Tue Jun 21 10:34:14 2022

Number of Points = 9932

Depth (nm)	Load (N)	Time (s)
-1.339175	112.045815	0.000000
-1.212556	119.194329	0.005005
-1.025397	108.020896	0.010010
-1.370650	100.234876	0.015014
-1.550165	93.370598	0.020019
-1.561338	86.680123	0.025024
-1.830409	75.734800	0.030029
-1.803961	60.340776	0.035034
-2.459513	48.057210	0.040038
-3.062972	49.443061	0.045043
-3.120420	29.388109	0.050048
-3.200850	35.038569	0.055053
-3.347250	28.698481	0.060058
-3.923957	15.142499	0.065062
-4.301346	9.680522	0.070067
-4.432001	0.595292	0.075072
-5.231559	8.856755	0.080077
-5.689263	4.988330	0.085082
-5.735050	7.406438	0.090086
-6.127048	8.891654	0.095091
-6.017081	7.681246	0.100096
-6.019546	11.146141	0.105101
-6.101401	3.605847	0.110106
-6.857819	6.964511	0.115110
-7.470590	6.652264	0.120115
-7.337218	-2.995672	0.125120
-7.684927	0.155995	0.130125
-7.625922	5.316068	0.135130
-7.807730	7.854183	0.140134
-8.339210	11.831736	0.145139
-8.470112	6.323025	0.150144
-9.197399	14.815048	0.155149
-8.998829	4.089326	0.160154
-9.110986	15.278275	0.165158
-9.276006	15.249059	0.170163
-9.811824	11.733771	0.175168
-10.844164	11.645316	0.180173
-10.786782	8.069689	0.185178
-10.670555	16.559378	0.190182
-10.953009	16.798051	0.195187
-10.809732	0.935413	0.200192
-10.982667	10.663497	0.205197
-10.992891	11.332666	0.210202
-11.769034	6.550430	0.215206
-12.477923	11.813786	0.220211
-12.479133	1.063527	0.225216
-12.666162	13.439403	0.230221
-12.327306	5.077008	0.235226
-12.588074	3.324939	0.240230
-13.349267	12.204219	0.245235
-13.520724	4.664949	0.250240
-14.184544	6.416783	0.255245
-13.869492	5.490911	0.260250
-14.300069	-1.544278	0.265254
-15.156887	10.071081	0.270259
-15.235784	4.292884	0.275264
-15.553603	17.030427	0.280269
-15.627606	0.637619	0.285274
-15.304839	8.328827	0.290278
-15.422488	18.250225	0.295283
-15.386767	5.274038	0.300288
-16.122239	10.699860	0.305293
-16.419790	9.040314	0.310298
-16.915273	4.572331	0.315302
-17.028654	15.702874	0.320307
-17.037121	10.672550	0.325312
-17.866320	14.042678	0.330317
-18.301586	15.566436	0.335322
-18.305828	17.245754	0.340326
-18.621991	13.570366	0.345331
-18.597658	8.734314	0.350336
-18.678910	6.845760	0.355341
-18.737446	12.754843	0.360346
-19.034632	7.032526	0.365350
-19.866582	10.747259	0.370355
-19.860019	-3.783819	0.375360
-20.123232	11.620325	0.380365
-20.107381	3.004960	0.385370
-20.075478	5.727712	0.390374
-21.310707	15.398459	0.395379
-21.318255	3.059725	0.400384
-21.682321	13.127695	0.405389
-21.318764	2.332030	0.410394
-21.421548	3.167092	0.415398
-21.880969	7.244601	0.420403
-22.576185	6.725784	0.425408
-23.271771	13.486478	0.430413
-23.445584	2.497414	0.435418
-23.173856	8.984853	0.440422
-23.644020	5.040151	0.445427
-23.424167	-5.177006	0.450432
-23.025461	6.399361	0.455437
-23.849071	9.180508	0.460442
-24.173711	11.649332	0.465446
-24.865339	16.101157	0.470451
-24.469683	9.908711	0.475456
-24.965632	11.297675	0.480461
-25.710872	10.959218	0.485466
-25.935151	10.718604	0.490470
-26.269985	12.168702	0.495475
-25.938913	7.243771	0.500480
-26.447547	4.674543	0.505485
-26.568566	9.479825	0.510490
-26.628197	6.178530	0.515494
-26.951446	17.899124	0.520499
-27.576151	6.836131	0.525504
-27.929387	9.150245	0.530509
-27.983376	9.134414	0.535514
-28.163080	9.955179	0.540518
-28.300079	22.824399	0.545523
-28.039138	4.390154	0.550528
-28.860941	12.785151	0.555533
-29.385856	10.751618	0.560538
-29.547824	11.565499	0.565542
-30.078522	13.982211	0.570547
-29.739453	1.567729	0.575552
-30.040639	8.969565	0.580557
-30.191089	8.962407	0.585562
-30.300297	0.512004	0.590566
-31.542696	19.081329	0.595571
-31.182530	5.076982	0.600576
-31.476409	12.924177	0.605581
-31.553873	7.385899	0.610586
-31.342578	3.724006	0.615590
-32.316317	6.025235	0.620595
-32.817727	-1.863925	0.625600
-33.051842	9.453352	0.630605
-33.514556	8.973193	0.635610
-33.123684	9.039194	0.640614
-33.456282	9.361554	0.645619
-33.420181	10.994724	0.650624
-33.445299	19.363567	0.655629
-33.742586	8.555380	0.660634
-34.598390	4.073068	0.665638
-35.212230	7.129688	0.670643
-35.020012	3.585605	0.675648
-35.122858	4.848103	0.680653
-35.348333	4.678333	0.685658
-34.960150	11.370066	0.690662
-35.931019	10.953533	0.695667
-36.164833	1.195510	0.700672
-36.546735	8.436468	0.705677
-36.778895	5.448102	0.710682
-36.758308	1.807135	0.715686
-36.891485	12.571346	0.720691
-37.125956	3.332024	0.725696
-37.930531	10.951804	0.730701
-38.321364	16.381732	0.735706
-37.932472	3.281551	0.740710
-38.164820	15.769518	0.745715
-38.364228	8.728015	0.750720
-39.078229	10.871583	0.755725
-39.403003	2.236061	0.760730
-39.592847	11.083874	0.765734
-39.856639	13.978928	0.770739
-39.326190	11.354649	0.775744
-39.594654	13.333466	0.780749
-40.343320	10.128712	0.785754
-40.600335	-0.760728	0.790758
-41.059519	17.584571	0.795763
-41.159921	8.114464	0.800768
-41.206876	6.079927	0.805773
-41.720928	6.034314	0.810778
-42.246682	0.216456	0.815782
-42.956472	7.996165	0.820787
-42.836491	12.043045	0.825792
-42.825865	12.141822	0.830797
-42.535590	11.264648	0.835802
-42.767420	6.669536	0.840806
-42.965779	8.119334	0.845811
-43.277393	8.015136	0.850816
-43.961353	15.355253	0.855821
-44.121585	6.045227	0.860826
-44.329940	-1.497793	0.865830
-44.530009	6.862916	0.870835
-45.042538	7.401751	0.875840
-45.676679	6.101051	0.880845
-45.858581	8.203272	0.885850
-45.443943	2.434715	0.890854
-45.949244	13.609633	0.895859
-45.640226	10.067716	0.900864
-46.138436	11.139350	0.905869
-46.822695	11.755957	0.910874
-46.662696	3.449822	0.915878
-47.424894	16.638452	0.920883
-47.354692	10.567190	0.925888
-47.611432	22.620726	0.930893
-48.026513	12.380831	0.935898
-48.374867	8.801355	0.940902
-48.996752	21.565770	0.945907
-49.197747	6.876461	0.950912
-49.211773	7.713006	0.955917
-48.795460	14.742848	0.960922
-49.039613	12.683938	0.965926
-49.276340	16.481457	0.970931
-49.176621	6.294844	0.975936
-50.271785	15.263968	0.980941
-50.538776	14.236752	0.985946
-50.285408	3.071179	0.990950
-51.000664	19.662557	0.995955
-51.334729	12.187512	1.000960
-52.033013	17.459971	1.005965
-52.287193	15.572231	1.010970
-52.096366	2.596611	1.015974
-52.250619	8.220607	1.020979
-52.109787	6.084920	1.025984
-52.366796	9.922895	1.030989
-52.505219	20.819995	1.035994
-52.696339	4.605438	1.040998
-53.275952	10.579301	1.046003
-53.351863	6.539715	1.051008
-54.190926	11.054635	1.056013
-54.853175	7.149641	1.061018
-54.597930	-0.474886	1.066022
-54.842575	7.976084	1.071027
-54.763666	-4.098322	1.076032
-55.323043	5.438796	1.081037
-55.224862	7.490293	1.086042
-55.244182	4.998695	1.091046
-56.218253	17.123460	1.096051
-56.847301	5.771508	1.101056
-56.909687	5.222097	1.106061
-56.886225	5.535617	1.111066
-56.678483	1.775252	1.116070
-57.199138	12.923309	1.121075
-56.963728	12.964732	1.126080
-57.187424	2.310128	1.131085
-57.953616	12.987752	1.136090
-58.237344	8.882730	1.141094
-59.112156	9.406181	1.146099
-58.691605	2.303457	1.151104
-58.988266	-3.947397	1.156109
-59.180425	4.764437	1.161114
-59.036339	1.526300	1.166118
-59.946707	6.849862	1.171123
-60.017041	-5.954826	1.176128
-60.134046	-0.482436	1.181133
-60.302063	7.143027	1.186138
-60.234776	1.643139	1.191142
-61.439904	4.996000	1.196147
-61.478418	-6.141751	1.201152
-61.745427	5.035337	1.206157
-61.690602	0.512539	1.211162
-61.764111	3.710955	1.216166
-62.041433	14.527847	1.221171
-62.047922	6.344397	1.226176
-62.856180	13.329770	1.231181
-63.051930	12.460070	1.236186
-63.073130	7.383709	1.241190
-63.354033	17.234655	1.246195
-63.395468	9.885399	1.251200
-63.792720	14.736031	1.256205
-64.502275	8.067122	1.261210
-64.711598	14.658493	1.266214
-65.214880	16.786508	1.271219
-64.651685	6.472231	1.276224
-65.158335	11.783402	1.281229
-65.224292	12.814436	1.286234
-65.515673	7.852281	1.291238
-66.297471	14.096626	1.296243
-66.606128	11.014962	1.301248
-66.524501	11.280567	1.306253
-66.650427	16.208614	1.311258
-66.115966	3.702969	1.316262
-66.850653	7.312011	1.321267
-67.424325	11.551906	1.326272
-67.737904	13.052754	1.331277
-68.383573	8.405410	1.336282
-68.369001	3.163287	1.341286
-68.373913	9.856175	1.346291
-68.900667	-3.271148	1.351296
-69.408741	5.496161	1.356301
-69.912333	10.353156	1.361306
-69.836507	9.174843	1.366310
-70.080079	15.553635	1.371315
-70.024305	1.596349	1.376320
-70.137295	7.390322	1.381325
-70.176521	5.647153	1.386330
-69.614999	1.999485	1.391334
-70.564566	-0.019364	1.396339
-71.197913	-5.096367	1.401344
-71.364578	-1.421553	1.406349
-71.627730	2.657198	1.411354
-72.337154	2.872851	1.416358
-72.900313	8.795248	1.421363
-72.758277	4.489874	1.426368
-72.942136	3.526840	1.431373
-73.237539	4.999024	1.436378
-72.874599	-1.509261	1.441382
-73.420944	6.435783	1.446387
-73.328016	1.723549	1.451392
-73.607998	4.769876	1.456397
-74.331417	-2.251142	1.461402
-74.441338	-2.061954	1.466406
-74.714025	10.074723	1.471411
-74.700217	6.309571	1.476416
-75.410233	2.966212	1.481421
-75.931605	10.810824	1.486426
-76.155236	7.130183	1.491430
-76.530415	7.357379	1.496435
-76.636549	-0.108042	1.501440
-76.249896	7.318608	1.506445
-76.426648	8.379633	1.511450
-76.168513	-3.031811	1.516454
-76.848452	8.806649	1.521459
-77.656769	-8.950847	1.526464
-77.741977	-2.083643	1.531469
-77.790754	-2.459286	1.536474
-77.891177	2.523931	1.541478
-78.893427	8.465962	1.546483
-79.204730	6.229919	1.551488
-79.318838	10.530065	1.556493
-79.482060	10.279343	1.561498
-79.346933	7.802226	1.566502
-79.449511	10.937180	1.571507
-79.523271	2.377311	1.576512
-80.336623	3.458711	1.581517
-80.929481	5.505261	1.586522
-80.799057	-1.356225	1.591526
-81.093027	4.999336	1.596531
-81.038270	0.250801	1.601536
-80.732342	3.371776	1.606541
-81.689534	11.402030	1.611546
-82.090811	4.193870	1.616550
-82.521635	-0.443267	1.621555
-82.841990	2.095888	1.626560
-82.845626	2.061063	1.631565
-82.995044	5.196274	1.636570
-82.799177	0.199015	1.641574
-83.887728	3.950331	1.646579
-83.868499	-5.472086	1.651584
-84.156352	-3.900710	1.656589
-84.534581	0.333654	1.661594
-84.316877	-0.029091	1.666598
-84.430857	5.999674	1.671603
-84.811607	6.062428	1.676608
-85.598100	-1.544286	1.681613
-85.879451	13.197645	1.686618
-85.616721	-3.919676	1.691622
-86.045499	2.103009	1.696627
-85.954352	-0.880089	1.701632
-86.117739	1.685957	1.706637
-87.105460	5.188512	1.711642
-87.201532	1.669283	1.716646
-87.520186	3.242209	1.721651
-87.315789	-2.218618	1.726656
-87.595356	0.233665	1.731661
-87.818539	3.890213	1.736666
-88.606686	-6.944208	1.741670
-89.023111	7.545596	1.746675
-89.105352	-2.221731	1.751680
-88.983448	6.053290	1.756685
-89.531346	-2.752667	1.761690
-88.929415	-9.539696	1.766694
-89.278220	2.238198	1.771699
-89.872069	1.677939	1.776704
-90.694629	3.358787	1.781709
-90.708702	8.268899	1.786714
-90.502155	6.896271	1.791718
-91.030533	-0.467845	1.796723
-90.759283	5.619470	1.801728
-91.760261	8.148406	1.806733
-92.068750	6.481996	1.811738
-92.077187	10.524091	1.816742
-92.245890	8.686530	1.821747
-92.132720	0.143066	1.826752
-92.596084	7.125786	1.831757
-93.427062	17.744092	1.836762
-93.639439	3.442468	1.841766
-93.971250	13.780770	1.846771
-94.353225	15.092653	1.851776
-94.195013	11.186765	1.856781
-94.160223	19.421953	1.861786
-93.899278	0.835774	1.866790
-94.085682	14.312267	1.871795
-95.097714	6.129984	1.876800
-95.550878	14.612333	1.881805
-95.497145	10.129576	1.886810
-95.402906	12.044380	1.891814
-95.794741	12.317750	1.896819
-96.880404	7.983830	1.901824
-96.924620	5.820378	1.906829
-97.517736	19.215244	1.911834
-97.173846	5.371267	1.916838
-97.590343	7.855109	1.921843
-97.438575	7.633917	1.926848
-97.361571	-0.141454	1.931853
-97.761289	8.885364	1.936858
-97.824048	9.564023	1.941862
-98.763752	12.340729	1.946867
-99.101235	12.427497	1.951872
-98.962982	6.470080	1.956877
-99.365235	0.483384	1.961882
-98.790556	2.967453	1.966886
-100.036491	12.622028	1.971891
-100.550115	1.489751	1.976896
-100.316035	3.773496	1.981901
-100.354806	1.353991	1.986906
-100.590910	3.835978	1.991910
-100.697357	3.581182	1.996915
-101.425289	7.762207	2.006912
-100.974413	10.619113	2.016909
-100.552139	1.123311	2.026906
-100.345175	3.547984	2.036902
-99.219972	9.571170	2.046899
-98.988479	4.280185	2.056896
-98.761353	7.205167	2.066893
-97.787052	1.186945	2.076890
-97.582259	9.146767	2.086886
-97.429138	11.217393	2.096883
-96.565365	12.479367	2.106880
-95.952494	10.448030	2.116877
-95.106506	8.581797	2.126874
-94.798288	12.199130	2.136870
-94.645696	12.513696	2.146867
-94.594135	11.308166	2.156864
-93.239484	5.668558	2.166861
-93.192983	8.448789	2.176858
-92.417389	5.230869	2.186854
-91.792249	1.917933	2.196851
-91.561676	2.515370	2.206848
-91.283444	10.765932	2.216845
-90.551948	12.759346	2.226842
-90.236345	6.320481	2.236838
-89.101381	6.939253	2.246835
-88.663315	4.449026	2.256832
-88.799525	7.346256	2.266829
-88.434569	7.438735	2.276826
-87.483914	10.449583	2.286822
-86.895340	9.590797	2.296819
-86.199674	2.682161	2.306816
-85.761195	8.059162	2.316813
-85.873999	2.057375	2.326810
-85.241751	7.538028	2.336806
-84.198317	4.603945	2.346803
-84.067418	7.551385	2.356800
-83.022251	11.126103	2.366797
-82.895868	12.754415	2.376794
-82.694512	8.663026	2.386790
-82.145281	11.582484	2.396787
-81.069495	19.838293	2.406784
-81.000748	9.565241	2.416781
-80.794044	6.657893	2.426778
-79.669112	8.166084	2.436774
-79.563938	4.321801	2.446771
-79.157768	8.099753	2.456768
-78.337088	11.732791	2.466765
-78.085351	7.341224	2.476762
-77.674458	-0.830839	2.486758
-76.718267	10.049355	2.496755
-76.601472	6.525608	2.506752
-76.029747	9.644854	2.516749
-75.542074	8.870749	2.526746
-74.989344	13.085401	2.536742
-74.479088	9.632235	2.546739
-73.177907	14.182130	2.556736
-73.371295	15.020099	2.566733
-73.618506	11.616106	2.576730
-72.761198	14.053610	2.586726
-72.066714	13.503897	2.596723
-70.803906	8.196235	2.606720
-70.942109	12.811612	2.616717
-70.446844	18.004154	2.626714
-70.321075	18.176356	2.636710
-69.259431	12.600292	2.646707
-68.635182	19.728371	2.656704
-68.514211	15.488469	2.666701
-68.128835	17.199754	2.676698
-67.394155	13.880335	2.686694
-67.208608	10.399143	2.696691
-66.107911	7.627084	2.706688
-65.623529	7.720139	2.716685
-65.808920	11.155837	2.726682
-65.093266	8.506029	2.736678
-64.202336	10.807164	2.746675
-64.073789	8.538713	2.756672
-63.507307	6.220461	2.766669
-62.503027	10.948945	2.776666
-62.543446	9.699570	2.786662
-62.125958	4.875700	2.796659
-61.162115	8.135305	2.806656
-61.047087	7.146094	2.816653
-60.601488	14.479807	2.826650
-59.682271	8.534136	2.836646
-59.322952	9.096819	2.846643
-59.182626	10.277068	2.856640
-58.039646	3.705930	2.866637
-57.620104	12.113690	2.876634
-57.677229	6.559696	2.886630
-57.081756	7.089397	2.896627
-56.098065	6.413549	2.906624
-55.892709	10.396462	2.916621
-55.828340	8.049330	2.926618
-54.866650	8.542886	2.936614
-54.379503	11.218533	2.946611
-53.778836	12.701717	2.956608
-53.100868	15.522605	2.966605
-52.993645	3.634433	2.976602
-52.808972	9.985881	2.986598
-51.916484	8.743838	2.996595
-51.450485	10.977034	3.006592
-50.702854	12.956325	3.016589
-50.221079	10.983058	3.026586
-49.974326	10.843193	3.036582
-49.531869	9.694446	3.046579
-48.835847	5.357540	3.056576
-48.296386	11.559346	3.066573
-48.246885	12.053402	3.076570
-47.436458	11.276236	3.086566
-46.908259	8.775630	3.096563
-45.994631	9.327136	3.106560
-45.573892	10.523979	3.116557
-45.522354	9.534613	3.126554
-45.175063	13.959736	3.136550
-44.180735	11.839549	3.146547
-43.525568	5.080083	3.156544
-43.176271	3.591899	3.166541
-43.358436	6.584467	3.176538
-42.658068	2.744563	3.186534
-42.115632	6.709593	3.196531
-41.024856	2.403542	3.206528
-40.720612	9.789116	3.216525
-40.716917	9.730995	3.226522
-39.918041	6.978298	3.236518
-39.170383	8.992361	3.246515
-38.953401	7.237809	3.256512
-38.225048	9.530110	3.266509
-37.758348	3.555252	3.276506
-37.315378	11.444225	3.286502
-37.167453	12.024727	3.296499
-36.180139	6.672596	3.306496
-35.986774	6.766030	3.316493
-35.288121	7.170766	3.326490
-34.465305	8.848539	3.336486
-34.270592	7.863126	3.346483
-34.225501	7.521331	3.356480
-33.209588	4.332384	3.366477
-32.715308	11.023391	3.376474
-32.596068	5.120297	3.386470
-31.473225	8.033885	3.396467
-31.153371	9.086008	3.406464
-30.908997	7.468986	3.416461
-30.669186	11.485516	3.426458
-29.628640	5.107198	3.436454
-29.200453	2.766209	3.446451
-29.147109	7.692481	3.456448
-27.895762	4.699281	3.466445
-27.647625	6.354459	3.476442
-27.430006	4.776248	3.486438
-27.199792	8.932084	3.496435
-26.354486	10.694654	3.506432
-25.990072	14.372437	3.516429
-24.718796	18.364378	3.526426
-24.782164	12.324560	3.536422
-24.648686	11.914582	3.546419
-23.892946	6.908047	3.556416
-23.476936	8.628490	3.566413
-23.083945	12.567097	3.576410
-21.923807	10.142640	3.586406
-21.334361	7.184953	3.596403
-21.422426	12.144721	3.606400
-21.368008	4.081082	3.616397
-20.123484	4.466756	3.626394
-19.991645	10.229455	3.636390
-19.414817	10.227580	3.646387
-18.384560	10.895126	3.656384
-18.145633	10.673572	3.666381
-17.971679	7.866095	3.676378
-17.362333	4.558152	3.686374
-16.751369	3.284688	3.696371
-16.700322	6.093609	3.706368
-15.520198	4.357199	3.716365
-15.132882	1.389517	3.726362
-15.103678	10.875145	3.736358
-14.185132	8.557480	3.746355
-13.465417	7.286556	3.756352
-13.337526	1.906227	3.766349
-13.105078	14.874452	3.776346
-12.231100	13.810740	3.786342
-11.987516	6.546232	3.796339
-11.201159	7.432983	3.806336
-10.454229	8.500140	3.816333
-10.289337	4.862917	3.826330
-10.146577	8.980877	3.836326
-9.216538	8.984532	3.846323
-8.723504	8.862373	3.856320
-8.337277	10.130139	3.866317
-7.288316	14.423664	3.876314
-7.013937	9.669333	3.886310
-6.994528	9.980862	3.896307
-6.712046	12.483929	3.906304
-5.472275	7.743417	3.916301
-5.240312	16.979908	3.926298
-5.192751	14.188024	3.936294
-4.248498	10.629211	3.946291
-3.945839	9.790119	3.956288
-2.951615	20.839702	3.966285
-2.796442	22.812387	3.976282
-2.575707	28.090316	3.986278
-2.339587	36.959014	3.996275
-1.915775	55.599923	4.006272
-1.250780	74.226604	4.016269
-0.689532	98.568125	4.026266
-0.685427	112.940367	4.036262
0.000000	130.790365	4.041267
-0.024661	157.330265	4.046272
0.439413	150.710056	4.051277
0.317084	164.348747	4.056282
0.641096	171.798295	4.061286
1.152808	190.235622	4.066291
1.021549	188.936481	4.071296
1.045645	190.059768	4.076301
0.886628	197.234304	4.081306
0.820746	191.395667	4.086310
1.139900	189.094265	4.091315
0.703780	194.878078	4.096320
1.180650	193.981445	4.101325
0.927922	188.333591	4.106330
1.108850	191.401706	4.111334
1.107794	185.534773	4.116339
0.608337	194.368248	4.121344
1.084038	191.882462	4.126349
1.201585	193.748442	4.131354
1.128616	191.289770	4.136358
1.094019	190.984984	4.141363
1.249289	195.025875	4.146368
1.162139	190.065552	4.151373
0.936308	198.838328	4.156378
0.836567	197.442403	4.161382
1.131002	202.688867	4.166387
1.144635	201.913341	4.171392
1.278993	195.099659	4.176397
1.395997	204.025436	4.181402
1.116988	197.575812	4.186406
1.016704	193.644008	4.191411
0.973692	196.173379	4.196416
1.313750	199.142525	4.201421
1.252274	216.852891	4.206426
1.178204	218.141622	4.211430
1.279367	207.088919	4.216435
1.229547	222.652512	4.221440
1.583020	206.895359	4.226445
1.435204	224.125506	4.231450
1.262594	216.871473	4.236454
1.299535	212.605545	4.241459
1.426347	217.065560	4.246464
1.669506	211.725127	4.251469
1.484672	217.873259	4.256474
1.314967	213.573468	4.261478
1.247402	218.600255	4.266483
1.372481	216.249880	4.271488
1.411619	219.851397	4.276493
1.348602	217.187422	4.281498
1.300078	221.031379	4.286502
1.608049	219.522355	4.291507
1.389009	213.687363	4.296512
1.539300	212.320287	4.301517
1.386968	214.162284	4.306522
1.251400	220.031119	4.311526
1.525528	212.226545	4.316531
1.329901	218.095852	4.321536
1.607559	220.136606	4.326541
1.351232	226.498258	4.331546
1.676920	231.411188	4.336550
1.706599	224.394796	4.341555
1.371412	234.134692	4.346560
1.721603	234.867131	4.351565
1.548297	249.776110	4.356570
1.634202	251.446249	4.361574
1.603230	238.931232	4.366579
1.450590	246.518156	4.371584
1.957061	242.675509	4.376589
1.732933	259.582266	4.381594
1.883658	254.197923	4.386598
1.834177	251.176297	4.391603
1.822608	252.601302	4.396608
1.715079	244.454186	4.401613
1.536202	256.610258	4.406618
1.636928	249.417708	4.411622
1.816653	247.591484	4.416627
1.793506	260.963022	4.421632
1.955760	251.226079	4.426637
1.870560	256.744011	4.431642
2.047352	253.125268	4.436646
1.901750	252.765847	4.441651
1.885369	263.083463	4.446656
1.976459	253.538669	4.451661
1.963707	252.120047	4.456666
1.773124	250.506697	4.461670
2.061401	253.090741	4.466675
1.746960	260.022467	4.471680
2.045739	249.413184	4.476685
1.739161	255.146955	4.481690
1.901969	248.088576	4.486694
2.124187	260.403593	4.491699
1.982944	251.041723	4.496704
1.948101	253.186719	4.501709
1.862684	250.397981	4.506714
1.723496	261.272292	4.511718
1.949097	247.670869	4.516723
1.979768	270.977711	4.521728
1.823535	271.373089	4.526733
2.047867	272.488879	4.531738
2.185125	276.795233	4.536742
2.537790	276.660361	4.541747
2.078257	273.773133	4.546752
2.496887	285.798516	4.551757
2.135430	276.167420	4.556762
2.238698	272.639782	4.561766
2.182791	265.600641	4.566771
2.246819	262.515421	4.571776
2.077756	269.396043	4.576781
2.048643	277.412654	4.581786
2.063555	282.056783	4.586790
2.162183	275.325549	4.591795
1.801475	283.270380	4.596800
2.160031	284.283826	4.601805
2.170163	279.217380	4.606810
2.344792	280.156298	4.611814
1.963937	280.564008	4.616819
1.972940	290.003628	4.621824
2.303188	282.251690	4.626829
2.446400	279.775363	4.631834
2.162927	284.885284	4.636838
2.306812	282.667751	4.641843
2.301537	312.140298	4.646848
2.421743	310.778589	4.651853
2.503749	320.755528	4.656858
2.444099	320.666040	4.661862
2.812220	311.826405	4.666867
2.477164	307.290325	4.671872
2.706385	292.684997	4.676877
2.308727	286.565986	4.681882
2.266008	289.928876	4.686886
2.456569	291.837440	4.691891
2.496712	312.467274	4.696896
2.661466	315.094871	4.701901
2.707348	311.357879	4.706906
2.380728	318.349665	4.711910
2.787789	317.358812	4.716915
2.803066	317.291648	4.721920
2.457700	299.270425	4.726925
2.575581	304.789674	4.731930
2.556473	307.402722	4.736934
2.946370	307.311415	4.741939
2.674295	303.465653	4.746944
2.624134	295.396036	4.751949
2.478745	296.633040	4.756954
2.421347	311.042368	4.761958
2.840234	310.525536	4.766963
2.911777	325.801546	4.771968
2.635709	312.973425	4.776973
2.447143	317.098318	4.781978
2.344273	315.163971	4.786982
2.696367	315.894125	4.791987
2.409060	324.573352	4.796992
2.520725	315.200547	4.801997
2.733326	324.656796	4.807002
2.450519	329.235782	4.812006
2.562139	318.173375	4.817011
2.731548	337.576300	4.822016
3.004717	343.863149	4.827021
3.187719	334.036087	4.832026
3.006403	339.489449	4.837030
3.152085	313.761754	4.842035
3.141251	319.031377	4.847040
2.741614	322.306162	4.852045
3.059562	312.562936	4.857050
2.872498	319.688497	4.862054
3.311495	317.811440	4.867059
2.870665	323.206338	4.872064
3.296574	314.769963	4.877069
2.942279	320.512843	4.882074
2.925618	317.658637	4.887078
2.887267	313.444616	4.892083
3.101199	322.804540	4.897088
3.054262	324.243302	4.902093
2.949407	319.719026	4.907098
2.590539	324.233644	4.912102
2.850683	323.547338	4.917107
2.959662	333.757808	4.922112
3.194350	337.737632	4.927117
3.053691	345.880298	4.932122
3.371532	345.733827	4.937126
3.393652	339.616523	4.942131
3.086999	342.582473	4.947136
3.206140	330.519491	4.952141
3.220249	333.981122	4.957146
3.082887	336.488250	4.962150
3.224925	340.430135	4.967155
3.126377	350.819235	4.972160
3.380421	346.581061	4.977165
3.367792	346.255269	4.982170
3.105399	347.249783	4.987174
3.271961	343.141934	4.992179
3.106481	350.829111	4.997184
3.175897	340.060409	5.002189
3.635237	343.665192	5.007194
3.336479	347.300983	5.012198
3.593763	345.831915	5.017203
3.314108	343.233983	5.022208
3.334771	334.527254	5.027213
3.586941	338.886822	5.032218
2.974953	344.848605	5.037222
3.511248	351.159572	5.042227
3.388928	347.188951	5.047232
3.565138	351.650890	5.052237
3.656737	353.332530	5.057242
3.381179	342.446897	5.062246
3.475026	338.482319	5.067251
3.494459	342.194677	5.072256
3.446082	349.813326	5.077261
3.568959	341.365151	5.082266
3.453736	345.192951	5.087270
3.494068	340.908468	5.092275
3.384350	356.705896	5.097280
3.677217	348.821189	5.102285
3.544013	346.627625	5.107290
3.417027	345.408278	5.112294
3.577361	346.097961	5.117299
3.486480	350.466977	5.122304
3.752872	343.194656	5.127309
3.676383	341.909522	5.132314
3.420800	344.260793	5.137318
3.674665	342.854255	5.142323
3.536996	348.545487	5.147328
3.509490	344.371103	5.152333
3.590741	347.977320	5.157338
3.713950	348.143298	5.162342
3.549503	350.426987	5.167347
3.807462	349.854314	5.172352
3.621129	344.995615	5.177357
3.663709	344.981947	5.182362
3.419764	345.852242	5.187366
3.852344	345.542517	5.192371
3.346545	348.780224	5.197376
3.510106	343.620072	5.202381
3.759515	357.921017	5.207386
3.747866	370.503759	5.212390
3.782963	374.951182	5.217395
3.774774	382.930440	5.222400
3.960403	379.679031	5.227405
4.099775	379.826151	5.232410
3.895183	383.120946	5.237414
3.924542	383.308386	5.242419
4.067658	379.220985	5.247424
3.692680	364.640847	5.252429
3.724673	370.272419	5.257434
3.692819	374.286719	5.262438
3.702664	372.693843	5.267443
3.643602	382.267338	5.272448
3.989247	375.661316	5.277453
3.928838	379.118720	5.282458
3.422069	379.186743	5.287462
3.707275	383.549734	5.292467
3.762968	385.418875	5.297472
4.141609	389.270286	5.302477
4.309099	382.317239	5.307482
3.918026	380.449551	5.312486
3.924393	375.169979	5.317491
4.229139	399.027198	5.322496
4.209434	401.904993	5.327501
4.283324	392.675152	5.332506
3.996511	384.448520	5.337510
4.139407	377.975134	5.342515
4.357515	401.640485	5.347520
3.820450	386.996587	5.352525
4.039484	391.346462	5.357530
4.315241	400.911295	5.362534
4.643143	396.401179	5.367539
4.246279	394.349344	5.372544
4.040832	380.389180	5.377549
4.518136	384.606300	5.382554
4.458580	384.852666	5.387558
4.274230	378.268098	5.392563
4.115845	380.322665	5.397568
4.323363	372.214089	5.402573
4.106956	384.454226	5.407578
4.453661	399.432941	5.412582
4.591492	391.039097	5.417587
3.995707	384.440563	5.422592
4.099083	391.946486	5.427597
4.133148	392.040002	5.432602
4.018003	404.545187	5.437606
4.254934	400.650044	5.442611
4.227944	405.289506	5.447616
4.599053	397.045884	5.452621
4.650433	409.608355	5.457626
4.819668	405.928666	5.462630
4.898084	403.755505	5.467635
4.674221	408.261210	5.472640
4.654886	400.022841	5.477645
4.591110	397.707658	5.482650
4.316121	392.675757	5.487654
4.750576	393.206977	5.492659
4.561147	399.435469	5.497664
4.803428	393.033830	5.502669
4.544134	388.370329	5.507674
4.526830	384.252263	5.512678
4.604585	375.883175	5.517683
4.208795	383.079243	5.522688
4.344598	397.428835	5.527693
4.650488	401.001221	5.532698
4.489219	401.187468	5.537702
4.686772	405.779486	5.542707
4.474573	410.844099	5.547712
4.571584	406.883518	5.552717
4.763581	400.382851	5.557722
4.464282	409.954504	5.562726
5.135405	405.502009	5.567731
4.751047	410.888769	5.572736
4.910605	407.798555	5.577741
5.113106	414.170347	5.582746
4.765816	412.490574	5.587750
4.812069	410.430879	5.592755
4.766546	415.163399	5.597760
4.859573	407.005090	5.602765
5.085752	403.888847	5.607770
4.868418	417.852723	5.612774
5.173535	402.287300	5.617779
4.918612	384.762306	5.622784
4.358012	383.705137	5.627789
4.831546	393.955924	5.632794
4.520076	407.574249	5.637798
4.930224	405.433577	5.642803
4.866046	402.926844	5.647808
4.950952	409.151355	5.652813
5.000063	407.719317	5.657818
4.660717	415.913864	5.662822
5.048275	406.578596	5.667827
5.025211	411.027964	5.672832
4.708052	403.518939	5.677837
5.019600	418.191304	5.682842
4.943905	404.187136	5.687846
4.993833	409.673274	5.692851
4.695793	421.973333	5.697856
4.560129	410.072266	5.702861
4.689503	411.772917	5.707866
4.886513	421.986629	5.712870
5.378163	433.737575	5.717875
5.104956	434.960827	5.722880
5.127024	431.160457	5.727885
5.068422	436.358699	5.732890
4.757755	444.122457	5.737894
5.284941	439.933159	5.742899
5.082388	450.373490	5.747904
5.128165	445.515792	5.752909
5.314549	451.838762	5.757914
5.139614	445.382062	5.762918
5.370943	443.259155	5.767923
5.187606	458.328459	5.772928
5.030917	444.217881	5.777933
4.943620	444.594152	5.782938
4.898888	441.732534	5.787942
5.347666	437.676597	5.792947
4.981877	449.472841	5.797952
4.981251	454.308646	5.802957
4.854447	441.457082	5.807962
4.757197	450.358292	5.812966
5.584383	462.456864	5.817971
5.542678	465.403040	5.822976
5.514996	461.175570	5.827981
5.509790	453.120134	5.832986
5.408507	448.779938	5.837990
5.406451	435.312152	5.842995
5.157310	451.088164	5.848000
5.263675	455.666880	5.853005
5.730303	468.868101	5.858010
5.425727	466.280590	5.863014
5.385657	462.111610	5.868019
5.582711	467.621162	5.873024
5.497074	465.322613	5.878029
5.388582	469.825020	5.883034
5.523026	465.923940	5.888038
5.906707	462.945003	5.893043
5.706379	452.259962	5.898048
5.684528	445.436515	5.903053
5.955136	439.137322	5.908058
5.232000	436.610442	5.913062
5.534732	437.613804	5.918067
5.477807	434.192183	5.923072
5.751768	436.567476	5.928077
5.668866	436.521108	5.933082
5.449757	443.577635	5.938086
5.476363	437.861135	5.943091
5.529512	457.338520	5.948096
5.910808	457.813817	5.953101
6.178176	457.384036	5.958106
5.444898	446.073670	5.963110
5.710019	445.529014	5.968115
5.692787	455.055369	5.973120
5.591253	453.332332	5.978125
5.954776	456.268832	5.983130
5.702715	464.951970	5.988134
5.811645	455.568679	5.993139
5.702516	467.113848	5.998144
5.931258	471.471216	6.003149
6.224877	461.654174	6.008154
5.407975	454.859757	6.013158
5.922212	458.619861	6.018163
5.878912	461.423032	6.023168
5.741394	465.922942	6.028173
5.943382	464.277915	6.033178
5.861536	469.508829	6.038182
5.888160	455.768289	6.043187
5.823622	467.400403	6.048192
6.180040	465.108972	6.053197
5.904106	459.585435	6.058202
5.815382	463.402956	6.063206
6.007772	466.704851	6.068211
5.868029	469.938013	6.073216
5.921335	471.265664	6.078221
5.961859	471.328313	6.083226
5.989553	477.397743	6.088230
5.904565	448.366070	6.093235
5.562261	450.325394	6.098240
5.880760	463.424053	6.103245
6.118037	466.364488	6.108250
6.157319	473.587620	6.113254
5.715532	450.035556	6.118259
5.520332	459.568493	6.123264
5.863603	466.320951	6.128269
6.232481	464.341227	6.133274
5.881747	467.397778	6.138278
6.078801	461.072866	6.143283
6.228791	465.284217	6.148288
5.661847	448.563668	6.153293
5.855321	441.105840	6.158298
5.812554	460.854863	6.163302
6.357071	451.682629	6.168307
5.846682	450.187928	6.173312
5.615701	439.887850	6.178317
5.806999	447.081851	6.183322
5.305783	459.838482	6.188326
6.234266	464.956957	6.193331
6.195269	474.035612	6.198336
6.038673	467.299590	6.203341
5.858278	450.562195	6.208346
5.692084	467.964183	6.213350
5.778199	452.047202	6.218355
6.102475	469.986044	6.223360
5.720212	464.199298	6.228365
5.924688	460.703799	6.233370
6.050475	477.276577	6.238374
6.083419	467.553609	6.243379
5.930466	469.691157	6.248384
5.665509	464.489043	6.253389
5.821513	453.990488	6.258394
5.865200	476.290828	6.263398
5.887308	462.515508	6.268403
5.922087	474.961587	6.273408
6.104773	469.616279	6.278413
6.022836	469.067718	6.283418
5.791686	468.458615	6.288422
5.798058	466.051094	6.293427
6.127540	478.981984	6.298432
5.979509	461.666538	6.303437
6.156290	451.833920	6.308442
5.680899	450.729879	6.313446
5.691348	449.341339	6.318451
6.177196	463.329718	6.323456
5.762304	452.923526	6.328461
6.007623	449.757139	6.333466
5.888655	449.980783	6.338470
5.649431	443.374291	6.343475
5.687882	457.452338	6.348480
5.734650	463.888222	6.353485
6.141825	465.935584	6.358490
5.910843	476.588044	6.363494
6.300792	468.751139	6.368499
6.030470	455.044180	6.373504
5.821038	452.235684	6.378509
5.974310	449.555390	6.383514
5.657425	444.667758	6.388518
5.790896	452.476577	6.393523
5.929166	465.809328	6.398528
5.865940	468.576726	6.403533
5.922497	464.818393	6.408538
6.073303	468.434038	6.413542
6.250494	465.976920	6.418547
5.875580	448.733394	6.423552
5.753301	441.659775	6.428557
5.981693	430.234778	6.433562
5.756653	441.799517	6.438566
5.662362	441.736485	6.443571
6.113828	451.683312	6.448576
6.258232	462.280707	6.453581
6.043318	444.747244	6.458586
5.486891	443.918688	6.463590
5.766113	449.197160	6.468595
5.918237	463.288950	6.473600
5.818264	467.997547	6.478605
5.929730	462.448934	6.483610
5.890723	472.822336	6.488614
5.940569	470.115750	6.493619
5.983913	473.262748	6.498624
5.855095	468.259505	6.503629
5.852804	464.744172	6.508634
6.042299	467.954193	6.513638
6.136705	460.904873	6.518643
5.655925	451.173641	6.523648
5.598729	462.717114	6.528653
6.276260	462.956281	6.533658
5.853522	461.558166	6.538662
5.767374	458.594274	6.543667
5.618129	461.031163	6.548672
5.504576	462.486297	6.553677
5.773647	465.712543	6.558682
5.705900	472.452549	6.563686
5.934781	465.564881	6.568691
5.924310	465.486982	6.573696
5.578254	468.493029	6.578701
5.708646	471.531284	6.583706
5.763007	475.897991	6.588710
5.839361	474.131090	6.593715
5.925664	470.562407	6.598720
5.602342	470.630049	6.603725
6.016685	466.934427	6.608730
5.611681	470.493905	6.613734
5.988930	469.104617	6.618739
6.027684	470.090518	6.623744
5.853094	476.223439	6.628749
6.166393	461.537132	6.633754
6.375725	468.116601	6.638758
6.103767	463.926026	6.643763
5.943801	466.613537	6.648768
6.175458	468.314228	6.653773
6.163218	462.120867	6.658778
6.065907	469.992576	6.663782
6.245921	461.178874	6.668787
6.267187	466.751872	6.673792
6.191884	456.631435	6.678797
5.937939	443.860322	6.683802
5.645297	439.025314	6.688806
6.173787	435.423280	6.693811
6.215191	443.909414	6.698816
5.948689	438.648560	6.703821
5.882379	436.812931	6.708826
5.770716	444.360605	6.713830
5.965521	442.883916	6.718835
6.083187	439.934626	6.723840
5.599864	445.251943	6.728845
5.852678	434.886953	6.733850
5.692334	438.308032	6.738854
5.680549	436.862000	6.743859
5.654405	445.178556	6.748864
5.845807	460.531154	6.753869
6.104815	464.131446	6.758874
6.060399	474.704269	6.763878
6.041245	458.355172	6.768883
6.070541	449.202540	6.773888
5.717525	454.276275	6.778893
6.152028	441.147254	6.783898
5.613089	448.845406	6.788902
6.075416	443.615028	6.793907
5.438434	447.771188	6.798912
5.702962	462.199181	6.803917
6.010563	460.304002	6.808922
6.056667	470.784278	6.813926
6.124622	461.110970	6.818931
6.299252	457.257506	6.823936
5.757982	455.372449	6.828941
5.595780	444.336546	6.833946
5.500007	457.555303	6.838950
5.985031	460.317563	6.843955
5.786222	465.401880	6.848960
5.943175	467.060871	6.853965
5.927494	471.197631	6.858970
5.964197	476.730976	6.863974
6.116619	472.140175	6.868979
6.319997	466.948523	6.873984
5.851467	459.926508	6.878989
5.753460	447.102535	6.883994
5.562392	447.336736	6.888998
5.840516	453.959274	6.894003
5.974715	470.422114	6.899008
5.888919	463.405987	6.904013
6.087427	459.995346	6.909018
5.894187	479.193670	6.914022
6.026525	473.366307	6.919027
6.064315	462.698467	6.924032
5.972183	457.285790	6.929037
5.668225	445.127014	6.934042
5.696005	449.784653	6.939046
6.017422	455.103895	6.944051
6.240776	472.584061	6.949056
5.892564	466.380617	6.954061
6.392618	436.136134	6.959066
5.782275	441.350356	6.964070
5.745006	434.375936	6.969075
5.651911	436.821087	6.974080
5.135463	439.071905	6.979085
5.858670	458.863210	6.984090
5.539257	465.640939	6.989094
5.874673	462.384443	6.994099
5.819642	472.566711	6.999104
6.089515	480.015309	7.004109
5.929959	461.611665	7.009114
5.903777	467.265535	7.014118
6.128949	472.395093	7.019123
6.406020	468.298709	7.024128
6.062431	476.841704	7.029133
6.366140	468.530861	7.034138
6.025960	451.596338	7.039142
6.070516	441.073226	7.044147
5.864639	440.235564	7.049152
5.799759	440.550697	7.054157
6.264742	426.979928	7.059162
5.920317	437.109844	7.064166
5.854444	433.972493	7.069171
6.141133	432.255228	7.074176
5.829893	438.805046	7.079181
6.218251	435.139191	7.084186
5.879619	444.647520	7.089190
6.016628	436.861198	7.094195
5.800646	440.298002	7.099200
5.458262	448.936689	7.104205
5.828002	436.853243	7.109210
5.665186	440.501869	7.114214
5.788897	443.426571	7.119219
5.943811	433.781308	7.124224
5.727440	436.688517	7.129229
5.865582	436.779995	7.134234
6.021121	442.820151	7.139238
6.120138	431.662461	7.144243
6.112737	441.967658	7.149248
6.045920	445.218931	7.154253
6.261578	428.938139	7.159258
6.105811	439.657449	7.164262
5.671468	442.091222	7.169267
6.372781	445.798046	7.174272
5.909735	443.261250	7.179277
6.151718	441.790957	7.184282
5.961726	451.269942	7.189286
5.810382	438.335022	7.194291
6.113059	435.424364	7.199296
5.781423	444.889305	7.204301
6.223965	441.488975	7.209306
5.703608	439.904754	7.214310
5.800888	438.737263	7.219315
5.917723	441.365120	7.224320
6.071472	450.597147	7.229325
6.349042	436.468147	7.234330
5.919686	443.019568	7.239334
5.882544	430.735317	7.244339
6.024351	431.352097	7.249344
5.897132	428.564723	7.254349
6.075816	415.528010	7.259354
5.787903	411.842912	7.264358
5.696035	418.185303	7.269363
5.954571	425.218972	7.274368
5.949717	431.024603	7.279373
6.153198	426.317613	7.284378
5.937273	421.192843	7.289382
5.616149	412.811244	7.294387
5.920030	421.189964	7.299392
5.920895	423.128771	7.304397
5.738513	424.755143	7.309402
5.733866	435.045868	7.314406
5.655144	435.224170	7.319411
6.138531	443.664743	7.324416
5.907512	441.417899	7.329421
6.076736	437.756360	7.334426
6.211060	445.553391	7.339430
6.079577	428.435344	7.344435
5.726525	418.051694	7.349440
5.530988	416.420794	7.354445
5.923232	426.056341	7.359450
5.990400	443.484190	7.364454
5.999957	434.812001	7.369459
6.077608	447.711945	7.374464
5.776020	435.799260	7.379469
6.035952	422.165950	7.384474
5.653490	428.836686	7.389478
6.127568	432.189218	7.394483
6.058318	431.610734	7.399488
5.760556	423.975939	7.404493
5.856605	408.519723	7.409498
5.701920	415.361915	7.414502
5.881934	426.859176	7.419507
6.068410	445.837698	7.424512
6.001246	444.976277	7.429517
6.132191	424.466324	7.434522
5.739859	425.459074	7.439526
5.901973	408.581534	7.444531
5.985505	411.451708	7.449536
5.900298	407.062882	7.454541
5.741443	399.910483	7.459546
5.986879	422.634375	7.464550
5.602957	413.605246	7.469555
5.910736	421.993977	7.474560
5.974479	441.573586	7.479565
6.049086	438.134328	7.484570
5.745813	443.648179	7.489574
5.810893	438.970615	7.494579
6.165527	442.899228	7.499584
5.919403	436.671195	7.504589
6.018472	431.513996	7.509594
5.746327	423.768593	7.514598
5.907571	436.357492	7.519603
6.113123	437.947257	7.524608
5.961806	415.056583	7.529613
5.867746	411.925088	7.534618
5.892295	419.240818	7.539622
5.944482	416.505831	7.544627
5.872157	414.349144	7.549632
5.840273	413.609364	7.554637
5.909576	410.210853	7.559642
5.859127	418.088393	7.564646
5.870674	413.117575	7.569651
5.716803	430.561093	7.574656
5.759858	428.867990	7.579661
5.945410	433.892993	7.584666
6.006065	437.200909	7.589670
5.987644	434.774015	7.594675
6.233046	433.561869	7.599680
5.984079	427.801610	7.604685
5.836868	411.163945	7.609690
5.527272	419.061900	7.614694
5.371918	430.435907	7.619699
5.591112	436.145042	7.624704
5.843230	451.143416	7.629709
6.046456	448.742178	7.634714
6.124577	445.416004	7.639718
5.970075	446.062708	7.644723
6.135934	444.942668	7.649728
5.954900	453.481821	7.654733
6.327009	446.128404	7.659738
6.048972	437.394116	7.664742
5.719209	421.312380	7.669747
5.920664	419.833803	7.674752
5.781982	426.417401	7.679757
6.324499	423.153459	7.684762
5.768032	428.783035	7.689766
5.792401	411.101845	7.694771
6.037543	415.878787	7.699776
5.756534	418.846425	7.704781
5.953780	417.827555	7.709786
5.569420	421.136733	7.714790
5.980343	429.658564	7.719795
6.146962	442.099363	7.724800
6.177803	429.326098	7.729805
6.117417	413.877427	7.734810
5.936252	416.058712	7.739814
5.946862	411.547653	7.744819
5.871208	408.997826	7.749824
5.742841	404.110367	7.754829
6.098400	399.920885	7.759834
5.744656	409.777631	7.764838
5.692997	404.774854	7.769843
5.799785	403.275643	7.774848
5.440141	418.553287	7.779853
5.764564	414.518342	7.784858
6.045606	432.712751	7.789862
6.020877	436.966641	7.794867
5.726701	437.332768	7.799872
5.535051	444.686678	7.804877
6.182157	448.321569	7.809882
5.815206	446.042768	7.814886
5.992557	441.103490	7.819891
5.952307	443.283547	7.824896
5.675831	441.461603	7.829901
6.135142	442.880881	7.834906
5.743945	445.192461	7.839910
6.009324	442.976889	7.844915
5.991834	443.779301	7.849920
5.927350	444.614556	7.854925
6.014126	438.411123	7.859930
5.836742	441.101118	7.864934
6.003546	440.307519	7.869939
5.937076	444.311979	7.874944
5.656151	443.634749	7.879949
6.064903	442.491263	7.884954
5.787427	445.383332	7.889958
5.615268	441.756021	7.894963
6.056017	439.952070	7.899968
5.704723	447.216381	7.904973
5.802998	441.343165	7.909978
6.133319	449.003745	7.914982
5.875994	442.954183	7.919987
6.205133	440.252071	7.924992
5.693728	447.014222	7.929997
6.366564	442.051508	7.935002
6.125468	441.479376	7.940006
5.871839	435.426640	7.945011
6.200569	419.110360	7.950016
6.085137	416.694797	7.955021
5.623172	404.045386	7.960026
5.638667	403.807487	7.965030
5.833887	429.368559	7.970035
5.720963	431.629125	7.975040
5.796379	443.756852	7.980045
5.984469	442.058084	7.985050
5.775060	436.817180	7.990054
5.668322	438.661126	7.995059
5.937372	435.841682	8.000064
5.962200	444.174267	8.005069
6.117524	445.100606	8.010074
5.497783	445.524983	8.015078
5.918958	449.229256	8.020083
5.982278	432.504609	8.025088
5.766678	441.121310	8.030093
6.348143	437.540500	8.035098
6.309421	445.561354	8.040102
5.831706	435.049348	8.045120
5.963814	440.086447	8.050138
5.838363	445.650413	8.055155
6.070907	442.877947	8.060173
6.058427	445.730292	8.065190
5.872477	432.730437	8.070208
5.810312	427.272133	8.075226
5.694526	444.833616	8.080243
5.910068	432.727445	8.085261
6.063013	438.894277	8.090278
5.687966	448.715998	8.095296
6.192120	447.414982	8.100314
5.947356	439.617593	8.105331
6.043224	441.178468	8.110349
5.643990	442.502452	8.115366
5.818475	437.727346	8.120384
5.990288	440.828484	8.125402
5.820904	442.929702	8.130419
5.898534	440.378150	8.135437
5.957981	442.565089	8.140454
6.062494	440.596444	8.145472
5.884464	439.365872	8.150490
6.056496	449.315099	8.155507
6.125751	439.193240	8.160525
6.051793	447.138269	8.165542
5.924717	440.807702	8.170560
5.859201	425.751839	8.175578
5.765151	446.112666	8.180595
6.303146	435.332722	8.185613
6.324557	438.360544	8.190630
6.117325	436.388209	8.195648
6.174399	430.206471	8.200666
5.952787	429.126807	8.205683
6.124825	437.631841	8.210701
5.903637	437.504202	8.215718
5.922804	437.709767	8.220736
6.268179	435.307567	8.225754
5.846525	444.439023	8.230771
5.929970	431.800829	8.235789
5.846203	438.973520	8.240806
5.827727	444.849078	8.245824
6.142491	430.761071	8.250842
6.128665	439.639770	8.255859
5.871410	435.136535	8.260877
5.797084	451.774888	8.265894
6.060216	461.200216	8.270912
6.486919	470.689796	8.275930
6.038113	481.558520	8.280947
6.169259	470.983707	8.285965
6.306000	472.190795	8.290982
6.046790	467.777040	8.296000
6.449913	461.946817	8.301018
6.228247	456.959764	8.306035
6.466687	449.881513	8.311053
5.835361	452.228503	8.316070
5.967091	450.180158	8.321088
6.366588	451.917119	8.326106
6.411123	453.886663	8.331123
6.106668	442.572444	8.336141
5.965571	441.214900	8.341158
5.778664	455.189221	8.346176
6.110514	460.358791	8.351194
6.068281	464.899804	8.356211
6.126189	466.707305	8.361229
6.476929	471.331466	8.366246
6.320114	474.806297	8.371264
6.616279	474.063894	8.376282
6.024891	472.370309	8.381299
6.295679	469.399393	8.386317
6.443816	465.623452	8.391334
5.994843	467.811125	8.396352
6.304202	469.092180	8.401370
6.008039	470.099514	8.406387
6.119129	466.940491	8.411405
6.301424	468.198889	8.416422
6.253208	479.892751	8.421440
6.552150	458.672017	8.426458
6.143916	468.845481	8.431475
6.078488	469.608126	8.436493
6.315853	462.561935	8.441510
6.082090	475.743894	8.446528
6.568934	462.068278	8.451546
6.120514	470.118039	8.456563
6.143128	470.045691	8.461581
6.285845	452.946015	8.466598
6.213443	465.552074	8.471616
6.355189	466.193215	8.476634
6.395030	471.287922	8.481651
6.122268	475.124250	8.486669
6.004836	471.728874	8.491686
6.031752	477.263881	8.496704
6.300826	488.215889	8.501722
6.512678	496.375803	8.506739
6.677537	491.032629	8.511757
6.731923	480.947848	8.516774
6.408555	473.563431	8.521792
6.327935	467.513525	8.526810
6.163231	474.645111	8.531827
6.209224	493.707114	8.536845
6.591712	495.852379	8.541862
6.843830	500.274195	8.546880
6.742326	478.328065	8.551898
6.201690	478.700731	8.556915
6.641647	473.532468	8.561933
6.758975	462.995772	8.566951
6.604301	464.981770	8.571968
6.769787	464.750145	8.576986
6.723213	467.253638	8.582003
6.362036	468.820320	8.587021
6.813745	467.861033	8.592039
6.545294	474.895632	8.597056
6.814028	473.602890	8.602074
6.694148	473.916907	8.607091
6.681951	473.308040	8.612109
7.012499	462.905711	8.617127
6.452438	456.337408	8.622144
6.679758	446.006116	8.627162
6.690327	439.459858	8.632179
6.376492	444.750119	8.637197
6.693386	438.920994	8.642215
6.340304	443.376870	8.647232
6.725425	438.343477	8.652250
6.353127	441.923858	8.657267
6.140107	440.906349	8.662285
6.698746	459.307086	8.667303
6.795351	475.225478	8.672320
6.524963	460.308616	8.677338
6.560674	456.185966	8.682355
6.253308	454.227258	8.687373
6.546342	464.770193	8.692391
6.473903	475.996247	8.697408
6.633451	464.022346	8.702426
6.461965	469.306365	8.707443
6.450468	466.043241	8.712461
6.596847	462.377624	8.717479
6.451556	473.276787	8.722496
6.612619	468.898945	8.727514
6.696202	474.238164	8.732531
6.674896	471.638426	8.737549
6.594033	470.264213	8.742567
6.506748	473.036437	8.747584
6.776898	466.885342	8.752602
6.846289	472.191873	8.757619
6.705383	463.844439	8.762637
7.045868	470.766984	8.767655
6.881640	465.851710	8.772672
6.714302	468.518694	8.777690
6.689288	473.133231	8.782707
6.502156	471.973648	8.787725
6.747673	471.879941	8.792743
6.573413	472.273233	8.797760
6.549946	461.940942	8.802778
6.693376	465.775276	8.807795
6.599751	473.367498	8.812813
6.684306	462.877566	8.817831
6.714077	471.583328	8.822848
6.940728	467.531609	8.827866
6.813573	467.541144	8.832883
6.705858	474.148566	8.837901
7.050552	472.780651	8.842919
6.607481	469.055956	8.847936
6.597582	463.529934	8.852954
6.841602	471.605970	8.857971
6.754445	471.950787	8.862989
6.796137	465.465895	8.868007
6.715133	474.354950	8.873024
7.043221	468.796383	8.878042
6.987266	463.181340	8.883059
6.603499	465.154686	8.888077
7.039494	467.746764	8.893095
6.634240	474.041078	8.898112
7.017907	470.572961	8.903130
6.690827	468.970443	8.908147
6.604024	473.723746	8.913165
6.560971	468.182150	8.918183
6.854987	468.144974	8.923200
6.551541	468.062647	8.928218
6.989693	464.673495	8.933235
6.996798	464.172251	8.938253
6.754833	466.171522	8.943271
6.643233	474.518636	8.948288
6.727455	476.655418	8.953306
6.875553	479.000505	8.958323
6.777659	479.661054	8.963341
7.136873	488.038278	8.968359
6.847138	476.753090	8.973376
6.792513	483.639499	8.978394
6.763519	488.222419	8.983411
6.816180	495.905184	8.988429
6.712222	497.139139	8.993447
6.730860	497.828224	8.998464
6.868104	502.739502	9.003482
7.241555	495.129460	9.008499
6.553904	503.851879	9.013517
6.891832	500.451758	9.018535
6.720638	507.845832	9.023552
6.723719	502.114708	9.028570
6.968437	500.360027	9.033587
6.712260	506.025577	9.038605
7.130914	499.637098	9.043623
6.804437	505.417037	9.048640
6.895189	511.539082	9.053658
6.719992	500.430961	9.058675
6.816713	525.903846	9.063693
7.097556	526.205049	9.068711
7.353623	529.588100	9.073728
7.289989	527.631540	9.078746
7.179323	507.603095	9.083763
7.273195	508.997587	9.088781
7.290271	490.836464	9.093799
7.129755	491.463292	9.098816
7.061560	493.546186	9.103834
7.257439	496.079414	9.108851
6.951822	504.708653	9.113869
7.142544	494.955791	9.118887
7.141538	498.288300	9.123904
6.898689	503.700478	9.128922
7.189303	498.290615	9.133939
7.069021	498.574387	9.138957
7.161211	497.093174	9.143975
7.192867	497.838761	9.148992
7.154660	504.735255	9.154010
7.626053	496.448017	9.159027
7.365704	497.427376	9.164045
7.405227	499.652660	9.169063
7.397789	503.957034	9.174080
7.378794	507.108087	9.179098
7.288464	500.615516	9.184115
7.246378	505.253754	9.189133
7.413657	501.507900	9.194151
7.252372	502.661394	9.199168
7.427155	503.978122	9.204186
7.388667	488.008927	9.209203
6.976404	487.852892	9.214221
7.328880	495.273625	9.219239
7.137814	499.753866	9.224256
7.293508	497.290552	9.229274
7.624913	493.088025	9.234291
6.920234	489.959756	9.239309
7.147075	482.112205	9.244327
6.795816	497.523326	9.249344
6.875598	493.944708	9.254362
7.058127	491.500571	9.259379
6.710337	504.845521	9.264397
7.036586	497.287583	9.269415
6.849581	510.451397	9.274432
6.948342	517.359467	9.279450
7.513533	531.579766	9.284467
7.230449	534.145266	9.289485
7.552519	522.710512	9.294503
7.567626	533.055437	9.299520
7.454296	526.155865	9.304538
7.156815	505.867628	9.309555
7.371612	505.898291	9.314573
7.467774	512.597748	9.319591
7.498106	500.833391	9.324608
7.183565	504.478627	9.329626
7.244128	511.515058	9.334643
7.653342	529.322160	9.339661
7.487689	516.673377	9.344679
7.566046	502.334510	9.349696
7.140296	505.223608	9.354714
7.406739	486.027961	9.359731
7.126989	498.853998	9.364749
7.604215	518.259753	9.369767
7.624411	525.521167	9.374784
7.450316	515.772799	9.379802
7.225528	504.667965	9.384819
7.081878	512.760582	9.389837
7.326849	526.734512	9.394855
7.573312	526.166271	9.399872
7.471149	525.956525	9.404890
7.779116	526.638447	9.409907
7.669891	532.341676	9.414925
7.619410	521.145176	9.419943
7.832300	508.273493	9.424960
7.384821	506.597803	9.429978
7.687259	495.237182	9.434995
7.547444	490.180269	9.440013
7.257357	492.667400	9.445031
7.425065	498.322398	9.450048
7.350178	501.451802	9.455066
7.628207	502.827215	9.460083
7.391399	517.431270	9.465101
7.504004	517.082818	9.470119
7.872049	517.825456	9.475136
7.725266	521.570861	9.480154
7.627042	511.405236	9.485171
7.346482	498.340289	9.490189
7.659846	503.606038	9.495207
7.508113	492.838304	9.500224
7.472816	523.561029	9.505242
7.781057	517.924043	9.510259
7.562616	527.669885	9.515277
7.890757	518.523148	9.520295
7.918852	505.840127	9.525312
7.446926	504.036605	9.530330
7.858211	489.991218	9.535347
7.151925	495.040400	9.540365
7.576467	497.119258	9.545383
7.815910	511.813135	9.550400
7.709092	523.920840	9.555418
7.433040	512.321374	9.560435
7.732825	526.835009	9.565453
7.720847	519.992077	9.570471
8.031608	522.663165	9.575488
7.480384	510.356954	9.580506
7.638281	504.555905	9.585523
7.488847	518.381766	9.590541
7.539930	519.681382	9.595559
7.989644	522.069439	9.600576
7.653243	528.844861	9.605594
7.747108	524.507655	9.610611
7.337223	528.722781	9.615629
7.416327	532.553021	9.620647
7.444861	530.371370	9.625664
7.692011	530.995061	9.630682
7.969537	522.924544	9.635699
7.642178	525.092480	9.640717
7.589906	526.978661	9.645735
7.874442	524.556799	9.650752
7.733276	525.854394	9.655770
7.842406	517.531074	9.660787
7.516527	530.059875	9.665805
7.627584	528.387752	9.670823
7.908353	524.973865	9.675840
7.642341	524.323171	9.680858
7.953087	531.961841	9.685875
7.768117	531.033179	9.690893
7.531416	529.043863	9.695911
8.078417	537.008351	9.700928
8.194592	555.021673	9.705946
7.985719	537.347487	9.710963
7.907277	531.984355	9.715981
7.662916	537.294046	9.720999
7.694348	520.352674	9.726016
7.675489	539.728602	9.731034
8.068548	555.372805	9.736051
8.394811	556.889440	9.741069
7.944292	546.417978	9.746087
8.313762	530.006999	9.751104
7.851576	527.801495	9.756122
7.991860	517.739275	9.761139
7.920957	530.465209	9.766157
7.776597	525.276566	9.771175
8.080673	525.632186	9.776192
7.711065	520.347978	9.781210
8.005764	519.277885	9.786227
7.847848	519.313772	9.791245
8.065746	536.820892	9.796263
8.075077	538.051641	9.801280
7.882790	535.289273	9.806298
8.145645	529.665901	9.811315
8.290182	538.205266	9.816333
8.291571	527.062176	9.821351
8.094753	522.868374	9.826368
8.065160	527.879722	9.831386
8.444045	527.354903	9.836403
7.968105	523.334476	9.841421
8.083745	520.941173	9.846439
8.124459	511.791053	9.851456
7.738153	512.981808	9.856474
8.039359	515.133843	9.861491
8.132120	522.360406	9.866509
7.831516	522.276427	9.871527
8.119226	513.131467	9.876544
7.934411	529.037660	9.881562
8.091447	534.910566	9.886579
8.017336	534.630825	9.891597
8.003996	556.013992	9.896615
8.391624	551.813163	9.901632
8.269654	554.175031	9.906650
8.116577	550.867227	9.911667
8.488285	544.306593	9.916685
8.127216	530.229822	9.921703
8.211574	520.675843	9.926720
8.110065	526.972634	9.931738
7.955381	523.386774	9.936755
8.245749	538.291718	9.941773
8.063398	542.168993	9.946791
8.686691	539.669777	9.951808
8.150426	543.938705	9.956826
7.880280	542.531856	9.961843
7.952678	542.644756	9.966861
8.172867	551.576299	9.971879
8.441357	554.325450	9.976896
8.359704	563.558736	9.981914
8.637701	557.167739	9.986931
8.484101	558.958898	9.991949
8.199794	550.292075	9.996967
8.594332	548.383652	10.001984
8.275440	527.352919	10.007002
8.025992	534.624933	10.012019
8.384800	536.284198	10.017037
8.209961	543.933601	10.022055
8.121299	552.140550	10.027072
8.219275	559.761516	10.032090
8.121047	554.865402	10.037107
8.213727	557.907625	10.042125
8.169310	555.707540	10.047143
8.294781	551.021022	10.052160
8.339097	565.447281	10.057178
8.442284	556.557048	10.062195
8.209422	553.374849	10.067213
8.517767	551.093125	10.072231
8.579808	552.062802	10.077248
8.575849	557.317929	10.082266
8.470629	553.762452	10.087283
8.885305	552.928970	10.092301
8.384920	554.520089	10.097319
8.383288	554.016155	10.102336
8.178076	544.673092	10.107354
8.447237	553.903790	10.112371
8.534704	556.389629	10.117389
8.369444	551.439855	10.122407
8.425220	548.661014	10.127424
8.300389	549.455939	10.132442
8.173472	553.411434	10.137459
8.547241	549.789240	10.142477
8.074672	552.467413	10.147495
8.668217	546.066490	10.152512
8.382323	542.994249	10.157530
8.557566	554.622427	10.162547
8.808672	542.076649	10.167565
8.617787	552.342122	10.172583
8.840192	545.156647	10.177600
8.475121	550.702262	10.182618
8.164471	544.781355	10.187635
8.547955	539.520459	10.192653
8.041026	539.381870	10.197671
8.635010	559.434835	10.202688
8.562793	576.385551	10.207706
8.583613	570.417621	10.212723
8.478606	582.014278	10.217741
8.777237	584.719470	10.222759
8.577157	579.086127	10.227776
8.707122	579.076904	10.232794
8.803447	583.615480	10.237811
9.221409	581.953159	10.242829
8.729628	571.941239	10.247847
8.608470	563.022604	10.252864
8.840525	548.552345	10.257882
8.685021	551.951587	10.262899
8.802912	543.276039	10.267917
8.642786	552.562664	10.272935
9.154213	549.505630	10.277952
8.851536	548.572443	10.282970
8.805326	560.255404	10.287987
8.836274	545.484219	10.293005
8.855549	553.502638	10.298023
8.738544	551.690730	10.303040
8.747095	557.932895	10.308058
8.665948	549.328685	10.313075
9.095634	554.628533	10.318093
8.839538	553.625432	10.323111
8.944573	552.625126	10.328128
9.199725	554.528117	10.333146
8.712516	548.117582	10.338163
8.877981	550.791869	10.343181
8.566011	548.943746	10.348199
8.775411	544.233097	10.353216
8.945242	544.280457	10.358234
8.877986	547.013553	10.363251
8.866496	545.493996	10.368269
8.752781	556.085647	10.373287
8.850464	548.357672	10.378304
8.819624	547.760352	10.383322
8.969057	555.901501	10.388339
9.138606	546.008816	10.393357
9.093210	555.181963	10.398375
8.805033	551.261138	10.403392
8.755659	555.935242	10.408410
8.824414	553.431791	10.413427
8.832963	545.956946	10.418445
8.494997	555.739723	10.423463
9.055338	553.228292	10.428480
8.778353	550.695877	10.433498
9.115426	558.806153	10.438515
9.302202	551.207312	10.443533
9.105018	549.320695	10.448551
8.799881	554.666635	10.453568
9.038255	551.999477	10.458586
8.883858	553.401030	10.463603
8.887115	548.839664	10.468621
8.488114	558.097544	10.473639
8.747658	558.767803	10.478656
9.159438	570.778452	10.483674
8.942713	579.994549	10.488691
9.172358	577.313479	10.493709
8.973275	573.838889	10.498727
9.293758	576.936893	10.503744
9.241189	568.423406	10.508762
9.000812	577.424141	10.513779
9.083725	573.409975	10.518797
8.865910	580.929120	10.523815
9.252104	585.443712	10.528832
9.315015	578.555087	10.533850
9.109697	575.114205	10.538867
9.023321	583.685926	10.543885
9.031676	583.364971	10.548903
8.877685	573.783699	10.553920
9.122037	570.991934	10.558938
9.158136	580.160656	10.563955
9.343869	581.320862	10.568973
9.227525	588.557083	10.573991
9.311798	585.833552	10.579008
9.586953	582.634347	10.584026
9.032526	583.150235	10.589043
9.066470	586.491738	10.594061
9.055608	583.859939	10.599079
9.305818	592.134214	10.604096
9.176508	582.645694	10.609114
8.921445	586.140558	10.614131
9.218197	577.815270	10.619149
9.217566	578.187097	10.624167
9.079363	571.643569	10.629184
9.113607	570.861270	10.634202
8.942117	578.062526	10.639219
9.122301	578.216630	10.644237
9.189664	575.908865	10.649255
9.116975	579.216846	10.654272
9.495731	584.951883	10.659290
9.070341	600.050992	10.664307
9.503424	607.064362	10.669325
9.395283	607.296128	10.674343
9.586011	604.716372	10.679360
9.638606	577.883472	10.684378
9.358789	582.352450	10.689395
9.253806	574.289737	10.694413
9.296431	578.037255	10.699431
9.366117	598.371366	10.704448
9.589699	609.662862	10.709466
9.297563	605.997388	10.714483
9.292856	610.312952	10.719501
9.881179	606.086356	10.724519
9.345705	601.334475	10.729536
9.477395	591.533850	10.734554
9.708184	600.041646	10.739571
9.610101	591.255779	10.744589
9.661706	590.330456	10.749607
9.931266	584.283146	10.754624
9.643960	578.563466	10.759642
9.671414	586.792345	10.764659
9.641870	576.414136	10.769677
9.450686	580.591290	10.774695
9.586658	585.839004	10.779712
9.725323	571.212742	10.784730
9.502590	581.236870	10.789747
9.465647	572.179884	10.794765
9.538895	581.374343	10.799783
9.741964	580.195214	10.804800
9.783206	572.798796	10.809818
9.540210	582.576296	10.814835
9.574322	578.324556	10.819853
9.537761	574.271909	10.824871
9.220313	582.316180	10.829888
9.893510	576.315414	10.834906
9.670884	584.582553	10.839923
9.426156	577.840927	10.844941
9.631672	589.705048	10.849959
9.672193	595.204776	10.854976
9.954732	586.402340	10.859994
9.465540	585.544914	10.865011
9.519087	575.935181	10.870029
9.593416	580.780528	10.875047
9.402902	577.243106	10.880064
9.685436	565.256242	10.885082
9.590792	589.385418	10.890099
9.754608	593.284121	10.895117
9.756430	606.689763	10.900135
9.620749	611.000639	10.905152
9.832127	604.411021	10.910170
9.919852	613.526729	10.915187
9.962108	602.837813	10.920205
9.668051	603.357828	10.925223
9.738661	606.181091	10.930240
9.843516	604.975707	10.935258
9.875716	623.720489	10.940275
9.808278	610.616810	10.945293
10.117337	612.202634	10.950311
9.914655	608.594782	10.955328
9.773523	588.781303	10.960346
9.571648	590.812335	10.965363
9.915667	604.672304	10.970381
9.745057	612.613541	10.975399
9.495015	612.008228	10.980416
10.068349	606.405853	10.985434
10.126353	612.376678	10.990451
9.954675	606.460293	10.995469
10.394196	608.508341	11.000487
9.846952	616.641465	11.005504
10.153557	605.355660	11.010522
10.144658	608.044854	11.015539
10.089196	591.471708	11.020557
9.978055	578.382772	11.025575
9.770327	582.101278	11.030592
10.063988	579.737933	11.035610
9.797961	585.008120	11.040627
10.109339	607.008806	11.045645
10.379800	602.308894	11.050663
10.283615	595.112375	11.055680
10.093151	583.042806	11.060698
10.055556	571.304210	11.065715
9.983796	576.553643	11.070733
10.098726	569.015899	11.075751
9.645319	580.939520	11.080768
10.055323	579.850528	11.085786
10.238206	598.251057	11.090803
10.052683	592.254692	11.095821
10.073384	589.179505	11.100839
10.310536	601.767878	11.105856
10.298681	600.481826	11.110874
10.124522	578.702299	11.115891
9.816255	590.542056	11.120909
10.566185	583.940823	11.125927
10.046657	593.310212	11.130944
10.108322	571.559751	11.135962
10.112285	584.592997	11.140979
10.297018	596.203495	11.145997
9.926751	593.505231	11.151015
10.224531	601.172065	11.156032
10.606406	591.976430	11.161050
10.053440	594.421875	11.166067
10.058730	587.896309	11.171085
10.293921	596.595881	11.176103
9.925410	600.328810	11.181120
10.381410	600.539992	11.186138
10.162847	608.230916	11.191155
10.148225	607.468124	11.196173
10.399957	598.284192	11.201191
10.149608	613.459047	11.206208
10.411755	607.477125	11.211226
10.254533	607.734734	11.216243
10.099668	606.973118	11.221261
10.168584	598.324151	11.226279
10.212527	603.425309	11.231296
10.425567	595.277249	11.236314
10.214850	599.535984	11.241331
10.141313	603.967662	11.246349
10.181543	604.645303	11.251367
9.882644	621.434798	11.256384
10.422860	616.718951	11.261402
10.339659	627.338469	11.266419
10.346153	633.346570	11.271437
11.119331	634.595717	11.276455
10.643694	632.658156	11.281472
10.737129	621.159227	11.286490
10.156004	612.986372	11.291507
10.267919	612.569927	11.296525
10.385011	607.021447	11.301543
10.512549	609.893942	11.306560
10.282988	614.149503	11.311578
10.324162	618.819261	11.316595
10.555236	634.075432	11.321613
10.941837	635.108687	11.326631
10.629694	637.663859	11.331648
10.522333	626.343442	11.336666
10.707096	620.679428	11.341683
10.742113	616.812149	11.346701
10.697892	606.496977	11.351719
10.488930	604.905788	11.356736
10.483403	601.690463	11.361754
10.528997	615.456558	11.366771
10.678870	628.356631	11.371789
10.837910	621.626469	11.376807
10.411653	621.125526	11.381824
10.654529	625.039884	11.386842
10.912437	621.654956	11.391859
10.589586	629.587555	11.396877
10.870006	624.475382	11.401895
10.665899	621.430327	11.406912
10.701312	617.122459	11.411930
10.609012	611.059866	11.416947
10.664944	631.177414	11.421965
10.850691	628.806734	11.426983
10.812219	636.264321	11.432000
11.128639	623.348628	11.437018
10.792729	605.283418	11.442035
10.430228	609.641300	11.447053
11.006344	603.976264	11.452071
10.632021	609.813177	11.457088
10.451805	618.907511	11.462106
10.966682	624.670020	11.467123
10.802562	625.646838	11.472141
10.965971	630.003070	11.477159
10.859195	631.355802	11.482176
10.807462	632.902950	11.487194
10.983051	623.909554	11.492211
10.878735	628.234925	11.497229
11.289789	619.018301	11.502247
10.774359	614.839045	11.507264
10.655636	601.272241	11.512282
11.164924	609.122153	11.517299
10.597284	610.986209	11.522317
10.794030	619.550436	11.527335
11.029120	626.649353	11.532352
11.146982	629.187648	11.537370
11.088818	625.960562	11.542387
11.093567	620.414145	11.547405
10.917791	612.570208	11.552423
11.018556	617.562362	11.557440
11.042854	619.885847	11.562458
11.121274	612.310823	11.567475
10.783097	615.706471	11.572493
10.900046	617.872497	11.577511
11.119724	624.393686	11.582528
11.190522	625.497736	11.587546
11.126099	623.299183	11.592563
10.958614	622.992778	11.597581
11.083005	620.424004	11.602599
10.923566	633.771339	11.607616
11.123720	633.981188	11.612634
10.848222	626.319101	11.617651
10.989743	632.093439	11.622669
11.299563	621.680658	11.627687
11.119452	625.669781	11.632704
10.953995	624.683948	11.637722
11.095805	626.829718	11.642739
10.989810	634.017792	11.647757
11.187053	626.515206	11.652775
11.136463	633.667730	11.657792
11.135325	625.555120	11.662810
11.398740	620.047757	11.667827
11.125546	618.466022	11.672845
10.955808	624.126159	11.677863
11.376354	629.403139	11.682880
10.908307	631.917201	11.687898
11.285589	630.797798	11.692915
11.279109	630.619841	11.697933
11.352526	627.277666	11.702951
11.170471	633.094167	11.707968
11.105135	628.131365	11.712986
11.281913	624.196520	11.718003
11.347287	641.813458	11.723021
11.580662	638.270394	11.728039
11.189017	635.574875	11.733056
11.204191	637.365655	11.738074
11.355098	640.087051	11.743091
11.268035	652.569712	11.748109
11.621601	655.639027	11.753127
11.626980	658.870322	11.758144
11.193096	654.288205	11.763162
11.366911	651.653372	11.768179
11.655099	653.917419	11.773197
11.667899	641.277958	11.778215
11.396283	629.806007	11.783232
11.373517	629.737827	11.788250
11.638498	634.141411	11.793267
11.361055	636.444395	11.798285
11.776764	640.436431	11.803303
11.623255	628.206780	11.808320
11.483443	631.117250	11.813338
11.623313	614.188526	11.818355
11.080252	621.243468	11.823373
11.224325	626.981556	11.828391
12.013045	642.494589	11.833408
11.965493	639.459826	11.838426
11.688490	628.333629	11.843443
11.580435	617.584952	11.848461
11.373342	616.670970	11.853479
11.408220	626.414296	11.858496
10.888400	642.923485	11.863514
11.682833	641.165357	11.868531
11.660986	651.029895	11.873549
12.030347	640.858015	11.878567
11.736516	647.889808	11.883584
11.589447	639.462005	11.888602
11.946568	637.943209	11.893619
11.651102	643.146248	11.898637
11.979570	640.215353	11.903655
11.847892	641.967854	11.908672
11.676577	641.880574	11.913690
12.131624	628.704929	11.918707
11.732402	624.247388	11.923725
11.597538	619.501208	11.928743
11.742057	628.550831	11.933760
11.621101	634.318635	11.938778
11.693163	636.379111	11.943795
11.416539	647.810152	11.948813
12.027638	643.065633	11.953831
11.803550	644.608253	11.958848
11.486115	653.106469	11.963866
11.722659	635.510965	11.968883
11.938982	648.712238	11.973901
11.979735	649.394912	11.978919
12.118850	646.532376	11.983936
12.098658	650.380071	11.988954
12.313574	646.570786	11.993971
12.215129	646.148231	11.998989
12.038330	637.458832	12.004007
12.135031	640.793104	12.009024
11.921425	645.119649	12.014042
12.238653	628.908346	12.019059
11.830570	620.808008	12.024077
11.870236	630.315519	12.029095
11.805954	627.583510	12.034112
12.006134	636.849498	12.039130
12.059863	635.419126	12.044147
12.033379	644.013245	12.049165
12.108674	641.493934	12.054183
11.979700	643.616832	12.059200
11.877948	643.259781	12.064218
11.955591	639.256706	12.069235
12.030907	642.767344	12.074253
12.158357	647.688951	12.079271
12.278129	648.451054	12.084288
11.787309	642.392631	12.089306
12.090443	641.474864	12.094323
12.012391	650.513326	12.099341
12.218124	648.175159	12.104359
12.211091	639.264353	12.109376
11.998327	644.547787	12.114394
12.107945	639.796549	12.119411
12.018677	631.052111	12.124429
12.011238	642.537387	12.129447
12.365490	636.273683	12.134464
12.187978	644.777463	12.139482
11.949122	639.343421	12.144499
12.250696	639.991567	12.149517
11.741836	647.229822	12.154535
12.397713	645.472197	12.159552
11.822977	661.751537	12.164570
12.569241	660.237196	12.169587
12.272987	665.036066	12.174605
12.108677	660.237272	12.179623
12.430487	667.076193	12.184640
12.378994	672.884475	12.189658
12.242490	666.793354	12.194675
12.555283	662.089170	12.199693
12.416124	662.255605	12.204711
12.321087	663.049735	12.209728
12.513357	666.911464	12.214746
12.541596	661.668212	12.219763
12.509568	666.538677	12.224781
12.300729	666.832785	12.229799
12.751171	663.667921	12.234816
12.276399	663.763558	12.239834
12.688474	656.354904	12.244851
12.736035	660.442943	12.249869
12.536513	657.466016	12.254887
12.759357	660.471156	12.259904
12.577264	656.930352	12.264922
12.529898	655.209650	12.269939
12.724997	659.412227	12.274957
12.496839	652.763487	12.279975
12.655255	656.232417	12.284992
12.441447	641.082206	12.290010
12.743618	642.422337	12.295027
12.523191	644.160796	12.300045
12.771842	656.399694	12.305063
12.557856	645.668144	12.310080
12.759723	655.727517	12.315098
12.757250	646.288818	12.320115
12.276631	646.469276	12.325133
12.488390	657.812763	12.330151
12.988801	655.192743	12.335168
12.833376	665.964396	12.340186
12.757858	664.144031	12.345203
12.758361	663.435814	12.350221
12.647929	669.370383	12.355239
13.151526	660.646255	12.360256
12.636326	653.877339	12.365274
12.669756	653.690017	12.370291
12.836531	656.299740	12.375309
12.594772	667.228201	12.380327
13.002279	664.349171	12.385344
12.710098	673.345942	12.390362
12.915318	662.850853	12.395379
12.452556	657.352311	12.400397
12.390419	659.824753	12.405415
12.533331	657.592257	12.410432
12.562572	660.082242	12.415450
12.573508	661.913882	12.420467
12.853504	662.234125	12.425485
12.622323	658.410915	12.430503
12.744978	667.089400	12.435520
13.141912	693.471849	12.440538
13.352003	680.224917	12.445555
13.143300	664.357737	12.450573
12.910132	671.201160	12.455591
13.055511	659.966026	12.460608
12.879005	664.711998	12.465626
12.705469	660.489107	12.470643
13.048520	672.477361	12.475661
12.841685	689.674101	12.480679
13.053680	690.450855	12.485696
13.116043	698.593309	12.490714
13.388813	695.666902	12.495731
13.560798	676.663619	12.500749
13.299854	668.001914	12.505767
13.589805	654.677611	12.510784
13.265094	662.230636	12.515802
13.052112	659.387819	12.520819
13.236258	661.042360	12.525837
13.244987	660.792991	12.530855
13.642699	657.602216	12.535872
13.084868	659.269388	12.540890
13.240344	665.279209	12.545907
13.287978	648.357847	12.550925
13.168843	660.458054	12.555943
13.472357	657.691120	12.560960
13.050375	657.562674	12.565978
13.252030	654.385074	12.570995
13.422740	655.501320	12.576013
12.925871	662.113618	12.581031
13.112210	663.955580	12.586048
13.113039	662.115093	12.591066
13.257472	655.026726	12.596083
13.054700	656.335123	12.601101
13.028082	656.359308	12.606119
13.106096	654.506828	12.611136
13.325587	670.568843	12.616154
13.147387	691.120885	12.621171
13.560563	684.919053	12.626189
13.645017	688.304574	12.631207
13.387342	678.996690	12.636224
13.285325	690.685448	12.641242
13.515784	691.405605	12.646259
13.397029	684.901719	12.651277
13.197079	700.121853	12.656295
13.722396	686.729417	12.661312
13.755698	689.928144	12.666330
13.663808	695.843511	12.671347
13.864614	698.738534	12.676365
13.624554	674.865178	12.681383
13.660824	663.038695	12.686400
13.604299	664.664589	12.691418
13.606811	666.656275	12.696435
13.460697	656.300858	12.701453
13.220066	657.859605	12.706471
13.347565	678.821613	12.711488
13.692966	684.856682	12.716506
13.446637	684.999526	12.721523
13.747898	682.616798	12.726541
13.725498	688.054541	12.731559
13.697706	685.709764	12.736576
13.579965	686.763152	12.741594
13.683287	688.840505	12.746611
13.767478	683.690731	12.751629
13.566871	693.204997	12.756647
13.892129	684.135998	12.761664
13.924344	679.409768	12.766682
13.768305	685.208202	12.771699
14.087207	687.524252	12.776717
13.981655	686.859972	12.781735
13.979899	682.555091	12.786752
13.926718	677.999292	12.791770
13.477474	684.397426	12.796787
13.598922	685.652533	12.801805
13.754078	683.534928	12.806823
13.750174	675.305827	12.811840
14.113642	676.620852	12.816858
13.794919	676.375313	12.821875
14.108756	678.549689	12.826893
13.961124	685.328564	12.831911
14.080475	684.975055	12.836928
13.815876	691.262306	12.841946
13.724518	688.076528	12.846963
14.273194	681.888480	12.851981
13.960089	683.340338	12.856999
13.839396	677.380446	12.862016
13.693644	683.546052	12.867034
13.527699	680.104138	12.872051
14.002510	676.076231	12.877069
13.964542	680.215049	12.882087
13.853978	674.860532	12.887104
14.131559	679.163623	12.892122
13.841928	681.262738	12.897139
14.094778	664.330605	12.902157
13.968056	686.010663	12.907175
14.329772	697.798613	12.912192
14.376959	691.125522	12.917210
14.070163	678.391716	12.922227
14.230301	672.554999	12.927245
14.275961	676.651231	12.932263
14.432304	677.679706	12.937280
14.646331	673.307602	12.942298
14.303608	677.997642	12.947315
14.249582	676.635500	12.952333
14.064637	685.868444	12.957351
14.433993	686.560090	12.962368
14.218192	679.371922	12.967386
13.824450	674.740241	12.972403
14.087204	675.663305	12.977421
14.342646	683.997783	12.982439
14.774967	695.215804	12.987456
14.436948	685.280311	12.992474
14.225044	686.863829	12.997491
14.283530	676.631991	13.002509
14.575742	680.144516	13.007527
14.181715	674.827094	13.012544
14.693983	683.761135	13.017562
14.147691	685.966132	13.022579
14.569495	684.721250	13.027597
14.433739	680.845622	13.032615
14.404965	692.271873	13.037632
14.629404	696.691243	13.042650
14.644743	701.741661	13.047667
14.885859	681.530928	13.052685
14.539499	680.244750	13.057703
14.463659	671.732304	13.062720
14.673370	668.953343	13.067738
14.376302	677.374582	13.072755
14.497745	665.556433	13.077773
14.711816	676.751134	13.082791
14.565959	665.206761	13.087808
14.638861	665.516417	13.092826
14.690887	679.272057	13.097843
14.956719	661.654352	13.102861
14.528109	663.108800	13.107879
14.467952	676.619642	13.112896
14.666891	666.710990	13.117914
14.364995	682.925097	13.122931
14.508111	689.000356	13.127949
14.601190	696.387766	13.132967
14.816564	692.846095	13.137984
14.668550	692.227821	13.143002
14.509879	708.233603	13.148019
15.060919	691.606768	13.153037
14.687774	700.592947	13.158055
14.664097	697.595949	13.163072
14.647282	696.805958	13.168090
14.650690	701.108000	13.173107
14.753938	702.820034	13.178125
14.936004	701.887274	13.183143
14.919293	700.459900	13.188160
14.884882	696.976911	13.193178
14.698110	697.331535	13.198195
15.173913	697.546919	13.203213
15.067728	706.775102	13.208231
15.179043	700.252403	13.213248
15.010414	699.600142	13.218266
14.970692	700.494951	13.223283
15.196152	694.434430	13.228301
15.075818	699.734859	13.233319
14.516648	700.073592	13.238336
15.118785	691.853966	13.243354
14.812456	701.701867	13.248371
14.872417	699.923627	13.253389
14.920583	703.095487	13.258407
14.924594	710.951170	13.263424
15.123268	703.041247	13.268442
15.230403	707.319029	13.273459
14.857884	706.262758	13.278477
15.198948	711.693865	13.283495
15.160325	717.942528	13.288512
15.451085	719.509347	13.293530
15.011521	722.403330	13.298547
15.376021	731.411864	13.303565
15.578859	719.905375	13.308583
15.243884	709.343019	13.313600
15.279554	695.871820	13.318618
15.237718	695.822151	13.323635
15.114925	692.563628	13.328653
15.263542	706.735951	13.333671
15.079027	718.507678	13.338688
15.313854	729.682052	13.343706
15.442871	727.607744	13.348723
15.449191	727.817803	13.353741
15.805193	720.988058	13.358759
15.465622	715.313986	13.363776
15.538254	703.112574	13.368794
15.144088	696.566497	13.373811
15.389580	701.313072	13.378829
15.444494	710.531902	13.383847
15.753777	719.132666	13.388864
15.625733	697.985063	13.393882
15.403339	696.955506	13.398899
15.008704	694.949802	13.403917
15.824809	708.400611	13.408935
15.266103	719.996911	13.413952
15.853442	725.747460	13.418970
15.739695	724.097582	13.423987
15.552860	713.220552	13.429005
15.733064	710.005550	13.434023
15.515358	704.743562	13.439040
15.703022	709.686713	13.444058
15.543714	719.319346	13.449075
15.805537	710.649790	13.454093
15.994037	698.694142	13.459111
15.711469	699.658295	13.464128
15.921701	693.540456	13.469146
15.660600	691.332731	13.474163
15.638988	690.790764	13.479181
15.458087	691.821936	13.484199
15.430525	699.336798	13.489216
15.858801	704.404662	13.494234
15.962586	721.735427	13.499251
15.809599	715.089567	13.504269
15.902697	716.867058	13.509287
15.799503	723.316168	13.514304
15.843166	707.625647	13.519322
16.017098	722.209123	13.524339
16.042784	708.072280	13.529357
16.083461	694.992357	13.534375
15.689110	689.203357	13.539392
15.979822	679.677115	13.544410
15.735198	686.483862	13.549427
15.561758	690.408515	13.554445
15.793039	707.276444	13.559463
15.619735	719.610064	13.564480
16.135074	714.326292	13.569498
16.039048	715.817795	13.574515
15.961542	716.050789	13.579533
15.942856	710.117691	13.584551
15.705792	718.551455	13.589568
15.755961	709.435478	13.594586
15.738921	714.249936	13.599603
15.976098	711.177460	13.604621
16.171531	715.039858	13.609639
15.719555	721.421531	13.614656
15.720103	723.516300	13.619674
15.760723	740.354816	13.624691
16.260120	741.837881	13.629709
16.462772	741.463097	13.634727
16.110355	745.839819	13.639744
16.289350	745.891764	13.644762
16.481696	739.913476	13.649779
16.319254	747.913269	13.654797
16.319723	742.630496	13.659815
16.307081	745.247503	13.664832
16.253588	744.352565	13.669850
16.437171	738.411946	13.674867
16.479994	740.904421	13.679885
16.796090	739.024712	13.684903
16.370053	743.273867	13.689920
16.657783	738.267133	13.694938
16.315581	716.476656	13.699955
16.285129	716.087325	13.704973
16.756186	717.757353	13.709991
16.370197	720.513732	13.715008
16.410744	708.906966	13.720026
16.530104	716.998262	13.725043
16.589115	723.361068	13.730061
16.568541	719.649417	13.735079
16.471888	717.784910	13.740096
16.485490	710.470951	13.745114
16.653692	725.440397	13.750131
16.277941	728.000604	13.755149
16.686852	731.462323	13.760167
16.610278	745.757004	13.765184
16.703822	738.403812	13.770202
16.546496	738.011475	13.775219
16.342129	739.976406	13.780237
16.538750	735.818180	13.785255
16.423072	743.474025	13.790272
16.638487	742.586919	13.795290
16.406120	731.299328	13.800307
16.542571	733.915267	13.805325
16.550218	735.623844	13.810343
16.242401	742.776887	13.815360
16.408941	733.463683	13.820378
16.815950	750.975361	13.825395
16.901485	770.434680	13.830413
17.190114	756.250317	13.835431
16.828558	753.254140	13.840448
16.758958	738.635436	13.845466
17.000191	735.959506	13.850483
17.004842	740.134982	13.855501
17.124641	728.896160	13.860519
16.970355	744.955976	13.865536
16.889109	729.956158	13.870554
16.792351	731.917049	13.875571
16.725019	729.815414	13.880589
16.967770	728.191145	13.885607
16.659163	750.419493	13.890624
17.047722	754.247954	13.895642
17.266497	770.604665	13.900659
17.311361	754.371405	13.905677
17.166782	740.250129	13.910695
17.377273	739.324864	13.915712
17.070277	732.948579	13.920730
17.281774	726.193151	13.925747
17.159812	731.245843	13.930765
17.058427	722.032125	13.935783
17.188136	734.702962	13.940800
17.052398	729.520696	13.945818
17.111090	739.237710	13.950835
16.955762	731.032471	13.955853
17.448586	737.694296	13.960871
17.391306	738.229436	13.965888
17.446995	732.236379	13.970906
17.232293	733.427080	13.975923
16.914517	729.505598	13.980941
17.254529	737.495018	13.985959
17.570741	756.978324	13.990976
17.495346	744.438418	13.995994
17.533967	731.763113	14.001011
17.207651	724.188127	14.006029
17.194962	723.047864	14.011047
17.310654	736.218635	14.016064
17.633436	754.680433	14.021082
17.567133	750.381891	14.026099
17.624754	745.289642	14.031117
17.622916	735.366557	14.036135
17.438751	731.448933	14.041152
17.329732	729.493564	14.046170
17.692817	734.113203	14.051187
17.514095	732.796112	14.056205
17.309130	726.572217	14.061223
17.331992	740.964596	14.066240
17.374717	746.477398	14.071258
17.508690	755.720564	14.076275
17.463362	762.235301	14.081293
17.941597	751.598887	14.086311
17.700095	749.363893	14.091328
17.872636	750.264895	14.096346
18.107089	749.887995	14.101363
17.700271	751.016418	14.106381
18.056568	746.617981	14.111399
17.841202	733.976463	14.116416
17.826084	735.080968	14.121434
17.772486	718.710515	14.126451
17.600255	723.511700	14.131469
17.922400	731.454471	14.136487
17.860015	737.650387	14.141504
17.888010	747.295327	14.146522
17.876113	739.851332	14.151539
17.729629	743.131412	14.156557
17.590243	734.859756	14.161575
17.808311	750.375269	14.166592
17.673113	752.668889	14.171610
17.933483	749.396118	14.176627
17.868909	754.123583	14.181645
17.828016	745.462798	14.186663
17.880928	749.422422	14.191680
17.632488	748.925099	14.196698
17.983158	743.001297	14.201715
17.554969	752.900510	14.206733
17.573079	754.868366	14.211751
17.882123	752.190259	14.216768
18.223877	771.262290	14.221786
18.698280	771.860172	14.226803
18.255959	765.357864	14.231821
18.397038	756.975585	14.236839
17.888706	752.058933	14.241856
18.005292	751.433454	14.246874
18.276239	741.389216	14.251891
18.159453	752.317121	14.256909
18.003097	764.493253	14.261927
18.327105	768.497752	14.266944
18.182134	770.601270	14.271962
18.509777	770.055404	14.276979
18.483497	774.511981	14.281997
18.337634	766.800406	14.287015
18.429696	757.386534	14.292032
18.207688	769.805419	14.297050
19.028153	765.824973	14.302067
18.595972	756.082576	14.307085
18.493476	742.966874	14.312103
18.690049	743.830039	14.317120
18.483690	749.767531	14.322138
18.485120	741.272958	14.327155
17.923652	745.715002	14.332173
18.351523	737.365162	14.337191
18.181674	746.694063	14.342208
18.225135	767.842933	14.347226
18.488696	759.896647	14.352243
18.628487	767.186597	14.357261
18.354991	765.884803	14.362279
18.432610	773.248433	14.367296
18.603220	767.663477	14.372314
18.778203	770.608457	14.377331
18.482183	773.919603	14.382349
18.413231	765.657920	14.387367
18.401434	769.546772	14.392384
18.592325	771.998987	14.397402
19.014357	766.915284	14.402419
18.672809	765.505080	14.407437
18.805798	769.061312	14.412455
18.631591	767.283259	14.417472
18.714266	760.923536	14.422490
18.925933	764.283679	14.427507
18.450221	771.840501	14.432525
18.807572	771.908581	14.437543
19.021692	781.282972	14.442560
18.932856	792.458233	14.447578
18.944527	771.160629	14.452595
18.754354	778.735919	14.457613
18.917455	788.835655	14.462631
19.183100	791.293603	14.467648
19.346203	793.415006	14.472666
19.228512	772.052606	14.477683
18.895745	768.981584	14.482701
18.964729	769.010016	14.487719
18.993040	761.584941	14.492736
18.738843	775.072885	14.497754
19.418246	784.452119	14.502771
19.195543	786.914950	14.507789
19.180255	776.310635	14.512807
19.028065	766.538797	14.517824
19.403378	770.504882	14.522842
19.473485	764.363370	14.527859
19.553383	760.618538	14.532877
19.305567	756.618933	14.537895
19.432477	756.944057	14.542912
19.137116	754.469568	14.547930
19.189428	757.263214	14.552947
19.258921	765.773401	14.557965
19.173951	750.192320	14.562983
19.262077	755.675956	14.568000
19.217126	756.833825	14.573018
19.390185	755.036064	14.578035
19.208749	759.104964	14.583053
19.196978	755.138318	14.588071
19.617584	771.840330	14.593088
19.409302	783.082211	14.598106
19.560742	782.932825	14.603123
19.288772	779.157675	14.608141
18.944152	787.984070	14.613159
19.215746	790.681573	14.618176
19.457177	794.252137	14.623194
19.468204	784.619001	14.628211
19.081192	783.970615	14.633229
19.292518	777.796659	14.638247
19.411377	780.586770	14.643264
19.488497	787.431224	14.648282
19.580910	788.494701	14.653299
19.673101	805.846376	14.658317
19.861661	806.728194	14.663335
19.950265	784.527326	14.668352
19.804243	790.933558	14.673370
19.941183	783.878262	14.678387
19.820801	790.842425	14.683405
19.670910	782.849634	14.688423
20.052584	781.965309	14.693440
19.656899	775.152928	14.698458
19.986383	787.934816	14.703475
19.918051	787.664348	14.708493
20.146784	781.919377	14.713511
19.983042	779.918734	14.718528
19.942545	782.622639	14.723546
19.897988	781.109715	14.728563
20.123672	785.408438	14.733581
19.817592	787.527219	14.738599
20.142857	782.293007	14.743616
19.753858	790.236247	14.748634
19.824401	787.105526	14.753651
19.912303	789.419686	14.758669
19.711426	791.834811	14.763687
20.096788	798.603035	14.768704
19.996437	814.621710	14.773722
20.061701	809.118352	14.778739
19.931594	813.268527	14.783757
20.062651	814.009480	14.788775
20.445615	813.405635	14.793792
20.378166	804.937393	14.798810
20.329647	798.737561	14.803827
20.523442	799.027202	14.808845
20.554648	809.869622	14.813863
20.794752	791.363948	14.818880
20.599454	775.912128	14.823898
20.489775	765.861612	14.828915
20.467269	760.131872	14.833933
19.890488	765.430743	14.838951
20.535589	763.453249	14.843968
20.241779	766.124690	14.848986
20.483036	767.408388	14.854003
20.214278	767.858868	14.859021
20.143045	771.346954	14.864039
20.574509	780.853458	14.869056
20.455649	792.689169	14.874074
20.695586	792.464108	14.879091
20.586417	805.569814	14.884109
20.332677	802.887648	14.889127
20.857123	797.068510	14.894144
20.274516	798.270530	14.899162
20.412432	799.148923	14.904179
20.578388	798.702659	14.909197
20.661678	797.156754	14.914215
20.604496	794.830212	14.919232
20.558053	788.675707	14.924250
20.916090	801.592636	14.929267
20.773604	799.290061	14.934285
20.566530	802.158946	14.939303
20.835882	791.984237	14.944320
20.936522	796.057618	14.949338
20.966935	799.647771	14.954355
20.904057	797.335951	14.959373
20.790256	797.836753	14.964391
20.715683	796.494144	14.969408
20.733606	798.906503	14.974426
20.522528	792.686349	14.979443
20.882574	795.538883	14.984461
20.558791	808.205742	14.989479
20.634185	798.043067	14.994496
20.740961	805.423537	14.999514
20.798090	818.149766	15.004531
21.280227	824.587032	15.009549
21.146665	833.652114	15.014567
21.488659	822.218172	15.019584
21.101174	801.220862	15.024602
20.995409	799.277542	15.029619
21.112225	798.305190	15.034637
20.903069	805.605303	15.039655
20.885700	807.886506	15.044672
21.249447	819.171089	15.049690
21.211379	830.160814	15.054707
21.522519	821.603891	15.059725
21.308117	833.660168	15.064743
21.527684	823.299597	15.069760
21.483015	824.188146	15.074778
21.080493	817.039886	15.079795
21.500149	814.768630	15.084813
21.417477	832.555963	15.089831
21.755107	817.684722	15.094848
21.462734	813.549574	15.099866
21.297637	796.368407	15.104883
21.532650	792.438836	15.109901
21.472733	793.457462	15.114919
21.391165	798.884176	15.119936
21.258825	806.893187	15.124954
21.476080	816.787134	15.129971
21.690830	822.180932	15.134989
21.680445	823.611022	15.140007
21.508041	819.894962	15.145024
21.759822	820.232874	15.150042
21.612587	826.400750	15.155059
21.849729	820.840583	15.160077
21.667993	821.530579	15.165095
21.826342	813.469017	15.170112
21.687567	820.698825	15.175130
21.663164	826.139704	15.180147
21.816922	823.278253	15.185165
21.492903	827.046387	15.190183
21.824459	816.753099	15.195200
21.799325	832.554623	15.200218
21.676221	829.440604	15.205235
21.991480	822.940775	15.210253
21.790521	829.782871	15.215271
22.205940	828.190234	15.220288
21.727804	822.495368	15.225306
21.705350	829.929137	15.230323
21.541276	824.758222	15.235341
21.697446	824.304524	15.240359
21.722951	830.545369	15.245376
21.421212	823.689852	15.250394
21.914359	826.689242	15.255411
22.135201	838.647077	15.260429
21.987055	853.215901	15.265447
22.434686	840.946381	15.270464
22.267122	831.969923	15.275482
21.931967	827.243458	15.280499
21.996266	827.032914	15.285517
22.269826	842.394457	15.290535
22.167586	833.352853	15.295552
22.249568	841.607484	15.300570
22.551735	842.980310	15.305587
22.628537	830.845820	15.310605
22.434045	824.538659	15.315623
22.436818	811.776709	15.320640
22.697310	800.991680	15.325658
22.062400	805.173079	15.330675
22.410552	799.887043	15.335693
22.158687	805.367942	15.340711
22.497539	806.356363	15.345728
22.322608	805.031158	15.350746
22.499740	823.710455	15.355763
22.795195	833.337933	15.360781
22.552204	824.893235	15.365799
22.486556	806.996017	15.370816
22.588383	809.750766	15.375834
22.543020	821.103486	15.380851
22.753726	825.127942	15.385869
22.232629	820.070869	15.390887
22.513348	827.296569	15.395904
22.893971	822.749207	15.400922
23.182938	830.881768	15.405939
23.232135	824.038216	15.410957
22.986818	813.693608	15.415975
22.936287	801.606601	15.420992
22.792961	791.322281	15.426010
23.103358	799.052084	15.431027
23.111940	790.888960	15.436045
22.691617	792.200322	15.441063
22.577076	793.980710	15.446080
22.892610	793.766359	15.451098
22.777121	797.141313	15.456115
22.696092	792.497970	15.461133
22.912950	796.453687	15.466151
22.833814	798.832513	15.471168
23.125323	804.708846	15.476186
23.034613	816.008444	15.481203
23.046522	809.186821	15.486221
22.865984	811.569054	15.491239
23.051114	821.322268	15.496256
23.141040	823.603817	15.501274
22.966681	826.994430	15.506291
23.340196	822.210068	15.511309
22.939740	825.644811	15.516327
23.188439	815.181001	15.521344
23.260842	819.442913	15.526362
22.887938	825.963496	15.531379
23.178472	825.498966	15.536397
23.294121	830.605648	15.541415
23.464250	827.828883	15.546432
23.542742	821.589508	15.551450
23.511252	821.016890	15.556467
23.554439	825.353323	15.561485
23.487726	829.170579	15.566503
23.308650	825.030840	15.571520
23.681958	822.475932	15.576538
23.632848	824.986399	15.581555
23.456460	818.847493	15.586573
23.553995	829.223848	15.591591
23.571645	822.956360	15.596608
23.345123	824.974574	15.601626
23.373543	832.063716	15.606643
23.454972	823.448770	15.611661
23.135273	822.103049	15.616679
23.432979	824.015169	15.621696
23.404808	817.934395	15.626714
23.322492	830.395156	15.631731
23.570899	839.518641	15.636749
23.544318	852.725667	15.641767
23.625846	857.041588	15.646784
24.054271	847.077499	15.651802
24.152082	857.513667	15.656819
23.995442	848.573578	15.661837
24.052451	841.700773	15.666855
23.948935	839.697630	15.671872
24.139459	826.283349	15.676890
23.922234	816.128566	15.681907
23.815360	816.500669	15.686925
23.783780	827.390110	15.691943
23.981872	836.649479	15.696960
24.384102	841.167791	15.701978
24.258876	838.715508	15.706995
23.927712	822.832223	15.712013
23.832397	825.632610	15.717031
24.123562	851.655698	15.722048
24.449814	846.054784	15.727066
24.081845	847.965326	15.732083
24.184891	843.291882	15.737101
24.456851	846.882993	15.742119
23.975020	849.648177	15.747136
24.493848	850.762305	15.752154
23.991889	855.307906	15.757171
24.453137	848.739406	15.762189
24.032577	852.000327	15.767207
24.231777	850.486796	15.772224
24.061448	853.992096	15.777242
23.974201	853.822393	15.782259
24.290784	844.205550	15.787277
24.244793	851.882979	15.792295
24.256363	855.305407	15.797312
24.305608	843.763632	15.802330
24.215759	854.077728	15.807347
24.444962	869.486012	15.812365
24.992647	878.090695	15.817383
24.540880	877.899857	15.822400
24.547962	861.320395	15.827418
24.362060	874.541223	15.832435
24.470494	869.360995	15.837453
24.912914	870.899963	15.842471
24.854664	875.135101	15.847488
24.976375	867.548848	15.852506
24.861379	877.353367	15.857523
25.395425	867.379257	15.862541
25.051116	844.446479	15.867559
24.923970	851.762166	15.872576
24.855095	838.273510	15.877594
24.938256	840.914038	15.882611
24.750609	837.156012	15.887629
25.055822	835.354468	15.892647
24.706042	852.779774	15.897664
24.749441	833.184626	15.902682
24.938378	847.383077	15.907699
24.726810	854.500550	15.912717
25.017675	860.719121	15.917735
24.653322	866.402911	15.922752
25.342562	860.274979	15.927770
25.083451	867.154672	15.932787
25.058556	860.896181	15.937805
24.986445	867.148087	15.942823
25.346333	863.393875	15.947840
25.093808	864.444004	15.952858
24.946999	862.145284	15.957875
25.310577	863.647701	15.962893
25.213127	860.588875	15.967911
24.957598	875.762876	15.972928
25.350923	863.146835	15.977946
25.216272	870.504323	15.982963
25.338980	867.150391	15.987981
25.434553	860.080256	15.992999
25.042190	867.041460	15.998016
25.228405	853.934941	16.003034
25.637226	873.838082	16.008051
25.774211	877.887750	16.013069
25.716487	859.468710	16.018087
25.688053	864.635086	16.023104
25.689629	852.090614	16.028122
25.599076	864.746458	16.033139
25.567897	863.062814	16.038157
25.687011	857.177705	16.043175
25.123361	854.838958	16.048192
25.631409	871.174649	16.053210
25.511698	885.571480	16.058227
25.689434	894.246878	16.063245
25.622806	889.636946	16.068263
25.870324	898.516137	16.073280
26.070274	889.328798	16.078298
26.145037	891.294771	16.083315
25.978328	885.482962	16.088333
26.176689	887.319025	16.093351
26.100707	888.904858	16.098368
26.182818	888.031944	16.103386
26.057648	885.332805	16.108403
25.980340	873.611971	16.113421
26.356936	866.721668	16.118439
25.937135	861.806462	16.123456
26.196129	851.384227	16.128474
25.751430	863.771955	16.133491
25.764512	866.181189	16.138509
26.140665	872.724604	16.143527
26.202297	882.140447	16.148544
26.511610	869.824126	16.153562
26.353132	876.270250	16.158579
26.095551	878.438096	16.163597
26.117273	879.242824	16.168615
26.156312	882.367809	16.173632
26.138077	873.355577	16.178650
26.212616	876.139659	16.183667
26.375525	890.051134	16.188685
26.386409	879.995539	16.193703
26.007052	880.328908	16.198720
26.278820	880.068263	16.203738
26.451947	873.551003	16.208755
26.082903	886.337620	16.213773
26.501466	894.196404	16.218791
26.466183	905.431774	16.223808
26.732277	903.397735	16.228826
26.800893	909.890518	16.233843
26.512646	904.914539	16.238861
26.906645	903.725032	16.243879
26.548108	912.078232	16.248896
26.541879	904.817856	16.253914
26.599787	909.188094	16.258931
26.382386	913.014968	16.263949
26.878097	908.323334	16.268967
26.414478	911.723281	16.273984
26.527152	904.748716	16.279002
26.838508	905.291716	16.284019
26.579512	909.921113	16.289037
27.021766	908.687395	16.294055
27.068959	909.669002	16.299072
26.924610	906.831308	16.304090
26.968274	908.852431	16.309107
26.475529	911.073393	16.314125
27.424001	924.435156	16.319143
27.221290	935.519539	16.324160
27.253389	919.324832	16.329178
27.176876	907.516443	16.334195
27.053151	909.644807	16.339213
27.211150	899.887267	16.344231
27.119852	906.331334	16.349248
27.279694	908.936343	16.354266
27.294780	923.305771	16.359283
27.474310	932.457646	16.364301
27.865466	920.263948	16.369319
27.539962	898.664927	16.374336
27.326845	891.852182	16.379354
27.535807	888.476876	16.384371
27.229262	889.844599	16.389389
27.790907	883.214187	16.394407
27.954781	889.604185	16.399424
27.731157	893.284453	16.404442
27.955676	881.335691	16.409459
27.663823	892.669832	16.414477
27.879855	884.645923	16.419495
27.714218	888.535477	16.424512
27.576586	889.559890	16.429530
27.766604	883.936247	16.434547
27.687007	893.870737	16.439565
27.622357	885.783859	16.444583
27.488807	888.918921	16.449600
27.544469	891.747468	16.454618
27.495754	887.116855	16.459635
27.595249	889.581860	16.464653
27.498455	891.590019	16.469671
27.459396	895.621994	16.474688
27.882881	913.418520	16.479706
27.601451	913.108141	16.484723
27.761097	927.179239	16.489741
27.911323	916.435615	16.494759
28.079081	927.469671	16.499776
28.154608	917.110448	16.504794
27.935564	910.341981	16.509811
27.538658	918.114949	16.514829
27.679538	914.670206	16.519847
27.763773	921.430868	16.524864
27.963967	932.935916	16.529882
28.407020	940.229668	16.534899
28.283201	947.287380	16.539917
28.389281	933.712586	16.544935
28.244392	941.902478	16.549952
28.263152	939.058242	16.554970
28.668202	930.544369	16.559987
28.139876	934.498319	16.565005
28.619768	937.828260	16.570023
28.426974	931.012133	16.575040
28.292604	934.272530	16.580058
27.968099	929.824967	16.585075
28.204971	940.481068	16.590093
28.739925	928.190328	16.595111
28.799127	926.292114	16.600128
28.510736	927.432040	16.605146
28.711692	922.788027	16.610163
28.622184	936.411433	16.615181
28.391959	929.351514	16.620199
28.679680	925.027766	16.625216
28.731322	925.171270	16.630234
28.809523	929.108644	16.635251
28.613825	940.412332	16.640269
28.331647	930.704037	16.645287
28.887763	946.017717	16.650304
28.927559	951.506669	16.655322
29.150181	947.381481	16.660339
28.783360	938.124581	16.665357
29.097636	938.077754	16.670375
28.977522	930.426397	16.675392
29.041035	942.578468	16.680410
28.904418	936.160894	16.685427
28.824577	953.802628	16.690445
28.989199	946.136793	16.695463
29.033331	951.755730	16.700480
29.116955	947.636236	16.705498
29.346986	954.620400	16.710515
28.939302	956.222583	16.715533
29.127552	946.740702	16.720551
29.423560	955.707956	16.725568
29.310277	953.341863	16.730586
29.495991	952.647058	16.735603
29.241517	953.768378	16.740621
29.471875	947.813636	16.745639
29.611225	952.753055	16.750656
29.282504	951.500150	16.755674
29.860108	949.258231	16.760691
29.789250	961.265643	16.765709
29.975117	944.864747	16.770727
29.781964	951.034371	16.775744
29.453501	949.070036	16.780762
29.831850	949.586198	16.785779
29.535484	957.702759	16.790797
29.711323	951.070456	16.795815
29.723273	948.812755	16.800832
29.345353	953.180764	16.805850
29.882286	949.222814	16.810867
29.897407	949.819592	16.815885
29.844704	948.358786	16.820903
29.847350	959.720981	16.825920
29.667675	956.956447	16.830938
29.820856	947.800438	16.835955
29.532328	951.698546	16.840973
29.714484	950.492934	16.845991
29.663756	953.857985	16.851008
29.539968	957.516620	16.856026
29.866146	966.084018	16.861043
30.168742	969.379152	16.866061
30.387128	972.469735	16.871079
30.458578	981.532452	16.876096
29.996689	980.701580	16.881114
30.531946	968.436348	16.886131
30.465526	980.900109	16.891149
30.517218	955.442633	16.896167
30.520931	947.955403	16.901184
29.915335	942.299312	16.906202
30.392191	937.632838	16.911219
30.301082	957.188962	16.916237
30.156967	965.638965	16.921255
30.600055	966.667616	16.926272
30.164209	974.080537	16.931290
30.780753	965.970978	16.936307
30.520403	967.377907	16.941325
30.632340	967.107113	16.946343
30.556555	963.924211	16.951360
30.678099	969.678756	16.956378
30.712052	968.865385	16.961395
30.730765	974.708216	16.966413
30.861695	967.358960	16.971431
30.612967	965.514485	16.976448
30.403113	965.079266	16.981466
30.653935	956.679495	16.986483
30.859789	965.836479	16.991501
30.824266	974.403540	16.996519
30.895166	961.643177	17.001536
30.858955	968.539941	17.006554
30.845513	961.519306	17.011571
30.909904	965.162531	17.016589
30.996649	963.812880	17.021607
31.036592	964.134299	17.026624
30.724182	977.251757	17.031642
30.984160	959.286665	17.036659
30.982326	953.503433	17.041677
31.045077	965.057640	17.046695
31.098390	954.055639	17.051712
31.059564	969.221407	17.056730
31.188126	988.273892	17.061747
31.458674	987.481184	17.066765
31.382150	996.584947	17.071783
31.804785	984.891479	17.076800
30.940777	981.631616	17.081818
31.280864	977.105489	17.086835
31.133483	993.215598	17.091853
31.378403	994.716811	17.096871
31.573775	984.338880	17.101888
31.345130	992.907614	17.106906
31.642790	993.793818	17.111923
31.617186	985.894510	17.116941
31.240055	986.668046	17.121959
31.661069	987.321628	17.126976
31.449405	991.540076	17.131994
31.324754	996.982655	17.137011
31.684320	985.122078	17.142029
31.408066	989.244138	17.147047
31.726793	998.895031	17.152064
31.936360	1004.183850	17.157082
32.104505	1004.586007	17.162099
32.376490	999.702659	17.167117
32.067705	998.548808	17.172135
31.851188	978.530388	17.177152
31.811311	981.886956	17.182170
31.992905	978.983468	17.187187
31.925668	987.258948	17.192205
31.740953	1003.934284	17.197223
32.189343	1007.304494	17.202240
32.247044	1014.384934	17.207258
32.422015	1002.211221	17.212275
32.531156	1005.381708	17.217293
32.144176	995.545849	17.222311
32.755771	1005.315963	17.227328
32.580509	989.639358	17.232346
32.297662	974.233724	17.237363
32.455101	969.159518	17.242381
32.460628	977.112719	17.247399
32.350445	969.567569	17.252416
32.197822	973.356961	17.257434
32.677602	977.829799	17.262451
32.721336	978.630887	17.267469
32.390014	976.841817	17.272487
32.465494	975.489700	17.277504
32.536736	990.931741	17.282522
32.451836	991.984830	17.287539
32.485867	1001.742312	17.292557
32.083243	998.858787	17.297575
32.584757	999.598643	17.302592
32.536902	1011.054274	17.307610
32.602326	1001.805681	17.312627
32.795771	991.795373	17.317645
32.566577	998.961892	17.322663
32.867653	1001.694313	17.327680
32.686619	1007.685582	17.332698
32.957796	1015.196012	17.337715
33.129228	1023.543799	17.342733
33.230031	1038.071182	17.347751
33.452995	1012.693516	17.352768
33.020556	1005.520988	17.357786
33.324434	988.534384	17.362803
33.237452	990.507861	17.367821
33.095787	993.967110	17.372839
33.348389	986.224484	17.377856
33.212251	988.329718	17.382874
33.124965	990.125300	17.387891
33.209559	1007.354843	17.392909
33.265422	1023.441566	17.397927
33.871484	1021.179178	17.402944
33.465980	1021.696006	17.407962
33.491274	1024.589052	17.412979
33.804317	1011.427936	17.417997
33.459721	1006.772267	17.423015
33.441343	991.913747	17.428032
33.365398	1000.139890	17.433050
33.333890	1013.949816	17.438067
33.516006	1018.235741	17.443085
33.030759	1018.002020	17.448103
33.417699	1026.733401	17.453120
33.101426	1031.336491	17.458138
33.657294	1033.807446	17.463155
33.570992	1040.654271	17.468173
33.420277	1058.462579	17.473191
33.956199	1051.110396	17.478208
33.918449	1051.882068	17.483226
34.175040	1049.746044	17.488243
34.506898	1043.018973	17.493261
34.052765	1052.437253	17.498279
34.394473	1040.039452	17.503296
34.217842	1044.941854	17.508314
34.177823	1043.885224	17.513331
34.444008	1030.723977	17.518349
34.446931	1048.206451	17.523367
34.005477	1021.184515	17.528384
34.403257	1024.024152	17.533402
34.107503	1027.372313	17.538419
34.736063	1036.019599	17.543437
34.424471	1029.378605	17.548455
34.647969	1013.086756	17.553472
34.443943	1012.110432	17.558490
34.450403	1007.002947	17.563507
34.797546	1001.209549	17.568525
34.666978	1007.796376	17.573543
34.722359	1010.256108	17.578560
34.536437	1005.461964	17.583578
34.573890	1007.641997	17.588595
34.493887	1003.508638	17.593613
34.803405	1009.251364	17.598631
34.721640	1009.063428	17.603648
34.643649	1014.007360	17.608666
34.380166	1008.185938	17.613683
34.806676	1021.265331	17.618701
34.655521	1027.772114	17.623719
35.241770	1036.869304	17.628736
35.012477	1045.137791	17.633754
34.889385	1050.288407	17.638771
35.169994	1036.812573	17.643789
34.923748	1045.717703	17.648807
34.688831	1034.426767	17.653824
34.787645	1040.641387	17.658842
35.071091	1043.288155	17.663859
35.079540	1035.965840	17.668877
35.182579	1037.535432	17.673895
34.997213	1030.462134	17.678912
34.792714	1026.211592	17.683930
34.405451	1041.367805	17.688947
34.683839	1050.402597	17.693965
34.612163	1067.954530	17.698983
35.820747	1056.472592	17.704000
35.486642	1072.931014	17.709018
35.338931	1066.400659	17.714035
35.855469	1062.420468	17.719053
35.483421	1071.911387	17.724071
35.370742	1061.762752	17.729088
35.538953	1070.207551	17.734106
35.418355	1063.760106	17.739123
35.730005	1062.127545	17.744141
35.469662	1074.521921	17.749159
35.842200	1076.044924	17.754176
35.830724	1082.477028	17.759194
35.869262	1087.162325	17.764211
36.314286	1088.789071	17.769229
35.914858	1076.262392	17.774247
35.934641	1068.201201	17.779264
35.944581	1060.532969	17.784282
35.516530	1063.295190	17.789299
35.862802	1074.939143	17.794317
35.760909	1086.260868	17.799335
35.971988	1083.363895	17.804352
35.972721	1096.028434	17.809370
35.975273	1089.503109	17.814387
36.216481	1089.618770	17.819405
35.834582	1094.409118	17.824423
36.106004	1089.589219	17.829440
36.386545	1098.237474	17.834458
36.201088	1103.744881	17.839475
36.585377	1102.623107	17.844493
36.637458	1109.444687	17.849511
36.649322	1101.097003	17.854528
36.801658	1089.560415	17.859546
36.736203	1078.380359	17.864563
36.455001	1070.682380	17.869581
36.450830	1078.491575	17.874599
36.696104	1075.159822	17.879616
36.774224	1067.577932	17.884634
36.557403	1078.006900	17.889651
36.883001	1083.802502	17.894669
36.768787	1088.424118	17.899687
36.777383	1098.908292	17.904704
37.069909	1102.162210	17.909722
36.943727	1104.972877	17.914739
37.192416	1096.785976	17.919757
36.987096	1083.884246	17.924775
37.358958	1073.512857	17.929792
37.147318	1064.762452	17.934810
36.946685	1070.606601	17.939827
37.033427	1072.139525	17.944845
37.111634	1075.913555	17.949863
36.877889	1072.893789	17.954880
37.148819	1081.745194	17.959898
37.060100	1091.454950	17.964915
37.101318	1099.259396	17.969933
37.166909	1099.333272	17.974951
37.194550	1100.904331	17.979968
37.817452	1094.209752	17.984986
37.661090	1108.443180	17.990003
37.670019	1096.404756	17.995021
37.695630	1105.200342	18.000039
37.285214	1105.645940	18.005056
37.721285	1094.198977	18.010074
37.382550	1107.297282	18.015091
37.738245	1094.617602	18.020109
37.530736	1100.188105	18.025127
37.867172	1099.299840	18.030144
37.828129	1094.529772	18.035162
37.964084	1094.093587	18.040179
37.758355	1096.009183	18.045197
37.493111	1099.550332	18.050215
37.623371	1102.317749	18.055232
37.916234	1089.586667	18.060250
37.969238	1094.373505	18.065267
37.734721	1094.595495	18.070285
37.901015	1091.270123	18.075303
37.630988	1098.387939	18.080320
37.875244	1110.960594	18.085338
37.894590	1126.216093	18.090355
38.347390	1118.622138	18.095373
38.433873	1126.612011	18.100391
38.475541	1122.247456	18.105408
38.420903	1124.991950	18.110426
38.266632	1117.707169	18.115443
38.523469	1119.196580	18.120461
38.422819	1124.006507	18.125479
38.507985	1113.247930	18.130496
38.706986	1109.509671	18.135514
38.232618	1125.956729	18.140531
38.658653	1107.541935	18.145549
38.856774	1119.495483	18.150567
38.503023	1109.550114	18.155584
38.409528	1109.741668	18.160602
38.397040	1113.718907	18.165619
38.720493	1105.219238	18.170637
38.547467	1113.428446	18.175655
38.592294	1133.954776	18.180672
38.927165	1136.077312	18.185690
38.487694	1148.152991	18.190707
38.718738	1140.698890	18.195725
38.715444	1147.179665	18.200743
38.826190	1152.072705	18.205760
38.805047	1139.645537	18.210778
38.792435	1144.608605	18.215795
39.143653	1150.045669	18.220813
39.262910	1151.775968	18.225831
39.331268	1160.582223	18.230848
39.876089	1149.187683	18.235866
39.637971	1136.673220	18.240883
39.614318	1126.773573	18.245901
39.764331	1125.143755	18.250919
39.449085	1121.951652	18.255936
39.864340	1117.321309	18.260954
39.687307	1123.781237	18.265971
39.790035	1122.792695	18.270989
39.924063	1120.172245	18.276007
39.838902	1122.254490	18.281024
40.101707	1113.429434	18.286042
39.816197	1128.524004	18.291059
39.784815	1119.007127	18.296077
39.865357	1115.734924	18.301095
39.988917	1116.370838	18.306112
39.963256	1100.419356	18.311130
39.557324	1098.690655	18.316147
39.831876	1100.625543	18.321165
39.847799	1116.122537	18.326183
39.615898	1123.546640	18.331200
39.645813	1115.929403	18.336218
39.751603	1116.684792	18.341235
39.475761	1118.887582	18.346253
39.488071	1128.690079	18.351271
39.812235	1146.082072	18.356288
40.052081	1148.428213	18.361306
39.938929	1154.467745	18.366323
39.839659	1152.079616	18.371341
39.997939	1155.953790	18.376359
40.160661	1172.402097	18.381376
40.288343	1173.812902	18.386394
40.543706	1189.188829	18.391411
40.436776	1183.726054	18.396429
40.748458	1185.568587	18.401447
40.749059	1182.000165	18.406464
40.837880	1177.991951	18.411482
40.958022	1184.605449	18.416499
40.826093	1180.482609	18.421517
40.840112	1177.326130	18.426535
40.617721	1173.210397	18.431552
41.155208	1167.349595	18.436570
40.895188	1173.179207	18.441587
41.201708	1173.749396	18.446605
41.093033	1169.335315	18.451623
41.263498	1174.852709	18.456640
41.340539	1166.515063	18.461658
40.801833	1149.280407	18.466675
40.965271	1164.325870	18.471693
41.418311	1167.709521	18.476711
40.739584	1178.342593	18.481728
40.830057	1169.596827	18.486746
41.260395	1166.531255	18.491763
40.902902	1170.703427	18.496781
41.110083	1161.914325	18.501799
41.225927	1174.401999	18.506816
41.529540	1174.751022	18.511834
41.416978	1180.693619	18.516851
41.486244	1200.729782	18.521869
41.617136	1190.258849	18.526887
41.790573	1191.592002	18.531904
42.163049	1195.464577	18.536922
42.048902	1188.170757	18.541939
41.078651	1171.094538	18.546957
41.828715	1176.938393	18.551975
41.504074	1190.208839	18.556992
41.825380	1189.758890	18.562010
42.193151	1201.078521	18.567027
42.047076	1198.602861	18.572045
42.347914	1200.446009	18.577063
42.022569	1190.049832	18.582080
42.302687	1189.940947	18.587098
42.208021	1197.168350	18.592115
42.236051	1187.780566	18.597133
42.516929	1190.189209	18.602151
42.342877	1204.892966	18.607168
42.287192	1182.096535	18.612186
42.130414	1180.041537	18.617203
42.016992	1191.116041	18.622221
42.318821	1198.158899	18.627239
42.508731	1200.701501	18.632256
42.410809	1193.077047	18.637274
42.430400	1191.370395	18.642291
42.397192	1189.565007	18.647309
42.519465	1180.347446	18.652327
42.187869	1193.782034	18.657344
42.334844	1190.215752	18.662362
42.134490	1195.150081	18.667379
42.495084	1210.484590	18.672397
42.676937	1214.065512	18.677415
42.773966	1225.704787	18.682432
42.948615	1226.639327	18.687450
42.866968	1218.767683	18.692467
42.473155	1226.908786	18.697485
42.887165	1218.750352	18.702503
42.781570	1217.645908	18.707520
42.802078	1215.347776	18.712538
42.832325	1220.311645	18.717555
43.042161	1233.351113	18.722573
43.306049	1228.476515	18.727591
43.048334	1232.722732	18.732608
43.130952	1232.849299	18.737626
43.399231	1243.020893	18.742643
43.677587	1233.616436	18.747661
43.813450	1233.965678	18.752679
43.596871	1226.462428	18.757696
43.639327	1230.161315	18.762714
43.628249	1230.724647	18.767731
43.714031	1234.833281	18.772749
43.934339	1229.455280	18.777767
43.779052	1239.021036	18.782784
43.682302	1229.140514	18.787802
43.851098	1225.542658	18.792819
43.586403	1224.726362	18.797837
44.037435	1223.025826	18.802855
44.113634	1226.337243	18.807872
44.207570	1227.664666	18.812890
44.322067	1226.400159	18.817907
44.086224	1224.470449	18.822925
44.245047	1210.135516	18.827943
43.797309	1224.346037	18.832960
44.251347	1220.962757	18.837978
43.997535	1216.740012	18.842995
44.133980	1220.993007	18.848013
44.225966	1219.213736	18.853031
44.261434	1217.224143	18.858048
44.041144	1215.662716	18.863066
44.251468	1220.146385	18.868083
44.181660	1230.555837	18.873101
44.796619	1240.081457	18.878119
44.417289	1249.885886	18.883136
44.554100	1251.670770	18.888154
45.046457	1244.002489	18.893171
44.897525	1249.839719	18.898189
44.766002	1240.789733	18.903207
44.767604	1249.107496	18.908224
44.628356	1236.123834	18.913242
44.750082	1236.832497	18.918259
44.869427	1250.720409	18.923277
45.187791	1246.439136	18.928295
45.050946	1237.315625	18.933312
45.059925	1237.008332	18.938330
45.071049	1238.237659	18.943347
44.739220	1249.147192	18.948365
45.104963	1238.020424	18.953383
45.127336	1248.053214	18.958400
44.859726	1250.374736	18.963418
44.923560	1253.275224	18.968435
45.091223	1272.298358	18.973453
45.214181	1260.607848	18.978471
45.311021	1276.206563	18.983488
45.259863	1283.726010	18.988506
45.831099	1267.599934	18.993523
45.533264	1272.315393	18.998541
45.908429	1275.475352	19.003559
45.620015	1284.425790	19.008576
45.758887	1280.056906	19.013594
46.124915	1272.490236	19.018611
45.523618	1275.712666	19.023629
45.618451	1265.152773	19.028647
45.405461	1280.130759	19.033664
45.488901	1276.779697	19.038682
45.883019	1286.486792	19.043699
45.436075	1299.168144	19.048717
45.834963	1296.062085	19.053735
45.909958	1291.944322	19.058752
46.533091	1297.871446	19.063770
46.332915	1290.082382	19.068787
46.184080	1301.515972	19.073805
46.546300	1293.018837	19.078823
46.372465	1293.984704	19.083840
46.326960	1294.695075	19.088858
46.619800	1298.934794	19.093875
46.788495	1291.664170	19.098893
47.069816	1283.042248	19.103911
46.899834	1292.688815	19.108928
46.728117	1282.786420	19.113946
46.926320	1282.983218	19.118963
46.673509	1294.790312	19.123981
46.751175	1279.445936	19.128999
46.756806	1283.892258	19.134016
47.031939	1286.560524	19.139034
47.200813	1271.519946	19.144051
47.269543	1290.938217	19.149069
47.323968	1287.671484	19.154087
47.256384	1284.976124	19.159104
47.163459	1283.338091	19.164122
47.053854	1277.934386	19.169139
46.994229	1284.560764	19.174157
47.003435	1277.048450	19.179175
47.237801	1272.076760	19.184192
47.158965	1273.186342	19.189210
47.236875	1280.927719	19.194227
46.856580	1276.390080	19.199245
47.017598	1280.591385	19.204263
47.314093	1285.039940	19.209280
47.245966	1297.368020	19.214298
47.747190	1303.559815	19.219315
47.472115	1303.144833	19.224333
47.507440	1307.596481	19.229351
47.796674	1305.974694	19.234368
47.684451	1311.557449	19.239386
47.813086	1302.119080	19.244403
47.624372	1302.650017	19.249421
47.648099	1301.698167	19.254439
48.019684	1317.150252	19.259456
47.679575	1336.927216	19.264474
47.989896	1331.596480	19.269491
48.003392	1338.966273	19.274509
48.149451	1328.498641	19.279527
48.131400	1338.670465	19.284544
48.301238	1343.232920	19.289562
48.444632	1330.101988	19.294579
48.349715	1336.428330	19.299597
48.234369	1333.019228	19.304615
48.627233	1332.828289	19.309632
48.483670	1342.015795	19.314650
48.935340	1326.122051	19.319667
48.816788	1336.666415	19.324685
48.617862	1332.723128	19.329703
48.540806	1332.092289	19.334720
48.128512	1335.344852	19.339738
48.605177	1339.340762	19.344755
48.511613	1329.575788	19.349773
48.780815	1339.957132	19.354791
48.886094	1356.972621	19.359808
48.883888	1358.136055	19.364826
49.172061	1355.251464	19.369843
48.987946	1366.204730	19.374861
49.020487	1356.366497	19.379879
49.464745	1349.632100	19.384896
49.021241	1365.544387	19.389914
49.269487	1362.362866	19.394931
48.864468	1352.037645	19.399949
49.278067	1358.247121	19.404967
49.254366	1355.757865	19.409984
49.310215	1364.695834	19.415002
49.308038	1349.699644	19.420019
49.792158	1369.690170	19.425037
49.534021	1371.847545	19.430055
50.092513	1368.030803	19.435072
50.016322	1374.863896	19.440090
49.964544	1360.663693	19.445107
49.862373	1352.290268	19.450125
49.761229	1353.690554	19.455143
49.570391	1349.138846	19.460160
49.795769	1360.503431	19.465178
50.133215	1371.522701	19.470195
49.975632	1374.027202	19.475213
50.211997	1380.392803	19.480231
50.375504	1377.159957	19.485248
50.219813	1378.872028	19.490266
50.516229	1373.235316	19.495283
50.187074	1373.375736	19.500301
50.272894	1371.369519	19.505319
50.491867	1377.121077	19.510336
50.504438	1383.178856	19.515354
50.693842	1364.324205	19.520371
50.635676	1369.854329	19.525389
50.463455	1372.358103	19.530407
50.536225	1366.508822	19.535424
50.193985	1373.389903	19.540442
50.404724	1371.673234	19.545459
50.628746	1371.051596	19.550477
50.909935	1380.988076	19.555495
50.869055	1386.177159	19.560512
50.704554	1391.344194	19.565530
50.968542	1388.249431	19.570547
51.225970	1392.064335	19.575565
51.106401	1396.806614	19.580583
51.376670	1384.994376	19.585600
51.339737	1394.574095	19.590618
51.254758	1388.075342	19.595635
51.620164	1398.860871	19.600653
51.414062	1376.904798	19.605671
51.730473	1377.674931	19.610688
51.547765	1395.267666	19.615706
51.648508	1384.692934	19.620723
51.476953	1381.239191	19.625741
51.517605	1385.599823	19.630759
51.805931	1382.970318	19.635776
51.516254	1381.531385	19.640794
51.703808	1372.660769	19.645811
52.033860	1376.220735	19.650829
51.637723	1382.265873	19.655847
51.831159	1377.248566	19.660864
51.615973	1385.969616	19.665882
51.955631	1375.134074	19.670899
51.706822	1381.344579	19.675917
51.674041	1387.026016	19.680935
52.029702	1392.154167	19.685952
52.021777	1409.800655	19.690970
52.300805	1404.027443	19.695987
52.391870	1410.510421	19.701005
52.212944	1413.596408	19.706023
52.317178	1406.508056	19.711040
52.240331	1415.292043	19.716058
52.525074	1413.783192	19.721075
52.746614	1412.938738	19.726093
52.306159	1412.729873	19.731111
52.461547	1412.865260	19.736128
52.393932	1406.224255	19.741146
52.660645	1420.706024	19.746163
52.888835	1436.112287	19.751181
53.006260	1443.664527	19.756199
53.277337	1429.038366	19.761216
52.867861	1431.992059	19.766234
52.944090	1435.424382	19.771251
53.026297	1430.915234	19.776269
52.752931	1434.280246	19.781287
52.935566	1437.013855	19.786304
52.945809	1430.642623	19.791322
52.879090	1434.132078	19.796339
53.123233	1447.388486	19.801357
52.898311	1457.455666	19.806375
53.621255	1453.408527	19.811392
53.386721	1462.559592	19.816410
53.645923	1468.478931	19.821427
53.779338	1457.867244	19.826445
53.774597	1464.466894	19.831463
53.897242	1448.313728	19.836480
53.570931	1460.411461	19.841498
53.920709	1451.959606	19.846515
53.859167	1461.805644	19.851533
53.984162	1451.666611	19.856551
54.149746	1448.801908	19.861568
54.062978	1460.328880	19.866586
54.015857	1457.420261	19.871603
54.009218	1446.949486	19.876621
54.228111	1467.031299	19.881639
54.383548	1467.415101	19.886656
54.527496	1477.865309	19.891674
54.295134	1475.425545	19.896691
54.586659	1473.540765	19.901709
54.620286	1476.418737	19.906727
54.826146	1457.848648	19.911744
55.004559	1470.810843	19.916762
54.711783	1464.007097	19.921779
54.546050	1467.683819	19.926797
54.720884	1473.783665	19.931815
54.903565	1468.470867	19.936832
54.741478	1467.261979	19.941850
55.046252	1470.833632	19.946867
54.786522	1469.490519	19.951885
54.637940	1466.488856	19.956903
54.898515	1461.394264	19.961920
54.760128	1468.474703	19.966938
54.749079	1464.846335	19.971955
55.311245	1481.656390	19.976973
54.969357	1489.108327	19.981991
55.232871	1501.262367	19.987008
55.388607	1497.524092	19.992026
55.156762	1503.714121	19.997043
55.362622	1500.302978	20.002061
54.984771	1508.947881	20.007079
55.418723	1499.980097	20.012096
55.198553	1511.778407	20.017114
55.674348	1512.335938	20.022131
55.685206	1519.075154	20.027149
55.795380	1524.054233	20.032167
55.948914	1522.215918	20.037184
56.040592	1518.517379	20.042202
56.162477	1521.869721	20.047219
56.017434	1513.502520	20.052237
56.317788	1524.574892	20.057255
56.553110	1509.715206	20.062272
56.353237	1515.651127	20.067290
56.299782	1518.189984	20.072307
56.126141	1510.548776	20.077325
55.909082	1517.791082	20.082343
56.258611	1510.841988	20.087360
56.464755	1509.076066	20.092378
56.434860	1520.118471	20.097395
56.382655	1511.508340	20.102413
56.684195	1528.602938	20.107431
57.066193	1536.925194	20.112448
57.037352	1535.360381	20.117466
56.896963	1535.260491	20.122483
56.659809	1519.812099	20.127501
56.981492	1531.278974	20.132519
57.273452	1541.348814	20.137536
57.318430	1539.315873	20.142554
56.913542	1542.006229	20.147571
57.188883	1550.766231	20.152589
56.984006	1544.974271	20.157607
57.086471	1546.953852	20.162624
57.356845	1542.815877	20.167642
57.256037	1539.870462	20.172659
57.514874	1536.138336	20.177677
57.208847	1533.448949	20.182695
57.052647	1526.667836	20.187712
57.455960	1539.238127	20.192730
57.343236	1552.272218	20.197747
57.752460	1560.833680	20.202765
57.505491	1555.627032	20.207783
57.703002	1548.593642	20.212800
57.970098	1550.380611	20.217818
57.842732	1555.441551	20.222835
57.807326	1543.556971	20.227853
58.032661	1565.376031	20.232871
58.146145	1574.915208	20.237888
58.540975	1577.523550	20.242906
58.329105	1583.761089	20.247923
58.364417	1580.257302	20.252941
58.511177	1581.985458	20.257959
58.608871	1579.865831	20.262976
58.518564	1576.963946	20.267994
58.480122	1575.265285	20.273011
58.795119	1573.730939	20.278029
58.699086	1567.059531	20.283047
58.857749	1565.432173	20.288064
58.934373	1563.803044	20.293082
58.803264	1564.798861	20.298099
59.172274	1566.798091	20.303117
58.645976	1560.993990	20.308135
58.670719	1567.439590	20.313152
58.810058	1559.986694	20.318170
58.792210	1564.744070	20.323187
59.225407	1564.274799	20.328205
58.937983	1576.158703	20.333223
59.318677	1587.104432	20.338240
59.529969	1590.310489	20.343258
59.652263	1601.502556	20.348275
59.318928	1591.194438	20.353293
59.444176	1597.113566	20.358311
59.363232	1592.631779	20.363328
59.488585	1598.869395	20.368346
59.360162	1592.124599	20.373363
59.598476	1588.378141	20.378381
59.736992	1599.086418	20.383399
59.535179	1592.797082	20.388416
59.888784	1595.479182	20.393434
59.772231	1619.259260	20.398451
59.927873	1618.382005	20.403469
60.060898	1625.283324	20.408487
60.183466	1618.988298	20.413504
60.312729	1620.419749	20.418522
60.232685	1623.510271	20.423539
60.554647	1618.288928	20.428557
60.682324	1607.284387	20.433575
60.580531	1610.774571	20.438592
61.108935	1609.515124	20.443610
60.659770	1606.672651	20.448627
60.904376	1613.340922	20.453645
60.693841	1614.360523	20.458663
60.761344	1611.071084	20.463680
60.965465	1604.081851	20.468698
61.117848	1615.325246	20.473715
60.988764	1611.335284	20.478733
60.856143	1611.587257	20.483751
61.091594	1611.861752	20.488768
61.102941	1605.893416	20.493786
61.185759	1611.794378	20.498803
60.917362	1606.015275	20.503821
61.042487	1618.186022	20.508839
60.851688	1630.949641	20.513856
61.331314	1628.918344	20.518874
61.126768	1635.860600	20.523891
61.475009	1642.049517	20.528909
61.527188	1635.490942	20.533927
61.495245	1629.528977	20.538944
61.643131	1637.851862	20.543962
61.749601	1648.607606	20.548979
62.066741	1658.995008	20.553997
62.220850	1659.007380	20.559015
62.001463	1660.349318	20.564032
62.332892	1653.236227	20.569050
62.134023	1654.290120	20.574067
62.342269	1647.116326	20.579085
62.272841	1643.056635	20.584103
62.123483	1657.975629	20.589120
62.547835	1650.016442	20.594138
62.342924	1654.000090	20.599155
62.503018	1649.572471	20.604173
62.773091	1649.253436	20.609191
62.493437	1653.665210	20.614208
62.649633	1655.142599	20.619226
62.224063	1647.023349	20.624243
62.345129	1649.388448	20.629261
62.610793	1670.429715	20.634279
62.819188	1671.010268	20.639296
63.135144	1673.460425	20.644314
62.991705	1675.581527	20.649331
63.044962	1683.507110	20.654349
63.168173	1673.845002	20.659367
63.288829	1681.141310	20.664384
63.463921	1670.904863	20.669402
63.277495	1677.038620	20.674419
63.166504	1677.548038	20.679437
63.279424	1666.564796	20.684455
63.196319	1678.918888	20.689472
63.688480	1696.042740	20.694490
63.686486	1701.512106	20.699507
63.958487	1705.615624	20.704525
63.821971	1706.819433	20.709543
63.775734	1709.109879	20.714560
63.918456	1704.356772	20.719578
63.902923	1709.115384	20.724595
63.905789	1704.029132	20.729613
64.302083	1703.323446	20.734631
64.090079	1708.155927	20.739648
64.425009	1702.607210	20.744666
64.503373	1705.204586	20.749683
64.445816	1709.487475	20.754701
64.323613	1700.334494	20.759719
64.416847	1707.370392	20.764736
64.583817	1701.463261	20.769754
64.154037	1702.268773	20.774771
64.371934	1698.029209	20.779789
64.581255	1710.614438	20.784807
64.880179	1717.172972	20.789824
64.682827	1731.081863	20.794842
64.686493	1736.432587	20.799859
64.488805	1732.022452	20.804877
65.150525	1724.588497	20.809895
64.771157	1731.190447	20.814912
65.034155	1735.373416	20.819930
64.867491	1746.350438	20.824947
65.273004	1749.712168	20.829965
65.242393	1749.868512	20.834983
65.447260	1753.885519	20.840000
65.431818	1744.303019	20.845018
65.854245	1750.124969	20.850035
65.454920	1742.281248	20.855053
65.815996	1741.962105	20.860071
65.790891	1741.276977	20.865088
66.103160	1740.863551	20.870106
66.090983	1744.846807	20.875123
66.117844	1745.214110	20.880141
66.198937	1747.349226	20.885159
65.940806	1749.301136	20.890176
66.557609	1749.770369	20.895194
66.135758	1744.617416	20.900211
66.396484	1759.747746	20.905229
66.533934	1765.377513	20.910247
66.268052	1765.987384	20.915264
66.422483	1768.389891	20.920282
66.946785	1781.033262	20.925299
66.845030	1774.246963	20.930317
66.578264	1765.982457	20.935335
66.631129	1766.366322	20.940352
66.877685	1763.869262	20.945370
66.717085	1766.772360	20.950387
66.760198	1760.866816	20.955405
67.096505	1762.654162	20.960423
66.837678	1763.743973	20.965440
67.121940	1771.140402	20.970458
67.092992	1789.842391	20.975475
67.112655	1793.934169	20.980493
67.371349	1793.154017	20.985511
67.325116	1795.756291	20.990528
67.265163	1789.783941	20.995546
67.403662	1789.837875	21.000563
67.164246	1792.793005	21.005581
67.154404	1794.355380	21.010599
67.491759	1813.225492	21.015616
68.068928	1806.413382	21.020634
68.349644	1810.567848	21.025651
68.440340	1810.442686	21.030669
68.441270	1808.290624	21.035687
68.064005	1815.684792	21.040704
67.980802	1799.298804	21.045722
68.231791	1809.876398	21.050739
68.432389	1809.036572	21.055757
68.538692	1806.009963	21.060775
68.578332	1807.122014	21.065792
68.584714	1804.049350	21.070810
68.552051	1807.792704	21.075827
68.517785	1805.668517	21.080845
68.613149	1799.108234	21.085863
68.556657	1797.146392	21.090880
68.460427	1803.850312	21.095898
68.870541	1803.604940	21.100915
68.387297	1811.193821	21.105933
69.103059	1818.766863	21.110951
69.181812	1828.119030	21.115968
68.977544	1825.053287	21.120986
69.415971	1825.475285	21.126003
69.364819	1827.711050	21.131021
69.248044	1825.487921	21.136039
69.431694	1827.507640	21.141056
69.815919	1822.765693	21.146074
69.599771	1817.910551	21.151091
69.269313	1825.234768	21.156109
69.587346	1822.481765	21.161127
69.490317	1831.831543	21.166144
69.987696	1847.301522	21.171162
69.990089	1857.134468	21.176179
69.950851	1846.744019	21.181197
70.134920	1850.523152	21.186215
70.097616	1862.735159	21.191232
70.239055	1850.837205	21.196250
70.156519	1849.876537	21.201267
70.511405	1853.684870	21.206285
70.674512	1842.947922	21.211303
70.690475	1851.050241	21.216320
70.455755	1843.373706	21.221338
70.480428	1837.960170	21.226355
70.477426	1842.403357	21.231373
71.112279	1860.870720	21.236391
70.949544	1874.183445	21.241408
70.957532	1872.348716	21.246426
71.035085	1882.723575	21.251443
70.830809	1879.346005	21.256461
70.892406	1873.362947	21.261479
71.119560	1883.516577	21.266496
70.722017	1874.708694	21.271514
71.056378	1872.434879	21.276531
71.267365	1881.390767	21.281549
72.162341	1891.769663	21.286567
71.613156	1899.834869	21.291584
71.464595	1890.076678	21.296602
71.613556	1888.325693	21.301619
71.646168	1881.736001	21.306637
71.959065	1889.803744	21.311655
72.046823	1892.855905	21.316672
71.767059	1883.366691	21.321690
71.847013	1891.221817	21.326707
71.750420	1885.227150	21.331725
72.385898	1880.094366	21.336743
72.355597	1891.109936	21.341760
72.198772	1905.520551	21.346778
72.099473	1913.839235	21.351795
72.173234	1924.534049	21.356813
72.642376	1916.414158	21.361831
72.657910	1913.677366	21.366848
72.554174	1919.142788	21.371866
72.944574	1907.130734	21.376883
72.476676	1911.878085	21.381901
72.835791	1914.072705	21.386919
72.535883	1921.219464	21.391936
73.102790	1924.874991	21.396954
73.097524	1935.939992	21.401971
72.768582	1937.446945	21.406989
73.375123	1941.373086	21.412007
73.147908	1935.564991	21.417024
73.384732	1939.051153	21.422042
73.376697	1935.321386	21.427059
73.352805	1933.115541	21.432077
73.431770	1926.192163	21.437095
73.680977	1949.375954	21.442112
73.776999	1965.761345	21.447130
74.025956	1956.451874	21.452147
74.231230	1961.941346	21.457165
74.651943	1949.806127	21.462183
74.801332	1935.444134	21.467200
74.389844	1922.696707	21.472218
74.580499	1914.909547	21.477235
74.007999	1918.873020	21.482253
74.398483	1921.259697	21.487271
74.349556	1916.929998	21.492288
74.361289	1917.878563	21.497306
74.815531	1938.884642	21.502323
74.904201	1954.599963	21.507341
74.969593	1945.263017	21.512359
74.774451	1944.636349	21.517376
74.894185	1942.809093	21.522394
75.309250	1942.267224	21.527411
74.970477	1947.172738	21.532429
75.039501	1943.662105	21.537447
74.960998	1949.833613	21.542464
75.054485	1945.005512	21.547482
75.173456	1937.471554	21.552499
74.757761	1942.907532	21.557517
75.416636	1952.132225	21.562535
75.559961	1960.204459	21.567552
75.318665	1969.341979	21.572570
75.408622	1964.596742	21.577587
75.488799	1975.308245	21.582605
75.718674	1972.252483	21.587623
75.988097	1985.716590	21.592640
76.070596	2005.039380	21.597658
76.427534	1985.649530	21.602675
76.225840	1997.180968	21.607693
76.282851	1989.531256	21.612711
76.195867	1988.443359	21.617728
76.362200	1998.520125	21.622746
76.498292	1990.262421	21.627763
76.109320	2000.206321	21.632781
76.724181	1984.045119	21.637799
76.478676	2002.111548	21.642816
76.630820	1996.822526	21.647834
76.777095	2008.884170	21.652851
76.929454	2024.654373	21.657869
77.381066	2023.483991	21.662887
77.430470	2023.050301	21.667904
77.649049	2018.920384	21.672922
77.434835	2010.161992	21.677939
77.464631	2013.266296	21.682957
77.633210	2008.929693	21.687975
77.872891	2010.969688	21.692992
77.201802	2003.587376	21.698010
77.464354	2002.252624	21.703027
77.653903	2016.413861	21.708045
77.623695	2009.573091	21.713063
77.640162	2010.051967	21.718080
77.723590	2016.477013	21.723098
77.985539	2006.801178	21.728115
77.750851	2015.178161	21.733133
77.671532	2013.167313	21.738151
78.052774	2029.251603	21.743168
77.743235	2043.476207	21.748186
78.060031	2042.302554	21.753203
78.237689	2042.084644	21.758221
78.182113	2045.753105	21.763239
78.474136	2046.047772	21.768256
78.687459	2062.650071	21.773274
78.864713	2069.429301	21.778291
79.018368	2065.683756	21.783309
78.788588	2069.175548	21.788327
78.771642	2063.147939	21.793344
78.921738	2067.826087	21.798362
79.191966	2055.024735	21.803379
79.227283	2061.095156	21.808397
79.198642	2056.827022	21.813415
79.456150	2069.202984	21.818432
79.410458	2085.823390	21.823450
79.264106	2077.493108	21.828467
79.546481	2081.557213	21.833485
79.453674	2087.374833	21.838503
79.764704	2083.291799	21.843520
79.822434	2086.203690	21.848538
79.957084	2075.666970	21.853555
79.991890	2085.384848	21.858573
79.915578	2086.636594	21.863591
80.327729	2103.454057	21.868608
80.292205	2107.061731	21.873626
80.461443	2106.199129	21.878643
80.422632	2113.509839	21.883661
80.174489	2108.275636	21.888679
80.498846	2107.462944	21.893696
80.501483	2106.872029	21.898714
80.824005	2104.211545	21.903731
80.503664	2112.294090	21.908749
80.672239	2122.969011	21.913767
81.196200	2140.186521	21.918784
81.211834	2135.384637	21.923802
81.404465	2130.998348	21.928819
81.458526	2135.800688	21.933837
81.253599	2128.602953	21.938855
81.534654	2132.596815	21.943872
81.215739	2139.313734	21.948890
81.819573	2121.216350	21.953907
82.124000	2127.941084	21.958925
81.732156	2124.184265	21.963943
81.833316	2123.536090	21.968960
81.599982	2117.086791	21.973978
81.744508	2123.027733	21.978995
81.785141	2135.567220	21.984013
81.959607	2148.171963	21.989031
82.163849	2139.120584	21.994048
82.147466	2152.187653	21.999066
82.158454	2151.074074	22.004083
82.396264	2156.914935	22.009101
82.395265	2157.845150	22.014119
82.822989	2166.877134	22.019136
82.696347	2182.461793	22.024154
82.900581	2180.128375	22.029171
82.724910	2186.053062	22.034189
82.853376	2182.175827	22.039207
82.681721	2181.538173	22.044224
82.751727	2180.534510	22.049242
83.126968	2180.353966	22.054259
83.350201	2173.651877	22.059277
83.069409	2177.182455	22.064295
83.568944	2174.286739	22.069312
83.587439	2188.770167	22.074330
83.706606	2192.279804	22.079347
83.611271	2197.454157	22.084365
83.673208	2207.880247	22.089383
83.969162	2200.158979	22.094400
83.792486	2200.263918	22.099418
84.195805	2195.368298	22.104435
84.155162	2195.877109	22.109453
83.914654	2200.770762	22.114471
84.481392	2198.195818	22.119488
83.949337	2193.014893	22.124506
84.158676	2192.046037	22.129523
84.227509	2202.715480	22.134541
84.452151	2218.139646	22.139559
84.649335	2220.107175	22.144576
84.448405	2219.773592	22.149594
84.716076	2221.552278	22.154611
84.648189	2225.197228	22.159629
84.718724	2226.425065	22.164647
85.234698	2233.420738	22.169664
85.196092	2231.642108	22.174682
85.164471	2242.260884	22.179699
85.359701	2231.389211	22.184717
85.078001	2239.961901	22.189735
85.529140	2238.105333	22.194752
85.047483	2238.749371	22.199770
85.391437	2254.860150	22.204787
85.565508	2258.811913	22.209805
85.613282	2268.833284	22.214823
85.795634	2267.420840	22.219840
85.791284	2268.479574	22.224858
86.135531	2281.913440	22.229875
86.687765	2282.652454	22.234893
86.357494	2295.389706	22.239911
86.742077	2284.896901	22.244928
86.801322	2287.273515	22.249946
86.786839	2287.246477	22.254963
87.067076	2277.172940	22.259981
86.785050	2274.584175	22.264999
87.051291	2267.362304	22.270016
86.797045	2267.849395	22.275034
87.245780	2265.811717	22.280051
87.375499	2267.222681	22.285069
87.297402	2276.121145	22.290087
87.533126	2261.672900	22.295104
87.350442	2273.110838	22.300122
87.667557	2268.448770	22.305139
87.797602	2268.887195	22.310157
87.645706	2263.360614	22.315175
87.757176	2256.672270	22.320192
87.758167	2264.640663	22.325210
87.825613	2265.444587	22.330227
88.016126	2259.011670	22.335245
87.736884	2265.927595	22.340263
87.799958	2258.992133	22.345280
87.626691	2286.164661	22.350298
87.621681	2282.797318	22.355315
87.880787	2289.899329	22.360333
87.953032	2307.691839	22.365351
88.269987	2313.805496	22.370368
88.335004	2321.322746	22.375386
88.134273	2323.873518	22.380403
88.712219	2329.873888	22.385421
88.527771	2350.685077	22.390439
89.100182	2349.913198	22.395456
89.518984	2356.847453	22.400474
89.204566	2360.240718	22.405491
89.376825	2355.930971	22.410509
89.480505	2357.376571	22.415527
89.267674	2357.990278	22.420544
89.656473	2359.473321	22.425562
89.529829	2351.114825	22.430579
89.931923	2343.785382	22.435597
89.439951	2359.562208	22.440615
89.735517	2342.548339	22.445632
89.528229	2355.828692	22.450650
89.640868	2367.800510	22.455667
89.929269	2375.048505	22.460685
89.971042	2380.598664	22.465703
90.032603	2366.061042	22.470720
90.201250	2379.674074	22.475738
90.118614	2396.726541	22.480755
90.436989	2397.822408	22.485773
90.424136	2416.233888	22.490791
90.845914	2402.385845	22.495808
90.948660	2404.130832	22.500826
90.562873	2405.848431	22.505843
91.039468	2401.992641	22.510861
91.065709	2427.883892	22.515879
91.711518	2433.859286	22.520896
91.397553	2427.462186	22.525914
91.714187	2427.369695	22.530931
92.166309	2422.295444	22.535949
92.124376	2426.351521	22.540967
91.972924	2407.537474	22.545984
92.112512	2394.480688	22.551002
91.985863	2396.021910	22.556019
92.119763	2389.507757	22.561037
91.980320	2388.886415	22.566055
91.977317	2415.995544	22.571072
92.045978	2404.904930	22.576090
92.300976	2412.816383	22.581107
92.604366	2420.024514	22.586125
92.405845	2423.688383	22.591143
92.284019	2417.602801	22.596160
92.593240	2417.733203	22.601178
92.887810	2444.530894	22.606195
92.715532	2439.395048	22.611213
92.947668	2449.547044	22.616231
92.698453	2446.066940	22.621248
92.750679	2446.952137	22.626266
92.622210	2456.676807	22.631283
93.252705	2461.925179	22.636301
92.921699	2477.193161	22.641319
93.203806	2470.365837	22.646336
93.180062	2465.057744	22.651354
93.648550	2491.532215	22.656371
94.055359	2486.809561	22.661389
93.990751	2498.249769	22.666407
94.034477	2494.776274	22.671424
94.461962	2490.489592	22.676442
94.236611	2503.358863	22.681459
94.391263	2491.261765	22.686477
94.444430	2501.254832	22.691495
94.174145	2501.127224	22.696512
94.578799	2493.287809	22.701530
94.557756	2503.998719	22.706547
94.833460	2507.994352	22.711565
95.032135	2520.328444	22.716583
94.685174	2522.897160	22.721600
94.932276	2516.922120	22.726618
94.815658	2516.668276	22.731635
94.869024	2512.635274	22.736653
94.727627	2511.779984	22.741671
95.218760	2527.730056	22.746688
95.434461	2542.839077	22.751706
95.324361	2551.542590	22.756723
95.489570	2544.836170	22.761741
95.826082	2554.220513	22.766759
95.743493	2545.819182	22.771776
96.131318	2553.907153	22.776794
95.672905	2548.815495	22.781811
95.760292	2552.609628	22.786829
96.167361	2568.250017	22.791847
96.314608	2576.949522	22.796864
96.303558	2565.974360	22.801882
96.281853	2567.791548	22.806899
96.263879	2566.350430	22.811917
96.389579	2585.511267	22.816935
96.733328	2594.466849	22.821952
96.982897	2590.024545	22.826970
96.922918	2601.152625	22.831987
97.123489	2593.381991	22.837005
97.318856	2600.997881	22.842023
97.415874	2590.997788	22.847040
97.604036	2583.992255	22.852058
97.241201	2593.846371	22.857075
97.660822	2594.304582	22.862093
98.056799	2606.647024	22.867111
97.871485	2605.613948	22.872128
98.180014	2597.869536	22.877146
98.022703	2601.809713	22.882163
97.991032	2603.882510	22.887181
98.160207	2601.226860	22.892199
97.995570	2594.720315	22.897216
98.529391	2595.006459	22.902234
98.138871	2600.039254	22.907251
98.494059	2611.140338	22.912269
98.558130	2629.832661	22.917287
98.787058	2629.535779	22.922304
98.911174	2625.563479	22.927322
98.650592	2629.877479	22.932339
98.824594	2635.232202	22.937357
99.035634	2642.246263	22.942375
99.067475	2656.464119	22.947392
99.150784	2656.222450	22.952410
99.486336	2653.345924	22.957427
99.478370	2654.934848	22.962445
99.296748	2656.603709	22.967463
99.476264	2670.045106	22.972480
100.111600	2675.179751	22.977498
99.907549	2691.039957	22.982515
100.082126	2689.140933	22.987533
100.361854	2688.010382	22.992551
100.301920	2680.713182	22.997568
100.649192	2676.522413	23.002586
100.617083	2680.216668	23.007603
100.817818	2672.202644	23.012621
100.733603	2671.209522	23.017639
100.669682	2682.403278	23.022656
100.652864	2669.473346	23.027674
100.490539	2697.925578	23.032691
100.802107	2698.511928	23.037709
101.004845	2702.307473	23.042727
101.559308	2706.447571	23.047744
101.746964	2695.907169	23.052762
101.329449	2695.862206	23.057779
101.233551	2693.576436	23.062797
101.715725	2705.412523	23.067815
101.713645	2723.781241	23.072832
101.723473	2721.553558	23.077850
101.801239	2726.202539	23.082867
101.899840	2728.651057	23.087885
101.800942	2731.549236	23.092903
101.844963	2732.418877	23.097920
102.055335	2725.129269	23.102938
102.118093	2753.475040	23.107955
102.245810	2742.933899	23.112973
102.457471	2755.239254	23.117991
102.535317	2750.988735	23.123008
103.147740	2769.149459	23.128026
102.829826	2779.715600	23.133043
103.060636	2781.843001	23.138061
103.394101	2778.947112	23.143079
103.276220	2780.438884	23.148096
103.353958	2774.117349	23.153114
103.433158	2787.608530	23.158131
103.774188	2778.519173	23.163149
103.899176	2776.422427	23.168167
104.109746	2776.338441	23.173184
103.807402	2756.927646	23.178202
103.846126	2765.025885	23.183219
103.874425	2779.824011	23.188237
104.251198	2781.861100	23.193255
104.010720	2796.083615	23.198272
104.099015	2787.973966	23.203290
104.358536	2802.466488	23.208307
104.739743	2808.801612	23.213325
104.787026	2819.734122	23.218343
104.792818	2820.749873	23.223360
105.149826	2826.560229	23.228378
105.063067	2819.841073	23.233395
105.206858	2822.138806	23.238413
105.339643	2814.614738	23.243431
105.148182	2820.328088	23.248448
105.453584	2814.149173	23.253466
105.656667	2823.338037	23.258483
105.478289	2835.244608	23.263501
105.727400	2837.740278	23.268519
105.983909	2849.299640	23.273536
105.996937	2845.256693	23.278554
106.033096	2849.581470	23.283571
105.945613	2840.607121	23.288589
105.915340	2839.602695	23.293607
106.291041	2867.372803	23.298624
106.463850	2868.162857	23.303642
106.590245	2873.993694	23.308659
106.470533	2867.880811	23.313677
106.721351	2872.421650	23.318695
106.925424	2884.421645	23.323712
107.212306	2884.281319	23.328730
107.309041	2891.796743	23.333747
107.203428	2882.357222	23.338765
107.299137	2884.086105	23.343783
107.873396	2886.195245	23.348800
107.720341	2887.344395	23.353818
107.991384	2889.017475	23.358835
107.982457	2882.166105	23.363853
108.041648	2890.222435	23.368871
107.806483	2885.534291	23.373888
108.419279	2887.038181	23.378906
108.109526	2901.345495	23.383923
108.403137	2913.838606	23.388941
108.490902	2909.565927	23.393959
108.467998	2913.038222	23.398976
108.726464	2910.944558	23.403994
108.749829	2908.637041	23.409011
108.690280	2916.075193	23.414029
108.673477	2905.675203	23.419047
108.609891	2923.538941	23.424064
109.073905	2931.957833	23.429082
109.082099	2933.802401	23.434099
109.340160	2944.614267	23.439117
109.318405	2934.054040	23.444135
109.207594	2945.418754	23.449152
109.551072	2956.419653	23.454170
109.957041	2957.976299	23.459187
110.089257	2966.804507	23.464205
110.176381	2959.833647	23.469223
110.186249	2963.132795	23.474240
110.361965	2954.415619	23.479258
110.190922	2959.831913	23.484275
110.380531	2958.317410	23.489293
110.695808	2960.015067	23.494311
110.374717	2971.863474	23.499328
110.845738	2972.545494	23.504346
110.845326	2968.914620	23.509363
110.791779	2983.379215	23.514381
110.930228	2975.739948	23.519399
110.514546	2991.558325	23.524416
110.770960	2999.122174	23.529434
111.172645	3000.789386	23.534451
111.254440	3014.025586	23.539469
111.738345	3024.401260	23.544487
111.598834	3037.587103	23.549504
111.584159	3038.006988	23.554522
111.838161	3038.693837	23.559539
112.060616	3057.010810	23.564557
112.567094	3053.938969	23.569575
112.323204	3058.948420	23.574592
112.490963	3061.333567	23.579610
112.851159	3050.846258	23.584627
112.880416	3053.021636	23.589645
113.033583	3050.539838	23.594663
113.105460	3050.232727	23.599680
113.280064	3055.016969	23.604698
113.554934	3044.201239	23.609715
113.689466	3043.936516	23.614733
113.558717	3045.760395	23.619751
113.481145	3044.268464	23.624768
113.961664	3059.785368	23.629786
113.745662	3056.537051	23.634803
113.973136	3065.815336	23.639821
114.321055	3057.175115	23.644839
114.496680	3068.235777	23.649856
114.591793	3057.464761	23.654874
114.652494	3050.626988	23.659891
114.696175	3064.627487	23.664909
114.680824	3063.039811	23.669927
114.449284	3061.303659	23.674944
114.563489	3057.520705	23.679962
114.588692	3062.007212	23.684979
114.741056	3088.520079	23.689997
114.540981	3090.827535	23.695015
114.945378	3096.219477	23.700032
115.122683	3095.478334	23.705050
115.151839	3102.276236	23.710067
115.084922	3114.489795	23.715085
115.429562	3106.989966	23.720103
115.009557	3128.065228	23.725120
115.123084	3138.877534	23.730138
115.800478	3142.950544	23.735155
116.049692	3146.590457	23.740173
116.610996	3159.913551	23.745191
116.426755	3179.890291	23.750208
116.490725	3176.400300	23.755226
116.863528	3165.659620	23.760243
116.966469	3167.612164	23.765261
117.214248	3150.763219	23.770279
117.075212	3159.869540	23.775296
117.426816	3157.787199	23.780314
117.507782	3151.052730	23.785331
117.195452	3150.883645	23.790349
117.615656	3151.172866	23.795367
117.476940	3153.250071	23.800384
117.653420	3150.569101	23.805402
117.980183	3142.867470	23.810419
117.751305	3149.701814	23.815437
117.945429	3141.518549	23.820455
117.891692	3164.090856	23.825472
118.238174	3171.367015	23.830490
118.362732	3180.154087	23.835507
118.147172	3181.973518	23.840525
118.291516	3174.509968	23.845543
118.201406	3187.702722	23.850560
118.550702	3195.825365	23.855578
118.579459	3201.472469	23.860595
118.571998	3206.605832	23.865613
118.920497	3220.245342	23.870631
119.110614	3234.578086	23.875648
119.480233	3236.173067	23.880666
119.293548	3239.894227	23.885683
119.671432	3239.342728	23.890701
119.677783	3246.694134	23.895719
120.151780	3259.827810	23.900736
120.226506	3260.476627	23.905754
120.853056	3252.064214	23.910771
120.322593	3249.085264	23.915789
120.411620	3246.582949	23.920807
120.672212	3249.434698	23.925824
120.747685	3247.994189	23.930842
120.941627	3239.932963	23.935859
121.014841	3242.712180	23.940877
120.752203	3241.628469	23.945895
121.033341	3248.151227	23.950912
121.096084	3263.603630	23.955930
121.204628	3263.136097	23.960947
121.585124	3271.884392	23.965965
121.473438	3274.186690	23.970983
121.533670	3269.818067	23.976000
121.936940	3292.588155	23.981018
122.233532	3290.384182	23.986035
122.060393	3297.360953	23.991053
121.989486	3289.756588	23.996071
122.129889	3294.814707	24.001088
122.484944	3300.927174	24.006106
122.530959	3298.146900	24.011123
122.352779	3320.263605	24.016141
122.304239	3323.784727	24.021159
122.771073	3326.711807	24.026176
122.704912	3327.559562	24.031194
122.818517	3336.027240	24.036211
122.864983	3342.938930	24.041229
122.992332	3344.950060	24.046247
123.586372	3359.153046	24.051264
123.569072	3380.310809	24.056282
123.849881	3379.517081	24.061299
124.149138	3384.773758	24.066317
124.262239	3382.194198	24.071335
124.298221	3385.197739	24.076352
124.094024	3384.794581	24.081370
124.150083	3376.534434	24.086387
124.143755	3397.349025	24.091405
124.360660	3402.390575	24.096423
124.688103	3392.879048	24.101440
124.793735	3397.626385	24.106458
125.101041	3393.564500	24.111475
124.952094	3407.142420	24.116493
125.078420	3413.419193	24.121511
125.440435	3423.044358	24.126528
125.375651	3423.719035	24.131546
125.811334	3420.380073	24.136563
125.801598	3422.733632	24.141581
125.599560	3416.661725	24.146599
125.501900	3428.518371	24.151616
125.893969	3445.126811	24.156634
125.966697	3450.402508	24.161651
125.989533	3456.562952	24.166669
126.350472	3460.317923	24.171687
126.875232	3473.032696	24.176704
126.368704	3482.446925	24.181722
126.687348	3480.527106	24.186739
126.651695	3484.315062	24.191757
126.964751	3482.241817	24.196775
127.163416	3495.608701	24.201792
127.366740	3503.514304	24.206810
127.543216	3490.000442	24.211827
127.648415	3504.664461	24.216845
127.671362	3498.526137	24.221863
128.025565	3514.726302	24.226880
127.895731	3527.917255	24.231898
128.185975	3525.770607	24.236915
128.223784	3530.795782	24.241933
128.446608	3526.398200	24.246951
128.699785	3526.616646	24.251968
128.520511	3522.925087	24.256986
128.852044	3541.550596	24.262003
128.895119	3556.635238	24.267021
129.082670	3557.633546	24.272039
129.301160	3554.854990	24.277056
129.479975	3554.882179	24.282074
129.474147	3555.145475	24.287091
129.767528	3561.818326	24.292109
129.767465	3572.503264	24.297127
129.880583	3578.204656	24.302144
129.763100	3586.248464	24.307162
129.767396	3580.910542	24.312179
129.944366	3589.639949	24.317197
130.270026	3605.834303	24.322215
130.657304	3613.754788	24.327232
130.260541	3621.589699	24.332250
130.669173	3610.087175	24.337267
130.763121	3615.621260	24.342285
131.078221	3627.223869	24.347303
130.991457	3639.808101	24.352320
130.882401	3639.392333	24.357338
131.371568	3629.111665	24.362355
131.657731	3632.677063	24.367373
131.739459	3647.148620	24.372391
132.045383	3657.331715	24.377408
132.164993	3655.592878	24.382426
132.580103	3658.547879	24.387443
132.584254	3655.025948	24.392461
132.793237	3649.418257	24.397479
132.751334	3650.382895	24.402496
132.975304	3663.096434	24.407514
132.633988	3657.632216	24.412531
133.023994	3652.808048	24.417549
133.047991	3646.514747	24.422567
133.238276	3641.141287	24.427584
133.184989	3649.935624	24.432602
133.086790	3643.604279	24.437619
133.508316	3659.509947	24.442637
133.502171	3671.908787	24.447655
133.543986	3673.100544	24.452672
133.699245	3673.065483	24.457690
133.680655	3666.484302	24.462707
133.813872	3680.050000	24.467725
133.794046	3701.682302	24.472743
134.490158	3695.867157	24.477760
134.237967	3701.912578	24.482778
134.462601	3715.218650	24.487795
134.992044	3734.126629	24.492813
134.808169	3732.126173	24.497831
135.007097	3732.978101	24.502848
135.050973	3737.753484	24.507866
135.123225	3732.421979	24.512883
135.392963	3747.951629	24.517901
135.357357	3744.004310	24.522919
135.963026	3751.190187	24.527936
135.285997	3748.305098	24.532954
135.886869	3763.716942	24.537971
136.117762	3773.290794	24.542989
136.198017	3780.259691	24.548007
136.274120	3778.033879	24.553024
136.022696	3793.128917	24.558042
136.723789	3797.661240	24.563059
136.434799	3804.699941	24.568077
136.241700	3815.715864	24.573095
136.971789	3824.687736	24.578112
136.923797	3831.842479	24.583130
137.186023	3833.376159	24.588147
137.370027	3850.139180	24.593165
137.460565	3862.761569	24.598183
138.045299	3864.322580	24.603200
138.036347	3862.134069	24.608218
138.088898	3861.270218	24.613235
138.201924	3863.128253	24.618253
138.123985	3886.123385	24.623271
138.288056	3879.767030	24.628288
138.471314	3890.955772	24.633306
138.453122	3890.635994	24.638323
138.978630	3903.711679	24.643341
138.763980	3920.235611	24.648359
139.285286	3907.112007	24.653376
139.319798	3913.785341	24.658394
139.539644	3931.003608	24.663411
139.668373	3929.825521	24.668429
140.038052	3938.421629	24.673447
140.089202	3937.287098	24.678464
139.968783	3939.551563	24.683482
140.157009	3930.604969	24.688499
140.647127	3946.861834	24.693517
140.247847	3949.214993	24.698535
140.554506	3950.006965	24.703552
140.819399	3960.599475	24.708570
140.821437	3960.278709	24.713587
141.084117	3960.175462	24.718605
140.947405	3965.733684	24.723623
141.248331	3973.776540	24.728640
141.453789	3991.565847	24.733658
141.636366	3980.963210	24.738675
141.822567	3975.406426	24.743693
141.596004	3980.440863	24.748711
142.103112	4005.764884	24.753728
141.823894	4013.947908	24.758746
142.075298	4017.841643	24.763763
142.145632	4012.385931	24.768781
142.291080	4022.758064	24.773799
142.513358	4034.701985	24.778816
143.002096	4039.329783	24.783834
143.058542	4034.162236	24.788851
143.420432	4040.364823	24.793869
143.413669	4041.884387	24.798887
143.485488	4030.348721	24.803904
143.655162	4032.113920	24.808922
143.400528	4042.319194	24.813939
143.839776	4043.227037	24.818957
143.674884	4067.211788	24.823975
143.849439	4060.144850	24.828992
143.754819	4073.447773	24.834010
144.042715	4087.989952	24.839027
143.984322	4089.188881	24.844045
144.208701	4106.413677	24.849063
144.590515	4118.353302	24.854080
144.526690	4129.537443	24.859098
144.993831	4128.740396	24.864115
145.374482	4134.142146	24.869133
145.368863	4143.028884	24.874151
145.594261	4136.841042	24.879168
145.444728	4134.677342	24.884186
145.772843	4157.735591	24.889203
146.212392	4156.921059	24.894221
146.219833	4163.102048	24.899239
146.395514	4159.603189	24.904256
146.424046	4163.684276	24.909274
146.561713	4161.582493	24.914291
146.499395	4171.122047	24.919309
146.327676	4182.456394	24.924327
146.686468	4181.229175	24.929344
147.123349	4196.752470	24.934362
147.405621	4209.927748	24.939379
147.733971	4216.510037	24.944397
147.416236	4209.438692	24.949415
148.028442	4207.743462	24.954432
147.733076	4220.103200	24.959450
147.896371	4242.557257	24.964467
148.105463	4236.332699	24.969485
148.057629	4251.227513	24.974503
148.375345	4246.941997	24.979520
148.463712	4259.510725	24.984538
148.817811	4262.048706	24.989555
149.198078	4265.011563	24.994573
148.941344	4278.545471	24.999591
149.461896	4280.979507	25.004608
149.536345	4295.159509	25.009626
149.726176	4292.576548	25.014643
149.949817	4295.604718	25.019661
149.976347	4300.644608	25.024679
149.973607	4301.976096	25.029696
150.132602	4296.462293	25.034714
150.028030	4314.141848	25.039731
150.362066	4317.386433	25.044749
150.138916	4325.374476	25.049767
150.573683	4336.132853	25.054784
151.054186	4350.400827	25.059802
150.892495	4360.902785	25.064819
151.165483	4349.037466	25.069837
151.186155	4348.583663	25.074855
151.573714	4366.372387	25.079872
151.667417	4375.967353	25.084890
151.599796	4383.320906	25.089907
151.924435	4382.286763	25.094925
151.680578	4387.639208	25.099943
151.909162	4403.460233	25.104960
152.211999	4403.688981	25.109978
152.231304	4415.365167	25.114995
152.756248	4424.093348	25.120013
152.864643	4432.184854	25.125031
152.925936	4436.283427	25.130048
152.844623	4435.641743	25.135066
152.975411	4441.417311	25.140083
153.239694	4444.663233	25.145101
153.587903	4458.375148	25.150119
153.312681	4463.189404	25.155136
153.710634	4460.286082	25.160154
153.806008	4484.915122	25.165171
153.912399	4493.169226	25.170189
153.901993	4487.275452	25.175207
154.061544	4501.202923	25.180224
154.319246	4522.883341	25.185242
154.483177	4524.106925	25.190259
155.044722	4527.842336	25.195277
155.056938	4542.916497	25.200295
155.506997	4545.691443	25.205312
155.817108	4543.850091	25.210330
155.455164	4556.797603	25.215347
156.061520	4542.935632	25.220365
155.822700	4547.035091	25.225383
156.270339	4563.220088	25.230400
156.548308	4567.609659	25.235418
156.489060	4575.047759	25.240435
156.611727	4572.694812	25.245453
156.673824	4579.568627	25.250471
156.761757	4575.717991	25.255488
157.250808	4585.044445	25.260506
156.895808	4590.179880	25.265523
157.588820	4578.508683	25.270541
157.467197	4582.738384	25.275559
157.622890	4585.271463	25.280576
157.864582	4596.251784	25.285594
157.883504	4610.904345	25.290611
158.058677	4606.755739	25.295629
158.356551	4609.730729	25.300647
158.382391	4628.591642	25.305664
158.749060	4631.914373	25.310682
158.370408	4642.863541	25.315699
159.015256	4642.067766	25.320717
159.131085	4651.196154	25.325735
159.310861	4667.696524	25.330752
159.697798	4665.699893	25.335770
159.446561	4664.014465	25.340787
159.474104	4662.572706	25.345805
159.384026	4684.787396	25.350823
159.623160	4690.706569	25.355840
160.432056	4689.003143	25.360858
159.930336	4698.006977	25.365875
160.323162	4710.241354	25.370893
160.448039	4724.342514	25.375911
160.735374	4729.720544	25.380928
160.656473	4742.983627	25.385946
161.229752	4757.073589	25.390963
161.293147	4753.841270	25.395981
161.578269	4757.943826	25.400999
161.454217	4768.883222	25.406016
161.890020	4778.596637	25.411034
161.882897	4781.458339	25.416051
162.175952	4783.283530	25.421069
162.325895	4791.501441	25.426087
162.558014	4802.147989	25.431104
162.549966	4795.555139	25.436122
162.708218	4814.176987	25.441139
162.609850	4805.519914	25.446157
162.979226	4823.116851	25.451175
163.379830	4834.913727	25.456192
163.496776	4829.101912	25.461210
163.376866	4836.478510	25.466227
163.423940	4836.419618	25.471245
163.879700	4843.047236	25.476263
163.616010	4858.784040	25.481280
163.921224	4862.150072	25.486298
163.969049	4861.273561	25.491315
164.482142	4882.583780	25.496333
164.470353	4892.037436	25.501351
164.406237	4886.569028	25.506368
165.112260	4894.987909	25.511386
165.032643	4915.878865	25.516403
165.020395	4914.371214	25.521421
165.443473	4918.310785	25.526439
165.563529	4941.639327	25.531456
165.846628	4938.599782	25.536474
165.752670	4950.880281	25.541491
165.885736	4945.875379	25.546509
166.242001	4956.044687	25.551527
166.628796	4963.228774	25.556544
166.681971	4965.105513	25.561562
166.919795	4971.267581	25.566579
166.971718	4977.915646	25.571597
167.086867	4988.721873	25.576615
167.219912	5004.028495	25.581632
167.591644	4990.767305	25.586650
167.573122	5008.505062	25.591667
167.708215	5010.011473	25.596685
168.060629	5008.296954	25.601703
168.185630	5020.623167	25.606720
168.400106	5022.087297	25.611738
168.592161	5039.160955	25.616755
168.559886	5040.532836	25.621773
169.059968	5042.139492	25.626791
168.892634	5050.149376	25.631808
169.436720	5048.956001	25.636826
169.203946	5062.228287	25.641843
169.309587	5066.205484	25.646861
169.876763	5069.628216	25.651879
169.843298	5082.702920	25.656896
170.067633	5091.107142	25.661914
170.558124	5093.840842	25.666931
170.650483	5095.589035	25.671949
170.906156	5094.197679	25.676967
171.211387	5089.094923	25.681984
171.050014	5105.314358	25.687002
171.398147	5101.794619	25.692020
171.357148	5111.753355	25.697037
171.728449	5102.352073	25.702055
171.710947	5119.022615	25.707072
171.822322	5103.936292	25.712090
171.868923	5118.969083	25.717108
171.839712	5133.582845	25.722125
172.030288	5141.246844	25.727143
171.980790	5153.542980	25.732160
172.122071	5155.739091	25.737178
172.319371	5165.830104	25.742196
172.741020	5190.325113	25.747213
173.310590	5195.087945	25.752231
173.095194	5198.468566	25.757248
173.294928	5208.864787	25.762266
173.423043	5216.001242	25.767284
173.802051	5221.116176	25.772301
174.035675	5227.910685	25.777319
174.134875	5245.323636	25.782336
174.502263	5249.046475	25.787354
174.412836	5248.547866	25.792372
174.723812	5253.112524	25.797389
174.811739	5248.646620	25.802407
174.645418	5268.046530	25.807424
175.244404	5269.607697	25.812442
175.521812	5280.803897	25.817460
175.447839	5275.891447	25.822477
176.087803	5278.123157	25.827495
175.711372	5302.576405	25.832512
176.372638	5297.922637	25.837530
176.321897	5294.856382	25.842548
176.438889	5297.291235	25.847565
176.628969	5294.855351	25.852583
176.262960	5318.846159	25.857600
176.757409	5320.080461	25.862618
177.040907	5323.169806	25.867636
177.032832	5345.199368	25.872653
177.396669	5357.984064	25.877671
177.100681	5364.343347	25.882688
177.587735	5370.717131	25.887706
177.630712	5385.815359	25.892724
177.839545	5384.509704	25.897741
178.376229	5396.809801	25.902759
178.261460	5416.022574	25.907776
178.489008	5409.517268	25.912794
178.635153	5426.706847	25.917812
178.925931	5434.581228	25.922829
179.197566	5433.614866	25.927847
179.271367	5453.747883	25.932864
179.151167	5459.791417	25.937882
179.329595	5468.627169	25.942900
179.745114	5493.335529	25.947917
180.197060	5492.075467	25.952935
180.206806	5508.981340	25.957952
180.471324	5512.892969	25.962970
180.529455	5522.277933	25.967988
180.680239	5526.851863	25.973005
181.350658	5530.397013	25.978023
181.687248	5549.987311	25.983040
181.746475	5540.305852	25.988058
182.029845	5544.562489	25.993076
182.032622	5545.517482	25.998093
182.019319	5536.185127	26.003111
182.267335	5551.211765	26.008128
182.590478	5564.510582	26.013146
182.997549	5563.547782	26.018164
182.712063	5563.081620	26.023181
183.124946	5569.122007	26.028199
183.089709	5565.556156	26.033216
183.470007	5593.341366	26.038234
183.333174	5591.844823	26.043252
183.215779	5596.189084	26.048269
183.440579	5608.388183	26.053287
183.537925	5623.031065	26.058304
183.911719	5643.267457	26.063322
184.217435	5653.594445	26.068340
184.146862	5662.367563	26.073357
184.489046	5669.178159	26.078375
184.381578	5689.459626	26.083392
184.675762	5691.071297	26.088410
184.933574	5709.784836	26.093428
184.896195	5715.691890	26.098445
185.535796	5724.117494	26.103463
185.645711	5739.041943	26.108480
186.095346	5754.082653	26.113498
186.260190	5759.719175	26.118516
186.322326	5768.787790	26.123533
186.615165	5779.788039	26.128551
186.703924	5778.221841	26.133568
186.458881	5785.615657	26.138586
187.124674	5794.607195	26.143604
187.260288	5805.887102	26.148621
187.714957	5800.213564	26.153639
187.573669	5812.806586	26.158656
188.077702	5827.357129	26.163674
188.216280	5831.592919	26.168692
188.249358	5840.933388	26.173709
188.066660	5837.541534	26.178727
188.370102	5840.146447	26.183744
188.385585	5857.781076	26.188762
188.520401	5862.286862	26.193780
189.003630	5874.987630	26.198797
189.625612	5869.090253	26.203815
189.748594	5873.802783	26.208832
189.716522	5880.450956	26.213850
189.638773	5891.629199	26.218868
189.494608	5916.086685	26.223885
189.773250	5932.316038	26.228903
190.028346	5947.493104	26.233920
190.031751	5951.969475	26.238938
190.973850	5966.649259	26.243956
190.913592	5978.313781	26.248973
191.544391	5971.684781	26.253991
191.639928	5980.773193	26.259008
192.217084	5980.847868	26.264026
192.759970	5981.107006	26.269044
192.582879	5979.111436	26.274061
192.863262	5986.483738	26.279079
192.551367	5996.941548	26.284096
192.085803	6001.004878	26.289114
192.311787	6018.935641	26.294132
192.421871	6036.166509	26.299149
192.731430	6039.894386	26.304167
192.895606	6056.294827	26.309184
192.974876	6083.962970	26.314202
193.471818	6081.973950	26.319220
193.644499	6098.903101	26.324237
193.991610	6107.701048	26.329255
194.385066	6112.555541	26.334272
194.835589	6121.496266	26.339290
195.219440	6128.131611	26.344308
195.262575	6147.630245	26.349325
195.343438	6140.945714	26.354343
195.616852	6142.594740	26.359360
195.302891	6153.779191	26.364378
195.514751	6166.765346	26.369396
195.472071	6181.818654	26.374413
195.717320	6211.769672	26.379431
195.819453	6214.541084	26.384448
196.379782	6218.411798	26.389466
196.881260	6228.410606	26.394484
196.979745	6235.911590	26.399501
197.508424	6219.709930	26.404519
197.681211	6244.310787	26.409536
197.500917	6256.583750	26.414554
197.619328	6260.406334	26.419572
197.624703	6267.168191	26.424589
197.720996	6277.670457	26.429607
198.049828	6293.416139	26.434624
197.768696	6300.208898	26.439642
198.210798	6325.115796	26.444660
198.220606	6339.854961	26.449677
199.031061	6343.257398	26.454695
199.131768	6356.176256	26.459712
199.307597	6375.213699	26.464730
199.568081	6377.617877	26.469748
199.789625	6380.731080	26.474765
199.964946	6389.040141	26.479783
200.348134	6397.814163	26.484800
200.318037	6403.543047	26.489818
200.439251	6397.211683	26.494836
200.534694	6419.546174	26.499853
200.421367	6432.240603	26.504871
200.692308	6446.433332	26.509888
200.625309	6466.869774	26.514906
201.096080	6478.216763	26.519924
201.355186	6500.281679	26.524941
201.668308	6505.025145	26.529959
201.873512	6518.367921	26.534976
201.986234	6536.242406	26.539994
202.577105	6535.234161	26.545012
202.694440	6550.913504	26.550029
203.208915	6559.613897	26.555047
203.399817	6571.311318	26.560064
203.569683	6579.107045	26.565082
203.993572	6569.029053	26.570100
204.035427	6584.880818	26.575117
204.249666	6577.191034	26.580135
204.335822	6591.082093	26.585152
204.386532	6603.100478	26.590170
204.696324	6605.231877	26.595188
204.443803	6616.091419	26.600205
204.918169	6630.471182	26.605223
205.020487	6639.838467	26.610240
205.499371	6657.598126	26.615258
205.834208	6666.344857	26.620276
205.407581	6673.325692	26.625293
205.909321	6691.432901	26.630311
206.298164	6704.117670	26.635328
206.653304	6714.526178	26.640346
207.008164	6723.764276	26.645364
207.060716	6732.193874	26.650381
207.195238	6735.571241	26.655399
207.464086	6743.529464	26.660416
207.537258	6743.236249	26.665434
207.967603	6752.778508	26.670452
207.940311	6763.678845	26.675469
208.204196	6779.156930	26.680487
207.969839	6783.569711	26.685504
208.368137	6794.394890	26.690522
208.825377	6808.708336	26.695540
208.755062	6824.262268	26.700557
208.762797	6836.713282	26.705575
208.864070	6846.549523	26.710592
209.406985	6865.213297	26.715610
209.656684	6873.920675	26.720628
210.029626	6884.678436	26.725645
210.160486	6896.963397	26.730663
210.393616	6898.833419	26.735680
210.623390	6922.240452	26.740698
211.244057	6918.777601	26.745716
211.328263	6930.677264	26.750733
211.339737	6947.843529	26.755751
211.741053	6952.031401	26.760768
211.672006	6961.830532	26.765786
211.853101	6973.228981	26.770804
211.814995	6985.659345	26.775821
212.226820	6991.176655	26.780839
212.736366	7008.189644	26.785856
212.673212	7022.155421	26.790874
212.962738	7022.274573	26.795892
213.231738	7043.272884	26.800909
213.081899	7054.259083	26.805927
213.298735	7054.948731	26.810944
213.802990	7069.282199	26.815962
214.192932	7074.581824	26.820980
214.311307	7088.538089	26.825997
214.333746	7110.174363	26.831015
214.753346	7110.628015	26.836032
214.718568	7113.704239	26.841050
214.792165	7125.708990	26.846068
215.120209	7139.506138	26.851085
215.564567	7148.769054	26.856103
215.992447	7154.411369	26.861120
215.685343	7162.496652	26.866138
216.149047	7156.505282	26.871156
216.315214	7181.905823	26.876173
216.326372	7196.357266	26.881191
216.863526	7190.247389	26.886208
216.744605	7211.561409	26.891226
217.263537	7220.284274	26.896244
217.587878	7219.095623	26.901261
217.579650	7244.074576	26.906279
218.022405	7244.116378	26.911296
218.139444	7246.524745	26.916314
218.706386	7258.859102	26.921332
218.688567	7266.743738	26.926349
219.087783	7274.300982	26.931367
219.106415	7271.998732	26.936384
219.082554	7290.954541	26.941402
219.014365	7296.575050	26.946420
219.627510	7305.194145	26.951437
219.668910	7323.180572	26.956455
219.814877	7330.474929	26.961472
220.422295	7356.401350	26.966490
220.329619	7370.371531	26.971508
220.582036	7382.174370	26.976525
220.566828	7397.123455	26.981543
221.265631	7405.184130	26.986560
221.333918	7428.753338	26.991578
221.440343	7433.350919	26.996596
221.820106	7447.072819	27.001613
221.782114	7467.951580	27.006631
222.494784	7479.448295	27.011648
222.416152	7494.499344	27.016666
222.692556	7501.906884	27.021684
223.116085	7515.927226	27.026701
222.745700	7538.412870	27.031719
223.370945	7537.025511	27.036736
223.314797	7558.260285	27.041754
223.583801	7565.543048	27.046772
224.148408	7581.602297	27.051789
224.517364	7593.817663	27.056807
224.541587	7611.796231	27.061824
224.587680	7619.799646	27.066842
224.886567	7622.858544	27.071860
225.203714	7638.661063	27.076877
225.275280	7651.674810	27.081895
225.770737	7659.428200	27.086912
225.722113	7676.450808	27.091930
226.042004	7690.975264	27.096948
226.339069	7698.554347	27.101965
226.687742	7710.361189	27.106983
226.996834	7721.284480	27.112000
227.114327	7731.480143	27.117018
227.508865	7739.126608	27.122036
227.935139	7744.214853	27.127053
227.897557	7743.865910	27.132071
228.203968	7751.507276	27.137088
227.953284	7766.557917	27.142106
228.245783	7778.026727	27.147124
228.556385	7781.713099	27.152141
228.517172	7805.241581	27.157159
228.376533	7805.621001	27.162176
228.718902	7826.986305	27.167194
229.282547	7839.420125	27.172212
229.753745	7849.444670	27.177229
229.955659	7866.707223	27.182247
229.931759	7868.790844	27.187264
230.481011	7886.104626	27.192282
230.735966	7901.752281	27.197300
230.882127	7902.061385	27.202317
231.179638	7922.235335	27.207335
231.298344	7919.417011	27.212352
231.613846	7931.183821	27.217370
231.631671	7950.391885	27.222388
232.337181	7954.271299	27.227405
232.020214	7971.823878	27.232423
232.509937	7971.523919	27.237440
232.715747	7988.799351	27.242458
233.075446	8000.852716	27.247476
233.512268	8015.057990	27.252493
233.342001	8022.944604	27.257511
233.375046	8036.664541	27.262528
233.609872	8048.793754	27.267546
233.898578	8060.753362	27.272564
234.374376	8077.087765	27.277581
234.642655	8085.654882	27.282599
234.997828	8088.918029	27.287616
235.116290	8111.392876	27.292634
235.296139	8119.926599	27.297652
235.491799	8135.494498	27.302669
235.556454	8152.118388	27.307687
236.078519	8170.878529	27.312704
235.802724	8178.434510	27.317722
236.285941	8199.349260	27.322740
236.532930	8208.072000	27.327757
236.723312	8224.291527	27.332775
237.261866	8222.546654	27.337792
237.367456	8249.191728	27.342810
237.605272	8255.202264	27.347828
238.201777	8255.752710	27.352845
238.227133	8281.602902	27.357863
238.510910	8290.340867	27.362880
238.979290	8293.812185	27.367898
239.098842	8313.842000	27.372916
239.358615	8316.619196	27.377933
239.464893	8318.741983	27.382951
239.896011	8330.912179	27.387968
239.946789	8340.290573	27.392986
240.261791	8347.407746	27.398004
240.596823	8365.710678	27.403021
240.852404	8371.329173	27.408039
241.056777	8373.385314	27.413056
241.479910	8392.710362	27.418074
241.424852	8384.170989	27.423092
241.956772	8394.259088	27.428109
241.790906	8414.155094	27.433127
242.140235	8426.136451	27.438144
242.218662	8430.204077	27.443162
242.198039	8451.919409	27.448180
243.207679	8451.616094	27.453197
242.796196	8475.762545	27.458215
243.006890	8490.611453	27.463232
243.296198	8502.961229	27.468250
243.528456	8526.192179	27.473268
243.681501	8534.777038	27.478285
243.951292	8555.933189	27.483303
243.881846	8566.637707	27.488320
244.274814	8578.640314	27.493338
244.647945	8590.030980	27.498356
245.170719	8610.956266	27.503373
245.122423	8625.876530	27.508391
245.457376	8631.854587	27.513408
245.871807	8640.897247	27.518426
245.689854	8651.455017	27.523444
246.255274	8664.801413	27.528461
246.396773	8680.181082	27.533479
246.992792	8682.153528	27.538496
247.308296	8682.778866	27.543514
247.162051	8706.006560	27.548532
248.022863	8712.388375	27.553549
248.034572	8718.182856	27.558567
248.443890	8718.848598	27.563584
248.447485	8726.234122	27.568602
248.536254	8748.026278	27.573620
248.608187	8752.832405	27.578637
249.304745	8774.377467	27.583655
249.770124	8778.129046	27.588672
249.536408	8788.351222	27.593690
249.802539	8802.926555	27.598708
250.373789	8806.022529	27.603725
250.628026	8815.138284	27.608743
250.811348	8839.683114	27.613760
251.063085	8838.209381	27.618778
251.057430	8850.345138	27.623796
251.466073	8868.657733	27.628813
251.460643	8881.252744	27.633831
251.424620	8896.106630	27.638848
252.324227	8910.038370	27.643866
252.406086	8929.842804	27.648884
252.807603	8923.970578	27.653901
253.122635	8944.020029	27.658919
253.129078	8964.505806	27.663936
253.415344	8965.355784	27.668954
253.014295	8989.154660	27.673972
253.667416	8998.581048	27.678989
253.922162	9022.748810	27.684007
254.321310	9035.648013	27.689024
254.445804	9049.007060	27.694042
254.291311	9072.421777	27.699060
255.015853	9089.785846	27.704077
255.119409	9107.550505	27.709095
255.268411	9124.832630	27.714112
256.046935	9148.439639	27.719130
256.132698	9159.614374	27.724148
256.542348	9162.682024	27.729165
256.989905	9170.941964	27.734183
256.662505	9176.117615	27.739200
257.239144	9197.443613	27.744218
257.463219	9208.980714	27.749236
257.318609	9217.416689	27.754253
257.966163	9248.244288	27.759271
258.325351	9254.606946	27.764288
258.665791	9265.092039	27.769306
258.881437	9296.751438	27.774324
259.165661	9292.882930	27.779341
259.726220	9305.356226	27.784359
259.429014	9317.976243	27.789376
259.886633	9322.184579	27.794394
260.511784	9345.274481	27.799412
260.533077	9352.685724	27.804429
260.835021	9356.961591	27.809447
260.719120	9380.847769	27.814464
261.286577	9384.475458	27.819482
261.209568	9406.149420	27.824500
261.713035	9407.202172	27.829517
261.691999	9424.269339	27.834535
261.986864	9448.699740	27.839552
262.489371	9447.375878	27.844570
262.290428	9464.478051	27.849588
262.695724	9477.201704	27.854605
262.978610	9500.453261	27.859623
263.086354	9512.679464	27.864640
263.310618	9531.611035	27.869658
263.429989	9557.374457	27.874676
263.620209	9568.135923	27.879693
263.950365	9585.911659	27.884711
264.252686	9609.277539	27.889728
264.792488	9619.357235	27.894746
265.155893	9646.192783	27.899764
265.490828	9652.098750	27.904781
265.702842	9672.660907	27.909799
265.672216	9686.844208	27.914816
266.446127	9693.069856	27.919834
266.550644	9703.797543	27.924852
266.676955	9729.436407	27.929869
267.227647	9739.003876	27.934887
267.343923	9750.768768	27.939904
267.851408	9760.300861	27.944922
267.780479	9776.912640	27.949940
268.317769	9788.099733	27.954957
268.314184	9790.868787	27.959975
268.707035	9819.434511	27.964992
268.990286	9828.888741	27.970010
268.908108	9847.047356	27.975028
269.365375	9863.972005	27.980045
269.754264	9885.284305	27.985063
269.861068	9906.291172	27.990080
270.368201	9908.059480	27.995098
270.547642	9933.566975	28.000116
270.681701	9953.542865	28.005133
270.782777	9959.422267	28.010151
271.125543	9986.075086	28.015168
271.372598	9993.659604	28.020186
271.645925	10021.032226	28.025204
272.047624	10040.678732	28.030221
272.181826	10059.799942	28.035239
272.298734	10074.608331	28.040256
273.054076	10097.990536	28.045274
273.498335	10126.493937	28.050292
273.574810	10143.448034	28.055309
273.890466	10146.796146	28.060327
273.924971	10163.912415	28.065344
274.421531	10170.854603	28.070362
274.629776	10193.309629	28.075380
274.906939	10210.087193	28.080397
275.356950	10220.296368	28.085415
275.585023	10241.470316	28.090432
275.943084	10255.190349	28.095450
275.947924	10269.800026	28.100468
276.365118	10283.719860	28.105485
276.874729	10304.132722	28.110503
277.072888	10322.862346	28.115520
277.381238	10319.713624	28.120538
277.583034	10351.946999	28.125556
277.874792	10361.478132	28.130573
278.229370	10377.925557	28.135591
278.433087	10390.472162	28.140608
278.468845	10402.655808	28.145626
278.988653	10417.534908	28.150644
278.936511	10429.643310	28.155661
279.347584	10444.380501	28.160679
279.737625	10473.091239	28.165696
280.047371	10486.050531	28.170714
279.937723	10494.853249	28.175732
280.085091	10523.435646	28.180749
280.728071	10530.973003	28.185767
280.840223	10553.156085	28.190784
281.048445	10555.527801	28.195802
281.505111	10580.126164	28.200820
281.854649	10597.352256	28.205837
282.175270	10604.865798	28.210855
282.516995	10623.705154	28.215872
282.950976	10634.904426	28.220890
283.201713	10642.210529	28.225908
283.407831	10662.153311	28.230925
283.815095	10661.907938	28.235943
283.986241	10674.601969	28.240960
284.616601	10688.181183	28.245978
284.493986	10700.008371	28.250996
284.584971	10714.641221	28.256013
284.989678	10722.427679	28.261031
285.340898	10754.373981	28.266048
285.733199	10757.471603	28.271066
286.004604	10768.940539	28.276084
285.835259	10789.571185	28.281101
286.578539	10801.444209	28.286119
286.747306	10819.825526	28.291136
287.116275	10841.982253	28.296154
287.203372	10852.440201	28.301172
287.474234	10876.560812	28.306189
288.052336	10886.727939	28.311207
288.362099	10909.112008	28.316224
288.545313	10917.431579	28.321242
288.673573	10939.185501	28.326260
288.845390	10953.428588	28.331277
289.703749	10963.851916	28.336295
290.007167	10977.639914	28.341312
290.291208	10992.663359	28.346330
290.366939	10999.413993	28.351348
290.110644	11019.156425	28.356365
290.971305	11031.695639	28.361383
291.037125	11060.172728	28.366400
291.389384	11076.663009	28.371418
291.828941	11091.274747	28.376436
291.926781	11109.909224	28.381453
292.397771	11121.000286	28.386471
292.618063	11147.130877	28.391488
292.763289	11158.684006	28.396506
293.195823	11170.999526	28.401524
293.195210	11198.027127	28.406541
293.948850	11204.960307	28.411559
293.890689	11226.342077	28.416576
294.107711	11239.374051	28.421594
294.481083	11261.275352	28.426612
294.678652	11281.412557	28.431629
295.149180	11292.735452	28.436647
295.193787	11321.238572	28.441664
295.324114	11336.514691	28.446682
295.894142	11367.266220	28.451700
296.072339	11392.788047	28.456717
296.900737	11402.003273	28.461735
296.822920	11422.964671	28.466752
297.173173	11447.147055	28.471770
297.571774	11455.123975	28.476788
297.895721	11486.247376	28.481805
298.394260	11483.588539	28.486823
298.320670	11516.200734	28.491840
298.890921	11522.500999	28.496858
299.069410	11553.018289	28.501876
299.143741	11564.611807	28.506893
299.752751	11584.419706	28.511911
300.029054	11593.456964	28.516928
300.359221	11611.809315	28.521946
300.527319	11622.437147	28.526964
301.036893	11643.339425	28.531981
301.318709	11649.939611	28.536999
301.366203	11660.169841	28.542016
301.664791	11674.756592	28.547034
302.167742	11685.563836	28.552052
301.847670	11699.958332	28.557069
302.490605	11719.995579	28.562087
302.442638	11750.538116	28.567104
303.010700	11765.289929	28.572122
303.484873	11776.081512	28.577140
303.217083	11803.143312	28.582157
304.135377	11821.628626	28.587175
304.577356	11842.050694	28.592192
304.696594	11850.170175	28.597210
305.195339	11870.081771	28.602228
305.245500	11896.088876	28.607245
305.710652	11899.622199	28.612263
306.079482	11922.056201	28.617280
306.387894	11928.163592	28.622298
306.926866	11950.895670	28.627316
306.798500	11966.139561	28.632333
307.341710	11974.620708	28.637351
307.756733	11990.193854	28.642368
308.185410	12018.161878	28.647386
308.546463	12021.543844	28.652404
308.537075	12038.696938	28.657421
308.855154	12051.738054	28.662439
308.840388	12066.972692	28.667456
309.054508	12088.587880	28.672474
309.556849	12102.110688	28.677492
309.599704	12138.710664	28.682509
309.911046	12150.777523	28.687527
310.150939	12186.240320	28.692544
310.476955	12205.799562	28.697562
310.905426	12230.573724	28.702580
311.049823	12252.358256	28.707597
311.524423	12268.131398	28.712615
312.079229	12304.294017	28.717632
312.381667	12323.305750	28.722650
312.816028	12342.199542	28.727668
312.899758	12364.173914	28.732685
313.511857	12376.503185	28.737703
313.734945	12398.284343	28.742720
314.035134	12421.507304	28.747738
314.312047	12436.208640	28.752756
314.566204	12461.097103	28.757773
315.036016	12479.186215	28.762791
315.492338	12506.048961	28.767808
315.719540	12515.846560	28.772826
316.035815	12542.989417	28.777844
315.971056	12565.250235	28.782861
316.546276	12580.414493	28.787879
316.809852	12602.704541	28.792896
317.090612	12620.374395	28.797914
317.671673	12633.887771	28.802932
318.116630	12662.159935	28.807949
318.507058	12668.692132	28.812967
318.602770	12683.864936	28.817984
318.581843	12702.519324	28.823002
318.814985	12725.378751	28.828020
319.401974	12751.974436	28.833037
319.654111	12763.953845	28.838055
320.087052	12788.865223	28.843072
320.420484	12809.364786	28.848090
320.942720	12824.441911	28.853108
320.677050	12853.046350	28.858125
321.345556	12871.211751	28.863143
321.454318	12886.272270	28.868160
321.671251	12908.925040	28.873178
322.269086	12920.699210	28.878196
322.361238	12947.982274	28.883213
322.529440	12971.911820	28.888231
322.943170	12983.749603	28.893248
323.088758	13019.089566	28.898266
323.511533	13035.445675	28.903284
323.627966	13055.986192	28.908301
324.142741	13081.105105	28.913319
324.476429	13106.983692	28.918336
324.567851	13126.423700	28.923354
325.116689	13156.194013	28.928372
325.215531	13179.736630	28.933389
325.771493	13212.142434	28.938407
326.196127	13228.408599	28.943424
326.180125	13250.629187	28.948442
326.979584	13269.878108	28.953460
327.133983	13305.778276	28.958477
327.267076	13328.891504	28.963495
327.870693	13342.485265	28.968512
328.050608	13379.525524	28.973530
328.573969	13400.126776	28.978548
328.822517	13432.271856	28.983565
328.967662	13449.752300	28.988583
329.614588	13484.684066	28.993600
329.926576	13502.860328	28.998618
330.285188	13525.197372	29.003636
330.408154	13555.826895	29.008653
330.703111	13578.073684	29.013671
330.945231	13604.459924	29.018688
330.906686	13642.294987	29.023706
331.966493	13664.133200	29.028724
332.297484	13692.203799	29.033741
332.280797	13717.380136	29.038759
333.150071	13739.899298	29.043776
333.176067	13768.173380	29.048794
333.951283	13771.301201	29.053812
334.205119	13814.147258	29.058829
334.342436	13821.758831	29.063847
334.834259	13843.505322	29.068864
334.920319	13872.198318	29.073882
335.483343	13893.476047	29.078900
335.879052	13914.926489	29.083917
336.048612	13933.785581	29.088935
336.500804	13951.173189	29.093952
336.780612	13987.600978	29.098970
336.906421	14008.016633	29.103988
337.347110	14027.972006	29.109005
337.662734	14049.134858	29.114023
338.288986	14067.173052	29.119040
338.164246	14094.470285	29.124058
338.823301	14124.347056	29.129076
339.296360	14144.974913	29.134093
339.452554	14175.619008	29.139111
340.124689	14184.087861	29.144128
340.444833	14210.238366	29.149146
340.628486	14228.370482	29.154164
340.882874	14255.851099	29.159181
341.172549	14281.496119	29.164199
341.398133	14292.521228	29.169216
341.447074	14322.956397	29.174234
341.924599	14345.780798	29.179252
342.431983	14368.920231	29.184269
342.842951	14393.331780	29.189287
343.497721	14419.978861	29.194304
343.750356	14431.102031	29.199322
343.967212	14454.716785	29.204340
344.178225	14462.730967	29.209357
344.524997	14492.664824	29.214375
344.829794	14496.846241	29.219392
345.441891	14520.069426	29.224410
345.524635	14550.119587	29.229428
345.949094	14561.453972	29.234445
346.026106	14597.153855	29.239463
346.629779	14608.531112	29.244480
346.470213	14636.637239	29.249498
346.736507	14664.316734	29.254516
347.112417	14698.864102	29.259533
347.265833	14714.068642	29.264551
348.147790	14736.832957	29.269568
347.991574	14778.884122	29.274586
348.526147	14800.180350	29.279604
349.203318	14833.202904	29.284621
349.165550	14859.949560	29.289639
349.751298	14891.469565	29.294656
349.764031	14910.592154	29.299674
350.457553	14945.544549	29.304692
350.812792	14969.863733	29.309709
350.694227	15011.291419	29.314727
351.439561	15029.608857	29.319744
352.064364	15061.270882	29.324762
352.517146	15085.985464	29.329780
352.805101	15123.539787	29.334797
353.165015	15145.740128	29.339815
353.543892	15155.993357	29.344832
354.078855	15191.911899	29.349850
354.736791	15212.393869	29.354868
354.469255	15237.514755	29.359885
354.873304	15262.225059	29.364903
355.496449	15293.542629	29.369920
355.459119	15318.344982	29.374938
356.057784	15343.916880	29.379956
356.247388	15369.524997	29.384973
356.747117	15399.056912	29.389991
357.223340	15415.289924	29.395008
357.393584	15446.414794	29.400026
357.758628	15469.970230	29.405044
358.353621	15499.038926	29.410061
357.974272	15528.434430	29.415079
358.753079	15551.715024	29.420096
358.901372	15586.208933	29.425114
359.322762	15610.079938	29.430132
359.755928	15644.403879	29.435149
359.913547	15673.721804	29.440167
360.419369	15702.031708	29.445184
360.985687	15740.353106	29.450202
361.679130	15761.430416	29.455220
361.905540	15790.431381	29.460237
362.245965	15816.614187	29.465255
362.758823	15835.872593	29.470272
363.005255	15864.912933	29.475290
363.566892	15890.357832	29.480308
363.572700	15912.144950	29.485325
364.022682	15940.990961	29.490343
364.294114	15954.536274	29.495360
364.507605	15991.127643	29.500378
365.094011	16011.025061	29.505396
365.669902	16031.510599	29.510413
365.730184	16066.198191	29.515431
366.456793	16091.089637	29.520448
366.431319	16117.429629	29.525466
366.882584	16134.592731	29.530484
366.945711	16166.250539	29.535501
367.423845	16201.534432	29.540519
367.771786	16223.380401	29.545536
368.461664	16255.178969	29.550554
368.800975	16271.879988	29.555572
369.299026	16297.139009	29.560589
369.500250	16326.907989	29.565607
369.862221	16346.368505	29.570624
369.793850	16367.202254	29.575642
370.348698	16387.942344	29.580660
370.721245	16413.442990	29.585677
371.014613	16454.998423	29.590695
371.672868	16482.294545	29.595712
372.046069	16505.210145	29.600730
372.491205	16520.172614	29.605748
372.578759	16539.763893	29.610765
372.938554	16571.962905	29.615783
373.385456	16586.171682	29.620800
373.657705	16627.439432	29.625818
374.255507	16651.703616	29.630836
374.545898	16678.275954	29.635853
375.060740	16700.022423	29.640871
375.081283	16733.858914	29.645888
375.706968	16762.406160	29.650906
375.543792	16792.107028	29.655924
376.667205	16819.210078	29.660941
376.820092	16858.442663	29.665959
377.461810	16882.212840	29.670976
377.833277	16910.173469	29.675994
378.150705	16934.161326	29.681012
378.439939	16957.220707	29.686029
378.929110	16987.986740	29.691047
379.123006	17017.206463	29.696064
379.322371	17049.492855	29.701082
379.730285	17081.232489	29.706100
380.588975	17103.863649	29.711117
380.606079	17137.156122	29.716135
381.160281	17164.368130	29.721152
381.334600	17187.601331	29.726170
381.514213	17221.521256	29.731188
382.012522	17248.846692	29.736205
382.303928	17289.252237	29.741223
382.675097	17322.957811	29.746240
383.173138	17346.219628	29.751258
383.686286	17381.128223	29.756276
384.135883	17412.242086	29.761293
384.537910	17451.002917	29.766311
384.731008	17472.489954	29.771328
385.257818	17506.051915	29.776346
385.217012	17537.872990	29.781364
385.802055	17571.141699	29.786381
385.883588	17613.937865	29.791399
386.503971	17642.588395	29.796416
386.805073	17676.309435	29.801434
387.071413	17720.011659	29.806452
387.769373	17750.241685	29.811469
387.640029	17796.777732	29.816487
388.317158	17817.165183	29.821504
389.106719	17865.622306	29.826522
389.164871	17897.161279	29.831540
390.046334	17933.969549	29.836557
390.091009	17961.305024	29.841575
390.646505	17989.484510	29.846592
391.095275	18019.004318	29.851610
391.611178	18056.972120	29.856628
391.660719	18082.531943	29.861645
392.057014	18123.131818	29.866663
392.366254	18158.288609	29.871680
393.004912	18194.623725	29.876698
392.948155	18222.791429	29.881716
393.440279	18254.427934	29.886733
393.739182	18285.584135	29.891751
394.312950	18306.563117	29.896768
394.826293	18345.708026	29.901786
395.187218	18387.946019	29.906804
395.451900	18405.563269	29.911821
395.698097	18440.954945	29.916839
395.895380	18469.872402	29.921856
396.722123	18502.823942	29.926874
396.982332	18543.530915	29.931892
397.348920	18578.795759	29.936909
397.641508	18613.615749	29.941927
397.940155	18653.968229	29.946944
398.170356	18688.019921	29.951962
398.553670	18732.162616	29.956980
398.854679	18770.377278	29.961997
399.506308	18820.357666	29.967015
399.919191	18857.441012	29.972032
400.375628	18896.170976	29.977050
400.508826	18933.294470	29.982068
401.224635	18966.470231	29.987085
401.651279	19012.931839	29.992103
401.763810	19058.665186	29.997120
402.334615	19088.653833	30.002138
402.673456	19136.557060	30.007156
403.359670	19172.375645	30.012173
403.913758	19208.194100	30.017191
404.380802	19244.943001	30.022208
404.661422	19281.287712	30.027226
405.316719	19319.030367	30.032244
405.561203	19351.605407	30.037261
406.207123	19387.252971	30.042279
406.482222	19426.211241	30.047296
407.261642	19448.276975	30.052314
407.384806	19493.577775	30.057332
407.746529	19513.064113	30.062349
408.029560	19552.960991	30.067367
408.186767	19592.256044	30.072384
408.958576	19628.584859	30.077402
409.069666	19679.549604	30.082420
409.682672	19707.041397	30.087437
410.257382	19742.669971	30.092455
410.431920	19778.735343	30.097472
411.020102	19810.426691	30.102490
411.234620	19851.800262	30.107508
412.088338	19891.652375	30.112525
412.310968	19917.060225	30.117543
412.637315	19963.298270	30.122560
413.143342	19990.433003	30.127578
413.447542	20032.331373	30.132596
413.996359	20056.521920	30.137613
414.329495	20097.756645	30.142631
414.476684	20138.167718	30.147648
415.016594	20168.502385	30.152666
415.177554	20202.762536	30.157684
415.698467	20238.695894	30.162701
416.167264	20288.832320	30.167719
416.495359	20328.118156	30.172736
416.920300	20360.111891	30.177754
417.444467	20404.558889	30.182772
418.194032	20447.472471	30.187789
418.400809	20482.200176	30.192807
418.721296	20520.705704	30.197824
419.397689	20551.841488	30.202842
419.882608	20593.238353	30.207860
420.528374	20627.288274	30.212877
421.042420	20658.460582	30.217895
421.275093	20689.301112	30.222912
421.680958	20708.798878	30.227930
421.890796	20743.212858	30.232948
422.562741	20769.753791	30.237965
422.734861	20800.070053	30.242983
422.904536	20833.771901	30.248000
423.096178	20861.535555	30.253018
423.680523	20909.346447	30.258036
424.025145	20939.128296	30.263053
424.522599	20974.827453	30.268071
424.636161	21005.115933	30.273088
425.191233	21054.270693	30.278106
425.193519	21092.278341	30.283124
425.819877	21135.616125	30.288141
426.584144	21182.381041	30.293159
426.758324	21211.182481	30.298176
427.395870	21255.650803	30.303194
427.596270	21297.340872	30.308212
428.157720	21340.045044	30.313229
428.470695	21382.448294	30.318247
428.972193	21433.312737	30.323264
429.692720	21470.089200	30.328282
430.350295	21518.132515	30.333300
430.436444	21549.181765	30.338317
431.331818	21593.884241	30.343335
431.594898	21634.330173	30.348352
432.463032	21665.459937	30.353370
432.534008	21699.189304	30.358388
433.033718	21732.792602	30.363405
433.475911	21758.386062	30.368423
433.798290	21799.670875	30.373440
434.463385	21834.587259	30.378458
434.675705	21873.104311	30.383476
435.397169	21908.661151	30.388493
435.436230	21941.970552	30.393511
435.753040	21998.256695	30.398528
436.067833	22025.934078	30.403546
436.389296	22074.053516	30.408564
436.846981	22119.849999	30.413581
437.306921	22158.553780	30.418599
437.649033	22205.618446	30.423616
438.499416	22247.699985	30.428634
438.681952	22298.088424	30.433652
439.370843	22332.166186	30.438669
439.809663	22367.695076	30.443687
440.259896	22418.881596	30.448704
440.888549	22442.679190	30.453722
441.725202	22494.713399	30.458740
441.341435	22532.925345	30.463757
442.069500	22570.201233	30.468775
442.513006	22611.597278	30.473792
443.161740	22656.322877	30.478810
443.522188	22700.415101	30.483828
443.916075	22744.225955	30.488845
444.587471	22782.293808	30.493863
444.726785	22820.131270	30.498880
445.432422	22857.663799	30.503898
445.590042	22895.755429	30.508916
446.150740	22943.057188	30.513933
446.722780	22966.297211	30.518951
446.649057	23015.035039	30.523968
447.595770	23045.266556	30.528986
447.926940	23093.429849	30.534004
448.497604	23127.881996	30.539021
449.148536	23170.594896	30.544039
449.058342	23212.137488	30.549056
449.638458	23242.351178	30.554074
449.820686	23294.027790	30.559092
450.547485	23335.520639	30.564109
451.106377	23365.750674	30.569127
451.937779	23405.990085	30.574144
452.011787	23434.502798	30.579162
452.702204	23463.635784	30.584180
453.072708	23504.683391	30.589197
453.852822	23524.597126	30.594215
453.778458	23562.946251	30.599232
454.478604	23591.585844	30.604250
454.692552	23628.960171	30.609268
454.860766	23664.132853	30.614285
455.179383	23693.111717	30.619303
455.540911	23747.607991	30.624320
455.863550	23777.213958	30.629338
456.492084	23832.155172	30.634356
456.742120	23885.074454	30.639373
457.445987	23926.009561	30.644391
457.973854	23978.971468	30.649408
458.323793	24014.887516	30.654426
458.843708	24062.148665	30.659444
459.153317	24109.268124	30.664461
459.784438	24162.547834	30.669479
460.068269	24205.060715	30.674496
460.555417	24253.349704	30.679514
461.082174	24299.052305	30.684532
461.576237	24349.346364	30.689549
462.463887	24384.423553	30.694567
462.778718	24442.515880	30.699584
463.214681	24482.313893	30.704602
463.831235	24518.341425	30.709620
463.876130	24574.179574	30.714637
464.260052	24602.455281	30.719655
465.202335	24658.911642	30.724672
465.554988	24707.854982	30.729690
465.940817	24748.444119	30.734708
466.284543	24792.361573	30.739725
466.816219	24831.759760	30.744743
467.618353	24891.195466	30.749760
468.054348	24927.446137	30.754778
468.636487	24964.937504	30.759796
468.604795	25016.367687	30.764813
469.390227	25064.171177	30.769831
469.628745	25110.740561	30.774848
470.369215	25158.851399	30.779866
470.931704	25199.093798	30.784884
471.382170	25251.665560	30.789901
471.923441	25285.669567	30.794919
472.315117	25333.579969	30.799936
472.873905	25373.842316	30.804954
473.441916	25410.371810	30.809972
473.683097	25463.634925	30.814989
474.375724	25490.681338	30.820007
474.849416	25544.549688	30.825024
474.841908	25592.290298	30.830042
475.578118	25640.974108	30.835060
475.708185	25690.628931	30.840077
476.605656	25727.580873	30.845095
477.300892	25772.448873	30.850112
477.852489	25816.274614	30.855130
478.458730	25847.698248	30.860148
478.692651	25893.097115	30.865165
479.327051	25926.651688	30.870183
479.794027	25966.403846	30.875200
480.600340	26003.929779	30.880218
481.014336	26035.653685	30.885236
481.398158	26069.262618	30.890253
481.775153	26105.219566	30.895271
482.085416	26145.020148	30.900288
482.380394	26181.265254	30.905306
483.404742	26217.049074	30.910324
483.374877	26252.751910	30.915341
483.942172	26284.504531	30.920359
484.076172	26324.852010	30.925376
484.363873	26368.129800	30.930394
485.168870	26404.164803	30.935412
485.165648	26459.332519	30.940429
485.849240	26493.744360	30.945447
486.198366	26557.064986	30.950464
486.843195	26597.580925	30.955482
487.304135	26634.673293	30.960500
487.382319	26688.724220	30.965517
488.180516	26726.767243	30.970535
488.658860	26777.171939	30.975552
488.793388	26839.604854	30.980570
489.392165	26888.478958	30.985588
489.988093	26938.634391	30.990605
490.665901	26987.120314	30.995623
491.041761	27051.867307	31.000640
491.485957	27106.190193	31.005658
492.271225	27154.412750	31.010676
492.572758	27200.434763	31.015693
493.358328	27243.730148	31.020711
493.862091	27292.602188	31.025728
494.474196	27341.311328	31.030746
494.598319	27392.000399	31.035764
495.563774	27443.859549	31.040781
495.996927	27482.614480	31.045799
496.423265	27538.897514	31.050816
496.597798	27584.566164	31.055834
497.713041	27631.240168	31.060852
497.754093	27688.126876	31.065869
498.327187	27736.449254	31.070887
498.907085	27784.704392	31.075904
499.344313	27828.339640	31.080922
500.021664	27873.578836	31.085940
499.701898	27928.380871	31.090957
500.759782	27977.999134	31.095975
501.456178	28038.551531	31.100992
501.892530	28083.843771	31.106010
502.868910	28136.655898	31.111028
502.955697	28179.290035	31.116045
503.734332	28225.809972	31.121063
503.937762	28269.948756	31.126080
504.620249	28327.917590	31.131098
505.013278	28365.905065	31.136116
505.061782	28435.184794	31.141133
505.878255	28470.950892	31.146151
506.450349	28528.834553	31.151168
506.587079	28578.679511	31.156186
507.001617	28629.686926	31.161204
507.209788	28686.009766	31.166221
508.143071	28747.689548	31.171239
508.542960	28793.538602	31.176256
509.154032	28863.099208	31.181274
509.829914	28914.149390	31.186292
510.238075	28973.872528	31.191309
510.856698	29025.923134	31.196327
511.420797	29072.266298	31.201344
511.759413	29127.442687	31.206362
512.860422	29182.723406	31.211380
512.954603	29241.045007	31.216397
513.246221	29288.872464	31.221415
513.776769	29345.103068	31.226432
514.458043	29400.173139	31.231450
515.420492	29447.009805	31.236468
515.567478	29501.171642	31.241485
516.108491	29536.436544	31.246503
516.730246	29589.378003	31.251520
517.540968	29631.548845	31.256538
517.895406	29665.172746	31.261556
518.283522	29713.856169	31.266573
518.588880	29759.922158	31.271591
519.234514	29805.181075	31.276608
519.777456	29854.984535	31.281626
520.551861	29896.357498	31.286644
521.180495	29941.622736	31.291661
521.548631	29990.029433	31.296679
521.765614	30030.794530	31.301696
521.965789	30081.024487	31.306714
522.766420	30132.442495	31.311732
523.272093	30191.368037	31.316749
523.415103	30238.926096	31.321767
524.278271	30298.654180	31.326784
524.530099	30348.876354	31.331802
525.219468	30400.395589	31.336820
525.422144	30451.323467	31.341837
526.268080	30513.175367	31.346855
526.698475	30560.080958	31.351872
527.045110	30618.201288	31.356890
527.797912	30678.598883	31.361908
528.254404	30746.618112	31.366925
529.039699	30813.961627	31.371943
529.301577	30863.530483	31.376960
529.881833	30926.301782	31.381978
530.602246	30970.664716	31.386996
530.887173	31025.322716	31.392013
531.569226	31080.606170	31.397031
532.197349	31141.915756	31.402048
532.494677	31200.352220	31.407066
533.238660	31257.030065	31.412084
533.566363	31322.255176	31.417101
534.313645	31382.103922	31.422119
535.205456	31431.330340	31.427136
535.573479	31498.843326	31.432154
536.201491	31546.902079	31.437172
536.771784	31600.164167	31.442189
537.053642	31649.567844	31.447207
537.736440	31698.482504	31.452224
538.449342	31773.805729	31.457242
538.747220	31817.344586	31.462260
539.347073	31877.522317	31.467277
539.853806	31938.605477	31.472295
540.622198	31987.639300	31.477312
540.820796	32055.822985	31.482330
541.423286	32094.254015	31.487348
542.008193	32170.691876	31.492365
542.518715	32218.686696	31.497383
543.178999	32271.503619	31.502400
543.285336	32328.407152	31.507418
544.055223	32388.164051	31.512436
544.627350	32441.731289	31.517453
545.533213	32498.402102	31.522471
546.146567	32557.529133	31.527488
546.607726	32612.320643	31.532506
547.147425	32673.104259	31.537524
547.710905	32722.505347	31.542541
548.209438	32784.372187	31.547559
548.860638	32830.824421	31.552576
549.384770	32893.280644	31.557594
550.064180	32936.528762	31.562612
550.400658	32986.596099	31.567629
550.971627	33041.153026	31.572647
551.946777	33099.328969	31.577664
551.994098	33154.597691	31.582682
552.715146	33195.270895	31.587700
553.246047	33249.412240	31.592717
553.415107	33294.358185	31.597735
554.113722	33339.582678	31.602752
554.569096	33396.933617	31.607770
555.143497	33450.954774	31.612788
555.198758	33505.879304	31.617805
555.680801	33561.399234	31.622823
556.421831	33608.794802	31.627840
556.772661	33680.190926	31.632858
557.546481	33735.849308	31.637876
558.389597	33802.557154	31.642893
558.415638	33862.224331	31.647911
559.603635	33917.439221	31.652928
560.084451	33975.478913	31.657946
560.496820	34028.392559	31.662964
561.356105	34083.110092	31.667981
561.698555	34150.255518	31.672999
562.752719	34194.770107	31.678016
563.104645	34261.488352	31.683034
563.628874	34306.586359	31.688052
564.165582	34362.390065	31.693069
564.626867	34422.675061	31.698087
565.745838	34470.023005	31.703104
565.747726	34530.595814	31.708122
566.583340	34591.131870	31.713140
567.014954	34644.523841	31.718157
567.529462	34710.292189	31.723175
568.074874	34758.531073	31.728192
568.790107	34816.449495	31.733210
569.198753	34877.120278	31.738228
570.055956	34938.745877	31.743245
569.963541	35002.150947	31.748263
570.719328	35058.820008	31.753280
571.574758	35129.867007	31.758298
571.744981	35183.969732	31.763316
572.600019	35238.492672	31.768333
573.016674	35320.018225	31.773351
573.746505	35373.940565	31.778368
574.151309	35439.174277	31.783386
574.977113	35509.198822	31.788404
575.353118	35570.691593	31.793421
575.955371	35639.453351	31.798439
576.801407	35693.404763	31.803456
577.116226	35770.776918	31.808474
577.613258	35834.904807	31.813492
578.329630	35890.844491	31.818509
578.868075	35963.462141	31.823527
579.638373	36021.100750	31.828544
579.921056	36086.186577	31.833562
580.799692	36156.245923	31.838580
581.553250	36205.647261	31.843597
581.943996	36283.248914	31.848615
582.326724	36340.665458	31.853632
582.814302	36409.057757	31.858650
583.567851	36477.216939	31.863668
584.589111	36537.709890	31.868685
585.037678	36609.353961	31.873703
585.799326	36666.699379	31.878720
586.020515	36722.044979	31.883738
586.753429	36780.673781	31.888756
587.422380	36835.049275	31.893773
587.727699	36911.004413	31.898791
588.495894	36974.457072	31.903808
588.637522	37040.062039	31.908826
589.433006	37102.516405	31.913844
590.268196	37163.884962	31.918861
590.602308	37226.479214	31.923879
591.494605	37290.818307	31.928896
592.021514	37337.763587	31.933914
592.680340	37399.831263	31.938932
593.413167	37443.911514	31.943949
593.498506	37496.198201	31.948967
594.201805	37551.403437	31.953984
594.797609	37616.442949	31.959002
595.030171	37678.752546	31.964020
595.876252	37738.233725	31.969037
596.386707	37808.051045	31.974055
597.078305	37862.116541	31.979072
597.600213	37939.880332	31.984090
598.221833	37998.802933	31.989108
599.275672	38057.303850	31.994125
599.358502	38122.363754	31.999143
599.979965	38177.211965	32.004160
600.429942	38244.070721	32.009178
600.996589	38309.938219	32.014196
601.840167	38369.418717	32.019213
602.303222	38448.327598	32.024231
603.021505	38509.388602	32.029248
603.719018	38580.311124	32.034266
604.088714	38645.710527	32.039284
605.047608	38710.602331	32.044301
605.355827	38773.095695	32.049319
605.934663	38838.293887	32.054336
606.826999	38903.026930	32.059354
606.809275	38978.924176	32.064372
607.720327	39041.883756	32.069389
608.436308	39123.600975	32.074407
609.017557	39190.924439	32.079424
609.986459	39259.591885	32.084442
610.590323	39328.042195	32.089460
611.577709	39391.451222	32.094477
611.778105	39451.786629	32.099495
612.400434	39521.090068	32.104512
613.326845	39593.007728	32.109530
613.627506	39663.296152	32.114548
614.440730	39730.766309	32.119565
614.609740	39787.588246	32.124583
615.651265	39863.310744	32.129600
616.692513	39930.816517	32.134618
617.323442	39994.965310	32.139636
617.772990	40047.820913	32.144653
617.787132	40119.468551	32.149671
618.314588	40187.016071	32.154688
618.990872	40249.860797	32.159706
619.387612	40326.537906	32.164724
620.017516	40405.866400	32.169741
620.746987	40480.200381	32.174759
621.228947	40550.730530	32.179776
622.251152	40619.286907	32.184794
622.682117	40692.635669	32.189812
623.937340	40763.764792	32.194829
624.014049	40841.008405	32.199847
624.837530	40906.950065	32.204864
625.616549	40977.176986	32.209882
625.822047	41053.191064	32.214900
626.862261	41119.804788	32.219917
627.243225	41190.796067	32.224935
628.234804	41255.536761	32.229952
628.780574	41316.847154	32.234970
629.196691	41396.070045	32.239988
629.992027	41446.731984	32.245005
630.586560	41534.724603	32.250023
630.745621	41598.805496	32.255040
631.943120	41669.104721	32.260058
632.194945	41737.227581	32.265076
632.922025	41799.099949	32.270093
633.338870	41883.963371	32.275111
634.099807	41936.978072	32.280128
634.508478	41991.958106	32.285146
635.270947	42067.000200	32.290164
635.988772	42125.623337	32.295181
636.194236	42199.631014	32.300199
636.621436	42271.540668	32.305216
637.764142	42341.819937	32.310234
638.363971	42420.874733	32.315252
639.212514	42487.228307	32.320269
639.773520	42563.464430	32.325287
640.255084	42627.160846	32.330304
641.072284	42699.866401	32.335322
641.280802	42776.783688	32.340340
642.195912	42842.546580	32.345357
642.770588	42916.982243	32.350375
643.266340	43008.518545	32.355392
644.235484	43068.012374	32.360410
644.741353	43141.664676	32.365428
645.666426	43222.307712	32.370445
645.926920	43299.272226	32.375463
646.669845	43378.550524	32.380480
647.385030	43437.089818	32.385498
647.613513	43525.730199	32.390516
648.433407	43593.611151	32.395533
649.285917	43686.386283	32.400551
650.066019	43761.407020	32.405568
650.602391	43847.162620	32.410586
651.264994	43917.659867	32.415604
652.012423	43996.078051	32.420621
652.420563	44067.470474	32.425639
653.124651	44152.151441	32.430656
654.093018	44226.527184	32.435674
654.550086	44315.878653	32.440692
655.432663	44384.768822	32.445709
655.980936	44461.011626	32.450727
657.016706	44541.228391	32.455744
657.740780	44612.955843	32.460762
657.956489	44689.428255	32.465780
658.867149	44763.522017	32.470797
659.540290	44844.851547	32.475815
660.175219	44916.819095	32.480832
661.097240	44995.019951	32.485850
661.555946	45071.191630	32.490868
662.272883	45143.515921	32.495885
662.913183	45211.527164	32.500903
663.393570	45294.415674	32.505920
664.254129	45362.469965	32.510938
664.846707	45446.584715	32.515956
665.328702	45517.597808	32.520973
665.957499	45598.091653	32.525991
666.754054	45679.862238	32.531008
667.156947	45756.222746	32.536026
668.056386	45843.556778	32.541044
668.758338	45920.373719	32.546061
669.672435	45999.126344	32.551079
670.196802	46075.152263	32.556096
670.527322	46149.391649	32.561114
671.274653	46225.378129	32.566132
672.113699	46301.908680	32.571149
672.625116	46391.163085	32.576167
673.334463	46472.983100	32.581184
674.071377	46535.624203	32.586202
674.878725	46630.574977	32.591220
675.568114	46710.457207	32.596237
676.335317	46780.237316	32.601255
676.894073	46852.884837	32.606272
677.557420	46927.072204	32.611290
678.251225	47007.169691	32.616308
678.998132	47061.271737	32.621325
679.555780	47129.846712	32.626343
680.289850	47203.887666	32.631360
681.079735	47278.257581	32.636378
681.577876	47344.266235	32.641396
682.005864	47417.584938	32.646413
682.831749	47491.561293	32.651431
683.163360	47576.044454	32.656448
684.110300	47641.683037	32.661466
684.535043	47725.535629	32.666484
685.576143	47805.812720	32.671501
685.803150	47886.218503	32.676519
686.300953	47972.305509	32.681536
686.868014	48054.850645	32.686554
687.839897	48137.512343	32.691572
688.826869	48215.099888	32.696589
689.553420	48300.120966	32.701607
690.275478	48382.183938	32.706624
690.833886	48465.528141	32.711642
691.701557	48557.636143	32.716660
692.215390	48635.483678	32.721677
692.959012	48715.327429	32.726695
693.477940	48808.208088	32.731712
694.771470	48890.387145	32.736730
695.301995	48981.564413	32.741748
695.675504	49063.962731	32.746765
696.667476	49148.466759	32.751783
697.410852	49229.677082	32.756800
698.222865	49309.098246	32.761818
698.413594	49394.364409	32.766836
699.281097	49470.293389	32.771853
700.427635	49563.648699	32.776871
700.936188	49643.936307	32.781888
701.527125	49726.753144	32.786906
702.063186	49824.957803	32.791924
703.000728	49898.921819	32.796941
703.657439	49988.140535	32.801959
704.466484	50070.186846	32.806976
705.314940	50155.641307	32.811994
705.782311	50238.436561	32.817012
706.243599	50330.771879	32.822029
706.933536	50413.404724	32.827047
707.786715	50513.831404	32.832064
708.698889	50598.569769	32.837082
709.380547	50684.471088	32.842100
710.173623	50765.445918	32.847117
711.203057	50859.654414	32.852135
711.916719	50944.660867	32.857152
712.589157	51013.635016	32.862170
713.181317	51097.872583	32.867188
713.863653	51192.550736	32.872205
714.406632	51272.330861	32.877223
715.025181	51365.940146	32.882240
715.862705	51451.225244	32.887258
716.532794	51529.071227	32.892276
717.167164	51618.907617	32.897293
718.203067	51713.637217	32.902311
718.153853	51807.801309	32.907328
719.193005	51882.239378	32.912346
719.639646	51982.892523	32.917364
720.544874	52077.942436	32.922381
721.350081	52171.385728	32.927399
721.703997	52267.551215	32.932416
722.374125	52360.278590	32.937434
723.375722	52450.165463	32.942452
724.011794	52548.041980	32.947469
724.919870	52631.766406	32.952487
725.447097	52720.734784	32.957504
726.532795	52799.142548	32.962522
727.094399	52894.834515	32.967540
727.545549	52977.959995	32.972557
728.721606	53053.504467	32.977575
729.442081	53150.264399	32.982592
730.094611	53227.248180	32.987610
730.568681	53309.947971	32.992628
731.194355	53396.388571	32.997645
732.062035	53488.349400	33.002663
732.280992	53583.956089	33.007680
733.277110	53672.630090	33.012698
734.388760	53762.188873	33.017716
734.872506	53852.199427	33.022733
735.612116	53940.841249	33.027751
736.242139	54044.918059	33.032768
736.989245	54135.189617	33.037786
737.585835	54229.365912	33.042804
738.489309	54327.074378	33.047821
739.165982	54420.252680	33.052839
739.722135	54520.591122	33.057856
740.795473	54623.725719	33.062874
741.077745	54727.092801	33.067892
742.044718	54833.733869	33.072909
742.910646	54920.912267	33.077927
743.422741	55025.696148	33.082944
744.576131	55124.871032	33.087962
745.221801	55221.160653	33.092980
746.097484	55335.408164	33.097997
746.897075	55435.483504	33.103015
747.688575	55541.734057	33.108032
748.385549	55640.430971	33.113050
749.300570	55730.675715	33.118068
749.696211	55833.593815	33.123085
750.878388	55934.891103	33.128103
751.588597	56039.514869	33.133120
752.434390	56134.208736	33.138138
752.943635	56231.025009	33.143156
753.468559	56334.372955	33.148173
754.783717	56431.966828	33.153191
755.206545	56532.495464	33.158208
755.922077	56622.195898	33.163226
756.597810	56726.854250	33.168244
757.359234	56837.249367	33.173261
758.425427	56933.610416	33.178279
759.198309	57041.401278	33.183296
759.969155	57134.336600	33.188314
760.894492	57231.651307	33.193332
761.296172	57334.765722	33.198349
762.355937	57430.169696	33.203367
762.979377	57535.580285	33.208384
763.905628	57632.018398	33.213402
764.596874	57730.694995	33.218420
765.277866	57825.841215	33.223437
765.905237	57919.865573	33.228455
766.818103	58026.836009	33.233472
767.187952	58124.038382	33.238490
768.454558	58228.865942	33.243508
769.390648	58332.882934	33.248525
770.172915	58428.944234	33.253543
771.095228	58524.685806	33.258560
772.163024	58627.734590	33.263578
772.824339	58704.668605	33.268596
773.367995	58803.463349	33.273613
774.524165	58898.763554	33.278631
774.831747	58994.343603	33.283648
775.798785	59083.741682	33.288666
776.636917	59174.381209	33.293684
777.145227	59260.721303	33.298701
778.073112	59336.703572	33.303719
778.700299	59433.812807	33.308736
779.333488	59520.070153	33.313754
779.863315	59610.364469	33.318772
780.706133	59699.867977	33.323789
781.311748	59793.297938	33.328807
782.085050	59895.984774	33.333824
782.766010	59995.628474	33.338842
783.705786	60074.961200	33.343860
784.205220	60185.525436	33.348877
785.106345	60283.686816	33.353895
785.877884	60382.824457	33.358912
786.155350	60490.254311	33.363930
787.585151	60591.831156	33.368948
787.912837	60707.160527	33.373965
788.897785	60801.442502	33.378983
789.703126	60906.613038	33.384000
790.245690	61026.712165	33.389018
791.149020	61135.369185	33.394036
791.592738	61242.238258	33.399053
792.739186	61356.803824	33.404071
793.681654	61474.785269	33.409088
794.566291	61576.615202	33.414106
795.468994	61691.311445	33.419124
796.140048	61806.217302	33.424141
797.036573	61909.532279	33.429159
798.141710	62021.194557	33.434176
798.743234	62128.225450	33.439194
799.514288	62230.848552	33.444212
800.016715	62341.771594	33.449229
800.651897	62449.348504	33.454247
801.622351	62558.583485	33.459264
802.216004	62681.408154	33.464282
803.221223	62789.918027	33.469300
804.278672	62912.591512	33.474317
805.168138	63016.576924	33.479335
805.938262	63141.416839	33.484352
806.436518	63250.278468	33.489370
807.746627	63365.340175	33.494388
808.326010	63482.653617	33.499405
809.486765	63582.304930	33.504423
810.221833	63700.984526	33.509440
810.956483	63804.032356	33.514458
812.191233	63915.670817	33.519476
812.742874	64032.486257	33.524493
813.409617	64134.567154	33.529511
814.615427	64244.960543	33.534528
815.197282	64361.696980	33.539546
816.099272	64460.187918	33.544564
817.099928	64571.501981	33.549581
817.835068	64681.874393	33.554599
818.558338	64783.866949	33.559616
819.001869	64895.799581	33.564634
820.418334	65010.264915	33.569652
821.036125	65115.310926	33.574669
822.118230	65218.769784	33.579687
822.708828	65331.603398	33.584704
823.557401	65442.163370	33.589722
824.102287	65543.708689	33.594740
824.731705	65658.895680	33.599757
825.868591	65769.169466	33.604775
826.654727	65876.726530	33.609792
827.230363	65990.615607	33.614810
828.244425	66102.169527	33.619828
828.930042	66217.040515	33.624845
829.536935	66332.481491	33.629863
830.872808	66441.587939	33.634880
831.487799	66542.848331	33.639898
832.140905	66642.471796	33.644916
832.921416	66753.954007	33.649933
833.889535	66854.613790	33.654951
834.771063	66968.084564	33.659968
835.448472	67071.069465	33.664986
836.492982	67179.058310	33.670004
837.091917	67285.521853	33.675021
837.970987	67396.491698	33.680039
838.753787	67495.010299	33.685056
839.497151	67624.269169	33.690074
840.204912	67725.949824	33.695092
840.822139	67857.228874	33.700109
841.380382	67969.177870	33.705127
842.071261	68088.275307	33.710144
842.957010	68216.667020	33.715162
844.161502	68342.395543	33.720180
845.002301	68471.011199	33.725197
845.863062	68594.882296	33.730215
846.992035	68720.910073	33.735232
847.561360	68848.573916	33.740250
848.368089	68974.485775	33.745268
849.674051	69099.658234	33.750285
850.393620	69223.366653	33.755303
851.081424	69339.171050	33.760320
851.779555	69470.838703	33.765338
852.470203	69587.314209	33.770356
853.202826	69720.046281	33.775373
854.253166	69861.237508	33.780391
855.623856	69982.534709	33.785408
856.506165	70110.249177	33.790426
857.582351	70232.677763	33.795444
858.177911	70359.138559	33.800461
859.066311	70481.574329	33.805479
860.013205	70608.553906	33.810496
860.769492	70746.296479	33.815514
862.106482	70862.861722	33.820532
863.074106	70987.083112	33.825549
863.688334	71108.062819	33.830567
864.800261	71226.526350	33.835584
865.153390	71362.524697	33.840602
866.318100	71478.400882	33.845620
867.634213	71606.545730	33.850637
868.381110	71727.627118	33.855655
869.355805	71841.677529	33.860672
869.572439	71968.665738	33.865690
870.812974	72079.872038	33.870708
871.543306	72211.083179	33.875725
872.164712	72347.220411	33.880743
873.228174	72462.157391	33.885760
874.317589	72589.978769	33.890778
875.221528	72721.170607	33.895796
876.177106	72840.358139	33.900813
876.775545	72969.951447	33.905831
877.816313	73093.262171	33.910848
878.332102	73229.422392	33.915866
879.762793	73341.761013	33.920884
880.521735	73472.348945	33.925901
881.490506	73600.145614	33.930919
882.472049	73712.206268	33.935936
883.121328	73849.644743	33.940954
883.922856	73970.021264	33.945972
884.917844	74094.211641	33.950989
885.752264	74212.155512	33.956007
886.989618	74339.766624	33.961024
887.482282	74469.879620	33.966042
888.584435	74587.699017	33.971060
889.482837	74696.217782	33.976077
890.428498	74821.508248	33.981095
891.431142	74924.780514	33.986112
891.830431	75048.847123	33.991130
892.581841	75154.135288	33.996148
893.192732	75270.818934	34.001165
894.242009	75386.621139	34.006183
895.170335	75508.231081	34.011200
896.030247	75635.191110	34.016218
896.791020	75758.322784	34.021236
897.667348	75879.431060	34.026253
898.508467	76007.300785	34.031271
899.485245	76134.048280	34.036288
900.201173	76267.974177	34.041306
901.135937	76391.352571	34.046324
902.009561	76525.178042	34.051341
902.993909	76673.128844	34.056359
904.453629	76790.028004	34.061376
904.778444	76917.204043	34.066394
905.575013	77050.564710	34.071412
906.501522	77184.657387	34.076429
907.311711	77311.831313	34.081447
908.529122	77442.335297	34.086464
909.377247	77597.297877	34.091482
910.549263	77725.793248	34.096500
911.654259	77858.886354	34.101517
912.434504	77997.467507	34.106535
913.287284	78117.662020	34.111552
914.169970	78255.588957	34.116570
915.358155	78393.567430	34.121588
915.969456	78523.570702	34.126605
917.147517	78663.595675	34.131623
918.112338	78792.201008	34.136640
919.343331	78925.355517	34.141658
920.239842	79055.143904	34.146676
920.982956	79185.730151	34.151693
922.227950	79315.993778	34.156711
923.361701	79438.932250	34.161728
924.167208	79570.933723	34.166746
924.806785	79703.387244	34.171764
925.828292	79828.712292	34.176781
926.641625	79964.516667	34.181799
927.977548	80083.003345	34.186816
929.108870	80208.805769	34.191834
929.670300	80338.422875	34.196852
930.636591	80471.820058	34.201869
931.515487	80607.706009	34.206887
932.649691	80726.615306	34.211904
933.656409	80857.983687	34.216922
934.334160	80988.407675	34.221940
935.525990	81122.385028	34.226957
935.958743	81248.884424	34.231975
937.006138	81383.386977	34.236992
937.965984	81514.830160	34.242010
938.525613	81647.390472	34.247028
939.975696	81771.617823	34.252045
940.806076	81910.347503	34.257063
941.765660	82042.065801	34.262080
942.652573	82173.044008	34.267098
943.362844	82313.858464	34.272116
944.509760	82449.495949	34.277133
945.237537	82586.101940	34.282151
946.533031	82717.477540	34.287168
947.379384	82857.893222	34.292186
948.318897	82997.623711	34.297204
949.068154	83127.782327	34.302221
949.885521	83266.655211	34.307239
950.934469	83396.784769	34.312256
952.100301	83530.160450	34.317274
952.813042	83667.464975	34.322292
954.138406	83780.714815	34.327309
954.843800	83912.239091	34.332327
955.669942	84034.335730	34.337344
956.691442	84156.134967	34.342362
957.288990	84291.602059	34.347380
958.430444	84420.513584	34.352397
959.400324	84558.862822	34.357415
960.567470	84688.581476	34.362432
960.935619	84819.546583	34.367450
961.990598	84951.885783	34.372468
963.112784	85091.111485	34.377485
963.811351	85230.800369	34.382503
964.863325	85371.735110	34.387520
965.787284	85515.786024	34.392538
966.487236	85656.603522	34.397556
967.683596	85797.738420	34.402573
968.110008	85957.667997	34.407591
969.508234	86109.623288	34.412608
970.588242	86253.792146	34.417626
971.346276	86392.649196	34.422644
972.491257	86542.611631	34.427661
973.325412	86689.139784	34.432679
974.841949	86839.618506	34.437696
974.872898	87012.364980	34.442714
974.976751	87197.484487	34.447732
976.556920	87335.901081	34.452749
979.637117	87448.714007	34.457767
979.637769	87633.594544	34.462784
980.361635	87789.551295	34.467802
981.454768	87932.968872	34.472820
982.192219	88086.488986	34.477837
984.546704	88209.436768	34.482855
984.985836	88383.473656	34.487872
985.672405	88536.448202	34.492890
986.914959	88666.796504	34.497908
986.968656	88850.506984	34.502925
988.639016	88991.506646	34.507943
989.299077	89148.482749	34.512960
990.119192	89303.110849	34.517978
991.745548	89455.790336	34.522996
992.108397	89629.260359	34.528013
993.855611	89756.765562	34.533031
995.513880	89903.519017	34.538048
996.161973	90063.914260	34.543066
998.035689	90185.736619	34.548084
999.248512	90319.718898	34.553101
999.064481	90477.919167	34.558119
1000.576309	90613.290285	34.563136
1000.871931	90765.805753	34.568154
1001.753220	90917.877251	34.573172
1003.446927	91047.334810	34.578189
1003.902563	91216.845312	34.583207
1004.498937	91367.473098	34.588224
1005.064389	91533.499328	34.593242
1006.719482	91686.852776	34.598260
1007.981046	91835.443091	34.603277
1009.392128	91983.642498	34.608295
1010.243794	92132.606209	34.613312
1011.638462	92273.366879	34.618330
1012.453042	92429.269128	34.623348
1012.919940	92576.064913	34.628365
1013.917307	92734.939019	34.633383
1015.027855	92875.452662	34.638400
1016.512420	93018.905453	34.643418
1017.291822	93176.869048	34.648436
1019.237783	93305.176604	34.653453
1019.585868	93453.548046	34.658471
1020.046066	93605.959151	34.663488
1020.779289	93744.115911	34.668506
1021.336995	93900.152287	34.673524
1022.613825	94029.327506	34.678541
1024.179998	94169.545361	34.683559
1025.035859	94308.672463	34.688576
1026.750931	94450.766249	34.693594
1026.937810	94593.664232	34.698612
1027.866049	94747.549508	34.703629
1028.584685	94899.039685	34.708647
1029.453138	95049.303314	34.713664
1030.526991	95215.333722	34.718682
1032.013852	95366.130030	34.723700
1033.183167	95519.011733	34.728717
1034.238327	95664.285390	34.733735
1035.132844	95817.486563	34.738752
1036.271519	95971.401610	34.743770
1036.754703	96138.592999	34.748788
1037.695533	96303.994319	34.753805
1038.958078	96469.387855	34.758823
1039.598341	96645.482503	34.763840
1040.886783	96803.125526	34.768858
1041.741949	96983.023277	34.773876
1042.345006	97156.196638	34.778893
1043.832843	97323.267814	34.783911
1044.825607	97490.073771	34.788928
1045.933025	97674.847344	34.793946
1047.222647	97848.443734	34.798964
1048.700845	98015.502110	34.803981
1050.020379	98193.337546	34.808999
1050.837146	98359.899802	34.814016
1051.662509	98527.411369	34.819034
1052.581062	98701.106625	34.824052
1053.377250	98878.805492	34.829069
1054.545054	99054.538521	34.834087
1055.487763	99235.007638	34.839104
1056.639375	99410.897754	34.844122
1057.648154	99599.006519	34.849140
1059.015220	99768.519657	34.854157
1060.265794	99949.595050	34.859175
1061.235232	100121.411205	34.864192
1062.402342	100293.955592	34.869210
1063.600439	100467.167145	34.874228
1064.892922	100639.389224	34.879245
1065.972220	100806.069688	34.884263
1066.599211	100982.715825	34.889280
1068.173876	101155.141638	34.894298
1069.093413	101330.716084	34.899316
1069.858695	101502.961464	34.904333
1070.974424	101687.712099	34.909351
1071.566908	101875.976027	34.914368
1073.103516	102037.985686	34.919386
1074.055415	102219.968569	34.924404
1074.942260	102400.418513	34.929421
1076.550694	102588.924889	34.934439
1077.396963	102765.527952	34.939456
1078.724821	102926.482247	34.944474
1079.684840	103103.923616	34.949492
1080.847649	103279.192427	34.954509
1082.350607	103455.558621	34.959527
1083.176615	103646.614544	34.964544
1084.365614	103809.699519	34.969562
1085.077984	103987.656413	34.974580
1085.969759	104177.438884	34.979597
1086.891575	104338.734960	34.984615
1087.927422	104533.359405	34.989632
1089.225569	104718.114017	34.994650
1090.333069	104902.952103	34.999668
1091.275532	105066.807537	35.004685
1092.541417	105231.522402	35.009703
1093.792132	105392.339936	35.014720
1095.135408	105551.749970	35.019738
1096.302293	105726.325164	35.024756
1097.319378	105880.750313	35.029773
1098.467703	106051.999724	35.034791
1099.111661	106213.682478	35.039808
1100.233230	106382.937287	35.044826
1101.140268	106557.687557	35.049844
1101.907960	106733.931239	35.054861
1103.095431	106911.360605	35.059879
1103.817018	107097.658345	35.064896
1104.709380	107284.562449	35.069914
1105.741870	107477.562434	35.074932
1106.973310	107681.322544	35.079949
1108.208822	107860.219531	35.084967
1109.468517	108063.357215	35.089984
1110.718805	108251.374178	35.095002
1111.883814	108435.403908	35.100020
1112.828324	108629.212019	35.105037
1114.494220	108825.460945	35.110055
1115.311540	109017.519515	35.115072
1116.816213	109201.688305	35.120090
1118.026282	109397.738059	35.125108
1118.740972	109584.484782	35.130125
1120.136129	109777.086547	35.135143
1120.631241	109977.742867	35.140160
1122.168046	110167.993190	35.145178
1123.096134	110362.614414	35.150196
1124.399167	110565.408960	35.155213
1125.779718	110759.020798	35.160231
1126.378964	110966.317670	35.165248
1127.895987	111156.274100	35.170266
1129.255823	111347.271263	35.175284
1130.468840	111547.845715	35.180301
1131.588575	111742.647715	35.185319
1132.978322	111950.695406	35.190336
1134.022209	112122.798522	35.195354
1134.853830	112325.405251	35.200372
1135.798015	112520.900503	35.205389
1136.935867	112721.964619	35.210407
1137.745123	112927.163819	35.215424
1139.252893	113121.037210	35.220442
1140.455689	113334.333023	35.225460
1141.562814	113532.937642	35.230477
1142.741986	113741.578299	35.235495
1144.150404	113940.934154	35.240512
1145.250349	114125.000012	35.245530
1146.498450	114342.894934	35.250548
1147.779908	114532.913366	35.255565
1149.237882	114723.436018	35.260583
1150.152343	114929.494001	35.265600
1151.418252	115118.784116	35.270618
1152.589482	115308.496581	35.275636
1153.871345	115511.393981	35.280653
1155.275309	115708.419147	35.285671
1156.482740	115895.456202	35.290688
1157.183880	116090.585673	35.295706
1158.337895	116288.137637	35.300724
1159.316440	116477.509652	35.305741
1160.620830	116678.333724	35.310759
1161.433218	116882.129396	35.315776
1162.856092	117075.030316	35.320794
1164.124004	117269.161858	35.325812
1164.892377	117467.545947	35.330829
1166.532822	117660.338808	35.335847
1167.584220	117864.076592	35.340864
1168.607773	118032.341771	35.345882
1170.166441	118217.523973	35.350900
1170.984724	118403.957481	35.355917
1172.386053	118589.636905	35.360935
1173.248764	118777.776082	35.365952
1173.910927	118955.217002	35.370970
1175.032780	119154.466561	35.375988
1176.328135	119354.651837	35.381005
1178.100903	119536.803915	35.386023
1179.183324	119727.485241	35.391040
1180.039037	119924.845288	35.396058
1180.637830	120120.829888	35.401076
1181.623959	120323.442548	35.406093
1182.597510	120541.670617	35.411111
1183.198621	120761.875361	35.416128
1184.433108	120982.737382	35.421146
1186.302696	121192.585213	35.426164
1188.070153	121408.268048	35.431181
1189.290629	121601.093002	35.436199
1190.841138	121818.081933	35.441216
1191.644822	122033.244312	35.446234
1192.903346	122250.892957	35.451252
1193.853215	122466.959416	35.456269
1195.236139	122679.648217	35.461287
1196.513405	122901.404542	35.466304
1197.092124	123117.955266	35.471322
1198.096144	123346.337403	35.476340
1199.230837	123565.422808	35.481357
1200.761371	123787.650748	35.486375
1202.115363	124015.029603	35.491392
1203.255293	124239.847469	35.496410
1204.876555	124454.347101	35.501428
1205.652098	124680.736643	35.506445
1207.679388	124901.673977	35.511463
1208.918440	125112.680086	35.516480
1210.316749	125338.147775	35.521498
1211.535591	125556.790084	35.526516
1212.135352	125784.344885	35.531533
1213.723914	125997.314543	35.536551
1214.658299	126224.639861	35.541568
1215.660376	126467.646727	35.546586
1216.921203	126681.359728	35.551604
1218.429211	126912.524442	35.556621
1219.632883	127134.247769	35.561639
1221.258444	127349.413410	35.566656
1222.575432	127571.438013	35.571674
1224.156533	127789.009627	35.576692
1225.238085	128004.510562	35.581709
1226.601547	128211.537359	35.586727
1227.723556	128431.901855	35.591744
1228.871026	128648.575152	35.596762
1229.966946	128862.330430	35.601780
1231.124831	129086.635688	35.606797
1232.377071	129311.712844	35.611815
1233.217133	129539.547006	35.616832
1234.373118	129762.070111	35.621850
1236.086354	129985.630837	35.626868
1237.264538	130203.083002	35.631885
1238.491387	130421.428621	35.636903
1239.658932	130654.667422	35.641920
1240.662371	130876.234828	35.646938
1242.171394	131095.983541	35.651956
1243.442000	131320.260652	35.656973
1244.955704	131536.094591	35.661991
1246.239298	131772.352086	35.667008
1247.113952	132000.984126	35.672026
1248.476330	132215.225027	35.677044
1249.107026	132443.786448	35.682061
1250.357743	132662.447674	35.687079
1251.858840	132878.482868	35.692096
1253.111568	133083.886375	35.697114
1254.501522	133296.494539	35.702132
1255.352287	133507.874775	35.707149
1256.828553	133720.902481	35.712167
1258.273383	133937.740031	35.717184
1259.134197	134163.625935	35.722202
1260.570441	134377.032193	35.727220
1261.867773	134601.365681	35.732237
1263.015723	134820.540153	35.737255
1264.464782	135036.889850	35.742272
1265.401980	135270.795885	35.747290
1267.058552	135489.244163	35.752308
1268.370296	135718.273782	35.757325
1269.301999	135940.813129	35.762343
1270.660141	136168.938037	35.767360
1271.785747	136390.243904	35.772378
1273.143796	136630.720809	35.777396
1274.074882	136867.910182	35.782413
1275.928770	137101.221169	35.787431
1276.864679	137336.435186	35.792448
1278.202395	137570.456017	35.797466
1279.471130	137809.219142	35.802484
1280.734674	138056.669987	35.807501
1282.108912	138292.198609	35.812519
1283.529435	138521.001215	35.817536
1284.401763	138774.252996	35.822554
1285.988693	138998.542831	35.827572
1287.552529	139250.010179	35.832589
1288.967315	139482.078845	35.837607
1290.094223	139722.971021	35.842624
1291.242116	139980.193000	35.847642
1292.833041	140202.841713	35.852660
1293.744729	140458.889049	35.857677
1295.281715	140701.000987	35.862695
1296.718771	140951.855087	35.867712
1297.734922	141195.654274	35.872730
1299.415440	141440.347117	35.877748
1300.477459	141680.680401	35.882765
1301.966570	141928.109243	35.887783
1303.434129	142167.174208	35.892800
1304.809596	142411.417068	35.897818
1305.923095	142652.357204	35.902836
1307.584155	142904.443739	35.907853
1308.732913	143140.511944	35.912871
1310.085178	143387.263570	35.917888
1311.208965	143632.215918	35.922906
1312.807158	143862.787149	35.927924
1313.787612	144121.132561	35.932941
1314.929381	144368.952997	35.937959
1316.642215	144608.716809	35.942976
1317.894602	144859.819557	35.947994
1319.170284	145101.611886	35.953012
1320.572812	145355.572029	35.958029
1321.553747	145597.353002	35.963047
1323.095683	145843.823958	35.968064
1324.360712	146091.255467	35.973082
1325.849454	146333.984688	35.978100
1327.353621	146586.249976	35.983117
1329.015992	146829.803524	35.988135
1330.364260	147063.962272	35.993152
1331.414394	147306.795840	35.998170
1332.814971	147536.713046	36.003188
1334.537655	147791.093892	36.008205
1335.659553	148025.651316	36.013223
1336.851662	148271.080429	36.018240
1338.628010	148505.012751	36.023258
1339.859978	148722.612155	36.028276
1340.887668	148943.772467	36.033293
1342.103414	149168.048414	36.038311
1343.618222	149391.819696	36.043328
1344.533884	149621.893431	36.048346
1346.217892	149842.925248	36.053364
1347.303064	150071.388323	36.058381
1348.356093	150305.020262	36.063399
1349.966501	150542.138291	36.068416
1351.244438	150786.973655	36.073434
1352.167083	151014.987339	36.078452
1353.222463	151260.230375	36.083469
1354.572351	151507.836255	36.088487
1355.939244	151765.080725	36.093504
1357.062773	152029.470201	36.098522
1358.474661	152274.749641	36.103540
1359.827153	152540.842533	36.108557
1360.866869	152801.623510	36.113575
1362.511026	153059.591909	36.118592
1363.596612	153330.402212	36.123610
1365.394637	153595.147625	36.128628
1366.428023	153859.310871	36.133645
1367.878421	154129.419548	36.138663
1369.198248	154400.262023	36.143680
1370.750076	154676.015139	36.148698
1372.277412	154940.446562	36.153716
1373.559584	155212.505946	36.158733
1374.741909	155490.089062	36.163751
1376.424004	155754.754079	36.168768
1377.627958	156041.305949	36.173786
1379.112097	156312.743312	36.178804
1380.649703	156592.672974	36.183821
1381.761580	156868.463337	36.188839
1383.719042	157146.665682	36.193856
1384.765833	157435.486205	36.198874
1386.207321	157708.919060	36.203892
1387.489161	157987.746301	36.208909
1388.562010	158276.061091	36.213927
1390.256917	158543.634816	36.218944
1391.874437	158836.671607	36.223962
1393.013419	159115.048109	36.228980
1394.422736	159389.208011	36.233997
1395.714884	159685.590417	36.239015
1397.435652	159970.676521	36.244032
1399.014656	160263.552246	36.249050
1400.459797	160532.854845	36.254068
1402.296450	160813.461874	36.259085
1403.353600	161097.079532	36.264103
1405.130173	161367.271585	36.269120
1406.317831	161650.934865	36.274138
1407.618429	161924.101809	36.279156
1408.951291	162208.214273	36.284173
1410.334709	162492.751660	36.289191
1411.900311	162767.834110	36.294208
1413.280856	163049.508350	36.299226
1414.621827	163329.922233	36.304244
1416.196744	163620.969610	36.309261
1417.444792	163907.644955	36.314279
1418.968579	164188.376806	36.319296
1420.273619	164471.722275	36.324314
1421.704971	164748.565165	36.329332
1423.187289	165042.517601	36.334349
1424.565796	165333.177565	36.339367
1426.390288	165609.136229	36.344384
1427.591209	165898.141756	36.349402
1429.302572	166170.189264	36.354420
1430.770203	166453.888681	36.359437
1431.804586	166735.707472	36.364455
1433.181534	166988.807819	36.369472
1435.001134	167265.602407	36.374490
1436.247302	167531.682623	36.379508
1437.656733	167796.278222	36.384525
1439.070059	168049.581588	36.389543
1440.418226	168314.190360	36.394560
1441.422871	168590.645603	36.399578
1442.893622	168859.868826	36.404596
1444.327726	169138.032922	36.409613
1445.606869	169411.224733	36.414631
1447.265094	169696.473902	36.419648
1448.363385	169988.327068	36.424666
1449.587666	170272.078022	36.429684
1451.408354	170551.354249	36.434701
1452.698730	170848.802618	36.439719
1454.504213	171126.168673	36.444736
1455.527581	171428.245876	36.449754
1456.834656	171719.783566	36.454772
1458.980930	172008.582943	36.459789
1460.064451	172304.145863	36.464807
1462.102185	172592.903304	36.469824
1463.309153	172897.294583	36.474842
1464.983346	173184.910121	36.479860
1466.610639	173480.885433	36.484877
1467.611309	173780.836715	36.489895
1469.411995	174074.540821	36.494912
1470.906291	174369.401427	36.499930
1472.157034	174668.301652	36.504948
1473.794931	174967.507776	36.509965
1475.052067	175276.157214	36.514983
1476.881423	175560.905805	36.520000
1478.176918	175872.420813	36.525018
1479.666219	176177.940941	36.530036
1481.342587	176476.109227	36.535053
1482.504965	176795.215989	36.540071
1484.131315	177095.274558	36.545088
1485.612899	177403.252913	36.550106
1486.819054	177707.636204	36.555124
1488.537189	178021.341199	36.560141
1490.043849	178329.143382	36.565159
1491.696431	178651.277676	36.570176
1493.202003	178964.300183	36.575194
1494.589124	179271.835893	36.580212
1495.938808	179576.028948	36.585229
1497.509038	179891.140588	36.590247
1498.865282	180205.883353	36.595264
1500.753448	180507.238708	36.600282
1502.110496	180829.181577	36.605300
1503.963839	181149.394414	36.610317
1504.939041	181459.397270	36.615335
1506.831612	181768.526896	36.620352
1508.209791	182091.463986	36.625370
1509.567031	182403.605044	36.630388
1511.020530	182716.887054	36.635405
1512.734999	183048.418096	36.640423
1514.250324	183360.525895	36.645440
1516.121863	183683.200633	36.650458
1517.631301	184007.612591	36.655476
1519.299351	184327.011877	36.660493
1520.847814	184650.558060	36.665511
1522.606048	184945.410133	36.670528
1524.284952	185257.666720	36.675546
1525.316969	185577.609890	36.680564
1527.095334	185878.188297	36.685581
1528.421042	186187.030426	36.690599
1530.496537	186501.868679	36.695616
1531.867927	186798.139945	36.700634
1533.197215	187098.202441	36.705652
1535.024621	187393.487512	36.710669
1536.384689	187678.861253	36.715687
1537.639446	187972.961836	36.720704
1539.260100	188252.532322	36.725722
1540.498299	188550.040559	36.730740
1542.099375	188837.474708	36.735757
1543.314700	189136.297204	36.740775
1545.247932	189435.078773	36.745792
1546.307691	189731.276894	36.750810
1547.163141	190040.496586	36.755828
1548.910459	190349.164309	36.760845
1549.879810	190673.601782	36.765863
1551.653944	190991.014891	36.770880
1553.196710	191333.692140	36.775898
1554.621946	191661.207868	36.780916
1556.280414	191982.314042	36.785933
1557.701136	192317.933300	36.790951
1558.882184	192653.822492	36.795968
1560.828993	192985.245307	36.800986
1562.226636	193332.108932	36.806004
1563.743536	193678.396192	36.811021
1565.115703	194025.788362	36.816039
1566.755828	194377.873501	36.821056
1568.501269	194720.510560	36.826074
1569.926916	195075.110573	36.831092
1571.725327	195419.596145	36.836109
1573.286701	195775.332873	36.841127
1574.691120	196129.320094	36.846144
1576.815906	196485.018396	36.851162
1578.259181	196843.306885	36.856180
1579.859158	197196.785105	36.861197
1581.262601	197564.085399	36.866215
1583.243406	197910.623318	36.871232
1584.783932	198275.492627	36.876250
1586.400261	198622.881570	36.881268
1587.997022	198980.407042	36.886285
1589.938563	199339.934206	36.891303
1591.387350	199693.602794	36.896320
1593.122177	200047.746479	36.901338
1594.722726	200416.057944	36.906356
1596.517883	200759.593764	36.911373
1597.998999	201108.871184	36.916391
1599.602207	201476.489429	36.921408
1601.110553	201833.256892	36.926426
1602.692825	202193.810231	36.931444
1604.378299	202556.532163	36.936461
1605.805563	202914.054757	36.941479
1607.477099	203276.668291	36.946496
1609.400546	203635.026594	36.951514
1609.906081	204012.056963	36.956532
1611.918435	204381.577559	36.961549
1613.817810	204757.187875	36.966567
1615.572319	205120.761618	36.971584
1617.266717	205486.429377	36.976602
1618.622400	205864.941056	36.981620
1620.365681	206218.110015	36.986637
1621.869648	206601.438494	36.991655
1623.373655	206971.220573	36.996672
1625.164194	207340.969742	37.001690
1626.660195	207714.286531	37.006708
1628.242998	208082.359261	37.011725
1630.317010	208463.291537	37.016743
1631.697553	208839.095953	37.021760
1633.525202	209205.190539	37.026778
1634.590511	209582.269413	37.031796
1636.536220	209957.528417	37.036813
1638.469277	210328.575437	37.041831
1640.197926	210696.610305	37.046848
1641.766546	211046.667213	37.051866
1643.050681	211391.159935	37.056884
1644.681449	211751.291810	37.061901
1646.362652	212099.124877	37.066919
1648.092849	212461.376562	37.071936
1649.827039	212812.835419	37.076954
1651.066484	213170.752015	37.081972
1652.644462	213523.534707	37.086989
1654.134539	213887.787391	37.092007
1655.742370	214263.349236	37.097024
1657.353943	214628.295910	37.102042
1659.022216	215010.047744	37.107060
1660.841198	215372.042358	37.112077
1662.433807	215761.479790	37.117095
1663.770738	216134.503316	37.122112
1665.839874	216519.572893	37.127130
1667.109109	216899.010802	37.132148
1668.934758	217269.494355	37.137165
1670.730230	217659.667822	37.142183
1672.285331	218056.714642	37.147200
1674.037607	218440.828106	37.152218
1675.591609	218838.487728	37.157236
1677.382649	219225.696341	37.162253
1679.133680	219619.288057	37.167271
1680.781380	220012.339546	37.172288
1682.569242	220406.436088	37.177306
1684.012610	220811.309318	37.182324
1685.599307	221218.751082	37.187341
1687.654394	221617.913090	37.192359
1689.228711	222020.686438	37.197376
1691.320905	222430.589082	37.202394
1692.840098	222809.524455	37.207412
1694.516834	223212.742319	37.212429
1696.316350	223625.008938	37.217447
1697.820123	224101.815501	37.222464
1699.764781	224497.627641	37.227482
1701.383709	224915.948313	37.232500
1703.141807	225314.359326	37.237517
1704.864520	225715.241272	37.242535
1706.459192	226132.325489	37.247552
1708.405257	226550.343648	37.252570
1709.761063	226954.211153	37.257588
1711.807489	227366.119338	37.262605
1713.726797	227775.484377	37.267623
1715.418673	228177.547515	37.272640
1717.335915	228587.880600	37.277658
1719.369993	229005.866603	37.282676
1720.966713	229397.814215	37.287693
1722.829994	229798.456749	37.292711
1724.431066	230209.786665	37.297728
1726.746141	230602.736581	37.302746
1728.294492	231013.772671	37.307764
1729.763375	231411.233476	37.312781
1731.754663	231825.805583	37.317799
1733.564093	232228.190892	37.322816
1735.272835	232623.684742	37.327834
1736.980334	233028.629068	37.332852
1738.721907	233422.163582	37.337869
1740.305081	233819.256007	37.342887
1742.149998	234217.576228	37.347904
1743.986043	234620.267922	37.352922
1745.785415	235026.522846	37.357940
1747.271814	235417.640224	37.362957
1749.359185	235824.052641	37.367975
1750.920690	236222.881500	37.372992
1752.860230	236623.477718	37.378010
1754.482638	237025.219458	37.383028
1756.132242	237418.676528	37.388045
1757.906739	237795.780298	37.393063
1759.411216	238190.583796	37.398080
1761.288300	238555.098061	37.403098
1762.806035	238950.993138	37.408116
1764.461415	239323.674055	37.413133
1766.331356	239713.542885	37.418151
1767.781208	240103.329385	37.423168
1769.198659	240495.992380	37.428186
1770.794451	240896.628339	37.433204
1772.633589	241302.737116	37.438221
1774.632801	241698.557568	37.443239
1775.914163	242112.278958	37.448256
1777.887361	242524.362618	37.453274
1779.678190	242936.400857	37.458292
1781.253578	243354.749766	37.463309
1783.312938	243773.756069	37.468327
1784.904661	244201.324732	37.473344
1786.946087	244611.622130	37.478362
1788.853371	245033.576712	37.483380
1790.435646	245453.019880	37.488397
1792.054851	245881.246883	37.493415
1793.777921	246315.909622	37.498432
1795.873566	246737.428911	37.503450
1797.186881	247167.156043	37.508468
1799.356319	247610.688507	37.513485
1801.285986	248035.716930	37.518503
1803.116764	248482.557918	37.523520
1804.787436	248932.143962	37.528538
1806.512067	249375.167582	37.533556
1808.181694	249816.320898	37.538573
1810.515734	250255.916922	37.543591
1812.126976	250694.311747	37.548608
1813.998450	251144.349406	37.553626
1815.872709	251592.100686	37.558644
1817.625585	252047.823547	37.563661
1819.856811	252490.435897	37.568679
1821.719506	252935.624319	37.573696
1823.314223	253381.797187	37.578714
1825.207332	253832.874657	37.583732
1826.867781	254285.819818	37.588749
1829.020348	254731.647215	37.593767
1830.734681	255182.627825	37.598784
1832.299876	255637.799368	37.603802
1834.394697	256091.918266	37.608820
1836.125832	256550.009455	37.613837
1838.261742	256995.357652	37.618855
1839.752523	257457.299207	37.623872
1841.850933	257913.450129	37.628890
1843.730118	258370.399385	37.633908
1845.528819	258834.830511	37.638925
1847.427950	259287.610323	37.643943
1849.360192	259754.229426	37.648960
1851.194626	260213.192821	37.653978
1853.490053	260673.273952	37.658996
1854.961436	261128.080158	37.664013
1857.369930	261578.844772	37.669031
1858.816408	262040.996348	37.674048
1860.682957	262492.917066	37.679066
1862.810683	262949.773490	37.684084
1864.386279	263410.886996	37.689101
1866.332513	263864.368882	37.694119
1868.188062	264325.283208	37.699136
1869.979002	264782.676859	37.704154
1872.137503	265227.688956	37.709172
1873.958530	265698.388231	37.714189
1876.192213	266143.539638	37.719207
1877.930040	266599.391057	37.724224
1879.805223	267024.862702	37.729242
1882.004208	267464.430000	37.734260
1883.534416	267897.629542	37.739277
1885.412288	268314.056063	37.744295
1887.010312	268740.537155	37.749312
1889.069266	269171.565013	37.754330
1891.135252	269596.418315	37.759348
1892.663143	270026.465967	37.764365
1894.744178	270454.135497	37.769383
1896.451167	270898.403502	37.774400
1898.205048	271328.259781	37.779418
1900.011725	271775.914096	37.784436
1901.268238	272226.579922	37.789453
1903.355340	272672.484623	37.794471
1905.081220	273132.673762	37.799488
1907.046528	273596.201152	37.804506
1908.897454	274050.703327	37.809524
1910.399074	274527.718216	37.814541
1912.631164	274991.884957	37.819559
1914.152145	275474.127759	37.824576
1916.133304	275948.291864	37.829594
1918.070327	276426.425057	37.834612
1919.892730	276910.164669	37.839629
1922.015993	277403.989025	37.844647
1924.232918	277889.515689	37.849664
1925.730484	278375.033010	37.854682
1927.824552	278866.013728	37.859700
1929.481614	279360.850298	37.864717
1931.642260	279861.368691	37.869735
1933.621237	280355.844739	37.874752
1935.507642	280858.260111	37.879770
1937.657865	281353.162445	37.884788
1939.887436	281863.646896	37.889805
1941.881343	282343.509116	37.894823
1943.788611	282850.563866	37.899840
1945.727272	283351.744181	37.904858
1948.167414	283847.836104	37.909876
1950.166916	284351.848240	37.914893
1952.231906	284840.302453	37.919911
1954.315660	285340.893739	37.924928
1955.926904	285844.863528	37.929946
1958.222157	286324.156006	37.934964
1959.840184	286830.915418	37.939981
1962.062953	287318.903665	37.944999
1964.228517	287826.940779	37.950016
1966.065354	288312.423836	37.955034
1968.526908	288814.947327	37.960052
1970.365249	289314.625405	37.965069
1972.397194	289812.186812	37.970087
1974.016465	290300.772003	37.975104
1976.275727	290803.880100	37.980122
1978.581352	291297.504356	37.985140
1980.320435	291802.218337	37.990157
1982.172139	292292.789384	37.995175
1984.370149	292790.082967	38.000192
1986.085636	293290.375092	38.005210
1988.379334	293781.806811	38.010228
1990.403988	294288.393466	38.015245
1992.561257	294774.865198	38.020263
1994.289079	295275.680030	38.025280
1996.229564	295775.009750	38.030298
1998.428851	296261.417235	38.035316
2000.346200	296764.479871	38.040333
2002.176023	297259.223834	38.045351
2004.442924	297759.353991	38.050368
2006.235755	298250.315001	38.055386
2008.478977	298759.130481	38.060404
2010.533650	299247.808414	38.065421
2012.506725	299733.957635	38.070439
2014.568337	300210.032284	38.075456
2016.440189	300688.701124	38.080474
2018.791804	301143.592378	38.085492
2020.490796	301616.240505	38.090509
2022.390655	302087.075292	38.095527
2024.429362	302552.043415	38.100544
2025.758930	303031.120114	38.105562
2028.129926	303502.504853	38.110580
2029.837011	303991.088854	38.115597
2031.491091	304480.390055	38.120615
2033.724082	304974.062783	38.125632
2035.416853	305482.907416	38.130650
2037.787387	305975.104183	38.135668
2039.300591	306479.731414	38.140685
2041.356338	306990.488101	38.145703
2043.609274	307506.593052	38.150720
2045.257187	308021.728076	38.155738
2047.270896	308529.358600	38.160756
2049.146362	309074.136810	38.165773
2051.230769	309598.713069	38.170791
2053.475038	310125.849785	38.175808
2055.556519	310667.154793	38.180826
2057.848078	311203.596387	38.185844
2059.768080	311747.510800	38.190861
2061.859215	312280.067238	38.195879
2063.918398	312813.183885	38.200896
2065.872902	313361.982103	38.205914
2068.170636	313900.714465	38.210932
2069.752742	314450.505664	38.215949
2071.945235	315006.946592	38.220967
2074.057714	315563.828127	38.225984
2076.301884	316122.207165	38.231002
2078.684487	316674.058395	38.236020
2080.548811	317230.079052	38.241037
2082.645530	317786.158466	38.246055
2084.943335	318354.769316	38.251072
2087.066609	318909.895716	38.256090
2089.127637	319457.029428	38.261108
2091.350254	320019.189178	38.266125
2093.434786	320575.806261	38.271143
2095.863182	321143.787864	38.276160
2097.754248	321716.931396	38.281178
2099.893929	322267.050250	38.286196
2102.271248	322838.910144	38.291213
2104.258067	323395.976074	38.296231
2106.630731	323953.024152	38.301248
2108.994524	324524.947116	38.306266
2111.255932	325080.607005	38.311284
2112.950035	325637.472636	38.316301
2115.238735	326194.057287	38.321319
2117.500049	326756.074526	38.326336
2119.863808	327321.217754	38.331354
2121.914756	327867.239035	38.336372
2123.941713	328431.716361	38.341389
2126.219820	328987.413343	38.346407
2128.602243	329542.681567	38.351424
2130.506034	330103.786366	38.356442
2132.603805	330656.678966	38.361460
2134.581562	331224.589610	38.366477
2136.368367	331772.039031	38.371495
2138.896126	332331.698529	38.376512
2140.724000	332902.993179	38.381530
2142.889256	333467.092764	38.386548
2145.406870	334036.078523	38.391565
2147.164365	334596.070438	38.396583
2149.652376	335153.372026	38.401600
2151.691472	335730.389689	38.406618
2153.962709	336277.383645	38.411636
2156.308357	336816.109735	38.416653
2158.096819	337357.282937	38.421671
2160.052275	337878.319011	38.426688
2162.139259	338419.304868	38.431706
2164.252572	338957.463110	38.436724
2166.202150	339501.277672	38.441741
2168.525158	340039.618217	38.446759
2170.676228	340587.398203	38.451776
2172.684373	341127.403443	38.456794
2174.735519	341680.137338	38.461812
2176.725675	342244.093693	38.466829
2178.627100	342803.667213	38.471847
2181.027417	343370.360089	38.476864
2182.845858	343937.903746	38.481882
2185.554157	344517.577836	38.486900
2187.630667	345086.334204	38.491917
2189.863607	345658.611038	38.496935
2191.974237	346219.987927	38.501952
2193.995163	346810.863313	38.506970
2196.457183	347390.770853	38.511988
2198.414932	347979.814387	38.517005
2200.457299	348571.171122	38.522023
2203.257155	349149.097157	38.527040
2205.033136	349755.074547	38.532058
2207.672038	350345.624287	38.537076
2209.724513	350939.663445	38.542093
2211.816291	351536.936291	38.547111
2214.206275	352131.385783	38.552128
2216.355411	352731.601817	38.557146
2218.761635	353342.475479	38.562164
2221.244308	353931.124732	38.567181
2223.147456	354547.976608	38.572199
2225.486207	355147.011015	38.577216
2227.957194	355756.621373	38.582234
2230.198743	356363.495015	38.587252
2232.380395	356965.523425	38.592269
2234.490351	357587.371050	38.597287
2236.978409	358188.823577	38.602304
2239.145334	358802.574941	38.607322
2241.554179	359407.650747	38.612340
2243.886250	360020.189303	38.617357
2246.103444	360640.018907	38.622375
2248.432868	361246.576969	38.627392
2250.985278	361863.389200	38.632410
2253.131966	362479.269322	38.637428
2255.334497	363078.843463	38.642445
2257.510327	363708.576390	38.647463
2259.945443	364322.933722	38.652480
2262.008879	364943.050407	38.657498
2263.945615	365565.131262	38.662516
2266.699741	366178.974888	38.667533
2269.007645	366803.866031	38.672551
2271.068478	367409.534464	38.677568
2273.184536	368044.887545	38.682586
2275.610161	368664.984711	38.687604
2278.085989	369289.476718	38.692621
2280.006427	369925.362426	38.697639
2282.608516	370551.333970	38.702656
2284.650553	371177.869071	38.707674
2286.777893	371802.679884	38.712692
2289.292818	372430.357964	38.717709
2291.330674	373059.904488	38.722727
2293.638758	373693.808253	38.727744
2296.061804	374328.873666	38.732762
2298.376033	374964.021644	38.737780
2300.824713	375592.973250	38.742797
2302.505956	376227.188248	38.747815
2305.541860	376843.416234	38.752832
2307.644181	377455.019702	38.757850
2309.699661	378065.808485	38.762868
2312.342087	378668.958001	38.767885
2314.518480	379271.717240	38.772903
2316.862912	379877.835864	38.777920
2318.794867	380478.433056	38.782938
2320.744328	381090.249499	38.787956
2323.138398	381701.575591	38.792973
2325.135595	382333.392476	38.797991
2327.476610	382952.082588	38.803008
2329.915438	383576.677830	38.808026
2332.221935	384208.306010	38.813044
2334.686812	384840.808453	38.818061
2336.799067	385483.193678	38.823079
2339.245459	386121.657278	38.828096
2341.321598	386766.279047	38.833114
2343.663202	387407.472139	38.838132
2346.210492	388053.941981	38.843149
2348.136241	388714.266425	38.848167
2350.786307	389364.063873	38.853184
2353.102783	390037.908731	38.858202
2355.386450	390708.119419	38.863220
2358.083726	391363.469147	38.868237
2360.350771	392035.199831	38.873255
2362.615714	392704.508051	38.878272
2365.345690	393369.922736	38.883290
2367.162793	394055.446121	38.888308
2369.882514	394731.680489	38.893325
2372.120627	395400.933098	38.898343
2374.492482	396088.700649	38.903360
2376.836970	396768.143934	38.908378
2379.255896	397464.032316	38.913396
2382.033126	398149.961393	38.918413
2384.187730	398838.891372	38.923431
2386.680660	399523.694504	38.928448
2389.294958	400222.322745	38.933466
2391.486920	400915.530173	38.938484
2393.774179	401602.648874	38.943501
2396.264092	402304.591462	38.948519
2398.766008	403005.577107	38.953536
2401.466140	403708.058159	38.958554
2403.726838	404407.021555	38.963572
2406.396608	405100.933963	38.968589
2408.315136	405807.367474	38.973607
2410.724767	406510.256272	38.978624
2413.172762	407214.336784	38.983642
2415.718590	407927.781835	38.988660
2418.326273	408638.081970	38.993677
2420.768778	409348.745354	38.998695
2423.312926	410059.930499	39.003712
2425.636415	410772.146414	39.008730
2427.607718	411481.463081	39.013748
2430.430597	412188.264604	39.018765
2432.800997	412912.168338	39.023783
2435.318319	413619.488458	39.028800
2437.973403	414348.725830	39.033818
2440.211466	415057.496732	39.038836
2442.824410	415776.240932	39.043853
2445.201586	416493.611101	39.048871
2447.706196	417209.851232	39.053888
2450.070871	417927.993694	39.058906
2452.388227	418645.186727	39.063924
2455.283056	419363.732886	39.068941
2457.560561	420085.247131	39.073959
2459.720713	420803.088415	39.078976
2462.532770	421517.560483	39.083994
2464.316812	422247.474815	39.089012
2467.199577	422956.500671	39.094029
2469.350372	423651.347352	39.099047
2472.004221	424341.837999	39.104064
2474.317200	425032.871721	39.109082
2476.694241	425729.748616	39.114100
2479.011904	426421.906592	39.119117
2481.459284	427130.731052	39.124135
2483.956551	427830.767732	39.129152
2486.445718	428525.975751	39.134170
2488.472192	429243.312344	39.139188
2490.957520	429951.591194	39.144205
2493.413484	430674.787135	39.149223
2495.687866	431395.054828	39.154240
2497.960424	432114.743876	39.159258
2500.362772	432857.167069	39.164276
2502.889518	433596.002922	39.169293
2505.491469	434344.723105	39.174311
2507.716883	435086.041062	39.179328
2510.240153	435832.296374	39.184346
2512.675207	436604.554875	39.189364
2515.677719	437365.003244	39.194381
2517.709136	438121.386019	39.199399
2520.402245	438892.157551	39.204416
2522.918062	439660.755969	39.209434
2525.191140	440442.574688	39.214452
2527.901699	441205.926475	39.219469
2530.595968	441988.532032	39.224487
2532.726877	442782.789016	39.229504
2535.895487	443560.706855	39.234522
2538.192692	444348.757866	39.239540
2540.948901	445138.930565	39.244557
2543.653510	445931.865292	39.249575
2546.172167	446723.233404	39.254592
2548.937552	447511.901304	39.259610
2551.252323	448322.617669	39.264628
2553.892991	449109.527343	39.269645
2556.524482	449903.287986	39.274663
2559.289247	450708.123613	39.279680
2562.410764	451499.163924	39.284698
2565.041533	452303.505311	39.289716
2567.799991	453092.067177	39.294733
2570.721523	453880.117084	39.299751
2573.213677	454660.066560	39.304768
2576.092107	455462.221855	39.309786
2578.708401	456247.248241	39.314804
2581.556763	457021.234468	39.319821
2583.852054	457803.826963	39.324839
2586.344643	458588.025079	39.329856
2589.097070	459369.521008	39.334874
2591.374601	460168.202389	39.339892
2594.248248	460958.412663	39.344909
2596.790400	461759.059411	39.349927
2599.283116	462555.587744	39.354944
2602.070419	463342.179154	39.359962
2604.463946	464151.851692	39.364980
2607.181373	464939.603773	39.369997
2610.077970	465731.691433	39.375015
2612.640752	466530.877086	39.380032
2615.456591	467323.923914	39.385050
2617.922224	468124.727447	39.390068
2620.219464	468919.916564	39.395085
2622.926347	469707.425876	39.400103
2625.061510	470512.933855	39.405120
2627.702024	471308.421648	39.410138
2630.514982	472122.843871	39.415156
2633.262880	472926.986175	39.420173
2635.782753	473730.576014	39.425191
2638.012113	474539.432916	39.430208
2640.860724	475328.856540	39.435226
2643.430522	476110.362380	39.440244
2645.681149	476879.412157	39.445261
2648.610048	477658.166868	39.450279
2651.232688	478428.252284	39.455296
2653.776933	479204.833115	39.460314
2656.212270	479997.003539	39.465332
2658.897090	480775.413269	39.470349
2661.491844	481555.622285	39.475367
2663.666221	482355.054635	39.480384
2666.309862	483144.679662	39.485402
2668.783204	483950.151689	39.490420
2671.320725	484758.505064	39.495437
2673.857270	485581.058604	39.500455
2676.261069	486390.924780	39.505472
2679.234181	487223.678868	39.510490
2681.787492	488059.491457	39.515508
2684.362521	488887.285522	39.520525
2687.093958	489727.430897	39.525543
2689.425393	490576.434019	39.530560
2692.568795	491422.284030	39.535578
2694.920604	492286.138421	39.540596
2697.264850	493149.193752	39.545613
2700.140328	494005.204941	39.550631
2702.521146	494884.515860	39.555648
2705.722188	495759.458264	39.560666
2707.966787	496645.007379	39.565684
2710.881011	497537.058984	39.570701
2713.674782	498420.153981	39.575719
2716.146365	499312.032919	39.580736
2719.008473	500214.543890	39.585754
2722.150353	501111.260105	39.590772
2724.513180	502010.981564	39.595789
2727.729723	502910.260983	39.600807
2730.126721	503821.628891	39.605824
2733.282888	504716.230051	39.610842
2736.376027	505628.895182	39.615860
2738.933390	506530.807027	39.620877
2742.088749	507434.889291	39.625895
2744.670687	508348.241697	39.630912
2747.442862	509256.368592	39.635930
2749.707297	510168.459758	39.640948
2752.937904	511080.591444	39.645965
2755.750249	511983.767607	39.650983
2758.626882	512910.822711	39.656000
2761.232139	513820.329101	39.661018
2764.129532	514743.694453	39.666036
2766.771886	515664.981256	39.671053
2769.788155	516585.597658	39.676071
2772.430815	517511.461406	39.681088
2775.463756	518419.016619	39.686106
2778.272083	519352.854570	39.691124
2780.831868	520278.465076	39.696141
2783.700022	521202.155242	39.701159
2786.422226	522121.028163	39.706176
2789.756643	523051.480575	39.711194
2792.423256	523975.740531	39.716212
2795.316603	524888.574780	39.721229
2798.446683	525811.688700	39.726247
2800.528833	526734.868184	39.731264
2803.643272	527661.093316	39.736282
2806.522840	528589.817010	39.741300
2809.487149	529512.124735	39.746317
2812.372462	530432.172717	39.751335
2814.963321	531359.108452	39.756352
2817.989338	532275.846224	39.761370
2820.607756	533203.717665	39.766388
2823.442756	534125.051808	39.771405
2826.655522	535030.512343	39.776423
2829.063907	535930.009776	39.781440
2832.026518	536806.463063	39.786458
2834.593420	537686.852999	39.791476
2837.140947	538569.405882	39.796493
2840.113584	539459.179742	39.801511
2842.476645	540347.539459	39.806528
2845.472858	541240.568508	39.811546
2848.184791	542137.159508	39.816564
2850.705678	543052.034156	39.821581
2853.616884	543959.039073	39.826599
2856.141969	544871.933177	39.831616
2859.334173	545783.903121	39.836634
2861.936878	546712.806799	39.841652
2864.675727	547641.374282	39.846669
2867.790812	548572.431793	39.851687
2870.183169	549514.907968	39.856704
2873.353603	550463.123260	39.861722
2876.104643	551409.783510	39.866740
2878.918657	552371.849512	39.871757
2881.740280	553310.624700	39.876775
2884.447011	554281.821016	39.881792
2887.141381	555250.235569	39.886810
2890.231061	556226.907132	39.891828
2893.263469	557205.376021	39.896845
2896.232112	558178.909910	39.901863
2898.818970	559166.553062	39.906880
2901.828192	560154.304097	39.911898
2905.125459	561135.252689	39.916916
2907.543685	562134.104485	39.921933
2911.127961	563128.619622	39.926951
2913.877859	564132.286726	39.931968
2916.560459	565130.012054	39.936986
2920.296403	566130.901499	39.942004
2922.674362	567133.544071	39.947021
2926.410106	568133.525040	39.952039
2928.791890	569140.127442	39.957056
2931.934113	570139.346922	39.962074
2935.254261	571151.057524	39.967092
2937.751047	572156.649927	39.972109
2941.030875	573159.825180	39.977127
2943.891929	574170.968729	39.982144
2947.156782	575185.527072	39.987162
2950.020641	576190.185102	39.992180
2953.024396	577209.740154	39.997197
2956.001865	578222.443646	40.002215
2959.021490	579244.638471	40.007232
2961.988051	580253.766702	40.012250
2965.309061	581275.041523	40.017268
2968.216164	582301.364780	40.022285
2971.345807	583304.799365	40.027303
2974.578121	584320.118251	40.032320
2977.122562	585342.886065	40.037338
2980.507844	586345.977469	40.042356
2983.568424	587369.190811	40.047373
2986.396506	588380.676599	40.052391
2989.526356	589392.729091	40.057408
2992.361866	590403.391381	40.062426
2996.012566	591405.915992	40.067444
2998.885826	592427.023944	40.072461
3002.029242	593428.709702	40.077479
3005.004101	594434.195908	40.082496
3007.780963	595438.025867	40.087514
3010.867125	596439.515011	40.092532
3013.448802	597465.293258	40.097549
3016.530726	598463.003423	40.102567
3019.599741	599486.069302	40.107584
3022.502997	600493.549634	40.112602
3025.869790	601491.102334	40.117620
3028.529546	602474.767346	40.122637
3031.386663	603447.302366	40.127655
3034.167213	604418.115539	40.132672
3037.160100	605393.966410	40.137690
3040.365541	606367.396367	40.142708
3042.773907	607349.481547	40.147725
3045.545678	608333.473116	40.152743
3048.678252	609329.027285	40.157760
3051.436641	610322.753900	40.162778
3054.641202	611334.928169	40.167796
3057.232508	612339.808839	40.172813
3060.949083	613363.469425	40.177831
3063.606780	614377.507986	40.182848
3066.108733	615404.581103	40.187866
3069.650543	616436.237409	40.192884
3072.571401	617479.348706	40.197901
3075.452389	618515.668362	40.202919
3079.026603	619568.171493	40.207936
3081.542319	620626.545479	40.212954
3084.719735	621677.360523	40.217972
3087.881497	622734.122940	40.222989
3091.142787	623807.005179	40.228007
3093.870628	624867.227705	40.233024
3096.676018	625950.513312	40.238042
3100.116708	627035.133016	40.243060
3103.487230	628129.293893	40.248077
3106.272408	629212.950594	40.253095
3109.628480	630298.349909	40.258112
3112.422099	631397.711496	40.263130
3115.991239	632498.727667	40.268148
3118.903976	633600.585172	40.273165
3121.850292	634710.856839	40.278183
3124.987337	635834.704476	40.283200
3128.072624	636941.471057	40.288218
3131.857303	638064.221823	40.293236
3134.989026	639185.760640	40.298253
3138.151140	640297.792958	40.303271
3141.578608	641418.690082	40.308288
3144.532813	642536.649389	40.313306
3148.151493	643656.920124	40.318324
3151.020400	644778.786721	40.323341
3154.274293	645891.889300	40.328359
3157.665019	647017.360717	40.333376
3160.727067	648150.736684	40.338394
3164.186768	649275.395504	40.343412
3167.059078	650405.008704	40.348429
3170.461851	651526.383183	40.353447
3173.702448	652645.714575	40.358464
3176.751038	653783.784324	40.363482
3180.213043	654896.795963	40.368500
3183.570911	656038.888649	40.373517
3186.803205	657155.667380	40.378535
3190.030251	658279.540592	40.383552
3193.073453	659420.493755	40.388570
3196.625935	660535.986310	40.393588
3199.761185	661657.443053	40.398605
3202.904822	662787.130893	40.403623
3206.310695	663924.059025	40.408640
3209.334716	665045.189706	40.413658
3212.426848	666174.189252	40.418676
3215.501230	667298.630190	40.423693
3218.720740	668430.426341	40.428711
3221.959823	669567.506185	40.433728
3224.915423	670709.221039	40.438746
3228.519123	671828.113580	40.443764
3231.738129	672968.964122	40.448781
3234.691049	674099.129845	40.453799
3237.894154	675231.106212	40.458816
3241.226254	676324.948566	40.463834
3244.279819	677418.161397	40.468852
3247.751297	678502.529600	40.473869
3250.800119	679597.622616	40.478887
3254.103198	680681.563753	40.483904
3257.002393	681776.720198	40.488922
3260.158232	682876.968552	40.493940
3263.030409	683970.625088	40.498957
3266.413755	685082.489481	40.503975
3269.489829	686195.211823	40.508992
3272.568510	687321.995927	40.514010
3275.745774	688444.056314	40.519028
3278.917790	689575.160051	40.524045
3282.040314	690715.608352	40.529063
3285.166607	691871.293365	40.534080
3288.459335	693022.335995	40.539098
3291.733047	694180.178072	40.544116
3294.728975	695344.908722	40.549133
3298.071082	696522.422966	40.554151
3301.359691	697695.821749	40.559168
3304.523965	698878.009228	40.564186
3308.247772	700074.371508	40.569204
3311.419510	701260.152520	40.574221
3314.660513	702454.087161	40.579239
3318.188345	703660.942518	40.584256
3321.129874	704877.437745	40.589274
3324.624741	706088.914536	40.594292
3328.004822	707309.354018	40.599309
3331.402585	708517.136321	40.604327
3335.010897	709732.983292	40.609344
3338.122635	710972.554434	40.614362
3341.467881	712212.104498	40.619380
3345.079687	713443.262260	40.624397
3348.321684	714682.220226	40.629415
3351.958893	715896.337548	40.634432
3355.204164	717147.204041	40.639450
3358.626221	718382.420299	40.644468
3362.342445	719620.224727	40.649485
3365.431873	720858.442979	40.654503
3368.808661	722118.680343	40.659520
3372.470765	723365.626800	40.664538
3375.890245	724611.287855	40.669556
3379.226966	725857.070475	40.674573
3382.477923	727113.055556	40.679591
3386.081095	728369.728456	40.684608
3389.346114	729619.001302	40.689626
3392.849622	730880.045587	40.694644
3396.230620	732147.679725	40.699661
3399.942984	733411.159441	40.704679
3403.416282	734670.185063	40.709696
3406.453852	735921.680606	40.714714
3409.931690	737187.122319	40.719732
3413.527237	738463.644570	40.724749
3416.738755	739731.489580	40.729767
3419.992772	740991.429245	40.734784
3423.166659	742271.897411	40.739802
3426.671851	743559.451121	40.744820
3430.020326	744848.693481	40.749837
3433.465636	746138.299429	40.754855
3437.206703	747415.912493	40.759872
3440.022712	748710.076905	40.764890
3443.552633	750012.334105	40.769908
3447.081789	751300.577781	40.774925
3450.389940	752596.967595	40.779943
3454.194610	753897.883779	40.784960
3457.286557	755201.454393	40.789978
3460.932612	756496.292734	40.794996
3464.201956	757782.985679	40.800000
3467.281445	759030.608811	40.805005
3470.800978	760217.074943	40.810010
3473.756453	761350.914062	40.815015
3476.854186	762422.563485	40.820020
3479.920080	763435.382055	40.825024
3483.149504	764383.197549	40.830029
3485.724034	765261.682686	40.835034
3488.640992	766081.197546	40.840039
3491.129445	766811.179646	40.845044
3493.667080	767485.338350	40.850048
3496.093437	768095.484853	40.855053
3497.886245	768649.260681	40.860058
3500.301343	769152.384645	40.865063
3502.034430	769602.273323	40.870068
3504.181477	769975.007352	40.875072
3505.913034	770293.940600	40.880077
3507.404261	770579.299825	40.885082
3508.882595	770815.582196	40.890087
3510.758722	770996.271180	40.895092
3512.213689	771131.062828	40.900096
3513.117617	771245.794547	40.905101
3514.230811	771292.508781	40.910106
3515.415455	771317.585042	40.915111
3516.706419	771309.047183	40.920116
3517.624302	771265.397688	40.925120
3518.543075	771190.663120	40.930125
3519.265437	771088.323481	40.935130
3520.171219	770959.743701	40.940135
3520.849551	770798.290036	40.945140
3521.253201	770622.245985	40.950144
3521.807994	770428.337942	40.955149
3522.576100	770219.116261	40.960154
3522.600226	769985.671570	40.965159
3523.390204	769727.949899	40.970164
3524.031987	769457.481679	40.975168
3524.175777	769185.558088	40.980173
3524.563321	768889.783145	40.985178
3525.140561	768569.374437	40.990183
3525.647519	768246.942918	40.995188
3525.861348	767921.194372	41.000192
3525.614319	767583.481562	41.005197
3526.099886	767216.650810	41.010202
3526.289905	766857.688034	41.015207
3526.301742	766493.167129	41.020212
3526.398800	766112.938147	41.025216
3526.239337	765735.049114	41.030221
3526.795866	765344.697658	41.035226
3526.915082	764971.752875	41.040231
3526.748819	764573.443745	41.045236
3527.133806	764161.265357	41.050240
3526.942342	763771.398942	41.055245
3527.160985	763355.012176	41.060250
3526.844643	762957.924181	41.065255
3526.933142	762532.488262	41.070260
3527.126342	762102.029457	41.075264
3527.259061	761691.631495	41.080269
3527.182247	761268.272430	41.085274
3526.774003	760847.016128	41.090279
3526.632643	760428.307047	41.095284
3527.030267	759995.671783	41.100288
3526.797698	759591.288321	41.105293
3526.710089	759152.912200	41.110298
3526.781228	758734.173145	41.115303
3526.337791	758302.517404	41.120308
3526.516331	757871.721671	41.125312
3525.882626	757445.970682	41.130317
3525.871616	757033.715474	41.135322
3525.625715	756612.937670	41.140327
3525.779377	756190.096380	41.145332
3525.793211	755775.498490	41.150336
3525.537253	755361.465601	41.155341
3525.548306	754936.702564	41.160346
3525.273691	754523.812311	41.165351
3525.377261	754110.195640	41.170356
3525.041175	753683.247877	41.175360
3524.937561	753268.484326	41.180365
3524.970622	752859.404270	41.185370
3524.746716	752460.221855	41.190375
3524.411511	752047.307290	41.195380
3524.859634	751631.623854	41.200384
3524.127053	751228.263280	41.205389
3524.212959	750824.746781	41.210394
3523.985986	750415.184799	41.215399
3523.927936	750021.924982	41.220404
3523.632721	749621.965435	41.225408
3523.417020	749227.357392	41.230413
3523.485880	748813.067270	41.235418
3523.204617	748428.904044	41.240423
3522.819903	748043.305896	41.245428
3522.894347	747646.049685	41.250432
3522.710905	747265.321435	41.255437
3522.400516	746896.209366	41.260442
3522.657368	746507.563131	41.265447
3522.214810	746126.278355	41.270452
3522.454666	745749.657048	41.275456
3521.818805	745376.276013	41.280461
3521.762563	744997.937275	41.285466
3521.700973	744637.180001	41.290471
3521.513502	744254.723939	41.295476
3521.344810	743895.779419	41.300480
3521.311378	743522.754733	41.305485
3521.045545	743164.583911	41.310490
3520.868425	742801.091411	41.315495
3520.814499	742460.753256	41.320500
3520.462670	742088.108675	41.325504
3520.121913	741746.402339	41.330509
3520.058396	741387.919672	41.335514
3519.997753	741045.345586	41.340519
3519.991304	740710.859105	41.345524
3520.062153	740363.831966	41.350528
3519.591044	740035.971953	41.355533
3519.732933	739685.886152	41.360538
3519.342808	739355.264040	41.365543
3518.891160	739019.493418	41.370548
3519.251514	738692.331389	41.375552
3518.986178	738357.936831	41.380557
3518.900900	738021.321608	41.385562
3518.701842	737702.523101	41.390567
3518.742802	737380.851932	41.395572
3518.772690	737057.982052	41.400576
3518.269066	736733.653016	41.405581
3517.870143	736422.258954	41.410586
3518.092448	736106.543921	41.415591
3517.606050	735795.337828	41.420596
3517.818251	735495.585649	41.425600
3517.377862	735204.541699	41.430605
3517.547473	734883.045891	41.435610
3517.394879	734578.171999	41.440615
3516.985910	734285.604631	41.445620
3517.058716	733988.888138	41.450624
3517.111229	733705.925874	41.455629
3516.899902	733398.541802	41.460634
3516.707542	733108.173163	41.465639
3516.398864	732813.654528	41.470644
3516.640749	732519.579041	41.475648
3516.199408	732247.638231	41.480653
3516.141031	731950.670307	41.485658
3515.866126	731676.553769	41.490663
3515.549903	731409.812786	41.495668
3515.559095	731125.826415	41.500672
3513.655109	730908.651032	41.505677
3513.920057	730647.929682	41.510682
3514.755650	730381.064095	41.515687
3515.908777	730095.169364	41.520692
3516.640945	729799.725747	41.525696
3517.786413	729507.472191	41.530701
3514.619778	729288.084080	41.535706
3514.465687	729009.350291	41.540711
3517.593962	728657.846224	41.545716
3518.124654	728352.971903	41.550720
3515.325659	728140.922598	41.555725
3512.270402	727945.009885	41.560730
3512.671746	727683.824341	41.565735
3515.439176	727368.884480	41.570740
3515.636376	727124.212043	41.575744
3510.489001	727001.300721	41.580749
3508.107185	726850.434573	41.585754
3513.847864	726507.028401	41.590759
3517.389004	726186.762784	41.595764
3512.776973	726060.478828	41.600768
3515.262624	725741.757147	41.605773
3514.130179	725519.306231	41.610778
3512.995387	725294.867503	41.615783
3514.103406	725034.472179	41.620788
3511.102476	724856.316496	41.625792
3512.069898	724620.709586	41.630797
3513.010873	724387.925197	41.635802
3511.776691	724201.683347	41.640807
3512.090057	723975.433606	41.645812
3511.366447	723786.471447	41.650816
3510.527303	723608.527267	41.655821
3510.824590	723412.845844	41.660826
3512.665453	723164.860330	41.665831
3512.843983	722944.552583	41.670836
3512.775371	722730.426312	41.675840
3515.492031	722434.836442	41.680845
3512.326818	722270.977946	41.685850
3509.851654	722127.922388	41.690855
3512.542860	721826.068770	41.695860
3511.147976	721659.824301	41.700864
3510.590393	721483.027362	41.705869
3513.857222	721198.507185	41.710874
3511.077567	721062.573119	41.715879
3510.867595	720861.015008	41.720884
3512.156865	720629.207855	41.725888
3509.518784	720492.844448	41.730893
3510.895563	720261.756377	41.735898
3511.814265	720066.290233	41.740903
3510.114967	719900.556516	41.745908
3510.905648	719697.764017	41.750912
3511.393640	719495.462762	41.755917
3510.672615	719320.580712	41.760922
3511.574882	719100.993914	41.765927
3511.288911	718914.923233	41.770932
3510.630488	718731.786188	41.775936
3510.491026	718532.540577	41.780941
3510.460625	718359.210792	41.785946
3510.461583	718178.234359	41.790951
3510.147722	718001.422494	41.795956
3509.812124	717831.405503	41.800960
3509.037546	717688.340410	41.805965
3509.209524	717511.289334	41.810970
3510.065413	717335.163465	41.815975
3509.996241	717169.602888	41.820980
3510.404954	716977.620722	41.825984
3510.690210	716791.011838	41.830989
3510.253286	716622.574366	41.835994
3510.295047	716431.731505	41.840999
3510.225241	716260.597106	41.846004
3509.594000	716100.664147	41.851008
3509.497089	715923.871927	41.856013
3508.850784	715778.272596	41.861018
3508.583198	715631.020764	41.866023
3508.475015	715477.191221	41.871028
3508.406899	715328.660914	41.876032
3508.343063	715181.814171	41.881037
3508.597581	715025.435892	41.886042
3508.770066	714885.193493	41.891047
3508.923059	714733.639296	41.896052
3509.527588	714565.187481	41.901056
3509.011745	714419.940103	41.906061
3509.268146	714247.966759	41.911066
3509.187406	714088.500302	41.916071
3509.171956	713946.437300	41.921076
3509.234444	713782.028912	41.926080
3508.935429	713623.582098	41.931085
3508.283413	713477.497342	41.936090
3508.271394	713332.197863	41.941095
3507.871273	713205.718490	41.946100
3507.908783	713058.569989	41.951104
3508.016907	712911.605807	41.956109
3507.617359	712781.646060	41.961114
3507.713161	712646.490884	41.966119
3508.102059	712514.908255	41.971124
3508.586053	712365.043752	41.976128
3507.804270	712221.489877	41.981133
3508.115793	712086.240599	41.986138
3508.505091	711950.132586	41.991143
3507.984650	711802.061547	41.996148
3508.046073	711657.565046	42.001152
3507.836228	711535.893642	42.006157
3507.899740	711394.767562	42.011162
3507.933602	711278.959078	42.016167
3507.539938	711147.930956	42.021172
3507.581461	710999.604422	42.026176
3507.299492	710882.651248	42.031181
3507.380377	710748.858249	42.036186
3506.977197	710625.716467	42.041191
3506.918753	710507.629207	42.046196
3506.709924	710380.828009	42.051200
3506.841933	710267.273148	42.056205
3506.985902	710151.282256	42.061210
3507.491522	710021.577940	42.066215
3507.336492	709909.654243	42.071220
3507.224602	709771.906054	42.076224
3507.275224	709656.519573	42.081229
3507.249977	709531.264194	42.086234
3507.384723	709408.661618	42.091239
3506.935318	709295.437871	42.096244
3506.993643	709166.092163	42.101248
3506.780082	709061.167578	42.106253
3506.729095	708964.456946	42.111258
3506.597163	708841.393669	42.116263
3506.153050	708733.226049	42.121268
3506.009024	708616.070120	42.126272
3506.084638	708516.404049	42.131277
3506.536336	708417.419660	42.136282
3506.320828	708319.040610	42.141287
3506.409105	708195.286252	42.146292
3506.481105	708087.373018	42.151296
3506.411324	707990.058608	42.156301
3506.581344	707874.131854	42.161306
3506.670823	707752.804110	42.166311
3506.314825	707666.010968	42.171316
3506.160508	707553.013497	42.176320
3505.665881	707457.997704	42.181325
3505.518506	707351.799785	42.186330
3506.059843	707251.942964	42.191335
3505.777610	707162.848186	42.196340
3505.681095	707055.396694	42.201344
3505.664199	706966.504468	42.206349
3505.603786	706869.374459	42.211354
3505.935474	706769.894227	42.216359
3505.649905	706696.637793	42.221364
3505.712522	706596.405268	42.226368
3505.860544	706491.588319	42.231373
3505.730938	706396.699301	42.236378
3505.894430	706298.830640	42.241383
3505.561157	706205.711392	42.246388
3505.555434	706121.129595	42.251392
3505.350087	706021.083527	42.256397
3505.297722	705941.822107	42.261402
3505.574331	705839.856797	42.266407
3505.474988	705761.197482	42.271412
3505.261753	705674.410376	42.276416
3505.064752	705588.513786	42.281421
3505.062124	705506.756656	42.286426
3505.447316	705418.676275	42.291431
3505.167116	705339.248172	42.296436
3505.128695	705245.722265	42.301440
3505.001829	705160.405923	42.306445
3505.129268	705073.705659	42.311450
3505.252919	704994.704574	42.316455
3505.120718	704914.205025	42.321460
3505.431549	704829.657758	42.326464
3505.500899	704744.056601	42.331469
3505.375730	704661.069779	42.336474
3505.371147	704568.226422	42.341479
3505.047340	704486.909970	42.346484
3505.202332	704399.304225	42.351488
3504.964128	704321.598542	42.356493
3505.027353	704243.643782	42.361498
3504.965773	704157.760328	42.366503
3505.020089	704086.114784	42.371508
3504.975365	703997.892059	42.376512
3504.710656	703914.275233	42.381517
3504.953609	703834.548380	42.386522
3504.945858	703751.732212	42.391527
3504.844993	703676.035018	42.396532
3504.915274	703591.962434	42.401536
3504.847165	703527.735022	42.406541
3504.781730	703438.218276	42.411546
3505.027499	703368.274144	42.416551
3504.710068	703294.944408	42.421556
3504.720002	703222.255685	42.426560
3504.468731	703137.883896	42.431565
3504.769545	703067.530797	42.436570
3504.685843	702998.830410	42.441575
3504.478551	702920.361788	42.446580
3504.722506	702828.005376	42.451584
3504.466311	702773.641218	42.456589
3504.414348	702696.387139	42.461594
3504.612563	702623.016448	42.466599
3504.648859	702558.416849	42.471604
3504.685390	702485.618203	42.476608
3504.516337	702419.461389	42.481613
3504.549932	702350.786239	42.486618
3504.257780	702278.040013	42.491623
3504.239739	702219.310178	42.496628
3504.207843	702144.979578	42.501632
3504.267279	702079.627259	42.506637
3504.242281	702006.934127	42.511642
3504.295381	701935.171652	42.516647
3504.261755	701868.690186	42.521652
3504.338509	701798.661894	42.526656
3504.708540	701736.485803	42.531661
3504.627457	701671.004495	42.536666
3504.698696	701604.106190	42.541671
3504.075733	701536.924208	42.546676
3504.495535	701468.277848	42.551680
3504.106832	701390.868888	42.556685
3504.202695	701335.344454	42.561690
3504.284193	701264.665060	42.566695
3504.048333	701191.254440	42.571700
3503.929153	701130.893981	42.576704
3503.608937	701064.403906	42.581709
3503.884010	701009.195740	42.586714
3504.342753	700945.260017	42.591719
3504.211449	700885.297432	42.596724
3504.392621	700812.262182	42.601728
3504.626779	700756.313697	42.606733
3504.311613	700670.735762	42.611738
3504.541250	700609.220855	42.616743
3504.278316	700544.158641	42.621748
3504.058034	700476.554238	42.626752
3504.167798	700422.512695	42.631757
3504.005174	700349.232023	42.636762
3504.092028	700286.446165	42.641767
3503.875103	700230.419538	42.646772
3504.152868	700164.271384	42.651776
3504.068524	700107.327499	42.656781
3503.869289	700034.298728	42.661786
3504.261534	699969.173979	42.666791
3504.070848	699918.807104	42.671796
3504.406248	699843.750245	42.676800
3504.049607	699783.767526	42.681805
3504.072506	699713.979908	42.686810
3504.200120	699648.250227	42.691815
3503.812768	699596.571888	42.696820
3504.168744	699535.426252	42.701824
3504.062376	699474.604898	42.706829
3504.003048	699414.719776	42.711834
3503.910642	699348.427632	42.716839
3503.864085	699285.855404	42.721844
3504.036502	699232.293253	42.726848
3503.666429	699181.554041	42.731853
3503.528308	699120.486926	42.736858
3503.723223	699056.034102	42.741863
3503.699553	699001.260159	42.746868
3503.861528	698937.706637	42.751872
3504.292557	698885.044211	42.756877
3504.214687	698818.944503	42.761882
3504.250026	698752.527387	42.766887
3503.949283	698692.478273	42.771892
3503.898293	698622.246752	42.776896
3503.863777	698567.571310	42.781901
3503.995022	698518.883204	42.786906
3504.108332	698456.527272	42.791911
3503.748473	698390.967914	42.796916
3503.736368	698329.128857	42.801921
3503.769279	698290.895142	42.806925
3503.544745	698227.449877	42.811930
3503.961269	698171.603982	42.816935
3503.434693	698127.645368	42.821940
3503.807215	698062.012591	42.826945
3503.782970	698020.854039	42.831949
3503.739715	697948.378751	42.836954
3504.015779	697888.726236	42.841959
3503.451692	697844.424386	42.846964
3503.856556	697782.065345	42.851969
3503.904766	697725.879592	42.856973
3503.600305	697651.207714	42.861978
3503.800703	697596.089798	42.866983
3503.561634	697545.518402	42.871988
3503.657011	697489.422800	42.876993
3503.303565	697446.824312	42.881997
3503.555522	697393.635584	42.887002
3503.477825	697336.424034	42.892007
3503.368642	697290.652350	42.897012
3503.423151	697244.853456	42.902017
3503.811064	697191.839980	42.907021
3503.712060	697140.447688	42.912026
3503.949911	697088.701279	42.917031
3503.785475	697032.546142	42.922036
3503.663620	696968.726847	42.927041
3503.608242	696914.293164	42.932045
3503.534562	696868.314557	42.937050
3503.489926	696808.061212	42.942055
3503.304314	696755.239055	42.947060
3503.594653	696703.034251	42.952065
3503.773946	696656.366484	42.957069
3503.459225	696609.332379	42.962074
3503.572051	696547.708831	42.967079
3503.577972	696497.439103	42.972084
3503.542101	696439.916511	42.977089
3503.840988	696390.443181	42.982093
3503.328098	696338.169680	42.987098
3503.479140	696277.781025	42.992103
3503.469145	696233.330038	42.997108
3503.373032	696186.705169	43.002113
3503.439055	696138.163825	43.007117
3503.287362	696093.089067	43.012122
3503.398718	696043.495522	43.017127
3503.366571	695989.151755	43.022132
3503.268210	695931.884775	43.027137
3503.794688	695881.625219	43.032141
3503.418744	695837.829247	43.037146
3503.591487	695781.809495	43.042151
3503.407712	695741.561657	43.047156
3503.740222	695681.984380	43.052161
3503.503567	695635.926756	43.057165
3503.326639	695585.632242	43.062170
3503.304583	695538.544207	43.067175
3503.104241	695492.032304	43.072180
3503.216254	695448.303181	43.077185
3503.381327	695396.061574	43.082189
3503.248850	695355.853256	43.087194
3503.372553	695304.214666	43.092199
3503.710728	695243.241099	43.097204
3503.325388	695191.138706	43.102209
3503.606463	695137.285119	43.107213
3503.755615	695087.928641	43.112218
3503.881401	695032.807028	43.117223
3503.583819	694980.390552	43.122228
3503.942592	694920.555176	43.127233
3503.731231	694868.521679	43.132237
3503.443573	694830.474986	43.137242
3503.554630	694770.878342	43.142247
3503.234695	694726.520587	43.147252
3503.156527	694673.618554	43.152257
3503.049059	694638.972875	43.157261
3503.171076	694594.790301	43.162266
3503.187991	694533.417195	43.167271
3503.122279	694491.701961	43.172276
3503.408390	694445.900141	43.177281
3503.511347	694387.794266	43.182285
3503.113543	694343.795562	43.187290
3503.482237	694290.817615	43.192295
3503.592764	694242.805630	43.197300
3503.255748	694191.982499	43.202305
3503.192223	694144.993363	43.207309
3502.924513	694112.013294	43.212314
3502.737461	694057.782673	43.217319
3502.623725	694032.635182	43.222324
3502.849439	693994.699255	43.227329
3502.820204	693956.854911	43.232333
3502.484576	693916.673538	43.237338
3502.933481	693873.179560	43.242343
3503.047335	693835.808491	43.247348
3503.013570	693785.878069	43.252353
3503.163462	693737.359494	43.257357
3503.178830	693693.687386	43.262362
3503.076751	693644.016112	43.267367
3503.231044	693605.493438	43.272372
3503.330555	693559.469107	43.277377
3503.270831	693509.989060	43.282381
3502.833537	693466.688857	43.287386
3502.805366	693421.679633	43.292391
3502.609283	693404.004823	43.297396
3502.514856	693357.116092	43.302401
3502.612533	693314.522833	43.307405
3502.644636	693286.663245	43.312410
3503.689155	693235.308559	43.317415
3503.541292	693214.491785	43.322420
3503.222155	693157.491968	43.327425
3503.256001	693113.266818	43.332429
3503.213453	693061.941031	43.337434
3502.551865	693024.893295	43.342439
3501.784845	693015.270427	43.347444
3502.024557	692967.230269	43.352449
3503.154208	692920.187283	43.357453
3503.554145	692867.245460	43.362458
3503.600498	692817.793829	43.367463
3503.045642	692787.293546	43.372468
3503.143367	692748.875973	43.377473
3503.028324	692699.897969	43.382477
3503.172561	692665.501582	43.387482
3503.157571	692607.055306	43.392487
3503.059975	692581.304125	43.397492
3503.106063	692541.401847	43.402497
3502.565248	692494.532382	43.407501
3502.669565	692459.196632	43.412506
3503.031050	692411.581120	43.417511
3502.986619	692377.811651	43.422516
3503.110320	692336.303822	43.427521
3503.477270	692270.280853	43.432525
3503.278899	692230.914923	43.437530
3503.580273	692181.915206	43.442535
3503.772169	692144.573931	43.447540
3503.982230	692078.077928	43.452545
3503.673938	692031.764677	43.457549
3503.159314	691984.092258	43.462554
3503.326335	691931.183263	43.467559
3502.904570	691906.180013	43.472564
3502.707912	691855.071663	43.477569
3502.894843	691807.282701	43.482573
3502.938750	691777.874257	43.487578
3503.213545	691718.827182	43.492583
3503.254519	691685.041020	43.497588
3503.210584	691633.856490	43.502593
3503.547465	691592.807574	43.507597
3503.375480	691549.404580	43.512602
3503.576823	691493.502354	43.517607
3503.456216	691440.538349	43.522612
3503.270229	691392.211612	43.527617
3503.470891	691353.024814	43.532621
3502.840250	691311.238513	43.537626
3503.139052	691261.885921	43.542631
3502.717075	691222.502637	43.547636
3502.624412	691182.418145	43.552641
3502.860247	691138.945959	43.557645
3502.828723	691112.085108	43.562650
3503.601049	691059.170722	43.567655
3503.097933	691017.262527	43.572660
3503.383880	690958.308103	43.577665
3503.238896	690916.141411	43.582669
3503.076688	690873.280810	43.587674
3503.095943	690809.344243	43.592679
3502.953253	690787.227350	43.597684
3502.902047	690742.158655	43.602689
3503.246308	690715.085431	43.607693
3502.920510	690674.390271	43.612698
3502.960696	690624.479726	43.617703
3502.783563	690599.332995	43.622708
3502.560928	690550.012646	43.627713
3502.844333	690505.036889	43.632717
3502.865277	690479.707918	43.637722
3503.244256	690430.088757	43.642727
3502.829110	690387.217750	43.647732
3502.854849	690347.110008	43.652737
3503.188284	690311.280215	43.657741
3502.933971	690260.620064	43.662746
3502.928728	690221.711033	43.667751
3503.046633	690175.915025	43.672756
3502.910493	690136.032043	43.677761
3503.082246	690102.417392	43.682765
3502.698866	690058.793212	43.687770
3502.714069	690013.411362	43.692775
3502.979040	689980.029685	43.697780
3503.082085	689939.758109	43.702785
3503.052845	689906.822707	43.707789
3502.670601	689871.606674	43.712794
3502.902502	689817.430528	43.717799
3502.894369	689777.674138	43.722804
3502.834852	689737.030363	43.727809
3502.983532	689691.326333	43.732813
3502.793123	689660.158185	43.737818
3502.821406	689625.669706	43.742823
3502.687946	689584.340777	43.747828
3503.013180	689544.926513	43.752833
3502.999682	689509.051166	43.757837
3503.060334	689472.566323	43.762842
3503.135092	689421.896974	43.767847
3502.934554	689379.284355	43.772852
3503.004150	689338.070120	43.777857
3503.061591	689302.530594	43.782861
3502.814252	689272.017388	43.787866
3502.758777	689225.249856	43.792871
3502.836165	689193.140233	43.797876
3503.130127	689148.504288	43.802881
3503.169471	689098.237056	43.807885
3502.847320	689078.484396	43.812890
3503.130568	689019.368399	43.817895
3502.889284	688971.187012	43.822900
3502.860256	688942.179399	43.827905
3503.081865	688903.923981	43.832909
3502.962203	688866.520867	43.837914
3503.023424	688815.452217	43.842919
3502.645866	688768.237730	43.847924
3502.729739	688743.291616	43.852929
3502.726413	688690.043217	43.857933
3502.344814	688658.753801	43.862938
3502.636239	688639.197668	43.867943
3502.355894	688599.232092	43.872948
3502.936381	688576.244097	43.877953
3502.944776	688539.216652	43.882957
3502.820671	688486.982282	43.887962
3502.624904	688445.310018	43.892967
3502.758943	688417.866389	43.897972
3502.564223	688381.468969	43.902977
3503.136548	688338.176629	43.907981
3502.729709	688305.596187	43.912986
3503.171946	688258.144408	43.917991
3502.987416	688232.444819	43.922996
3502.762276	688186.595674	43.928001
3502.700972	688148.333898	43.933005
3502.638867	688109.325559	43.938010
3502.873218	688068.426750	43.943015
3502.423707	688042.670742	43.948020
3502.413212	688016.294860	43.953025
3502.825483	687975.366313	43.958029
3502.694649	687941.494835	43.963034
3502.872737	687891.745479	43.968039
3502.880815	687848.991699	43.973044
3502.843722	687816.846265	43.978049
3503.220763	687774.081106	43.983053
3503.251380	687740.630208	43.988058
3503.199189	687685.293551	43.993063
3503.054857	687647.043330	43.998068
3502.775215	687612.548109	44.003073
3502.945276	687570.711980	44.008077
3503.008773	687524.363963	44.013082
3503.108010	687481.692967	44.018087
3502.967894	687436.074858	44.023092
3502.763343	687402.810775	44.028097
3502.780161	687359.555511	44.033101
3502.780876	687322.076380	44.038106
3502.913451	687280.842365	44.043111
3502.588269	687250.982188	44.048116
3502.446383	687205.761396	44.053121
3502.749308	687174.005613	44.058125
3502.351460	687155.903744	44.063130
3502.579334	687113.707556	44.068135
3502.658076	687082.486135	44.073140
3502.693244	687039.524962	44.078145
3502.939470	687008.076588	44.083149
3502.664666	686977.361033	44.088154
3502.597675	686931.379902	44.093159
3502.805354	686893.317363	44.098164
3502.832303	686859.216726	44.103169
3502.587733	686816.997449	44.108173
3502.500185	686783.214047	44.113178
3502.759283	686748.925413	44.118183
3502.784920	686719.752319	44.123188
3502.650829	686684.283817	44.128193
3503.076376	686641.206653	44.133197
3502.830958	686611.380996	44.138202
3503.079861	686568.033928	44.143207
3502.836194	686529.347348	44.148212
3502.604776	686499.220349	44.153217
3502.850911	686458.760320	44.158221
3502.765662	686423.780527	44.163226
3503.062178	686383.112747	44.168231
3503.097798	686353.190153	44.173236
3502.879230	686311.760690	44.178241
3503.324089	686268.827912	44.183245
3502.798495	686218.189723	44.188250
3502.665018	686172.315250	44.193255
3502.939616	686143.945530	44.198260
3503.037096	686111.124725	44.203265
3502.821821	686063.072865	44.208269
3502.851881	686022.298032	44.213274
3502.843721	685976.700602	44.218279
3502.868348	685947.425627	44.223284
3502.635310	685905.050855	44.228289
3502.760992	685869.685700	44.233293
3502.386448	685840.127684	44.238298
3502.649555	685794.534421	44.243303
3502.664945	685755.403596	44.248308
3502.648543	685722.948624	44.253313
3502.495837	685699.675900	44.258317
3502.395467	685675.846889	44.263322
3502.640490	685637.723146	44.268327
3502.619750	685596.158250	44.273332
3502.804372	685573.427011	44.278337
3502.822192	685527.673695	44.283341
3502.756820	685503.091718	44.288346
3502.403354	685459.241211	44.293351
3502.581591	685418.737951	44.298356
3502.596658	685380.750588	44.303361
3502.862714	685357.806256	44.308365
3502.662071	685319.605261	44.313370
3502.943552	685280.478329	44.318375
3502.713234	685250.645703	44.323380
3502.749927	685214.197401	44.328385
3502.713480	685165.065838	44.333389
3502.741172	685132.452135	44.338394
3502.834606	685096.939931	44.343399
3502.466803	685054.882106	44.348404
3502.495279	685033.170957	44.353409
3502.881116	684993.079666	44.358413
3502.702722	684952.533521	44.363418
3502.592455	684913.967425	44.368423
3502.934767	684879.707810	44.373428
3502.728097	684861.420483	44.378433
3503.175671	684819.924231	44.383437
3503.124133	684781.895553	44.388442
3503.214078	684737.619989	44.393447
3503.362217	684695.674637	44.398452
3503.143365	684658.270462	44.403457
3502.927735	684589.847640	44.408461
3502.964632	684556.682686	44.413466
3503.167251	684507.010294	44.418471
3503.071346	684472.821356	44.423476
3502.898798	684433.217919	44.428481
3503.106153	684387.477425	44.433485
3502.855398	684341.563238	44.438490
3502.889154	684299.435750	44.443495
3503.083216	684255.539004	44.448500
3502.654191	684235.345246	44.453505
3502.710846	684191.520623	44.458509
3502.540752	684161.923451	44.463514
3502.915586	684118.245209	44.468519
3502.834712	684070.758152	44.473524
3502.828778	684043.025601	44.478529
3502.874454	683999.500611	44.483533
3502.570621	683972.912343	44.488538
3502.537084	683939.955916	44.493543
3502.759427	683890.127537	44.498548
3502.611788	683862.119033	44.503553
3502.786494	683831.866469	44.508557
3502.429882	683795.726256	44.513562
3502.630227	683748.191180	44.518567
3502.910947	683727.530797	44.523572
3502.738463	683697.633753	44.528577
3502.769069	683647.536885	44.533581
3502.839842	683622.180493	44.538586
3502.991266	683569.374442	44.543591
3502.934763	683545.731797	44.548596
3502.575937	683510.985046	44.553601
3503.035152	683462.957685	44.558605
3502.868742	683425.490010	44.563610
3502.727235	683385.578138	44.568615
3502.664346	683348.740422	44.573620
3502.939711	683307.116284	44.578625
3502.813686	683265.309119	44.583629
3502.903157	683234.819645	44.588634
3503.029779	683208.158217	44.593639
3502.850889	683167.056452	44.598644
3502.673419	683127.398356	44.603649
3502.696584	683075.506914	44.608653
3502.487515	683060.204147	44.613658
3502.419343	683014.054002	44.618663
3502.583578	682983.003605	44.623668
3502.078183	682962.869402	44.628673
3502.577411	682914.981962	44.633677
3502.651079	682888.178934	44.638682
3502.361959	682841.914934	44.643687
3502.519985	682826.152905	44.648692
3502.388653	682795.001178	44.653697
3502.436245	682760.333994	44.658701
3502.252941	682729.190607	44.663706
3502.435986	682692.508915	44.668711
3502.494343	682665.707759	44.673716
3502.290010	682640.941760	44.678721
3502.345523	682604.728919	44.683725
3502.505091	682575.520471	44.688730
3502.313699	682545.523170	44.693735
3502.554125	682511.420861	44.698740
3502.281111	682486.167765	44.703745
3502.685737	682452.237378	44.708749
3502.380070	682426.142900	44.713754
3502.764988	682394.954546	44.718759
3502.648902	682352.792967	44.723764
3502.359984	682320.271179	44.728769
3502.794933	682299.532361	44.733773
3502.588313	682261.568533	44.738778
3502.732137	682226.485064	44.743783
3502.944273	682185.912069	44.748788
3502.664081	682161.406277	44.753793
3502.799512	682110.287685	44.758797
3502.707359	682080.870128	44.763802
3502.584198	682039.953321	44.768807
3502.850390	682003.404576	44.773812
3502.839172	681976.164646	44.778817
3502.968728	681930.026255	44.783821
3502.695793	681898.446584	44.788826
3502.814045	681861.921652	44.793831
3502.872675	681827.846757	44.798836
3503.022576	681788.128910	44.803841
3502.874537	681737.204357	44.808845
3502.520600	681714.004414	44.813850
3502.529507	681676.201860	44.818855
3502.850113	681637.252098	44.823860
3502.679151	681597.536492	44.828865
3502.919214	681546.995173	44.833869
3502.650381	681524.228969	44.838874
3502.441669	681493.683222	44.843879
3502.735212	681469.927727	44.848884
3502.690495	681425.160251	44.853889
3502.875574	681384.090115	44.858893
3502.788455	681361.094341	44.863898
3502.615140	681321.676762	44.868903
3503.105041	681283.345082	44.873908
3502.668758	681251.939516	44.878913
3502.925767	681199.899305	44.883917
3502.610523	681172.308631	44.888922
3502.742016	681127.809511	44.893927
3502.927423	681091.469677	44.898932
3502.672821	681059.884095	44.903937
3503.159095	681008.751365	44.908941
3502.710286	680977.048075	44.913946
3502.767638	680934.452933	44.918951
3502.824482	680898.183326	44.923956
3502.524409	680863.616066	44.928961
3502.845107	680820.279684	44.933965
3503.014175	680792.359021	44.938970
3502.366608	680745.545788	44.943975
3502.646308	680709.437952	44.948980
3502.529223	680679.571726	44.953985
3502.704242	680642.634117	44.958989
3502.473717	680625.537665	44.963994
3502.366265	680581.075271	44.968999
3502.586960	680553.344616	44.974004
3502.541482	680527.699956	44.979009
3502.244478	680484.563396	44.984013
3502.327624	680466.269320	44.989018
3502.705003	680422.323998	44.994023
3502.816441	680394.162570	44.999028
3502.429839	680375.696662	45.004033
3502.614936	680326.104100	45.009037
3502.427925	680295.351544	45.014042
3502.471610	680255.495142	45.019047
3502.523913	680233.619242	45.024052
3502.275994	680206.612313	45.029057
3502.310716	680163.021087	45.034061
3502.386607	680143.631698	45.039066
3502.400421	680110.155565	45.044071
3502.716952	680074.437672	45.049076
3502.279070	680046.764197	45.054081
3502.430594	680017.000998	45.059085
3502.341222	679991.212637	45.064090
3502.373121	679952.552382	45.069095
3502.496017	679920.751242	45.074100
3502.368883	679891.083366	45.079105
3502.596815	679850.098950	45.084109
3502.791470	679820.328010	45.089114
3502.450573	679785.215465	45.094119
3502.313284	679763.419503	45.099124
3502.242845	679732.795302	45.104129
3502.374871	679699.248384	45.109133
3502.257029	679669.877153	45.114138
3502.493152	679639.351572	45.119143
3502.544714	679604.223485	45.124148
3502.168635	679575.043948	45.129153
3502.512172	679555.908114	45.134157
3502.569093	679520.828642	45.139162
3502.204751	679493.141382	45.144167
3502.507127	679459.266627	45.149172
3502.318776	679437.079778	45.154177
3502.526309	679382.895359	45.159181
3502.539847	679375.321118	45.164186
3502.333125	679337.843383	45.169191
3502.816952	679298.906655	45.174196
3502.472636	679277.143656	45.179201
3502.449946	679236.247627	45.184205
3502.750684	679200.279868	45.189210
3502.257660	679171.865585	45.194215
3502.232595	679130.321849	45.199220
3502.343415	679123.677911	45.204225
3502.426862	679088.592425	45.209229
3502.486391	679056.748931	45.214234
3502.243096	679034.171620	45.219239
3502.329942	678995.896848	45.224244
3501.945042	678967.015750	45.229249
3502.051609	678947.867886	45.234253
3502.132001	678932.111980	45.239258
3502.325638	678903.882639	45.244263
3502.272198	678872.007304	45.249268
3502.158720	678851.052187	45.254273
3502.071937	678816.442091	45.259277
3502.355565	678793.328991	45.264282
3502.167838	678747.326568	45.269287
3502.618555	678728.171363	45.274292
3502.294045	678708.745295	45.279297
3502.179976	678674.637365	45.284301
3502.299550	678630.227792	45.289306
3502.336207	678607.553487	45.294311
3502.526769	678572.548034	45.299316
3502.171855	678550.834885	45.304321
3502.437754	678517.012511	45.309325
3502.511968	678491.342466	45.314330
3502.474478	678455.228257	45.319335
3502.740374	678420.757853	45.324340
3502.545988	678390.398729	45.329345
3502.519848	678354.730654	45.334349
3502.515701	678315.471621	45.339354
3502.439246	678291.021578	45.344359
3502.861381	678257.670737	45.349364
3502.155247	678223.808168	45.354369
3502.445467	678190.379175	45.359373
3502.311462	678159.361646	45.364378
3502.287693	678134.802864	45.369383
3502.313384	678100.321024	45.374388
3502.016955	678082.782298	45.379393
3502.242623	678056.986445	45.384397
3502.575270	678027.884527	45.389402
3502.345163	677993.494262	45.394407
3502.488198	677972.345414	45.399412
3502.122348	677941.066411	45.404417
3502.474242	677906.978520	45.409421
3502.444471	677880.078304	45.414426
3502.724547	677850.585895	45.419431
3502.744131	677818.495598	45.424436
3502.514998	677788.837773	45.429441
3502.880284	677749.814418	45.434445
3502.682056	677720.051631	45.439450
3502.610879	677684.338568	45.444455
3502.650200	677648.806464	45.449460
3502.617217	677614.033528	45.454465
3502.701998	677579.540013	45.459469
3502.517159	677533.082640	45.464474
3502.203062	677512.257200	45.469479
3502.321916	677474.817916	45.474484
3502.340511	677446.513324	45.479489
3502.553310	677415.386331	45.484493
3502.443699	677397.068116	45.489498
3502.532680	677360.131563	45.494503
3502.360027	677323.636594	45.499508
3502.314538	677303.563664	45.504513
3502.688761	677263.739551	45.509517
3502.449842	677236.822103	45.514522
3502.517664	677204.173623	45.519527
3502.444208	677167.013927	45.524532
3502.416658	677148.183414	45.529537
3502.283119	677102.413029	45.534541
3502.252759	677091.106997	45.539546
3502.281128	677057.467926	45.544551
3502.414992	677027.996997	45.549556
3501.978797	677008.884733	45.554561
3502.437280	676981.552653	45.559565
3502.387410	676938.059821	45.564570
3502.586069	676911.368304	45.569575
3502.414919	676870.635776	45.574580
3502.135931	676856.729438	45.579585
3502.423326	676804.709298	45.584589
3502.485346	676787.059221	45.589594
3502.354452	676756.883602	45.594599
3502.543267	676729.096911	45.599604
3502.404203	676694.636993	45.604609
3502.160856	676664.629096	45.609613
3502.633594	676641.180492	45.614618
3502.570378	676610.395271	45.619623
3502.526296	676569.241832	45.624628
3502.487706	676554.398460	45.629633
3502.260616	676515.766522	45.634637
3502.501166	676489.963866	45.639642
3502.223739	676458.665287	45.644647
3502.499531	676416.710983	45.649652
3502.360150	676390.571996	45.654657
3502.307710	676355.548388	45.659661
3502.238012	676345.693080	45.664666
3501.892424	676314.754076	45.669671
3502.251593	676276.174040	45.674676
3501.914608	676267.160021	45.679681
3502.283127	676227.481912	45.684685
3502.099729	676220.336210	45.689690
3501.796410	676183.509455	45.694695
3502.608796	676159.355837	45.699700
3502.371181	676127.850248	45.704705
3502.180713	676099.725502	45.709709
3502.062588	676068.499028	45.714714
3502.234529	676039.816043	45.719719
3502.208436	676014.205509	45.724724
3502.063845	676010.990179	45.729729
3502.275198	675973.230599	45.734733
3502.319561	675951.296055	45.739738
3502.296345	675909.239229	45.744743
3502.431431	675881.508697	45.749748
3502.238264	675862.702869	45.754753
3502.507467	675825.830196	45.759757
3502.566177	675794.573664	45.764762
3502.299278	675776.726691	45.769767
3502.624993	675724.146005	45.774772
3502.130250	675703.246594	45.779777
3502.351009	675674.105914	45.784781
3502.367700	675639.865604	45.789786
3502.384471	675619.878452	45.794791
3502.481004	675579.993222	45.799796
3502.370526	675554.495002	45.804801
3502.240947	675509.912211	45.809805
3502.411968	675414.993512	45.814810
3502.208284	675284.052614	45.819815
3502.166733	675078.324122	45.824820
3501.927659	674835.691642	45.829825
3501.899073	674523.089376	45.834829
3501.696001	674162.854238	45.839834
3501.318606	673738.082690	45.844839
3501.540683	673253.473842	45.849844
3501.067193	672707.387321	45.854849
3500.652947	672099.638191	45.859853
3500.248645	671459.838853	45.864858
3499.718743	670742.779924	45.869863
3499.664506	669964.302167	45.874868
3499.078009	669138.620286	45.879873
3498.306280	668250.901697	45.884877
3497.554301	667306.482524	45.889882
3497.013906	666302.520911	45.894887
3496.638481	665236.461581	45.899892
3495.851310	664119.007293	45.904897
3494.916317	662935.774717	45.909901
3494.324450	661696.890683	45.914906
3493.449345	660396.497497	45.919911
3492.436620	659032.849618	45.924916
3491.243928	657631.892130	45.929921
3490.200560	656153.355315	45.934925
3489.462612	654633.490041	45.939930
3488.234560	653054.925432	45.944935
3487.369696	651406.302328	45.949940
3485.951658	649716.821115	45.954945
3484.920029	647970.114244	45.959949
3483.919578	646172.610396	45.964954
3482.043003	644312.734148	45.969959
3481.032046	642393.066280	45.974964
3479.423792	640437.724027	45.979969
3477.960616	638428.557264	45.984973
3476.745862	636362.817811	45.989978
3474.999684	634256.367450	45.994983
3473.752774	632089.542208	45.999988
3471.924686	629879.358266	46.004993
3470.011882	627623.205663	46.009997
3468.401440	625316.286209	46.015002
3466.275145	622979.446579	46.020007
3464.791529	620588.627299	46.025012
3463.024848	618165.952557	46.030017
3460.855702	615685.305500	46.035021
3458.993030	613167.895838	46.040026
3456.844806	610611.342925	46.045031
3454.838658	608017.610900	46.050036
3452.621765	605380.815934	46.055041
3450.463845	602709.973171	46.060045
3448.348472	599996.984128	46.065050
3445.889989	597257.354235	46.070055
3443.484886	594470.613051	46.075060
3441.314671	591656.597496	46.080065
3438.700672	588817.014143	46.085069
3436.662029	585916.549648	46.090074
3433.891280	583004.249193	46.095079
3431.675789	580041.580469	46.100084
3428.659773	577061.431845	46.105089
3426.369492	574046.843154	46.110093
3423.662804	571012.327342	46.115098
3420.998416	567949.798785	46.120103
3418.485799	564849.107370	46.125108
3415.849562	561736.415462	46.130113
3412.834545	558577.562765	46.135117
3410.445922	555394.930587	46.140122
3407.219817	552193.942623	46.145127
3404.485578	548959.505410	46.150132
3401.532918	545714.762790	46.155137
3398.428935	542438.373436	46.160141
3395.355295	539143.308678	46.165146
3392.398354	535830.257143	46.170151
3389.510330	532493.925033	46.175156
3386.749721	529133.791748	46.180161
3383.007085	525744.530622	46.185165
3380.514401	522348.287122	46.190170
3377.312203	518937.257647	46.195175
3374.220729	515495.746573	46.200180
3370.888777	512033.100405	46.205185
3367.741848	508553.036771	46.210189
3364.597621	505068.123165	46.215194
3360.927422	501560.705872	46.220199
3357.845229	498039.044441	46.225204
3354.235837	494504.286256	46.230209
3350.841861	490963.800657	46.235213
3347.275327	487393.013314	46.240218
3343.647346	483833.052047	46.245223
3340.597840	480242.820400	46.250228
3336.874018	476652.750044	46.255233
3333.488135	473049.720115	46.260237
3329.997240	469431.528568	46.265242
3326.199294	465818.884547	46.270247
3322.877810	462182.990988	46.275252
3318.942014	458550.789407	46.280257
3315.525277	454901.220798	46.285261
3311.931339	451246.419927	46.290266
3308.124878	447597.204119	46.295271
3304.612521	443929.260270	46.300276
3300.759162	440261.009586	46.305281
3296.891991	436581.045130	46.310285
3293.288943	432903.942903	46.315290
3289.754183	429226.044099	46.320295
3285.649719	425540.613216	46.325300
3281.739944	421855.301123	46.330305
3278.152095	418172.282941	46.335309
3274.513400	414479.521647	46.340314
3270.759224	410787.575590	46.345319
3266.852702	407090.367996	46.350324
3263.143006	403403.017172	46.355329
3259.061670	399700.684715	46.360333
3255.530399	396006.347829	46.365338
3251.631373	392307.136985	46.370343
3247.636193	388598.748430	46.375348
3243.509574	384905.649802	46.380353
3239.758538	381209.039978	46.385357
3236.203150	377511.604109	46.390362
3231.714606	373832.280055	46.395367
3227.739956	370135.754910	46.400372
3223.641634	366459.398660	46.405377
3219.599255	362776.824673	46.410381
3215.873035	359100.159332	46.415386
3211.706110	355430.279092	46.420391
3208.080312	351764.186691	46.425396
3204.191913	348113.350005	46.430401
3200.185385	344445.954523	46.435405
3196.215959	340789.949235	46.440410
3192.245893	337142.555608	46.445415
3188.002882	333493.753884	46.450420
3183.927120	329854.656717	46.455425
3179.864249	326214.103598	46.460429
3175.727673	322584.873553	46.465434
3171.697124	318971.736568	46.470439
3167.844135	315356.696196	46.475444
3163.679598	311761.179345	46.480449
3159.722147	308164.135268	46.485453
3155.729459	304574.042919	46.490458
3151.383959	300991.781687	46.495463
3147.539048	297419.132796	46.500468
3143.253208	293859.675919	46.505473
3139.300117	290305.630818	46.510477
3135.491135	286755.664917	46.515482
3131.431508	283222.944278	46.520487
3127.385398	279684.058751	46.525492
3123.287122	276160.371224	46.530497
3118.795320	272655.056509	46.535501
3115.323722	269144.615111	46.540506
3111.143107	265661.305064	46.545511
3106.867519	262170.475689	46.550516
3102.797290	258695.416697	46.555521
3098.343689	255224.087160	46.560525
3094.555854	251762.971477	46.565530
3090.333578	248326.319401	46.570535
3086.266629	244894.101870	46.575540
3082.540503	241471.569803	46.580545
3078.367508	238060.645216	46.585549
3074.560553	234656.491918	46.590554
3070.061465	231270.855250	46.595559
3066.385142	227877.213435	46.600564
3062.362957	224505.945014	46.605569
3058.164035	221144.806990	46.610573
3054.182292	217787.733505	46.615578
3049.815589	214447.742115	46.620583
3045.944409	211100.812239	46.625588
3042.090281	207791.957495	46.630593
3037.778847	204471.360305	46.635597
3033.967524	201088.797171	46.640602
3029.599191	197798.092593	46.645607
3025.868052	194516.556358	46.650612
3021.737342	191251.557569	46.655617
3017.743967	188002.326420	46.660621
3013.799027	184746.702482	46.665626
3009.423055	181517.617532	46.670631
3005.452526	178278.584208	46.675636
3000.980558	175069.510033	46.680641
2996.985294	171876.686598	46.685645
2993.056786	168687.273823	46.690650
2988.882507	165521.620117	46.695655
2984.959077	162364.776908	46.700660
2980.987153	159219.394041	46.705665
2976.957455	156078.394299	46.710669
2972.834096	152947.856185	46.715674
2968.702325	149840.931602	46.720679
2964.489015	146741.079652	46.725684
2960.669148	143652.969798	46.730689
2956.501895	140574.338538	46.735693
2952.330289	137508.782227	46.740698
2948.359386	134475.539414	46.745703
2944.396864	131435.241803	46.750708
2940.049850	128415.030880	46.755713
2935.859789	125407.880662	46.760717
2932.110065	122403.875305	46.765722
2927.651070	119419.776350	46.770727
2923.880273	116457.183139	46.775732
2919.571215	113503.380459	46.780737
2915.599638	110564.615739	46.785741
2911.354985	107642.083353	46.790746
2907.291420	104732.712849	46.795751
2902.865840	101834.240581	46.800756
2898.921049	98956.469869	46.805761
2894.519029	96099.135587	46.810765
2890.853435	93237.417985	46.815770
2886.241965	90419.919761	46.820775
2881.902839	87596.747723	46.825780
2877.694214	84814.729583	46.830785
2873.591702	82035.061078	46.835789
2869.480394	79274.521477	46.840794
2865.368600	76542.131456	46.845799
2860.661399	73810.421833	46.850804
2856.550663	71116.003040	46.855809
2851.651043	68440.692772	46.860813
2847.514920	65780.442501	46.865818
2842.822749	63157.377180	46.870823
2837.847829	60547.591580	46.875828
2833.401746	57974.748348	46.880833
2828.323297	55446.789644	46.885837
2823.430331	52936.102898	46.890842
2817.747266	50493.171256	46.895847
2811.113395	48096.668390	46.900852
2803.322405	45789.233957	46.905857
2795.042100	43575.280778	46.910861
2786.969379	41439.312786	46.915866
2778.369451	39409.828068	46.920871
2770.433786	37462.452197	46.925876
2762.944261	35616.365376	46.930881
2755.387805	33859.293470	46.935885
2748.894445	32206.520541	46.940890
2741.662326	30633.500145	46.945895
2735.640620	29150.024829	46.950900
2729.444786	27740.958679	46.955905
2723.334711	26411.149831	46.960909
2717.854887	25149.309038	46.965914
2712.158242	23953.291344	46.970919
2707.213865	22818.179212	46.975924
2702.259705	21749.769723	46.980929
2697.343272	20727.369940	46.985933
2692.545691	19751.750343	46.990938
2687.563416	18823.754499	46.995943
2683.129180	17937.957668	47.000948
2678.539386	17089.377396	47.005953
2674.011889	16292.373657	47.010957
2670.133254	15520.871043	47.015962
2665.470071	14793.818212	47.020967
2661.293040	14088.160849	47.025972
2657.360543	13405.413495	47.030977
2653.053378	12751.033258	47.035981
2649.112122	12123.744431	47.040986
2644.949611	11531.773962	47.045991
2640.967983	10930.583378	47.050996
2636.460916	10383.728151	47.056001
2632.405182	9859.765190	47.061005
2628.395396	9352.337928	47.066010
2623.996716	8859.223018	47.071015
2620.013773	8397.274497	47.076020
2615.973977	7946.161987	47.081025
2612.078796	7528.230035	47.086029
2608.784165	7112.205520	47.091034
2604.709039	6713.740506	47.096039
2600.652294	6319.211857	47.101044
2597.324428	5948.535603	47.106049
2593.303793	5585.227260	47.111053
2589.485209	5233.255754	47.116058
2585.921153	4897.290078	47.121063
2582.634207	4565.476946	47.126068
2579.080366	4243.940571	47.131073
2575.671537	3920.826671	47.136077
2572.202113	3598.137600	47.141082
2568.730282	3300.452251	47.146087
2565.062749	2985.023151	47.151092
2561.924050	2693.125665	47.156097
2558.171886	2400.387494	47.161101
2554.775040	2099.656143	47.166106
2550.924637	1819.267426	47.171111
2547.418283	1543.563191	47.176116
2543.739939	1277.563032	47.181121
2540.084527	1007.995123	47.186125
2536.565432	744.468394	47.191130
2532.816233	492.430941	47.196135
2528.495129	251.777592	47.201140
2521.628769	111.339527	47.206145
2507.948975	180.551846	47.211149
2500.879380	175.270819	47.216154
2496.528322	184.974788	47.221159
2494.644821	185.650042	47.226164
2493.346335	177.767134	47.231169
2491.684832	171.941241	47.236173
2489.258273	170.174240	47.241178
2486.581773	177.869171	47.246183
2483.643492	176.171238	47.251188
2480.191425	172.225140	47.256193
2476.615976	172.830760	47.261197
2473.530501	170.724952	47.266202
2469.784432	172.896815	47.271207
2466.342620	173.248706	47.276212
2463.638127	167.992027	47.281217
2460.075278	177.296353	47.286221
2457.015039	163.704487	47.291226
2453.369814	174.315195	47.296231
2450.074948	169.136234	47.301236
2446.620004	169.176139	47.306241
2443.490777	166.014299	47.311245
2440.033860	157.471580	47.316250
2436.920490	168.542325	47.321255
2433.264051	168.359152	47.326260
2429.797843	164.775377	47.331265
2426.119689	164.957718	47.336269
2423.653559	161.040147	47.341274
2419.786675	159.570524	47.346279
2416.248431	171.090899	47.351284
2412.552287	166.189358	47.356289
2408.998171	169.627493	47.361293
2405.836872	162.272541	47.366298
2402.978492	163.529084	47.371303
2398.865256	165.548478	47.376308
2395.509664	169.458848	47.381313
2391.837004	169.375278	47.386317
2388.793685	160.100668	47.391322
2385.167547	158.032660	47.396327
2381.833950	163.340724	47.401332
2378.862703	161.788017	47.406337
2375.312669	158.864610	47.411341
2372.275888	147.945880	47.416346
2368.776880	151.674308	47.421351
2364.712231	158.334269	47.426356
2361.119064	151.084193	47.431361
2357.181920	153.250184	47.436365
2354.442502	148.504732	47.441370
2351.092017	152.107222	47.446375
2347.712826	155.304379	47.451380
2344.161759	158.396114	47.456385
2340.151447	165.752027	47.461389
2336.924091	155.160000	47.466394
2333.560690	161.224092	47.471399
2329.989401	156.638476	47.476404
2326.813652	147.176993	47.481409
2322.984837	159.229065	47.486413
2319.750585	157.991946	47.491418
2316.240997	160.917008	47.496423
2313.002654	155.847619	47.501428
2309.441625	162.143074	47.506433
2305.643014	160.713579	47.511437
2302.285134	157.069194	47.516442
2299.012307	160.146207	47.521447
2295.441458	161.554177	47.526452
2292.156538	158.431956	47.531457
2288.129899	159.639492	47.536461
2284.853541	158.883162	47.541466
2281.279549	157.279058	47.546471
2278.291916	155.821277	47.551476
2274.693917	149.155014	47.556481
2270.867112	160.571550	47.561485
2267.880406	149.779017	47.566490
2264.184882	151.333298	47.571495
2260.664100	155.535262	47.576500
2257.372142	151.850230	47.581505
2253.548063	159.910551	47.586509
2250.291653	141.177178	47.591514
2246.472938	152.259278	47.596519
2243.122307	154.369967	47.601524
2239.716454	157.817878	47.606529
2235.937035	162.635836	47.611533
2232.932999	151.172468	47.616538
2229.432913	161.903009	47.621543
2225.784216	150.807558	47.626548
2222.481933	145.233341	47.631553
2218.545709	150.709870	47.636557
2215.588930	155.581269	47.641562
2212.051246	151.069134	47.646567
2208.486315	150.297747	47.651572
2204.730204	151.270448	47.656577
2201.315740	153.761323	47.661581
2197.736884	155.131610	47.666586
2194.533415	151.957333	47.671591
2190.588721	151.565195	47.676596
2187.608133	149.304910	47.681601
2184.082103	166.301573	47.686605
2180.810663	151.367562	47.691610
2176.993680	148.281374	47.696615
2173.583646	151.945316	47.701620
2170.510875	142.137788	47.706625
2166.260465	146.328857	47.711629
2162.855842	144.196028	47.716634
2159.500756	147.303681	47.721639
2155.561004	152.841622	47.726644
2152.374536	154.053416	47.731649
2148.787054	161.004568	47.736653
2145.580324	148.419701	47.741658
2142.040588	148.937177	47.746663
2138.730192	160.317866	47.751668
2135.436602	144.055905	47.756673
2131.465623	147.584175	47.761677
2127.983840	147.684387	47.766682
2124.458892	144.506015	47.771687
2121.120872	157.186219	47.776692
2117.872031	144.556234	47.781697
2113.972788	146.438301	47.786701
2110.585788	146.471763	47.791706
2107.155130	146.645049	47.796711
2103.609488	149.443201	47.801716
2100.256074	154.537834	47.806721
2096.711206	155.148940	47.811725
2093.200208	144.751952	47.816730
2090.025635	150.018345	47.821735
2085.840544	147.401709	47.826740
2082.772061	144.852102	47.831745
2079.073829	141.790590	47.836749
2075.441142	137.091191	47.841754
2072.050623	153.140986	47.846759
2068.528048	156.377199	47.851764
2064.989436	144.862324	47.856769
2062.052489	139.126268	47.861773
2058.432242	150.780170	47.866778
2054.932491	149.267778	47.871783
2051.052168	152.174913	47.876788
2047.555394	144.541928	47.881793
2044.477021	140.135629	47.886797
2040.433914	145.634480	47.891802
2036.950775	142.029134	47.896807
2033.754239	144.774814	47.901812
2030.408882	133.979730	47.906817
2026.374960	150.972521	47.911821
2023.119947	140.735988	47.916826
2019.913196	142.860361	47.921831
2016.035102	143.535437	47.926836
2012.509858	147.647331	47.931841
2008.998756	151.336164	47.936845
2006.065655	146.852420	47.941850
2002.689089	146.616838	47.946855
1998.941877	143.436590	47.951860
1995.588371	136.558694	47.956865
1991.683174	137.989143	47.961869
1987.859654	143.221869	47.966874
1984.675366	148.576759	47.971879
1980.924606	143.074815	47.976884
1977.850308	131.051168	47.981889
1974.167002	143.943972	47.986893
1970.709476	136.922245	47.991898
1967.452939	145.874346	47.996903
1963.486906	145.379356	48.001908
1960.459132	135.741372	48.006913
1956.699848	141.996191	48.011917
1953.300140	137.277158	48.016922
1949.753265	141.321625	48.021927
1946.235196	137.878214	48.026932
1943.091409	143.818655	48.031937
1939.134908	134.439259	48.036941
1935.692393	135.774193	48.041946
1932.456738	138.871940	48.046951
1929.050413	135.595191	48.051956
1925.685864	135.035622	48.056961
1921.964942	139.154242	48.061965
1918.016687	133.847779	48.066970
1914.749152	137.097623	48.071975
1911.139669	135.238977	48.076980
1907.822723	124.996002	48.081985
1903.867551	137.575973	48.086989
1900.418722	135.447876	48.091994
1896.873224	131.824917	48.096999
1893.743284	139.063763	48.102004
1890.784176	132.982392	48.107009
1887.342540	139.840749	48.112013
1883.569765	143.644326	48.117018
1879.799403	132.960809	48.122023
1876.083015	142.190202	48.127028
1872.713255	146.760191	48.132033
1869.138914	149.058454	48.137037
1865.723696	144.193649	48.142042
1862.373156	142.188469	48.147047
1858.942747	142.127451	48.152052
1855.539415	142.122941	48.157057
1851.496920	137.505031	48.162061
1848.094036	141.008360	48.167066
1845.093055	124.519941	48.172071
1841.210054	140.019907	48.177076
1837.903306	149.048264	48.182081
1834.168993	139.933203	48.187085
1830.830856	137.674982	48.192090
1827.499662	138.803540	48.197095
1823.486569	148.995666	48.202100
1820.211870	136.341784	48.207105
1816.483928	141.503199	48.212109
1813.086777	136.812466	48.217114
1810.228703	137.996284	48.222119
1806.146042	145.070110	48.227124
1802.621840	135.407092	48.232129
1798.884508	142.267387	48.237133
1795.721775	135.851087	48.242138
1792.311136	138.121179	48.247143
1788.565310	135.409952	48.252148
1785.548441	134.571041	48.257153
1782.010498	139.943822	48.262157
1778.425158	132.892451	48.267162
1774.855494	136.782933	48.272167
1770.984973	143.360164	48.277172
1768.096608	132.411655	48.282177
1764.060585	139.545692	48.287181
1760.701114	141.694673	48.292186
1757.486543	132.906856	48.297191
1753.601536	146.487500	48.302196
1750.203957	136.500692	48.307201
1746.675295	133.157659	48.312205
1743.334862	139.605897	48.317210
1739.812620	137.597993	48.322215
1736.032872	135.606781	48.327220
1732.803001	130.245348	48.332225
1729.187924	133.176796	48.337229
1725.817225	129.049705	48.342234
1722.555465	130.644425	48.347239
1718.812358	130.809420	48.352244
1715.268681	131.116707	48.357249
1711.625106	137.935327	48.362253
1708.376896	131.875993	48.367258
1704.473523	134.495340	48.372263
1700.772895	132.889119	48.377268
1697.848370	127.123832	48.382273
1694.129867	139.159465	48.387277
1690.761690	132.920848	48.392282
1687.434338	137.281677	48.397287
1683.981952	140.296002	48.402292
1680.478123	127.859480	48.407297
1676.591648	137.098756	48.412301
1673.328575	133.279532	48.417306
1669.658538	137.793292	48.422311
1666.075193	138.689320	48.427316
1662.942828	137.306958	48.432321
1659.320483	140.801681	48.437325
1655.845723	136.212892	48.442330
1652.320677	127.778582	48.447335
1648.398801	140.668186	48.452340
1645.044018	132.893673	48.457345
1641.536602	135.177492	48.462349
1638.268913	132.587886	48.467354
1634.628139	135.165677	48.472359
1631.018325	133.806771	48.477364
1627.750288	129.659239	48.482369
1624.170836	124.991278	48.487373
1620.806844	130.139074	48.492378
1617.626989	135.228032	48.497383
1613.385295	134.013999	48.502388
1610.295960	123.368186	48.507393
1606.306469	124.676118	48.512397
1603.010636	141.608599	48.517402
1599.947303	139.092605	48.522407
1596.189308	133.796237	48.527412
1592.759092	130.375687	48.532417
1588.690952	136.112876	48.537421
1585.506203	130.784157	48.542426
1582.345772	129.256116	48.547431
1578.677363	132.984264	48.552436
1575.316950	132.744742	48.557441
1571.806433	130.104928	48.562445
1567.869110	125.402607	48.567450
1564.762167	121.991813	48.572455
1561.110486	137.453144	48.577460
1557.644228	122.498404	48.582465
1554.220870	120.346233	48.587469
1550.825312	130.579775	48.592474
1547.240431	126.379677	48.597479
1543.129524	133.616639	48.602484
1540.189062	121.653713	48.607489
1536.782858	126.250662	48.612493
1533.363563	121.561047	48.617498
1529.990285	128.347558	48.622503
1525.913054	127.271207	48.627508
1522.626412	127.729163	48.632513
1519.108724	136.401833	48.637517
1515.544817	133.930729	48.642522
1511.992176	132.056295	48.647527
1508.476286	132.750075	48.652532
1504.989710	131.129558	48.657537
1501.720611	136.305365	48.662541
1498.060594	131.849736	48.667546
1494.885949	121.292114	48.672551
1490.878527	128.007223	48.677556
1487.649743	126.813587	48.682561
1483.825510	121.383814	48.687565
1480.360370	126.966184	48.692570
1477.500730	120.255733	48.697575
1473.659662	134.489987	48.702580
1470.466879	116.825078	48.707585
1466.518790	122.543904	48.712589
1463.133654	127.501709	48.717594
1459.751352	120.761808	48.722599
1455.983040	125.501538	48.727604
1452.773882	123.405412	48.732609
1449.093342	123.967194	48.737613
1445.442075	126.645136	48.742618
1442.127051	129.561151	48.747623
1438.376591	129.449732	48.752628
1435.027298	123.660105	48.757633
1431.435527	126.787431	48.762637
1428.193228	119.274730	48.767642
1424.551746	121.991524	48.772647
1420.588064	130.638113	48.777652
1417.478492	120.671484	48.782657
1413.718228	130.948417	48.787661
1410.408558	115.829800	48.792666
1407.178207	119.982573	48.797671
1403.858757	122.481973	48.802676
1400.192316	121.561821	48.807681
1396.755055	115.889383	48.812685
1392.347293	128.753097	48.817690
1389.191682	117.387869	48.822695
1385.577426	125.533903	48.827700
1382.704429	117.189792	48.832705
1379.366337	119.480152	48.837709
1375.819643	122.866869	48.842714
1372.477483	125.106007	48.847719
1368.471955	130.945508	48.852724
1364.874083	125.247541	48.857729
1361.130939	119.173979	48.862733
1357.647301	128.045370	48.867738
1354.734891	122.194056	48.872743
1350.927604	122.934342	48.877748
1347.715033	125.364216	48.882753
1344.040930	121.861231	48.887757
1340.614310	121.465481	48.892762
1336.767469	113.013200	48.897767
1333.201441	122.947667	48.902772
1329.989418	115.557521	48.907777
1326.552952	121.015865	48.912781
1323.141457	116.130948	48.917786
1319.421203	112.939515	48.922791
1315.702372	117.455876	48.927796
1312.660236	121.438674	48.932801
1309.185202	122.594924	48.937805
1305.411239	117.758093	48.942810
1302.035801	116.203826	48.947815
1298.146794	122.418797	48.952820
1294.893645	122.947549	48.957825
1291.471609	120.360625	48.962829
1287.964339	123.090069	48.967834
1284.444874	115.281706	48.972839
1280.455581	119.612508	48.977844
1277.239716	112.419983	48.982849
1274.193482	124.560648	48.987853
1270.852419	124.482137	48.992858
1267.191953	120.286280	48.997863
1263.333553	128.017302	49.002868
1259.655070	115.030652	49.007873
1256.029139	112.571592	49.012877
1253.081517	119.836715	49.017882
1249.412643	113.867998	49.022887
1245.860694	117.041963	49.027892
1242.283947	120.769813	49.032897
1239.178142	123.081271	49.037901
1235.367755	114.456308	49.042906
1231.837859	121.998462	49.047911
1228.622142	126.688457	49.052916
1225.351958	115.272446	49.057921
1221.365241	125.613785	49.062925
1217.567263	116.715248	49.067930
1214.201715	119.415792	49.072935
1210.680122	127.648457	49.077940
1207.324354	111.701129	49.082945
1204.149147	115.576540	49.087949
1200.389764	118.797460	49.092954
1197.057603	116.725406	49.097959
1193.185592	119.822080	49.102964
1189.880794	113.044527	49.107969
1186.370632	119.328775	49.112973
1182.644900	115.677974	49.117978
1179.465548	123.918411	49.122983
1175.847332	119.143959	49.127988
1172.457023	114.501148	49.132993
1169.055078	118.168185	49.137997
1165.153109	123.378191	49.143002
1162.069242	106.623246	49.148007
1157.968715	124.347894	49.153012
1154.666992	108.341163	49.158017
1151.132803	107.482824	49.163021
1147.754607	112.641570	49.168026
1144.647866	112.167033	49.173031
1140.157387	118.509986	49.178036
1137.033524	114.156258	49.183041
1133.563271	111.757599	49.188045
1130.406504	117.275411	49.193050
1127.259002	111.010832	49.198055
1123.530878	110.512947	49.203060
1119.933841	109.240155	49.208065
1116.270084	110.992334	49.213069
1112.574838	112.446217	49.218074
1109.610139	106.497757	49.223079
1105.813113	119.462599	49.228084
1101.935254	105.435357	49.233089
1098.860660	109.356954	49.238093
1095.214847	108.712478	49.243098
1091.814009	90.313312	49.248103
1088.034047	106.075749	49.253108
1084.974396	98.499188	49.258113
1081.327755	106.699130	49.263117
1078.046913	109.235393	49.268122
1074.622319	103.834637	49.273127
1070.711463	113.878783	49.278132
1067.355497	110.100046	49.283137
1063.688890	115.549067	49.288141
1059.964493	105.860021	49.293146
1056.627341	116.517167	49.298151
1053.067074	115.631445	49.303156
1049.698532	109.447481	49.308161
1046.019493	110.230750	49.313165
1042.400192	115.774975	49.318170
1039.205584	109.794525	49.323175
1035.783765	110.488699	49.328180
1032.543516	102.898624	49.333185
1028.656264	116.136555	49.338189
1025.376708	111.915217	49.343194
1021.757539	111.540102	49.348199
1018.184578	122.819007	49.353204
1014.554363	109.241284	49.358209
1011.152713	114.676329	49.363213
1007.470918	112.555476	49.368218
1004.004215	115.346899	49.373223
1000.885004	109.405911	49.378228
997.191846	106.889706	49.383233
993.793647	111.859660	49.388237
990.224777	113.685840	49.393242
986.772234	104.378156	49.398247
983.179564	113.852137	49.403252
979.802944	111.619864	49.408257
976.367281	110.171710	49.413261
972.407439	115.520697	49.418266
968.959900	109.609361	49.423271
965.319520	110.464843	49.428276
962.009921	114.939257	49.433281
958.730891	113.149474	49.438285
955.403090	113.872759	49.443290
951.856579	107.992014	49.448295
948.012529	112.221321	49.453300
944.432684	106.743532	49.458305
941.120976	111.465375	49.463309
937.482075	113.920250	49.468314
934.695583	103.084399	49.473319
930.655367	116.742175	49.478324
927.027705	106.510759	49.483329
923.452473	102.885025	49.488333
919.660022	115.473904	49.493338
916.654876	108.638136	49.498343
913.292349	119.121375	49.503348
909.571363	112.819196	49.508353
906.472035	112.379514	49.513357
902.494677	118.415822	49.518362
899.270108	107.147656	49.523367
895.385554	115.879045	49.528372
891.928103	108.849130	49.533377
888.494658	111.197444	49.538381
885.122015	109.365183	49.543386
881.621312	115.934024	49.548391
877.977403	111.830485	49.553396
874.402476	112.778225	49.558401
871.068315	114.122263	49.563405
867.421301	115.293673	49.568410
864.369857	103.287677	49.573415
860.927343	111.187417	49.578420
856.994205	111.715874	49.583425
853.494165	104.861958	49.588429
849.810586	104.131577	49.593434
846.780237	102.809681	49.598439
842.851554	100.438535	49.603444
839.494161	92.407017	49.608449
835.998017	103.234647	49.613453
832.623692	117.921389	49.618458
829.177421	109.548970	49.623463
825.250174	120.459368	49.628468
821.890749	108.620377	49.633473
818.199512	108.117634	49.638477
815.127860	108.740834	49.643482
811.873770	106.300168	49.648487
807.935731	106.508214	49.653492
804.369310	105.790263	49.658497
800.794847	103.388389	49.663501
797.465419	113.962328	49.668506
793.997889	109.441921	49.673511
790.348325	112.549494	49.678516
787.275169	99.959288	49.683521
784.277105	100.744586	49.688525
780.185523	104.970769	49.693530
776.425664	105.028206	49.698535
772.817921	107.968241	49.703540
769.245266	108.936804	49.708545
765.822497	105.865561	49.713549
762.393603	111.212933	49.718554
759.061059	101.823046	49.723559
755.566750	109.469362	49.728564
751.819291	114.019904	49.733569
748.775920	109.680384	49.738573
744.612733	117.325270	49.743578
741.584253	102.658238	49.748583
737.976690	116.524216	49.753588
734.289429	115.388026	49.758593
730.859419	115.485856	49.763597
727.305386	107.353949	49.768602
723.918128	99.410347	49.773607
720.359511	100.524629	49.778612
716.945688	107.180249	49.783617
713.642871	98.937733	49.788621
709.481137	111.098060	49.793626
706.398476	92.733652	49.798631
703.270998	101.570234	49.803636
699.716311	100.253879	49.808641
695.866908	102.749885	49.813645
692.061269	103.770274	49.818650
689.082938	94.292450	49.823655
685.329478	103.658256	49.828660
681.779468	102.386727	49.833665
678.578559	102.414728	49.838669
674.566342	102.813360	49.843674
671.612535	95.480092	49.848679
667.627972	100.937809	49.853684
664.248164	106.728439	49.858689
661.181953	108.151834	49.863693
657.513223	104.658419	49.868698
653.796050	94.897132	49.873703
650.094014	100.847838	49.878708
646.710557	101.282581	49.883713
643.492119	102.352287	49.888717
639.977540	106.947270	49.893722
636.429547	101.122497	49.898727
632.562191	100.981363	49.903732
628.940902	104.038602	49.908737
625.909148	106.030965	49.913741
622.280581	97.853472	49.918746
618.931845	95.926888	49.923751
615.225849	100.646108	49.928756
611.557181	103.651604	49.933761
608.235612	97.303947	49.938765
604.728644	101.066910	49.943770
601.554198	96.830098	49.948775
598.143863	100.414867	49.953780
594.324770	98.715507	49.958785
591.191457	95.185465	49.963789
587.069063	102.839913	49.968794
583.772645	99.204450	49.973799
579.878267	105.023641	49.978804
576.733788	108.374208	49.983809
573.608770	93.235682	49.988813
569.701213	102.839602	49.993818
566.544565	94.903764	49.998823
562.611784	101.249303	50.003828
559.070623	100.287216	50.008833
555.776619	94.437264	50.013837
552.197904	97.643020	50.018842
549.125681	98.474097	50.023847
545.273956	89.766656	50.028852
541.728051	103.905929	50.033857
538.529586	97.691686	50.038861
534.581931	113.412989	50.043866
531.262547	93.299843	50.048871
527.590737	101.651369	50.053876
524.251063	92.271354	50.058881
520.671902	91.518646	50.063885
516.990306	107.014382	50.068890
513.844574	95.211358	50.073895
510.180975	98.092563	50.078900
506.716002	94.778690	50.083905
503.313972	98.207444	50.088909
499.454692	98.151919	50.093914
496.032028	104.029483	50.098919
493.198677	99.508979	50.103924
489.092637	92.301002	50.108929
485.629000	104.599170	50.113933
482.136507	99.139104	50.118938
478.914053	93.566275	50.123943
475.412854	97.173078	50.128948
471.418383	106.290820	50.133953
468.111753	93.540410	50.138957
464.691577	95.458429	50.143962
461.417478	89.734321	50.148967
457.646231	95.279855	50.153972
454.065421	97.175330	50.158977
450.620115	88.683706	50.163981
446.809504	97.468126	50.168986
443.526652	95.255297	50.173991
440.449118	103.028623	50.178996
436.829269	100.480249	50.184001
433.362484	99.239356	50.189005
429.554738	98.163427	50.194010
425.975289	98.712473	50.199015
422.121201	106.696219	50.204020
419.004196	101.745748	50.209025
416.047975	92.607056	50.214029
412.306747	102.731577	50.219034
408.656187	91.339375	50.224039
405.165644	94.248858	50.229044
401.650164	103.790591	50.234049
398.268484	91.038853	50.239053
394.242696	97.876689	50.244058
391.135193	101.248100	50.249063
387.406623	93.647810	50.254068
384.315395	96.107010	50.259073
380.983744	93.654650	50.264077
377.318180	108.400716	50.269082
373.355834	98.220085	50.274087
370.049437	99.010912	50.279092
366.406557	97.846973	50.284097
363.044864	99.767825	50.289101
359.278663	100.743098	50.294106
355.990500	97.229588	50.299111
352.702709	93.728453	50.304116
349.399885	106.049037	50.309121
345.823892	101.305028	50.314125
342.212727	109.264224	50.319130
338.518969	104.354216	50.324135
334.649762	99.412079	50.329140
331.344188	95.911141	50.334145
328.302746	90.626186	50.339149
324.505703	99.901995	50.344154
321.062688	96.493671	50.349159
317.507216	104.484118	50.354164
313.652849	92.831315	50.359169
310.422564	98.263751	50.364173
307.160717	101.785088	50.369178
303.926545	93.746854	50.374183
300.414150	101.082330	50.379188
296.359466	101.159577	50.384193
292.855357	94.092129	50.389197
289.272040	99.977489	50.394202
285.856379	96.074090	50.399207
282.374883	101.040186	50.404212
279.274295	97.298355	50.409217
275.575012	97.195235	50.414221
271.751796	104.953962	50.419226
268.290407	91.899011	50.424231
265.186930	99.484140	50.429236
261.358490	93.565423	50.434241
257.922726	95.013761	50.439245
254.146423	99.552113	50.444250
251.258625	90.314806	50.449255
247.537261	101.355944	50.454260
243.714038	109.427277	50.459265
240.620833	101.637489	50.464269
236.956180	100.927191	50.469274
233.288946	98.959506	50.474279
230.016171	95.786323	50.479284
226.106296	92.578499	50.484289
222.886757	92.218211	50.489293
219.461092	96.341961	50.494298
216.070295	95.452554	50.499303
212.539520	88.032221	50.504308
208.805758	90.305259	50.509313
205.680489	82.256191	50.514317
202.057064	93.855983	50.519322
198.621599	85.276722	50.524327
194.925547	92.348645	50.529332
191.460699	99.527933	50.534337
188.110345	93.431671	50.539341
184.123185	100.546470	50.544346
181.166921	97.093400	50.549351
177.257734	95.168781	50.554356
173.481621	99.378407	50.559361
170.000733	86.691655	50.564365
166.814341	99.010637	50.569370
163.412742	94.933135	50.574375
160.334235	88.356176	50.579380
156.604569	93.823045	50.584385
153.400106	96.922956	50.589389
149.093225	96.699718	50.594394
145.590262	99.806232	50.599399
142.479027	95.447820	50.604404
138.730575	97.316248	50.609409
135.354355	91.480849	50.614413
131.631314	92.373200	50.619418
128.437501	87.245644	50.624423
124.678682	82.881193	50.629428
121.005915	98.692257	50.634433
117.855646	88.858946	50.639437
114.568544	86.723648	50.644442
111.195353	86.943790	50.649447
107.776973	101.004813	50.654452
103.901017	100.549644	50.659457
100.228653	93.060894	50.664461
96.624571	98.720538	50.669466
93.327729	86.038909	50.674471
89.798294	92.580519	50.679476
86.295821	92.621593	50.684481
82.895107	87.547274	50.689485
78.942128	96.492904	50.694490
75.827123	94.561996	50.699495
72.022845	92.192283	50.704500
68.606766	98.669954	50.709505
65.507878	85.562877	50.714509
61.802016	100.004039	50.719514
58.710830	97.331363	50.724519
55.197842	96.671296	50.729524
51.090507	95.388186	50.734529
47.595451	92.591175	50.739533
44.035151	96.618161	50.744538
40.730579	91.911971	50.749543
37.155560	91.905701	50.754548
33.690654	97.281077	50.759553
30.317147	96.078352	50.764557
26.738113	96.247396	50.769562
23.163705	105.037249	50.774567
19.931833	95.070120	50.779572
16.428601	106.107482	50.784577
12.897594	98.403202	50.789581
9.172834	108.018947	50.794586
5.818153	96.617212	50.799591
2.310266	103.790942	50.804596