Tue Jun 21 10:28:06 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.618530	94.992417	0.000000
0.783550	89.889717	0.005005
0.907683	99.063493	0.010010
1.002763	105.385853	0.015014
0.959417	93.318369	0.020019
0.882671	91.062797	0.025024
0.963431	82.765974	0.030029
0.566490	66.851408	0.035034
0.582354	67.615515	0.040038
0.554317	51.709732	0.045043
-0.228809	38.136585	0.050048
-0.206006	28.386942	0.055053
-0.698082	19.362126	0.060058
-1.096736	4.608825	0.065062
-0.974516	-2.677757	0.070067
-1.841424	-1.758199	0.075072
-2.357342	-9.206495	0.080077
-2.111404	-14.217183	0.085082
-2.439986	-5.878213	0.090086
-3.021611	-5.909684	0.095091
-3.705617	-4.550363	0.100096
-3.495630	-1.644771	0.105101
-3.247583	-12.732314	0.110106
-3.908490	-10.216298	0.115110
-4.898247	-13.664313	0.120115
-5.048013	-8.460199	0.125120
-4.954276	-4.747995	0.130125
-5.075927	-2.948797	0.135130
-5.290409	-2.550492	0.140134
-5.241261	-1.026244	0.145139
-5.606546	-3.455036	0.150144
-5.585991	-7.399703	0.155149
-5.970157	-3.133576	0.160154
-6.530802	-1.982346	0.165158
-6.306173	-8.949429	0.170163
-6.824124	-0.339337	0.175168
-7.597225	3.103589	0.180173
-7.895457	-3.171888	0.185178
-8.295090	-0.899034	0.190182
-8.319276	-2.800398	0.195187
-8.275380	-3.557843	0.200192
-8.307956	2.293067	0.205197
-8.137350	-6.647883	0.210202
-9.161597	1.407675	0.215206
-9.503147	-12.015166	0.220211
-9.756674	-0.598965	0.225216
-9.620394	0.876519	0.230221
-10.075376	1.116526	0.235226
-10.375265	10.155631	0.240230
-9.927274	-8.276648	0.245235
-10.993369	-1.744881	0.250240
-11.586518	-4.908106	0.255245
-11.577853	3.722331	0.260250
-11.951771	6.398225	0.265254
-11.589535	0.957226	0.270259
-11.765365	-2.168743	0.275264
-11.882871	4.555227	0.280269
-11.951694	-2.016944	0.285274
-12.711460	1.251699	0.290278
-13.028433	-6.207834	0.295283
-13.509003	2.262278	0.300288
-13.115404	0.804996	0.305293
-13.523288	0.080924	0.310298
-14.582257	2.888019	0.315302
-14.414796	-4.014938	0.320307
-14.923417	-5.825031	0.325312
-14.776573	-9.004037	0.330317
-14.682476	-3.286783	0.335322
-15.048506	-0.076434	0.340326
-15.237234	-7.808211	0.345331
-15.888315	-2.352557	0.350336
-16.168665	-3.547473	0.355341
-16.047155	-5.935316	0.360346
-16.014710	-3.101952	0.365350
-16.663283	-2.401869	0.370355
-17.441832	-1.514502	0.375360
-17.757290	-4.857898	0.380365
-17.489862	-8.711824	0.385370
-17.986865	-0.277473	0.390374
-17.654836	-11.635457	0.395379
-18.277051	-5.274086	0.400384
-18.898037	3.546656	0.405389
-19.046511	-2.145830	0.410394
-19.238426	-4.081776	0.415398
-19.016668	1.754249	0.420403
-19.546343	3.072625	0.425408
-19.452794	-0.940371	0.430413
-20.175732	-2.394898	0.435418
-21.132682	-3.901445	0.440422
-20.932924	-3.285603	0.445427
-21.035626	-8.266187	0.450432
-21.180186	-4.051577	0.455437
-20.677718	-8.772438	0.460442
-21.455642	-8.644712	0.465446
-21.133846	-4.187649	0.470451
-22.062957	2.038264	0.475456
-22.728678	-6.914560	0.480461
-22.563511	-5.555356	0.485466
-22.945476	0.070434	0.490470
-22.997428	-6.625098	0.495475
-22.698869	1.363750	0.500480
-23.469094	1.838496	0.505485
-23.763863	-5.163740	0.510490
-24.281257	2.043613	0.515494
-24.381401	-4.731162	0.520499
-24.338839	0.366118	0.525504
-24.740189	1.139519	0.530509
-25.293792	-2.687375	0.535514
-25.843800	4.996021	0.540518
-25.885008	-6.299173	0.545523
-26.005922	4.161878	0.550528
-25.848300	7.511461	0.555533
-25.782630	-4.010805	0.560538
-26.425851	4.310615	0.565542
-26.988384	2.026378	0.570547
-27.348383	4.136973	0.575552
-27.587536	1.810630	0.580557
-27.426868	-3.455697	0.585562
-27.405174	4.146839	0.590566
-27.497475	-4.911204	0.595571
-28.466829	1.880618	0.600576
-28.690081	2.655705	0.605581
-28.686137	-1.395337	0.610586
-29.073615	3.327972	0.615590
-28.717343	-9.445164	0.620595
-29.688705	-6.637380	0.625600
-30.091971	-4.220462	0.630605
-30.367560	-1.078173	0.635610
-30.550512	-0.739552	0.640614
-30.602064	-4.677606	0.645619
-30.643889	-3.040614	0.650624
-30.685623	-9.699159	0.655629
-31.438645	-0.047879	0.660634
-32.304552	7.426561	0.665638
-32.220496	-3.166741	0.670643
-32.233467	2.895029	0.675648
-32.413759	3.844353	0.680653
-32.430600	2.335257	0.685658
-32.360389	4.722510	0.690662
-32.319687	-1.281714	0.695667
-33.554923	2.148352	0.700672
-34.081984	-1.385357	0.705677
-33.951214	-6.944903	0.710682
-34.354613	-0.792037	0.715686
-34.118044	-3.832772	0.720691
-34.116938	-2.944864	0.725696
-34.712482	-5.555351	0.730701
-35.170370	-5.289799	0.735706
-35.677770	1.382506	0.740710
-35.354906	1.940468	0.745715
-35.255375	-0.594106	0.750720
-36.109206	5.087332	0.755725
-37.038357	-0.497777	0.760730
-37.018092	2.868828	0.765734
-37.119429	-3.684537	0.770739
-37.232291	-5.252126	0.775744
-37.348335	-12.553315	0.780749
-37.169874	-9.927062	0.785754
-37.516544	5.287259	0.790758
-38.027135	-16.143609	0.795763
-38.706569	-9.342377	0.800768
-38.990705	-11.461764	0.805773
-38.708511	-10.708022	0.810778
-38.955049	0.899619	0.815782
-38.713106	-13.491662	0.820787
-39.866436	-3.423233	0.825792
-40.192729	-2.281406	0.830797
-40.447310	-11.112474	0.835802
-40.634012	-2.997094	0.840806
-40.255834	-13.010784	0.845811
-40.619067	-4.518864	0.850816
-40.753492	-9.237461	0.855821
-41.002485	-11.659458	0.860826
-41.661082	-1.865948	0.865830
-42.025384	-13.981227	0.870835
-41.973542	-7.918749	0.875840
-42.083018	-10.292613	0.880845
-42.513119	-13.393242	0.885850
-43.090312	-9.537572	0.890854
-43.096178	-8.641998	0.895859
-43.613427	-2.686162	0.900864
-43.546290	-8.443949	0.905869
-43.444112	-1.720646	0.910874
-44.604697	0.676055	0.915878
-44.791865	-8.567554	0.920883
-44.871644	-12.592296	0.925888
-45.030852	-6.944197	0.930893
-45.140175	-2.989589	0.935898
-45.470293	-6.593403	0.940902
-45.084096	-10.061082	0.945907
-45.190101	-6.815255	0.950912
-45.955077	3.450927	0.955917
-46.578235	-14.832569	0.960922
-46.902516	-6.643101	0.965926
-46.547800	-8.957675	0.970931
-46.872253	-9.625704	0.975936
-47.710922	-15.474231	0.980941
-48.094908	-4.942390	0.985946
-48.441709	3.787166	0.990950
-48.619248	-2.768773	0.995955
-48.463519	-2.819536	1.000960
-48.589950	-1.568528	1.005965
-48.525494	-1.667520	1.010970
-48.423749	-0.849954	1.015974
-48.977525	-6.376254	1.020979
-49.772880	-11.466300	1.025984
-49.857286	-8.957738	1.030989
-49.587669	-11.725703	1.035994
-50.565184	-0.534548	1.040998
-51.010068	1.204121	1.046003
-51.430178	-4.526455	1.051008
-51.944994	-12.295195	1.056013
-51.162291	-5.151001	1.061018
-51.281994	4.460917	1.066022
-51.305941	-1.792291	1.071027
-51.634674	-4.915234	1.076032
-52.035182	-3.240746	1.081037
-52.820761	-7.449934	1.086042
-53.026469	-2.982280	1.091046
-53.103407	-8.107827	1.096051
-53.167132	-6.865034	1.101056
-53.924022	2.080632	1.106061
-53.910999	-10.610597	1.111066
-54.556472	3.682322	1.116070
-54.463132	-4.039529	1.121075
-54.476694	0.681848	1.126080
-54.525315	-0.009955	1.131085
-54.693456	-10.239831	1.136090
-55.263446	-2.201873	1.141094
-55.784643	-3.801888	1.146099
-56.226623	6.349633	1.151104
-56.310686	-1.571551	1.156109
-56.175979	-9.283674	1.161114
-56.700325	-3.868935	1.166118
-56.960928	-3.057864	1.171123
-57.688466	-3.857459	1.176128
-58.002753	-4.382722	1.181133
-57.710714	3.635421	1.186138
-58.034115	-0.352333	1.191142
-58.076903	-3.323915	1.196147
-58.117854	7.714120	1.201152
-58.213098	2.022490	1.206157
-58.860579	-1.087133	1.211162
-59.504072	1.438441	1.216166
-59.577786	-2.010501	1.221171
-59.757859	-1.509753	1.226176
-59.675211	-8.867723	1.231181
-59.578859	-6.287073	1.236186
-60.117858	1.515269	1.241190
-60.705741	-1.850102	1.246195
-61.319606	1.531336	1.251200
-61.042051	-2.097336	1.256205
-61.220194	-2.119053	1.261210
-61.425421	-5.401371	1.266214
-61.891621	-0.108937	1.271219
-62.652601	1.178681	1.276224
-62.949142	1.924665	1.281229
-62.593489	-6.496958	1.286234
-63.157663	1.882216	1.291238
-62.810847	-1.146980	1.296243
-62.944142	-6.110260	1.301248
-63.770456	-2.574451	1.306253
-64.139015	-3.048891	1.311258
-64.501023	-3.852385	1.316262
-64.484265	-6.050806	1.321267
-64.529251	-0.411162	1.326272
-64.534295	-2.038243	1.331277
-64.746759	-3.465214	1.336282
-65.767105	-1.286501	1.341286
-65.611797	-0.884313	1.346291
-66.102515	-3.682060	1.351296
-65.853674	-2.833206	1.356301
-66.264627	-1.593490	1.361306
-67.243572	2.154079	1.366310
-67.098469	-8.849124	1.371315
-67.711151	-2.108077	1.376320
-67.777818	0.241458	1.381325
-67.701066	-10.661624	1.386330
-67.835266	3.661867	1.391334
-67.715287	-9.253288	1.396339
-68.124898	3.072225	1.401344
-68.311797	6.733420	1.406349
-68.631486	-4.766659	1.411354
-69.317365	-1.287653	1.416358
-69.336729	1.990990	1.421363
-69.745369	-0.740232	1.426368
-69.683161	-4.001324	1.431373
-70.214313	-2.124639	1.436378
-70.741174	1.409138	1.441382
-70.841747	-2.912898	1.446387
-71.015940	-4.267470	1.451392
-71.063864	-0.889575	1.456397
-70.775082	2.913857	1.461402
-71.740046	3.587609	1.466406
-72.146444	-13.566717	1.471411
-72.353163	1.423535	1.476416
-72.881208	6.599919	1.481421
-72.983893	-5.713198	1.486426
-72.966509	-1.025364	1.491430
-72.947456	-10.060005	1.496435
-73.159479	-1.904518	1.501440
-74.235331	2.259097	1.506445
-74.061324	0.701819	1.511450
-74.561652	0.509288	1.516454
-74.430587	0.694082	1.521459
-74.345323	-1.843654	1.526464
-74.690776	8.599921	1.531469
-74.702504	-7.204888	1.536474
-75.528471	0.849022	1.541478
-75.705082	0.607024	1.546483
-75.923179	2.780949	1.551488
-76.087748	-2.273253	1.556493
-76.203544	-0.955137	1.561498
-77.383734	1.743188	1.566502
-77.588696	-5.108548	1.571507
-77.360353	-4.249591	1.576512
-77.312119	-4.731487	1.581517
-77.475207	-3.231885	1.586522
-77.733233	2.357595	1.591526
-77.762626	-3.951540	1.596531
-78.662195	-1.403881	1.601536
-79.172693	1.360939	1.606541
-79.028352	-0.506765	1.611546
-79.522972	4.586531	1.616550
-79.110216	6.972899	1.621555
-79.406945	3.889255	1.626560
-79.729506	5.408165	1.631565
-79.933231	0.203566	1.636570
-80.317485	-1.382026	1.641574
-80.250607	4.425771	1.646579
-80.747112	-0.090781	1.651584
-81.704392	6.773249	1.656589
-81.692881	-3.146570	1.661594
-82.350296	-2.582555	1.666598
-82.024961	-6.381742	1.671603
-81.854011	6.754769	1.676608
-82.091661	-1.569388	1.681613
-82.422015	4.249139	1.686618
-83.691288	2.237453	1.691622
-83.547784	-5.882832	1.696627
-83.536483	1.942828	1.701632
-84.106215	1.579456	1.706637
-83.862130	-3.997475	1.711642
-84.070225	7.979722	1.716646
-84.142309	6.715590	1.721651
-84.034069	0.377936	1.726656
-84.848186	6.216196	1.731661
-85.327549	-2.987702	1.736666
-85.561849	2.007820	1.741670
-85.583664	-5.386524	1.746675
-85.513393	5.509357	1.751680
-86.758263	-0.503169	1.756685
-86.926887	1.242045	1.761690
-87.235259	0.790396	1.766694
-87.320423	-7.516584	1.771699
-87.203866	-1.354121	1.776704
-87.254671	-0.480507	1.781709
-87.248668	-7.172411	1.786714
-87.554623	-2.651450	1.791718
-88.453695	-5.574952	1.796723
-88.393236	-1.560056	1.801728
-89.034796	5.560712	1.806733
-88.943994	-10.015193	1.811738
-88.948892	6.044930	1.816742
-89.072632	0.386439	1.821747
-89.935694	-0.963961	1.826752
-90.141288	-3.956530	1.831757
-90.286868	-4.663454	1.836762
-90.408668	2.568370	1.841766
-90.716810	2.737496	1.846771
-90.709216	-2.206886	1.851776
-91.664750	3.535605	1.856781
-91.581449	-1.156494	1.861786
-91.730248	-0.181798	1.866790
-92.035853	-1.776073	1.871795
-91.911995	4.670923	1.876800
-91.929760	-0.545331	1.881805
-92.585445	-2.380982	1.886810
-93.022766	1.014634	1.891814
-93.221751	-4.470961	1.896819
-93.147821	-4.399842	1.901824
-93.871450	-8.649077	1.906829
-94.519645	-0.398069	1.911834
-94.833189	-2.425754	1.916838
-94.493135	-2.021605	1.921843
-94.983316	-4.865809	1.926848
-95.237384	-2.035317	1.931853
-95.092350	-10.090733	1.936858
-95.562463	3.348881	1.941862
-95.310623	-8.406671	1.946867
-95.416509	3.018820	1.951872
-96.285356	0.888726	1.956877
-96.714323	-0.524487	1.961882
-96.636840	8.071853	1.966886
-96.581217	5.659597	1.971891
-97.714026	-2.781522	1.976896
-98.258800	2.440652	1.981901
-97.523150	-4.187191	1.986906
-97.910072	8.562387	1.991910
-98.318274	0.636281	1.996915
-98.668515	4.040347	2.006912
-98.399257	-0.179864	2.016909
-97.353687	-2.545270	2.026906
-97.246620	-4.512412	2.036902
-97.063829	-4.989647	2.046899
-96.093602	-3.166783	2.056896
-95.661937	0.448866	2.066893
-95.365116	-0.861706	2.076890
-94.145774	-2.658981	2.086886
-94.120999	-3.688778	2.096883
-93.992420	-5.429689	2.106880
-93.797246	-7.052803	2.116877
-92.579120	-8.112681	2.126874
-91.644949	2.431695	2.136870
-91.863522	-4.507722	2.146867
-91.386513	-4.898929	2.156864
-90.979140	1.281464	2.166861
-90.002221	-5.222282	2.176858
-89.909812	-12.190278	2.186854
-88.986371	-6.178539	2.196851
-88.524083	1.337139	2.206848
-88.278402	-2.198283	2.216845
-87.709367	1.437098	2.226842
-86.786110	-2.339366	2.236838
-86.503882	1.672694	2.246835
-86.383375	-3.837621	2.256832
-85.915001	0.069910	2.266829
-85.221005	-2.783200	2.276826
-84.926080	-5.516475	2.286822
-84.218047	1.268534	2.296819
-83.775674	1.354900	2.306816
-83.073594	1.475314	2.316813
-82.369680	2.185022	2.326810
-82.327183	6.805440	2.336806
-82.016102	-5.668958	2.346803
-80.997619	-1.744254	2.356800
-80.914049	-12.763483	2.366797
-79.831956	-6.422359	2.376794
-79.492349	-4.635142	2.386790
-79.354016	-1.284877	2.396787
-79.208863	-0.102079	2.406784
-77.864259	-10.915614	2.416781
-77.546858	-7.177308	2.426778
-77.405153	0.193284	2.436774
-76.561898	-5.727968	2.446771
-76.052831	-6.596517	2.456768
-75.709459	-11.943189	2.466765
-74.850805	-9.000298	2.476762
-74.657016	-4.491284	2.486758
-74.557168	-10.229747	2.496755
-73.518980	-4.391123	2.506752
-73.104986	-5.295893	2.516749
-72.615751	-1.877482	2.526746
-71.833034	-6.181143	2.536742
-71.539939	0.296973	2.546739
-71.445691	-3.679081	2.556736
-70.506068	-8.904585	2.566733
-69.867172	-0.549957	2.576730
-69.703454	-4.266230	2.586726
-69.559451	-4.531946	2.596723
-68.837360	-2.778037	2.606720
-68.164363	-7.335011	2.616717
-67.044828	-8.765429	2.626714
-67.021251	-13.419552	2.636710
-66.547879	-12.359673	2.646707
-66.198649	-9.419551	2.656704
-65.857403	-9.113515	2.666701
-65.201014	-7.702998	2.676698
-64.892944	-7.243079	2.686694
-63.936901	-1.426413	2.696691
-63.580233	-1.422472	2.706688
-63.275379	0.392040	2.716685
-62.397584	-6.037986	2.726682
-62.078751	-10.671455	2.736678
-61.937964	-5.733001	2.746675
-60.779023	-6.121352	2.756672
-60.406821	-5.946107	2.766669
-60.332886	-2.834333	2.776666
-59.616513	-6.129391	2.786662
-59.081584	-2.392726	2.796659
-58.890971	-7.293241	2.806656
-57.975830	0.179851	2.816653
-57.258975	1.293461	2.826650
-57.053354	-0.723196	2.836646
-57.036013	0.228846	2.846643
-56.033314	-8.373185	2.856640
-55.809332	-0.418320	2.866637
-55.179192	-4.492210	2.876634
-54.271417	-12.089796	2.886630
-54.103120	-0.623884	2.896627
-54.090103	-2.245876	2.906624
-52.925554	1.758579	2.916621
-52.910499	-0.068451	2.926618
-51.727313	-3.632870	2.936614
-51.360071	-2.796665	2.946611
-51.285103	-1.084369	2.956608
-50.924473	-7.844865	2.966605
-49.769284	-10.281169	2.976602
-49.889669	-5.300252	2.986598
-48.974269	-2.149802	2.996595
-48.450151	4.726926	3.006592
-48.240872	0.065953	3.016589
-47.584471	-0.520930	3.026586
-46.994895	-7.462986	3.036582
-46.558199	2.810702	3.046579
-45.892764	-5.529000	3.056576
-45.327517	-4.425056	3.066573
-44.957112	-3.237868	3.076570
-44.702093	-5.134472	3.086566
-44.247557	-3.305822	3.096563
-43.237314	-8.653269	3.106560
-43.164623	-7.007578	3.116557
-42.877233	-7.663561	3.126554
-41.781840	-6.054256	3.136550
-41.509194	-3.903649	3.146547
-41.366920	-6.478074	3.156544
-40.766766	-7.476896	3.166541
-40.203883	-3.087289	3.176538
-38.948297	1.811586	3.186534
-38.963631	-5.856999	3.196531
-38.552751	-6.721732	3.206528
-38.424882	-8.765425	3.216525
-37.319395	-6.713022	3.226522
-36.668738	-3.015474	3.236518
-36.827803	-14.391280	3.246515
-36.418982	-5.562078	3.256512
-35.529226	-11.330583	3.266509
-34.760780	-7.047136	3.276506
-34.574606	-11.108160	3.286502
-33.500891	-8.442917	3.296499
-33.467102	-8.865047	3.306496
-33.250235	-8.020339	3.316493
-32.916898	-4.440166	3.326490
-31.867620	-9.735392	3.336486
-31.627928	-9.358199	3.346483
-31.238750	-7.903031	3.356480
-30.616571	-9.068508	3.366477
-30.217280	-19.568798	3.376474
-29.267664	-7.243155	3.386470
-28.852358	-13.336364	3.396467
-28.827746	-8.340535	3.406464
-28.121512	-6.164121	3.416461
-27.434804	-6.909743	3.426458
-27.090164	-9.706176	3.436454
-26.045632	-9.518773	3.446451
-25.760702	-4.000953	3.456448
-25.750457	-11.670216	3.466445
-25.293595	-13.289834	3.476442
-24.319271	-9.528517	3.486438
-24.201521	-8.236261	3.496435
-23.693783	-11.660563	3.506432
-22.963183	-4.728324	3.516429
-22.569305	-5.079281	3.526426
-21.927223	-4.001296	3.536422
-20.940699	-3.481824	3.546419
-21.010301	-5.165020	3.556416
-20.670906	-5.761249	3.566413
-20.463564	-13.524006	3.576410
-19.483642	-10.676267	3.586406
-18.879218	-12.422473	3.596403
-18.200110	-14.249411	3.606400
-17.727608	-9.264325	3.616397
-17.432637	-11.411957	3.626394
-17.634087	-6.964734	3.636390
-16.493239	-11.038623	3.646387
-16.289799	-4.712417	3.656384
-15.415026	-4.279159	3.666381
-14.473588	-12.910753	3.676378
-14.273285	-3.590591	3.686374
-14.074056	-7.377750	3.696371
-13.840911	-5.693227	3.706368
-12.903129	-10.374261	3.716365
-12.515141	-8.812790	3.726362
-11.956824	-14.981250	3.736358
-11.186087	-13.048272	3.746355
-11.259621	-10.703213	3.756352
-10.413581	-13.143637	3.766349
-9.789733	-8.875165	3.776346
-9.374182	-13.988977	3.786342
-9.406657	-17.794669	3.796339
-8.466078	-10.980186	3.806336
-8.098257	-20.171984	3.816333
-7.310539	-14.469892	3.826330
-6.527671	-14.867084	3.836326
-6.608740	-10.238456	3.846323
-6.022365	-13.080647	3.856320
-5.811528	-13.137910	3.866317
-4.862754	-14.064839	3.876314
-4.704557	-11.567087	3.886310
-4.117203	-13.000254	3.896307
-3.660770	-0.907289	3.906304
-3.140836	1.468720	3.916301
-2.687172	9.109930	3.926298
-2.455780	20.682588	3.936294
-1.932137	32.180975	3.946291
-1.402729	50.804403	3.956288
-1.107500	69.450824	3.966285
-0.623444	91.921137	3.976282
0.012526	111.194839	3.986278
0.000000	138.984125	3.991283
0.574617	139.099815	3.996288
0.397377	155.690472	4.001293
0.599938	159.295499	4.006298
0.942830	179.204691	4.011302
0.691146	179.807088	4.016307
0.992369	167.024767	4.021312
1.118939	189.304872	4.026317
1.249385	189.074774	4.031322
1.425201	202.328667	4.036326
1.213209	206.781438	4.041331
1.550406	198.365720	4.046336
1.404564	204.015827	4.051341
1.438241	190.270387	4.056346
1.151634	194.033386	4.061350
1.255881	196.062986	4.066355
1.538725	201.531794	4.071360
1.286690	204.265091	4.076365
1.499015	193.397624	4.081370
1.471090	199.078524	4.086374
1.410305	203.515727	4.091379
1.529374	197.326172	4.096384
1.601568	202.169969	4.101389
1.293564	203.637542	4.106394
1.474670	204.078091	4.111398
1.275750	210.161658	4.116403
1.818789	196.537886	4.121408
1.537740	203.557204	4.126413
1.741178	197.997390	4.131418
1.548146	205.237359	4.136422
1.299916	198.845773	4.141427
1.717685	197.292711	4.146432
1.743807	200.912757	4.151437
1.564867	198.479321	4.156442
1.745788	208.958810	4.161446
1.496476	199.727925	4.166451
1.781439	204.865450	4.171456
1.541477	204.022784	4.176461
1.831572	207.144062	4.181466
1.974647	207.456325	4.186470
1.600882	209.055558	4.191475
2.045247	193.282752	4.196480
1.636791	202.811186	4.201485
1.975787	195.671151	4.206490
1.563506	188.757744	4.211494
1.477798	193.201637	4.216499
1.726863	198.818712	4.221504
1.666607	207.732409	4.226509
1.482531	207.001851	4.231514
1.577576	207.457045	4.236518
1.719431	209.938241	4.241523
1.990220	210.955160	4.246528
1.440858	211.131072	4.251533
1.696390	214.467251	4.256538
1.841344	203.455037	4.261542
1.420240	215.349469	4.266547
1.966624	207.218003	4.271552
1.881861	211.509992	4.276557
1.905178	200.502332	4.281562
2.062946	219.986976	4.286566
2.009030	211.295018	4.291571
1.953519	210.619935	4.296576
2.099999	213.773480	4.301581
1.789728	205.716184	4.306586
1.913795	211.472167	4.311590
1.685769	209.822391	4.316595
1.944521	220.599212	4.321600
2.041698	237.341062	4.326605
2.187423	240.197746	4.331610
2.385690	239.914779	4.336614
1.887433	229.046749	4.341619
2.166357	212.939600	4.346624
1.935848	221.931227	4.351629
2.096182	232.888341	4.356634
2.235375	233.163556	4.361638
2.253686	240.779795	4.366643
2.601185	221.716618	4.371648
1.808836	222.265675	4.376653
1.913614	212.773877	4.381658
1.881123	230.172419	4.386662
2.323957	236.397188	4.391667
2.599889	236.663179	4.396672
2.197434	238.216056	4.401677
2.445409	243.886806	4.406682
2.320544	225.591143	4.411686
2.071303	221.688922	4.416691
2.269651	221.762135	4.421696
2.238550	245.852948	4.426701
2.085671	234.169158	4.431706
2.329228	234.054913	4.436710
2.128887	234.770370	4.441715
2.559481	232.505557	4.446720
2.413866	237.170138	4.451725
2.598998	239.031440	4.456730
2.492807	239.794652	4.461734
2.341354	247.225487	4.466739
2.598842	232.883892	4.471744
2.254604	221.737770	4.476749
2.536650	226.178397	4.481754
2.481517	222.689818	4.486758
2.349918	220.036797	4.491763
2.447175	225.621200	4.496768
2.483162	235.409755	4.501773
2.515173	232.826531	4.506778
2.571555	239.552002	4.511782
2.521355	240.427699	4.516787
2.866089	227.634768	4.521792
2.444144	219.363888	4.526797
2.183820	217.856214	4.531802
2.330089	223.568663	4.536806
2.392845	235.193346	4.541811
2.564636	236.630017	4.546816
2.276746	242.174799	4.551821
2.485245	247.986277	4.556826
2.739766	245.976767	4.561830
2.375187	243.415208	4.566835
2.895446	244.475279	4.571840
2.753394	243.901353	4.576845
2.808541	247.856615	4.581850
2.560528	250.413032	4.586854
2.547519	248.372045	4.591859
2.885864	245.100299	4.596864
3.023943	244.983984	4.601869
3.028688	237.799426	4.606874
2.417003	244.892063	4.611878
2.455150	241.330609	4.616883
2.881421	242.097214	4.621888
2.660093	249.174942	4.626893
2.422534	253.169006	4.631898
2.625364	241.652456	4.636902
2.565780	248.267285	4.641907
2.679490	232.122156	4.646912
2.776348	248.869795	4.651917
2.494182	241.581387	4.656922
2.819664	255.878334	4.661926
2.847170	278.678182	4.666931
2.768592	273.758632	4.671936
2.774341	279.930882	4.676941
2.869740	270.573214	4.681946
3.209276	267.736592	4.686950
2.746650	278.387026	4.691955
3.234606	271.922048	4.696960
2.889100	282.692806	4.701965
2.994056	274.532181	4.706970
3.258969	275.016872	4.711974
3.149793	275.662966	4.716979
3.406251	276.161687	4.721984
3.320694	270.137217	4.726989
2.969894	263.332195	4.731994
2.942546	244.782372	4.736998
2.869654	243.404882	4.742003
2.796321	249.095885	4.747008
3.199856	272.793503	4.752013
2.983589	268.523499	4.757018
3.226511	276.091511	4.762022
3.032533	281.082419	4.767027
3.178779	272.272822	4.772032
2.949080	280.674507	4.777037
2.877336	279.958299	4.782042
3.089230	274.066715	4.787046
2.687066	275.977517	4.792051
3.024920	267.051141	4.797056
2.971907	272.028176	4.802061
3.237529	278.637909	4.807066
3.161643	266.279672	4.812070
3.237862	271.904676	4.817075
3.663930	272.822674	4.822080
3.185142	270.844012	4.827085
3.246246	276.813309	4.832090
3.323453	278.061994	4.837094
3.262474	288.069896	4.842099
3.526119	278.479921	4.847104
3.284642	274.489573	4.852109
3.296643	274.228175	4.857114
3.301113	271.300416	4.862118
3.366383	274.157404	4.867123
3.405703	271.538627	4.872128
3.442676	276.954836	4.877133
3.405874	273.367896	4.882138
3.650212	273.512626	4.887142
3.299709	279.375833	4.892147
3.484006	271.785402	4.897152
3.508449	282.109301	4.902157
3.693213	277.010572	4.907162
3.389898	286.726089	4.912166
3.388941	285.460611	4.917171
3.222561	281.911703	4.922176
3.235412	297.320950	4.927181
3.747690	310.957114	4.932186
3.885403	311.718224	4.937190
3.493535	312.263128	4.942195
3.561429	290.347272	4.947200
3.623327	309.671879	4.952205
3.250093	303.741407	4.957210
3.486517	302.118709	4.962214
3.431549	303.660820	4.967219
3.296355	306.132456	4.972224
3.502547	313.520479	4.977229
3.349540	309.707679	4.982234
3.600332	306.472521	4.987238
3.413848	316.426630	4.992243
3.625095	305.916444	4.997248
3.474243	314.035527	5.002253
3.540929	322.906760	5.007258
3.922503	330.927819	5.012262
3.797531	343.349342	5.017267
4.145906	334.642994	5.022272
3.743807	319.173032	5.027277
3.374750	313.632989	5.032282
3.541209	318.192636	5.037286
3.743753	328.548644	5.042291
4.048626	333.280937	5.047296
3.936509	343.181309	5.052301
4.115194	339.134985	5.057306
4.124961	331.860552	5.062310
3.736336	326.052405	5.067315
4.037015	317.782583	5.072320
4.089210	323.331859	5.077325
3.703352	307.892371	5.082330
3.938145	317.060780	5.087334
3.943108	337.061457	5.092339
4.291398	323.525274	5.097344
3.947747	313.725427	5.102349
3.800516	310.598210	5.107354
4.008414	317.962470	5.112358
3.548732	329.108953	5.117363
4.114219	336.996550	5.122368
4.260870	342.611890	5.127373
4.165586	347.485439	5.132378
4.341216	339.110608	5.137382
4.224096	338.033876	5.142387
3.642494	309.296404	5.147392
4.123754	333.297971	5.152397
4.261208	331.091355	5.157402
4.194540	336.761356	5.162406
3.833976	348.107130	5.167411
4.402133	342.673553	5.172416
4.223612	345.199534	5.177421
4.318284	349.262733	5.182426
4.212244	343.555987	5.187430
3.789334	342.501276	5.192435
4.338733	351.568866	5.197440
3.982275	344.216342	5.202445
4.372764	349.450306	5.207450
4.398250	337.556140	5.212454
4.160500	350.955408	5.217459
4.397435	340.721561	5.222464
4.133142	350.662133	5.227469
4.098702	347.495511	5.232474
4.525021	348.356047	5.237478
3.978594	349.191768	5.242483
4.083759	347.914238	5.247488
3.750530	348.400099	5.252493
3.936284	345.161888	5.257498
4.026796	344.809342	5.262502
4.168369	353.799027	5.267507
4.511450	357.914436	5.272512
4.437292	374.453131	5.277517
4.349549	377.979196	5.282522
4.562484	371.473284	5.287526
4.354275	380.106691	5.292531
4.578556	373.527068	5.297536
4.616684	381.993389	5.302541
4.525509	369.123139	5.307546
4.787519	374.649135	5.312550
4.169293	361.725661	5.317555
4.630636	369.192034	5.322560
4.685676	375.072189	5.327565
4.635079	364.550068	5.332570
4.406384	354.309447	5.337574
4.245154	375.751822	5.342579
4.695444	370.530356	5.347584
4.652360	385.100001	5.352589
4.273990	375.750271	5.357594
4.541207	372.427129	5.362598
4.357076	378.015360	5.367603
4.439033	378.306568	5.372608
4.504346	376.938544	5.377613
4.249285	378.170426	5.382618
4.733893	374.384442	5.387622
4.331493	375.686504	5.392627
4.614572	380.806640	5.397632
4.470988	378.391593	5.402637
4.591344	392.333284	5.407642
4.752823	401.879552	5.412646
4.762890	409.988417	5.417651
4.882507	409.212691	5.422656
4.953309	413.766696	5.427661
4.945822	401.758353	5.432666
5.150615	386.312744	5.437670
4.524501	385.339435	5.442675
4.638010	377.979325	5.447680
4.765310	393.557582	5.452685
4.736335	400.349354	5.457690
5.068023	410.690150	5.462694
5.168238	405.874550	5.467699
5.086493	398.231612	5.472704
5.007944	395.027093	5.477709
4.704650	384.388537	5.482714
4.908940	390.982228	5.487718
4.755276	403.360992	5.492723
5.167777	401.322934	5.497728
4.961978	413.663174	5.502733
5.083380	409.382604	5.507738
5.007795	409.524663	5.512742
5.091874	424.678133	5.517747
5.108057	407.363159	5.522752
4.819488	405.130185	5.527757
5.064199	403.272651	5.532762
4.954779	407.967403	5.537766
4.814172	410.959940	5.542771
5.119859	403.104248	5.547776
5.049701	412.460756	5.552781
4.995545	412.930993	5.557786
4.902283	404.661631	5.562790
4.992236	412.834429	5.567795
5.092654	405.632175	5.572800
5.082216	407.214678	5.577805
5.197630	409.286266	5.582810
5.301044	408.744505	5.587814
4.946118	418.103967	5.592819
5.308522	412.461314	5.597824
4.907046	415.401143	5.602829
4.937217	417.366866	5.607834
5.058000	412.263098	5.612838
5.167987	415.199142	5.617843
5.314163	412.417405	5.622848
4.979115	412.135919	5.627853
5.280574	421.565283	5.632858
5.424583	431.505786	5.637862
5.294871	434.787798	5.642867
5.327994	427.320993	5.647872
5.007747	436.290701	5.652877
5.196605	427.710767	5.657882
5.245429	439.328438	5.662886
5.450785	436.468617	5.667891
5.505267	434.875639	5.672896
5.275301	438.557091	5.677901
5.501581	433.270278	5.682906
5.297316	430.966901	5.687910
5.532729	433.600774	5.692915
5.424099	430.376758	5.697920
5.597550	439.063232	5.702925
5.221253	435.848215	5.707930
5.662397	439.846765	5.712934
5.360585	439.601215	5.717939
5.716384	431.009423	5.722944
5.373632	439.199815	5.727949
5.381825	436.070122	5.732954
5.482377	437.943875	5.737958
4.855217	451.991444	5.742963
5.197917	429.969696	5.747968
5.729507	448.750190	5.752973
5.601456	456.874846	5.757978
5.698370	463.141991	5.762982
5.754697	470.750469	5.767987
6.098472	455.581339	5.772992
5.697855	439.299747	5.777997
5.791669	438.584139	5.783002
5.962532	435.354691	5.788006
5.515493	442.214130	5.793011
5.378281	427.745110	5.798016
5.493766	444.747207	5.803021
5.539305	457.344043	5.808026
5.874018	457.184115	5.813030
5.503519	473.339023	5.818035
5.844223	467.622192	5.823040
6.023498	463.165469	5.828045
6.110508	460.280643	5.833050
6.047549	451.531043	5.838054
5.693863	446.211006	5.843059
5.762418	433.852792	5.848064
5.648478	442.834518	5.853069
5.654404	451.779430	5.858074
6.154113	444.955250	5.863078
5.846832	456.674528	5.868083
5.993099	458.394090	5.873088
6.220075	457.653274	5.878093
6.111859	448.523002	5.883098
5.798187	429.131158	5.888102
5.839454	441.799534	5.893107
5.936461	450.165760	5.898112
5.542757	455.085601	5.903117
5.731377	455.666998	5.908122
5.890246	461.170242	5.913126
5.925696	462.335278	5.918131
5.952023	459.566669	5.923136
6.015849	460.454282	5.928141
6.017417	465.441285	5.933146
5.968367	463.134697	5.938150
5.881125	465.899953	5.943155
5.914263	454.570796	5.948160
6.176025	468.475721	5.953165
5.807315	460.641884	5.958170
6.103557	452.861734	5.963174
6.017532	466.261632	5.968179
5.931359	453.328913	5.973184
6.082265	471.058291	5.978189
6.314655	476.353802	5.983194
6.699296	459.580038	5.988198
6.313411	464.969045	5.993203
6.349121	455.182265	5.998208
6.089474	460.478930	6.003213
6.181220	454.099221	6.008218
6.001323	460.308204	6.013222
5.966264	464.638604	6.018227
6.296276	452.725892	6.023232
6.094928	461.679478	6.028237
5.872740	467.333837	6.033242
6.512377	475.671793	6.038246
6.116221	470.865944	6.043251
6.163800	468.373445	6.048256
6.423574	476.171823	6.053261
6.389187	466.526888	6.058266
6.459546	462.793494	6.063270
5.926598	467.834672	6.068275
5.946278	461.378682	6.073280
6.058956	459.756922	6.078285
6.327430	469.093305	6.083290
6.519721	468.592079	6.088294
5.884439	460.864152	6.093299
6.057553	461.263407	6.098304
6.309329	478.940569	6.103309
6.295894	482.182615	6.108314
6.375694	460.947343	6.113318
5.953047	470.363438	6.118323
6.355716	465.469320	6.123328
6.349182	464.175150	6.128333
6.034824	467.578718	6.133338
6.034241	461.747506	6.138342
5.976008	467.114228	6.143347
6.469875	476.343236	6.148352
6.645957	473.364524	6.153357
6.294008	469.090883	6.158362
6.550742	463.578589	6.163366
6.135930	452.003919	6.168371
6.076202	447.157761	6.173376
5.908786	450.934434	6.178381
6.038456	451.885343	6.183386
6.288767	445.385052	6.188390
6.291219	457.992773	6.193395
6.282176	447.701904	6.198400
6.372970	458.441779	6.203405
5.885705	459.858150	6.208410
6.184156	455.449382	6.213414
6.089599	457.779530	6.218419
5.878307	461.642210	6.223424
6.034496	479.046887	6.228429
6.312498	477.623901	6.233434
6.584776	471.757370	6.238438
6.176595	473.653405	6.243443
6.129571	462.676940	6.248448
6.085551	461.707090	6.253453
6.346984	472.111856	6.258458
6.674218	471.926723	6.263462
6.211790	478.105140	6.268467
6.404647	464.427426	6.273472
6.154621	449.867543	6.278477
5.973866	458.177546	6.283482
6.348633	456.684073	6.288486
6.249977	464.905101	6.293491
6.202483	456.079725	6.298496
6.024595	461.164328	6.303501
6.093128	462.118849	6.308506
6.168283	453.199360	6.313510
6.011895	468.902618	6.318515
6.431451	467.379428	6.323520
6.536325	462.705716	6.328525
6.266404	457.812464	6.333530
6.153131	454.103757	6.338534
6.220218	462.529015	6.343539
6.462737	451.996779	6.348544
6.432093	456.677316	6.353549
6.495290	458.837283	6.358554
6.467580	454.431808	6.363558
6.185127	465.966218	6.368563
6.339704	449.977888	6.373568
6.419254	460.155826	6.378573
6.523165	464.140761	6.383578
6.589796	454.058970	6.388582
6.119928	458.549974	6.393587
6.484063	456.688052	6.398592
6.300093	446.190921	6.403597
6.162886	435.872341	6.408602
6.319608	428.951434	6.413606
6.014428	432.047006	6.418611
5.837039	430.455915	6.423616
6.152482	440.936177	6.428621
6.053253	452.745324	6.433626
6.187546	447.811190	6.438630
6.360954	455.443886	6.443635
6.178262	457.088466	6.448640
6.383833	452.304938	6.453645
6.154792	452.504377	6.458650
6.629262	453.686504	6.463654
6.334800	455.419845	6.468659
6.091726	431.286467	6.473664
6.034962	431.548154	6.478669
6.291047	442.216247	6.483674
6.205721	443.679529	6.488678
6.113021	444.795926	6.493683
5.992023	442.714382	6.498688
6.486987	453.319245	6.503693
6.165866	446.652102	6.508698
6.380033	438.283071	6.513702
6.166613	434.971225	6.518707
6.122025	431.021841	6.523712
6.161670	437.670444	6.528717
6.402973	437.140383	6.533722
6.366966	425.789346	6.538726
6.189946	421.079640	6.543731
6.128079	418.994228	6.548736
5.881615	420.955635	6.553741
6.026678	449.936674	6.558746
6.286495	443.112357	6.563750
6.019686	450.942467	6.568755
6.253226	459.294378	6.573760
6.125428	455.835737	6.578765
5.840515	456.061399	6.583770
6.154467	450.082793	6.588774
5.903069	457.919631	6.593779
6.336846	455.326675	6.598784
5.999403	451.631605	6.603789
5.662168	465.700246	6.608794
6.122356	443.566472	6.613798
6.174385	454.169298	6.618803
6.469168	460.436830	6.623808
6.050982	459.575905	6.628813
6.127945	460.074359	6.633818
6.203177	455.197759	6.638822
6.263532	448.866467	6.643827
6.022327	451.497962	6.648832
6.274046	454.222085	6.653837
5.915692	463.813424	6.658842
6.187976	455.537575	6.663846
6.180700	464.487048	6.668851
5.969353	457.234765	6.673856
6.200045	460.942361	6.678861
6.103491	472.058614	6.683866
6.231131	471.604799	6.688870
6.117918	479.004745	6.693875
6.538367	480.608655	6.698880
6.454490	462.916889	6.703885
6.167480	468.558499	6.708890
6.426542	463.517462	6.713894
6.460429	463.051150	6.718899
6.288440	454.878272	6.723904
6.254514	458.451882	6.728909
6.212628	455.688649	6.733914
6.653922	453.065835	6.738918
6.393827	468.799686	6.743923
6.441169	462.346811	6.748928
6.418298	452.690110	6.753933
6.252994	456.624900	6.758938
6.453057	456.507398	6.763942
6.462245	456.989447	6.768947
6.350546	453.135434	6.773952
6.154841	430.343229	6.778957
6.186048	436.017582	6.783962
6.234577	429.205563	6.788966
5.898203	448.208521	6.793971
6.117617	448.846783	6.798976
6.686452	457.113965	6.803981
6.276946	446.299363	6.808986
6.504131	430.044462	6.813990
6.262922	434.121664	6.818995
5.952831	429.940562	6.824000
6.235246	427.431482	6.829005
6.026626	431.564660	6.834010
6.334423	425.153725	6.839014
6.163141	427.749365	6.844019
6.329987	422.766828	6.849024
6.344368	423.058570	6.854029
6.004525	428.921055	6.859034
6.287730	421.854093	6.864038
6.245546	429.141808	6.869043
6.091013	432.916542	6.874048
6.167028	427.812288	6.879053
6.311746	423.082458	6.884058
6.364414	431.115803	6.889062
6.164827	436.602420	6.894067
6.188658	428.015080	6.899072
6.295606	424.998688	6.904077
6.004686	431.444696	6.909082
5.929799	420.290534	6.914086
5.977581	435.726893	6.919091
6.296836	443.471399	6.924096
6.176989	453.723990	6.929101
6.023571	454.208693	6.934106
6.280031	448.150212	6.939110
6.090698	460.497236	6.944115
6.258283	454.715932	6.949120
6.318194	460.414353	6.954125
5.993807	468.774589	6.959130
6.349144	456.884124	6.964134
5.968350	463.840153	6.969139
6.246545	463.244977	6.974144
6.465332	461.154528	6.979149
6.451885	462.975527	6.984154
6.507793	447.223375	6.989158
6.315481	445.845907	6.994163
6.161256	431.715375	6.999168
6.195561	429.336380	7.004173
6.013872	427.062024	7.009178
6.117179	430.681577	7.014182
6.118227	434.057774	7.019187
6.533090	444.123936	7.024192
6.503099	431.338028	7.029197
6.270658	433.807632	7.034202
6.244888	424.225234	7.039206
6.139992	434.860939	7.044211
6.196027	436.672995	7.049216
5.987037	426.650083	7.054221
5.971495	435.326212	7.059226
6.517596	417.565305	7.064230
6.409451	426.085669	7.069235
6.164581	418.751731	7.074240
6.259153	427.447116	7.079245
5.953334	431.991068	7.084250
5.693669	423.558029	7.089254
6.025028	443.198129	7.094259
6.274754	453.902606	7.099264
6.418000	454.760491	7.104269
6.055903	453.225638	7.109274
6.445006	450.168439	7.114278
6.187717	445.812823	7.119283
6.232812	444.684357	7.124288
6.078961	443.425832	7.129293
6.125549	451.392704	7.134298
6.299253	456.975781	7.139302
6.276998	450.226388	7.144307
6.330259	450.162402	7.149312
6.329593	442.377548	7.154317
6.038417	437.693253	7.159322
5.887448	434.946902	7.164326
6.074824	454.851219	7.169331
6.340220	452.212736	7.174336
6.452951	449.231890	7.179341
6.280397	446.714474	7.184346
6.201308	434.407152	7.189350
6.116990	436.102140	7.194355
6.046382	449.980190	7.199360
6.192884	454.065028	7.204365
6.162535	469.656838	7.209370
6.395929	457.112846	7.214374
6.364885	462.398101	7.219379
6.255955	431.952300	7.224384
6.147534	428.572944	7.229389
5.872317	436.184406	7.234394
6.234031	452.707052	7.239398
6.339802	462.352570	7.244403
6.284098	465.967282	7.249408
6.254618	458.804669	7.254413
6.099325	454.451303	7.259418
6.431695	448.403933	7.264422
6.378160	450.333002	7.269427
6.162602	437.141895	7.274432
6.210102	432.689635	7.279437
6.098123	431.500350	7.284442
6.430834	430.695059	7.289446
6.213812	433.321560	7.294451
6.085891	426.051728	7.299456
6.086523	429.098041	7.304461
5.791421	433.243172	7.309466
6.459746	447.387026	7.314470
6.191878	457.300434	7.319475
6.715365	456.046966	7.324480
6.107277	434.632391	7.329485
6.096022	438.091535	7.334490
6.134625	426.321229	7.339494
6.363443	431.428660	7.344499
6.005657	429.441385	7.349504
6.267432	436.127405	7.354509
5.864116	436.253282	7.359514
6.341902	446.328760	7.364518
6.610159	448.152840	7.369523
6.003760	440.017962	7.374528
6.253073	431.511095	7.379533
5.919667	435.299070	7.384538
6.112115	443.197778	7.389542
6.558228	446.551587	7.394547
6.238228	452.103536	7.399552
6.264421	438.018901	7.404557
5.954992	434.593104	7.409562
6.172305	431.215064	7.414566
6.115022	454.821333	7.419571
6.227074	462.147264	7.424576
6.328377	455.525414	7.429581
6.184749	445.335768	7.434586
6.352456	443.689505	7.439590
6.205951	445.698499	7.444595
5.967014	439.614702	7.449600
6.629327	441.910490	7.454605
6.221994	446.521183	7.459610
6.388929	428.925666	7.464614
6.407726	429.407702	7.469619
6.242955	431.895109	7.474624
6.350819	427.490084	7.479629
5.955697	438.558070	7.484634
6.141392	427.412061	7.489638
6.139869	431.804192	7.494643
6.116499	441.942130	7.499648
6.224000	428.328509	7.504653
6.184288	430.429340	7.509658
6.449792	426.186868	7.514662
6.155972	431.427415	7.519667
6.090745	441.312782	7.524672
6.374403	429.720547	7.529677
6.082434	428.797677	7.534682
6.337834	426.904823	7.539686
6.281752	437.172697	7.544691
6.171519	429.658587	7.549696
6.094559	431.883792	7.554701
6.415229	429.644850	7.559706
6.513382	428.915106	7.564710
6.239794	433.257368	7.569715
6.014643	430.123098	7.574720
6.211085	430.851795	7.579725
5.910586	432.613366	7.584730
6.146322	432.998501	7.589734
6.154892	436.656833	7.594739
6.132781	427.288335	7.599744
6.153200	426.911281	7.604749
6.082350	439.876272	7.609754
6.197170	422.371683	7.614758
6.194085	427.691370	7.619763
6.196081	426.911242	7.624768
6.044161	428.807067	7.629773
6.412353	438.074427	7.634778
6.449486	439.409881	7.639782
6.107401	437.789425	7.644787
6.174242	435.548507	7.649792
6.331570	434.587548	7.654797
6.219144	434.236439	7.659802
6.525324	431.554895	7.664806
6.225452	429.648413	7.669811
6.286455	428.732018	7.674816
6.336307	431.913845	7.679821
6.123091	435.332823	7.684826
6.074723	425.752983	7.689830
6.124126	432.495085	7.694835
6.090104	427.415959	7.699840
6.467285	433.302192	7.704845
6.035363	429.736045	7.709850
6.336028	427.091332	7.714854
6.152520	433.333266	7.719859
6.220426	425.158174	7.724864
6.377187	435.455134	7.729869
6.136809	431.554550	7.734874
6.561416	436.776184	7.739878
6.415038	431.233562	7.744883
6.181059	433.955423	7.749888
6.166746	429.729684	7.754893
6.465632	437.301139	7.759898
6.516553	426.864189	7.764902
6.288517	434.339370	7.769907
6.505217	430.771591	7.774912
6.759651	430.663636	7.779917
6.361889	426.371149	7.784922
6.442808	409.038546	7.789926
5.822748	409.605649	7.794931
6.168148	401.252402	7.799936
5.998618	408.232231	7.804941
5.958749	415.371946	7.809946
6.289671	419.837097	7.814950
6.324561	420.251741	7.819955
6.350694	425.454894	7.824960
6.139451	419.484923	7.829965
5.951087	429.564332	7.834970
6.128576	419.333764	7.839974
6.337298	433.133576	7.844979
6.123989	433.013877	7.849984
6.295492	427.533470	7.854989
5.829150	424.125962	7.859994
5.940330	429.573351	7.864998
6.215605	423.484335	7.870003
6.100097	428.601815	7.875008
6.383141	430.260046	7.880013
6.071971	439.390860	7.885018
6.184449	433.274924	7.890022
5.900834	431.852783	7.895027
6.193742	431.842850	7.900032
6.551451	424.037735	7.905037
6.107917	433.106594	7.910042
6.269195	427.120520	7.915046
6.143396	429.114045	7.920051
6.084114	426.470720	7.925056
6.179338	429.699301	7.930061
6.094158	430.140339	7.935066
6.444784	429.067449	7.940070
6.324196	428.444376	7.945075
6.312474	426.853086	7.950080
6.527896	428.420491	7.955085
5.872788	430.575667	7.960090
6.122115	425.725700	7.965094
6.395506	426.809496	7.970099
6.283920	426.625788	7.975104
6.412065	423.327243	7.980109
6.304878	426.397527	7.985114
6.598006	419.334448	7.990118
6.301793	426.923623	7.995136
6.221819	411.032215	8.000154
6.166369	409.367200	8.005171
5.883577	423.280813	8.010189
6.033627	429.076103	8.015206
6.187577	432.472103	8.020224
6.435010	441.512453	8.025242
6.429029	430.319065	8.030259
6.268802	431.503082	8.035277
6.412448	427.534001	8.040294
6.317285	432.582946	8.045312
6.262357	428.529236	8.050330
6.399126	425.086453	8.055347
6.150882	413.940869	8.060365
5.932629	418.152382	8.065382
6.376375	429.744870	8.070400
6.297080	429.100656	8.075418
6.372716	431.317389	8.080435
6.156860	432.693281	8.085453
6.430712	428.514267	8.090470
6.675794	431.543037	8.095488
5.964202	433.568104	8.100506
6.208913	427.105498	8.105523
5.831902	428.830100	8.110541
6.389947	437.186972	8.115558
6.213237	430.952996	8.120576
6.108683	431.560118	8.125594
6.455190	424.209854	8.130611
6.258530	437.830695	8.135629
6.315511	424.110728	8.140646
6.412063	435.326296	8.145664
6.238612	427.505675	8.150682
6.090305	429.140835	8.155699
6.378830	427.781627	8.160717
6.427476	429.562703	8.165734
6.498452	430.062418	8.170752
6.176947	433.377910	8.175770
6.427775	431.211223	8.180787
6.222504	438.889238	8.185805
6.515482	431.581888	8.190822
6.237089	430.851360	8.195840
6.170780	432.872125	8.200858
6.283016	425.111671	8.205875
5.894057	432.971664	8.210893
6.145249	443.018799	8.215910
6.840144	451.313060	8.220928
6.603806	452.445316	8.225946
6.876226	444.533730	8.230963
6.310227	436.116738	8.235981
6.226418	427.792332	8.240998
6.579555	435.928232	8.246016
6.422222	434.323388	8.251034
6.701085	424.467776	8.256051
6.185092	434.433692	8.261069
6.373475	443.583027	8.266086
6.471353	447.523710	8.271104
6.349586	460.328880	8.276122
6.520977	451.183518	8.281139
6.674199	458.076640	8.286157
6.808919	457.100157	8.291174
6.322372	442.875928	8.296192
6.288725	444.875539	8.301210
6.317173	450.930720	8.306227
6.331660	456.435498	8.311245
6.570052	460.984762	8.316262
6.553572	462.505188	8.321280
6.177674	463.023001	8.326298
6.655224	458.024477	8.331315
6.739938	464.996068	8.336333
6.318761	458.639188	8.341350
7.055659	462.973434	8.346368
6.233196	471.335317	8.351386
6.857145	463.934173	8.356403
6.799959	468.089108	8.361421
6.369346	473.316440	8.366438
6.905315	462.783234	8.371456
6.795078	466.415102	8.376474
6.989997	458.164399	8.381491
6.583375	449.540311	8.386509
6.445241	442.143923	8.391526
6.754179	437.462478	8.396544
6.535345	455.318788	8.401562
6.958593	448.025289	8.406579
6.668099	443.447040	8.411597
6.595443	427.798480	8.416614
6.393043	425.223612	8.421632
6.756557	439.976802	8.426650
6.962522	442.275885	8.431667
6.658156	432.228283	8.436685
6.486541	435.667566	8.441702
6.364271	430.404425	8.446720
6.448059	447.396894	8.451738
6.806512	457.372738	8.456755
6.857897	455.801829	8.461773
7.007851	454.242747	8.466790
6.959200	441.318154	8.471808
6.596616	435.702707	8.476826
6.537855	431.393547	8.481843
6.182399	450.406251	8.486861
6.549409	452.681619	8.491878
7.049403	456.125828	8.496896
6.561180	464.704980	8.501914
6.687741	455.983938	8.506931
6.325782	464.901211	8.511949
6.468300	458.013617	8.516966
6.704487	457.447270	8.521984
6.743419	464.052059	8.527002
6.895450	456.952275	8.532019
6.739641	460.060426	8.537037
6.159038	465.793858	8.542054
6.694095	453.450110	8.547072
6.775330	465.692966	8.552090
6.924506	462.919136	8.557107
6.937688	462.902476	8.562125
6.777264	472.204658	8.567143
6.845676	463.504067	8.572160
6.798909	469.745714	8.577178
6.754977	458.765071	8.582195
6.861664	470.742121	8.587213
6.649495	464.937004	8.592231
6.750057	457.950066	8.597248
6.331846	465.609618	8.602266
6.870995	474.672937	8.607283
6.871043	482.267765	8.612301
6.850222	487.654787	8.617319
7.115039	485.197608	8.622336
6.968728	497.051623	8.627354
6.937572	491.448200	8.632371
6.715233	482.539659	8.637389
6.976277	488.353006	8.642407
7.491583	483.120482	8.647424
7.123275	480.112677	8.652442
6.638752	468.245406	8.657459
6.962861	465.631768	8.662477
6.761151	467.275577	8.667495
6.843610	462.665287	8.672512
6.664409	469.459928	8.677530
7.211091	479.397925	8.682547
6.798384	475.045795	8.687565
6.628089	479.516884	8.692583
7.081290	490.669300	8.697600
6.894521	488.185528	8.702618
7.179245	492.268893	8.707635
7.417002	494.110978	8.712653
7.158907	491.506742	8.717671
6.996206	470.109864	8.722688
6.305056	470.360414	8.727706
6.822295	474.323388	8.732723
7.017782	490.743116	8.737741
6.773328	494.917258	8.742759
6.986347	487.965028	8.747776
7.050419	501.638806	8.752794
7.024020	495.209059	8.757811
7.254624	495.921107	8.762829
7.153072	492.457737	8.767847
7.314859	488.131331	8.772864
6.973609	499.658401	8.777882
7.051074	495.911467	8.782899
7.368680	486.716678	8.787917
7.122173	482.511619	8.792935
7.021884	474.900891	8.797952
7.017481	488.283852	8.802970
7.132214	485.197436	8.807987
7.110587	488.133580	8.813005
6.907437	498.821696	8.818023
7.243859	487.127110	8.823040
6.919953	494.876369	8.828058
6.960310	489.747685	8.833075
7.423583	484.364339	8.838093
7.129790	480.155890	8.843111
7.033289	482.284804	8.848128
6.942022	495.630977	8.853146
7.044653	497.956430	8.858163
6.911982	494.409834	8.863181
7.131865	492.376404	8.868199
7.097961	484.233849	8.873216
7.093165	495.339479	8.878234
7.226076	490.242316	8.883251
7.235530	494.118526	8.888269
7.437200	506.755813	8.893287
7.317430	490.363271	8.898304
7.193274	486.043272	8.903322
7.131665	499.292418	8.908339
6.949793	493.858035	8.913357
7.034623	492.676046	8.918375
6.947733	490.614878	8.923392
7.222167	499.437616	8.928410
7.082724	498.491766	8.933427
7.113184	487.136211	8.938445
6.968305	501.926208	8.943463
7.048150	497.605494	8.948480
6.724897	503.089842	8.953498
6.933767	514.710462	8.958515
7.378426	516.146069	8.963533
7.617479	532.779676	8.968551
7.523321	523.060175	8.973568
7.438686	530.347417	8.978586
7.671211	519.053844	8.983603
7.388814	502.205968	8.988621
7.455811	505.704172	8.993639
7.416223	495.004458	8.998656
7.326444	494.926112	9.003674
7.457154	489.812976	9.008691
7.685928	488.192023	9.013709
7.835698	487.711043	9.018727
7.849960	493.717805	9.023744
7.585061	503.176864	9.028762
7.338227	498.828951	9.033779
7.770745	489.459630	9.038797
6.937079	488.141173	9.043815
7.595016	487.810478	9.048832
7.473133	491.533643	9.053850
7.421112	493.447924	9.058867
7.703428	482.511462	9.063885
7.192390	464.380319	9.068903
7.363344	462.439832	9.073920
7.526828	476.923643	9.078938
7.181130	481.787138	9.083955
7.749022	471.558264	9.088973
7.350475	479.261611	9.093991
7.205376	462.310536	9.099008
7.151337	474.783069	9.104026
7.249666	482.349616	9.109043
7.554656	482.694842	9.114061
7.442751	487.418254	9.119079
7.642217	488.874383	9.124096
7.485676	488.302403	9.129114
7.360206	486.769634	9.134131
7.546579	480.775887	9.139149
7.281094	493.676728	9.144167
7.647957	483.732299	9.149184
7.393183	492.690890	9.154202
7.291208	495.612784	9.159219
7.813722	484.725319	9.164237
7.533086	492.975841	9.169255
7.688246	479.700363	9.174272
7.677948	478.876623	9.179290
7.090864	482.776419	9.184307
7.586518	487.691725	9.189325
7.575877	489.142491	9.194343
7.770166	477.378738	9.199360
7.649128	483.970460	9.204378
7.769085	486.055264	9.209395
7.747045	481.160718	9.214413
7.640917	485.427889	9.219431
7.631007	484.974138	9.224448
7.999761	476.155110	9.229466
7.462443	476.457938	9.234483
7.752459	475.396687	9.239501
7.540314	478.328159	9.244519
7.552645	479.441679	9.249536
7.531928	477.328810	9.254554
7.528467	489.125308	9.259571
7.660525	478.618033	9.264589
7.483016	485.401378	9.269607
7.598665	484.439468	9.274624
7.809890	481.801413	9.279642
7.408523	491.543084	9.284659
7.979466	489.140520	9.289677
7.526185	488.654879	9.294695
7.552157	490.802487	9.299712
7.660000	489.060624	9.304730
7.652483	494.074998	9.309747
7.688695	489.324534	9.314765
7.637165	494.004881	9.319783
7.725851	491.289288	9.324800
7.792054	490.883953	9.329818
7.600849	491.131436	9.334835
7.744927	485.870428	9.339853
7.666011	501.087463	9.344871
7.512946	487.429976	9.349888
7.390276	492.187847	9.354906
7.452435	491.206055	9.359923
7.430465	489.398095	9.364941
6.919758	497.733958	9.369959
7.317161	509.174348	9.374976
7.531811	517.942631	9.379994
7.589537	523.998307	9.385011
7.759766	513.103414	9.390029
7.702785	521.735589	9.395047
7.482128	526.873057	9.400064
7.834850	520.323438	9.405082
7.851940	532.576181	9.410099
8.356458	523.906288	9.415117
7.864144	531.497636	9.420135
7.869629	525.907620	9.425152
8.244310	515.768778	9.430170
7.860485	525.258960	9.435187
8.025840	526.857346	9.440205
7.706800	523.879363	9.445223
7.835808	514.484503	9.450240
7.898011	515.671652	9.455258
7.727946	517.238971	9.460275
7.653164	514.384312	9.465293
8.320194	514.800880	9.470311
8.101452	519.748671	9.475328
8.444490	510.639217	9.480346
8.223270	521.735432	9.485363
8.234204	517.146811	9.490381
8.171600	520.733011	9.495399
8.148558	521.187278	9.500416
8.253679	521.175668	9.505434
8.079934	524.488756	9.510451
8.198654	511.692482	9.515469
8.188211	500.237595	9.520487
7.865538	495.583562	9.525504
8.059814	487.190637	9.530522
7.724304	484.753541	9.535539
8.095845	499.158829	9.540557
7.852989	511.123127	9.545575
8.124514	517.334919	9.550592
7.974623	510.515800	9.555610
7.935068	520.349731	9.560627
8.172229	516.394865	9.565645
8.118883	524.784920	9.570663
8.245870	521.643519	9.575680
8.169791	508.785612	9.580698
7.940466	497.855128	9.585715
8.057672	498.682600	9.590733
8.277141	500.629479	9.595751
7.774320	504.991082	9.600768
8.087048	506.858941	9.605786
7.926475	521.331891	9.610803
8.193783	513.507332	9.615821
8.155068	518.718403	9.620839
8.257288	524.219700	9.625856
8.469874	516.011510	9.630874
8.079162	516.786879	9.635891
8.080160	512.411111	9.640909
8.163784	523.110217	9.645927
8.120783	522.049190	9.650944
8.346357	521.448971	9.655962
8.264598	522.941239	9.660979
8.008406	516.972341	9.665997
8.244945	526.087571	9.671015
8.043873	531.231443	9.676032
8.496493	520.608857	9.681050
8.371736	528.367278	9.686067
7.955262	507.380260	9.691085
8.231110	519.488578	9.696103
7.985797	529.588854	9.701120
8.118972	523.136608	9.706138
8.236210	531.894260	9.711155
8.343124	524.379897	9.716173
8.258398	528.452800	9.721191
7.841176	530.619082	9.726208
8.025221	522.728586	9.731226
7.700153	534.788400	9.736243
8.090284	526.772049	9.741261
7.988259	521.949787	9.746279
7.847600	526.994486	9.751296
8.163199	533.448774	9.756314
8.468759	544.263103	9.761331
8.364474	552.917693	9.766349
8.489779	548.655575	9.771367
8.554243	565.247462	9.776384
8.338079	537.087141	9.781402
8.250169	530.186494	9.786419
8.100609	548.238512	9.791437
8.351002	549.926159	9.796455
7.977893	555.467203	9.801472
8.208168	561.307916	9.806490
8.326282	559.163385	9.811507
8.423278	562.049194	9.816525
8.527103	561.608101	9.821543
8.201410	555.624320	9.826560
8.310182	546.412505	9.831578
8.455152	546.981462	9.836595
8.400249	550.390027	9.841613
8.724223	554.368491	9.846631
8.265794	557.851357	9.851648
8.474990	555.896850	9.856666
8.421302	551.081337	9.861683
8.591268	550.798966	9.866701
8.479541	560.517323	9.871719
8.252223	555.320744	9.876736
8.461943	551.772552	9.881754
8.321288	548.992177	9.886771
8.555883	552.596095	9.891789
8.639580	543.716759	9.896807
8.478803	555.465937	9.901824
8.545329	555.208569	9.906842
8.615562	561.623385	9.911859
8.453193	560.944106	9.916877
8.684926	557.235585	9.921895
8.845411	560.149461	9.926912
8.721790	548.792014	9.931930
8.676472	549.645614	9.936947
8.871177	548.584001	9.941965
8.862287	549.136313	9.946983
8.754601	559.434277	9.952000
8.844634	551.008189	9.957018
8.463149	553.600023	9.962035
8.534659	559.515053	9.967053
8.826842	547.194718	9.972071
8.688075	558.147392	9.977088
8.908588	544.949613	9.982106
8.595496	558.650663	9.987123
8.653954	563.277387	9.992141
8.659463	553.024467	9.997159
8.738060	564.318687	10.002176
8.606346	549.426980	10.007194
8.608855	556.325813	10.012211
8.632702	559.298532	10.017229
8.445537	558.210394	10.022247
8.723514	557.360566	10.027264
8.622995	553.767296	10.032282
8.768420	554.125956	10.037299
8.450935	558.046477	10.042317
8.790278	548.154002	10.047335
8.685137	560.817927	10.052352
8.554191	556.412031	10.057370
8.365239	558.190539	10.062387
8.704774	561.092088	10.067405
8.883686	557.788351	10.072423
8.539488	555.426693	10.077440
8.704577	548.651456	10.082458
8.804641	559.176419	10.087475
8.630879	559.641473	10.092493
8.734508	550.563175	10.097511
8.742612	556.963083	10.102528
8.863799	547.451198	10.107546
8.782019	550.251655	10.112563
8.548274	550.483744	10.117581
9.253254	562.342307	10.122599
8.870263	557.480540	10.127616
8.924165	554.010115	10.132634
9.205376	543.315510	10.137651
8.781566	548.757474	10.142669
9.233130	539.739474	10.147687
9.140971	544.861379	10.152704
8.878510	544.559675	10.157722
8.755228	545.135653	10.162739
8.968681	549.816624	10.167757
9.238488	547.144253	10.172775
8.792003	543.379548	10.177792
8.747730	551.425421	10.182810
8.993828	550.368288	10.187827
8.629537	560.098154	10.192845
9.009325	547.809372	10.197863
8.887767	555.028728	10.202880
8.881377	543.017466	10.207898
9.184689	549.580874	10.212915
8.891426	554.777222	10.217933
9.147339	551.454437	10.222951
8.885554	554.755931	10.227968
9.172733	546.029501	10.232986
9.246547	543.347462	10.238003
9.125542	542.707985	10.243021
9.141810	550.461764	10.248039
8.955055	550.986445	10.253056
8.696488	543.827850	10.258074
8.799688	557.099357	10.263091
8.675713	578.035176	10.268109
9.027958	575.562916	10.273127
8.916412	586.282376	10.278144
9.215739	582.287871	10.283162
9.096068	584.253716	10.288179
8.992754	586.970349	10.293197
9.478154	574.717204	10.298215
9.284214	583.094550	10.303232
9.095304	576.032666	10.308250
9.340709	583.684152	10.313267
9.295537	585.434525	10.318285
9.345254	573.625155	10.323303
8.929078	582.660522	10.328320
8.790372	579.319617	10.333338
9.255545	569.946415	10.338355
9.103048	577.607492	10.343373
9.315565	571.897158	10.348391
8.975181	567.266507	10.353408
8.934861	577.143905	10.358426
9.187261	575.632212	10.363443
9.067221	575.765163	10.368461
9.255362	573.957044	10.373479
9.040131	578.849946	10.378496
9.151231	578.238367	10.383514
9.578433	578.526354	10.388531
9.023116	572.900254	10.393549
9.127890	573.416424	10.398567
9.051892	577.828818	10.403584
9.360799	574.638189	10.408602
9.512268	575.894611	10.413619
9.195669	574.639727	10.418637
9.553959	568.435600	10.423655
9.324115	578.873877	10.428672
9.346194	573.514348	10.433690
9.580984	576.823771	10.438707
9.591879	579.475431	10.443725
9.637528	563.138682	10.448743
9.601034	567.696097	10.453760
9.730326	572.872477	10.458778
9.626250	567.326767	10.463795
9.713136	571.328748	10.468813
9.620946	565.168511	10.473831
9.865511	567.552356	10.478848
9.525062	560.783665	10.483866
9.473754	550.286628	10.488883
9.124060	545.240230	10.493901
9.280068	557.491642	10.498919
9.473364	565.745805	10.503936
9.667755	564.361822	10.508954
9.853364	554.263712	10.513971
9.238991	561.200921	10.518989
9.466884	544.322236	10.524007
9.216611	551.085770	10.529024
9.473473	565.633331	10.534042
9.392128	573.520404	10.539059
9.323497	577.781588	10.544077
9.758699	577.278536	10.549095
9.401526	573.988374	10.554112
9.429344	580.200786	10.559130
9.588185	576.509448	10.564147
9.405416	577.536195	10.569165
9.641347	580.234051	10.574183
9.746609	578.097551	10.579200
9.534308	572.963829	10.584218
9.785322	574.511622	10.589235
9.373756	579.753157	10.594253
9.426987	581.449047	10.599271
9.630014	580.225434	10.604288
9.624295	580.281977	10.609306
9.636415	579.481683	10.614323
9.499751	587.567282	10.619341
9.752439	582.588435	10.624359
9.563672	580.893905	10.629376
9.438570	578.801850	10.634394
9.584853	582.650306	10.639411
9.352308	575.955467	10.644429
9.884005	579.409021	10.649447
9.752394	568.668592	10.654464
9.513631	585.278430	10.659482
9.763476	574.235083	10.664499
9.555444	581.623486	10.669517
9.564112	574.723756	10.674535
9.656674	592.147186	10.679552
9.974667	599.286692	10.684570
10.090850	593.846617	10.689587
9.969300	586.372418	10.694605
10.063158	567.524295	10.699623
10.169016	562.728813	10.704640
10.146119	565.992720	10.709658
10.090235	563.865978	10.714675
9.851365	582.711516	10.719693
9.995360	576.622394	10.724711
9.895323	566.393241	10.729728
9.800863	581.224174	10.734746
10.025866	566.491872	10.739763
9.801538	576.549730	10.744781
10.001179	571.200955	10.749799
9.921511	578.780685	10.754816
9.594423	578.577866	10.759834
9.909724	567.295747	10.764851
9.785539	576.899255	10.769869
9.916271	576.862342	10.774887
9.850660	570.322922	10.779904
9.668342	580.719080	10.784922
9.815996	580.894312	10.789939
9.935170	583.688269	10.794957
9.430046	574.299763	10.799975
9.551919	568.696167	10.804992
9.849693	591.469919	10.810010
10.188361	587.550783	10.815027
10.142746	603.534994	10.820045
9.749712	584.843454	10.825063
9.388932	593.721631	10.830080
9.863569	596.022898	10.835098
10.301961	597.390461	10.840115
10.210539	598.682381	10.845133
10.400423	601.257165	10.850151
10.349908	604.079618	10.855168
10.151526	596.366970	10.860186
10.176519	580.369430	10.865203
9.894734	584.130906	10.870221
10.233268	589.670650	10.875239
10.063603	594.618999	10.880256
9.932064	600.364137	10.885274
10.216096	595.768261	10.890291
10.235293	604.990193	10.895309
10.185175	599.073354	10.900327
10.244287	596.646480	10.905344
10.172515	602.793508	10.910362
10.109245	589.675358	10.915379
10.106434	584.688034	10.920397
10.232988	593.854782	10.925415
10.530605	584.794339	10.930432
10.065323	584.929737	10.935450
9.981093	577.718243	10.940467
10.534619	597.090811	10.945485
10.288755	587.756210	10.950503
10.222338	567.916580	10.955520
10.108988	573.869313	10.960538
10.828217	585.688529	10.965555
10.508217	576.977983	10.970573
10.225137	574.083400	10.975591
10.217248	565.460540	10.980608
10.051266	572.487274	10.985626
10.187596	566.043936	10.990643
9.850558	573.893827	10.995661
10.501500	582.900512	11.000679
10.471673	595.867723	11.005696
10.397527	605.292895	11.010714
10.636475	601.027298	11.015731
10.208567	587.940398	11.020749
10.316451	589.011530	11.025767
10.426533	594.730828	11.030784
10.263996	596.377809	11.035802
10.303308	600.814027	11.040819
10.419103	599.791459	11.045837
10.091022	599.495502	11.050855
10.763840	592.433034	11.055872
10.170249	601.867451	11.060890
10.161331	601.345820	11.065907
10.256480	604.318552	11.070925
10.331815	600.928420	11.075943
10.869542	599.558836	11.080960
10.067964	601.462021	11.085978
10.597171	594.649697	11.090995
10.483919	609.229453	11.096013
10.283972	604.206661	11.101031
10.452837	600.011327	11.106048
10.036226	602.360182	11.111066
10.331185	598.602995	11.116083
10.384290	601.448444	11.121101
10.436831	596.692094	11.126119
10.340677	603.238804	11.131136
10.376902	618.094586	11.136154
10.740332	622.617682	11.141171
10.954928	630.357360	11.146189
10.510585	621.743358	11.151207
10.730414	611.819455	11.156224
10.386209	624.942286	11.161242
10.840551	613.954413	11.166259
10.687893	612.920789	11.171277
10.505479	612.609765	11.176295
10.837521	615.222031	11.181312
10.861648	607.237902	11.186330
10.558918	597.573362	11.191347
10.609290	597.697778	11.196365
10.662033	608.911278	11.201383
10.940116	610.140437	11.206400
10.678490	603.941710	11.211418
10.442949	595.401803	11.216435
10.894523	609.512070	11.221453
10.827014	615.263539	11.226471
10.720623	614.980475	11.231488
10.425210	621.836156	11.236506
10.646827	626.756335	11.241523
10.964850	631.141292	11.246541
10.668188	625.845942	11.251559
11.100540	619.772042	11.256576
10.740759	632.557321	11.261594
10.554670	632.389023	11.266611
10.897990	629.881226	11.271629
10.803079	620.500744	11.276647
10.767123	620.892196	11.281664
10.961319	632.253146	11.286682
11.091938	633.666559	11.291699
10.960007	628.354953	11.296717
10.719226	627.595354	11.301735
11.056792	618.006653	11.306752
10.684910	630.457735	11.311770
10.796645	627.607994	11.316787
10.995935	626.942048	11.321805
10.715868	624.429611	11.326823
10.803007	618.634516	11.331840
10.657608	630.857948	11.336858
10.847621	623.821480	11.341875
10.899920	626.771786	11.346893
10.883083	628.036004	11.351911
11.028323	622.933606	11.356928
11.020889	626.226460	11.361946
10.908965	630.655841	11.366963
10.656117	622.646312	11.371981
10.618314	634.773195	11.376999
10.990211	644.180433	11.382016
10.762100	657.893086	11.387034
11.067958	655.656828	11.392051
10.958552	655.632515	11.397069
10.929156	657.414533	11.402087
11.381031	653.197910	11.407104
11.488482	663.064673	11.412122
11.394638	656.056691	11.417139
11.516107	643.725967	11.422157
10.967059	638.008653	11.427175
10.996088	631.694073	11.432192
11.197394	633.559926	11.437210
11.454936	641.976710	11.442227
11.427726	627.201473	11.447245
11.018558	623.056970	11.452263
11.347797	615.236080	11.457280
11.250634	622.194357	11.462298
11.175834	618.247621	11.467315
11.367826	613.481165	11.472333
11.199664	623.967916	11.477351
11.570538	619.608031	11.482368
11.600204	625.573714	11.487386
11.426376	622.624813	11.492403
11.591817	624.734778	11.497421
11.414986	622.346183	11.502439
11.568180	613.012018	11.507456
11.245628	621.570515	11.512474
11.081140	625.215733	11.517491
11.572709	616.708553	11.522509
11.111683	621.402813	11.527527
11.441199	616.513590	11.532544
11.262834	623.631368	11.537562
11.327666	615.729859	11.542579
11.271141	622.551100	11.547597
11.035744	622.409470	11.552615
11.455337	617.158501	11.557632
11.291454	625.631280	11.562650
11.211908	627.120436	11.567667
10.951812	614.134852	11.572685
11.205206	628.835006	11.577703
11.632534	638.194874	11.582720
11.555286	643.064554	11.587738
11.787792	648.402991	11.592755
11.663612	626.400931	11.597773
11.060746	636.160901	11.602791
11.353108	626.287573	11.607808
11.276076	641.840044	11.612826
11.393179	646.657071	11.617843
11.509863	652.267036	11.622861
11.229059	660.443859	11.627879
11.799446	655.871016	11.632896
11.501489	664.184533	11.637914
11.561497	656.093261	11.642931
11.615026	650.956044	11.647949
11.378890	652.571126	11.652967
11.699189	654.307048	11.657984
11.315788	659.472690	11.663002
11.293852	663.356502	11.668019
11.683605	658.637595	11.673037
11.424799	664.759322	11.678055
11.259215	652.830828	11.683072
11.574720	658.159462	11.688090
11.385482	667.867100	11.693107
11.449141	663.818690	11.698125
11.391251	682.443052	11.703143
11.862673	680.527780	11.708160
11.863209	683.873654	11.713178
11.986389	689.855764	11.718195
12.138399	679.921789	11.723213
11.971574	670.670501	11.728231
11.765033	648.030117	11.733248
11.966067	650.148365	11.738266
11.772707	649.506102	11.743283
11.688000	645.409827	11.748301
11.745752	649.672937	11.753319
11.596270	648.612408	11.758336
11.858045	651.413471	11.763354
11.783432	643.832264	11.768371
11.914704	640.426169	11.773389
11.751561	652.086054	11.778407
12.060512	656.974460	11.783424
12.055212	655.438507	11.788442
11.785705	645.220830	11.793459
12.007420	651.430296	11.798477
12.162722	649.755551	11.803495
11.954966	644.273436	11.808512
11.910591	642.102260	11.813530
11.653295	644.499539	11.818547
11.938623	642.572963	11.823565
11.996600	643.303959	11.828583
11.982833	648.053686	11.833600
12.132996	651.132664	11.838618
11.785989	645.357484	11.843635
11.671501	644.256517	11.848653
11.620227	669.133732	11.853671
11.818376	669.080931	11.858688
12.092217	674.345214	11.863706
11.874617	681.546283	11.868723
12.203658	678.814084	11.873741
12.086492	670.599790	11.878759
12.266992	670.160563	11.883776
12.414011	678.961396	11.888794
12.108503	680.522224	11.893811
12.188624	678.179649	11.898829
12.348430	685.797332	11.903847
12.283955	680.408401	11.908864
12.490436	665.818434	11.913882
12.551201	673.813908	11.918899
12.347426	642.354287	11.923917
11.801958	656.102168	11.928935
11.963843	646.685840	11.933952
12.085261	651.188786	11.938970
12.041807	672.355873	11.943987
12.357375	668.016550	11.949005
12.496442	674.662127	11.954023
12.255655	677.737348	11.959040
12.306854	672.939467	11.964058
12.188591	675.642450	11.969075
12.357074	673.943474	11.974093
12.128332	678.874863	11.979111
12.490819	675.256467	11.984128
12.419484	685.048918	11.989146
12.222029	680.237093	11.994163
12.443526	677.523096	11.999181
12.312089	680.240072	12.004199
12.308407	676.730733	12.009216
12.269746	673.879511	12.014234
12.231894	675.229098	12.019251
12.483991	672.906862	12.024269
12.219676	677.321730	12.029287
12.240892	673.909443	12.034304
12.513112	677.961073	12.039322
12.244676	680.801516	12.044339
12.344898	681.036175	12.049357
12.378966	677.458777	12.054375
12.184859	683.852065	12.059392
12.322322	678.724561	12.064410
12.363708	674.433393	12.069427
12.496901	672.904819	12.074445
12.496672	678.367627	12.079463
12.387003	680.973918	12.084480
12.407682	673.588323	12.089498
12.310038	679.199145	12.094515
12.465622	678.692395	12.099533
12.616812	684.524204	12.104551
12.526980	687.873626	12.109568
12.676095	693.338086	12.114586
12.791646	697.474715	12.119603
12.576188	688.662941	12.124621
12.477603	686.923153	12.129639
12.719655	692.800546	12.134656
13.045546	684.951043	12.139674
12.278512	681.097266	12.144691
12.428902	678.885173	12.149709
12.485851	701.757625	12.154727
12.564542	707.966782	12.159744
12.936119	690.896044	12.164762
12.694765	697.542817	12.169779
12.584578	698.061124	12.174797
12.860511	698.882402	12.179815
12.675376	704.605352	12.184832
12.789043	699.629017	12.189850
12.642637	702.524844	12.194867
12.494287	696.397475	12.199885
12.705202	702.377266	12.204903
12.749510	707.382341	12.209920
12.566962	685.567805	12.214938
12.899546	701.566652	12.219955
12.974767	691.170608	12.224973
12.737502	701.196439	12.229991
13.036072	703.622935	12.235008
13.296087	691.222384	12.240026
12.904413	690.247624	12.245043
13.327098	692.605537	12.250061
13.000070	696.929226	12.255079
13.063922	702.642440	12.260096
12.957331	690.372277	12.265114
12.553361	696.380267	12.270131
12.979060	690.340904	12.275149
13.201351	695.999930	12.280167
12.881084	702.686149	12.285184
13.075509	702.054862	12.290202
12.770482	706.077289	12.295219
13.013896	701.114900	12.300237
12.875744	708.419748	12.305255
12.868283	708.722237	12.310272
12.989125	695.747516	12.315290
13.102888	704.668824	12.320307
12.926780	696.554822	12.325325
12.861369	706.306937	12.330343
12.933974	700.672477	12.335360
13.133402	703.313411	12.340378
13.253741	720.144230	12.345395
13.134257	717.992173	12.350413
13.059270	713.690345	12.355431
13.181964	730.463308	12.360448
13.231535	721.589520	12.365466
13.205676	731.097713	12.370483
13.612088	730.505335	12.375501
13.572067	705.459073	12.380519
13.644003	697.008738	12.385536
13.320435	689.705728	12.390554
13.131546	702.712359	12.395571
12.954669	700.071411	12.400589
13.402089	696.229903	12.405607
13.107251	698.059029	12.410624
12.973978	692.385046	12.415642
13.167950	705.366862	12.420659
13.191905	723.496251	12.425677
13.330753	730.793823	12.430695
13.418649	734.545692	12.435712
13.845837	723.859860	12.440730
13.707205	711.145404	12.445747
13.695408	704.932431	12.450765
13.883579	690.958431	12.455783
13.598877	691.470597	12.460800
13.730834	693.252671	12.465818
13.418841	698.412406	12.470835
13.642022	701.925342	12.475853
13.622051	695.650344	12.480871
13.553871	701.459433	12.485888
13.523444	690.281715	12.490906
13.864579	693.327505	12.495923
13.393919	704.948592	12.500941
13.743785	700.669719	12.505959
13.435834	696.832432	12.510976
13.821917	695.606055	12.515994
13.650146	691.292309	12.521011
13.673996	695.059498	12.526029
13.331692	678.804190	12.531047
13.334952	693.183246	12.536064
13.308212	684.715795	12.541082
13.376962	700.561490	12.546099
13.191019	695.700120	12.551117
13.410544	689.433101	12.556135
12.975165	701.538474	12.561152
13.512490	692.172148	12.566170
13.202474	704.390222	12.571187
13.437016	718.297563	12.576205
13.685343	722.168525	12.581223
13.721002	724.161814	12.586240
13.821408	723.320911	12.591258
13.835676	721.180956	12.596275
13.271592	728.498866	12.601293
13.681546	725.254469	12.606311
13.654968	728.989861	12.611328
13.741350	727.215503	12.616346
13.501892	722.848392	12.621363
13.786180	718.513447	12.626381
13.776597	728.572850	12.631399
13.638941	737.359834	12.636416
14.000359	728.981619	12.641434
14.204550	729.353386	12.646451
13.957976	735.608935	12.651469
14.186314	725.086338	12.656487
13.951624	731.526521	12.661504
13.984861	731.444338	12.666522
14.108787	728.000860	12.671539
13.783497	720.273733	12.676557
14.098312	717.558843	12.681575
13.683203	726.237048	12.686592
13.659430	722.052715	12.691610
13.881304	721.163747	12.696627
13.734147	728.387030	12.701645
14.062259	736.482747	12.706663
14.319392	745.047285	12.711680
14.318360	737.044815	12.716698
14.305797	739.652751	12.721715
13.982432	730.763551	12.726733
14.116780	714.241098	12.731751
13.819390	731.105669	12.736768
13.880060	722.171385	12.741786
14.112402	735.423630	12.746803
14.229618	747.252505	12.751821
14.619363	748.938358	12.756839
14.412445	739.629498	12.761856
14.501822	725.340347	12.766874
14.118296	724.942157	12.771891
14.151928	722.504523	12.776909
14.548839	709.662414	12.781927
14.102482	721.960555	12.786944
14.129293	713.580671	12.791962
14.141812	714.090864	12.796979
13.951950	726.496134	12.801997
14.193545	720.142382	12.807015
14.666100	736.149582	12.812032
14.408275	727.374722	12.817050
14.476777	731.628200	12.822067
14.324527	730.450020	12.827085
14.693072	715.745773	12.832103
14.215790	722.715861	12.837120
14.267232	722.816873	12.842138
14.410848	722.732160	12.847155
14.397772	722.924954	12.852173
14.272597	725.247615	12.857191
14.182069	722.628583	12.862208
14.188738	736.150468	12.867226
14.510947	745.532533	12.872243
14.551816	748.088712	12.877261
14.555344	742.273560	12.882279
14.519421	748.996175	12.887296
14.485656	754.046080	12.892314
14.760903	746.016360	12.897331
14.362479	755.583504	12.902349
14.540543	756.604840	12.907367
14.694423	749.427062	12.912384
14.724682	755.611976	12.917402
14.708257	750.984709	12.922419
14.547601	758.075208	12.927437
14.747130	749.074217	12.932455
14.317325	753.208257	12.937472
14.527963	745.887231	12.942490
14.983571	750.710439	12.947507
14.625605	750.998531	12.952525
14.814531	752.000352	12.957543
14.550875	755.730522	12.962560
14.818053	750.510652	12.967578
14.780129	743.031978	12.972595
14.786417	744.365601	12.977613
15.085951	742.146124	12.982631
14.837058	750.475183	12.987648
14.743485	747.363763	12.992666
14.814788	755.831132	12.997683
14.916051	754.649552	13.002701
15.268198	735.429732	13.007719
14.535797	740.365016	13.012736
14.802581	727.924341	13.017754
14.725798	726.501000	13.022771
14.635309	746.962236	13.027789
14.763583	750.016514	13.032807
14.763435	753.760133	13.037824
14.749174	746.971597	13.042842
15.019156	750.909843	13.047859
14.633814	749.271072	13.052877
14.880267	742.262604	13.057895
14.990279	749.368513	13.062912
14.525751	747.226346	13.067930
14.752508	751.388273	13.072947
14.646548	754.597868	13.077965
15.091904	748.783563	13.082983
14.988154	751.036542	13.088000
15.095541	773.770833	13.093018
15.219089	774.411847	13.098035
14.892648	769.701664	13.103053
15.163564	770.948165	13.108071
15.508150	778.025480	13.113088
15.087275	760.806373	13.118106
15.007991	749.448523	13.123123
14.785917	750.975465	13.128141
14.761702	759.746433	13.133159
14.838899	773.486975	13.138176
15.205831	771.919293	13.143194
15.500819	773.077560	13.148211
15.363501	773.051964	13.153229
15.455896	765.678858	13.158247
15.296477	781.426598	13.163264
15.067345	785.666387	13.168282
15.215615	769.117163	13.173299
15.188398	778.127996	13.178317
15.285832	783.227837	13.183335
15.188230	783.029137	13.188352
14.989006	778.339222	13.193370
15.417068	778.781788	13.198387
15.127305	782.649745	13.203405
15.369066	770.463167	13.208423
15.427706	774.817498	13.213440
15.424534	781.229207	13.218458
15.132008	776.039020	13.223475
15.054811	783.699540	13.228493
15.345615	785.772629	13.233511
15.380109	789.689646	13.238528
15.735657	802.818402	13.243546
15.699218	795.164268	13.248563
15.433670	795.854753	13.253581
15.424252	791.142459	13.258599
15.441242	793.973846	13.263616
15.586173	800.516544	13.268634
15.804348	802.681578	13.273651
15.799257	802.425829	13.278669
15.689978	782.735140	13.283687
15.640449	780.551413	13.288704
15.418102	779.139967	13.293722
15.966479	776.816291	13.298739
15.692799	778.019120	13.303757
15.248952	776.774266	13.308775
15.898501	790.156282	13.313792
15.795747	793.293310	13.318810
15.823895	775.389234	13.323827
15.401655	781.780184	13.328845
15.593340	793.603062	13.333863
15.779533	795.075788	13.338880
15.781174	801.853226	13.343898
15.971376	795.337884	13.348915
15.650763	812.276070	13.353933
15.777358	808.779772	13.358951
16.195758	798.650042	13.363968
15.801483	805.597367	13.368986
16.178033	795.364338	13.374003
15.945879	798.755460	13.379021
15.741047	791.550845	13.384039
15.998442	801.157051	13.389056
15.732619	805.933998	13.394074
15.898258	798.494814	13.399091
15.684492	804.826843	13.404109
15.723801	800.491105	13.409127
15.828833	802.376858	13.414144
15.886841	804.020804	13.419162
16.207555	797.479912	13.424179
16.083510	809.257845	13.429197
15.827287	803.478988	13.434215
16.359193	800.581687	13.439232
15.789086	797.066118	13.444250
16.132619	797.441583	13.449267
15.988581	798.819787	13.454285
16.139722	792.761679	13.459303
16.396250	793.788528	13.464320
16.235748	800.484159	13.469338
15.998246	794.264825	13.474355
15.972934	802.624602	13.479373
16.118509	802.126592	13.484391
16.319367	796.700770	13.489408
16.117156	805.311877	13.494426
16.301714	797.932550	13.499443
15.805178	806.781756	13.504461
15.516791	809.840869	13.509479
16.403163	813.405818	13.514496
16.728743	820.718178	13.519514
16.646342	808.975386	13.524531
16.014690	808.704496	13.529549
16.288110	804.086301	13.534567
16.501428	791.749699	13.539584
16.269858	791.223987	13.544602
16.058283	790.246168	13.549619
15.960507	809.298920	13.554637
16.001408	818.988622	13.559655
16.641206	826.243443	13.564672
16.285953	828.321553	13.569690
16.514147	828.712969	13.574707
16.793063	831.248247	13.579725
16.710137	834.503254	13.584743
16.861793	824.313745	13.589760
16.742720	833.983886	13.594778
16.784031	824.540961	13.599795
16.390654	813.368533	13.604813
16.459643	824.705084	13.609831
16.776830	833.084931	13.614848
16.412918	830.887904	13.619866
16.912688	832.000849	13.624883
16.632793	823.786649	13.629901
16.709269	824.257515	13.634919
16.650845	811.931644	13.639936
16.533412	818.958324	13.644954
16.657711	823.090782	13.649971
16.835419	826.091223	13.654989
16.764724	831.719683	13.660007
16.761418	822.215647	13.665024
16.814398	828.285416	13.670042
16.954232	827.551753	13.675059
16.935338	826.665248	13.680077
16.562422	816.885033	13.685095
16.930849	816.568220	13.690112
16.483130	835.069925	13.695130
16.817632	825.034775	13.700147
16.597234	829.603823	13.705165
16.675487	828.500060	13.710183
16.800614	820.684914	13.715200
16.772934	832.792560	13.720218
16.833102	827.332940	13.725235
16.725147	833.083707	13.730253
16.713891	823.496739	13.735271
16.867707	819.131798	13.740288
16.542834	828.797827	13.745306
16.963441	837.829024	13.750323
17.188302	846.942244	13.755341
17.203334	841.570011	13.760359
17.082662	837.385551	13.765376
16.808680	838.882515	13.770394
17.324587	832.143547	13.775411
17.293538	844.249004	13.780429
17.102442	834.739444	13.785447
16.819818	827.788233	13.790464
17.282267	843.479123	13.795482
17.249551	845.661694	13.800499
17.142644	843.920117	13.805517
17.102280	846.520077	13.810535
17.353876	845.925773	13.815552
17.194026	851.152094	13.820570
17.218504	851.574881	13.825587
17.234404	847.441422	13.830605
17.196803	848.407141	13.835623
17.165792	842.102024	13.840640
17.201983	844.247595	13.845658
17.326559	845.566364	13.850675
17.386548	842.454299	13.855693
16.995585	842.621877	13.860711
17.765936	838.307195	13.865728
17.261773	846.258909	13.870746
17.035094	845.662310	13.875763
17.385251	843.027763	13.880781
17.240866	839.025173	13.885799
17.483990	846.160263	13.890816
17.323468	845.702309	13.895834
17.286502	844.430624	13.900851
17.057987	844.861053	13.905869
17.227241	844.393765	13.910887
17.603165	859.369504	13.915904
17.786310	871.847764	13.920922
17.865592	854.185119	13.925939
17.767189	841.311933	13.930957
17.344150	844.598065	13.935975
17.805853	835.570145	13.940992
17.786260	839.094181	13.946010
17.720124	835.740022	13.951027
17.492232	837.298642	13.956045
17.485254	849.796162	13.961063
17.881974	836.775248	13.966080
17.606911	839.110147	13.971098
17.551293	846.310059	13.976115
18.116016	863.595772	13.981133
17.766618	860.468032	13.986151
17.725104	845.181987	13.991168
17.864230	850.148967	13.996186
17.940513	861.127266	14.001203
17.888475	844.869385	14.006221
17.710957	858.193540	14.011239
17.940991	864.258808	14.016256
18.074787	867.409041	14.021274
17.940837	866.904167	14.026291
17.768447	847.882872	14.031309
17.564256	862.523592	14.036327
17.719907	867.188248	14.041344
18.025410	877.157386	14.046362
18.027010	868.517826	14.051379
18.076620	875.066497	14.056397
17.623572	872.753127	14.061415
18.187150	868.473857	14.066432
17.774093	871.474890	14.071450
18.053464	870.928740	14.076467
18.117746	869.131649	14.081485
18.063392	877.767523	14.086503
17.874973	875.372146	14.091520
17.794701	872.372273	14.096538
17.789312	876.875418	14.101555
18.003209	878.506943	14.106573
18.301090	896.354573	14.111591
18.500938	884.642148	14.116608
18.425665	883.163033	14.121626
18.167815	885.907669	14.126643
18.127328	874.650386	14.131661
18.340325	882.432579	14.136679
18.323039	875.599214	14.141696
18.197411	886.582226	14.146714
18.215826	880.551573	14.151731
18.527700	888.369757	14.156749
18.433345	895.056443	14.161767
18.434421	891.361236	14.166784
18.150571	888.177756	14.171802
18.290156	899.472358	14.176819
18.586420	898.066753	14.181837
18.533875	902.366699	14.186855
18.629333	901.526212	14.191872
18.460937	896.559514	14.196890
18.370200	900.956725	14.201907
18.564190	910.728611	14.206925
18.525044	903.024874	14.211943
18.544749	896.955420	14.216960
18.898624	902.255739	14.221978
18.568254	895.190756	14.226995
18.957242	890.538046	14.232013
18.767763	880.171927	14.237031
18.645775	870.798139	14.242048
18.546752	875.302615	14.247066
18.269441	876.732814	14.252083
18.709524	883.071168	14.257101
18.819407	900.750728	14.262119
18.780798	884.732698	14.267136
18.796261	898.176106	14.272154
18.815522	905.706152	14.277171
18.989920	898.404834	14.282189
19.039635	887.400310	14.287207
19.227381	875.036381	14.292224
18.974778	878.925767	14.297242
18.441989	873.591088	14.302259
18.639097	869.382343	14.307277
18.297543	878.465363	14.312295
18.508555	890.692972	14.317312
18.691300	897.873910	14.322330
18.557780	900.387340	14.327347
18.898075	903.443153	14.332365
18.813332	902.748249	14.337383
18.904917	899.637239	14.342400
18.846135	895.672426	14.347418
18.515595	898.918451	14.352435
18.582645	911.438800	14.357453
18.536130	930.539116	14.362471
19.133784	927.776175	14.367488
19.121578	928.246375	14.372506
19.137738	929.462242	14.377523
19.563188	931.165038	14.382541
19.410688	932.753308	14.387559
19.569147	925.825074	14.392576
19.709160	926.737766	14.397594
19.435734	909.354319	14.402611
19.443460	898.774045	14.407629
18.917337	898.179392	14.412647
19.048596	893.683526	14.417664
19.325885	910.018504	14.422682
19.298073	923.920657	14.427699
19.477697	927.533373	14.432717
19.251406	931.132206	14.437735
19.332371	920.016189	14.442752
19.164064	925.286846	14.447770
19.149992	932.254337	14.452787
19.801754	924.431853	14.457805
19.323949	922.120212	14.462823
19.490726	928.919966	14.467840
19.669690	926.031874	14.472858
19.602924	922.834487	14.477875
19.832571	923.743754	14.482893
19.263010	924.649932	14.487911
19.579245	923.151258	14.492928
19.709959	921.715980	14.497946
19.684139	926.055994	14.502963
19.784928	917.938149	14.507981
19.612701	899.306117	14.512999
19.477975	896.942788	14.518016
19.726417	899.216993	14.523034
19.449086	913.442332	14.528051
19.669738	919.204463	14.533069
19.582246	926.184108	14.538087
19.660850	921.996941	14.543104
19.856321	919.951359	14.548122
19.780589	926.188536	14.553139
19.785865	921.874147	14.558157
19.858312	918.078536	14.563175
19.735193	920.630009	14.568192
20.003774	910.584855	14.573210
19.721260	914.310706	14.578227
19.783361	918.051537	14.583245
19.834345	910.710415	14.588263
19.503642	911.647511	14.593280
19.873138	918.019220	14.598298
19.612512	922.093795	14.603315
19.478462	915.674613	14.608333
19.940840	921.749853	14.613351
19.817957	917.880685	14.618368
19.880228	921.843133	14.623386
19.803228	934.947962	14.628403
20.005691	938.586425	14.633421
20.028564	945.272619	14.638439
19.943535	949.318518	14.643456
20.369266	943.417237	14.648474
20.083492	945.378350	14.653491
20.151956	942.192424	14.658509
20.164882	942.723815	14.663527
20.249114	945.648816	14.668544
20.185660	942.857947	14.673562
20.078908	939.761268	14.678579
20.043911	941.409606	14.683597
20.083283	943.044448	14.688615
20.270694	941.880871	14.693632
20.347754	945.299954	14.698650
20.487935	946.916923	14.703667
20.542509	938.444529	14.708685
20.349898	939.842992	14.713703
20.427914	942.293450	14.718720
20.505255	938.104913	14.723738
20.576695	934.718503	14.728755
20.566313	930.668505	14.733773
20.846809	950.129247	14.738791
20.937730	943.079516	14.743808
20.701840	941.270706	14.748826
20.477122	944.238204	14.753843
20.645317	941.072376	14.758861
20.320427	937.029575	14.763879
20.739123	947.055602	14.768896
20.931059	937.760889	14.773914
20.620423	934.940481	14.778931
20.643856	924.818987	14.783949
21.096466	930.537989	14.788967
20.682599	914.648992	14.793984
20.513740	904.157007	14.799002
20.481764	912.078988	14.804019
20.579294	924.379744	14.809037
20.771776	936.120319	14.814055
20.816864	936.915271	14.819072
20.987194	939.131554	14.824090
20.529604	938.103520	14.829107
20.976774	937.542968	14.834125
20.783717	933.871235	14.839143
20.820157	936.598644	14.844160
20.695480	935.126524	14.849178
20.340305	931.966262	14.854195
20.521875	940.930414	14.859213
20.858386	932.171584	14.864231
20.330248	939.890710	14.869248
21.031991	933.265409	14.874266
20.833796	940.730303	14.879283
20.977097	958.367390	14.884301
21.472150	967.444208	14.889319
20.574955	955.201997	14.894336
20.766387	958.640331	14.899354
21.070983	968.236070	14.904371
20.949889	971.708048	14.909389
20.977578	963.914870	14.914407
20.741277	973.421052	14.919424
21.319170	970.768064	14.924442
21.206015	970.190849	14.929459
21.365871	970.723501	14.934477
21.146957	968.885500	14.939495
21.097036	967.930898	14.944512
21.503708	952.770919	14.949530
21.257431	959.198549	14.954547
21.441594	965.192321	14.959565
21.558334	961.632662	14.964583
21.323089	971.133549	14.969600
21.546435	963.720556	14.974618
21.319134	969.324606	14.979635
21.028404	969.537003	14.984653
21.680699	960.757362	14.989671
21.594545	970.176476	14.994688
21.668167	960.134441	14.999706
21.301347	963.762849	15.004723
21.174164	965.130009	15.009741
21.539520	968.684029	15.014759
21.242682	961.871326	15.019776
21.672873	980.177834	15.024794
21.519420	989.270715	15.029811
21.512875	991.855651	15.034829
21.881503	994.441453	15.039847
21.780117	991.193094	15.044864
21.679802	988.076049	15.049882
21.910215	1001.394981	15.054899
22.138264	999.624298	15.059917
21.744345	980.316699	15.064935
21.544234	973.926540	15.069952
21.893113	982.179573	15.074970
21.947103	986.402848	15.079987
21.628665	977.048140	15.085005
21.659152	983.527979	15.090023
21.542972	993.119396	15.095040
22.171070	990.204557	15.100058
21.887644	984.773825	15.105075
21.989486	986.711308	15.110093
21.931819	980.736914	15.115111
22.174679	991.155853	15.120128
22.367755	979.976742	15.125146
22.170881	982.724683	15.130163
22.012915	989.558553	15.135181
22.116142	989.557295	15.140199
22.006685	988.483422	15.145216
22.351117	976.345427	15.150234
22.258598	980.087075	15.155251
22.220377	987.099139	15.160269
22.443359	977.526436	15.165287
22.022063	979.271814	15.170304
22.278546	982.932838	15.175322
22.388738	984.348091	15.180339
22.121314	978.450162	15.185357
22.768089	974.051580	15.190375
22.231699	961.389396	15.195392
22.348418	959.457238	15.200410
22.190151	947.117872	15.205427
21.974141	958.114326	15.210445
22.274348	973.246016	15.215463
22.413517	983.739991	15.220480
22.613704	976.787896	15.225498
22.277704	980.317115	15.230515
22.506046	991.508508	15.235533
22.556371	995.220206	15.240551
22.396169	992.514637	15.245568
22.671219	981.450687	15.250586
22.452249	987.676176	15.255603
22.474273	989.583178	15.260621
22.436523	981.199668	15.265639
22.376076	991.565291	15.270656
22.369074	985.744704	15.275674
22.326752	985.245126	15.280691
22.605835	988.179207	15.285709
22.500741	988.312835	15.290727
22.728359	992.782942	15.295744
22.705610	994.702870	15.300762
22.655049	1002.379165	15.305779
22.698701	1021.307188	15.310797
23.060365	1017.374688	15.315815
22.674377	1017.964263	15.320832
22.752553	1016.183358	15.325850
22.828463	1012.408409	15.330867
22.878687	1018.827516	15.335885
23.379394	1018.708868	15.340903
23.183660	1017.652822	15.345920
23.336307	1015.865491	15.350938
23.203171	1003.110122	15.355955
22.813643	997.572549	15.360973
22.692158	984.081434	15.365991
22.952448	995.541939	15.371008
22.822525	1009.356356	15.376026
23.217229	1000.525650	15.381043
22.931596	1020.459738	15.386061
23.103012	1008.426742	15.391079
23.050269	1016.694330	15.396096
23.141544	1011.823175	15.401114
23.182832	1013.588018	15.406131
22.704224	1016.308603	15.411149
22.929563	1012.741580	15.416167
23.046808	1016.397717	15.421184
22.943617	1012.850056	15.426202
23.205621	1028.576294	15.431219
22.980372	1041.759302	15.436237
23.510700	1038.413416	15.441255
23.188946	1032.642568	15.446272
23.602649	1028.221150	15.451290
23.810866	1023.147956	15.456307
23.411093	1035.365798	15.461325
23.633007	1033.957532	15.466343
23.682970	1036.462649	15.471360
23.449050	1039.483261	15.476378
23.685661	1035.116756	15.481395
23.548619	1036.576889	15.486413
23.812302	1026.779708	15.491431
23.717401	1029.820998	15.496448
23.671820	1025.960261	15.501466
24.036245	1029.656571	15.506483
23.626992	1017.616967	15.511501
23.781561	1012.597934	15.516519
23.738776	1001.468492	15.521536
23.847141	1004.058024	15.526554
23.763276	998.517080	15.531571
23.783146	1004.487286	15.536589
23.838727	1007.257994	15.541607
23.938599	1010.426471	15.546624
23.623552	997.046922	15.551642
23.803731	1011.794602	15.556659
23.834803	1020.100674	15.561677
24.011235	1021.695113	15.566695
24.092000	1027.800910	15.571712
24.011439	1025.552997	15.576730
24.196258	1025.769718	15.581747
23.682634	1025.366289	15.586765
24.279869	1018.796052	15.591783
24.030748	1025.217093	15.596800
23.918035	1024.606339	15.601818
23.923739	1026.026694	15.606835
23.744570	1031.470046	15.611853
23.979307	1029.465190	15.616871
23.900765	1028.784606	15.621888
23.696205	1034.877417	15.626906
24.267584	1024.234038	15.631923
24.054681	1033.871416	15.636941
24.113324	1027.215168	15.641959
24.212689	1037.855530	15.646976
24.108017	1054.104307	15.651994
24.765225	1050.347264	15.657011
24.356323	1067.616085	15.662029
24.198648	1061.559010	15.667047
24.260163	1058.690736	15.672064
24.404948	1059.559734	15.677082
24.325933	1054.170718	15.682099
24.236201	1059.913433	15.687117
24.568238	1052.518225	15.692135
24.373660	1049.868337	15.697152
24.328404	1056.527672	15.702170
24.550322	1048.729848	15.707187
24.532351	1059.050688	15.712205
24.694671	1045.321981	15.717223
24.684782	1047.707880	15.722240
24.392378	1054.595928	15.727258
24.491824	1053.942562	15.732275
24.113889	1054.934728	15.737293
24.699825	1077.296140	15.742311
24.674755	1079.541649	15.747328
24.786352	1078.510297	15.752346
25.305022	1070.494825	15.757363
25.124710	1071.443640	15.762381
25.220188	1065.472199	15.767399
25.139266	1049.885794	15.772416
25.016806	1043.134335	15.777434
25.229999	1042.493629	15.782451
24.951110	1051.247093	15.787469
24.839095	1036.011508	15.792487
25.243148	1041.270891	15.797504
25.073045	1041.273950	15.802522
25.050588	1037.326707	15.807539
24.973384	1035.895533	15.812557
25.480189	1035.164872	15.817575
25.587949	1038.353309	15.822592
25.245936	1043.164203	15.827610
25.416852	1033.966610	15.832627
25.587624	1041.266523	15.837645
25.359081	1039.486798	15.842663
25.514255	1039.139549	15.847680
25.299534	1043.709294	15.852698
25.517011	1037.055874	15.857715
25.525570	1033.672768	15.862733
25.354503	1029.232042	15.867751
25.441213	1022.342417	15.872768
25.225294	1020.587375	15.877786
25.496801	1027.185978	15.882803
25.383453	1032.961333	15.887821
25.366448	1031.285947	15.892839
25.448451	1036.954550	15.897856
25.608008	1038.105737	15.902874
25.784000	1027.123116	15.907891
25.638896	1025.155960	15.912909
25.425145	1031.127855	15.917927
25.661175	1027.005534	15.922944
25.345931	1037.538571	15.927962
25.650088	1023.554514	15.932979
25.556171	1035.158344	15.937997
25.441492	1024.117560	15.943015
25.770365	1030.457462	15.948032
25.253182	1033.204516	15.953050
25.263603	1025.722817	15.958067
25.292178	1039.250001	15.963085
25.485929	1042.532857	15.968103
25.645742	1057.659532	15.973120
25.635188	1074.776970	15.978138
25.971876	1065.605451	15.983155
25.763964	1071.984649	15.988173
25.991067	1070.377890	15.993191
25.999103	1059.967134	15.998208
25.921055	1071.305772	16.003226
26.075242	1066.548981	16.008243
25.831849	1066.842908	16.013261
26.002078	1066.826619	16.018279
25.792220	1071.685715	16.023296
25.936158	1071.925346	16.028314
26.036122	1062.350128	16.033331
25.741496	1080.582293	16.038349
26.072759	1079.789756	16.043367
26.357132	1095.943055	16.048384
26.218528	1092.903980	16.053402
26.510368	1095.669833	16.058419
26.344874	1094.593814	16.063437
26.491346	1100.410027	16.068455
26.775903	1091.549085	16.073472
26.138808	1095.639981	16.078490
26.593646	1089.388561	16.083507
26.552097	1092.025372	16.088525
26.743335	1091.137914	16.093543
26.756884	1061.840993	16.098560
26.253140	1065.925155	16.103578
26.374215	1060.271515	16.108595
26.512243	1064.359641	16.113613
26.918116	1079.792827	16.118631
26.980827	1068.251786	16.123648
26.615887	1064.866743	16.128666
26.557753	1060.074247	16.133683
26.553566	1071.853398	16.138701
26.428074	1078.312649	16.143719
26.843725	1084.995280	16.148736
26.438962	1092.634604	16.153754
26.630803	1087.005063	16.158771
26.769602	1093.755980	16.163789
26.810787	1091.846943	16.168807
27.015280	1088.432957	16.173824
26.770616	1093.682063	16.178842
26.924019	1091.870583	16.183859
26.977536	1093.781044	16.188877
26.889253	1085.995197	16.193895
27.051185	1086.262163	16.198912
26.830529	1099.022425	16.203930
26.897091	1088.189767	16.208947
26.646829	1085.321934	16.213965
27.146316	1088.025844	16.218983
27.225065	1089.689220	16.224000
27.435985	1086.750927	16.229018
27.082449	1086.831602	16.234035
27.017584	1094.952424	16.239053
26.739014	1091.886921	16.244071
27.165824	1080.225742	16.249088
26.920470	1112.534006	16.254106
27.649237	1108.093466	16.259123
27.311494	1109.301809	16.264141
27.172765	1106.132441	16.269159
27.498889	1119.673415	16.274176
27.306678	1115.029085	16.279194
27.679023	1107.054359	16.284211
27.750688	1110.673184	16.289229
27.333228	1123.025122	16.294247
27.605127	1113.874932	16.299264
27.440907	1117.887533	16.304282
27.548481	1110.347975	16.309299
27.779629	1108.202762	16.314317
27.458281	1112.177208	16.319335
27.476750	1106.067721	16.324352
27.411940	1112.507096	16.329370
27.786528	1112.626255	16.334387
27.821983	1112.538585	16.339405
27.543913	1106.478594	16.344423
27.994228	1107.404087	16.349440
27.730751	1114.982234	16.354458
27.853816	1101.845786	16.359475
27.736878	1105.876145	16.364493
27.436793	1107.160533	16.369511
27.749886	1105.655670	16.374528
27.516468	1109.502566	16.379546
27.778630	1122.606510	16.384563
28.110872	1128.954949	16.389581
28.069232	1142.103703	16.394599
28.257019	1139.106634	16.399616
28.276804	1144.726918	16.404634
28.220050	1132.418231	16.409651
28.066218	1121.488976	16.414669
27.997846	1124.229837	16.419687
28.205130	1140.528227	16.424704
28.365607	1135.341252	16.429722
28.376350	1127.531900	16.434739
28.621071	1128.760722	16.439757
28.503908	1127.706619	16.444775
28.453674	1102.325982	16.449792
28.464953	1099.927816	16.454810
28.507491	1088.469625	16.459827
28.328299	1090.111148	16.464845
28.567361	1095.924626	16.469863
28.416912	1090.562385	16.474880
28.377083	1096.497632	16.479898
28.338281	1091.141707	16.484915
28.512301	1104.535812	16.489933
28.276801	1113.451018	16.494951
28.727676	1115.606306	16.499968
28.327067	1125.085064	16.504986
28.485187	1129.055710	16.510003
28.779410	1124.226896	16.515021
28.612423	1129.078517	16.520039
28.704026	1126.587128	16.525056
28.663137	1124.073977	16.530074
28.965530	1129.688011	16.535091
29.043882	1127.484634	16.540109
28.589331	1130.596126	16.545127
29.300120	1126.277059	16.550144
29.169987	1132.902451	16.555162
29.024999	1126.605854	16.560179
29.123039	1124.575591	16.565197
28.833819	1126.789258	16.570215
28.909764	1123.604024	16.575232
29.015884	1135.504717	16.580250
29.109384	1129.022570	16.585267
29.135439	1120.036704	16.590285
28.874213	1125.956655	16.595303
28.947591	1120.755367	16.600320
29.134111	1131.011687	16.605338
28.991842	1126.341761	16.610355
29.207350	1127.147873	16.615373
28.866836	1120.261626	16.620391
28.943890	1128.323534	16.625408
28.907757	1123.072270	16.630426
29.011610	1142.716831	16.635443
29.399357	1145.086114	16.640461
29.360046	1156.300687	16.645479
29.716000	1152.261229	16.650496
29.292704	1149.349203	16.655514
28.962108	1152.330334	16.660531
29.332455	1153.294663	16.665549
29.452995	1147.974536	16.670567
29.510186	1151.022160	16.675584
29.380914	1147.565005	16.680602
29.217972	1148.204656	16.685619
29.688956	1150.855031	16.690637
29.488137	1160.526707	16.695655
29.963517	1162.901560	16.700672
29.760064	1167.625377	16.705690
30.015528	1175.562888	16.710707
30.022989	1154.372510	16.715725
29.752498	1147.038052	16.720743
29.962988	1146.671405	16.725760
29.681395	1145.466186	16.730778
29.617951	1164.358575	16.735795
29.919209	1168.661820	16.740813
29.947043	1175.014622	16.745831
30.096281	1176.008478	16.750848
30.041724	1171.700777	16.755866
29.991081	1173.432437	16.760883
30.290492	1170.640101	16.765901
30.199851	1172.010677	16.770919
30.238060	1169.345842	16.775936
30.108079	1170.793402	16.780954
30.063445	1175.709422	16.785971
30.466967	1168.544049	16.790989
30.132200	1170.979826	16.796007
30.351898	1169.269955	16.801024
30.883775	1168.558365	16.806042
30.246296	1172.249748	16.811059
30.612197	1169.102711	16.816077
30.471056	1169.104517	16.821095
30.629610	1168.590962	16.826112
30.603125	1171.543394	16.831130
30.200204	1175.101058	16.836147
30.642921	1169.675215	16.841165
29.999965	1177.676062	16.846183
30.413738	1168.545260	16.851200
30.658606	1169.078409	16.856218
30.181476	1172.720013	16.861235
30.691301	1167.276366	16.866253
30.402156	1174.478486	16.871271
30.618983	1165.310221	16.876288
30.665908	1159.654650	16.881306
30.502164	1165.017150	16.886323
30.942682	1170.106371	16.891341
30.891130	1180.714736	16.896359
31.053772	1182.306751	16.901376
30.957022	1171.226280	16.906394
30.800065	1175.882165	16.911411
31.068540	1174.640583	16.916429
30.673473	1174.277359	16.921447
30.866752	1173.496643	16.926464
31.409259	1169.928639	16.931482
30.979105	1173.730177	16.936499
31.016357	1174.272115	16.941517
31.182599	1168.494425	16.946535
31.332270	1171.863740	16.951552
31.458547	1171.899610	16.956570
31.164546	1182.787093	16.961587
31.182938	1176.474052	16.966605
30.969614	1175.724050	16.971623
30.877959	1178.947898	16.976640
31.124285	1174.400221	16.981658
31.139876	1179.513351	16.986675
31.200116	1170.759584	16.991693
31.294083	1179.850189	16.996711
31.042776	1190.685727	17.001728
31.527073	1198.390088	17.006746
31.365285	1205.576251	17.011763
31.468226	1204.420343	17.016781
31.333834	1207.123333	17.021799
31.417624	1210.566556	17.026816
31.661618	1198.221009	17.031834
31.571265	1210.963724	17.036851
31.846806	1199.177506	17.041869
31.623492	1204.784130	17.046887
31.702412	1206.829766	17.051904
31.604330	1203.832383	17.056922
31.775826	1205.415849	17.061939
31.885340	1199.887692	17.066957
31.976305	1203.632081	17.071975
31.914885	1211.637436	17.076992
32.213295	1210.208221	17.082010
32.223561	1209.503869	17.087027
32.041717	1201.751566	17.092045
31.835650	1201.495231	17.097063
32.082604	1218.020988	17.102080
32.290642	1221.055460	17.107098
32.378107	1231.699894	17.112115
32.417829	1216.050432	17.117133
32.058732	1204.113397	17.122151
32.240591	1204.041641	17.127168
32.400240	1212.404083	17.132186
32.445668	1214.761557	17.137203
32.610826	1203.765645	17.142221
32.446180	1202.194213	17.147239
32.131807	1200.535372	17.152256
32.488731	1202.855439	17.157274
32.172754	1210.969084	17.162291
32.566091	1213.657524	17.167309
32.803242	1213.758105	17.172327
32.538833	1212.522082	17.177344
32.934568	1214.132196	17.182362
32.824957	1217.908226	17.187379
32.955350	1204.846854	17.192397
32.740068	1195.727287	17.197415
32.585724	1189.238518	17.202432
32.477151	1195.911153	17.207450
32.774524	1207.866058	17.212467
32.940282	1210.484704	17.217485
32.947523	1213.246524	17.222503
32.621543	1207.788113	17.227520
33.010178	1219.038167	17.232538
32.718344	1219.616882	17.237555
33.008326	1225.851496	17.242573
32.883759	1222.923061	17.247591
32.961127	1214.393594	17.252608
32.989495	1203.817960	17.257626
33.302356	1217.043508	17.262643
33.447441	1209.650837	17.267661
33.124588	1216.210540	17.272679
33.304285	1219.094983	17.277696
33.183080	1203.890675	17.282714
33.059592	1218.956941	17.287731
33.136941	1216.041922	17.292749
33.267985	1214.760496	17.297767
32.998785	1212.485132	17.302784
33.110835	1213.489872	17.307802
32.980565	1214.412693	17.312819
32.977209	1228.604764	17.317837
33.404408	1236.806383	17.322855
33.572728	1243.522952	17.327872
33.449142	1234.638567	17.332890
33.817792	1254.467766	17.337907
33.426153	1245.230524	17.342925
33.576659	1246.700149	17.347943
33.506652	1243.774486	17.352960
33.667377	1235.028453	17.357978
33.234462	1243.004789	17.362995
33.564997	1236.794759	17.368013
34.133528	1232.271271	17.373031
33.813218	1240.082112	17.378048
34.133752	1238.173257	17.383066
33.725284	1239.751187	17.388083
33.747727	1245.495081	17.393101
34.193194	1247.726479	17.398119
33.911475	1258.511195	17.403136
34.140862	1238.936678	17.408154
33.903822	1249.056523	17.413171
33.926581	1253.684248	17.418189
34.790163	1263.353752	17.423207
34.311267	1258.961569	17.428224
34.388694	1239.808662	17.433242
34.304248	1240.886491	17.438259
34.339982	1237.185856	17.443277
34.424539	1227.180024	17.448295
34.481302	1236.145330	17.453312
34.406554	1231.465766	17.458330
34.451574	1228.219097	17.463347
34.084893	1239.896197	17.468365
34.152656	1237.301260	17.473383
34.104414	1250.713792	17.478400
34.731538	1257.165816	17.483418
34.571396	1262.171067	17.488435
34.355847	1266.700857	17.493453
34.939396	1268.952306	17.498471
34.598113	1269.756530	17.503488
34.544260	1264.219969	17.508506
34.643511	1260.680067	17.513523
34.419790	1267.216684	17.518541
34.788637	1265.363998	17.523559
34.582825	1262.640343	17.528576
34.773139	1255.986604	17.533594
35.091245	1271.804193	17.538611
34.957173	1265.558487	17.543629
34.863369	1260.864748	17.548647
34.774682	1282.731090	17.553664
34.806755	1286.652177	17.558682
34.924386	1283.031669	17.563699
35.015677	1279.102931	17.568717
35.491393	1277.960487	17.573735
35.268179	1282.930914	17.578752
35.461626	1283.819033	17.583770
35.498522	1285.061809	17.588787
35.177230	1278.875837	17.593805
35.416416	1273.184453	17.598823
35.212494	1276.214710	17.603840
35.500121	1278.843502	17.608858
35.798043	1284.707147	17.613875
35.660227	1281.738769	17.618893
35.770174	1274.920379	17.623911
35.449728	1250.694851	17.628928
35.723239	1253.643687	17.633946
35.526685	1248.064226	17.638963
35.570323	1266.062648	17.643981
36.028051	1269.674671	17.648999
35.863293	1278.959747	17.654016
35.778249	1252.851963	17.659034
35.657335	1255.558241	17.664051
36.110144	1256.886474	17.669069
35.440459	1256.359274	17.674087
35.544449	1271.972166	17.679104
35.869618	1281.080451	17.684122
35.899600	1281.307461	17.689139
36.024538	1280.662857	17.694157
35.981431	1281.346842	17.699175
35.914896	1283.055949	17.704192
36.095051	1276.313727	17.709210
35.858898	1280.777249	17.714227
36.015905	1284.050494	17.719245
36.289357	1273.366122	17.724263
36.127511	1278.717717	17.729280
36.178506	1275.675951	17.734298
36.109089	1275.526513	17.739315
35.864697	1273.480492	17.744333
36.254286	1293.192102	17.749351
36.057295	1303.593929	17.754368
36.320659	1309.151500	17.759386
36.041722	1307.576935	17.764403
36.536566	1308.579713	17.769421
36.616941	1297.250928	17.774439
36.484753	1303.310601	17.779456
36.785963	1299.886459	17.784474
36.707254	1297.056714	17.789491
36.523663	1303.435129	17.794509
36.557149	1301.065931	17.799527
36.653152	1301.331615	17.804544
36.628304	1294.459159	17.809562
36.896257	1301.843496	17.814579
36.770042	1305.397497	17.819597
36.852718	1311.011759	17.824615
37.092224	1332.450212	17.829632
37.011407	1336.006152	17.834650
37.053155	1323.993202	17.839667
37.034258	1333.002193	17.844685
37.126719	1334.165301	17.849703
36.776532	1343.984262	17.854720
37.053058	1331.037168	17.859738
37.111529	1337.257014	17.864755
37.068199	1339.076456	17.869773
37.499921	1331.025644	17.874791
36.983302	1339.566667	17.879808
36.920436	1328.693462	17.884826
37.423521	1330.939348	17.889843
37.352635	1325.194171	17.894861
37.444553	1328.775049	17.899879
37.495614	1331.697742	17.904896
37.696774	1330.639340	17.909914
37.702714	1330.905763	17.914931
37.470604	1331.634039	17.919949
37.660410	1327.828344	17.924967
37.585194	1335.186844	17.929984
37.275817	1335.680279	17.935002
37.552028	1328.797328	17.940019
37.639167	1348.079568	17.945037
38.039846	1352.910491	17.950055
38.362372	1357.570893	17.955072
37.924988	1336.551167	17.960090
37.856886	1324.831993	17.965107
37.698997	1322.589754	17.970125
38.206227	1339.306792	17.975143
38.012403	1340.917693	17.980160
38.297771	1344.262215	17.985178
37.986322	1333.208910	17.990195
37.751398	1337.881297	17.995213
38.327800	1338.530814	18.000231
38.549633	1348.125929	18.005248
38.509086	1343.016658	18.010266
38.520026	1335.387088	18.015283
38.185352	1328.559621	18.020301
38.543044	1322.712771	18.025319
38.289511	1323.659945	18.030336
38.497282	1324.077198	18.035354
38.824370	1338.585514	18.040371
38.382505	1331.375013	18.045389
38.273741	1321.253890	18.050407
38.386930	1335.701167	18.055424
38.426820	1343.579186	18.060442
38.460839	1337.850492	18.065459
38.585245	1340.886237	18.070477
38.582058	1333.913329	18.075495
38.616451	1338.311597	18.080512
38.467689	1341.391000	18.085530
38.650868	1342.201690	18.090547
38.657812	1343.021089	18.095565
38.668221	1350.400851	18.100583
38.994966	1366.227737	18.105600
38.765496	1365.029223	18.110618
39.009159	1371.713686	18.115635
39.171583	1373.807328	18.120653
39.262651	1371.656141	18.125671
39.245144	1374.888224	18.130688
39.024530	1373.996507	18.135706
39.460712	1374.675149	18.140723
39.039853	1369.789077	18.145741
39.434257	1353.967362	18.150759
39.177457	1368.320423	18.155776
39.180006	1356.008431	18.160794
39.399251	1358.035969	18.165811
39.329245	1373.619507	18.170829
39.316888	1366.974476	18.175847
39.496159	1364.130741	18.180864
39.395214	1368.017969	18.185882
39.613703	1372.467259	18.190899
39.731483	1380.598145	18.195917
40.103217	1380.134323	18.200935
40.085223	1369.419798	18.205952
39.689658	1360.204003	18.210970
40.047434	1355.350815	18.215987
39.801778	1358.244299	18.221005
39.978749	1349.151028	18.226023
39.919022	1348.362198	18.231040
39.739987	1357.248903	18.236058
39.897659	1353.774896	18.241075
39.772431	1374.024999	18.246093
40.176124	1380.521159	18.251111
40.251056	1383.985967	18.256128
40.348713	1389.089514	18.261146
40.472309	1381.703863	18.266163
39.974161	1369.907439	18.271181
40.480239	1372.101261	18.276199
40.325136	1380.477723	18.281216
40.314541	1373.076895	18.286234
40.678480	1381.074503	18.291251
40.411610	1378.282985	18.296269
40.489938	1371.334357	18.301287
40.078588	1378.053268	18.306304
40.304665	1379.307246	18.311322
40.560270	1372.848942	18.316339
40.340948	1383.403337	18.321357
40.386085	1373.597244	18.326375
40.820699	1373.464738	18.331392
40.734532	1386.880912	18.336410
40.936926	1376.297605	18.341427
40.905280	1377.969843	18.346445
40.738646	1374.768426	18.351463
40.772826	1382.681662	18.356480
40.623851	1379.378109	18.361498
40.790030	1368.283487	18.366515
40.840709	1387.587168	18.371533
41.094710	1400.000581	18.376551
41.364370	1400.818608	18.381568
41.190818	1416.557916	18.386586
41.667988	1408.610955	18.391603
40.890974	1398.456338	18.396621
40.746401	1400.134679	18.401639
40.716007	1398.793357	18.406656
41.037841	1401.318476	18.411674
41.313537	1407.833480	18.416691
41.415018	1411.294291	18.421709
41.218011	1404.954226	18.426727
41.470849	1405.564017	18.431744
41.696805	1411.790805	18.436762
41.663552	1411.907816	18.441779
41.328617	1411.692106	18.446797
41.879353	1428.263849	18.451815
42.145012	1431.156146	18.456832
41.489042	1423.220035	18.461850
42.103484	1421.633750	18.466867
41.851190	1413.034745	18.471885
42.154468	1419.098734	18.476903
41.967697	1407.782214	18.481920
41.701987	1412.966015	18.486938
41.781043	1414.652604	18.491955
42.215589	1418.938180	18.496973
42.359022	1422.197955	18.501991
42.503781	1425.046490	18.507008
42.085744	1415.873358	18.512026
42.381493	1408.288324	18.517043
42.306758	1421.938066	18.522061
42.375689	1421.887764	18.527079
42.476391	1416.953111	18.532096
42.572256	1411.366510	18.537114
42.531806	1396.850208	18.542131
42.491781	1404.354881	18.547149
42.249733	1397.945111	18.552167
42.290895	1412.835879	18.557184
42.225195	1416.946415	18.562202
42.426958	1410.035598	18.567219
42.373449	1414.985840	18.572237
42.282379	1425.774536	18.577255
42.641854	1415.164406	18.582272
42.686303	1414.222497	18.587290
42.551367	1407.360740	18.592307
42.382393	1425.738250	18.597325
42.619840	1441.530394	18.602343
42.898133	1449.383165	18.607360
43.002435	1449.208897	18.612378
43.241219	1441.429344	18.617395
43.128043	1437.191511	18.622413
43.273368	1448.758397	18.627431
43.275100	1446.622386	18.632448
42.829630	1445.175381	18.637466
43.148185	1439.107411	18.642483
43.556554	1446.831164	18.647501
43.574561	1437.911405	18.652519
43.529657	1432.058344	18.657536
43.386161	1450.614734	18.662554
43.470636	1441.218617	18.667571
43.411137	1442.636421	18.672589
43.476725	1438.075683	18.677607
43.445073	1432.414126	18.682624
43.628866	1434.218413	18.687642
43.404888	1440.488612	18.692659
43.591165	1442.838547	18.697677
43.393194	1435.081316	18.702695
44.038188	1434.620277	18.707712
43.553018	1442.086866	18.712730
43.845034	1450.695628	18.717747
44.113475	1465.019682	18.722765
43.808895	1464.451309	18.727783
44.055512	1458.371227	18.732800
44.046752	1471.653398	18.737818
44.359226	1463.631712	18.742835
43.644241	1453.484111	18.747853
43.875333	1459.594321	18.752871
44.644058	1457.127766	18.757888
44.234168	1458.427213	18.762906
44.429049	1456.519847	18.767923
44.663903	1452.303910	18.772941
44.365343	1464.000212	18.777959
44.412122	1452.187116	18.782976
44.257856	1462.481975	18.787994
44.636179	1458.274563	18.793011
44.359813	1453.581466	18.798029
44.029415	1457.495293	18.803047
44.403034	1458.339416	18.808064
44.528031	1465.435300	18.813082
44.420945	1476.547154	18.818099
44.820687	1477.713724	18.823117
44.686762	1492.303245	18.828135
44.923485	1486.851954	18.833152
44.526373	1481.398924	18.838170
45.093025	1483.766591	18.843187
44.979360	1488.088631	18.848205
45.013927	1486.957409	18.853223
45.125032	1479.189530	18.858240
44.898847	1495.027395	18.863258
45.236267	1485.599998	18.868275
45.154569	1484.899050	18.873293
44.907476	1480.223539	18.878311
45.192534	1487.567338	18.883328
45.293599	1503.950630	18.888346
45.395053	1505.859109	18.893363
45.694201	1515.955699	18.898381
45.515384	1506.468099	18.903399
45.841932	1506.812935	18.908416
45.855213	1510.639947	18.913434
45.815229	1509.781304	18.918451
45.483213	1504.650950	18.923469
45.358738	1506.038180	18.928487
45.884125	1500.226883	18.933504
45.645653	1502.916843	18.938522
45.963994	1506.598853	18.943539
46.077022	1502.622365	18.948557
45.526324	1503.865603	18.953575
45.671092	1500.798424	18.958592
46.164648	1494.377441	18.963610
45.905715	1498.539680	18.968627
46.024573	1498.340560	18.973645
45.985706	1504.407693	18.978663
46.200074	1492.131386	18.983680
45.936404	1500.917620	18.988698
46.091065	1509.835378	18.993715
46.181277	1510.263047	18.998733
45.852398	1519.691977	19.003751
46.007490	1522.529764	19.008768
45.997115	1524.371724	19.013786
46.201787	1523.115090	19.018803
46.699325	1534.443800	19.023821
46.322819	1530.643244	19.028839
46.488337	1541.466306	19.033856
46.414512	1548.946724	19.038874
46.541529	1555.058457	19.043891
46.762526	1550.774708	19.048909
47.018080	1557.338387	19.053927
47.224008	1552.583905	19.058944
47.419474	1551.710683	19.063962
46.996751	1553.768955	19.068979
47.119491	1548.805019	19.073997
46.749914	1552.698979	19.079015
47.343928	1546.341263	19.084032
47.491571	1557.753910	19.089050
47.333497	1553.703794	19.094067
47.585480	1539.981063	19.099085
47.287308	1546.135243	19.104103
47.791321	1550.371953	19.109120
47.540801	1546.253288	19.114138
47.613744	1545.394054	19.119155
47.792310	1543.472451	19.124173
47.650424	1531.653919	19.129191
47.481017	1512.852569	19.134208
47.438524	1519.465976	19.139226
47.245107	1529.382717	19.144243
47.431018	1534.367369	19.149261
47.738508	1549.388972	19.154279
47.954012	1530.923866	19.159296
47.619323	1540.212826	19.164314
47.673866	1544.249549	19.169331
47.703491	1538.954972	19.174349
47.666888	1542.548519	19.179367
47.972758	1556.512917	19.184384
48.102001	1570.428228	19.189402
48.313118	1566.432726	19.194419
48.446229	1564.431638	19.199437
48.369179	1571.369687	19.204455
48.557701	1562.824379	19.209472
48.765183	1559.708615	19.214490
48.150299	1550.611697	19.219507
48.730447	1551.543282	19.224525
48.050969	1554.606666	19.229543
48.442676	1554.552525	19.234560
48.333001	1559.209750	19.239578
48.393263	1564.477816	19.244595
48.395044	1557.318157	19.249613
48.498344	1562.338938	19.254631
48.405036	1561.669436	19.259648
48.856804	1559.517948	19.264666
48.845564	1562.033678	19.269683
48.871285	1546.213759	19.274701
48.723699	1558.512299	19.279719
49.068181	1571.596301	19.284736
49.216118	1580.332536	19.289754
49.280010	1579.141728	19.294771
48.978356	1558.484265	19.299789
49.101791	1567.952109	19.304807
49.205986	1573.053848	19.309824
49.426892	1573.860666	19.314842
49.542348	1582.648737	19.319859
49.637559	1578.218880	19.324877
49.437598	1579.532394	19.329895
49.414672	1576.449266	19.334912
49.600139	1569.820999	19.339930
49.553606	1567.391388	19.344947
49.747887	1571.988052	19.349965
49.525512	1570.870629	19.354983
49.551211	1568.013703	19.360000
49.548515	1570.511878	19.365018
49.318543	1576.116587	19.370035
49.472923	1566.471024	19.375053
49.586548	1573.724353	19.380071
49.974828	1587.806236	19.385088
50.010563	1599.750044	19.390106
49.692957	1604.378720	19.395123
50.129928	1606.616304	19.400141
49.953752	1600.780585	19.405159
50.223252	1604.895511	19.410176
50.155865	1601.182336	19.415194
50.291847	1604.250469	19.420211
50.389144	1594.904104	19.425229
50.448865	1601.152589	19.430247
50.504340	1587.976528	19.435264
50.516369	1601.203006	19.440282
50.283529	1604.606619	19.445299
50.520491	1598.326113	19.450317
50.661174	1602.572211	19.455335
50.711803	1595.462321	19.460352
50.614857	1608.123775	19.465370
50.698195	1624.876667	19.470387
50.685863	1628.406373	19.475405
50.495873	1630.411945	19.480423
50.258782	1620.944554	19.485440
50.724802	1625.458444	19.490458
50.882548	1628.751719	19.495475
51.304733	1633.604761	19.500493
51.383883	1644.572905	19.505511
51.256844	1632.280576	19.510528
51.425148	1622.290151	19.515546
51.330397	1637.052850	19.520563
51.704774	1637.251581	19.525581
51.475205	1624.842769	19.530599
51.138177	1618.351783	19.535616
51.699798	1633.484933	19.540634
51.690900	1646.018059	19.545651
51.866810	1643.657904	19.550669
51.657313	1648.721451	19.555687
51.878342	1647.271547	19.560704
52.335306	1639.177815	19.565722
51.768225	1626.107560	19.570739
51.915295	1614.293089	19.575757
51.798278	1619.535802	19.580775
52.144739	1619.574981	19.585792
51.975782	1616.684135	19.590810
51.987474	1645.106837	19.595827
52.118405	1634.281249	19.600845
51.930648	1649.661332	19.605863
52.237746	1645.975116	19.610880
52.177086	1640.048993	19.615898
51.903743	1651.027477	19.620915
52.071717	1645.529640	19.625933
52.215560	1649.139003	19.630951
52.201593	1643.654364	19.635968
52.412171	1638.727037	19.640986
52.246858	1652.979779	19.646003
52.707644	1651.068126	19.651021
52.874400	1668.005284	19.656039
52.916801	1669.691277	19.661056
52.911822	1651.546790	19.666074
52.747855	1659.769357	19.671091
52.874270	1662.970189	19.676109
53.103884	1655.379451	19.681127
53.167863	1655.655955	19.686144
53.358600	1661.957575	19.691162
52.738190	1646.204777	19.696179
53.324223	1649.258242	19.701197
53.440273	1648.372574	19.706215
53.085678	1661.467681	19.711232
53.445347	1648.523092	19.716250
53.251256	1655.780167	19.721267
53.370781	1651.543902	19.726285
53.642496	1656.300605	19.731303
53.410784	1653.041795	19.736320
53.810304	1653.937941	19.741338
53.489573	1661.214412	19.746355
53.793364	1644.346769	19.751373
53.776222	1653.089906	19.756391
53.389680	1651.063040	19.761408
53.972580	1648.171713	19.766426
53.736981	1654.151793	19.771443
53.951926	1652.347776	19.776461
53.411677	1644.744358	19.781479
53.771984	1661.957732	19.786496
53.852426	1673.044975	19.791514
53.623954	1680.836498	19.796531
54.107070	1681.649119	19.801549
54.096764	1679.077665	19.806567
53.853320	1678.907824	19.811584
54.181717	1681.422849	19.816602
54.255308	1693.951804	19.821619
54.067308	1701.076788	19.826637
54.446038	1706.340595	19.831655
54.663333	1713.905961	19.836672
54.608564	1707.512298	19.841690
54.936374	1706.451011	19.846707
54.906394	1704.956048	19.851725
54.796497	1700.684528	19.856743
54.897150	1708.444404	19.861760
55.136807	1700.166147	19.866778
54.720608	1699.333566	19.871795
55.049717	1700.134681	19.876813
54.880075	1698.277013	19.881831
55.150897	1697.846035	19.886848
55.329129	1694.846900	19.891866
55.065520	1690.112247	19.896883
55.114466	1695.929086	19.901901
55.242298	1694.432010	19.906919
55.244500	1714.407517	19.911936
55.224166	1714.420028	19.916954
55.581856	1728.740966	19.921971
55.693690	1723.550432	19.926989
55.653872	1724.671299	19.932007
55.602786	1731.373228	19.937024
56.210481	1721.253292	19.942042
55.755546	1725.155915	19.947059
55.881980	1723.863401	19.952077
55.800686	1715.200086	19.957095
55.705481	1726.337711	19.962112
55.709029	1724.004115	19.967130
56.022564	1726.855470	19.972147
56.031387	1722.115462	19.977165
56.238127	1712.156018	19.982183
56.097583	1717.128247	19.987200
56.298112	1714.982511	19.992218
56.114377	1719.313855	19.997235
56.041683	1719.008653	20.002253
56.389070	1713.508645	20.007271
56.264446	1715.108912	20.012288
56.656716	1730.033188	20.017306
56.677538	1739.355133	20.022323
56.442431	1745.544225	20.027341
56.744369	1737.237920	20.032359
56.521625	1741.293048	20.037376
56.814615	1740.159964	20.042394
56.888418	1739.282074	20.047411
56.423777	1740.650451	20.052429
57.146522	1735.628448	20.057447
56.602211	1739.908475	20.062464
57.036451	1742.800478	20.067482
56.756100	1749.541951	20.072499
57.009942	1758.881232	20.077517
57.307994	1769.393135	20.082535
57.101886	1767.237163	20.087552
57.721449	1770.587862	20.092570
57.609472	1776.807366	20.097587
57.173928	1771.916508	20.102605
57.597843	1753.582380	20.107623
57.064652	1768.467014	20.112640
57.246237	1768.051203	20.117658
57.138220	1773.380275	20.122675
57.785915	1788.378063	20.127693
58.085244	1795.361767	20.132711
57.961514	1800.713529	20.137728
58.231562	1803.218156	20.142746
57.968528	1794.892374	20.147763
57.791340	1790.576852	20.152781
58.239146	1791.434697	20.157799
58.407586	1781.407926	20.162816
58.218053	1787.496967	20.167834
58.279273	1785.890438	20.172851
58.491643	1785.443151	20.177869
58.824185	1778.818396	20.182887
58.398389	1781.500049	20.187904
58.797374	1782.745510	20.192922
58.648058	1780.732497	20.197939
58.242226	1788.123119	20.202957
58.907617	1780.306226	20.207975
58.559782	1792.719998	20.212992
58.796591	1779.505088	20.218010
58.913664	1780.109029	20.223027
58.527264	1779.923093	20.228045
58.866683	1777.086232	20.233063
58.363149	1795.394377	20.238080
59.048677	1800.963329	20.243098
59.436673	1812.955275	20.248115
59.375847	1809.192538	20.253133
59.433164	1806.476792	20.258151
59.289402	1812.488971	20.263168
59.474373	1809.182788	20.268186
59.372894	1813.062735	20.273203
58.989556	1811.269965	20.278221
59.269494	1808.050421	20.283239
59.122542	1815.703708	20.288256
59.481381	1811.537619	20.293274
59.701721	1817.691091	20.298291
59.613187	1823.825235	20.303309
59.565859	1829.300579	20.308327
59.829662	1825.149828	20.313344
59.869691	1821.652676	20.318362
59.881404	1820.037412	20.323379
60.042373	1823.087671	20.328397
60.262156	1819.871392	20.333415
60.039945	1820.080718	20.338432
60.080532	1814.780295	20.343450
60.254994	1813.190840	20.348467
60.119761	1822.560329	20.353485
60.272339	1823.162330	20.358503
60.415393	1844.898179	20.363520
60.463325	1845.388765	20.368538
60.569740	1850.010691	20.373555
60.478838	1855.901534	20.378573
60.823068	1836.362763	20.383591
60.705073	1849.622005	20.388608
60.885719	1844.570828	20.393626
61.007128	1842.275968	20.398643
60.880749	1847.488811	20.403661
60.928803	1838.058720	20.408679
60.614931	1840.669487	20.413696
60.662328	1853.304879	20.418714
61.287142	1866.437993	20.423731
61.099230	1865.117199	20.428749
61.489997	1873.875993	20.433767
61.116582	1881.303024	20.438784
61.242099	1874.062494	20.443802
61.461867	1865.284284	20.448819
61.275905	1872.501135	20.453837
61.581248	1866.391487	20.458855
61.712004	1873.400777	20.463872
62.203531	1877.146724	20.468890
62.435177	1867.932284	20.473907
62.032782	1863.398120	20.478925
62.524606	1854.882749	20.483943
62.423177	1855.332711	20.488960
62.486176	1849.915965	20.493978
62.260531	1847.023831	20.498995
62.248821	1859.028846	20.504013
62.456284	1849.581408	20.509031
62.358959	1846.527081	20.514048
62.376213	1842.261634	20.519066
62.652740	1843.579740	20.524083
62.364784	1846.027159	20.529101
62.692923	1852.629734	20.534119
62.682504	1846.715687	20.539136
62.940051	1852.210244	20.544154
62.899118	1839.216078	20.549171
62.879634	1846.078181	20.554189
62.813960	1851.575468	20.559207
62.987090	1846.101905	20.564224
63.003317	1845.786702	20.569242
63.086821	1844.419001	20.574259
62.870861	1844.091061	20.579277
63.087940	1832.844764	20.584295
63.292863	1858.055884	20.589312
63.172118	1874.522753	20.594330
63.355032	1872.262587	20.599347
63.590090	1885.494505	20.604365
63.447302	1888.589562	20.609383
63.496187	1889.235901	20.614400
63.149651	1875.564337	20.619418
63.418808	1876.239952	20.624435
63.173882	1877.177463	20.629453
63.305082	1878.888148	20.634471
63.335228	1895.154853	20.639488
63.355846	1903.990701	20.644506
63.822781	1907.651355	20.649523
63.295306	1905.228094	20.654541
63.713917	1918.256809	20.659559
64.119705	1928.528930	20.664576
63.939578	1928.497425	20.669594
64.255091	1937.473838	20.674611
64.078704	1931.296681	20.679629
63.768441	1923.801109	20.684647
63.736617	1938.027678	20.689664
64.222356	1940.816701	20.694682
64.390928	1944.963786	20.699699
64.586535	1960.508264	20.704717
65.149309	1955.126055	20.709735
64.820810	1957.379411	20.714752
65.000292	1958.726195	20.719770
65.517984	1948.702908	20.724787
65.339721	1950.155383	20.729805
65.707703	1952.906425	20.734823
65.341619	1946.977212	20.739840
65.179146	1952.439773	20.744858
65.523613	1940.058105	20.749875
65.356604	1942.337477	20.754893
65.671138	1935.082551	20.759911
65.769305	1942.149238	20.764928
65.805656	1944.386670	20.769946
65.959372	1937.365857	20.774963
66.024031	1925.764406	20.779981
66.231813	1903.868164	20.784999
65.678106	1906.857637	20.790016
65.607640	1908.918258	20.795034
65.814625	1897.966899	20.800051
65.770498	1922.054374	20.805069
65.975510	1929.895509	20.810087
65.838664	1928.454047	20.815104
65.865595	1938.418817	20.820122
66.110041	1934.080294	20.825139
65.665772	1936.309901	20.830157
65.909827	1942.939824	20.835175
66.001042	1962.615078	20.840192
65.964379	1959.590843	20.845210
66.580558	1965.085904	20.850227
66.333989	1977.125565	20.855245
66.757395	1969.493138	20.860263
66.548982	1970.014362	20.865280
66.436237	1989.521448	20.870298
66.668314	1986.364912	20.875315
66.580496	2003.381598	20.880333
66.722632	2000.977769	20.885351
67.018378	1993.938531	20.890368
66.945461	2000.510329	20.895386
67.114567	2003.693927	20.900403
67.193301	2019.614125	20.905421
67.324291	2019.411417	20.910439
67.577037	2017.665274	20.915456
67.387620	2014.943494	20.920474
67.706879	2010.592168	20.925491
67.723488	2006.825223	20.930509
67.779715	2006.883720	20.935527
67.833858	2004.193269	20.940544
68.128688	2017.063030	20.945562
68.338888	2003.638157	20.950579
67.906182	2010.688441	20.955597
68.056204	2003.041026	20.960615
68.161236	2002.740644	20.965632
67.947840	1998.836189	20.970650
68.474274	2001.760222	20.975667
67.956391	2010.162050	20.980685
68.132330	2005.388379	20.985703
68.091939	2000.828488	20.990720
67.973488	2005.833766	20.995738
68.302709	2013.207514	21.000755
68.295761	2033.002264	21.005773
68.525238	2032.991916	21.010791
68.717783	2033.548330	21.015808
68.730969	2031.615467	21.020826
68.657673	2028.703192	21.025843
68.660534	2032.039523	21.030861
68.746365	2030.024157	21.035879
69.250151	2047.951235	21.040896
69.005060	2062.855377	21.045914
69.372728	2060.348051	21.050931
69.213246	2063.189205	21.055949
69.182010	2056.887960	21.060967
69.266993	2056.159387	21.065984
69.023154	2065.493853	21.071002
69.603870	2062.481551	21.076019
69.436441	2061.719179	21.081037
69.575347	2058.144577	21.086055
69.927759	2074.923090	21.091072
69.994871	2071.579671	21.096090
70.272214	2075.671772	21.101107
70.073663	2073.057009	21.106125
70.122878	2073.045405	21.111143
70.596094	2071.209207	21.116160
70.603435	2068.395782	21.121178
70.819329	2049.221705	21.126195
70.574383	2045.864211	21.131213
70.500487	2041.785067	21.136231
70.509279	2044.115662	21.141248
70.142530	2038.221958	21.146266
70.449990	2046.327694	21.151283
70.788370	2057.391796	21.156301
70.572929	2058.496489	21.161319
70.884304	2066.418116	21.166336
70.582460	2075.519665	21.171354
70.657372	2067.382276	21.176371
70.603351	2071.181198	21.181389
70.644928	2068.056188	21.186407
71.182224	2083.747371	21.191424
70.960115	2089.208437	21.196442
71.225119	2094.598300	21.201459
71.486989	2108.090151	21.206477
71.210662	2104.227586	21.211495
71.289310	2102.243716	21.216512
71.656676	2093.017696	21.221530
71.739809	2093.815859	21.226547
71.604319	2089.513821	21.231565
71.632888	2096.839749	21.236583
72.298402	2115.253925	21.241600
72.030418	2115.191294	21.246618
72.065133	2115.600216	21.251635
72.104607	2115.183123	21.256653
72.255739	2114.639665	21.261671
72.639727	2108.964949	21.266688
72.224122	2121.694545	21.271706
72.529393	2112.370523	21.276723
72.541844	2105.806898	21.281741
72.677512	2114.486803	21.286759
72.843986	2107.938227	21.291776
72.558841	2105.461423	21.296794
72.723928	2102.610061	21.301811
72.767520	2109.203560	21.306829
72.567627	2104.785799	21.311847
72.904181	2097.391715	21.316864
72.752300	2107.069260	21.321882
72.676222	2101.344340	21.326899
72.949340	2106.896649	21.331917
72.828777	2121.003034	21.336935
73.092572	2132.698854	21.341952
73.066067	2132.638761	21.346970
73.395838	2132.808665	21.351987
73.496220	2136.367463	21.357005
73.531035	2135.666485	21.362023
73.545416	2134.638564	21.367040
73.517195	2137.657611	21.372058
73.730110	2132.102554	21.377075
73.710630	2139.756154	21.382093
73.669008	2151.904148	21.387111
73.818719	2148.247812	21.392128
74.105486	2158.983512	21.397146
74.226866	2160.898618	21.402163
74.043567	2154.003590	21.407181
73.786381	2163.276542	21.412199
73.994671	2156.110369	21.417216
74.152179	2179.590818	21.422234
74.407697	2174.777935	21.427251
74.766712	2189.069160	21.432269
74.303933	2186.904836	21.437287
74.668590	2178.121359	21.442304
74.860604	2191.305151	21.447322
74.738594	2183.497563	21.452339
74.393554	2192.107099	21.457357
74.850293	2201.845354	21.462375
75.110744	2207.917535	21.467392
75.123606	2211.744789	21.472410
75.643413	2206.544816	21.477427
75.346607	2197.783837	21.482445
75.419764	2206.196179	21.487463
75.424175	2198.564116	21.492480
75.443200	2198.800434	21.497498
75.442914	2199.402957	21.502515
75.917124	2218.751332	21.507533
75.745602	2221.467730	21.512551
76.387930	2215.331680	21.517568
76.408251	2221.427877	21.522586
76.099048	2207.182490	21.527603
76.102107	2202.078709	21.532621
76.199533	2218.579112	21.537639
76.172736	2220.875073	21.542656
76.413438	2225.265420	21.547674
76.476653	2224.797541	21.552691
76.698778	2215.988821	21.557709
76.676699	2220.556146	21.562727
76.946580	2224.955835	21.567744
76.630122	2222.499944	21.572762
76.697141	2221.376289	21.577779
77.119961	2213.871800	21.582797
76.472353	2224.029546	21.587815
76.734223	2215.024473	21.592832
76.868714	2225.492901	21.597850
77.209956	2234.953044	21.602867
76.978633	2238.877431	21.607885
77.011970	2249.837054	21.612903
77.774150	2244.900494	21.617920
77.225279	2243.219728	21.622938
77.200671	2245.073580	21.627955
77.285396	2238.515255	21.632973
77.454388	2245.240418	21.637991
77.895128	2250.815027	21.643008
77.743189	2263.288080	21.648026
77.921840	2271.182180	21.653043
78.070599	2271.688371	21.658061
78.010055	2277.703093	21.663079
78.274946	2263.166921	21.668096
78.317443	2266.633754	21.673114
78.180199	2271.207170	21.678131
78.499196	2266.643996	21.683149
78.332434	2267.731193	21.688167
78.349953	2263.067144	21.693184
78.335730	2268.182420	21.698202
78.211158	2276.384614	21.703219
78.764819	2281.845652	21.708237
78.802642	2296.543323	21.713255
78.839155	2291.676111	21.718272
79.080268	2288.105007	21.723290
79.055251	2296.963202	21.728307
79.237491	2281.383561	21.733325
79.035887	2293.914076	21.738343
79.137114	2287.894757	21.743360
79.033314	2289.686919	21.748378
79.186216	2302.115829	21.753395
79.431991	2312.555259	21.758413
79.581113	2323.845779	21.763431
79.568972	2308.086869	21.768448
79.899396	2314.631388	21.773466
79.662759	2317.182985	21.778483
79.570145	2309.688985	21.783501
79.679259	2323.489008	21.788519
80.209449	2328.759058	21.793536
80.086798	2336.921988	21.798554
80.276274	2340.073935	21.803571
80.824791	2338.650459	21.808589
80.516220	2337.803955	21.813607
80.893282	2329.241185	21.818624
80.923833	2338.196507	21.823642
80.751563	2339.803151	21.828659
80.567009	2337.672270	21.833677
80.962852	2336.414631	21.838695
80.691485	2328.685245	21.843712
80.679407	2336.299132	21.848730
80.655761	2341.004554	21.853747
81.018230	2335.236465	21.858765
80.871957	2360.192360	21.863783
80.831136	2363.463550	21.868800
81.282825	2370.343152	21.873818
81.144782	2368.620729	21.878835
81.452972	2363.039579	21.883853
81.391839	2374.097612	21.888871
81.749642	2384.502006	21.893888
81.944682	2395.827104	21.898906
81.703279	2384.841766	21.903923
82.235373	2387.236958	21.908941
82.118793	2395.139450	21.913959
82.081729	2390.801346	21.918976
82.099828	2380.629389	21.923994
82.039663	2390.538000	21.929011
82.609914	2379.661598	21.934029
82.207464	2383.278116	21.939047
82.197660	2389.361255	21.944064
82.494107	2405.248558	21.949082
82.641730	2418.815505	21.954099
82.854710	2415.093117	21.959117
82.569997	2424.388499	21.964135
82.860311	2419.714670	21.969152
82.826980	2419.298600	21.974170
82.833590	2415.199728	21.979187
83.244364	2421.020714	21.984205
83.376733	2439.182194	21.989223
83.213136	2444.725826	21.994240
83.469232	2442.249908	21.999258
83.191604	2444.480734	22.004275
83.750475	2432.173026	22.009293
83.705152	2429.172969	22.014311
83.669916	2437.070676	22.019328
83.720157	2438.703484	22.024346
83.650108	2443.312677	22.029363
83.790937	2431.255299	22.034381
83.628125	2437.844527	22.039399
83.818219	2453.475063	22.044416
83.988604	2459.855186	22.049434
83.782992	2462.804449	22.054451
84.354047	2458.381781	22.059469
84.323449	2468.351692	22.064487
84.252010	2472.033903	22.069504
84.706346	2483.218884	22.074522
84.273442	2493.538903	22.079539
84.578642	2492.975041	22.084557
84.676923	2497.013827	22.089575
84.982122	2487.512812	22.094592
85.197240	2487.102063	22.099610
85.157156	2493.563901	22.104627
85.539551	2496.574877	22.109645
85.375363	2497.901442	22.114663
85.655768	2511.920924	22.119680
85.900995	2509.634602	22.124698
85.895749	2499.711329	22.129715
85.967017	2486.088953	22.134733
85.598300	2485.998507	22.139751
86.009353	2492.365175	22.144768
86.241340	2501.678601	22.149786
86.176750	2508.872106	22.154803
86.540562	2498.213672	22.159821
86.154814	2482.258161	22.164839
86.150635	2500.252545	22.169856
86.659031	2502.972959	22.174874
86.110951	2506.277376	22.179891
86.364757	2503.604572	22.184909
86.643343	2497.074675	22.189927
86.334277	2501.910478	22.194944
86.418414	2488.425741	22.199962
86.319201	2511.199547	22.204979
86.733498	2517.603486	22.209997
86.593062	2522.532643	22.215015
86.818760	2512.959338	22.220032
86.929245	2527.884188	22.225050
86.910986	2548.373241	22.230067
87.497634	2543.010507	22.235085
87.444954	2546.685299	22.240103
87.279567	2548.709749	22.245120
87.555131	2544.045807	22.250138
87.546549	2551.629296	22.255155
87.827638	2560.785012	22.260173
88.151977	2574.977210	22.265191
87.864066	2580.483595	22.270208
88.122590	2570.507943	22.275226
88.184847	2580.438140	22.280243
88.324197	2574.618711	22.285261
88.623878	2575.723587	22.290279
88.197182	2583.966123	22.295296
88.421442	2575.137555	22.300314
88.450672	2574.122895	22.305331
88.336044	2581.456617	22.310349
88.680596	2591.686167	22.315367
88.991015	2602.384005	22.320384
89.222292	2602.723385	22.325402
89.054858	2605.131671	22.330419
88.932706	2600.874530	22.335437
89.277744	2601.269489	22.340455
89.172433	2602.946181	22.345472
89.362783	2590.259967	22.350490
89.289542	2598.745977	22.355507
89.543096	2592.951336	22.360525
89.551518	2598.558280	22.365543
89.576850	2603.130466	22.370560
89.795498	2615.580633	22.375578
89.528980	2626.186991	22.380595
90.032972	2621.866727	22.385613
90.022824	2621.605091	22.390631
90.060135	2619.521694	22.395648
90.124645	2612.309428	22.400666
90.030982	2625.234963	22.405683
90.297886	2638.967405	22.410701
90.572470	2640.745780	22.415719
90.583064	2652.162239	22.420736
90.790609	2641.683923	22.425754
90.651396	2651.300648	22.430771
90.755259	2654.709766	22.435789
90.990180	2650.009605	22.440807
90.808883	2648.834114	22.445824
91.297768	2648.888700	22.450842
91.323158	2664.868788	22.455859
91.757787	2667.625463	22.460877
91.838679	2671.673867	22.465895
91.675078	2674.018532	22.470912
92.009890	2654.312964	22.475930
91.465268	2650.593507	22.480947
92.011049	2647.624681	22.485965
92.083447	2654.325067	22.490983
92.190196	2669.327842	22.496000
92.110912	2654.716393	22.501018
92.420137	2657.496979	22.506035
92.128942	2657.111392	22.511053
92.267220	2653.878121	22.516071
92.347522	2660.257887	22.521088
92.693525	2661.275961	22.526106
92.616607	2656.969973	22.531123
92.196786	2658.294385	22.536141
92.768242	2674.540002	22.541159
92.489059	2686.767119	22.546176
92.582448	2690.241369	22.551194
92.333204	2698.934540	22.556211
92.679706	2703.028351	22.561229
92.901664	2711.906918	22.566247
92.891216	2721.359049	22.571264
93.369083	2725.344889	22.576282
93.391918	2726.198347	22.581299
93.771996	2723.166779	22.586317
93.655024	2726.224258	22.591335
94.193400	2729.694531	22.596352
94.330625	2722.792246	22.601370
94.562918	2722.080201	22.606387
94.681295	2725.374718	22.611405
94.645057	2719.780385	22.616423
94.841403	2729.789272	22.621440
94.751912	2706.055155	22.626458
94.617600	2693.235590	22.631475
94.849027	2701.340480	22.636493
94.938111	2714.692165	22.641511
94.559118	2708.588008	22.646528
95.013373	2710.678401	22.651546
94.724866	2717.867734	22.656563
94.460961	2713.169431	22.661581
94.847433	2718.494516	22.666599
94.557716	2726.560498	22.671616
94.851124	2739.900817	22.676634
95.065655	2746.306429	22.681651
94.940046	2749.835064	22.686669
95.256805	2750.946182	22.691687
95.438092	2780.261060	22.696704
95.757602	2783.431336	22.701722
95.764195	2781.433718	22.706739
95.592529	2777.631612	22.711757
95.893860	2769.550471	22.716775
96.148648	2777.864934	22.721792
96.088412	2780.052333	22.726810
96.399812	2792.799121	22.731827
96.312175	2796.749072	22.736845
96.498342	2804.302409	22.741863
96.589013	2808.226778	22.746880
96.831774	2794.852139	22.751898
97.187416	2802.833751	22.756915
96.382830	2805.968082	22.761933
97.002002	2790.809725	22.766951
96.766591	2805.517680	22.771968
97.216472	2827.176148	22.776986
97.138832	2824.918826	22.782003
97.265967	2820.054557	22.787021
97.200848	2828.363348	22.792039
97.262369	2828.398136	22.797056
97.692230	2849.257521	22.802074
97.759659	2854.870536	22.807091
97.984295	2853.154551	22.812109
98.156517	2842.563829	22.817127
98.215317	2853.587383	22.822144
98.487296	2857.255349	22.827162
98.703198	2845.304917	22.832179
98.569058	2852.654990	22.837197
98.526789	2850.131157	22.842215
98.585487	2848.695030	22.847232
98.923116	2836.396077	22.852250
98.828484	2840.245614	22.857267
99.036132	2847.346953	22.862285
98.975184	2834.326133	22.867303
98.923855	2846.805830	22.872320
99.152693	2853.095329	22.877338
99.174828	2869.858515	22.882355
99.108929	2865.617187	22.887373
99.302474	2865.827376	22.892391
99.046941	2876.213562	22.897408
99.455398	2875.866077	22.902426
99.636498	2889.186534	22.907443
99.464038	2897.278468	22.912461
99.880948	2888.754864	22.917479
99.728255	2898.508630	22.922496
99.927094	2911.455270	22.927514
100.399491	2915.776741	22.932531
100.345489	2914.423841	22.937549
100.692010	2916.117890	22.942567
100.418572	2924.092687	22.947584
100.557706	2915.900912	22.952602
100.859414	2914.445412	22.957619
100.664536	2919.939661	22.962637
101.051482	2920.418251	22.967655
101.196741	2937.114664	22.972672
101.275621	2940.387417	22.977690
101.595464	2939.077745	22.982707
101.484725	2935.715946	22.987725
101.812968	2938.445006	22.992743
101.241260	2941.072260	22.997760
101.478144	2929.427373	23.002778
101.666201	2931.411857	23.007795
101.654102	2941.451061	23.012813
101.819884	2931.043251	23.017831
101.775141	2943.920396	23.022848
101.842900	2961.169478	23.027866
101.949246	2964.019147	23.032883
101.929397	2961.851459	23.037901
102.202093	2955.341640	23.042919
101.850067	2982.117008	23.047936
102.340864	2987.146542	23.052954
102.628460	2998.296899	23.057971
102.508073	2992.947525	23.062989
102.853044	2994.283539	23.068007
103.201588	3016.870945	23.073024
103.107868	3017.578347	23.078042
103.404610	3020.940649	23.083059
102.957350	3026.754701	23.088077
102.933080	3016.117253	23.093095
103.329218	3027.104371	23.098112
103.556487	3045.040589	23.103130
104.095982	3045.266739	23.108147
103.962206	3050.304024	23.113165
103.895015	3043.385832	23.118183
104.098402	3038.433272	23.123200
104.261894	3044.750598	23.128218
104.341624	3035.881128	23.133235
104.451886	3038.867184	23.138253
104.523890	3031.484964	23.143271
104.673330	3051.748863	23.148288
104.938256	3066.119868	23.153306
105.290040	3062.409783	23.158323
104.843073	3063.303245	23.163341
105.427155	3058.569171	23.168359
104.999332	3052.648176	23.173376
105.101653	3062.398802	23.178394
105.653466	3060.893612	23.183411
105.669219	3069.286789	23.188429
105.918559	3056.022265	23.193447
105.873590	3055.669134	23.198464
105.582509	3056.513162	23.203482
105.674182	3051.262134	23.208499
105.665469	3069.901296	23.213517
105.754029	3081.181920	23.218535
105.855858	3083.535854	23.223552
105.951236	3088.798229	23.228570
106.147441	3093.454090	23.233587
106.013222	3116.721236	23.238605
106.510515	3108.733867	23.243623
106.685813	3112.814004	23.248640
106.577477	3111.874847	23.253658
107.019126	3112.356592	23.258675
107.111601	3136.707607	23.263693
107.344494	3138.626815	23.268711
107.065127	3135.769319	23.273728
107.535130	3131.931760	23.278746
107.635859	3128.769183	23.283763
107.636618	3137.685404	23.288781
107.972967	3134.697616	23.293799
107.772028	3128.287800	23.298816
107.592325	3136.325540	23.303834
107.797286	3137.136661	23.308851
107.908085	3161.347265	23.313869
108.157841	3157.517028	23.318887
108.103724	3172.939483	23.323904
108.218510	3166.360830	23.328922
108.269616	3156.634524	23.333939
108.348833	3189.419002	23.338957
108.474236	3191.024482	23.343975
108.407676	3184.584914	23.348992
108.530949	3194.845593	23.354010
108.827853	3204.523143	23.359027
108.960125	3213.603873	23.364045
109.522645	3215.853990	23.369063
109.300781	3220.388142	23.374080
109.632300	3208.277332	23.379098
109.798472	3212.299551	23.384115
109.791932	3213.754814	23.389133
109.695499	3211.701750	23.394151
109.922885	3203.607824	23.399168
109.958900	3206.368778	23.404186
110.363123	3226.208002	23.409203
109.935065	3233.877024	23.414221
110.463674	3237.695526	23.419239
110.529197	3243.010539	23.424256
110.550150	3240.651391	23.429274
110.732104	3239.603921	23.434291
110.521732	3238.698187	23.439309
110.688572	3227.180831	23.444327
111.085691	3234.952234	23.449344
110.904964	3268.007104	23.454362
111.176364	3264.761512	23.459379
111.291281	3263.894055	23.464397
111.474166	3261.917193	23.469415
111.342157	3260.754756	23.474432
111.000308	3273.998326	23.479450
111.813932	3282.679643	23.484467
111.562873	3278.913395	23.489485
111.712960	3280.644734	23.494503
111.957057	3293.539706	23.499520
111.864947	3310.321493	23.504538
112.169328	3310.596419	23.509555
112.176208	3311.836059	23.514573
112.733823	3315.785227	23.519591
112.740137	3327.623015	23.524608
112.595737	3342.678651	23.529626
113.250729	3329.382566	23.534643
113.146994	3341.743366	23.539661
112.990374	3330.604329	23.544679
113.391421	3317.266037	23.549696
113.165321	3330.925973	23.554714
113.612518	3324.305213	23.559731
113.884651	3340.232147	23.564749
113.953010	3350.353973	23.569767
114.026065	3350.165567	23.574784
113.997054	3354.850526	23.579802
114.210773	3345.917353	23.584819
114.530548	3346.824451	23.589837
114.239040	3343.183796	23.594855
114.316278	3342.087901	23.599872
114.558291	3348.884927	23.604890
114.637932	3337.442564	23.609907
114.591969	3340.986494	23.614925
114.671364	3357.060330	23.619943
114.843044	3361.686077	23.624960
114.682814	3367.830727	23.629978
115.114792	3370.863988	23.634995
115.039488	3381.500227	23.640013
114.866759	3396.044008	23.645031
115.313625	3395.362165	23.650048
115.297695	3409.127941	23.655066
115.621123	3401.948043	23.660083
115.684350	3418.568779	23.665101
116.116514	3434.576020	23.670119
116.106367	3429.041687	23.675136
116.151791	3429.365004	23.680154
116.238726	3424.276073	23.685171
116.552449	3422.702383	23.690189
116.338244	3422.165033	23.695207
116.940584	3431.821292	23.700224
116.789652	3442.077920	23.705242
117.080036	3446.966751	23.710259
116.999102	3453.518436	23.715277
116.936460	3455.666951	23.720295
117.365655	3443.763832	23.725312
117.312623	3451.470880	23.730330
117.681642	3444.200334	23.735347
117.895096	3450.205973	23.740365
117.689016	3446.137714	23.745383
117.619025	3437.386517	23.750400
117.162762	3458.222937	23.755418
117.768041	3458.321262	23.760435
118.059520	3473.370220	23.765453
117.816543	3473.949973	23.770471
118.261591	3484.495012	23.775488
118.161103	3503.429053	23.780506
118.335468	3497.763741	23.785523
118.415449	3501.616031	23.790541
118.570713	3511.480628	23.795559
119.118006	3528.706462	23.800576
118.926254	3527.997259	23.805594
119.243147	3531.368150	23.810611
119.416551	3524.925724	23.815629
119.565182	3529.671887	23.820647
119.687015	3529.513597	23.825664
119.703953	3541.222606	23.830682
120.023821	3545.517929	23.835699
120.047290	3552.920985	23.840717
120.158712	3554.005523	23.845735
120.578904	3546.972158	23.850752
120.370340	3548.738888	23.855770
120.193436	3545.010698	23.860787
120.720934	3550.561575	23.865805
120.515735	3538.925642	23.870823
121.197577	3555.411421	23.875840
120.728955	3564.460723	23.880858
120.995326	3565.983054	23.885875
121.050863	3569.988246	23.890893
121.205103	3571.666561	23.895911
121.294444	3563.095634	23.900928
121.629214	3588.568805	23.905946
121.680095	3591.803019	23.910963
121.996037	3594.387758	23.915981
121.576308	3593.066605	23.920999
122.085161	3590.306899	23.926016
121.949113	3596.208233	23.931034
122.469610	3588.262851	23.936051
122.605732	3602.545031	23.941069
122.485735	3621.813198	23.946087
122.717926	3617.162027	23.951104
122.760210	3624.961268	23.956122
122.479055	3617.267509	23.961139
122.997587	3613.739953	23.966157
122.932618	3621.167922	23.971175
123.392920	3625.069100	23.976192
123.448345	3650.961113	23.981210
123.274592	3641.654857	23.986227
123.803120	3639.912101	23.991245
123.328319	3648.890417	23.996263
123.748294	3631.659227	24.001280
123.775759	3655.205169	24.006298
123.770077	3663.982186	24.011315
124.069348	3657.979166	24.016333
123.959231	3661.156967	24.021351
124.341066	3669.779266	24.026368
124.451115	3682.530195	24.031386
124.430045	3688.115637	24.036403
124.998124	3682.818993	24.041421
124.588649	3697.088033	24.046439
124.653247	3683.373580	24.051456
124.950395	3705.658640	24.056474
125.105462	3719.184931	24.061491
125.675952	3716.465400	24.066509
125.311571	3718.775734	24.071527
125.895676	3714.432858	24.076544
125.809069	3721.588828	24.081562
125.909235	3716.740559	24.086579
126.118824	3729.895184	24.091597
125.906545	3748.458604	24.096615
126.503125	3741.344369	24.101632
126.333913	3747.189825	24.106650
126.160529	3748.497932	24.111667
126.521354	3749.678614	24.116685
126.503325	3766.304902	24.121703
126.511643	3767.603404	24.126720
126.501770	3767.240508	24.131738
127.007802	3777.719737	24.136755
127.049584	3791.230589	24.141773
126.897915	3805.945303	24.146791
127.588636	3797.519994	24.151808
127.333999	3801.374600	24.156826
127.279465	3821.253916	24.161843
127.948838	3815.636083	24.166861
127.969348	3825.767713	24.171879
128.191406	3821.789518	24.176896
128.470873	3842.450692	24.181914
128.314639	3842.363245	24.186931
128.568261	3851.722725	24.191949
128.493728	3852.399817	24.196967
129.310413	3847.790019	24.201984
129.173313	3847.133966	24.207002
129.132658	3846.302079	24.212019
129.362515	3853.666776	24.217037
129.453799	3866.110286	24.222055
129.676023	3857.093514	24.227072
129.898751	3868.553704	24.232090
129.732921	3865.276820	24.237107
129.983600	3867.601898	24.242125
129.744981	3869.217317	24.247143
130.223218	3863.538972	24.252160
130.241505	3881.830879	24.257178
130.468961	3894.591287	24.262195
130.685743	3890.787990	24.267213
130.481125	3891.826043	24.272231
130.947940	3890.202944	24.277248
130.614764	3888.331133	24.282266
130.717305	3908.473179	24.287283
131.137082	3913.445475	24.292301
130.818673	3920.978153	24.297319
131.291439	3920.558973	24.302336
131.484171	3928.126732	24.307354
131.508270	3934.097756	24.312371
131.477889	3934.947098	24.317389
131.836641	3948.708016	24.322407
132.002073	3943.663411	24.327424
132.315581	3960.824476	24.332442
132.437534	3963.851301	24.337459
132.592140	3956.527029	24.342477
132.435588	3964.102232	24.347495
132.653468	3961.992699	24.352512
133.075256	3976.062152	24.357530
132.960771	3985.371616	24.362547
133.214885	3993.357658	24.367565
133.366041	3987.109701	24.372583
133.305306	3986.679619	24.377600
133.313879	3985.836424	24.382618
133.440065	3983.887761	24.387635
133.837250	3994.037071	24.392653
134.181618	4014.428239	24.397671
134.110643	4014.502292	24.402688
134.107586	4019.142989	24.407706
134.137131	4018.460913	24.412723
133.890161	4014.037406	24.417741
134.089208	4027.530300	24.422759
134.339545	4032.459022	24.427776
134.636185	4037.017818	24.432794
134.684526	4049.696966	24.437811
135.070899	4047.807598	24.442829
135.165094	4063.033117	24.447847
135.207458	4062.571000	24.452864
135.313551	4059.768036	24.457882
135.268429	4069.375564	24.462899
135.803100	4076.905685	24.467917
135.583596	4092.984086	24.472935
135.658307	4089.981555	24.477952
136.029248	4101.257510	24.482970
136.139395	4115.310169	24.487987
136.592721	4112.429232	24.493005
136.376214	4119.493091	24.498023
136.307877	4120.998439	24.503040
137.223958	4133.683623	24.508058
136.846195	4147.608393	24.513075
137.408352	4143.523410	24.518093
137.209554	4153.138318	24.523111
137.656571	4140.817482	24.528128
137.772546	4136.139330	24.533146
137.451362	4136.677713	24.538163
137.950295	4156.526068	24.543181
137.940052	4166.465733	24.548199
138.209685	4168.036411	24.553216
138.158772	4178.752237	24.558234
138.252338	4166.507224	24.563251
138.258854	4178.841374	24.568269
138.803196	4188.181276	24.573287
138.832254	4192.708815	24.578304
139.214080	4191.975496	24.583322
138.514376	4201.339449	24.588339
139.036376	4204.607228	24.593357
139.149670	4222.837337	24.598375
139.259033	4219.395900	24.603392
139.133051	4227.593047	24.608410
139.767017	4248.224812	24.613427
140.181478	4249.150155	24.618445
140.536578	4257.133788	24.623463
140.248971	4250.229109	24.628480
140.596587	4247.833447	24.633498
140.803922	4245.268851	24.638515
141.021614	4238.030871	24.643533
141.344365	4236.103187	24.648551
141.197181	4239.053343	24.653568
141.356842	4240.051583	24.658586
141.185564	4245.492772	24.663603
141.454731	4253.685939	24.668621
141.484737	4264.605000	24.673639
141.436537	4262.904110	24.678656
141.488301	4255.868426	24.683674
141.968181	4265.956183	24.688691
142.079467	4287.390407	24.693709
142.016907	4292.435593	24.698727
142.134063	4304.019112	24.703744
142.374328	4295.481077	24.708762
142.197160	4301.060292	24.713779
142.449966	4315.362001	24.718797
142.516856	4326.450619	24.723815
142.779525	4324.211555	24.728832
143.038279	4325.190245	24.733850
142.515964	4341.241854	24.738867
143.290173	4343.597673	24.743885
143.809628	4350.105854	24.748903
143.331456	4347.180632	24.753920
143.809070	4358.633636	24.758938
143.682018	4368.128116	24.763955
144.019676	4372.686521	24.768973
144.216408	4373.257297	24.773991
144.012067	4368.262749	24.779008
144.627743	4382.298107	24.784026
144.640756	4400.439495	24.789043
144.605976	4404.115301	24.794061
144.674096	4409.828780	24.799079
144.767805	4420.527915	24.804096
144.988391	4427.119473	24.809114
145.159540	4430.520991	24.814131
145.193102	4430.622629	24.819149
145.642671	4449.441542	24.824167
145.534530	4459.028240	24.829184
145.818563	4455.887816	24.834202
145.859406	4468.754405	24.839219
146.222178	4476.470689	24.844237
146.504754	4480.491686	24.849255
146.553346	4472.353862	24.854272
146.548014	4475.490852	24.859290
147.256472	4502.916620	24.864307
147.229963	4499.011698	24.869325
147.222516	4505.511096	24.874343
147.637840	4509.628255	24.879360
147.743749	4500.728816	24.884378
147.500159	4498.979131	24.889395
147.805105	4502.486885	24.894413
147.734979	4515.957034	24.899431
148.002881	4525.286203	24.904448
148.254858	4519.936479	24.909466
148.130217	4529.605494	24.914483
148.750773	4544.893973	24.919501
148.601359	4547.060940	24.924519
148.729078	4552.548814	24.929536
148.847568	4554.132742	24.934554
148.676163	4564.864054	24.939571
148.935435	4566.030900	24.944589
149.505336	4570.076018	24.949607
149.160375	4580.733692	24.954624
149.621904	4596.780188	24.959642
149.709288	4611.638003	24.964659
150.197878	4603.294170	24.969677
150.161956	4607.422270	24.974695
150.259805	4610.736731	24.979712
150.501341	4616.738960	24.984730
150.437950	4631.822583	24.989747
151.052325	4626.464805	24.994765
151.248290	4625.815005	24.999783
151.333350	4627.106780	25.004800
151.308516	4629.446085	25.009818
151.205975	4632.299141	25.014835
151.614114	4654.184818	25.019853
151.665545	4652.927324	25.024871
151.529072	4660.557029	25.029888
152.061478	4654.507160	25.034906
151.829473	4666.976476	25.039923
152.060402	4683.145506	25.044941
152.435718	4680.341177	25.049959
152.661320	4690.687886	25.054976
152.611811	4686.812714	25.059994
152.555042	4702.722247	25.065011
152.713996	4712.316070	25.070029
153.204691	4719.961681	25.075047
152.763208	4724.011256	25.080064
153.261367	4723.702053	25.085082
153.436610	4745.508281	25.090099
153.453675	4759.268990	25.095117
153.600410	4743.138341	25.100135
153.773032	4760.611069	25.105152
153.837693	4768.057102	25.110170
154.147318	4783.658762	25.115187
154.603788	4771.776120	25.120205
154.718950	4778.886958	25.125223
154.543759	4800.777268	25.130240
154.704833	4796.778999	25.135258
154.875720	4798.197553	25.140275
154.824129	4816.003586	25.145293
155.629852	4822.125132	25.150311
155.396462	4826.942812	25.155328
155.568556	4822.860805	25.160346
155.865962	4848.834441	25.165363
156.093990	4854.872863	25.170381
156.260382	4851.444687	25.175399
156.345453	4859.111840	25.180416
156.518862	4850.323103	25.185434
156.844144	4874.312221	25.190451
156.683892	4885.542010	25.195469
157.191634	4879.515042	25.200487
157.011519	4884.744481	25.205504
157.323672	4885.344998	25.210522
157.266612	4891.949640	25.215539
157.539015	4894.323257	25.220557
157.557068	4896.684641	25.225575
157.765669	4906.448355	25.230592
158.019774	4918.338859	25.235610
157.920483	4928.718249	25.240627
158.023313	4934.713635	25.245645
158.701151	4940.250758	25.250663
158.753527	4960.883666	25.255680
159.034779	4953.205609	25.260698
158.992728	4960.229147	25.265715
158.960165	4961.501043	25.270733
159.402214	4974.681235	25.275751
159.859291	4982.184477	25.280768
160.131622	4984.832196	25.285786
160.082134	4987.470188	25.290803
160.209423	4984.998272	25.295821
160.036045	4985.446053	25.300839
160.253511	5002.065770	25.305856
160.394959	5008.327292	25.310874
160.467393	5006.555945	25.315891
160.545378	5015.859355	25.320909
161.007117	5041.378450	25.325927
160.748776	5041.504791	25.330944
161.072874	5036.474524	25.335962
161.404894	5063.525703	25.340979
161.598510	5069.007574	25.345997
162.042378	5072.416063	25.351015
161.692845	5070.796475	25.356032
161.860540	5089.041423	25.361050
162.364040	5098.728082	25.366067
162.367465	5101.532176	25.371085
162.833161	5096.786392	25.376103
162.765020	5103.089739	25.381120
162.483451	5106.781363	25.386138
163.122626	5118.698054	25.391155
163.160275	5125.710045	25.396173
163.500969	5121.575634	25.401191
163.032471	5120.837350	25.406208
163.389481	5135.106016	25.411226
163.289378	5148.948682	25.416243
163.654624	5156.807447	25.421261
164.169826	5174.328668	25.426279
163.822022	5174.554879	25.431296
164.291872	5175.181282	25.436314
164.711210	5191.168427	25.441331
164.740844	5208.568452	25.446349
165.314685	5203.531441	25.451367
165.082325	5195.588610	25.456384
165.598583	5194.265146	25.461402
165.476899	5202.948815	25.466419
165.597739	5215.365661	25.471437
165.875902	5222.448140	25.476455
166.082342	5225.918810	25.481472
165.827080	5229.034320	25.486490
166.127761	5232.986357	25.491507
166.274814	5252.964453	25.496525
166.368764	5250.700425	25.501543
166.708354	5263.103147	25.506560
166.791112	5270.770096	25.511578
167.201924	5274.129759	25.516595
166.939528	5280.864644	25.521613
167.384251	5288.589029	25.526631
167.721160	5305.057765	25.531648
167.992832	5302.813137	25.536666
168.151373	5309.540566	25.541683
168.064104	5314.155419	25.546701
168.535776	5323.537964	25.551719
168.544859	5322.722967	25.556736
168.657225	5323.863787	25.561754
168.688214	5330.586351	25.566771
168.775424	5346.202552	25.571789
169.057492	5352.648068	25.576807
169.074228	5361.320722	25.581824
169.131113	5365.862894	25.586842
169.500460	5380.785807	25.591859
169.694207	5387.042760	25.596877
169.795246	5390.812088	25.601895
169.926621	5411.868047	25.606912
170.140617	5420.988510	25.611930
170.656874	5423.204487	25.616947
170.673955	5439.499484	25.621965
170.838747	5443.309464	25.626983
170.928304	5449.462401	25.632000
171.034757	5450.938938	25.637018
171.271683	5459.021512	25.642035
171.492224	5476.116142	25.647053
171.858564	5475.478272	25.652071
171.758040	5479.247911	25.657088
172.089307	5493.736968	25.662106
172.354229	5504.605396	25.667123
172.375185	5505.287227	25.672141
172.513200	5501.751770	25.677159
172.587458	5513.675649	25.682176
172.805722	5520.646888	25.687194
173.324244	5518.325923	25.692212
173.193673	5528.806971	25.697229
173.487212	5543.598458	25.702247
173.746972	5555.104946	25.707264
173.694449	5552.911592	25.712282
173.847310	5558.350762	25.717300
174.204446	5578.852902	25.722317
174.469421	5579.105263	25.727335
174.466192	5581.289911	25.732352
174.412077	5588.376370	25.737370
174.901662	5591.411171	25.742388
174.628954	5607.045472	25.747405
175.027329	5605.797413	25.752423
175.153865	5610.074516	25.757440
175.159701	5621.366330	25.762458
175.779130	5625.417706	25.767476
175.661571	5640.300970	25.772493
176.029451	5633.988132	25.777511
176.140575	5637.977167	25.782528
176.559947	5646.770771	25.787546
176.739950	5659.329393	25.792564
176.564613	5664.955252	25.797581
176.597287	5660.023442	25.802599
176.886466	5671.527507	25.807616
177.071568	5686.422929	25.812634
177.508370	5687.501402	25.817652
177.283235	5703.566621	25.822669
177.655237	5707.785786	25.827687
177.753328	5718.105450	25.832704
177.623878	5723.369308	25.837722
177.988861	5741.099544	25.842740
178.327858	5756.992664	25.847757
178.343033	5751.418667	25.852775
178.949149	5771.826282	25.857792
178.722413	5768.112504	25.862810
178.716018	5772.857447	25.867828
178.989563	5791.762245	25.872845
179.393198	5789.270446	25.877863
179.795965	5799.275873	25.882880
179.762346	5822.587859	25.887898
180.295659	5814.181645	25.892916
180.380478	5823.207947	25.897933
180.557319	5824.750054	25.902951
180.384427	5842.478874	25.907968
180.460415	5851.787833	25.912986
180.878194	5850.234099	25.918004
180.929280	5877.626967	25.923021
181.291890	5892.253760	25.928039
181.528926	5884.058021	25.933056
181.848971	5908.391410	25.938074
182.210747	5907.354169	25.943092
182.040551	5910.134379	25.948109
182.506552	5913.953680	25.953127
182.839414	5910.084217	25.958144
182.783304	5927.698497	25.963162
183.135329	5924.985236	25.968180
183.025117	5936.396515	25.973197
183.073931	5923.302979	25.978215
183.412223	5929.418076	25.983232
183.293264	5954.242439	25.988250
183.740138	5957.654566	25.993268
183.764783	5961.854118	25.998285
184.271538	5972.620612	26.003303
184.454440	5975.687358	26.008320
184.343772	5994.017242	26.013338
184.825053	5982.842390	26.018356
184.683404	6015.845358	26.023373
184.681794	6016.056009	26.028391
184.958471	6020.167383	26.033408
185.070182	6041.965444	26.038426
185.415719	6045.096644	26.043444
185.673635	6053.833717	26.048461
185.757968	6069.032879	26.053479
186.270465	6080.533354	26.058496
186.135030	6083.993076	26.063514
186.357011	6088.712909	26.068532
186.278604	6105.604883	26.073549
186.490470	6115.747658	26.078567
187.084301	6129.255765	26.083584
187.050579	6135.949215	26.088602
187.391873	6130.819668	26.093620
187.486871	6132.576200	26.098637
187.785703	6154.563975	26.103655
188.223119	6154.274264	26.108672
188.058238	6177.105991	26.113690
188.330796	6164.944005	26.118708
188.484264	6173.796102	26.123725
188.564359	6188.869272	26.128743
188.741528	6194.559044	26.133760
188.795200	6195.993194	26.138778
189.064426	6204.855288	26.143796
189.075785	6208.259230	26.148813
189.522179	6213.542128	26.153831
189.922898	6227.965228	26.158848
189.199596	6249.444980	26.163866
190.132741	6256.683354	26.168884
190.229294	6274.138847	26.173901
190.627125	6269.139308	26.178919
191.015565	6271.979902	26.183936
191.046758	6285.429272	26.188954
191.340894	6300.484442	26.193972
191.581056	6305.303723	26.198989
191.264739	6306.141454	26.204007
191.667760	6306.540319	26.209024
191.550288	6326.227242	26.214042
191.977838	6323.808592	26.219060
192.294247	6340.262902	26.224077
192.645198	6351.348452	26.229095
192.894730	6355.873195	26.234112
192.837515	6362.057874	26.239130
193.147720	6368.904787	26.244148
193.312480	6375.192925	26.249165
193.710593	6376.326688	26.254183
193.849089	6377.519183	26.259200
193.626036	6408.290872	26.264218
193.916214	6418.167255	26.269236
194.118839	6419.163253	26.274253
194.194607	6428.655322	26.279271
194.595450	6436.998753	26.284288
194.716859	6452.740348	26.289306
195.402448	6462.413462	26.294324
195.306568	6465.836000	26.299341
195.469986	6467.930960	26.304359
195.678733	6471.314884	26.309376
195.786043	6494.361931	26.314394
196.033317	6494.966169	26.319412
196.417441	6501.969461	26.324429
196.495379	6518.399634	26.329447
196.913948	6522.898017	26.334464
196.902493	6526.683089	26.339482
196.794058	6524.525636	26.344500
197.245362	6537.414966	26.349517
197.613382	6559.237471	26.354535
197.186304	6555.664579	26.359552
197.527124	6570.772140	26.364570
198.249475	6581.475794	26.369588
198.119904	6581.468189	26.374605
198.458954	6594.627410	26.379623
198.820276	6612.863332	26.384640
198.651446	6614.347744	26.389658
199.040598	6613.901397	26.394676
198.954444	6631.500953	26.399693
199.279239	6645.014659	26.404711
199.742070	6642.207321	26.409728
199.757087	6659.401057	26.414746
199.664874	6666.050065	26.419764
200.034231	6668.282668	26.424781
200.031766	6676.658336	26.429799
200.296956	6682.396726	26.434816
200.670508	6696.326952	26.439834
200.573837	6692.157421	26.444852
201.012250	6717.724840	26.449869
201.319530	6717.525979	26.454887
201.218427	6716.395970	26.459904
201.557013	6735.381712	26.464922
201.691927	6744.727127	26.469940
202.041107	6752.455450	26.474957
202.373170	6767.746599	26.479975
202.607385	6772.495331	26.484992
202.619882	6770.502926	26.490010
202.963384	6785.399155	26.495028
202.974931	6800.183366	26.500045
203.342218	6816.424956	26.505063
203.535683	6805.915494	26.510080
203.618749	6829.120636	26.515098
204.018954	6825.363470	26.520116
203.978219	6834.370962	26.525133
204.205766	6854.658338	26.530151
204.490470	6859.917023	26.535168
204.299875	6874.878910	26.540186
204.499711	6881.557641	26.545204
204.899328	6896.908622	26.550221
205.006761	6914.986854	26.555239
205.651851	6922.181857	26.560256
205.418389	6932.757269	26.565274
205.828473	6941.996596	26.570292
206.055206	6951.060699	26.575309
206.215176	6971.654788	26.580327
206.912525	6979.557950	26.585344
206.754637	6981.065789	26.590362
207.050124	6990.443055	26.595380
207.480993	6997.911434	26.600397
207.304232	7007.884389	26.605415
207.407028	7021.807738	26.610432
207.830876	7039.916438	26.615450
208.086039	7039.459180	26.620468
208.343968	7054.461199	26.625485
208.396512	7070.074600	26.630503
208.610974	7070.417271	26.635520
208.826204	7086.690612	26.640538
209.248746	7101.191241	26.645556
209.466361	7087.811231	26.650573
209.921650	7110.213171	26.655591
210.025242	7118.618775	26.660608
209.900246	7120.292109	26.665626
210.178780	7125.488103	26.670644
210.481436	7133.756788	26.675661
210.405912	7150.260280	26.680679
210.703409	7143.659970	26.685696
210.749756	7166.427431	26.690714
210.805939	7175.730995	26.695732
211.377331	7186.143404	26.700749
211.283440	7212.101422	26.705767
211.660441	7214.932268	26.710784
211.709086	7229.906083	26.715802
212.163549	7236.633396	26.720820
212.400231	7247.731404	26.725837
212.712848	7264.399978	26.730855
212.886639	7266.939946	26.735872
213.143117	7287.507441	26.740890
213.164273	7293.484949	26.745908
213.589664	7295.538227	26.750925
213.422733	7312.816352	26.755943
213.780792	7319.271365	26.760960
213.869448	7331.298204	26.765978
214.108708	7341.849193	26.770996
214.565683	7359.478585	26.776013
214.598674	7358.229445	26.781031
214.600117	7379.377271	26.786048
215.168967	7387.271192	26.791066
214.989072	7391.596354	26.796084
215.422091	7409.739405	26.801101
215.569373	7426.566277	26.806119
216.429770	7436.248078	26.811136
216.514687	7441.161149	26.816154
216.704543	7449.083968	26.821172
217.061370	7444.153871	26.826189
216.737606	7452.686323	26.831207
216.833714	7459.496685	26.836224
216.895897	7474.411775	26.841242
217.232589	7499.192265	26.846260
217.766873	7500.676943	26.851277
217.957764	7526.364623	26.856295
218.321971	7525.756181	26.861312
218.352368	7530.835057	26.866330
218.602947	7552.045059	26.871348
218.671210	7556.790780	26.876365
219.034319	7565.675906	26.881383
219.280885	7574.754413	26.886400
219.719735	7585.997999	26.891418
219.515363	7588.736106	26.896436
219.770540	7597.710011	26.901453
219.699268	7613.357044	26.906471
220.369237	7626.721499	26.911488
220.415417	7643.037574	26.916506
220.746226	7656.132876	26.921524
220.999662	7672.221682	26.926541
221.035262	7674.529375	26.931559
221.629885	7694.055209	26.936576
221.767958	7695.445591	26.941594
222.036626	7711.784771	26.946612
222.330053	7719.850486	26.951629
222.717207	7732.900289	26.956647
222.457056	7736.423549	26.961664
222.831166	7753.099787	26.966682
222.925066	7775.085925	26.971700
223.332295	7785.042250	26.976717
223.347297	7795.233657	26.981735
223.611956	7790.649551	26.986752
223.702348	7814.115650	26.991770
223.988301	7828.396153	26.996788
224.531352	7845.231210	27.001805
224.432515	7861.417909	27.006823
224.826367	7873.752259	27.011840
225.362620	7885.232004	27.016858
225.198460	7893.501166	27.021876
225.596066	7904.305169	27.026893
225.904202	7917.576163	27.031911
225.788415	7921.097621	27.036928
226.177115	7929.419435	27.041946
226.366718	7948.447833	27.046964
226.705433	7954.535292	27.051981
226.740377	7972.059565	27.056999
226.998495	7985.861943	27.062016
227.437328	7995.723369	27.067034
227.692258	8004.770804	27.072052
228.122634	8009.233789	27.077069
228.027328	8023.583095	27.082087
228.239443	8039.023726	27.087104
228.301225	8045.125553	27.092122
228.210518	8061.934200	27.097140
228.884157	8063.239109	27.102157
228.961745	8096.204583	27.107175
229.218291	8099.930697	27.112192
229.252123	8106.359356	27.117210
229.622774	8122.708071	27.122228
230.294336	8120.298394	27.127245
230.008664	8134.031010	27.132263
230.140473	8149.396815	27.137280
230.226138	8163.253890	27.142298
230.475074	8176.437221	27.147316
230.968021	8191.084740	27.152333
231.224787	8211.258726	27.157351
231.450379	8221.305262	27.162368
231.842894	8226.904189	27.167386
232.061865	8250.979046	27.172404
231.888955	8247.408590	27.177421
232.613624	8273.362807	27.182439
232.690229	8281.136213	27.187456
232.758827	8297.685567	27.192474
233.009286	8317.514914	27.197492
233.243442	8327.371829	27.202509
233.485046	8340.005879	27.207527
233.581464	8350.996323	27.212544
233.961928	8365.754002	27.217562
234.430421	8378.959448	27.222580
234.500978	8396.217548	27.227597
234.955079	8401.351815	27.232615
234.874326	8424.324866	27.237632
235.437736	8426.665034	27.242650
235.425327	8453.623833	27.247668
236.012595	8462.001284	27.252685
236.467385	8471.530299	27.257703
236.170266	8491.886131	27.262720
236.606380	8494.879155	27.267738
236.659539	8503.824782	27.272756
237.115442	8520.938877	27.277773
237.376830	8533.806918	27.282791
237.557157	8535.589769	27.287808
238.180702	8538.389499	27.292826
237.856871	8562.941464	27.297844
238.196120	8569.853847	27.302861
238.740033	8580.179560	27.307879
238.652919	8596.808566	27.312896
239.144340	8596.228659	27.317914
238.926351	8612.372820	27.322932
239.586530	8630.621458	27.327949
239.417665	8640.725677	27.332967
239.907142	8651.562247	27.337984
240.085946	8672.595772	27.343002
240.061923	8684.234226	27.348020
240.267259	8698.624961	27.353037
240.808268	8707.608109	27.358055
240.815129	8725.983910	27.363072
241.459848	8740.824234	27.368090
241.444528	8760.847802	27.373108
242.054655	8774.092365	27.378125
242.020223	8772.898391	27.383143
242.437833	8789.729218	27.388160
242.757492	8799.491132	27.393178
242.494848	8816.653591	27.398196
243.094490	8819.903992	27.403213
243.411604	8836.080328	27.408231
243.477598	8858.820165	27.413248
243.965970	8859.844647	27.418266
244.163719	8879.187124	27.423284
244.592096	8871.242570	27.428301
244.825845	8884.777981	27.433319
244.733514	8902.596909	27.438336
245.134468	8904.245598	27.443354
245.411785	8914.730673	27.448372
245.395428	8920.504665	27.453389
245.870921	8940.252633	27.458407
245.896207	8947.811132	27.463424
246.270038	8950.609734	27.468442
246.468518	8972.522699	27.473460
246.343851	8977.331502	27.478477
246.708618	8987.793484	27.483495
246.794113	9004.160372	27.488512
247.430748	9014.983859	27.493530
247.508777	9036.589925	27.498548
247.372008	9041.837178	27.503565
247.996156	9052.248388	27.508583
247.803461	9072.877572	27.513600
248.423102	9092.676705	27.518618
248.693368	9100.430269	27.523636
248.881346	9125.797227	27.528653
249.041435	9136.690229	27.533671
249.596993	9151.477947	27.538688
250.023377	9165.112480	27.543706
249.761473	9183.532506	27.548724
250.148295	9202.137436	27.553741
250.737076	9208.621991	27.558759
250.711541	9224.307930	27.563776
251.504172	9233.868136	27.568794
251.519988	9250.661972	27.573812
251.577288	9262.610375	27.578829
251.905597	9273.995563	27.583847
252.001286	9295.215402	27.588864
252.546751	9303.099187	27.593882
252.410855	9313.248789	27.598900
252.939714	9327.918196	27.603917
253.280139	9344.600888	27.608935
253.237208	9349.408876	27.613952
253.502421	9376.814852	27.618970
253.926594	9384.226386	27.623988
253.972854	9407.948705	27.629005
254.469602	9429.567919	27.634023
254.213359	9449.310019	27.639040
254.578620	9453.135839	27.644058
255.074814	9483.908616	27.649076
255.126353	9491.963276	27.654093
255.610875	9512.295790	27.659111
255.628526	9528.547607	27.664128
255.950957	9530.792332	27.669146
256.326628	9557.685595	27.674164
256.482264	9559.196132	27.679181
256.927114	9583.073315	27.684199
256.738490	9605.349801	27.689216
257.269877	9616.528300	27.694234
257.574462	9631.435212	27.699252
258.024319	9656.999154	27.704269
258.506099	9652.573958	27.709287
258.482938	9686.555953	27.714304
259.223499	9685.411670	27.719322
259.317780	9703.019400	27.724340
259.662621	9714.470704	27.729357
259.798292	9716.670742	27.734375
260.056786	9739.732112	27.739392
260.461975	9745.727324	27.744410
260.462240	9753.643283	27.749428
260.671177	9770.128384	27.754445
261.470179	9770.426358	27.759463
261.366305	9774.719091	27.764480
261.531603	9794.998451	27.769498
261.723450	9815.964353	27.774516
261.885981	9823.655745	27.779533
262.491215	9828.447184	27.784551
262.191938	9837.783563	27.789568
262.792912	9861.335949	27.794586
262.695744	9874.644936	27.799604
263.087463	9880.602250	27.804621
263.454191	9895.339194	27.809639
263.493016	9905.721803	27.814656
263.725752	9922.271662	27.819674
264.151707	9940.447126	27.824692
264.216111	9956.021989	27.829709
264.699407	9963.550845	27.834727
264.732709	9988.053744	27.839744
264.927709	10003.130403	27.844762
265.455366	10016.804047	27.849780
265.637094	10029.296506	27.854797
265.900167	10043.996385	27.859815
266.055738	10061.280807	27.864832
266.701872	10072.528082	27.869850
266.583244	10091.019179	27.874868
266.773556	10102.493977	27.879885
267.438202	10121.176100	27.884903
267.227079	10142.366696	27.889920
267.946711	10143.745328	27.894938
267.961195	10172.310519	27.899956
267.741709	10196.741343	27.904973
268.491090	10209.625283	27.909991
268.757509	10237.480805	27.915008
269.138609	10243.728360	27.920026
269.357411	10264.940917	27.925044
269.464584	10276.290942	27.930061
270.186523	10300.878074	27.935079
270.224669	10321.401314	27.940096
270.585634	10341.700184	27.945114
270.855221	10345.902100	27.950132
271.089569	10374.250839	27.955149
271.232726	10375.511411	27.960167
271.641096	10404.216652	27.965184
271.830403	10413.867984	27.970202
272.298800	10435.054420	27.975220
272.507329	10449.464318	27.980237
273.262594	10470.247210	27.985255
273.433758	10469.831346	27.990272
273.618843	10497.228861	27.995290
274.061771	10502.831279	28.000308
274.177552	10511.691238	28.005325
274.354678	10519.504239	28.010343
274.204216	10528.844745	28.015360
274.640018	10543.009116	28.020378
274.869379	10556.865744	28.025396
275.253738	10579.931909	28.030413
275.345879	10590.729209	28.035431
275.273517	10611.672914	28.040448
275.745150	10631.327488	28.045466
275.775852	10666.807432	28.050484
276.295730	10688.805049	28.055501
276.683182	10705.911542	28.060519
276.871499	10731.934899	28.065536
277.432900	10751.278526	28.070554
277.743770	10769.666216	28.075572
277.546873	10782.548893	28.080589
278.332652	10807.160899	28.085607
278.470027	10822.624462	28.090624
278.639230	10842.609834	28.095642
279.147105	10858.992207	28.100660
279.294798	10881.839558	28.105677
280.036047	10882.670267	28.110695
279.950729	10917.968273	28.115712
280.114537	10920.875264	28.120730
280.913139	10936.785721	28.125748
280.990776	10948.784796	28.130765
281.260025	10952.566206	28.135783
281.162474	10977.787955	28.140800
281.622285	10980.058209	28.145818
282.188601	10993.098356	28.150836
282.304845	11019.487071	28.155853
282.513477	11016.019080	28.160871
282.658382	11029.989367	28.165888
283.259097	11040.784725	28.170906
283.402724	11057.331592	28.175924
283.251300	11068.755705	28.180941
284.082700	11080.868051	28.185959
283.899171	11101.455762	28.190976
284.246439	11119.057829	28.195994
284.558461	11127.088311	28.201012
284.403871	11158.652740	28.206029
284.697795	11170.928180	28.211047
285.553009	11201.953667	28.216064
285.788924	11216.772568	28.221082
285.710466	11225.527978	28.226100
285.948715	11255.352535	28.231117
286.848551	11269.606192	28.236135
287.159157	11294.015535	28.241152
287.303681	11309.049771	28.246170
287.443694	11326.123819	28.251188
287.704706	11342.400999	28.256205
287.953588	11363.631295	28.261223
287.871174	11383.974140	28.266240
288.609714	11403.352262	28.271258
288.946188	11427.893042	28.276276
289.252220	11446.291759	28.281293
289.699915	11460.079932	28.286311
289.851646	11488.174842	28.291328
290.043209	11497.156740	28.296346
290.346605	11516.994670	28.301364
290.738873	11527.493943	28.306381
291.070783	11544.411970	28.311399
291.250671	11573.961554	28.316416
291.187801	11589.306143	28.321434
291.848231	11598.702139	28.326452
292.085186	11626.345110	28.331469
292.413863	11633.460699	28.336487
292.435999	11669.620277	28.341504
292.945890	11694.521982	28.346522
293.477551	11710.097621	28.351540
293.716575	11733.331314	28.356557
293.859778	11740.305886	28.361575
294.539399	11765.077178	28.366592
294.636367	11784.243638	28.371610
294.922898	11800.395717	28.376628
295.045548	11819.011158	28.381645
295.250327	11829.078370	28.386663
295.891204	11855.017594	28.391680
296.246781	11874.774837	28.396698
296.561277	11886.603033	28.401716
297.001855	11904.491494	28.406733
297.041742	11916.155580	28.411751
297.502097	11934.611251	28.416768
297.795975	11954.506447	28.421786
298.080321	11967.423867	28.426804
297.976917	11982.479279	28.431821
298.511401	11999.397345	28.436839
298.928835	12025.985253	28.441856
298.881346	12040.721023	28.446874
299.111531	12047.306280	28.451892
299.709027	12068.024378	28.456909
300.076432	12093.531769	28.461927
300.235961	12103.272561	28.466944
300.422139	12121.869955	28.471962
300.652527	12128.152649	28.476980
300.797587	12148.788152	28.481997
301.350705	12173.292627	28.487015
301.634596	12183.233503	28.492032
301.904670	12208.355341	28.497050
302.010147	12216.712089	28.502068
302.221331	12238.348464	28.507085
302.518627	12263.946520	28.512103
302.817024	12287.718004	28.517120
302.873271	12309.605468	28.522138
303.305485	12328.362510	28.527156
303.602220	12352.096543	28.532173
304.175660	12376.358429	28.537191
304.279647	12403.600822	28.542208
304.542288	12426.404535	28.547226
305.336799	12432.707437	28.552244
305.729091	12453.775170	28.557261
305.806442	12476.617502	28.562279
306.440739	12499.002075	28.567296
306.625892	12515.486825	28.572314
307.217286	12525.670129	28.577332
307.079156	12551.129540	28.582349
307.635542	12563.203429	28.587367
307.888267	12584.414201	28.592384
307.530462	12594.704231	28.597402
308.071951	12621.198514	28.602420
308.343679	12647.507409	28.607437
308.694499	12669.078696	28.612455
309.262219	12690.204374	28.617472
309.542791	12714.786298	28.622490
309.940239	12723.262026	28.627508
310.037558	12752.620977	28.632525
310.688254	12772.563702	28.637543
310.851145	12799.607899	28.642560
311.113760	12812.874715	28.647578
311.352024	12833.943221	28.652596
312.050431	12853.701647	28.657613
312.074848	12868.988868	28.662631
312.672142	12882.890601	28.667648
312.812717	12906.660746	28.672666
313.107168	12923.652603	28.677684
313.650043	12947.594185	28.682701
313.810216	12959.258020	28.687719
314.417890	12980.623310	28.692736
314.412098	12992.283120	28.697754
314.745789	13009.772870	28.702772
314.986142	13039.195340	28.707789
315.111537	13060.550731	28.712807
315.454379	13075.687733	28.717824
315.676706	13108.284109	28.722842
316.526824	13115.462184	28.727860
316.271031	13133.426288	28.732877
316.535821	13161.155516	28.737895
317.215098	13174.123573	28.742912
317.404272	13207.236243	28.747930
317.611962	13224.925163	28.752948
317.950758	13257.710585	28.757965
318.127208	13281.487947	28.762983
318.796676	13296.537998	28.768000
318.970944	13319.786252	28.773018
319.547320	13341.759216	28.778036
319.476651	13368.267785	28.783053
320.203784	13384.841794	28.788071
320.300285	13397.225669	28.793088
320.521685	13425.161100	28.798106
320.898103	13445.077554	28.803124
321.169408	13462.628549	28.808141
321.476789	13480.835504	28.813159
321.403828	13500.263780	28.818176
322.025254	13524.974899	28.823194
322.484081	13538.179887	28.828212
322.722591	13565.296364	28.833229
322.812632	13579.957177	28.838247
323.396923	13601.470568	28.843264
323.955800	13631.435534	28.848282
324.085876	13644.431831	28.853300
324.428957	13656.196698	28.858317
324.659346	13683.472316	28.863335
324.928024	13691.583744	28.868352
324.921762	13721.703879	28.873370
325.553456	13736.632934	28.878388
325.915919	13761.724541	28.883405
325.918099	13790.722863	28.888423
326.437168	13805.875504	28.893440
326.684776	13838.562137	28.898458
327.230004	13850.214886	28.903476
327.460197	13887.545872	28.908493
327.926741	13913.063347	28.913511
328.351348	13935.454662	28.918528
328.278126	13966.145818	28.923546
328.932970	13985.189434	28.928564
329.323745	14014.719574	28.933581
329.276464	14030.886568	28.938599
329.764711	14051.507078	28.943616
330.185845	14081.725770	28.948634
330.736974	14102.682666	28.953652
331.048782	14131.475891	28.958669
331.551993	14155.012891	28.963687
331.737469	14162.419647	28.968704
331.581378	14197.318815	28.973722
331.866098	14220.792781	28.978740
332.557413	14243.435097	28.983757
332.454438	14271.241263	28.988775
333.160409	14291.986798	28.993792
333.384043	14319.923387	28.998810
333.945688	14345.109007	29.003828
334.349422	14380.923012	29.008845
334.516615	14405.165327	29.013863
334.988565	14419.643900	29.018880
335.338787	14449.244579	29.023898
335.730912	14469.397671	29.028916
336.228345	14487.320543	29.033933
336.612961	14518.215920	29.038951
336.726420	14528.583612	29.043968
337.238689	14549.774469	29.048986
337.804978	14568.423642	29.054004
338.129340	14596.443324	29.059021
338.373575	14611.564975	29.064039
338.561406	14624.530425	29.069056
338.713511	14652.931759	29.074074
339.068334	14660.704736	29.079092
339.500087	14684.624708	29.084109
339.825624	14711.988736	29.089127
340.300697	14728.794967	29.094144
340.087119	14751.973903	29.099162
340.679955	14778.381237	29.104180
341.122132	14798.345198	29.109197
341.022267	14824.790027	29.114215
341.874300	14848.612307	29.119232
341.673020	14872.181829	29.124250
342.401066	14892.959150	29.129268
343.083730	14926.538954	29.134285
342.943953	14953.175001	29.139303
343.603583	14964.896300	29.144320
343.502753	14999.676119	29.149338
343.968768	15016.151581	29.154356
344.330816	15050.889572	29.159373
344.824015	15067.273899	29.164391
345.065266	15078.296949	29.169408
345.573578	15102.485411	29.174426
345.664097	15124.757121	29.179444
346.070724	15144.081170	29.184461
346.490549	15171.871679	29.189479
347.012922	15182.436897	29.194496
347.281166	15205.651783	29.199514
347.422024	15234.479966	29.204532
347.848782	15249.852551	29.209549
347.860418	15281.477808	29.214567
348.336228	15293.043782	29.219584
348.762676	15322.001381	29.224602
348.625630	15343.374812	29.229620
349.411128	15381.722177	29.234637
349.717400	15404.568532	29.239655
350.288240	15422.943672	29.244672
350.031725	15457.275797	29.249690
350.934342	15491.671486	29.254708
351.156102	15519.448078	29.259725
351.078652	15548.859877	29.264743
351.829015	15574.422807	29.269760
352.327155	15609.736826	29.274778
352.660215	15633.099206	29.279796
353.202925	15661.650418	29.284813
353.332753	15697.925590	29.289831
353.810263	15707.261260	29.294848
353.866439	15742.878838	29.299866
354.325972	15765.383512	29.304884
354.888132	15798.691870	29.309901
355.015815	15819.670609	29.314919
355.623510	15842.514971	29.319936
356.030236	15878.678511	29.324954
356.365175	15900.964407	29.329972
356.920108	15921.089184	29.334989
356.776179	15954.959214	29.340007
357.127195	15983.110826	29.345024
357.582977	16005.556552	29.350042
357.816940	16039.164030	29.355060
358.386678	16061.330895	29.360077
358.845098	16101.691749	29.365095
359.315454	16122.210642	29.370112
359.406620	16149.910607	29.375130
359.511168	16185.160173	29.380148
360.212239	16213.508017	29.385165
360.560943	16242.774858	29.390183
360.949591	16267.169259	29.395200
361.489065	16297.468593	29.400218
361.659559	16327.947269	29.405236
361.890145	16347.013412	29.410253
362.426721	16374.031600	29.415271
363.130032	16400.123767	29.420288
363.359767	16436.633074	29.425306
363.630849	16451.113586	29.430324
364.140761	16472.167027	29.435341
364.517403	16505.010992	29.440359
364.672328	16522.945487	29.445376
364.802555	16552.714038	29.450394
365.134449	16585.877672	29.455412
365.722461	16613.497758	29.460429
365.697900	16650.238778	29.465447
366.156124	16676.215892	29.470464
366.574627	16709.608188	29.475482
366.907441	16735.147451	29.480500
367.484771	16764.889674	29.485517
367.579908	16795.216171	29.490535
368.245271	16824.147899	29.495552
368.477650	16851.866651	29.500570
369.204512	16875.417822	29.505588
369.612754	16891.266321	29.510605
369.594398	16914.447501	29.515623
369.979942	16939.101923	29.520640
370.555214	16960.463585	29.525658
370.440946	16983.761618	29.530676
371.149718	17002.750952	29.535693
371.491034	17034.933456	29.540711
371.741536	17053.910419	29.545728
372.227205	17085.027179	29.550746
372.636193	17112.550047	29.555764
373.120999	17126.108305	29.560781
373.653670	17160.540333	29.565799
374.053699	17173.816310	29.570816
374.277982	17199.421541	29.575834
374.182363	17229.162478	29.580852
375.443482	17264.952770	29.585869
375.350163	17284.650542	29.590887
376.010948	17308.733462	29.595904
375.893870	17334.683870	29.600922
376.661749	17352.591906	29.605940
376.972535	17382.272160	29.610957
377.157696	17411.665870	29.615975
377.651782	17438.850466	29.620992
377.824830	17460.370772	29.626010
378.089185	17490.517626	29.631028
378.305906	17517.992593	29.636045
378.908684	17551.619341	29.641063
379.105511	17585.250288	29.646080
379.624372	17621.604006	29.651098
379.800932	17655.717669	29.656116
380.326524	17686.356036	29.661133
380.907369	17725.557707	29.666151
381.429670	17751.432897	29.671168
381.607297	17786.971708	29.676186
381.851695	17827.214547	29.681204
382.479259	17851.614305	29.686221
382.715309	17889.475160	29.691239
383.149160	17917.751922	29.696256
383.560450	17941.030523	29.701274
383.812959	17983.063195	29.706292
384.387506	18006.557637	29.711309
384.504025	18040.010471	29.716327
384.951605	18072.442235	29.721344
385.632820	18095.216065	29.726362
385.888733	18140.893261	29.731380
386.280583	18157.172897	29.736397
386.617142	18192.772973	29.741415
386.940632	18234.903307	29.746432
387.228909	18265.772766	29.751450
387.637063	18301.656021	29.756468
388.139042	18339.481769	29.761485
388.352542	18370.098954	29.766503
388.648803	18397.034097	29.771520
389.385460	18430.831217	29.776538
389.513249	18473.123810	29.781556
390.016043	18494.210953	29.786573
390.796064	18531.087809	29.791591
391.211102	18560.551124	29.796608
391.625210	18586.789189	29.801626
392.076319	18607.985924	29.806644
392.594299	18631.665599	29.811661
393.036996	18660.973173	29.816679
393.493223	18681.938990	29.821696
393.841451	18698.604730	29.826714
393.839655	18738.278837	29.831732
394.486354	18742.073694	29.836749
395.008394	18771.607956	29.841767
394.851155	18789.457828	29.846784
395.485254	18806.431074	29.851802
395.389142	18846.980235	29.856820
396.105710	18873.036269	29.861837
396.091813	18906.253876	29.866855
396.608434	18933.771404	29.871872
396.965791	18959.806621	29.876890
397.047444	19006.598082	29.881908
397.668421	19036.748619	29.886925
397.964446	19068.545268	29.891943
398.580418	19103.724259	29.896960
398.851111	19146.075305	29.901978
399.110815	19181.404859	29.906996
399.726301	19200.374315	29.912013
400.004324	19242.177336	29.917031
400.528789	19275.743277	29.922048
401.219327	19311.362830	29.927066
401.333100	19344.519186	29.932084
402.065821	19378.129694	29.937101
401.846510	19400.926645	29.942119
402.477213	19442.441624	29.947136
403.060173	19475.362935	29.952154
403.405674	19511.066817	29.957172
403.901437	19545.751098	29.962189
404.446850	19578.946842	29.967207
404.816340	19613.336848	29.972224
405.571039	19641.183479	29.977242
405.733890	19679.640680	29.982260
406.162700	19711.490674	29.987277
406.459988	19736.280510	29.992295
407.086758	19766.666316	29.997312
407.428688	19800.115318	30.002330
407.431446	19832.893713	30.007348
407.994217	19870.838993	30.012365
408.332470	19906.664737	30.017383
408.703838	19939.662970	30.022400
409.487733	19982.003718	30.027418
409.719996	20013.670818	30.032436
410.396997	20045.707403	30.037453
411.060946	20077.848689	30.042471
411.307344	20105.058127	30.047488
411.556260	20134.851262	30.052506
412.076738	20174.675670	30.057524
412.633619	20200.775970	30.062541
412.837058	20223.975482	30.067559
413.018953	20263.823025	30.072576
413.815588	20288.332383	30.077594
414.085807	20321.365448	30.082612
414.199766	20340.819664	30.087629
414.732388	20378.733243	30.092647
415.103220	20413.365891	30.097664
415.835071	20451.749612	30.102682
416.034634	20482.748204	30.107700
416.221664	20514.340170	30.112717
416.889235	20551.268472	30.117735
416.935752	20593.248761	30.122752
417.114374	20625.906571	30.127770
417.797042	20670.358036	30.132788
418.352234	20687.689968	30.137805
418.679385	20734.932801	30.142823
419.336847	20774.556219	30.147840
419.817664	20806.845881	30.152858
420.227192	20844.293687	30.157876
420.611145	20888.341078	30.162893
420.936289	20906.958465	30.167911
421.157051	20943.598934	30.172928
421.991788	20967.547985	30.177946
422.428886	20997.625266	30.182964
422.676021	21023.905817	30.187981
423.182364	21046.170229	30.192999
423.572438	21077.273982	30.198016
424.126600	21102.434841	30.203034
424.181793	21142.313312	30.208052
424.850815	21169.413535	30.213069
425.514845	21196.883578	30.218087
425.640314	21226.746375	30.223104
426.014062	21253.480922	30.228122
426.517368	21287.082766	30.233140
426.632908	21320.471345	30.238157
426.819381	21353.088269	30.243175
427.165238	21396.172025	30.248192
427.848702	21426.045319	30.253210
428.271305	21468.990422	30.258228
428.716477	21501.258932	30.263245
429.428500	21532.665012	30.268263
429.414278	21575.975951	30.273280
429.986311	21621.283909	30.278298
430.458752	21652.395588	30.283316
430.597515	21692.838618	30.288333
431.675584	21728.440160	30.293351
431.689890	21777.960917	30.298368
432.415689	21814.429819	30.303386
432.515282	21844.952348	30.308404
432.834893	21887.668004	30.313421
433.514098	21915.392145	30.318439
433.903401	21970.100507	30.323456
434.907475	22006.342441	30.328474
434.991171	22047.197510	30.333492
435.427629	22081.018555	30.338509
435.712850	22115.534835	30.343527
436.317493	22155.143429	30.348544
436.664614	22193.623167	30.353562
437.171377	22230.996458	30.358580
437.307069	22267.783169	30.363597
438.202623	22301.618558	30.368615
438.457485	22351.585261	30.373632
438.757713	22387.531364	30.378650
439.336766	22432.972785	30.383668
439.578696	22469.900035	30.388685
440.066343	22506.493412	30.393703
440.362419	22558.492750	30.398720
440.936222	22594.939605	30.403738
441.346636	22640.888851	30.408756
441.674179	22680.252811	30.413773
442.356675	22712.487508	30.418791
442.542976	22766.353722	30.423808
443.362548	22801.606088	30.428826
443.726525	22842.730481	30.433844
444.373014	22879.616902	30.438861
444.731522	22911.271691	30.443879
445.090938	22951.790007	30.448896
445.709889	22996.652350	30.453914
446.005837	23030.145317	30.458932
446.682868	23069.726722	30.463949
446.943976	23107.372820	30.468967
447.338398	23145.738079	30.473984
447.920909	23181.028887	30.479002
448.395519	23230.693734	30.484020
448.706607	23261.894990	30.489037
449.343412	23301.644435	30.494055
449.460313	23345.961594	30.499072
450.091625	23370.999522	30.504090
450.425276	23410.737890	30.509108
450.922344	23450.387807	30.514125
451.246565	23478.975904	30.519143
451.819334	23521.688463	30.524160
452.276809	23556.215430	30.529178
452.684455	23596.963839	30.534196
452.883356	23633.359843	30.539213
453.823458	23661.270744	30.544231
453.614429	23712.871494	30.549248
454.445570	23747.480514	30.554266
455.098326	23777.498654	30.559284
455.276230	23821.232941	30.564301
455.638498	23851.548441	30.569319
456.016380	23900.447495	30.574336
456.525139	23932.009929	30.579354
456.962896	23977.234424	30.584372
457.072279	24013.590858	30.589389
458.250021	24050.442366	30.594407
458.281353	24096.418841	30.599424
459.050222	24129.894055	30.604442
459.411155	24172.485600	30.609460
459.830375	24217.486712	30.614477
460.518842	24250.871386	30.619495
460.900877	24298.297977	30.624512
461.067097	24330.624327	30.629530
461.934240	24375.387723	30.634548
462.474563	24421.397540	30.639565
463.066040	24451.666713	30.644583
463.159800	24497.621317	30.649600
463.628212	24526.668296	30.654618
464.198880	24566.551486	30.659636
464.522121	24616.347915	30.664653
465.264525	24639.883763	30.669671
465.335838	24690.091121	30.674688
466.267236	24724.256579	30.679706
466.604799	24767.080563	30.684724
466.850430	24821.028592	30.689741
467.687038	24862.499130	30.694759
467.962096	24922.107379	30.699776
468.435999	24943.335107	30.704794
468.938825	24986.507630	30.709812
469.186488	25032.261566	30.714829
469.983189	25065.730853	30.719847
470.323269	25107.473399	30.724864
471.195947	25148.566472	30.729882
471.627438	25184.944630	30.734900
471.785808	25231.745284	30.739917
472.683467	25265.721848	30.744935
472.780057	25308.359957	30.749952
473.129047	25347.653963	30.754970
473.720480	25383.009349	30.759988
474.180115	25433.883239	30.765005
474.729964	25470.964731	30.770023
475.191671	25515.662566	30.775040
475.735503	25554.984734	30.780058
476.387146	25595.781107	30.785076
476.749008	25628.705218	30.790093
477.091870	25662.414791	30.795111
477.541843	25707.780615	30.800128
477.847696	25753.561535	30.805146
478.417495	25797.400026	30.810164
478.720246	25842.923046	30.815181
479.622285	25875.922266	30.820199
480.227970	25925.246763	30.825216
480.296552	25960.241946	30.830234
480.894027	25995.925639	30.835252
481.145146	26044.154671	30.840269
481.779901	26086.409143	30.845287
482.047451	26134.869130	30.850304
482.227232	26175.650328	30.855322
483.189042	26217.494560	30.860340
483.271467	26256.642334	30.865357
483.936575	26287.965580	30.870375
484.228874	26329.018723	30.875392
484.866340	26378.225699	30.880410
485.447370	26418.048382	30.885428
485.711870	26462.658284	30.890445
486.531733	26500.044294	30.895463
486.612357	26545.924519	30.900480
486.717119	26597.800579	30.905498
487.479787	26628.556276	30.910516
487.886141	26688.846032	30.915533
488.384452	26739.755225	30.920551
489.174954	26780.039329	30.925568
489.739425	26829.612968	30.930586
490.378573	26868.304083	30.935604
491.035572	26911.477998	30.940621
491.347925	26951.772225	30.945639
491.773918	27003.126324	30.950656
491.898487	27041.802033	30.955674
492.949167	27075.192195	30.960692
493.401765	27133.772413	30.965709
493.955746	27185.979677	30.970727
494.486842	27226.452854	30.975744
494.751604	27270.209913	30.980762
495.127448	27305.059177	30.985780
495.541005	27358.788609	30.990797
496.137421	27405.125185	30.995815
496.928415	27451.445461	31.000832
497.228686	27497.900689	31.005850
497.799169	27533.768682	31.010868
498.322196	27583.925472	31.015885
498.806232	27619.385230	31.020903
499.682139	27670.382941	31.025920
499.885473	27711.681212	31.030938
500.618193	27756.377850	31.035956
500.815144	27799.986578	31.040973
501.748591	27842.722739	31.045991
502.191198	27888.953562	31.051008
502.489652	27930.817071	31.056026
503.038213	27970.478344	31.061044
503.426354	28024.497960	31.066061
504.066862	28062.970689	31.071079
504.720560	28111.713008	31.076096
504.799186	28155.837493	31.081114
505.277776	28196.857920	31.086132
505.563112	28256.684162	31.091149
506.181897	28302.158190	31.096167
506.813572	28355.311994	31.101184
507.187481	28408.022781	31.106202
508.106669	28450.652381	31.111220
508.343629	28499.117718	31.116237
509.270761	28558.050105	31.121255
509.744837	28599.687408	31.126272
509.921085	28644.434240	31.131290
510.682617	28685.238639	31.136308
510.901633	28731.770545	31.141325
511.698611	28784.658539	31.146343
511.899584	28824.757851	31.151360
512.451338	28872.916596	31.156378
512.927761	28916.614373	31.161396
513.415958	28971.765572	31.166413
513.631387	29028.217715	31.171431
514.596016	29073.759567	31.176448
514.947627	29119.469227	31.181466
515.507313	29167.630626	31.186484
516.046545	29218.294219	31.191501
516.427872	29262.680589	31.196519
517.226607	29304.947312	31.201536
517.445695	29361.787978	31.206554
518.252042	29396.690078	31.211572
518.546042	29449.190072	31.216589
519.069373	29477.065795	31.221607
520.033497	29518.299240	31.226624
520.146239	29571.252355	31.231642
520.761944	29600.349734	31.236660
521.200200	29654.536464	31.241677
521.981627	29697.772422	31.246695
522.594590	29736.956961	31.251712
522.981881	29783.056822	31.256730
523.334248	29827.969990	31.261748
523.818440	29865.068580	31.266765
524.096333	29913.499509	31.271783
524.723711	29956.947743	31.276800
525.279282	30007.393217	31.281818
525.941618	30056.947223	31.286836
526.176595	30100.457587	31.291853
526.800380	30153.684418	31.296871
527.279200	30211.264157	31.301888
527.589200	30261.959231	31.306906
528.305892	30308.564416	31.311924
528.720928	30361.308981	31.316941
529.545939	30416.680332	31.321959
529.980708	30468.024238	31.326976
530.451515	30519.191954	31.331994
531.246674	30565.380979	31.337012
531.523459	30624.156590	31.342029
531.982198	30668.805048	31.347047
532.907461	30724.854915	31.352064
533.202644	30781.851649	31.357082
533.513783	30839.644189	31.362100
534.387275	30893.150613	31.367117
535.118011	30947.337103	31.372135
535.662084	31003.416223	31.377152
536.158017	31042.152911	31.382170
536.925075	31093.503606	31.387188
537.440037	31144.555398	31.392205
537.612864	31192.615978	31.397223
538.364528	31226.322307	31.402240
538.955543	31280.769586	31.407258
539.600694	31323.950057	31.412276
540.081069	31380.356442	31.417293
540.505760	31429.565533	31.422311
541.088468	31477.880908	31.427328
541.729595	31529.894236	31.432346
542.236558	31578.042565	31.437364
542.804640	31625.155431	31.442381
543.424341	31679.065939	31.447399
544.141974	31725.154085	31.452416
544.249011	31773.015718	31.457434
544.881439	31821.099774	31.462452
545.326069	31867.495357	31.467469
545.773452	31919.485092	31.472487
546.486236	31976.779449	31.477504
546.913017	32031.013246	31.482522
547.610632	32075.919188	31.487540
548.154543	32140.313283	31.492557
548.433263	32200.687297	31.497575
549.023728	32236.814044	31.502592
549.483707	32300.474769	31.507610
550.266134	32353.931266	31.512628
550.745541	32413.294606	31.517645
551.208188	32445.703700	31.522663
551.742985	32497.352495	31.527680
552.239837	32556.546187	31.532698
553.117381	32609.833098	31.537716
553.609988	32657.374567	31.542733
554.158583	32703.177675	31.547751
554.875852	32738.523983	31.552768
555.243423	32793.012879	31.557786
555.850421	32835.827842	31.562804
556.407195	32884.779296	31.567821
556.556171	32929.150221	31.572839
557.202383	32987.001609	31.577856
557.484479	33038.605433	31.582874
558.426178	33087.108773	31.587892
558.769130	33143.209007	31.592909
559.218633	33198.771113	31.597927
559.919028	33243.868886	31.602944
560.335544	33306.669454	31.607962
560.922729	33357.759845	31.612980
561.375920	33414.306569	31.617997
561.606083	33469.520822	31.623015
562.740834	33526.232829	31.628032
562.818040	33585.054425	31.633050
563.623680	33647.469929	31.638068
564.138163	33700.501453	31.643085
564.843819	33761.037326	31.648103
565.605761	33816.508635	31.653120
566.199627	33886.966065	31.658138
567.012092	33934.902977	31.663156
567.603704	33998.696308	31.668173
568.096296	34056.257852	31.673191
568.720784	34099.224433	31.678208
568.846430	34160.390948	31.683226
569.970286	34213.995352	31.688244
570.483613	34272.652373	31.693261
571.029898	34324.127835	31.698279
571.694025	34373.819848	31.703296
572.108633	34428.993919	31.708314
572.908808	34483.589966	31.713332
573.196714	34541.325791	31.718349
573.679420	34599.802755	31.723367
574.358257	34647.078865	31.728384
574.932978	34719.695036	31.733402
575.861285	34763.827955	31.738420
576.561342	34825.880022	31.743437
576.479605	34887.124353	31.748455
577.578713	34928.830933	31.753472
577.816866	34990.070025	31.758490
578.409573	35053.548181	31.763508
579.132253	35112.245896	31.768525
579.268108	35165.003558	31.773543
580.060586	35220.748733	31.778560
580.466246	35287.433559	31.783578
581.013686	35348.900425	31.788596
581.646000	35409.068968	31.793613
581.984469	35483.412611	31.798631
582.787993	35538.775067	31.803648
583.536592	35605.467450	31.808666
583.945306	35667.059347	31.813684
584.608630	35720.293138	31.818701
585.182317	35785.727461	31.823719
586.017519	35847.561861	31.828736
586.566902	35913.799155	31.833754
586.982031	35975.451008	31.838772
587.615811	36028.472827	31.843789
588.347156	36097.003579	31.848807
589.124924	36144.200978	31.853824
589.765842	36198.910643	31.858842
590.009057	36257.956533	31.863860
590.727282	36314.197110	31.868877
591.238004	36367.779988	31.873895
591.928908	36429.555039	31.878912
592.550578	36481.898460	31.883930
592.612952	36537.923157	31.888948
593.467564	36591.705452	31.893965
593.630591	36649.594937	31.898983
594.611917	36699.553355	31.904000
595.235573	36758.992431	31.909018
595.785678	36814.580634	31.914036
596.439537	36863.334344	31.919053
596.762325	36927.220404	31.924071
597.954343	36978.893303	31.929088
598.067621	37038.345142	31.934106
598.697812	37096.711110	31.939124
599.824495	37153.555850	31.944141
599.851429	37209.478012	31.949159
600.496760	37276.783876	31.954176
601.122952	37339.623792	31.959194
601.899004	37391.278312	31.964212
602.579018	37453.929807	31.969229
602.824302	37515.640251	31.974247
603.682093	37569.813157	31.979264
604.238827	37639.101440	31.984282
604.433875	37702.945076	31.989300
605.678910	37759.251328	31.994317
605.747325	37833.040105	31.999335
606.322193	37898.087307	32.004352
607.003333	37959.862871	32.009370
607.532892	38032.070537	32.014388
608.435238	38099.008650	32.019405
608.662966	38177.084186	32.024423
609.499799	38231.350911	32.029440
610.247430	38307.071475	32.034458
610.836021	38375.053651	32.039476
611.403651	38441.966331	32.044493
611.723809	38506.524392	32.049511
612.558146	38575.167405	32.054528
613.334060	38642.810245	32.059546
613.652173	38717.359888	32.064564
614.527591	38785.592855	32.069581
615.019639	38852.535325	32.074599
615.837176	38918.152079	32.079616
616.454680	38989.765008	32.084634
616.733735	39054.155029	32.089652
617.763093	39116.435618	32.094669
618.278146	39195.945271	32.099687
619.059039	39251.603739	32.104704
619.553895	39333.052360	32.109722
620.205420	39391.418986	32.114740
621.112823	39458.973640	32.119757
621.347716	39521.421770	32.124775
622.098455	39591.559765	32.129792
622.641601	39657.675974	32.134810
623.140250	39728.269729	32.139828
623.775198	39799.283151	32.144845
624.620619	39871.411089	32.149863
625.215471	39943.284028	32.154880
625.872583	40010.039260	32.159898
626.335396	40082.733256	32.164916
627.216665	40138.046342	32.169933
627.722787	40213.357000	32.174951
628.446733	40275.445821	32.179968
629.181203	40345.620952	32.184986
629.777635	40418.489892	32.190004
630.271840	40475.512753	32.195021
630.530977	40540.331136	32.200039
631.188082	40608.092424	32.205056
631.975045	40687.165768	32.210074
632.653607	40760.868523	32.215092
633.348429	40812.820794	32.220109
633.925319	40880.406938	32.225127
634.462329	40943.229774	32.230144
635.139435	41001.215283	32.235162
635.552350	41068.987092	32.240180
636.294049	41134.826350	32.245197
636.891728	41198.160918	32.250215
637.624686	41267.323252	32.255232
638.313280	41335.473467	32.260250
638.695791	41402.392818	32.265268
639.643009	41464.085641	32.270285
640.121997	41529.635121	32.275303
640.710387	41590.087023	32.280320
641.602183	41666.413197	32.285338
642.161581	41732.196341	32.290356
642.642938	41805.061369	32.295373
642.998477	41869.136008	32.300391
643.975458	41949.364067	32.305408
644.471084	42024.645950	32.310426
644.944522	42093.983745	32.315444
645.956432	42165.199624	32.320461
646.737545	42233.066316	32.325479
647.180086	42306.779539	32.330496
648.115820	42379.221199	32.335514
648.375373	42449.546020	32.340532
649.247743	42515.643240	32.345549
649.744624	42600.424156	32.350567
650.125400	42671.140198	32.355584
651.089854	42742.063042	32.360602
651.410126	42810.263817	32.365620
652.296038	42881.661148	32.370637
652.988393	42968.880393	32.375655
653.793177	43047.392534	32.380672
654.549871	43125.887704	32.385690
654.986428	43203.735237	32.390708
655.703368	43273.589671	32.395725
656.062318	43346.319951	32.400743
656.663891	43427.099559	32.405760
657.683045	43505.874957	32.410778
658.019872	43592.909654	32.415796
658.981800	43662.608187	32.420813
659.095577	43752.948448	32.425831
660.247952	43818.132510	32.430848
661.377122	43906.313188	32.435866
661.793097	43983.977923	32.440884
662.385174	44059.956170	32.445901
663.149920	44128.877588	32.450919
663.685905	44215.197050	32.455936
664.631811	44279.425419	32.460954
665.199470	44356.210914	32.465972
665.867336	44426.636648	32.470989
666.620382	44511.068086	32.476007
667.190380	44575.991168	32.481024
668.132197	44652.693873	32.486042
668.978753	44736.283568	32.491060
669.497719	44798.917136	32.496077
670.184247	44871.052867	32.501095
670.671734	44940.695702	32.506112
671.603940	45007.480189	32.511130
671.941469	45087.413852	32.516148
672.482508	45158.753765	32.521165
673.209047	45229.886430	32.526183
673.462273	45315.155684	32.531200
674.564840	45383.549003	32.536218
675.508282	45464.587111	32.541236
676.049501	45528.624604	32.546253
676.951453	45615.022563	32.551271
677.310754	45682.895747	32.556288
678.456875	45743.016179	32.561306
678.793218	45819.643805	32.566324
679.240769	45878.380291	32.571341
679.857426	45950.863275	32.576359
680.489485	46024.048180	32.581376
681.336579	46077.764592	32.586394
681.568520	46158.617069	32.591412
682.224835	46228.707238	32.596429
682.808716	46305.848502	32.601447
683.620647	46384.341814	32.606464
684.376436	46454.656360	32.611482
685.097010	46549.971703	32.616500
685.258059	46616.156815	32.621517
686.301571	46701.569994	32.626535
686.977226	46789.652864	32.631552
687.753393	46859.880276	32.636570
688.227085	46944.261424	32.641588
688.707295	47020.851150	32.646605
689.794910	47108.535761	32.651623
690.511065	47190.717829	32.656640
691.319061	47272.512413	32.661658
691.649912	47353.982053	32.666676
692.450007	47437.660837	32.671693
692.859761	47520.239239	32.676711
693.934325	47603.867032	32.681728
694.808364	47692.015999	32.686746
695.726603	47783.385636	32.691764
695.965303	47853.554034	32.696781
696.859153	47948.238193	32.701799
697.433304	48033.798154	32.706816
698.341866	48110.049791	32.711834
699.066965	48192.042044	32.716852
700.086021	48276.193587	32.721869
700.571784	48356.767059	32.726887
701.000831	48443.316102	32.731904
701.952012	48531.620405	32.736922
702.640966	48618.247255	32.741940
703.285431	48693.610068	32.746957
704.550433	48779.002225	32.751975
704.720111	48854.261030	32.756992
705.720879	48943.102248	32.762010
706.161919	49022.561563	32.767028
707.042196	49103.287671	32.772045
707.789949	49181.784153	32.777063
708.424142	49276.909461	32.782080
709.348661	49351.836894	32.787098
709.978122	49444.686640	32.792116
710.688173	49520.076586	32.797133
711.250989	49594.366794	32.802151
711.613463	49679.593255	32.807168
712.546416	49766.289142	32.812186
713.231249	49860.676200	32.817204
714.119323	49958.014839	32.822221
714.933450	50032.148298	32.827239
715.777879	50120.471239	32.832256
716.664133	50189.179734	32.837274
717.332853	50284.291664	32.842292
717.740929	50349.005353	32.847309
718.712227	50431.023276	32.852327
718.946434	50515.911411	32.857344
719.824729	50602.474800	32.862362
720.140979	50696.554199	32.867380
721.062372	50786.579397	32.872397
722.150485	50872.408078	32.877415
722.588005	50956.954967	32.882432
723.840530	51033.281314	32.887450
724.136483	51116.298270	32.892468
724.780148	51202.625190	32.897485
725.431104	51286.083215	32.902503
726.293697	51369.569763	32.907520
726.970146	51435.727265	32.912538
727.957047	51521.916700	32.917556
728.580579	51592.777333	32.922573
729.124544	51670.088882	32.927591
729.532897	51745.970148	32.932608
730.576090	51831.355638	32.937626
731.030897	51913.307325	32.942644
731.595586	52005.709398	32.947661
732.645723	52083.317911	32.952679
733.402907	52175.120361	32.957696
733.872695	52268.044785	32.962714
734.287945	52350.484991	32.967732
735.092346	52437.112995	32.972749
735.757793	52523.044146	32.977767
736.623943	52621.262129	32.982784
737.170028	52714.959459	32.987802
737.961442	52816.798252	32.992820
738.801179	52913.385750	32.997837
739.624919	53005.686519	33.002855
740.138963	53103.390235	33.007872
741.250137	53197.274385	33.012890
741.677154	53302.309685	33.017908
742.380422	53406.472188	33.022925
743.278467	53488.799413	33.027943
743.911870	53602.660090	33.032960
744.703041	53688.253328	33.037978
745.298408	53795.961252	33.042996
746.447781	53897.259941	33.048013
746.919657	53993.174371	33.053031
747.850622	54095.066208	33.058048
748.593818	54191.909735	33.063066
749.535265	54284.026442	33.068084
750.149714	54382.326456	33.073101
751.315298	54482.519764	33.078119
751.590193	54586.632998	33.083136
752.696258	54687.822864	33.088154
753.356181	54786.648116	33.093172
754.173040	54884.367440	33.098189
755.232614	54966.181275	33.103207
755.506781	55070.126572	33.108224
756.674958	55165.331252	33.113242
757.612062	55256.328501	33.118260
758.308891	55350.082930	33.123277
759.247717	55449.945847	33.128295
759.626197	55537.397229	33.133312
760.671075	55634.160002	33.138330
761.177147	55728.345851	33.143348
761.995183	55826.107534	33.148365
762.884134	55909.962866	33.153383
763.787339	56008.456979	33.158400
764.642797	56098.030892	33.163418
765.354484	56192.886325	33.168436
766.210874	56283.465626	33.173453
767.025797	56370.595720	33.178471
767.657421	56466.628390	33.183488
768.686490	56552.321039	33.188506
769.192576	56643.882498	33.193524
769.592752	56735.449257	33.198541
770.836988	56826.023741	33.203559
771.357323	56927.107049	33.208576
771.603668	57008.975340	33.213594
772.982048	57107.611136	33.218612
773.620902	57206.274954	33.223629
774.311859	57292.766056	33.228647
774.931101	57400.312638	33.233664
775.572852	57490.509520	33.238682
776.563561	57587.511907	33.243700
777.352657	57683.397983	33.248717
777.823824	57776.531285	33.253735
778.615778	57864.891334	33.258752
779.251943	57949.789192	33.263770
780.012006	58038.945215	33.268788
780.388751	58147.464874	33.273805
781.486683	58233.153327	33.278823
781.934760	58342.054048	33.283840
782.886966	58439.660959	33.288858
783.830864	58541.447008	33.293876
784.276439	58641.085148	33.298893
785.297615	58739.143438	33.303911
786.153211	58852.017807	33.308928
786.691754	58944.273235	33.313946
787.858289	59060.276187	33.318964
788.630906	59161.979940	33.323981
789.512893	59268.083710	33.328999
790.241431	59361.074321	33.334016
790.741569	59453.825059	33.339034
791.778063	59564.170785	33.344052
792.710966	59676.126888	33.349069
793.244843	59771.881825	33.354087
794.087004	59892.594747	33.359104
795.050992	59997.955646	33.364122
795.699306	60099.905869	33.369140
796.414247	60210.415737	33.374157
797.326647	60309.788942	33.379175
798.267629	60423.024508	33.384192
799.309773	60530.258672	33.389210
799.502122	60638.702089	33.394228
800.771701	60745.191892	33.399245
801.713411	60847.975860	33.404263
802.172757	60962.267421	33.409280
802.718828	61069.181964	33.414298
803.873977	61174.801755	33.419316
804.740621	61295.228197	33.424333
805.713108	61401.764245	33.429351
806.476360	61505.130923	33.434368
807.375941	61613.835450	33.439386
808.549559	61711.649011	33.444404
808.956093	61830.549260	33.449421
809.796249	61930.542767	33.454439
810.546639	62047.415339	33.459456
811.626465	62147.471394	33.464474
812.459984	62248.883402	33.469492
812.915491	62349.081624	33.474509
814.219549	62456.573324	33.479527
814.528502	62570.696457	33.484544
815.482208	62685.339354	33.489562
816.677093	62789.507076	33.494580
816.896971	62901.339617	33.499597
817.971060	63000.294593	33.504615
819.120763	63119.148901	33.509632
819.518115	63220.340742	33.514650
820.510016	63325.827929	33.519668
821.163286	63435.670057	33.524685
822.375836	63553.068919	33.529703
823.091286	63645.682928	33.534720
823.607173	63756.756837	33.539738
824.485055	63860.729544	33.544756
825.291181	63984.190661	33.549773
826.186508	64090.209746	33.554791
827.148177	64200.674986	33.559808
827.581853	64314.938823	33.564826
828.678718	64398.820105	33.569844
829.247262	64523.954663	33.574861
830.705972	64631.065449	33.579879
831.392153	64737.457469	33.584896
832.223547	64839.849732	33.589914
833.137232	64937.038835	33.594932
833.914753	65034.712392	33.599949
834.344648	65125.066499	33.604967
834.989377	65227.175453	33.609984
835.938783	65322.147844	33.615002
836.852847	65423.928737	33.620020
837.202720	65540.362552	33.625037
838.148897	65641.450115	33.630055
839.174513	65760.106148	33.635072
839.511261	65870.133589	33.640090
840.503571	65981.772751	33.645108
841.326277	66101.172333	33.650125
842.178886	66213.202507	33.655143
842.855719	66328.625677	33.660160
843.676341	66445.991867	33.665178
844.674438	66571.276258	33.670196
845.195071	66686.183523	33.675213
846.378429	66802.069224	33.680231
847.121332	66934.415611	33.685248
848.019758	67063.361018	33.690266
848.870106	67177.590528	33.695284
849.870347	67309.062161	33.700301
851.032301	67421.186695	33.705319
851.889739	67535.284199	33.710336
852.561334	67659.434122	33.715354
853.668045	67782.956434	33.720372
854.141274	67897.802264	33.725389
855.329939	68024.277688	33.730407
856.250092	68138.260587	33.735424
857.146163	68265.083001	33.740442
857.790565	68377.702848	33.745460
859.112077	68504.070646	33.750477
860.039106	68615.450022	33.755495
860.672449	68734.579675	33.760512
861.424268	68853.045476	33.765530
862.388152	68954.158633	33.770548
863.575021	69079.761768	33.775565
864.498564	69200.875675	33.780583
865.551897	69315.980985	33.785600
866.018473	69435.995736	33.790618
866.953081	69540.366522	33.795636
867.519662	69662.047921	33.800653
868.653674	69781.423093	33.805671
869.284840	69896.930152	33.810688
869.924754	70030.786148	33.815706
871.199636	70140.383414	33.820724
871.720545	70266.647459	33.825741
872.595184	70400.498558	33.830759
873.625036	70524.397254	33.835776
874.542518	70656.712629	33.840794
875.429467	70770.734047	33.845812
876.301943	70908.136073	33.850829
877.192386	71014.633358	33.855847
878.333538	71136.051032	33.860864
879.472047	71261.567460	33.865882
880.107332	71382.052097	33.870900
880.598629	71500.297378	33.875917
881.458469	71623.364184	33.880935
882.734597	71746.375492	33.885952
883.619973	71880.019004	33.890970
884.307938	71985.201295	33.895988
885.178719	72103.032983	33.901005
885.933033	72235.473554	33.906023
887.023176	72348.932181	33.911040
887.923393	72472.800264	33.916058
889.030299	72590.722029	33.921076
889.527804	72712.520603	33.926093
890.718045	72823.789726	33.931111
891.523443	72941.358524	33.936128
892.331744	73048.119711	33.941146
893.441196	73158.139100	33.946164
894.044936	73267.395251	33.951181
894.832605	73387.549618	33.956199
895.816581	73501.853955	33.961216
896.238334	73630.816488	33.966234
897.487849	73743.642584	33.971252
898.276749	73866.208911	33.976269
899.130088	73997.916532	33.981287
899.850835	74108.808181	33.986304
900.522283	74231.029163	33.991322
901.546694	74361.856890	33.996340
902.320224	74494.187834	34.001357
903.201104	74625.995864	34.006375
904.078851	74755.578971	34.011392
904.780959	74891.219191	34.016410
905.538352	75015.536402	34.021428
906.588242	75164.446717	34.026445
907.611387	75306.240873	34.031463
908.660705	75448.499641	34.036480
909.349480	75586.404268	34.041498
910.647830	75717.333895	34.046516
911.452590	75864.031516	34.051533
912.111533	75999.103798	34.056551
913.368662	76139.896903	34.061568
913.917214	76276.981484	34.066586
915.061097	76412.488411	34.071604
915.826064	76562.796159	34.076621
916.730263	76711.620806	34.081639
917.941910	76842.362691	34.086656
918.554394	76986.259551	34.091674
919.932014	77132.143424	34.096692
920.530190	77268.207551	34.101709
921.585888	77421.154917	34.106727
922.307511	77561.533235	34.111744
923.510652	77706.836166	34.116762
924.481587	77848.724772	34.121780
925.288024	77985.296484	34.126797
925.844571	78144.916129	34.131815
927.134608	78291.543164	34.136832
927.963995	78434.281205	34.141850
928.848257	78578.927737	34.146868
929.680891	78734.090641	34.151885
930.671651	78881.707218	34.156903
932.236237	79025.130795	34.161920
932.990620	79171.554844	34.166938
934.195083	79312.737226	34.171956
934.981311	79454.976487	34.176973
936.097379	79593.233720	34.181991
936.984972	79735.875496	34.187008
938.078160	79877.851576	34.192026
938.953904	80013.430953	34.197044
940.278533	80149.215257	34.202061
940.794777	80285.342816	34.207079
941.781267	80431.357073	34.212096
942.734511	80572.310509	34.217114
943.503833	80708.379774	34.222132
944.739003	80845.448279	34.227149
945.396273	80985.213275	34.232167
946.384177	81130.175297	34.237184
947.366523	81274.019394	34.242202
948.386279	81414.150943	34.247220
949.337432	81557.293428	34.252237
950.340369	81692.355663	34.257255
951.436879	81819.254676	34.262272
952.188406	81963.818222	34.267290
953.340694	82088.153577	34.272308
954.157284	82213.835750	34.277325
954.838786	82356.110460	34.282343
956.001147	82474.682661	34.287360
956.645858	82605.950237	34.292378
957.742251	82739.193742	34.297396
958.159203	82868.020385	34.302413
959.486399	83014.292160	34.307431
960.170703	83148.669088	34.312448
960.925506	83298.770176	34.317466
962.013143	83439.630461	34.322484
962.856694	83586.245244	34.327501
963.771186	83735.000418	34.332519
964.745977	83877.786471	34.337536
965.524903	84021.308103	34.342554
966.571874	84173.277339	34.347572
967.791214	84323.219674	34.352589
968.510817	84483.059161	34.357607
969.537024	84639.476605	34.362624
970.165344	84794.790339	34.367642
971.340787	84950.217113	34.372660
972.483188	85095.450607	34.377677
973.238149	85264.673154	34.382695
974.187189	85419.444472	34.387712
975.620192	85578.483805	34.392730
976.434567	85731.463454	34.397748
977.550176	85896.404114	34.402765
978.584591	86058.537222	34.407783
979.525001	86200.033360	34.412800
980.598915	86363.978098	34.417818
981.541108	86514.910512	34.422836
982.659948	86677.502188	34.427853
983.387532	86834.192497	34.432871
984.673230	86988.779283	34.437888
986.204106	87150.723924	34.442906
987.194238	87302.273594	34.447924
988.275102	87445.658719	34.452941
989.182602	87609.259952	34.457959
990.018003	87746.308781	34.462976
991.326714	87898.296856	34.467994
991.966288	88038.391958	34.473012
993.375343	88189.264199	34.478029
993.938345	88346.105640	34.483047
994.996013	88497.822650	34.488064
995.973271	88652.110580	34.493082
997.011763	88808.503069	34.498100
998.039259	88959.012952	34.503117
999.045799	89122.823390	34.508135
1000.392929	89275.073375	34.513152
1001.122982	89424.065897	34.518170
1002.324128	89583.056588	34.523188
1003.391425	89720.996079	34.528205
1004.261963	89884.796249	34.533223
1004.965075	90027.601194	34.538240
1005.982289	90190.803284	34.543258
1007.025427	90339.781366	34.548276
1008.464451	90504.776509	34.553293
1009.080504	90657.668788	34.558311
1009.981021	90799.698863	34.563328
1011.037429	90976.133578	34.568346
1012.040828	91118.268767	34.573364
1013.301865	91274.868368	34.578381
1014.234944	91431.257389	34.583399
1014.751937	91584.488361	34.588416
1015.891596	91745.054119	34.593434
1017.181030	91907.083541	34.598452
1018.230422	92064.444768	34.603469
1019.112511	92218.505466	34.608487
1020.433123	92364.323461	34.613504
1021.330403	92503.655098	34.618522
1022.165040	92655.144021	34.623540
1023.269174	92791.430301	34.628557
1024.041408	92945.969479	34.633575
1025.226160	93078.940043	34.638592
1026.116672	93238.044080	34.643610
1026.792136	93391.994436	34.648628
1027.912474	93538.301954	34.653645
1028.723645	93705.251903	34.658663
1029.760314	93855.923638	34.663680
1030.601997	94019.528584	34.668698
1031.400895	94183.983555	34.673716
1032.812790	94348.287629	34.678733
1033.328578	94519.748150	34.683751
1034.501931	94691.297363	34.688768
1035.387744	94861.300157	34.693786
1036.595729	95027.769338	34.698804
1038.151429	95197.131955	34.703821
1038.500783	95385.641202	34.708839
1039.570648	95550.269346	34.713856
1040.894571	95726.105330	34.718874
1042.126898	95901.843759	34.723892
1043.333505	96071.687855	34.728909
1043.995810	96250.517215	34.733927
1045.393665	96424.953236	34.738944
1046.396632	96605.507646	34.743962
1047.270172	96778.962987	34.748980
1048.352899	96947.402833	34.753997
1049.337618	97133.237376	34.759015
1050.203254	97308.096736	34.764032
1051.791593	97480.008024	34.769050
1052.732288	97668.506342	34.774068
1053.998413	97844.493383	34.779085
1054.870095	98024.687196	34.784103
1056.482724	98192.547636	34.789120
1057.389054	98367.882432	34.794138
1058.385828	98547.267931	34.799156
1059.537582	98719.323159	34.804173
1060.796653	98896.369628	34.809191
1061.876720	99074.288955	34.814208
1063.011731	99243.488877	34.819226
1063.786598	99414.598156	34.824244
1065.267411	99585.832451	34.829261
1065.924478	99763.041466	34.834279
1067.135024	99927.852247	34.839296
1068.500357	100104.110802	34.844314
1069.478860	100276.363479	34.849332
1070.651621	100436.074396	34.854349
1071.921901	100618.360683	34.859367
1072.726850	100780.983700	34.864384
1073.527389	100947.242756	34.869402
1074.444088	101130.477546	34.874420
1075.646983	101306.182383	34.879437
1076.854072	101482.774152	34.884455
1078.059640	101652.852088	34.889472
1078.942344	101823.554378	34.894490
1080.105575	102009.059391	34.899508
1081.184103	102182.460662	34.904525
1082.269655	102370.285882	34.909543
1083.071004	102537.086908	34.914560
1084.668709	102707.372874	34.919578
1085.533604	102893.395764	34.924596
1086.744129	103068.275470	34.929613
1087.733845	103248.461132	34.934631
1088.672277	103414.966505	34.939648
1089.896791	103590.214658	34.944666
1090.693984	103764.420169	34.949684
1091.661346	103936.433081	34.954701
1092.703165	104103.419653	34.959719
1093.835520	104264.313302	34.964736
1094.747256	104431.893377	34.969754
1096.030894	104604.212985	34.974772
1097.450918	104776.713810	34.979789
1098.574088	104944.832112	34.984807
1099.623825	105111.139862	34.989824
1100.862805	105286.852876	34.994842
1101.337882	105451.003381	34.999860
1102.483577	105633.547989	35.004877
1103.725800	105800.689487	35.009895
1104.631951	105982.288201	35.014912
1105.835853	106161.736451	35.019930
1106.754484	106341.714367	35.024948
1107.953239	106526.738798	35.029965
1108.968783	106706.563832	35.034983
1109.881517	106891.650744	35.040000
1111.142530	107077.162664	35.045018
1112.208708	107268.255809	35.050036
1113.349299	107462.035902	35.055053
1114.507243	107638.613788	35.060071
1115.401678	107833.247893	35.065088
1116.610579	108028.388737	35.070106
1117.385291	108227.567391	35.075124
1118.996954	108418.540528	35.080141
1119.577920	108631.598778	35.085159
1121.049182	108824.079994	35.090176
1122.312907	109025.387698	35.095194
1122.915523	109230.327609	35.100212
1124.395709	109420.341523	35.105229
1125.654901	109622.617099	35.110247
1126.839941	109828.174585	35.115264
1128.165089	110025.337346	35.120282
1129.074315	110233.438948	35.125300
1130.631305	110429.679577	35.130317
1131.553539	110628.940103	35.135335
1132.483462	110823.868449	35.140352
1133.687279	111030.622626	35.145370
1134.806526	111249.287496	35.150388
1135.859028	111428.187635	35.155405
1137.358743	111635.480163	35.160423
1138.214499	111846.440463	35.165440
1139.442861	112050.943295	35.170458
1140.480102	112260.166528	35.175476
1141.884714	112460.754059	35.180493
1143.135935	112666.017755	35.185511
1144.152406	112877.187357	35.190528
1145.605332	113074.920886	35.195546
1146.499815	113279.500622	35.200564
1147.873135	113482.596446	35.205581
1148.995736	113681.161680	35.210599
1150.172774	113884.026816	35.215616
1151.497267	114080.331740	35.220634
1152.382915	114282.487775	35.225652
1153.371067	114492.597353	35.230669
1154.535717	114692.353703	35.235687
1155.693227	114896.192245	35.240704
1156.864378	115110.913233	35.245722
1157.972412	115315.345780	35.250740
1159.220556	115525.559424	35.255757
1160.637492	115727.067821	35.260775
1161.666675	115927.121345	35.265792
1162.968463	116133.035480	35.270810
1164.016489	116337.345927	35.275828
1165.373630	116540.897200	35.280845
1166.392049	116743.973761	35.285863
1167.627961	116942.619157	35.290880
1168.957270	117137.005854	35.295898
1169.567254	117321.743719	35.300916
1170.829740	117516.524150	35.305933
1172.282243	117698.781077	35.310951
1173.144765	117893.668189	35.315968
1174.471696	118089.202091	35.320986
1175.496044	118279.174058	35.326004
1176.420562	118476.500364	35.331021
1177.412934	118682.559944	35.336039
1178.295276	118893.226193	35.341056
1179.685500	119096.511277	35.346074
1180.558967	119305.940182	35.351092
1181.757049	119520.461596	35.356109
1183.140230	119729.644551	35.361127
1183.740564	119951.680878	35.366144
1185.305176	120167.895155	35.371162
1186.435280	120387.997116	35.376180
1187.602351	120603.773441	35.381197
1189.001874	120826.571313	35.386215
1189.923334	121050.565053	35.391232
1191.398619	121266.612085	35.396250
1192.413728	121500.338788	35.401268
1193.752487	121729.527751	35.406285
1195.331188	121940.747038	35.411303
1196.036630	122174.948438	35.416320
1197.355488	122405.210409	35.421338
1198.412243	122630.549696	35.426356
1199.801873	122856.963556	35.431373
1200.927151	123081.940072	35.436391
1202.135541	123310.592442	35.441408
1203.706745	123538.451527	35.446426
1204.832734	123771.759458	35.451444
1205.961379	124000.012027	35.456461
1207.312332	124225.783569	35.461479
1208.041956	124464.029030	35.466496
1209.675147	124682.533317	35.471514
1211.060430	124929.076773	35.476532
1212.274996	125154.168035	35.481549
1213.752443	125376.682690	35.486567
1214.901974	125605.907114	35.491584
1216.735921	125837.301491	35.496602
1217.999106	126049.362171	35.501620
1219.213695	126277.680992	35.506637
1220.731467	126492.288238	35.511655
1221.825904	126715.775826	35.516672
1222.963456	126932.705076	35.521690
1224.332844	127149.711602	35.526708
1225.349821	127363.888027	35.531725
1226.813033	127574.810751	35.536743
1227.698441	127807.225942	35.541760
1228.997485	128004.362889	35.546778
1230.252506	128239.724228	35.551796
1231.505663	128464.060100	35.556813
1232.602128	128680.298530	35.561831
1233.874452	128905.407602	35.566848
1235.269256	129126.822117	35.571866
1236.317633	129351.819302	35.576884
1237.697992	129571.160521	35.581901
1239.241448	129781.907414	35.586919
1240.200178	130006.163537	35.591936
1241.429243	130224.165298	35.596954
1242.848208	130445.014655	35.601972
1243.858562	130674.007850	35.606989
1245.449058	130883.195123	35.612007
1246.366283	131111.395575	35.617024
1247.959050	131320.598022	35.622042
1249.442103	131545.006512	35.627060
1250.319845	131761.682450	35.632077
1251.556522	131958.955808	35.637095
1252.341580	132165.470370	35.642112
1253.818226	132367.536442	35.647130
1254.880932	132577.138946	35.652148
1255.912712	132780.713641	35.657165
1257.596345	132995.375793	35.662183
1258.511725	133217.126155	35.667200
1259.500451	133426.239299	35.672218
1260.784908	133638.385516	35.677236
1261.761433	133861.588070	35.682253
1263.585844	134076.221421	35.687271
1264.535758	134303.513573	35.692288
1265.725712	134526.013474	35.697306
1267.299765	134753.712698	35.702324
1268.194885	134989.132473	35.707341
1269.495410	135210.896096	35.712359
1270.707152	135438.355672	35.717376
1271.786756	135661.540752	35.722394
1273.213269	135901.506739	35.727412
1274.516109	136144.233431	35.732429
1276.134786	136383.017408	35.737447
1277.546838	136618.223865	35.742464
1278.617554	136845.665683	35.747482
1279.796562	137078.454247	35.752500
1280.921788	137331.197089	35.757517
1282.506400	137564.048775	35.762535
1283.625852	137805.689425	35.767552
1285.393547	138034.532904	35.772570
1286.638665	138279.047008	35.777588
1287.513070	138522.964830	35.782605
1289.248551	138749.586924	35.787623
1290.276233	138993.596910	35.792640
1291.856763	139227.918868	35.797658
1293.206729	139471.828295	35.802676
1294.180263	139704.605502	35.807693
1295.358168	139953.010055	35.812711
1297.056895	140208.760740	35.817728
1298.410699	140451.953756	35.822746
1299.711414	140683.326764	35.827764
1300.743655	140932.688110	35.832781
1302.241509	141171.221450	35.837799
1303.582034	141423.629358	35.842816
1305.092254	141669.404553	35.847834
1306.365526	141905.938511	35.852852
1307.173650	142155.941664	35.857869
1308.427576	142388.563783	35.862887
1310.147946	142641.906823	35.867904
1311.540772	142895.242423	35.872922
1312.857311	143143.190368	35.877940
1314.364858	143386.403820	35.882957
1315.606234	143630.816922	35.887975
1316.631991	143883.586228	35.892992
1318.132152	144120.959906	35.898010
1319.743836	144360.485254	35.903028
1320.887501	144615.890689	35.908045
1322.516550	144853.882023	35.913063
1323.686648	145105.583570	35.918080
1325.345324	145344.778027	35.923098
1326.739492	145586.528794	35.928116
1327.702069	145831.434218	35.933133
1329.398434	146064.945734	35.938151
1330.577852	146299.393894	35.943168
1331.776519	146548.044408	35.948186
1333.166739	146788.028355	35.953204
1334.367201	147026.269719	35.958221
1335.870474	147269.497511	35.963239
1337.368879	147510.914128	35.968256
1338.196435	147751.098853	35.973274
1339.922666	147970.387796	35.978292
1340.750653	148197.918081	35.983309
1342.419700	148420.922516	35.988327
1343.410944	148652.119316	35.993344
1345.008303	148881.632016	35.998362
1346.553454	149103.760551	36.003380
1347.588052	149349.108806	36.008397
1348.690053	149574.027575	36.013415
1349.870188	149817.401643	36.018432
1350.964045	150049.680924	36.023450
1352.626048	150300.905598	36.028468
1353.529722	150543.607110	36.033485
1354.952531	150789.027466	36.038503
1356.113378	151043.383982	36.043520
1357.579322	151302.904819	36.048538
1358.651351	151554.387538	36.053556
1359.776184	151821.083937	36.058573
1361.363429	152073.550389	36.063591
1362.538025	152349.932865	36.068608
1363.776799	152620.598827	36.073626
1365.358667	152887.049540	36.078644
1366.515381	153160.269720	36.083661
1368.101559	153430.351212	36.088679
1369.642125	153704.805619	36.093696
1370.883341	153978.081025	36.098714
1372.784175	154244.234671	36.103732
1373.653187	154524.831099	36.108749
1375.084832	154796.203404	36.113767
1376.326667	155080.560360	36.118784
1377.926679	155352.733210	36.123802
1379.432510	155627.600079	36.128820
1380.642059	155907.008414	36.133837
1382.164315	156184.629141	36.138855
1383.821305	156460.478946	36.143872
1384.956898	156741.491045	36.148890
1386.955347	157004.057146	36.153908
1388.036012	157283.407620	36.158925
1389.776322	157557.183437	36.163943
1391.191235	157841.797903	36.168960
1392.550327	158110.033301	36.173978
1394.322802	158388.300270	36.178996
1395.383676	158657.996725	36.184013
1396.668579	158928.342997	36.189031
1398.417191	159202.369577	36.194048
1400.028150	159481.254260	36.199066
1401.442792	159752.371083	36.204084
1402.837091	160015.969912	36.209101
1403.878798	160282.698860	36.214119
1405.698884	160564.474234	36.219136
1407.110810	160839.227032	36.224154
1408.618288	161097.612429	36.229172
1409.890152	161373.432215	36.234189
1411.386261	161640.919415	36.239207
1412.620476	161916.444501	36.244224
1414.047143	162185.101165	36.249242
1415.854575	162456.081830	36.254260
1416.894477	162721.367550	36.259277
1418.638208	162988.949236	36.264295
1419.964218	163269.796686	36.269312
1421.246347	163537.318526	36.274330
1422.527260	163801.670307	36.279348
1424.022361	164087.582943	36.284365
1425.146407	164359.183425	36.289383
1426.968211	164628.069277	36.294400
1427.884877	164916.328744	36.299418
1429.755205	165182.025310	36.304436
1430.885975	165464.150036	36.309453
1432.149192	165730.673489	36.314471
1433.846097	165994.690730	36.319488
1435.277433	166262.103185	36.324506
1436.945951	166511.155870	36.329524
1437.728530	166773.704732	36.334541
1439.219228	167034.755069	36.339559
1440.954089	167293.076581	36.344576
1441.973406	167563.559497	36.349594
1443.673917	167826.749579	36.354612
1444.848350	168099.291068	36.359629
1446.283721	168373.592928	36.364647
1447.503450	168638.910135	36.369664
1448.654806	168929.060227	36.374682
1450.583537	169197.334322	36.379700
1451.522965	169495.720303	36.384717
1452.907583	169780.596568	36.389735
1454.566025	170064.274608	36.394752
1455.975934	170357.944092	36.399770
1457.339014	170643.704834	36.404788
1458.699642	170960.024631	36.409805
1460.227556	171244.442098	36.414823
1461.626218	171532.194718	36.419840
1463.231792	171848.594269	36.424858
1464.539100	172140.096567	36.429876
1466.097196	172450.962453	36.434893
1467.326430	172754.905096	36.439911
1468.891454	173046.827239	36.444928
1470.177539	173375.256740	36.449946
1471.918923	173673.041911	36.454964
1473.617431	173985.760099	36.459981
1474.711162	174294.811130	36.464999
1476.773661	174603.094904	36.470016
1478.136713	174926.039862	36.475034
1479.885128	175227.323407	36.480052
1481.152563	175538.879119	36.485069
1482.748746	175845.496438	36.490087
1484.275062	176154.246624	36.495104
1485.443059	176478.135084	36.500122
1486.944450	176777.146428	36.505140
1488.522947	177092.252150	36.510157
1490.274109	177407.597846	36.515175
1491.398051	177724.648289	36.520192
1493.150599	178048.805683	36.525210
1494.913566	178364.967675	36.530228
1496.287671	178686.399503	36.535245
1497.887309	178999.812927	36.540263
1499.594400	179309.098335	36.545280
1500.796296	179628.863811	36.550298
1502.643738	179937.380970	36.555316
1504.362135	180250.046231	36.560333
1505.920187	180559.630271	36.565351
1508.030925	180860.341761	36.570368
1509.016545	181176.915943	36.575386
1510.681745	181474.328391	36.580404
1512.208454	181780.992847	36.585421
1513.858614	182079.401191	36.590439
1516.077150	182387.681024	36.595456
1517.278773	182685.735315	36.600474
1518.942450	182973.459139	36.605492
1520.323416	183282.847149	36.610509
1521.828308	183576.299511	36.615527
1523.814918	183867.858766	36.620544
1525.189925	184177.202074	36.625562
1526.618011	184459.654290	36.630580
1528.434215	184759.496981	36.635597
1529.576815	185067.144718	36.640615
1531.442263	185363.060319	36.645632
1532.724678	185647.230874	36.650650
1534.439864	185926.507848	36.655668
1535.761857	186207.145917	36.660685
1536.926015	186476.539548	36.665703
1538.758656	186744.300775	36.670720
1539.797177	187018.833282	36.675738
1541.284316	187303.321072	36.680756
1542.653447	187583.805826	36.685773
1544.057705	187868.310111	36.690791
1545.849487	188156.534573	36.695808
1546.969781	188459.444158	36.700826
1548.506245	188746.977480	36.705844
1549.721351	189046.675538	36.710861
1551.241464	189351.618223	36.715879
1552.773232	189641.797103	36.720896
1554.381523	189957.353464	36.725914
1555.833892	190261.880421	36.730932
1557.485120	190570.565254	36.735949
1558.676935	190894.827624	36.740967
1560.505979	191203.232434	36.745984
1562.130242	191528.086872	36.751002
1563.843627	191833.276846	36.756020
1565.413202	192164.922707	36.761037
1566.481466	192483.082349	36.766055
1568.345988	192801.835688	36.771072
1569.360933	193143.658223	36.776090
1571.161829	193464.951779	36.781108
1572.643539	193808.097287	36.786125
1574.503048	194138.220425	36.791143
1575.817863	194466.213601	36.796160
1577.444448	194810.952905	36.801178
1579.165427	195145.471352	36.806196
1580.740075	195479.203203	36.811213
1582.062271	195821.205199	36.816231
1584.428322	196162.236712	36.821248
1585.535139	196493.715063	36.826266
1587.615860	196828.550906	36.831284
1589.263450	197173.629347	36.836301
1590.794726	197504.890290	36.841319
1592.329528	197848.899013	36.846336
1593.812232	198192.397567	36.851354
1595.833365	198530.286122	36.856372
1597.283259	198867.902542	36.861389
1598.638954	199213.928374	36.866407
1600.667402	199546.716873	36.871424
1602.164604	199881.613454	36.876442
1603.943464	200229.326545	36.881460
1605.670569	200567.591065	36.886477
1607.100060	200900.281828	36.891495
1609.015481	201245.438077	36.896512
1610.606242	201585.609075	36.901530
1612.179352	201915.106695	36.906548
1614.011990	202257.221594	36.911565
1615.151309	202601.839645	36.916583
1617.153780	202933.442111	36.921600
1618.719121	203262.553515	36.926618
1620.375029	203609.109760	36.931636
1622.499314	203931.161157	36.936653
1623.817045	204277.306586	36.941671
1625.546623	204603.120928	36.946688
1627.293072	204941.758055	36.951706
1628.962544	205270.530941	36.956724
1630.694890	205601.770826	36.961741
1632.035489	205941.952306	36.966759
1633.949966	206264.035535	36.971776
1635.348217	206605.530921	36.976794
1637.004555	206932.548068	36.981812
1638.727838	207261.891862	36.986829
1640.042259	207597.754957	36.991847
1641.770187	207916.510861	36.996864
1643.504167	208242.123799	37.001882
1644.828049	208552.860503	37.006900
1646.784229	208867.976269	37.011917
1648.278157	209179.982438	37.016935
1649.870004	209485.484970	37.021952
1651.768566	209819.863933	37.026970
1652.814863	210137.369670	37.031988
1654.624657	210447.258616	37.037005
1655.879537	210782.128668	37.042023
1658.133875	211101.927280	37.047040
1659.253202	211430.854119	37.052058
1660.706026	211759.396958	37.057076
1662.705205	212088.384110	37.062093
1664.393033	212426.896899	37.067111
1665.988444	212759.788157	37.072128
1667.441086	213101.466174	37.077146
1669.177242	213442.057377	37.082164
1670.593660	213785.978905	37.087181
1672.067859	214136.393866	37.092199
1674.119442	214479.247979	37.097216
1675.710567	214832.922517	37.102234
1677.698395	215181.351777	37.107252
1679.224862	215524.118687	37.112269
1680.674575	215882.671461	37.117287
1682.760490	216233.196384	37.122304
1684.061366	216589.846151	37.127322
1685.564271	216954.413409	37.132340
1687.783034	217309.669678	37.137357
1689.095563	217684.404897	37.142375
1691.156414	218037.861186	37.147392
1693.040220	218396.580012	37.152410
1694.697904	218759.782174	37.157428
1696.668801	219116.279478	37.162445
1697.847336	219479.614119	37.167463
1699.843287	219851.501342	37.172480
1701.718564	220206.062458	37.177498
1703.309581	220574.336284	37.182516
1705.474844	220933.423699	37.187533
1706.882479	221299.952363	37.192551
1708.761842	221661.400708	37.197568
1710.652169	222020.460899	37.202586
1712.171390	222398.505989	37.207604
1713.822535	222810.692676	37.212621
1715.486417	223184.703386	37.217639
1717.631851	223538.392352	37.222656
1719.315019	223908.363684	37.227674
1720.912513	224267.123674	37.232692
1722.629840	224636.151847	37.237709
1724.298618	225007.094155	37.242727
1726.029502	225364.311387	37.247744
1727.525595	225723.752835	37.252762
1729.523829	226098.403206	37.257780
1731.549511	226457.911685	37.262797
1732.804699	226830.299343	37.267815
1734.262238	227199.606620	37.272832
1735.959668	227576.851024	37.277850
1737.356188	227952.063376	37.282868
1739.249050	228318.253828	37.287885
1740.886956	228727.439716	37.292903
1742.911889	229100.621011	37.297920
1744.757463	229475.229972	37.302938
1746.725865	229862.621627	37.307956
1748.384485	230229.186021	37.312973
1750.172284	230613.663038	37.317991
1752.004146	230988.989442	37.323008
1753.394866	231364.161050	37.328026
1755.040567	231740.256719	37.333044
1757.093258	232114.863627	37.338061
1758.912617	232479.349500	37.343079
1760.249143	232839.242137	37.348096
1762.131545	233197.419740	37.353114
1763.571234	233561.818395	37.358132
1765.386470	233921.304157	37.363149
1767.036415	234292.147062	37.368167
1768.742402	234660.288963	37.373184
1770.642306	235027.561374	37.378202
1771.841284	235399.167003	37.383220
1773.563219	235783.718113	37.388237
1775.119754	236171.269369	37.393255
1777.247605	236558.930300	37.398272
1778.970353	236944.042555	37.403290
1780.464864	237348.193924	37.408308
1782.444940	237727.549824	37.413325
1784.005987	238133.215950	37.418343
1785.595859	238533.264277	37.423360
1787.658559	238926.351319	37.428378
1789.157749	239340.412754	37.433396
1791.347924	239748.975598	37.438413
1792.999315	240161.362328	37.443431
1794.833076	240567.470733	37.448448
1796.854201	240977.410075	37.453466
1798.220464	241394.316942	37.458484
1800.211604	241798.216892	37.463501
1802.260313	242218.746628	37.468519
1804.075359	242634.235156	37.473536
1805.982138	243048.185049	37.478554
1807.478529	243469.290697	37.483572
1809.366381	243889.036809	37.488589
1811.460109	244307.784248	37.493607
1813.009739	244735.843344	37.498624
1814.845643	245151.764067	37.503642
1816.815346	245591.922920	37.508660
1818.492675	246015.847463	37.513677
1820.387589	246439.355576	37.518695
1822.134884	246864.997039	37.523712
1824.130043	247308.329318	37.528730
1825.985522	247749.830790	37.533748
1827.539665	248168.316637	37.538765
1829.762903	248603.585422	37.543783
1831.568335	249040.955910	37.548800
1833.552554	249477.789252	37.553818
1835.491740	249915.849801	37.558836
1837.430648	250339.608853	37.563853
1839.062061	250786.078631	37.568871
1840.708522	251225.230195	37.573888
1842.756185	251657.990457	37.578906
1844.477668	252090.931916	37.583924
1846.439919	252533.690347	37.588941
1848.286651	252967.068954	37.593959
1850.556168	253401.571944	37.598976
1852.490509	253840.550687	37.603994
1854.034994	254280.254518	37.609012
1856.094980	254709.280254	37.614029
1857.946024	255153.785857	37.619047
1859.469743	255591.842437	37.624064
1861.733119	256027.566917	37.629082
1863.740902	256462.825656	37.634100
1865.803447	256900.895212	37.639117
1867.733877	257333.728177	37.644135
1869.450128	257763.040104	37.649152
1871.515696	258187.696377	37.654170
1873.234703	258617.058702	37.659188
1875.275451	259041.998519	37.664205
1876.874794	259483.548756	37.669223
1878.465474	259918.241486	37.674240
1880.597078	260340.651240	37.679258
1882.394991	260759.457945	37.684276
1884.236191	261171.627148	37.689293
1886.065667	261580.775186	37.694311
1887.978024	261985.844887	37.699328
1889.951566	262390.497892	37.704346
1891.321491	262818.900845	37.709364
1893.795079	263228.602388	37.714381
1895.391310	263641.700235	37.719399
1896.924202	264064.512351	37.724416
1898.980589	264486.932937	37.729434
1900.578713	264925.178907	37.734452
1902.517195	265353.029283	37.739469
1904.537892	265779.925860	37.744487
1906.013336	266221.569752	37.749504
1907.974721	266655.512099	37.754522
1909.823250	267108.982269	37.759540
1911.871325	267555.255393	37.764557
1913.919172	268006.761136	37.769575
1915.281703	268452.790913	37.774592
1917.277420	268898.842660	37.779610
1919.232852	269355.925428	37.784628
1921.232098	269817.217287	37.789645
1923.007791	270278.469264	37.794663
1924.696462	270749.794521	37.799680
1926.757779	271210.718635	37.804698
1928.395334	271683.194113	37.809716
1930.466352	272159.534716	37.814733
1932.608087	272644.296572	37.819751
1934.214109	273123.887729	37.824768
1936.222942	273595.358924	37.829786
1938.072605	274087.482451	37.834804
1940.104502	274583.512349	37.839821
1942.054906	275066.701095	37.844839
1943.637308	275561.583958	37.849856
1945.673650	276052.859915	37.854874
1947.382385	276561.868925	37.859892
1949.892891	277062.971314	37.864909
1951.708687	277556.871447	37.869927
1953.742918	278060.971426	37.874944
1955.965117	278561.940099	37.879962
1958.006545	279073.072781	37.884980
1960.016977	279572.676792	37.889997
1962.120531	280068.657075	37.895015
1963.996200	280571.887795	37.900032
1966.226695	281073.128026	37.905050
1968.082234	281571.736206	37.910068
1970.064017	282073.141710	37.915085
1972.309804	282580.750941	37.920103
1974.245452	283073.499224	37.925120
1976.322981	283568.051517	37.930138
1978.450571	284071.509887	37.935156
1980.523489	284571.851351	37.940173
1982.766691	285054.153713	37.945191
1984.620640	285558.820938	37.950208
1986.766080	286044.387637	37.955226
1988.805080	286549.224171	37.960244
1990.857647	287035.488752	37.965261
1993.078336	287520.733293	37.970279
1994.983128	288014.232713	37.975296
1997.193268	288495.690916	37.980314
1998.973431	288989.690014	37.985332
2000.885004	289469.162010	37.990349
2003.192251	289960.632039	37.995367
2004.988373	290440.906941	38.000384
2007.241720	290928.775356	38.005402
2009.246357	291411.501359	38.010420
2011.249847	291904.004608	38.015437
2013.269982	292365.515449	38.020455
2015.240976	292828.429617	38.025472
2017.493966	293277.020881	38.030490
2019.276224	293736.660712	38.035508
2021.638790	294188.786299	38.040525
2023.735068	294642.097030	38.045543
2025.392150	295094.183099	38.050560
2027.720318	295547.121700	38.055578
2029.594592	296000.336570	38.060596
2031.406380	296458.360247	38.065613
2033.349210	296913.033106	38.070631
2035.394337	297386.024922	38.075648
2037.550134	297847.287632	38.080666
2039.344225	298316.608498	38.085684
2041.004332	298785.720751	38.090701
2043.213782	299254.359164	38.095719
2044.717123	299744.725674	38.100736
2047.204413	300222.101371	38.105754
2048.990708	300719.095954	38.110772
2050.906925	301207.431338	38.115789
2052.916297	301688.205789	38.120807
2054.730466	302197.937625	38.125824
2056.910423	302700.596654	38.130842
2058.978724	303208.071431	38.135860
2061.160417	303711.511948	38.140877
2063.356288	304205.398118	38.145895
2065.094993	304724.321952	38.150912
2067.218702	305233.833258	38.155930
2069.750675	305751.553402	38.160948
2071.955356	306263.965878	38.165965
2073.980852	306766.094063	38.170983
2075.738009	307282.231316	38.176000
2078.095319	307793.085571	38.181018
2080.329363	308316.959564	38.186036
2081.869611	308835.103801	38.191053
2084.336575	309351.517227	38.196071
2086.385082	309888.464859	38.201088
2088.780981	310403.257928	38.206106
2090.727096	310926.070439	38.211124
2092.640451	311453.227322	38.216141
2094.984689	311979.141321	38.221159
2097.270291	312501.506183	38.226176
2099.287864	313030.336378	38.231194
2101.115287	313556.553265	38.236212
2103.389573	314086.679454	38.241229
2105.699113	314609.914353	38.246247
2107.559947	315150.613991	38.251264
2109.908793	315676.221663	38.256282
2112.303019	316212.736940	38.261300
2113.986240	316744.261578	38.266317
2116.417440	317274.160543	38.271335
2118.278980	317816.033130	38.276352
2120.934240	318340.275218	38.281370
2122.807428	318877.846205	38.286388
2124.807036	319412.878260	38.291405
2127.100623	319940.849441	38.296423
2129.173597	320477.892166	38.301440
2131.276035	321013.986173	38.306458
2133.473588	321546.657688	38.311476
2135.467522	322082.760790	38.316493
2137.818800	322618.318002	38.321511
2139.764588	323157.060651	38.326528
2141.940626	323694.643526	38.331546
2143.961222	324222.142276	38.336564
2146.132833	324771.624438	38.341581
2148.596234	325305.464424	38.346599
2150.515986	325844.518103	38.351616
2152.703865	326385.350730	38.356634
2154.798732	326915.022795	38.361652
2156.717060	327435.427098	38.366669
2159.166230	327943.248152	38.371687
2161.129540	328457.111216	38.376704
2163.363071	328964.273526	38.381722
2165.541663	329480.351520	38.386740
2167.175162	329997.428805	38.391757
2169.892890	330499.775575	38.396775
2171.629044	331035.054466	38.401792
2173.913714	331555.614979	38.406810
2176.144467	332067.370433	38.411828
2177.949359	332596.047915	38.416845
2180.293512	333120.747248	38.421863
2182.219867	333667.849954	38.426880
2184.612018	334202.888311	38.431898
2186.534431	334735.434983	38.436916
2188.666569	335286.701225	38.441933
2190.666855	335829.505019	38.446951
2192.820571	336395.961577	38.451968
2195.054637	336940.263755	38.456986
2197.718122	337496.394397	38.462004
2199.603225	338061.328725	38.467021
2201.399658	338613.402111	38.472039
2203.756881	339177.916174	38.477056
2206.021047	339751.272495	38.482074
2208.313632	340328.526473	38.487092
2210.206091	340908.174969	38.492109
2212.958262	341468.079952	38.497127
2214.884088	342057.354546	38.502144
2217.058985	342644.854984	38.507162
2219.471596	343219.009429	38.512180
2221.519041	343798.598000	38.517197
2224.024466	344388.408372	38.522215
2226.581228	344970.055946	38.527232
2228.607965	345555.946102	38.532250
2230.851687	346146.006093	38.537268
2233.083883	346739.918119	38.542285
2235.622940	347327.528685	38.547303
2237.626370	347908.494847	38.552320
2240.139239	348504.850165	38.557338
2242.303477	349094.783838	38.562356
2244.728165	349695.782103	38.567373
2247.098397	350292.238772	38.572391
2249.494295	350878.583243	38.577408
2251.487535	351469.554134	38.582426
2254.306255	352065.151510	38.587444
2256.474174	352653.159309	38.592461
2258.891590	353235.535356	38.597479
2261.065580	353831.037210	38.602496
2263.528827	354420.291603	38.607514
2266.014538	355000.653097	38.612532
2268.158752	355602.123374	38.617549
2270.355169	356169.042923	38.622567
2272.863436	356759.094466	38.627584
2274.999099	357345.367799	38.632602
2277.529578	357929.233353	38.637620
2279.716414	358520.276884	38.642637
2282.108841	359095.648868	38.647655
2284.338723	359687.759288	38.652672
2286.816540	360269.468677	38.657690
2289.057439	360857.297682	38.662708
2291.196141	361446.301903	38.667725
2293.437444	362023.432653	38.672743
2295.774086	362610.052793	38.677760
2298.074237	363196.517941	38.682778
2300.373282	363780.183858	38.687796
2302.250967	364381.084933	38.692813
2304.902160	364959.017731	38.697831
2307.505754	365539.232739	38.702848
2309.263459	366097.610441	38.707866
2311.588041	366647.718204	38.712884
2313.890777	367210.428699	38.717901
2316.065511	367768.078633	38.722919
2317.941430	368330.715860	38.727936
2320.383553	368897.157371	38.732954
2322.660574	369454.054824	38.737972
2324.647191	370040.084945	38.742989
2326.888218	370620.711826	38.748007
2329.041100	371200.608417	38.753024
2331.306709	371791.357976	38.758042
2333.653679	372380.765520	38.763060
2335.539449	372984.036666	38.768077
2337.514479	373584.670550	38.773095
2339.789290	374196.327801	38.778112
2342.304390	374809.456431	38.783130
2344.900541	375424.970210	38.788148
2346.900176	376055.381960	38.793165
2349.179350	376671.991065	38.798183
2351.580761	377309.515802	38.803200
2353.691183	377954.329336	38.808218
2356.163492	378583.298003	38.813236
2358.411988	379232.375421	38.818253
2360.773758	379874.194768	38.823271
2363.566226	380528.203517	38.828288
2365.829961	381179.953892	38.833306
2368.349238	381815.953940	38.838324
2370.416261	382482.721833	38.843341
2372.831862	383131.036311	38.848359
2374.871546	383795.297182	38.853376
2377.463829	384470.203328	38.858394
2380.097172	385135.910662	38.863412
2382.618099	385798.783223	38.868429
2385.080288	386459.243248	38.873447
2387.464257	387138.386731	38.878464
2389.934234	387799.806250	38.883482
2392.610256	388476.819250	38.888500
2395.076227	389154.486010	38.893517
2397.522598	389815.283747	38.898535
2400.174184	390487.440600	38.903552
2402.660826	391168.481980	38.908570
2405.046743	391828.942300	38.913588
2407.456717	392503.376111	38.918605
2410.142569	393165.354792	38.923623
2412.836762	393833.071182	38.928640
2415.107138	394498.662926	38.933658
2418.082861	395158.091302	38.938676
2420.525394	395830.822912	38.943693
2422.751950	396492.879689	38.948711
2425.414968	397147.626673	38.953728
2427.513314	397813.932529	38.958746
2429.990986	398468.173659	38.963764
2432.570367	399133.406910	38.968781
2435.162488	399797.710455	38.973799
2437.557666	400467.986174	38.978816
2439.706186	401139.376508	38.983834
2442.756374	401787.011279	38.988852
2445.242938	402457.503819	38.993869
2447.563013	403109.992445	38.998887
2449.888021	403755.877320	39.003904
2452.698577	404418.186884	39.008922
2454.938587	405089.645254	39.013940
2457.384121	405740.024731	39.018957
2459.432776	406399.600358	39.023975
2462.617050	407054.640542	39.028992
2464.863445	407732.544337	39.034010
2467.617885	408371.308733	39.039028
2469.500577	409016.585756	39.044045
2471.935065	409655.093937	39.049063
2474.514098	410280.390673	39.054080
2476.807443	410912.888586	39.059098
2479.498144	411526.916062	39.064116
2481.849347	412151.902470	39.069133
2483.759477	412784.748248	39.074151
2486.282754	413415.628646	39.079168
2488.434520	414058.155342	39.084186
2491.151907	414697.533604	39.089204
2493.119921	415352.722311	39.094221
2495.477015	416007.855552	39.099239
2497.919940	416672.986815	39.104256
2500.342431	417343.219791	39.109274
2502.785883	418006.062414	39.114292
2505.449549	418679.943067	39.119309
2507.666747	419357.298011	39.124327
2510.161369	420043.426367	39.129344
2512.337938	420737.412731	39.134362
2515.062881	421420.806613	39.139380
2517.096590	422121.690555	39.144397
2519.940025	422828.244490	39.149415
2522.267647	423538.610419	39.154432
2524.872655	424258.176322	39.159450
2527.315649	424961.747453	39.164468
2530.088796	425686.306891	39.169485
2532.156512	426403.265153	39.174503
2534.860897	427129.412895	39.179520
2537.311485	427864.693585	39.184538
2539.961253	428597.741883	39.189556
2542.533672	429336.399729	39.194573
2544.842738	430081.304665	39.199591
2547.841109	430823.642542	39.204608
2550.102765	431571.798571	39.209626
2552.738504	432315.617030	39.214644
2555.641442	433074.603287	39.219661
2558.236413	433824.757887	39.224679
2560.770116	434567.002540	39.229696
2563.177474	435328.780221	39.234714
2565.830262	436076.321250	39.239732
2568.202626	436840.686021	39.244749
2571.112804	437593.246183	39.249767
2573.909865	438356.325787	39.254784
2576.467023	439121.342019	39.259802
2578.947058	439882.195530	39.264820
2581.502687	440645.945415	39.269837
2584.062611	441414.930534	39.274855
2586.548006	442174.034940	39.279872
2589.041498	442957.903177	39.284890
2591.812285	443725.356206	39.289908
2594.559042	444500.931372	39.294925
2597.297908	445269.903593	39.299943
2599.972274	446035.520383	39.304960
2602.619236	446815.177294	39.309978
2605.583790	447584.687350	39.314996
2608.043548	448361.182707	39.320013
2610.496195	449121.768795	39.325031
2613.457590	449899.237965	39.330048
2615.867191	450672.824588	39.335066
2618.834380	451436.985073	39.340084
2621.448629	452202.389649	39.345101
2624.096758	452965.990580	39.350119
2626.859999	453734.753063	39.355136
2629.492954	454501.232968	39.360154
2631.932713	455259.069600	39.365172
2635.037507	456023.948548	39.370189
2637.642318	456795.201541	39.375207
2640.497602	457555.614844	39.380224
2642.911605	458298.124486	39.385242
2645.706055	459020.170102	39.390260
2648.458365	459736.736944	39.395277
2650.985467	460454.376942	39.400295
2654.144722	461166.073603	39.405312
2656.517706	461881.412939	39.410330
2659.216903	462593.791517	39.415348
2661.452293	463301.065357	39.420365
2664.309451	464021.908448	39.425383
2666.927454	464745.139966	39.430400
2669.647301	465464.486957	39.435418
2672.229525	466203.640817	39.440436
2675.210742	466929.207737	39.445453
2677.452625	467669.372580	39.450471
2680.401970	468398.629064	39.455488
2682.918566	469145.715750	39.460506
2685.267987	469875.772984	39.465524
2687.876254	470613.540581	39.470541
2690.514700	471367.947466	39.475559
2693.290014	472126.090871	39.480576
2695.644668	472873.310403	39.485594
2698.363469	473634.181038	39.490612
2701.249600	474401.964352	39.495629
2703.901393	475171.573237	39.500647
2706.659194	475938.001079	39.505664
2709.467151	476723.582551	39.510682
2711.869877	477497.025186	39.515700
2714.701241	478276.829274	39.520717
2717.125281	479058.839007	39.525735
2720.316561	479840.385707	39.530752
2722.553584	480639.831765	39.535770
2725.328621	481441.224195	39.540788
2728.286478	482234.219381	39.545805
2730.584141	483031.226894	39.550823
2733.602051	483838.380089	39.555840
2735.941728	484648.940853	39.560858
2738.874054	485462.951405	39.565876
2741.953001	486275.739310	39.570893
2744.602440	487102.190376	39.575911
2747.360504	487902.386627	39.580928
2750.412244	488721.628246	39.585946
2753.091572	489549.776194	39.590964
2756.079365	490365.973210	39.595981
2758.641658	491185.482464	39.600999
2761.312782	491996.608002	39.606016
2764.097974	492837.349232	39.611034
2767.052587	493661.823260	39.616052
2770.030199	494494.226239	39.621069
2772.171943	495325.212717	39.626087
2775.320535	496140.704923	39.631104
2778.439805	496990.015580	39.636122
2781.087403	497816.760116	39.641140
2783.987245	498646.701369	39.646157
2786.404306	499482.229913	39.651175
2789.614570	500302.957762	39.656192
2792.941999	501137.799074	39.661210
2795.494971	501972.322519	39.666228
2798.474395	502795.436245	39.671245
2801.502302	503637.059467	39.676263
2804.159704	504450.763055	39.681280
2806.722611	505287.436010	39.686298
2809.928918	506112.261558	39.691316
2812.855918	506942.385403	39.696333
2815.603310	507761.303323	39.701351
2818.777781	508584.344088	39.706368
2821.216447	509399.448268	39.711386
2823.898314	510224.552939	39.716404
2826.891061	511044.472407	39.721421
2829.565911	511859.109397	39.726439
2832.577400	512644.969665	39.731456
2835.390220	513424.120287	39.736474
2838.072727	514198.667584	39.741492
2841.147896	514979.562491	39.746509
2843.612469	515763.492263	39.751527
2846.697071	516542.291688	39.756544
2849.539389	517325.072661	39.761562
2852.077126	518109.275077	39.766580
2854.933266	518899.531843	39.771597
2857.615094	519691.590453	39.776615
2860.435291	520493.610477	39.781632
2863.005682	521293.916877	39.786650
2865.690619	522107.158403	39.791668
2868.378620	522909.828657	39.796685
2871.279675	523739.065291	39.801703
2873.848095	524563.778460	39.806720
2877.015786	525389.656995	39.811738
2879.265830	526236.691209	39.816756
2882.521311	527073.138380	39.821773
2885.270026	527915.211314	39.826791
2888.216961	528770.798280	39.831808
2890.922928	529621.944997	39.836826
2893.587116	530491.324379	39.841844
2896.316899	531349.264479	39.846861
2899.439796	532227.375769	39.851879
2902.229636	533096.982576	39.856896
2905.434493	533968.381622	39.861914
2908.266093	534867.319810	39.866932
2911.270060	535743.627747	39.871949
2913.919118	536638.811956	39.876967
2916.899461	537522.513534	39.881984
2919.959552	538422.902802	39.887002
2922.720248	539330.479420	39.892020
2926.041957	540227.944228	39.897037
2928.924659	541131.813567	39.902055
2931.641389	542036.105178	39.907072
2935.087325	542952.793561	39.912090
2937.907874	543854.788133	39.917108
2940.760813	544769.041182	39.922125
2943.531234	545687.220827	39.927143
2946.862862	546607.610749	39.932160
2949.927653	547527.229226	39.937178
2952.824685	548443.294448	39.942196
2956.281895	549351.161951	39.947213
2959.261330	550269.957515	39.952231
2962.352347	551195.911832	39.957248
2965.387610	552104.570812	39.962266
2968.116074	553016.888798	39.967284
2971.520680	553926.872594	39.972301
2974.291882	554850.016449	39.977319
2977.128518	555761.527851	39.982336
2980.444862	556668.425902	39.987354
2983.328534	557591.412596	39.992372
2986.662112	558511.095807	39.997389
2989.032184	559423.991319	40.002407
2992.222371	560354.271236	40.007424
2995.449901	561276.994711	40.012442
2998.298327	562204.136053	40.017460
3001.266860	563117.430210	40.022477
3004.042268	564047.315784	40.027495
3007.172140	564972.155098	40.032512
3010.407178	565883.704671	40.037530
3013.382462	566825.359525	40.042548
3016.503663	567747.240217	40.047565
3019.660922	568663.677016	40.052583
3022.713910	569582.173866	40.057600
3026.011503	570496.849775	40.062618
3028.485280	571403.715474	40.067636
3031.719205	572287.303849	40.072653
3034.439493	573169.008138	40.077671
3037.683047	574036.262489	40.082688
3040.670429	574915.291400	40.087706
3043.754041	575793.941793	40.092724
3046.447413	576664.767941	40.097741
3049.411596	577552.897152	40.102759
3052.450492	578438.141370	40.107776
3055.291453	579333.688262	40.112794
3058.230048	580221.530200	40.117812
3060.816281	581114.983542	40.122829
3064.118654	582023.449458	40.127847
3066.978911	582942.150824	40.132864
3070.204313	583863.079617	40.137882
3072.793933	584793.369455	40.142900
3075.888454	585722.903165	40.147917
3078.701674	586665.446021	40.152935
3081.961667	587609.495820	40.157952
3085.004553	588555.462148	40.162970
3087.414952	589511.231444	40.167988
3090.775890	590472.079894	40.173005
3093.787283	591436.466428	40.178023
3096.967814	592425.349472	40.183040
3099.879294	593391.397452	40.188058
3103.071976	594385.175062	40.193076
3105.802374	595369.827777	40.198093
3109.294660	596360.333240	40.203111
3111.955561	597361.359911	40.208128
3115.384639	598366.230673	40.213146
3118.245088	599385.480553	40.218164
3121.626017	600384.826216	40.223181
3125.130896	601403.041047	40.228199
3127.744434	602425.568251	40.233216
3131.441690	603447.575445	40.238234
3134.355698	604470.121028	40.243252
3137.693425	605487.049573	40.248269
3140.963638	606521.164284	40.253287
3144.134043	607550.797439	40.258304
3147.247299	608577.343969	40.263322
3150.387335	609612.548240	40.268340
3153.838434	610642.102724	40.273357
3157.294377	611682.016587	40.278375
3160.261809	612714.261201	40.283392
3163.561824	613741.453829	40.288410
3166.719428	614790.628914	40.293428
3169.676449	615812.935000	40.298445
3172.992218	616868.337102	40.303463
3176.451756	617911.015333	40.308480
3179.777219	618944.818068	40.313498
3182.711343	620005.179763	40.318516
3186.026902	621028.839328	40.323533
3189.390935	622084.928730	40.328551
3192.257954	623124.606399	40.333568
3195.618426	624166.800670	40.338586
3198.434633	625214.029713	40.343604
3201.757480	626263.021220	40.348621
3205.207676	627323.227751	40.353639
3208.650985	628381.631679	40.358656
3211.647096	629437.556661	40.363674
3214.520767	630485.456554	40.368692
3217.999297	631539.344228	40.373709
3221.266742	632593.910007	40.378727
3224.359452	633661.428099	40.383744
3227.608194	634703.553691	40.388762
3230.904764	635770.972209	40.393780
3234.310778	636823.390930	40.398797
3237.386956	637878.002670	40.403815
3240.475013	638919.930913	40.408832
3244.062011	639933.183540	40.413850
3247.119479	640954.305518	40.418868
3250.008046	641961.586205	40.423885
3253.182335	642973.558460	40.428903
3256.286182	643984.294684	40.433920
3259.661317	644991.345025	40.438938
3262.843071	646020.665076	40.443956
3266.079132	647042.691864	40.448973
3269.412474	648076.961996	40.453991
3272.341771	649108.550271	40.459008
3275.846287	650133.408205	40.464026
3278.694728	651184.183720	40.469044
3281.580746	652224.676612	40.474061
3285.349955	653259.732962	40.479079
3287.753760	654338.199776	40.484096
3291.091621	655399.308308	40.489114
3294.530095	656487.830277	40.494132
3298.003205	657554.610868	40.499149
3301.111307	658642.499462	40.504167
3304.288795	659736.080938	40.509184
3307.948524	660830.156887	40.514202
3310.490135	661925.488308	40.519220
3314.118716	663035.747771	40.524237
3317.434392	664151.305946	40.529255
3320.413424	665276.842335	40.534272
3323.776911	666397.704798	40.539290
3327.702151	667533.517492	40.544308
3331.047447	668656.157115	40.549325
3334.185534	669779.891795	40.554343
3337.607438	670922.842652	40.559360
3340.965925	672063.974639	40.564378
3344.051815	673208.195253	40.569396
3347.624085	674358.211687	40.574413
3351.361476	675501.497598	40.579431
3354.563637	676657.207090	40.584448
3358.238416	677805.091093	40.589466
3361.586533	678964.663521	40.594484
3364.715649	680124.573529	40.599501
3368.363759	681286.238971	40.604519
3371.730726	682447.604942	40.609536
3375.230361	683608.106248	40.614554
3378.862550	684769.232567	40.619572
3382.232010	685925.586407	40.624589
3385.725682	687089.666194	40.629607
3389.540150	688254.238125	40.634624
3393.250928	689399.815403	40.639642
3396.414106	690568.860636	40.644660
3399.946626	691716.007658	40.649677
3403.568371	692872.766842	40.654695
3406.830352	694044.317690	40.659712
3410.424367	695193.189284	40.664730
3413.733710	696348.951677	40.669748
3417.179325	697505.928737	40.674765
3420.940902	698668.205287	40.679783
3423.927448	699827.580105	40.684800
3427.424499	700979.033806	40.689818
3430.838299	702143.681707	40.694836
3434.668585	703310.285470	40.699853
3438.264388	704461.459941	40.704871
3441.323414	705623.716810	40.709888
3444.807605	706777.077998	40.714906
3448.098675	707936.705598	40.719924
3451.930127	709097.374846	40.724941
3455.070851	710258.544920	40.729959
3458.560684	711413.013447	40.734976
3462.599540	712565.601023	40.739994
3465.970212	713725.219837	40.745012
3469.234843	714857.090223	40.750016
3473.100339	715934.545432	40.755021
3476.069359	716979.271757	40.760026
3479.223887	717947.605517	40.765031
3482.317607	718859.153003	40.770036
3485.535641	719710.232595	40.775040
3488.689486	720490.035040	40.780045
3491.424856	721206.868661	40.785050
3494.425980	721852.853701	40.790055
3496.675794	722431.247634	40.795060
3499.083581	722937.354493	40.800064
3501.940189	723384.819687	40.805069
3503.778999	723781.081028	40.810074
3506.095503	724106.322844	40.815079
3507.772730	724378.132991	40.820084
3509.541071	724594.612323	40.825088
3511.618926	724768.713214	40.830093
3512.953126	724896.151808	40.835098
3514.346655	724965.746991	40.840103
3515.774304	725018.635711	40.845108
3516.860988	725014.492291	40.850112
3518.773134	724971.707966	40.855117
3519.257608	724894.171891	40.860122
3520.593212	724766.888244	40.865127
3521.553849	724636.690939	40.870132
3522.087582	724471.127329	40.875136
3523.167962	724269.341025	40.880141
3523.776012	724057.864011	40.885146
3524.555371	723803.877981	40.890151
3525.278277	723552.074276	40.895156
3525.700636	723268.590110	40.900160
3526.239133	722955.584129	40.905165
3526.727269	722637.815881	40.910170
3527.336033	722299.740629	40.915175
3527.836101	721948.532359	40.920180
3528.127718	721580.388473	40.925184
3528.380558	721205.293642	40.930189
3528.427951	720812.961582	40.935194
3528.892851	720408.146384	40.940199
3529.178499	720003.936052	40.945204
3529.174574	719591.621352	40.950208
3529.450968	719158.610338	40.955213
3529.296558	718736.657542	40.960218
3529.656339	718289.751187	40.965223
3529.816947	717853.368649	40.970228
3529.958901	717404.714956	40.975232
3529.785478	716956.982069	40.980237
3529.655250	716504.604758	40.985242
3529.675348	716047.068558	40.990247
3529.831408	715583.581235	40.995252
3529.479310	715133.299983	41.000256
3529.803591	714668.593442	41.005261
3529.984887	714211.327863	41.010266
3529.833433	713727.047949	41.015271
3530.082964	713258.901799	41.020276
3529.346321	712796.351361	41.025280
3529.448547	712314.082805	41.030285
3529.223105	711855.615442	41.035290
3529.297711	711386.104220	41.040295
3529.400052	710910.853985	41.045300
3528.955951	710445.049603	41.050304
3529.096176	709966.662638	41.055309
3528.540270	709509.116222	41.060314
3528.832043	709036.460917	41.065319
3528.769178	708566.370230	41.070324
3528.471651	708104.038677	41.075328
3528.466848	707630.311854	41.080333
3528.406535	707163.222613	41.085338
3528.345538	706693.575241	41.090343
3528.094923	706233.717763	41.095348
3528.194492	705766.923692	41.100352
3527.706511	705304.870310	41.105357
3527.545643	704845.669082	41.110362
3527.368908	704394.493747	41.115367
3527.271314	703936.177656	41.120372
3526.530465	703483.010892	41.125376
3527.199477	703034.655986	41.130381
3526.455474	702601.963517	41.135386
3526.385518	702152.442658	41.140391
3526.482984	701713.356083	41.145396
3526.246058	701273.308576	41.150400
3526.276740	700830.163227	41.155405
3525.994724	700388.488204	41.160410
3525.721018	699956.779668	41.165415
3525.493742	699526.632730	41.170420
3525.458663	699096.184460	41.175424
3525.150454	698662.827191	41.180429
3524.959382	698236.339209	41.185434
3525.161517	697811.903461	41.190439
3524.936160	697386.374188	41.195444
3524.380193	696971.817068	41.200448
3524.850284	696546.033181	41.205453
3524.497867	696138.811889	41.210458
3524.115704	695726.653824	41.215463
3523.909786	695309.922204	41.220468
3523.919455	694905.816825	41.225472
3523.669361	694499.149698	41.230477
3523.396558	694105.647548	41.235482
3523.267171	693687.036561	41.240487
3523.218396	693299.579532	41.245492
3522.783950	692909.781562	41.250496
3522.725951	692510.154628	41.255501
3522.465997	692117.457822	41.260506
3522.388046	691732.375037	41.265511
3522.530789	691353.806388	41.270516
3521.829163	690974.664305	41.275520
3521.937410	690593.780553	41.280525
3521.386512	690219.308367	41.285530
3521.485533	689852.077794	41.290535
3521.222288	689484.643089	41.295540
3520.903589	689133.574549	41.300544
3521.118560	688759.313388	41.305549
3520.830147	688405.175766	41.310554
3520.872624	688049.426863	41.315559
3520.221551	687693.728437	41.320564
3520.138140	687342.750428	41.325568
3520.059236	686994.097463	41.330573
3519.950021	686652.803008	41.335578
3519.705202	686304.200573	41.340583
3519.348035	685966.654510	41.345588
3519.450307	685628.821047	41.350592
3519.649234	685288.021818	41.355597
3519.166739	684958.324804	41.360602
3518.822479	684634.567588	41.365607
3518.820848	684296.303411	41.370612
3518.534617	683974.504742	41.375616
3518.780762	683654.001197	41.380621
3518.623290	683340.076030	41.385626
3518.496188	683009.552792	41.390631
3518.285035	682698.851214	41.395636
3517.971922	682391.641882	41.400640
3517.960455	682068.286571	41.405645
3517.743834	681773.391430	41.410650
3517.551855	681453.580213	41.415655
3517.525251	681147.278054	41.420660
3517.333114	680847.318625	41.425664
3517.522461	680542.604400	41.430669
3517.048099	680248.001595	41.435674
3516.774551	679952.758508	41.440679
3516.889045	679645.436629	41.445684
3516.514881	679368.971619	41.450688
3516.572974	679076.186447	41.455693
3516.366848	678789.912069	41.460698
3516.194593	678502.975565	41.465703
3515.978715	678229.190509	41.470708
3516.013633	677955.505498	41.475712
3515.909943	677670.574668	41.480717
3516.129646	677407.455859	41.485722
3516.195577	677108.677730	41.490727
3515.783411	676841.760364	41.495732
3515.371238	676564.071728	41.500736
3515.651816	676298.918214	41.505741
3515.227015	676036.115918	41.510746
3515.281616	675766.599050	41.515751
3515.263694	675506.306213	41.520756
3514.719035	675246.342094	41.525760
3514.848233	674978.185615	41.530765
3514.472583	674730.140849	41.535770
3514.314053	674470.789273	41.540775
3514.412709	674221.456621	41.545780
3513.915785	673978.396281	41.550784
3513.989459	673717.240959	41.555789
3513.713246	673492.076418	41.560794
3513.793890	673238.333932	41.565799
3513.716041	673009.037461	41.570804
3513.484319	672776.271122	41.575808
3513.466810	672537.581063	41.580813
3513.492043	672309.297429	41.585818
3513.170146	672073.288004	41.590823
3513.008037	671849.760347	41.595828
3512.832266	671621.443281	41.600832
3512.656231	671401.696473	41.605837
3512.210157	671176.055674	41.610842
3512.292989	670962.139462	41.615847
3512.000477	670757.105899	41.620852
3512.134921	670549.304898	41.625856
3512.275996	670330.478151	41.630861
3511.796502	670146.654598	41.635866
3512.043693	669923.911434	41.640871
3511.775205	669718.103360	41.645876
3511.775814	669515.039131	41.650880
3511.646088	669309.448653	41.655885
3511.559403	669115.117488	41.660890
3511.360545	668913.619240	41.665895
3511.329526	668720.567491	41.670900
3511.078434	668533.832219	41.675904
3511.397459	668334.929551	41.680909
3510.924523	668142.487492	41.685914
3510.881651	667952.364775	41.690919
3511.090391	667766.635953	41.695924
3510.498016	667581.634062	41.700928
3510.491135	667393.190130	41.705933
3510.587471	667224.827518	41.710938
3510.412765	667041.641788	41.715943
3510.634716	666863.674762	41.720948
3510.376759	666678.849645	41.725952
3510.561336	666505.221986	41.730957
3510.522579	666326.838947	41.735962
3510.078576	666152.659939	41.740967
3509.851518	665979.190319	41.745972
3510.048954	665806.994591	41.750976
3509.938466	665636.642516	41.755981
3509.980059	665466.910922	41.760986
3509.728082	665295.578288	41.765991
3509.875906	665141.688767	41.770996
3509.512328	664963.633182	41.776000
3509.698144	664798.256541	41.781005
3509.304073	664643.200969	41.786010
3509.544142	664478.957458	41.791015
3509.312908	664325.217089	41.796020
3509.172372	664167.717044	41.801024
3509.282951	664002.937864	41.806029
3509.030547	663851.538597	41.811034
3508.972995	663703.597791	41.816039
3509.032225	663552.242260	41.821044
3508.885872	663391.137643	41.826048
3509.230685	663243.023656	41.831053
3508.931444	663097.558544	41.836058
3508.498475	662940.336103	41.841063
3508.866411	662799.996407	41.846068
3508.624681	662663.797412	41.851072
3508.916090	662505.749856	41.856077
3508.782467	662366.534519	41.861082
3508.556753	662219.796393	41.866087
3508.460780	662076.478294	41.871092
3508.147225	661939.632114	41.876096
3508.429216	661798.792947	41.881101
3508.122458	661652.957931	41.886106
3508.089260	661519.752946	41.891111
3508.002613	661385.506796	41.896116
3508.081259	661257.021339	41.901120
3508.085907	661115.818639	41.906125
3507.999108	660997.489276	41.911130
3507.972791	660854.840389	41.916135
3507.961361	660712.835842	41.921140
3507.875981	660581.573231	41.926144
3508.145918	660450.499876	41.931149
3507.776953	660322.125702	41.936154
3507.724516	660184.413022	41.941159
3507.663858	660062.423967	41.946164
3507.656096	659932.837010	41.951168
3507.850699	659817.541854	41.956173
3507.852738	659686.502337	41.961178
3507.712355	659556.882302	41.966183
3507.728298	659439.415592	41.971188
3507.323640	659318.721923	41.976192
3507.735037	659187.358620	41.981197
3507.670334	659053.525911	41.986202
3507.266521	658935.473284	41.991207
3507.213122	658809.024089	41.996212
3506.789546	658697.062623	42.001216
3507.522891	658572.976985	42.006221
3507.020586	658475.404556	42.011226
3507.378755	658346.584939	42.016231
3507.211868	658227.386305	42.021236
3506.889699	658109.160438	42.026240
3507.004841	657987.465923	42.031245
3506.840402	657891.030267	42.036250
3506.870056	657778.933655	42.041255
3506.729957	657671.107811	42.046260
3506.558457	657557.593826	42.051264
3506.752537	657447.663284	42.056269
3506.520240	657340.647893	42.061274
3506.475970	657233.700214	42.066279
3506.899195	657127.872730	42.071284
3506.411419	657018.748792	42.076288
3506.637319	656907.009325	42.081293
3506.277643	656817.186576	42.086298
3506.120928	656709.702423	42.091303
3506.489685	656600.782237	42.096308
3506.155987	656501.664246	42.101312
3506.188169	656399.788374	42.106317
3506.059509	656305.678238	42.111322
3506.016723	656217.395772	42.116327
3506.221941	656113.790535	42.121332
3506.089713	656026.719611	42.126336
3506.073887	655914.908803	42.131341
3505.982121	655829.926919	42.136346
3505.799001	655737.618144	42.141351
3505.995699	655631.562156	42.146356
3505.659452	655554.608696	42.151360
3505.744589	655449.617894	42.156365
3505.571357	655360.300447	42.161370
3505.784631	655265.075216	42.166375
3505.672577	655176.195502	42.171380
3505.423163	655100.023265	42.176384
3505.573211	655009.750385	42.181389
3505.486607	654923.810889	42.186394
3505.593987	654831.196020	42.191399
3505.595865	654747.787594	42.196404
3505.285858	654659.834853	42.201408
3505.447230	654578.546378	42.206413
3505.117983	654499.485778	42.211418
3505.459364	654414.719983	42.216423
3505.666584	654326.379358	42.221428
3505.238254	654252.028153	42.226432
3505.691032	654158.600840	42.231437
3505.233272	654077.210464	42.236442
3505.113683	653989.619958	42.241447
3505.250504	653897.490966	42.246452
3505.072257	653816.102329	42.251456
3505.356380	653730.840604	42.256461
3505.278241	653663.120608	42.261466
3505.097327	653586.425886	42.266471
3505.235687	653512.225486	42.271476
3505.391195	653431.977527	42.276480
3505.299270	653360.311529	42.281485
3505.087927	653283.319757	42.286490
3505.118871	653197.046146	42.291495
3505.411509	653115.873873	42.296500
3505.434910	653030.898849	42.301504
3505.365939	652948.635851	42.306509
3505.042171	652875.655780	42.311514
3505.138268	652791.965549	42.316519
3504.938310	652706.874685	42.321524
3505.167486	652637.548412	42.326528
3504.985379	652555.800355	42.331533
3504.745314	652485.401344	42.336538
3504.953654	652412.679879	42.341543
3505.009421	652337.485152	42.346548
3504.803695	652261.133957	42.351552
3504.947248	652185.274160	42.356557
3504.981080	652113.578424	42.361562
3505.062618	652050.966825	42.366567
3505.042833	651977.180667	42.371572
3504.620545	651903.160528	42.376576
3504.895129	651824.178887	42.381581
3504.753887	651760.902730	42.386586
3504.590769	651691.884300	42.391591
3504.890615	651618.742261	42.396596
3504.443792	651553.466734	42.401600
3504.565205	651475.207021	42.406605
3504.506451	651414.063419	42.411610
3504.591520	651341.854053	42.416615
3504.477772	651262.082578	42.421620
3504.151325	651200.681998	42.426624
3504.376187	651142.138036	42.431629
3504.507705	651083.858930	42.436634
3504.402085	651015.625753	42.441639
3504.798455	650956.352942	42.446644
3504.233358	650887.944781	42.451648
3504.606123	650809.538489	42.456653
3504.685969	650749.816957	42.461658
3504.454737	650686.298968	42.466663
3504.182537	650613.943334	42.471668
3503.999085	650545.020233	42.476672
3504.313757	650489.605525	42.481677
3504.136611	650437.269570	42.486682
3504.174484	650374.154951	42.491687
3504.085483	650315.707824	42.496692
3504.080420	650261.443822	42.501696
3504.543445	650199.207430	42.506701
3504.419376	650146.511426	42.511706
3504.349196	650081.114212	42.516711
3504.327131	650015.358858	42.521716
3504.219568	649957.912076	42.526720
3504.534700	649888.402591	42.531725
3503.986702	649832.976483	42.536730
3504.256764	649766.072012	42.541735
3504.697556	649699.288873	42.546740
3504.206397	649638.455487	42.551744
3504.351638	649579.315830	42.556749
3504.129854	649511.941022	42.561754
3504.132545	649466.516393	42.566759
3503.813752	649416.397186	42.571764
3503.940041	649360.157736	42.576768
3504.119836	649290.816316	42.581773
3504.171123	649236.787330	42.586778
3503.863207	649171.823125	42.591783
3504.300355	649118.729385	42.596788
3504.076341	649065.844259	42.601792
3504.010216	649000.839102	42.606797
3503.936380	648953.725634	42.611802
3504.190246	648893.714464	42.616807
3504.413415	648833.158269	42.621812
3503.995787	648778.554404	42.626816
3504.525506	648713.948955	42.631821
3504.100776	648654.747833	42.636826
3504.105676	648592.576947	42.641831
3504.416491	648538.101620	42.646836
3503.948850	648468.761245	42.651840
3504.494835	648409.898489	42.656845
3503.847102	648355.929962	42.661850
3504.128354	648302.457774	42.666855
3503.994356	648241.607020	42.671860
3504.334054	648194.671733	42.676864
3504.223957	648123.420862	42.681869
3503.930605	648051.749873	42.686874
3504.217558	647991.927775	42.691879
3504.022241	647940.331439	42.696884
3503.811593	647892.685758	42.701888
3504.100003	647836.211131	42.706893
3503.911289	647780.164668	42.711898
3503.833223	647727.698255	42.716903
3503.870876	647681.909917	42.721908
3503.735394	647618.406653	42.726912
3503.916428	647571.694528	42.731917
3504.093956	647519.184911	42.736922
3504.151647	647454.799097	42.741927
3503.960070	647404.398956	42.746932
3503.879216	647355.829664	42.751936
3504.129473	647292.460709	42.756941
3503.795978	647239.134150	42.761946
3503.720530	647189.563506	42.766951
3504.283783	647129.040970	42.771956
3503.847396	647078.029750	42.776960
3503.696381	647021.722929	42.781965
3503.741362	646973.980787	42.786970
3503.748835	646910.199576	42.791975
3503.878303	646863.192755	42.796980
3503.526459	646813.815761	42.801985
3503.705470	646766.900297	42.806989
3503.776127	646712.604617	42.811994
3503.787445	646651.820267	42.816999
3503.924292	646612.258945	42.822004
3503.666677	646564.214823	42.827009
3503.811034	646514.254733	42.832013
3503.963627	646457.044958	42.837018
3503.871096	646412.771905	42.842023
3503.826696	646350.795235	42.847028
3503.626367	646301.240800	42.852033
3504.011641	646244.391379	42.857037
3503.782722	646194.041323	42.862042
3503.669545	646143.471990	42.867047
3503.713625	646093.826273	42.872052
3503.835733	646052.415609	42.877057
3503.906099	645999.215892	42.882061
3503.492388	645949.794870	42.887066
3503.331005	645896.782768	42.892071
3503.620622	645842.396337	42.897076
3503.402107	645800.790821	42.902081
3503.657918	645757.107363	42.907085
3503.758885	645714.399051	42.912090
3503.723262	645660.365177	42.917095
3503.686631	645607.530965	42.922100
3503.510161	645566.267491	42.927105
3503.481176	645512.631663	42.932109
3503.666662	645465.709091	42.937114
3503.671854	645416.166438	42.942119
3503.478282	645362.256983	42.947124
3503.609475	645327.340836	42.952129
3503.488080	645274.518852	42.957133
3503.408128	645234.387950	42.962138
3503.242964	645190.371473	42.967143
3503.323698	645149.563847	42.972148
3503.287251	645101.026377	42.977153
3503.827604	645038.595351	42.982157
3503.715554	645004.618063	42.987162
3503.360493	644962.731633	42.992167
3503.496979	644909.665274	42.997172
3503.410946	644857.835177	43.002177
3503.354095	644814.399154	43.007181
3503.319374	644779.258484	43.012186
3503.063820	644730.055411	43.017191
3503.266960	644692.325483	43.022196
3503.112239	644654.054435	43.027201
3503.388751	644608.412782	43.032205
3502.979007	644566.383735	43.037210
3503.425347	644520.263736	43.042215
3503.904250	644481.337668	43.047220
3503.614242	644433.688726	43.052225
3503.329710	644377.089188	43.057229
3503.269841	644342.801099	43.062234
3503.550460	644304.007020	43.067239
3503.741127	644248.578396	43.072244
3503.784202	644203.723356	43.077249
3503.747415	644156.681360	43.082253
3503.886841	644099.160442	43.087258
3503.787610	644058.178087	43.092263
3503.507426	644005.775645	43.097268
3503.393749	643956.945433	43.102273
3503.702439	643908.295384	43.107277
3503.593981	643862.013823	43.112282
3503.581911	643813.466176	43.117287
3503.694667	643753.547705	43.122292
3503.349310	643728.004603	43.127297
3503.946851	643668.455750	43.132301
3504.036817	643628.690499	43.137306
3503.694125	643569.045993	43.142311
3503.787350	643526.629752	43.147316
3503.581379	643483.012599	43.152321
3503.756152	643426.832093	43.157325
3503.526446	643380.618321	43.162330
3503.782410	643327.223997	43.167335
3504.056848	643280.476677	43.172340
3503.780240	643234.419977	43.177345
3503.855847	643173.604165	43.182349
3503.562049	643122.549491	43.187354
3503.561753	643076.096521	43.192359
3503.761887	643031.810473	43.197364
3503.539248	642984.693672	43.202369
3503.691897	642930.664244	43.207373
3503.180363	642881.444389	43.212378
3503.396619	642835.604696	43.217383
3503.672419	642784.504473	43.222388
3503.523848	642743.124910	43.227393
3503.388718	642702.293022	43.232397
3503.505049	642671.920682	43.237402
3503.540329	642621.559353	43.242407
3503.677446	642576.031568	43.247412
3503.614463	642532.736822	43.252417
3503.673369	642477.620306	43.257421
3503.468494	642437.898992	43.262426
3503.247296	642384.678373	43.267431
3503.704992	642334.746090	43.272436
3503.523380	642295.720489	43.277441
3503.497178	642251.268320	43.282445
3503.483458	642208.814210	43.287450
3503.521701	642156.249756	43.292455
3503.877262	642115.984769	43.297460
3503.540750	642065.932002	43.302465
3503.468300	642004.633533	43.307469
3503.691370	641966.440145	43.312474
3503.675219	641911.332940	43.317479
3503.613345	641861.784018	43.322484
3503.412126	641823.059897	43.327489
3503.743360	641767.044508	43.332493
3503.693266	641722.193896	43.337498
3503.640520	641682.994687	43.342503
3503.747327	641632.416652	43.347508
3503.519902	641596.146505	43.352513
3503.757169	641522.391444	43.357517
3503.434203	641483.185986	43.362522
3503.721667	641435.977976	43.367527
3503.693805	641385.871017	43.372532
3503.580641	641338.878611	43.377537
3503.895663	641286.514139	43.382541
3503.778897	641243.672903	43.387546
3503.578093	641199.745057	43.392551
3503.565625	641143.632857	43.397556
3503.613828	641101.464023	43.402561
3503.809554	641047.517566	43.407565
3503.478858	641008.261547	43.412570
3503.751128	640966.755427	43.417575
3503.665889	640909.803702	43.422580
3503.493218	640873.571984	43.427585
3503.683809	640817.274492	43.432589
3504.009196	640763.255160	43.437594
3503.457608	640714.931721	43.442599
3503.597120	640674.596640	43.447604
3503.759528	640624.404589	43.452609
3503.772090	640565.984390	43.457613
3503.591055	640518.899374	43.462618
3503.231450	640481.946834	43.467623
3503.497991	640423.634022	43.472628
3503.521295	640382.266596	43.477633
3503.363634	640334.076514	43.482637
3503.386272	640296.660185	43.487642
3503.221756	640242.518772	43.492647
3503.173383	640199.962006	43.497652
3503.477464	640159.597785	43.502657
3503.216851	640120.026706	43.507661
3503.536582	640086.011889	43.512666
3503.414584	640045.217247	43.517671
3503.556388	639989.973643	43.522676
3503.309838	639958.502625	43.527681
3503.654924	639910.577843	43.532685
3503.320203	639862.064589	43.537690
3503.080423	639815.436199	43.542695
3503.676822	639764.468160	43.547700
3503.587333	639735.521580	43.552705
3503.663321	639680.337177	43.557709
3503.479623	639639.901233	43.562714
3503.295174	639582.958494	43.567719
3503.441700	639545.719098	43.572724
3503.408393	639497.654663	43.577729
3503.523529	639460.270068	43.582733
3503.107549	639417.570553	43.587738
3503.519461	639368.381702	43.592743
3503.606873	639325.949008	43.597748
3503.574034	639284.036175	43.602753
3503.524811	639239.174561	43.607757
3503.357368	639201.885614	43.612762
3503.450041	639154.749243	43.617767
3503.467602	639096.269844	43.622772
3503.321725	639068.131044	43.627777
3503.477909	639015.931246	43.632781
3503.594935	638972.741868	43.637786
3503.233959	638925.779250	43.642791
3503.504342	638884.515157	43.647796
3503.051345	638840.068506	43.652801
3503.059836	638793.044401	43.657805
3503.313219	638763.488320	43.662810
3503.161421	638725.694825	43.667815
3503.467876	638674.869230	43.672820
3503.441933	638630.351304	43.677825
3503.443577	638589.780643	43.682829
3503.191760	638549.301613	43.687834
3503.281741	638505.264301	43.692839
3503.620689	638456.833514	43.697844
3503.126157	638424.998459	43.702849
3503.649026	638379.238414	43.707853
3503.262813	638335.879163	43.712858
3503.543045	638287.207124	43.717863
3503.407496	638235.251556	43.722868
3503.204145	638205.969249	43.727873
3503.183344	638155.295078	43.732877
3503.111601	638118.086494	43.737882
3503.161389	638070.902211	43.742887
3503.475326	638034.880471	43.747892
3503.166035	637987.704950	43.752897
3503.461438	637940.879826	43.757901
3503.664267	637905.576344	43.762906
3503.311197	637859.708197	43.767911
3503.219388	637819.900343	43.772916
3503.172728	637770.829478	43.777921
3503.320678	637731.432040	43.782925
3503.302578	637690.060626	43.787930
3503.513373	637655.105185	43.792935
3503.496872	637620.787440	43.797940
3503.129398	637568.316405	43.802945
3502.943615	637537.578429	43.807949
3502.986213	637498.347555	43.812954
3503.239487	637455.229443	43.817959
3502.969220	637418.201145	43.822964
3503.205056	637390.395118	43.827969
3503.097659	637347.085832	43.832973
3503.394626	637301.158122	43.837978
3503.146105	637257.321367	43.842983
3503.348188	637216.612224	43.847988
3503.310265	637175.542211	43.852993
3503.246839	637139.129250	43.857997
3503.150359	637095.616983	43.863002
3503.129683	637062.398792	43.868007
3503.523164	637007.147782	43.873012
3503.132325	636968.186455	43.878017
3503.205842	636920.993019	43.883021
3503.187031	636890.175572	43.888026
3503.232568	636845.838317	43.893031
3503.270881	636804.604171	43.898036
3502.928075	636771.288026	43.903041
3502.995397	636738.054294	43.908045
3503.083217	636701.865045	43.913050
3503.170187	636659.121268	43.918055
3503.306411	636620.171850	43.923060
3502.737464	636584.440658	43.928065
3503.023072	636550.820113	43.933069
3503.117162	636514.278930	43.938074
3503.065364	636476.260591	43.943079
3503.380695	636434.529006	43.948084
3503.059080	636391.651312	43.953089
3503.338150	636351.926809	43.958093
3503.091534	636316.641941	43.963098
3503.010593	636275.725562	43.968103
3503.162017	636237.272568	43.973108
3502.709745	636198.268431	43.978113
3502.788119	636159.727113	43.983117
3503.170549	636130.692666	43.988122
3503.098270	636089.724090	43.993127
3502.830179	636046.786112	43.998132
3502.972080	636013.938075	44.003137
3503.080836	635976.742094	44.008141
3502.876827	635941.599043	44.013146
3502.802713	635919.094154	44.018151
3503.096022	635880.666500	44.023156
3502.867614	635847.528689	44.028161
3502.858284	635812.803470	44.033165
3502.960162	635777.859654	44.038170
3502.917116	635747.493159	44.043175
3503.333096	635708.143951	44.048180
3503.060632	635672.811114	44.053185
3503.086664	635623.718109	44.058189
3503.146559	635602.391404	44.063194
3503.203346	635557.346239	44.068199
3503.370014	635517.687114	44.073204
3503.078977	635473.899867	44.078209
3502.882768	635428.245307	44.083213
3503.021231	635393.744539	44.088218
3503.188450	635360.439901	44.093223
3503.357156	635308.869895	44.098228
3503.235776	635280.866881	44.103233
3503.182133	635235.187982	44.108237
3503.159834	635190.704720	44.113242
3503.096847	635154.935271	44.118247
3503.071661	635115.806649	44.123252
3502.952677	635084.499933	44.128257
3503.365812	635053.055396	44.133261
3503.409714	635015.116030	44.138266
3503.161145	634974.622494	44.143271
3503.407911	634928.292234	44.148276
3503.103015	634898.316712	44.153281
3502.964931	634860.006423	44.158285
3503.296278	634824.721338	44.163290
3502.982323	634772.527603	44.168295
3503.229689	634732.151580	44.173300
3503.131234	634697.187107	44.178305
3503.041279	634658.167529	44.183309
3502.958152	634622.199393	44.188314
3503.060899	634588.552603	44.193319
3503.088247	634551.515081	44.198324
3503.075024	634517.787083	44.203329
3503.113755	634475.592782	44.208333
3502.946033	634428.928244	44.213338
3503.227892	634400.005645	44.218343
3503.389565	634353.536720	44.223348
3503.256615	634316.925147	44.228353
3502.892963	634266.838999	44.233357
3502.988775	634238.797396	44.238362
3502.861602	634203.235445	44.243367
3502.794648	634177.072217	44.248372
3502.665512	634139.908882	44.253377
3502.993051	634107.124342	44.258381
3502.781245	634081.835543	44.263386
3502.879917	634044.233952	44.268391
3503.069160	634018.728773	44.273396
3502.684096	633987.362513	44.278401
3502.831447	633939.392680	44.283405
3503.170493	633909.758634	44.288410
3503.023732	633876.100617	44.293415
3503.199395	633830.327734	44.298420
3502.935697	633800.342265	44.303425
3502.938102	633760.253094	44.308429
3502.907844	633721.620568	44.313434
3502.766430	633689.012092	44.318439
3503.006724	633646.931378	44.323444
3503.178463	633615.272053	44.328449
3503.147116	633572.735309	44.333453
3502.642495	633545.091085	44.338458
3502.876049	633501.459358	44.343463
3503.019703	633470.855271	44.348468
3503.162694	633446.157119	44.353473
3503.267628	633399.393004	44.358477
3502.908345	633361.313869	44.363482
3502.942638	633326.823440	44.368487
3503.041520	633281.060808	44.373492
3503.060803	633253.629787	44.378497
3503.255780	633214.207508	44.383501
3503.244386	633180.975408	44.388506
3503.025205	633140.069503	44.393511
3503.507215	633099.348205	44.398516
3503.193736	633065.715052	44.403521
3502.911577	633019.263286	44.408525
3503.418565	632987.096352	44.413530
3503.195049	632939.032893	44.418535
3503.216583	632892.180153	44.423540
3502.886579	632863.654454	44.428545
3502.875201	632823.864289	44.433549
3502.815101	632780.127790	44.438554
3502.896292	632749.732105	44.443559
3503.044531	632720.676730	44.448564
3502.734569	632686.290975	44.453569
3503.018190	632652.407941	44.458573
3502.998107	632614.370302	44.463578
3502.862876	632584.810667	44.468583
3503.161447	632539.712654	44.473588
3503.127032	632514.240670	44.478593
3503.046971	632480.817449	44.483597
3503.266719	632441.438240	44.488602
3502.880578	632397.003047	44.493607
3503.025585	632363.041812	44.498612
3503.140833	632331.037534	44.503617
3503.145089	632286.837876	44.508621
3503.409555	632249.302638	44.513626
3503.079677	632211.765091	44.518631
3502.988100	632165.728643	44.523636
3503.066162	632137.133724	44.528641
3503.127100	632095.927305	44.533645
3503.279167	632065.317734	44.538650
3503.342048	632018.554395	44.543655
3503.268699	631976.268383	44.548660
3503.171892	631940.443459	44.553665
3503.208063	631894.284657	44.558669
3503.083854	631848.352311	44.563674
3502.721545	631823.683550	44.568679
3502.999337	631787.195682	44.573684
3503.190460	631756.879126	44.578689
3503.094794	631713.444396	44.583693
3503.051300	631680.162777	44.588698
3503.147453	631641.802112	44.593703
3503.031352	631606.129404	44.598708
3502.935495	631571.154067	44.603713
3502.918622	631535.114354	44.608717
3503.113614	631494.033665	44.613722
3503.039628	631466.763524	44.618727
3503.629317	631421.362451	44.623732
3503.202056	631372.574498	44.628737
3503.127118	631336.944155	44.633741
3503.144061	631308.156815	44.638746
3502.672591	631266.884700	44.643751
3503.175558	631220.545903	44.648756
3502.804533	631186.866149	44.653761
3502.873826	631148.357931	44.658765
3502.779420	631122.291728	44.663770
3502.524643	631093.498515	44.668775
3503.038665	631055.567472	44.673780
3502.874290	631026.709118	44.678785
3502.707311	630998.201546	44.683789
3503.197043	630953.615921	44.688794
3503.320384	630919.152980	44.693799
3503.321565	630883.858997	44.698804
3503.114101	630841.540463	44.703809
3503.197580	630797.221371	44.708813
3503.161046	630759.930679	44.713818
3502.919834	630728.881403	44.718823
3503.084510	630691.256933	44.723828
3502.660303	630653.529114	44.728833
3502.752182	630617.067834	44.733837
3502.860130	630583.707733	44.738842
3502.895327	630556.016734	44.743847
3502.706565	630515.095597	44.748852
3502.964603	630498.081431	44.753857
3503.069301	630453.306822	44.758861
3503.083263	630419.561175	44.763866
3502.910303	630387.698615	44.768871
3503.204604	630350.702413	44.773876
3503.135002	630306.005966	44.778881
3502.951278	630268.887988	44.783885
3503.088940	630241.479672	44.788890
3503.137612	630196.312683	44.793895
3503.181393	630158.556042	44.798900
3502.998657	630131.050038	44.803905
3502.932746	630088.605028	44.808909
3503.115754	630050.324397	44.813914
3502.676659	630015.550657	44.818919
3502.912650	629980.965960	44.823924
3502.594237	629953.181451	44.828929
3502.741618	629918.561085	44.833933
3502.997652	629890.531551	44.838938
3503.018428	629848.421761	44.843943
3502.812348	629807.600871	44.848948
3502.907256	629779.948067	44.853953
3502.886006	629749.560609	44.858957
3503.056792	629713.133277	44.863962
3502.645980	629670.142606	44.868967
3503.300809	629639.092676	44.873972
3502.825071	629605.925809	44.878977
3502.931675	629559.244502	44.883981
3502.983907	629529.595333	44.888986
3502.983183	629506.664035	44.893991
3502.964141	629457.900094	44.898996
3502.341515	629431.966829	44.904001
3502.732464	629391.646784	44.909005
3502.577871	629365.285746	44.914010
3502.732659	629333.165721	44.919015
3502.589506	629303.848534	44.924020
3502.851584	629283.977775	44.929025
3503.013927	629241.391614	44.934029
3502.888421	629210.168596	44.939034
3502.689013	629175.903370	44.944039
3502.962115	629139.657489	44.949044
3502.619258	629114.929108	44.954049
3502.784716	629090.166979	44.959053
3503.162752	629053.402804	44.964058
3503.036018	629022.079292	44.969063
3502.739980	628984.574746	44.974068
3502.545313	628961.423869	44.979073
3502.932679	628908.234216	44.984077
3502.825323	628889.374957	44.989082
3502.644181	628860.763809	44.994087
3502.955045	628825.461999	44.999092
3502.895699	628792.674615	45.004097
3502.456311	628758.347438	45.009101
3503.030818	628730.713013	45.014106
3502.877337	628704.300074	45.019111
3502.713088	628657.609358	45.024116
3502.652981	628638.391357	45.029121
3502.908394	628600.844655	45.034125
3502.935662	628565.889154	45.039130
3502.587150	628528.491786	45.044135
3503.257322	628489.874879	45.049140
3502.901949	628461.892248	45.054145
3502.761457	628428.215782	45.059149
3502.851639	628387.791267	45.064154
3502.524761	628350.289558	45.069159
3502.677612	628312.608516	45.074164
3502.569363	628294.449389	45.079169
3502.696800	628257.373235	45.084173
3503.009906	628229.129612	45.089178
3502.974661	628213.411985	45.094183
3502.827037	628167.016822	45.099188
3502.765598	628139.034979	45.104193
3502.702350	628097.783364	45.109197
3503.041047	628066.380336	45.114202
3502.575458	628042.020204	45.119207
3502.828612	628009.529438	45.124212
3502.525105	627982.688742	45.129217
3502.954815	627950.619387	45.134221
3502.836359	627917.538585	45.139226
3502.751045	627875.738905	45.144231
3503.052518	627839.634147	45.149236
3502.766814	627812.940319	45.154241
3502.758864	627778.739185	45.159245
3503.073805	627741.179641	45.164250
3502.872035	627709.514081	45.169255
3502.996803	627672.887026	45.174260
3502.643590	627651.762517	45.179265
3502.920304	627606.446769	45.184269
3503.116043	627568.806105	45.189274
3502.863862	627546.212476	45.194279
3502.772384	627507.216737	45.199284
3502.889002	627475.748407	45.204289
3503.028543	627455.293487	45.209293
3503.038988	627405.964402	45.214298
3502.890203	627378.645977	45.219303
3502.982013	627344.577246	45.224308
3503.158561	627315.101729	45.229313
3502.748965	627276.808595	45.234317
3502.859534	627247.644239	45.239322
3502.825123	627206.484577	45.244327
3502.894241	627167.260811	45.249332
3502.696304	627148.413388	45.254337
3502.836598	627117.340739	45.259341
3502.999790	627080.655238	45.264346
3502.353095	627039.245261	45.269351
3502.695439	627019.958019	45.274356
3502.529266	626984.678636	45.279361
3502.889454	626955.672672	45.284365
3502.904678	626919.361565	45.289370
3502.609511	626896.222748	45.294375
3502.838922	626855.268662	45.299380
3503.070738	626821.125108	45.304385
3502.747711	626789.226385	45.309389
3503.038731	626745.106581	45.314394
3502.509250	626731.621729	45.319399
3502.862848	626687.441293	45.324404
3502.932690	626658.883025	45.329409
3502.834668	626622.289075	45.334413
3503.316256	626589.706261	45.339418
3503.064179	626554.539776	45.344423
3503.199265	626523.516341	45.349428
3503.068472	626491.484885	45.354433
3503.163638	626452.003783	45.359437
3503.172645	626410.733731	45.364442
3502.831596	626369.220700	45.369447
3503.045873	626333.225385	45.374452
3502.858582	626305.109213	45.379457
3502.906776	626270.142731	45.384461
3502.608639	626232.228150	45.389466
3502.628986	626201.222686	45.394471
3502.904167	626165.417108	45.399476
3502.517649	626139.537050	45.404481
3502.374358	626111.413118	45.409485
3503.026010	626070.787129	45.414490
3502.823613	626044.976672	45.419495
3503.086812	626007.720072	45.424500
3502.795245	625976.514929	45.429505
3502.739570	625949.928783	45.434509
3502.947015	625908.273493	45.439514
3502.738607	625873.598427	45.444519
3502.929304	625841.962821	45.449524
3503.023488	625807.888800	45.454529
3502.933084	625778.703466	45.459533
3503.153118	625735.292406	45.464538
3502.981233	625710.628105	45.469543
3502.803300	625668.334172	45.474548
3502.943844	625650.279804	45.479553
3503.000014	625613.356469	45.484557
3502.971786	625568.382853	45.489562
3502.983115	625539.280278	45.494567
3503.029805	625485.678917	45.499572
3502.710337	625455.578781	45.504577
3502.694659	625434.394255	45.509581
3502.981952	625398.534031	45.514586
3502.673449	625374.692878	45.519591
3502.799545	625329.843096	45.524596
3502.888716	625301.077666	45.529601
3502.828854	625271.034410	45.534605
3502.726427	625243.402350	45.539610
3502.894167	625213.221249	45.544615
3502.744522	625170.870601	45.549620
3502.662054	625143.385262	45.554625
3502.724276	625111.668493	45.559629
3502.918894	625075.071118	45.564634
3502.851287	625045.980211	45.569639
3503.064475	625004.771273	45.574644
3502.633732	624979.246323	45.579649
3502.823390	624943.300487	45.584653
3502.390861	624905.453439	45.589658
3502.249495	624883.887812	45.594663
3502.839632	624850.530473	45.599668
3502.530427	624823.833038	45.604673
3502.637918	624803.578695	45.609677
3502.744967	624778.766103	45.614682
3502.188098	624749.604741	45.619687
3502.622125	624718.176181	45.624692
3502.098982	624702.283327	45.629697
3501.775532	624670.378350	45.634701
3502.227707	624652.621593	45.639706
3502.354883	624636.521297	45.644711
3502.674865	624603.408076	45.649716
3502.399122	624590.379616	45.654721
3502.379813	624555.418663	45.659725
3502.454606	624528.506940	45.664730
3502.517196	624497.539680	45.669735
3502.620623	624470.372632	45.674740
3502.677662	624442.261399	45.679745
3502.511217	624415.238866	45.684749
3502.687542	624381.196872	45.689754
3502.188235	624362.845033	45.694759
3502.339422	624334.217074	45.699764
3502.299120	624317.993619	45.704769
3502.382714	624287.222665	45.709773
3502.681436	624257.568323	45.714778
3502.567446	624236.347539	45.719783
3502.711137	624201.759325	45.724788
3502.515774	624173.789169	45.729793
3502.533303	624149.340533	45.734797
3502.673209	624113.299933	45.739802
3502.436362	624103.420403	45.744807
3502.595520	624070.883081	45.749812
3502.557581	624050.100247	45.754817
3502.675934	623991.169604	45.759821
3502.763315	623903.689559	45.764826
3502.429125	623780.560098	45.769831
3502.349547	623569.968924	45.774836
3502.051733	623324.090690	45.779841
3501.920887	623011.146713	45.784845
3501.834704	622650.790911	45.789850
3501.507966	622233.095083	45.794855
3501.289277	621746.771609	45.799860
3501.073692	621214.577440	45.804865
3500.966437	620624.111283	45.809869
3500.486888	619955.698234	45.814874
3500.046460	619255.463822	45.819879
3499.859630	618482.368456	45.824884
3499.112346	617666.805827	45.829889
3498.871795	616773.200432	45.834893
3498.372233	615822.464546	45.839898
3497.375837	614815.224433	45.844903
3497.077480	613751.769415	45.849908
3496.009667	612627.661846	45.854913
3495.536109	611446.771432	45.859917
3494.663876	610204.429118	45.864922
3493.621830	608897.918582	45.869927
3492.797996	607541.452429	45.874932
3491.855468	606132.560083	45.879937
3490.869319	604650.284404	45.884941
3490.079007	603116.992670	45.889946
3488.790428	601541.212666	45.894951
3487.763976	599885.200616	45.899956
3486.676515	598184.123891	45.904961
3485.409677	596436.677879	45.909965
3484.335886	594624.148125	45.914970
3482.496042	592762.990129	45.919975
3481.513209	590849.649437	45.924980
3479.908342	588887.713312	45.929985
3478.485283	586867.930618	45.934989
3477.098433	584804.775383	45.939994
3475.194076	582688.565618	45.944999
3474.083302	580522.127548	45.950004
3471.672464	578316.997916	45.955009
3469.955490	576061.813979	45.960013
3468.317718	573756.602724	45.965018
3466.112097	571428.318081	45.970023
3464.342980	569044.976315	45.975028
3462.343298	566620.100999	45.980033
3460.177842	564148.626836	45.985037
3458.344562	561643.945480	45.990042
3455.828715	559103.287954	45.995047
3453.398054	556529.382897	46.000052
3450.965202	553920.063314	46.005057
3449.162798	551276.267452	46.010061
3446.596692	548597.705840	46.015066
3444.310942	545892.257978	46.020071
3441.863101	543150.707580	46.025076
3439.432889	540366.906257	46.030081
3436.707919	537564.848976	46.035085
3434.430523	534727.101446	46.040090
3431.493921	531860.038623	46.045095
3429.030986	528956.597706	46.050100
3426.180440	526045.027242	46.055105
3423.291636	523095.275919	46.060109
3420.724427	520116.511601	46.065114
3417.743452	517131.426631	46.070119
3415.166619	514101.943818	46.075124
3412.076339	511057.557703	46.080129
3409.374799	507990.789107	46.085133
3406.122833	504897.945275	46.090138
3402.718411	501798.977341	46.095143
3400.073459	498659.095369	46.100148
3396.978360	495508.075687	46.105153
3393.429923	492337.420890	46.110157
3390.634303	489160.997198	46.115162
3386.971944	485966.575485	46.120167
3384.097343	482761.373597	46.125172
3380.614621	479519.144586	46.130177
3377.275463	476274.390886	46.135181
3373.949950	473015.390966	46.140186
3370.383732	469759.057017	46.145191
3367.233741	466469.875656	46.150196
3363.560609	463180.526956	46.155201
3359.882485	459886.271698	46.160205
3356.472725	456571.053193	46.165210
3352.712204	453260.524890	46.170215
3349.400936	449922.519479	46.175220
3345.724581	446604.079085	46.180225
3342.122049	443253.006648	46.185229
3338.510181	439906.546630	46.190234
3334.222307	436563.044691	46.195239
3330.570429	433202.707518	46.200244
3326.986433	429868.973948	46.205249
3323.090098	426502.081469	46.210253
3319.273379	423135.873419	46.215258
3315.363879	419777.420298	46.220263
3311.631641	416410.008856	46.225268
3307.793434	413051.416546	46.230273
3304.036822	409687.225411	46.235277
3300.003953	406322.734255	46.240282
3296.379822	402971.684212	46.245287
3292.593939	399606.999227	46.250292
3288.731873	396239.621124	46.255297
3284.696835	392887.388131	46.260301
3280.905328	389517.054646	46.265306
3276.638262	386152.355483	46.270311
3273.138305	382788.928183	46.275316
3269.313522	379437.233363	46.280321
3264.959417	376088.240905	46.285325
3261.430418	372729.176464	46.290330
3256.927893	369391.774360	46.295335
3253.015606	366044.688538	46.300340
3248.836282	362717.748863	46.305345
3244.936815	359389.640103	46.310349
3241.284849	356059.791340	46.315354
3237.048469	352742.595111	46.320359
3233.546846	349422.834878	46.325364
3229.242424	346117.718477	46.330369
3225.367579	342808.810000	46.335373
3221.438214	339493.143679	46.340378
3217.196820	336205.584328	46.345383
3213.133282	332909.950461	46.350388
3208.799592	329627.906925	46.355393
3204.700754	326356.377984	46.360397
3200.743645	323094.320247	46.365402
3196.418824	319831.059659	46.370407
3192.454629	316573.154394	46.375412
3188.455500	313330.658800	46.380417
3184.512102	310096.235917	46.385421
3180.480137	306864.470221	46.390426
3176.232270	303667.651486	46.395431
3172.162614	300451.058099	46.400436
3168.327671	297255.810494	46.405441
3163.902438	294064.535298	46.410445
3160.230082	290878.470842	46.415450
3156.268104	287711.828900	46.420455
3152.245970	284538.707217	46.425460
3148.121810	281385.248844	46.430465
3144.280621	278231.101866	46.435469
3140.003268	275082.122669	46.440474
3135.652728	271963.064794	46.445479
3131.749087	268841.353867	46.450484
3127.956248	265719.956040	46.455489
3123.605345	262616.511184	46.460493
3120.013358	259519.348961	46.465498
3115.427263	256440.939574	46.470503
3111.900114	253356.807743	46.475508
3107.523276	250300.358450	46.480513
3103.745452	247248.387343	46.485517
3099.775746	244188.756280	46.490522
3095.386062	241159.176330	46.495527
3091.261325	238120.728575	46.500532
3087.384800	235108.337719	46.505537
3083.231229	232105.186295	46.510541
3079.112393	229111.076223	46.515546
3075.138956	226120.647607	46.520551
3071.210582	223150.780748	46.525556
3067.207590	220179.626914	46.530561
3063.003700	217229.060738	46.535565
3058.934477	214281.487917	46.540570
3054.708554	211348.114600	46.545575
3051.330913	208422.223760	46.550580
3047.260687	205517.021070	46.555585
3042.777232	202610.073352	46.560589
3039.031231	199622.405845	46.565594
3034.960747	196748.214000	46.570599
3031.144450	193866.429838	46.575604
3027.082767	191000.598662	46.580609
3022.999237	188154.797838	46.585613
3019.045766	185299.850175	46.590618
3014.975828	182474.029892	46.595623
3011.315380	179650.809752	46.600628
3007.421059	176829.715678	46.605633
3003.332432	174012.985589	46.610637
2999.293284	171213.331822	46.615642
2995.214596	168431.712852	46.620647
2991.457206	165647.438106	46.625652
2987.253912	162876.171007	46.630657
2983.551637	160124.079565	46.635661
2979.619987	157363.954031	46.640666
2975.247371	154629.600837	46.645671
2971.428764	151904.197007	46.650676
2967.583982	149178.190199	46.655681
2963.389280	146468.727467	46.660685
2959.693013	143762.206358	46.665690
2955.309275	141091.307763	46.670695
2951.543658	138395.851603	46.675700
2947.338345	135744.203346	46.680705
2943.412180	133093.089172	46.685709
2939.891769	130436.710245	46.690714
2935.543725	127794.248410	46.695719
2931.649746	125175.620487	46.700724
2927.644208	122563.638775	46.705729
2923.652927	119965.272625	46.710733
2919.793685	117380.948028	46.715738
2915.637266	114794.896894	46.720743
2911.963060	112220.153578	46.725748
2907.717558	109666.659074	46.730753
2903.710328	107120.385957	46.735757
2899.797460	104579.353884	46.740762
2895.602150	102066.531359	46.745767
2891.547599	99543.125145	46.750772
2887.540031	97039.508216	46.755777
2883.762770	94558.028230	46.760781
2879.843151	92074.624547	46.765786
2875.902058	89614.242427	46.770791
2872.109763	87166.642656	46.775796
2867.394065	84716.783642	46.780801
2863.325080	82287.397521	46.785805
2859.624718	79870.942013	46.790810
2855.274808	77478.878865	46.795815
2851.269264	75086.424532	46.800820
2847.199538	72715.067178	46.805825
2843.160076	70362.302690	46.810829
2839.288864	68018.800174	46.815834
2834.640376	65689.729295	46.820839
2830.503753	63373.443611	46.825844
2826.357181	61092.795908	46.830849
2822.022050	58810.456062	46.835853
2817.892079	56556.189302	46.840858
2813.431444	54320.233575	46.845863
2809.416218	52101.418804	46.850868
2805.223833	49901.681302	46.855873
2800.422139	47723.124531	46.860877
2796.208373	45562.317293	46.865882
2791.312900	43438.857485	46.870887
2786.637849	41341.761345	46.875892
2781.733335	39277.609748	46.880897
2775.244749	37268.176863	46.885901
2767.800780	35354.878520	46.890906
2759.825335	33509.961510	46.895911
2752.531059	31713.972434	46.900916
2745.095252	30013.117966	46.905921
2737.757782	28386.843256	46.910925
2731.484974	26821.819195	46.915930
2724.623659	25349.689124	46.920935
2718.271525	23935.279757	46.925940
2712.627943	22608.030269	46.930945
2706.344452	21346.979781	46.935949
2701.452448	20131.211095	46.940954
2695.469569	18990.546862	46.945959
2690.571277	17907.942450	46.950964
2685.394607	16869.213016	46.955969
2680.269102	15883.284926	46.960973
2675.558567	14952.245964	46.965978
2670.775489	14058.931703	46.970983
2666.114077	13200.025605	46.975988
2661.926406	12382.025846	46.980993
2656.647473	11612.557928	46.985997
2651.864284	10888.324768	46.991002
2646.713250	10208.357105	46.996007
2642.121673	9556.405123	47.001012
2637.116171	8959.135924	47.006017
2632.095009	8387.446313	47.011021
2627.717966	7849.644267	47.016026
2622.953254	7354.031647	47.021031
2618.541518	6884.743554	47.026036
2614.026163	6442.461092	47.031041
2609.591629	6028.681174	47.036045
2605.982744	5625.769960	47.041050
2601.867590	5277.268278	47.046055
2597.994248	4920.215314	47.051060
2594.482311	4588.577380	47.056065
2590.807494	4270.313135	47.061069
2587.571518	3954.383944	47.066074
2583.813317	3660.776051	47.071079
2580.739353	3359.210059	47.076084
2577.211724	3073.631047	47.081089
2573.516307	2791.358589	47.086093
2570.155595	2519.534561	47.091098
2567.016947	2257.446748	47.096103
2563.566181	1992.778448	47.101108
2560.532670	1728.798909	47.106113
2556.855604	1471.021312	47.111117
2553.835877	1203.210584	47.116122
2550.206285	967.331999	47.121127
2546.913389	708.308492	47.126132
2543.230938	474.376593	47.131137
2538.646315	251.363346	47.136141
2532.914084	87.271948	47.141146
2519.475733	156.762313	47.146151
2512.247212	151.900618	47.151156
2508.226885	157.806428	47.156161
2505.619828	158.126690	47.161165
2504.551968	151.270572	47.166170
2502.454871	157.579254	47.171175
2500.041398	154.566048	47.176180
2497.468495	159.104177	47.181185
2494.355898	158.099657	47.186189
2491.087726	148.789463	47.191194
2487.542347	148.420381	47.196199
2484.223663	151.107405	47.201204
2480.958383	145.869472	47.206209
2477.321475	155.693970	47.211213
2474.309588	142.882691	47.216218
2471.151597	144.656152	47.221223
2467.719395	149.165622	47.226228
2464.211648	153.899114	47.231233
2460.861088	154.982295	47.236237
2457.736116	142.011693	47.241242
2454.236263	146.577331	47.246247
2451.023434	144.457238	47.251252
2447.654940	140.147097	47.256257
2444.423434	145.171272	47.261261
2440.907543	139.301409	47.266266
2437.236668	145.156098	47.271271
2433.873055	150.359368	47.276276
2430.142904	148.702982	47.281281
2427.358861	143.247120	47.286285
2424.634965	141.975224	47.291290
2419.916311	150.339199	47.296295
2416.954311	143.495809	47.301300
2413.352713	144.550996	47.306305
2409.710932	151.388990	47.311309
2406.766909	135.950020	47.316314
2402.912608	140.578934	47.321319
2399.546663	139.941120	47.326324
2396.495912	139.817844	47.331329
2393.057147	149.581858	47.336333
2389.811453	139.492486	47.341338
2385.961335	148.840330	47.346343
2382.399051	139.525887	47.351348
2379.322263	134.612130	47.356353
2375.656061	142.481925	47.361357
2372.296240	133.296682	47.366362
2368.896414	138.295404	47.371367
2365.448316	130.944222	47.376372
2361.676762	133.599320	47.381377
2358.346910	138.705495	47.386381
2354.986384	137.212923	47.391386
2351.570190	144.061272	47.396391
2348.046770	144.021185	47.401396
2344.495706	136.775226	47.406401
2340.635150	146.800122	47.411405
2337.500367	136.139732	47.416410
2334.108753	143.254588	47.421415
2330.623388	135.069504	47.426420
2327.334193	136.847544	47.431425
2323.493461	142.968146	47.436429
2320.390749	130.006024	47.441434
2316.874254	140.121744	47.446439
2313.248011	135.781039	47.451444
2309.812371	141.392338	47.456449
2306.478996	130.529332	47.461453
2302.827884	134.438029	47.466458
2299.310558	138.447388	47.471463
2295.620800	135.093625	47.476468
2292.396578	135.997399	47.481473
2288.842871	141.226811	47.486477
2285.537629	131.558614	47.491482
2281.990703	136.268694	47.496487
2278.610984	135.452078	47.501492
2274.992954	138.816002	47.506497
2271.256237	140.909705	47.511501
2267.820185	133.314275	47.516506
2264.516912	133.858145	47.521511
2261.050650	131.803112	47.526516
2257.721257	133.221964	47.531521
2254.429117	134.822932	47.536525
2250.981034	130.451285	47.541530
2247.096066	138.315446	47.546535
2243.568112	135.053019	47.551540
2239.989350	136.144423	47.556545
2236.789896	134.407280	47.561549
2233.503890	133.097660	47.566554
2229.608725	136.951584	47.571559
2226.290664	142.693108	47.576564
2222.655287	137.093963	47.581569
2219.258364	143.708324	47.586573
2215.644697	128.986301	47.591578
2212.429465	131.050977	47.596583
2208.809404	137.794342	47.601588
2205.343102	129.577994	47.606593
2201.566528	133.016494	47.611597
2198.573388	128.659759	47.616602
2195.142333	133.883584	47.621607
2191.289135	136.403692	47.626612
2187.658063	138.988757	47.631617
2184.068928	138.216455	47.636621
2181.166840	134.206618	47.641626
2177.492348	139.643916	47.646631
2174.131145	133.933037	47.651636
2170.237760	135.332194	47.656641
2166.717115	139.530848	47.661645
2163.582686	137.254145	47.666650
2159.713561	136.551576	47.671655
2156.404672	127.426375	47.676660
2152.991565	133.335193	47.681665
2149.472069	139.358672	47.686669
2145.924432	123.036435	47.691674
2142.189245	135.917190	47.696679
2138.946528	126.402973	47.701684
2135.586543	129.282540	47.706689
2131.751389	138.446134	47.711693
2128.863167	118.781611	47.716698
2124.951392	133.761631	47.721703
2121.687680	126.644435	47.726708
2118.410086	122.839522	47.731713
2114.278480	138.176136	47.736717
2110.920149	136.304086	47.741722
2107.275402	129.831380	47.746727
2103.776850	124.437670	47.751732
2100.804105	125.208871	47.756737
2097.068934	131.412055	47.761741
2093.750613	133.075075	47.766746
2089.836647	130.793747	47.771751
2086.477629	130.788863	47.776756
2083.019500	119.036316	47.781761
2079.345336	123.324908	47.786765
2075.955557	123.035811	47.791770
2072.302962	132.480107	47.796775
2068.811805	122.051058	47.801780
2065.772140	127.150539	47.806785
2062.535082	127.170723	47.811789
2059.023210	122.755489	47.816794
2055.006294	134.511413	47.821799
2051.245370	137.020337	47.826804
2047.885072	134.176953	47.831809
2044.357451	135.677033	47.836813
2041.350706	125.559136	47.841818
2037.369627	134.193945	47.846823
2033.799426	130.043917	47.851828
2030.902058	123.582832	47.856833
2027.063958	129.652493	47.861837
2023.412470	122.239464	47.866842
2019.918612	132.335836	47.871847
2015.973215	132.857253	47.876852
2013.115730	132.434904	47.881857
2009.893212	130.532209	47.886861
2006.454716	125.359348	47.891866
2002.748954	120.630243	47.896871
1999.135598	126.736415	47.901876
1996.228654	125.489865	47.906881
1992.264918	133.486408	47.911885
1989.007201	118.531366	47.916890
1984.952512	124.687938	47.921895
1981.495034	127.215472	47.926900
1978.196813	129.312949	47.931905
1974.361656	132.806878	47.936909
1971.474384	118.473268	47.941914
1967.760144	124.813196	47.946919
1963.957951	119.729445	47.951924
1960.597687	125.403899	47.956929
1956.984007	119.206612	47.961933
1953.831616	119.143224	47.966938
1950.292710	128.828915	47.971943
1946.793854	122.530576	47.976948
1943.252228	119.641443	47.981953
1939.555110	123.288428	47.986957
1935.909132	127.470838	47.991962
1932.500510	121.998078	47.996967
1928.919914	123.261301	48.001972
1925.739429	112.918020	48.006977
1922.100063	121.964953	48.011981
1918.701540	121.786738	48.016986
1914.855797	121.913674	48.021991
1911.863121	124.371985	48.026996
1908.581574	115.443757	48.032001
1904.198675	118.157743	48.037005
1901.493771	114.986975	48.042010
1897.494639	125.986230	48.047015
1894.426359	115.653250	48.052020
1891.003934	106.661481	48.057025
1887.087960	123.488846	48.062029
1883.718065	120.758865	48.067034
1879.969253	124.700181	48.072039
1876.331669	122.580983	48.077044
1873.196736	113.253227	48.082049
1869.476616	121.127917	48.087053
1866.307965	118.162831	48.092058
1862.721945	118.584359	48.097063
1858.868272	124.560611	48.102068
1855.960046	116.697172	48.107073
1852.061680	120.529020	48.112077
1848.565140	121.529771	48.117082
1844.932740	124.896570	48.122087
1841.839816	114.145789	48.127092
1838.315138	111.764062	48.132097
1834.499011	120.897478	48.137101
1831.210537	109.388865	48.142106
1827.823701	107.360110	48.147111
1824.072647	113.662211	48.152116
1820.793053	107.586275	48.157121
1816.640371	116.459751	48.162125
1813.325660	114.763252	48.167130
1809.892255	118.175942	48.172135
1806.738644	121.805469	48.177140
1803.416471	112.978364	48.182145
1799.568210	108.258763	48.187149
1796.296869	116.839646	48.192154
1792.564611	117.787811	48.197159
1789.333513	121.995724	48.202164
1785.756094	117.681718	48.207169
1782.036796	125.613958	48.212173
1778.617217	115.967823	48.217178
1775.339971	115.473667	48.222183
1771.674659	116.188980	48.227188
1768.026943	113.378685	48.232193
1764.376938	119.275774	48.237197
1761.107576	109.360732	48.242202
1757.894197	122.269976	48.247207
1754.458231	115.813993	48.252212
1750.428752	107.481885	48.257217
1747.079116	118.032745	48.262221
1743.849260	115.060490	48.267226
1739.799895	113.361089	48.272231
1736.415702	112.975800	48.277236
1733.306501	111.653505	48.282241
1729.668638	121.171957	48.287245
1725.869548	113.478089	48.292250
1722.706843	119.046449	48.297255
1718.768764	117.099569	48.302260
1715.416696	111.650988	48.307265
1712.060744	120.356807	48.312269
1708.751608	106.375892	48.317274
1705.066554	122.068609	48.322279
1701.649017	119.498191	48.327284
1698.378717	119.688301	48.332289
1694.729946	115.060548	48.337293
1691.384631	107.322527	48.342298
1687.290323	116.306443	48.347303
1683.978545	116.742788	48.352308
1680.613370	122.930131	48.357313
1676.880781	117.398219	48.362317
1673.711905	113.957718	48.367322
1669.872913	116.454964	48.372327
1666.556840	116.377371	48.377332
1663.077544	101.404568	48.382337
1659.505184	121.045796	48.387341
1656.347255	107.972566	48.392346
1652.863969	116.096193	48.397351
1648.787945	116.541417	48.402356
1645.348553	107.583043	48.407361
1642.339936	124.393458	48.412365
1638.983821	111.526249	48.417370
1635.059469	113.880741	48.422375
1631.254657	124.137069	48.427380
1628.006128	115.966126	48.432385
1624.330948	121.711577	48.437389
1621.107837	114.883279	48.442394
1617.594837	114.205589	48.447399
1613.981500	116.531601	48.452404
1610.668128	122.336079	48.457409
1606.415435	117.859494	48.462413
1603.134854	111.920246	48.467418
1599.931246	106.443871	48.472423
1597.041507	108.051211	48.477428
1593.530630	110.475553	48.482433
1589.731490	116.235788	48.487437
1586.102512	112.221736	48.492442
1582.294828	116.126825	48.497447
1578.794729	113.665853	48.502452
1575.600362	108.190336	48.507457
1571.939636	118.598131	48.512461
1568.424774	114.413483	48.517466
1564.901928	113.006913	48.522471
1561.330655	113.903793	48.527476
1558.247495	107.834079	48.532481
1554.460009	110.288173	48.537485
1551.232736	99.155284	48.542490
1547.556501	104.527398	48.547495
1543.951397	111.952320	48.552500
1540.732862	100.272156	48.557505
1536.866130	109.580892	48.562509
1533.070760	109.219888	48.567514
1529.865426	106.707681	48.572519
1526.519359	104.297076	48.577524
1523.200521	104.470662	48.582529
1519.355001	112.413678	48.587533
1516.000435	100.825477	48.592538
1512.714308	111.323551	48.597543
1508.585167	116.952488	48.602548
1505.336990	105.263434	48.607553
1501.900095	107.302449	48.612557
1498.744366	108.586952	48.617562
1494.751877	110.760217	48.622567
1491.615930	106.455984	48.627572
1488.271691	102.822988	48.632577
1484.098980	107.063959	48.637581
1481.038034	97.221863	48.642586
1477.543477	112.028360	48.647591
1474.001026	100.093539	48.652596
1470.815832	99.690555	48.657601
1466.708177	112.953368	48.662605
1463.565301	103.245198	48.667610
1459.944021	108.998829	48.672615
1456.302559	105.013985	48.677620
1452.750046	104.031158	48.682625
1449.312849	103.997418	48.687629
1445.918542	103.270249	48.692634
1442.440627	116.417167	48.697639
1439.048269	110.148415	48.702644
1436.058263	110.998264	48.707649
1431.766438	112.786316	48.712653
1428.387698	109.772197	48.717658
1424.521920	104.849403	48.722663
1421.211525	105.323594	48.727668
1417.825489	102.533288	48.732673
1414.083107	111.957135	48.737677
1411.032625	109.232540	48.742682
1407.281038	103.627043	48.747687
1403.650039	104.615612	48.752692
1400.787864	107.531012	48.757697
1397.267780	104.488378	48.762701
1393.695217	103.101013	48.767706
1390.025671	104.095568	48.772711
1386.023569	111.021631	48.777716
1382.819456	103.082523	48.782721
1379.218501	105.120327	48.787725
1375.659205	102.348428	48.792730
1372.250854	101.989500	48.797735
1368.680151	104.415607	48.802740
1365.578703	102.281221	48.807745
1361.613013	99.026129	48.812749
1358.175795	102.521855	48.817754
1354.802349	103.918020	48.822759
1351.116596	108.172551	48.827764
1348.259923	100.256755	48.832769
1344.467654	107.441608	48.837773
1340.980087	101.718726	48.842778
1337.507998	115.725139	48.847783
1333.444372	108.217238	48.852788
1330.312135	100.254649	48.857793
1326.579437	113.973603	48.862797
1323.615295	103.141167	48.867802
1319.822724	107.212290	48.872807
1316.150791	107.397817	48.877812
1312.581374	102.497377	48.882817
1309.152752	101.710663	48.887821
1305.846007	104.236058	48.892826
1302.519251	106.067370	48.897831
1298.821740	106.298580	48.902836
1295.620146	106.875055	48.907841
1291.822023	102.398825	48.912845
1288.011010	100.008422	48.917850
1284.668178	103.328557	48.922855
1281.190598	109.842982	48.927860
1278.142125	103.274593	48.932865
1274.386759	107.122924	48.937869
1270.522533	107.325278	48.942874
1267.223064	101.949857	48.947879
1263.842320	100.254415	48.952884
1260.486177	109.920397	48.957889
1256.752165	107.305744	48.962893
1253.350046	106.473843	48.967898
1249.432208	106.137660	48.972903
1245.871986	105.817944	48.977908
1242.652068	100.215675	48.982913
1239.057286	107.433871	48.987917
1236.015246	99.849147	48.992922
1232.605343	98.557765	48.997927
1228.819449	105.753688	49.002932
1225.320199	96.347350	49.007937
1221.556326	97.271396	49.012941
1218.259230	98.800278	49.017946
1214.879561	101.418700	49.022951
1211.271883	110.449427	49.027956
1207.671785	104.561141	49.032961
1204.112160	108.411307	49.037965
1200.742347	98.912943	49.042970
1197.392451	104.272018	49.047975
1193.724837	108.892889	49.052980
1190.434175	108.611928	49.057985
1186.176319	112.361851	49.062989
1183.370905	101.483351	49.067994
1179.673472	102.194571	49.072999
1176.312078	110.750462	49.078004
1172.528730	94.662313	49.083009
1169.213041	100.358328	49.088013
1165.625886	98.358258	49.093018
1162.080141	97.897289	49.098023
1158.560515	97.339650	49.103028
1155.031822	100.237713	49.108033
1151.697788	107.648680	49.113037
1148.347704	100.986198	49.118042
1145.154019	103.247327	49.123047
1140.908498	100.638211	49.128052
1137.635712	89.550294	49.133057
1133.691948	101.115592	49.138061
1130.636937	94.433547	49.143066
1127.171385	97.486757	49.148071
1123.637084	95.486469	49.153076
1120.191280	96.595603	49.158081
1116.437483	101.925606	49.163085
1113.125719	96.882092	49.168090
1109.577671	96.328599	49.173095
1106.018770	98.882997	49.178100
1102.878291	91.938044	49.183105
1099.249789	98.814005	49.188109
1095.755387	100.780929	49.193114
1092.095495	103.120363	49.198119
1088.240836	95.478895	49.203124
1085.153354	96.675036	49.208129
1081.391676	105.720263	49.213133
1078.199882	92.434475	49.218138
1074.779877	100.843038	49.223143
1070.912001	101.883073	49.228148
1067.649170	92.297871	49.233153
1064.022557	94.173211	49.238157
1060.583091	95.299694	49.243162
1057.078458	97.091722	49.248167
1053.107688	109.285138	49.253172
1050.440002	100.975204	49.258177
1046.735825	102.534224	49.263181
1043.400620	101.973019	49.268186
1039.533304	91.846054	49.273191
1036.016266	99.701369	49.278196
1032.630462	90.980742	49.283201
1028.963893	109.414596	49.288205
1025.586025	98.447943	49.293210
1021.939020	101.295616	49.298215
1018.343106	102.953185	49.303220
1014.927088	96.351643	49.308225
1011.578775	96.517647	49.313229
1008.201266	95.481566	49.318234
1004.850854	95.801253	49.323239
1000.983825	103.720982	49.328244
997.466235	96.345717	49.333249
993.856207	111.446492	49.338253
990.507191	100.325121	49.343258
987.282044	99.256163	49.348263
983.226245	104.516428	49.353268
980.118812	99.999074	49.358273
976.440005	104.902180	49.363277
972.961216	94.325627	49.368282
969.543388	104.171307	49.373287
966.061628	107.711979	49.378292
962.474198	93.395111	49.383297
959.338544	102.346767	49.388301
955.546641	106.184223	49.393306
951.755969	95.651570	49.398311
948.044389	103.969711	49.403316
944.791330	96.657306	49.408321
941.319323	102.558706	49.413325
937.890133	94.188305	49.418330
934.643445	95.598939	49.423335
930.701037	99.976552	49.428340
927.656484	96.701537	49.433345
923.977020	101.426595	49.438349
920.525141	92.882950	49.443354
916.662446	94.673127	49.448359
913.294962	93.153761	49.453364
910.087534	87.377019	49.458369
906.321417	97.229820	49.463373
903.070821	93.454115	49.468378
899.601342	106.967411	49.473383
895.962545	103.694001	49.478388
892.452893	90.494096	49.483393
888.638846	100.052716	49.488397
885.391619	92.627506	49.493402
881.959254	91.268476	49.498407
878.501102	103.597860	49.503412
874.754297	98.628263	49.508417
871.290545	101.486396	49.513421
867.849021	101.074530	49.518426
864.305455	103.126921	49.523431
860.766420	101.635770	49.528436
857.723017	93.211892	49.533441
853.932817	102.651942	49.538445
850.191369	107.231810	49.543450
847.006659	103.323294	49.548455
843.404016	99.470686	49.553460
839.905349	93.629093	49.558465
836.216013	107.382051	49.563469
832.927211	93.519518	49.568474
829.241078	93.397774	49.573479
825.698724	98.399392	49.578484
822.395503	97.356888	49.583489
818.544837	101.755928	49.588493
815.343514	99.290351	49.593498
812.295001	94.569199	49.598503
808.585249	97.938520	49.603508
805.077234	91.472156	49.608513
801.217374	91.165850	49.613517
797.486226	90.342546	49.618522
794.570513	102.628238	49.623527
790.654981	99.840361	49.628532
787.576509	89.010292	49.633537
783.786107	95.242911	49.638541
780.054603	90.856172	49.643546
776.786217	100.351454	49.648551
773.380239	91.363442	49.653556
770.248183	92.925730	49.658561
766.216123	96.150471	49.663565
762.854239	87.021184	49.668570
759.185393	104.773978	49.673575
755.624497	101.592785	49.678580
752.149366	91.482727	49.683585
748.534213	92.803878	49.688589
745.509058	95.164488	49.693594
742.009820	98.909105	49.698599
738.141771	101.529332	49.703604
734.931243	92.649524	49.708609
730.980350	93.955779	49.713613
727.808086	90.430106	49.718618
724.245435	94.240479	49.723623
720.816923	93.465845	49.728628
717.350502	89.189825	49.733633
713.788084	98.590126	49.738637
710.297819	90.816118	49.743642
706.992858	88.451242	49.748647
703.112249	94.964464	49.753652
699.735061	82.419303	49.758657
696.129121	92.288383	49.763661
692.985028	93.767467	49.768666
689.420362	85.155464	49.773671
685.283701	90.827385	49.778676
682.067571	84.509785	49.783681
678.631129	91.533463	49.788685
675.151153	81.110715	49.793690
671.799125	86.342033	49.798695
668.235957	88.797030	49.803700
664.888525	89.834982	49.808705
661.399286	91.771387	49.813709
657.844673	79.818621	49.818714
654.259066	91.651614	49.823719
650.326156	102.173153	49.828724
647.260174	84.487631	49.833729
644.019653	94.342866	49.838733
640.251175	81.661409	49.843738
636.436253	85.846098	49.848743
632.866946	95.477887	49.853748
629.799749	89.249943	49.858753
625.760099	101.616299	49.863757
622.490749	86.717686	49.868762
619.453112	92.326432	49.873767
615.686905	97.392871	49.878772
612.539412	88.061493	49.883777
608.988554	96.320731	49.888781
605.172558	95.295744	49.893786
601.537753	99.662209	49.898791
597.825688	91.178472	49.903796
594.735493	91.027785	49.908801
590.837816	95.610420	49.913805
588.018359	85.118125	49.918810
583.928179	85.614205	49.923815
580.561534	86.095556	49.928820
577.046120	85.930581	49.933825
573.232730	82.973664	49.938829
570.068957	84.218695	49.943834
566.994865	78.867329	49.948839
563.050138	97.573635	49.953844
559.618798	87.392176	49.958849
555.888032	90.135476	49.963853
552.486489	95.682130	49.968858
549.150272	95.268484	49.973863
545.726952	96.777890	49.978868
542.550203	91.797940	49.983873
538.135507	94.720927	49.988877
534.896747	88.588539	49.993882
531.124711	84.539862	49.998887
528.021797	92.767069	50.003892
524.573728	85.389600	50.008897
521.190810	93.642819	50.013901
517.682363	101.255344	50.018906
514.364436	92.586091	50.023911
510.211717	98.512233	50.028916
506.991666	86.799061	50.033921
503.418228	96.089840	50.038925
500.274016	95.759900	50.043930
496.825346	93.972892	50.048935
493.153701	97.404046	50.053940
489.549300	97.085933	50.058945
486.057729	97.416544	50.063949
482.333107	92.264847	50.068954
478.926712	92.411857	50.073959
475.468045	94.381434	50.078964
472.402222	89.452450	50.083969
468.323433	93.308769	50.088973
465.070687	93.489169	50.093978
461.690372	80.295113	50.098983
457.857366	81.522704	50.103988
454.543665	88.065448	50.108993
450.862584	85.969035	50.113997
447.566404	84.610904	50.119002
443.410538	87.126866	50.124007
439.906022	91.791382	50.129012
437.061680	85.174661	50.134017
433.603378	88.810713	50.139021
430.196194	87.908064	50.144026
426.733997	89.472342	50.149031
423.517258	83.262205	50.154036
420.056613	82.195743	50.159041
415.757822	89.948213	50.164045
412.258997	92.765729	50.169050
408.667017	82.898908	50.174055
405.425004	91.435348	50.179060
402.069822	88.901224	50.184065
398.482190	95.051654	50.189069
394.652543	90.090680	50.194074
391.359417	92.291436	50.199079
387.609408	95.811027	50.204084
384.726658	86.797936	50.209089
380.980423	88.503587	50.214093
377.173740	82.038487	50.219098
374.073237	82.101405	50.224103
370.373709	89.695534	50.229108
367.330327	88.521574	50.234113
363.413768	91.407280	50.239117
359.865551	83.291129	50.244122
356.405930	92.372351	50.249127
352.760979	85.169108	50.254132
349.462603	93.161783	50.259137
345.752054	88.594366	50.264141
342.239868	88.146068	50.269146
339.053375	95.702078	50.274151
335.427373	89.353138	50.279156
332.209719	87.412390	50.284161
328.183086	98.483093	50.289165
325.026155	95.136146	50.294170
321.592590	91.754675	50.299175
317.568346	86.596286	50.304180
314.438457	86.802641	50.309185
310.598821	79.437091	50.314189
307.378572	86.455243	50.319194
303.887410	86.097626	50.324199
300.267585	80.159342	50.329204
296.970572	81.190018	50.334209
292.919094	80.667238	50.339213
289.601702	71.923904	50.344218
286.267214	80.208137	50.349223
282.438943	79.324199	50.354228
279.769303	83.352564	50.359233
276.035059	80.258694	50.364237
272.602947	80.634889	50.369242
268.869923	77.530366	50.374247
265.213419	85.499495	50.379252
261.817303	76.041440	50.384257
258.283030	83.601194	50.389261
254.562452	79.569908	50.394266
251.442011	79.203064	50.399271
247.713521	86.903710	50.404276
244.244174	81.430551	50.409281
240.529163	88.326013	50.414285
237.260777	90.158111	50.419290
234.153589	92.771419	50.424295
230.435048	79.234555	50.429300
226.807572	78.090294	50.434305
223.391948	85.401328	50.439309
219.875784	84.493405	50.444314
216.315412	84.683478	50.449319
212.137104	94.040066	50.454324
209.490287	82.109915	50.459329
205.717880	87.730647	50.464333
202.670037	82.008960	50.469338
198.826482	85.950113	50.474343
194.882221	91.741583	50.479348
191.896722	81.694052	50.484353
187.879312	80.690352	50.489357
184.611392	85.410219	50.494362
181.234731	90.199991	50.499367
177.695628	88.999108	50.504372
174.373273	86.172808	50.509377
170.817358	91.604202	50.514381
166.936024	88.530439	50.519386
163.869733	91.624642	50.524391
160.363813	99.613132	50.529396
156.822522	87.007226	50.534401
152.796689	88.638986	50.539405
149.447753	82.945285	50.544410
146.336513	87.533271	50.549415
142.817010	86.703124	50.554420
139.297050	81.870304	50.559425
135.976725	87.499325	50.564429
132.345939	88.302801	50.569434
128.878854	88.851452	50.574439
124.677448	83.905716	50.579444
121.995635	86.224108	50.584449
118.107476	93.082032	50.589453
114.462430	94.932775	50.594458
111.352632	91.571087	50.599463
107.353116	91.759169	50.604468
104.355909	81.748971	50.609473
100.580673	91.624808	50.614477
97.112915	90.962944	50.619482
93.991805	79.607709	50.624487
89.924285	100.536160	50.629492
86.373201	79.525461	50.634497
82.659285	89.758991	50.639501
79.604754	94.439263	50.644506
76.357373	92.120606	50.649511
72.689158	87.049935	50.654516
69.352940	87.823438	50.659521
65.655894	94.336986	50.664525
62.109198	92.726409	50.669530
58.740324	83.282176	50.674535
54.632181	95.175476	50.679540
51.802699	83.664636	50.684545
48.144630	96.502063	50.689549
45.012120	87.292604	50.694554
41.367674	84.988613	50.699559
37.708575	96.523806	50.704564
34.127424	80.155521	50.709569
30.399960	93.269075	50.714573
27.269587	86.116104	50.719578
23.406222	89.857630	50.724583
20.000260	88.645886	50.729588
16.739497	77.119470	50.734593
12.838355	88.545175	50.739597