.841046	49.548455
843.231044	82.883717	49.553460
839.603426	89.182867	49.558465
836.487629	79.989263	49.563469
833.150181	80.181969	49.568474
828.959787	84.404487	49.573479
825.845073	78.356665	49.578484
822.129346	82.615724	49.583489
818.715373	78.934936	49.588493
814.982156	74.132801	49.593498
811.601272	84.376581	49.598503
808.379623	74.030696	49.603508
804.635375	83.375525	49.608513
801.060762	81.797507	49.613517
797.719173	76.083043	49.618522
794.070735	82.763767	49.623527
790.833860	75.304301	49.628532
787.175425	81.908341	49.633537
783.789090	76.846583	49.638541
780.400709	83.103439	49.643546
776.532689	83.165303	49.648551
773.042062	79.731273	49.653556
769.374118	87.548551	49.658561
766.179218	76.504832	49.663565
762.867862	76.626378	49.668570
758.880112	78.675711	49.673575
755.529073	78.674768	49.678580
751.869180	78.136261	49.683585
748.631428	81.211619	49.688589
745.563105	66.654711	49.693594
741.613833	83.823775	49.698599
738.328172	73.599047	49.703604
734.470548	75.616416	49.708609
731.023320	74.636036	49.713613
727.465522	73.697236	49.718618
723.713491	79.570280	49.723623
720.822509	73.704179	49.728628
717.002696	76.877030	49.733633
713.632641	79.157126	49.738637
710.347654	78.745288	49.743642
706.452047	78.957214	49.748647
703.190134	81.318294	49.753652
699.258232	87.416480	49.758657
695.926238	86.142370	49.763661
692.722956	77.110766	49.768666
689.250750	80.327764	49.773671
686.087313	81.906305	49.778676
682.363550	80.426667	49.783681
678.254413	78.210586	49.788685
674.870968	74.251752	49.793690
671.166977	82.385081	49.798695
668.287473	78.588760	49.803700
664.655625	79.184913	49.808705
661.123850	76.753744	49.813709
657.598176	76.915364	49.818714
653.829596	77.320629	49.823719
650.398186	68.892770	49.828724
647.136293	80.661919	49.833729
643.603766	73.231360	49.838733
639.882235	63.859698	49.843738
636.177792	75.152683	49.848743
633.174666	72.022527	49.853748
629.682575	74.924555	49.858753
625.970610	78.015900	49.863757
622.983677	62.983867	49.868762
618.957975	68.345385	49.873767
615.136397	74.469981	49.878772
611.789597	81.563493	49.883777
607.901820	72.879651	49.888781
605.003454	72.075557	49.893786
601.353340	74.769316	49.898791
598.496597	76.122531	49.903796
594.732676	74.432938	49.908801
591.194113	69.385280	49.913805
587.614557	73.388348	49.918810
583.828418	79.370156	49.923815
580.624402	71.001427	49.928820
577.145001	70.144698	49.933825
573.391122	74.329161	49.938829
569.783667	64.774901	49.943834
566.210985	68.658049	49.948839
562.968772	68.056315	49.953844
559.394343	70.781393	49.958849
556.081317	69.256202	49.963853
552.618217	58.008609	49.968858
548.918259	70.575507	49.973863
545.392077	67.114993	49.978868
541.893173	65.789885	49.983873
537.960309	68.183169	49.988877
534.824329	69.278534	49.993882
531.105811	74.402422	49.998887
527.921363	72.364412	50.003892
524.514544	67.246468	50.008897
520.783002	79.268446	50.013901
517.593127	63.898300	50.018906
513.986728	70.537347	50.023911
510.447211	67.148729	50.028916
506.810780	66.689626	50.033921
502.990105	61.481922	50.038925
499.975073	63.135493	50.043930
496.123754	77.772478	50.048935
492.904129	58.392078	50.053940
489.928420	71.525901	50.058945
485.740347	66.152466	50.063949
482.223671	65.942931	50.068954
478.737578	67.821681	50.073959
475.893626	69.345725	50.078964
471.902085	70.898257	50.083969
468.157156	72.949105	50.088973
465.035116	71.025137	50.093978
461.108567	72.232635	50.098983
457.666775	67.014368	50.103988
454.048574	75.098931	50.108993
450.744546	71.298820	50.113997
447.572749	65.623448	50.119002
443.809896	66.730068	50.124007
440.444813	59.912935	50.129012
436.975087	75.006397	50.134017
433.327762	60.459151	50.139021
429.818627	65.502882	50.144026
426.098316	71.415311	50.149031
422.683714	66.644080	50.154036
419.034366	75.193617	50.159041
415.692134	76.520340	50.164045
412.448277	65.452274	50.169050
408.328640	61.252402	50.174055
405.210344	73.082982	50.179060
401.927281	69.883883	50.184065
398.356486	70.141192	50.189069
395.125845	71.146551	50.194074
391.332392	72.508700	50.199079
387.611090	75.065229	50.204084
384.009246	73.874307	50.209089
380.520507	62.508764	50.214093
377.639103	58.697773	50.219098
373.529922	63.643521	50.224103
370.503528	60.698564	50.229108
367.023131	60.045033	50.234113
363.510843	63.697919	50.239117
359.643548	57.665704	50.244122
356.185759	61.906319	50.249127
352.860676	58.802820	50.254132
349.066034	64.641178	50.259137
345.840982	51.823250	50.264141
342.335510	58.306793	50.269146
338.444328	61.268982	50.274151
335.063917	57.336767	50.279156
331.804994	64.472359	50.284161
328.084600	69.338802	50.289165
325.006197	56.893655	50.294170
321.109817	64.308421	50.299175
317.786431	59.968359	50.304180
314.025832	57.401507	50.309185
310.567378	68.349322	50.314189
307.384376	61.699697	50.319194
303.311996	64.870695	50.324199
300.233934	60.111353	50.329204
296.969693	70.197630	50.334209
293.379649	65.830486	50.339213
289.534295	73.334320	50.344218
286.151305	59.515053	50.349223
282.726732	61.014361	50.354228
279.083721	62.624621	50.359233
275.424080	67.421454	50.364237
272.483716	58.730511	50.369242
268.381208	66.297843	50.374247
265.190857	60.410594	50.379252
261.771500	67.139048	50.384257
258.203084	68.462286	50.389261
254.739481	57.304050	50.394266
251.053437	73.060966	50.399271
247.900513	60.807990	50.404276
244.419691	67.716143	50.409281
240.213020	66.100948	50.414285
237.037027	57.679724	50.419290
233.499557	65.304316	50.424295
229.818706	58.324342	50.429300
226.584177	62.901062	50.434305
222.868309	63.354807	50.439309
219.838698	63.646011	50.444314
215.987897	68.560773	50.449319
212.898453	62.234760	50.454324
209.490078	59.009990	50.459329
205.945071	61.915777	50.464333
202.086607	60.797292	50.469338
198.213702	71.430769	50.474343
194.650976	59.380463	50.479348
191.545220	64.243537	50.484353
187.925438	63.205137	50.489357
184.770134	60.468733	50.494362
181.151348	59.096874	50.499367
177.381573	58.089630	50.504372
174.139659	56.427265	50.509377
170.382263	65.099461	50.514381
167.301059	60.341136	50.519386
163.394172	68.678346	50.524391
160.165559	69.212306	50.529396
156.646119	72.080945	50.534401
152.947135	68.774092	50.539405
149.603748	76.705839	50.544410
145.640526	75.028528	50.549415
142.498306	72.861669	50.554420
139.186693	67.404264	50.559425
135.556248	67.199049	50.564429
132.373720	63.740602	50.569434
128.092996	69.828343	50.574439
125.063397	62.999744	50.579444
121.312291	56.546354	50.584449
117.971514	62.409411	50.589453
114.477007	64.526449	50.594458
111.209324	65.730554	50.599463
107.649699	67.401350	50.604468
103.836602	66.382202	50.609473
100.505366	70.956278	50.614477
97.147454	74.078833	50.619482
93.432150	74.204033	50.624487
89.858153	68.414386	50.629492
86.255588	70.142827	50.634497
82.911946	73.847932	50.639501
79.642141	66.517847	50.644506
76.002093	68.825960	50.649511
72.654278	65.220680	50.654516
69.026431	75.851181	50.659521
65.360344	70.226580	50.664525
61.980565	69.723782	50.669530
58.146982	68.125731	50.674535
54.988612	63.216678	50.679540
51.326672	66.015065	50.684545
48.236070	70.872966	50.689549
44.724611	63.663834	50.694554
40.993943	67.484559	50.699559
37.522841	58.118587	50.704564
33.743383	60.522240	50.709569
30.195002	66.633848	50.714573
26.797336	61.134549	50.719578
23.413342	68.644099	50.724583
20.207853	72.053262	50.729588
16.545674	73.772689	50.734593
12.963225	75.202646	50.739597
9.709347	69.772296	50.744602
5.842744	73.221483	50.749607
2.289489	73.340452	50.754612