Tue Jun 21 10:31:10 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.500040	82.411075	0.000000
0.405647	83.217905	0.005005
0.611545	80.708134	0.010010
0.473819	79.198721	0.015014
0.521995	82.150256	0.020019
0.592647	68.800600	0.025024
0.177191	70.171889	0.030029
-0.349343	53.995651	0.035034
-0.175959	53.725882	0.040038
-0.406093	54.201763	0.045043
-0.467664	37.747662	0.050048
-0.890882	34.089004	0.055053
-1.455599	19.952455	0.060058
-1.629705	17.747946	0.065062
-1.909885	21.121869	0.070067
-2.204071	8.293060	0.075072
-3.029483	4.510385	0.080077
-2.901764	9.451474	0.085082
-2.981632	11.925535	0.090086
-3.818875	7.839741	0.095091
-4.021420	8.264875	0.100096
-4.714842	11.624939	0.105101
-4.651379	18.440487	0.110106
-4.492911	3.820711	0.115110
-4.821324	19.666812	0.120115
-4.462688	9.634654	0.125120
-4.716082	8.256883	0.130125
-5.349283	12.499515	0.135130
-5.813432	9.782213	0.140134
-6.201455	6.075900	0.145139
-5.893078	5.019307	0.150144
-6.656251	4.040305	0.155149
-7.498202	11.754465	0.160154
-7.742240	10.919785	0.165158
-7.723588	10.621964	0.170163
-7.192188	12.462003	0.175168
-7.660270	11.073212	0.180173
-7.927100	10.548766	0.185178
-7.520551	7.078115	0.190182
-8.480208	13.857856	0.195187
-8.990504	6.705820	0.200192
-9.262830	9.712782	0.205197
-9.447869	13.531131	0.210202
-9.132914	5.376145	0.215206
-9.836391	17.445225	0.220211
-10.694719	9.374807	0.225216
-11.002668	10.865041	0.230221
-10.667149	12.329825	0.235226
-10.643882	4.238927	0.240230
-10.642249	10.536251	0.245235
-10.897347	15.112321	0.250240
-11.335164	14.581657	0.255245
-11.648641	17.892816	0.260250
-11.794521	18.037037	0.265254
-12.343689	15.102539	0.270259
-12.456058	9.412761	0.275264
-13.292012	9.841750	0.280269
-13.817239	16.699133	0.285274
-13.711562	10.405518	0.290278
-13.662496	15.040741	0.295283
-13.758408	14.324205	0.300288
-13.727631	12.925622	0.305293
-14.238513	15.800211	0.310298
-13.824471	5.432885	0.315302
-14.878542	14.423797	0.320307
-14.976781	2.839889	0.325312
-15.449895	5.910883	0.330317
-15.532265	17.781602	0.335322
-15.657570	11.704626	0.340326
-16.358555	8.363504	0.345331
-16.679649	16.992293	0.350336
-16.926874	8.374510	0.355341
-16.995737	6.498304	0.360346
-16.938936	-1.547231	0.365350
-17.164699	13.449708	0.370355
-17.003134	3.234700	0.375360
-17.618154	9.744843	0.380365
-18.089967	7.816174	0.385370
-18.239137	10.714928	0.390374
-18.771691	19.260927	0.395379
-18.625706	12.019749	0.400384
-19.589182	15.405788	0.405389
-19.942464	9.325915	0.410394
-20.037374	3.577600	0.415398
-19.713241	14.750520	0.420403
-19.999340	9.707561	0.425408
-20.508592	15.418158	0.430413
-20.767781	15.501419	0.435418
-20.622265	9.447875	0.440422
-20.824950	20.031183	0.445427
-21.338576	4.546495	0.450432
-21.561813	17.324200	0.455437
-22.108123	19.222921	0.460442
-21.727700	13.706887	0.465446
-21.888763	17.359059	0.470451
-22.776565	17.577399	0.475456
-23.086617	14.131876	0.480461
-23.608285	18.360185	0.485466
-23.273110	5.755723	0.490470
-23.434622	8.970874	0.495475
-23.513094	13.981232	0.500480
-24.000766	15.957267	0.505485
-24.788440	19.121006	0.510490
-24.587524	5.563553	0.515494
-24.909684	10.714510	0.520499
-25.252037	7.761554	0.525504
-25.295285	13.613627	0.530509
-25.172335	23.196797	0.535514
-26.205752	16.351415	0.540518
-26.956725	23.252894	0.545523
-26.638427	13.342658	0.550528
-26.723236	22.200300	0.555533
-26.937262	21.990540	0.560538
-26.739718	14.339250	0.565542
-27.166007	17.512803	0.570547
-27.101245	26.504335	0.575552
-27.951728	24.110504	0.580557
-28.575413	16.624412	0.585562
-28.118885	12.033308	0.590566
-28.495984	18.878595	0.595571
-28.252253	6.648621	0.600576
-29.259652	9.503411	0.605581
-29.734273	11.397956	0.610586
-29.652534	13.535640	0.615590
-29.959203	12.020271	0.620595
-30.229465	15.948441	0.625600
-29.902696	16.061752	0.630605
-30.237231	11.512453	0.635610
-30.392858	16.694244	0.640614
-31.016588	21.283804	0.645619
-30.939826	18.647822	0.650624
-31.608163	16.627378	0.655629
-32.332841	22.740890	0.660634
-32.720170	11.519599	0.665638
-32.836272	19.662745	0.670643
-32.970812	23.919104	0.675648
-32.387939	18.329681	0.680653
-32.664292	14.222443	0.685658
-32.944728	17.582004	0.690662
-33.821236	18.685688	0.695667
-34.036055	14.095647	0.700672
-34.023118	11.738016	0.705677
-34.624897	17.468081	0.710682
-34.320228	17.152891	0.715686
-35.118164	18.668028	0.720691
-35.518117	19.229258	0.725696
-36.047652	16.405572	0.730701
-35.943763	19.197104	0.735706
-35.801577	23.767376	0.740710
-36.075605	22.063278	0.745715
-35.828603	16.373977	0.750720
-36.029175	25.059968	0.755725
-36.926651	19.100405	0.760730
-37.090785	22.949828	0.765734
-37.281318	21.224997	0.770739
-37.467997	17.338526	0.775744
-37.959353	14.083066	0.780749
-38.924272	19.181021	0.785754
-38.403430	14.643202	0.790758
-38.754018	20.691016	0.795763
-39.019669	20.212750	0.800768
-39.024273	17.569324	0.805773
-39.071670	24.916299	0.810778
-39.048452	19.933807	0.815782
-40.022964	26.943544	0.820787
-40.463808	27.435770	0.825792
-40.798384	17.544453	0.830797
-41.041555	22.505128	0.835802
-40.344472	17.161219	0.840806
-40.618671	27.719867	0.845811
-41.223313	25.828982	0.850816
-41.893067	28.896435	0.855821
-42.199296	27.067035	0.860826
-42.206922	21.007077	0.865830
-42.814613	18.147395	0.870835
-42.471637	13.975484	0.875840
-41.939317	21.451613	0.880845
-43.301314	19.324436	0.885850
-43.621553	10.104250	0.890854
-43.905322	22.218679	0.895859
-43.910532	22.252779	0.900864
-43.786294	24.105579	0.905869
-44.616034	22.389909	0.910874
-45.091455	20.125188	0.915878
-45.717471	22.661673	0.920883
-45.565368	19.550071	0.925888
-45.804576	24.593365	0.930893
-45.547215	25.252746	0.935898
-45.685751	20.389196	0.940902
-45.977637	20.823011	0.945907
-45.976411	17.820656	0.950912
-46.196273	13.379254	0.955917
-47.024634	25.260836	0.960922
-47.075803	15.942019	0.965926
-47.378526	25.604363	0.970931
-47.799248	23.458062	0.975936
-47.858112	17.803429	0.980941
-48.625735	19.855230	0.985946
-48.709195	15.012753	0.990950
-48.981610	24.166482	0.995955
-48.948273	15.682404	1.000960
-48.844677	21.624614	1.005965
-49.160998	18.795615	1.010970
-49.377239	21.986284	1.015974
-50.268679	20.259718	1.020979
-50.380847	20.221152	1.025984
-50.594638	26.096142	1.030989
-50.668967	22.289338	1.035994
-50.115346	23.355893	1.040998
-51.055806	25.875583	1.046003
-51.623247	18.360842	1.051008
-51.802237	26.992742	1.056013
-52.273962	25.234163	1.061018
-52.258075	18.086161	1.066022
-52.710997	23.975493	1.071027
-52.255160	16.975648	1.076032
-52.389976	17.997751	1.081037
-53.391073	16.797678	1.086042
-53.514745	20.280660	1.091046
-54.113712	19.135155	1.096051
-54.369491	23.083031	1.101056
-54.124564	23.695137	1.106061
-54.580662	30.726771	1.111066
-54.070471	15.074704	1.116070
-55.065694	22.257184	1.121075
-55.236652	19.204016	1.126080
-55.251372	22.774727	1.131085
-55.693662	15.603936	1.136090
-55.599409	9.314188	1.141094
-56.511860	26.362079	1.146099
-56.581970	16.966084	1.151104
-56.539588	13.003005	1.156109
-57.124714	16.643312	1.161114
-56.892811	18.116569	1.166118
-57.234160	27.330654	1.171123
-57.723014	18.932657	1.176128
-58.126693	24.419957	1.181133
-58.504010	29.776797	1.186138
-58.504768	19.387580	1.191142
-58.608365	23.159490	1.196147
-58.477346	17.440457	1.201152
-58.625051	21.529091	1.206157
-59.879523	25.523758	1.211162
-59.777895	20.526703	1.216166
-59.895653	15.058044	1.221171
-59.979658	15.366068	1.226176
-60.136570	20.936426	1.231181
-61.192627	24.576186	1.236186
-61.413264	5.031982	1.241190
-61.639712	22.271339	1.246195
-61.892264	23.264791	1.251200
-61.669100	14.627326	1.256205
-62.208861	22.465107	1.261210
-61.705894	16.444322	1.266214
-61.960098	25.857095	1.271219
-62.190325	26.119872	1.276224
-63.154802	23.562000	1.281229
-63.389632	27.604482	1.286234
-63.389874	25.867280	1.291238
-63.362181	24.012971	1.296243
-64.287043	18.357898	1.301248
-64.620338	16.511079	1.306253
-65.023516	18.545152	1.311258
-64.943794	15.718451	1.316262
-64.851981	21.912633	1.321267
-64.971628	10.836064	1.326272
-64.867430	4.339840	1.331277
-65.376070	21.477534	1.336282
-66.178877	14.766248	1.341286
-66.666162	33.286687	1.346291
-66.777473	23.653214	1.351296
-66.552460	23.234785	1.356301
-66.908249	24.299601	1.361306
-66.502645	15.974296	1.366310
-67.972972	20.324392	1.371315
-67.985883	10.124268	1.376320
-67.993430	15.778421	1.381325
-68.251174	12.022912	1.386330
-67.904058	11.413570	1.391334
-68.567217	22.073332	1.396339
-69.037224	15.383891	1.401344
-69.440806	12.611971	1.406349
-69.771491	17.215755	1.411354
-69.526508	9.556611	1.416358
-69.611106	20.362883	1.421363
-70.072115	12.676603	1.426368
-70.449484	21.029960	1.431373
-71.118008	10.415673	1.436378
-71.166384	7.268406	1.441382
-71.535458	10.731248	1.446387
-71.645440	15.555212	1.451392
-71.320555	10.249854	1.456397
-71.530731	17.402175	1.461402
-72.023357	0.073497	1.466406
-72.792510	8.445948	1.471411
-72.814269	12.132868	1.476416
-72.955745	9.839883	1.481421
-73.116629	18.729260	1.486426
-73.140291	8.991691	1.491430
-74.455618	10.071756	1.496435
-74.561142	7.024924	1.501440
-74.475780	10.834407	1.506445
-74.623037	11.227497	1.511450
-74.780421	13.856871	1.516454
-74.947341	12.709675	1.521459
-74.968167	14.663062	1.526464
-74.843289	11.035010	1.531469
-75.709267	13.617947	1.536474
-75.858993	6.564078	1.541478
-76.401679	11.708143	1.546483
-76.415205	12.193343	1.551488
-76.441606	18.756776	1.556493
-77.326297	17.091259	1.561498
-77.907272	5.118637	1.566502
-78.026414	20.151593	1.571507
-77.964130	6.168565	1.576512
-77.985398	8.792366	1.581517
-77.894404	13.977516	1.586522
-78.071247	8.685590	1.591526
-78.480386	16.443128	1.596531
-79.176615	7.729810	1.601536
-79.106436	8.001643	1.606541
-79.766308	25.416579	1.611546
-79.406218	13.266986	1.616550
-80.037326	20.352464	1.621555
-79.962753	15.246622	1.626560
-80.698324	19.470697	1.631565
-81.120273	20.109377	1.636570
-81.154894	13.551878	1.641574
-81.141293	23.452111	1.646579
-81.333171	20.803391	1.651584
-81.528447	15.629759	1.656589
-82.191772	23.262847	1.661594
-82.233145	18.302697	1.666598
-82.154940	20.480825	1.671603
-82.767293	18.348703	1.676608
-82.487946	12.788628	1.681613
-83.498685	18.632207	1.686618
-84.015813	16.102474	1.691622
-84.214698	15.442658	1.696627
-84.326972	18.476002	1.701632
-84.056189	18.213978	1.706637
-84.335957	19.889779	1.711642
-84.099118	14.147303	1.716646
-85.099680	21.852423	1.721651
-85.688325	22.500160	1.726656
-85.730524	16.875330	1.731661
-85.923173	26.272382	1.736666
-85.633844	20.286384	1.741670
-85.794065	24.032349	1.746675
-86.311928	14.633553	1.751680
-86.779235	15.918711	1.756685
-87.417864	25.489473	1.761690
-87.497935	16.500061	1.766694
-87.645184	15.300274	1.771699
-87.465027	12.308150	1.776704
-87.591652	18.864698	1.781709
-88.669476	19.936021	1.786714
-88.929667	20.414712	1.791718
-89.407125	19.827277	1.796723
-89.327108	12.540787	1.801728
-89.331298	18.064144	1.806733
-89.336232	22.158140	1.811738
-89.217114	9.658133	1.816742
-89.785214	18.524964	1.821747
-90.324977	17.388012	1.826752
-90.386662	13.154851	1.831757
-91.063161	27.054479	1.836762
-90.927851	16.874797	1.841766
-91.172364	24.615731	1.846771
-91.397228	20.810179	1.851776
-92.009769	25.408549	1.856781
-92.613127	24.088742	1.861786
-92.223217	11.156324	1.866790
-92.451063	24.339325	1.871795
-92.661768	12.830485	1.876800
-92.454838	17.858892	1.881805
-93.372884	17.305353	1.886810
-93.812266	13.394632	1.891814
-94.170881	17.229692	1.896819
-94.214941	17.943922	1.901824
-94.166095	18.559097	1.906829
-94.277898	18.651698	1.911834
-94.428864	10.304710	1.916838
-95.058861	18.030154	1.921843
-95.529984	21.296978	1.926848
-95.492181	13.707073	1.931853
-95.623366	10.558325	1.936858
-95.709342	16.596848	1.941862
-96.352036	16.072694	1.946867
-96.717102	14.344607	1.951872
-97.230046	11.290855	1.956877
-97.401316	17.086970	1.961882
-96.970884	9.557744	1.966886
-97.156240	7.283671	1.971891
-97.384894	13.069555	1.976896
-97.806180	8.292110	1.981901
-98.530818	13.651016	1.986906
-98.533597	20.872787	1.991910
-98.786042	21.147929	1.996915
-98.911951	11.860802	2.006912
-98.767617	11.907803	2.016909
-98.837384	10.007485	2.026906
-98.038261	10.105693	2.036902
-97.281877	4.223328	2.046899
-96.024300	8.497663	2.056896
-96.407873	9.582483	2.066893
-95.793281	10.958219	2.076890
-95.673158	15.520123	2.086886
-94.719752	12.039192	2.096883
-94.313329	5.039542	2.106880
-93.939220	14.191988	2.116877
-93.054880	14.213251	2.126874
-93.062280	14.647162	2.136870
-92.450977	7.899093	2.146867
-91.562147	6.892955	2.156864
-91.335742	14.166714	2.166861
-90.383358	11.468986	2.176858
-90.142513	11.911379	2.186854
-90.098636	7.799230	2.196851
-88.939728	6.714774	2.206848
-88.669714	10.343353	2.216845
-88.626280	15.226193	2.226842
-87.785248	19.925570	2.236838
-87.112790	14.502462	2.246835
-86.839848	14.018589	2.256832
-85.920892	14.469403	2.266829
-85.538248	17.921262	2.276826
-85.513164	20.036193	2.286822
-84.834407	18.528794	2.296819
-84.116211	18.734854	2.306816
-83.859410	17.104097	2.316813
-83.358265	14.525953	2.326810
-82.711395	12.044994	2.336806
-82.460186	8.006193	2.346803
-81.288740	14.093229	2.356800
-81.230230	12.943240	2.366797
-81.273884	10.683534	2.376794
-80.148774	14.638188	2.386790
-79.699112	15.168700	2.396787
-79.194182	11.195959	2.406784
-78.288575	13.526450	2.416781
-77.991679	17.268736	2.426778
-78.039518	14.463989	2.436774
-77.672108	20.694855	2.446771
-76.543718	20.998166	2.456768
-76.320513	14.421262	2.466765
-75.234461	20.780888	2.476762
-74.838164	19.427953	2.486758
-74.723377	14.491979	2.496755
-74.622244	15.835979	2.506752
-73.643075	15.915834	2.516749
-73.489963	23.184349	2.526746
-72.918890	27.072891	2.536742
-71.848273	24.036088	2.546739
-71.602629	26.210520	2.556736
-71.474628	16.142223	2.566733
-70.543529	23.452612	2.576730
-70.199626	25.944890	2.586726
-69.676688	19.542014	2.596723
-68.939505	24.052315	2.606720
-68.540544	27.331551	2.616717
-68.596751	26.797073	2.626714
-67.702093	17.947572	2.636710
-67.091894	18.292442	2.646707
-66.857213	18.199607	2.656704
-65.846143	21.878157	2.666701
-65.378680	18.547058	2.676698
-65.497747	16.242539	2.686694
-64.912333	16.213532	2.696691
-64.012881	15.177385	2.706688
-63.830736	12.728735	2.716685
-63.327017	9.379977	2.726682
-62.331890	21.079022	2.736678
-61.980865	13.606829	2.746675
-61.990636	10.587521	2.756672
-60.826990	11.418085	2.766669
-60.811920	16.864399	2.776666
-60.518591	9.567734	2.786662
-59.216584	9.050569	2.796659
-59.126741	15.348544	2.806656
-58.901648	17.791343	2.816653
-58.170071	13.257070	2.826650
-58.018720	15.371639	2.836646
-57.246978	11.941150	2.846643
-56.300853	7.328275	2.856640
-56.311966	14.505038	2.866637
-55.645657	15.706046	2.876634
-54.529407	19.253370	2.886630
-54.531754	12.669165	2.896627
-54.600540	13.255306	2.906624
-53.676318	15.115429	2.916621
-53.058745	9.806926	2.926618
-53.059908	20.318882	2.936614
-52.442792	14.424411	2.946611
-51.601244	11.730030	2.956608
-50.864341	19.504111	2.966605
-50.125864	22.818804	2.976602
-49.861258	22.566107	2.986598
-49.815547	21.454198	2.996595
-49.555059	18.477071	3.006592
-48.386861	18.303146	3.016589
-48.261242	20.674098	3.026586
-47.997894	14.166814	3.036582
-46.680475	16.378336	3.046579
-46.435235	16.979851	3.056576
-46.421931	12.776933	3.066573
-45.763609	18.292576	3.076570
-45.153053	15.973926	3.086566
-44.629932	16.452562	3.096563
-43.731189	15.372870	3.106560
-43.360744	19.519888	3.116557
-43.340633	17.811160	3.126554
-43.075750	15.235592	3.136550
-42.110962	14.003887	3.146547
-41.678417	15.484664	3.156544
-40.557909	18.804260	3.166541
-40.756633	17.887540	3.176538
-40.145294	22.094843	3.186534
-39.759546	19.718185	3.196531
-38.770989	13.241762	3.206528
-38.619707	10.523579	3.216525
-38.540632	12.979692	3.226522
-37.641655	21.680885	3.236518
-37.134216	21.938056	3.246515
-36.650532	18.484931	3.256512
-35.783130	13.079535	3.266509
-35.538070	14.617639	3.276506
-35.355178	15.564586	3.286502
-34.390414	12.994239	3.296499
-33.721888	8.883762	3.306496
-33.580557	10.520449	3.316493
-33.587528	17.184780	3.326490
-32.826410	11.125587	3.336486
-32.322136	9.957302	3.346483
-31.180144	13.161113	3.356480
-31.062661	12.027835	3.366477
-30.779911	9.947820	3.376474
-29.913021	16.090446	3.386470
-29.315442	13.664879	3.396467
-29.517891	12.288004	3.406464
-28.528360	14.193037	3.416461
-27.671497	21.614920	3.426458
-27.931470	16.765307	3.436454
-27.206860	16.421616	3.446451
-26.163434	16.106931	3.456448
-26.106077	14.650479	3.466445
-26.125719	14.893968	3.476442
-25.140834	18.584175	3.486438
-24.727973	19.371327	3.496435
-23.534787	13.779403	3.506432
-23.052238	11.621449	3.516429
-23.024218	20.031591	3.526426
-22.954775	18.838693	3.536422
-22.287783	23.683682	3.546419
-21.470759	16.417658	3.556416
-21.219339	19.239221	3.566413
-20.093647	19.070761	3.576410
-19.921615	20.005084	3.586406
-19.773968	18.495348	3.596403
-19.463590	15.095820	3.606400
-18.567740	23.402167	3.616397
-18.240502	14.795813	3.626394
-17.214717	14.550836	3.636390
-16.509130	9.312724	3.646387
-16.658109	19.770916	3.656384
-16.657998	15.064557	3.666381
-15.380523	16.032773	3.676378
-14.978222	13.961611	3.686374
-14.834409	12.342653	3.696371
-13.886339	17.146826	3.706368
-13.315167	11.421198	3.716365
-13.333235	18.243857	3.726362
-12.589716	15.925915	3.736358
-11.910372	15.409524	3.746355
-11.633485	14.735122	3.756352
-10.697939	11.480239	3.766349
-10.233843	18.120705	3.776346
-10.222260	12.045544	3.786342
-9.780362	14.529898	3.796339
-8.658619	16.616558	3.806336
-8.470784	15.721181	3.816333
-8.131989	13.973710	3.826330
-7.830492	18.616830	3.836326
-7.096268	12.482662	3.846323
-6.651440	14.864182	3.856320
-5.945362	10.869598	3.866317
-5.414114	14.590077	3.876314
-5.282293	19.142346	3.886310
-4.068084	16.010651	3.896307
-3.780471	13.836372	3.906304
-3.944610	14.259290	3.916301
-3.339209	18.535354	3.926298
-2.980356	30.771122	3.936294
-2.318748	46.454843	3.946291
-1.779879	52.098171	3.956288
-1.515925	66.238811	3.966285
-1.160342	84.395863	3.976282
-0.608118	109.044914	3.986278
0.000000	119.539525	3.991283
0.011974	133.678274	3.996288
0.203432	129.855054	4.001293
0.795726	145.827657	4.006298
0.336265	153.095914	4.011302
0.592634	146.406892	4.016307
0.706032	158.816391	4.021312
0.979417	146.179619	4.026317
0.686454	150.682867	4.031322
0.665868	150.180393	4.036326
0.845624	139.937023	4.041331
0.641145	154.800531	4.046336
0.656674	149.319813	4.051341
0.579111	154.855768	4.056346
0.755863	156.201816	4.061350
0.469743	143.779648	4.066355
0.637665	156.425800	4.071360
0.737649	153.172432	4.076365
0.988181	155.968519	4.081370
0.745113	154.447929	4.086374
1.148618	151.140947	4.091379
0.576978	163.478984	4.096384
0.958928	147.727444	4.101389
0.600498	150.822099	4.106394
0.748412	179.549306	4.111398
1.097549	177.368242	4.116403
1.138060	184.737048	4.121408
1.387553	182.550580	4.126413
0.904369	160.345545	4.131418
0.739298	160.121163	4.136422
1.121220	154.969904	4.141427
0.872216	167.720032	4.146432
1.086186	166.095343	4.151437
1.270904	179.844010	4.156442
0.870238	169.360474	4.161446
1.115699	170.244233	4.166451
0.777554	177.150232	4.171456
1.144215	180.565475	4.176461
1.020254	186.028612	4.181466
1.006503	179.487314	4.186470
1.415021	188.739336	4.191475
0.992917	187.706407	4.196480
1.240620	180.553486	4.201485
1.040387	190.901874	4.206490
0.792581	189.361542	4.211494
1.013636	184.360443	4.216499
0.884959	188.331712	4.221504
1.195810	182.583628	4.226509
1.116251	190.345087	4.231514
0.905391	190.084873	4.236518
0.882316	190.313150	4.241523
0.879234	204.393874	4.246528
1.195659	208.434118	4.251533
1.383240	222.643129	4.256538
1.534911	219.448086	4.261542
1.567748	221.329664	4.266547
1.378070	224.800337	4.271552
1.634863	216.191919	4.276557
1.374700	199.627266	4.281562
1.497185	197.468339	4.286566
1.414806	193.987637	4.291571
1.420604	194.454053	4.296576
1.445101	190.579137	4.301581
1.388385	197.956354	4.306586
1.292511	204.366006	4.311590
1.606277	198.361685	4.316595
1.669251	194.086119	4.321600
1.652544	190.585466	4.326605
1.818734	187.943724	4.331610
1.370066	189.570743	4.336614
1.657700	190.373322	4.341619
1.391861	191.523693	4.346624
1.681178	189.935267	4.351629
1.521701	188.432208	4.356634
1.371200	191.243599	4.361638
1.704299	181.537217	4.366643
1.368815	187.128128	4.371648
1.569742	187.193017	4.376653
1.537542	189.093649	4.381658
1.444013	185.552042	4.386662
1.997362	190.164395	4.391667
1.397495	194.246054	4.396672
1.796152	189.170157	4.401677
1.674693	196.279060	4.406682
1.269044	186.146806	4.411686
1.703829	198.625467	4.416691
1.895968	210.246044	4.421696
1.941357	215.181887	4.426701
1.896251	207.046950	4.431706
1.767316	195.574343	4.436710
2.066328	189.534778	4.441715
1.688325	183.895828	4.446720
1.969386	187.460225	4.451725
1.524694	186.261524	4.456730
1.527034	193.406759	4.461734
2.019853	198.885181	4.466739
1.961415	217.507107	4.471744
1.937609	199.331728	4.476749
1.854441	195.765512	4.481754
1.619939	189.421988	4.486758
1.847871	195.753548	4.491763
1.985111	210.744047	4.496768
1.981037	213.373326	4.501773
1.979985	219.419181	4.506778
1.646113	212.971530	4.511782
1.958861	209.469993	4.516787
1.692279	226.620326	4.521792
1.851036	217.966375	4.526797
2.018580	227.349099	4.531802
1.800517	220.087593	4.536806
2.151605	222.471974	4.541811
1.823477	220.114350	4.546816
2.117615	211.223086	4.551821
1.859832	225.277530	4.556826
1.703306	224.100571	4.561830
1.893378	223.819748	4.566835
1.916885	219.846320	4.571840
2.056380	216.707167	4.576845
2.005452	220.432318	4.581850
2.191282	219.701876	4.586854
2.151034	215.721049	4.591859
1.781733	226.167313	4.596864
2.196959	243.330861	4.601869
2.498390	249.779725	4.606874
2.306296	234.359366	4.611878
2.260957	226.577888	4.616883
2.137486	224.098560	4.621888
1.944460	228.963576	4.626893
2.346526	237.758284	4.631898
2.518859	242.763495	4.636902
2.475202	230.513245	4.641907
2.121136	223.632424	4.646912
2.452106	217.952628	4.651917
2.280315	214.794572	4.656922
2.059591	217.801514	4.661926
2.377016	219.051061	4.666931
2.200009	232.750941	4.671936
2.763101	240.198607	4.676941
2.169709	241.022756	4.681946
1.837503	229.490641	4.686950
2.432538	246.435566	4.691955
2.434113	257.459809	4.696960
2.433658	256.523802	4.701965
2.574851	246.492965	4.706970
2.443164	259.022853	4.711974
2.521775	250.087927	4.716979
2.504270	251.954559	4.721984
2.826781	248.697278	4.726989
2.409524	248.152345	4.731994
2.729825	247.123165	4.736998
2.563147	232.538860	4.742003
2.088655	233.785551	4.747008
2.546619	237.216275	4.752013
2.666954	245.515556	4.757018
2.679245	247.179720	4.762022
2.508680	244.081247	4.767027
2.618556	257.989985	4.772032
2.526982	252.766335	4.777037
2.784254	253.350164	4.782042
2.394473	258.837808	4.787046
2.632428	253.663192	4.792051
2.327477	255.694246	4.797056
2.649276	256.873610	4.802061
2.674748	263.198269	4.807066
2.376958	252.138979	4.812070
2.486091	247.021020	4.817075
2.411818	252.849117	4.822080
2.400174	242.476938	4.827085
2.644471	244.006975	4.832090
2.822889	246.669978	4.837094
2.738480	246.744425	4.842099
2.470300	259.757105	4.847104
2.763436	254.943160	4.852109
3.170769	268.236492	4.857114
2.851282	264.939882	4.862118
2.548446	250.169916	4.867123
2.777086	262.147784	4.872128
2.902333	269.882276	4.877133
3.138757	281.742836	4.882138
3.075239	269.676802	4.887142
3.186079	250.616506	4.892147
2.794623	253.842354	4.897152
2.593939	257.673418	4.902157
3.044636	258.201735	4.907162
2.755429	256.049995	4.912166
2.924896	262.999456	4.917171
2.889224	275.918000	4.922176
3.068677	278.773438	4.927181
3.045033	282.422255	4.932186
3.129691	276.962210	4.937190
3.264913	271.022158	4.942195
3.055766	271.041878	4.947200
3.014230	256.537074	4.952205
2.914575	256.360074	4.957210
2.879533	260.165880	4.962214
3.023684	265.167675	4.967219
2.930910	283.833452	4.972224
3.054663	281.195958	4.977229
2.876226	286.185463	4.982234
3.126551	280.982544	4.987238
3.394139	273.936008	4.992243
3.042084	287.515538	4.997248
3.052613	282.573739	5.002253
3.443839	275.966524	5.007258
3.155289	286.573903	5.012262
3.465250	272.904817	5.017267
3.280577	282.703670	5.022272
3.566922	282.264822	5.027277
3.432910	278.803110	5.032282
3.119737	280.333306	5.037286
3.379331	270.843876	5.042291
3.048277	280.753401	5.047296
3.320173	279.014717	5.052301
3.265217	279.406144	5.057306
3.022190	289.973624	5.062310
3.432577	281.686459	5.067315
3.190038	288.474258	5.072320
3.421579	281.344490	5.077325
3.307018	279.758799	5.082330
3.409812	289.844739	5.087334
3.421377	274.855148	5.092339
3.195272	275.777533	5.097344
3.368052	279.627076	5.102349
3.517482	280.629754	5.107354
3.261829	282.017617	5.112358
3.578454	281.921660	5.117363
3.192865	283.613232	5.122368
3.380675	272.368534	5.127373
3.353234	279.212472	5.132378
3.170630	282.998910	5.137382
3.122171	275.144712	5.142387
2.934750	282.231819	5.147392
3.675161	303.314774	5.152397
3.592003	301.332363	5.157402
3.350255	313.000790	5.162406
3.650324	310.321070	5.167411
3.472086	307.492038	5.172416
3.558335	311.296322	5.177421
3.546764	312.489255	5.182426
3.356430	319.030039	5.187430
3.803999	313.266371	5.192435
3.447988	320.682945	5.197440
3.745049	316.962963	5.202445
3.714383	309.661109	5.207450
3.548340	320.663029	5.212454
3.865354	313.261370	5.217459
3.805199	312.092521	5.222464
3.821389	315.046437	5.227469
3.843276	306.809579	5.232474
3.293103	320.356429	5.237478
3.891103	317.303148	5.242483
3.429444	311.415939	5.247488
3.908338	306.652917	5.252493
3.636105	311.087854	5.257498
3.564654	315.359697	5.262502
3.457700	303.848835	5.267507
3.469129	317.054830	5.272512
3.478247	334.082469	5.277517
3.809628	337.382029	5.282522
3.888116	343.348851	5.287526
3.976374	336.912945	5.292531
4.083046	340.804235	5.297536
3.963946	350.574907	5.302541
4.062307	336.347607	5.307546
3.881616	350.670802	5.312550
4.067731	339.593876	5.317555
4.132245	348.661614	5.322560
4.369962	344.171179	5.327565
4.171857	338.653740	5.332570
4.042546	337.665262	5.337574
3.808989	320.126749	5.342579
3.844804	342.928420	5.347584
4.245507	338.120121	5.352589
4.185567	341.263463	5.357594
3.974377	345.655939	5.362598
4.161124	345.619377	5.367603
4.491556	351.636837	5.372608
4.232834	327.444297	5.377613
4.146751	315.337958	5.382618
3.846093	318.377494	5.387622
4.028403	316.585361	5.392627
4.088650	333.556975	5.397632
4.384561	333.660996	5.402637
4.206860	328.577089	5.407642
4.435631	333.642447	5.412646
4.317448	319.791230	5.417651
4.165161	319.706417	5.422656
4.016781	311.941761	5.427661
4.462926	307.858464	5.432666
4.034338	312.639572	5.437670
4.436627	316.305485	5.442675
4.150417	325.442337	5.447680
4.200406	336.684373	5.452685
4.373348	341.410678	5.457690
4.376612	342.837173	5.462694
4.392287	342.412753	5.467699
4.232315	344.054144	5.472704
4.456353	342.536108	5.477709
4.207669	338.800719	5.482714
4.114719	343.817529	5.487718
4.358366	343.776873	5.492723
4.192714	350.987098	5.497728
4.620899	340.047493	5.502733
4.416129	346.227182	5.507738
4.054439	346.573102	5.512742
4.026047	331.347545	5.517747
4.210897	346.019879	5.522752
4.220037	348.618971	5.527757
4.266862	348.981902	5.532762
4.182796	356.690909	5.537766
4.992702	362.535439	5.542771
4.696201	353.516143	5.547776
4.347367	351.016884	5.552781
4.319577	355.189746	5.557786
4.525030	370.316121	5.562790
5.119339	363.744309	5.567795
4.974783	358.661218	5.572800
4.679668	350.261731	5.577805
4.466383	343.593166	5.582810
4.493409	350.121256	5.587814
4.680793	349.759376	5.592819
4.341487	352.496287	5.597824
4.720199	348.060648	5.602829
4.790825	345.468646	5.607834
4.556873	345.961743	5.612838
5.193928	353.316900	5.617843
4.816984	347.502873	5.622848
4.646871	340.996871	5.627853
4.946011	347.726375	5.632858
4.434350	350.579642	5.637862
4.578590	344.732001	5.642867
4.783725	355.541450	5.647872
4.797880	365.576995	5.652877
4.737932	378.488593	5.657882
4.721339	382.971403	5.662886
4.744840	379.167252	5.667891
4.708589	390.082606	5.672896
4.780989	371.687441	5.677901
5.084021	380.676234	5.682906
4.818256	369.231878	5.687910
5.147287	376.574312	5.692915
4.843386	388.204147	5.697920
4.966631	380.899862	5.702925
5.028767	374.857219	5.707930
5.173780	374.877495	5.712934
5.086425	374.774826	5.717939
4.863379	375.856159	5.722944
4.961304	379.405341	5.727949
5.007369	378.200349	5.732954
4.967649	384.134860	5.737958
5.281695	376.916004	5.742963
5.041138	376.699777	5.747968
5.053415	369.748756	5.752973
5.331979	374.065469	5.757978
4.885087	372.508356	5.762982
4.870171	364.373863	5.767987
4.754473	378.106147	5.772992
4.903560	372.911673	5.777997
5.004597	383.582086	5.783002
4.968558	375.623165	5.788006
5.154090	385.425113	5.793011
5.099663	385.173723	5.798016
4.698101	379.713246	5.803021
5.100427	377.567157	5.808026
4.900305	388.540234	5.813030
5.083659	375.730514	5.818035
5.175229	383.310992	5.823040
5.101146	378.613467	5.828045
5.306298	381.400534	5.833050
5.206606	379.198253	5.838054
5.335447	384.687482	5.843059
4.960431	399.943160	5.848064
5.219141	399.313519	5.853069
5.333736	400.638110	5.858074
5.107102	403.317102	5.863078
5.058088	391.345859	5.868083
5.484401	402.439193	5.873088
5.142972	398.154363	5.878093
5.283017	396.265026	5.883098
5.102146	405.579650	5.888102
5.329530	397.393966	5.893107
4.726482	401.798459	5.898112
4.822299	410.461044	5.903117
5.434839	422.651544	5.908122
5.364438	433.007603	5.913126
5.557917	434.448786	5.918131
5.846210	432.983447	5.923136
5.752885	426.410228	5.928141
5.754150	416.152029	5.933146
5.308049	402.838123	5.938150
5.617896	408.060581	5.943155
5.281977	411.420532	5.948160
5.438361	417.084001	5.953165
5.599404	428.164052	5.958170
5.683956	430.223379	5.963174
5.603804	425.763849	5.968179
5.705961	423.382502	5.973184
5.393930	412.779729	5.978189
5.719834	417.825084	5.983194
5.595893	434.289362	5.988198
5.688642	431.765908	5.993203
5.496667	444.789410	5.998208
5.726503	437.687481	6.003213
5.598575	439.398762	6.008218
5.687949	437.830790	6.013222
5.744403	433.999659	6.018227
5.668516	435.874600	6.023232
5.729059	434.964595	6.028237
5.616997	437.748747	6.033242
5.867101	434.646686	6.038246
5.884827	415.599831	6.043251
5.633258	406.795069	6.048256
5.551829	404.910831	6.053261
5.507163	403.784798	6.058266
5.292789	412.359626	6.063270
5.788220	419.815228	6.068275
5.830293	436.813448	6.073280
5.966033	425.933458	6.078285
5.596359	408.781672	6.083290
5.821596	406.089069	6.088294
5.638223	404.319788	6.093299
5.438092	402.989797	6.098304
5.588067	397.090274	6.103309
5.985570	393.937764	6.108314
5.551051	408.979522	6.113318
5.910828	399.329170	6.118323
5.534414	400.867284	6.123328
5.786634	400.636158	6.128333
5.607999	393.607216	6.133338
5.298092	406.656924	6.138342
5.873142	402.719008	6.143347
5.801663	403.673222	6.148352
6.107712	408.573068	6.153357
5.878496	407.805769	6.158362
5.470635	403.888332	6.163366
6.041248	401.875599	6.168371
5.842910	408.705268	6.173376
6.014948	402.966670	6.178381
5.999794	406.548200	6.183386
5.566547	407.026939	6.188390
5.909578	398.278239	6.193395
5.785933	408.855631	6.198400
5.909240	396.339019	6.203405
5.426632	386.677597	6.208410
5.626436	401.087415	6.213414
5.589105	385.809411	6.218419
5.621838	398.245682	6.223424
5.637356	403.178243	6.228429
5.951483	395.037793	6.233434
5.482719	393.831023	6.238438
5.477586	390.225397	6.243443
5.780800	402.938742	6.248448
5.713567	405.296713	6.253453
5.704184	398.055231	6.258458
5.584152	397.879826	6.263462
5.604992	398.586484	6.268467
5.453580	404.691055	6.273472
5.764308	398.823325	6.278477
5.866242	402.055909	6.283482
5.639366	400.623191	6.288486
5.454067	385.297858	6.293491
5.863249	393.878746	6.298496
5.469551	396.173161	6.303501
5.485318	394.330254	6.308506
5.772072	403.033642	6.313510
5.793259	397.456386	6.318515
5.529394	407.922018	6.323520
5.819133	400.107463	6.328525
6.041087	386.075342	6.333530
5.715680	383.422813	6.338534
5.694458	375.726661	6.343539
5.620424	380.391258	6.348544
5.412450	371.431492	6.353549
5.715214	381.307366	6.358554
5.302644	384.205997	6.363558
5.620717	382.242385	6.368563
5.565750	400.243326	6.373568
5.821963	401.000601	6.378573
5.859615	391.909373	6.383578
5.556664	386.581753	6.388582
5.504272	385.646051	6.393587
5.365549	387.400555	6.398592
5.840981	394.128910	6.403597
5.743761	398.735190	6.408602
5.674412	404.459123	6.413606
5.940586	400.039934	6.418611
5.773624	389.078667	6.423616
5.328365	383.126553	6.428621
5.778697	383.260456	6.433626
5.502888	386.232742	6.438630
5.573989	386.439310	6.443635
5.695302	397.257536	6.448640
5.735366	398.267676	6.453645
5.790578	392.161051	6.458650
5.453701	389.774460	6.463654
5.791045	386.923185	6.468659
5.725977	388.239242	6.473664
5.738139	389.619077	6.478669
5.854830	376.411115	6.483674
5.498766	380.704057	6.488678
5.622735	380.300974	6.493683
5.602517	388.516254	6.498688
5.622548	385.010460	6.503693
5.608592	381.020106	6.508698
5.513173	389.456228	6.513702
5.940928	394.047999	6.518707
5.872833	392.112812	6.523712
5.523100	390.971187	6.528717
5.955919	388.210469	6.533722
5.614918	384.395040	6.538726
6.049335	381.612943	6.543731
5.608939	390.044818	6.548736
5.963873	383.894091	6.553741
5.931871	382.613815	6.558746
5.726190	390.331334	6.563750
6.235967	379.250118	6.568755
6.007977	384.623199	6.573760
5.740044	385.098046	6.578765
5.711606	376.018364	6.583770
5.632099	378.259564	6.588774
6.012508	380.053217	6.593779
5.406606	359.030540	6.598784
5.349057	352.152855	6.603789
5.425262	365.099519	6.608794
5.233892	381.525770	6.613798
5.158536	379.076140	6.618803
5.198730	383.247027	6.623808
5.433090	382.246871	6.628813
5.796721	378.432772	6.633818
5.352555	374.663044	6.638822
5.481946	377.241044	6.643827
5.375847	377.867486	6.648832
5.431646	389.102876	6.653837
5.682301	399.240773	6.658842
5.766322	407.063069	6.663846
5.754973	398.480995	6.668851
5.898666	396.823123	6.673856
5.277141	382.997378	6.678861
5.652809	391.335365	6.683866
5.699084	405.805342	6.688870
5.555034	405.073867	6.693875
5.836033	405.543659	6.698880
5.941794	403.618952	6.703885
5.849219	398.469025	6.708890
5.430861	389.504223	6.713894
5.769346	384.763441	6.718899
5.831704	383.983580	6.723904
5.473286	378.568057	6.728909
5.679556	387.338044	6.733914
5.668476	387.467049	6.738918
5.611431	383.823449	6.743923
5.706913	378.919847	6.748928
5.451180	391.299685	6.753933
5.758851	384.623969	6.758938
5.413591	387.742538	6.763942
5.704495	387.757995	6.768947
5.917474	387.164147	6.773952
5.663846	392.676258	6.778957
5.854306	388.935233	6.783962
5.454652	385.059462	6.788966
5.614377	390.939441	6.793971
5.208330	380.436917	6.798976
5.481347	390.439480	6.803981
5.700758	398.812029	6.808986
5.785491	402.197439	6.813990
5.759194	408.906858	6.818995
5.655277	393.271638	6.824000
5.335840	391.972454	6.829005
5.900624	397.351216	6.834010
5.580962	413.025571	6.839014
5.740425	405.707580	6.844019
5.737381	409.653563	6.849024
5.484149	406.408114	6.854029
5.726460	403.117905	6.859034
5.506720	411.025431	6.864038
5.565111	405.219414	6.869043
5.676614	409.948019	6.874048
5.414544	416.256220	6.879053
5.845791	403.720974	6.884058
5.742811	412.575732	6.889062
5.774208	412.962138	6.894067
5.999465	410.719068	6.899072
5.719186	394.233315	6.904077
5.824320	385.741087	6.909082
5.548908	382.833804	6.914086
5.435710	380.780579	6.919091
5.137006	394.292167	6.924096
5.560017	405.590099	6.929101
6.138936	405.708235	6.934106
6.140669	392.019832	6.939110
6.044338	393.521038	6.944115
5.654620	384.506109	6.949120
5.606089	388.756614	6.954125
5.740707	386.293526	6.959130
5.287746	385.774036	6.964134
5.656306	382.488185	6.969139
5.650703	388.713254	6.974144
5.495268	387.158790	6.979149
5.991045	382.893005	6.984154
5.539832	390.760902	6.989158
5.778601	383.719088	6.994163
5.599258	383.361100	6.999168
5.707818	391.109072	7.004173
6.009647	389.926847	7.009178
5.650167	392.357284	7.014182
5.857033	383.271589	7.019187
5.966218	382.077654	7.024192
5.758073	381.373568	7.029197
6.045225	381.956402	7.034202
5.706013	384.066753	7.039206
5.693891	387.373475	7.044211
5.881733	391.437823	7.049216
5.744718	384.845018	7.054221
5.758291	378.329501	7.059226
5.535985	392.364013	7.064230
5.473494	385.777812	7.069235
5.457748	386.577160	7.074240
5.627820	388.935103	7.079245
5.607345	388.582974	7.084250
5.592267	397.648134	7.089254
6.028234	388.198495	7.094259
5.978729	387.846042	7.099264
5.674364	381.143603	7.104269
5.356960	370.365527	7.109274
5.685417	379.219668	7.114278
5.709003	378.324864	7.119283
5.526336	378.524513	7.124288
5.187007	380.654025	7.129293
5.566080	375.354766	7.134298
5.161466	386.352428	7.139302
5.374187	373.993700	7.144307
5.390774	380.184898	7.149312
5.575781	386.303612	7.154317
5.891744	379.700725	7.159322
5.285725	393.083425	7.164326
5.527945	383.372430	7.169331
5.524834	384.861554	7.174336
5.328968	385.225798	7.179341
5.562424	386.873877	7.184346
5.725444	404.875826	7.189350
5.778837	400.884182	7.194355
5.709948	396.153625	7.199360
5.618115	396.597338	7.204365
5.740701	383.734921	7.209370
5.596275	395.248960	7.214374
5.471257	390.793514	7.219379
5.798770	397.238911	7.224384
5.420434	397.370318	7.229389
5.802493	404.661162	7.234394
5.881707	412.729943	7.239398
6.070388	388.332584	7.244403
5.920498	385.892336	7.249408
5.717516	391.761926	7.254413
5.585352	392.694613	7.259418
5.676816	395.796713	7.264422
6.001417	389.060767	7.269427
5.766300	390.517070	7.274432
5.457014	390.790968	7.279437
5.710363	385.650859	7.284442
5.595295	387.231537	7.289446
5.569733	382.910589	7.294451
5.511368	380.307972	7.299456
5.222218	377.105181	7.304461
5.664515	387.491951	7.309466
5.653629	387.646578	7.314470
5.538037	384.421756	7.319475
5.563123	387.493207	7.324480
5.423279	392.384791	7.329485
6.051328	387.157770	7.334490
5.393815	383.554598	7.339494
5.620479	387.816366	7.344499
5.399638	392.274983	7.349504
5.453909	399.747583	7.354509
5.687718	405.659504	7.359514
5.640542	412.655563	7.364518
6.003230	408.670520	7.369523
6.187352	407.976268	7.374528
5.550435	390.119855	7.379533
5.879333	387.908764	7.384538
5.610852	392.734820	7.389542
5.849329	387.733929	7.394547
5.762687	381.912666	7.399552
5.736953	390.488213	7.404557
5.700109	387.107477	7.409562
5.587061	390.105304	7.414566
5.658280	385.336750	7.419571
5.771545	381.637914	7.424576
5.797897	382.311098	7.429581
5.617578	383.111056	7.434586
5.564467	384.064397	7.439590
5.777619	381.288944	7.444595
5.394791	382.629398	7.449600
5.319889	383.970961	7.454605
5.816417	386.244060	7.459610
5.692708	384.281970	7.464614
5.969563	382.552912	7.469619
5.795596	387.484877	7.474624
5.775405	383.503646	7.479629
5.577086	381.666985	7.484634
5.441509	387.131129	7.489638
5.606714	390.785406	7.494643
5.743695	384.102434	7.499648
5.512180	388.898293	7.504653
5.873965	383.722665	7.509658
5.784821	395.446398	7.514662
5.626782	394.478855	7.519667
5.566439	388.316575	7.524672
5.225758	390.415330	7.529677
5.592266	382.080517	7.534682
5.380599	391.512518	7.539686
5.361936	384.576875	7.544691
5.356126	388.395239	7.549696
5.406131	391.616686	7.554701
5.816036	395.902184	7.559706
5.885648	406.523747	7.564710
5.731645	400.399862	7.569715
5.579667	396.325994	7.574720
5.188086	400.532270	7.579725
5.448534	393.751888	7.584730
5.570980	415.488887	7.589734
5.993729	410.871491	7.594739
6.080309	407.299418	7.599744
5.853033	410.789185	7.604749
5.878703	393.142542	7.609754
5.766781	394.754669	7.614758
5.702850	386.511259	7.619763
5.673329	391.547576	7.624768
5.671511	392.677725	7.629773
5.675221	381.272015	7.634778
5.501226	389.765155	7.639782
5.587582	387.971735	7.644787
5.672982	384.906825	7.649792
5.710436	397.228449	7.654797
5.881386	382.262880	7.659802
5.606491	392.646261	7.664806
5.724255	386.929286	7.669811
5.633144	394.756698	7.674816
5.317213	389.744994	7.679821
5.801159	393.488772	7.684826
5.704049	395.530224	7.689830
5.665340	391.936077	7.694835
5.786391	399.312172	7.699840
5.417235	395.292619	7.704845
5.647307	397.108997	7.709850
5.683107	396.742221	7.714854
5.521909	388.403815	7.719859
5.225084	395.869233	7.724864
5.619779	400.647638	7.729869
5.612794	397.930341	7.734874
5.359199	400.994464	7.739878
5.591739	408.347957	7.744883
5.885541	407.971809	7.749888
5.789940	413.324555	7.754893
5.873029	413.282662	7.759898
5.703939	398.188478	7.764902
5.595390	392.611592	7.769907
5.481743	388.359299	7.774912
5.547416	399.030844	7.779917
5.676732	397.723458	7.784922
5.666701	404.739017	7.789926
6.071540	400.867768	7.794931
5.764650	397.030703	7.799936
5.508682	398.410143	7.804941
5.748830	387.040858	7.809946
5.588794	392.137070	7.814950
5.596744	391.740767	7.819955
5.841696	385.728430	7.824960
5.543217	395.378265	7.829965
5.771188	387.742866	7.834970
5.683855	391.605712	7.839974
5.323058	394.913537	7.844979
6.050696	388.979931	7.849984
5.675027	392.587805	7.854989
5.806959	392.435602	7.859994
5.543570	396.102439	7.864998
5.663381	394.322029	7.870003
5.828692	391.258882	7.875008
5.630462	396.484560	7.880013
5.990019	391.806592	7.885018
5.542776	395.098145	7.890022
5.506057	382.731380	7.895027
5.486149	389.197795	7.900032
5.860422	389.731076	7.905037
5.786628	387.794465	7.910042
5.508428	385.752775	7.915046
5.398697	388.524100	7.920051
5.548952	390.677724	7.925056
5.148825	390.879046	7.930061
5.863800	383.499666	7.935066
5.760075	391.564984	7.940070
5.948121	388.442424	7.945075
5.771713	391.153354	7.950080
5.847832	391.916177	7.955085
5.574682	391.819014	7.960090
5.648247	396.450492	7.965094
5.580863	391.678444	7.970099
5.681380	395.779354	7.975104
5.827404	394.107678	7.980109
5.919861	388.348716	7.985114
5.643435	392.895670	7.990118
5.511986	394.578175	7.995136
5.409302	393.474090	8.000154
5.225127	398.743639	8.005171
5.780053	380.330023	8.010189
5.377864	391.586586	8.015206
5.430023	393.421395	8.020224
5.528959	399.361725	8.025242
5.518946	409.884711	8.030259
5.967066	413.388272	8.035277
5.783155	419.052636	8.040294
5.945821	413.467151	8.045312
5.823964	399.933330	8.050330
5.586365	392.977628	8.055347
5.887481	384.696599	8.060365
5.840111	393.431411	8.065382
5.683704	395.234030	8.070400
5.718656	395.699157	8.075418
5.668151	393.867983	8.080435
5.676345	388.291552	8.085453
5.711890	393.919567	8.090470
5.497164	399.052454	8.095488
5.760364	399.560881	8.100506
5.772750	411.881990	8.105523
5.790671	410.232775	8.110541
5.727877	409.951548	8.115558
5.546182	418.480682	8.120576
6.052226	415.743628	8.125594
5.762277	410.251595	8.130611
5.701678	406.804104	8.135629
6.063204	410.690479	8.140646
5.824957	392.432599	8.145664
5.899025	395.530218	8.150682
5.315230	393.028552	8.155699
5.679685	405.239785	8.160717
5.685437	408.946706	8.165734
5.660200	410.309527	8.170752
6.007820	409.580644	8.175770
5.966997	415.733085	8.180787
5.837594	411.400597	8.185805
6.011303	407.588151	8.190822
5.927758	411.785019	8.195840
5.799041	408.965689	8.200858
5.912522	412.332355	8.205875
5.930899	409.034962	8.210893
6.120701	413.705032	8.215910
6.294680	411.877822	8.220928
5.804316	396.557135	8.225946
5.801231	399.134698	8.230963
5.602501	395.824443	8.235981
5.905875	405.979612	8.240998
5.787982	403.350799	8.246016
5.992922	402.153848	8.251034
5.905412	414.272226	8.256051
5.936524	413.536899	8.261069
5.887973	412.094937	8.266086
6.252649	415.836118	8.271104
6.173197	411.598501	8.276122
5.992465	411.968251	8.281139
6.067737	398.725189	8.286157
5.748383	394.073990	8.291174
5.611084	393.886984	8.296192
5.901042	408.733386	8.301210
5.896317	414.593650	8.306227
6.009296	418.402886	8.311245
5.956745	408.345114	8.316262
5.956340	413.084276	8.321280
6.454442	410.735516	8.326298
6.090889	417.373256	8.331315
6.037584	418.189981	8.336333
5.792364	417.196498	8.341350
6.039024	414.528378	8.346368
6.298223	408.177360	8.351386
5.740913	412.288322	8.356403
6.043558	409.668211	8.361421
6.411024	415.245011	8.366438
5.937270	410.970135	8.371456
5.989765	399.533267	8.376474
5.715455	416.930799	8.381491
5.990891	416.130607	8.386509
5.854878	413.515028	8.391526
5.771958	411.980930	8.396544
5.936932	410.554393	8.401562
5.714079	414.121624	8.406579
6.140717	416.031817	8.411597
6.076093	417.565519	8.416614
5.469468	420.138900	8.421632
5.926742	404.826233	8.426650
5.927500	420.089206	8.431667
6.162693	407.194628	8.436685
6.340506	409.290500	8.441702
5.849538	403.818568	8.446720
5.945414	410.567615	8.451738
6.114649	428.052921	8.456755
6.309078	436.081232	8.461773
6.384548	439.609501	8.466790
5.988593	425.463615	8.471808
6.110856	417.918037	8.476826
5.982698	421.430025	8.481843
6.077739	429.764139	8.486861
6.554533	430.664331	8.491878
6.060725	433.643017	8.496896
6.347586	431.007408	8.501914
6.138299	444.330531	8.506931
6.175355	435.545210	8.511949
6.231239	432.852186	8.516966
6.235711	434.509477	8.521984
6.005147	433.964320	8.527002
6.341793	444.120894	8.532019
6.129290	443.171594	8.537037
6.340719	438.526380	8.542054
6.241785	444.342811	8.547072
6.450824	439.807433	8.552090
6.271291	434.212075	8.557107
6.169044	426.702685	8.562125
6.106550	424.530014	8.567143
6.309121	452.130133	8.572160
6.499608	428.163048	8.577178
6.193791	429.482773	8.582195
6.200039	431.959197	8.587213
6.338628	431.744615	8.592231
6.376580	438.193840	8.597248
6.352002	436.803216	8.602266
6.122020	443.353893	8.607283
6.353440	442.079331	8.612301
6.487546	439.723721	8.617319
6.399004	431.869368	8.622336
6.354818	422.377088	8.627354
6.442007	421.869465	8.632371
6.000567	417.452042	8.637389
6.484169	425.426952	8.642407
6.340615	432.324309	8.647424
6.373667	422.905453	8.652442
6.479989	421.007365	8.657459
6.288889	416.983101	8.662477
6.486270	421.657036	8.667495
6.112156	428.342786	8.672512
6.198416	425.571707	8.677530
6.275546	438.868065	8.682547
6.613602	447.526291	8.687565
6.628569	439.983116	8.692583
6.371261	454.911719	8.697600
6.436162	433.132784	8.702618
6.630214	444.923677	8.707635
6.217469	439.467321	8.712653
6.376656	431.015689	8.717671
6.183244	432.889002	8.722688
5.997033	438.210472	8.727706
6.372439	439.733315	8.732723
6.435773	449.203708	8.737741
6.216773	449.484527	8.742759
6.140894	457.062370	8.747776
6.292741	443.459962	8.752794
6.493360	446.100251	8.757811
6.251920	443.686757	8.762829
6.555523	439.135721	8.767847
6.074155	438.581507	8.772864
6.341973	442.144457	8.777882
6.463562	450.138580	8.782899
6.254542	448.698385	8.787917
6.797726	458.292066	8.792935
6.956832	450.922248	8.797952
6.655790	443.569184	8.802970
6.323915	441.455094	8.807987
6.151070	447.265263	8.813005
6.578171	437.148714	8.818023
6.411282	451.802125	8.823040
6.869161	460.144868	8.828058
6.848808	449.640037	8.833075
6.624687	449.382965	8.838093
6.683090	445.905327	8.843111
6.394109	446.283161	8.848128
6.238657	439.299467	8.853146
6.527857	445.086861	8.858163
6.467220	461.159391	8.863181
6.952738	460.489555	8.868199
6.498218	462.967288	8.873216
6.467830	453.788626	8.878234
6.559263	447.646265	8.883251
6.916911	459.326621	8.888269
6.775555	456.829431	8.893287
6.510736	462.557598	8.898304
6.477549	460.171226	8.903322
6.620312	467.672715	8.908339
6.481651	479.598250	8.913357
6.928786	470.399163	8.918375
6.574397	469.690664	8.923392
6.736262	477.444094	8.928410
6.737316	473.752143	8.933427
6.627940	475.926287	8.938445
6.705765	471.418336	8.943463
6.660220	476.111058	8.948480
6.601563	473.549584	8.953498
7.014868	469.501005	8.958515
6.511474	470.569022	8.963533
6.844243	465.541331	8.968551
6.801352	475.625547	8.973568
6.642202	467.224641	8.978586
6.556486	471.201231	8.983603
6.453676	474.914531	8.988621
6.426077	467.572275	8.993639
6.292601	477.067204	8.998656
6.294019	467.557504	9.003674
6.565244	471.862165	9.008691
6.283130	476.833217	9.013709
6.843468	483.888232	9.018727
7.012692	500.593363	9.023744
6.702367	493.427430	9.028762
6.978628	492.016904	9.033779
6.666954	487.532110	9.038797
6.924642	482.355835	9.043815
6.919047	488.098563	9.048832
6.754537	472.343948	9.053850
6.848013	476.348737	9.058867
6.734140	487.410983	9.063885
7.052282	488.274857	9.068903
6.984661	483.500260	9.073920
6.759979	477.072264	9.078938
6.607683	471.846765	9.083955
6.912103	493.022483	9.088973
7.111778	505.547873	9.093991
6.986730	488.711781	9.099008
6.546877	480.771887	9.104026
6.910871	490.015956	9.109043
6.867779	502.797276	9.114061
7.238911	499.152692	9.119079
7.079355	492.483016	9.124096
6.679845	470.640783	9.129114
6.736090	481.439439	9.134131
7.027863	504.227782	9.139149
7.224328	503.112339	9.144167
6.939111	488.533520	9.149184
6.904657	480.728843	9.154202
6.913074	471.144758	9.159219
6.940947	486.643841	9.164237
6.923710	493.912406	9.169255
7.034940	500.053481	9.174272
7.173613	493.330878	9.179290
6.947862	482.620881	9.184307
6.864519	481.087436	9.189325
7.064169	484.078457	9.194343
6.791392	494.844014	9.199360
6.819162	501.244757	9.204378
6.869226	500.829297	9.209395
7.100925	506.951410	9.214413
7.102712	500.393194	9.219431
7.007257	506.044320	9.224448
6.741536	505.958887	9.229466
7.159270	508.920887	9.234483
6.954832	507.875569	9.239501
7.348904	508.241472	9.244519
6.959669	516.457019	9.249536
7.130174	511.120970	9.254554
6.980257	501.332392	9.259571
6.948234	508.511294	9.264589
7.327765	510.328716	9.269607
7.231139	505.468960	9.274624
6.884413	511.815194	9.279642
7.217350	506.375090	9.284659
6.980887	519.711439	9.289677
6.717751	510.764775	9.294695
6.985798	507.919487	9.299712
6.833490	507.817636	9.304730
6.964788	498.070480	9.309747
6.908040	504.899759	9.314765
7.267758	510.254467	9.319783
6.911669	506.058695	9.324800
7.102893	519.423232	9.329818
7.510052	525.486772	9.334835
7.363622	523.816732	9.339853
7.010933	504.579314	9.344871
7.147388	508.077423	9.349888
7.346586	520.848162	9.354906
7.359307	506.816602	9.359923
7.106795	509.051261	9.364941
6.977723	510.757050	9.369959
7.260103	514.433936	9.374976
7.298752	532.111247	9.379994
7.591913	527.910512	9.385011
7.095081	512.174077	9.390029
7.312612	504.027092	9.395047
7.237613	506.602606	9.400064
7.126931	515.860730	9.405082
7.632022	523.507352	9.410099
7.204563	511.304659	9.415117
7.269887	505.636448	9.420135
7.284337	516.424924	9.425152
7.296275	507.408501	9.430170
7.686877	503.461895	9.435187
7.204669	515.022524	9.440205
7.094898	506.149082	9.445223
7.445785	511.163741	9.450240
7.416837	515.757081	9.455258
7.295106	508.571524	9.460275
7.055716	513.261123	9.465293
7.442699	524.049133	9.470311
7.560082	529.960870	9.475328
7.372469	529.586144	9.480346
7.300145	516.303451	9.485363
7.642477	530.450596	9.490381
7.646097	522.391579	9.495399
7.583640	507.558941	9.500416
7.625127	511.205838	9.505434
7.667004	507.878747	9.510451
7.640484	511.185749	9.515469
7.504663	507.161953	9.520487
7.599431	503.626316	9.525504
7.447522	509.140542	9.530522
7.394083	503.937635	9.535539
7.342580	507.127128	9.540557
7.461140	505.513598	9.545575
7.313847	503.076631	9.550592
7.178565	505.735350	9.555610
7.360282	499.682538	9.560627
7.107251	503.024291	9.565645
7.213245	512.312867	9.570663
7.923578	525.190493	9.575680
7.469153	527.520002	9.580698
7.748989	520.376402	9.585715
7.404885	508.869112	9.590733
7.281214	510.366738	9.595751
7.827074	508.412390	9.600768
7.664499	509.187375	9.605786
7.612020	510.346660	9.610803
7.209550	502.399974	9.615821
7.456805	516.700636	9.620839
7.947209	521.075506	9.625856
7.516005	516.620929	9.630874
7.536234	496.478126	9.635891
7.424168	504.961134	9.640909
7.495027	519.464028	9.645927
7.824907	525.516744	9.650944
7.716485	529.117411	9.655962
7.594977	518.402725	9.660979
7.685512	522.717047	9.665997
7.723083	525.117438	9.671015
7.707226	521.999497	9.676032
7.613945	512.230469	9.681050
7.527043	504.921439	9.686067
7.546525	519.733213	9.691085
7.535919	517.753695	9.696103
7.471304	522.303929	9.701120
7.354364	532.746680	9.706138
7.654980	523.631465	9.711155
7.336169	528.204110	9.716173
7.492806	527.128329	9.721191
7.785343	520.364293	9.726208
7.978472	525.419252	9.731226
7.941361	520.524048	9.736243
7.604723	525.464383	9.741261
7.301803	530.846350	9.746279
7.591176	522.972085	9.751296
7.631086	525.019948	9.756314
7.824509	523.727460	9.761331
7.542813	531.731520	9.766349
7.677175	529.626427	9.771367
7.901668	526.567498	9.776384
7.632117	524.943828	9.781402
7.719022	523.271762	9.786419
7.708891	533.015968	9.791437
8.110178	547.978704	9.796455
7.872328	531.028971	9.801472
7.528568	540.058007	9.806490
7.738475	548.250731	9.811507
7.954286	556.908986	9.816525
8.026697	557.733245	9.821543
7.683048	550.801726	9.826560
7.594283	540.730180	9.831578
7.786092	551.456244	9.836595
8.002441	557.226415	9.841613
8.058873	561.520609	9.846631
8.310928	555.469513	9.851648
7.691606	550.945689	9.856666
7.992279	541.904859	9.861683
8.038075	543.010671	9.866701
7.797847	548.809202	9.871719
7.977656	541.340644	9.876736
8.117121	554.637802	9.881754
8.319576	541.575514	9.886771
7.887634	525.632860	9.891789
7.625908	525.874696	9.896807
7.846187	528.561740	9.901824
7.684498	556.232991	9.906842
7.824186	556.268799	9.911859
8.151271	558.581297	9.916877
7.983134	562.359959	9.921895
7.993519	549.475325	9.926912
7.918857	557.441572	9.931930
7.820176	556.492707	9.936947
8.092132	565.915241	9.941965
7.756390	563.115598	9.946983
8.111649	557.997349	9.952000
8.024319	561.228020	9.957018
7.905068	558.739947	9.962035
7.913813	553.445826	9.967053
8.030452	556.974982	9.972071
8.000562	551.668166	9.977088
8.163622	557.612702	9.982106
8.020926	552.199968	9.987123
8.347996	551.025299	9.992141
7.952408	561.364810	9.997159
8.065938	564.022690	10.002176
8.049962	556.777870	10.007194
7.981947	564.085583	10.012211
8.082946	556.692858	10.017229
8.082656	569.395103	10.022247
8.072227	557.575256	10.027264
8.044734	551.028363	10.032282
7.870618	554.453115	10.037299
8.204728	561.757228	10.042317
8.159909	581.621501	10.047335
8.414469	562.521432	10.052352
8.216807	556.951077	10.057370
8.482134	564.931497	10.062387
8.276608	548.142720	10.067405
8.258630	546.004981	10.072423
8.355066	551.589114	10.077440
8.383023	554.357613	10.082458
8.271628	560.069071	10.087475
8.757940	547.832747	10.092493
8.369857	556.691388	10.097511
8.302138	552.702953	10.102528
8.360764	549.367372	10.107546
8.195882	551.563315	10.112563
8.518451	552.422523	10.117581
8.361075	553.935970	10.122599
8.317718	545.740241	10.127616
8.173850	555.822333	10.132634
8.245905	543.943369	10.137651
8.418213	555.181488	10.142669
8.112533	550.864372	10.147687
8.413686	542.851542	10.152704
8.158843	554.839875	10.157722
8.372041	553.259287	10.162739
8.407619	550.862695	10.167757
8.141307	562.359068	10.172775
8.515927	550.561485	10.177792
8.390950	550.526756	10.182810
8.376362	549.954099	10.187827
8.654466	550.860431	10.192845
8.433123	551.495159	10.197863
8.417977	543.153037	10.202880
8.554392	550.063137	10.207898
8.327874	555.826923	10.212915
8.495755	552.234289	10.217933
8.544607	556.687404	10.222951
8.775069	545.861664	10.227968
8.651788	546.288237	10.232986
8.641996	546.744638	10.238003
8.720077	547.912028	10.243021
8.480635	541.669509	10.248039
8.703655	545.788486	10.253056
8.548118	544.195734	10.258074
8.630031	549.608465	10.263091
8.821161	550.036515	10.268109
8.208512	557.574953	10.273127
8.380521	548.526292	10.278144
8.430386	550.964806	10.283162
8.505849	553.069182	10.288179
8.695778	552.763819	10.293197
8.303113	557.556956	10.298215
8.268083	551.422307	10.303232
8.309265	556.169586	10.308250
8.185607	564.505736	10.313267
8.570232	561.480516	10.318285
8.416453	557.702972	10.323303
8.533974	553.196691	10.328320
8.521509	559.935792	10.333338
8.649620	570.972988	10.338355
8.658519	570.550760	10.343373
8.392934	570.894016	10.348391
8.598708	579.604927	10.353408
9.079449	582.194130	10.358426
8.581529	584.531637	10.363443
8.839303	579.069311	10.368461
8.685933	593.337571	10.373479
8.730390	577.806497	10.378496
8.710485	575.876736	10.383514
8.803601	571.972286	10.388531
8.800198	559.079692	10.393549
8.461823	563.457175	10.398567
8.591219	576.216882	10.403584
8.833870	586.647956	10.408602
8.581566	587.608264	10.413619
8.810825	591.209128	10.418637
8.632542	590.097075	10.423655
9.014750	582.121784	10.428672
8.921364	581.284632	10.433690
8.975341	591.533777	10.438707
8.673530	581.192779	10.443725
8.800614	588.043815	10.448743
8.971185	588.830957	10.453760
9.133880	580.332997	10.458778
8.678673	571.240358	10.463795
8.811533	571.253479	10.468813
8.736514	582.313493	10.473831
9.072392	578.324358	10.478848
9.026042	575.302591	10.483866
8.691541	571.257941	10.488883
8.981929	567.112966	10.493901
8.876588	572.585451	10.498919
8.772758	576.086752	10.503936
9.081223	581.724758	10.508954
8.921123	581.620653	10.513971
8.938825	577.750736	10.518989
9.076008	582.062861	10.524007
8.808151	583.454457	10.529024
8.871630	571.488709	10.534042
8.767967	587.820054	10.539059
9.282476	574.982030	10.544077
9.053914	590.861257	10.549095
9.078345	578.870671	10.554112
9.129574	573.978537	10.559130
8.739551	574.448298	10.564147
8.908981	570.901856	10.569165
9.003140	582.648179	10.574183
8.939422	589.029663	10.579200
9.072804	579.477176	10.584218
8.630616	588.629028	10.589235
8.798446	590.219328	10.594253
8.551283	592.483819	10.599271
8.765331	587.861748	10.604288
8.953023	587.276851	10.609306
8.684765	583.533020	10.614323
8.702504	592.051270	10.619341
9.124882	604.895154	10.624359
9.328171	620.563737	10.629376
9.471329	610.718686	10.634394
9.030484	606.984924	10.639411
9.146561	608.335780	10.644429
9.308679	608.849930	10.649447
9.465341	591.944836	10.654464
9.040553	591.163347	10.659482
8.667619	591.107083	10.664499
8.901940	598.843459	10.669517
9.112467	620.138042	10.674535
9.298534	619.623882	10.679552
9.160684	612.129549	10.684570
9.211006	620.897128	10.689587
9.221097	622.816288	10.694605
9.305955	614.513470	10.699623
9.466231	622.605011	10.704640
9.308614	618.259028	10.709658
9.318298	621.273856	10.714675
9.467842	619.300874	10.719693
9.392627	623.637553	10.724711
9.384283	620.943518	10.729728
9.357138	614.827222	10.734746
9.033782	620.696235	10.739763
9.343249	623.383487	10.744781
9.654457	614.179069	10.749799
9.307522	616.846281	10.754816
9.439871	605.030706	10.759834
9.374739	604.938433	10.764851
9.405969	599.877370	10.769869
9.236629	596.062828	10.774887
9.249788	600.033708	10.779904
9.692366	606.524655	10.784922
9.237971	597.634019	10.789939
9.430491	602.498369	10.794957
9.282771	602.940604	10.799975
9.302753	615.079526	10.804992
9.760356	608.855799	10.810010
9.289790	623.828538	10.815027
9.544390	616.476685	10.820045
9.646690	614.772141	10.825063
9.515214	598.896579	10.830080
9.597997	582.890286	10.835098
9.440184	591.923794	10.840115
9.497412	582.887821	10.845133
9.444064	580.257147	10.850151
9.250854	583.894503	10.855168
9.728260	596.484403	10.860186
9.399436	611.435628	10.865203
9.528268	615.957795	10.870221
9.815029	613.003491	10.875239
9.529134	605.826964	10.880256
9.740763	592.427899	10.885274
9.028686	598.569132	10.890291
9.159283	607.116337	10.895309
9.296763	606.670849	10.900327
9.244238	621.779468	10.905344
9.571271	615.240767	10.910362
9.376639	613.212974	10.915379
9.715759	619.630120	10.920397
9.912382	616.205733	10.925415
9.733531	625.045906	10.930432
9.740864	616.785450	10.935450
9.419567	622.247061	10.940467
9.242058	616.772554	10.945485
9.209340	614.631734	10.950503
9.446141	623.240097	10.955520
10.219147	623.494440	10.960538
9.896081	623.658644	10.965555
10.022424	616.796110	10.970573
9.973335	607.552151	10.975591
10.134817	620.197926	10.980608
10.296903	607.839270	10.985626
10.010730	613.527331	10.990643
9.765029	610.382475	10.995661
9.825765	611.188593	11.000679
9.970333	615.799880	11.005696
9.761350	606.000939	11.010714
9.849729	612.785172	11.015731
9.998381	608.814434	11.020749
10.021836	610.107797	11.025767
9.553123	598.341761	11.030784
9.834253	612.055837	11.035802
9.736781	620.759706	11.040819
9.805718	616.319125	11.045837
10.038739	616.137720	11.050855
9.497863	620.856605	11.055872
9.767877	606.262895	11.060890
9.518050	612.722053	11.065907
9.648946	615.551464	11.070925
9.912758	612.270273	11.075943
9.567740	615.861912	11.080960
9.877494	610.616151	11.085978
9.651853	617.760632	11.090995
9.641416	616.162939	11.096013
9.971558	612.732191	11.101031
9.630700	616.561709	11.106048
9.841773	633.360834	11.111066
9.879774	644.044522	11.116083
10.222834	641.781241	11.121101
10.352407	635.928338	11.126119
9.741372	635.268627	11.131136
9.905288	630.188338	11.136154
9.927400	630.485530	11.141171
10.039474	643.646168	11.146189
10.184875	640.772350	11.151207
9.843407	641.697035	11.156224
10.086705	641.578884	11.161242
9.901710	645.051125	11.166259
9.677181	640.778416	11.171277
9.912466	637.804681	11.176295
10.083933	647.287209	11.181312
9.915887	642.627610	11.186330
9.974998	640.631021	11.191347
9.969012	641.224186	11.196365
10.415391	649.615588	11.201383
10.365661	640.225661	11.206400
10.314397	648.158949	11.211418
10.328652	652.862293	11.216435
10.239660	652.706652	11.221453
10.435451	647.989560	11.226471
10.029541	648.274957	11.231488
10.375614	640.012330	11.236506
10.159980	639.332418	11.241523
9.917452	644.144024	11.246541
10.225633	643.675387	11.251559
10.343395	656.354414	11.256576
10.151139	645.302360	11.261594
10.115612	645.822470	11.266611
10.425183	649.151402	11.271629
10.451344	646.983901	11.276647
10.520385	646.375739	11.281664
10.483636	641.886908	11.286682
10.109773	647.700518	11.291699
10.148296	651.053075	11.296717
10.138723	637.296923	11.301735
10.129794	656.388664	11.306752
10.299654	646.768682	11.311770
9.966617	645.766105	11.316787
10.024479	662.094205	11.321805
10.335194	662.254243	11.326823
10.242140	679.739961	11.331840
10.450254	679.803217	11.336858
10.614157	682.879522	11.341875
10.215923	683.021924	11.346893
10.766359	681.327413	11.351911
10.351196	685.420812	11.356928
10.572171	682.591162	11.361946
10.808543	676.217045	11.366963
10.625782	667.529012	11.371981
10.603037	650.436645	11.376999
10.337762	656.527929	11.382016
10.396425	643.724193	11.387034
10.277626	654.109857	11.392051
10.637929	670.234350	11.397069
11.132746	659.799966	11.402087
10.572652	655.502903	11.407104
10.612223	648.651574	11.412122
10.337241	642.806213	11.417139
10.569002	637.354866	11.422157
10.997580	636.504897	11.427175
10.631531	638.933560	11.432192
10.489920	632.829125	11.437210
10.527201	640.616258	11.442227
10.294895	645.414362	11.447245
10.359747	643.494376	11.452263
10.499942	650.901897	11.457280
10.840509	664.383750	11.462298
10.963726	661.300622	11.467315
10.506943	658.096621	11.472333
10.622728	662.444987	11.477351
10.797780	666.497732	11.482368
10.881164	663.460173	11.487386
10.887429	650.596609	11.492403
10.179309	653.288598	11.497421
10.842562	659.344232	11.502439
11.064069	672.619837	11.507456
10.768584	653.327487	11.512474
10.940683	648.452911	11.517491
10.763696	645.215572	11.522509
10.633202	638.062114	11.527527
10.642477	644.407519	11.532544
10.850554	660.962697	11.537562
11.220411	659.421704	11.542579
10.650247	655.383774	11.547597
10.723190	638.971202	11.552615
10.897171	650.868129	11.557632
10.667681	654.430805	11.562650
11.025635	655.449110	11.567667
11.041287	671.597607	11.572685
10.885815	651.236074	11.577703
10.780681	653.839632	11.582720
10.710548	671.055813	11.587738
10.904513	671.978841	11.592755
10.976903	677.622904	11.597773
11.270940	674.975634	11.602791
11.092688	664.720019	11.607808
10.690335	657.699752	11.612826
11.148603	658.450674	11.617843
10.828748	653.267819	11.622861
10.890209	663.027218	11.627879
10.641036	675.511131	11.632896
10.927096	671.070407	11.637914
11.255646	663.832262	11.642931
10.818043	684.374860	11.647949
11.195477	672.311577	11.652967
10.931035	674.267148	11.657984
11.119862	675.158352	11.663002
11.100869	673.920317	11.668019
10.714878	672.900129	11.673037
11.370244	668.572258	11.678055
11.356614	677.555565	11.683072
11.401612	675.086926	11.688090
11.364228	670.763142	11.693107
11.387147	678.931784	11.698125
11.159929	654.481188	11.703143
11.102858	662.436309	11.708160
10.834360	668.144296	11.713178
11.014619	669.572319	11.718195
11.232122	678.386259	11.723213
11.083570	665.408562	11.728231
11.076701	678.825526	11.733248
10.584318	676.593501	11.738266
11.207700	672.225651	11.743283
11.008817	677.116256	11.748301
10.954665	675.862390	11.753319
10.999701	683.385678	11.758336
10.769003	668.676408	11.763354
11.360523	676.528860	11.768371
11.152642	693.773781	11.773389
11.518241	691.187882	11.778407
11.575851	705.984269	11.783424
11.229638	689.844584	11.788442
11.359660	675.174389	11.793459
11.068789	686.062948	11.798477
11.311454	692.011872	11.803495
11.340389	697.287176	11.808512
11.425647	707.525706	11.813530
11.426740	697.392725	11.818547
11.457479	703.126367	11.823565
11.733674	704.858568	11.828583
11.826218	701.983650	11.833600
11.334932	685.323140	11.838618
11.255585	672.626087	11.843635
11.299378	680.757417	11.848653
11.087967	693.141790	11.853671
11.607572	699.077534	11.858688
11.494496	707.331305	11.863706
11.653474	687.717610	11.868723
11.317589	700.439905	11.873741
11.276547	700.062556	11.878759
11.714015	694.201164	11.883776
11.601573	707.875778	11.888794
12.117386	698.340596	11.893811
11.698621	701.664562	11.898829
11.664532	674.639186	11.903847
11.092406	679.156583	11.908864
11.526988	688.195984	11.913882
11.653018	686.276098	11.918899
11.587019	702.493262	11.923917
11.682761	702.749524	11.928935
11.951192	694.707982	11.933952
11.593605	702.182207	11.938970
11.708935	702.752531	11.943987
11.480306	701.338982	11.949005
11.146201	702.430946	11.954023
11.766247	707.268627	11.959040
11.203664	706.739464	11.964058
11.487635	698.443392	11.969075
11.549784	705.725682	11.974093
11.707778	704.991771	11.979111
11.635013	706.413273	11.984128
11.351875	695.693143	11.989146
11.629427	702.069340	11.994163
11.872023	722.323381	11.999181
11.824740	721.670309	12.004199
11.872214	716.725014	12.009216
11.713648	721.153471	12.014234
12.378696	715.723257	12.019251
12.142020	714.693696	12.024269
11.871538	705.537910	12.029287
11.894863	695.860672	12.034304
11.714473	701.606440	12.039322
12.061920	690.148861	12.044339
11.790559	690.620628	12.049357
11.873525	690.452652	12.054375
11.807094	691.690044	12.059392
11.587768	691.016646	12.064410
12.071542	710.242602	12.069427
12.156448	712.239537	12.074445
11.594102	701.617209	12.079463
12.466433	709.659386	12.084480
11.712972	713.713935	12.089498
11.779159	702.752501	12.094515
12.111384	714.837041	12.099533
12.035653	727.293063	12.104551
12.349549	716.895686	12.109568
12.096413	717.193185	12.114586
12.055429	699.657353	12.119603
11.708705	705.188947	12.124621
12.025896	720.749799	12.129639
12.652962	719.103616	12.134656
11.868226	712.469458	12.139674
11.978191	702.982975	12.144691
12.135205	715.859871	12.149709
11.804831	725.815288	12.154727
12.011426	719.090593	12.159744
12.314556	723.567788	12.164762
12.521312	719.631099	12.169779
12.361647	728.754752	12.174797
12.219237	723.380294	12.179815
12.604616	706.143911	12.184832
12.229972	703.561696	12.189850
12.035881	688.903821	12.194867
12.036220	702.249144	12.199885
12.125947	708.908006	12.204903
12.549250	719.565343	12.209920
12.219984	710.609042	12.214938
11.940996	712.904016	12.219955
12.463488	720.532501	12.224973
12.052505	723.073337	12.229991
12.459841	716.122893	12.235008
12.182408	729.782723	12.240026
12.399769	723.976271	12.245043
12.044807	730.661930	12.250061
12.032975	728.464490	12.255079
12.399222	716.762847	12.260096
11.951219	731.520942	12.265114
11.847362	723.891799	12.270131
12.076571	720.714735	12.275149
12.235598	738.520175	12.280167
12.788025	743.230095	12.285184
12.185350	746.964031	12.290202
12.522369	747.638190	12.295219
12.444473	753.004427	12.300237
12.550684	751.279537	12.305255
12.542065	749.639012	12.310272
12.285302	756.389913	12.315290
12.728162	748.584799	12.320307
12.777860	749.204967	12.325325
12.633288	754.285411	12.330343
12.658544	753.329790	12.335360
12.309475	742.151279	12.340378
12.466871	750.302809	12.345395
12.436651	752.354244	12.350413
12.216596	758.369185	12.355431
12.610828	749.097793	12.360448
12.605755	753.729964	12.365466
12.655305	755.053662	12.370483
12.714322	755.594338	12.375501
12.568408	756.645301	12.380519
12.831617	753.964542	12.385536
12.727278	750.416348	12.390554
12.733701	755.021420	12.395571
12.670478	750.919598	12.400589
12.377682	751.798436	12.405607
13.133027	750.754203	12.410624
12.716214	754.308158	12.415642
12.893196	752.089291	12.420659
13.114308	750.811884	12.425677
12.709202	755.613834	12.430695
13.055920	747.815980	12.435712
12.969188	751.413303	12.440730
12.892078	747.611403	12.445747
13.121206	746.632653	12.450765
13.024703	742.698145	12.455783
12.872481	730.970539	12.460800
12.909870	737.956173	12.465818
13.011975	746.441248	12.470835
12.812291	740.257415	12.475853
12.730447	739.320317	12.480871
12.925407	738.100782	12.485888
12.746631	749.216479	12.490906
12.849917	746.818488	12.495923
13.151423	747.696549	12.500941
12.645671	744.174672	12.505959
12.821741	751.154276	12.510976
13.012625	753.078552	12.515994
12.946963	749.639303	12.521011
12.923647	748.888565	12.526029
12.673720	754.215182	12.531047
13.082653	730.648443	12.536064
13.239892	746.856245	12.541082
12.870246	749.621723	12.546099
12.850187	750.157778	12.551117
12.828282	749.981185	12.556135
12.648331	749.317010	12.561152
12.871117	754.118132	12.566170
12.987232	771.370115	12.571187
13.620164	767.064041	12.576205
13.143322	777.490572	12.581223
13.004722	767.938915	12.586240
13.334146	778.049663	12.591258
12.931031	772.655369	12.596275
13.220837	770.839448	12.601293
13.021172	780.739794	12.606311
13.404109	769.278642	12.611328
13.103481	774.524296	12.616346
12.841070	778.664075	12.621363
13.189448	768.831790	12.626381
13.106849	784.354188	12.631399
13.187430	783.332714	12.636416
13.451375	773.156946	12.641434
13.580040	778.254748	12.646451
13.572537	778.752112	12.651469
13.500394	776.357182	12.656487
13.717698	776.224832	12.661504
13.358293	779.266952	12.666522
13.617675	774.410952	12.671539
13.509535	779.491671	12.676557
13.462600	776.715027	12.681575
13.381214	784.815175	12.686592
13.866530	773.791768	12.691610
13.522251	766.838996	12.696627
13.530930	755.422111	12.701645
13.488676	747.308766	12.706663
13.260113	747.864780	12.711680
13.747715	763.849402	12.716698
13.440120	759.706944	12.721715
13.537129	753.259027	12.726733
13.355173	771.746525	12.731751
13.439133	779.803937	12.736768
13.671293	770.084197	12.741786
13.175587	774.791318	12.746803
13.786259	772.464022	12.751821
14.072082	773.176187	12.756839
14.131115	768.906091	12.761856
13.691328	754.617562	12.766874
13.341198	744.245481	12.771891
13.808032	737.611929	12.776909
13.372691	738.604523	12.781927
13.673831	753.438972	12.786944
13.843235	772.434794	12.791962
13.583181	771.405951	12.796979
13.760743	762.086575	12.801997
13.745574	767.498726	12.807015
13.852989	764.909114	12.812032
13.870753	756.000041	12.817050
13.833749	759.714322	12.822067
13.908396	751.410759	12.827085
13.389215	756.426470	12.832103
13.865829	755.874824	12.837120
13.723629	759.754154	12.842138
13.645678	773.338080	12.847155
13.657211	763.021447	12.852173
13.674387	769.522673	12.857191
13.747313	766.379746	12.862208
13.718739	768.330522	12.867226
13.552610	778.152088	12.872243
13.817837	769.225651	12.877261
14.017115	769.122662	12.882279
13.599361	764.048889	12.887296
13.826786	757.514811	12.892314
13.827424	765.141942	12.897331
14.102558	775.189242	12.902349
13.960100	778.500932	12.907367
13.730675	772.066119	12.912384
14.132406	789.568844	12.917402
13.915175	802.309367	12.922419
14.360726	804.312734	12.927437
14.317127	792.812358	12.932455
14.264084	780.942707	12.937472
14.203155	772.246645	12.942490
13.888367	776.927351	12.947507
14.147800	760.827453	12.952525
13.949607	769.770906	12.957543
14.069945	776.638103	12.962560
14.090459	791.322611	12.967578
14.057794	798.834019	12.972595
14.539547	801.985663	12.977613
13.917377	806.211397	12.982631
14.123088	798.435292	12.987648
14.303273	789.291048	12.992666
13.895401	798.279867	12.997683
13.983679	795.169429	13.002701
14.355183	800.715979	13.007719
14.189882	797.636507	13.012736
14.459516	794.638158	13.017754
14.257427	799.433668	13.022771
14.249227	797.955658	13.027789
14.377858	792.575663	13.032807
14.417525	795.154086	13.037824
14.353685	792.303865	13.042842
14.126031	799.618833	13.047859
14.665899	793.851466	13.052877
14.309126	797.529734	13.057895
14.471304	801.949194	13.062912
14.328885	791.321439	13.067930
14.179569	795.290534	13.072947
14.670082	789.159313	13.077965
14.572919	796.754625	13.082983
14.304470	791.850597	13.088000
14.937617	798.075043	13.093018
14.565341	796.523862	13.098035
14.483441	785.458552	13.103053
14.501389	793.821769	13.108071
14.437545	797.040922	13.113088
14.717985	789.955167	13.118106
14.479955	801.024023	13.123123
14.814178	789.030400	13.128141
14.669853	791.342061	13.133159
14.628358	798.988389	13.138176
14.830429	794.815067	13.143194
15.012900	804.065960	13.148211
15.016907	784.890774	13.153229
14.705994	791.516412	13.158247
14.471625	797.516417	13.163264
14.733960	786.911795	13.168282
14.779950	795.862858	13.173299
14.430265	791.195499	13.178317
14.443118	792.439848	13.183335
14.526611	786.368939	13.188352
15.064327	789.767993	13.193370
14.769008	795.740297	13.198387
15.116339	794.041614	13.203405
14.977620	791.527398	13.208423
14.716345	790.749135	13.213440
14.881139	787.376042	13.218458
14.541049	792.260933	13.223475
14.639216	793.472258	13.228493
14.930144	793.790685	13.233511
14.714783	792.209191	13.238528
15.258114	787.101456	13.243546
14.880689	798.616599	13.248563
15.155899	785.895780	13.253581
15.244820	790.906077	13.258599
14.798415	789.191985	13.263616
14.930987	792.041229	13.268634
14.614665	795.215186	13.273651
14.939104	794.377730	13.278669
15.115067	803.597025	13.283687
15.089651	818.152556	13.288704
15.422282	810.327083	13.293722
14.824980	800.482089	13.298739
14.848845	796.687864	13.303757
14.822524	821.708765	13.308775
14.738479	830.646343	13.313792
15.670441	826.062795	13.318810
15.580692	828.484316	13.323827
15.442438	830.211148	13.328845
15.244775	813.461329	13.333863
15.186147	800.800108	13.338880
15.184732	801.007503	13.343898
15.049965	815.639798	13.348915
15.401879	822.632047	13.353933
15.194734	821.684985	13.358951
15.369423	829.644332	13.363968
15.511890	828.032715	13.368986
15.494281	825.174833	13.374003
15.018868	805.987673	13.379021
15.487213	806.484586	13.384039
15.267522	820.556961	13.389056
15.422190	817.530403	13.394074
15.287856	821.294672	13.399091
15.213367	811.444984	13.404109
15.442686	823.424608	13.409127
15.082233	834.271252	13.414144
15.227816	820.119972	13.419162
15.392491	823.628047	13.424179
15.205960	824.155057	13.429197
15.073843	821.848394	13.434215
15.342777	825.975788	13.439232
15.562011	817.496681	13.444250
15.234318	821.625629	13.449267
15.170600	833.906134	13.454285
15.009997	827.695717	13.459303
14.845206	841.071257	13.464320
15.410074	836.038676	13.469338
15.645487	849.155051	13.474355
15.709157	846.476216	13.479373
15.814575	843.723150	13.484391
15.859583	846.025513	13.489408
15.917212	838.300286	13.494426
15.636217	838.841758	13.499443
15.531319	841.083514	13.504461
15.750804	841.956660	13.509479
15.528552	844.912304	13.514496
16.068297	838.541821	13.519514
15.825460	844.287747	13.524531
15.927297	846.959028	13.529549
16.115093	838.570939	13.534567
15.877325	842.539733	13.539584
16.096557	837.415179	13.544602
15.838657	831.201974	13.549619
15.695946	838.086773	13.554637
15.812209	843.631117	13.559655
15.881336	850.552494	13.564672
15.741308	838.533431	13.569690
15.982166	842.761931	13.574707
16.033203	844.545604	13.579725
15.799722	844.412312	13.584743
15.115571	847.772379	13.589760
15.781150	842.992790	13.594778
15.631671	844.017579	13.599795
15.665096	845.681734	13.604813
16.098356	849.562249	13.609831
16.211167	873.419698	13.614848
15.969035	868.205002	13.619866
16.121669	863.474127	13.624883
16.057379	866.889029	13.629901
16.303237	863.383998	13.634919
16.233622	863.539697	13.639936
16.288311	847.983824	13.644954
16.005069	843.632203	13.649971
16.073840	845.988109	13.654989
16.144647	845.897733	13.660007
16.279694	855.369097	13.665024
16.444696	856.786673	13.670042
16.534571	846.792430	13.675059
16.246726	837.129229	13.680077
16.326285	831.275479	13.685095
16.303949	835.421580	13.690112
16.268709	844.279828	13.695130
16.306455	833.654098	13.700147
15.926638	837.143287	13.705165
16.119816	842.778040	13.710183
16.221608	860.675377	13.715200
16.453504	866.676937	13.720218
16.374304	868.432575	13.725235
16.482163	866.925893	13.730253
16.811644	867.228883	13.735271
16.730065	848.656345	13.740288
16.787411	840.561496	13.745306
16.327225	827.813997	13.750323
16.519459	838.708096	13.755341
16.783856	825.141438	13.760359
16.422805	844.390138	13.765376
16.406599	834.301663	13.770394
16.516177	836.732302	13.775411
16.497392	829.753161	13.780429
16.512385	829.351176	13.785447
16.086726	830.342960	13.790464
16.250945	845.870610	13.795482
16.908714	851.974078	13.800499
16.542627	866.087270	13.805517
16.625810	864.158316	13.810535
16.563990	868.935738	13.815552
16.628388	864.196639	13.820570
16.836352	874.871239	13.825587
16.749749	866.622268	13.830605
17.085263	868.793070	13.835623
16.648686	867.019864	13.840640
16.932404	859.440250	13.845658
16.993955	866.991600	13.850675
16.781149	858.823764	13.855693
16.790593	841.780577	13.860711
16.766000	845.516445	13.865728
16.939998	851.333895	13.870746
16.753651	853.813145	13.875763
16.719376	865.357732	13.880781
17.125643	859.245552	13.885799
17.108480	866.881586	13.890816
16.953643	852.408780	13.895834
16.909120	842.467107	13.900851
16.926417	841.605708	13.905869
17.112428	842.304483	13.910887
16.635650	847.195097	13.915904
16.994026	869.131258	13.920922
17.358463	875.504557	13.925939
17.003502	872.121059	13.930957
17.044304	861.811324	13.935975
16.995645	865.314972	13.940992
17.058990	865.841156	13.946010
16.841199	863.791182	13.951027
16.911994	870.259557	13.956045
16.889308	869.990183	13.961063
17.137277	870.466505	13.966080
16.980306	871.513402	13.971098
16.896336	867.732291	13.976115
16.843968	872.866794	13.981133
16.822342	864.927128	13.986151
16.934194	881.303210	13.991168
16.799442	893.837640	13.996186
17.186992	901.405494	14.001203
17.246446	902.563005	14.006221
17.443457	895.051666	14.011239
17.303633	903.781997	14.016256
17.457130	907.477367	14.021274
17.397230	901.209695	14.026291
17.441494	900.970964	14.031309
17.250204	897.694998	14.036327
17.146415	909.583397	14.041344
17.211350	902.275807	14.046362
17.704958	890.350985	14.051379
17.581844	893.706739	14.056397
17.512226	899.129921	14.061415
17.428658	900.482760	14.066432
17.090394	894.615500	14.071450
17.297718	894.613536	14.076467
17.127224	899.397546	14.081485
17.170647	897.242505	14.086503
17.139161	903.443591	14.091520
17.352109	922.840637	14.096538
17.626763	929.155600	14.101555
17.414280	936.292537	14.106573
17.660684	934.197183	14.111591
17.575183	931.617047	14.116608
17.452621	930.466217	14.121626
17.929247	926.404477	14.126643
17.486497	933.660641	14.131661
17.856112	922.616526	14.136679
17.884532	925.163764	14.141696
17.797133	924.822825	14.146714
18.164885	926.174552	14.151731
17.951317	925.222248	14.156749
17.936784	924.245254	14.161767
18.283299	930.492809	14.166784
18.058137	927.322440	14.171802
18.211368	920.571850	14.176819
17.592045	914.241695	14.181837
18.019966	912.497372	14.186855
17.740662	914.459765	14.191872
17.569515	922.625239	14.196890
17.907242	922.563101	14.201907
17.703344	934.081892	14.206925
17.858691	927.476218	14.211943
17.943979	929.536501	14.216960
17.944317	930.917967	14.221978
17.938657	921.602459	14.226995
17.657757	931.886021	14.232013
17.940467	924.560469	14.237031
17.934235	923.449823	14.242048
17.440661	929.215646	14.247066
18.126077	939.704936	14.252083
17.921638	957.469243	14.257101
18.011546	954.444720	14.262119
18.124306	955.726080	14.267136
17.976880	961.135791	14.272154
18.660340	962.466739	14.277171
18.038259	955.843335	14.282189
18.173919	958.325578	14.287207
18.379770	949.548234	14.292224
17.982252	953.364776	14.297242
18.631536	953.507731	14.302259
18.526927	960.894129	14.307277
18.439867	954.771872	14.312295
18.308853	960.044224	14.317312
18.464506	951.061814	14.322330
18.500999	945.206886	14.327347
18.232145	953.351942	14.332365
18.331788	952.171402	14.337383
18.640169	941.051984	14.342400
18.577030	946.231600	14.347418
18.392747	952.600521	14.352435
18.467844	953.668835	14.357453
18.843494	944.651968	14.362471
18.640039	951.510263	14.367488
18.312395	953.160993	14.372506
18.639041	946.597022	14.377523
18.408175	950.313529	14.382541
18.474016	951.046776	14.387559
18.293433	951.011411	14.392576
18.292790	960.899387	14.397594
18.790628	949.271839	14.402611
18.442995	953.766707	14.407629
18.335805	949.107174	14.412647
18.550007	944.430644	14.417664
18.464904	960.552033	14.422682
19.028868	969.830796	14.427699
18.932687	974.178130	14.432717
18.675628	952.485045	14.437735
18.898102	957.611465	14.442752
18.751994	958.151864	14.447770
19.402635	965.497059	14.452787
18.895162	959.766843	14.457805
18.872018	946.149666	14.462823
18.909230	940.482408	14.467840
18.778589	945.986573	14.472858
18.883109	942.841135	14.477875
18.923907	949.929052	14.482893
19.082189	946.057023	14.487911
18.997037	945.820825	14.492928
18.561179	946.459594	14.497946
18.984581	953.480615	14.502963
18.636305	969.160571	14.507981
19.199445	981.124410	14.512999
19.303055	976.805539	14.518016
19.236824	971.194373	14.523034
19.549920	976.545942	14.528051
19.517426	958.109628	14.533069
19.342820	943.112866	14.538087
19.369159	941.155915	14.543104
19.114025	944.945728	14.548122
19.330940	936.159080	14.553139
18.828177	936.535317	14.558157
18.731975	938.362279	14.563175
19.331788	950.443244	14.568192
19.269205	961.003655	14.573210
19.478648	969.919485	14.578227
19.337341	970.364212	14.583245
19.357909	967.578719	14.588263
19.685060	961.687465	14.593280
19.163396	959.748029	14.598298
19.308768	956.771012	14.603315
19.678274	967.277201	14.608333
19.269301	956.375371	14.613351
19.375261	960.143583	14.618368
19.450189	977.583318	14.623386
19.539546	981.138151	14.628403
19.450297	976.259113	14.633421
19.401570	977.790828	14.638439
19.306328	975.130805	14.643456
19.678646	979.622209	14.648474
19.581294	978.562866	14.653491
19.729007	978.101894	14.658509
19.182663	980.370707	14.663527
19.577370	972.157331	14.668544
19.153333	970.998152	14.673562
19.517432	965.764138	14.678579
19.676629	978.217680	14.683597
19.511715	978.371052	14.688615
19.589708	966.598060	14.693632
19.551908	983.642705	14.698650
19.770510	987.775721	14.703667
20.006883	1000.085798	14.708685
19.657284	1000.536670	14.713703
19.752270	994.765341	14.718720
19.727524	1002.880631	14.723738
20.060800	1009.249698	14.728755
19.962210	1008.151582	14.733773
19.660272	1012.333006	14.738791
20.146228	1005.950890	14.743808
19.999730	1013.301337	14.748826
19.728240	1006.771032	14.753843
20.340474	1004.983188	14.758861
19.797544	1004.949558	14.763879
19.780530	1001.190004	14.768896
19.856094	1002.828301	14.773914
19.997746	1001.977402	14.778931
20.273662	1001.121594	14.783949
19.907192	1005.914072	14.788967
20.216520	1003.574833	14.793984
20.290879	1000.817040	14.799002
20.252225	990.277473	14.804019
20.365762	994.052706	14.809037
20.102727	1004.384930	14.814055
20.110228	1000.338257	14.819072
20.153424	1001.398865	14.824090
20.173167	995.716370	14.829107
20.129686	988.501098	14.834125
20.060330	1004.215610	14.839143
20.266345	992.960749	14.844160
19.928048	1001.812578	14.849178
20.181008	997.926434	14.854195
20.044853	1007.156196	14.859213
19.959339	1016.561430	14.864231
20.456066	1024.333305	14.869248
20.245552	1024.492653	14.874266
20.407651	1034.145468	14.879283
20.612493	1026.262704	14.884301
20.509001	1030.039633	14.889319
20.732044	1029.520912	14.894336
20.433719	1021.365576	14.899354
20.453329	1026.094524	14.904371
20.762081	1031.171645	14.909389
20.422843	1022.461686	14.914407
20.718866	1016.510608	14.919424
20.489621	1019.043836	14.924442
20.553968	1016.936493	14.929459
20.650580	1028.167413	14.934477
20.527132	1021.654712	14.939495
20.797655	1020.995064	14.944512
20.849947	1024.708795	14.949530
20.393722	1024.449397	14.954547
20.837935	1023.719257	14.959565
20.945930	1029.670140	14.964583
20.925287	1023.910073	14.969600
20.325774	1031.423728	14.974618
20.500200	1030.058364	14.979635
20.946293	1033.499809	14.984653
20.953801	1043.960090	14.989671
21.193007	1027.409738	14.994688
20.873912	1030.619240	14.999706
20.868068	1028.921534	15.004723
20.980897	1029.304103	15.009741
20.959101	1042.521892	15.014759
21.214713	1042.596182	15.019776
21.333564	1036.566957	15.024794
20.857532	1033.129063	15.029811
21.189462	1020.161268	15.034829
20.710085	1016.208990	15.039847
21.201186	1021.500392	15.044864
21.276231	1039.401971	15.049882
20.908441	1044.914340	15.054899
21.305235	1047.585632	15.059917
21.024680	1052.233588	15.064935
21.378306	1045.961161	15.069952
21.165112	1050.020423	15.074970
21.109087	1055.428416	15.079987
21.250910	1051.608692	15.085005
20.939895	1060.445801	15.090023
21.292307	1051.225248	15.095040
21.474601	1057.724450	15.100058
21.333990	1053.601110	15.105075
21.562070	1043.537400	15.110093
21.220238	1048.010074	15.115111
21.721875	1042.286741	15.120128
21.394457	1043.906735	15.125146
21.584995	1049.719947	15.130163
21.777941	1047.098802	15.135181
21.710147	1055.821228	15.140199
21.638783	1050.804170	15.145216
21.469681	1053.950652	15.150234
21.313519	1050.415695	15.155251
21.709662	1041.948509	15.160269
21.296689	1047.312854	15.165287
21.610030	1048.150392	15.170304
21.462636	1053.347539	15.175322
21.600931	1045.459643	15.180339
21.672372	1038.189493	15.185357
21.531398	1045.465815	15.190375
21.565900	1042.948070	15.195392
21.737502	1052.244217	15.200410
21.762249	1050.466250	15.205427
22.050567	1049.012343	15.210445
21.864954	1052.445801	15.215463
21.847320	1047.550157	15.220480
21.847678	1053.527140	15.225498
21.526767	1046.882959	15.230515
22.069105	1050.811997	15.235533
22.014731	1075.576938	15.240551
22.270436	1072.959176	15.245568
22.035780	1061.510315	15.250586
21.920599	1057.946524	15.255603
22.173127	1051.527454	15.260621
21.724191	1052.344371	15.265639
22.093879	1066.411891	15.270656
21.945305	1078.503105	15.275674
21.737154	1078.748673	15.280691
21.878012	1080.379316	15.285709
21.696511	1090.185909	15.290727
21.788988	1081.198531	15.295744
22.220996	1077.744909	15.300762
22.266703	1076.120156	15.305779
22.150447	1083.439645	15.310797
22.067342	1074.991565	15.315815
22.112457	1080.806034	15.320832
22.083281	1078.720468	15.325850
22.114517	1095.349880	15.330867
22.227715	1105.545859	15.335885
22.568854	1105.272534	15.340903
22.512837	1095.830618	15.345920
22.627343	1094.470052	15.350938
23.015391	1102.900101	15.355955
22.681099	1075.522173	15.360973
22.563682	1075.984599	15.365991
22.474996	1067.377216	15.371008
22.666298	1064.217383	15.376026
22.600068	1061.313967	15.381043
22.800719	1063.136275	15.386061
22.531714	1064.000167	15.391079
22.503439	1057.677591	15.396096
22.760418	1055.525353	15.401114
22.630571	1068.438626	15.406131
22.962006	1058.937300	15.411149
22.741431	1064.603245	15.416167
23.052369	1061.427539	15.421184
22.914927	1056.489922	15.426202
22.989350	1060.977530	15.431219
22.874202	1054.171325	15.436237
22.978504	1064.602994	15.441255
22.977288	1054.456777	15.446272
22.966231	1059.380570	15.451290
23.163680	1066.214263	15.456307
22.994887	1066.018289	15.461325
23.075843	1052.309374	15.466343
22.730411	1058.084571	15.471360
22.840937	1057.968326	15.476378
22.676570	1060.640813	15.481395
22.802200	1065.241985	15.486413
22.691849	1059.623920	15.491431
22.760054	1053.588509	15.496448
23.102121	1059.409703	15.501466
22.945256	1064.913922	15.506483
23.176909	1078.160638	15.511501
23.322476	1087.815043	15.516519
23.435154	1083.163549	15.521536
23.071033	1059.973917	15.526554
23.165748	1069.933177	15.531571
23.402349	1066.588684	15.536589
23.107174	1059.078453	15.541607
23.066181	1053.037896	15.546624
23.306388	1075.501775	15.551642
23.034772	1091.489228	15.556659
23.220580	1078.146381	15.561677
23.485161	1088.888917	15.566695
23.510069	1081.442600	15.571712
23.611074	1079.637829	15.576730
23.022675	1081.947871	15.581747
23.426671	1085.521492	15.586765
23.369449	1081.413863	15.591783
23.262438	1094.668247	15.596800
23.300737	1084.961122	15.601818
23.148075	1085.693155	15.606835
23.363615	1086.974436	15.611853
23.592248	1085.970158	15.616871
23.157169	1085.890323	15.621888
23.690761	1103.076697	15.626906
23.743015	1116.423228	15.631923
24.175113	1111.883790	15.636941
23.838336	1113.795095	15.641959
23.599165	1100.248592	15.646976
23.571680	1104.536164	15.651994
23.539679	1111.835416	15.657011
23.741223	1113.422551	15.662029
23.996694	1110.845765	15.667047
23.924660	1115.300161	15.672064
24.351476	1111.105288	15.677082
23.916786	1117.452750	15.682099
24.016344	1113.533319	15.687117
23.827485	1107.521950	15.692135
24.242064	1114.687808	15.697152
24.136723	1117.433206	15.702170
23.805175	1114.294587	15.707187
24.135320	1113.771908	15.712205
24.085236	1116.240054	15.717223
24.143098	1117.259660	15.722240
24.588879	1105.233936	15.727258
24.084876	1094.702851	15.732275
24.027050	1096.775044	15.737293
24.227390	1106.409367	15.742311
24.091781	1122.786131	15.747328
24.168539	1106.663762	15.752346
24.168945	1118.951198	15.757363
24.081133	1113.486069	15.762381
24.492491	1117.874201	15.767399
24.234466	1113.428172	15.772416
24.616010	1105.870035	15.777434
24.346037	1112.186283	15.782451
24.131045	1100.775080	15.787469
24.779580	1106.237287	15.792487
24.260565	1112.705793	15.797504
24.211952	1102.734710	15.802522
24.236781	1109.927310	15.807539
24.368842	1109.093741	15.812557
24.452916	1114.116363	15.817575
24.605285	1109.957093	15.822592
24.434162	1102.281029	15.827610
24.480343	1117.488351	15.832627
24.268885	1112.688559	15.837645
24.704051	1108.928511	15.842663
24.811750	1129.053458	15.847680
25.082689	1126.017036	15.852698
24.852106	1112.059664	15.857715
24.581622	1115.161136	15.862733
24.522313	1108.951154	15.867751
24.344544	1112.779377	15.872768
24.892403	1123.513612	15.877786
25.128783	1126.250850	15.882803
24.995857	1125.637138	15.887821
25.378247	1126.532537	15.892839
25.199983	1118.187195	15.897856
24.941348	1107.961130	15.902874
25.017012	1098.920623	15.907891
24.854957	1101.597458	15.912909
25.250293	1102.184029	15.917927
24.803635	1098.101512	15.922944
25.109412	1091.104336	15.927962
24.981860	1102.292116	15.932979
24.763276	1114.350463	15.937997
25.077363	1123.960451	15.943015
25.276024	1133.588771	15.948032
25.535966	1125.516523	15.953050
25.211954	1127.707991	15.958067
25.180382	1118.242723	15.963085
25.167990	1123.754929	15.968103
24.843743	1133.962734	15.973120
25.264721	1119.310475	15.978138
25.318152	1139.809766	15.983155
25.168388	1135.189509	15.988173
25.093737	1133.237840	15.993191
24.877025	1129.058579	15.998208
25.452491	1125.408756	16.003226
25.356355	1132.394632	16.008243
25.530887	1152.734521	16.013261
25.892094	1150.147307	16.018279
25.652271	1145.561644	16.023296
25.670204	1130.972964	16.028314
25.647879	1133.027078	16.033331
25.696382	1126.527592	16.038349
25.874227	1120.946032	16.043367
25.288956	1126.322793	16.048384
25.780583	1125.252524	16.053402
25.541255	1134.276618	16.058419
26.013688	1149.046471	16.063437
25.985401	1137.316144	16.068455
25.299965	1140.007605	16.073472
25.746687	1146.504002	16.078490
25.810597	1148.891074	16.083507
25.894357	1155.667649	16.088525
25.813319	1155.732726	16.093543
25.724945	1162.765360	16.098560
25.938186	1154.132736	16.103578
26.064084	1151.312053	16.108595
26.140743	1149.540833	16.113613
26.107579	1152.060905	16.118631
26.034739	1150.714034	16.123648
26.159604	1149.776933	16.128666
26.123518	1149.064904	16.133683
26.000678	1156.304417	16.138701
26.291352	1142.037483	16.143719
25.873911	1148.729729	16.148736
26.230977	1153.533937	16.153754
26.277984	1154.728173	16.158771
26.180449	1154.738109	16.163789
26.364690	1151.273530	16.168807
26.429539	1148.410202	16.173824
26.619569	1149.418161	16.178842
26.635749	1146.261326	16.183859
26.350286	1149.396387	16.188877
26.494375	1146.776623	16.193895
26.123644	1155.291794	16.198912
26.332054	1146.640290	16.203930
26.307746	1157.122451	16.208947
26.471942	1158.340981	16.213965
26.497245	1148.541876	16.218983
26.272716	1154.766760	16.224000
26.308322	1147.865475	16.229018
26.499327	1153.138900	16.234035
26.346679	1169.163032	16.239053
26.513019	1172.239820	16.244071
26.633058	1168.403202	16.249088
26.850524	1172.516772	16.254106
27.122278	1175.271783	16.259123
26.794330	1169.860177	16.264141
26.851047	1167.351331	16.269159
26.758191	1182.610479	16.274176
26.993399	1173.245092	16.279194
26.868624	1175.437040	16.284211
26.604833	1173.658413	16.289229
26.852952	1165.154256	16.294247
26.929639	1170.680862	16.299264
26.838516	1171.026735	16.304282
27.129694	1170.678219	16.309299
26.920186	1174.566042	16.314317
27.278317	1171.060461	16.319335
26.786000	1174.082539	16.324352
27.215031	1176.276089	16.329370
27.067500	1165.878049	16.334387
27.149752	1171.110435	16.339405
27.236388	1163.795978	16.344423
27.013447	1167.933261	16.349440
27.001194	1169.723121	16.354458
26.991912	1175.627734	16.359475
27.082857	1174.549402	16.364493
27.540697	1185.269454	16.369511
27.327844	1187.841726	16.374528
27.270425	1196.157798	16.379546
27.673635	1186.897259	16.384563
27.633134	1192.555479	16.389581
27.783173	1180.123168	16.394599
27.660152	1171.839120	16.399616
27.574229	1164.146949	16.404634
27.739956	1160.972828	16.409651
27.193350	1167.590409	16.414669
27.736511	1155.777649	16.419687
27.312790	1159.056075	16.424704
27.610065	1170.691261	16.429722
28.042739	1178.058085	16.434739
27.879528	1187.587308	16.439757
28.025527	1166.916916	16.444775
27.908611	1160.870385	16.449792
27.656865	1153.761960	16.454810
27.792477	1157.924906	16.459827
27.491513	1156.142594	16.464845
27.565179	1173.905585	16.469863
27.948573	1177.437759	16.474880
28.058850	1189.510999	16.479898
28.698004	1183.997516	16.484915
28.185779	1184.469021	16.489933
28.298263	1161.767231	16.494951
28.084431	1155.769426	16.499968
28.100520	1145.252577	16.504986
28.075721	1147.064197	16.510003
27.650333	1154.461284	16.515021
28.429023	1167.769460	16.520039
28.653321	1170.150449	16.525056
28.208130	1156.492738	16.530074
28.236685	1152.297267	16.535091
27.920542	1138.889062	16.540109
28.142823	1140.975113	16.545127
28.377720	1163.836839	16.550144
28.590231	1171.152323	16.555162
28.563116	1153.179046	16.560179
28.014613	1148.464185	16.565197
28.416695	1156.871468	16.570215
28.521491	1183.632217	16.575232
28.295102	1179.108885	16.580250
29.011897	1177.541892	16.585267
28.404750	1174.722511	16.590285
28.643548	1166.942318	16.595303
28.630376	1169.646085	16.600320
28.261406	1176.762195	16.605338
29.107432	1171.338080	16.610355
28.589384	1169.462188	16.615373
28.814464	1170.499383	16.620391
28.840819	1168.680192	16.625408
28.477017	1178.337504	16.630426
28.865014	1174.419508	16.635443
29.005712	1176.461201	16.640461
28.789071	1172.485454	16.645479
29.004554	1168.598388	16.650496
28.403171	1169.650389	16.655514
28.689930	1168.342789	16.660531
28.600069	1183.051062	16.665549
28.787610	1168.207889	16.670567
28.775949	1167.504412	16.675584
28.555486	1162.619877	16.680602
28.762340	1170.370537	16.685619
28.830441	1183.162549	16.690637
28.918687	1181.867740	16.695655
28.773781	1186.158243	16.700672
29.124011	1183.140570	16.705690
29.277527	1177.249641	16.710707
28.974327	1190.179122	16.715725
29.236185	1184.797009	16.720743
29.379042	1181.495178	16.725760
29.142351	1185.559153	16.730778
29.399983	1186.739381	16.735795
29.191445	1188.515290	16.740813
29.393159	1180.440845	16.745831
29.358775	1194.223038	16.750848
29.392512	1204.991676	16.755866
29.756778	1203.526360	16.760883
29.824488	1219.944361	16.765901
29.611170	1193.220192	16.770919
29.675865	1176.391105	16.775936
29.344373	1182.245533	16.780954
29.857575	1185.520394	16.785971
30.084726	1199.059684	16.790989
29.831466	1185.785116	16.796007
29.934923	1178.197403	16.801024
29.767382	1174.498951	16.806042
29.843922	1169.240046	16.811059
29.983310	1162.417629	16.816077
29.982561	1168.477909	16.821095
30.123618	1165.668492	16.826112
29.762004	1173.442813	16.831130
29.963136	1171.676569	16.836147
29.774271	1176.193240	16.841165
29.922239	1168.178094	16.846183
30.004066	1176.609284	16.851200
29.861850	1192.779348	16.856218
30.169661	1192.126904	16.861235
30.281757	1204.478982	16.866253
30.354887	1202.951247	16.871271
30.228702	1186.213991	16.876288
30.263518	1180.350196	16.881306
30.252748	1166.649675	16.886323
30.237293	1181.588928	16.891341
30.403878	1183.660193	16.896359
30.255943	1168.764304	16.901376
30.024756	1182.358214	16.906394
30.273278	1191.759423	16.911411
30.356652	1201.037593	16.916429
30.454213	1203.979323	16.921447
30.241201	1202.160395	16.926464
30.340757	1205.589185	16.931482
30.473461	1197.885992	16.936499
30.092968	1198.203011	16.941517
30.321103	1207.538709	16.946535
29.995161	1190.941214	16.951552
30.203396	1218.941558	16.956570
30.583172	1230.357228	16.961587
30.793042	1234.020507	16.966605
30.746752	1220.526210	16.971623
31.146655	1222.352158	16.976640
30.618558	1219.894866	16.981658
30.951542	1225.142838	16.986675
31.081784	1222.287565	16.991693
31.059528	1226.946738	16.996711
31.320966	1219.652129	17.001728
30.990035	1224.174228	17.006746
30.999975	1221.057780	17.011763
30.920111	1225.563896	17.016781
31.078330	1227.229475	17.021799
31.339442	1216.121625	17.026816
30.901425	1223.494852	17.031834
31.502726	1224.770535	17.036851
31.257521	1222.264432	17.041869
31.015310	1219.849170	17.046887
31.297687	1225.505118	17.051904
31.465632	1223.125875	17.056922
31.615303	1221.946479	17.061939
31.316921	1222.785323	17.066957
31.519272	1225.077043	17.071975
31.564914	1213.981252	17.076992
31.211270	1222.120017	17.082010
31.316973	1211.130421	17.087027
31.298413	1219.762505	17.092045
31.231478	1219.837451	17.097063
31.721695	1212.632519	17.102080
31.325627	1215.642210	17.107098
31.289255	1219.988765	17.112115
31.411571	1215.899796	17.117133
31.437606	1217.916387	17.122151
31.480928	1222.620210	17.127168
31.409972	1216.819978	17.132186
31.481980	1232.631390	17.137203
31.701641	1244.437748	17.142221
31.780699	1256.267790	17.147239
32.000167	1243.635747	17.152256
31.688933	1262.190116	17.157274
31.982514	1253.745705	17.162291
31.962361	1255.219174	17.167309
32.139976	1252.228888	17.172327
32.205593	1250.757904	17.177344
31.783188	1261.597780	17.182362
32.193250	1256.491489	17.187379
31.949481	1258.827952	17.192397
32.036968	1254.377031	17.197415
32.146486	1248.297696	17.202432
32.076116	1256.607679	17.207450
31.897501	1245.750962	17.212467
32.211289	1245.303428	17.217485
31.835053	1235.334935	17.222503
32.321166	1246.158219	17.227520
31.979486	1254.995004	17.232538
31.995036	1270.665019	17.237555
32.078554	1274.141755	17.242573
32.219800	1275.835739	17.247591
32.635691	1273.387873	17.252608
32.209655	1274.889576	17.257626
32.434443	1267.919117	17.262643
32.980834	1276.769097	17.267661
32.439156	1264.405194	17.272679
32.811737	1276.996869	17.277696
32.521174	1269.814111	17.282714
32.819781	1277.370108	17.287731
32.756223	1275.199659	17.292749
32.607351	1278.474329	17.297767
32.737480	1266.058632	17.302784
32.740959	1272.412340	17.307802
32.725759	1261.754139	17.312819
33.147288	1262.891487	17.317837
32.719900	1273.140476	17.322855
32.982595	1281.497288	17.327872
32.977844	1294.099489	17.332890
32.906124	1300.305821	17.337907
33.225520	1300.138848	17.342925
33.231357	1303.241452	17.347943
33.350771	1297.806510	17.352960
33.312874	1296.006999	17.357978
33.508032	1285.108048	17.362995
33.385155	1259.685298	17.368013
32.962650	1269.555138	17.373031
33.190119	1266.823125	17.378048
33.677381	1291.707383	17.383066
33.396794	1283.288739	17.388083
33.665245	1276.863397	17.393101
33.477423	1271.815945	17.398119
33.702059	1260.132619	17.403136
33.324614	1265.075022	17.408154
33.486367	1263.623156	17.413171
33.713429	1254.806695	17.418189
33.228147	1261.503529	17.423207
33.550453	1273.204333	17.428224
33.582667	1286.920857	17.433242
33.416824	1291.016041	17.438259
33.935112	1294.422759	17.443277
33.863489	1292.822529	17.448295
33.888291	1288.729609	17.453312
34.105931	1297.381286	17.458330
34.084899	1297.313988	17.463347
33.995955	1298.980738	17.468365
33.920794	1288.859997	17.473383
34.349103	1290.578890	17.478400
34.327104	1292.294789	17.483418
34.293479	1278.757793	17.488435
34.330610	1266.037422	17.493453
34.018780	1269.532377	17.498471
34.147768	1256.292877	17.503488
34.114506	1257.842137	17.508506
33.914363	1252.156194	17.513523
34.246628	1263.448657	17.518541
33.980625	1289.097390	17.523559
34.226982	1275.779385	17.528576
34.057729	1289.189121	17.533594
34.414780	1290.052901	17.538611
34.174232	1291.175473	17.543629
34.048168	1296.748688	17.548647
34.133852	1288.647732	17.553664
34.114585	1290.852539	17.558682
34.132413	1296.368464	17.563699
34.569286	1304.899594	17.568717
34.603759	1315.033552	17.573735
34.615290	1318.603712	17.578752
34.627448	1321.701730	17.583770
34.361403	1310.393705	17.588787
34.832568	1316.272753	17.593805
34.602754	1318.202590	17.598823
34.750657	1316.834901	17.603840
34.692495	1311.114403	17.608858
34.754255	1318.360433	17.613875
34.861544	1316.938052	17.618893
34.577075	1315.354561	17.623911
34.562962	1320.601379	17.628928
34.792415	1318.694605	17.633946
34.873250	1325.281191	17.638963
35.179905	1340.436153	17.643981
35.417960	1342.412142	17.648999
35.258083	1338.102549	17.654016
35.346075	1332.251151	17.659034
35.188849	1330.468245	17.664051
34.915892	1317.504694	17.669069
35.145438	1334.925136	17.674087
35.356601	1336.798098	17.679104
35.548687	1333.909337	17.684122
35.608163	1340.308131	17.689139
35.576659	1343.979909	17.694157
35.614221	1344.648173	17.699175
35.512782	1332.375883	17.704192
35.460827	1332.568032	17.709210
35.246490	1342.481794	17.714227
35.809493	1337.662746	17.719245
35.414729	1336.607743	17.724263
35.650801	1332.494002	17.729280
35.519644	1339.079477	17.734298
35.606860	1334.722277	17.739315
35.879394	1334.561095	17.744333
35.839651	1339.706654	17.749351
35.890113	1338.062582	17.754368
35.922079	1339.869943	17.759386
35.747806	1343.968899	17.764403
36.034067	1348.699462	17.769421
35.912262	1343.988687	17.774439
35.752774	1341.322703	17.779456
36.278973	1338.816799	17.784474
35.997610	1337.790262	17.789491
36.178407	1334.135272	17.794509
36.021375	1347.852873	17.799527
36.191833	1346.618846	17.804544
36.318979	1354.522952	17.809562
35.886070	1360.520222	17.814579
36.455357	1364.535037	17.819597
36.255876	1370.446415	17.824615
36.183337	1365.285751	17.829632
36.316606	1362.956321	17.834650
36.414830	1361.706302	17.839667
36.634911	1360.919562	17.844685
36.685367	1358.966439	17.849703
36.310394	1357.919574	17.854720
36.561438	1350.428990	17.859738
36.335183	1362.282504	17.864755
36.761112	1356.127900	17.869773
36.632719	1360.598785	17.874791
36.556590	1356.091070	17.879808
36.859610	1358.249215	17.884826
36.698608	1360.429864	17.889843
37.008542	1351.473644	17.894861
36.648018	1354.224330	17.899879
36.776842	1358.149875	17.904896
36.924070	1365.785705	17.909914
37.261741	1378.790719	17.914931
37.092154	1359.670730	17.919949
37.052470	1358.184495	17.924967
37.274371	1354.321909	17.929984
37.088740	1352.013003	17.935002
37.096696	1361.158484	17.940019
37.284393	1373.059209	17.945037
37.068883	1375.332349	17.950055
37.297498	1385.072400	17.955072
37.290054	1384.841044	17.960090
37.307419	1392.496422	17.965107
37.702612	1386.800039	17.970125
37.671623	1392.722502	17.975143
37.590609	1387.957323	17.980160
37.702717	1379.713756	17.985178
37.477787	1367.377635	17.990195
37.643710	1363.443216	17.995213
37.563103	1372.739980	18.000231
38.005237	1375.545949	18.005248
37.901724	1361.148024	18.010266
37.865219	1358.673875	18.015283
37.585035	1350.112609	18.020301
37.749200	1351.874067	18.025319
37.725034	1365.968102	18.030336
37.781301	1368.454503	18.035354
37.833500	1383.326843	18.040371
37.989868	1376.158219	18.045389
37.710706	1377.058060	18.050407
38.120678	1368.758485	18.055424
38.454538	1370.307203	18.060442
38.196173	1373.842933	18.065459
38.324228	1372.074594	18.070477
37.994752	1367.032062	18.075495
38.159330	1364.497058	18.080512
38.461394	1358.374380	18.085530
38.561093	1367.018854	18.090547
38.375219	1364.117081	18.095565
38.452766	1364.838961	18.100583
38.019458	1361.219903	18.105600
38.460141	1355.376238	18.110618
38.313582	1362.317811	18.115635
38.556672	1362.735511	18.120653
38.363439	1358.697179	18.125671
38.298081	1368.984709	18.130688
38.869965	1356.629648	18.135706
38.500019	1365.191259	18.140723
38.532879	1358.784421	18.145741
38.706282	1355.803475	18.150759
38.501654	1382.753598	18.155776
38.836125	1383.698287	18.160794
38.896545	1382.764757	18.165811
38.608540	1381.583019	18.170829
38.803802	1399.097792	18.175847
38.776287	1383.001850	18.180864
39.046424	1382.490282	18.185882
38.905260	1387.640446	18.190899
39.131510	1379.905138	18.195917
39.013211	1378.016569	18.200935
39.050162	1389.345819	18.205952
39.235031	1382.078379	18.210970
38.765288	1380.366112	18.215987
39.153159	1396.300584	18.221005
39.236979	1395.336014	18.226023
39.470535	1415.307032	18.231040
39.420183	1408.441123	18.236058
39.561360	1407.217845	18.241075
39.760385	1409.300305	18.246093
39.394383	1407.574794	18.251111
39.183214	1415.074326	18.256128
40.138033	1397.600371	18.261146
39.540274	1412.090209	18.266163
39.773002	1405.072311	18.271181
39.815168	1410.893299	18.276199
39.928460	1410.593132	18.281216
40.119330	1404.127435	18.286234
39.873830	1403.804395	18.291251
39.985510	1396.212458	18.296269
40.107392	1379.066205	18.301287
40.032742	1377.101905	18.306304
39.939812	1376.028416	18.311322
39.657393	1374.198519	18.316339
40.062373	1384.479438	18.321357
40.163693	1396.892115	18.326375
39.843220	1399.105474	18.331392
40.497260	1408.284946	18.336410
40.020513	1407.604532	18.341427
39.795842	1402.690302	18.346445
39.969782	1400.333661	18.351463
39.992778	1402.329520	18.356480
39.870092	1398.151939	18.361498
40.101645	1413.019806	18.366515
40.239324	1422.204079	18.371533
40.768034	1429.795672	18.376551
40.756535	1436.346414	18.381568
40.500792	1428.563333	18.386586
40.409572	1425.058087	18.391603
40.860834	1429.842062	18.396621
41.218984	1421.882139	18.401639
40.757023	1424.965377	18.406656
41.083427	1422.980333	18.411674
40.772640	1421.525596	18.416691
41.066638	1423.002574	18.421709
41.333001	1419.918429	18.426727
40.775357	1418.779367	18.431744
41.122969	1409.871993	18.436762
41.341035	1423.157869	18.441779
41.076386	1418.654974	18.446797
41.138100	1412.251210	18.451815
41.265238	1415.547135	18.456832
41.239262	1418.021179	18.461850
41.082123	1413.863471	18.466867
41.213803	1414.425604	18.471885
41.535716	1404.086284	18.476903
41.042461	1412.617945	18.481920
41.255603	1414.534684	18.486938
41.219333	1416.012411	18.491955
41.353959	1413.387084	18.496973
41.301468	1411.358088	18.501991
41.489758	1415.824189	18.507008
41.189878	1413.960171	18.512026
41.299217	1424.436918	18.517043
41.203186	1430.771736	18.522061
41.771227	1443.402443	18.527079
41.620934	1443.392374	18.532096
42.065393	1434.872883	18.537114
42.067326	1450.271715	18.542131
41.679047	1450.059717	18.547149
42.076403	1445.890107	18.552167
41.782773	1446.680537	18.557184
42.064056	1442.214008	18.562202
41.857547	1443.924650	18.567219
41.823151	1447.826851	18.572237
42.275866	1445.788212	18.577255
41.845704	1448.716979	18.582272
41.908988	1450.467986	18.587290
41.823187	1459.971960	18.592307
42.315542	1466.806606	18.597325
42.431831	1470.742917	18.602343
42.434941	1464.733085	18.607360
42.349309	1465.683955	18.612378
42.940891	1465.788445	18.617395
42.759646	1456.346572	18.622413
43.183355	1457.408772	18.627431
42.412434	1448.938944	18.632448
42.877718	1447.006098	18.637466
42.841898	1430.726837	18.642483
42.569483	1429.850385	18.647501
43.014649	1429.996047	18.652519
42.868527	1432.280934	18.657536
42.720482	1426.630000	18.662554
43.062718	1437.362285	18.667571
43.049277	1445.419243	18.672589
43.152010	1425.854872	18.677607
42.922874	1435.676656	18.682624
43.098280	1429.189100	18.687642
43.377135	1435.266179	18.692659
42.818526	1437.176064	18.697677
43.211012	1433.207656	18.702695
43.220895	1445.815825	18.707712
43.649360	1446.058347	18.712730
43.363689	1454.093852	18.717747
43.239608	1448.194850	18.722765
43.244604	1449.698030	18.727783
43.513346	1446.365851	18.732800
43.345084	1447.089460	18.737818
43.668479	1446.638756	18.742835
43.537668	1449.500632	18.747853
43.683447	1440.191232	18.752871
43.621338	1452.255034	18.757888
43.713432	1442.746648	18.762906
43.650093	1449.653615	18.767923
43.594156	1458.268792	18.772941
43.883593	1449.110794	18.777959
43.535301	1455.007869	18.782976
43.562888	1446.218031	18.787994
44.113874	1456.298446	18.793011
43.840423	1467.678363	18.798029
44.129401	1473.577797	18.803047
44.081411	1484.036148	18.808064
43.920010	1487.288921	18.813082
44.376546	1477.235134	18.818099
43.779502	1481.523812	18.823117
44.122643	1479.718666	18.828135
44.132769	1485.418217	18.833152
43.983575	1480.867052	18.838170
44.238773	1480.025674	18.843187
44.213967	1482.961735	18.848205
44.594884	1487.430213	18.853223
44.758609	1493.378347	18.858240
44.621147	1501.369651	18.863258
44.587559	1495.430843	18.868275
44.512956	1492.276765	18.873293
44.450410	1492.713975	18.878311
44.705265	1498.774974	18.883328
44.321764	1495.145668	18.888346
44.859580	1488.322490	18.893363
44.758440	1499.364058	18.898381
45.186712	1485.382685	18.903399
45.017193	1494.232436	18.908416
44.866240	1491.866586	18.913434
44.890997	1486.088199	18.918451
44.746584	1490.728701	18.923469
45.063347	1496.020792	18.928487
45.369615	1507.642934	18.933504
45.269070	1513.474205	18.938522
45.396411	1507.848902	18.943539
45.587754	1523.016839	18.948557
45.445209	1503.601644	18.953575
45.282495	1499.906644	18.958592
45.120414	1517.433477	18.963610
45.290631	1518.332932	18.968627
45.463035	1524.217830	18.973645
45.715414	1522.384401	18.978663
45.683071	1521.899292	18.983680
45.465248	1519.840571	18.988698
46.004356	1514.575823	18.993715
45.976820	1522.605628	18.998733
45.777053	1513.934106	19.003751
46.151340	1515.049769	19.008768
45.764409	1508.951748	19.013786
45.958160	1511.056354	19.018803
45.683394	1517.084584	19.023821
46.055540	1512.030159	19.028839
45.483204	1510.789191	19.033856
45.613744	1508.455468	19.038874
46.271644	1523.945757	19.043891
46.474250	1536.252012	19.048909
46.559107	1530.690822	19.053927
46.295793	1537.397081	19.058944
46.272601	1533.259682	19.063962
46.891758	1530.223005	19.068979
47.003933	1529.068299	19.073997
46.950998	1507.761497	19.079015
46.507435	1505.446457	19.084032
46.638952	1504.985004	19.089050
46.609286	1500.442781	19.094067
46.397046	1506.041365	19.099085
46.618671	1514.583450	19.104103
46.514232	1521.207491	19.109120
47.126690	1524.173474	19.114138
47.220800	1527.411112	19.119155
46.883265	1527.211182	19.124173
46.922751	1524.170095	19.129191
47.158669	1519.675230	19.134208
46.669409	1525.639767	19.139226
46.919101	1517.667439	19.144243
46.829304	1520.616631	19.149261
47.106179	1518.532691	19.154279
47.440979	1516.289948	19.159296
46.972116	1520.709774	19.164314
47.157812	1527.043258	19.169331
46.978336	1546.827326	19.174349
47.228919	1553.942201	19.179367
47.103705	1558.372458	19.184384
47.274875	1561.342227	19.189402
47.369860	1555.115966	19.194419
47.117300	1554.462989	19.199437
47.462270	1565.535067	19.204455
47.704633	1579.840283	19.209472
47.467110	1581.615916	19.214490
47.934509	1572.031529	19.219507
47.818714	1587.403141	19.224525
47.824397	1580.206224	19.229543
47.971548	1577.282733	19.234560
47.821165	1576.283309	19.239578
48.289667	1576.039678	19.244595
48.403542	1590.183107	19.249613
48.291317	1586.741538	19.254631
48.401926	1574.235912	19.259648
48.176599	1586.096923	19.264666
48.473668	1580.227348	19.269683
48.327339	1578.989852	19.274701
48.099723	1576.763454	19.279719
48.585316	1569.776054	19.284736
48.280191	1576.635710	19.289754
48.891463	1573.270016	19.294771
48.356360	1570.333510	19.299789
48.411796	1572.808271	19.304807
48.501235	1577.220314	19.309824
48.460347	1572.925992	19.314842
48.885421	1583.910410	19.319859
49.001726	1597.245176	19.324877
48.844065	1594.505617	19.329895
49.175282	1601.048895	19.334912
49.065768	1613.125789	19.339930
49.241476	1588.158177	19.344947
48.898657	1586.383530	19.349965
48.981785	1591.421426	19.354983
48.979296	1599.001847	19.360000
49.305697	1591.298670	19.365018
50.007564	1596.047109	19.370035
49.571219	1596.665900	19.375053
49.571969	1572.529252	19.380071
49.193206	1565.053479	19.385088
49.252609	1584.496861	19.390106
49.283536	1582.455999	19.395123
49.382653	1588.322742	19.400141
49.533439	1599.201800	19.405159
49.663343	1588.421316	19.410176
49.620541	1590.058804	19.415194
49.759388	1591.101252	19.420211
49.497374	1600.460081	19.425229
49.464012	1600.081437	19.430247
49.946844	1600.951969	19.435264
49.684276	1610.669163	19.440282
49.776744	1612.887799	19.445299
49.749315	1622.988508	19.450317
49.883265	1626.184924	19.455335
49.990984	1626.837253	19.460352
49.754407	1624.462725	19.465370
50.007435	1612.240575	19.470387
50.000677	1632.511509	19.475405
50.102787	1635.119891	19.480423
50.496708	1646.715419	19.485440
50.574919	1654.098253	19.490458
50.862056	1651.474799	19.495475
50.790888	1649.015791	19.500493
50.605523	1650.109959	19.505511
50.820551	1651.263027	19.510528
50.700805	1643.893935	19.515546
50.714230	1650.020560	19.520563
50.868615	1645.395851	19.525581
50.693798	1640.561873	19.530599
50.935083	1649.484243	19.535616
50.867946	1655.599013	19.540634
50.964746	1641.200337	19.545651
50.873071	1645.076639	19.550669
50.852243	1645.495134	19.555687
50.901374	1638.053594	19.560704
51.109290	1637.057044	19.565722
51.417433	1638.832884	19.570739
51.279246	1642.966887	19.575757
51.326911	1650.833519	19.580775
51.540504	1654.002581	19.585792
51.271861	1666.538151	19.590810
51.326406	1654.724425	19.595827
51.722766	1659.597485	19.600845
51.753473	1666.029524	19.605863
51.852001	1661.780203	19.610880
51.942193	1664.414973	19.615898
51.842301	1657.124083	19.620915
51.907584	1664.147643	19.625933
51.876289	1665.743469	19.630951
51.768848	1667.655842	19.635968
51.653059	1664.822328	19.640986
51.784190	1654.260495	19.646003
51.948726	1657.395554	19.651021
51.926752	1663.060327	19.656039
52.173721	1653.001757	19.661056
51.915807	1660.769385	19.666074
52.016569	1661.113024	19.671091
52.116289	1656.812719	19.676109
51.985817	1677.025061	19.681127
52.352359	1683.034175	19.686144
52.093169	1686.671687	19.691162
52.305778	1688.140515	19.696179
52.566220	1688.466769	19.701197
52.475420	1691.017338	19.706215
52.897475	1680.898657	19.711232
52.721158	1674.983414	19.716250
52.770652	1680.079270	19.721267
53.078297	1681.976064	19.726285
52.873443	1684.988040	19.731303
53.036183	1672.812682	19.736320
53.122739	1676.171288	19.741338
53.094897	1674.928732	19.746355
53.075704	1673.348128	19.751373
53.208663	1697.518081	19.756391
53.360762	1696.519747	19.761408
53.568972	1689.496332	19.766426
53.376207	1682.329471	19.771443
53.558942	1665.072431	19.776461
53.364173	1674.826865	19.781479
53.872326	1673.414456	19.786496
53.475321	1670.584985	19.791514
53.600686	1678.495065	19.796531
53.600949	1679.670704	19.801549
53.610960	1693.843237	19.806567
53.548148	1692.763557	19.811584
53.707896	1702.836475	19.816602
53.899948	1689.814906	19.821619
54.522117	1698.214786	19.826637
54.332295	1694.407299	19.831655
54.440523	1699.398553	19.836672
54.480140	1693.608180	19.841690
54.166730	1676.622650	19.846707
54.174879	1660.582326	19.851725
54.378130	1683.415416	19.856743
54.096227	1679.970031	19.861760
54.406885	1682.889955	19.866778
54.370652	1686.382675	19.871795
54.389113	1675.145384	19.876813
54.299389	1692.340746	19.881831
54.338900	1680.167282	19.886848
54.541127	1683.648077	19.891866
54.281036	1684.973519	19.896883
54.413091	1685.621821	19.901901
54.341547	1686.921556	19.906919
54.550068	1711.663276	19.911936
54.785569	1714.358641	19.916954
54.665047	1719.490535	19.921971
54.930811	1711.919387	19.926989
54.830078	1715.155075	19.932007
54.940543	1705.747031	19.937024
54.965203	1712.884821	19.942042
54.963027	1709.139174	19.947059
55.143071	1720.696943	19.952077
55.055133	1734.707384	19.957095
55.215279	1731.891162	19.962112
55.329027	1742.563067	19.967130
55.513054	1742.661816	19.972147
55.359823	1737.669113	19.977165
54.940192	1739.912323	19.982183
55.384987	1734.924932	19.987200
55.356588	1734.844679	19.992218
55.338148	1761.166986	19.997235
55.898324	1761.690073	20.002253
55.436114	1765.888783	20.007271
56.055924	1758.401906	20.012288
56.153845	1771.033165	20.017306
56.261447	1765.007490	20.022323
56.552074	1750.886858	20.027341
56.098449	1761.704296	20.032359
56.468075	1756.511232	20.037376
56.520176	1754.307784	20.042394
56.203540	1757.683955	20.047411
56.491022	1755.349800	20.052429
56.352883	1753.979436	20.057447
56.836049	1751.341617	20.062464
56.717761	1753.726274	20.067482
56.668670	1751.484463	20.072499
56.908940	1744.884067	20.077517
56.821069	1761.822897	20.082535
56.617618	1752.010499	20.087552
56.783097	1750.212693	20.092570
56.770300	1751.228293	20.097587
57.014058	1748.278538	20.102605
56.539410	1748.976512	20.107623
56.947480	1749.530689	20.112640
56.934542	1752.195542	20.117658
56.796505	1756.416560	20.122675
57.020720	1762.331160	20.127693
57.178273	1777.011235	20.132711
57.357813	1779.443827	20.137728
57.551075	1781.351699	20.142746
57.021579	1777.219327	20.147763
57.273455	1783.674637	20.152781
56.982333	1780.146503	20.157799
57.393843	1775.011853	20.162816
57.488349	1790.904364	20.167834
57.881311	1804.936424	20.172851
58.021234	1805.955087	20.177869
57.994023	1811.733382	20.182887
57.940816	1803.439403	20.187904
58.439035	1809.599995	20.192922
58.251251	1801.420034	20.197939
58.465205	1794.958621	20.202957
58.000849	1778.301521	20.207975
58.347318	1763.198391	20.212992
58.308145	1769.068809	20.218010
58.360465	1783.928915	20.223027
58.579788	1788.642746	20.228045
58.522428	1797.652053	20.233063
58.465077	1796.115157	20.238080
58.753002	1788.807629	20.243098
58.369617	1790.539326	20.248115
58.542322	1794.232517	20.253133
58.534649	1795.941770	20.258151
58.639740	1792.765356	20.263168
58.643595	1786.741890	20.268186
58.651244	1794.121513	20.273203
58.671748	1792.396527	20.278221
58.569941	1796.937545	20.283239
58.762043	1808.104795	20.288256
59.259237	1806.405210	20.293274
58.744321	1818.156076	20.298291
58.843650	1809.666363	20.303309
59.227770	1811.087906	20.308327
59.068179	1813.971938	20.313344
59.374530	1806.355441	20.318362
59.341945	1812.297226	20.323379
59.269931	1801.698455	20.328397
59.080574	1816.647429	20.333415
59.266877	1831.974380	20.338432
59.387999	1834.670988	20.343450
59.423892	1845.536173	20.348467
59.706140	1834.384225	20.353485
59.639642	1836.333541	20.358503
59.606567	1845.252633	20.363520
60.042471	1844.339583	20.368538
60.041089	1857.103105	20.373555
60.406957	1862.245851	20.378573
60.304975	1861.145479	20.383591
60.334366	1857.604808	20.388608
60.519381	1854.458851	20.393626
60.430137	1863.901042	20.398643
60.604962	1856.885050	20.403661
60.508054	1850.011692	20.408679
60.463602	1855.899553	20.413696
60.609678	1847.599326	20.418714
60.488041	1856.649232	20.423731
60.737733	1851.739386	20.428749
60.910133	1856.377147	20.433767
60.622956	1855.160587	20.438784
60.859496	1854.857722	20.443802
60.614914	1859.640906	20.448819
60.337235	1856.323130	20.453837
60.843409	1879.644944	20.458855
60.729188	1879.533230	20.463872
61.146581	1875.232235	20.468890
61.209802	1881.557404	20.473907
61.457610	1879.343582	20.478925
61.243710	1875.619171	20.483943
61.379247	1882.807973	20.488960
61.580101	1867.953660	20.493978
61.486419	1883.959711	20.498995
61.577820	1888.123876	20.504013
61.842839	1904.517807	20.509031
61.676938	1900.201573	20.514048
62.168853	1893.426767	20.519066
62.169838	1899.731933	20.524083
62.377929	1895.936463	20.529101
62.328234	1874.180580	20.534119
62.018667	1871.936211	20.539136
62.360025	1859.960663	20.544154
62.222729	1862.094542	20.549171
62.475764	1860.421205	20.554189
62.075947	1861.981611	20.559207
62.295332	1875.704281	20.564224
62.469367	1881.856768	20.569242
62.223152	1888.472944	20.574259
62.570923	1893.433260	20.579277
62.631678	1895.356394	20.584295
62.518860	1894.074346	20.589312
62.713162	1888.990191	20.594330
62.563192	1895.643190	20.599347
62.774151	1885.110897	20.604365
62.942610	1885.668139	20.609383
62.577342	1887.064950	20.614400
62.817671	1902.249952	20.619418
62.629219	1924.281308	20.624435
63.059260	1909.919727	20.629453
63.073675	1919.815271	20.634471
62.998909	1920.086797	20.639488
63.400540	1921.003472	20.644506
62.963254	1924.752419	20.649523
63.311187	1921.968063	20.654541
63.516120	1945.781598	20.659559
63.609327	1952.635701	20.664576
63.912473	1952.281648	20.669594
63.894324	1957.894713	20.674611
63.857115	1953.765821	20.679629
64.174149	1947.850283	20.684647
63.989052	1949.155061	20.689664
64.384347	1946.908935	20.694682
64.300670	1951.583219	20.699699
64.318556	1935.154770	20.704717
64.237190	1924.358640	20.709735
63.954837	1919.814826	20.714752
64.352318	1932.609220	20.719770
64.380550	1942.156814	20.724787
64.485070	1940.329709	20.729805
64.696023	1938.266472	20.734823
64.717697	1935.408180	20.739840
64.844276	1940.056309	20.744858
64.970743	1934.819194	20.749875
64.451218	1931.344591	20.754893
64.859069	1938.961569	20.759911
64.941509	1931.967533	20.764928
64.617557	1933.477194	20.769946
64.294041	1935.444274	20.774963
64.720166	1944.258256	20.779981
65.213797	1956.921000	20.784999
65.188434	1968.994473	20.790016
65.246106	1970.642136	20.795034
65.172294	1969.946157	20.800051
65.432223	1958.472612	20.805069
65.642091	1958.374166	20.810087
65.263944	1968.742231	20.815104
65.607666	1961.016320	20.820122
65.725350	1962.225295	20.825139
65.499732	1966.831745	20.830157
65.549542	1952.303550	20.835175
65.727901	1982.232709	20.840192
65.802324	1981.322810	20.845210
65.706774	1990.420839	20.850227
65.519291	1987.358973	20.855245
65.864968	1988.958164	20.860263
65.790445	1992.689976	20.865280
65.870292	2009.893440	20.870298
66.166887	2013.726411	20.875315
66.339787	2022.084320	20.880333
66.705605	2012.001510	20.885351
66.347607	2012.106148	20.890368
66.717727	2013.539872	20.895386
66.661502	2008.219200	20.900403
66.856353	2005.979876	20.905421
67.127279	2001.468053	20.910439
67.059751	2004.334120	20.915456
67.008392	2002.652506	20.920474
66.965971	2000.991853	20.925491
66.928692	2006.065175	20.930509
67.242097	1999.592330	20.935527
67.105955	2005.237941	20.940544
67.238050	2006.477212	20.945562
67.410845	2016.911177	20.950579
67.289386	2030.631363	20.955597
67.771434	2029.256713	20.960615
67.856129	2040.073795	20.965632
67.642190	2031.768117	20.970650
67.718715	2028.631820	20.975667
67.572640	2026.504456	20.980685
67.794837	2030.233605	20.985703
67.782146	2029.012922	20.990720
67.686606	2033.305720	20.995738
67.614074	2040.402665	21.000755
67.912660	2032.605055	21.005773
68.329221	2029.112448	21.010791
67.940942	2031.683193	21.015808
68.176913	2021.564394	21.020826
68.083543	2028.952587	21.025843
68.038001	2044.151597	21.030861
68.571355	2052.500629	21.035879
68.540784	2049.483245	21.040896
68.600572	2061.332449	21.045914
68.796014	2057.404385	21.050931
68.752394	2056.602613	21.055949
68.933882	2053.706813	21.060967
68.517706	2059.282666	21.065984
68.659077	2044.236847	21.071002
69.100739	2052.030178	21.076019
68.738635	2053.559160	21.081037
69.163069	2047.557296	21.086055
69.200212	2064.672614	21.091072
69.401341	2072.076635	21.096090
69.529168	2074.360351	21.101107
69.814022	2073.649077	21.106125
69.598809	2065.673523	21.111143
69.470978	2063.830543	21.116160
69.805890	2059.889623	21.121178
69.803459	2064.189061	21.126195
69.354553	2074.665764	21.131213
69.701078	2070.524487	21.136231
69.623924	2074.091001	21.141248
69.918701	2069.834667	21.146266
69.642772	2063.522762	21.151283
69.722659	2067.902668	21.156301
70.181782	2083.716603	21.161319
69.867264	2086.716103	21.166336
70.136363	2104.610407	21.171354
70.146143	2095.514478	21.176371
70.358457	2096.827878	21.181389
70.557793	2093.065702	21.186407
70.377653	2093.712169	21.191424
70.846173	2112.527432	21.196442
71.073362	2120.190949	21.201459
70.724736	2119.168012	21.206477
70.996543	2118.118334	21.211495
71.264935	2118.253119	21.216512
71.176277	2114.031519	21.221530
71.523771	2109.704632	21.226547
71.405754	2108.470278	21.231565
71.572634	2100.741295	21.236583
71.604903	2098.428480	21.241600
71.442426	2082.845512	21.246618
71.467564	2088.624691	21.251635
71.469589	2098.302709	21.256653
71.502237	2103.395194	21.261671
71.457473	2101.613655	21.266688
71.855057	2102.309353	21.271706
72.048396	2094.389370	21.276723
71.862198	2101.818953	21.281741
72.026289	2094.645177	21.286759
71.774207	2101.671876	21.291776
71.796549	2100.514680	21.296794
72.297467	2102.168103	21.301811
71.971806	2097.627863	21.306829
72.305911	2095.075302	21.311847
71.938982	2115.236811	21.316864
72.201473	2132.295600	21.321882
72.290961	2127.714960	21.326899
72.142601	2142.291697	21.331917
72.294791	2142.297293	21.336935
72.525018	2142.007280	21.341952
72.590918	2146.834422	21.346970
72.659520	2153.150936	21.351987
72.683409	2156.833421	21.357005
72.851683	2146.993476	21.362023
72.933278	2149.745112	21.367040
72.883832	2148.832090	21.372058
72.954854	2156.430929	21.377075
73.156180	2169.289495	21.382093
73.119320	2185.694337	21.387111
73.894868	2182.854095	21.392128
73.522219	2182.950528	21.397146
73.547926	2178.292242	21.402163
73.386685	2174.397616	21.407181
73.458996	2175.894840	21.412199
73.814805	2174.776129	21.417216
73.688854	2179.018095	21.422234
73.834543	2180.097249	21.427251
74.084989	2198.492800	21.432269
74.450108	2199.708859	21.437287
74.464153	2198.995567	21.442304
74.202745	2194.291504	21.447322
74.634409	2199.220312	21.452339
74.517263	2195.546735	21.457357
74.443452	2189.734011	21.462375
74.456411	2192.899396	21.467392
74.505490	2194.963483	21.472410
74.662808	2186.405299	21.477427
74.747577	2193.446346	21.482445
75.095102	2196.264592	21.487463
75.139477	2196.519151	21.492480
74.878997	2188.810094	21.497498
75.151044	2190.759701	21.502515
74.920257	2193.762680	21.507533
75.310867	2206.474184	21.512551
75.278529	2224.007497	21.517568
75.203102	2218.887578	21.522586
75.555418	2227.056830	21.527603
75.480030	2228.899393	21.532621
75.933284	2224.264401	21.537639
75.691086	2222.050952	21.542656
75.579373	2227.381563	21.547674
75.899229	2222.969060	21.552691
75.687624	2220.847006	21.557709
75.378702	2226.365000	21.562727
75.818169	2230.807073	21.567744
75.947532	2238.751425	21.572762
76.367194	2236.016953	21.577779
76.167043	2247.821145	21.582797
76.286240	2242.918217	21.587815
76.467967	2243.184681	21.592832
76.242454	2247.451024	21.597850
76.591533	2238.025199	21.602867
76.401174	2263.241736	21.607885
76.779665	2271.019259	21.612903
77.018625	2269.797443	21.617920
76.934327	2267.423191	21.622938
77.186811	2269.650862	21.627955
76.972791	2266.716568	21.632973
77.357547	2267.556924	21.637991
77.259463	2271.865563	21.643008
77.161305	2267.509661	21.648026
77.108154	2265.824378	21.653043
77.435493	2267.792399	21.658061
77.237117	2274.193327	21.663079
77.489313	2261.536535	21.668096
77.199312	2284.187208	21.673114
77.453554	2286.305924	21.678131
77.360450	2287.378953	21.683149
77.664682	2291.481608	21.688167
77.702972	2283.719098	21.693184
77.641257	2302.031413	21.698202
78.321824	2304.277190	21.703219
78.198762	2309.562855	21.708237
78.042910	2315.692573	21.713255
78.317112	2315.660250	21.718272
78.272990	2314.339231	21.723290
78.443623	2318.808125	21.728307
78.302175	2314.764116	21.733325
78.544228	2315.881264	21.738343
78.860655	2314.117460	21.743360
78.722181	2339.083391	21.748378
79.001016	2332.832285	21.753395
78.784413	2337.159384	21.758413
79.101307	2337.562927	21.763431
79.041798	2338.965058	21.768448
79.191076	2332.859032	21.773466
79.242275	2331.872246	21.778483
79.458035	2336.120277	21.783501
79.425574	2335.804067	21.788519
79.690167	2333.896474	21.793536
79.278471	2340.465038	21.798554
80.051165	2342.469572	21.803571
79.449608	2351.811442	21.808589
79.616972	2355.808424	21.813607
80.215414	2356.411032	21.818624
80.190532	2362.327342	21.823642
80.188210	2350.820942	21.828659
80.276532	2359.345014	21.833677
80.053311	2355.822433	21.838695
80.529304	2357.131176	21.843712
80.297304	2363.717244	21.848730
80.289405	2356.669861	21.853747
80.557846	2362.340350	21.858765
80.602059	2374.811694	21.863783
80.680757	2368.231488	21.868800
80.421845	2375.692533	21.873818
81.021993	2369.404354	21.878835
80.976398	2373.505108	21.883853
80.425770	2381.010912	21.888871
80.861630	2376.414978	21.893888
81.019556	2398.226258	21.898906
81.787093	2399.597369	21.903923
82.044418	2395.138870	21.908941
81.657384	2402.797528	21.913959
81.925189	2393.793749	21.918976
81.654716	2396.901375	21.923994
82.015844	2393.176122	21.929011
82.049731	2393.203275	21.934029
82.239010	2394.167347	21.939047
82.353018	2382.288495	21.944064
82.063427	2372.066322	21.949082
82.271608	2370.566115	21.954099
82.298950	2383.222552	21.959117
82.389193	2385.646797	21.964135
82.398527	2387.442673	21.969152
82.548508	2395.279355	21.974170
82.282172	2391.478457	21.979187
82.483367	2385.878407	21.984205
82.151757	2392.077415	21.989223
82.173699	2385.145163	21.994240
82.383583	2404.845774	21.999258
82.664734	2410.256289	22.004275
82.731185	2417.604424	22.009293
82.654802	2422.068181	22.014311
82.792707	2416.599078	22.019328
82.914974	2443.602037	22.024346
83.478308	2447.298035	22.029363
83.134226	2440.788587	22.034381
83.214580	2455.960853	22.039399
83.528904	2451.014528	22.044416
83.524736	2456.669161	22.049434
83.590778	2441.973245	22.054451
83.860263	2451.336317	22.059469
83.832174	2479.826914	22.064487
84.274408	2471.332430	22.069504
84.060448	2467.655525	22.074522
84.175979	2470.710671	22.079539
84.434493	2466.052731	22.084557
84.247420	2466.646026	22.089575
84.559196	2469.073370	22.094592
84.502423	2464.892854	22.099610
84.627818	2460.343182	22.104627
84.773482	2451.580472	22.109645
84.746510	2466.567752	22.114663
84.593590	2450.528870	22.119680
84.706774	2470.068006	22.124698
85.029677	2488.677509	22.129715
84.897485	2491.349635	22.134733
84.948157	2491.802380	22.139751
85.005148	2492.097771	22.144768
84.980779	2487.978817	22.149786
85.138557	2484.164764	22.154803
85.826934	2492.658852	22.159821
85.455207	2505.522416	22.164839
85.964761	2494.312677	22.169856
85.884310	2498.392461	22.174874
85.776704	2501.161311	22.179891
86.413973	2501.064938	22.184909
85.996792	2505.226463	22.189927
86.292046	2498.854456	22.194944
86.315622	2500.619245	22.199962
86.424538	2498.855918	22.204979
86.583416	2496.408296	22.209997
86.135980	2500.123228	22.215015
86.591836	2497.972517	22.220032
86.645885	2515.974561	22.225050
86.739307	2521.405173	22.230067
87.000960	2537.056981	22.235085
86.685624	2532.150313	22.240103
86.981383	2532.676660	22.245120
87.012845	2528.559081	22.250138
87.098475	2529.835618	22.255155
87.017369	2527.566316	22.260173
87.150990	2532.424100	22.265191
87.376031	2544.012833	22.270208
87.579660	2555.165327	22.275226
87.487087	2545.210437	22.280243
87.673396	2550.682771	22.285261
87.438432	2562.063410	22.290279
87.796415	2556.579081	22.295296
87.563871	2555.354598	22.300314
87.870128	2565.354604	22.305331
88.518529	2569.792894	22.310349
88.223204	2584.841256	22.315367
88.343727	2578.741076	22.320384
88.507591	2584.862061	22.325402
88.255740	2583.042308	22.330419
88.521521	2578.715436	22.335437
88.387890	2579.094362	22.340455
88.480018	2577.390897	22.345472
88.481948	2580.670005	22.350490
88.820226	2595.786711	22.355507
89.372217	2594.352401	22.360525
88.897293	2607.781596	22.365543
89.070638	2602.731392	22.370560
89.210103	2597.141487	22.375578
89.304463	2601.472295	22.380595
89.633863	2596.684462	22.385613
89.407345	2593.189933	22.390631
89.251438	2592.842972	22.395648
89.471142	2601.508820	22.400666
89.326280	2627.681861	22.405683
89.828285	2621.701191	22.410701
89.793771	2624.653250	22.415719
89.910321	2623.296153	22.420736
89.917501	2626.122009	22.425754
89.740440	2635.001216	22.430771
90.243632	2641.748763	22.435789
89.906660	2650.463104	22.440807
90.202107	2641.095134	22.445824
90.477943	2638.456459	22.450842
90.482798	2667.790033	22.455859
90.887060	2671.364382	22.460877
90.869369	2682.184689	22.465895
91.049096	2688.219224	22.470912
91.207491	2686.191367	22.475930
90.979910	2675.364589	22.480947
91.368983	2675.778241	22.485965
91.532204	2688.145874	22.490983
91.594534	2674.131505	22.496000
91.749874	2674.019250	22.501018
91.360129	2680.165393	22.506035
91.741216	2670.333194	22.511053
91.488886	2687.268762	22.516071
91.921315	2696.214032	22.521088
92.059449	2694.239138	22.526106
91.950049	2700.358165	22.531123
92.163781	2697.807328	22.536141
92.245432	2696.976119	22.541159
92.478670	2690.410745	22.546176
92.547455	2692.952378	22.551194
92.471473	2695.524674	22.556211
92.660317	2691.098297	22.561229
92.488935	2714.193766	22.566247
92.602180	2725.828311	22.571264
92.962177	2723.373734	22.576282
92.949635	2720.327642	22.581299
93.050675	2724.277822	22.586317
93.079753	2721.699283	22.591335
93.486632	2721.477659	22.596352
93.552473	2714.752968	22.601370
93.195892	2718.530079	22.606387
93.855106	2728.802484	22.611405
93.736759	2736.664474	22.616423
93.825427	2744.197681	22.621440
94.193758	2749.869492	22.626458
94.022514	2751.045653	22.631475
94.271031	2750.862848	22.636493
93.993588	2744.388304	22.641511
94.058251	2739.291085	22.646528
94.222485	2735.123514	22.651546
94.073252	2736.150744	22.656563
93.974490	2742.909018	22.661581
94.430974	2761.706590	22.666599
94.318180	2763.228613	22.671616
94.607913	2768.436637	22.676634
94.331422	2771.692193	22.681651
94.899159	2773.404321	22.686669
95.038036	2781.800166	22.691687
95.107619	2780.581551	22.696704
95.303841	2785.571580	22.701722
95.425350	2792.669419	22.706739
95.599451	2789.835737	22.711757
95.640246	2779.719628	22.716775
95.276484	2786.708820	22.721792
95.746791	2784.727740	22.726810
95.872192	2787.046612	22.731827
96.130048	2779.261677	22.736845
95.989115	2778.404713	22.741863
96.386639	2778.798858	22.746880
96.581531	2781.657054	22.751898
96.072738	2775.820059	22.756915
96.240890	2775.776948	22.761933
95.998594	2786.756572	22.766951
96.046592	2805.792709	22.771968
96.213199	2803.619371	22.776986
95.930947	2816.399866	22.782003
96.251499	2827.909212	22.787021
96.672804	2837.924995	22.792039
96.705287	2844.872230	22.797056
97.271300	2850.964929	22.802074
97.317435	2862.128758	22.807091
97.711923	2856.274866	22.812109
97.967551	2861.766937	22.817127
98.072875	2861.306240	22.822144
98.040757	2847.375863	22.827162
97.739202	2840.233169	22.832179
98.052021	2845.268879	22.837197
98.119376	2855.566916	22.842215
97.966773	2862.173907	22.847232
98.516091	2850.788420	22.852250
98.233379	2860.748326	22.857267
98.237737	2864.498391	22.862285
98.318920	2862.145866	22.867303
98.207896	2852.681669	22.872320
98.454537	2852.318057	22.877338
98.263043	2861.184032	22.882355
98.450130	2872.519430	22.887373
98.734666	2883.057928	22.892391
98.566784	2876.260045	22.897408
99.036892	2879.860159	22.902426
99.143781	2901.291587	22.907443
99.389266	2902.043613	22.912461
99.176212	2901.912030	22.917479
99.211668	2901.483374	22.922496
99.515654	2906.178412	22.927514
99.037536	2910.196968	22.932531
99.487294	2916.220745	22.937549
99.717152	2929.476433	22.942567
99.745772	2931.583378	22.947584
99.914961	2924.547367	22.952602
100.136105	2949.409846	22.957619
100.387954	2956.961813	22.962637
100.469148	2948.689068	22.967655
100.763997	2954.779850	22.972672
100.885974	2944.733271	22.977690
100.880357	2956.094730	22.982707
100.907482	2948.495957	22.987725
100.981941	2943.403742	22.992743
100.955249	2938.490496	22.997760
101.123499	2945.647601	23.002778
101.022553	2946.930652	23.007795
101.142016	2941.970369	23.012813
101.733072	2964.094623	23.017831
101.498590	2966.415622	23.022848
101.783188	2968.567206	23.027866
101.746164	2968.613976	23.032883
101.847687	2966.573057	23.037901
101.739047	2966.901786	23.042919
101.807760	2973.709604	23.047936
101.846283	2968.633175	23.052954
101.815395	2980.133886	23.057971
102.092918	2981.194420	23.062989
102.089786	3000.763324	23.068007
102.156923	2997.188190	23.073024
102.310622	2997.981012	23.078042
102.228025	3001.790392	23.083059
102.831250	3018.092888	23.088077
102.956981	3027.422231	23.093095
103.002792	3036.525419	23.098112
103.131598	3034.969389	23.103130
103.197254	3033.798259	23.108147
102.983050	3031.093397	23.113165
103.474824	3029.341433	23.118183
103.129546	3044.375669	23.123200
103.331572	3052.717894	23.128218
103.385774	3057.249197	23.133235
103.695349	3060.032152	23.138253
103.704789	3057.679271	23.143271
103.617431	3071.573088	23.148288
104.298839	3067.436743	23.153306
104.344113	3078.791440	23.158323
104.531707	3078.992771	23.163341
104.871049	3072.754585	23.168359
104.790952	3070.538585	23.173376
104.912771	3074.303507	23.178394
105.067832	3080.060755	23.183411
104.569483	3080.228792	23.188429
104.845364	3075.163821	23.193447
104.760135	3097.964857	23.198464
105.308167	3099.894481	23.203482
105.141476	3110.117646	23.208499
105.142749	3111.360161	23.213517
105.789753	3101.573833	23.218535
105.547027	3110.949267	23.223552
105.524427	3120.426858	23.228570
105.631301	3127.043367	23.233587
105.468172	3139.851257	23.238605
105.900655	3132.964886	23.243623
105.860820	3147.167076	23.248640
106.349101	3154.711493	23.253658
106.235547	3153.860606	23.258675
106.631126	3157.080172	23.263693
106.925169	3142.221426	23.268711
106.851799	3149.127262	23.273728
107.199161	3153.410822	23.278746
107.254217	3154.893280	23.283763
107.231890	3151.347098	23.288781
107.085265	3144.572353	23.293799
106.985325	3158.852622	23.298816
107.095683	3144.707425	23.303834
107.573310	3160.737137	23.308851
107.421446	3173.234496	23.313869
108.022560	3174.087122	23.318887
107.929648	3175.802370	23.323904
107.610580	3166.273992	23.328922
107.550051	3169.048946	23.333939
107.801025	3177.305173	23.338957
107.777592	3188.044883	23.343975
107.901046	3190.772842	23.348992
108.329802	3189.063976	23.354010
108.829204	3200.202219	23.359027
108.588913	3202.691555	23.364045
108.774863	3195.653434	23.369063
108.903813	3198.035961	23.374080
109.143982	3188.186609	23.379098
109.336498	3190.516480	23.384115
109.114373	3193.734378	23.389133
109.035890	3194.019926	23.394151
109.007581	3223.000942	23.399168
109.376416	3222.054828	23.404186
109.312487	3225.029588	23.409203
109.084068	3224.854477	23.414221
109.816030	3231.154129	23.419239
109.635029	3254.750465	23.424256
109.557068	3251.530041	23.429274
109.764482	3252.200585	23.434291
109.708526	3266.721728	23.439309
110.322499	3267.100920	23.444327
110.311915	3277.367253	23.449344
110.346622	3275.362950	23.454362
110.621643	3264.591145	23.459379
110.508387	3286.272565	23.464397
110.786791	3286.818352	23.469415
110.927866	3295.895288	23.474432
111.181864	3296.544734	23.479450
111.673640	3289.398844	23.484467
111.517777	3295.498628	23.489485
111.508245	3289.644532	23.494503
111.347700	3296.293970	23.499520
111.724265	3309.982829	23.504538
111.789165	3315.867703	23.509555
111.901953	3314.965946	23.514573
112.072340	3319.701341	23.519591
112.286980	3319.963166	23.524608
112.153379	3328.250072	23.529626
112.815361	3319.915622	23.534643
112.435091	3314.506799	23.539661
112.387626	3318.237203	23.544679
112.288993	3335.959139	23.549696
112.763321	3347.910786	23.554714
112.923956	3341.881236	23.559731
112.492660	3344.502228	23.564749
112.755610	3356.653858	23.569767
113.386783	3371.058184	23.574784
113.092284	3381.118806	23.579802
113.807410	3371.767541	23.584819
113.654805	3374.204980	23.589837
113.852282	3365.196146	23.594855
113.800873	3368.674429	23.599872
113.868238	3384.396664	23.604890
114.086596	3387.010508	23.609907
114.029038	3401.562360	23.614925
114.533763	3395.082861	23.619943
114.253997	3392.876248	23.624960
114.434217	3390.060346	23.629978
114.549414	3386.628365	23.634995
114.459504	3405.180526	23.640013
114.642934	3416.177910	23.645031
114.621707	3420.062280	23.650048
114.998286	3421.927015	23.655066
115.175975	3423.586069	23.660083
115.414058	3441.813465	23.665101
115.705407	3447.341568	23.670119
115.824806	3449.996220	23.675136
115.677219	3452.012316	23.680154
115.974785	3439.499837	23.685171
115.759937	3452.112978	23.690189
115.760070	3441.512563	23.695207
116.049407	3449.451129	23.700224
115.883121	3447.233201	23.705242
116.231633	3447.248428	23.710259
116.165916	3465.859656	23.715277
116.515300	3470.939917	23.720295
116.567595	3468.790140	23.725312
116.723458	3466.803159	23.730330
116.822348	3465.411902	23.735347
116.705007	3483.539119	23.740365
117.091183	3489.867384	23.745383
117.061553	3500.895771	23.750400
117.028780	3495.294296	23.755418
117.254438	3487.651760	23.760435
117.292668	3509.526545	23.765453
117.384938	3517.527304	23.770471
117.678303	3517.611905	23.775488
117.778717	3515.829005	23.780506
118.392432	3517.280822	23.785523
118.263816	3521.199928	23.790541
118.122093	3531.729509	23.795559
118.332090	3538.718932	23.800576
118.512447	3544.482008	23.805594
119.045080	3544.428952	23.810611
119.087436	3541.852410	23.815629
119.261603	3535.762271	23.820647
119.391197	3541.173469	23.825664
119.328113	3540.149617	23.830682
119.219021	3540.507176	23.835699
119.194430	3539.271019	23.840717
119.293994	3553.782430	23.845735
119.733819	3562.486790	23.850752
119.403241	3562.701863	23.855770
119.912311	3559.082965	23.860787
119.609724	3566.853810	23.865805
120.077421	3582.339075	23.870823
120.206390	3588.697759	23.875840
120.510060	3597.122673	23.880858
120.526602	3587.362071	23.885875
120.344344	3599.917565	23.890893
120.529492	3593.794873	23.895911
120.721608	3610.320408	23.900928
120.797507	3618.385355	23.905946
121.137747	3619.294982	23.910963
121.085627	3625.604125	23.915981
121.304960	3618.294506	23.920999
121.381056	3627.976959	23.926016
121.398179	3642.879710	23.931034
121.800367	3639.652161	23.936051
122.050954	3657.147328	23.941069
121.858423	3638.330735	23.946087
122.198573	3642.572313	23.951104
122.104902	3646.223426	23.956122
122.576854	3649.046150	23.961139
122.444531	3669.434628	23.966157
122.659243	3657.792895	23.971175
122.512247	3659.065120	23.976192
122.761978	3663.491776	23.981210
123.089097	3653.157596	23.986227
123.195128	3656.438595	23.991245
123.347055	3653.559211	23.996263
123.492643	3652.941018	24.001280
122.787999	3681.745845	24.006298
123.390932	3681.362604	24.011315
123.630454	3684.497475	24.016333
123.403152	3686.589800	24.021351
123.595205	3699.704351	24.026368
123.696278	3711.935036	24.031386
124.007122	3707.742935	24.036403
124.024558	3723.450151	24.041421
123.837078	3719.165331	24.046439
124.032861	3735.888844	24.051456
124.110323	3743.184593	24.056474
124.568609	3745.010247	24.061491
124.650422	3750.981868	24.066509
124.975731	3764.309089	24.071527
125.056675	3768.243962	24.076544
125.284602	3770.910232	24.081562
125.497779	3771.179790	24.086579
125.600993	3771.386834	24.091597
125.705626	3763.218062	24.096615
125.893601	3763.357915	24.101632
125.863819	3757.212861	24.106650
125.982168	3770.090034	24.111667
126.015273	3780.895209	24.116685
126.131449	3794.031853	24.121703
126.599408	3791.905746	24.126720
126.478597	3793.730025	24.131738
126.825951	3790.743053	24.136755
126.620086	3789.406162	24.141773
126.558194	3805.409704	24.146791
127.017792	3815.795031	24.151808
127.052922	3819.380758	24.156826
127.165981	3818.562797	24.161843
127.133637	3820.290137	24.166861
127.277779	3836.235975	24.171879
127.726515	3838.335701	24.176896
127.161135	3844.335363	24.181914
127.722010	3842.083221	24.186931
127.535143	3861.131571	24.191949
127.758204	3868.301289	24.196967
127.871676	3864.622998	24.201984
128.406776	3884.824080	24.207002
128.722069	3888.274055	24.212019
128.759775	3897.695274	24.217037
128.811599	3899.296466	24.222055
128.780264	3888.639533	24.227072
128.920486	3900.149604	24.232090
129.142547	3904.526965	24.237107
129.546588	3917.517219	24.242125
129.191405	3920.817537	24.247143
129.959855	3917.786026	24.252160
129.591616	3935.118957	24.257178
129.793003	3921.330093	24.262195
129.840014	3935.811970	24.267213
130.217109	3944.131989	24.272231
130.350880	3942.908170	24.277248
130.038702	3944.907478	24.282266
130.336160	3948.083212	24.287283
130.383325	3950.836536	24.292301
130.238521	3962.986058	24.297319
130.819534	3967.436312	24.302336
131.048700	3981.009987	24.307354
130.951696	3979.006137	24.312371
130.998819	3990.445848	24.317389
131.204015	4005.054380	24.322407
131.755931	3996.121564	24.327424
131.400774	4006.878167	24.332442
131.936095	3992.277144	24.337459
132.304069	3994.785994	24.342477
131.876053	4016.470527	24.347495
132.281881	4013.830582	24.352512
132.221585	4021.666277	24.357530
132.660074	4032.766378	24.362547
132.349859	4029.070779	24.367565
132.485740	4028.165552	24.372583
132.811488	4038.296767	24.377600
133.062231	4052.229193	24.382618
133.281721	4053.326188	24.387635
133.200808	4055.199806	24.392653
133.415324	4056.170046	24.397671
133.914260	4050.086579	24.402688
133.748595	4050.411776	24.407706
133.526590	4045.098166	24.412723
133.420280	4044.101519	24.417741
133.551914	4067.511863	24.422759
133.817720	4067.085990	24.427776
133.655452	4079.348747	24.432794
133.774204	4081.724829	24.437811
134.017677	4099.332317	24.442829
134.031434	4115.346883	24.447847
134.373721	4114.952449	24.452864
134.542055	4125.067254	24.457882
134.685217	4128.459154	24.462899
135.143698	4148.553558	24.467917
135.232980	4156.308642	24.472935
135.754534	4153.962951	24.477952
135.590313	4160.559810	24.482970
135.813409	4150.929254	24.487987
136.222307	4163.450329	24.493005
136.131673	4175.100414	24.498023
136.569714	4170.450841	24.503040
136.700273	4180.167933	24.508058
136.603239	4169.424031	24.513075
137.032590	4168.520612	24.518093
136.695913	4169.623066	24.523111
137.051909	4167.943472	24.528128
137.013504	4167.036378	24.533146
137.405039	4173.300247	24.538163
137.436406	4180.196283	24.543181
137.177746	4198.000419	24.548199
137.528699	4187.519401	24.553216
137.569807	4196.260597	24.558234
137.662400	4204.908219	24.563251
137.768284	4212.736973	24.568269
137.713455	4223.622771	24.573287
137.904423	4218.128901	24.578304
138.437417	4241.731367	24.583322
138.471823	4249.610563	24.588339
138.604916	4254.851716	24.593357
138.521449	4267.616622	24.598375
138.966071	4259.071565	24.603392
138.757409	4266.898082	24.608410
138.763037	4280.700397	24.613427
139.263570	4284.197759	24.618445
139.315829	4288.497023	24.623463
139.987822	4300.759652	24.628480
139.813563	4308.189875	24.633498
140.277038	4302.377584	24.638515
140.675992	4307.309338	24.643533
140.697339	4310.548186	24.648551
140.691837	4300.341106	24.653568
141.041434	4294.320860	24.658586
140.888232	4301.776732	24.663603
141.166952	4295.213005	24.668621
141.113957	4297.251350	24.673639
141.181975	4292.203867	24.678656
141.128360	4299.651914	24.683674
141.076821	4293.257846	24.688691
141.433612	4311.463454	24.693709
141.370926	4330.899365	24.698727
141.252601	4319.199662	24.703744
141.770073	4328.655117	24.708762
141.845167	4349.929985	24.713779
142.147434	4352.078842	24.718797
141.924405	4360.911898	24.723815
142.427299	4353.021041	24.728832
142.190395	4364.834878	24.733850
142.449451	4368.110775	24.738867
142.710896	4381.178576	24.743885
142.277193	4385.733944	24.748903
142.562004	4394.055307	24.753920
142.831713	4415.198812	24.758938
142.892645	4420.889842	24.763955
143.166951	4427.564632	24.768973
143.486685	4440.933126	24.773991
143.719784	4434.683249	24.779008
143.761492	4442.677890	24.784026
144.122259	4469.397180	24.789043
144.088819	4463.040211	24.794061
144.250412	4472.049067	24.799079
144.644342	4470.717558	24.804096
144.813624	4473.824841	24.809114
145.142882	4488.574732	24.814131
145.140145	4485.034455	24.819149
145.400441	4485.799470	24.824167
145.821018	4482.259203	24.829184
146.052684	4478.024881	24.834202
145.717098	4482.235625	24.839219
146.147632	4477.979404	24.844237
145.953102	4485.457957	24.849255
145.889741	4475.258767	24.854272
146.031703	4481.920050	24.859290
146.020025	4499.910451	24.864307
146.267367	4507.052817	24.869325
146.352807	4508.183853	24.874343
146.657409	4517.984172	24.879360
146.809769	4529.009928	24.884378
146.760917	4527.801336	24.889395
146.843273	4524.665152	24.894413
147.229602	4555.616587	24.899431
147.499894	4564.393287	24.904448
147.655351	4561.626955	24.909466
147.741758	4569.915892	24.914483
147.902094	4577.002603	24.919501
148.226448	4580.669385	24.924519
148.631306	4590.258627	24.929536
148.532654	4584.189624	24.934554
148.123390	4591.931380	24.939571
148.651077	4594.722609	24.944589
148.501956	4607.961741	24.949607
148.428062	4606.853371	24.954624
149.011052	4619.900427	24.959642
149.048646	4631.895047	24.964659
149.279189	4636.234982	24.969677
149.307405	4644.076811	24.974695
149.618831	4663.025915	24.979712
150.191958	4677.930136	24.984730
149.839888	4673.733337	24.989747
150.518157	4675.114339	24.994765
150.249020	4676.191468	24.999783
150.521297	4691.228204	25.004800
150.665750	4693.164605	25.009818
150.791592	4698.548868	25.014835
150.889747	4693.352932	25.019853
150.950210	4697.681665	25.024871
151.113256	4717.751682	25.029888
151.337814	4718.869939	25.034906
151.384425	4728.061003	25.039923
151.669768	4723.464115	25.044941
151.808500	4742.373388	25.049959
151.687491	4747.822163	25.054976
152.222433	4747.941601	25.059994
151.924564	4752.629733	25.065011
152.231678	4744.428506	25.070029
152.533490	4762.142852	25.075047
152.713291	4778.544862	25.080064
152.960683	4776.844596	25.085082
152.764533	4777.982891	25.090099
153.019601	4775.351244	25.095117
153.323817	4792.939216	25.100135
153.411424	4792.230167	25.105152
153.899306	4787.176020	25.110170
153.749943	4791.033901	25.115187
153.868521	4783.158416	25.120205
154.040204	4804.198966	25.125223
154.053722	4818.183949	25.130240
154.597676	4818.393254	25.135258
154.260778	4822.969733	25.140275
154.574342	4822.566652	25.145293
154.738218	4840.106243	25.150311
155.088215	4856.836138	25.155328
155.016092	4849.367073	25.160346
155.453015	4853.668964	25.165363
155.577493	4858.252553	25.170381
155.269318	4880.622516	25.175399
155.658549	4882.298685	25.180416
156.025143	4871.807538	25.185434
156.140442	4876.406828	25.190451
156.350108	4889.719897	25.195469
156.435295	4893.797294	25.200487
156.290516	4893.899317	25.205504
156.776043	4894.982258	25.210522
156.871503	4920.700350	25.215539
156.839899	4918.583168	25.220557
156.891212	4925.603028	25.225575
156.863899	4936.944704	25.230592
157.464144	4943.532676	25.235610
157.182573	4950.339096	25.240627
157.839969	4963.589129	25.245645
157.978267	4973.423567	25.250663
157.748126	4981.663531	25.255680
158.419932	4977.556253	25.260698
158.436161	5003.881427	25.265715
158.791933	5010.276779	25.270733
158.729292	5007.759910	25.275751
158.701317	5017.389568	25.280768
159.123014	5017.949111	25.285786
158.981942	5043.249768	25.290803
159.418530	5041.848146	25.295821
159.745103	5039.792149	25.300839
159.807290	5052.053155	25.305856
160.337387	5063.386912	25.310874
159.958392	5064.983153	25.315891
160.099043	5058.160017	25.320909
160.294361	5072.781417	25.325927
160.283527	5082.308255	25.330944
160.756498	5091.573860	25.335962
160.595365	5092.817429	25.340979
160.586831	5095.026508	25.345997
161.070361	5119.752124	25.351015
161.424310	5115.503689	25.356032
161.261568	5124.133446	25.361050
161.527439	5140.122281	25.366067
161.808260	5151.025609	25.371085
162.102561	5145.657650	25.376103
162.190917	5149.089561	25.381120
162.489616	5159.574093	25.386138
162.488405	5173.681542	25.391155
162.664910	5176.252214	25.396173
162.932648	5171.691191	25.401191
162.514384	5178.963747	25.406208
163.459596	5188.585974	25.411226
163.197486	5199.424066	25.416243
163.412859	5198.834824	25.421261
163.577461	5202.514814	25.426279
163.519287	5198.496040	25.431296
163.971536	5216.657756	25.436314
163.953549	5226.323692	25.441331
163.887521	5227.019907	25.446349
164.518555	5226.438246	25.451367
164.169613	5244.284497	25.456384
164.773671	5251.522515	25.461402
164.700378	5267.696794	25.466419
164.842184	5261.206528	25.471437
164.949403	5279.175772	25.476455
165.057146	5295.552446	25.481472
165.420646	5293.134314	25.486490
165.210768	5318.084512	25.491507
165.577911	5320.366106	25.496525
165.882615	5326.391999	25.501543
165.968908	5345.887194	25.506560
166.184096	5340.473986	25.511578
166.130316	5348.480957	25.516595
166.421741	5360.255325	25.521613
167.051039	5363.277966	25.526631
167.020442	5375.760934	25.531648
167.640878	5374.487942	25.536666
167.577033	5398.223251	25.541683
167.702497	5393.342328	25.546701
168.135541	5397.024390	25.551719
167.890655	5404.751141	25.556736
168.453488	5398.779450	25.561754
168.335601	5404.271250	25.566771
168.351182	5415.772351	25.571789
168.596933	5427.292063	25.576807
168.611027	5427.473324	25.581824
168.877719	5437.764866	25.586842
169.065508	5449.757296	25.591859
169.240925	5450.312736	25.596877
169.278511	5457.856495	25.601895
169.249047	5471.338023	25.606912
169.640778	5487.478858	25.611930
169.882862	5485.076072	25.616947
169.904272	5497.486731	25.621965
170.470442	5507.708263	25.626983
170.310824	5517.979860	25.632000
170.361747	5516.653861	25.637018
170.709580	5530.006031	25.642035
170.935552	5539.401792	25.647053
171.213305	5544.757258	25.652071
171.063516	5555.306063	25.657088
171.422906	5562.966719	25.662106
171.575270	5577.854821	25.667123
171.412985	5579.071051	25.672141
171.850706	5586.380869	25.677159
171.849812	5601.128181	25.682176
171.901723	5603.735302	25.687194
172.735678	5626.788328	25.692212
172.655578	5632.830788	25.697229
173.088364	5630.216048	25.702247
172.723921	5643.735852	25.707264
172.929776	5653.912378	25.712282
173.522924	5659.525199	25.717300
173.473424	5663.757412	25.722317
173.855530	5671.501784	25.727335
174.072776	5686.619467	25.732352
174.188211	5687.838561	25.737370
174.299542	5693.039692	25.742388
174.277557	5686.882748	25.747405
175.161893	5678.813099	25.752423
174.671508	5698.219899	25.757440
174.948849	5713.471792	25.762458
174.745739	5720.485294	25.767476
174.874223	5713.591431	25.772493
175.507407	5721.953490	25.777511
175.868678	5738.276051	25.782528
175.549069	5739.590011	25.787546
175.634511	5740.580942	25.792564
175.834156	5763.526523	25.797581
176.167963	5767.485015	25.802599
175.969528	5784.182247	25.807616
176.524911	5786.825767	25.812634
176.678387	5784.066640	25.817652
176.533667	5794.913271	25.822669
176.923046	5810.013602	25.827687
176.916641	5820.972822	25.832704
176.908296	5828.803177	25.837722
177.208061	5839.150153	25.842740
177.566685	5845.117701	25.847757
178.187659	5860.654673	25.852775
178.110907	5888.290767	25.857792
178.195182	5878.596294	25.862810
178.657641	5901.312690	25.867828
178.785946	5910.024648	25.872845
179.079771	5906.700384	25.877863
179.196165	5910.463345	25.882880
179.513709	5925.498493	25.887898
179.765075	5934.924154	25.892916
179.685317	5942.679749	25.897933
179.772159	5931.811265	25.902951
179.939435	5950.628261	25.907968
179.954409	5962.572503	25.912986
179.987960	5973.199926	25.918004
180.393944	5994.136328	25.923021
180.962153	5995.413598	25.928039
180.641722	6001.790556	25.933056
181.223267	6015.762901	25.938074
181.444135	6025.088123	25.943092
181.141385	6030.386270	25.948109
181.714531	6043.191982	25.953127
181.872658	6053.196302	25.958144
182.077785	6058.586021	25.963162
182.461671	6060.947655	25.968180
182.436349	6084.759529	25.973197
182.441515	6081.540513	25.978215
182.818499	6086.696221	25.983232
182.910431	6094.149372	25.988250
183.213061	6107.518967	25.993268
183.448926	6115.684734	25.998285
183.672752	6113.825979	26.003303
183.602101	6127.903243	26.008320
183.546907	6138.841617	26.013338
183.811434	6136.481490	26.018356
183.984457	6156.019248	26.023373
184.441513	6164.747810	26.028391
184.435434	6181.282081	26.033408
184.741747	6188.596607	26.038426
185.071601	6202.404425	26.043444
184.885942	6213.782683	26.048461
185.316328	6215.491571	26.053479
185.680473	6231.007629	26.058496
185.599220	6238.947922	26.063514
185.987099	6233.675164	26.068532
186.027663	6256.037380	26.073549
186.503157	6243.865389	26.078567
186.420412	6254.544547	26.083584
186.619910	6248.987128	26.088602
186.938426	6263.050495	26.093620
186.543572	6276.606587	26.098637
186.995575	6278.787636	26.103655
187.309832	6292.758006	26.108672
187.276666	6303.699148	26.113690
187.515931	6314.070630	26.118708
187.650947	6322.526510	26.123725
187.882509	6339.458745	26.128743
188.126404	6340.261229	26.133760
187.956838	6348.331981	26.138778
188.073682	6365.795989	26.143796
188.431218	6378.558905	26.148813
189.063288	6390.283165	26.153831
188.897591	6402.393123	26.158848
188.958428	6408.573225	26.163866
189.573244	6422.486864	26.168884
189.611141	6435.476023	26.173901
189.656066	6448.836585	26.178919
190.033931	6466.417385	26.183936
190.631421	6453.725671	26.188954
190.763431	6476.164425	26.193972
190.885740	6479.283036	26.198989
191.033677	6476.152150	26.204007
191.232768	6489.904678	26.209024
191.364176	6496.965537	26.214042
191.765605	6508.556361	26.219060
191.618013	6514.631596	26.224077
191.637241	6519.493805	26.229095
192.136323	6537.405908	26.234112
192.034959	6545.628513	26.239130
192.389356	6552.937611	26.244148
192.583491	6573.083606	26.249165
192.622582	6577.718064	26.254183
193.307029	6596.352544	26.259200
193.193357	6607.089830	26.264218
193.951735	6602.671658	26.269236
193.852807	6607.521161	26.274253
194.132381	6618.960529	26.279271
194.576583	6625.007151	26.284288
194.685557	6623.258719	26.289306
194.900923	6624.498363	26.294324
194.677301	6626.619601	26.299341
194.899141	6625.236072	26.304359
195.096360	6643.748840	26.309376
195.366630	6653.316729	26.314394
195.687077	6650.906312	26.319412
195.541307	6653.417158	26.324429
196.011319	6672.588963	26.329447
196.234715	6687.537240	26.334464
195.885066	6689.428087	26.339482
196.225459	6698.321976	26.344500
196.604721	6706.782524	26.349517
196.663994	6706.871254	26.354535
196.985577	6725.262708	26.359552
196.997944	6743.716400	26.364570
197.184804	6749.498485	26.369588
197.292935	6764.524203	26.374605
197.531778	6764.216156	26.379623
197.789915	6777.320366	26.384640
197.469342	6801.113665	26.389658
198.354648	6807.410277	26.394676
198.302322	6824.219104	26.399693
198.725430	6833.015096	26.404711
198.920546	6851.367770	26.409728
199.108195	6863.464481	26.414746
199.496888	6859.242131	26.419764
199.395966	6874.613689	26.424781
199.636774	6890.180744	26.429799
200.141330	6899.357123	26.434816
200.183435	6904.537819	26.439834
200.436287	6896.746181	26.444852
200.485496	6916.718900	26.449869
200.724212	6925.554920	26.454887
200.436306	6925.878351	26.459904
200.693605	6943.773442	26.464922
200.879782	6951.554820	26.469940
201.428578	6969.574184	26.474957
201.474425	6987.613028	26.479975
201.543970	6989.232081	26.484992
201.567478	7016.840940	26.490010
202.114629	7011.801494	26.495028
202.534132	7036.774654	26.500045
202.660778	7037.329564	26.505063
202.590626	7049.999987	26.510080
202.838710	7075.154394	26.515098
203.081405	7074.931561	26.520116
203.379638	7090.227798	26.525133
203.318227	7108.501933	26.530151
203.361348	7111.665285	26.535168
203.916033	7130.039100	26.540186
204.191001	7142.094787	26.545204
204.371088	7161.985497	26.550221
204.837725	7177.205891	26.555239
205.324426	7166.661058	26.560256
205.313220	7184.255078	26.565274
205.724041	7192.528708	26.570292
205.386019	7195.299104	26.575309
205.750160	7212.326902	26.580327
206.084692	7219.430863	26.585344
206.243844	7223.925119	26.590362
206.056483	7236.889208	26.595380
206.612272	7243.062530	26.600397
206.537950	7260.932532	26.605415
207.234808	7272.190656	26.610432
207.061210	7288.258356	26.615450
207.203828	7296.563837	26.620468
207.398896	7302.545625	26.625485
207.461129	7317.962282	26.630503
207.907191	7337.216838	26.635520
207.698480	7349.144803	26.640538
208.083170	7367.788069	26.645556
208.304340	7379.585815	26.650573
208.780304	7400.978021	26.655591
209.345681	7407.651581	26.660608
209.342439	7434.264434	26.665626
209.391065	7429.727227	26.670644
209.676601	7444.793538	26.675661
209.916675	7466.925930	26.680679
210.754204	7457.861201	26.685696
210.409640	7467.015424	26.690714
211.127342	7475.148604	26.695732
211.104928	7497.106299	26.700749
211.088140	7493.289619	26.705767
211.472071	7492.330535	26.710784
211.353383	7509.853697	26.715802
211.534050	7529.836144	26.720820
211.801908	7524.092098	26.725837
211.972195	7544.468555	26.730855
212.278176	7551.085080	26.735872
212.279271	7564.737407	26.740890
212.755551	7574.167775	26.745908
212.996641	7581.829306	26.750925
212.545377	7609.523300	26.755943
213.430052	7612.905844	26.760960
213.277540	7623.371397	26.765978
214.064761	7636.567541	26.770996
214.126394	7650.821180	26.776013
213.729015	7650.536518	26.781031
214.007552	7652.737816	26.786048
214.464136	7658.632336	26.791066
214.836989	7672.713956	26.796084
215.301526	7683.813907	26.801101
214.654764	7694.950529	26.806119
215.078229	7707.582297	26.811136
215.136824	7720.209096	26.816154
215.575626	7737.878109	26.821172
215.642341	7754.654820	26.826189
216.241135	7767.916925	26.831207
216.284386	7774.882668	26.836224
216.694083	7788.093384	26.841242
217.247165	7789.796319	26.846260
216.887041	7808.290064	26.851277
217.281351	7816.703817	26.856295
217.798770	7816.217302	26.861312
217.769919	7836.905162	26.866330
218.332930	7840.021981	26.871348
218.724943	7860.867064	26.876365
218.650623	7868.502964	26.881383
219.018175	7866.031006	26.886400
219.267574	7879.167506	26.891418
219.426128	7884.587615	26.896436
219.636587	7891.073580	26.901453
219.303969	7909.096559	26.906471
219.880629	7909.271371	26.911488
220.096319	7929.556520	26.916506
220.462854	7940.450737	26.921524
220.665260	7946.838805	26.926541
220.691434	7965.464138	26.931559
220.831963	7965.290505	26.936576
221.211798	7985.747058	26.941594
221.394900	7989.278910	26.946612
221.788444	7993.438400	26.951629
221.655289	8018.492775	26.956647
222.410735	8022.546676	26.961664
222.358801	8031.244737	26.966682
222.323060	8050.551558	26.971700
222.793455	8059.837462	26.976717
222.908026	8067.048324	26.981735
223.141162	8088.062583	26.986752
223.147421	8098.844038	26.991770
223.445645	8107.978868	26.996788
223.769458	8113.808100	27.001805
223.686786	8128.504337	27.006823
224.320906	8136.208994	27.011840
224.489100	8152.109912	27.016858
224.564654	8170.038045	27.021876
225.109618	8172.259907	27.026893
224.968751	8196.695893	27.031911
225.353397	8200.771837	27.036928
225.341022	8216.464027	27.041946
225.385568	8236.806256	27.046964
225.922519	8246.060769	27.051981
226.067381	8258.976992	27.056999
226.434246	8267.154482	27.062016
227.024864	8279.126484	27.067034
226.904781	8296.670432	27.072052
227.666509	8311.528760	27.077069
227.710438	8317.951089	27.082087
228.260009	8314.963687	27.087104
228.386624	8314.156650	27.092122
228.421563	8319.183020	27.097140
228.572037	8334.304042	27.102157
228.768398	8354.819800	27.107175
228.734267	8356.668846	27.112192
229.045281	8357.304355	27.117210
229.258566	8375.821206	27.122228
229.624837	8381.235459	27.127245
229.550644	8383.560633	27.132263
229.804872	8384.292983	27.137280
230.404204	8407.681166	27.142298
229.948469	8418.278570	27.147316
230.484928	8427.981498	27.152333
230.428763	8439.413950	27.157351
230.837421	8464.157189	27.162368
230.907726	8480.298358	27.167386
231.332458	8503.852652	27.172404
231.742358	8505.792063	27.177421
231.677146	8516.712457	27.182439
232.157217	8526.713883	27.187456
232.114163	8541.602454	27.192474
232.720588	8555.214505	27.197492
232.785239	8563.150707	27.202509
233.319112	8589.885327	27.207527
233.287166	8599.286213	27.212544
233.523265	8598.420075	27.217562
233.775810	8618.006777	27.222580
234.126974	8624.279901	27.227597
233.951341	8639.239350	27.232615
234.653339	8650.392049	27.237632
234.731945	8662.586168	27.242650
234.667121	8683.781302	27.247668
235.316016	8696.001569	27.252685
235.391787	8712.650958	27.257703
235.587173	8722.675213	27.262720
236.166884	8734.766741	27.267738
236.035122	8752.105941	27.272756
236.088283	8765.150402	27.277773
236.420268	8789.946226	27.282791
236.928959	8794.307441	27.287808
237.197924	8801.644328	27.292826
237.474355	8825.307149	27.297844
237.433495	8831.278939	27.302861
237.749849	8849.409029	27.307879
237.798766	8871.760927	27.312896
238.442608	8888.302283	27.317914
238.417692	8899.510104	27.322932
238.855978	8904.955155	27.327949
239.069694	8927.631984	27.332967
239.183499	8939.536102	27.337984
239.395951	8961.892566	27.343002
239.463661	8980.692603	27.348020
239.927086	8983.199075	27.353037
240.551008	8993.509423	27.358055
240.369853	9013.630035	27.363072
240.965362	9024.657253	27.368090
241.082149	9036.678327	27.373108
241.475692	9050.974380	27.378125
241.566350	9057.693351	27.383143
242.083741	9070.942451	27.388160
242.469125	9089.937393	27.393178
242.559318	9099.757933	27.398196
243.097111	9090.087273	27.403213
243.053383	9099.444711	27.408231
243.368733	9110.325359	27.413248
243.678901	9100.780604	27.418266
243.768319	9105.706034	27.423284
243.682662	9123.792692	27.428301
243.828394	9142.127033	27.433319
243.954582	9143.741657	27.438336
244.448481	9159.365145	27.443354
244.126570	9177.707612	27.448372
244.338774	9190.384196	27.453389
244.860472	9205.428048	27.458407
245.058161	9223.961855	27.463424
245.491132	9232.693740	27.468442
245.532773	9247.222321	27.473460
245.852628	9265.824186	27.478477
246.031728	9276.578610	27.483495
246.172229	9286.225501	27.488512
246.644440	9302.288365	27.493530
246.341638	9320.747575	27.498548
247.037675	9345.806202	27.503565
247.347231	9367.874585	27.508583
247.683846	9385.370909	27.513600
247.736342	9395.117515	27.518618
248.081929	9414.678762	27.523636
248.442506	9424.149867	27.528653
248.625630	9445.267149	27.533671
249.353500	9457.257499	27.538688
249.801548	9458.500608	27.543706
249.506526	9470.755613	27.548724
249.919703	9488.726234	27.553741
250.005458	9499.525408	27.558759
250.124786	9523.044313	27.563776
250.596178	9523.589515	27.568794
250.849541	9545.492552	27.573812
251.239815	9552.476467	27.578829
251.442272	9560.284787	27.583847
251.474688	9581.603662	27.588864
251.770612	9588.550428	27.593882
251.821352	9602.876935	27.598900
252.052498	9606.999923	27.603917
252.325528	9620.677529	27.608935
252.734546	9642.883447	27.613952
253.178570	9654.709800	27.618970
253.335127	9670.874917	27.623988
253.976881	9682.522817	27.629005
253.930780	9701.701778	27.634023
253.991513	9711.593745	27.639040
254.437973	9720.052659	27.644058
254.323886	9743.822445	27.649076
254.665163	9756.036152	27.654093
254.993098	9772.168275	27.659111
255.012324	9787.271428	27.664128
255.455345	9811.970886	27.669146
255.671842	9823.437970	27.674164
255.803896	9847.014329	27.679181
256.230529	9858.202432	27.684199
256.406769	9878.899944	27.689216
256.873353	9894.425469	27.694234
257.475861	9917.626263	27.699252
257.556025	9914.695006	27.704269
257.942765	9934.406851	27.709287
257.924890	9948.365295	27.714304
258.396459	9947.238735	27.719322
258.616695	9974.935154	27.724340
258.918350	9980.888489	27.729357
258.963342	9995.139091	27.734375
259.084503	10010.779418	27.739392
259.807431	10015.627837	27.744410
259.937748	10029.379047	27.749428
260.340558	10045.840967	27.754445
260.775738	10064.068573	27.759463
260.574680	10082.678042	27.764480
261.304794	10086.074908	27.769498
261.160761	10094.016475	27.774516
261.180337	10103.798897	27.779533
261.749171	10104.385504	27.784551
262.129299	10128.538868	27.789568
262.483721	10130.285984	27.794586
262.684780	10134.960054	27.799604
262.647053	10143.207845	27.804621
263.313825	10151.515498	27.809639
263.222332	10162.775399	27.814656
263.519199	10181.746897	27.819674
263.389540	10195.069373	27.824692
263.877715	10201.400013	27.829709
264.193209	10219.472709	27.834727
264.146202	10237.945773	27.839744
264.610344	10248.417316	27.844762
264.640771	10255.817993	27.849780
264.931869	10282.577508	27.854797
265.348062	10293.001081	27.859815
265.152453	10320.602271	27.864832
265.836928	10340.132186	27.869850
265.986208	10361.750249	27.874868
266.252698	10378.341433	27.879885
266.721219	10396.887700	27.884903
266.855776	10407.258699	27.889920
267.118524	10419.615903	27.894938
267.385896	10451.171275	27.899956
267.791713	10463.265328	27.904973
267.868456	10473.674301	27.909991
268.184398	10504.023427	27.915008
268.758146	10514.139016	27.920026
268.894011	10528.124512	27.925044
269.316174	10546.773955	27.930061
269.680888	10575.134494	27.935079
269.522312	10580.013975	27.940096
269.990887	10591.621875	27.945114
270.057919	10602.844025	27.950132
270.413387	10631.154194	27.955149
270.777638	10642.803036	27.960167
270.754069	10665.388448	27.965184
271.545829	10681.548706	27.970202
271.396782	10698.353180	27.975220
272.030485	10718.950050	27.980237
272.361503	10722.954375	27.985255
272.637797	10750.753148	27.990272
273.290528	10756.109766	27.995290
273.219315	10775.302826	28.000308
273.072645	10792.017188	28.005325
273.645939	10805.404228	28.010343
274.004687	10826.201169	28.015360
274.067631	10831.795677	28.020378
274.298961	10855.021449	28.025396
274.508814	10864.928046	28.030413
275.222454	10876.760310	28.035431
274.968914	10902.957869	28.040448
275.547188	10911.044997	28.045466
275.912710	10934.368426	28.050484
276.038649	10948.701015	28.055501
276.339590	10970.804540	28.060519
276.876669	10982.511685	28.065536
277.209129	10997.768181	28.070554
277.438076	11011.029606	28.075572
277.711624	11021.429993	28.080589
278.322605	11031.429445	28.085607
278.384242	11044.121386	28.090624
278.566247	11058.198976	28.095642
278.960723	11069.620944	28.100660
278.888148	11080.647506	28.105677
279.316866	11087.487852	28.110695
279.438820	11105.944971	28.115712
279.711524	11132.969728	28.120730
280.063389	11145.999768	28.125748
279.910914	11146.893331	28.130765
280.339420	11157.575428	28.135783
280.655945	11181.805505	28.140800
280.816463	11197.602772	28.145818
281.205830	11203.830409	28.150836
280.937083	11227.328583	28.155853
281.785313	11239.658839	28.160871
281.994885	11265.187840	28.165888
282.458164	11282.796053	28.170906
282.686727	11296.010503	28.175924
282.798680	11311.248644	28.180941
283.313448	11317.643085	28.185959
283.368790	11350.740959	28.190976
283.903677	11361.010064	28.195994
284.204656	11378.604277	28.201012
284.149831	11394.374350	28.206029
284.667696	11407.268395	28.211047
284.773013	11426.330580	28.216064
285.118528	11448.358046	28.221082
285.732461	11460.957319	28.226100
285.798116	11483.864746	28.231117
286.328584	11495.248749	28.236135
286.352492	11520.366088	28.241152
286.891336	11529.129768	28.246170
287.168071	11539.997971	28.251188
286.964893	11567.207802	28.256205
287.721137	11571.619422	28.261223
287.834774	11588.466430	28.266240
288.367140	11605.135417	28.271258
288.509177	11623.696957	28.276276
288.660134	11643.605927	28.281293
289.226203	11655.876054	28.286311
289.260436	11678.133423	28.291328
289.589478	11683.586482	28.296346
290.014893	11697.071231	28.301364
289.898696	11736.791462	28.306381
290.506419	11751.955835	28.311399
290.487774	11767.877863	28.316416
290.791319	11800.298944	28.321434
291.370142	11818.025713	28.326452
291.333826	11838.829469	28.331469
291.681085	11848.327850	28.336487
292.069156	11871.738722	28.341504
292.194996	11895.191458	28.346522
292.873075	11915.155336	28.351540
293.326433	11934.417370	28.356557
293.389548	11960.858901	28.361575
293.576511	11975.921364	28.366592
293.892100	11985.789086	28.371610
294.651899	12015.705141	28.376628
294.399665	12033.169442	28.381645
294.893072	12046.414732	28.386663
295.301195	12072.377013	28.391680
295.199321	12082.239829	28.396698
295.916244	12095.306336	28.401716
296.296588	12127.404917	28.406733
296.719901	12128.280444	28.411751
296.977376	12154.453742	28.416768
297.165634	12161.646367	28.421786
297.404047	12170.995915	28.426804
297.499597	12192.564647	28.431821
298.109717	12220.920547	28.436839
298.375792	12226.395244	28.441856
298.491658	12250.425332	28.446874
298.942354	12259.520749	28.451892
299.277509	12289.301159	28.456909
299.105388	12289.091778	28.461927
299.554982	12316.801523	28.466944
299.731263	12336.711879	28.471962
300.505935	12345.733234	28.476980
300.179351	12366.681839	28.481997
300.864183	12379.660913	28.487015
300.963579	12397.803335	28.492032
301.120066	12420.378722	28.497050
301.687219	12427.715191	28.502068
301.618065	12457.517131	28.507085
301.981753	12477.316270	28.512103
302.117016	12498.809496	28.517120
302.473135	12512.977723	28.522138
302.964229	12541.429528	28.527156
303.111685	12560.271750	28.532173
303.682447	12577.494826	28.537191
304.421029	12604.306247	28.542208
304.551242	12619.711215	28.547226
304.898400	12633.879456	28.552244
305.124956	12639.475874	28.557261
305.090953	12658.849380	28.562279
305.891485	12677.471753	28.567296
305.843039	12699.548793	28.572314
306.486266	12713.589303	28.577332
306.424422	12746.058567	28.582349
306.564708	12747.961192	28.587367
307.120155	12771.463853	28.592384
307.216766	12796.388324	28.597402
307.882426	12820.240001	28.602420
308.397199	12840.170591	28.607437
308.700455	12862.534765	28.612455
308.655175	12870.064208	28.617472
309.173924	12895.960643	28.622490
309.783695	12901.257335	28.627508
309.584833	12923.487224	28.632525
310.091775	12937.230574	28.637543
310.602230	12957.639529	28.642560
310.669837	12973.452328	28.647578
311.292694	12985.301176	28.652596
311.536673	13000.952431	28.657613
311.689579	13018.103305	28.662631
312.096277	13040.855617	28.667648
311.932679	13066.869993	28.672666
312.666500	13078.576043	28.677684
312.838039	13106.014818	28.682701
313.220461	13127.036156	28.687719
313.616154	13139.137045	28.692736
313.647726	13156.807723	28.697754
314.294754	13177.123431	28.702772
314.614540	13191.400701	28.707789
314.582663	13211.066062	28.712807
315.017771	13228.663722	28.717824
315.324903	13244.695595	28.722842
315.821223	13264.489501	28.727860
316.071032	13290.177349	28.732877
316.352415	13310.701885	28.737895
316.679809	13325.286903	28.742912
316.630286	13359.701664	28.747930
317.254683	13372.608015	28.752948
317.332472	13401.927174	28.757965
317.897425	13422.590881	28.762983
318.587726	13436.824376	28.768000
318.506822	13461.566488	28.773018
319.004893	13471.050318	28.778036
319.042448	13484.770960	28.783053
319.560461	13511.992320	28.788071
319.862482	13515.162147	28.793088
320.387069	13546.013539	28.798106
320.817719	13556.963213	28.803124
320.882022	13587.698598	28.808141
321.035514	13589.109003	28.813159
321.409932	13602.947348	28.818176
321.582554	13635.152629	28.823194
322.038598	13646.950772	28.828212
322.298468	13660.127295	28.833229
322.582112	13680.119235	28.838247
322.787684	13685.899153	28.843264
323.008376	13713.524661	28.848282
323.199914	13720.109097	28.853300
323.632233	13758.750583	28.858317
323.981450	13778.492238	28.863335
324.154630	13797.709874	28.868352
324.393704	13825.778540	28.873370
325.091586	13852.861954	28.878388
325.605778	13872.155620	28.883405
325.875831	13896.925406	28.888423
326.202648	13917.367537	28.893440
325.999776	13945.805849	28.898458
326.644009	13964.676215	28.903476
327.070741	13982.066465	28.908493
327.199021	14011.137228	28.913511
327.733633	14023.958093	28.918528
328.065901	14053.729599	28.923546
328.380692	14069.702703	28.928564
328.637272	14102.265375	28.933581
328.578908	14126.576078	28.938599
329.307858	14142.419238	28.943616
330.044651	14172.918332	28.948634
330.199080	14180.594993	28.953652
330.621865	14202.701662	28.958669
330.912157	14219.676606	28.963687
331.728379	14235.177595	28.968704
331.603810	14258.935225	28.973722
332.271118	14265.734282	28.978740
332.457365	14291.861336	28.983757
332.964184	14300.143248	28.988775
333.369265	14313.118169	28.993792
333.793798	14332.108856	28.998810
333.910855	14345.583804	29.003828
334.212483	14362.177190	29.008845
334.251236	14387.356376	29.013863
334.823394	14394.636177	29.018880
334.979115	14423.060093	29.023898
335.351764	14436.908895	29.028916
335.331460	14462.053841	29.033933
335.403210	14493.506807	29.038951
336.139357	14514.796060	29.043968
336.025235	14546.856735	29.048986
336.365688	14569.048450	29.054004
337.206909	14598.345841	29.059021
337.489064	14627.986414	29.064039
337.476472	14648.641667	29.069056
337.757846	14668.917313	29.074074
338.265539	14697.158937	29.079092
338.566453	14726.995172	29.084109
339.217289	14750.161801	29.089127
339.710930	14768.531605	29.094144
339.728267	14793.872570	29.099162
340.031788	14812.888572	29.104180
340.565283	14837.215847	29.109197
340.698512	14864.241513	29.114215
341.238712	14877.772952	29.119232
341.526235	14906.965524	29.124250
342.154982	14934.845505	29.129268
342.300222	14951.347162	29.134285
342.669197	14969.189336	29.139303
343.308013	14988.534621	29.144320
343.086582	15013.091129	29.149338
343.546914	15028.394869	29.154356
343.905983	15050.220069	29.159373
343.944253	15075.498110	29.164391
344.714642	15095.798947	29.169408
344.646414	15112.827851	29.174426
344.979031	15134.930213	29.179444
345.766134	15155.171617	29.184461
345.866049	15179.446646	29.189479
346.516335	15193.261170	29.194496
346.454228	15220.677536	29.199514
346.766347	15239.795060	29.204532
347.289955	15274.180445	29.209549
347.258483	15299.460916	29.214567
347.991010	15322.159325	29.219584
348.077937	15348.211505	29.224602
348.383004	15371.463035	29.229620
349.134399	15397.074323	29.234637
349.064817	15423.827123	29.239655
349.776504	15441.345140	29.244672
350.127027	15479.496695	29.249690
350.448597	15504.447947	29.254708
350.976779	15517.854235	29.259725
351.305859	15546.134764	29.264743
351.775543	15568.246547	29.269760
351.890756	15595.727183	29.274778
352.565634	15610.043944	29.279796
353.033166	15635.901185	29.284813
353.382545	15650.379035	29.289831
353.811871	15668.582384	29.294848
353.883898	15695.952121	29.299866
354.233615	15715.037179	29.304884
354.568585	15728.330609	29.309901
354.838466	15755.833198	29.314919
355.254296	15772.429600	29.319936
355.762279	15800.316854	29.324954
355.691805	15820.423605	29.329972
356.133957	15831.831578	29.334989
356.326263	15864.168797	29.340007
357.052158	15887.386084	29.345024
357.125852	15916.070468	29.350042
357.510434	15939.252897	29.355060
358.040528	15961.787094	29.360077
358.330862	15992.363468	29.365095
358.815914	16020.636336	29.370112
358.885764	16041.397906	29.375130
359.354156	16069.976251	29.380148
359.874691	16086.538301	29.385165
359.937601	16131.244062	29.390183
360.644038	16143.998749	29.395200
360.881126	16180.118443	29.400218
361.147778	16203.736888	29.405236
361.486697	16233.610547	29.410253
361.819410	16256.901311	29.415271
362.169806	16280.258535	29.420288
362.807193	16313.873815	29.425306
362.950582	16329.213886	29.430324
363.526292	16360.038469	29.435341
363.624398	16385.634898	29.440359
364.066106	16408.460179	29.445376
364.490300	16434.481896	29.450394
364.972637	16452.667882	29.455412
365.575987	16482.074211	29.460429
365.642827	16510.598405	29.465447
366.388682	16527.137794	29.470464
366.775099	16555.408988	29.475482
366.948709	16574.845748	29.480500
367.468920	16594.653915	29.485517
367.578134	16618.611114	29.490535
367.671543	16626.866478	29.495552
367.924153	16656.750457	29.500570
368.180139	16688.394642	29.505588
368.881573	16699.670458	29.510605
368.935067	16727.314514	29.515623
369.063663	16754.843727	29.520640
369.678317	16782.814294	29.525658
370.007800	16811.982803	29.530676
370.576936	16833.781905	29.535693
370.764648	16873.747998	29.540711
371.342657	16889.300391	29.545728
371.582069	16931.516912	29.550746
371.728315	16939.182030	29.555764
372.040140	16968.251276	29.560781
372.677677	17006.495995	29.565799
373.184424	17023.868344	29.570816
373.508885	17061.296454	29.575834
373.720405	17091.098167	29.580852
374.199584	17117.308900	29.585869
374.213357	17151.257661	29.590887
374.886129	17169.865326	29.595904
375.473700	17205.647087	29.600922
375.852860	17243.028722	29.605940
376.367275	17265.107003	29.610957
376.476168	17291.319394	29.615975
377.104701	17313.334715	29.620992
377.632736	17336.686101	29.626010
377.980693	17364.271449	29.631028
378.654982	17379.805218	29.636045
379.045121	17407.757252	29.641063
379.056174	17426.323393	29.646080
379.486297	17450.296465	29.651098
379.699534	17487.742368	29.656116
380.281510	17501.489749	29.661133
380.338990	17519.104068	29.666151
381.176662	17552.043985	29.671168
381.536062	17581.489490	29.676186
381.418487	17612.989184	29.681204
382.066859	17630.876276	29.686221
382.273711	17667.447175	29.691239
382.412715	17698.890379	29.696256
383.236669	17727.688610	29.701274
383.098392	17767.846374	29.706292
384.326124	17792.627463	29.711309
384.535985	17825.444827	29.716327
384.713128	17849.632171	29.721344
385.096872	17878.982743	29.726362
385.209802	17906.284726	29.731380
385.697268	17932.462272	29.736397
385.869659	17969.288610	29.741415
386.147603	17999.369440	29.746432
386.911550	18028.931649	29.751450
387.027981	18064.042862	29.756468
387.454548	18095.677262	29.761485
387.495104	18133.181571	29.766503
387.897852	18167.328138	29.771520
388.801810	18199.351926	29.776538
389.146650	18230.098390	29.781556
389.832470	18257.810594	29.786573
390.150914	18298.333872	29.791591
390.464078	18310.720232	29.796608
390.954687	18347.190486	29.801626
391.430745	18382.206593	29.806644
391.962345	18397.189531	29.811661
392.651108	18438.211502	29.816679
392.932790	18461.846440	29.821696
393.148301	18478.765627	29.826714
393.464230	18508.716550	29.831732
393.856841	18522.265957	29.836749
394.171042	18544.125266	29.841767
394.325442	18561.693117	29.846784
394.928392	18590.912502	29.851802
395.284125	18612.050888	29.856820
395.663302	18637.166008	29.861837
396.000015	18666.497375	29.866855
396.289924	18695.746681	29.871872
396.794770	18705.716404	29.876890
397.007970	18741.336417	29.881908
397.588824	18768.549759	29.886925
397.930051	18796.004593	29.891943
397.946783	18836.831349	29.896960
398.349396	18858.269704	29.901978
398.591054	18901.305893	29.906996
399.146999	18932.529499	29.912013
399.456472	18964.605852	29.917031
400.015700	18993.737013	29.922048
400.653059	19027.143393	29.927066
400.991938	19067.280488	29.932084
401.490499	19093.032364	29.937101
401.506426	19132.362287	29.942119
402.167548	19165.753975	29.947136
402.616766	19192.553098	29.952154
402.724450	19227.345015	29.957172
403.549320	19267.864084	29.962189
403.735162	19299.532724	29.967207
404.075099	19333.600633	29.972224
404.706600	19364.233954	29.977242
404.889899	19404.556835	29.982260
405.224446	19435.759690	29.987277
405.915622	19464.417367	29.992295
406.284819	19503.412222	29.997312
407.214974	19530.282066	30.002330
407.445766	19560.698282	30.007348
407.816713	19593.049446	30.012365
408.097474	19621.319688	30.017383
408.644535	19648.782848	30.022400
409.398290	19667.081943	30.027418
409.790480	19706.434500	30.032436
410.016336	19732.341276	30.037453
410.659830	19749.637091	30.042471
410.353854	19781.425871	30.047488
411.175087	19800.008766	30.052506
411.404624	19842.730910	30.057524
411.593475	19871.455073	30.062541
412.081131	19904.503294	30.067559
412.426913	19944.135262	30.072576
413.009957	19974.353616	30.077594
413.660108	20013.084014	30.082612
414.090793	20045.464003	30.087629
414.489399	20073.034410	30.092647
414.571425	20107.214368	30.097664
415.600619	20137.944104	30.102682
415.303772	20167.403447	30.107700
416.280563	20185.582640	30.112717
416.423525	20225.791194	30.117735
416.566057	20247.780466	30.122752
417.552951	20274.492339	30.127770
417.531372	20306.684382	30.132788
418.270853	20341.716178	30.137805
418.706578	20360.560575	30.142823
419.015701	20403.461745	30.147840
419.516074	20426.552436	30.152858
419.684569	20460.226889	30.157876
420.312598	20492.214030	30.162893
420.694384	20514.586597	30.167911
420.654232	20553.968542	30.172928
421.346383	20569.573291	30.177946
421.678016	20610.842583	30.182964
421.895731	20633.277147	30.187981
422.093537	20662.527783	30.192999
422.851711	20698.216274	30.198016
423.616500	20728.205672	30.203034
423.889371	20765.434612	30.208052
424.163580	20793.439876	30.213069
424.742994	20813.229079	30.218087
424.791768	20848.860278	30.223104
425.520100	20877.004955	30.228122
425.409093	20916.585520	30.233140
425.762890	20948.756084	30.238157
426.407792	20986.083189	30.243175
426.363209	21024.500453	30.248192
427.006816	21062.354557	30.253210
427.668279	21113.300299	30.258228
428.425574	21147.162490	30.263245
429.024377	21184.778318	30.268263
429.261283	21213.498394	30.273280
429.467987	21247.835046	30.278298
429.891436	21286.284243	30.283316
430.441862	21328.753655	30.288333
431.293206	21367.602089	30.293351
431.322805	21395.185274	30.298368
431.838122	21423.520637	30.303386
431.988773	21460.741379	30.308404
432.301879	21502.607193	30.313421
432.758703	21534.804396	30.318439
433.512349	21591.505625	30.323456
433.887518	21616.914412	30.328474
434.400662	21658.632406	30.333492
434.656699	21692.126116	30.338509
435.433962	21730.651797	30.343527
435.543229	21775.399648	30.348544
436.509985	21805.286588	30.353562
436.742823	21847.865048	30.358580
437.312007	21882.262835	30.363597
437.948963	21913.305133	30.368615
438.241912	21951.662336	30.373632
438.654150	21972.584314	30.378650
439.136271	22010.147181	30.383668
439.380375	22045.098937	30.388685
440.217085	22074.522224	30.393703
440.145799	22109.731290	30.398720
440.866848	22141.496454	30.403738
441.363747	22180.031713	30.408756
441.545675	22210.985871	30.413773
442.239819	22248.337577	30.418791
442.266485	22292.364091	30.423808
442.760965	22322.095158	30.428826
443.383395	22367.341493	30.433844
443.431241	22404.392100	30.438861
444.412619	22429.469996	30.443879
444.806643	22473.217007	30.448896
444.965898	22515.175433	30.453914
445.423363	22557.814689	30.458932
446.049724	22587.683657	30.463949
446.803097	22612.903628	30.468967
446.963323	22657.874014	30.473984
447.833268	22686.107078	30.479002
448.201510	22728.780450	30.484020
448.205907	22760.324771	30.489037
448.823248	22793.959550	30.494055
448.935322	22834.791233	30.499072
449.619364	22871.021681	30.504090
450.064569	22912.421285	30.509108
450.463312	22950.958769	30.514125
450.877584	22972.208058	30.519143
451.000904	23013.918207	30.524160
451.157858	23050.737709	30.529178
451.727390	23091.084316	30.534196
452.339645	23125.887489	30.539213
452.887110	23159.364251	30.544231
453.376600	23202.304163	30.549248
453.837401	23238.805718	30.554266
454.187971	23276.763729	30.559284
454.470604	23323.439170	30.564301
455.092256	23352.179620	30.569319
455.375923	23411.688031	30.574336
456.163566	23440.716545	30.579354
456.633895	23481.510993	30.584372
457.154254	23531.124891	30.589389
457.454244	23560.308424	30.594407
457.897777	23597.717186	30.599424
458.320253	23640.158365	30.604442
458.958494	23680.258457	30.609460
458.885187	23732.117397	30.614477
459.845747	23762.485058	30.619495
459.999621	23803.826228	30.624512
460.505769	23838.836075	30.629530
461.391909	23881.674213	30.634548
461.855196	23929.161934	30.639565
462.570827	23953.928095	30.644583
462.548612	24011.238882	30.649600
463.405974	24044.907378	30.654618
464.241334	24080.084018	30.659636
463.951163	24126.659320	30.664653
464.985005	24161.380652	30.669671
465.196682	24192.576342	30.674688
465.520153	24226.519630	30.679706
466.421087	24266.022528	30.684724
466.625722	24309.330916	30.689741
467.008328	24341.186163	30.694759
467.275792	24383.847234	30.699776
468.200118	24429.515884	30.704794
468.707732	24470.503650	30.709812
468.736896	24508.839295	30.714829
469.712712	24538.578163	30.719847
469.998322	24583.346781	30.724864
470.414681	24614.307509	30.729882
471.066543	24651.922235	30.734900
471.660342	24691.284543	30.739917
472.085359	24729.451091	30.744935
472.221085	24767.432194	30.749952
472.528216	24806.958906	30.754970
473.163037	24846.727969	30.759988
473.316737	24892.512761	30.765005
474.121216	24936.001031	30.770023
474.284564	24977.889127	30.775040
474.810322	25016.853407	30.780058
475.513869	25056.015452	30.785076
475.633507	25109.578246	30.790093
476.251753	25146.161907	30.795111
476.480793	25203.709507	30.800128
477.048859	25246.575313	30.805146
477.582384	25291.383605	30.810164
477.758717	25335.522506	30.815181
478.585814	25384.291430	30.820199
479.043350	25435.130875	30.825216
479.340576	25480.726309	30.830234
480.179026	25523.825634	30.835252
480.440018	25572.486901	30.840269
481.297257	25609.366349	30.845287
481.619398	25651.296045	30.850304
482.090214	25705.546982	30.855322
482.754883	25733.267072	30.860340
483.147487	25776.913948	30.865357
483.559792	25806.710419	30.870375
484.157356	25838.040807	30.875392
484.145762	25884.060615	30.880410
484.850710	25916.363822	30.885428
485.361747	25963.767260	30.890445
485.737253	26010.609708	30.895463
486.488158	26050.248792	30.900480
486.745546	26087.108663	30.905498
487.366593	26124.794801	30.910516
487.642747	26164.742975	30.915533
488.089030	26215.233297	30.920551
488.757585	26255.343861	30.925568
489.070800	26298.181906	30.930586
489.746738	26342.152388	30.935604
490.047705	26391.711499	30.940621
489.955337	26432.759063	30.945639
490.989616	26494.111240	30.950656
491.237302	26536.563266	30.955674
492.045662	26581.348361	30.960692
492.381861	26640.252035	30.965709
492.839660	26683.556046	30.970727
493.686603	26732.293959	30.975744
493.773810	26785.100789	30.980762
494.693912	26829.562056	30.985780
494.962246	26873.538249	30.990797
495.707341	26925.886498	30.995815
496.268330	26973.820702	31.000832
496.404436	27021.020951	31.005850
497.404906	27071.740674	31.010868
497.384274	27118.497103	31.015885
497.905808	27167.659167	31.020903
498.886350	27212.584597	31.025920
499.569448	27269.291082	31.030938
499.866148	27300.863183	31.035956
500.333990	27357.785385	31.040973
500.983071	27390.677880	31.045991
501.529621	27435.716712	31.051008
501.976613	27474.794214	31.056026
502.673332	27518.243742	31.061044
502.932462	27575.387315	31.066061
503.373137	27614.601825	31.071079
504.071826	27659.076625	31.076096
504.172365	27707.694734	31.081114
505.050732	27742.196665	31.086132
505.671887	27796.788909	31.091149
506.057776	27837.416799	31.096167
506.450201	27887.024987	31.101184
506.494225	27930.227073	31.106202
507.401996	27975.560854	31.111220
508.059168	28036.561327	31.116237
508.452988	28069.822279	31.121255
509.255868	28116.482979	31.126272
509.624724	28160.688707	31.131290
510.066753	28202.680455	31.136308
510.735294	28248.073461	31.141325
511.247249	28290.053849	31.146343
511.697821	28338.631572	31.151360
512.099195	28374.541831	31.156378
512.924991	28423.953650	31.161396
513.227167	28468.710655	31.166413
513.847262	28517.276599	31.171431
514.341296	28549.780517	31.176448
514.502323	28592.535834	31.181466
515.089916	28623.945475	31.186484
515.768968	28684.969836	31.191501
516.464226	28728.163937	31.196519
516.541827	28756.503404	31.201536
517.152732	28805.412390	31.206554
517.953845	28841.374195	31.211572
518.272834	28884.195577	31.216589
518.805278	28922.694322	31.221607
519.485251	28958.023361	31.226624
519.797978	29001.855618	31.231642
520.361659	29037.680444	31.236660
520.661262	29080.918802	31.241677
521.047540	29117.653354	31.246695
521.264723	29166.710526	31.251712
521.700061	29225.291056	31.256730
523.120331	29272.786542	31.261748
523.311591	29320.958755	31.266765
523.671215	29366.241732	31.271783
524.070910	29408.584116	31.276800
524.333765	29462.862271	31.281818
525.092657	29507.798759	31.286836
525.308121	29572.912859	31.291853
526.090916	29619.085574	31.296871
526.876540	29673.621771	31.301888
526.888671	29737.315684	31.306906
527.646389	29781.167754	31.311924
528.214058	29825.395275	31.316941
528.756685	29887.885085	31.321959
529.337926	29930.119814	31.326976
529.845080	29994.029319	31.331994
529.979590	30047.541761	31.337012
530.763258	30110.191245	31.342029
531.495358	30165.681188	31.347047
531.888255	30222.035131	31.352064
532.455521	30276.498905	31.357082
533.379379	30327.130358	31.362100
533.932134	30374.781848	31.367117
534.370114	30420.931698	31.372135
534.968666	30469.777962	31.377152
535.562557	30525.048966	31.382170
536.434001	30574.620218	31.387188
536.945179	30625.106265	31.392205
537.697145	30679.827846	31.397223
538.026135	30714.921921	31.402240
538.709605	30767.001618	31.407258
539.155097	30807.553972	31.412276
539.643647	30851.686737	31.417293
539.928674	30894.660626	31.422311
540.452567	30947.025985	31.427328
541.022883	31001.078166	31.432346
541.810669	31039.646584	31.437364
542.216928	31093.401206	31.442381
542.725949	31135.982080	31.447399
543.532080	31186.619712	31.452416
544.149143	31235.319896	31.457434
544.710645	31289.462766	31.462452
545.215961	31324.544655	31.467469
545.713075	31387.100955	31.472487
546.107365	31418.512882	31.477504
546.452014	31470.562371	31.482522
546.911125	31519.800632	31.487540
547.327308	31586.069041	31.492557
547.959425	31630.710092	31.497575
548.548422	31677.784839	31.502592
549.199004	31737.830587	31.507610
549.480789	31784.464216	31.512628
550.432874	31850.095912	31.517645
550.682013	31899.780170	31.522663
551.029395	31951.865330	31.527680
551.911508	31999.804339	31.532698
552.365975	32047.621757	31.537716
552.903888	32089.212508	31.542733
553.135839	32151.020219	31.547751
553.922366	32190.146714	31.552768
554.117583	32230.945691	31.557786
554.938858	32287.538265	31.562804
555.370302	32340.800259	31.567821
555.989828	32387.600473	31.572839
556.554247	32430.184762	31.577856
556.747257	32490.179395	31.582874
557.628987	32550.432622	31.587892
558.360530	32601.512636	31.592909
558.617547	32655.126294	31.597927
559.330722	32710.835631	31.602944
559.935609	32761.750887	31.607962
560.742223	32821.234892	31.612980
560.947130	32870.575763	31.617997
561.348198	32927.631192	31.623015
562.257827	32978.304158	31.628032
562.476464	33039.659604	31.633050
563.043132	33100.481184	31.638068
564.126545	33155.657319	31.643085
564.462123	33213.030590	31.648103
565.035879	33268.565938	31.653120
565.698579	33324.121455	31.658138
566.187229	33375.912875	31.663156
566.723761	33443.518908	31.668173
567.257007	33491.614338	31.673191
568.048901	33554.729074	31.678208
568.723447	33610.444462	31.683226
569.097259	33658.724506	31.688244
569.759454	33720.034147	31.693261
570.307220	33768.557095	31.698279
570.953910	33830.475575	31.703296
571.350800	33893.420186	31.708314
571.593503	33950.028572	31.713332
572.256496	34009.824323	31.718349
573.161859	34073.780482	31.723367
573.862133	34128.325599	31.728384
574.237090	34195.541494	31.733402
574.760600	34250.103606	31.738420
575.555437	34310.257242	31.743437
575.987900	34367.668681	31.748455
577.154134	34426.517872	31.753472
577.272622	34477.165049	31.758490
578.196054	34539.399958	31.763508
578.797370	34586.073256	31.768525
578.815246	34648.770801	31.773543
579.664451	34701.020807	31.778560
580.023339	34770.191838	31.783578
580.630442	34825.877987	31.788596
581.390813	34880.346022	31.793613
582.045953	34935.775249	31.798631
582.726121	34985.945909	31.803648
583.380058	35040.324738	31.808666
583.740103	35100.073262	31.813684
584.775241	35156.885718	31.818701
585.419686	35205.488086	31.823719
585.947237	35258.948014	31.828736
586.604396	35305.743339	31.833754
587.282185	35360.668331	31.838772
587.838828	35397.753799	31.843789
588.056193	35458.376079	31.848807
589.141233	35505.580843	31.853824
589.608006	35557.331691	31.858842
590.080731	35602.147921	31.863860
590.700819	35655.028788	31.868877
591.011227	35714.765472	31.873895
591.252894	35761.627570	31.878912
591.815397	35812.110359	31.883930
592.257383	35862.206096	31.888948
593.243130	35917.571026	31.893965
593.291680	35977.667511	31.898983
594.049759	36028.977005	31.904000
594.848834	36085.578965	31.909018
595.435713	36143.816361	31.914036
596.051715	36189.150041	31.919053
596.258222	36251.193879	31.924071
596.886273	36298.129156	31.929088
597.347823	36366.475043	31.934106
597.982764	36418.667648	31.939124
598.789219	36479.969153	31.944141
598.999798	36540.971773	31.949159
599.572501	36603.899933	31.954176
600.434652	36676.567825	31.959194
600.950957	36738.019208	31.964212
601.961065	36801.544806	31.969229
602.154654	36865.562374	31.974247
603.062473	36917.891178	31.979264
603.263552	36984.811679	31.984282
603.934422	37047.608357	31.989300
604.917695	37108.431388	31.994317
605.338418	37179.274247	31.999335
606.031713	37248.453100	32.004352
606.780863	37314.346714	32.009370
607.387897	37369.813469	32.014388
608.371043	37423.336989	32.019405
608.812941	37485.806931	32.024423
609.190459	37539.989668	32.029440
610.331312	37606.280364	32.034458
610.749175	37670.910720	32.039476
611.084885	37726.802220	32.044493
611.848995	37783.674096	32.049511
612.174121	37844.876778	32.054528
612.654858	37912.082688	32.059546
613.075653	37977.404902	32.064564
614.133624	38035.298978	32.069581
614.731163	38118.805155	32.074599
615.356396	38171.724082	32.079616
616.092878	38231.259674	32.084634
616.647880	38302.049965	32.089652
617.632862	38360.083410	32.094669
617.949580	38427.160529	32.099687
618.692845	38478.678266	32.104704
619.309847	38545.532531	32.109722
619.574806	38615.939580	32.114740
620.721340	38680.781239	32.119757
620.945353	38746.299745	32.124775
621.841730	38805.880203	32.129792
622.737178	38873.440866	32.134810
623.140592	38932.793949	32.139828
623.601175	38984.473519	32.144845
624.519876	39059.572163	32.149863
625.116468	39109.667057	32.154880
625.899422	39178.604810	32.159898
626.185204	39232.372129	32.164916
626.683080	39292.894495	32.169933
627.326435	39350.293141	32.174951
627.913128	39420.208117	32.179968
628.885305	39479.655119	32.184986
629.675856	39551.522430	32.190004
630.033847	39605.424105	32.195021
630.708438	39664.198050	32.200039
630.958859	39717.912664	32.205056
632.043835	39781.347879	32.210074
632.406848	39854.073137	32.215092
633.175588	39903.447232	32.220109
633.628728	39955.399094	32.225127
634.253129	40007.610036	32.230144
634.898794	40058.034021	32.235162
635.534747	40123.817597	32.240180
636.002761	40182.870452	32.245197
636.419779	40243.766048	32.250215
637.190203	40307.431902	32.255232
638.056717	40370.921081	32.260250
638.193479	40440.406121	32.265268
638.915452	40505.753812	32.270285
639.235635	40570.372672	32.275303
639.960838	40639.959995	32.280320
640.836938	40700.800092	32.285338
641.382664	40775.853808	32.290356
642.027452	40839.981099	32.295373
642.609687	40917.056096	32.300391
643.400475	40995.716429	32.305408
644.309383	41061.006747	32.310426
644.458152	41136.171796	32.315444
645.443341	41191.751725	32.320461
645.963838	41263.736691	32.325479
646.599446	41332.034447	32.330496
647.435621	41403.134279	32.335514
648.105014	41482.710204	32.340532
648.959958	41543.802827	32.345549
649.342533	41623.467848	32.350567
649.865520	41687.536144	32.355584
650.538840	41752.530071	32.360602
651.392586	41836.279092	32.365620
651.758280	41890.119863	32.370637
652.648346	41976.824875	32.375655
653.188068	42044.222395	32.380672
653.825817	42108.680429	32.385690
654.508185	42194.265302	32.390708
655.404183	42265.279615	32.395725
656.314578	42341.554840	32.400743
656.726599	42416.353172	32.405760
657.443337	42476.467742	32.410778
658.295476	42557.584015	32.415796
659.194949	42619.200067	32.420813
660.047076	42687.855331	32.425831
660.333903	42747.508325	32.430848
660.898833	42813.752067	32.435866
661.541613	42892.577531	32.440884
662.222641	42950.454718	32.445901
663.078934	43029.160191	32.450919
663.425667	43104.565656	32.455936
664.378836	43168.476323	32.460954
664.562584	43239.691115	32.465972
665.313641	43314.332768	32.470989
665.951337	43384.873119	32.476007
666.566212	43467.251340	32.481024
667.378191	43534.331360	32.486042
667.989051	43612.230556	32.491060
668.758753	43679.949572	32.496077
669.513842	43752.517890	32.501095
669.892310	43827.914705	32.506112
671.193310	43895.685535	32.511130
671.687131	43978.752253	32.516148
672.216496	44042.082424	32.521165
672.963591	44108.048018	32.526183
673.501940	44183.561900	32.531200
674.296133	44263.548995	32.536218
674.724485	44323.770897	32.541236
675.518475	44395.425903	32.546253
676.116473	44464.350759	32.551271
676.668170	44539.519692	32.556288
677.729627	44605.586593	32.561306
678.179146	44670.113019	32.566324
678.994046	44734.942345	32.571341
679.780210	44802.950033	32.576359
680.192089	44865.408815	32.581376
680.905263	44927.243275	32.586394
681.496930	45001.946431	32.591412
682.069395	45068.746325	32.596429
682.720207	45133.774682	32.601447
683.147315	45198.641338	32.606464
684.154009	45270.539208	32.611482
684.744316	45338.672804	32.616500
685.319514	45413.042441	32.621517
685.992694	45489.694975	32.626535
686.439009	45565.201204	32.631552
687.246340	45634.193600	32.636570
687.839939	45727.634164	32.641588
688.583505	45804.825782	32.646605
689.091528	45877.995779	32.651623
689.933328	45964.787231	32.656640
690.802181	46042.795909	32.661658
691.658238	46120.336510	32.666676
692.232488	46205.313370	32.671693
692.840032	46281.979973	32.676711
693.534723	46367.420786	32.681728
694.561559	46438.858723	32.686746
694.889980	46516.813492	32.691764
695.959310	46594.687068	32.696781
696.659327	46669.195727	32.701799
697.106792	46746.531743	32.706816
698.054200	46825.408549	32.711834
698.923111	46912.850390	32.716852
699.327394	46985.776553	32.721869
700.250651	47065.059409	32.726887
700.985742	47146.852743	32.731904
701.665834	47209.293835	32.736922
702.246985	47293.484921	32.741940
702.835590	47365.425169	32.746957
703.889036	47452.226305	32.751975
704.308718	47544.296092	32.756992
705.457155	47617.436325	32.762010
705.956857	47695.449695	32.767028
706.411009	47778.877570	32.772045
707.481474	47854.668619	32.777063
707.796112	47925.516223	32.782080
708.670693	48014.383332	32.787098
708.900782	48096.864323	32.792116
709.931309	48181.446076	32.797133
710.674915	48270.595011	32.802151
711.411699	48356.148314	32.807168
712.282139	48433.215914	32.812186
712.918334	48512.896516	32.817204
713.525863	48593.235944	32.822221
714.175962	48677.731226	32.827239
714.611668	48763.351943	32.832256
715.748147	48849.918297	32.837274
716.405424	48941.576506	32.842292
716.924692	49019.481491	32.847309
717.912557	49107.899088	32.852327
718.376678	49199.189372	32.857344
719.271089	49277.169153	32.862362
720.098239	49359.171482	32.867380
720.495088	49442.167584	32.872397
721.489616	49527.734006	32.877415
721.837803	49614.449995	32.882432
722.777138	49696.814212	32.887450
723.790547	49795.934589	32.892468
724.458930	49877.709557	32.897485
725.407683	49945.026493	32.902503
725.920345	50032.506765	32.907520
726.759221	50102.403939	32.912538
727.693728	50172.740368	32.917556
728.085746	50252.351700	32.922573
728.683187	50317.305480	32.927591
729.269988	50397.099966	32.932608
730.352377	50473.167853	32.937626
730.825428	50555.957149	32.942644
731.128904	50634.340230	32.947661
732.156037	50711.466837	32.952679
732.465283	50796.495256	32.957696
733.083410	50884.290426	32.962714
733.908490	50966.656846	32.967732
734.661414	51063.337821	32.972749
735.316674	51154.653101	32.977767
735.954766	51246.186440	32.982784
736.605593	51338.779418	32.987802
737.502505	51437.965379	32.992820
737.899297	51535.061383	32.997837
739.153691	51616.285583	33.002855
739.777971	51717.394346	33.007872
740.700330	51818.593311	33.012890
741.564251	51909.795493	33.017908
742.103944	52003.995719	33.022925
742.828521	52092.410489	33.027943
743.378555	52191.461821	33.032960
744.323140	52293.632489	33.037978
745.049746	52381.713398	33.042996
745.462627	52487.315087	33.048013
746.543708	52582.521515	33.053031
747.048219	52685.026051	33.058048
747.944253	52784.996095	33.063066
748.946830	52893.408626	33.068084
749.670515	52991.076944	33.073101
750.572561	53083.883042	33.078119
751.175289	53186.790939	33.083136
751.972017	53272.040133	33.088154
752.969093	53377.448897	33.093172
753.519972	53470.630812	33.098189
754.620970	53555.938316	33.103207
755.298551	53663.246337	33.108224
755.706045	53761.349874	33.113242
756.489190	53856.156864	33.118260
757.048600	53965.280435	33.123277
758.144799	54057.414561	33.128295
758.678698	54159.846112	33.133312
759.617640	54262.697705	33.138330
760.630791	54366.744360	33.143348
761.072477	54464.030673	33.148365
762.042406	54556.813537	33.153383
762.789194	54663.805955	33.158400
763.333865	54752.666841	33.163418
764.433252	54855.905684	33.168436
764.600536	54960.613495	33.173453
765.986306	55059.307250	33.178471
766.473695	55161.574765	33.183488
767.050294	55263.783821	33.188506
768.329716	55370.426574	33.193524
768.848010	55462.580702	33.198541
769.791568	55561.899831	33.203559
770.573181	55670.838088	33.208576
771.135678	55763.024211	33.213594
771.982674	55855.770307	33.218612
772.665399	55967.424673	33.223629
773.654287	56065.411866	33.228647
774.069580	56169.731169	33.233664
774.738820	56261.604957	33.238682
775.707484	56352.108980	33.243700
776.599065	56462.606801	33.248717
777.080966	56544.073909	33.253735
777.791834	56639.089421	33.258752
778.618194	56737.833494	33.263770
779.652224	56826.944983	33.268788
779.979043	56932.951152	33.273805
781.092108	57022.859292	33.278823
781.919906	57120.252716	33.283840
782.367195	57219.567404	33.288858
783.563748	57309.949607	33.293876
783.725856	57408.035910	33.298893
784.901123	57516.419907	33.303911
785.911062	57615.649813	33.308928
786.383473	57710.419162	33.313946
787.327629	57806.911964	33.318964
787.749679	57914.999298	33.323981
788.708471	58005.999036	33.328999
789.567034	58128.411089	33.334016
790.064162	58232.955105	33.339034
791.601691	58332.474142	33.344052
791.510352	58444.232434	33.349069
792.598353	58542.265917	33.354087
793.210962	58659.798878	33.359104
794.008325	58764.536139	33.364122
795.030458	58880.485918	33.369140
795.729101	58999.763519	33.374157
796.594298	59087.661649	33.379175
797.468881	59204.705743	33.384192
798.129409	59325.325057	33.389210
799.315043	59424.421056	33.394228
799.753085	59543.359450	33.399245
800.756547	59653.673029	33.404263
801.457773	59760.422145	33.409280
802.301711	59870.320887	33.414298
803.325926	59979.514157	33.419316
804.154584	60101.437497	33.424333
804.631203	60216.372809	33.429351
805.639256	60329.880988	33.434368
806.235430	60437.851876	33.439386
807.202710	60555.602617	33.444404
807.717046	60673.441594	33.449421
808.774909	60785.332396	33.454439
809.735275	60903.964820	33.459456
810.359863	61023.336076	33.464474
811.484124	61129.636858	33.469492
812.182596	61245.445099	33.474509
813.105018	61346.654482	33.479527
814.177775	61465.612887	33.484544
814.669279	61580.250029	33.489562
815.616587	61693.074254	33.494580
816.322558	61807.329560	33.499597
817.068094	61923.765919	33.504615
818.279687	62031.845700	33.509632
818.423042	62135.412730	33.514650
819.150019	62260.987569	33.519668
819.830852	62390.350667	33.524685
821.377982	62502.220497	33.529703
822.236459	62615.911482	33.534720
822.999640	62727.943806	33.539738
823.767957	62835.405826	33.544756
824.718940	62949.721771	33.549773
825.442254	63068.709330	33.554791
826.316324	63177.887610	33.559808
826.874059	63287.232566	33.564826
828.123395	63392.835378	33.569844
828.716849	63517.573957	33.574861
829.322529	63625.635894	33.579879
830.328034	63743.493416	33.584896
831.447290	63851.104956	33.589914
831.921133	63949.544111	33.594932
832.665958	64068.780394	33.599949
833.293489	64170.374817	33.604967
834.382964	64271.356015	33.609984
835.129565	64382.628831	33.615002
835.723782	64488.939799	33.620020
836.455253	64609.919803	33.625037
837.315038	64721.118816	33.630055
838.321742	64829.784457	33.635072
839.181548	64949.063666	33.640090
839.758329	65051.593742	33.645108
840.493267	65182.103221	33.650125
841.323815	65297.469815	33.655143
842.244249	65427.615098	33.660160
843.028994	65543.287748	33.665178
843.822555	65668.296927	33.670196
844.672042	65788.669994	33.675213
845.572383	65910.887660	33.680231
846.592412	66040.015097	33.685248
847.188429	66171.969842	33.690266
848.074167	66295.892782	33.695284
849.026674	66425.451012	33.700301
849.776322	66549.056562	33.705319
850.670865	66674.573449	33.710336
851.556714	66807.419925	33.715354
852.352408	66931.993724	33.720372
853.545581	67070.809783	33.725389
854.314390	67193.562443	33.730407
855.147812	67311.506483	33.735424
856.050292	67450.784071	33.740442
857.304732	67578.358489	33.745460
857.824059	67700.377699	33.750477
858.911474	67827.595576	33.755495
859.759112	67947.772652	33.760512
860.644086	68080.342767	33.765530
861.620813	68200.746508	33.770548
862.382998	68325.580643	33.775565
863.270828	68458.095742	33.780583
864.564316	68571.658655	33.785600
865.249880	68705.884268	33.790618
866.128700	68827.142356	33.795636
866.867879	68949.903768	33.800653
867.879816	69078.842465	33.805671
868.750406	69195.994160	33.810688
869.550389	69327.681935	33.815706
870.338376	69436.255753	33.820724
871.167946	69576.691150	33.825741
872.053206	69694.096072	33.830759
873.039212	69815.468512	33.835776
873.699179	69961.195279	33.840794
874.603536	70084.169849	33.845812
875.438256	70203.046569	33.850829
876.367995	70331.361452	33.855847
877.356720	70454.431687	33.860864
878.350795	70582.073486	33.865882
879.327475	70710.661099	33.870900
880.281018	70837.508056	33.875917
880.899610	70955.039863	33.880935
881.902651	71084.529598	33.885952
883.076424	71199.928453	33.890970
884.059015	71320.007328	33.895988
884.665742	71438.700938	33.901005
885.792036	71558.947083	33.906023
886.697614	71680.020853	33.911040
887.409054	71798.616916	33.916058
888.125985	71932.395903	33.921076
889.468356	72045.988119	33.926093
889.936588	72166.852372	33.931111
891.145515	72273.106991	33.936128
891.856614	72386.558764	33.941146
892.582962	72489.099955	33.946164
893.190301	72598.099027	33.951181
894.086319	72727.951467	33.956199
894.644194	72845.901994	33.961216
895.965988	72977.766095	33.966234
896.564127	73086.611037	33.971252
897.730887	73211.842994	33.976269
898.128091	73337.632976	33.981287
899.333720	73458.445700	33.986304
900.090297	73590.628329	33.991322
901.234940	73719.496935	33.996340
902.020793	73844.068230	34.001357
902.802808	73966.281911	34.006375
903.737666	74096.401694	34.011392
904.556674	74236.445357	34.016410
905.496853	74366.300241	34.021428
906.371688	74487.938609	34.026445
907.476784	74627.153225	34.031463
908.092807	74760.542508	34.036480
908.920922	74898.052756	34.041498
910.037338	75042.922282	34.046516
911.118514	75167.249862	34.051533
911.795734	75305.711004	34.056551
912.818115	75439.897356	34.061568
913.907295	75578.836011	34.066586
915.081975	75717.053025	34.071604
915.983398	75849.503579	34.076621
916.692494	75977.641551	34.081639
918.105953	76113.196738	34.086656
918.890648	76246.718906	34.091674
919.703192	76384.652105	34.096692
920.877800	76516.308797	34.101709
921.455662	76647.128848	34.106727
922.147195	76780.340729	34.111744
922.982054	76918.020546	34.116762
924.243655	77062.208820	34.121780
925.272119	77193.001839	34.126797
925.898346	77329.656068	34.131815
927.020502	77466.020388	34.136832
928.081039	77604.717125	34.141850
929.192206	77740.028607	34.146868
930.068838	77876.480313	34.151885
930.830540	78017.183576	34.156903
931.856548	78153.289670	34.161920
932.830002	78286.894052	34.166938
933.830284	78419.805309	34.171956
934.636771	78551.319817	34.176973
935.582414	78690.029625	34.181991
936.560472	78823.832536	34.187008
937.804439	78962.583252	34.192026
938.439563	79099.879373	34.197044
939.608097	79234.140308	34.202061
940.153975	79373.426497	34.207079
941.088507	79504.476266	34.212096
942.101210	79644.243605	34.217114
943.000805	79786.611493	34.222132
944.190922	79919.911396	34.227149
945.110245	80061.929827	34.232167
946.023708	80196.150095	34.237184
946.878115	80343.564495	34.242202
947.928482	80480.876247	34.247220
948.894442	80615.564775	34.252237
949.580316	80756.266030	34.257255
950.603744	80886.208331	34.262272
951.537832	81021.157582	34.267290
952.317153	81152.584162	34.272308
953.648108	81277.340874	34.277325
954.466559	81413.678064	34.282343
955.537640	81528.027930	34.287360
956.307435	81667.582176	34.292378
956.888168	81794.831871	34.297396
958.005031	81921.031986	34.302413
958.647448	82064.905432	34.307431
959.883002	82200.469763	34.312448
960.618560	82340.185608	34.317466
961.158346	82484.654382	34.322484
962.382625	82626.663661	34.327501
963.105645	82778.012761	34.332519
964.719412	82932.290390	34.337536
965.668254	83066.521672	34.342554
966.415810	83204.791937	34.347572
967.350331	83351.352015	34.352589
968.134225	83502.853981	34.357607
968.937860	83649.646384	34.362624
970.110907	83810.804296	34.367642
970.944430	83959.586743	34.372660
972.277796	84111.425748	34.377677
973.345314	84260.892729	34.382695
974.424168	84417.426294	34.387712
975.007862	84555.706413	34.392730
975.887664	84711.920550	34.397748
977.197438	84861.699338	34.402765
978.187773	85023.933567	34.407783
979.344244	85179.345805	34.412800
980.202516	85322.324308	34.417818
980.696462	85478.189770	34.422836
982.397779	85637.627840	34.427853
983.179308	85790.030953	34.432871
983.901025	85941.268009	34.437888
985.057663	86104.197258	34.442906
985.989480	86254.230972	34.447924
987.036543	86407.315546	34.452941
988.306551	86569.988827	34.457959
989.413782	86715.307584	34.462976
990.757978	86862.378843	34.467994
991.572068	87015.828622	34.473012
992.607860	87161.415059	34.478029
993.564915	87319.582810	34.483047
994.562628	87463.665017	34.488064
995.541395	87612.547914	34.493082
996.714373	87763.133537	34.498100
997.910686	87907.508341	34.503117
998.698409	88056.830621	34.508135
999.697505	88206.011309	34.513152
1001.051172	88352.191660	34.518170
1001.618455	88508.602924	34.523188
1002.970278	88648.134343	34.528205
1003.852899	88802.900655	34.533223
1004.968782	88950.370690	34.538240
1006.005186	89096.614400	34.543258
1006.778349	89241.421662	34.548276
1008.482422	89387.651682	34.553293
1009.298098	89541.016252	34.558311
1010.066010	89675.827848	34.563328
1011.183623	89820.024737	34.568346
1011.895300	89972.643497	34.573364
1012.946757	90111.562285	34.578381
1013.702413	90257.910136	34.583399
1014.847828	90420.377212	34.588416
1015.905642	90565.265645	34.593434
1016.511998	90719.469783	34.598452
1018.067004	90854.480617	34.603469
1018.586058	91019.466621	34.608487
1019.793301	91160.061862	34.613504
1020.836457	91295.830672	34.618522
1021.694218	91438.827067	34.623540
1023.021090	91568.917615	34.628557
1023.845184	91718.718701	34.633575
1024.902852	91847.310941	34.638592
1025.819205	92001.813767	34.643610
1026.896501	92143.866608	34.648628
1027.993832	92292.898191	34.653645
1029.012210	92430.418006	34.658663
1029.782397	92586.258883	34.663680
1031.106700	92729.337635	34.668698
1031.745899	92875.296477	34.673716
1032.998504	93028.870422	34.678733
1033.853186	93177.922213	34.683751
1034.792248	93329.486459	34.688768
1035.836152	93485.389082	34.693786
1036.946487	93644.275639	34.698804
1037.889031	93792.759630	34.703821
1038.796736	93959.283691	34.708839
1039.506708	94113.409889	34.713856
1040.707099	94270.500606	34.718874
1041.468819	94447.534283	34.723892
1042.528984	94602.871612	34.728909
1043.669779	94782.547882	34.733927
1044.901420	94951.740630	34.738944
1046.136491	95125.383982	34.743962
1047.224658	95300.875904	34.748980
1048.170693	95469.055953	34.753997
1049.299032	95635.080064	34.759015
1050.628779	95797.862569	34.764032
1052.037969	95961.588871	34.769050
1052.726416	96132.613967	34.774068
1053.578802	96288.451982	34.779085
1054.996363	96459.846205	34.784103
1055.909240	96622.468796	34.789120
1057.213394	96790.079455	34.794138
1058.407497	96962.450977	34.799156
1059.304817	97121.945786	34.804173
1060.397507	97296.191218	34.809191
1061.385724	97453.894212	34.814208
1062.708425	97618.601585	34.819226
1063.628528	97795.316318	34.824244
1065.091474	97950.031805	34.829261
1066.073651	98111.633328	34.834279
1066.709113	98283.726421	34.839296
1068.110403	98442.228296	34.844314
1069.289998	98614.233673	34.849332
1070.265938	98777.701773	34.854349
1071.161314	98937.683205	34.859367
1071.889785	99110.108406	34.864384
1073.395131	99284.919772	34.869402
1074.619026	99448.154928	34.874420
1075.429871	99614.219810	34.879437
1076.424071	99783.161482	34.884455
1077.255149	99955.999635	34.889472
1078.657984	100130.453875	34.894490
1079.644585	100301.147665	34.899508
1080.923807	100464.373841	34.904525
1082.116370	100644.906485	34.909543
1083.134093	100810.071191	34.914560
1084.345090	100968.480951	34.919578
1085.160748	101138.898333	34.924596
1086.335514	101300.842799	34.929613
1087.648987	101471.756253	34.934631
1088.426914	101652.959695	34.939648
1089.556996	101811.989529	34.944666
1090.561079	101983.204456	34.949684
1091.525940	102131.556587	34.954701
1092.708462	102281.906096	34.959719
1093.399359	102453.296213	34.964736
1094.831867	102607.829634	34.969754
1095.665965	102779.546482	34.974772
1096.629326	102939.775873	34.979789
1097.372714	103108.749145	34.984807
1098.937204	103278.163978	34.989824
1099.906512	103444.271641	34.994842
1100.866811	103627.010062	34.999860
1101.783617	103791.824190	35.004877
1103.108182	103960.510587	35.009895
1103.877442	104144.778609	35.014912
1105.307947	104314.462931	35.019930
1106.358227	104497.433169	35.024948
1106.813769	104689.862294	35.029965
1108.149738	104869.203743	35.034983
1109.230867	105069.384446	35.040000
1110.979131	105238.148302	35.045018
1111.498853	105434.384428	35.050036
1112.875863	105611.913015	35.055053
1114.286112	105800.772772	35.060071
1115.198316	106002.964253	35.065088
1116.495678	106179.559899	35.070106
1117.582375	106375.012637	35.075124
1118.590614	106560.461209	35.080141
1119.809749	106732.032503	35.085159
1120.962673	106936.800424	35.090176
1121.890577	107111.576106	35.095194
1123.090714	107308.840821	35.100212
1124.263823	107506.757429	35.105229
1125.732277	107689.427186	35.110247
1126.193719	107887.882241	35.115264
1127.728326	108080.778113	35.120282
1128.882400	108272.737623	35.125300
1129.668345	108470.649326	35.130317
1131.127117	108656.506558	35.135335
1131.686169	108861.057971	35.140352
1133.327469	109054.057156	35.145370
1134.952659	109258.080638	35.150388
1135.965822	109443.801599	35.155405
1136.945738	109645.933275	35.160423
1138.225781	109848.092837	35.165440
1139.170611	110025.823367	35.170458
1140.342692	110227.420891	35.175476
1141.647796	110425.146986	35.180493
1142.696238	110619.572695	35.185511
1143.625345	110827.675280	35.190528
1145.171667	111020.121364	35.195546
1146.000381	111223.733815	35.200564
1147.278632	111422.624311	35.205581
1148.756855	111623.446732	35.210599
1149.873594	111820.175220	35.215616
1150.959227	112005.812874	35.220634
1152.325826	112205.530506	35.225652
1153.461508	112406.453245	35.230669
1154.801371	112597.956321	35.235687
1155.643741	112793.736263	35.240704
1157.083443	112978.827818	35.245722
1157.825579	113172.511323	35.250740
1158.937187	113372.140130	35.255757
1160.444939	113563.178675	35.260775
1161.524422	113766.046185	35.265792
1162.798648	113942.480525	35.270810
1164.126263	114145.841866	35.275828
1164.936675	114342.651469	35.280845
1166.330389	114533.614122	35.285863
1167.433922	114724.689388	35.290880
1168.437191	114902.530174	35.295898
1169.596324	115087.390627	35.300916
1170.579292	115276.893185	35.305933
1171.950577	115456.450378	35.310951
1172.663939	115637.295768	35.315968
1173.810080	115826.065508	35.320986
1174.990691	116010.903091	35.326004
1175.865608	116221.740831	35.331021
1177.049977	116399.383678	35.336039
1178.238920	116605.940494	35.341056
1179.508090	116794.670969	35.346074
1180.632999	117002.837705	35.351092
1181.369617	117204.671501	35.356109
1183.021730	117391.910832	35.361127
1183.851895	117604.831466	35.366144
1185.570527	117804.847273	35.371162
1186.773118	118005.532637	35.376180
1187.822291	118210.996384	35.381197
1188.957180	118415.307022	35.386215
1189.902992	118629.090394	35.391232
1191.625604	118836.677387	35.396250
1192.678531	119048.317363	35.401268
1193.576222	119266.193560	35.406285
1194.905079	119467.932570	35.411303
1196.365709	119687.290129	35.416320
1197.281433	119892.141560	35.421338
1198.694495	120115.070949	35.426356
1199.560643	120333.112371	35.431373
1200.946604	120546.799011	35.436391
1202.170207	120761.920647	35.441408
1203.408284	120974.773135	35.446426
1205.070483	121190.002805	35.451444
1206.101822	121410.115817	35.456461
1207.389013	121617.705774	35.461479
1208.655222	121842.117161	35.466496
1209.823397	122057.029271	35.471514
1211.257002	122265.689406	35.476532
1212.169802	122475.438247	35.481549
1213.502023	122693.027145	35.486567
1214.817558	122917.996091	35.491584
1215.914859	123128.352666	35.496602
1217.037499	123350.872815	35.501620
1218.247620	123576.421747	35.506637
1220.118879	123782.954366	35.511655
1220.791942	124009.444434	35.516672
1222.113218	124220.671442	35.521690
1223.396441	124442.361998	35.526708
1224.719552	124666.113407	35.531725
1225.874475	124874.863070	35.536743
1227.091603	125095.010437	35.541760
1228.604847	125314.489421	35.546778
1229.799923	125527.178548	35.551796
1230.970544	125757.046767	35.556813
1232.299990	125954.507594	35.561831
1233.553077	126181.450279	35.566848
1234.768240	126403.508557	35.571866
1236.285409	126614.225470	35.576884
1237.643909	126826.845903	35.581901
1238.752496	127043.793177	35.586919
1239.956558	127260.916317	35.591936
1241.102027	127466.491130	35.596954
1242.410585	127674.600702	35.601972
1243.389612	127898.115684	35.606989
1244.907355	128112.556515	35.612007
1246.290433	128321.532688	35.617024
1247.412261	128536.561565	35.622042
1248.727894	128743.561681	35.627060
1249.785846	128959.757491	35.632077
1250.952807	129150.648923	35.637095
1251.917726	129350.739434	35.642112
1252.932389	129546.842803	35.647130
1254.618510	129752.622164	35.652148
1255.652227	129966.420489	35.657165
1256.728099	130170.211912	35.662183
1257.830978	130383.329794	35.667200
1258.765282	130607.733430	35.672218
1259.941076	130813.844893	35.677236
1261.145750	131042.123875	35.682253
1262.871636	131260.456061	35.687271
1263.968395	131484.927761	35.692288
1264.943625	131709.839453	35.697306
1266.721090	131928.940954	35.702324
1267.594407	132156.978422	35.707341
1269.184753	132381.679060	35.712359
1270.399570	132608.129375	35.717376
1271.601769	132831.528190	35.722394
1272.740449	133049.094878	35.727412
1273.951914	133291.320920	35.732429
1275.552951	133522.797379	35.737447
1276.590431	133758.133832	35.742464
1278.105298	133994.610122	35.747482
1279.521795	134218.376060	35.752500
1280.517546	134465.616115	35.757517
1282.212979	134682.797429	35.762535
1283.536421	134922.570260	35.767552
1284.489358	135164.421876	35.772570
1285.996387	135387.775131	35.777588
1287.394635	135629.417096	35.782605
1288.687089	135858.894518	35.787623
1290.228028	136094.684305	35.792640
1291.283015	136333.243911	35.797658
1292.768824	136561.920852	35.802676
1293.970886	136807.394694	35.807693
1295.154412	137034.540011	35.812711
1296.587110	137272.638188	35.817728
1297.882649	137518.951279	35.822746
1299.294517	137753.316043	35.827764
1300.496707	137999.965060	35.832781
1301.755370	138238.327064	35.837799
1303.408492	138474.394008	35.842816
1304.520624	138722.394502	35.847834
1306.159999	138944.443662	35.852852
1306.789417	139201.542496	35.857869
1308.321817	139437.090867	35.862887
1309.951155	139674.450717	35.867904
1310.766584	139919.212243	35.872922
1312.568213	140158.525018	35.877940
1313.797693	140399.734577	35.882957
1315.209343	140635.869064	35.887975
1316.248365	140877.151483	35.892992
1317.431818	141116.585765	35.898010
1319.587812	141357.648889	35.903028
1320.547667	141600.851479	35.908045
1321.867552	141833.116419	35.913063
1323.351388	142077.592550	35.918080
1324.605969	142327.307349	35.923098
1325.986557	142562.014471	35.928116
1327.437625	142808.479320	35.933133
1328.652554	143037.713525	35.938151
1330.210022	143280.613444	35.943168
1331.222597	143515.856951	35.948186
1332.686581	143748.820895	35.953204
1333.556875	143983.355516	35.958221
1334.800000	144225.793943	35.963239
1336.446459	144465.237956	35.968256
1337.761693	144704.446644	35.973274
1338.886905	144930.385356	35.978292
1340.547522	145171.645231	35.983309
1341.799088	145385.302758	35.988327
1342.874733	145606.092448	35.993344
1343.897614	145853.080343	35.998362
1345.384203	146069.518470	36.003380
1346.666510	146314.386797	36.008397
1347.977303	146543.817892	36.013415
1349.459160	146778.624794	36.018432
1350.472872	147022.045779	36.023450
1352.170397	147272.241920	36.028468
1353.217891	147512.198293	36.033485
1354.267691	147749.517881	36.038503
1356.134345	147999.678357	36.043520
1357.181871	148253.463663	36.048538
1358.892450	148487.939336	36.053556
1360.136380	148741.835050	36.058573
1361.345710	148992.554790	36.063591
1362.960199	149251.567414	36.068608
1363.975621	149500.749923	36.073626
1365.449895	149742.666862	36.078644
1366.785315	150010.241334	36.083661
1368.385330	150264.291504	36.088679
1369.780650	150521.662251	36.093696
1370.947314	150793.316228	36.098714
1372.176200	151047.242758	36.103732
1373.303852	151312.362128	36.108749
1374.755958	151582.300334	36.113767
1376.509745	151842.385902	36.118784
1377.674158	152120.150729	36.123802
1379.002123	152384.876620	36.128820
1380.729076	152654.929197	36.133837
1382.030409	152925.662858	36.138855
1383.734917	153185.093414	36.143872
1385.133285	153449.332987	36.148890
1386.848343	153701.560480	36.153908
1388.484790	153975.429935	36.158925
1389.807095	154235.006789	36.163943
1390.987032	154495.167029	36.168960
1391.941676	154746.448740	36.173978
1393.692684	155021.029634	36.178996
1394.984728	155285.844670	36.184013
1396.010974	155560.067061	36.189031
1398.033279	155832.972392	36.194048
1399.156109	156113.436486	36.199066
1400.866922	156369.284457	36.204084
1401.754418	156636.128924	36.209101
1403.136523	156917.431130	36.214119
1405.263700	157179.532915	36.219136
1406.077541	157450.175309	36.224154
1407.398028	157724.338577	36.229172
1409.177987	158003.603641	36.234189
1410.373509	158278.209951	36.239207
1412.098977	158541.718999	36.244224
1413.360546	158824.158098	36.249242
1414.642544	159091.993863	36.254260
1415.967824	159369.656161	36.259277
1417.186437	159652.044636	36.264295
1418.865659	159922.103736	36.269312
1420.303348	160198.547827	36.274330
1421.531410	160474.622430	36.279348
1422.925821	160763.155182	36.284365
1424.177369	161045.357413	36.289383
1425.859003	161316.046840	36.294400
1427.117237	161614.529180	36.299418
1428.815444	161888.340576	36.304436
1430.479737	162162.514600	36.309453
1431.698012	162434.099774	36.314471
1433.371120	162689.676184	36.319488
1434.870950	162951.182431	36.324506
1435.969369	163204.852286	36.329524
1437.149633	163468.381077	36.334541
1438.522057	163730.230337	36.339559
1439.964057	163995.431952	36.344576
1441.214631	164261.796050	36.349594
1442.276259	164541.210817	36.354612
1444.075801	164819.147832	36.359629
1445.332363	165101.541052	36.364647
1446.707530	165374.400378	36.369664
1447.955718	165669.436065	36.374682
1449.185033	165947.398362	36.379700
1450.530039	166240.201427	36.384717
1452.029024	166528.184738	36.389735
1453.674194	166822.198220	36.394752
1454.627666	167136.350660	36.399770
1456.078186	167435.805734	36.404788
1457.916301	167742.812070	36.409805
1459.195633	168040.789504	36.414823
1460.635557	168344.579318	36.419840
1462.107087	168656.436217	36.424858
1463.657541	168967.279776	36.429876
1465.075710	169277.462097	36.434893
1466.360156	169585.435295	36.439911
1467.921038	169899.075135	36.444928
1469.375616	170210.615529	36.449946
1470.957599	170531.755703	36.454964
1472.354424	170853.423598	36.459981
1473.737306	171173.420972	36.464999
1475.464369	171484.620343	36.470016
1476.738329	171820.680152	36.475034
1478.707364	172141.399446	36.480052
1480.099358	172457.787412	36.485069
1481.370956	172784.171902	36.490087
1483.286692	173105.274551	36.495104
1484.806674	173432.916858	36.500122
1486.283956	173755.657244	36.505140
1487.925198	174074.628989	36.510157
1489.636034	174402.703232	36.515175
1491.169994	174716.836421	36.520192
1492.407459	175036.591900	36.525210
1494.089306	175347.938126	36.530228
1495.864122	175676.924124	36.535245
1497.158414	175994.277867	36.540263
1498.896334	176310.862335	36.545280
1500.257834	176630.531533	36.550298
1501.552004	176950.505811	36.555316
1503.772565	177252.396137	36.560333
1504.987221	177580.649674	36.565351
1506.419591	177900.124899	36.570368
1508.206962	178213.146905	36.575386
1509.634973	178531.256136	36.580404
1511.400784	178851.596060	36.585421
1512.588045	179167.502588	36.590439
1514.383879	179464.183751	36.595456
1515.920873	179788.082993	36.600474
1517.219676	180097.554628	36.605492
1518.565896	180411.462530	36.610509
1519.967748	180742.104204	36.615527
1521.806181	181056.708880	36.620544
1523.006454	181379.937481	36.625562
1524.413370	181702.803912	36.630580
1526.211289	182020.479910	36.635597
1527.687407	182348.822014	36.640615
1529.417942	182663.758673	36.645632
1530.926714	182975.002141	36.650650
1532.505462	183289.002885	36.655668
1534.176632	183589.599140	36.660685
1535.522863	183908.274802	36.665703
1537.098772	184204.904588	36.670720
1538.598693	184509.456359	36.675738
1540.195287	184799.383960	36.680756
1542.032763	185085.351062	36.685773
1542.961875	185398.328825	36.690791
1544.434545	185699.756386	36.695808
1545.880504	186000.885339	36.700826
1547.317664	186309.113053	36.705844
1549.248939	186624.876983	36.710861
1550.588599	186936.018367	36.715879
1552.114197	187252.690595	36.720896
1553.444781	187567.188071	36.725914
1555.012286	187882.282819	36.730932
1556.587851	188203.763021	36.735949
1557.438996	188539.264667	36.740967
1558.901861	188865.857462	36.745984
1560.431129	189195.424241	36.751002
1562.493030	189542.169056	36.756020
1563.741582	189868.091945	36.761037
1565.449349	190215.495843	36.766055
1566.688459	190565.860839	36.771072
1568.372910	190908.753380	36.776090
1569.790238	191251.514280	36.781108
1571.764941	191596.749358	36.786125
1573.116752	191958.287826	36.791143
1574.611883	192300.838656	36.796160
1576.085111	192655.962971	36.801178
1577.631697	193012.854501	36.806196
1579.338300	193370.813415	36.811213
1580.822874	193730.689937	36.816231
1582.588036	194096.476210	36.821248
1584.052895	194460.714606	36.826266
1585.781143	194812.051184	36.831284
1587.602628	195174.774770	36.836301
1589.098045	195533.326673	36.841319
1590.798325	195898.346842	36.846336
1592.553313	196265.238971	36.851354
1594.083886	196620.985320	36.856372
1595.787776	196975.321117	36.861389
1597.088161	197344.389161	36.866407
1598.949376	197705.482436	36.871424
1600.632786	198080.204420	36.876442
1602.506889	198442.086671	36.881460
1603.982690	198794.578052	36.886477
1605.785959	199161.452704	36.891495
1607.375235	199525.406443	36.896512
1609.173293	199890.635327	36.901530
1610.576444	200247.374010	36.906548
1612.538423	200599.413383	36.911565
1614.088895	200966.745607	36.916583
1615.611726	201321.781325	36.921600
1616.867452	201680.633836	36.926618
1618.390225	202055.048266	36.931636
1620.410455	202410.705517	36.936653
1622.168603	202781.834446	36.941671
1623.762158	203142.377850	36.946688
1625.458074	203501.864958	36.951706
1626.849646	203875.180345	36.956724
1628.455426	204239.777411	36.961741
1629.976525	204606.205926	36.966759
1631.627861	204975.509661	36.971776
1633.328300	205332.617706	36.976794
1634.928566	205702.098453	36.981812
1636.700028	206071.819330	36.986829
1638.334070	206435.520686	36.991847
1639.967339	206800.925323	36.996864
1641.624299	207145.973560	37.001882
1642.915692	207499.311737	37.006900
1644.339105	207837.582934	37.011917
1646.316782	208199.127790	37.016935
1647.941815	208548.771211	37.021952
1649.268009	208887.278710	37.026970
1650.719815	209258.870227	37.031988
1652.379275	209609.426718	37.037005
1653.895886	209976.223613	37.042023
1655.374392	210329.593872	37.047040
1657.138771	210699.476702	37.052058
1658.913898	211072.305332	37.057076
1660.565527	211438.578307	37.062093
1662.071157	211809.499115	37.067111
1663.750319	212197.205406	37.072128
1665.404629	212564.600110	37.077146
1667.280115	212949.889976	37.082164
1668.895039	213336.088038	37.087181
1670.488098	213708.805521	37.092199
1672.124293	214097.543019	37.097216
1673.917377	214477.113225	37.102234
1675.389605	214867.455684	37.107252
1677.263991	215252.095098	37.112269
1678.833358	215653.904445	37.117287
1680.523008	216048.228694	37.122304
1682.577737	216434.570139	37.127322
1683.850451	216832.572953	37.132340
1685.890302	217230.831633	37.137357
1687.249894	217621.661049	37.142375
1689.157446	218023.703683	37.147392
1690.608580	218427.677392	37.152410
1692.263000	218824.964740	37.157428
1693.937355	219233.400275	37.162445
1695.865403	219644.360770	37.167463
1697.000230	220051.821886	37.172480
1699.203498	220459.768445	37.177498
1700.859546	220873.724894	37.182516
1702.710492	221277.084745	37.187533
1704.074652	221701.912526	37.192551
1705.583087	222113.231132	37.197568
1707.853852	222529.454382	37.202586
1709.374580	223019.334265	37.207604
1711.118072	223444.842527	37.212621
1712.947938	223862.515009	37.217639
1714.673469	224278.428229	37.222656
1716.672516	224683.426629	37.227674
1717.979454	225108.098583	37.232692
1719.935842	225523.876365	37.237709
1722.024489	225941.386298	37.242727
1723.478762	226352.728585	37.247744
1725.482123	226775.157585	37.252762
1726.764056	227196.132321	37.257780
1728.745043	227611.100069	37.262797
1730.001388	228030.303683	37.267815
1731.820091	228456.400858	37.272832
1733.945021	228883.210807	37.277850
1735.506244	229316.947965	37.282868
1737.485806	229737.002577	37.287885
1739.105841	230159.607097	37.292903
1740.748339	230591.378866	37.297920
1742.966708	231006.774779	37.302938
1744.547649	231435.866690	37.307956
1746.279122	231846.519164	37.312973
1747.864750	232277.314551	37.317991
1749.368137	232709.394777	37.323008
1751.385121	233114.364365	37.328026
1752.382655	233547.267051	37.333044
1754.375210	233958.034295	37.338061
1756.411356	234384.188661	37.343079
1757.986128	234790.937310	37.348096
1760.400525	235191.401050	37.353114
1761.534516	235605.641684	37.358132
1763.280232	236003.423527	37.363149
1764.865354	236422.265449	37.368167
1766.659363	236837.365149	37.373184
1768.637795	237240.242392	37.378202
1769.943106	237662.435536	37.383220
1771.850863	238080.465764	37.388237
1773.459460	238503.601289	37.393255
1775.187189	238940.231941	37.398272
1777.183384	239359.317073	37.403290
1778.871109	239794.457374	37.408308
1780.767107	240224.763116	37.413325
1782.425798	240653.965778	37.418343
1784.284274	241100.714685	37.423360
1786.161586	241533.718628	37.428378
1787.631364	241975.757727	37.433396
1789.400735	242412.667637	37.438413
1791.273983	242857.740763	37.443431
1792.951820	243301.271962	37.448448
1794.977406	243751.732184	37.453466
1796.751523	244197.560581	37.458484
1798.568401	244656.820646	37.463501
1800.266325	245103.806145	37.468519
1801.983836	245565.421068	37.473536
1804.004126	246014.183640	37.478554
1805.571912	246474.325834	37.483572
1806.841230	246941.325921	37.488589
1809.269585	247400.920774	37.493607
1810.726231	247871.955598	37.498624
1812.691962	248343.770623	37.503642
1814.800674	248817.848861	37.508660
1816.826136	249289.020033	37.513677
1818.703262	249748.784825	37.518695
1820.301413	250228.715395	37.523712
1822.363467	250687.154990	37.528730
1824.216749	251163.157633	37.533748
1825.926503	251625.974746	37.538765
1827.883712	252087.074744	37.543783
1829.239312	252566.005864	37.548800
1831.341425	253045.906370	37.553818
1833.661685	253523.510270	37.558836
1835.432790	253996.683366	37.563853
1837.603616	254462.474560	37.568871
1839.352599	254941.977190	37.573888
1841.232059	255403.066503	37.578906
1843.130836	255882.925815	37.583924
1845.353745	256330.647389	37.588941
1847.113993	256814.772194	37.593959
1848.764187	257278.440211	37.598976
1850.939357	257746.594190	37.603994
1852.805251	258215.891630	37.609012
1854.483427	258681.155558	37.614029
1856.769104	259139.688889	37.619047
1858.194871	259613.809407	37.624064
1859.920845	260069.158057	37.629082
1861.788927	260542.062239	37.634100
1863.960425	261017.659759	37.639117
1866.125488	261485.789640	37.644135
1867.945834	261952.604513	37.649152
1869.989693	262414.301641	37.654170
1871.674881	262877.048524	37.659188
1873.714610	263335.443483	37.664205
1875.438868	263789.774971	37.669223
1877.165748	264253.479542	37.674240
1879.568649	264693.828258	37.679258
1881.386770	265136.686552	37.684276
1883.177892	265572.156671	37.689293
1885.114531	266003.512529	37.694311
1886.934466	266439.536087	37.699328
1888.581340	266869.389503	37.704346
1890.419299	267296.772292	37.709364
1892.482743	267734.939149	37.714381
1894.302100	268177.794633	37.719399
1895.733473	268622.771365	37.724416
1897.731858	269059.728251	37.729434
1899.765595	269512.885877	37.734452
1901.720539	269961.356426	37.739469
1903.538174	270400.831069	37.744487
1905.393129	270872.484376	37.749504
1907.350809	271314.830625	37.754522
1909.251315	271765.644822	37.759540
1910.896744	272232.631210	37.764557
1912.759174	272696.177073	37.769575
1914.556254	273154.423831	37.774592
1916.378209	273616.984170	37.779610
1918.369610	274091.277121	37.784628
1920.219641	274569.402934	37.789645
1922.322191	275050.509044	37.794663
1924.090537	275520.035102	37.799680
1925.964807	276001.989906	37.804698
1927.826592	276484.657043	37.809716
1929.781822	276973.404265	37.814733
1931.609821	277457.217990	37.819751
1933.754474	277948.725992	37.824768
1935.814698	278438.011406	37.829786
1937.652857	278929.720109	37.834804
1939.783094	279424.402208	37.839821
1941.573840	279919.418533	37.844839
1943.684516	280398.707826	37.849856
1945.432993	280901.018879	37.854874
1947.514393	281400.860417	37.859892
1949.294538	281898.692770	37.864909
1951.735726	282396.516157	37.869927
1953.620752	282906.495624	37.874944
1955.414727	283399.317239	37.879962
1957.709746	283906.457182	37.884980
1959.666694	284407.529654	37.889997
1962.045880	284897.684527	37.895015
1963.632693	285408.518144	37.900032
1965.873710	285900.724711	37.905050
1968.109979	286403.649614	37.910068
1970.442587	286904.524819	37.915085
1972.316232	287391.529073	37.920103
1974.018622	287883.411446	37.925120
1976.395259	288372.462894	37.930138
1978.408625	288862.004383	37.935156
1980.249252	289360.767541	37.940173
1982.193764	289845.236725	37.945191
1984.345733	290339.829918	37.950208
1986.140538	290829.984368	37.955226
1988.180315	291320.579068	37.960244
1990.320109	291821.162867	37.965261
1992.479698	292302.945534	37.970279
1994.230162	292807.475723	37.975296
1996.005330	293293.102436	37.980314
1998.331264	293791.462920	37.985332
2000.045250	294280.803939	37.990349
2002.371913	294770.651283	37.995367
2004.213227	295269.669515	38.000384
2006.456616	295750.535035	38.005402
2008.457946	296251.782917	38.010420
2010.404294	296744.808358	38.015437
2012.540139	297223.221412	38.020455
2014.717744	297688.316570	38.025472
2016.278050	298146.019039	38.030490
2018.673999	298609.219929	38.035508
2020.157942	299078.029902	38.040525
2021.970519	299537.767117	38.045543
2023.991923	300007.728505	38.050560
2025.787980	300477.953436	38.055578
2028.242664	300955.534278	38.060596
2029.692839	301430.764238	38.065613
2032.097388	301911.802655	38.070631
2033.921899	302399.486888	38.075648
2035.892356	302880.185640	38.080666
2037.750001	303371.211711	38.085684
2039.642924	303871.499182	38.090701
2041.414296	304369.822994	38.095719
2043.461539	304872.619070	38.100736
2045.654115	305378.105705	38.105754
2047.524225	305890.829808	38.110772
2049.478885	306402.622640	38.115789
2051.954510	306925.500639	38.120807
2053.494495	307442.993570	38.125824
2055.483445	307955.304633	38.130842
2057.906977	308487.882602	38.135860
2059.680923	309018.532714	38.140877
2061.835954	309536.215659	38.145895
2063.927864	310072.926565	38.150912
2065.845622	310606.005725	38.155930
2067.971635	311136.456617	38.160948
2070.039469	311692.257219	38.165965
2072.386620	312222.435588	38.170983
2074.106968	312761.068419	38.176000
2076.474508	313310.382987	38.181018
2078.789448	313854.547250	38.186036
2080.628637	314405.032866	38.191053
2082.866645	314944.681688	38.196071
2085.158158	315495.820778	38.201088
2087.318429	316037.911986	38.206106
2089.700838	316583.212662	38.211124
2091.400499	317131.872078	38.216141
2093.627497	317675.133097	38.221159
2095.653981	318227.030905	38.226176
2097.910957	318785.894401	38.231194
2100.067034	319328.823888	38.236212
2102.219842	319884.673848	38.241229
2104.558381	320431.703080	38.246247
2106.642589	320983.568690	38.251264
2108.468674	321533.314020	38.256282
2110.910845	322090.341683	38.261300
2113.461409	322648.768487	38.266317
2115.316142	323194.356207	38.271335
2117.676014	323743.816673	38.276352
2119.419635	324293.805672	38.281370
2121.849145	324838.141629	38.286388
2123.935863	325398.397734	38.291405
2126.237938	325937.463965	38.296423
2128.506898	326495.648735	38.301440
2130.672426	327036.047905	38.306458
2133.105802	327579.749233	38.311476
2134.512477	328141.209094	38.316493
2136.893417	328676.937033	38.321511
2139.264645	329219.922541	38.326528
2141.456253	329770.117258	38.331546
2143.155411	330323.205968	38.336564
2144.889789	330877.679767	38.341581
2147.439988	331424.981304	38.346599
2149.867089	331971.434664	38.351616
2151.799335	332525.529446	38.356634
2154.035408	333061.189022	38.361652
2155.704937	333603.562564	38.366669
2158.361522	334128.099429	38.371687
2160.290121	334654.680644	38.376704
2162.099695	335178.001661	38.381722
2164.657375	335696.167853	38.386740
2166.572165	336221.415833	38.391757
2168.123212	336755.044642	38.396775
2170.610351	337296.915576	38.401792
2172.422923	337836.353814	38.406810
2174.883382	338379.639268	38.411828
2176.508144	338933.489384	38.416845
2179.168633	339480.664458	38.421863
2180.942552	340041.331202	38.426880
2182.943578	340595.354761	38.431898
2185.435113	341153.352306	38.436916
2187.411656	341716.276470	38.441933
2189.696281	342281.579936	38.446951
2192.246804	342860.005783	38.451968
2194.282503	343424.397916	38.456986
2196.646947	343984.947444	38.462004
2198.520852	344564.733470	38.467021
2200.756428	345145.772462	38.472039
2203.163130	345722.258455	38.477056
2205.219881	346302.297451	38.482074
2207.853190	346887.259081	38.487092
2209.746493	347475.406261	38.492109
2211.951962	348059.078529	38.497127
2214.262108	348637.828073	38.502144
2216.303292	349237.906510	38.507162
2218.649326	349819.071224	38.512180
2221.148146	350419.540461	38.517197
2223.521540	351007.080153	38.522215
2225.819127	351598.354848	38.527232
2227.705300	352191.541914	38.532250
2230.099636	352783.342859	38.537268
2232.388823	353385.328559	38.542285
2234.590259	353991.025051	38.547303
2237.172840	354594.239451	38.552320
2239.319664	355192.467720	38.557338
2241.713722	355780.624009	38.562356
2243.971606	356392.239647	38.567373
2246.448844	356994.472778	38.572391
2249.002237	357586.357853	38.577408
2250.880505	358186.109795	38.582426
2253.348656	358783.776559	38.587444
2255.620335	359384.080240	38.592461
2258.051542	359981.557825	38.597479
2260.330703	360579.051614	38.602496
2262.390990	361177.841109	38.607514
2265.161241	361775.058290	38.612532
2267.132132	362379.349674	38.617549
2269.661652	362973.112737	38.622567
2272.008209	363569.560698	38.627584
2274.053226	364165.465772	38.632602
2276.378123	364763.218056	38.637620
2278.626448	365358.792025	38.642637
2280.873231	365956.919049	38.647655
2283.091679	366560.824986	38.652672
2285.244854	367166.938911	38.657690
2287.920527	367766.488425	38.662708
2290.376434	368381.994262	38.667725
2292.170188	368980.274629	38.672743
2294.863002	369578.320810	38.677760
2296.730778	370181.997498	38.682778
2299.311719	370778.825003	38.687796
2301.354439	371372.358143	38.692813
2303.539477	371983.942032	38.697831
2306.235973	372572.528451	38.702848
2308.489900	373161.076752	38.707866
2310.600596	373730.947138	38.712884
2313.080105	374301.102525	38.717901
2315.184888	374867.252716	38.722919
2317.753274	375435.067126	38.727936
2319.590960	376017.017141	38.732954
2322.049497	376589.573182	38.737972
2324.058527	377166.378213	38.742989
2326.358683	377754.739953	38.748007
2328.583681	378335.344210	38.753024
2331.068807	378930.476575	38.758042
2333.229656	379532.168912	38.763060
2335.527205	380130.049684	38.768077
2337.513535	380743.489512	38.773095
2339.942087	381333.466486	38.778112
2342.501834	381951.784562	38.783130
2344.995162	382555.091583	38.788148
2347.188383	383179.760550	38.793165
2349.320202	383798.469391	38.798183
2352.087109	384412.776810	38.803200
2353.999829	385038.901473	38.808218
2356.555453	385653.980701	38.813236
2359.047080	386289.213907	38.818253
2361.020185	386915.443987	38.823271
2363.645150	387537.497872	38.828288
2366.077486	388183.122339	38.833306
2368.154965	388818.246279	38.838324
2370.901322	389467.645681	38.843341
2373.178736	390110.087097	38.848359
2375.544967	390751.233053	38.853376
2378.209452	391405.598955	38.858394
2380.179451	392053.956642	38.863412
2382.603837	392698.955739	38.868429
2385.087925	393348.747129	38.873447
2387.688366	394000.380927	38.878464
2389.809811	394661.989750	38.883482
2391.924240	395326.347680	38.888500
2394.657456	395980.172056	38.893517
2397.524343	396638.116315	38.898535
2400.057139	397292.704977	38.903552
2402.034920	397969.748270	38.908570
2404.606055	398618.826843	38.913588
2407.011994	399280.766356	38.918605
2409.347575	399955.144749	38.923623
2411.829396	400621.399575	38.928640
2414.417498	401285.036668	38.933658
2416.835542	401949.294483	38.938676
2419.511836	402624.034988	38.943693
2421.918031	403287.275089	38.948711
2424.735739	403944.629325	38.953728
2427.256541	404613.444003	38.958746
2429.950656	405271.522089	38.963764
2432.078268	405936.771982	38.968781
2434.355494	406602.893182	38.973799
2437.382102	407245.136183	38.978816
2439.633077	407914.244581	38.983834
2442.030402	408573.153742	38.988852
2444.742958	409234.325437	38.993869
2447.290169	409888.288570	38.998887
2449.885329	410528.295596	39.003904
2452.135043	411206.264390	39.008922
2454.748800	411841.550611	39.013940
2457.326620	412490.708075	39.018957
2459.469196	413146.405553	39.023975
2462.224256	413805.227600	39.028992
2464.517126	414448.887413	39.034010
2467.467566	415098.982488	39.039028
2469.805169	415733.789282	39.044045
2472.011883	416353.178689	39.049063
2474.616655	416962.787967	39.054080
2476.976673	417573.208170	39.059098
2479.055378	418184.419895	39.064116
2481.126729	418816.864373	39.069133
2483.553473	419443.460838	39.074151
2486.368871	420060.811020	39.079168
2488.371659	420699.955213	39.084186
2491.012378	421323.101703	39.089204
2493.400810	421967.669720	39.094221
2495.411726	422611.827526	39.099239
2497.926576	423254.011803	39.104256
2500.316120	423915.543033	39.109274
2502.418621	424582.116616	39.114292
2505.293354	425249.607888	39.119309
2507.334778	425916.661365	39.124327
2509.671474	426582.533875	39.129344
2512.160148	427270.437267	39.134362
2514.727953	427960.181125	39.139380
2517.701522	428644.522380	39.144397
2519.424972	429344.541421	39.149415
2522.149474	430032.478164	39.154432
2524.552960	430738.165477	39.159450
2526.987831	431444.484507	39.164468
2529.604402	432156.674657	39.169485
2532.151424	432884.394017	39.174503
2534.280498	433591.660211	39.179520
2536.855309	434313.053798	39.184538
2539.473670	435049.550731	39.189556
2542.039527	435781.578927	39.194573
2544.286694	436516.267921	39.199591
2547.244396	437258.002232	39.204608
2549.807112	437995.981975	39.209626
2552.308986	438735.313924	39.214644
2555.288457	439488.559645	39.219661
2557.416569	440241.110840	39.224679
2560.112823	440983.018263	39.229696
2562.877801	441737.235299	39.234714
2565.216495	442490.484993	39.239732
2568.106750	443230.716439	39.244749
2570.440306	444002.584254	39.249767
2573.163569	444752.252453	39.254784
2576.350706	445519.878406	39.259802
2578.823254	446270.344878	39.264820
2581.691227	447024.665612	39.269837
2584.225068	447792.621860	39.274855
2587.155006	448540.910117	39.279872
2589.825897	449291.490882	39.284890
2592.464397	450039.521512	39.289908
2595.208508	450784.675947	39.294925
2597.742360	451537.273090	39.299943
2600.598769	452285.390166	39.304960
2603.316279	453020.354929	39.309978
2605.875062	453777.064526	39.314996
2609.008987	454512.312264	39.320013
2611.335430	455254.695564	39.325031
2614.288674	455987.493259	39.330048
2616.876665	456729.274374	39.335066
2619.180405	457471.732662	39.340084
2622.045576	458202.695644	39.345101
2624.670244	458940.193626	39.350119
2627.432943	459682.950047	39.355136
2630.285651	460416.514151	39.360154
2632.592828	461156.055756	39.365172
2635.313246	461885.290913	39.370189
2637.877197	462628.425470	39.375207
2640.335058	463367.000566	39.380224
2643.223031	464090.010861	39.385242
2645.431338	464801.987583	39.390260
2648.452575	465493.487457	39.395277
2650.618428	466203.600672	39.400295
2653.350282	466911.825821	39.405312
2656.083896	467607.896634	39.410330
2658.456250	468325.073803	39.415348
2661.280158	469028.152878	39.420365
2663.315098	469748.667514	39.425383
2665.749835	470463.783749	39.430400
2668.424852	471190.302535	39.435418
2670.978567	471928.635764	39.440436
2673.649518	472656.766178	39.445453
2676.240242	473397.713386	39.450471
2678.668527	474137.546767	39.455488
2681.426123	474891.440628	39.460506
2684.000178	475647.001168	39.465524
2686.426545	476389.624647	39.470541
2688.976703	477166.291051	39.475559
2691.841361	477936.357552	39.480576
2694.362534	478705.842370	39.485594
2696.885575	479489.435071	39.490612
2699.811454	480266.413180	39.495629
2702.533430	481055.612108	39.500647
2705.262746	481845.936809	39.505664
2707.835200	482639.635792	39.510682
2710.319347	483439.070249	39.515700
2713.236091	484244.102872	39.520717
2716.024730	485047.706675	39.525735
2718.759171	485853.706317	39.530752
2721.653922	486673.676752	39.535770
2724.394891	487485.204385	39.540788
2727.377465	488283.732571	39.545805
2729.937259	489112.982726	39.550823
2732.334148	489919.356382	39.555840
2735.782140	490738.439597	39.560858
2738.358723	491570.396102	39.565876
2741.567848	492379.297001	39.570893
2744.197186	493204.655883	39.575911
2746.916832	494017.698257	39.580928
2749.878141	494841.712348	39.585946
2752.522967	495667.050572	39.590964
2755.648454	496490.402576	39.595981
2758.311281	497325.142126	39.600999
2760.947154	498142.389702	39.606016
2763.898269	498970.946168	39.611034
2766.258569	499804.956408	39.616052
2769.215879	500628.032142	39.621069
2772.259478	501470.067953	39.626087
2774.977873	502298.345641	39.631104
2777.832350	503124.491497	39.636122
2780.706936	503969.100412	39.641140
2783.368720	504790.100627	39.646157
2786.217536	505630.442368	39.651175
2789.004117	506470.397951	39.656192
2791.798736	507295.989352	39.661210
2794.449657	508146.922155	39.666228
2797.228610	508977.270020	39.671245
2800.034055	509825.013071	39.676263
2802.735570	510659.420164	39.681280
2805.604483	511503.030741	39.686298
2808.444266	512354.514677	39.691316
2811.445056	513186.924861	39.696333
2813.930777	514028.246160	39.701351
2816.772430	514879.593254	39.706368
2820.077157	515722.301178	39.711386
2822.370555	516561.804547	39.716404
2825.645196	517412.639529	39.721421
2828.388417	518241.597898	39.726439
2831.200879	519051.758067	39.731456
2834.152986	519857.872527	39.736474
2836.484727	520666.918399	39.741492
2839.261696	521472.019559	39.746509
2841.746926	522277.529252	39.751527
2844.499451	523093.529643	39.756544
2847.453828	523911.568139	39.761562
2850.295750	524732.552274	39.766580
2853.009542	525550.188901	39.771597
2855.787998	526377.892245	39.776615
2858.179392	527213.368281	39.781632
2861.160941	528050.261060	39.786650
2864.172773	528899.487656	39.791668
2866.743858	529745.918781	39.796685
2869.599175	530602.574931	39.801703
2872.151655	531465.825742	39.806720
2875.027492	532323.384879	39.811738
2877.637012	533206.557998	39.816756
2880.599964	534075.023047	39.821773
2883.675000	534965.360939	39.826791
2886.108358	535860.933353	39.831808
2889.272097	536754.920645	39.836826
2891.922963	537661.768272	39.841844
2894.600239	538546.867858	39.846861
2897.505283	539470.666247	39.851879
2900.272255	540381.447496	39.856896
2903.278030	541304.808031	39.861914
2906.246404	542233.295567	39.866932
2909.137235	543165.205309	39.871949
2912.367712	544113.645203	39.876967
2914.849698	545042.881964	39.881984
2918.244133	545975.024229	39.887002
2920.910417	546914.766886	39.892020
2923.912309	547867.765575	39.897037
2926.847018	548812.865898	39.902055
2929.189699	549764.534680	39.907072
2932.530011	550726.429448	39.912090
2935.859947	551686.951122	39.917108
2938.345801	552653.073283	39.922125
2941.459919	553623.094158	39.927143
2944.476250	554585.774076	39.932160
2947.784969	555549.643528	39.937178
2950.347905	556527.486110	39.942196
2953.548877	557500.830714	39.947213
2956.359204	558472.761785	39.952231
2959.300790	559458.064266	39.957248
2962.416712	560428.193855	39.962266
2965.403201	561418.768111	39.967284
2968.525140	562402.414297	39.972301
2971.423161	563382.809131	39.977319
2973.985209	564372.777876	39.982336
2977.038314	565346.320004	39.987354
2980.290716	566365.199032	39.992372
2983.116919	567350.980127	39.997389
2986.157037	568351.661856	40.002407
2988.913200	569359.591544	40.007424
2991.961345	570347.013476	40.012442
2995.035935	571353.779425	40.017460
2998.263916	572339.310459	40.022477
3001.325790	573343.461194	40.027495
3004.194664	574351.879429	40.032512
3007.444281	575340.384022	40.037530
3010.083855	576356.155483	40.042548
3012.736067	577358.547322	40.047565
3016.427039	578366.205371	40.052583
3019.124636	579381.118404	40.057600
3022.291174	580376.760887	40.062618
3025.431720	581377.442830	40.067636
3028.107864	582340.959229	40.072653
3031.485781	583295.859678	40.077671
3034.243845	584271.796847	40.082688
3037.419121	585226.779929	40.087706
3039.745115	586200.126531	40.092724
3042.842973	587166.149154	40.097741
3046.372293	588137.787618	40.102759
3049.150043	589115.736554	40.107776
3052.022904	590087.826481	40.112794
3055.324688	591064.527286	40.117812
3058.206953	592044.674611	40.122829
3061.506155	593032.989618	40.127847
3064.066476	594026.153499	40.132864
3067.183976	595023.400052	40.137882
3070.249007	596022.874865	40.142900
3073.169052	597028.198665	40.147917
3076.551081	598045.680275	40.152935
3079.261860	599060.379180	40.157952
3082.782892	600087.274282	40.162970
3085.876188	601106.888549	40.167988
3088.773658	602134.255178	40.173005
3092.244231	603159.933657	40.178023
3094.629957	604195.810594	40.183040
3098.032745	605224.919135	40.188058
3101.185170	606266.687995	40.193076
3104.072709	607320.665395	40.198093
3107.389992	608364.566160	40.203111
3110.169941	609419.816475	40.208128
3113.391022	610468.891515	40.213146
3116.493589	611542.199592	40.218164
3119.634339	612603.943770	40.223181
3123.138341	613680.331081	40.228199
3126.121980	614754.649323	40.233216
3129.211128	615823.695299	40.238234
3132.392277	616910.872392	40.243252
3135.609007	617989.136915	40.248269
3138.780567	619064.403282	40.253287
3141.569437	620160.820483	40.258304
3145.033300	621249.119088	40.263322
3148.189857	622344.855372	40.268340
3151.002007	623441.436812	40.273357
3154.203322	624541.789721	40.278375
3157.170360	625649.162775	40.283392
3160.612424	626747.351165	40.288410
3163.902638	627867.878782	40.293428
3166.758493	628983.665199	40.298445
3170.330790	630100.264793	40.303463
3172.972018	631222.642195	40.308480
3176.670560	632330.396339	40.313498
3179.943486	633447.788764	40.318516
3183.001922	634566.245322	40.323533
3186.403065	635670.500136	40.328551
3189.831404	636802.980257	40.333568
3192.808290	637923.334908	40.338586
3196.103609	639043.515568	40.343604
3199.229521	640171.584766	40.348621
3202.563159	641284.380585	40.353639
3205.746194	642407.804307	40.358656
3208.888861	643531.659552	40.363674
3212.447433	644655.770827	40.368692
3215.380598	645783.600215	40.373709
3219.053479	646894.878383	40.378727
3222.045344	648026.086936	40.383744
3225.198001	649150.362433	40.388762
3228.508666	650262.822851	40.393780
3231.503961	651394.696738	40.398797
3234.847678	652505.157027	40.403815
3237.648578	653632.373057	40.408832
3240.893023	654714.152440	40.413850
3244.100120	655802.842834	40.418868
3247.046549	656891.804197	40.423885
3250.395598	657966.783029	40.428903
3253.165400	659056.677908	40.433920
3256.683142	660146.775644	40.438938
3259.965252	661247.045533	40.443956
3262.715645	662355.591143	40.448973
3265.695528	663462.528163	40.453991
3268.795274	664584.895425	40.459008
3272.100804	665698.637897	40.464026
3275.115366	666831.156215	40.469044
3278.486424	667980.296825	40.474061
3281.561463	669116.463542	40.479079
3284.476191	670276.543993	40.484096
3287.678964	671436.533980	40.489114
3290.990800	672597.755432	40.494132
3293.873368	673772.378026	40.499149
3297.381687	674952.914534	40.504167
3300.359692	676152.128593	40.509184
3303.367369	677355.656187	40.514202
3306.878964	678547.564553	40.519220
3310.248635	679765.478267	40.524237
3313.698922	680982.174372	40.529255
3316.808169	682201.596909	40.534272
3319.960333	683434.905893	40.539290
3323.640168	684667.911553	40.544308
3326.580943	685904.595905	40.549325
3329.830770	687154.415784	40.554343
3333.203740	688411.538219	40.559360
3336.291150	689661.831735	40.564378
3340.025000	690926.037808	40.569396
3343.249174	692199.279253	40.574413
3346.564301	693475.201485	40.579431
3349.614697	694746.569371	40.584448
3353.551484	696021.080663	40.589466
3357.293910	697287.356733	40.594484
3360.282054	698573.309324	40.599501
3363.727279	699852.107043	40.604519
3367.262429	701145.920737	40.609536
3370.723566	702424.339147	40.614554
3374.416595	703714.077495	40.619572
3377.881580	705003.562294	40.624589
3381.433317	706292.691606	40.629607
3384.965266	707579.699327	40.634624
3388.587073	708867.192511	40.639642
3392.336233	710160.264393	40.644660
3395.667073	711440.336475	40.649677
3399.081446	712718.419865	40.654695
3402.977551	713991.281517	40.659712
3406.508353	715266.238400	40.664730
3410.025478	716544.468009	40.669748
3413.656853	717814.914769	40.674765
3417.318325	719082.591414	40.679783
3420.812143	720355.840015	40.684800
3424.038326	721610.839021	40.689818
3427.694756	722872.251807	40.694836
3430.843856	724141.662896	40.699853
3434.642432	725395.547735	40.704871
3438.309788	726654.204672	40.709888
3441.609170	727919.844042	40.714906
3445.145866	729169.833854	40.719924
3448.877805	730422.316280	40.724941
3452.256792	731673.329956	40.729959
3455.967881	732923.157149	40.734976
3459.006070	734177.197012	40.739994
3462.559092	735413.579524	40.745012
3466.189584	736653.777304	40.750016
3469.807101	737835.139412	40.755021
3472.969049	738956.344363	40.760026
3476.008371	740029.827213	40.765031
3479.640048	741034.914772	40.770036
3482.174786	741980.070604	40.775040
3485.590860	742847.387185	40.780045
3488.425060	743653.347776	40.785050
3490.917412	744388.143100	40.790055
3493.805690	745045.986723	40.795060
3495.874686	745643.607325	40.800064
3498.308347	746190.066097	40.805069
3500.773021	746667.043642	40.810074
3502.754964	747097.024357	40.815079
3504.866432	747443.544091	40.820084
3506.548801	747754.589577	40.825088
3508.355872	747999.931492	40.830093
3509.694751	748197.758725	40.835098
3511.124627	748370.810862	40.840103
3512.923675	748470.522519	40.845108
3514.251641	748556.821537	40.850112
3515.481558	748573.369012	40.855117
3517.038372	748567.232783	40.860122
3517.798781	748522.539514	40.865127
3518.605379	748446.758990	40.870132
3519.579632	748337.251477	40.875136
3520.545726	748202.197581	40.880141
3521.295805	748035.898256	40.885146
3521.760898	747861.143032	40.890151
3522.772238	747651.010987	40.895156
3522.742199	747427.652776	40.900160
3523.961321	747161.236156	40.905165
3524.080745	746907.198553	40.910170
3524.748904	746615.649532	40.915175
3525.320042	746309.970250	40.920180
3525.728205	745994.321742	40.925184
3526.010574	745659.107553	40.930189
3526.309227	745320.465614	40.935194
3526.141392	744977.733546	40.940199
3526.852850	744610.124081	40.945204
3526.747208	744238.528725	40.950208
3527.120748	743849.829515	40.955213
3527.143227	743476.298291	40.960218
3527.117771	743090.742178	40.965223
3527.689373	742675.845511	40.970228
3527.474566	742274.853103	40.975232
3527.845701	741861.034513	40.980237
3527.513777	741440.732569	40.985242
3527.673873	741017.211377	40.990247
3527.962920	740603.241577	40.995252
3527.851307	740167.156772	41.000256
3527.709775	739731.300243	41.005261
3527.766715	739314.382937	41.010266
3527.657710	738872.389310	41.015271
3528.086687	738425.186679	41.020276
3528.034541	737997.383548	41.025280
3528.134436	737536.628701	41.030285
3527.882607	737094.015675	41.035290
3527.768115	736650.860645	41.040295
3527.929780	736197.837006	41.045300
3527.471860	735750.779180	41.050304
3527.118525	735300.511613	41.055309
3527.158164	734854.905632	41.060314
3526.920791	734419.814283	41.065319
3527.058417	733965.629077	41.070324
3526.657028	733526.407806	41.075328
3526.572058	733081.021109	41.080333
3526.755858	732636.951799	41.085338
3526.690935	732214.139795	41.090343
3526.380874	731757.477903	41.095348
3525.947172	731324.083911	41.100352
3526.091721	730897.652839	41.105357
3526.045656	730477.322052	41.110362
3525.556934	730026.633813	41.115367
3525.825993	729598.826324	41.120372
3525.198445	729169.905799	41.125376
3525.014416	728741.929789	41.130381
3525.206819	728309.014755	41.135386
3524.932323	727893.591253	41.140391
3524.893812	727469.338966	41.145396
3524.605267	727048.078477	41.150400
3524.526776	726632.112673	41.155405
3524.407102	726216.776664	41.160410
3524.400795	725807.793033	41.165415
3524.502454	725389.157833	41.170420
3524.079210	724976.881422	41.175424
3523.803267	724558.761708	41.180429
3523.828615	724151.821488	41.185434
3523.691769	723750.092069	41.190439
3523.732832	723335.030092	41.195444
3523.301660	722936.085238	41.200448
3523.102947	722536.587112	41.205453
3523.150398	722141.589865	41.210458
3522.740492	721737.229782	41.215463
3522.890633	721341.880036	41.220468
3522.451132	720956.871727	41.225472
3522.434254	720558.686128	41.230477
3522.139087	720177.882039	41.235482
3521.766011	719799.106430	41.240487
3521.908810	719401.483776	41.245492
3521.360315	719035.546028	41.250496
3521.491277	718660.107026	41.255501
3521.464663	718286.809748	41.260506
3521.210603	717912.690104	41.265511
3521.573072	717541.725782	41.270516
3521.056686	717182.050452	41.275520
3520.958303	716797.885208	41.280525
3520.919814	716431.799121	41.285530
3520.644467	716075.558732	41.290535
3520.524447	715713.721179	41.295540
3519.926070	715359.984261	41.300544
3520.301102	714990.244720	41.305549
3520.155306	714654.066722	41.310554
3520.175571	714295.370267	41.315559
3519.646494	713952.330321	41.320564
3519.470189	713605.843901	41.325568
3519.506489	713249.978598	41.330573
3519.137377	712921.113054	41.335578
3518.978196	712574.829739	41.340583
3518.884580	712237.703356	41.345588
3518.307566	711912.406415	41.350592
3518.802040	711580.318925	41.355597
3518.707827	711261.419766	41.360602
3517.980983	710931.444032	41.365607
3517.906136	710608.694981	41.370612
3517.851342	710299.681542	41.375616
3517.761518	709983.613100	41.380621
3517.853200	709669.985380	41.385626
3517.439798	709350.074348	41.390631
3517.220996	709046.752159	41.395636
3517.330802	708746.840714	41.400640
3517.387993	708434.166384	41.405645
3516.990604	708116.143068	41.410650
3516.794752	707815.305911	41.415655
3516.722413	707509.024994	41.420660
3516.846262	707229.666727	41.425664
3516.567423	706929.408129	41.430669
3516.187261	706637.251024	41.435674
3516.052082	706347.427596	41.440679
3516.272830	706060.466157	41.445684
3515.786215	705784.836969	41.450688
3515.875003	705486.056869	41.455693
3515.754243	705203.146517	41.460698
3515.438925	704936.601749	41.465703
3515.140663	704650.424048	41.470708
3515.033038	704387.156386	41.475712
3515.226735	704108.828062	41.480717
3515.052102	703840.885013	41.485722
3514.788402	703570.315210	41.490727
3515.031710	703308.646129	41.495732
3514.497237	703036.265992	41.500736
3514.397477	702787.555821	41.505741
3514.389812	702513.681266	41.510746
3514.277580	702264.262542	41.515751
3514.459315	701999.483436	41.520756
3514.064327	701754.320413	41.525760
3514.076807	701503.517648	41.530765
3513.645890	701251.687432	41.535770
3513.467722	701001.199800	41.540775
3513.502560	700760.311296	41.545780
3513.397511	700517.003928	41.550784
3513.661052	700285.457823	41.555789
3513.392851	700040.673057	41.560794
3512.942416	699809.927836	41.565799
3513.100987	699569.135234	41.570804
3513.144191	699338.445361	41.575808
3513.070449	699104.239462	41.580813
3513.051203	698868.179104	41.585818
3512.694169	698639.376012	41.590823
3512.705452	698406.728204	41.595828
3512.217755	698180.817947	41.600832
3512.252156	697958.892393	41.605837
3512.061051	697751.216913	41.610842
3511.871902	697529.466505	41.615847
3512.012385	697309.545462	41.620852
3512.285127	697114.705092	41.625856
3511.974135	696878.887993	41.630861
3511.788201	696665.667146	41.635866
3511.516209	696454.742554	41.640871
3511.937621	696245.737332	41.645876
3511.821451	696044.125279	41.650880
3511.594114	695818.807698	41.655885
3511.381602	695610.239986	41.660890
3511.549194	695413.290866	41.665895
3511.209272	695201.054613	41.670900
3511.082770	695009.217364	41.675904
3510.993812	694802.649216	41.680909
3510.747003	694616.641893	41.685914
3510.404071	694415.179299	41.690919
3510.545315	694222.534903	41.695924
3510.435891	694029.330800	41.700928
3510.287487	693841.599993	41.705933
3510.605752	693658.165276	41.710938
3510.569131	693472.944907	41.715943
3510.509117	693278.074943	41.720948
3510.157336	693100.807443	41.725952
3510.173378	692921.734827	41.730957
3510.425283	692720.881952	41.735962
3510.007443	692531.625863	41.740967
3510.327565	692359.754527	41.745972
3509.603720	692189.743273	41.750976
3510.004905	692005.166445	41.755981
3510.065493	691823.626824	41.760986
3510.019313	691658.120373	41.765991
3509.936045	691469.731871	41.770996
3509.885477	691300.090240	41.776000
3509.580220	691113.770616	41.781005
3509.711838	690954.988160	41.786010
3509.323568	690774.197740	41.791015
3509.585773	690607.078653	41.796020
3509.146118	690439.773564	41.801024
3509.405885	690260.010376	41.806029
3509.761225	690103.066730	41.811034
3509.430969	689943.844889	41.816039
3509.295930	689760.703401	41.821044
3509.051404	689603.601068	41.826048
3508.826474	689436.739497	41.831053
3508.828716	689275.311267	41.836058
3508.699290	689120.918463	41.841063
3508.786375	688950.861374	41.846068
3508.598240	688814.189034	41.851072
3508.878755	688652.654016	41.856077
3509.018319	688489.347723	41.861082
3508.378919	688341.395727	41.866087
3508.521222	688175.246537	41.871092
3508.063016	688034.426309	41.876096
3508.343373	687885.220347	41.881101
3508.205447	687734.886339	41.886106
3508.086495	687598.283704	41.891111
3508.328263	687441.212830	41.896116
3507.994665	687300.460161	41.901120
3508.079098	687162.523317	41.906125
3508.378192	687017.928938	41.911130
3508.309730	686875.732270	41.916135
3508.387062	686711.956106	41.921140
3508.017147	686574.931371	41.926144
3508.122224	686434.142714	41.931149
3508.305511	686285.623250	41.936154
3507.822436	686138.704546	41.941159
3508.175352	685982.486082	41.946164
3508.173229	685844.991458	41.951168
3507.915413	685708.034704	41.956173
3507.940209	685566.349724	41.961178
3507.648604	685424.714668	41.966183
3507.792443	685280.416861	41.971188
3507.548291	685149.224417	41.976192
3507.242861	685011.219507	41.981197
3507.494190	684881.484920	41.986202
3507.050856	684758.335299	41.991207
3507.459442	684621.999172	41.996212
3507.172815	684489.161197	42.001216
3507.347506	684360.527166	42.006221
3507.035413	684227.390830	42.011226
3506.801317	684102.206243	42.016231
3507.174848	683978.463351	42.021236
3506.790728	683856.436976	42.026240
3506.680484	683728.538067	42.031245
3506.717788	683606.787460	42.036250
3506.755450	683499.525291	42.041255
3506.844077	683373.530609	42.046260
3506.713675	683252.649427	42.051264
3506.415582	683138.168185	42.056269
3506.582756	683017.981805	42.061274
3506.640317	682900.500971	42.066279
3506.589283	682776.014986	42.071284
3506.444454	682679.280657	42.076288
3506.331012	682550.021207	42.081293
3506.257500	682438.681357	42.086298
3506.115483	682345.528631	42.091303
3506.321888	682212.626079	42.096308
3506.034788	682132.792004	42.101312
3505.983073	682012.279872	42.106317
3506.043531	681911.320207	42.111322
3505.949614	681809.986439	42.116327
3506.377055	681689.839347	42.121332
3505.965547	681604.741940	42.126336
3506.169173	681485.525532	42.131341
3506.127699	681381.190077	42.136346
3505.994518	681272.037337	42.141351
3506.077486	681164.092854	42.146356
3505.925689	681062.561142	42.151360
3505.526427	680954.992506	42.156365
3505.803521	680849.602358	42.161370
3505.936473	680770.484147	42.166375
3505.874177	680651.300731	42.171380
3505.611651	680548.287291	42.176384
3505.500985	680457.301875	42.181389
3505.455210	680353.603000	42.186394
3505.414667	680258.967844	42.191399
3505.626447	680155.822043	42.196404
3505.509844	680067.623245	42.201408
3505.359502	679969.117801	42.206413
3505.576935	679876.030230	42.211418
3505.224728	679781.142636	42.216423
3505.369118	679688.613166	42.221428
3505.383518	679592.417848	42.226432
3505.362519	679496.924783	42.231437
3505.355639	679401.278954	42.236442
3504.859266	679322.899620	42.241447
3505.101599	679229.004346	42.246452
3505.386996	679136.844648	42.251456
3504.940663	679053.223900	42.256461
3504.893372	678960.320166	42.261466
3504.580189	678881.458525	42.266471
3504.905786	678786.548650	42.271476
3505.435191	678713.176365	42.276480
3504.984471	678616.599139	42.281485
3505.039590	678523.076287	42.286490
3505.253144	678448.608062	42.291495
3504.755388	678354.028705	42.296500
3504.776757	678267.533740	42.301504
3505.033175	678178.109501	42.306509
3505.072175	678093.652751	42.311514
3504.538071	678004.157797	42.316519
3504.632562	677935.933060	42.321524
3505.055538	677853.254347	42.326528
3505.070110	677764.314388	42.331533
3504.966309	677680.574954	42.336538
3504.692569	677595.866243	42.341543
3505.297478	677505.132434	42.346548
3504.946801	677433.090871	42.351552
3504.515876	677354.883368	42.356557
3504.601927	677272.653617	42.361562
3504.658355	677185.644498	42.366567
3504.809955	677094.931547	42.371572
3504.714795	677027.179835	42.376576
3504.328282	676939.842764	42.381581
3504.837145	676867.854496	42.386586
3504.476142	676790.876468	42.391591
3504.801563	676706.359888	42.396596
3504.805028	676631.961526	42.401600
3504.681473	676550.706716	42.406605
3504.872978	676468.801296	42.411610
3504.546164	676393.608300	42.416615
3504.665851	676311.713330	42.421620
3504.749440	676221.451559	42.426624
3505.036091	676145.358134	42.431629
3504.625499	676058.564919	42.436634
3504.420630	675987.135956	42.441639
3504.272047	675909.168761	42.446644
3504.588615	675833.815389	42.451648
3504.393672	675757.150286	42.456653
3504.421798	675686.228818	42.461658
3504.327662	675619.214223	42.466663
3504.087078	675545.046731	42.471668
3503.941025	675473.703811	42.476672
3504.135014	675404.696534	42.481677
3504.557460	675323.141688	42.486682
3504.158222	675259.663465	42.491687
3504.550884	675174.224809	42.496692
3504.121724	675111.647612	42.501696
3504.336287	675031.071419	42.506701
3504.564091	674962.454020	42.511706
3504.095903	674886.474702	42.516711
3504.188618	674812.445826	42.521716
3504.335429	674758.393852	42.526720
3504.320624	674681.291489	42.531725
3504.547110	674608.136103	42.536730
3504.201659	674535.373443	42.541735
3504.096022	674457.686091	42.546740
3504.202823	674395.314833	42.551744
3504.001579	674326.564089	42.556749
3504.199434	674247.778267	42.561754
3503.927681	674187.511607	42.566759
3504.227216	674108.558326	42.571764
3504.181821	674049.050992	42.576768
3504.072428	673987.510161	42.581773
3504.536603	673908.727448	42.586778
3504.012834	673845.409665	42.591783
3504.360303	673770.283792	42.596788
3504.075600	673689.778311	42.601792
3504.135739	673627.858251	42.606797
3504.013552	673553.356348	42.611802
3503.706182	673495.433944	42.616807
3503.967293	673418.824041	42.621812
3503.878274	673365.949400	42.626816
3503.837172	673298.959275	42.631821
3504.236272	673221.078792	42.636826
3503.894699	673169.889695	42.641831
3504.189155	673104.836883	42.646836
3503.974478	673035.530519	42.651840
3503.683051	672980.244380	42.656845
3503.939364	672914.498622	42.661850
3503.948492	672849.491057	42.666855
3503.910643	672776.265221	42.671860
3503.864616	672706.280561	42.676864
3503.853969	672647.057714	42.681869
3504.002628	672583.670452	42.686874
3503.853200	672510.909609	42.691879
3504.000556	672436.753250	42.696884
3503.763001	672384.794923	42.701888
3503.765762	672329.107494	42.706893
3503.993296	672260.570065	42.711898
3503.675004	672194.365552	42.716903
3503.698133	672128.403445	42.721908
3503.852183	672076.777730	42.726912
3503.425776	672019.513949	42.731917
3503.746432	671945.474728	42.736922
3503.882229	671889.812634	42.741927
3503.851349	671831.186261	42.746932
3503.666218	671766.452499	42.751936
3503.659812	671702.436706	42.756941
3503.433468	671636.761549	42.761946
3503.384081	671582.324741	42.766951
3503.740644	671530.662663	42.771956
3503.454652	671463.550229	42.776960
3503.195466	671413.983327	42.781965
3503.089075	671374.362858	42.786970
3503.106139	671321.509091	42.791975
3503.293077	671264.488666	42.796980
3503.276205	671212.736800	42.801985
3503.042605	671157.729571	42.806989
3503.614585	671099.547773	42.811994
3503.234985	671048.802131	42.816999
3503.435350	670989.733530	42.822004
3503.330568	670940.487723	42.827009
3503.104412	670884.330855	42.832013
3503.646923	670834.529080	42.837018
3503.419258	670778.371829	42.842023
3503.600186	670704.645067	42.847028
3503.604114	670655.030818	42.852033
3503.439733	670603.948140	42.857037
3503.592811	670555.754831	42.862042
3503.239585	670500.663755	42.867047
3503.351022	670430.287186	42.872052
3503.085678	670388.744059	42.877057
3503.072930	670347.408452	42.882061
3503.224566	670293.230270	42.887066
3503.246215	670240.619021	42.892071
3503.364527	670184.002304	42.897076
3502.983290	670126.919036	42.902081
3503.190576	670074.026943	42.907085
3503.355836	670013.910837	42.912090
3503.131882	669984.476667	42.917095
3503.134807	669917.106159	42.922100
3503.180109	669869.824720	42.927105
3502.977429	669816.001392	42.932109
3503.034207	669774.203015	42.937114
3503.152100	669729.003358	42.942119
3503.451493	669669.860326	42.947124
3503.427275	669620.743971	42.952129
3503.290795	669571.496252	42.957133
3503.595161	669501.878889	42.962138
3503.365375	669463.966291	42.967143
3503.381695	669407.012646	42.972148
3503.165512	669346.855420	42.977153
3503.155800	669298.632664	42.982157
3503.281978	669241.859406	42.987162
3503.211101	669196.788058	42.992167
3503.249148	669141.873943	42.997172
3503.221489	669094.052073	43.002177
3503.250928	669042.380439	43.007181
3503.319717	668981.076757	43.012186
3503.170481	668944.295860	43.017191
3503.300320	668886.223195	43.022196
3503.558441	668833.415547	43.027201
3503.435210	668785.657743	43.032205
3503.522813	668727.541193	43.037210
3502.994279	668682.243571	43.042215
3503.107789	668619.832969	43.047220
3503.288226	668564.493060	43.052225
3502.866258	668524.364032	43.057229
3503.258728	668463.053544	43.062234
3502.831764	668415.792799	43.067239
3503.255266	668372.481443	43.072244
3503.395993	668330.912248	43.077249
3503.144774	668273.197877	43.082253
3503.140052	668217.088444	43.087258
3503.129161	668164.770291	43.092263
3503.369605	668116.201051	43.097268
3502.892519	668071.041660	43.102273
3503.011833	668023.688948	43.107277
3502.738300	667981.488209	43.112282
3503.085273	667944.023145	43.117287
3503.164974	667881.214246	43.122292
3503.065118	667829.407685	43.127297
3503.167860	667788.540671	43.132301
3503.469094	667744.249041	43.137306
3502.735252	667695.389288	43.142311
3503.025828	667643.068470	43.147316
3503.120190	667592.026677	43.152321
3502.970979	667549.653897	43.157325
3503.150686	667497.051269	43.162330
3502.855374	667454.851781	43.167335
3502.951119	667401.713782	43.172340
3503.313276	667358.557566	43.177345
3503.043350	667310.567120	43.182349
3503.152620	667258.174303	43.187354
3503.076050	667221.075475	43.192359
3503.629453	667158.682567	43.197364
3503.317991	667105.011435	43.202369
3503.213997	667064.374908	43.207373
3503.291088	667002.907461	43.212378
3503.049150	666958.252742	43.217383
3503.360132	666905.724986	43.222388
3503.105139	666864.513895	43.227393
3503.049871	666811.148073	43.232397
3503.057567	666762.360868	43.237402
3502.611892	666710.455554	43.242407
3503.041015	666649.476545	43.247412
3503.161321	666617.281459	43.252417
3503.042577	666569.262367	43.257421
3502.903711	666514.811202	43.262426
3502.823647	666468.630970	43.267431
3503.056344	666429.183386	43.272436
3502.905447	666383.812581	43.277441
3502.974829	666345.788358	43.282445
3503.002193	666295.299410	43.287450
3502.971506	666253.699516	43.292455
3503.115446	666196.805397	43.297460
3502.550270	666152.798808	43.302465
3502.949918	666102.496931	43.307469
3503.269678	666056.598035	43.312474
3503.009754	666020.572384	43.317479
3503.085385	665968.178032	43.322484
3502.936212	665922.156209	43.327489
3503.415319	665863.857907	43.332493
3503.289328	665822.571170	43.337498
3502.877638	665775.045353	43.342503
3503.021900	665712.760317	43.347508
3503.101145	665676.128701	43.352513
3503.133821	665622.492302	43.357517
3503.067279	665572.813246	43.362522
3502.890799	665543.008267	43.367527
3502.722575	665488.605983	43.372532
3503.071146	665454.922554	43.377537
3502.755344	665400.643868	43.382541
3503.268113	665352.764059	43.387546
3502.999645	665306.160238	43.392551
3502.805132	665252.708877	43.397556
3503.061378	665204.371682	43.402561
3502.957998	665162.479671	43.407565
3503.398023	665121.246318	43.412570
3503.061614	665066.170856	43.417575
3503.334199	665013.988291	43.422580
3503.049277	664960.949341	43.427585
3503.028576	664915.001293	43.432589
3503.288173	664863.219194	43.437594
3503.065898	664817.852723	43.442599
3503.018181	664763.176993	43.447604
3503.060302	664730.190140	43.452609
3502.859041	664680.428867	43.457613
3503.075531	664630.249237	43.462618
3502.908575	664586.668766	43.467623
3503.076551	664528.313825	43.472628
3502.631256	664487.273528	43.477633
3502.994704	664459.471817	43.482637
3503.021128	664405.180995	43.487642
3502.780356	664359.416236	43.492647
3503.019128	664306.187579	43.497652
3503.108801	664264.209937	43.502657
3502.710096	664214.329091	43.507661
3502.892328	664167.046704	43.512666
3502.853181	664120.948202	43.517671
3502.985705	664079.062485	43.522676
3502.998226	664048.123968	43.527681
3502.734971	663994.277738	43.532685
3502.737070	663949.069779	43.537690
3502.584699	663898.747517	43.542695
3502.713618	663859.056970	43.547700
3503.147199	663823.008576	43.552705
3502.894770	663781.184994	43.557709
3503.031751	663738.099480	43.562714
3502.878540	663692.317114	43.567719
3503.031782	663642.891246	43.572724
3502.991548	663601.381216	43.577729
3502.960795	663547.793574	43.582733
3503.113682	663503.806184	43.587738
3503.001822	663446.339099	43.592743
3502.884748	663404.940684	43.597748
3503.043771	663357.209034	43.602753
3502.742714	663320.780802	43.607757
3502.986528	663259.910595	43.612762
3502.870988	663230.238095	43.617767
3502.683260	663178.271125	43.622772
3502.761962	663141.480224	43.627777
3502.694985	663102.916693	43.632781
3503.112067	663050.699668	43.637786
3502.823952	663007.730837	43.642791
3503.047747	662964.777269	43.647796
3503.259834	662918.980935	43.652801
3502.883986	662867.143092	43.657805
3502.742063	662811.773136	43.662810
3502.692799	662779.044172	43.667815
3502.831665	662740.944318	43.672820
3502.643540	662702.648671	43.677825
3502.729610	662655.674139	43.682829
3503.285708	662616.956091	43.687834
3502.767464	662569.481856	43.692839
3503.250964	662515.953456	43.697844
3502.921360	662469.196228	43.702849
3503.012186	662414.035166	43.707853
3502.954901	662372.223214	43.712858
3502.633569	662334.497025	43.717863
3502.620595	662282.396617	43.722868
3502.875626	662235.242479	43.727873
3502.631575	662199.349590	43.732877
3502.839734	662157.542876	43.737882
3502.720785	662132.708586	43.742887
3502.949802	662077.922096	43.747892
3503.188737	662026.078244	43.752897
3502.791814	661989.511050	43.757901
3502.987980	661944.311620	43.762906
3502.563775	661908.896514	43.767911
3502.663269	661865.758907	43.772916
3502.677092	661814.549923	43.777921
3502.556136	661775.440980	43.782925
3502.522504	661732.424534	43.787930
3502.359005	661709.093787	43.792935
3502.825966	661655.463532	43.797940
3502.839034	661623.369212	43.802945
3502.697342	661584.312823	43.807949
3503.097561	661536.732074	43.812954
3502.632507	661499.824877	43.817959
3502.590896	661449.621314	43.822964
3502.598036	661412.785711	43.827969
3502.501366	661366.284228	43.832973
3502.675798	661330.818271	43.837978
3502.566872	661295.698348	43.842983
3502.602324	661264.647301	43.847988
3502.801535	661217.447491	43.852993
3502.566192	661180.451310	43.857997
3502.600823	661133.328122	43.863002
3502.211930	661110.082984	43.868007
3502.542309	661066.055249	43.873012
3502.539254	661016.242391	43.878017
3502.516623	660984.002095	43.883021
3502.771013	660948.271995	43.888026
3502.361396	660909.706256	43.893031
3502.550849	660861.607871	43.898036
3502.562109	660829.311561	43.903041
3502.836284	660784.842583	43.908045
3502.824828	660751.351806	43.913050
3502.867883	660714.008481	43.918055
3502.526267	660665.197991	43.923060
3502.779820	660634.658056	43.928065
3502.815240	660585.685208	43.933069
3502.711034	660541.127716	43.938074
3502.758930	660502.984127	43.943079
3502.631467	660458.380171	43.948084
3502.803429	660430.249019	43.953089
3502.501477	660388.319062	43.958093
3502.646938	660343.819357	43.963098
3502.731915	660306.667224	43.968103
3502.940211	660261.058611	43.973108
3502.645529	660223.469547	43.978113
3502.533722	660188.795345	43.983117
3502.823311	660152.008246	43.988122
3502.704304	660109.947106	43.993127
3503.007340	660064.222122	43.998132
3502.666331	660024.293760	44.003137
3502.900749	659973.737562	44.008141
3502.664682	659933.591859	44.013146
3502.578225	659888.279661	44.018151
3502.921161	659846.790212	44.023156
3502.887789	659805.013157	44.028161
3503.043826	659773.238594	44.033165
3502.875768	659716.956684	44.038170
3502.457868	659676.240839	44.043175
3502.483567	659648.530888	44.048180
3502.722367	659612.898291	44.053185
3502.606179	659581.267800	44.058189
3502.934038	659529.296114	44.063194
3502.750249	659486.394292	44.068199
3502.881889	659444.538576	44.073204
3502.693260	659402.435925	44.078209
3502.587754	659366.709396	44.083213
3502.907149	659310.244966	44.088218
3502.775465	659281.511539	44.093223
3503.110042	659233.081651	44.098228
3502.943019	659185.033711	44.103233
3502.537042	659146.510285	44.108237
3502.681679	659095.415168	44.113242
3502.726825	659064.704955	44.118247
3502.757644	659024.012285	44.123252
3502.703168	658970.103673	44.128257
3502.842464	658933.636282	44.133261
3502.894979	658881.307120	44.138266
3502.788187	658839.687793	44.143271
3502.558262	658799.386622	44.148276
3502.792019	658767.146650	44.153281
3502.263754	658733.234832	44.158285
3502.760855	658688.819394	44.163290
3502.667857	658652.439155	44.168295
3502.198588	658608.532069	44.173300
3502.535198	658573.029332	44.178305
3502.615294	658537.718513	44.183309
3502.651226	658497.771696	44.188314
3502.657233	658461.673990	44.193319
3502.752301	658413.479206	44.198324
3502.741837	658377.833243	44.203329
3502.603005	658334.120106	44.208333
3503.162638	658298.529696	44.213338
3502.707350	658257.614365	44.218343
3502.813111	658200.080309	44.223348
3502.639493	658156.471964	44.228353
3502.759956	658125.996027	44.233357
3502.792303	658074.165143	44.238362
3502.873128	658038.403042	44.243367
3502.357112	657994.101461	44.248372
3502.659756	657948.965773	44.253377
3502.313103	657920.862907	44.258381
3502.565175	657896.156361	44.263386
3502.483026	657851.832572	44.268391
3502.651608	657816.404706	44.273396
3502.669193	657768.319367	44.278401
3502.220534	657743.827763	44.283405
3502.678508	657693.023187	44.288410
3502.601537	657656.536735	44.293415
3502.729221	657619.367323	44.298420
3502.340905	657574.343762	44.303425
3502.180450	657550.653011	44.308429
3502.298281	657502.599778	44.313434
3502.374410	657470.031983	44.318439
3502.603354	657432.994973	44.323444
3502.684738	657395.732477	44.328449
3502.394470	657356.034473	44.333453
3502.505565	657314.921997	44.338458
3502.314790	657284.894185	44.343463
3502.431143	657251.170586	44.348468
3502.511313	657205.618736	44.353473
3502.296830	657182.435324	44.358477
3502.168480	657140.812310	44.363482
3502.148424	657111.205232	44.368487
3502.302914	657077.524684	44.373492
3502.038194	657041.266609	44.378497
3502.145572	657022.773489	44.383501
3502.283091	656984.751173	44.388506
3501.902672	656969.584044	44.393511
3502.263658	656927.529952	44.398516
3502.227659	656886.140309	44.403521
3502.136452	656856.194643	44.408525
3502.566476	656820.620227	44.413530
3502.101297	656792.084230	44.418535
3502.211506	656764.402106	44.423540
3502.332139	656742.161134	44.428545
3502.359917	656702.807555	44.433549
3502.445046	656648.763264	44.438554
3502.323196	656629.308459	44.443559
3502.246191	656595.814210	44.448564
3502.558844	656555.114760	44.453569
3502.639074	656515.352296	44.458573
3502.657673	656474.551157	44.463578
3502.419212	656453.067815	44.468583
3502.236135	656399.615651	44.473588
3502.807947	656364.515590	44.478593
3502.539212	656335.646269	44.483597
3502.642950	656284.443335	44.488602
3502.451368	656251.066664	44.493607
3502.531251	656215.098313	44.498612
3502.487950	656180.198829	44.503617
3502.488878	656146.240761	44.508621
3502.782201	656104.443986	44.513626
3502.530050	656081.813500	44.518631
3502.590006	656017.882027	44.523636
3502.526112	655996.868310	44.528641
3502.597881	655952.610443	44.533645
3502.453766	655905.141881	44.538650
3502.337293	655878.193766	44.543655
3502.252338	655846.945557	44.548660
3502.335078	655804.033590	44.553665
3502.458578	655768.955339	44.558669
3502.434244	655723.613593	44.563674
3502.333175	655698.809887	44.568679
3502.576823	655650.926617	44.573684
3502.566485	655623.910375	44.578689
3502.384976	655594.874678	44.583693
3502.488136	655551.408892	44.588698
3502.273690	655520.330806	44.593703
3502.757013	655480.447792	44.598708
3502.777024	655451.228640	44.603713
3502.427828	655408.685773	44.608717
3502.831083	655358.127850	44.613722
3502.667835	655332.134850	44.618727
3502.885189	655291.745532	44.623732
3502.761561	655251.462178	44.628737
3502.340923	655213.924526	44.633741
3502.991207	655160.877677	44.638746
3502.875883	655126.635584	44.643751
3502.706780	655077.169403	44.648756
3502.526984	655029.203055	44.653761
3502.525506	654998.238059	44.658765
3502.554157	654944.493372	44.663770
3502.729590	654927.433486	44.668775
3502.608369	654879.256978	44.673780
3502.627790	654831.656399	44.678785
3502.640464	654801.137956	44.683789
3502.511731	654761.402836	44.688794
3502.694896	654728.708426	44.693799
3502.534161	654692.374595	44.698804
3502.649318	654641.510851	44.703809
3502.561625	654609.509976	44.708813
3502.870463	654568.053751	44.713818
3502.718609	654532.966527	44.718823
3502.593268	654491.032112	44.723828
3502.493439	654444.747929	44.728833
3502.356982	654426.190215	44.733837
3502.835721	654380.509655	44.738842
3502.685639	654340.776357	44.743847
3502.717212	654295.019242	44.748852
3502.626469	654267.313261	44.753857
3502.567179	654216.126437	44.758861
3502.730829	654181.635299	44.763866
3502.684549	654135.240945	44.768871
3502.590899	654098.544232	44.773876
3502.503450	654053.105302	44.778881
3502.722024	654018.055105	44.783885
3502.818381	653977.380652	44.788890
3502.679614	653941.739726	44.793895
3502.786761	653894.519768	44.798900
3502.854366	653856.896491	44.803905
3502.532230	653813.543076	44.808909
3502.307757	653771.522038	44.813914
3502.133874	653740.082000	44.818919
3502.515353	653690.168484	44.823924
3502.689499	653662.317256	44.828929
3502.390707	653639.788739	44.833933
3502.550696	653590.260873	44.838938
3502.613299	653566.423856	44.843943
3502.624613	653519.018091	44.848948
3502.380653	653473.852045	44.853953
3502.368724	653445.980918	44.858957
3502.866188	653411.132376	44.863962
3502.401730	653377.591122	44.868967
3502.680623	653331.189365	44.873972
3502.668172	653289.081386	44.878977
3502.425107	653263.795425	44.883981
3502.366303	653208.607068	44.888986
3502.435358	653180.222316	44.893991
3502.353617	653154.559818	44.898996
3502.220357	653097.834555	44.904001
3502.109834	653080.169205	44.909005
3502.312930	653032.629601	44.914010
3502.085295	653007.490304	44.919015
3502.123876	652974.963784	44.924020
3502.349519	652936.062106	44.929025
3502.205532	652921.399261	44.934029
3502.283691	652875.627904	44.939034
3502.405376	652849.831186	44.944039
3502.349431	652816.120801	44.949044
3502.287846	652778.214981	44.954049
3502.415328	652750.169057	44.959053
3502.404736	652700.015428	44.964058
3501.979182	652678.754501	44.969063
3502.087086	652649.662446	44.974068
3502.451675	652598.547273	44.979073
3502.258268	652574.800012	44.984077
3502.362855	652537.665193	44.989082
3502.310086	652497.508801	44.994087
3502.340957	652465.231664	44.999092
3502.501803	652425.839093	45.004097
3502.204109	652395.114583	45.009101
3502.293309	652363.976523	45.014106
3502.180522	652323.279784	45.019111
3502.287592	652301.330788	45.024116
3502.551118	652269.064634	45.029121
3502.361452	652226.581680	45.034125
3502.672139	652190.160972	45.039130
3502.387643	652153.488496	45.044135
3502.313100	652118.879553	45.049140
3502.327331	652094.497422	45.054145
3502.334830	652058.425944	45.059149
3502.601820	652008.822590	45.064154
3502.612580	651974.998437	45.069159
3502.365877	651939.218210	45.074164
3502.945029	651913.893236	45.079169
3502.433640	651874.359451	45.084173
3502.527139	651839.322165	45.089178
3502.761193	651796.168027	45.094183
3502.585985	651755.629127	45.099188
3502.656553	651710.902823	45.104193
3502.319539	651678.334024	45.109197
3502.507113	651639.283658	45.114202
3502.182064	651603.615054	45.119207
3502.329402	651562.472643	45.124212
3502.503530	651533.666177	45.129217
3502.253047	651510.475351	45.134221
3502.273678	651460.060506	45.139226
3502.246949	651434.684267	45.144231
3502.461693	651403.472550	45.149236
3502.012554	651365.675160	45.154241
3502.118116	651339.477480	45.159245
3502.359669	651300.316964	45.164250
3502.170715	651277.665047	45.169255
3502.350557	651246.408626	45.174260
3502.229786	651203.760056	45.179265
3502.258855	651176.825103	45.184269
3502.132628	651138.523969	45.189274
3502.595416	651106.221213	45.194279
3501.955197	651077.297796	45.199284
3502.243704	651040.177043	45.204289
3502.109678	651014.017985	45.209293
3502.600734	650973.516003	45.214298
3502.365764	650946.424078	45.219303
3502.346923	650906.155736	45.224308
3502.303915	650878.982031	45.229313
3502.038026	650852.344628	45.234317
3502.131933	650815.055243	45.239322
3502.150128	650777.478401	45.244327
3502.242638	650751.780980	45.249332
3502.397845	650711.782968	45.254337
3502.012788	650677.519970	45.259341
3502.187764	650653.307685	45.264346
3502.213899	650622.324466	45.269351
3502.243883	650587.143342	45.274356
3502.058401	650552.697130	45.279361
3502.155673	650531.545313	45.284365
3502.277925	650492.801019	45.289370
3502.154891	650460.442805	45.294375
3502.114121	650432.817812	45.299380
3502.377340	650385.005813	45.304385
3502.249658	650368.837489	45.309389
3502.297457	650320.710907	45.314394
3502.180234	650302.092333	45.319399
3502.259642	650260.306160	45.324404
3502.430817	650222.252307	45.329409
3502.215739	650199.652210	45.334413
3502.275102	650164.714597	45.339418
3502.293705	650146.123319	45.344423
3502.157114	650112.417059	45.349428
3502.186188	650077.634039	45.354433
3502.090203	650051.666063	45.359437
3502.319548	650003.558007	45.364442
3502.241783	649979.385735	45.369447
3502.467500	649949.516838	45.374452
3502.535997	649912.827904	45.379457
3502.351368	649879.378622	45.384461
3502.395857	649841.494104	45.389466
3502.301101	649807.130309	45.394471
3502.322490	649779.743117	45.399476
3502.435001	649735.500744	45.404481
3502.337987	649709.132283	45.409485
3502.274954	649663.619278	45.414490
3502.325158	649627.531964	45.419495
3502.298250	649602.101120	45.424500
3502.414343	649566.152641	45.429505
3502.319523	649536.785073	45.434509
3502.348784	649498.452021	45.439514
3502.253038	649469.833986	45.444519
3502.291230	649428.750737	45.449524
3502.494053	649398.284301	45.454529
3502.218465	649372.294183	45.459533
3502.255992	649335.158482	45.464538
3501.713044	649307.513180	45.469543
3502.125492	649280.909721	45.474548
3502.489398	649248.467343	45.479553
3502.443517	649210.945141	45.484557
3502.336905	649182.128181	45.489562
3502.149898	649155.223380	45.494567
3502.030179	649112.615673	45.499572
3502.066432	649089.172068	45.504577
3502.051421	649060.089793	45.509581
3502.337941	649027.609478	45.514586
3502.385901	648994.268831	45.519591
3502.121563	648959.730170	45.524596
3502.548548	648921.229422	45.529601
3502.010312	648893.632172	45.534605
3502.464085	648863.222709	45.539610
3502.394074	648827.302245	45.544615
3502.185785	648796.052144	45.549620
3502.383152	648757.188801	45.554625
3501.931722	648724.829105	45.559629
3502.289874	648697.183558	45.564634
3502.193191	648666.064588	45.569639
3502.063843	648633.801454	45.574644
3502.415021	648591.563722	45.579649
3502.322327	648566.490923	45.584653
3502.398880	648531.644731	45.589658
3502.329946	648499.321232	45.594663
3501.967613	648471.144086	45.599668
3502.296880	648442.503059	45.604673
3502.087923	648418.798429	45.609677
3502.203400	648381.496418	45.614682
3501.988693	648350.495872	45.619687
3501.977885	648322.560249	45.624692
3502.331733	648288.367207	45.629697
3502.154411	648260.508827	45.634701
3502.259134	648221.858589	45.639706
3502.603770	648186.267329	45.644711
3502.276060	648158.883253	45.649716
3502.358475	648121.035960	45.654721
3502.500776	648092.424744	45.659725
3502.210137	648054.938546	45.664730
3502.343322	648024.129561	45.669735
3502.476979	647977.576904	45.674740
3502.528835	647947.480797	45.679745
3502.532813	647925.239299	45.684749
3502.461768	647873.571984	45.689754
3502.521046	647845.623486	45.694759
3502.376818	647808.462102	45.699764
3502.797323	647757.562857	45.704769
3502.466162	647725.280076	45.709773
3502.271187	647678.430321	45.714778
3502.579372	647654.288804	45.719783
3502.005192	647617.447466	45.724788
3502.286924	647590.261301	45.729793
3501.945351	647563.627604	45.734797
3502.203314	647528.348188	45.739802
3502.262706	647499.249130	45.744807
3501.967916	647473.607121	45.749812
3502.520670	647429.132088	45.754817
3502.272381	647391.186595	45.759821
3502.154558	647289.841440	45.764826
3501.979430	647144.969138	45.769831
3502.091390	646948.663492	45.774836
3502.063090	646695.343530	45.779841
3501.656398	646391.342595	45.784845
3501.709859	646010.223664	45.789850
3501.408370	645585.706527	45.794855
3500.887948	645100.215560	45.799860
3501.011296	644553.749845	45.804865
3500.317382	643957.390188	45.809869
3499.943406	643300.989948	45.814874
3499.710961	642582.066685	45.819879
3498.941331	641805.119984	45.824884
3498.594175	640984.282557	45.829889
3497.955037	640099.154312	45.834893
3497.445218	639154.001354	45.839898
3496.915511	638144.579619	45.844903
3496.218819	637083.052747	45.849908
3495.558734	635953.008987	45.854913
3494.604187	634770.294820	45.859917
3493.642093	633531.091733	45.864922
3492.978629	632231.775731	45.869927
3492.101975	630879.167893	45.874932
3491.398640	629449.852415	45.879937
3490.500251	627975.708253	45.884941
3489.354086	626435.691276	45.889946
3488.181595	624846.417742	45.894951
3486.737277	623199.641053	45.899956
3485.834037	621498.108266	45.904961
3484.702349	619751.744222	45.909965
3483.407775	617928.840389	45.914970
3481.791167	616072.599668	45.919975
3480.455644	614154.728889	45.924980
3479.167985	612184.965289	45.929985
3477.345554	610179.881403	45.934989
3476.173823	608118.847097	45.939994
3474.667902	605996.878429	45.944999
3472.790630	603833.723210	45.950004
3471.416027	601626.255203	45.955009
3469.456066	599364.489669	45.960013
3467.926277	597051.645186	45.965018
3466.201507	594719.138522	45.970023
3463.977632	592339.532727	45.975028
3462.510399	589890.337155	45.980033
3460.557421	587425.089957	45.985037
3458.910806	584889.266261	45.990042
3456.774469	582330.067317	45.995047
3454.247349	579721.719239	46.000052
3452.182813	577068.984221	46.005057
3450.075089	574390.687746	46.010061
3447.909554	571667.850305	46.015066
3445.604657	568899.958712	46.020071
3443.173223	566122.780554	46.025076
3440.919575	563297.090841	46.030081
3438.678566	560441.928884	46.035085
3436.234132	557546.083721	46.040090
3433.908342	554624.396408	46.045095
3431.185190	551663.687385	46.050100
3428.686708	548667.011166	46.055105
3426.088861	545652.253119	46.060109
3423.360559	542595.358731	46.065114
3420.758338	539525.521542	46.070119
3418.076185	536416.993849	46.075124
3415.846646	533273.455370	46.080129
3412.539288	530123.106349	46.085133
3410.054312	526939.940730	46.090138
3406.886493	523721.214842	46.095143
3404.249342	520490.856542	46.100148
3401.544191	517209.310246	46.105153
3398.102559	513921.026025	46.110157
3395.376712	510615.409209	46.115162
3392.455363	507278.505584	46.120167
3389.257743	503933.828643	46.125172
3386.362778	500551.805936	46.130177
3382.860366	497172.330304	46.135181
3379.873318	493757.285855	46.140186
3376.853428	490333.468667	46.145191
3373.418749	486884.701105	46.150196
3370.537638	483425.954710	46.155201
3367.031585	479943.201767	46.160205
3363.939057	476444.978007	46.165210
3360.785614	472931.920993	46.170215
3357.258477	469407.124537	46.175220
3353.883380	465858.751819	46.180225
3350.406195	462307.721967	46.185229
3346.970753	458744.593766	46.190234
3343.453622	455164.880851	46.195239
3340.034950	451572.612752	46.200244
3336.551423	447963.054766	46.205249
3333.143521	444362.155734	46.210253
3329.535334	440728.329014	46.215258
3326.138405	437101.534161	46.220263
3322.560079	433464.750326	46.225268
3319.081931	429822.252500	46.230273
3315.236310	426166.005605	46.235277
3311.731512	422494.629675	46.240282
3307.988442	418832.953676	46.245287
3304.519481	415146.631168	46.250292
3301.127121	411454.743026	46.255297
3296.903483	407771.316843	46.260301
3293.657611	404079.127221	46.265306
3289.732190	400380.793797	46.270311
3285.466399	396670.223612	46.275316
3281.954821	392966.658856	46.280321
3278.379123	389260.414230	46.285325
3274.626934	385556.120598	46.290330
3270.692268	381838.743219	46.295335
3266.729178	378130.510573	46.300340
3263.072291	374407.253679	46.305345
3258.876692	370706.017169	46.310349
3255.499313	366981.379601	46.315354
3251.594554	363271.719509	46.320359
3247.485499	359553.421131	46.325364
3243.796295	355841.476957	46.330369
3239.903170	352137.276251	46.335373
3235.837590	348418.921981	46.340378
3231.955434	344710.130259	46.345383
3227.841304	341004.699053	46.350388
3224.104384	337315.698282	46.355393
3220.093220	333612.634241	46.360397
3216.110106	329910.407138	46.365402
3211.991644	326207.605685	46.370407
3207.811212	322525.052704	46.375412
3204.296048	318828.582887	46.380417
3199.817866	315153.658025	46.385421
3195.806358	311475.515034	46.390426
3191.382145	307817.759899	46.395431
3187.253669	304163.867803	46.400436
3183.582388	300517.593062	46.405441
3179.231000	296888.328355	46.410445
3175.628961	293256.651306	46.415450
3171.874971	289643.068737	46.420455
3167.854052	286018.199647	46.425460
3163.393404	282398.279971	46.430465
3159.413423	278799.825294	46.435469
3155.505432	275200.096882	46.440474
3151.269019	271605.615441	46.445479
3147.444074	268022.204576	46.450484
3143.730874	264457.387466	46.455489
3139.251358	260899.172000	46.460493
3134.992992	257324.434053	46.465498
3130.834866	253781.670713	46.470503
3126.687552	250240.600355	46.475508
3122.888236	246712.842485	46.480513
3118.416975	243201.300715	46.485517
3114.325387	239694.478766	46.490522
3110.403051	236204.238249	46.495527
3106.371561	232722.409011	46.500532
3102.210429	229235.278258	46.505537
3098.202812	225777.646144	46.510541
3094.200061	222325.481272	46.515546
3090.127392	218884.814942	46.520551
3086.087670	215448.254928	46.525556
3082.283761	212013.791283	46.530561
3078.413444	208595.588697	46.535565
3074.213043	205199.274116	46.540570
3070.062591	201711.973085	46.545575
3065.746153	198317.964297	46.550580
3061.660037	194923.921161	46.555585
3057.796943	191570.492437	46.560589
3053.580840	188216.147504	46.565594
3049.253544	184876.814004	46.570599
3044.627341	181550.684292	46.575604
3041.037161	178238.957232	46.580609
3037.048079	174943.008007	46.585613
3032.871624	171637.718774	46.590618
3029.037216	168360.045447	46.595623
3024.720331	165088.349120	46.600628
3020.691559	161832.901995	46.605633
3016.450166	158602.503755	46.610637
3012.401957	155368.971269	46.615642
3008.199137	152147.770789	46.620647
3003.782892	148956.947831	46.625652
2999.782144	145764.333281	46.630657
2995.748070	142593.058848	46.635661
2991.760411	139435.193951	46.640666
2987.666377	136291.098434	46.645671
2983.360490	133165.432633	46.650676
2979.594992	130035.021606	46.655681
2975.249404	126933.517312	46.660685
2970.815906	123836.556359	46.665690
2966.984951	120755.592122	46.670695
2962.820234	117706.381043	46.675700
2958.626311	114644.311519	46.680705
2954.390655	111631.464695	46.685709
2950.113650	108605.630715	46.690714
2945.887272	105603.070487	46.695719
2941.342650	102622.193319	46.700724
2937.669673	99657.000680	46.705729
2933.131405	96708.897201	46.710733
2929.201983	93781.606481	46.715738
2925.000325	90866.795601	46.720743
2920.225385	87968.677968	46.725748
2916.301357	85082.838313	46.730753
2911.754751	82242.891126	46.735757
2907.408991	79398.383991	46.740762
2903.370440	76580.429973	46.745767
2898.605117	73793.056673	46.750772
2894.499467	71004.197740	46.755777
2889.692852	68267.520400	46.760781
2885.429212	65532.036785	46.765786
2880.083485	62840.853094	46.770791
2874.976842	60170.712687	46.775796
2870.298738	57547.360511	46.780801
2864.265552	54970.184034	46.785805
2857.200567	52486.824128	46.790810
2848.836855	50098.123105	46.795815
2839.879032	47785.924036	46.800820
2831.738004	45564.270047	46.805825
2823.010400	43435.028867	46.810829
2815.569713	41416.043337	46.815834
2807.925917	39483.165902	46.820839
2800.426532	37668.206124	46.825844
2793.560700	35929.772629	46.830849
2786.584740	34286.584063	46.835853
2780.161275	32723.839566	46.840858
2774.112940	31256.144213	46.845863
2767.851658	29852.273039	46.850868
2762.220800	28537.245955	46.855873
2756.670625	27289.501569	46.860877
2751.202822	26096.717396	46.865882
2745.684491	24959.201745	46.870887
2740.792110	23885.575555	46.875892
2736.058144	22858.129880	46.880897
2731.045896	21889.964371	46.885901
2726.514889	20974.072298	46.890906
2722.195348	20087.402553	46.895911
2716.849069	19244.974686	46.900916
2712.606508	18449.580689	46.905921
2707.438243	17696.572011	46.910925
2703.190128	16980.932108	46.915930
2698.456504	16295.854199	46.920935
2693.412513	15651.520470	46.925940
2689.205750	15049.448238	46.930945
2684.661610	14473.178358	46.935949
2680.286200	13922.929626	46.940954
2676.259079	13405.171707	46.945959
2671.728125	12911.731405	46.950964
2667.981350	12431.482911	46.955969
2663.596915	11996.866017	46.960973
2659.797668	11563.616064	46.965978
2656.265182	11148.800173	46.970983
2652.638128	10763.283873	46.975988
2648.773322	10377.808091	46.980993
2645.219469	10003.675161	46.985997
2641.813749	9640.215326	46.991002
2638.704603	9291.336685	46.996007
2635.228307	8944.940626	47.001012
2631.813765	8588.988597	47.006017
2628.453524	8256.674867	47.011021
2625.087669	7921.123865	47.016026
2621.906393	7582.690600	47.021031
2618.285442	7258.669687	47.026036
2615.311779	6928.785283	47.031041
2611.755975	6612.231049	47.036045
2608.851083	6288.178051	47.041050
2605.721589	5958.077322	47.046055
2602.107761	5639.038590	47.051060
2598.960703	5298.584157	47.056065
2595.748519	4980.635790	47.061069
2592.161451	4657.392786	47.066074
2589.081067	4334.477841	47.071079
2585.828063	4009.547518	47.076084
2582.327909	3684.241497	47.081089
2578.473227	3357.740244	47.086093
2574.993667	3028.715479	47.091098
2571.913214	2713.031427	47.096103
2567.929086	2403.269226	47.101108
2564.467157	2077.707619	47.106113
2561.085599	1772.099088	47.111117
2557.638415	1466.422121	47.116122
2553.561666	1166.425567	47.121127
2549.776253	859.559207	47.126132
2546.087842	576.975430	47.131137
2541.383736	309.687609	47.136141
2534.917021	116.389772	47.141146
2520.088803	173.895454	47.146151
2511.456860	178.349793	47.151156
2507.485149	174.729805	47.156161
2504.878079	177.546826	47.161165
2502.964527	174.830791	47.166170
2501.739730	168.413614	47.171175
2499.396707	169.240484	47.176180
2496.852251	171.493435	47.181185
2494.026614	175.365210	47.186189
2490.478409	171.805977	47.191194
2487.564416	166.830936	47.196199
2483.714644	173.877651	47.201204
2480.471874	168.423862	47.206209
2477.158655	171.938618	47.211213
2473.318485	171.403491	47.216218
2470.737586	163.731876	47.221223
2467.292316	174.469999	47.226228
2463.930844	167.372032	47.231233
2460.494643	167.878899	47.236237
2456.684915	165.747404	47.241242
2454.016972	158.169106	47.246247
2450.206240	165.619077	47.251252
2447.133131	158.181859	47.256257
2443.779792	164.755725	47.261261
2440.131311	161.429568	47.266266
2436.736399	161.956475	47.271271
2433.300887	169.864912	47.276276
2430.406959	159.159963	47.281281
2427.273139	173.272536	47.286285
2423.664863	168.597439	47.291290
2419.584619	156.645165	47.296295
2415.642276	161.525009	47.301300
2413.278505	154.224313	47.306305
2409.882927	158.838077	47.311309
2405.778109	154.339686	47.316314
2402.335147	156.958466	47.321319
2398.695402	160.405804	47.326324
2395.561594	161.270111	47.331329
2391.973035	158.106971	47.336333
2389.207085	162.395400	47.341338
2386.401626	154.810836	47.346343
2382.143627	157.088579	47.351348
2378.937387	154.749582	47.356353
2374.859947	155.566806	47.361357
2371.187777	158.540767	47.366362
2368.102759	159.259294	47.371367
2365.221955	161.214986	47.376372
2362.036390	156.747031	47.381377
2357.869517	163.740007	47.386381
2354.130936	158.130758	47.391386
2351.070096	158.447466	47.396391
2347.427164	162.138095	47.401396
2344.014903	159.544422	47.406401
2340.471646	158.490715	47.411405
2336.857855	154.713515	47.416410
2333.318673	154.413376	47.421415
2329.853447	163.756906	47.426420
2326.621576	158.254267	47.431425
2323.326586	158.630367	47.436429
2319.738245	164.259558	47.441434
2316.371683	157.663397	47.446439
2312.519237	157.413806	47.451444
2309.191243	154.219751	47.456449
2305.733835	157.005957	47.461453
2301.991757	154.290145	47.466458
2298.912184	150.330650	47.471463
2295.293714	148.691058	47.476468
2291.776164	151.461547	47.481473
2288.187934	155.886370	47.486477
2284.708082	160.619508	47.491482
2281.585122	155.925975	47.496487
2277.924403	150.773607	47.501492
2274.607030	163.106938	47.506497
2271.099744	158.035411	47.511501
2267.481758	155.013587	47.516506
2263.788667	157.293480	47.521511
2260.387262	161.030928	47.526516
2257.397536	155.022638	47.531521
2253.471938	151.550959	47.536525
2250.007562	160.366115	47.541530
2246.587617	154.836173	47.546535
2243.024363	158.187713	47.551540
2239.484575	155.479401	47.556545
2236.088676	161.255073	47.561549
2232.618958	160.753697	47.566554
2229.450481	152.005860	47.571559
2225.665346	152.210947	47.576564
2222.169777	150.848905	47.581569
2218.764183	158.104266	47.586573
2215.047702	154.765437	47.591578
2212.046258	144.609051	47.596583
2208.058417	153.896063	47.601588
2204.523327	155.995395	47.606593
2201.061267	159.751776	47.611597
2197.585301	155.932785	47.616602
2194.549638	154.171585	47.621607
2190.942005	158.741369	47.626612
2187.439128	154.939657	47.631617
2183.746321	150.424349	47.636621
2179.929954	151.505490	47.641626
2176.771591	149.584587	47.646631
2173.318116	150.496291	47.651636
2169.786699	141.787315	47.656641
2166.245867	150.441680	47.661645
2163.061882	150.943814	47.666650
2159.713662	148.162096	47.671655
2155.532240	163.165300	47.676660
2152.280177	146.901019	47.681665
2148.669155	147.799286	47.686669
2145.606044	151.676709	47.691674
2142.464926	144.896246	47.696679
2138.268193	156.082467	47.701684
2134.878816	152.883084	47.706689
2131.274706	156.522855	47.711693
2127.708103	145.195296	47.716698
2124.597852	147.130993	47.721703
2120.741577	153.532150	47.726708
2117.398285	149.446218	47.731713
2113.902865	151.236935	47.736717
2110.163011	152.069082	47.741722
2106.998990	151.600793	47.746727
2103.401293	153.212843	47.751732
2100.365411	147.215442	47.756737
2096.416360	146.549405	47.761741
2092.756273	150.763628	47.766746
2089.568495	140.862282	47.771751
2085.839828	150.319709	47.776756
2082.466585	154.696937	47.781761
2079.055477	149.872142	47.786765
2075.301753	147.411030	47.791770
2072.168498	150.693259	47.796775
2068.351369	146.137006	47.801780
2065.627359	146.900696	47.806785
2061.610459	152.789684	47.811789
2058.181386	148.863598	47.816794
2054.674078	142.353049	47.821799
2050.742131	146.316580	47.826804
2047.195949	150.787511	47.831809
2043.850719	152.927434	47.836813
2040.357229	143.238823	47.841818
2036.895058	146.942838	47.846823
2033.649028	149.909027	47.851828
2030.152366	141.636074	47.856833
2026.396286	142.779999	47.861837
2023.192934	145.495628	47.866842
2019.889032	150.817752	47.871847
2015.748814	151.503951	47.876852
2012.396793	147.802574	47.881857
2008.862599	153.288839	47.886861
2005.230382	147.756646	47.891866
2001.973705	146.782752	47.896871
1998.610803	146.925388	47.901876
1994.991311	142.994489	47.906881
1991.273723	146.447668	47.911885
1988.155961	140.723569	47.916890
1984.821502	140.116166	47.921895
1980.994302	140.713006	47.926900
1977.632252	145.715991	47.931905
1974.221530	141.920144	47.936909
1970.474910	143.052880	47.941914
1967.300854	142.578645	47.946919
1963.677650	147.904205	47.951924
1959.885676	138.638131	47.956929
1956.382515	139.201995	47.961933
1953.168065	137.191246	47.966938
1949.644521	141.907941	47.971943
1946.074519	151.548634	47.976948
1942.848092	150.654640	47.981953
1939.283698	141.203977	47.986957
1935.288346	141.404543	47.991962
1932.073037	132.155145	47.996967
1928.207264	146.034806	48.001972
1925.203439	147.690193	48.006977
1921.730660	144.194724	48.011981
1918.166997	144.355578	48.016986
1914.419041	143.564123	48.021991
1910.634973	150.156568	48.026996
1907.577544	150.206780	48.032001
1904.444179	141.477864	48.037005
1900.724996	144.511632	48.042010
1897.167281	141.808912	48.047015
1893.669112	156.321732	48.052020
1890.072253	141.483577	48.057025
1886.452527	157.278663	48.062029
1882.939613	150.471585	48.067034
1879.664310	138.012540	48.072039
1876.003174	149.536147	48.077044
1872.820531	141.851821	48.082049
1868.873171	146.337240	48.087053
1865.413848	146.033135	48.092058
1862.177475	140.879690	48.097063
1858.410229	156.790330	48.102068
1855.547544	142.225811	48.107073
1851.482834	140.432344	48.112077
1847.861452	147.795015	48.117082
1845.159243	144.538187	48.122087
1841.237549	153.004856	48.127092
1837.783491	144.092154	48.132097
1833.936404	139.621170	48.137101
1830.088992	152.851780	48.142106
1827.026587	135.874257	48.147111
1823.241368	143.962193	48.152116
1820.229110	139.299839	48.157121
1816.586503	141.089229	48.162125
1812.813070	141.520436	48.167130
1809.666880	133.551891	48.172135
1806.041942	142.391668	48.177140
1802.546311	139.505108	48.182145
1799.179491	145.241916	48.187149
1795.213240	145.570798	48.192154
1792.401128	138.587449	48.197159
1788.662255	149.035827	48.202164
1785.346468	141.123335	48.207169
1781.468271	133.586151	48.212173
1777.800417	149.505477	48.217178
1774.474076	141.421078	48.222183
1770.864654	147.081354	48.227188
1767.377352	139.065389	48.232193
1764.047294	145.178392	48.237197
1760.652034	149.537958	48.242202
1757.164191	141.343892	48.247207
1753.435051	151.249978	48.252212
1750.146334	132.780136	48.257217
1746.757227	146.073614	48.262221
1742.816591	150.265368	48.267226
1739.808246	147.439648	48.272231
1735.986038	150.623765	48.277236
1732.603984	141.430678	48.282241
1728.992324	142.840076	48.287245
1725.190406	135.092606	48.292250
1722.139107	127.151079	48.297255
1718.241707	137.879071	48.302260
1715.138963	141.474787	48.307265
1711.539945	135.966759	48.312269
1708.111573	137.391675	48.317274
1704.640919	135.345479	48.322279
1700.847030	139.803501	48.327284
1697.494445	142.135503	48.332289
1694.397381	140.904764	48.337293
1690.286703	147.321824	48.342298
1687.061214	134.434378	48.347303
1683.473816	139.218837	48.352308
1679.927859	147.701098	48.357313
1676.394098	142.706250	48.362317
1672.855639	148.011698	48.367322
1669.727881	136.928176	48.372327
1665.908691	143.876087	48.377332
1662.407855	142.662549	48.382337
1659.069221	131.220583	48.387341
1655.164988	134.321814	48.392346
1652.122321	134.479275	48.397351
1648.204143	137.297464	48.402356
1645.213726	135.131907	48.407361
1641.778955	128.856386	48.412365
1637.950219	132.812065	48.417370
1634.888988	135.035979	48.422375
1630.745072	139.152870	48.427380
1627.617895	142.651246	48.432385
1623.935517	137.636202	48.437389
1620.129872	145.674378	48.442394
1616.883921	134.127737	48.447399
1613.359053	139.649630	48.452404
1610.265333	138.882536	48.457409
1606.553796	132.276842	48.462413
1602.818599	145.210810	48.467418
1599.549643	131.364450	48.472423
1595.726131	128.115254	48.477428
1592.448104	131.553918	48.482433
1589.260983	139.055963	48.487437
1585.406490	133.874026	48.492442
1582.231263	133.587323	48.497447
1578.339357	143.425302	48.502452
1574.708808	127.988766	48.507457
1571.436476	134.946630	48.512461
1567.887517	137.147773	48.517466
1564.310917	137.342408	48.522471
1560.709263	132.280533	48.527476
1557.589172	131.071452	48.532481
1553.839596	135.417280	48.537485
1550.162000	134.686520	48.542490
1546.903450	130.523079	48.547495
1543.474071	137.098421	48.552500
1540.363668	121.535321	48.557505
1536.605582	128.985516	48.562509
1532.766188	127.557472	48.567514
1529.500004	133.677236	48.572519
1525.575113	131.405101	48.577524
1522.401150	134.346490	48.582529
1519.050946	132.039977	48.587533
1515.507595	130.270176	48.592538
1511.919024	124.348746	48.597543
1508.212035	124.023277	48.602548
1504.627855	131.023638	48.607553
1501.580249	124.796141	48.612557
1497.664241	123.665943	48.617562
1494.341140	124.834638	48.622567
1491.009092	126.768118	48.627572
1487.486702	124.046468	48.632577
1484.155048	135.331164	48.637581
1480.186663	132.779326	48.642586
1476.912916	129.507854	48.647591
1473.131205	125.785347	48.652596
1470.055539	130.699302	48.657601
1466.571133	131.879084	48.662605
1462.766319	132.282210	48.667610
1459.470493	117.703956	48.672615
1455.901226	130.087049	48.677620
1452.063256	127.326410	48.682625
1448.780794	128.713189	48.687629
1445.386354	125.337759	48.692634
1442.393105	129.806925	48.697639
1438.212378	132.388454	48.702644
1434.855645	126.318657	48.707649
1431.455966	127.124123	48.712653
1427.512909	123.009768	48.717658
1424.367859	126.755726	48.722663
1420.687241	136.660131	48.727668
1417.649287	131.726229	48.732673
1413.797464	134.331567	48.737677
1410.303105	131.126206	48.742682
1406.682295	125.327016	48.747687
1402.936318	130.254510	48.752692
1399.302962	125.107827	48.757697
1396.224175	123.301201	48.762701
1392.543312	123.720999	48.767706
1389.556470	120.002367	48.772711
1385.863880	134.041625	48.777716
1382.231658	133.377898	48.782721
1378.631146	130.718973	48.787725
1375.089735	141.179592	48.792730
1371.840454	123.292838	48.797735
1368.291971	128.873860	48.802740
1364.796667	126.878967	48.807745
1361.225459	136.475045	48.812749
1357.468041	137.312856	48.817754
1354.483980	128.686578	48.822759
1350.356579	131.384285	48.827764
1347.356378	133.328335	48.832769
1344.021726	123.105336	48.837773
1340.502267	138.073100	48.842778
1336.884814	122.816183	48.847783
1333.449196	138.434728	48.852788
1329.929529	132.191251	48.857793
1326.157122	125.905490	48.862797
1322.408406	138.633485	48.867802
1319.545759	127.682846	48.872807
1315.636232	132.170539	48.877812
1312.357095	125.332998	48.882817
1308.631566	133.209361	48.887821
1304.817104	134.399618	48.892826
1301.949761	123.939564	48.897831
1297.994779	126.698210	48.902836
1294.958123	130.251098	48.907841
1291.556543	125.226433	48.912845
1287.820863	132.942277	48.917850
1284.353276	122.483776	48.922855
1280.583044	129.168917	48.927860
1277.052680	126.599913	48.932865
1273.635706	122.211854	48.937869
1270.103948	133.681311	48.942874
1266.890052	120.386782	48.947879
1263.218347	126.020808	48.952884
1259.785338	127.963050	48.957889
1256.166757	129.113861	48.962893
1252.361135	125.033778	48.967898
1249.109660	124.136914	48.972903
1245.546235	129.667212	48.977908
1242.270903	129.265668	48.982913
1238.803572	115.601613	48.987917
1235.145324	123.537156	48.992922
1231.808805	122.954514	48.997927
1228.208374	126.850868	49.002932
1224.706546	134.944286	49.007937
1221.146573	128.486941	49.012941
1217.522334	132.220686	49.017946
1214.244552	124.305338	49.022951
1210.770299	127.425633	49.027956
1207.045530	128.631137	49.032961
1203.646301	127.471606	49.037965
1199.929318	129.422949	49.042970
1196.634357	122.177655	49.047975
1193.188047	123.007976	49.052980
1189.482285	127.769733	49.057985
1186.228563	128.456329	49.062989
1182.752884	124.976526	49.067994
1179.289286	130.746316	49.072999
1175.475145	128.512815	49.078004
1171.988664	124.729328	49.083009
1168.684647	126.265897	49.088013
1165.176724	135.849277	49.093018
1161.670125	120.748056	49.098023
1157.771502	126.580507	49.103028
1154.142322	114.298802	49.108033
1151.086813	115.799625	49.113037
1147.562802	126.774730	49.118042
1144.206739	119.390000	49.123047
1140.546484	134.163300	49.128052
1137.087018	124.442416	49.133057
1133.895087	128.161780	49.138061
1130.041548	135.173196	49.143066
1126.662388	123.200446	49.148071
1123.112446	123.888110	49.153076
1119.331609	126.524772	49.158081
1115.949166	132.228105	49.163085
1112.409523	131.474891	49.168090
1109.099560	126.945341	49.173095
1105.322831	134.911820	49.178100
1102.116058	130.993930	49.183105
1098.619524	125.129069	49.188109
1095.589390	120.758692	49.193114
1092.034814	120.309496	49.198119
1088.102742	125.442249	49.203124
1084.056792	124.134781	49.208129
1080.486801	124.616221	49.213133
1077.523994	127.486088	49.218138
1074.061614	125.315875	49.223143
1069.844930	129.570192	49.228148
1066.977566	133.644225	49.233153
1063.919314	127.070706	49.238157
1060.227171	128.034721	49.243162
1056.646401	123.686549	49.248167
1053.059038	137.240546	49.253172
1049.092892	129.732197	49.258177
1046.034730	117.293417	49.263181
1042.750644	122.962576	49.268186
1039.394188	129.534093	49.273191
1035.584728	126.654647	49.278196
1031.718908	120.565162	49.283201
1028.712341	129.988371	49.288205
1024.768893	131.944545	49.293210
1021.135310	124.638167	49.298215
1017.781971	124.125955	49.303220
1014.510993	125.682036	49.308225
1011.316742	121.831412	49.313229
1007.417963	127.147972	49.318234
1004.053840	123.096533	49.323239
1000.300198	120.915540	49.328244
996.932896	126.470420	49.333249
993.587621	127.054878	49.338253
989.731031	129.674572	49.343258
986.544964	120.049313	49.348263
982.846201	126.553545	49.353268
979.333887	126.267160	49.358273
975.971759	123.294255	49.363277
972.225561	123.034910	49.368282
969.154236	120.400702	49.373287
965.529708	120.956175	49.378292
961.743786	124.448868	49.383297
958.093229	124.467751	49.388301
955.107635	124.254713	49.393306
951.529742	117.865098	49.398311
947.879915	126.502371	49.403316
944.236150	116.902718	49.408321
941.434901	117.285157	49.413325
937.488006	122.326354	49.418330
933.876972	122.067184	49.423335
930.166126	124.981129	49.428340
926.740584	128.976268	49.433345
923.313918	134.050636	49.438349
919.582462	124.711779	49.443354
916.153732	122.511856	49.448359
912.683944	132.055944	49.453364
909.106275	129.676610	49.458369
905.706033	121.034057	49.463373
902.504900	132.341526	49.468378
899.251919	124.227955	49.473383
895.448874	125.016266	49.478388
892.092506	120.866938	49.483393
888.689667	120.673225	49.488397
884.760690	125.980276	49.493402
881.443850	113.284070	49.498407
877.713479	116.739225	49.503412
874.013347	115.725423	49.508417
870.490802	121.020519	49.513421
867.124459	123.056613	49.518426
863.991131	119.799087	49.523431
860.446117	123.195184	49.528436
856.922192	115.399382	49.533441
853.755540	118.546617	49.538445
849.846504	117.796694	49.543450
845.945719	113.916040	49.548455
842.663911	122.047326	49.553460
839.188279	125.668374	49.558465
835.938282	117.288946	49.563469
832.367077	121.042629	49.568474
829.089656	117.845469	49.573479
825.643046	116.624999	49.578484
821.595635	120.225782	49.583489
817.936629	117.009064	49.588493
814.255859	125.430535	49.593498
811.313689	115.877562	49.598503
807.942301	116.737618	49.603508
804.396165	119.598765	49.608513
800.916025	113.193113	49.613517
797.025663	124.157415	49.618522
794.000162	120.315945	49.623527
790.348713	135.193201	49.628532
786.712256	125.542354	49.633537
783.557160	124.570491	49.638541
779.656977	121.434546	49.643546
776.355477	113.227874	49.648551
772.603887	117.649627	49.653556
769.014296	118.187837	49.658561
765.765881	117.562949	49.663565
762.017106	122.880155	49.668570
758.739948	116.524435	49.673575
755.326815	123.044541	49.678580
751.810933	121.983590	49.683585
748.437381	120.457260	49.688589
744.752252	124.584865	49.693594
741.259583	121.439758	49.698599
737.795414	116.817217	49.703604
733.809803	115.839116	49.708609
730.736395	121.342603	49.713613
726.974446	127.991869	49.718618
723.395077	116.698879	49.723623
720.407444	114.732410	49.728628
716.418006	119.506926	49.733633
713.689169	118.097947	49.738637
709.709304	119.679557	49.743642
706.317280	110.909132	49.748647
702.970365	115.949936	49.753652
699.037909	114.956364	49.758657
695.930116	113.901752	49.763661
692.284864	128.562747	49.768666
688.653887	117.212417	49.773671
684.846267	123.451508	49.778676
681.053705	117.277614	49.783681
678.219310	116.715329	49.788685
674.562292	123.105736	49.793690
671.062951	115.804503	49.798695
667.557798	118.219704	49.803700
664.061675	115.887274	49.808705
660.897861	111.067106	49.813709
657.260511	126.411968	49.818714
653.805406	107.033347	49.823719
650.021606	117.014362	49.828724
646.417664	122.375582	49.833729
643.033898	116.272819	49.838733
639.543765	119.570611	49.843738
636.188079	107.882339	49.848743
632.688945	113.469542	49.853748
629.162687	116.114609	49.858753
625.991093	109.430730	49.863757
621.875339	117.992192	49.868762
618.581817	107.649549	49.873767
614.900623	117.240452	49.878772
611.449523	122.275078	49.883777
608.148659	116.292422	49.888781
604.266908	126.754609	49.893786
600.986207	111.611227	49.898791
597.541405	120.036045	49.903796
594.108148	122.144587	49.908801
590.802559	115.952761	49.913805
587.022124	121.930501	49.918810
583.795056	118.291061	49.923815
579.829889	118.593589	49.928820
576.254916	119.315427	49.933825
572.869811	109.914865	49.938829
569.086640	113.082606	49.943834
566.381829	112.279516	49.948839
562.818525	125.101281	49.953844
559.385245	118.649996	49.958849
555.799376	107.954398	49.963853
551.862669	125.302095	49.968858
548.597764	119.488179	49.973863
544.900384	117.806218	49.978868
541.421513	111.817355	49.983873
537.976947	107.700671	49.988877
534.377164	111.535285	49.993882
530.754832	110.022667	49.998887
527.462402	110.898286	50.003892
524.140608	120.264223	50.008897
520.603804	114.770607	50.013901
516.961758	108.590316	50.018906
513.515845	119.919572	50.023911
510.140757	112.586870	50.028916
506.259426	114.635830	50.033921
503.039022	110.380256	50.038925
499.405328	112.953612	50.043930
495.871827	113.962486	50.048935
492.473413	108.968740	50.053940
488.912277	106.352197	50.058945
485.640548	105.927925	50.063949
481.713335	117.537931	50.068954
478.483459	105.868845	50.073959
475.151617	114.549153	50.078964
471.468429	109.118484	50.083969
468.160431	109.780049	50.088973
464.646868	112.972132	50.093978
461.046448	114.131823	50.098983
457.407374	101.166883	50.103988
453.829840	113.097926	50.108993
450.774458	104.816664	50.113997
446.870655	120.950501	50.119002
443.638440	104.827564	50.124007
439.712893	105.404274	50.129012
435.941246	110.236523	50.134017
432.950509	107.422622	50.139021
429.349763	112.635278	50.144026
426.028025	114.325098	50.149031
422.623799	114.112638	50.154036
418.946426	113.743510	50.159041
415.290969	111.870216	50.164045
411.550607	108.739542	50.169050
408.381150	105.457161	50.174055
404.830027	106.950721	50.179060
401.187025	104.611246	50.184065
397.954204	102.720908	50.189069
394.319363	107.310323	50.194074
390.805914	101.690612	50.199079
387.505670	107.836494	50.204084
383.776470	106.332808	50.209089
380.180249	100.944468	50.214093
376.365071	113.583075	50.219098
373.472785	103.724414	50.224103
369.922818	100.381903	50.229108
366.595886	106.215295	50.234113
363.245669	103.830157	50.239117
359.366321	105.757358	50.244122
355.563942	113.800677	50.249127
352.349972	105.151662	50.254132
348.889505	111.253445	50.259137
345.584182	103.866520	50.264141
341.912246	105.266068	50.269146
338.550087	101.187616	50.274151
334.721057	96.298630	50.279156
330.846838	99.436252	50.284161
327.817774	107.927025	50.289165
324.271220	106.599968	50.294170
320.860755	102.364948	50.299175
317.895960	102.510818	50.304180
314.011579	101.906089	50.309185
310.443389	95.498869	50.314189
306.465525	103.166336	50.319194
302.999735	95.810749	50.324199
299.583498	100.316101	50.329204
295.993612	91.665230	50.334209
292.970620	93.482117	50.339213
289.328389	103.151660	50.344218
285.926243	102.095749	50.349223
282.427098	101.208438	50.354228
278.168172	104.621921	50.359233
275.367551	104.944098	50.364237
271.369944	108.027013	50.369242
268.530132	102.060678	50.374247
265.019318	95.039366	50.379252
261.209211	99.511079	50.384257
258.203014	99.227732	50.389261
254.209515	102.773325	50.394266
250.643145	101.567815	50.399271
246.903897	94.935984	50.404276
243.684437	95.110643	50.409281
240.324033	94.794774	50.414285
236.676417	105.817588	50.419290
233.378107	98.109523	50.424295
229.704855	105.756034	50.429300
225.864229	102.079524	50.434305
222.864065	101.755934	50.439309
219.065259	103.325378	50.444314
215.704260	95.672502	50.449319
212.070059	97.245882	50.454324
208.326284	100.023784	50.459329
205.095554	101.712715	50.464333
201.416835	105.906588	50.469338
198.449064	95.577291	50.474343
194.594594	105.448395	50.479348
191.202235	103.444323	50.484353
187.741043	100.322300	50.489357
184.607079	105.521411	50.494362
180.616067	100.198213	50.499367
177.148958	105.083662	50.504372
173.488329	109.831642	50.509377
170.074879	99.430910	50.514381
166.688133	100.542839	50.519386
163.240107	97.430695	50.524391
159.679647	103.895296	50.529396
156.202050	109.622357	50.534401
153.143835	104.651314	50.539405
149.250139	105.219068	50.544410
145.493845	99.584131	50.549415
142.119624	101.660357	50.554420
138.282393	104.768935	50.559425
135.099072	93.762998	50.564429
131.594221	97.202342	50.569434
128.502845	94.484853	50.574439
124.844903	101.851654	50.579444
120.944862	107.405369	50.584449
117.454419	91.692348	50.589453
114.123752	110.234920	50.594458
110.349741	99.322852	50.599463
107.197344	104.822649	50.604468
103.614538	105.296347	50.609473
100.372785	102.827357	50.614477
96.629715	107.263839	50.619482
93.240520	99.720719	50.624487
89.603163	104.400187	50.629492
85.710732	108.438520	50.634497
82.493918	100.538501	50.639501
79.040279	107.376794	50.644506
75.709285	98.101121	50.649511
72.058210	101.250172	50.654516
68.628078	103.350907	50.659521
65.422609	103.068921	50.664525
61.576439	103.442996	50.669530
57.845635	99.699916	50.674535
54.184413	99.281859	50.679540
50.697733	105.214943	50.684545
47.221851	100.173625	50.689549
43.884290	112.026544	50.694554
40.657692	108.466985	50.699559
36.832683	104.017868	50.704564
33.613030	99.735907	50.709569
30.407761	102.223905	50.714573
26.795706	112.500392	50.719578
23.178514	115.319654	50.724583
19.419065	102.345283	50.729588
15.691448	105.244797	50.734593
12.430356	101.655059	50.739597
8.845434	101.624602	50.744602
5.216789	99.662968	50.749607
1.960590	103.676531	50.754612